Fri Mar 05 19:40:46 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.601107	100.283058	0.000000
-0.055565	82.582489	0.005005
-0.765079	50.029197	0.010010
-2.764109	10.009824	0.015014
-7.198369	7.284178	0.020019
-12.432137	4.465298	0.025024
-17.069184	11.189527	0.030029
-21.411094	7.304315	0.035034
-25.045796	0.704345	0.040038
-29.194545	2.805953	0.045043
-32.845571	0.308654	0.050048
-36.391041	13.032527	0.055053
-39.991151	5.165505	0.060058
-43.753840	9.629316	0.065062
-47.625645	11.987974	0.070067
-51.153130	10.376158	0.075072
-55.179432	17.947620	0.080077
-58.723864	10.278323	0.085082
-62.757627	12.248105	0.090086
-66.394406	14.197140	0.095091
-70.233983	6.913990	0.100096
-74.174964	9.288455	0.105101
-77.773919	11.073778	0.110106
-81.129479	15.061113	0.115110
-84.755641	12.769657	0.120115
-88.774753	4.821327	0.125120
-92.794941	11.005737	0.130125
-96.606445	7.920706	0.135130
-100.344613	8.444641	0.140134
-103.996540	17.653240	0.145139
-107.287312	7.004127	0.150144
-111.649987	13.164364	0.155149
-115.336700	6.572832	0.160154
-119.082562	6.003626	0.165158
-122.963723	14.764704	0.170163
-126.309003	3.665428	0.175168
-130.165213	5.729992	0.180173
-134.044334	0.806059	0.185178
-137.777179	1.015391	0.190182
-142.111618	2.850354	0.195187
-145.617926	-1.197920	0.200192
-149.747145	10.242576	0.205197
-153.468098	2.951678	0.210202
-156.992938	2.810884	0.215206
-161.072387	7.096759	0.220211
-164.087758	4.862502	0.225216
-167.691205	7.285757	0.230221
-171.641502	7.212876	0.235226
-175.141193	1.708073	0.240230
-179.382254	7.945212	0.245235
-182.811054	4.904904	0.250240
-186.890527	6.732375	0.255245
-190.733550	7.481339	0.260250
-194.616879	-6.851423	0.265254
-198.292039	5.778238	0.270259
-201.841069	-1.451708	0.275264
-205.703842	11.414488	0.280269
-209.380229	9.135969	0.285274
-213.328115	6.060276	0.290278
-217.193829	7.888376	0.295283
-220.714912	5.850016	0.300288
-224.279476	11.990306	0.305293
-227.531762	7.852726	0.310298
-231.541337	9.230727	0.315302
-235.611776	10.716218	0.320307
-239.427263	11.260593	0.325312
-243.661110	12.139825	0.330317
-247.326788	2.613617	0.335322
-250.743802	2.834216	0.340326
-254.463730	9.362041	0.345331
-258.174999	1.697610	0.350336
-261.936093	8.165784	0.355341
-265.724353	3.054104	0.360346
-269.557528	4.648437	0.365350
-273.719167	13.222700	0.370355
-276.913294	10.151379	0.375360
-280.752219	12.336423	0.380365
-284.736630	13.701033	0.385370
-288.385033	5.559840	0.390374
-292.573569	12.733375	0.395379
-295.941206	6.332473	0.400384
-299.647120	16.920326	0.405389
-303.449224	4.903920	0.410394
-307.170306	9.273178	0.415398
-311.215396	9.083194	0.420403
-314.662775	12.309646	0.425408
-318.696524	14.961086	0.430413
-322.363509	13.032899	0.435418
-325.811458	17.563587	0.440422
-329.713263	15.108352	0.445427
-333.451987	12.898324	0.450432
-337.625605	15.616278	0.455437
-341.011494	16.481735	0.460442
-344.577973	14.446074	0.465446
-348.803862	14.518404	0.470451
-352.526656	4.976254	0.475456
-356.327284	15.167727	0.480461
-359.813146	9.638916	0.485466
-363.514659	13.812749	0.490470
-367.588949	17.456329	0.495475
-371.194537	15.531030	0.500480
-375.004433	19.682763	0.505485
-378.798439	18.363140	0.510490
-382.313502	11.269970	0.515494
-386.167253	18.437520	0.520499
-389.777117	10.243026	0.525504
-393.963308	13.819361	0.530509
-397.514180	3.830371	0.535514
-401.174527	8.688385	0.540518
-405.234673	11.101334	0.545523
-408.777460	11.446317	0.550528
-412.907252	12.823313	0.555533
-416.559130	9.183460	0.560538
-420.047083	8.013730	0.565542
-424.045436	12.304438	0.570547
-427.681320	10.705759	0.575552
-431.266995	14.282460	0.580557
-434.856816	10.773074	0.585562
-438.588253	5.734602	0.590566
-442.573092	19.891654	0.595571
-446.342198	8.371689	0.600576
-450.451067	11.778079	0.605581
-454.212945	8.078582	0.610586
-457.878011	8.963554	0.615590
-461.421770	11.704137	0.620595
-465.180305	5.873683	0.625600
-468.870842	10.190998	0.630605
-472.862490	6.572379	0.635610
-476.545048	10.183542	0.640614
-480.351743	16.566290	0.645619
-483.796134	3.548484	0.650624
-487.988351	10.967357	0.655629
-491.980008	11.929771	0.660634
-495.287146	11.257970	0.665638
-498.709467	15.751689	0.670643
-502.403345	4.454772	0.675648
-506.510284	14.966620	0.680653
-510.311641	14.577198	0.685658
-513.991085	16.292444	0.690662
-518.282571	18.405068	0.695667
-521.724765	13.397801	0.700672
-525.679843	10.837862	0.705677
-529.261129	4.455660	0.710682
-532.829462	0.698571	0.715686
-536.753432	7.992678	0.720691
-540.119895	8.068422	0.725696
-544.080472	9.773425	0.730701
-548.031501	11.926336	0.735706
-551.621941	3.156576	0.740710
-555.832027	16.384692	0.745715
-559.540261	4.738507	0.750720
-562.904802	12.611917	0.755725
-566.842508	15.079695	0.760730
-570.330980	14.619889	0.765734
-574.297560	15.761359	0.770739
-578.220552	11.184214	0.775744
-582.027157	19.451541	0.780749
-585.869373	16.796404	0.785754
-589.230825	7.517041	0.790758
-593.253392	15.814152	0.795763
-596.690204	3.192703	0.800768
-600.593246	9.906410	0.805773
-604.564708	13.702690	0.810778
-608.133947	7.074263	0.815782
-611.772256	18.123266	0.820787
-615.582206	16.989496	0.825792
-619.486959	11.199999	0.830797
-623.140671	20.300814	0.835802
-627.030278	13.991675	0.840806
-631.049291	19.896072	0.845811
-634.272025	7.089091	0.850816
-638.084883	16.265814	0.855821
-642.075858	10.873326	0.860826
-645.779165	1.618711	0.865830
-650.017180	13.919473	0.870835
-653.373881	6.085498	0.875840
-657.095466	2.933397	0.880845
-660.906426	10.245913	0.885850
-664.810531	11.669283	0.890854
-668.433560	16.681003	0.895859
-671.937656	3.540574	0.900864
-675.657411	8.233448	0.905869
-679.605600	12.120747	0.910874
-683.157868	6.200924	0.915878
-687.334367	5.624152	0.920883
-690.949735	11.014719	0.925888
-694.881187	14.773215	0.930893
-698.498139	5.714617	0.935898
-701.936557	12.010470	0.940902
-706.087700	15.619588	0.945907
-709.520932	9.456858	0.950912
-713.352346	9.626069	0.955917
-717.134131	7.109726	0.960922
-721.262334	7.346877	0.965926
-725.120233	15.069113	0.970931
-728.716362	10.066258	0.975936
-732.284089	8.767815	0.980941
-736.207951	11.503312	0.985946
-739.933285	7.822093	0.990950
-743.828201	14.858000	0.995955
-747.403515	10.974624	1.000960
-750.626578	15.309118	1.005965
-754.573960	17.750365	1.010970
-758.352766	16.219193	1.015974
-762.369776	8.079332	1.020979
-766.369119	0.323008	1.025984
-769.828729	13.262795	1.030989
-774.036496	7.914650	1.035994
-777.372983	11.086185	1.040998
-781.358489	11.253327	1.046003
-784.887757	11.475285	1.051008
-789.083199	13.929428	1.056013
-793.094130	15.180851	1.061018
-796.373254	5.700992	1.066022
-800.017749	14.491508	1.071027
-803.721956	13.440488	1.076032
-807.272192	13.276330	1.081037
-811.261418	20.477229	1.086042
-815.052179	13.840380	1.091046
-818.942754	12.819175	1.096051
-822.456742	7.369684	1.101056
-826.437580	12.371023	1.106061
-830.353365	15.767694	1.111066
-833.971332	11.538038	1.116070
-837.698465	11.176702	1.121075
-841.330576	10.316065	1.126080
-844.957625	4.391105	1.131085
-848.988807	9.558220	1.136090
-852.446974	6.507825	1.141094
-856.302908	9.822430	1.146099
-860.089794	7.893753	1.151104
-863.831844	10.458470	1.156109
-868.088467	18.870712	1.161114
-871.600300	9.737244	1.166118
-875.869029	14.838304	1.171123
-878.847990	6.835472	1.176128
-882.690763	17.119621	1.181133
-886.558617	15.374238	1.186138
-890.058183	14.131370	1.191142
-894.293090	14.215575	1.196147
-897.645735	7.395285	1.201152
-901.295348	14.799069	1.206157
-905.435483	11.417822	1.211162
-909.092377	5.704314	1.216166
-913.075066	11.437784	1.221171
-916.466134	6.039749	1.226176
-920.395595	8.591942	1.231181
-924.280133	19.154065	1.236186
-927.772839	10.296744	1.241190
-931.916600	21.045405	1.246195
-935.306803	13.865327	1.251200
-939.030185	2.469789	1.256205
-942.852888	9.541769	1.261210
-946.808752	12.930845	1.266214
-950.854787	19.729475	1.271219
-954.326436	10.657521	1.276224
-957.756499	4.803744	1.281229
-961.554640	9.769782	1.286234
-965.426329	5.192984	1.291238
-969.420771	5.680413	1.296243
-972.696415	3.856246	1.301248
-976.363344	10.132251	1.306253
-980.503831	7.279467	1.311258
-984.206136	0.198265	1.316262
-988.432700	9.470057	1.321267
-992.083290	1.458095	1.326272
-995.961476	10.570112	1.331277
-999.387611	11.465017	1.336282
-1002.958375	7.759506	1.341286
-1007.344733	16.640581	1.346291
-1010.773630	14.840976	1.351296
-1014.542799	10.088595	1.356301
-1018.489949	6.069573	1.361306
-1021.723693	5.043007	1.366310
-1025.528660	8.540541	1.371315
-1029.186551	8.302476	1.376320
-1033.119579	10.476963	1.381325
-1037.246250	7.816034	1.386330
-1040.523497	7.379914	1.391334
-1044.701621	17.000444	1.396339
-1048.339157	7.540442	1.401344
-1052.180615	7.604581	1.406349
-1055.940550	10.278114	1.411354
-1059.411874	3.811361	1.416358
-1063.325594	12.377243	1.421363
-1066.983196	23.120906	1.426368
-1071.157489	22.131310	1.431373
-1074.910146	20.733663	1.436378
-1078.052718	12.105999	1.441382
-1081.996389	9.453724	1.446387
-1085.670895	3.828476	1.451392
-1089.612213	10.192695	1.456397
-1093.770336	17.608722	1.461402
-1097.257233	13.071518	1.466406
-1100.879783	21.072080	1.471411
-1104.364995	3.272678	1.476416
-1108.194576	1.340200	1.481421
-1112.468766	13.187057	1.486426
-1116.309267	8.613412	1.491430
-1119.764744	9.959456	1.496435
-1123.481981	5.949567	1.501440
-1126.959293	2.787535	1.506445
-1130.985811	11.850954	1.511450
-1134.727885	10.528982	1.516454
-1138.285928	18.943470	1.521459
-1142.356262	16.727870	1.526464
-1146.135709	11.438044	1.531469
-1149.877371	15.054958	1.536474
-1153.429120	-0.089208	1.541478
-1158.111037	9.889648	1.546483
-1161.189369	8.452066	1.551488
-1164.523219	16.739260	1.556493
-1168.551179	12.678234	1.561498
-1172.234855	0.295900	1.566502
-1176.060339	-2.308888	1.571507
-1179.763038	-3.864162	1.576512
-1183.963650	8.857272	1.581517
-1187.917505	10.721542	1.586522
-1191.105300	13.764208	1.591526
-1194.833348	6.085088	1.596531
-1198.532360	7.101215	1.601536
-1202.172902	5.190684	1.606541
-1206.031357	14.821835	1.611546
-1210.422165	10.468866	1.616550
-1214.275783	16.814527	1.621555
-1217.474225	4.015586	1.626560
-1220.873664	-0.885491	1.631565
-1224.677129	8.109271	1.636570
-1228.558503	-0.231215	1.641574
-1232.689257	1.891667	1.646579
-1236.467584	7.525159	1.651584
-1240.023276	13.022108	1.656589
-1244.365513	10.121663	1.661594
-1247.606474	1.847458	1.666598
-1251.324563	2.352644	1.671603
-1255.103386	14.462665	1.676608
-1258.808451	10.217665	1.681613
-1262.534371	13.318160	1.686618
-1266.558356	10.388903	1.691622
-1270.443141	10.383067	1.696627
-1273.897934	13.375536	1.701632
-1277.631846	8.505992	1.706637
-1281.563715	8.332672	1.711642
-1285.304084	5.044252	1.716646
-1289.081990	8.753915	1.721651
-1293.008623	12.172004	1.726656
-1296.597458	16.581535	1.731661
-1300.702462	11.118576	1.736666
-1304.118594	8.044792	1.741670
-1307.616874	12.414614	1.746675
-1311.285649	10.433083	1.751680
-1315.140901	9.250943	1.756685
-1318.812731	14.670405	1.761690
-1322.513190	-1.047323	1.766694
-1326.702235	3.737434	1.771699
-1330.836955	10.615541	1.776704
-1334.182593	8.120287	1.781709
-1337.980588	12.754166	1.786714
-1341.408030	7.602290	1.791718
-1345.631892	11.184734	1.796723
-1349.280512	14.498493	1.801728
-1353.074493	3.979124	1.806733
-1356.758266	20.621924	1.811738
-1360.235786	5.504068	1.816742
-1363.805257	10.303252	1.821747
-1367.972812	12.656188	1.826752
-1371.693531	6.647731	1.831757
-1375.613946	14.291108	1.836762
-1379.283557	3.152646	1.841766
-1383.117723	10.979342	1.846771
-1386.800035	8.438716	1.851776
-1390.410200	5.295203	1.856781
-1394.283342	19.027416	1.861786
-1397.715318	12.088123	1.866790
-1401.745153	14.789647	1.871795
-1405.542910	11.166843	1.876800
-1409.283992	-1.327310	1.881805
-1413.358738	5.355258	1.886810
-1416.701280	2.706670	1.891814
-1420.804129	14.532932	1.896819
-1424.483133	12.308799	1.901824
-1428.111904	8.512325	1.906829
-1431.884671	9.685708	1.911834
-1435.535711	0.939712	1.916838
-1439.471060	9.834500	1.921843
-1443.331704	9.348861	1.926848
-1447.027444	5.441719	1.931853
-1451.079065	5.756207	1.936858
-1454.823878	3.407046	1.941862
-1458.310789	11.507835	1.946867
-1462.285728	13.205638	1.951872
-1465.323082	7.209340	1.956877
-1469.655324	11.873782	1.961882
-1473.093940	5.927555	1.966886
-1477.151763	13.254061	1.971891
-1480.871045	14.838420	1.976896
-1484.550148	14.210241	1.981901
-1488.593691	15.086462	1.986906
-1491.720800	7.122387	1.991910
-1495.905074	8.322347	1.996915
-1499.563694	12.655560	2.006912
-1500.816771	11.646899	2.016909
-1498.362382	13.166097	2.026906
-1495.491572	14.642297	2.036902
-1492.989767	11.587621	2.046899
-1491.083205	8.753001	2.056896
-1489.559020	9.374328	2.066893
-1487.763967	12.058585	2.076890
-1485.958077	13.005855	2.086886
-1483.722613	7.431223	2.096883
-1481.799596	9.164999	2.106880
-1479.796640	5.754431	2.116877
-1478.014677	7.738163	2.126874
-1476.258844	9.080297	2.136870
-1474.272685	6.845573	2.146867
-1472.325790	8.011853	2.156864
-1470.465807	9.103631	2.166861
-1468.658979	4.125013	2.176858
-1466.837020	1.888167	2.186854
-1464.902288	8.232157	2.196851
-1462.790800	1.891086	2.206848
-1460.886542	5.682080	2.216845
-1459.179909	9.919981	2.226842
-1457.209925	9.412061	2.236838
-1455.208839	8.206009	2.246835
-1453.386200	15.000589	2.256832
-1451.659706	8.830115	2.266829
-1449.799077	14.289150	2.276826
-1447.625928	16.218168	2.286822
-1446.403895	9.157422	2.296819
-1444.018742	8.549882	2.306816
-1442.331488	5.878309	2.316813
-1440.111903	8.445684	2.326810
-1438.677011	7.353984	2.336806
-1436.250987	7.300431	2.346803
-1434.602849	4.235656	2.356800
-1432.783927	9.789801	2.366797
-1431.037555	10.552435	2.376794
-1428.886033	5.453922	2.386790
-1426.798795	1.363593	2.396787
-1425.495398	5.621869	2.406784
-1423.903098	10.459152	2.416781
-1421.324116	11.050595	2.426778
-1419.524334	9.268912	2.436774
-1417.701438	9.131941	2.446771
-1415.679576	5.481559	2.456768
-1414.047908	7.022039	2.466765
-1412.066060	10.363289	2.476762
-1410.256380	19.425761	2.486758
-1408.301014	10.479213	2.496755
-1406.649531	7.783393	2.506752
-1404.508968	5.265062	2.516749
-1402.510594	3.333178	2.526746
-1400.838773	10.232473	2.536742
-1399.198666	5.383227	2.546739
-1397.064168	4.920073	2.556736
-1395.214702	5.315705	2.566733
-1393.033893	0.728849	2.576730
-1391.403539	4.704278	2.586726
-1389.595659	-0.152870	2.596723
-1387.794195	5.972525	2.606720
-1385.804030	9.550886	2.616717
-1383.756277	7.746902	2.626714
-1382.085939	11.164889	2.636710
-1380.110873	1.119431	2.646707
-1378.265390	-6.731078	2.656704
-1376.700131	3.343167	2.666701
-1374.603245	4.262889	2.676698
-1372.304573	-7.373826	2.686694
-1370.592165	-2.735734	2.696691
-1368.884974	-6.035704	2.706688
-1367.026204	-4.455756	2.716685
-1364.895007	3.350548	2.726682
-1363.337191	0.524489	2.736678
-1361.422338	3.979139	2.746675
-1359.512150	3.553505	2.756672
-1357.637844	1.347837	2.766669
-1355.594006	8.610772	2.776666
-1353.955579	1.087103	2.786662
-1352.212311	8.208682	2.796659
-1350.060875	0.388161	2.806656
-1348.125870	4.153805	2.816653
-1346.190334	5.939376	2.826650
-1344.666288	3.320840	2.836646
-1342.609727	6.283878	2.846643
-1340.612285	6.025871	2.856640
-1338.813396	12.227512	2.866637
-1337.025592	7.162034	2.876634
-1334.963041	3.682048	2.886630
-1333.383560	2.797794	2.896627
-1331.319243	4.062241	2.906624
-1329.302686	12.987457	2.916621
-1327.662911	10.045670	2.926618
-1325.751762	6.493609	2.936614
-1323.899572	4.343612	2.946611
-1321.842606	8.427652	2.956608
-1320.024180	2.537817	2.966605
-1318.076354	5.905122	2.976602
-1316.141377	4.346614	2.986598
-1314.588227	7.055518	2.996595
-1312.510309	7.728861	3.006592
-1310.675987	10.950131	3.016589
-1309.094276	5.923976	3.026586
-1306.684676	6.425816	3.036582
-1305.165915	13.757053	3.046579
-1303.453560	5.192112	3.056576
-1301.431633	6.654423	3.066573
-1299.330395	7.761412	3.076570
-1297.562193	5.133827	3.086566
-1295.434529	10.292888	3.096563
-1293.586560	1.767829	3.106560
-1292.100320	13.392682	3.116557
-1289.876776	13.968529	3.126554
-1288.264301	16.499011	3.136550
-1286.305331	12.276171	3.146547
-1284.427972	10.755331	3.156544
-1282.413609	13.139393	3.166541
-1280.719343	10.446284	3.176538
-1278.742359	9.662660	3.186534
-1276.430647	16.345964	3.196531
-1274.989566	8.694451	3.206528
-1273.392659	10.654279	3.216525
-1271.215807	9.131309	3.226522
-1269.351093	17.327731	3.236518
-1267.504583	10.366072	3.246515
-1265.598397	9.593789	3.256512
-1263.841250	12.203767	3.266509
-1261.894967	10.662441	3.276506
-1259.847653	10.117050	3.286502
-1258.024439	11.765937	3.296499
-1256.272466	10.148343	3.306496
-1254.426712	11.954678	3.316493
-1252.639730	17.272513	3.326490
-1250.663268	11.831117	3.336486
-1248.715088	16.280004	3.346483
-1247.129090	18.153177	3.356480
-1244.857356	12.928216	3.366477
-1243.048517	15.899411	3.376474
-1241.157121	11.196370	3.386470
-1239.292299	11.341777	3.396467
-1237.645472	11.705227	3.406464
-1235.557614	12.678627	3.416461
-1233.754151	14.215432	3.426458
-1231.765138	20.770426	3.436454
-1229.733938	8.693465	3.446451
-1228.117265	17.027511	3.456448
-1226.203814	11.035692	3.466445
-1224.441905	13.371783	3.476442
-1222.474480	16.172355	3.486438
-1220.520153	13.186623	3.496435
-1218.887670	11.195020	3.506432
-1216.694245	12.881017	3.516429
-1214.895147	11.653807	3.526426
-1213.162918	15.172546	3.536422
-1211.209991	8.408636	3.546419
-1209.361623	18.252986	3.556416
-1207.336996	13.007601	3.566413
-1205.597864	17.231030	3.576410
-1203.755340	10.371106	3.586406
-1201.819629	12.788351	3.596403
-1199.852731	9.581151	3.606400
-1198.116195	10.553957	3.616397
-1196.407881	13.962853	3.626394
-1194.300251	5.574734	3.636390
-1192.469143	12.589236	3.646387
-1190.612559	16.514411	3.656384
-1188.349615	17.575103	3.666381
-1186.617365	16.718609	3.676378
-1185.448289	15.420120	3.686374
-1182.915307	16.016034	3.696371
-1180.942664	9.438465	3.706368
-1179.511606	13.715942	3.716365
-1177.586384	17.906461	3.726362
-1175.411774	14.929730	3.736358
-1173.566785	4.995234	3.746355
-1171.781139	15.287019	3.756352
-1169.936062	13.861434	3.766349
-1167.839286	14.018734	3.776346
-1166.129296	16.727913	3.786342
-1164.287532	16.776017	3.796339
-1162.138537	11.357613	3.806336
-1160.605296	16.506122	3.816333
-1158.674767	14.312139	3.826330
-1156.821447	11.696301	3.836326
-1155.156977	19.980127	3.846323
-1153.103712	20.363876	3.856320
-1151.057607	14.516679	3.866317
-1149.524606	15.335770	3.876314
-1147.196064	20.889157	3.886310
-1145.609810	15.729743	3.896307
-1143.493603	11.522913	3.906304
-1141.584646	10.593972	3.916301
-1140.006926	18.470110	3.926298
-1138.262450	15.991699	3.936294
-1135.915658	13.783246	3.946291
-1134.379351	11.094984	3.956288
-1132.096989	8.721580	3.966285
-1130.766573	13.357820	3.976282
-1128.927960	10.389094	3.986278
-1126.564716	9.212227	3.996275
-1124.648348	8.451061	4.006272
-1123.199245	5.928336	4.016269
-1121.133741	14.245925	4.026266
-1119.088316	11.428859	4.036262
-1117.271012	11.629334	4.046259
-1115.327409	10.202241	4.056256
-1113.695491	14.780787	4.066253
-1111.965437	13.891541	4.076250
-1110.036175	11.061486	4.086246
-1107.923860	13.644771	4.096243
-1105.840894	9.345398	4.106240
-1104.100218	9.659193	4.116237
-1102.611885	15.367557	4.126234
-1100.556262	12.236244	4.136230
-1098.510493	13.068080	4.146227
-1096.742727	12.881759	4.156224
-1094.659668	11.163955	4.166221
-1092.901265	15.450706	4.176218
-1091.079234	6.606251	4.186214
-1089.479491	8.993650	4.196211
-1087.481271	5.018901	4.206208
-1085.348358	11.235220	4.216205
-1083.599692	10.883017	4.226202
-1081.844982	3.858810	4.236198
-1079.577776	8.733655	4.246195
-1078.647367	2.054460	4.256192
-1076.567242	4.005027	4.266189
-1074.251198	9.702591	4.276186
-1072.452736	7.586645	4.286182
-1070.318649	5.058597	4.296179
-1068.769975	5.638392	4.306176
-1066.700902	7.437580	4.316173
-1064.690839	-0.473772	4.326170
-1062.833710	2.999841	4.336166
-1060.187807	11.278339	4.346163
-1058.621233	10.633175	4.356160
-1057.204277	7.750894	4.366157
-1055.546149	12.925291	4.376154
-1053.583398	13.293604	4.386150
-1051.935468	4.603339	4.396147
-1050.045649	5.355951	4.406144
-1047.726486	2.158849	4.416141
-1046.229793	8.440648	4.426138
-1044.314167	2.058623	4.436134
-1042.165690	7.825652	4.446131
-1040.291947	6.215584	4.456128
-1038.664148	6.242745	4.466125
-1036.865295	11.639385	4.476122
-1034.667969	6.039678	4.486118
-1032.736682	1.905154	4.496115
-1031.213182	5.801627	4.506112
-1028.993907	9.954718	4.516109
-1027.350981	11.773150	4.526106
-1025.759710	7.385115	4.536102
-1023.539502	9.043329	4.546099
-1021.414560	2.010477	4.556096
-1019.964836	5.216126	4.566093
-1017.830170	5.583817	4.576090
-1016.097900	8.201125	4.586086
-1013.988668	5.560259	4.596083
-1012.294052	6.516225	4.606080
-1010.501909	10.393435	4.616077
-1008.549159	12.263384	4.626074
-1006.647980	5.348434	4.636070
-1004.723959	4.289300	4.646067
-1002.841481	2.521549	4.656064
-1001.048579	4.224435	4.666061
-999.324020	13.968772	4.676058
-997.420962	9.312999	4.686054
-995.340693	11.820987	4.696051
-993.445873	7.487060	4.706048
-992.183059	7.714727	4.716045
-990.039012	5.597262	4.726042
-988.055542	10.394418	4.736038
-986.325780	13.746361	4.746035
-983.797770	9.483290	4.756032
-982.150566	6.924232	4.766029
-980.603250	8.724829	4.776026
-978.635025	8.664435	4.786022
-976.205984	10.014563	4.796019
-974.102948	7.952617	4.806016
-972.732118	7.760390	4.816013
-971.089026	11.644098	4.826010
-969.063572	9.635615	4.836006
-967.302745	9.191554	4.846003
-965.547773	11.528956	4.856000
-963.374122	8.113623	4.865997
-961.710053	14.706614	4.875994
-959.642770	10.809345	4.885990
-957.754610	12.462298	4.895987
-956.146909	5.316418	4.905984
-954.057969	5.503585	4.915981
-952.361829	7.799877	4.925978
-950.156690	8.481624	4.935974
-948.841811	12.570988	4.945971
-946.668027	14.285648	4.955968
-944.736543	10.632737	4.965965
-942.736569	8.642561	4.975962
-940.724751	15.715228	4.985958
-939.244154	9.066523	4.995955
-937.268680	12.462899	5.005952
-935.405014	6.379788	5.015949
-933.690863	12.399530	5.025946
-931.502696	8.640851	5.035942
-929.665645	8.693052	5.045939
-927.898708	12.065938	5.055936
-925.828457	9.396644	5.065933
-923.933329	12.275353	5.075930
-922.482320	11.527178	5.085926
-920.394129	12.451863	5.095923
-918.423102	14.445283	5.105920
-916.448875	12.861876	5.115917
-914.845729	14.623592	5.125914
-912.786923	8.776139	5.135910
-910.963948	14.623764	5.145907
-909.036251	12.616750	5.155904
-907.181646	13.525109	5.165901
-905.268150	11.056159	5.175898
-903.347133	10.717586	5.185894
-901.767929	6.096296	5.195891
-899.901899	8.240729	5.205888
-897.634992	2.511598	5.215885
-896.047991	13.152751	5.225882
-894.147406	9.653241	5.235878
-892.349892	6.667581	5.245875
-890.403224	5.761234	5.255872
-888.343504	13.832081	5.265869
-886.599550	9.975513	5.275866
-884.592148	7.906829	5.285862
-882.855694	8.134622	5.295859
-880.658038	9.698685	5.305856
-878.880504	5.389912	5.315853
-877.242057	7.097063	5.325850
-875.296841	9.963067	5.335846
-873.391093	7.686433	5.345843
-871.657606	8.959973	5.355840
-869.874958	9.354076	5.365837
-867.818140	8.831191	5.375834
-865.994690	7.568773	5.385830
-864.216534	8.754650	5.395827
-862.087767	7.266584	5.405824
-860.353631	11.464241	5.415821
-858.515783	14.298477	5.425818
-856.187219	8.223209	5.435814
-854.444481	10.546862	5.445811
-852.950144	14.009175	5.455808
-850.926412	6.386326	5.465805
-849.004711	8.690848	5.475802
-847.279322	6.787277	5.485798
-845.256630	4.553551	5.495795
-843.510774	6.055660	5.505792
-841.652174	8.471328	5.515789
-839.969190	13.322969	5.525786
-837.640143	8.248694	5.535782
-835.542996	3.817809	5.545779
-834.049270	-1.274510	5.555776
-832.489353	1.305751	5.565773
-830.319518	13.205369	5.575770
-828.396703	5.699722	5.585766
-826.408005	6.356184	5.595763
-824.664063	5.011769	5.605760
-822.821179	8.345755	5.615757
-820.782357	9.238947	5.625754
-818.853403	14.727077	5.635750
-817.445047	4.339984	5.645747
-815.426428	7.757991	5.655744
-813.296645	14.534026	5.665741
-811.366341	12.013514	5.675738
-809.419663	10.488284	5.685734
-807.791383	10.534476	5.695731
-806.102752	9.952074	5.705728
-803.913007	10.759579	5.715725
-802.202056	18.148889	5.725722
-800.561209	16.465706	5.735718
-798.210784	9.520152	5.745715
-796.276774	7.858010	5.755712
-794.614227	7.764523	5.765709
-792.785300	5.902864	5.775706
-790.910898	10.021313	5.785702
-789.207591	7.167627	5.795699
-787.217438	7.759153	5.805696
-785.443987	4.220048	5.815693
-783.245136	16.301397	5.825690
-781.336150	11.175891	5.835686
-779.340800	11.438172	5.845683
-777.651411	2.907237	5.855680
-775.927511	10.837653	5.865677
-774.159203	12.871492	5.875674
-772.180965	15.913888	5.885670
-770.087169	9.577798	5.895667
-767.939454	6.270994	5.905664
-766.446671	9.923087	5.915661
-764.639628	14.822853	5.925658
-762.947600	7.491506	5.935654
-760.970569	12.623054	5.945651
-758.968158	6.344212	5.955648
-757.056544	16.186755	5.965645
-755.298448	10.764856	5.975642
-753.575683	9.820194	5.985638
-751.375208	6.762341	5.995635
-749.659865	14.687833	6.005632
-747.546694	18.820268	6.015629
-745.911533	10.845911	6.025626
-743.989519	5.222562	6.035622
-742.150957	11.937838	6.045619
-740.138933	11.172748	6.055616
-738.334532	10.811894	6.065613
-736.805533	10.435053	6.075610
-734.920030	13.691249	6.085606
-732.577894	12.511830	6.095603
-730.611175	10.647144	6.105600
-728.748582	16.837540	6.115597
-727.047799	16.589569	6.125594
-725.098609	14.405582	6.135590
-723.342594	9.108775	6.145587
-721.295803	16.261323	6.155584
-719.654948	14.889246	6.165581
-717.658787	11.679336	6.175578
-715.764648	15.777328	6.185574
-714.064651	18.205815	6.195571
-712.053854	7.683025	6.205568
-710.348952	12.573894	6.215565
-708.702864	16.989426	6.225562
-706.429801	15.596860	6.235558
-704.539121	14.134346	6.245555
-702.475647	14.875281	6.255552
-700.678197	11.106610	6.265549
-698.816877	14.966701	6.275546
-697.042694	19.514932	6.285542
-695.406848	22.514213	6.295539
-693.390589	13.973725	6.305536
-691.264707	11.287846	6.315533
-689.571957	12.902769	6.325530
-687.600992	20.326415	6.335526
-685.597356	12.675321	6.345523
-684.122663	15.703518	6.355520
-682.391697	12.359168	6.365517
-680.216872	21.747621	6.375514
-678.064026	12.918477	6.385510
-676.178618	18.840009	6.395507
-674.465931	12.650155	6.405504
-672.828789	16.572931	6.415501
-671.088668	20.461886	6.425498
-668.689181	17.640729	6.435494
-667.080061	17.462710	6.445491
-665.066063	11.783668	6.455488
-663.120794	18.175648	6.465485
-661.646859	16.596597	6.475482
-659.765918	12.454613	6.485478
-657.745348	10.499276	6.495475
-655.887669	14.666302	6.505472
-653.631280	15.371720	6.515469
-651.769305	5.749072	6.525466
-650.127804	17.010138	6.535462
-648.372278	13.987151	6.545459
-646.452118	12.126814	6.555456
-644.486091	19.424971	6.565453
-642.523204	16.787281	6.575450
-640.836272	19.581070	6.585446
-638.893622	13.292918	6.595443
-637.135865	15.716971	6.605440
-635.037145	16.267596	6.615437
-633.142546	17.809260	6.625434
-631.645310	17.064928	6.635430
-629.740450	19.103905	6.645427
-627.548224	8.378506	6.655424
-625.404185	9.292953	6.665421
-623.770699	11.091077	6.675418
-622.260155	17.374125	6.685414
-620.189280	22.391336	6.695411
-618.288567	23.597297	6.705408
-616.363534	16.252498	6.715405
-614.632180	12.454973	6.725402
-612.575731	11.256576	6.735398
-610.599331	14.672038	6.745395
-608.856010	11.287871	6.755392
-606.782636	16.528904	6.765389
-605.174253	18.626318	6.775386
-603.622752	18.471758	6.785382
-601.389414	13.697202	6.795379
-599.267637	21.962103	6.805376
-597.664009	21.573429	6.815373
-595.828597	21.457203	6.825370
-593.747464	15.255910	6.835366
-591.968572	14.842399	6.845363
-590.287809	13.228771	6.855360
-588.083366	12.028858	6.865357
-586.339810	14.887852	6.875354
-584.476743	12.435102	6.885350
-582.610640	11.567139	6.895347
-580.788666	17.385201	6.905344
-578.888108	17.236476	6.915341
-577.104402	17.209051	6.925338
-575.169779	13.458030	6.935334
-573.144849	14.255762	6.945331
-571.064280	10.683538	6.955328
-569.450960	17.029152	6.965325
-567.826470	10.168191	6.975322
-565.776726	5.495628	6.985318
-563.759981	9.081528	6.995315
-561.882845	12.839732	7.005312
-560.004953	13.035697	7.015309
-558.350369	16.065241	7.025306
-556.395259	12.421489	7.035302
-554.516847	11.947898	7.045299
-552.347363	5.628318	7.055296
-551.207612	10.773794	7.065293
-548.897461	16.351272	7.075290
-546.672175	7.982774	7.085286
-544.991044	6.694384	7.095283
-543.253137	4.233237	7.105280
-541.436840	10.879607	7.115277
-539.478215	5.981619	7.125274
-537.492645	3.327760	7.135270
-535.838417	8.556857	7.145267
-533.757097	3.517697	7.155264
-531.783559	6.930525	7.165261
-530.075177	7.671486	7.175258
-528.332043	4.966355	7.185254
-526.053348	12.099413	7.195251
-524.535004	5.822278	7.205248
-522.819738	9.799000	7.215245
-520.830726	10.918305	7.225242
-518.657598	9.758194	7.235238
-517.025998	9.060368	7.245235
-515.006916	6.557490	7.255232
-513.124118	12.634314	7.265229
-511.372508	13.412595	7.275226
-509.536499	4.391036	7.285222
-507.439154	7.672006	7.295219
-505.432239	5.382659	7.305216
-503.765413	10.584506	7.315213
-501.799733	13.063876	7.325210
-500.108686	6.230222	7.335206
-498.218301	10.974788	7.345203
-496.352145	6.971079	7.355200
-494.494229	11.802939	7.365197
-492.698475	14.941038	7.375194
-490.669115	19.568680	7.385190
-488.857949	11.730579	7.395187
-486.592148	13.617291	7.405184
-484.817309	10.483967	7.415181
-483.402310	6.552319	7.425178
-481.327130	8.385793	7.435174
-479.162910	15.564025	7.445171
-477.399086	12.053516	7.455168
-475.558646	4.416017	7.465165
-474.134973	10.861460	7.475162
-471.810712	18.031510	7.485158
-470.124889	13.548194	7.495155
-468.169796	15.614018	7.505152
-466.179954	15.503230	7.515149
-464.601401	12.527583	7.525146
-462.422809	10.651383	7.535142
-460.442568	5.538423	7.545139
-458.495998	9.664573	7.555136
-456.992182	11.819840	7.565133
-455.243749	13.628149	7.575130
-453.103570	17.293912	7.585126
-451.243441	12.321718	7.595123
-449.357158	5.895869	7.605120
-447.209023	5.031920	7.615117
-445.500539	6.057137	7.625114
-443.877670	10.124464	7.635110
-442.053161	6.421131	7.645107
-440.235255	4.147810	7.655104
-438.100127	7.223861	7.665101
-436.311630	6.532615	7.675098
-434.308698	7.005555	7.685094
-432.497133	7.119053	7.695091
-430.261126	6.410036	7.705088
-428.703537	5.092506	7.715085
-427.053404	12.458668	7.725082
-424.915185	12.406327	7.735078
-423.098287	13.250038	7.745075
-421.267771	13.185255	7.755072
-419.279495	11.601589	7.765069
-417.446033	7.153156	7.775066
-415.960586	8.321377	7.785062
-413.842190	9.045900	7.795059
-412.044891	5.362723	7.805056
-409.980967	11.192817	7.815053
-407.999331	7.622315	7.825050
-406.039981	9.561194	7.835046
-404.118739	11.447739	7.845043
-402.540213	12.102157	7.855040
-400.794768	5.998832	7.865037
-398.681404	3.642049	7.875034
-396.768967	14.108476	7.885030
-394.905048	7.060969	7.895027
-393.324251	9.365040	7.905024
-390.831662	8.572460	7.915021
-389.446504	15.693590	7.925018
-387.715419	18.073145	7.935014
-385.639988	10.739239	7.945011
-383.809486	17.639267	7.955008
-381.723661	13.112670	7.965005
-379.978574	14.122617	7.975002
-377.978493	11.597621	7.984998
-376.261704	12.479456	7.994995
-374.439777	15.337151	8.004992
-372.756779	7.175381	8.014989
-370.270587	6.816477	8.024986
-368.639398	9.534101	8.034982
-366.963555	11.093538	8.044979
-364.672794	11.582163	8.054976
-362.896887	8.090332	8.064973
-361.504563	6.031856	8.074970
-359.712070	4.555287	8.084966
-357.477814	10.833502	8.094963
-355.266193	0.991024	8.104960
-353.561137	7.787942	8.114957
-351.922398	7.996988	8.124954
-350.045968	11.266003	8.134950
-348.162096	11.917498	8.144947
-346.197860	9.033511	8.154944
-344.204309	9.792238	8.164941
-342.333715	10.990598	8.174938
-340.523883	16.878693	8.184934
-338.769394	9.395533	8.194931
-336.370952	11.223320	8.204928
-335.121528	14.333496	8.214925
-333.516451	17.873215	8.224922
-331.265531	16.814538	8.234918
-329.257906	13.827320	8.244915
-327.331992	12.793688	8.254912
-325.374517	13.234503	8.264909
-323.516915	18.514983	8.274906
-321.656058	17.671742	8.284902
-320.009365	18.741652	8.294899
-318.135452	11.736812	8.304896
-316.243557	5.848588	8.314893
-314.089869	10.942858	8.324890
-312.311107	11.543266	8.334886
-310.722557	9.758233	8.344883
-308.500683	7.731576	8.354880
-306.970579	12.061707	8.364877
-305.211488	13.056842	8.374874
-303.113095	13.535181	8.384870
-300.813757	10.097208	8.394867
-299.285395	8.580739	8.404864
-297.513127	9.469565	8.414861
-295.748289	15.494352	8.424858
-293.725718	15.310588	8.434854
-291.690458	13.192153	8.444851
-289.661243	16.583674	8.454848
-288.103330	12.365633	8.464845
-286.389926	12.757018	8.474842
-284.184338	15.086171	8.484838
-282.355986	18.757657	8.494835
-280.517959	10.272772	8.504832
-278.715532	6.495712	8.514829
-276.952238	15.241307	8.524826
-274.936695	11.360757	8.534822
-272.899521	11.705209	8.544819
-271.182166	11.336495	8.554816
-269.151735	15.826794	8.564813
-267.327966	11.975282	8.574810
-265.396730	14.100347	8.584807
-263.669420	16.041646	8.594803
-261.497333	15.500883	8.604800
-259.806837	10.470639	8.614797
-258.185118	13.589330	8.624794
-256.227851	17.128154	8.634791
-254.100679	15.835087	8.644787
-252.540627	12.703050	8.654784
-250.411856	11.540785	8.664781
-248.513181	11.627887	8.674778
-246.897122	11.212199	8.684775
-244.668093	15.983457	8.694771
-243.077609	13.730787	8.704768
-241.085923	11.046186	8.714765
-239.523026	12.461108	8.724762
-237.486491	13.367802	8.734759
-235.128932	8.460059	8.744755
-233.485658	8.949517	8.754752
-231.809361	11.186351	8.764749
-229.921103	12.675668	8.774746
-228.036475	14.775044	8.784743
-225.939778	3.657842	8.794739
-224.015811	1.689859	8.804736
-222.249018	3.776466	8.814733
-220.328952	7.799680	8.824730
-218.710084	8.577256	8.834727
-216.709362	7.544404	8.844723
-214.965896	1.989418	8.854720
-212.847672	5.396799	8.864717
-211.172040	7.804281	8.874714
-209.218836	4.996373	8.884711
-207.418261	7.957081	8.894707
-205.423205	5.906714	8.904704
-203.409369	6.258107	8.914701
-201.778696	10.414364	8.924698
-199.663944	4.612238	8.934695
-198.059068	3.554152	8.944691
-196.532619	0.568042	8.954688
-194.097439	-1.290446	8.964685
-192.390537	-0.297952	8.974682
-190.503319	1.150508	8.984679
-188.604775	1.502943	8.994675
-186.469145	0.129638	9.004672
-184.935751	-0.852295	9.014669
-182.965688	-0.269687	9.024666
-181.210224	2.552974	9.034663
-179.309264	4.376622	9.044659
-177.029083	2.399200	9.054656
-175.673980	4.224694	9.064653
-173.942492	7.771193	9.074650
-172.174374	2.695463	9.084647
-170.216055	5.332603	9.094643
-168.124210	5.411049	9.104640
-166.235424	5.005580	9.114637
-164.080592	7.136101	9.124634
-161.952904	8.530423	9.134631
-160.377896	7.800814	9.144627
-158.671290	2.501222	9.154624
-156.591387	4.921603	9.164621
-154.851201	9.227788	9.174618
-152.827559	5.747100	9.184615
-151.212228	2.033144	9.194611
-149.067106	3.216272	9.204608
-147.229383	1.678956	9.214605
-145.298513	5.774720	9.224602
-143.843933	7.792782	9.234599
-141.830435	3.906350	9.244595
-139.792510	0.044444	9.254592
-137.791317	2.562664	9.264589
-136.085732	2.947508	9.274586
-134.240543	0.234264	9.284583
-132.104606	2.184669	9.294579
-130.154301	3.061001	9.304576
-128.570786	1.111098	9.314573
-126.817605	7.246825	9.324570
-124.558050	9.520148	9.334567
-122.907201	9.237940	9.344563
-121.507876	6.556370	9.354560
-119.506826	9.707793	9.364557
-117.160603	14.043631	9.374554
-115.381938	15.094205	9.384551
-113.874880	12.092288	9.394547
-111.746794	15.333978	9.404544
-109.809364	17.669765	9.414541
-107.923040	16.082090	9.424538
-105.397079	9.868638	9.434535
-104.704848	14.427327	9.444531
-102.488127	15.565916	9.454528
-100.250314	16.871671	9.464525
-98.551802	18.833476	9.474522
-96.507839	19.161206	9.484519
-94.531723	18.722911	9.494515
-93.044672	16.788419	9.504512
-91.152752	12.015097	9.514509
-89.639356	12.159055	9.524506
-87.394894	14.820090	9.534503
-85.151087	8.661147	9.544499
-83.223200	13.706397	9.554496
-81.850135	15.669609	9.564493
-79.760471	13.752670	9.574490
-77.925159	18.550589	9.584487
-75.932825	17.396030	9.594483
-74.208717	19.289032	9.604480
-72.188561	15.540539	9.614477
-70.326350	16.749926	9.624474
-68.628358	20.077639	9.634471
-66.732031	17.787340	9.644467
-64.616241	13.655698	9.654464
-62.837666	15.904759	9.664461
-60.965079	17.630398	9.674458
-59.488181	21.774976	9.684455
-57.288744	24.331118	9.694451
-54.293522	15.546511	9.704448
-52.762286	22.606666	9.714445
-51.578283	15.377328	9.724442
-50.063314	22.455870	9.734439
-48.742531	22.714266	9.744435
-46.469496	26.311847	9.754432
-43.900749	18.725821	9.764429
-41.947158	12.876896	9.774426
-40.499132	19.130850	9.784423
-38.647363	15.854512	9.794419
-36.490752	11.012165	9.804416
-35.082513	14.705073	9.814413
-33.118674	16.970394	9.824410
-31.025189	20.291889	9.834407
-29.034626	17.942375	9.844403
-27.030427	7.320078	9.854400
-25.166527	14.328762	9.864397
-23.523049	12.266726	9.874394
-21.733212	11.856626	9.884391
-19.747320	19.262705	9.894387
-17.685091	12.253299	9.904384
-15.952645	17.462416	9.914381
-14.116187	19.384910	9.924378
-12.344656	17.280349	9.934375
-10.240372	12.138472	9.944371
-8.318865	13.679504	9.954368
-6.690190	10.909307	9.964365
-4.838884	11.509425	9.974362
-3.349102	25.462091	9.984359
-2.246903	55.203113	9.994355
-0.581097	111.077886	10.004352
0.000000	149.762237	10.009357
0.959021	180.374280	10.014362
1.228836	222.191859	10.019367
1.908988	240.179157	10.024371
2.594555	268.458511	10.029376
2.837262	282.319313	10.034381
3.216525	296.383854	10.039386
3.430730	315.215131	10.044391
3.522541	319.781678	10.049395
3.636405	329.149765	10.054400
3.645061	335.197748	10.059405
3.882992	329.176808	10.064410
3.914896	336.982570	10.069415
3.666285	329.708263	10.074419
3.805396	340.272410	10.079424
3.603665	343.332461	10.084429
4.015766	339.698093	10.089434
3.878813	341.998745	10.094439
4.042054	345.590372	10.099443
4.037721	350.359925	10.104448
4.065622	356.835364	10.109453
4.087188	345.788392	10.114458
4.131713	354.197711	10.119463
4.197006	353.329489	10.124467
4.181949	355.856710	10.129472
4.276992	371.553102	10.134477
4.595285	385.543875	10.139482
4.596948	384.927079	10.144487
4.380438	375.859328	10.149491
4.570830	378.995615	10.154496
4.798144	384.131939	10.159501
4.453377	379.541203	10.164506
4.806240	392.931946	10.169511
4.735383	401.105801	10.174515
4.792531	408.880767	10.179520
4.772177	402.174002	10.184525
5.017692	393.294325	10.189530
4.724738	408.822404	10.194535
4.767178	410.528314	10.199539
5.052245	404.594444	10.204544
4.983035	405.340430	10.209549
5.193744	407.282857	10.214554
4.888640	409.167207	10.219559
4.919463	416.146842	10.224563
5.295411	411.821195	10.229568
4.845854	419.298509	10.234573
5.131588	409.887270	10.239578
5.065644	420.479452	10.244583
5.242473	417.046599	10.249587
5.320940	418.409288	10.254592
4.982446	424.036429	10.259597
5.598574	437.970285	10.264602
5.519045	449.420962	10.269607
5.621115	460.636095	10.274611
5.651870	459.088961	10.279616
5.601034	459.117641	10.284621
5.782921	459.117086	10.289626
5.588671	463.164742	10.294631
6.086117	467.072110	10.299635
6.327212	462.427326	10.304640
5.574623	472.900404	10.309645
5.895995	461.274077	10.314650
5.832506	475.541880	10.319655
5.787742	473.767087	10.324659
6.192462	470.233215	10.329664
6.031059	477.521092	10.334669
5.945106	470.350083	10.339674
6.111916	484.565392	10.344679
6.131483	475.313262	10.349683
6.191653	478.511344	10.354688
6.051455	490.656146	10.359693
6.352729	488.523373	10.364698
6.318273	483.458896	10.369703
6.234176	488.268026	10.374707
6.132166	483.234826	10.379712
6.403971	503.563191	10.384717
6.607407	493.105282	10.389722
6.603788	510.355134	10.394727
6.721291	511.747876	10.399731
6.868959	505.654526	10.404736
6.580576	509.319806	10.409741
6.921951	503.140364	10.414746
6.989975	516.628695	10.419751
6.804668	508.356999	10.424755
6.886922	513.846100	10.429760
6.560752	518.053589	10.434765
6.872962	515.381311	10.439770
6.635597	515.714140	10.444775
6.828120	521.792012	10.449779
6.860429	524.054656	10.454784
7.017797	543.947154	10.459789
7.281754	541.651587	10.464794
7.071284	559.175771	10.469799
7.447161	558.664865	10.474803
7.303154	559.318707	10.479808
7.093661	551.940274	10.484813
7.425531	546.602874	10.489818
7.353585	553.958524	10.494823
7.529291	562.094719	10.499827
7.737237	559.599918	10.504832
7.474102	564.456554	10.509837
7.615615	556.594765	10.514842
7.410721	564.438419	10.519847
7.465069	564.128613	10.524851
7.757592	574.029775	10.529856
7.693147	592.210397	10.534861
7.946914	595.492747	10.539866
7.839929	600.460111	10.544871
7.781127	596.530194	10.549875
8.158553	598.606911	10.554880
7.996454	599.550655	10.559885
8.144350	600.511190	10.564890
7.837120	609.303203	10.569895
8.100992	603.438867	10.574899
7.919453	601.783648	10.579904
8.033044	611.571444	10.584909
8.076105	603.709563	10.589914
7.999128	621.152602	10.594919
8.274573	637.205299	10.599923
8.310633	636.250256	10.604928
8.370698	640.842470	10.609933
8.523005	646.214787	10.614938
8.474830	650.840038	10.619943
8.438356	643.900758	10.624947
8.421814	640.046092	10.629952
8.442902	644.518363	10.634957
8.588263	640.689915	10.639962
8.673231	653.164805	10.644967
9.257115	665.433967	10.649971
9.142407	668.540131	10.654976
8.832593	660.286630	10.659981
8.814698	662.180396	10.664986
8.504032	673.712271	10.669991
8.599757	678.516437	10.674995
9.048573	682.154066	10.680000
8.705038	688.007625	10.685005
8.879682	681.728541	10.690010
8.797374	692.454424	10.695015
9.081155	706.974583	10.700019
9.218536	716.471638	10.705024
9.433597	727.856621	10.710029
9.619246	714.767764	10.715034
9.609372	727.934387	10.720039
9.375239	727.060283	10.725043
9.673189	726.279515	10.730048
9.482441	732.408357	10.735053
9.372865	732.670343	10.740058
9.809740	733.444439	10.745063
9.781817	732.040682	10.750067
9.296224	733.685766	10.755072
9.482063	740.033678	10.760077
10.098906	731.958778	10.765082
9.713378	744.723265	10.770087
9.567140	737.659516	10.775091
9.705733	747.785631	10.780096
9.652329	771.429106	10.785101
9.833317	775.264026	10.790106
10.066441	769.145897	10.795111
9.947913	773.109018	10.800115
10.159109	771.859514	10.805120
10.163226	779.854459	10.810125
10.354017	771.303418	10.815130
9.897609	776.805991	10.820135
10.096058	793.637577	10.825139
10.632368	799.096943	10.830144
10.463560	810.199426	10.835149
10.930654	814.507566	10.840154
10.708615	813.800270	10.845159
10.757216	820.968085	10.850163
10.916231	808.785454	10.855168
10.553753	790.319542	10.860173
10.714832	791.036701	10.865178
10.461411	805.824001	10.870183
10.672003	814.120362	10.875187
10.988971	809.185810	10.880192
10.867541	816.309776	10.885197
10.887726	813.520012	10.890202
10.620532	812.189105	10.895207
10.692886	822.819449	10.900211
11.034762	820.828394	10.905216
10.795137	830.738912	10.910221
11.062860	810.418797	10.915226
10.708246	836.750372	10.920231
10.761397	843.188883	10.925235
10.986782	847.565549	10.930240
10.986764	850.729156	10.935245
11.085615	848.335290	10.940250
11.074815	861.672502	10.945255
11.258721	874.650646	10.950259
12.169318	891.228401	10.955264
11.556054	887.809488	10.960269
11.780043	880.743391	10.965274
11.520568	888.673199	10.970279
11.593879	894.154407	10.975283
12.111105	891.551870	10.980288
11.913785	891.607069	10.985293
11.864749	886.439116	10.990298
11.849697	898.819777	10.995303
11.967744	914.191370	11.000307
12.460252	915.754588	11.005312
12.054894	915.402973	11.010317
12.044939	894.171343	11.015322
12.089456	905.063244	11.020327
12.123877	921.388100	11.025331
12.686838	911.135915	11.030336
12.264241	904.849487	11.035341
12.257884	897.892665	11.040346
12.066613	910.973263	11.045351
12.468911	913.602756	11.050355
12.404046	920.090088	11.055360
12.540736	926.941113	11.060365
12.763522	929.096164	11.065370
12.796905	930.967592	11.070375
12.512192	930.284480	11.075379
12.678381	936.823281	11.080384
12.477057	935.544938	11.085389
12.797425	929.163653	11.090394
12.654894	926.339893	11.095399
12.420476	935.752882	11.100403
12.740759	936.897268	11.105408
12.725606	935.869945	11.110413
12.684113	937.765934	11.115418
12.942532	934.014000	11.120423
12.883224	940.710202	11.125427
12.931410	938.646120	11.130432
12.872946	944.063205	11.135437
13.131206	954.115180	11.140442
12.901787	960.884258	11.145447
13.162131	970.243589	11.150451
13.467148	963.699147	11.155456
13.182550	971.468994	11.160461
13.307146	969.522038	11.165466
13.063419	970.847855	11.170471
12.824570	970.945949	11.175475
12.990133	975.967747	11.180480
13.210938	981.125824	11.185485
13.859004	1002.208632	11.190490
13.839504	1001.603071	11.195495
14.095058	998.498169	11.200499
14.078085	975.570632	11.205504
13.708491	985.132955	11.210509
13.907472	974.044592	11.215514
13.743545	974.048730	11.220519
13.624695	980.959464	11.225523
13.956889	991.184188	11.230528
13.845917	1005.884311	11.235533
14.033030	1009.078033	11.240538
14.101807	1011.569917	11.245543
13.997395	1013.863906	11.250547
14.361586	1011.364610	11.255552
14.045336	1014.075611	11.260557
14.110290	1007.564709	11.265562
14.015364	1018.911048	11.270567
14.211533	1015.782497	11.275571
14.431592	1019.608096	11.280576
13.981344	1020.687718	11.285581
14.711591	1014.658941	11.290586
14.452022	1015.324925	11.295591
14.402258	1016.189273	11.300595
14.630766	1008.447415	11.305600
14.331105	1016.844201	11.310605
14.856647	1025.082564	11.315610
14.960312	1033.892878	11.320615
14.501878	1023.947037	11.325619
14.866188	1031.132414	11.330624
14.659316	1043.187378	11.335629
15.090521	1039.018326	11.340634
14.806775	1040.560280	11.345639
14.969935	1034.432697	11.350643
15.274697	1029.514212	11.355648
15.105141	1042.974688	11.360653
14.867762	1035.909559	11.365658
15.559149	1039.450240	11.370663
14.958146	1034.690413	11.375667
15.500169	1035.222238	11.380672
14.951150	1046.631564	11.385677
15.382453	1038.617632	11.390682
15.408602	1037.888086	11.395687
14.827975	1041.708926	11.400691
15.385228	1041.356748	11.405696
15.249893	1042.419261	11.410701
15.694431	1052.572491	11.415706
15.521583	1058.692305	11.420711
15.731085	1060.023116	11.425715
15.980012	1066.963546	11.430720
15.461370	1066.866554	11.435725
15.924803	1060.721031	11.440730
16.015545	1071.851706	11.445735
16.220292	1072.990875	11.450739
16.096112	1050.987128	11.455744
15.887834	1045.443944	11.460749
15.813925	1044.670429	11.465754
16.133811	1064.922522	11.470759
16.300374	1063.505060	11.475763
16.467282	1062.797220	11.480768
16.123743	1052.599628	11.485773
15.894433	1044.402458	11.490778
16.070291	1064.653867	11.495783
15.847827	1076.905324	11.500787
16.237326	1069.355390	11.505792
16.152824	1074.770368	11.510797
16.368438	1080.404004	11.515802
16.299880	1080.153217	11.520807
16.128527	1085.239830	11.525811
16.432911	1091.993218	11.530816
16.495107	1095.826669	11.535821
16.841954	1102.355655	11.540826
16.932169	1099.491584	11.545831
16.842308	1110.558047	11.550835
17.142725	1098.666457	11.555840
16.464691	1098.415102	11.560845
16.542968	1103.775741	11.565850
16.948853	1100.992217	11.570855
17.004956	1106.660767	11.575859
16.947607	1105.454069	11.580864
17.080478	1114.400132	11.585869
16.859962	1108.903034	11.590874
17.410895	1118.138836	11.595879
17.083834	1112.560952	11.600883
17.458986	1097.164246	11.605888
17.369269	1103.081572	11.610893
17.236077	1100.894998	11.615898
17.080771	1111.254337	11.620903
17.340107	1111.058492	11.625907
17.390506	1101.944559	11.630912
17.195786	1111.609968	11.635917
17.442456	1103.480359	11.640922
17.457854	1106.712531	11.645927
17.316353	1129.443326	11.650931
17.720060	1137.360540	11.655936
17.872382	1135.330287	11.660941
17.808663	1138.843186	11.665946
17.964526	1141.311740	11.670951
17.800674	1142.426121	11.675955
17.973019	1138.415031	11.680960
17.944375	1140.567636	11.685965
18.271487	1143.713826	11.690970
18.251837	1137.169047	11.695975
18.031672	1145.933301	11.700979
18.223655	1135.593463	11.705984
18.311051	1141.933597	11.710989
18.457243	1138.095425	11.715994
18.366889	1131.413682	11.720999
17.912773	1127.237567	11.726003
18.266993	1132.464312	11.731008
18.001227	1142.508529	11.736013
18.394960	1135.951439	11.741018
18.323637	1134.956717	11.746023
18.349453	1143.363168	11.751027
18.639346	1140.025663	11.756032
18.515739	1150.438324	11.761037
18.573088	1150.520718	11.766042
18.472184	1152.427787	11.771047
18.479080	1153.745187	11.776051
18.530706	1148.938005	11.781056
18.532770	1157.578505	11.786061
18.834198	1166.352626	11.791066
19.067174	1169.113260	11.796071
18.783141	1171.077928	11.801075
19.098324	1160.245301	11.806080
18.712205	1181.264645	11.811085
18.839043	1177.161448	11.816090
18.888243	1171.097719	11.821095
18.779674	1171.055178	11.826099
18.983830	1169.396726	11.831104
18.740901	1184.291553	11.836109
19.173564	1203.825633	11.841114
19.580377	1202.112776	11.846119
19.185229	1199.821301	11.851123
19.489056	1197.566586	11.856128
19.605197	1194.876571	11.861133
19.741726	1192.120221	11.866138
19.554835	1193.616778	11.871143
19.681407	1192.383892	11.876147
20.056714	1195.257458	11.881152
19.541135	1205.291096	11.886157
19.718522	1201.041047	11.891162
19.748259	1196.109597	11.896167
19.736068	1210.321049	11.901171
20.120195	1202.297205	11.906176
19.942329	1208.611862	11.911181
19.880421	1200.749053	11.916186
19.930285	1202.310359	11.921191
19.964312	1204.441937	11.926195
19.736005	1192.248217	11.931200
19.560314	1206.365885	11.936205
19.495317	1200.717781	11.941210
20.118309	1206.822696	11.946215
20.148029	1226.575628	11.951219
20.391639	1230.488998	11.956224
20.440987	1227.901100	11.961229
20.460218	1217.927828	11.966234
20.829784	1223.338254	11.971239
20.683329	1227.679719	11.976243
20.842806	1219.745316	11.981248
20.657474	1209.014562	11.986253
20.582807	1203.221331	11.991258
20.613936	1203.579164	11.996263
20.467477	1215.323413	12.001267
20.498987	1216.337249	12.006272
20.603091	1217.091905	12.011277
20.919624	1210.384656	12.016282
21.180429	1220.303937	12.021287
20.571110	1223.173691	12.026291
20.926258	1213.441758	12.031296
20.874423	1214.975128	12.036301
20.910904	1219.553939	12.041306
21.037988	1217.546625	12.046311
20.912936	1220.282365	12.051315
20.729300	1213.145494	12.056320
20.945414	1213.101632	12.061325
20.644216	1207.778226	12.066330
20.894315	1205.560467	12.071335
20.747737	1224.882587	12.076339
20.823315	1209.677058	12.081344
20.895775	1218.923003	12.086349
20.689565	1217.631219	12.091354
20.810034	1204.687947	12.096359
20.577853	1220.554152	12.101363
20.844285	1224.411837	12.106368
20.992924	1229.199861	12.111373
20.948970	1220.025203	12.116378
20.815944	1206.485222	12.121383
20.387225	1208.201715	12.126387
20.994171	1206.567332	12.131392
20.901942	1217.520705	12.136397
20.800158	1214.592610	12.141402
21.002961	1200.194763	12.146407
20.517425	1202.923336	12.151411
20.759123	1197.404525	12.156416
20.770628	1220.098442	12.161421
20.841395	1218.346134	12.166426
21.007171	1219.362211	12.171431
20.870078	1219.382570	12.176435
20.766214	1208.509503	12.181440
20.774288	1206.809776	12.186445
20.406703	1207.136578	12.191450
20.917322	1223.228114	12.196455
21.090749	1231.145836	12.201459
20.966033	1213.644483	12.206464
20.628530	1209.079131	12.211469
20.736743	1201.141876	12.216474
21.180126	1204.443013	12.221479
20.766926	1209.768530	12.226483
20.985398	1198.754165	12.231488
20.826018	1202.951016	12.236493
20.769173	1215.773885	12.241498
20.952783	1208.263027	12.246503
20.950412	1207.594797	12.251507
21.032951	1205.268134	12.256512
20.784189	1212.967733	12.261517
20.952645	1207.457447	12.266522
21.177256	1206.869717	12.271527
20.722127	1211.610520	12.276531
20.977298	1199.241902	12.281536
21.126801	1205.187352	12.286541
20.923651	1215.287870	12.291546
21.012564	1210.701819	12.296551
21.121146	1207.137730	12.301555
21.057029	1181.659372	12.306560
20.729627	1187.682457	12.311565
20.753541	1185.409306	12.316570
21.006032	1177.100519	12.321575
20.733988	1174.456650	12.326579
20.884218	1170.668292	12.331584
20.943143	1179.462175	12.336589
20.897582	1175.187764	12.341594
20.935187	1173.131644	12.346599
20.966469	1180.654086	12.351603
20.934625	1175.324004	12.356608
21.125142	1188.172055	12.361613
20.519665	1179.057020	12.366618
20.813113	1175.271051	12.371623
21.039967	1184.847190	12.376627
20.900616	1175.957455	12.381632
21.060067	1174.227280	12.386637
20.858635	1180.492064	12.391642
20.842434	1183.517965	12.396647
20.461718	1185.245723	12.401651
20.815195	1184.210054	12.406656
20.665704	1193.150736	12.411661
20.369770	1184.785902	12.416666
20.693274	1182.310415	12.421671
20.443387	1183.085258	12.426675
20.653407	1181.176693	12.431680
20.590822	1191.600153	12.436685
20.670086	1191.770522	12.441690
21.233143	1187.591438	12.446695
20.797721	1189.599179	12.451699
20.980244	1187.433204	12.456704
20.758490	1183.801951	12.461709
21.028247	1183.855198	12.466714
21.461945	1183.336630	12.471719
20.899942	1189.725164	12.476723
21.004257	1192.626182	12.481728
21.007693	1184.391809	12.486733
20.757430	1194.365776	12.491738
20.788686	1187.133137	12.496743
20.762154	1203.345020	12.501747
21.201031	1194.978108	12.506752
21.118742	1198.266884	12.511757
20.773240	1197.191299	12.516762
20.947202	1178.405925	12.521767
20.553191	1181.783843	12.526771
20.790439	1173.144727	12.531776
20.783046	1177.618550	12.536781
20.795910	1176.060000	12.541786
20.769050	1176.740918	12.546791
20.454558	1179.230878	12.551795
20.842260	1192.918027	12.556800
20.851725	1195.277467	12.561805
20.618340	1199.405689	12.566810
21.020347	1190.185155	12.571815
20.855771	1197.324074	12.576819
20.816300	1198.617332	12.581824
20.738140	1199.350592	12.586829
20.817981	1201.110559	12.591834
20.927069	1194.314969	12.596839
20.715538	1192.454713	12.601843
20.921132	1193.554330	12.606848
20.572245	1184.045103	12.611853
20.604833	1203.152523	12.616858
21.123360	1203.563515	12.621863
20.892918	1199.533067	12.626867
21.051857	1192.414112	12.631872
20.916729	1183.291869	12.636877
20.958376	1180.041261	12.641882
20.840825	1180.042732	12.646887
20.658087	1183.875846	12.651891
20.557905	1180.986929	12.656896
20.804946	1174.770209	12.661901
20.749673	1170.416918	12.666906
20.879876	1173.547209	12.671911
20.532530	1183.896225	12.676915
20.962315	1173.275562	12.681920
20.771246	1188.498038	12.686925
20.692838	1184.675175	12.691930
21.046351	1179.886070	12.696935
20.908410	1179.957030	12.701939
20.896285	1182.971242	12.706944
21.034332	1179.148552	12.711949
20.773255	1189.479081	12.716954
20.687975	1184.971287	12.721959
20.852659	1188.875155	12.726963
20.861045	1185.470566	12.731968
20.524458	1185.682028	12.736973
20.492225	1185.873334	12.741978
20.981233	1182.923562	12.746983
20.520195	1189.221870	12.751987
21.114430	1188.354398	12.756992
20.707735	1191.221792	12.761997
20.477548	1188.039772	12.767002
20.839646	1191.202471	12.772007
20.616775	1196.661643	12.777011
20.958786	1205.601216	12.782016
21.259812	1203.897346	12.787021
20.881535	1200.696362	12.792026
21.089866	1187.786403	12.797031
20.796279	1193.122801	12.802035
20.816620	1185.168028	12.807040
21.047123	1196.612424	12.812045
20.962036	1195.509497	12.817050
20.669540	1185.633279	12.822055
20.665417	1201.180792	12.827059
20.766208	1197.091206	12.832064
20.853366	1195.164385	12.837069
20.722771	1193.969362	12.842074
20.784602	1193.428097	12.847079
20.594527	1193.581496	12.852083
20.841107	1189.296758	12.857088
20.898267	1189.667786	12.862093
20.651487	1193.131042	12.867098
21.140089	1195.729476	12.872103
20.945728	1198.678132	12.877107
21.016884	1193.870974	12.882112
21.095749	1202.043477	12.887117
20.991872	1198.587399	12.892122
21.109139	1199.125473	12.897127
21.177076	1200.429988	12.902131
21.138283	1194.531683	12.907136
20.900248	1177.346514	12.912141
20.554568	1169.142599	12.917146
20.940351	1170.942082	12.922151
20.792944	1175.493434	12.927155
20.558006	1174.576848	12.932160
20.643249	1181.715341	12.937165
20.806136	1194.506299	12.942170
21.014865	1194.555086	12.947175
20.966803	1179.274684	12.952179
20.723423	1175.121718	12.957184
20.451771	1176.816309	12.962189
20.586076	1187.293525	12.967194
20.933840	1192.448777	12.972199
20.678855	1205.877294	12.977203
20.906559	1204.300245	12.982208
20.962056	1201.026921	12.987213
20.742864	1208.308608	12.992218
20.776482	1190.100733	12.997223
20.596256	1211.087282	13.002227
20.791275	1202.317678	13.007232
21.151275	1208.661675	13.012237
20.729043	1201.780501	13.017242
20.740810	1196.952849	13.022247
20.729534	1218.406086	13.027251
21.143020	1210.289238	13.032256
20.997406	1183.765658	13.037261
20.503559	1180.592573	13.042266
20.686422	1169.281112	13.047271
20.943005	1190.527570	13.052275
20.697854	1180.426167	13.057280
21.026432	1175.197883	13.062285
20.649558	1183.433602	13.067290
20.753427	1169.748631	13.072295
20.542290	1185.786496	13.077299
20.721355	1188.860107	13.082304
21.197162	1208.379428	13.087309
20.812211	1191.864275	13.092314
20.783765	1182.619353	13.097319
20.662691	1179.326884	13.102323
20.771945	1187.073454	13.107328
20.726478	1201.151422	13.112333
20.889993	1201.895025	13.117338
20.967103	1192.999142	13.122343
20.636229	1191.952766	13.127347
20.738728	1181.575124	13.132352
20.735363	1207.072271	13.137357
20.569003	1213.214772	13.142362
21.140766	1208.174788	13.147367
20.975765	1214.722380	13.152371
20.809519	1199.732063	13.157376
20.888229	1192.110202	13.162381
20.807465	1186.925123	13.167386
20.920177	1180.802371	13.172391
20.780967	1195.125537	13.177395
20.801718	1185.316060	13.182400
20.875634	1186.190656	13.187405
20.783058	1186.572950	13.192410
21.244663	1190.621864	13.197415
20.637960	1185.829777	13.202419
20.909340	1183.422533	13.207424
21.222048	1193.609505	13.212429
21.006525	1186.701677	13.217434
21.085273	1183.954545	13.222439
20.645636	1184.950476	13.227443
20.703219	1189.612651	13.232448
20.943925	1185.596954	13.237453
20.758183	1189.050473	13.242458
20.875247	1196.059309	13.247463
20.957727	1199.987331	13.252467
20.972977	1187.415698	13.257472
21.073638	1194.619552	13.262477
20.862796	1191.716742	13.267482
21.047128	1184.344563	13.272487
20.755236	1190.813028	13.277491
20.824809	1185.938310	13.282496
20.730935	1171.026373	13.287501
20.802682	1185.050935	13.292506
21.019934	1173.418572	13.297511
20.677973	1164.512270	13.302515
20.608996	1166.127222	13.307520
21.000604	1183.759569	13.312525
20.659706	1184.339177	13.317530
20.818478	1188.568865	13.322535
20.740195	1188.254967	13.327539
20.655085	1192.119824	13.332544
20.883642	1186.784477	13.337549
20.766836	1188.123187	13.342554
20.845869	1188.642125	13.347559
20.667537	1196.896652	13.352563
21.041438	1188.341395	13.357568
20.902767	1191.984542	13.362573
21.133287	1175.046366	13.367578
21.119818	1168.998942	13.372583
20.218491	1171.681854	13.377587
20.328337	1168.667970	13.382592
20.797914	1177.896286	13.387597
21.130588	1189.887395	13.392602
20.935219	1177.101763	13.397607
20.891228	1177.846919	13.402611
20.990763	1164.564797	13.407616
20.899172	1169.618215	13.412621
20.524048	1167.806134	13.417626
20.803174	1158.594179	13.422631
20.911938	1170.781846	13.427635
20.881078	1163.961279	13.432640
20.953315	1156.283694	13.437645
20.697097	1166.649704	13.442650
20.700097	1168.939202	13.447655
20.652579	1159.000272	13.452659
20.918220	1162.823372	13.457664
20.615986	1159.070910	13.462669
20.413169	1161.270222	13.467674
20.967829	1179.676133	13.472679
20.972364	1199.366808	13.477683
20.550246	1179.985745	13.482688
20.782682	1182.334853	13.487693
20.868613	1199.528658	13.492698
21.076687	1185.775008	13.497703
20.722048	1173.883748	13.502707
20.559834	1174.977368	13.507712
20.816967	1179.361689	13.512717
20.809364	1194.018705	13.517722
20.854051	1193.560605	13.522727
20.732824	1188.035023	13.527731
21.156192	1190.836263	13.532736
20.752532	1179.242999	13.537741
20.731042	1171.786951	13.542746
20.829600	1169.848854	13.547751
20.675653	1168.280637	13.552755
20.589061	1175.623166	13.557760
20.942966	1178.870754	13.562765
20.722741	1188.951898	13.567770
21.161207	1182.439696	13.572775
20.587983	1177.475102	13.577779
20.470984	1174.174099	13.582784
20.840749	1189.146264	13.587789
21.073255	1200.021019	13.592794
20.759491	1181.680889	13.597799
21.037212	1185.696048	13.602803
20.788082	1177.924617	13.607808
20.783954	1181.150458	13.612813
20.525937	1174.515938	13.617818
20.742913	1175.631087	13.622823
20.599145	1178.366650	13.627827
20.801179	1198.423246	13.632832
21.016208	1201.256140	13.637837
20.741729	1204.767975	13.642842
20.944636	1206.240211	13.647847
20.467590	1194.873122	13.652851
20.811434	1202.266869	13.657856
20.674639	1205.534376	13.662861
20.451224	1211.818450	13.667866
21.393186	1209.326326	13.672871
20.723631	1207.293097	13.677875
21.256767	1208.994960	13.682880
21.224241	1193.601670	13.687885
20.944007	1186.104876	13.692890
20.761432	1174.895854	13.697895
20.499442	1177.979881	13.702899
20.783846	1181.730602	13.707904
20.604676	1176.458712	13.712909
20.352799	1180.249232	13.717914
20.785353	1185.159128	13.722919
20.912467	1202.833683	13.727923
20.767371	1207.581811	13.732928
21.320158	1204.167664	13.737933
20.996804	1194.192275	13.742938
20.901260	1180.576948	13.747943
20.751018	1184.491618	13.752947
20.780957	1185.418963	13.757952
20.886461	1177.887459	13.762957
20.508515	1175.419766	13.767962
20.855398	1169.578238	13.772967
20.904461	1183.450286	13.777971
20.756220	1194.196516	13.782976
20.880731	1175.128852	13.787981
20.847159	1181.046718	13.792986
20.966148	1170.344731	13.797991
20.814567	1178.754264	13.802995
20.805034	1176.607884	13.808000
20.718361	1174.210437	13.813005
20.306381	1181.388808	13.818010
20.667613	1176.000763	13.823015
20.848523	1187.374207	13.828019
20.907607	1187.297040	13.833024
21.047064	1185.037002	13.838029
20.677940	1181.530187	13.843034
20.985166	1175.362220	13.848039
20.687083	1178.882544	13.853043
20.949831	1178.459056	13.858048
20.809297	1178.760683	13.863053
20.567086	1177.767981	13.868058
20.987794	1183.365791	13.873063
20.656384	1190.529739	13.878067
20.726391	1186.230584	13.883072
21.185762	1183.799664	13.888077
20.428602	1191.209727	13.893082
20.656582	1176.885164	13.898087
20.659857	1177.525003	13.903091
20.776210	1181.912854	13.908096
21.002629	1173.652385	13.913101
20.774264	1191.134446	13.918106
20.960737	1184.217700	13.923111
20.810345	1185.892952	13.928115
20.888470	1187.788820	13.933120
20.803736	1182.452977	13.938125
20.790964	1190.146466	13.943130
21.118998	1179.576723	13.948135
20.869999	1181.469567	13.953139
20.961962	1182.125225	13.958144
20.954879	1191.062117	13.963149
20.713343	1192.745598	13.968154
20.951119	1187.005050	13.973159
20.820481	1196.970978	13.978163
20.765058	1196.543039	13.983168
20.999034	1189.162940	13.988173
20.849783	1178.013261	13.993178
20.826635	1186.630990	13.998183
20.757988	1190.210924	14.003187
20.836060	1187.255725	14.008192
21.243996	1181.881240	14.013210
21.127320	1185.933217	14.018227
20.936902	1177.506950	14.023245
21.176038	1177.413823	14.028263
20.849619	1170.901627	14.033280
20.798168	1153.606394	14.038298
20.694076	1160.728515	14.043315
20.890884	1165.737237	14.048333
21.048031	1173.037924	14.053351
21.034824	1178.964200	14.058368
21.248140	1177.409110	14.063386
20.755264	1167.305456	14.068403
20.922981	1180.728335	14.073421
20.973848	1179.347021	14.078439
21.045573	1184.487386	14.083456
21.178837	1181.243025	14.088474
21.091884	1188.222425	14.093491
21.181511	1178.537097	14.098509
21.174075	1190.476222	14.103527
21.120681	1183.502043	14.108544
21.264216	1176.993543	14.113562
20.864717	1181.595576	14.118579
20.795702	1177.384593	14.123597
20.993388	1185.982878	14.128615
21.131801	1182.314545	14.133632
21.218267	1186.027378	14.138650
21.041484	1192.604249	14.143667
21.274869	1182.778011	14.148685
21.004962	1193.945735	14.153703
20.902333	1187.783236	14.158720
21.334627	1187.719077	14.163738
21.054401	1187.464964	14.168755
21.279824	1190.932261	14.173773
21.396946	1203.535807	14.178791
21.419986	1208.654057	14.183808
21.463697	1202.128433	14.188826
21.349915	1209.173471	14.193843
21.505306	1216.677384	14.198861
21.743313	1228.133791	14.203879
21.640263	1218.919623	14.208896
21.402463	1202.344623	14.213914
21.449247	1201.001712	14.218931
21.498603	1196.990497	14.223949
21.788309	1207.593915	14.228967
21.426777	1203.860595	14.233984
21.641930	1209.360344	14.239002
21.407055	1220.329016	14.244019
21.479078	1228.706692	14.249037
21.670907	1224.045098	14.254055
21.381518	1229.063746	14.259072
21.873713	1231.709844	14.264090
21.966996	1239.851323	14.269107
21.676638	1237.728462	14.274125
21.648139	1234.849670	14.279143
21.592078	1234.375754	14.284160
21.865119	1229.646149	14.289178
21.489799	1235.734024	14.294195
21.849372	1235.173368	14.299213
21.765067	1233.220567	14.304231
21.593517	1241.707887	14.309248
21.772746	1226.620523	14.314266
21.863625	1229.796252	14.319283
21.567041	1239.566675	14.324301
21.540114	1242.913782	14.329319
21.384661	1238.079480	14.334336
21.793075	1249.604682	14.339354
21.723369	1258.736452	14.344371
22.153007	1263.931446	14.349389
21.980202	1264.479761	14.354407
21.899163	1266.188513	14.359424
21.959504	1266.440087	14.364442
21.938945	1261.368754	14.369459
22.112530	1259.753924	14.374477
22.252053	1255.635502	14.379495
21.961556	1270.940562	14.384512
22.131601	1262.390685	14.389530
21.993344	1264.706324	14.394547
21.698354	1274.520562	14.399565
21.859906	1264.081222	14.404583
21.925895	1277.913680	14.409600
22.092636	1281.749017	14.414618
22.361118	1287.617824	14.419635
22.705389	1297.946758	14.424653
22.813495	1291.009692	14.429671
22.404461	1273.156282	14.434688
22.456789	1267.102745	14.439706
22.308046	1270.547941	14.444723
22.249664	1271.131489	14.449741
22.778960	1271.679509	14.454759
22.465771	1270.941430	14.459776
22.373348	1270.220051	14.464794
22.354129	1271.727030	14.469811
22.187518	1265.349756	14.474829
22.576074	1273.760345	14.479847
22.489394	1277.865766	14.484864
22.246852	1284.461032	14.489882
22.716147	1291.062319	14.494899
22.898025	1283.032799	14.499917
22.767710	1281.922625	14.504935
22.677644	1275.169761	14.509952
22.689897	1258.507623	14.514970
22.544717	1263.931154	14.519987
22.442430	1278.155401	14.525005
22.664091	1278.717880	14.530023
22.614978	1293.542434	14.535040
22.860203	1296.526816	14.540058
22.879718	1295.916573	14.545075
22.901174	1289.907276	14.550093
23.028048	1287.738311	14.555111
22.857228	1290.196005	14.560128
22.752033	1275.621154	14.565146
22.873283	1273.364997	14.570163
22.970592	1288.935419	14.575181
22.754861	1275.814401	14.580199
22.771196	1293.549688	14.585216
22.878043	1284.830548	14.590234
22.849389	1294.484341	14.595251
22.827854	1297.039351	14.600269
22.768266	1292.071761	14.605287
22.834059	1295.131953	14.610304
22.718969	1289.400844	14.615322
22.643228	1292.919347	14.620339
22.615600	1299.787089	14.625357
22.575232	1287.835191	14.630375
22.732870	1305.463009	14.635392
22.984927	1317.772992	14.640410
23.044633	1325.138063	14.645427
22.964080	1326.108977	14.650445
23.296585	1318.602839	14.655463
23.253685	1327.703634	14.660480
23.462363	1322.112787	14.665498
23.443072	1321.268053	14.670515
23.394906	1322.359647	14.675533
23.657307	1320.228838	14.680551
23.434173	1328.161278	14.685568
23.449208	1322.041305	14.690586
23.329229	1324.945511	14.695603
23.299832	1322.195836	14.700621
23.379125	1322.019661	14.705639
23.580224	1319.304011	14.710656
23.698266	1319.450427	14.715674
23.638167	1307.876048	14.720691
23.116848	1302.730409	14.725709
23.508319	1306.729688	14.730727
23.286278	1320.384751	14.735744
23.705221	1313.505066	14.740762
23.576641	1313.453284	14.745779
23.440561	1327.225207	14.750797
23.760152	1313.461910	14.755815
23.713121	1315.294235	14.760832
23.390122	1315.888529	14.765850
23.873309	1313.746102	14.770867
23.865736	1316.053491	14.775885
23.965553	1311.837564	14.780903
23.778612	1311.664526	14.785920
23.915488	1294.342233	14.790938
23.898980	1288.051123	14.795955
23.373040	1296.055437	14.800973
23.825151	1293.033910	14.805991
23.747510	1308.039212	14.811008
23.661111	1312.946861	14.816026
23.838634	1306.598053	14.821043
23.299704	1314.607596	14.826061
23.760818	1312.703076	14.831079
23.720446	1313.054087	14.836096
23.972201	1307.376148	14.841114
23.748611	1311.078689	14.846131
23.415327	1311.268773	14.851149
23.815269	1298.744832	14.856167
23.550244	1329.562575	14.861184
23.774931	1337.842031	14.866202
24.055351	1347.764322	14.871219
23.842446	1352.493954	14.876237
24.403515	1349.186043	14.881255
24.384500	1349.152966	14.886272
24.079908	1356.291430	14.891290
24.210486	1346.052032	14.896307
23.773359	1351.080128	14.901325
23.972423	1350.217870	14.906343
24.084161	1350.077420	14.911360
24.145825	1352.016686	14.916378
24.365049	1352.585849	14.921395
24.131054	1348.685855	14.926413
24.191844	1349.489505	14.931431
23.695584	1355.565258	14.936448
23.865416	1359.640802	14.941466
24.277111	1372.354818	14.946483
24.407479	1382.110723	14.951501
24.854619	1371.869583	14.956519
24.832898	1374.706216	14.961536
24.964440	1365.467123	14.966554
24.564300	1347.656248	14.971571
24.433645	1342.138391	14.976589
24.285626	1334.644391	14.981607
24.181542	1349.130122	14.986624
24.377238	1357.061846	14.991642
24.581791	1365.102276	14.996659
24.391155	1371.755371	15.001677
24.516689	1371.619013	15.006695
24.789832	1361.824067	15.011712
24.797732	1373.894607	15.016730
25.098033	1365.995595	15.021747
24.876961	1367.110050	15.026765
24.833509	1372.127276	15.031783
24.855712	1372.364485	15.036800
24.911013	1364.268589	15.041818
25.127799	1359.923878	15.046835
24.526460	1372.706656	15.051853
24.679611	1373.770864	15.056871
25.026649	1362.699384	15.061888
24.673113	1371.432888	15.066906
24.868980	1375.417765	15.071923
24.773791	1367.816217	15.076941
25.134728	1363.972345	15.081959
24.956581	1368.919815	15.086976
24.881007	1372.183472	15.091994
25.103709	1367.483874	15.097011
24.995392	1377.314026	15.102029
25.143913	1360.798356	15.107047
24.890450	1369.174542	15.112064
25.228469	1370.539609	15.117082
24.993333	1365.906741	15.122099
24.844401	1374.552557	15.127117
25.082523	1362.477526	15.132135
25.152831	1363.619442	15.137152
24.805354	1364.401691	15.142170
25.127021	1363.485271	15.147187
24.920696	1374.232420	15.152205
25.557682	1391.186123	15.157223
25.380432	1398.463178	15.162240
25.268235	1392.034696	15.167258
25.196269	1387.371078	15.172275
25.617877	1392.450994	15.177293
25.504166	1395.693997	15.182311
25.570050	1378.941368	15.187328
25.256349	1374.050460	15.192346
25.697439	1374.209848	15.197363
25.361623	1375.768907	15.202381
25.242847	1375.619603	15.207399
25.531799	1387.377906	15.212416
25.567719	1398.806904	15.217434
25.836372	1400.737545	15.222451
25.887558	1391.497881	15.227469
25.589094	1385.655977	15.232487
25.739889	1371.844040	15.237504
25.576200	1367.182473	15.242522
25.727448	1380.971543	15.247539
25.524710	1396.119587	15.252557
25.926060	1395.000114	15.257575
25.893660	1395.568512	15.262592
25.786672	1394.775515	15.267610
25.853369	1378.021184	15.272627
25.684660	1384.655057	15.277645
25.925310	1390.890152	15.282663
25.894675	1393.704615	15.287680
25.578291	1402.716151	15.292698
25.919095	1393.715019	15.297715
25.634907	1394.529648	15.302733
25.883153	1390.485085	15.307751
25.904782	1394.052578	15.312768
25.650543	1397.453280	15.317786
26.035596	1393.968933	15.322803
25.759498	1393.594603	15.327821
25.818686	1391.908339	15.332839
26.128357	1391.953404	15.337856
25.866798	1390.456728	15.342874
26.124332	1383.409267	15.347891
26.350900	1404.831470	15.352909
26.394336	1399.954381	15.357927
26.352396	1390.382708	15.362944
26.578021	1391.097148	15.367962
26.719907	1379.717019	15.372979
26.257079	1388.007055	15.377997
26.230633	1386.935363	15.383015
26.215678	1383.209642	15.388032
26.065839	1384.619486	15.393050
26.459344	1378.170131	15.398067
26.668544	1379.175062	15.403085
26.206087	1385.673310	15.408103
26.592958	1385.586508	15.413120
26.592716	1391.545410	15.418138
26.555436	1379.830478	15.423155
26.522653	1383.441254	15.428173
26.472294	1380.474681	15.433191
26.329014	1379.324094	15.438208
26.186351	1391.997552	15.443226
26.399579	1383.209476	15.448243
26.643625	1394.139646	15.453261
27.065568	1407.327127	15.458279
27.128639	1392.379245	15.463296
26.583687	1386.125183	15.468314
26.852365	1383.101433	15.473331
26.780591	1392.903744	15.478349
26.798537	1393.442089	15.483367
26.929442	1380.251533	15.488384
26.446707	1391.646840	15.493402
26.604299	1388.445746	15.498419
26.625291	1404.046553	15.503437
26.679477	1419.778155	15.508455
27.265234	1418.435780	15.513472
27.447860	1420.350257	15.518490
27.197087	1402.507626	15.523507
27.033054	1397.135075	15.528525
26.960329	1394.850060	15.533543
27.436916	1375.669177	15.538560
26.804744	1400.717406	15.543578
27.171281	1393.315917	15.548595
27.152574	1397.736157	15.553613
27.065223	1404.082562	15.558631
27.157624	1397.578186	15.563648
26.943597	1404.002212	15.568666
27.254218	1402.611696	15.573683
27.178400	1407.472856	15.578701
27.326371	1423.769181	15.583719
27.611291	1421.966685	15.588736
27.493648	1413.946324	15.593754
27.457969	1387.507168	15.598771
27.497591	1393.329148	15.603789
27.368858	1393.503912	15.608807
27.358347	1386.735161	15.613824
27.384071	1385.327950	15.618842
27.698434	1391.798261	15.623859
27.248022	1392.340518	15.628877
27.443938	1397.486320	15.633895
27.816644	1394.269792	15.638912
27.575306	1402.716424	15.643930
27.618680	1390.554451	15.648947
27.620153	1397.604794	15.653965
27.499351	1398.061446	15.658983
27.483577	1390.658011	15.664000
27.456523	1396.654226	15.669018
27.911647	1401.387443	15.674035
27.884026	1393.485660	15.679053
27.750782	1389.426435	15.684071
27.709406	1383.917919	15.689088
27.720857	1400.446784	15.694106
27.600228	1398.181207	15.699123
28.096117	1402.642073	15.704141
27.456789	1406.551735	15.709159
27.806925	1411.705193	15.714176
27.970516	1420.323213	15.719194
28.165087	1423.819084	15.724211
28.345165	1420.987215	15.729229
27.961420	1410.295744	15.734247
28.226627	1394.087838	15.739264
28.072116	1389.044117	15.744282
27.859414	1384.848124	15.749299
27.952818	1389.124635	15.754317
27.956203	1405.575352	15.759335
28.001194	1410.642194	15.764352
28.000036	1420.448205	15.769370
27.998264	1422.576142	15.774387
27.996242	1425.081657	15.779405
28.072941	1422.691005	15.784423
28.366672	1412.460147	15.789440
28.244716	1422.043172	15.794458
28.186852	1413.229099	15.799475
28.336273	1421.181611	15.804493
28.426078	1421.070614	15.809511
28.435527	1424.645563	15.814528
28.305518	1423.061833	15.819546
28.708901	1428.713335	15.824563
28.938941	1410.446358	15.829581
28.247722	1429.018273	15.834599
28.418274	1423.401220	15.839616
28.378542	1430.160839	15.844634
28.400661	1431.754840	15.849651
28.692333	1423.414353	15.854669
28.319177	1418.816066	15.859687
28.673028	1415.884121	15.864704
27.985702	1418.720739	15.869722
28.463006	1419.367511	15.874739
28.595068	1436.404160	15.879757
28.381708	1445.501540	15.884775
28.626413	1443.140721	15.889792
28.322773	1441.442318	15.894810
28.499080	1449.245047	15.899827
28.441292	1439.085179	15.904845
28.423471	1442.161097	15.909863
28.870128	1446.200379	15.914880
28.994872	1471.864208	15.919898
29.284403	1474.148618	15.924915
29.282053	1447.634822	15.929933
28.848926	1455.187104	15.934951
28.985446	1437.181196	15.939968
28.772371	1439.697565	15.944986
28.752024	1461.359800	15.950003
29.292427	1463.567230	15.955021
29.489931	1476.149540	15.960039
29.451569	1458.693761	15.965056
29.268622	1456.147095	15.970074
29.311957	1450.194806	15.975091
29.580713	1438.452252	15.980109
28.892462	1446.373206	15.985127
29.003267	1437.813012	15.990144
29.266333	1445.759209	15.995162
29.535252	1463.286884	16.000179
29.503511	1443.178643	16.005197
29.048874	1446.424122	16.010215
29.280856	1448.583996	16.015232
29.622278	1463.257557	16.020250
29.556074	1469.538481	16.025267
29.620115	1461.729797	16.030285
29.262278	1452.364201	16.035303
29.569630	1464.545150	16.040320
29.622798	1469.521830	16.045338
29.426890	1469.394265	16.050355
29.791624	1467.195989	16.055373
29.351174	1474.770686	16.060391
29.377630	1472.255115	16.065408
29.326269	1462.196455	16.070426
29.289486	1481.704651	16.075443
29.633288	1474.324052	16.080461
29.372951	1475.886027	16.085479
29.516734	1466.554465	16.090496
29.567231	1471.887874	16.095514
29.717299	1493.621295	16.100531
29.932050	1493.602059	16.105549
29.746346	1495.231572	16.110567
30.058500	1493.988674	16.115584
30.120623	1500.155546	16.120602
30.096008	1502.456244	16.125619
30.334606	1494.594533	16.130637
30.070395	1505.712820	16.135655
30.158440	1503.351808	16.140672
30.340920	1503.034114	16.145690
29.831644	1507.888932	16.150707
29.960647	1503.734365	16.155725
30.040209	1504.387160	16.160743
30.101056	1500.189192	16.165760
30.155289	1501.092215	16.170778
29.902087	1501.680102	16.175795
30.342736	1490.231787	16.180813
30.222743	1499.298580	16.185831
30.385969	1501.095034	16.190848
30.477405	1496.056095	16.195866
30.279989	1498.212100	16.200883
30.373113	1490.614275	16.205901
30.471540	1493.430981	16.210919
30.214836	1498.095284	16.215936
30.221211	1498.947735	16.220954
30.205926	1510.480159	16.225971
30.510198	1517.492491	16.230989
30.286515	1532.387604	16.236007
30.500988	1530.332052	16.241024
31.014872	1518.613262	16.246042
30.606397	1528.161827	16.251059
30.759675	1531.503856	16.256077
30.794332	1528.861907	16.261095
30.955939	1531.883271	16.266112
31.040330	1531.369640	16.271130
30.656085	1525.113482	16.276147
30.930847	1522.724260	16.281165
30.752172	1530.919503	16.286183
30.811649	1528.797433	16.291200
31.371136	1525.469286	16.296218
30.886841	1519.525614	16.301235
31.315691	1513.659683	16.306253
31.089503	1506.521779	16.311271
30.850275	1499.463039	16.316288
30.908403	1499.385410	16.321306
30.601537	1523.476655	16.326323
30.883986	1519.277160	16.331341
30.977267	1523.743287	16.336359
31.014387	1528.437817	16.341376
31.040728	1523.637348	16.346394
31.181483	1528.735364	16.351411
31.371194	1522.382160	16.356429
31.277020	1526.765709	16.361447
31.267837	1524.132326	16.366464
31.447296	1522.245174	16.371482
31.106122	1528.211315	16.376499
31.043586	1522.784776	16.381517
31.144701	1526.448167	16.386535
31.184405	1538.298258	16.391552
31.414967	1545.073811	16.396570
31.566297	1555.058521	16.401587
31.592798	1546.324511	16.406605
31.561257	1552.970404	16.411623
31.611130	1556.791419	16.416640
31.947885	1545.339182	16.421658
31.843526	1545.473878	16.426675
31.984151	1539.701099	16.431693
31.565698	1527.467159	16.436711
31.477369	1536.521845	16.441728
31.574232	1544.168975	16.446746
31.775556	1550.968858	16.451763
31.602467	1545.780175	16.456781
31.913989	1543.042154	16.461799
31.818254	1551.018892	16.466816
31.862670	1547.118485	16.471834
31.861590	1562.956587	16.476851
32.043292	1557.671200	16.481869
31.992140	1546.063743	16.486887
31.692894	1557.375641	16.491904
32.154356	1545.148431	16.496922
31.862814	1553.395510	16.501939
31.731240	1552.949358	16.506957
31.925347	1549.777013	16.511975
32.018509	1550.732821	16.516992
32.148035	1544.559886	16.522010
32.084160	1560.838240	16.527027
32.331626	1575.212282	16.532045
32.201562	1578.626255	16.537063
32.068540	1595.131976	16.542080
32.560664	1586.875048	16.547098
32.555954	1582.385479	16.552115
32.498262	1581.916531	16.557133
32.536922	1578.129510	16.562151
32.402667	1578.054248	16.567168
32.609597	1576.363278	16.572186
32.390101	1579.990510	16.577203
32.657059	1573.440912	16.582221
32.590494	1585.186075	16.587239
32.514591	1581.561263	16.592256
32.562133	1577.845975	16.597274
32.876152	1581.167098	16.602291
32.798047	1579.649007	16.607309
32.645724	1582.350774	16.612327
32.864490	1581.176249	16.617344
33.203567	1573.587919	16.622362
32.714628	1563.602912	16.627379
32.905067	1552.461094	16.632397
33.045156	1563.490560	16.637415
32.615340	1564.778327	16.642432
33.081520	1573.694258	16.647450
33.149475	1587.017016	16.652467
33.044593	1575.643844	16.657485
32.766146	1562.817298	16.662503
32.501038	1577.747380	16.667520
32.852613	1578.280501	16.672538
32.956048	1582.122082	16.677555
33.420268	1575.561471	16.682573
33.339530	1571.883161	16.687591
33.417875	1579.302805	16.692608
33.670399	1570.026984	16.697626
33.466314	1578.590477	16.702643
33.461289	1572.117292	16.707661
33.701158	1561.109162	16.712679
32.905703	1551.861276	16.717696
33.499641	1557.843462	16.722714
33.414086	1579.912692	16.727731
33.686718	1581.987448	16.732749
33.750069	1570.308225	16.737767
33.465156	1568.506928	16.742784
32.985454	1555.592932	16.747802
33.520814	1555.627173	16.752819
33.522357	1576.099192	16.757837
33.613091	1577.046737	16.762855
33.322234	1573.182492	16.767872
33.656143	1563.589301	16.772890
33.496124	1574.260783	16.777907
33.379000	1575.284739	16.782925
33.663499	1561.839851	16.787943
33.263369	1575.951436	16.792960
33.227214	1572.369053	16.797978
33.602166	1587.912032	16.802995
33.717443	1598.409058	16.808013
33.949359	1600.680655	16.813031
33.746739	1614.402111	16.818048
34.072307	1598.998427	16.823066
34.202886	1610.911952	16.828083
34.193950	1610.363651	16.833101
33.998201	1605.066084	16.838119
33.758276	1606.434472	16.843136
33.836875	1608.549618	16.848154
34.145029	1612.151694	16.853171
33.757984	1603.975198	16.858189
33.946786	1599.005642	16.863207
34.056386	1621.794962	16.868224
34.428243	1627.272238	16.873242
34.595042	1633.503487	16.878259
34.304496	1632.853801	16.883277
34.693819	1618.018043	16.888295
34.381445	1619.692942	16.893312
34.428844	1610.045525	16.898330
34.404374	1625.655394	16.903347
34.528544	1617.759955	16.908365
34.599378	1619.342275	16.913383
34.452710	1633.151570	16.918400
34.847715	1624.466497	16.923418
34.740246	1624.390896	16.928435
34.639711	1626.107518	16.933453
35.110883	1623.782127	16.938471
34.487663	1614.303801	16.943488
34.753598	1620.380014	16.948506
34.602922	1629.193006	16.953523
34.763525	1623.903094	16.958541
35.021737	1618.312099	16.963559
34.961364	1625.594223	16.968576
34.962021	1626.501079	16.973594
34.850245	1625.571186	16.978611
34.980255	1628.507943	16.983629
34.919133	1624.624348	16.988647
34.687746	1627.813809	16.993664
34.964477	1619.993928	16.998682
35.159509	1625.266588	17.003699
35.090819	1623.010782	17.008717
35.027756	1620.839026	17.013735
34.724001	1630.361517	17.018752
35.076903	1617.824356	17.023770
35.195654	1625.519951	17.028787
35.206773	1646.244597	17.033805
35.746597	1649.367693	17.038823
35.384205	1643.189011	17.043840
35.450539	1631.909616	17.048858
35.373919	1633.060043	17.053875
35.443408	1639.140065	17.058893
35.464347	1644.984003	17.063911
35.312319	1646.005665	17.068928
35.588852	1658.165737	17.073946
35.559781	1653.687896	17.078963
35.235361	1650.241922	17.083981
35.437163	1640.338614	17.088999
35.325310	1651.822841	17.094016
35.531303	1641.719079	17.099034
35.594156	1644.325188	17.104051
35.476941	1654.094808	17.109069
35.784926	1645.658780	17.114087
35.415827	1655.791060	17.119104
35.730988	1657.392621	17.124122
36.020700	1672.954005	17.129139
35.985428	1677.870925	17.134157
36.436899	1669.734485	17.139175
36.217489	1668.302633	17.144192
35.975942	1656.133968	17.149210
35.910200	1661.710152	17.154227
36.183459	1673.912446	17.159245
36.158037	1671.286346	17.164263
36.189761	1682.929392	17.169280
36.619598	1680.512266	17.174298
36.700367	1669.502686	17.179315
36.387059	1650.448210	17.184333
36.481462	1649.528693	17.189351
36.144507	1651.543372	17.194368
36.411982	1642.991892	17.199386
36.285097	1640.352877	17.204403
36.349331	1649.476900	17.209421
36.257803	1664.603553	17.214439
36.301822	1678.527990	17.219456
36.545004	1677.265403	17.224474
36.322625	1671.721935	17.229491
36.334144	1675.849561	17.234509
36.531238	1675.542118	17.239527
36.551822	1678.234416	17.244544
36.509493	1671.705000	17.249562
36.533173	1672.167718	17.254579
35.967127	1681.825674	17.259597
36.902772	1680.518716	17.264615
36.912313	1692.564089	17.269632
36.768908	1692.816705	17.274650
37.159545	1687.070064	17.279667
36.897653	1695.884316	17.284685
36.996436	1703.089181	17.289703
36.997998	1698.936007	17.294720
37.150878	1688.132001	17.299738
37.103463	1691.768783	17.304755
37.079384	1700.636350	17.309773
37.346687	1684.968149	17.314791
37.270324	1693.107051	17.319808
37.256813	1694.570690	17.324826
37.516839	1688.699367	17.329843
37.351324	1700.312533	17.334861
37.409826	1692.292241	17.339879
37.508583	1686.007744	17.344896
37.308503	1689.723146	17.349914
37.649619	1687.672545	17.354931
37.477917	1693.900388	17.359949
37.774577	1679.261827	17.364967
37.882851	1680.696602	17.369984
37.159335	1669.418089	17.375002
37.339210	1674.292043	17.380019
37.113149	1690.313250	17.385037
37.507182	1681.883929	17.390055
37.536104	1681.783427	17.395072
37.473340	1690.225341	17.400090
37.558726	1690.670353	17.405107
37.287544	1685.270737	17.410125
37.490970	1683.980668	17.415143
37.803944	1704.891647	17.420160
37.713160	1718.890321	17.425178
38.056966	1706.615672	17.430195
38.015189	1715.239879	17.435213
38.116003	1708.298273	17.440231
38.109482	1711.470764	17.445248
38.062311	1717.198172	17.450266
38.202578	1711.976756	17.455283
37.905983	1710.642157	17.460301
38.469717	1709.532946	17.465319
38.554785	1719.071350	17.470336
38.312418	1721.667948	17.475354
38.332923	1713.411445	17.480371
38.136860	1715.958969	17.485389
38.530569	1714.173696	17.490407
38.507145	1715.898481	17.495424
38.616702	1720.309374	17.500442
38.847746	1710.385623	17.505459
38.441089	1714.682992	17.510477
38.531536	1719.760783	17.515495
38.821580	1715.150227	17.520512
38.297330	1714.354543	17.525530
38.818837	1719.420217	17.530547
38.282157	1720.239736	17.535565
38.536767	1713.968125	17.540583
38.746885	1717.300346	17.545600
38.711854	1721.850709	17.550618
38.982218	1715.079483	17.555635
38.650043	1718.451786	17.560653
38.790462	1709.312525	17.565671
38.972404	1709.828660	17.570688
38.518448	1714.452126	17.575706
38.723746	1716.478651	17.580723
38.907010	1727.288986	17.585741
39.155350	1736.668434	17.590759
39.039678	1735.487458	17.595776
38.980155	1748.858225	17.600794
39.095670	1735.633621	17.605811
39.057616	1745.995538	17.610829
38.900118	1749.147283	17.615847
38.863185	1744.280537	17.620864
38.986646	1753.454958	17.625882
39.167134	1751.254564	17.630899
39.278850	1743.785783	17.635917
39.255552	1744.089247	17.640935
39.363826	1759.055924	17.645952
39.314305	1773.261226	17.650970
39.582829	1770.509571	17.655987
39.378017	1783.850842	17.661005
40.056827	1770.751884	17.666023
40.270911	1771.768650	17.671040
39.734876	1760.530954	17.676058
39.939168	1740.715011	17.681075
39.617599	1740.314099	17.686093
39.569369	1746.412941	17.691111
39.984370	1751.732366	17.696128
39.816603	1761.833394	17.701146
40.270023	1764.292287	17.706163
39.985728	1756.612937	17.711181
39.685447	1743.636334	17.716199
40.046231	1747.465232	17.721216
39.774056	1765.702523	17.726234
40.135172	1767.797803	17.731251
39.935436	1773.447313	17.736269
40.159052	1769.861206	17.741287
40.439562	1766.170852	17.746304
40.323113	1771.084233	17.751322
40.322775	1763.659269	17.756339
39.799270	1776.485828	17.761357
40.120196	1774.286629	17.766375
40.458536	1767.845117	17.771392
40.494757	1773.905332	17.776410
40.436776	1771.409468	17.781427
40.366701	1772.477846	17.786445
40.234704	1777.579337	17.791463
40.271094	1766.165393	17.796480
40.559448	1787.490213	17.801498
40.539211	1789.305739	17.806515
40.802084	1806.189031	17.811533
40.729823	1805.650036	17.816551
40.544523	1798.034318	17.821568
40.458421	1802.476441	17.826586
40.584586	1797.716593	17.831603
40.734702	1802.177674	17.836621
41.130325	1797.503060	17.841639
41.287279	1797.754967	17.846656
41.108949	1810.326718	17.851674
41.215188	1803.779054	17.856691
41.172528	1802.669803	17.861709
41.025242	1801.415207	17.866727
41.291019	1800.370029	17.871744
41.143549	1809.235317	17.876762
41.095586	1803.859834	17.881779
40.907827	1797.509294	17.886797
41.436448	1801.651231	17.891815
41.285278	1797.671833	17.896832
41.134295	1800.788728	17.901850
41.386177	1793.738826	17.906867
41.731716	1796.072563	17.911885
41.426636	1797.740812	17.916903
41.542755	1786.064011	17.921920
41.329555	1799.810138	17.926938
41.618899	1795.038425	17.931955
41.463793	1793.332020	17.936973
41.514522	1798.321786	17.941991
41.657780	1810.715613	17.947008
41.517789	1826.696500	17.952026
41.410320	1827.842423	17.957043
41.806825	1829.215514	17.962061
41.512583	1837.832865	17.967079
41.858841	1829.238035	17.972096
41.927059	1826.180096	17.977114
41.787682	1831.391327	17.982131
42.201058	1821.963056	17.987149
42.134109	1820.753065	17.992167
42.339374	1815.457535	17.997184
42.614148	1819.234885	18.002202
42.414431	1813.780562	18.007219
42.641204	1816.487195	18.012237
42.530561	1817.519572	18.017255
42.604278	1806.129533	18.022272
42.505918	1815.613093	18.027290
42.448316	1817.461325	18.032307
42.743402	1818.754629	18.037325
42.243959	1808.638984	18.042343
42.653821	1803.307681	18.047360
42.506541	1815.571660	18.052378
42.599508	1811.915138	18.057395
42.730412	1815.967918	18.062413
42.737824	1820.170176	18.067431
42.428769	1816.789355	18.072448
42.505456	1825.499346	18.077466
42.625117	1824.446794	18.082483
42.712985	1817.445849	18.087501
42.681332	1825.488026	18.092519
42.670422	1819.320855	18.097536
42.841620	1825.052807	18.102554
42.587666	1816.902942	18.107571
42.540024	1820.880373	18.112589
42.687763	1838.785715	18.117607
42.593998	1837.616967	18.122624
42.586205	1848.866876	18.127642
42.519209	1855.108764	18.132659
42.867797	1860.208359	18.137677
42.709984	1872.440243	18.142695
43.234799	1874.981370	18.147712
43.031598	1878.492811	18.152730
42.923765	1876.498054	18.157747
43.332191	1867.196394	18.162765
43.543411	1870.099799	18.167783
43.716426	1864.470386	18.172800
44.064622	1876.318746	18.177818
43.729394	1875.687186	18.182835
43.701626	1870.462624	18.187853
43.716273	1877.232654	18.192871
43.889519	1876.173126	18.197888
43.334669	1874.971726	18.202906
43.397471	1870.280166	18.207923
43.655955	1869.222775	18.212941
43.394371	1872.631835	18.217959
43.844949	1869.576617	18.222976
43.943050	1893.811538	18.227994
43.957669	1893.244525	18.233011
44.389804	1892.305738	18.238029
44.229068	1894.203463	18.243047
44.257706	1879.776559	18.248064
44.071807	1871.830541	18.253082
44.389447	1870.935972	18.258099
44.550112	1864.340272	18.263117
44.370690	1869.949611	18.268135
44.325630	1857.714044	18.273152
44.633992	1861.037708	18.278170
44.369435	1859.109637	18.283187
44.483112	1857.286421	18.288205
44.142561	1863.488565	18.293223
44.323781	1849.119159	18.298240
44.363717	1883.992921	18.303258
44.678322	1886.468468	18.308275
45.004899	1884.335211	18.313293
44.624580	1890.519325	18.318311
44.934800	1897.179301	18.323328
44.881100	1890.654746	18.328346
44.974152	1893.021688	18.333363
44.944795	1892.663049	18.338381
44.825500	1889.583089	18.343399
44.979703	1885.397651	18.348416
45.048900	1885.779180	18.353434
44.784512	1884.821697	18.358451
45.311770	1877.523330	18.363469
44.661069	1892.390166	18.368487
44.952126	1882.573925	18.373504
45.124595	1881.464180	18.378522
44.847712	1884.679042	18.383539
45.005202	1880.434876	18.388557
44.876928	1884.808240	18.393575
44.835775	1882.643176	18.398592
44.867119	1899.785313	18.403610
45.225979	1909.011171	18.408627
45.529790	1904.473084	18.413645
45.386482	1911.943980	18.418663
45.628445	1905.173264	18.423680
45.661160	1907.939967	18.428698
45.673919	1908.960535	18.433715
45.668110	1898.754301	18.438733
45.505948	1912.651280	18.443751
45.558970	1898.179567	18.448768
45.651623	1910.992136	18.453786
45.317794	1911.924825	18.458803
45.673226	1918.966163	18.463821
45.467276	1942.628272	18.468839
46.036844	1946.258746	18.473856
46.117526	1943.998731	18.478874
45.969034	1939.642889	18.483891
46.231351	1940.165878	18.488909
46.007843	1947.379004	18.493927
46.372762	1928.978177	18.498944
46.242882	1943.163425	18.503962
46.159597	1940.872142	18.508979
46.506010	1939.440475	18.513997
45.790932	1933.756033	18.519015
46.110929	1939.137087	18.524032
46.014412	1940.902659	18.529050
46.216921	1959.471927	18.534067
46.864767	1966.278662	18.539085
46.607592	1969.149029	18.544103
46.815669	1960.833369	18.549120
46.810706	1975.174916	18.554138
46.668562	1974.731223	18.559155
46.997116	1959.768735	18.564173
46.852720	1962.736740	18.569191
46.887252	1965.209774	18.574208
46.665842	1968.012298	18.579226
46.787918	1965.766916	18.584243
47.053817	1957.174603	18.589261
46.873234	1969.458180	18.594279
47.244180	1964.070888	18.599296
46.946641	1956.753791	18.604314
46.964722	1965.702104	18.609331
47.187693	1964.341249	18.614349
46.965125	1959.057268	18.619367
47.382588	1958.221498	18.624384
47.439181	1953.099863	18.629402
47.039914	1964.612083	18.634419
47.278876	1957.472135	18.639437
47.412447	1967.332538	18.644455
47.796780	1987.174611	18.649472
47.616897	1976.255924	18.654490
47.577280	1982.831724	18.659507
47.534652	1981.669754	18.664525
47.661651	1984.267267	18.669543
47.347872	1988.025261	18.674560
47.836083	1984.551857	18.679578
47.904211	1984.093505	18.684595
47.767662	1981.320679	18.689613
47.950380	1991.749028	18.694631
47.894825	1991.723350	18.699648
47.739274	1986.989493	18.704666
47.629111	1994.669878	18.709683
47.826981	1985.830404	18.714701
48.033339	1989.961654	18.719719
47.817363	1989.447145	18.724736
48.122085	1999.528829	18.729754
48.164493	2007.289502	18.734771
48.524592	2015.881257	18.739789
48.342093	2012.614708	18.744807
48.442542	2023.459710	18.749824
48.517137	2015.663205	18.754842
48.273175	2020.650493	18.759859
48.599486	2014.012576	18.764877
48.444541	2018.200670	18.769895
48.319269	2020.480534	18.774912
48.670660	2016.435869	18.779930
48.712884	2013.406420	18.784947
48.744990	2019.554703	18.789965
48.804290	2020.172999	18.794983
48.632239	2023.217004	18.800000
49.045257	2018.054234	18.805018
48.733962	2019.273580	18.810035
48.800186	2025.392040	18.815053
48.831948	2020.992480	18.820071
48.949357	2044.272037	18.825088
49.068852	2041.019458	18.830106
49.013982	2049.794612	18.835123
49.133233	2039.532152	18.840141
49.433140	2040.923030	18.845159
49.684810	2051.437173	18.850176
49.664845	2036.847965	18.855194
49.328995	2045.748159	18.860211
49.513910	2030.710973	18.865229
49.738794	2035.067387	18.870247
49.394476	2040.807703	18.875264
49.432502	2037.986572	18.880282
49.680884	2031.342986	18.885299
49.764080	2041.268106	18.890317
49.933676	2037.140736	18.895335
49.657077	2036.219798	18.900352
50.110428	2030.223119	18.905370
49.852865	2039.822670	18.910387
49.473083	2030.410643	18.915405
49.945447	2028.818872	18.920423
49.602965	2039.156397	18.925440
50.183908	2029.268657	18.930458
49.733354	2040.982612	18.935475
50.316399	2032.832068	18.940493
50.041579	2042.745069	18.945511
49.845078	2057.000832	18.950528
50.280977	2055.307900	18.955546
50.390324	2063.742245	18.960563
50.495300	2066.500600	18.965581
50.515603	2059.781682	18.970599
50.165448	2068.213015	18.975616
50.353185	2066.121539	18.980634
50.577485	2068.904912	18.985651
50.535254	2065.909372	18.990669
50.555218	2060.935125	18.995687
50.663504	2062.367577	19.000704
50.701086	2049.151186	19.005722
50.593808	2063.526443	19.010739
50.577654	2060.384376	19.015757
50.938099	2066.000505	19.020775
50.520846	2080.146767	19.025792
50.696069	2085.946612	19.030810
50.551881	2087.363486	19.035827
50.995999	2085.520578	19.040845
50.960511	2091.989581	19.045863
50.997193	2089.976466	19.050880
51.445695	2081.493395	19.055898
51.741275	2077.147706	19.060915
51.362811	2073.111666	19.065933
51.046163	2079.973955	19.070951
51.282767	2082.568951	19.075968
51.596749	2073.710906	19.080986
51.756089	2083.897639	19.086003
52.148036	2077.461601	19.091021
52.043745	2078.699065	19.096039
51.651303	2074.929542	19.101056
51.883193	2069.908121	19.106074
51.698679	2077.068684	19.111091
51.400813	2080.072987	19.116109
51.815852	2078.009757	19.121127
51.709292	2081.457067	19.126144
52.062075	2088.847362	19.131162
51.956676	2102.835364	19.136179
52.326005	2104.838144	19.141197
52.539233	2105.951820	19.146215
52.333575	2095.943287	19.151232
52.206595	2078.664504	19.156250
51.958931	2081.869242	19.161267
52.191573	2094.159386	19.166285
52.314358	2099.458687	19.171303
51.969427	2106.116270	19.176320
52.201292	2101.132598	19.181338
52.257574	2107.556296	19.186355
52.347897	2101.766148	19.191373
52.578151	2101.683876	19.196391
52.308225	2111.555241	19.201408
52.510774	2115.318231	19.206426
52.508103	2123.728787	19.211443
52.542746	2129.726476	19.216461
52.811115	2128.479499	19.221479
52.639906	2137.620927	19.226496
53.143468	2133.058780	19.231514
53.059881	2128.758601	19.236531
52.774817	2125.891446	19.241549
53.052818	2130.963067	19.246567
52.999367	2138.816969	19.251584
53.330130	2130.371526	19.256602
53.448841	2134.464095	19.261619
53.465330	2142.136944	19.266637
53.572768	2135.017100	19.271655
53.359491	2137.779816	19.276672
53.636280	2126.238368	19.281690
53.169490	2129.322321	19.286707
53.164609	2139.850700	19.291725
53.477339	2146.427801	19.296743
53.505217	2163.905096	19.301760
53.616753	2159.187580	19.306778
53.667552	2155.467693	19.311795
53.329978	2157.124644	19.316813
53.525880	2156.199921	19.321831
53.753394	2163.963406	19.326848
53.551802	2163.783251	19.331866
53.783013	2170.864974	19.336883
53.888925	2185.739651	19.341901
54.514034	2183.999225	19.346919
54.313922	2181.575513	19.351936
54.444883	2183.100324	19.356954
54.279329	2176.289074	19.361971
54.156702	2180.704100	19.366989
54.445739	2180.129494	19.372007
54.419379	2186.298970	19.377024
54.747337	2185.799961	19.382042
54.609967	2184.259795	19.387059
54.611527	2181.339051	19.392077
54.639374	2179.181816	19.397095
54.700646	2178.047309	19.402112
54.675458	2176.289462	19.407130
54.735213	2172.531172	19.412147
54.756342	2176.864277	19.417165
54.981787	2169.313429	19.422183
54.691937	2174.923190	19.427200
54.778010	2176.803614	19.432218
54.910574	2182.051044	19.437235
54.858599	2183.977082	19.442253
55.408871	2176.310713	19.447271
54.912607	2185.909099	19.452288
55.231902	2203.457953	19.457306
55.295004	2197.090040	19.462323
55.403270	2205.939167	19.467341
55.635148	2199.714237	19.472359
55.259607	2205.995256	19.477376
55.260966	2197.227110	19.482394
55.440810	2197.264572	19.487411
55.115456	2202.542563	19.492429
55.473689	2190.616811	19.497447
55.430063	2199.574322	19.502464
55.631162	2210.461618	19.507482
56.019977	2223.551301	19.512499
55.745618	2230.288143	19.517517
56.411490	2224.615387	19.522535
56.332191	2238.416869	19.527552
56.277045	2224.232668	19.532570
56.101149	2203.565083	19.537587
56.220791	2200.100069	19.542605
56.218409	2194.541765	19.547623
55.979407	2199.371006	19.552640
56.070962	2212.629219	19.557658
56.331197	2222.487687	19.562675
56.312697	2225.357794	19.567693
56.583623	2223.939714	19.572711
56.273020	2230.233985	19.577728
56.446820	2227.130807	19.582746
56.380914	2225.560361	19.587763
56.491634	2225.772456	19.592781
56.876942	2218.345538	19.597799
56.537240	2225.674867	19.602816
56.580006	2227.976732	19.607834
56.667761	2229.771944	19.612851
56.505788	2247.053081	19.617869
56.774555	2257.517452	19.622887
56.965203	2268.251502	19.627904
56.619331	2271.396431	19.632922
56.951676	2263.028532	19.637939
56.688766	2263.486634	19.642957
57.035736	2273.554692	19.647975
57.390509	2284.102903	19.652992
57.622110	2289.374693	19.658010
57.643509	2284.688030	19.663027
57.761268	2290.227323	19.668045
58.085483	2278.190510	19.673063
57.871947	2272.724058	19.678080
57.702332	2262.218834	19.683098
57.880846	2249.515448	19.688115
57.487217	2248.747665	19.693133
57.674695	2263.056445	19.698151
57.777420	2264.312824	19.703168
57.831583	2280.100420	19.708186
57.941271	2272.037823	19.713203
57.930211	2284.547122	19.718221
58.433149	2268.659017	19.723239
58.322922	2273.964079	19.728256
58.338065	2266.453799	19.733274
58.763740	2263.070537	19.738291
58.185643	2263.784203	19.743309
58.584860	2261.123311	19.748327
58.658541	2259.641508	19.753344
58.661746	2264.068741	19.758362
59.011724	2263.436432	19.763379
58.534183	2249.565770	19.768397
58.786140	2243.679782	19.773415
58.777635	2251.089238	19.778432
59.009373	2247.545768	19.783450
58.850760	2240.049841	19.788467
58.341132	2237.894150	19.793485
58.529964	2244.001014	19.798503
58.860652	2251.682807	19.803520
58.712285	2258.187190	19.808538
58.973853	2259.883107	19.813555
59.184656	2262.227398	19.818573
58.683445	2262.076933	19.823591
58.909016	2270.337906	19.828608
59.267005	2290.781614	19.833626
59.601372	2290.432604	19.838643
59.434341	2299.380754	19.843661
59.137458	2294.719676	19.848679
59.130144	2304.013625	19.853696
59.571454	2305.238034	19.858714
59.413056	2298.645828	19.863731
59.362745	2296.818034	19.868749
59.630994	2294.543785	19.873767
59.550397	2305.387980	19.878784
59.616632	2311.497907	19.883802
59.891865	2322.016355	19.888819
59.655898	2330.848876	19.893837
60.172831	2325.752020	19.898855
60.050834	2327.973201	19.903872
60.047607	2324.924979	19.908890
60.175547	2329.805078	19.913907
60.218060	2323.881668	19.918925
60.156470	2330.531135	19.923943
60.150282	2333.197147	19.928960
60.071070	2328.411674	19.933978
60.435515	2335.388852	19.938995
60.510627	2356.344211	19.944013
60.367242	2365.138391	19.949031
60.525856	2360.447912	19.954048
60.574793	2359.552907	19.959066
61.195156	2353.979392	19.964083
60.954199	2362.988925	19.969101
61.241803	2364.608336	19.974119
60.985350	2365.112606	19.979136
61.122760	2364.256979	19.984154
61.500169	2358.977850	19.989171
60.983235	2351.882749	19.994189
60.898691	2357.634459	19.999207
60.921574	2358.081595	20.004224
60.822321	2362.746230	20.009242
60.995188	2362.295547	20.014259
61.252242	2379.449448	20.019277
61.464532	2380.775675	20.024295
61.366869	2395.333000	20.029312
61.404520	2394.317085	20.034330
61.686007	2390.443932	20.039347
61.392537	2390.444397	20.044365
61.447589	2396.277690	20.049383
61.600436	2394.176001	20.054400
61.846356	2413.438991	20.059418
62.227176	2421.447180	20.064435
62.182929	2420.270487	20.069453
62.347325	2420.353676	20.074471
62.250103	2413.329263	20.079488
62.133595	2420.765467	20.084506
62.600074	2406.014147	20.089523
62.247320	2401.111810	20.094541
62.155546	2409.206372	20.099559
62.517416	2407.792651	20.104576
62.071530	2414.830664	20.109594
62.050581	2409.107696	20.114611
62.285215	2412.256826	20.119629
62.077882	2410.915001	20.124647
62.392607	2415.732304	20.129664
62.404393	2432.992243	20.134682
62.613121	2438.487194	20.139699
62.711996	2430.821890	20.144717
62.716553	2439.351824	20.149735
63.023034	2440.669328	20.154752
62.831477	2437.564592	20.159770
63.063864	2429.358059	20.164787
63.060832	2433.395402	20.169805
63.364459	2442.728735	20.174823
63.857765	2458.688762	20.179840
63.490190	2443.021889	20.184858
63.650205	2431.294311	20.189875
63.242769	2435.428399	20.194893
63.198308	2441.956409	20.199911
63.617831	2444.227327	20.204928
63.801584	2462.963055	20.209946
63.776759	2469.264553	20.214963
63.973362	2459.919216	20.219981
63.991611	2463.697531	20.224999
63.834585	2453.788758	20.230016
63.788386	2462.948995	20.235034
64.287185	2458.286039	20.240051
63.901004	2460.967053	20.245069
63.652141	2456.114202	20.250087
63.771994	2459.720567	20.255104
64.303718	2467.912377	20.260122
64.322743	2472.974291	20.265139
64.432324	2471.231886	20.270157
64.635688	2478.709138	20.275175
65.008041	2455.269903	20.280192
64.737515	2478.315475	20.285210
65.002899	2457.025754	20.290227
64.718383	2464.361346	20.295245
64.816559	2457.756467	20.300263
65.110186	2460.104888	20.305280
65.475618	2460.686967	20.310298
65.183867	2442.077943	20.315315
64.984231	2443.827769	20.320333
64.971435	2440.513607	20.325351
65.163077	2437.457882	20.330368
65.004762	2459.024827	20.335386
65.433831	2456.683217	20.340403
65.556718	2459.386089	20.345421
65.229083	2463.159784	20.350439
65.473934	2465.600936	20.355456
65.345791	2463.595177	20.360474
65.389269	2457.442661	20.365491
65.443011	2462.801874	20.370509
65.729648	2460.980891	20.375527
65.760028	2458.680051	20.380544
65.471408	2459.931211	20.385562
65.509752	2459.095311	20.390579
65.886765	2467.967026	20.395597
65.962212	2498.261766	20.400615
65.806112	2494.327011	20.405632
65.791318	2496.501230	20.410650
65.977849	2491.349246	20.415667
66.190379	2483.712198	20.420685
66.287041	2496.624541	20.425703
66.263879	2495.484596	20.430720
66.114410	2501.186936	20.435738
66.456219	2505.579121	20.440755
66.619712	2516.881675	20.445773
66.327927	2526.615216	20.450791
66.453130	2520.888561	20.455808
66.741207	2521.809417	20.460826
66.897614	2521.704312	20.465843
66.771961	2512.234923	20.470861
66.770077	2525.603501	20.475879
67.265372	2518.885708	20.480896
67.135426	2531.911307	20.485914
67.265805	2526.954689	20.490931
66.992975	2522.729409	20.495949
66.840323	2525.871107	20.500967
67.250667	2530.995705	20.505984
67.311128	2553.242130	20.511002
67.281021	2547.861164	20.516019
67.474173	2551.134144	20.521037
67.271011	2558.222402	20.526055
67.998185	2543.409705	20.531072
67.724496	2550.325142	20.536090
67.745026	2554.337523	20.541107
67.985731	2550.765021	20.546125
67.808386	2560.562140	20.551143
68.018131	2555.918508	20.556160
67.931693	2571.916839	20.561178
67.998523	2570.979638	20.566195
68.258231	2576.752048	20.571213
67.950178	2572.990958	20.576231
68.348299	2565.884329	20.581248
68.264971	2572.248690	20.586266
68.313077	2575.077567	20.591283
68.350971	2574.925287	20.596301
68.364891	2572.961359	20.601319
68.296439	2577.699809	20.606336
68.779776	2587.877702	20.611354
69.066457	2587.230305	20.616371
69.083333	2591.859974	20.621389
68.924973	2592.573575	20.626407
69.178212	2589.695992	20.631424
69.442013	2595.422134	20.636442
69.477046	2599.606054	20.641459
69.584871	2588.227271	20.646477
69.326319	2578.354269	20.651495
69.057265	2569.631383	20.656512
69.242426	2572.712925	20.661530
69.258793	2579.343780	20.666547
69.708340	2589.054317	20.671565
69.441205	2588.493666	20.676583
69.550023	2595.295422	20.681600
69.334269	2589.470514	20.686618
69.277596	2592.354647	20.691635
69.233773	2585.610317	20.696653
69.491237	2602.167386	20.701671
69.921841	2607.363507	20.706688
69.883350	2609.764917	20.711706
70.172081	2626.929003	20.716723
69.902663	2616.294704	20.721741
70.122242	2628.743132	20.726759
70.070774	2620.049231	20.731776
69.948726	2616.183739	20.736794
70.055988	2652.409423	20.741811
70.706002	2652.418317	20.746829
70.711656	2654.365903	20.751847
70.836093	2643.654615	20.756864
70.909048	2648.203777	20.761882
70.980362	2647.857382	20.766899
71.084896	2646.387926	20.771917
70.995034	2655.268137	20.776935
70.756986	2648.771067	20.781952
70.889170	2642.315643	20.786970
71.134520	2646.477048	20.791987
70.908226	2644.314651	20.797005
70.547915	2647.137879	20.802023
70.927709	2659.199732	20.807040
71.219593	2671.590256	20.812058
71.445450	2668.378785	20.817075
71.407143	2674.190894	20.822093
71.431880	2676.752139	20.827111
71.518923	2668.567078	20.832128
71.543495	2678.759988	20.837146
71.515327	2699.965933	20.842163
71.913257	2701.777814	20.847181
71.881538	2703.758111	20.852199
71.827196	2700.647954	20.857216
72.025728	2710.542552	20.862234
72.419741	2701.067254	20.867251
72.381978	2696.212907	20.872269
72.000974	2704.546476	20.877287
72.640482	2703.264652	20.882304
72.616454	2691.131223	20.887322
72.525742	2701.298484	20.892339
72.735623	2696.459707	20.897357
72.735693	2703.177384	20.902375
72.706269	2699.220798	20.907392
72.494167	2701.387970	20.912410
72.833643	2697.038246	20.917427
72.845373	2698.391769	20.922445
73.168374	2721.465781	20.927463
73.229431	2716.977173	20.932480
73.453044	2708.559500	20.937498
73.171836	2714.546445	20.942515
73.255024	2701.132618	20.947533
73.117963	2704.016221	20.952551
73.167756	2714.135126	20.957568
73.241881	2720.603445	20.962586
73.516095	2722.866905	20.967603
73.220074	2715.619975	20.972621
73.254266	2727.231997	20.977639
73.236463	2721.661006	20.982656
73.628066	2740.447325	20.987674
73.320471	2749.507051	20.992691
73.566007	2747.241075	20.997709
73.843029	2751.401393	21.002727
73.626671	2750.171886	21.007744
73.988854	2765.554553	21.012762
73.681141	2778.482863	21.017779
74.137294	2776.976985	21.022797
74.241303	2777.537054	21.027815
74.346466	2781.270127	21.032832
74.847551	2783.045902	21.037850
74.315619	2788.753496	21.042867
74.662782	2791.218506	21.047885
74.747297	2801.630846	21.052903
74.928617	2805.624734	21.057920
75.104815	2803.844134	21.062938
75.110975	2798.874984	21.067955
75.463386	2804.464366	21.072973
75.723368	2806.152736	21.077991
75.199289	2795.035034	21.083008
75.622464	2790.599568	21.088026
75.449676	2791.018139	21.093043
75.604209	2775.313269	21.098061
75.427448	2801.434987	21.103079
75.518244	2798.640693	21.108096
75.740559	2795.885995	21.113114
75.543992	2808.956289	21.118131
75.792282	2793.911360	21.123149
75.511606	2807.697510	21.128167
75.355990	2807.933996	21.133184
75.966288	2799.260312	21.138202
75.732320	2811.173960	21.143219
76.005828	2818.205206	21.148237
76.087324	2823.352460	21.153255
76.246135	2820.851734	21.158272
76.101161	2833.259360	21.163290
76.057750	2833.268713	21.168307
76.259271	2821.421719	21.173325
76.223435	2835.790274	21.178343
76.503409	2860.093765	21.183360
76.556019	2854.873337	21.188378
76.420065	2865.917136	21.193395
76.758836	2858.959062	21.198413
76.621768	2860.617937	21.203431
76.632297	2860.101096	21.208448
76.886944	2868.644888	21.213466
76.785819	2881.051068	21.218483
77.217120	2880.306655	21.223501
77.463507	2889.065735	21.228519
77.202965	2882.182773	21.233536
77.445154	2876.386193	21.238554
77.413844	2880.207917	21.243571
77.619792	2873.956947	21.248589
77.788017	2874.421039	21.253607
77.695536	2877.420278	21.258624
77.807879	2873.969642	21.263642
77.521040	2879.863944	21.268659
77.919462	2884.646819	21.273677
77.914940	2900.782690	21.278695
77.977283	2909.114108	21.283712
78.412659	2897.279316	21.288730
78.406459	2908.576197	21.293747
78.405040	2902.786991	21.298765
78.650721	2899.083820	21.303783
78.459252	2898.271958	21.308800
78.904296	2907.472127	21.313818
78.660315	2907.481214	21.318835
78.958651	2903.971019	21.323853
78.943435	2899.401698	21.328871
78.958297	2904.623323	21.333888
78.999700	2895.467649	21.338906
78.854267	2896.263370	21.343923
79.074514	2901.571807	21.348941
78.955690	2908.802533	21.353959
78.851362	2910.065244	21.358976
79.056836	2922.992076	21.363994
79.113544	2933.708647	21.369011
79.332542	2924.915583	21.374029
79.007191	2928.869952	21.379047
79.056926	2939.079483	21.384064
79.557446	2954.042259	21.389082
79.780377	2967.587777	21.394099
79.771219	2964.911652	21.399117
79.910153	2958.085301	21.404135
79.814719	2960.633508	21.409152
80.071730	2964.376237	21.414170
80.033220	2964.340758	21.419187
80.017635	2975.092486	21.424205
80.534977	2987.949977	21.429223
80.059597	2991.601053	21.434240
80.350353	2984.817342	21.439258
80.635645	2986.312908	21.444275
80.828639	2986.164996	21.449293
81.154937	2982.128007	21.454311
80.927090	2988.444012	21.459328
81.125436	2980.186752	21.464346
81.048812	2980.073183	21.469363
81.278657	2984.377963	21.474381
81.040478	2982.972566	21.479399
81.059508	2985.569386	21.484416
80.889714	2977.749986	21.489434
81.223604	2984.355561	21.494451
80.928118	2977.503297	21.499469
81.062497	2994.804133	21.504487
81.461829	3001.916877	21.509504
81.511742	3011.858979	21.514522
81.375797	3021.651376	21.519539
81.410179	3018.213139	21.524557
81.774900	3021.170962	21.529575
81.512319	3045.663544	21.534592
82.222753	3048.950901	21.539610
81.776189	3051.995628	21.544627
82.161802	3047.907472	21.549645
82.155753	3049.132496	21.554663
82.158234	3049.737085	21.559680
82.224283	3048.765368	21.564698
82.128519	3065.346254	21.569715
82.319019	3077.592034	21.574733
82.603363	3078.069080	21.579751
82.466814	3080.162114	21.584768
82.779899	3074.004890	21.589786
82.875846	3078.178445	21.594803
82.941093	3080.882760	21.599821
83.339347	3079.793560	21.604839
83.447582	3096.109108	21.609856
83.742317	3090.688726	21.614874
83.842733	3078.249585	21.619891
83.515205	3076.871800	21.624909
83.745930	3062.625463	21.629927
83.406105	3066.346189	21.634944
83.662271	3055.383899	21.639962
83.633122	3067.001572	21.644979
83.644611	3082.257216	21.649997
84.053856	3080.512576	21.655015
83.710932	3091.388960	21.660032
83.904615	3079.129242	21.665050
83.820101	3092.197651	21.670067
83.779354	3089.397534	21.675085
84.261480	3085.502432	21.680103
84.296465	3108.221021	21.685120
84.743386	3113.375393	21.690138
84.349538	3109.127547	21.695155
84.233441	3109.758915	21.700173
84.729654	3110.361075	21.705191
84.708893	3121.573127	21.710208
84.832215	3110.109660	21.715226
84.863003	3113.350450	21.720243
84.981876	3120.931970	21.725261
85.280417	3128.205589	21.730279
84.903263	3144.186401	21.735296
85.314735	3134.152682	21.740314
85.568551	3139.060964	21.745331
85.150135	3143.733478	21.750349
85.438530	3130.700302	21.755367
84.944906	3147.203134	21.760384
85.454003	3131.979396	21.765402
85.801080	3142.000845	21.770419
85.547433	3166.479618	21.775437
86.116105	3163.118191	21.780455
85.914211	3167.011243	21.785472
86.105543	3169.392614	21.790490
85.966665	3171.318480	21.795507
85.832545	3170.956063	21.800525
85.906388	3166.790157	21.805543
85.881760	3180.169253	21.810560
86.257943	3180.545129	21.815578
86.352764	3195.040300	21.820595
86.254982	3199.911063	21.825613
87.068993	3191.490214	21.830631
86.908922	3194.763031	21.835648
86.913820	3195.397920	21.840666
86.818355	3190.603742	21.845683
87.132907	3210.538853	21.850701
87.575861	3213.105869	21.855719
87.377214	3221.918814	21.860736
87.374002	3221.306609	21.865754
87.346436	3221.911277	21.870771
87.595103	3217.401252	21.875789
88.170133	3215.492499	21.880807
87.854865	3212.749508	21.885824
88.038220	3218.608295	21.890842
88.185762	3213.517341	21.895859
88.125296	3208.601941	21.900877
88.113068	3200.731335	21.905895
88.162637	3222.273332	21.910912
88.329516	3213.722038	21.915930
88.721735	3209.496696	21.920947
88.319485	3213.039407	21.925965
88.608255	3205.599860	21.930983
87.977679	3211.803977	21.936000
88.152487	3215.848575	21.941018
88.436420	3219.428963	21.946035
88.561763	3241.820269	21.951053
88.938017	3240.869082	21.956071
88.768536	3247.323778	21.961088
88.718759	3240.977345	21.966106
88.976814	3230.859470	21.971123
89.114990	3246.112388	21.976141
89.622862	3259.838503	21.981159
89.533564	3271.536728	21.986176
89.474840	3271.362877	21.991194
89.664064	3273.255313	21.996211
89.499785	3281.668707	22.001229
89.811038	3277.081819	22.006247
89.372921	3274.672275	22.011264
89.681353	3269.436077	22.016282
90.010914	3271.561791	22.021299
89.622392	3272.755789	22.026317
90.242676	3283.503100	22.031335
90.424795	3290.007942	22.036352
90.082821	3290.806705	22.041370
90.339269	3289.280709	22.046387
90.101850	3295.312035	22.051405
90.393174	3287.700552	22.056423
90.010969	3295.315657	22.061440
90.360816	3313.463544	22.066458
90.893962	3323.355544	22.071475
90.556889	3331.491305	22.076493
90.776336	3324.506417	22.081511
90.867044	3321.860713	22.086528
91.075588	3338.778835	22.091546
91.556922	3344.737257	22.096563
91.147614	3349.118111	22.101581
91.545982	3345.432960	22.106599
91.423340	3346.128313	22.111616
91.241274	3355.649029	22.116634
91.535752	3351.876608	22.121651
91.496465	3357.933789	22.126669
91.708374	3369.755547	22.131687
91.738200	3379.376218	22.136704
91.874853	3377.255735	22.141722
92.074913	3376.268132	22.146739
92.130014	3378.356605	22.151757
92.401133	3381.677913	22.156775
92.197702	3397.728841	22.161792
92.316502	3402.970254	22.166810
92.647056	3404.833091	22.171827
92.479207	3401.425440	22.176845
92.307207	3412.919852	22.181863
92.489468	3419.214694	22.186880
92.905932	3428.723397	22.191898
93.159203	3423.405477	22.196915
93.049438	3436.579696	22.201933
93.491955	3434.917030	22.206951
93.529867	3427.366338	22.211968
93.584333	3430.416987	22.216986
93.698479	3424.255943	22.222003
93.699156	3432.516469	22.227021
93.609348	3432.677963	22.232039
93.767436	3437.457656	22.237056
93.773417	3456.138837	22.242074
93.794805	3462.549030	22.247091
94.016694	3461.716843	22.252109
94.400748	3450.201307	22.257127
94.364518	3449.164848	22.262144
94.177969	3458.090855	22.267162
94.428730	3456.579908	22.272179
94.304297	3462.445395	22.277197
94.728910	3473.150892	22.282215
94.662107	3486.445742	22.287232
94.990715	3486.342279	22.292250
95.217291	3479.641735	22.297267
95.099068	3489.632999	22.302285
95.347608	3490.258154	22.307303
95.268286	3491.758427	22.312320
94.977845	3496.899937	22.317338
95.278222	3480.509485	22.322355
95.211552	3489.910409	22.327373
95.228775	3491.559695	22.332391
95.240505	3487.993591	22.337408
95.394618	3513.564291	22.342426
95.568019	3511.142148	22.347443
95.537283	3520.240008	22.352461
95.668305	3511.890135	22.357479
96.177318	3520.233271	22.362496
96.244444	3534.866140	22.367514
96.393977	3535.385941	22.372531
96.371715	3540.257360	22.377549
96.235967	3542.344824	22.382567
96.375464	3542.074068	22.387584
96.283863	3541.259615	22.392602
96.272263	3531.206561	22.397619
96.637287	3553.454712	22.402637
96.841018	3562.914828	22.407655
97.209603	3555.160303	22.412672
97.157469	3559.762736	22.417690
97.265278	3549.670962	22.422707
97.263095	3551.191192	22.427725
97.352507	3557.898947	22.432743
97.716936	3560.134783	22.437760
97.473407	3570.481984	22.442778
97.703689	3576.630000	22.447795
97.788346	3586.850934	22.452813
97.942252	3584.439755	22.457831
98.113860	3576.125066	22.462848
98.288842	3587.308620	22.467866
98.478659	3578.475768	22.472883
98.244514	3579.524813	22.477901
98.275385	3586.335528	22.482919
98.557769	3575.068169	22.487936
98.229769	3579.274074	22.492954
98.682593	3600.167051	22.497971
98.710942	3613.258832	22.502989
98.783888	3609.232969	22.508007
99.092350	3610.137278	22.513024
98.726641	3617.331415	22.518042
99.146267	3614.696141	22.523059
99.145615	3612.665172	22.528077
99.294512	3620.305883	22.533095
99.198610	3632.157272	22.538112
99.138671	3647.352521	22.543130
99.496958	3640.445250	22.548147
99.281355	3645.390800	22.553165
99.357012	3644.640136	22.558183
99.758668	3663.082273	22.563200
99.836118	3679.304261	22.568218
100.231429	3667.984998	22.573235
100.224288	3672.093351	22.578253
100.245749	3671.013064	22.583271
100.066364	3661.689162	22.588288
99.846935	3673.660975	22.593306
100.358700	3693.857147	22.598323
100.704452	3701.023620	22.603341
100.751099	3693.776623	22.608359
100.806379	3694.368886	22.613376
100.474693	3709.072604	22.618394
100.906557	3701.437711	22.623411
101.341482	3712.549230	22.628429
101.345534	3720.619007	22.633447
101.435682	3721.293031	22.638464
101.335421	3731.133703	22.643482
101.612515	3714.355733	22.648499
101.692835	3716.385166	22.653517
101.339914	3715.268604	22.658535
101.781170	3714.329051	22.663552
101.733172	3721.275911	22.668570
102.064307	3738.290586	22.673587
101.904441	3737.534207	22.678605
102.318863	3748.952675	22.683623
102.662306	3747.319934	22.688640
102.740581	3748.758129	22.693658
102.763405	3751.766691	22.698675
102.694422	3744.977852	22.703693
102.703919	3748.488856	22.708711
102.885880	3739.263829	22.713728
103.132921	3742.182356	22.718746
103.106430	3737.461958	22.723763
103.217509	3748.265642	22.728781
103.230278	3761.585811	22.733799
103.562635	3764.448258	22.738816
103.424932	3774.410568	22.743834
103.723721	3767.836832	22.748851
103.593402	3767.841950	22.753869
103.443822	3774.878980	22.758887
103.747039	3764.058915	22.763904
103.704720	3774.705359	22.768922
103.724775	3799.136819	22.773939
103.647223	3802.870183	22.778957
103.918951	3802.842657	22.783975
103.824265	3800.541884	22.788992
104.005252	3822.328125	22.794010
104.270646	3826.976769	22.799027
104.456314	3830.596580	22.804045
104.226975	3853.880819	22.809063
104.551352	3858.994428	22.814080
104.552549	3864.006960	22.819098
104.895509	3864.346463	22.824115
105.294603	3868.237478	22.829133
105.452509	3884.389437	22.834151
105.576794	3887.491982	22.839168
105.599450	3887.062851	22.844186
105.545728	3881.761468	22.849203
105.628563	3883.677244	22.854221
105.318934	3885.862497	22.859239
105.598562	3876.331529	22.864256
105.577252	3892.064460	22.869274
106.044923	3894.193419	22.874291
106.059512	3910.910276	22.879309
106.131284	3904.975269	22.884327
106.488404	3906.017373	22.889344
106.428668	3915.980720	22.894362
106.617406	3912.491700	22.899379
106.867690	3911.739136	22.904397
106.288004	3918.232789	22.909415
106.391034	3928.928541	22.914432
106.548367	3937.336651	22.919450
106.827402	3943.477049	22.924467
106.823400	3964.980691	22.929485
106.944515	3965.504253	22.934503
107.337723	3967.247040	22.939520
107.240965	3982.848924	22.944538
107.366817	3976.195684	22.949555
107.973117	3989.799807	22.954573
107.703238	4010.508889	22.959591
108.123399	4009.566390	22.964608
107.955929	3999.400989	22.969626
107.985490	4011.892699	22.974643
108.192826	4008.532853	22.979661
108.057125	4016.684865	22.984679
108.387430	4025.137818	22.989696
108.337607	4043.461265	22.994714
108.641244	4043.095887	22.999731
109.336136	4033.234277	23.004749
109.189796	4048.890551	23.009767
109.255528	4029.958173	23.014784
109.014930	4043.217518	23.019802
109.052643	4042.125959	23.024819
109.118769	4045.980436	23.029837
109.384057	4055.728420	23.034855
109.886748	4057.733818	23.039872
109.956900	4064.102671	23.044890
109.940960	4054.468464	23.049907
110.240173	4058.350284	23.054925
110.339379	4050.234104	23.059943
110.398190	4049.173794	23.064960
110.512537	4058.726366	23.069978
110.558529	4056.168690	23.074995
110.943237	4048.655994	23.080013
110.807883	4061.200790	23.085031
110.806412	4049.333257	23.090048
110.905812	4059.383034	23.095066
110.407702	4050.544740	23.100083
110.456104	4043.103768	23.105101
110.449069	4070.434975	23.110119
110.733610	4078.088910	23.115136
111.151572	4085.416342	23.120154
111.054414	4084.390340	23.125171
111.083081	4095.776190	23.130189
111.069572	4108.303170	23.135207
111.601810	4106.161985	23.140224
111.805905	4116.335922	23.145242
111.747190	4114.902580	23.150259
112.196102	4119.643990	23.155277
112.453690	4142.298003	23.160295
112.587731	4133.090599	23.165312
112.662099	4133.073304	23.170330
112.489099	4127.585527	23.175347
112.427403	4135.592068	23.180365
112.506455	4130.938890	23.185383
112.882667	4139.999776	23.190400
113.029382	4128.818138	23.195418
113.148235	4129.086397	23.200435
113.401318	4119.188979	23.205453
113.024375	4134.731072	23.210471
113.370961	4124.687364	23.215488
113.189515	4141.840099	23.220506
113.261846	4146.140449	23.225523
113.339772	4154.269486	23.230541
113.430183	4155.789961	23.235559
113.738833	4160.153328	23.240576
113.576168	4182.077503	23.245594
113.597852	4178.200477	23.250611
114.200932	4190.573352	23.255629
114.066659	4197.783573	23.260647
114.324795	4204.846263	23.265664
113.990526	4211.105810	23.270682
114.043303	4225.344378	23.275699
114.376591	4218.223700	23.280717
114.481240	4249.860280	23.285735
114.463543	4244.117982	23.290752
114.857114	4246.577421	23.295770
115.344717	4261.629353	23.300787
115.923544	4267.688255	23.305805
115.759899	4281.247859	23.310823
115.825888	4265.623173	23.315840
115.879636	4268.545881	23.320858
115.909021	4276.384571	23.325875
116.162286	4266.219551	23.330893
116.035737	4266.646520	23.335911
116.274761	4264.519814	23.340928
116.139466	4267.122589	23.345946
116.034913	4273.603566	23.350963
116.303693	4276.852292	23.355981
116.091867	4305.570486	23.360999
116.487608	4294.902845	23.366016
116.508960	4297.683614	23.371034
116.651027	4318.164595	23.376051
116.683979	4321.828547	23.381069
117.239418	4325.181833	23.386087
117.095788	4319.488694	23.391104
117.100246	4331.866674	23.396122
117.284270	4349.082523	23.401139
117.664559	4353.216611	23.406157
117.565607	4361.056142	23.411175
118.060631	4353.803406	23.416192
117.993636	4351.374619	23.421210
117.831860	4352.252476	23.426227
118.257705	4343.978633	23.431245
118.102472	4347.250145	23.436263
118.588572	4371.981923	23.441280
118.516930	4380.285194	23.446298
118.552471	4377.567069	23.451315
119.036559	4373.352715	23.456333
118.878785	4374.318045	23.461351
118.923415	4372.598362	23.466368
119.079437	4381.784979	23.471386
118.713873	4378.830294	23.476403
119.089149	4395.490189	23.481421
119.156298	4406.417006	23.486439
119.119496	4409.928470	23.491456
119.225597	4427.065579	23.496474
119.314711	4436.709744	23.501491
119.532868	4437.904640	23.506509
119.696679	4456.212630	23.511527
119.980217	4470.341475	23.516544
120.216133	4471.705043	23.521562
120.081236	4483.543666	23.526579
120.923967	4481.150739	23.531597
120.627920	4484.856179	23.536615
120.659177	4483.706615	23.541632
120.859943	4494.023738	23.546650
120.675874	4512.675202	23.551667
121.165682	4502.266973	23.556685
121.326013	4511.083233	23.561703
121.018324	4515.195689	23.566720
121.222903	4519.737034	23.571738
121.435846	4538.681602	23.576755
121.481801	4546.030036	23.581773
121.691076	4539.765247	23.586791
121.665338	4551.127083	23.591808
121.828874	4569.857719	23.596826
121.504830	4575.364483	23.601843
121.866322	4580.922426	23.606861
122.145230	4581.150224	23.611879
122.214073	4598.128264	23.616896
122.705502	4596.349899	23.621914
122.639149	4602.789528	23.626931
122.578574	4601.705733	23.631949
122.636008	4607.663041	23.636967
123.043375	4617.563394	23.641984
123.377908	4612.282443	23.647002
123.246315	4632.648583	23.652019
123.342613	4625.260257	23.657037
123.659556	4645.400699	23.662055
123.692938	4652.109235	23.667072
123.944347	4638.624337	23.672090
123.859250	4648.849477	23.677107
124.322978	4653.358194	23.682125
124.133546	4654.282174	23.687143
123.954360	4651.990020	23.692160
124.476718	4672.281835	23.697178
123.932571	4687.578966	23.702195
124.557558	4684.064262	23.707213
124.614621	4691.815367	23.712231
124.703776	4687.865298	23.717248
125.175716	4707.014240	23.722266
125.103371	4720.069565	23.727283
125.187209	4710.637726	23.732301
125.488909	4719.420556	23.737319
125.388039	4712.925864	23.742336
125.528081	4714.337785	23.747354
125.696565	4737.886470	23.752371
125.945985	4738.496597	23.757389
126.136216	4741.403931	23.762407
125.907870	4743.438669	23.767424
125.873253	4739.945736	23.772442
125.801945	4756.351549	23.777459
126.181972	4755.998365	23.782477
126.648102	4751.957487	23.787495
126.710147	4762.008981	23.792512
127.238660	4764.376188	23.797530
127.046900	4787.282216	23.802547
127.273354	4794.386432	23.807565
127.433370	4787.691192	23.812583
127.127552	4792.640493	23.817600
127.414475	4784.434187	23.822618
127.261423	4797.923344	23.827635
127.579848	4813.372578	23.832653
127.932261	4821.634442	23.837671
127.943751	4817.206596	23.842688
128.453568	4810.985031	23.847706
128.205658	4834.039334	23.852723
127.871328	4835.415191	23.857741
128.309794	4840.068032	23.862759
128.516807	4852.015283	23.867776
128.624786	4846.626404	23.872794
128.527306	4860.837620	23.877811
129.016492	4869.877799	23.882829
129.372127	4870.802994	23.887847
129.026647	4877.992152	23.892864
129.036292	4877.588669	23.897882
129.558644	4895.460049	23.902899
129.535712	4901.339030	23.907917
129.773079	4896.838168	23.912935
129.842750	4905.182926	23.917952
130.212325	4894.836078	23.922970
130.108114	4911.860168	23.927987
130.023529	4932.380504	23.933005
130.253355	4931.921457	23.938023
130.355488	4939.084116	23.943040
130.446557	4938.394655	23.948058
130.621061	4956.524549	23.953075
130.893436	4967.909977	23.958093
131.362222	4964.794598	23.963111
131.309687	4967.522762	23.968128
131.558369	4961.883255	23.973146
131.378767	4961.436780	23.978163
131.541555	4962.856899	23.983181
131.825412	4967.926224	23.988199
131.481617	4967.627872	23.993216
131.924082	4974.855079	23.998234
131.900219	4983.375287	24.003251
132.360806	4992.687590	24.008269
132.711001	4988.329203	24.013287
132.709052	4994.415719	24.018304
132.680538	4982.904201	24.023322
132.394697	4990.799827	24.028339
133.009531	5002.728592	24.033357
133.251966	5013.944175	24.038375
132.899675	5022.820452	24.043392
133.223314	5013.159009	24.048410
133.456023	5016.956497	24.053427
133.278766	5017.876983	24.058445
133.830398	5024.641519	24.063463
133.787982	5034.192972	24.068480
134.149097	5037.911773	24.073498
134.150545	5042.544674	24.078515
134.100582	5043.837445	24.083533
134.410398	5035.429881	24.088551
134.196015	5048.289432	24.093568
134.723029	5046.818463	24.098586
134.561489	5068.233184	24.103603
134.413625	5066.464654	24.108621
134.572681	5068.621761	24.113639
134.771738	5080.329726	24.118656
134.786224	5095.979560	24.123674
135.088629	5104.959980	24.128691
135.165090	5103.021932	24.133709
135.779786	5107.793880	24.138727
135.688687	5125.870351	24.143744
135.725136	5124.243934	24.148762
135.960651	5125.027018	24.153779
135.723267	5132.113308	24.158797
136.432138	5146.828765	24.163815
136.521775	5153.237466	24.168832
136.392826	5151.116599	24.173850
136.521285	5152.863986	24.178867
136.503435	5171.966540	24.183885
137.270801	5179.297031	24.188903
137.234103	5178.951281	24.193920
137.487030	5176.745132	24.198938
137.709848	5174.614590	24.203955
137.149531	5177.404089	24.208973
137.579858	5182.126785	24.213991
137.475927	5199.949702	24.219008
137.661771	5211.991096	24.224026
137.672847	5202.037136	24.229043
137.549722	5214.477109	24.234061
137.824791	5224.264436	24.239079
137.642499	5238.958437	24.244096
137.897922	5250.202026	24.249114
138.662376	5265.650639	24.254131
138.390375	5280.867221	24.259149
138.441468	5282.903107	24.264167
138.564742	5298.663262	24.269184
138.744292	5306.704352	24.274202
139.037793	5307.032116	24.279219
139.281810	5328.177207	24.284237
139.682579	5322.304040	24.289255
139.463381	5338.753748	24.294272
139.633252	5335.611214	24.299290
140.266047	5344.996988	24.304307
140.144734	5357.149630	24.309325
140.524907	5356.637490	24.314343
140.290054	5367.262282	24.319360
140.416264	5363.805711	24.324378
140.824207	5380.303379	24.329395
140.498024	5395.136129	24.334413
141.130213	5391.905707	24.339431
140.904505	5394.827566	24.344448
140.915352	5398.759660	24.349466
141.363326	5412.459590	24.354483
141.176286	5426.953912	24.359501
141.653271	5428.704768	24.364519
141.731225	5440.511791	24.369536
142.075743	5454.639729	24.374554
142.217457	5457.237093	24.379571
142.201605	5462.234004	24.384589
142.451429	5453.664259	24.389607
142.302534	5465.752939	24.394624
142.408547	5484.283845	24.399642
143.016758	5485.393822	24.404659
142.901947	5490.153973	24.409677
142.756411	5482.382079	24.414695
143.000339	5511.057480	24.419712
142.925656	5520.257204	24.424730
143.187441	5518.185701	24.429747
143.493207	5540.565901	24.434765
143.816435	5542.644975	24.439783
143.792144	5549.348953	24.444800
143.677662	5549.915648	24.449818
144.345430	5564.195921	24.454835
144.699339	5566.569076	24.459853
145.054384	5565.990129	24.464871
145.086289	5566.328926	24.469888
144.982661	5560.296915	24.474906
145.579993	5555.749475	24.479923
145.399063	5551.131797	24.484941
145.620671	5550.854999	24.489959
145.586597	5550.224015	24.494976
145.398922	5555.825048	24.499994
145.655888	5553.675633	24.505011
145.590387	5569.886306	24.510029
145.855545	5583.638362	24.515047
145.769372	5585.625368	24.520064
146.038875	5590.332928	24.525082
146.172767	5588.786122	24.530099
146.177072	5616.171882	24.535117
146.344359	5613.264944	24.540135
146.467819	5616.445878	24.545152
146.504968	5635.921055	24.550170
146.728087	5634.589752	24.555187
146.550998	5648.767998	24.560205
147.041097	5662.682527	24.565223
147.090990	5676.389529	24.570240
147.278853	5681.700996	24.575258
147.781955	5694.382980	24.580275
147.695189	5721.885736	24.585293
147.967829	5715.690601	24.590311
148.094536	5716.417112	24.595328
147.863573	5737.129483	24.600346
148.044964	5738.707213	24.605363
148.559121	5748.186120	24.610381
148.657713	5752.118479	24.615399
148.622281	5772.008233	24.620416
148.935027	5770.292846	24.625434
149.406863	5763.883400	24.630451
149.765931	5781.848770	24.635469
149.862724	5792.202264	24.640487
149.794481	5791.638873	24.645504
149.976478	5803.380030	24.650522
150.638362	5794.619293	24.655539
150.548236	5798.897249	24.660557
150.557107	5803.363196	24.665575
151.070093	5794.934614	24.670592
151.305794	5799.170848	24.675610
151.309346	5790.768418	24.680627
151.281620	5797.750000	24.685645
151.266222	5799.594358	24.690663
151.339705	5794.796781	24.695680
151.408499	5787.255694	24.700698
151.323669	5794.587051	24.705715
151.556976	5817.223910	24.710733
151.768821	5818.215369	24.715751
151.755867	5820.049899	24.720768
152.095215	5822.355396	24.725786
152.045958	5841.032669	24.730803
152.216452	5851.744239	24.735821
152.410374	5852.809367	24.740839
152.829999	5849.202047	24.745856
152.330959	5872.305084	24.750874
152.637269	5882.816424	24.755891
152.729525	5887.737233	24.760909
152.730653	5901.473461	24.765927
153.387085	5912.071404	24.770944
153.120143	5912.191928	24.775962
153.375698	5935.594102	24.780979
153.752039	5948.331922	24.785997
153.724045	5952.026454	24.791015
154.011930	5954.759531	24.796032
153.870372	5974.178673	24.801050
154.150800	5972.206419	24.806067
154.245072	5985.154468	24.811085
154.492753	5988.482474	24.816103
154.817280	6003.407202	24.821120
154.815258	6009.605084	24.826138
154.965335	6005.708681	24.831155
155.039959	6026.266516	24.836173
155.231598	6034.491757	24.841191
155.671462	6034.703365	24.846208
155.436857	6043.680287	24.851226
156.145862	6053.432025	24.856243
156.189171	6066.041298	24.861261
156.053957	6070.922118	24.866279
156.320489	6070.313994	24.871296
156.561877	6091.801277	24.876314
156.655335	6096.135021	24.881331
156.467798	6103.965993	24.886349
156.575260	6115.397486	24.891367
156.838371	6123.668030	24.896384
156.794938	6129.825357	24.901402
156.963882	6149.050452	24.906419
157.293923	6161.785610	24.911437
157.465058	6169.073980	24.916455
157.857128	6192.468957	24.921472
158.012866	6202.158729	24.926490
158.263146	6196.636522	24.931507
158.349789	6219.915800	24.936525
158.381527	6229.129679	24.941543
158.699418	6236.889578	24.946560
158.384585	6241.846300	24.951578
159.000259	6255.151272	24.956595
159.183625	6259.916056	24.961613
159.188126	6266.079172	24.966631
159.680082	6279.716250	24.971648
160.003560	6282.708078	24.976666
160.149455	6277.768978	24.981683
160.212681	6284.825982	24.986701
160.444815	6296.953724	24.991719
160.695122	6276.623161	24.996736
160.587936	6291.967924	25.001754
160.717132	6300.020732	25.006771
160.997899	6309.866883	25.011789
160.795581	6312.999986	25.016807
161.507336	6308.781060	25.021824
161.091911	6329.486686	25.026842
161.612353	6331.981335	25.031859
161.682489	6334.725598	25.036877
161.634844	6350.957094	25.041895
162.247012	6335.125910	25.046912
162.086762	6344.689913	25.051930
162.274311	6348.047259	25.056947
162.561357	6365.621193	25.061965
162.495070	6363.315488	25.066983
162.584224	6371.714618	25.072000
162.552861	6381.743552	25.077018
162.749812	6393.015433	25.082035
163.096299	6401.785049	25.087053
163.464757	6406.811488	25.092071
163.831284	6398.762341	25.097088
163.897896	6393.304751	25.102106
164.359712	6388.615805	25.107123
164.052814	6395.070958	25.112141
164.437495	6411.224937	25.117159
164.827831	6408.963656	25.122176
164.725048	6415.169904	25.127194
164.479749	6405.853982	25.132211
164.704105	6408.849838	25.137229
164.684219	6421.186239	25.142247
164.950117	6430.183519	25.147264
164.964727	6444.422443	25.152282
165.176286	6452.034966	25.157299
165.558886	6471.346797	25.162317
165.257829	6482.492790	25.167335
165.501073	6482.726315	25.172352
165.754339	6503.478996	25.177370
166.068043	6512.684290	25.182387
166.162866	6514.961219	25.187405
166.133176	6539.689180	25.192423
166.490851	6540.138144	25.197440
166.694363	6548.866912	25.202458
166.868304	6572.852758	25.207475
166.935614	6574.957837	25.212493
167.306159	6570.683874	25.217511
168.138489	6568.502382	25.222528
168.260297	6585.299587	25.227546
168.333203	6586.314039	25.232563
168.735559	6573.244725	25.237581
168.726301	6586.712580	25.242599
168.824096	6569.716845	25.247616
168.884166	6580.330100	25.252634
168.861567	6572.151706	25.257651
169.028086	6590.151119	25.262669
168.981082	6598.020529	25.267687
169.597933	6602.231635	25.272704
169.352440	6615.357935	25.277722
169.365082	6606.724631	25.282739
170.109971	6620.088016	25.287757
169.848262	6634.389273	25.292775
170.017097	6632.875343	25.297792
169.930875	6639.838321	25.302810
169.826980	6660.034449	25.307827
170.363474	6665.346553	25.312845
170.232014	6685.446398	25.317863
170.706357	6687.666780	25.322880
170.716313	6692.953474	25.327898
171.191910	6703.124468	25.332915
171.418124	6716.864905	25.337933
171.191106	6737.698423	25.342951
171.522903	6733.053704	25.347968
171.607021	6754.019395	25.352986
171.671445	6756.807922	25.358003
172.266492	6762.062730	25.363021
172.523378	6776.120143	25.368039
172.961319	6774.407504	25.373056
172.657363	6802.232503	25.378074
172.830511	6805.270439	25.383091
173.230262	6790.011618	25.388109
173.026399	6809.000374	25.393127
173.177888	6816.537686	25.398144
173.357230	6822.505563	25.403162
173.652554	6832.500814	25.408179
173.748928	6841.054850	25.413197
174.015645	6861.151248	25.418215
173.999538	6868.991483	25.423232
174.018209	6875.848936	25.428250
174.288909	6888.681521	25.433267
174.743734	6895.870730	25.438285
174.712712	6910.303853	25.443303
175.169965	6913.816611	25.448320
175.128963	6933.519182	25.453338
175.507044	6926.480564	25.458355
175.874925	6936.129913	25.463373
175.815881	6949.926275	25.468391
176.179991	6941.896108	25.473408
176.223786	6943.930239	25.478426
176.142766	6960.241683	25.483443
176.896961	6968.181834	25.488461
176.577791	6983.339219	25.493479
176.698751	6971.882583	25.498496
176.922679	6990.333627	25.503514
177.277709	6999.760032	25.508531
177.610435	6999.886455	25.513549
177.669796	7014.044040	25.518567
177.688323	7024.813734	25.523584
177.901615	7031.064266	25.528602
178.026432	7033.465535	25.533619
178.531148	7034.033492	25.538637
178.404723	7055.112645	25.543655
178.999514	7049.720893	25.548672
179.182072	7054.521472	25.553690
179.176977	7055.525574	25.558707
179.410838	7061.395156	25.563725
179.463114	7075.207720	25.568743
179.692189	7092.023805	25.573760
179.864327	7086.756863	25.578778
179.476082	7094.515703	25.583795
180.030274	7108.780968	25.588813
179.581227	7126.166687	25.593831
180.041072	7123.315499	25.598848
180.401687	7151.380227	25.603866
180.824178	7152.185550	25.608883
180.987507	7151.647346	25.613901
181.203888	7150.762341	25.618919
181.355623	7161.636793	25.623936
181.618046	7182.107275	25.628954
181.676264	7177.068551	25.633971
182.056727	7170.141959	25.638989
181.978480	7167.472153	25.644007
182.353627	7174.759181	25.649024
182.605425	7201.481292	25.654042
182.372363	7208.050130	25.659059
182.615798	7206.809876	25.664077
182.284552	7220.542873	25.669095
182.775614	7238.129381	25.674112
182.971258	7244.042112	25.679130
183.121167	7261.380101	25.684148
183.410472	7275.603565	25.689165
183.349504	7283.691160	25.694183
183.744509	7300.297690	25.699200
183.792172	7305.095464	25.704218
183.996085	7331.727086	25.709236
184.481502	7327.093890	25.714253
184.384767	7346.277127	25.719271
184.904677	7353.412907	25.724288
184.870534	7363.952040	25.729306
184.700562	7373.430123	25.734324
185.346552	7395.168745	25.739341
185.421382	7401.902606	25.744359
185.527136	7409.803170	25.749376
185.768988	7420.822389	25.754394
185.800344	7430.626431	25.759412
186.203084	7441.682964	25.764429
186.347135	7466.669608	25.769447
186.564341	7454.697601	25.774464
187.087382	7468.184469	25.779482
187.795537	7478.253614	25.784500
188.060984	7474.462762	25.789517
188.148617	7481.501494	25.794535
188.236629	7474.421525	25.799552
188.447364	7477.182927	25.804570
188.562000	7469.167073	25.809588
188.468093	7468.053758	25.814605
188.616679	7475.092998	25.819623
188.792451	7469.261951	25.824640
189.180684	7477.684057	25.829658
189.069529	7500.239914	25.834676
189.129185	7506.571795	25.839693
189.086666	7500.248340	25.844711
189.215035	7509.597112	25.849728
189.474185	7520.276871	25.854746
189.106591	7534.875204	25.859764
189.694279	7551.400939	25.864781
189.720430	7566.631332	25.869799
189.985470	7585.627367	25.874816
190.384571	7592.364698	25.879834
190.383752	7618.905149	25.884852
190.820459	7627.772848	25.889869
191.099758	7637.481630	25.894887
191.137668	7645.977779	25.899904
191.547161	7656.677732	25.904922
191.630888	7669.638374	25.909940
191.548528	7660.877182	25.914957
191.457587	7686.051162	25.919975
191.453570	7694.041770	25.924992
191.852851	7709.133348	25.930010
192.261863	7731.648331	25.935028
192.573648	7742.627526	25.940045
193.153070	7756.924805	25.945063
193.459420	7758.901454	25.950080
193.652076	7759.515261	25.955098
193.712101	7772.680425	25.960116
193.839163	7781.554303	25.965133
194.076400	7781.119180	25.970151
194.116265	7792.812181	25.975168
194.448157	7804.117917	25.980186
194.151762	7814.258526	25.985204
194.848541	7820.688835	25.990221
194.987210	7836.606609	25.995239
195.072394	7846.131656	26.000256
195.574068	7842.787770	26.005274
195.575789	7874.102270	26.010292
195.960811	7873.874928	26.015309
195.985140	7873.395843	26.020327
195.948702	7884.946853	26.025344
196.427683	7883.973517	26.030362
196.481216	7905.744391	26.035380
196.541403	7905.119523	26.040397
196.865483	7917.189868	26.045415
197.205042	7923.046878	26.050432
197.518321	7930.549520	26.055450
197.411852	7941.071476	26.060468
197.689220	7953.727658	26.065485
197.827889	7961.029956	26.070503
197.824342	7973.234807	26.075520
198.238440	7991.766547	26.080538
198.130515	8003.262552	26.085556
198.463314	8026.756038	26.090573
198.470581	8034.889423	26.095591
198.443987	8051.228005	26.100608
198.755315	8059.227158	26.105626
198.986663	8082.505559	26.110644
199.728849	8087.907361	26.115661
199.741795	8091.131235	26.120679
199.757651	8118.269527	26.125696
200.435214	8114.452160	26.130714
200.394654	8122.394920	26.135732
200.653141	8142.732792	26.140749
200.727400	8158.966100	26.145767
200.710342	8168.242468	26.150784
201.168269	8178.262280	26.155802
201.382809	8188.837498	26.160820
201.508332	8184.046596	26.165837
201.825044	8206.067102	26.170855
201.661978	8225.983627	26.175872
202.036856	8220.217337	26.180890
202.153284	8239.059271	26.185908
202.065988	8255.007219	26.190925
202.339581	8258.621193	26.195943
202.514239	8287.755632	26.200960
203.058486	8291.377221	26.205978
202.792091	8307.757066	26.210996
203.218673	8329.565873	26.216013
203.360270	8343.525113	26.221031
203.517180	8368.765781	26.226048
204.078734	8375.727022	26.231066
204.360492	8390.374539	26.236084
204.416197	8394.083480	26.241101
204.785116	8398.589203	26.246119
204.818344	8422.807419	26.251136
205.183703	8415.467965	26.256154
205.134182	8438.217252	26.261172
205.561150	8450.832302	26.266189
205.588952	8452.483996	26.271207
205.807502	8493.941575	26.276224
206.371828	8494.254975	26.281242
206.396870	8513.636302	26.286260
206.575321	8534.569783	26.291277
206.874428	8536.485134	26.296295
207.001527	8537.934902	26.301312
207.462064	8563.737749	26.306330
207.450907	8580.084283	26.311348
207.522218	8576.158853	26.316365
207.820216	8584.684895	26.321383
207.643282	8605.899404	26.326400
208.336599	8599.210298	26.331418
208.500084	8628.045398	26.336436
208.854853	8634.303956	26.341453
209.208002	8640.555692	26.346471
209.314265	8661.262422	26.351488
209.555801	8658.051115	26.356506
210.039845	8655.640796	26.361524
210.362578	8648.865952	26.366541
210.849226	8640.051248	26.371559
210.419577	8648.827104	26.376576
211.081067	8655.899242	26.381594
210.995776	8677.421880	26.386612
210.991526	8668.523311	26.391629
211.259060	8676.419216	26.396647
211.183636	8681.760359	26.401664
211.782621	8702.257968	26.406682
211.722986	8714.465676	26.411700
211.593697	8701.661835	26.416717
211.920185	8705.214369	26.421735
211.829735	8718.543246	26.426752
212.139266	8726.851914	26.431770
212.391502	8736.992637	26.436788
212.321764	8750.961160	26.441805
212.822427	8762.795899	26.446823
212.838966	8780.284003	26.451840
213.219749	8784.092702	26.456858
213.369538	8812.751709	26.461876
213.592416	8805.798342	26.466893
213.983493	8826.035348	26.471911
213.970869	8851.994390	26.476928
214.349103	8857.207402	26.481946
214.394908	8883.311029	26.486964
214.303321	8884.812220	26.491981
214.755630	8897.258747	26.496999
214.834835	8919.558970	26.502016
215.251482	8933.081445	26.507034
215.209421	8942.060094	26.512052
215.303663	8972.367058	26.517069
215.797814	8981.771368	26.522087
215.697274	9012.846040	26.527104
216.247201	9012.871764	26.532122
216.945578	9033.071472	26.537140
217.174795	9028.840207	26.542157
217.853995	9039.921539	26.547175
218.092196	9056.566045	26.552192
217.985560	9061.156832	26.557210
218.142942	9059.848309	26.562228
218.206178	9068.166134	26.567245
218.929631	9079.946723	26.572263
218.873301	9090.836864	26.577280
219.142111	9094.360520	26.582298
219.349366	9088.924384	26.587316
219.434561	9112.006162	26.592333
219.604840	9117.023023	26.597351
219.666287	9132.980063	26.602368
219.815796	9144.833312	26.607386
219.811752	9155.328379	26.612404
219.741908	9165.755642	26.617421
220.429685	9184.801612	26.622439
220.027023	9203.138476	26.627456
220.424474	9219.906511	26.632474
220.548084	9231.588467	26.637492
220.742771	9253.818445	26.642509
221.230873	9278.578173	26.647527
221.221778	9290.567781	26.652544
221.837210	9317.008674	26.657562
222.367312	9324.941762	26.662580
222.576309	9348.896186	26.667597
222.799087	9363.057488	26.672615
223.144717	9374.599497	26.677632
223.467889	9378.293982	26.682650
223.540506	9394.572960	26.687668
223.935134	9398.391417	26.692685
224.441750	9398.812809	26.697703
224.375427	9416.218460	26.702720
224.740585	9415.423724	26.707738
225.083475	9407.724583	26.712756
224.949358	9419.457213	26.717773
225.085302	9400.142843	26.722791
225.232580	9421.543694	26.727808
225.457327	9433.959661	26.732826
225.709420	9435.736251	26.737844
225.775759	9445.517149	26.742861
225.879649	9457.525866	26.747879
226.051599	9473.571500	26.752896
226.282714	9491.121449	26.757914
226.671822	9498.388905	26.762932
226.567318	9518.215962	26.767949
227.048281	9543.972389	26.772967
226.828237	9543.015562	26.777984
227.170600	9560.756406	26.783002
227.496775	9580.855648	26.788020
227.631544	9590.421513	26.793037
227.860801	9612.022837	26.798055
228.219557	9633.260427	26.803072
228.255435	9648.548835	26.808090
228.640792	9665.204400	26.813108
228.437943	9692.387091	26.818125
228.863224	9700.286330	26.823143
229.217079	9725.258646	26.828160
229.535694	9739.574622	26.833178
229.737152	9771.276767	26.838196
229.756974	9783.795337	26.843213
230.184624	9791.805606	26.848231
230.359405	9818.352649	26.853248
230.546898	9834.262796	26.858266
231.089395	9844.409155	26.863284
231.256774	9869.856084	26.868301
231.886246	9873.867421	26.873319
232.136616	9879.503721	26.878336
232.029365	9898.561256	26.883354
232.846024	9902.270071	26.888372
233.194186	9903.859447	26.893389
233.268146	9919.343922	26.898407
233.295417	9927.968192	26.903424
233.700427	9929.651605	26.908442
233.588544	9939.710316	26.913460
233.710321	9961.581899	26.918477
234.285101	9962.251760	26.923495
234.346548	9983.148072	26.928512
234.484865	10002.131177	26.933530
234.642324	10001.966457	26.938548
234.951079	10028.778980	26.943565
235.006977	10038.375411	26.948583
235.138126	10043.584158	26.953600
235.281990	10073.872447	26.958618
235.749236	10076.116529	26.963636
235.787888	10105.684631	26.968653
235.850755	10124.430045	26.973671
236.201885	10146.170896	26.978688
236.713508	10153.858683	26.983706
236.585949	10182.739621	26.988724
236.520388	10190.360064	26.993741
237.059943	10203.770445	26.998759
237.323280	10221.803660	27.003776
237.750869	10248.421737	27.008794
238.066462	10255.032720	27.013812
238.283082	10281.028908	27.018829
238.320734	10292.402324	27.023847
238.647362	10305.699567	27.028864
238.930730	10311.865150	27.033882
239.220997	10321.129666	27.038900
239.289030	10348.064553	27.043917
239.521137	10360.454142	27.048935
239.845186	10382.590402	27.053952
239.967821	10392.084339	27.058970
240.355863	10405.957026	27.063988
240.308510	10425.406464	27.069005
240.697949	10444.556295	27.074023
241.093964	10456.207192	27.079040
241.518599	10481.161218	27.084058
241.630443	10483.602498	27.089076
241.865035	10513.173613	27.094093
242.114806	10507.429552	27.099111
242.154908	10527.413536	27.104128
242.490539	10552.954032	27.109146
242.935079	10557.611276	27.114164
242.890632	10576.353502	27.119181
243.185396	10588.671509	27.124199
243.637279	10613.003597	27.129216
243.524402	10620.862398	27.134234
244.067789	10637.134575	27.139252
244.076570	10646.676728	27.144269
244.761205	10663.288843	27.149287
245.130150	10670.393629	27.154304
245.147864	10699.661652	27.159322
245.727708	10705.055284	27.164340
245.604968	10717.998740	27.169357
246.063512	10735.948724	27.174375
246.111260	10738.190519	27.179392
246.350140	10761.277874	27.184410
246.565954	10765.111022	27.189428
246.655752	10782.482737	27.194445
246.762765	10804.569608	27.199463
247.100143	10823.786461	27.204480
247.254380	10840.845750	27.209498
247.777615	10853.180680	27.214516
248.020677	10877.329653	27.219533
247.890057	10883.731068	27.224551
248.894367	10894.006798	27.229568
248.969062	10903.467379	27.234586
249.390824	10915.568652	27.239604
249.271996	10937.363520	27.244621
249.677055	10942.742599	27.249639
249.944883	10958.939419	27.254656
249.943681	10978.680304	27.259674
250.381294	10974.160280	27.264692
250.487802	10998.249360	27.269709
250.680110	11005.677997	27.274727
250.783451	11016.085621	27.279744
250.706301	11032.632258	27.284762
250.987563	11038.334118	27.289780
251.255527	11062.952040	27.294797
251.445077	11088.112185	27.299815
251.426196	11101.376664	27.304832
251.634000	11133.374230	27.309850
252.199407	11153.294591	27.314868
252.483619	11180.401924	27.319885
252.541125	11206.052791	27.324903
253.089320	11218.794888	27.329920
253.403200	11246.536306	27.334938
253.656013	11259.623816	27.339956
254.150579	11276.012884	27.344973
254.133292	11291.789766	27.349991
254.312879	11318.500423	27.355008
254.241563	11352.077713	27.360026
254.859761	11356.091060	27.365044
255.053014	11381.809722	27.370061
255.566457	11404.102647	27.375079
255.660634	11422.241788	27.380096
255.695767	11452.226294	27.385114
256.269502	11462.019119	27.390132
256.226989	11488.913251	27.395149
256.428009	11510.258520	27.400167
258.033386	11511.765149	27.405184
258.618443	11514.275400	27.410202
259.298356	11508.590692	27.415220
259.637608	11507.770277	27.420237
259.736311	11512.898324	27.425255
260.085162	11512.320174	27.430272
260.317463	11517.080222	27.435290
260.371720	11505.770674	27.440308
260.586026	11506.997474	27.445325
260.267105	11505.459282	27.450343
260.865849	11504.494989	27.455360
260.373561	11515.529170	27.460378
260.710574	11507.016864	27.465396
261.087135	11512.506948	27.470413
260.832711	11538.912528	27.475431
261.342841	11540.386543	27.480448
261.485329	11569.114332	27.485466
261.467234	11571.330345	27.490484
261.723184	11594.472921	27.495501
262.113781	11608.271540	27.500519
262.376369	11622.589384	27.505536
262.157044	11648.791415	27.510554
262.454092	11672.500553	27.515572
262.554894	11694.163705	27.520589
262.721717	11726.680858	27.525607
263.030392	11751.257206	27.530624
263.072621	11772.959519	27.535642
263.435495	11789.342590	27.540660
263.622836	11827.735042	27.545677
263.837462	11855.589029	27.550695
264.496617	11882.629986	27.555712
264.553908	11909.849570	27.560730
264.767131	11927.511662	27.565748
265.332682	11944.837018	27.570765
265.261576	11968.231824	27.575783
265.717224	11975.891300	27.580800
265.849332	12008.033634	27.585818
266.180402	12022.099302	27.590836
266.707902	12050.268597	27.595853
267.375298	12051.292171	27.600871
267.609496	12061.823696	27.605888
267.708147	12078.126997	27.610906
267.844359	12101.590106	27.615924
268.456416	12119.936206	27.620941
268.683111	12156.623861	27.625959
268.820798	12155.675956	27.630976
269.400020	12190.510740	27.635994
269.487537	12190.418150	27.641012
270.013697	12215.709124	27.646029
269.946020	12232.673513	27.651047
270.271035	12242.378194	27.656064
270.218251	12274.972454	27.661082
270.549892	12299.280773	27.666100
271.016354	12310.297699	27.671117
271.152760	12343.330479	27.676135
271.623722	12351.228562	27.681152
271.600360	12371.280978	27.686170
271.555215	12389.837435	27.691188
272.078097	12413.946225	27.696205
272.437171	12442.286744	27.701223
272.926002	12452.689797	27.706240
273.502640	12469.290033	27.711258
273.669495	12484.532093	27.716276
274.344984	12497.992322	27.721293
274.506550	12507.695677	27.726311
275.020743	12511.720213	27.731328
275.028410	12535.277092	27.736346
275.723775	12528.488562	27.741364
275.746139	12533.474060	27.746381
275.938892	12552.607540	27.751399
276.146340	12558.102726	27.756416
276.458334	12569.075588	27.761434
276.383735	12585.433614	27.766452
277.427664	12584.071452	27.771469
277.427127	12586.789558	27.776487
277.378349	12599.759034	27.781504
277.609092	12609.391016	27.786522
277.647032	12614.189869	27.791540
278.414140	12633.031582	27.796557
278.689996	12639.621811	27.801575
278.979928	12635.975338	27.806592
279.243834	12668.066380	27.811610
279.294268	12674.881072	27.816628
279.589623	12676.574612	27.821645
279.901129	12694.460631	27.826663
279.993151	12714.663949	27.831680
279.930586	12733.732876	27.836698
280.148952	12746.106935	27.841716
280.171324	12759.708296	27.846733
280.049031	12792.876562	27.851751
280.467946	12814.374308	27.856768
280.607341	12836.734476	27.861786
281.251642	12867.929366	27.866804
281.679573	12888.095116	27.871821
281.724056	12917.484466	27.876839
281.984673	12942.245543	27.881856
282.106918	12973.341732	27.886874
282.667290	12998.630135	27.891892
282.865124	13012.546853	27.896909
283.043106	13033.129286	27.901927
283.612727	13048.107780	27.906944
283.799839	13075.806236	27.911962
283.851071	13098.667989	27.916980
284.419743	13120.017928	27.921997
284.450723	13151.384852	27.927015
285.102700	13157.424075	27.932032
285.232045	13199.948229	27.937050
285.623235	13222.815610	27.942068
285.907806	13235.941093	27.947085
286.219766	13267.951155	27.952103
286.765992	13272.802824	27.957120
287.290310	13302.226270	27.962138
287.339971	13317.611625	27.967156
287.778063	13332.272982	27.972173
287.868939	13345.595129	27.977191
288.391999	13358.446950	27.982208
288.664471	13381.287049	27.987226
288.736857	13396.746989	27.992244
289.310654	13410.365833	27.997261
289.177257	13434.469068	28.002279
290.005186	13442.596378	28.007296
290.411467	13454.943129	28.012314
290.958602	13480.626259	28.017332
291.695002	13490.662418	28.022349
291.736525	13504.824810	28.027367
291.925618	13506.127921	28.032384
292.246508	13525.863677	28.037402
292.360684	13533.464232	28.042420
292.749517	13527.893672	28.047437
292.845532	13543.294597	28.052455
293.149977	13562.070895	28.057472
293.354594	13565.734841	28.062490
293.263623	13589.633879	28.067508
293.595553	13600.039706	28.072525
293.824161	13621.579455	28.077543
293.932933	13632.440045	28.082560
293.983395	13668.800379	28.087578
294.312883	13682.909462	28.092596
295.000269	13688.365367	28.097613
294.693469	13717.628831	28.102631
295.234888	13733.515892	28.107648
295.697909	13751.113331	28.112666
295.813598	13776.143972	28.117684
296.086852	13797.825829	28.122701
296.090820	13814.668774	28.127719
296.337158	13847.553863	28.132736
296.674920	13862.694198	28.137754
296.661657	13894.552937	28.142772
297.687441	13909.838122	28.147789
297.937274	13943.595762	28.152807
297.929304	13957.575960	28.157824
298.501508	13979.832217	28.162842
298.825609	14004.587656	28.167860
299.381835	14009.156055	28.172877
299.956677	14036.051833	28.177895
300.004810	14046.368094	28.182912
300.284844	14061.486831	28.187930
300.377615	14078.114192	28.192948
300.716804	14103.431320	28.197965
300.970317	14122.996029	28.202983
301.407232	14141.976084	28.208000
301.321392	14171.649575	28.213018
301.705148	14187.370160	28.218036
302.321945	14225.892680	28.223053
302.400448	14241.956094	28.228071
302.698978	14261.102216	28.233088
302.812699	14290.358396	28.238106
302.822032	14310.166962	28.243124
303.540875	14316.094841	28.248141
304.016799	14352.395581	28.253159
304.138220	14376.149421	28.258176
304.602726	14394.011969	28.263194
304.703861	14430.014835	28.268212
305.265967	14439.270731	28.273229
305.481408	14467.235539	28.278247
305.764864	14499.372777	28.283264
306.110224	14517.827953	28.288282
305.832590	14550.929922	28.293300
306.515430	14567.063465	28.298317
306.800615	14602.747702	28.303335
307.263384	14633.116172	28.308352
307.553486	14639.168109	28.313370
307.687299	14671.267365	28.318388
308.038166	14685.082496	28.323405
308.125205	14725.194913	28.328423
308.272686	14731.654970	28.333440
308.677033	14756.881413	28.338458
309.085876	14783.925018	28.343476
310.335445	14794.302318	28.348493
310.631228	14829.964927	28.353511
311.170602	14842.890390	28.358528
311.558572	14846.106808	28.363546
311.444486	14863.106306	28.368564
311.630402	14859.406319	28.373581
311.670421	14880.791024	28.378599
312.167521	14896.146706	28.383616
312.340386	14903.594819	28.388634
312.352400	14934.132360	28.393652
312.790577	14953.724718	28.398669
313.123551	14979.882706	28.403687
313.408450	15004.930602	28.408704
313.596063	15018.384036	28.413722
313.604235	15043.651065	28.418740
314.247047	15065.031968	28.423757
314.405925	15103.536387	28.428775
314.685454	15133.028034	28.433792
315.195557	15154.584121	28.438810
315.134197	15195.225556	28.443828
315.767668	15207.353696	28.448845
316.131877	15246.593330	28.453863
316.160891	15277.259232	28.458880
316.680738	15295.153672	28.463898
317.133273	15317.666639	28.468916
317.569487	15340.258211	28.473933
317.706611	15351.333674	28.478951
318.043648	15363.960976	28.483968
318.852663	15382.537462	28.488986
318.663467	15418.421421	28.494004
318.990089	15444.365795	28.499021
319.510967	15466.880193	28.504039
319.720041	15497.134828	28.509056
320.156163	15512.483626	28.514074
320.339559	15544.668324	28.519092
321.069536	15573.318282	28.524109
321.433628	15573.314847	28.529127
321.474213	15595.080907	28.534144
322.048340	15598.560984	28.539162
322.274971	15621.941868	28.544180
322.420916	15637.534251	28.549197
322.850085	15657.885328	28.554215
323.155079	15676.557259	28.559232
323.908222	15689.852463	28.564250
323.821032	15721.555337	28.569268
324.378074	15738.609843	28.574285
324.671736	15765.211100	28.579303
324.739533	15796.904191	28.584320
325.586321	15813.165266	28.589338
325.590227	15835.654736	28.594356
326.092500	15848.185248	28.599373
326.525027	15854.222646	28.604391
326.546950	15888.857879	28.609408
327.128996	15894.548280	28.614426
327.225095	15909.247821	28.619444
327.209540	15924.859147	28.624461
327.568853	15949.998680	28.629479
327.627180	15963.375330	28.634496
328.275017	15973.552337	28.639514
328.050090	16009.933853	28.644532
328.221397	16043.812450	28.649549
328.442399	16079.439289	28.654567
328.627464	16090.623870	28.659584
329.095114	16127.280872	28.664602
329.123042	16155.285030	28.669620
329.769315	16185.717180	28.674637
329.721704	16216.615837	28.679655
329.857584	16270.275934	28.684672
330.445157	16304.596190	28.689690
330.855683	16342.142240	28.694708
331.021564	16376.234810	28.699725
331.827722	16409.126314	28.704743
332.433033	16431.378104	28.709760
333.348066	16454.645820	28.714778
333.573674	16472.828661	28.719796
334.091073	16488.993160	28.724813
334.266699	16504.630111	28.729831
334.524827	16530.867126	28.734848
334.900863	16546.109616	28.739866
334.972877	16571.422903	28.744884
335.247161	16594.754955	28.749901
336.096411	16611.707374	28.754919
336.160069	16635.505103	28.759936
336.581462	16657.229885	28.764954
336.753842	16689.502184	28.769972
337.001892	16708.209635	28.774989
337.192716	16732.262029	28.780007
337.513672	16764.400973	28.785024
337.854903	16789.861266	28.790042
338.224327	16833.627196	28.795060
338.378372	16850.537332	28.800077
338.986228	16876.376509	28.805095
339.432194	16905.264748	28.810112
339.628963	16917.848560	28.815130
340.083997	16946.561822	28.820148
340.354875	16973.223513	28.825165
341.132547	16993.888512	28.830183
341.447898	17020.359350	28.835200
341.721562	17039.104850	28.840218
342.199110	17046.663016	28.845236
342.118164	17081.833817	28.850253
342.845587	17094.818810	28.855271
342.813595	17130.403157	28.860288
343.044560	17144.810938	28.865306
343.114808	17183.287622	28.870324
343.644975	17202.356992	28.875341
344.615898	17233.526444	28.880359
344.484286	17259.164434	28.885376
345.201509	17282.692083	28.890394
345.384099	17309.993003	28.895412
345.500565	17335.156169	28.900429
346.374073	17360.454629	28.905447
346.584734	17391.459346	28.910464
346.842297	17414.275436	28.915482
346.796659	17437.864263	28.920500
347.506079	17457.823463	28.925517
347.482029	17483.839945	28.930535
347.438229	17503.410984	28.935552
348.100995	17525.639452	28.940570
348.371098	17559.666445	28.945588
348.318961	17593.718881	28.950605
349.042420	17613.379595	28.955623
349.406769	17646.394537	28.960640
349.629880	17671.488105	28.965658
350.089120	17703.131378	28.970676
350.270723	17728.240313	28.975693
350.671307	17758.141496	28.980711
350.801330	17798.525115	28.985728
351.363655	17828.714436	28.990746
351.365594	17859.737207	28.995764
351.341293	17891.065008	29.000781
352.129437	17914.459090	29.005799
352.830203	17940.795869	29.010816
353.438326	17956.472648	29.015834
353.914046	17985.975683	29.020852
354.172664	18009.067677	29.025869
355.193231	18023.088635	29.030887
355.526157	18053.808261	29.035904
355.478750	18065.278168	29.040922
356.040186	18090.064560	29.045940
356.072828	18115.873455	29.050957
356.821612	18131.752016	29.055975
356.602706	18170.040604	29.060992
356.830062	18188.722038	29.066010
356.941955	18207.268742	29.071028
357.096712	18248.411017	29.076045
357.828966	18275.165403	29.081063
357.975078	18318.927012	29.086080
358.410602	18337.846719	29.091098
358.884997	18376.784801	29.096116
359.394520	18413.669290	29.101133
359.831949	18439.574852	29.106151
359.992244	18487.128099	29.111168
360.141824	18514.542698	29.116186
360.501279	18543.925157	29.121204
360.816711	18577.746359	29.126221
361.368283	18608.884225	29.131239
361.278776	18657.630602	29.136256
361.992156	18674.179171	29.141274
362.739207	18709.997331	29.146292
362.692339	18740.993410	29.151309
363.499830	18778.335638	29.156327
363.425980	18795.344054	29.161344
364.041448	18832.027996	29.166362
364.528712	18861.980485	29.171380
364.655886	18898.075820	29.176397
365.032782	18915.233812	29.181415
365.448785	18960.068059	29.186432
365.898916	18980.323709	29.191450
366.341779	19010.978094	29.196468
366.477981	19041.411702	29.201485
366.882467	19064.248142	29.206503
367.259216	19090.886950	29.211520
367.539159	19119.935108	29.216538
368.199986	19144.643559	29.221556
368.129415	19181.341575	29.226573
368.730431	19201.732143	29.231591
368.950204	19236.870121	29.236608
368.914485	19266.384241	29.241626
369.676997	19294.254553	29.246644
369.758946	19339.076579	29.251661
370.186731	19371.018046	29.256679
370.947554	19405.774098	29.261696
371.361220	19425.821157	29.266714
371.671901	19457.017215	29.271732
372.260487	19490.101919	29.276749
372.657052	19518.801495	29.281767
372.729874	19552.178380	29.286784
372.891646	19579.642516	29.291802
373.585479	19601.859561	29.296820
373.482484	19650.070569	29.301837
374.390098	19680.093489	29.306855
374.770978	19712.222282	29.311872
375.123582	19744.036318	29.316890
375.467377	19783.031401	29.321908
375.684915	19814.176471	29.326925
376.193311	19841.776407	29.331943
376.588357	19883.277656	29.336960
376.979970	19902.854768	29.341978
377.245287	19930.050625	29.346996
377.467785	19963.551798	29.352013
377.849374	19999.552431	29.357031
378.277618	20038.240166	29.362048
378.552869	20076.901975	29.367066
378.941910	20097.919306	29.372084
379.097144	20145.166544	29.377101
380.120206	20165.574598	29.382119
380.515191	20207.189330	29.387136
380.819798	20250.707432	29.392154
381.076739	20265.328562	29.397172
381.170447	20299.131723	29.402189
382.020680	20343.419568	29.407207
382.853035	20382.123692	29.412224
383.098169	20409.707122	29.417242
383.636929	20439.441011	29.422260
383.886144	20464.542390	29.427277
384.320018	20481.165775	29.432295
385.014872	20495.149532	29.437312
385.189687	20519.524940	29.442330
385.925583	20543.473917	29.447348
385.890070	20565.890455	29.452365
386.632444	20583.729570	29.457383
386.580234	20598.764113	29.462400
386.883363	20635.911971	29.467418
387.490538	20653.888477	29.472436
387.381020	20673.740927	29.477453
387.831796	20696.837777	29.482471
388.166497	20720.069713	29.487488
388.266503	20749.890642	29.492506
388.969175	20774.874585	29.497524
388.962934	20806.585329	29.502541
389.416353	20830.003272	29.507559
389.937706	20852.236981	29.512576
390.102811	20887.637021	29.517594
391.121173	20907.282483	29.522612
391.889189	20915.297934	29.527629
392.374534	20940.923186	29.532647
392.861541	20968.350137	29.537664
392.814319	20987.539386	29.542682
393.343022	20994.958242	29.547700
393.569612	21027.237173	29.552717
393.837315	21054.573209	29.557735
393.977537	21080.199338	29.562752
394.493246	21109.163213	29.567770
394.928261	21136.446743	29.572788
394.817691	21166.517017	29.577805
395.162450	21191.805163	29.582823
395.404953	21228.960933	29.587840
395.910329	21263.723226	29.592858
396.298490	21296.637734	29.597876
396.695167	21333.300580	29.602893
397.241258	21376.066236	29.607911
397.340222	21415.494626	29.612928
397.671460	21448.944622	29.617946
398.367984	21479.006603	29.622964
398.749142	21525.627365	29.627981
398.949159	21564.884085	29.632999
399.985665	21592.294663	29.638016
399.952673	21641.105083	29.643034
400.387560	21666.761610	29.648052
400.901004	21697.964467	29.653069
400.774855	21748.549536	29.658087
401.399473	21780.283006	29.663104
401.759116	21819.432228	29.668122
402.448421	21851.216179	29.673140
402.958789	21891.408757	29.678157
403.091654	21922.032379	29.683175
403.798167	21950.572813	29.688192
404.211127	21993.436966	29.693210
404.577926	22016.822435	29.698228
405.251446	22057.746330	29.703245
405.472995	22089.679327	29.708263
405.862667	22127.134318	29.713280
406.077706	22166.466537	29.718298
406.670202	22190.171515	29.723316
406.966387	22226.201091	29.728333
407.409826	22268.538944	29.733351
407.954295	22300.881672	29.738368
408.052129	22340.804023	29.743386
408.616058	22359.085521	29.748404
409.083132	22384.740451	29.753421
409.621010	22414.129297	29.758439
410.011639	22439.053765	29.763456
410.184847	22461.601986	29.768474
410.898658	22489.013563	29.773492
411.026869	22521.152121	29.778509
411.552310	22547.812484	29.783527
411.902390	22568.808610	29.788544
412.358144	22614.716555	29.793562
412.793637	22639.519983	29.798580
412.708235	22675.843734	29.803597
413.265635	22715.766268	29.808615
413.904797	22745.293183	29.813632
414.093821	22791.378037	29.818650
414.784617	22817.920355	29.823668
414.676448	22853.584154	29.828685
415.087179	22886.930798	29.833703
415.836217	22927.618070	29.838720
415.717890	22971.270530	29.843738
416.204554	23007.989873	29.848756
416.790507	23057.099862	29.853773
416.898255	23098.049642	29.858791
417.706574	23129.115400	29.863808
417.614975	23172.357720	29.868826
418.369961	23218.243365	29.873844
418.920904	23259.353733	29.878861
419.476535	23298.915691	29.883879
420.046199	23343.741093	29.888896
420.454413	23385.862270	29.893914
420.753474	23416.352811	29.898932
421.458113	23460.217340	29.903949
422.156492	23488.286093	29.908967
422.636520	23518.444741	29.913984
422.851907	23551.746713	29.919002
423.431289	23572.618627	29.924020
424.123323	23601.065103	29.929037
424.420920	23633.786228	29.934055
424.904470	23635.800561	29.939072
425.249651	23668.594521	29.944090
425.689356	23685.849724	29.949108
426.390162	23722.610646	29.954125
426.327494	23746.068670	29.959143
426.719495	23778.244936	29.964160
426.993497	23828.839038	29.969178
427.443128	23861.905051	29.974196
428.022475	23903.216574	29.979213
428.161452	23952.997622	29.984231
428.594684	23982.543111	29.989248
429.138550	24023.959851	29.994266
429.420768	24062.729943	29.999284
429.751855	24083.588526	30.004301
429.921233	24133.573248	30.009319
430.612726	24161.043266	30.014336
431.034141	24206.038870	30.019354
431.578785	24237.040105	30.024372
432.238361	24262.918686	30.029389
432.541187	24290.832107	30.034407
433.024899	24319.787268	30.039424
433.021355	24360.989615	30.044442
433.603547	24398.646944	30.049460
433.682443	24435.841805	30.054477
434.019767	24478.110291	30.059495
434.391261	24520.422284	30.064512
434.841420	24569.384488	30.069530
435.360045	24605.289489	30.074548
436.002533	24654.005472	30.079565
436.052670	24702.700967	30.084583
436.739683	24738.859088	30.089600
437.202248	24771.505062	30.094618
437.800864	24818.853140	30.099636
438.419085	24849.454699	30.104653
438.579872	24879.781799	30.109671
439.194491	24914.612682	30.114688
439.747440	24971.948480	30.119706
440.271699	24999.964931	30.124724
440.403519	25048.276644	30.129741
440.808323	25093.201769	30.134759
441.074627	25135.152448	30.139776
441.654395	25178.390915	30.144794
441.980319	25218.842657	30.149812
443.002527	25247.475805	30.154829
443.270255	25286.043990	30.159847
444.224179	25318.215764	30.164864
444.493525	25361.121326	30.169882
445.291809	25381.748831	30.174900
446.148442	25412.063762	30.179917
445.827367	25435.919928	30.184935
446.666033	25464.469268	30.189952
446.888812	25506.994266	30.194970
447.154365	25536.531532	30.199988
447.666577	25577.296398	30.205005
447.732656	25610.485435	30.210023
448.236010	25650.485385	30.215040
448.750995	25681.504392	30.220058
449.144246	25726.084143	30.225076
449.750317	25749.268396	30.230093
450.067895	25796.229281	30.235111
451.387779	25817.506111	30.240128
452.140768	25836.498086	30.245146
452.656077	25867.664720	30.250164
453.559767	25881.663328	30.255181
454.202777	25895.181170	30.260199
454.290519	25894.938014	30.265216
454.548349	25924.478801	30.270234
454.901232	25939.559413	30.275252
455.377128	25956.427655	30.280269
455.539141	25986.784227	30.285287
455.760119	26003.066827	30.290304
455.911878	26029.218250	30.295322
456.383410	26059.490986	30.300340
456.656063	26082.620125	30.305357
456.756376	26110.837626	30.310375
457.434420	26139.780094	30.315392
457.644513	26181.197301	30.320410
458.135542	26210.319375	30.325428
458.324381	26245.073667	30.330445
458.380981	26293.253001	30.335463
458.911406	26331.169714	30.340480
459.319032	26374.996610	30.345498
459.553649	26428.002534	30.350516
459.986547	26470.559633	30.355533
460.394440	26526.944045	30.360551
460.817911	26573.299459	30.365568
461.400966	26625.888910	30.370586
462.013654	26673.070053	30.375604
463.491253	26700.512172	30.380621
463.921271	26734.497986	30.385639
464.470648	26767.798344	30.390656
465.182079	26806.683172	30.395674
465.043799	26837.943207	30.400692
465.633900	26882.969875	30.405709
465.865719	26922.343431	30.410727
466.540287	26954.775722	30.415744
467.012004	26997.786558	30.420762
467.467821	27037.741598	30.425780
468.173728	27063.425099	30.430797
468.425541	27108.299083	30.435815
468.810301	27144.862171	30.440832
469.373195	27182.395969	30.445850
469.761238	27225.713827	30.450868
470.116310	27259.754444	30.455885
470.274985	27300.135645	30.460903
471.075941	27345.958062	30.465920
471.678411	27387.097617	30.470938
471.569884	27442.992355	30.475956
472.336203	27486.392466	30.480973
472.467612	27537.240001	30.485991
472.630821	27581.245414	30.491008
473.423105	27623.571818	30.496026
474.036519	27681.467041	30.501044
474.935343	27716.023940	30.506061
475.031756	27763.132152	30.511079
475.866645	27797.696260	30.516096
476.544568	27847.956610	30.521114
476.506551	27893.890597	30.526132
477.141172	27929.548972	30.531149
477.344514	27981.869262	30.536167
478.024250	28020.139625	30.541184
478.766101	28074.139323	30.546202
479.188203	28117.113767	30.551220
479.718337	28161.779298	30.556237
479.719855	28207.665327	30.561255
480.249135	28254.862015	30.566272
480.871104	28294.292579	30.571290
481.031770	28342.788420	30.576308
482.331429	28374.827730	30.581325
482.271425	28426.923514	30.586343
482.925095	28452.894899	30.591360
484.162913	28473.141201	30.596378
484.687356	28500.542053	30.601396
485.296109	28524.856615	30.606413
485.653386	28561.179873	30.611431
486.140810	28579.886475	30.616448
486.754195	28607.066903	30.621466
486.475271	28635.410679	30.626484
486.981664	28665.490497	30.631501
487.702358	28705.344426	30.636519
487.971972	28741.206139	30.641536
488.319606	28782.277950	30.646554
488.463521	28830.253148	30.651572
489.102169	28864.838192	30.656589
489.426687	28924.277811	30.661607
489.986256	28971.311018	30.666624
490.643302	29015.678174	30.671642
490.693576	29058.046160	30.676660
491.253111	29100.820086	30.681677
491.359467	29159.423840	30.686695
491.766737	29208.275379	30.691712
492.356834	29271.399422	30.696730
492.758470	29330.643856	30.701748
493.374302	29383.170853	30.706765
493.637540	29437.353763	30.711783
494.400837	29502.818171	30.716800
494.868683	29551.856506	30.721818
494.936898	29617.033382	30.726836
495.607963	29672.291521	30.731853
496.006662	29737.236571	30.736871
496.507407	29800.621171	30.741888
497.617145	29846.645744	30.746906
498.354852	29900.931121	30.751924
499.249099	29932.194948	30.756941
500.261749	29977.857122	30.761959
500.737715	30012.158475	30.766976
501.549712	30039.697356	30.771994
501.994144	30089.691363	30.777012
502.788722	30106.604589	30.782029
503.133181	30136.504890	30.787047
503.811045	30169.184223	30.792064
504.244769	30207.024549	30.797082
504.247998	30238.601108	30.802100
504.615197	30262.444545	30.807117
504.925044	30310.232177	30.812135
505.319459	30352.709454	30.817152
506.263248	30386.130146	30.822170
506.169320	30428.516774	30.827188
507.111095	30477.343705	30.832205
507.494729	30523.821551	30.837223
507.587532	30570.276511	30.842240
508.256422	30607.947916	30.847258
508.455752	30655.323897	30.852276
509.013846	30696.699548	30.857293
509.218346	30750.439107	30.862311
509.251749	30783.822806	30.867328
509.943433	30807.341115	30.872346
510.069373	30872.718680	30.877364
510.644566	30916.590242	30.882381
511.030639	30975.438060	30.887399
511.671836	31032.877402	30.892416
512.160062	31092.492684	30.897434
512.338900	31167.223436	30.902452
512.771639	31228.205074	30.907469
513.005274	31284.720420	30.912487
513.486247	31362.738992	30.917504
514.129931	31427.541388	30.922522
514.891305	31501.668624	30.927540
515.427311	31558.656871	30.932557
516.281785	31625.059352	30.937575
516.842965	31688.356512	30.942592
517.464512	31752.161279	30.947610
517.766324	31809.089976	30.952628
518.156431	31866.799195	30.957645
519.040300	31928.197027	30.962663
519.758392	31992.028327	30.967680
520.635366	32045.371827	30.972698
521.038770	32105.169788	30.977716
521.626413	32150.626736	30.982733
522.145525	32201.776935	30.987751
523.007714	32258.413016	30.992768
523.906427	32289.346485	30.997786
524.705826	32334.347787	31.002804
525.455356	32366.644947	31.007821
526.213640	32404.202206	31.012839
526.515508	32446.884053	31.017856
527.388095	32476.698188	31.022874
527.156868	32513.514858	31.027892
527.814233	32546.586796	31.032909
528.330417	32587.396980	31.037927
528.968550	32633.567559	31.042944
529.436780	32664.942298	31.047962
529.788514	32714.181963	31.052980
530.144197	32748.180331	31.057997
530.949541	32788.554043	31.063015
530.904677	32838.683209	31.068032
531.689890	32876.850422	31.073050
531.868451	32927.360403	31.078068
532.237077	32981.883415	31.083085
533.032593	33030.995014	31.088103
533.530938	33087.756525	31.093120
533.966875	33128.577673	31.098138
534.559258	33187.933311	31.103156
535.310523	33226.950059	31.108173
535.762050	33281.817097	31.113191
536.018715	33342.402684	31.118208
536.505869	33383.419648	31.123226
536.754314	33437.942810	31.128244
537.167978	33498.946908	31.133261
537.982406	33544.147730	31.138279
537.990390	33596.308961	31.143296
538.725385	33647.662544	31.148314
538.872879	33714.394112	31.153332
539.449763	33775.663277	31.158349
540.009914	33837.595827	31.163367
540.078868	33900.476997	31.168384
541.076741	33964.090063	31.173402
541.182347	34031.940917	31.178420
541.946126	34116.882410	31.183437
542.718835	34183.360213	31.188455
543.154057	34260.504345	31.193472
543.892402	34313.003918	31.198490
544.437216	34387.093453	31.203508
545.457801	34435.486049	31.208525
546.689197	34481.816359	31.213543
547.839868	34520.206602	31.218560
548.821520	34546.751791	31.223578
549.450124	34574.182456	31.228596
549.967521	34608.970740	31.233613
550.594841	34642.057958	31.238631
550.787434	34675.676378	31.243648
551.438689	34716.341020	31.248666
551.907535	34745.058565	31.253684
552.360122	34770.014196	31.258701
553.186772	34803.019540	31.263719
553.334867	34840.471422	31.268736
553.877419	34874.215796	31.273754
554.567166	34910.298331	31.278772
554.608118	34955.118568	31.283789
554.875268	34998.031631	31.288807
555.273655	35055.112155	31.293824
555.766742	35098.369421	31.298842
555.932993	35163.885185	31.303860
556.435284	35212.342100	31.308877
557.379100	35274.704446	31.313895
557.537187	35346.421001	31.318912
558.434734	35394.311010	31.323930
559.044050	35447.950877	31.328948
559.452264	35507.451323	31.333965
560.215994	35550.654042	31.338983
560.459166	35613.862327	31.344000
561.447304	35666.539211	31.349018
561.823843	35727.737103	31.354036
562.610718	35777.261787	31.359053
563.197246	35815.445330	31.364071
563.502091	35890.806307	31.369088
564.080296	35924.934957	31.374106
564.855461	35989.754727	31.379124
565.339235	36040.389490	31.384141
566.312820	36070.717430	31.389159
566.913076	36127.028471	31.394176
567.675496	36154.377362	31.399194
568.065865	36198.971851	31.404212
568.573064	36245.624214	31.409229
569.337148	36283.433698	31.414247
569.435170	36330.715884	31.419264
569.707826	36382.009633	31.424282
570.213274	36425.768142	31.429300
570.776135	36473.312513	31.434317
570.973534	36539.836142	31.439335
571.489255	36590.885280	31.444352
572.123794	36644.074046	31.449370
572.322844	36703.161131	31.454388
572.924650	36766.431729	31.459405
573.722592	36824.613469	31.464423
574.059811	36894.192252	31.469440
574.314502	36962.841628	31.474458
575.105813	37020.586792	31.479476
575.760148	37083.949547	31.484493
576.327196	37154.829814	31.489511
576.865656	37232.597127	31.494528
577.455516	37293.623267	31.499546
578.251477	37361.644106	31.504564
578.430983	37432.451664	31.509581
579.298279	37491.822953	31.514599
580.161331	37556.399838	31.519616
580.488217	37621.284676	31.524634
581.509582	37683.760304	31.529652
582.323501	37744.992053	31.534669
583.251744	37790.490549	31.539687
583.528586	37863.898630	31.544704
584.167451	37913.716500	31.549722
584.889627	37976.879442	31.554740
585.356134	38027.858778	31.559757
586.144544	38071.579651	31.564775
586.369839	38139.111107	31.569792
586.808081	38200.812720	31.574810
587.519758	38260.143693	31.579828
587.886028	38325.911108	31.584845
588.385111	38385.604348	31.589863
588.705628	38455.851315	31.594880
589.749866	38520.830341	31.599898
590.307959	38589.940999	31.604916
590.080906	38659.186440	31.609933
591.054597	38715.582257	31.614951
591.806574	38788.620655	31.619968
592.099044	38857.530298	31.624986
593.274941	38923.790785	31.630004
594.201222	38981.032336	31.635021
595.286323	39035.429389	31.640039
595.569902	39101.146748	31.645056
595.977211	39150.475309	31.650074
596.567061	39206.099730	31.655092
596.841267	39279.848649	31.660109
597.743692	39339.924110	31.665127
597.826944	39396.039817	31.670144
598.354912	39470.704737	31.675162
599.303480	39519.558681	31.680180
599.551244	39580.882495	31.685197
600.216297	39634.999868	31.690215
600.837919	39706.750989	31.695232
601.374719	39752.613554	31.700250
601.812317	39821.551293	31.705268
602.322716	39891.363948	31.710285
603.265389	39949.812498	31.715303
603.630032	40013.180300	31.720320
604.200108	40074.733677	31.725338
605.230317	40135.841841	31.730356
605.252217	40202.158623	31.735373
606.167048	40262.060321	31.740391
606.709622	40333.183264	31.745408
607.366136	40410.179925	31.750426
608.109413	40466.905255	31.755444
608.062279	40538.375278	31.760461
609.354857	40596.704091	31.765479
610.031693	40658.991641	31.770496
610.198819	40726.403838	31.775514
611.155876	40807.006758	31.780532
611.700507	40871.341014	31.785549
612.104388	40933.360781	31.790567
612.779852	41005.780592	31.795584
613.473988	41074.005980	31.800602
614.868331	41131.421505	31.805620
615.556791	41191.586449	31.810637
616.420433	41243.299112	31.815655
616.943128	41293.959134	31.820672
617.505734	41342.834029	31.825690
618.699197	41394.579789	31.830708
618.983128	41445.029103	31.835725
619.348653	41491.690063	31.840743
620.073104	41557.281993	31.845760
620.747107	41599.241745	31.850778
621.860799	41647.733261	31.855796
622.373608	41711.552144	31.860813
622.873369	41757.463833	31.865831
623.486620	41813.040969	31.870848
623.540153	41870.978447	31.875866
624.649908	41905.703190	31.880884
625.017873	41959.197069	31.885901
625.675988	42012.297945	31.890919
626.246351	42074.191231	31.895936
626.814033	42122.853048	31.900954
627.498636	42173.518270	31.905972
627.720854	42242.753960	31.910989
628.054014	42304.515514	31.916007
628.960576	42373.494502	31.921024
629.621647	42430.797730	31.926042
629.923958	42492.974932	31.931060
630.584937	42569.576812	31.936077
630.877972	42636.547450	31.941095
631.128233	42709.020062	31.946112
631.643605	42774.577372	31.951130
632.436396	42844.847575	31.956148
633.086513	42921.247708	31.961165
633.566244	42990.161488	31.966183
634.357297	43056.287925	31.971200
634.947039	43136.452392	31.976218
635.671388	43207.898959	31.981236
636.027307	43282.167803	31.986253
636.776426	43348.838295	31.991271
637.599813	43424.080598	31.996288
637.967182	43495.837556	32.001306
638.744489	43565.535876	32.006324
639.133564	43646.422341	32.011341
639.890682	43724.480882	32.016359
640.584977	43798.877866	32.021376
641.095162	43881.007964	32.026394
641.910463	43941.979341	32.031412
642.743996	44012.405524	32.036429
644.306954	44073.712575	32.041447
644.805248	44142.372456	32.046464
645.383087	44206.669695	32.051482
646.040235	44255.840629	32.056500
646.437375	44307.245588	32.061517
647.092960	44369.297554	32.066535
647.949058	44442.658883	32.071552
648.189110	44505.326414	32.076570
649.021904	44576.319691	32.081588
649.981523	44646.084805	32.086605
650.448077	44710.969478	32.091623
650.967802	44780.562262	32.096640
651.825293	44846.293754	32.101658
652.541312	44909.505281	32.106676
653.282984	44974.637366	32.111693
653.958406	45039.436371	32.116711
654.577971	45108.547658	32.121728
655.301199	45169.512762	32.126746
655.950268	45244.598258	32.131764
656.533036	45307.068975	32.136781
657.226641	45383.274252	32.141799
657.642231	45446.327340	32.146816
658.056324	45512.885957	32.151834
659.002680	45575.665707	32.156852
659.351516	45656.451175	32.161869
660.129346	45727.416873	32.166887
660.996465	45793.487976	32.171904
661.632224	45873.339070	32.176922
662.075790	45952.113741	32.181940
662.604873	46018.110162	32.186957
663.335807	46092.189291	32.191975
663.864001	46168.809231	32.196992
664.831532	46251.480263	32.202010
665.879503	46323.515925	32.207028
666.876391	46400.661705	32.212045
667.315820	46475.230570	32.217063
668.164057	46533.527128	32.222080
668.248865	46607.159174	32.227098
668.605389	46664.597403	32.232116
669.636277	46725.487388	32.237133
670.159020	46788.162247	32.242151
670.609225	46850.129513	32.247168
670.980122	46933.387795	32.252186
671.672314	46995.793469	32.257204
672.237249	47068.713658	32.262221
672.558604	47154.120063	32.267239
673.388078	47226.686425	32.272256
673.642840	47308.557758	32.277274
674.810732	47399.238569	32.282292
675.452078	47475.063688	32.287309
675.783655	47562.300470	32.292327
676.753778	47647.369321	32.297344
676.727053	47733.648005	32.302362
677.597120	47799.757733	32.307380
678.578560	47888.094815	32.312397
679.152628	47969.476627	32.317415
680.015673	48056.138997	32.322432
680.854496	48132.541318	32.327450
681.321809	48220.564345	32.332468
682.240279	48309.178606	32.337485
682.796924	48399.681046	32.342503
683.934497	48474.629973	32.347520
684.430735	48559.636670	32.352538
685.124127	48643.208216	32.357556
686.120180	48721.241490	32.362573
686.726211	48796.894878	32.367591
688.005508	48863.596606	32.372608
688.907170	48940.052359	32.377626
689.845752	49006.316616	32.382644
690.353140	49078.793549	32.387661
691.193631	49142.887165	32.392679
691.884352	49203.369684	32.397696
692.442041	49287.413954	32.402714
692.658746	49353.463105	32.407732
693.464978	49421.895764	32.412749
693.996214	49499.675129	32.417767
694.741628	49575.590486	32.422784
695.346579	49649.856057	32.427802
695.949876	49733.431294	32.432820
696.377624	49819.067104	32.437837
697.206630	49907.422729	32.442855
697.876256	49981.376440	32.447872
698.228257	50075.476423	32.452890
699.205524	50159.262347	32.457908
699.945968	50231.631125	32.462925
700.676475	50326.480030	32.467943
701.304534	50401.013284	32.472960
702.070797	50482.495911	32.477978
703.180739	50569.289007	32.482996
704.317566	50632.671778	32.488013
705.112712	50693.291048	32.493031
706.089127	50757.435101	32.498048
706.422587	50833.304626	32.503066
706.916198	50890.911427	32.508084
708.057837	50961.272139	32.513101
708.185372	51020.916351	32.518119
708.903040	51088.315443	32.523136
709.102463	51161.436846	32.528154
709.783717	51228.381502	32.533172
710.584052	51309.010375	32.538189
711.283282	51389.529470	32.543207
711.598998	51460.162491	32.548224
712.182538	51543.509472	32.553242
712.624908	51631.808921	32.558260
713.652480	51713.113521	32.563277
713.981491	51808.122548	32.568295
715.003049	51900.411801	32.573312
715.511012	51982.074913	32.578330
716.230987	52071.389588	32.583348
717.408216	52162.140503	32.588365
717.477833	52243.410643	32.593383
718.594271	52324.284099	32.598400
719.888498	52405.334761	32.603418
721.309425	52480.520504	32.608436
722.445590	52554.429481	32.613453
722.935722	52628.536294	32.618471
723.903770	52690.113176	32.623488
724.600418	52748.078648	32.628506
725.359135	52811.541933	32.633524
726.008957	52879.261523	32.638541
726.885706	52955.558483	32.643559
727.752901	53009.861713	32.648576
728.139886	53080.158327	32.653594
728.500788	53157.207375	32.658612
729.480428	53219.835242	32.663629
729.856031	53303.674795	32.668647
730.591548	53371.426771	32.673664
730.957236	53452.364828	32.678682
731.905401	53538.598307	32.683700
732.490999	53609.086293	32.688717
732.771625	53697.115416	32.693735
733.701023	53776.563772	32.698752
734.066954	53864.570657	32.703770
734.436184	53964.890422	32.708788
735.527111	54051.261427	32.713805
736.401331	54146.950303	32.718823
736.794861	54240.143728	32.723840
737.280239	54335.147425	32.728858
738.513544	54424.092120	32.733876
739.772446	54512.607053	32.738893
740.365831	54613.399738	32.743911
741.297837	54692.075183	32.748928
742.389115	54776.770322	32.753946
742.757141	54861.644120	32.758964
743.521490	54944.570770	32.763981
743.994301	55028.977279	32.768999
744.621920	55121.834912	32.774016
746.119306	55182.389017	32.779034
746.893149	55249.106525	32.784052
747.834697	55310.926949	32.789069
748.275912	55391.293402	32.794087
749.463229	55448.052996	32.799104
750.616978	55510.550556	32.804122
750.868030	55581.626582	32.809140
751.637338	55626.814728	32.814157
752.456396	55701.756087	32.819175
752.981968	55772.441919	32.824192
753.651964	55837.647117	32.829210
754.332453	55901.799696	32.834228
755.349893	55973.010933	32.839245
755.720778	56046.816025	32.844263
756.609009	56118.405104	32.849280
757.568383	56194.759301	32.854298
757.929220	56274.523696	32.859316
758.286435	56355.447551	32.864333
758.700883	56446.745341	32.869351
759.602064	56518.535954	32.874368
760.168417	56607.256504	32.879386
760.875797	56708.639204	32.884404
761.406150	56800.586390	32.889421
761.859073	56902.869328	32.894439
762.790882	56998.788080	32.899456
763.860575	57089.883731	32.904474
764.154314	57203.315447	32.909492
764.919591	57298.646666	32.914509
765.686657	57412.301071	32.919527
766.300479	57521.289300	32.924544
766.930675	57630.212424	32.929562
767.703980	57733.197164	32.934580
768.438699	57840.229619	32.939597
768.760296	57957.238435	32.944615
769.855501	58066.658373	32.949632
770.742037	58174.988250	32.954650
771.560949	58298.587827	32.959668
772.451030	58418.265214	32.964685
773.272529	58522.500046	32.969703
773.781007	58639.638112	32.974720
775.152166	58749.106549	32.979738
775.857791	58850.195006	32.984756
777.085997	58946.834394	32.989773
778.114730	59054.414289	32.994791
778.881260	59156.025128	32.999808
780.287704	59241.186316	33.004826
780.330165	59342.045174	33.009844
781.322199	59434.143464	33.014861
782.081284	59543.354067	33.019879
782.562415	59654.361875	33.024896
783.657197	59750.385730	33.029914
784.781329	59839.686523	33.034932
785.634615	59926.195522	33.039949
785.861553	60017.231294	33.044967
786.626332	60115.383964	33.049984
787.465587	60197.195057	33.055002
787.816686	60293.715810	33.060020
789.361978	60387.003185	33.065037
789.941330	60471.711192	33.070055
790.941934	60557.129275	33.075072
791.620445	60636.350312	33.080090
791.884003	60731.921057	33.085108
792.905645	60814.558345	33.090125
793.744179	60904.332785	33.095143
794.447570	61000.314833	33.100160
795.629029	61091.980647	33.105178
795.982281	61191.464322	33.110196
796.840640	61280.924802	33.115213
797.253749	61384.984826	33.120231
797.763892	61491.104552	33.125248
798.446928	61585.798189	33.130266
799.442647	61702.230530	33.135284
800.272860	61802.825645	33.140301
801.056762	61907.407389	33.145319
801.820764	62013.691741	33.150336
803.318300	62109.698294	33.155354
804.130905	62211.030984	33.160372
805.031563	62304.537845	33.165389
805.777454	62403.659106	33.170407
806.269919	62510.639977	33.175424
807.167437	62602.743582	33.180442
807.735777	62725.922754	33.185460
808.600887	62824.458827	33.190477
809.632151	62921.806865	33.195495
810.131162	63038.073854	33.200512
810.946079	63134.118463	33.205530
811.669801	63253.894195	33.210548
812.630383	63366.814945	33.215565
813.231096	63482.436872	33.220583
814.288150	63593.357244	33.225600
814.778802	63699.429276	33.230618
815.823317	63806.478001	33.235636
816.612635	63922.189425	33.240653
817.377136	64034.058970	33.245671
817.967536	64151.114040	33.250688
819.146151	64255.478516	33.255706
820.158529	64369.824430	33.260724
820.734031	64482.869925	33.265741
821.323121	64590.181862	33.270759
822.342258	64714.113782	33.275776
823.174092	64816.208932	33.280794
823.627097	64947.827938	33.285812
824.688102	65060.944852	33.290829
825.664566	65173.472661	33.295847
826.338024	65295.299949	33.300864
827.127676	65405.044823	33.305882
827.750474	65529.395662	33.310900
828.915093	65643.974455	33.315917
829.810179	65756.108046	33.320935
830.689784	65870.670383	33.325952
831.828729	65982.115856	33.330970
832.495294	66090.311350	33.335988
833.895943	66169.093085	33.341005
835.428491	66254.101535	33.346023
835.897920	66348.536974	33.351040
836.960137	66432.755651	33.356058
838.035247	66514.158441	33.361076
838.539401	66590.649395	33.366093
839.438537	66686.234115	33.371111
839.849604	66772.591984	33.376128
840.844034	66856.229497	33.381146
841.311968	66955.440683	33.386164
841.940411	67055.883941	33.391181
843.030269	67155.230905	33.396199
843.660665	67247.159309	33.401216
844.500697	67351.291252	33.406234
845.461926	67455.587666	33.411252
846.061130	67557.668030	33.416269
846.845356	67674.596798	33.421287
847.028336	67781.078267	33.426304
848.088752	67883.642871	33.431322
848.562964	68012.992484	33.436340
849.328994	68131.525206	33.441357
850.160372	68248.828969	33.446375
850.716224	68383.215744	33.451392
851.848333	68504.687001	33.456410
852.780269	68639.224169	33.461428
853.427407	68762.183044	33.466445
854.343103	68881.738924	33.471463
855.321298	69012.436442	33.476480
856.893660	69131.592412	33.481498
857.795864	69246.875520	33.486516
858.338922	69370.379162	33.491533
859.392729	69489.297624	33.496551
860.248156	69617.308330	33.501568
861.251565	69721.635421	33.506586
862.162331	69845.658476	33.511604
862.632660	69961.797951	33.516621
863.708646	70083.066804	33.521639
864.003660	70208.618031	33.526656
865.566042	70325.116588	33.531674
866.451762	70443.814851	33.536692
867.337889	70571.807933	33.541709
868.496204	70681.662906	33.546727
869.280778	70810.052793	33.551744
870.107824	70924.852236	33.556762
870.818890	71042.703643	33.561780
871.481877	71157.277808	33.566797
872.313671	71281.619435	33.571815
872.838968	71411.097037	33.576832
874.047068	71524.828359	33.581850
874.480692	71657.664685	33.586868
875.167136	71802.959971	33.591885
876.729606	71917.686054	33.596903
877.520243	72046.259917	33.601920
878.809711	72153.764265	33.606938
879.836946	72261.222462	33.611956
880.761173	72374.972240	33.616973
882.273501	72476.022928	33.621991
882.434652	72579.785113	33.627008
883.149615	72678.846884	33.632026
884.285255	72779.339801	33.637044
884.856640	72891.069736	33.642061
886.267087	72984.379484	33.647079
887.187742	73097.426227	33.652096
888.446661	73193.181270	33.657114
889.458819	73298.227249	33.662132
890.134016	73402.512228	33.667149
890.809240	73492.522682	33.672167
891.399952	73599.779516	33.677184
892.377248	73703.209130	33.682202
892.976272	73815.837171	33.687220
893.386045	73939.118760	33.692237
894.556593	74050.007825	33.697255
895.201889	74179.212577	33.702272
896.398034	74291.583967	33.707290
897.149447	74412.311597	33.712308
897.824041	74538.006680	33.717325
898.693625	74651.803386	33.722343
899.513257	74788.055897	33.727360
900.782332	74910.713778	33.732378
901.607068	75033.063930	33.737396
902.106128	75172.169665	33.742413
903.469917	75299.946459	33.747431
903.967998	75434.358573	33.752448
904.880035	75555.099087	33.757466
906.015615	75685.088657	33.762484
907.274327	75806.837252	33.767501
908.359693	75915.740413	33.772519
908.741223	76054.662360	33.777536
909.902173	76176.605695	33.782554
910.763800	76307.546617	33.787572
911.490201	76435.356163	33.792589
912.557282	76567.688098	33.797607
913.333075	76704.263856	33.802624
914.388617	76833.053722	33.807642
915.491221	76958.657816	33.812660
915.846729	77098.039770	33.817677
916.745433	77216.213598	33.822695
917.664395	77363.142702	33.827712
918.936597	77499.309820	33.832730
919.560895	77628.963389	33.837748
920.543445	77771.220793	33.842765
921.492689	77895.224359	33.847783
922.450735	78038.720033	33.852800
923.144099	78177.688993	33.857818
924.423620	78318.954853	33.862836
925.280591	78457.115908	33.867853
926.266561	78592.406694	33.872871
926.868818	78729.510294	33.877888
928.376876	78852.134963	33.882906
929.010295	78969.906020	33.887924
929.610344	79100.470315	33.892941
930.813794	79219.011746	33.897959
931.339816	79348.432651	33.902976
932.530113	79478.880144	33.907994
933.728717	79591.805075	33.913012
934.683235	79719.124737	33.918029
935.432072	79845.991180	33.923047
935.878018	79980.352974	33.928064
936.988676	80105.823345	33.933082
938.025130	80248.993243	33.938100
938.521776	80380.865301	33.943117
939.400649	80516.343776	33.948135
940.457662	80651.308044	33.953152
941.051868	80815.589885	33.958170
941.991579	80948.716239	33.963188
942.857631	81109.853294	33.968205
943.899689	81253.282086	33.973223
944.740188	81402.996036	33.978240
945.712180	81560.952583	33.983258
946.977554	81707.920727	33.988276
947.829804	81855.967120	33.993293
948.788710	82014.592967	33.998311
949.797231	82145.124064	34.003328
950.608902	82318.145239	34.008346
951.856353	82452.711553	34.013364
952.759854	82612.962847	34.018381
954.083847	82756.078928	34.023399
954.977936	82897.171772	34.028416
955.631589	83045.827155	34.033434
956.985062	83195.731516	34.038452
958.143584	83339.408960	34.043469
959.209556	83479.017927	34.048487
960.347242	83628.283218	34.053504
961.228928	83769.662064	34.058522
962.093535	83914.629372	34.063540
963.296100	84055.446967	34.068557
964.290940	84193.270081	34.073575
965.414391	84328.253789	34.078592
966.452562	84472.299508	34.083610
967.703935	84595.599446	34.088628
968.286781	84742.014543	34.093645
969.366709	84868.669055	34.098663
970.347301	85011.431448	34.103680
971.424259	85138.277723	34.108698
972.612259	85269.096775	34.113716
973.486112	85405.138692	34.118733
974.608900	85530.728095	34.123751
975.385556	85661.058584	34.128768
976.531186	85787.992650	34.133786
977.735964	85920.102915	34.138804
978.649736	86058.286143	34.143821
979.142723	86182.354559	34.148839
980.541932	86304.869471	34.153856
981.685441	86424.561383	34.158874
983.259605	86539.740260	34.163892
983.975199	86654.265945	34.168909
985.020289	86742.852487	34.173927
985.764955	86873.435739	34.178944
986.409634	86987.639353	34.183962
987.294601	87089.032204	34.188980
987.970818	87233.520907	34.193997
988.930080	87345.646573	34.199015
989.827002	87472.320343	34.204032
990.456901	87607.713163	34.209050
991.468487	87744.051552	34.214068
991.854014	87886.055141	34.219085
993.003573	88021.525976	34.224103
993.949368	88163.410640	34.229120
994.474555	88308.183514	34.234138
995.837815	88458.173913	34.239156
996.547945	88607.118325	34.244173
997.656801	88765.296353	34.249191
998.813682	88916.397807	34.254208
999.684548	89060.981591	34.259226
1000.683953	89215.898205	34.264244
1001.406959	89383.172728	34.269261
1002.930320	89532.961693	34.274279
1003.900755	89686.583512	34.279296
1004.502905	89851.749638	34.284314
1005.780855	90004.774579	34.289332
1006.714531	90173.235892	34.294349
1008.098895	90312.528801	34.299367
1008.990736	90470.051740	34.304384
1009.979134	90626.276605	34.309402
1011.292434	90776.638767	34.314420
1012.034115	90941.746653	34.319437
1012.993728	91095.152405	34.324455
1014.084379	91247.690895	34.329472
1014.670032	91418.727983	34.334490
1015.836390	91567.499839	34.339508
1017.181313	91735.730639	34.344525
1018.335549	91902.285379	34.349543
1019.500210	92043.768306	34.354560
1020.541040	92204.960989	34.359578
1021.576071	92349.546682	34.364596
1022.721080	92504.121822	34.369613
1024.128769	92660.408268	34.374631
1025.427778	92789.901475	34.379648
1026.367115	92948.168272	34.384666
1027.683953	93080.430705	34.389684
1028.687650	93231.067576	34.394701
1029.877493	93360.575155	34.399719
1031.214682	93496.764748	34.404736
1032.686607	93632.718685	34.409754
1033.571260	93754.319971	34.414772
1034.459598	93899.476742	34.419789
1035.119818	94025.871835	34.424807
1036.372486	94171.838995	34.429824
1037.252204	94307.157501	34.434842
1038.231301	94414.002819	34.439860
1039.411951	94541.469277	34.444877
1040.460152	94657.052907	34.449895
1041.652814	94759.532929	34.454912
1042.230377	94892.853561	34.459930
1043.476540	95010.982041	34.464948
1044.264847	95136.755772	34.469965
1045.179045	95260.207633	34.474983
1046.145295	95395.911140	34.480000
1046.928127	95532.485965	34.485018
1048.380835	95669.334616	34.490036
1049.166875	95801.071324	34.495053
1049.994996	95937.856481	34.500071
1051.230689	96065.152031	34.505088
1052.463438	96197.547480	34.510106
1053.587755	96326.899177	34.515124
1054.652193	96468.274251	34.520141
1055.441076	96616.842489	34.525159
1056.419138	96739.735593	34.530176
1057.091135	96894.966648	34.535194
1058.344572	97035.777479	34.540212
1059.195772	97185.421304	34.545229
1059.790383	97348.214947	34.550247
1061.033020	97499.234638	34.555264
1062.043764	97666.278910	34.560282
1063.378847	97816.115623	34.565300
1064.351531	97970.192738	34.570317
1065.301229	98126.874732	34.575335
1066.652348	98288.422318	34.580352
1067.169266	98445.017164	34.585370
1068.184560	98615.787676	34.590388
1069.517694	98775.500514	34.595405
1070.182136	98942.299178	34.600423
1071.485625	99105.429122	34.605440
1072.294451	99285.328999	34.610458
1073.441731	99444.645826	34.615476
1074.267079	99630.530967	34.620493
1075.450534	99811.938113	34.625511
1076.586221	99979.567762	34.630528
1077.578304	100155.256807	34.635546
1079.031613	100332.670723	34.640564
1079.994925	100501.147763	34.645581
1080.860722	100669.837679	34.650599
1082.706986	100843.371392	34.655616
1083.616338	101017.397087	34.660634
1084.546003	101186.074268	34.665652
1085.693831	101360.241765	34.670669
1086.870922	101534.108522	34.675687
1088.033573	101692.672745	34.680704
1089.043523	101869.960106	34.685722
1089.767446	102037.954833	34.690740
1090.723027	102210.223017	34.695757
1091.883268	102390.477047	34.700775
1092.948473	102567.798871	34.705792
1094.191643	102739.620236	34.710810
1095.514436	102901.805632	34.715828
1096.418665	103067.007485	34.720845
1097.174608	103243.605272	34.725863
1098.528262	103396.284701	34.730880
1099.083197	103571.157748	34.735898
1100.238509	103739.785781	34.740916
1101.586841	103911.744517	34.745933
1102.535031	104089.159685	34.750951
1103.492718	104263.980131	34.755968
1104.740629	104433.129944	34.760986
1106.319721	104604.012857	34.766004
1107.334258	104783.897014	34.771021
1107.706881	104959.752215	34.776039
1109.025216	105145.045813	34.781056
1110.325526	105326.046713	34.786074
1110.800255	105509.059840	34.791092
1112.203317	105695.015056	34.796109
1113.572195	105878.838095	34.801127
1115.707894	106036.903348	34.806144
1116.297169	106211.353668	34.811162
1118.078576	106371.116597	34.816180
1119.601622	106539.743958	34.821197
1120.637437	106696.868294	34.826215
1122.241661	106859.757435	34.831232
1123.305680	107017.594540	34.836250
1124.528917	107177.932597	34.841268
1125.848708	107329.674296	34.846285
1126.876323	107500.545354	34.851303
1127.767667	107648.433209	34.856320
1128.842898	107806.723054	34.861338
1129.824459	107979.813672	34.866356
1130.750670	108143.129426	34.871373
1131.531430	108315.969562	34.876391
1132.943718	108472.811399	34.881408
1134.002546	108645.483075	34.886426
1134.548852	108821.927488	34.891444
1136.015767	108999.011625	34.896461
1137.113191	109182.092823	34.901479
1138.268777	109350.874162	34.906496
1139.579750	109521.790326	34.911514
1140.803047	109710.824216	34.916532
1142.020537	109896.891893	34.921549
1142.988920	110065.929469	34.926567
1144.637444	110243.405169	34.931584
1145.577392	110417.722342	34.936602
1146.604656	110573.265330	34.941620
1148.188011	110733.563201	34.946637
1149.000577	110897.472450	34.951655
1150.827402	111051.175914	34.956672
1151.742020	111233.554549	34.961690
1152.974009	111416.434774	34.966708
1154.219952	111589.356944	34.971725
1155.196042	111755.556350	34.976743
1156.261375	111923.641724	34.981760
1157.207850	112090.696323	34.986778
1158.058204	112261.343911	34.991796
1159.335815	112419.245191	34.996813
1160.303037	112589.021854	35.001831
1161.256649	112743.450725	35.006848
1162.417772	112899.860619	35.011866
1163.799849	113061.465297	35.016884
1164.979045	113225.268304	35.021901
1165.818555	113408.713024	35.026919
1166.731595	113566.989728	35.031936
1168.004271	113743.056218	35.036954
1168.751476	113923.081856	35.041972
1169.755471	114098.060369	35.046989
1170.763835	114297.450748	35.052007
1172.258358	114474.949488	35.057024
1173.307372	114667.378790	35.062042
1174.410710	114852.583710	35.067060
1175.564971	115041.922318	35.072077
1176.429102	115245.882393	35.077095
1178.035852	115423.445920	35.082112
1178.972248	115624.035768	35.087130
1180.121791	115826.796540	35.092148
1181.559989	116012.881031	35.097165
1182.773227	116212.861696	35.102183
1183.797614	116411.107530	35.107200
1184.831568	116608.523979	35.112218
1185.869918	116816.046120	35.117236
1187.671682	117009.804344	35.122253
1188.807836	117215.611018	35.127271
1189.839512	117413.445574	35.132288
1191.496730	117615.335701	35.137306
1192.609970	117816.826369	35.142324
1194.166013	118005.154321	35.147341
1195.178136	118198.559520	35.152359
1196.667365	118390.750590	35.157376
1198.374484	118574.265532	35.162394
1199.540597	118766.485441	35.167412
1200.888140	118928.943353	35.172429
1201.837490	119135.016645	35.177447
1203.438038	119305.117330	35.182464
1204.867498	119480.666543	35.187482
1206.206325	119658.903482	35.192500
1207.286311	119834.042067	35.197517
1208.531001	120022.769772	35.202535
1209.669216	120191.632661	35.207552
1210.928893	120378.169608	35.212570
1211.677026	120558.469591	35.217588
1213.169422	120747.416427	35.222605
1214.229873	120936.737251	35.227623
1214.908429	121119.471112	35.232640
1216.502012	121304.733061	35.237658
1217.785434	121478.989067	35.242676
1219.184826	121658.775098	35.247693
1220.550341	121839.644280	35.252711
1221.682871	122016.676168	35.257728
1223.206185	122189.999488	35.262746
1224.136863	122360.099818	35.267764
1225.741890	122510.209175	35.272781
1226.641034	122697.706425	35.277799
1227.409945	122847.304669	35.282816
1228.814778	123013.432771	35.287834
1229.830254	123198.495893	35.292852
1230.957626	123364.860282	35.297869
1231.752486	123555.255300	35.302887
1232.988838	123727.836294	35.307904
1234.332998	123920.198483	35.312922
1235.372307	124103.984792	35.317940
1236.424168	124291.114279	35.322957
1237.367455	124490.688105	35.327975
1238.618673	124692.355099	35.332992
1239.888550	124890.600645	35.338010
1240.709407	125096.949733	35.343028
1241.943358	125290.073896	35.348045
1243.703820	125489.335186	35.353063
1244.959700	125679.697255	35.358080
1246.462209	125896.166331	35.363098
1247.624268	126098.364654	35.368116
1249.094580	126296.005921	35.373133
1250.063394	126501.138763	35.378151
1251.136528	126700.315516	35.383168
1252.567887	126908.620757	35.388186
1253.777211	127124.348130	35.393204
1255.045881	127343.298046	35.398221
1256.090475	127554.747948	35.403239
1257.304650	127762.562148	35.408256
1258.629948	127988.893624	35.413274
1259.730738	128203.405242	35.418292
1261.062501	128428.054425	35.423309
1262.329003	128640.478164	35.428327
1263.739718	128865.992466	35.433344
1265.037275	129077.350463	35.438362
1266.412583	129291.370796	35.443380
1267.400017	129503.288076	35.448397
1268.669293	129719.684943	35.453415
1269.867954	129959.899685	35.458432
1271.434696	130179.496082	35.463450
1272.447889	130399.017496	35.468468
1273.891329	130627.910835	35.473485
1275.084376	130845.671462	35.478503
1276.597076	131069.020871	35.483520
1278.200644	131275.177684	35.488538
1279.495735	131501.073680	35.493556
1280.652382	131710.738193	35.498573
1281.615432	131936.196324	35.503591
1283.416560	132156.074946	35.508608
1284.975398	132366.808005	35.513626
1286.034918	132593.320300	35.518644
1287.606116	132785.378708	35.523661
1289.039417	133006.323320	35.528679
1290.332952	133201.228806	35.533696
1291.809455	133412.033359	35.538714
1292.794020	133618.698350	35.543732
1293.859274	133807.448325	35.548749
1295.297911	133989.374002	35.553767
1296.389214	134206.378265	35.558784
1297.929598	134399.998238	35.563802
1298.749938	134604.681733	35.568820
1300.302406	134799.290804	35.573837
1301.850350	134996.436144	35.578855
1303.056453	135191.749140	35.583872
1304.458891	135393.291902	35.588890
1305.629154	135587.054675	35.593908
1306.755559	135792.635591	35.598925
1307.806997	136003.754706	35.603943
1309.066303	136219.784283	35.608960
1310.453281	136424.365177	35.613978
1311.416981	136644.259092	35.618996
1312.775049	136872.810316	35.624013
1314.029745	137087.833262	35.629031
1314.746034	137319.303172	35.634048
1316.450366	137534.435321	35.639066
1317.871322	137757.230190	35.644084
1319.106395	137995.858882	35.649101
1320.780408	138223.483278	35.654119
1321.924306	138442.538232	35.659136
1323.588909	138666.467096	35.664154
1325.063220	138880.606411	35.669172
1326.715319	139088.141739	35.674189
1328.525293	139303.726152	35.679207
1329.879193	139514.670199	35.684224
1331.510236	139725.014061	35.689242
1332.724563	139940.634366	35.694260
1333.996695	140144.473432	35.699277
1335.971353	140352.967454	35.704295
1337.218304	140551.528431	35.709312
1339.082246	140737.141560	35.714330
1340.216811	140940.171407	35.719348
1342.011736	141136.000320	35.724365
1343.418379	141317.583374	35.729383
1344.609511	141514.486585	35.734400
1345.942944	141703.295077	35.739418
1347.519860	141894.093905	35.744436
1348.895544	142081.681310	35.749453
1349.948136	142263.060117	35.754471
1351.161568	142461.689604	35.759488
1352.620973	142651.092307	35.764506
1353.634809	142842.163985	35.769524
1354.736684	143048.964730	35.774541
1356.417431	143240.427202	35.779559
1357.296107	143458.026984	35.784576
1358.549512	143645.288485	35.789594
1360.082743	143853.445654	35.794612
1361.529952	144054.659303	35.799629
1362.703970	144270.316605	35.804647
1363.816913	144469.798878	35.809664
1365.455105	144668.767996	35.814682
1366.568659	144870.470913	35.819700
1367.464794	145059.876485	35.824717
1369.048131	145248.210652	35.829735
1370.292118	145458.008962	35.834752
1371.524751	145636.564938	35.839770
1372.713923	145854.271554	35.844788
1373.936985	146057.929456	35.849805
1375.149055	146270.184699	35.854823
1375.948568	146474.356260	35.859840
1377.518168	146693.618067	35.864858
1379.296495	146913.570766	35.869876
1380.157535	147143.254028	35.874893
1381.739326	147364.635477	35.879911
1382.725006	147584.465261	35.884928
1384.269485	147828.876308	35.889946
1385.830024	148048.364403	35.894964
1387.202397	148270.850259	35.899981
1388.518521	148495.311504	35.904999
1389.805043	148748.492211	35.910016
1391.341968	148970.310241	35.915034
1392.727679	149219.295478	35.920052
1393.864779	149457.191568	35.925069
1395.533679	149685.458906	35.930087
1396.920383	149933.638136	35.935104
1398.550497	150169.775019	35.940122
1399.570418	150410.042045	35.945140
1400.769004	150661.159877	35.950157
1402.589595	150895.294032	35.955175
1403.863553	151145.997921	35.960192
1405.502762	151393.362097	35.965210
1406.859661	151636.538534	35.970228
1407.786972	151890.447336	35.975245
1409.534919	152139.093004	35.980263
1410.808890	152388.031391	35.985280
1412.337846	152638.503253	35.990298
1413.784833	152892.616085	35.995316
1415.330092	153136.470926	36.000333
1416.801450	153399.091094	36.005351
1418.103145	153648.414864	36.010368
1419.764899	153897.974891	36.015386
1421.462018	154139.365888	36.020404
1422.943337	154400.686386	36.025421
1424.507925	154635.331370	36.030439
1425.709679	154892.617408	36.035456
1427.258694	155132.885237	36.040474
1428.693727	155377.420497	36.045492
1430.559905	155615.866227	36.050509
1431.908678	155853.153240	36.055527
1433.499268	156102.043460	36.060544
1435.292013	156336.232833	36.065562
1436.758846	156563.197337	36.070580
1437.721447	156807.538949	36.075597
1439.263942	157039.274929	36.080615
1440.722961	157292.455191	36.085632
1442.124420	157527.184016	36.090650
1443.257010	157757.125950	36.095668
1444.526454	157981.163952	36.100685
1446.397679	158208.607598	36.105703
1447.594754	158436.033042	36.110720
1448.877073	158659.287169	36.115738
1450.390273	158883.406371	36.120756
1451.428691	159118.127525	36.125773
1453.473052	159330.866585	36.130791
1455.161076	159559.413326	36.135808
1456.804792	159774.919781	36.140826
1458.270356	160003.593518	36.145844
1459.531880	160228.687005	36.150861
1461.127224	160446.069379	36.155879
1462.443838	160681.010355	36.160896
1463.786511	160903.850627	36.165914
1465.112362	161145.362198	36.170932
1466.106787	161379.166901	36.175949
1467.879932	161636.335947	36.180967
1469.035916	161876.611268	36.185984
1470.503401	162125.614573	36.191002
1471.681261	162376.314273	36.196020
1472.583368	162626.336645	36.201037
1474.352442	162881.739740	36.206055
1475.949634	163151.350698	36.211072
1477.355340	163406.409384	36.216090
1478.928196	163663.206156	36.221108
1480.125085	163946.152417	36.226125
1481.654525	164206.599788	36.231143
1482.940162	164479.504114	36.236160
1484.178714	164750.388695	36.241178
1485.531009	165029.310835	36.246196
1487.180811	165304.027790	36.251213
1488.780443	165579.541103	36.256231
1490.269353	165849.328567	36.261248
1491.672770	166141.707798	36.266266
1493.660854	166414.007431	36.271284
1494.986037	166699.972985	36.276301
1496.768047	166952.459645	36.281319
1498.300635	167229.619259	36.286336
1499.823539	167507.175642	36.291354
1501.410842	167779.865923	36.296372
1502.622588	168055.598549	36.301389
1504.098978	168335.299279	36.306407
1506.051122	168622.562314	36.311424
1507.266558	168895.890446	36.316442
1509.348610	169159.950164	36.321460
1511.179141	169442.507426	36.326477
1513.002776	169705.698669	36.331495
1514.531427	169967.999909	36.336512
1516.567383	170229.309042	36.341530
1518.013588	170476.012030	36.346548
1519.373999	170737.025983	36.351565
1521.260746	170999.340723	36.356583
1522.848773	171249.603212	36.361600
1524.071206	171492.073330	36.366618
1525.502393	171730.566707	36.371636
1526.676331	171987.457886	36.376653
1528.434672	172231.737519	36.381671
1529.888796	172467.910299	36.386688
1531.446482	172710.816687	36.391706
1532.749626	172955.566337	36.396724
1534.035156	173211.470927	36.401741
1535.802673	173446.990822	36.406759
1536.707443	173683.207324	36.411776
1538.383056	173943.558064	36.416794
1540.110507	174180.775844	36.421812
1541.171091	174444.766887	36.426829
1542.836869	174695.850588	36.431847
1544.344242	174973.563859	36.436864
1545.727794	175220.521890	36.441882
1547.352290	175490.697149	36.446900
1548.706149	175768.389471	36.451917
1550.262222	176027.186754	36.456935
1552.310904	176294.407412	36.461952
1553.639923	176559.422463	36.466970
1555.664734	176821.829406	36.471988
1556.995726	177100.092545	36.477005
1558.608560	177357.062239	36.482023
1560.002954	177632.654620	36.487040
1561.589306	177904.919694	36.492058
1563.346489	178171.031517	36.497076
1564.450119	178454.769878	36.502093
1566.625043	178717.152195	36.507111
1568.204420	178998.255808	36.512128
1569.731916	179265.273756	36.517146
1571.249572	179555.944523	36.522164
1572.591835	179823.629770	36.527181
1574.089239	180101.480280	36.532199
1575.809745	180379.259088	36.537216
1577.225444	180675.790032	36.542234
1579.065558	180946.054963	36.547252
1580.166978	181242.715841	36.552269
1581.873213	181526.696058	36.557287
1583.475331	181818.472535	36.562304
1584.628860	182107.822618	36.567322
1586.583508	182395.182176	36.572340
1587.988363	182697.768272	36.577357
1589.450685	182991.110051	36.582375
1591.211874	183295.356597	36.587392
1592.962243	183583.048167	36.592410
1594.799585	183879.051637	36.597428
1596.498855	184175.155130	36.602445
1597.954128	184468.761539	36.607463
1599.724173	184746.712340	36.612480
1601.250544	185044.701621	36.617498
1602.876703	185332.830186	36.622516
1604.934049	185616.933039	36.627533
1606.851832	185897.164195	36.632551
1608.657384	186163.228098	36.637568
1610.533223	186436.756509	36.642586
1612.143946	186698.666920	36.647604
1613.771594	186959.243717	36.652621
1615.564932	187221.559540	36.657639
1617.229264	187458.999949	36.662656
1618.665574	187713.253784	36.667674
1620.524018	187942.404729	36.672692
1621.650691	188211.392700	36.677709
1623.208431	188464.159291	36.682727
1624.913570	188707.792314	36.687744
1626.060575	188970.943935	36.692762
1627.788762	189238.243271	36.697780
1629.036138	189513.107776	36.702797
1630.541064	189773.821217	36.707815
1632.420654	190054.019935	36.712832
1633.829054	190328.432080	36.717850
1635.440618	190609.476111	36.722868
1637.111744	190878.760721	36.727885
1638.352236	191160.476039	36.732903
1640.161066	191446.582606	36.737920
1641.488188	191732.830806	36.742938
1643.436233	192014.184875	36.747956
1644.669045	192312.622113	36.752973
1646.197268	192605.595122	36.757991
1648.039607	192890.308757	36.763008
1649.621557	193202.199390	36.768026
1651.470546	193493.108783	36.773044
1653.206110	193785.916218	36.778061
1654.588791	194090.965272	36.783079
1656.148329	194402.701952	36.788096
1657.316076	194711.507531	36.793114
1659.480323	195024.383103	36.798132
1661.449172	195323.241756	36.803149
1663.205937	195636.465012	36.808167
1665.144483	195925.279992	36.813184
1666.767949	196245.001037	36.818202
1668.498033	196545.833908	36.823220
1670.362445	196840.605696	36.828237
1671.929251	197144.146012	36.833255
1674.116499	197430.048725	36.838272
1675.515710	197747.187278	36.843290
1677.553215	198032.736272	36.848308
1679.007132	198336.187157	36.853325
1680.666282	198637.639825	36.858343
1682.758645	198923.045276	36.863360
1684.037188	199226.973319	36.868378
1686.050785	199510.972815	36.873396
1688.282669	199805.626584	36.878413
1690.083506	200096.288645	36.883431
1691.727205	200377.165478	36.888448
1693.393927	200676.140493	36.893466
1695.169190	200953.343775	36.898484
1696.619055	201247.697936	36.903501
1698.166195	201542.330165	36.908519
1700.008012	201817.851699	36.913536
1701.356180	202121.238948	36.918554
1703.412627	202376.889298	36.923572
1705.170087	202640.179045	36.928589
1706.265889	202917.982354	36.933607
1708.234865	203183.563988	36.938624
1710.047501	203449.958702	36.943642
1711.381503	203718.918647	36.948660
1713.041758	204004.444338	36.953677
1714.312626	204291.239200	36.958695
1716.120001	204562.006637	36.963712
1717.376888	204850.101281	36.968730
1718.923323	205147.468869	36.973748
1720.326701	205449.786031	36.978765
1722.014423	205742.488138	36.983783
1724.326897	206048.764290	36.988800
1725.891935	206359.832238	36.993818
1727.817007	206655.040058	36.998836
1729.927967	206958.382400	37.003853
1731.274605	207265.249778	37.008871
1733.159370	207567.450515	37.013888
1734.403913	207884.505662	37.018906
1736.129048	208199.340744	37.023924
1737.886995	208514.349969	37.028941
1739.548541	208832.765658	37.033959
1741.798576	209149.413825	37.038976
1743.153073	209472.629481	37.043994
1744.577847	209780.995084	37.049012
1746.553383	210106.768704	37.054029
1748.374600	210442.064548	37.059047
1750.294820	210763.876742	37.064064
1751.911651	211091.108874	37.069082
1753.495396	211426.130234	37.074100
1755.258072	211756.186390	37.079117
1757.074274	212090.564924	37.084135
1758.802631	212419.106446	37.089152
1760.460976	212760.280256	37.094170
1762.395088	213101.234322	37.099188
1763.910596	213434.537549	37.104205
1765.556883	213784.745307	37.109223
1767.416667	214114.417051	37.114240
1769.340016	214460.013824	37.119258
1771.084216	214807.837233	37.124276
1773.134932	215156.261272	37.129293
1775.239652	215490.230234	37.134311
1777.284945	215824.540363	37.139328
1778.787624	216160.753829	37.144346
1781.253916	216494.949585	37.149364
1783.224271	216813.304325	37.154381
1784.848379	217150.163503	37.159399
1787.013947	217471.423130	37.164416
1788.540724	217796.251798	37.169434
1790.074932	218123.569316	37.174452
1791.912077	218447.615266	37.179469
1793.863713	218780.265625	37.184487
1795.888150	219103.027799	37.189504
1797.583507	219418.238191	37.194522
1799.708679	219726.868166	37.199540
1801.575449	220020.596066	37.204557
1802.893992	220312.723446	37.209575
1804.722273	220613.722519	37.214592
1806.339642	220912.000997	37.219610
1807.720357	221230.341730	37.224628
1809.391367	221595.173231	37.229645
1811.311302	221903.349548	37.234663
1813.045901	222208.699610	37.239680
1814.508867	222536.593846	37.244698
1815.990561	222856.093453	37.249716
1818.268509	223183.149985	37.254733
1819.568137	223521.067237	37.259751
1821.476468	223847.702684	37.264768
1823.345069	224182.827837	37.269786
1824.905243	224520.149266	37.274804
1826.909689	224855.928640	37.279821
1828.790671	225201.734908	37.284839
1831.494310	225527.704905	37.289856
1833.335027	225869.152296	37.294874
1835.130288	226200.945119	37.299892
1836.887705	226525.888315	37.304909
1838.871065	226868.980596	37.309927
1841.081805	227195.632152	37.314944
1842.563173	227535.479883	37.319962
1844.284040	227862.338720	37.324980
1846.320582	228204.869192	37.329997
1848.252960	228548.738172	37.335015
1850.348978	228882.957134	37.340032
1852.241837	229218.200085	37.345050
1853.859767	229557.170499	37.350068
1855.836020	229882.777242	37.355085
1857.645643	230222.024499	37.360103
1859.814166	230557.660436	37.365120
1862.175615	230884.835054	37.370138
1864.130875	231218.754832	37.375156
1866.014918	231537.753349	37.380173
1868.191838	231877.735714	37.385191
1870.125305	232194.925381	37.390208
1871.852953	232526.473136	37.395226
1873.373471	232845.660734	37.400244
1875.550584	233166.218261	37.405261
1877.514528	233508.526022	37.410279
1879.444422	233831.359994	37.415296
1881.522552	234146.729810	37.420314
1883.157883	234476.800327	37.425332
1885.133541	234789.699394	37.430349
1886.899056	235127.218504	37.435367
1888.826089	235438.400185	37.440384
1890.809077	235767.784748	37.445402
1892.833768	236098.916249	37.450420
1894.719839	236413.663172	37.455437
1896.552501	236745.741539	37.460455
1898.135423	237063.205380	37.465472
1900.424903	237375.783013	37.470490
1902.224221	237679.905240	37.475508
1904.475024	237974.457378	37.480525
1905.902211	238273.484278	37.485543
1907.557786	238564.043171	37.490560
1909.613048	238871.125176	37.495578
1911.070224	239173.477036	37.500596
1913.207298	239472.750063	37.505613
1915.146750	239783.231041	37.510631
1917.072898	240091.454396	37.515648
1919.446636	240391.098637	37.520666
1920.832412	240705.098889	37.525684
1923.184680	241005.560888	37.530701
1924.989658	241319.724831	37.535719
1927.059197	241625.592621	37.540736
1928.949628	241932.683400	37.545754
1930.685909	242250.594442	37.550772
1932.603288	242557.504693	37.555789
1934.487244	242876.409898	37.560807
1936.264509	243192.259401	37.565824
1938.635812	243512.384277	37.570842
1940.749593	243831.458593	37.575860
1943.127543	244126.666137	37.580877
1945.507996	244441.864152	37.585895
1947.681670	244742.769798	37.590912
1949.334714	245042.412496	37.595930
1951.146331	245357.728318	37.600948
1953.412261	245653.820611	37.605965
1955.267912	245961.180390	37.610983
1957.241452	246265.982050	37.616000
1958.821596	246575.164941	37.621018
1960.945368	246889.621844	37.626036
1963.106606	247197.926437	37.631053
1964.922251	247511.823948	37.636071
1966.779339	247818.527030	37.641088
1968.925685	248138.317251	37.646106
1970.513145	248454.132627	37.651124
1972.674570	248771.153047	37.656141
1974.695233	249098.001364	37.661159
1976.304064	249427.125625	37.666176
1978.318885	249737.947915	37.671194
1980.100575	250063.693065	37.676212
1982.055201	250397.768531	37.681229
1983.768731	250741.967355	37.686247
1985.726229	251064.917805	37.691264
1987.998724	251396.988898	37.696282
1989.640280	251740.489911	37.701300
1992.033730	252081.078105	37.706317
1994.096523	252415.140337	37.711335
1996.219891	252745.510305	37.716352
1998.439550	253061.157878	37.721370
2000.373195	253391.889330	37.726388
2002.734537	253731.495014	37.731405
2004.655100	254060.299151	37.736423
2006.626433	254374.667397	37.741440
2008.927592	254690.126912	37.746458
2010.690556	254988.119406	37.751476
2012.748392	255284.592225	37.756493
2014.940865	255583.812955	37.761511
2016.617582	255883.979615	37.766528
2018.654691	256180.787220	37.771546
2020.379138	256484.274849	37.776564
2022.330802	256797.608379	37.781581
2023.995893	257096.813258	37.786599
2025.606944	257404.867159	37.791616
2028.135637	257723.343327	37.796634
2029.407386	258064.703788	37.801652
2031.440158	258376.527834	37.806669
2033.588910	258710.027693	37.811687
2034.870098	259050.295715	37.816704
2036.933761	259404.767157	37.821722
2038.910322	259751.987726	37.826740
2040.807527	260105.826046	37.831757
2042.831051	260460.686296	37.836775
2044.422593	260818.054193	37.841792
2046.540171	261184.153865	37.846810
2048.577055	261561.393243	37.851828
2051.238868	261914.375809	37.856845
2053.475637	262281.829656	37.861863
2055.620244	262645.945356	37.866880
2057.708937	263008.012687	37.871898
2059.954374	263378.133693	37.876916
2061.978027	263749.535020	37.881933
2064.079347	264116.377261	37.886951
2065.958815	264482.086513	37.891968
2068.123111	264853.568237	37.896986
2070.210123	265226.637558	37.902004
2072.793982	265592.871163	37.907021
2074.741253	265956.640339	37.912039
2076.359199	266342.766043	37.917056
2078.852154	266701.368612	37.922074
2080.735773	267088.011643	37.927092
2083.219056	267460.156206	37.932109
2085.505197	267832.433910	37.937127
2087.496983	268207.171861	37.942144
2089.672864	268562.320312	37.947162
2092.169268	268938.604476	37.952180
2094.357765	269303.506199	37.957197
2096.621327	269667.202246	37.962215
2098.519011	270028.593990	37.967232
2100.873846	270380.336319	37.972250
2103.084324	270756.539719	37.977268
2105.411274	271104.425440	37.982285
2107.331801	271462.664108	37.987303
2109.231297	271826.571179	37.992320
2112.016552	272184.495083	37.997338
2114.125405	272536.886806	38.002356
2116.051000	272902.034776	38.007373
2118.281439	273240.918148	38.012391
2120.508456	273596.924012	38.017408
2122.623830	273939.661643	38.022426
2124.450709	274279.599880	38.027444
2126.879716	274599.094502	38.032461
2128.574475	274914.945883	38.037479
2130.467306	275248.217999	38.042496
2133.375850	275560.066358	38.047514
2134.985149	275898.667332	38.052532
2136.909119	276224.288039	38.057549
2139.025520	276554.654036	38.062567
2140.782542	276901.436781	38.067584
2142.702187	277245.627936	38.072602
2144.538832	277594.989079	38.077620
2146.439365	277945.102113	38.082637
2148.751852	278318.038173	38.087655
2150.117497	278684.214566	38.092672
2152.329057	279043.905840	38.097690
2154.404481	279430.520729	38.102708
2156.327629	279808.497067	38.107725
2158.819842	280185.087418	38.112743
2161.186138	280579.378269	38.117760
2163.267941	280948.437738	38.122778
2165.441306	281347.610790	38.127796
2167.560992	281726.901345	38.132813
2170.139638	282111.047111	38.137831
2172.112558	282507.151993	38.142848
2174.534648	282894.827696	38.147866
2176.446845	283279.891230	38.152884
2178.770021	283681.274341	38.157901
2181.002501	284066.337262	38.162919
2182.901669	284471.927639	38.167936
2185.387990	284865.154821	38.172954
2187.801167	285266.115768	38.177972
2190.057373	285661.131485	38.182989
2192.523695	286051.744153	38.188007
2194.839977	286445.911220	38.193024
2197.707086	286823.453167	38.198042
2200.061730	287210.297236	38.203060
2202.327111	287599.263456	38.208077
2204.798716	287967.239124	38.213095
2207.015336	288342.672432	38.218112
2209.515636	288723.598113	38.223130
2211.367368	289099.825021	38.228148
2213.402587	289476.377984	38.233165
2216.090986	289854.554258	38.238183
2218.070892	290230.606919	38.243200
2220.640253	290591.044562	38.248218
2222.695424	290981.385919	38.253236
2224.786012	291357.521021	38.258253
2227.035140	291736.170673	38.263271
2229.238560	292117.214820	38.268288
2231.319464	292495.686734	38.273306
2233.511107	292873.429208	38.278324
2235.698029	293248.377545	38.283341
2238.225564	293635.845402	38.288359
2240.150941	294027.523222	38.293376
2242.370753	294379.094307	38.298394
2244.770967	294737.621808	38.303412
2246.947960	295085.388164	38.308429
2249.287929	295440.875730	38.313447
2251.376796	295794.675136	38.318464
2253.593958	296139.308836	38.323482
2255.649871	296499.361084	38.328500
2257.671820	296855.252120	38.333517
2260.123375	297207.137073	38.338535
2261.867017	297584.433811	38.343552
2264.117283	297948.643730	38.348570
2266.338498	298331.908800	38.353588
2268.422772	298701.249229	38.358605
2270.767426	299069.658528	38.363623
2272.836949	299457.085608	38.368640
2275.261837	299841.077049	38.373658
2277.412944	300233.899895	38.378676
2279.857665	300629.901211	38.383693
2282.200929	301011.388082	38.388711
2284.393812	301395.539597	38.393728
2286.618581	301805.899118	38.398746
2289.015127	302190.702186	38.403764
2291.196471	302600.660018	38.408781
2293.648237	302992.666157	38.413799
2295.885929	303391.842835	38.418816
2298.581709	303806.008475	38.423834
2300.430284	304201.028041	38.428852
2302.756463	304612.760628	38.433869
2305.165593	305009.644880	38.438887
2307.378958	305425.355403	38.443904
2309.950280	305837.604232	38.448922
2312.145598	306245.745723	38.453940
2314.361487	306665.338210	38.458957
2316.857215	307072.184865	38.463975
2319.406206	307482.272993	38.468992
2321.889828	307906.365569	38.474010
2324.445653	308302.505298	38.479028
2326.578460	308721.265893	38.484045
2329.299173	309119.967612	38.489063
2331.554490	309534.133997	38.494080
2334.067346	309955.623992	38.499098
2336.498444	310345.833218	38.504116
2338.558389	310757.638680	38.509133
2341.190668	311172.425253	38.514151
2343.354736	311577.455012	38.519168
2345.902903	311989.635775	38.524186
2348.425090	312394.935972	38.529204
2350.628439	312802.621909	38.534221
2353.448083	313198.728329	38.539239
2355.794576	313607.531470	38.544256
2357.822434	314012.116560	38.549274
2360.454508	314412.819924	38.554292
2362.391194	314825.442254	38.559309
2364.996761	315220.127242	38.564327
2367.557252	315634.984070	38.569344
2369.733251	316025.162310	38.574362
2372.116155	316398.060932	38.579380
2374.362981	316780.605547	38.584397
2376.698630	317160.747185	38.589415
2378.603170	317539.203214	38.594432
2380.967638	317922.765978	38.599450
2383.384800	318303.575905	38.604468
2385.371148	318680.973123	38.609485
2387.708997	319081.272324	38.614503
2390.110192	319485.851890	38.619520
2392.242844	319885.342012	38.624538
2394.458050	320298.201527	38.629556
2396.259425	320711.912044	38.634573
2398.932113	321116.212719	38.639591
2401.325584	321542.854078	38.644608
2403.171404	321970.799193	38.649626
2405.655088	322391.149161	38.654644
2407.636803	322841.264899	38.659661
2410.221020	323272.895956	38.664679
2412.930660	323713.114184	38.669696
2415.303424	324159.656274	38.674714
2418.274911	324596.018959	38.679732
2420.413816	325042.542549	38.684749
2422.964461	325485.366887	38.689767
2425.862645	325921.581722	38.694784
2428.246886	326369.912958	38.699802
2431.118983	326798.864104	38.704820
2433.265073	327241.742807	38.709837
2435.808471	327690.320647	38.714855
2438.247743	328135.128590	38.719872
2441.022100	328586.610391	38.724890
2443.360739	329034.958879	38.729908
2445.580520	329488.681710	38.734925
2448.024759	329926.266414	38.739943
2450.649010	330373.723623	38.744960
2452.873634	330830.967233	38.749978
2455.809825	331281.467505	38.754996
2457.978179	331738.282642	38.760013
2460.411176	332193.910244	38.765031
2463.206956	332652.550007	38.770048
2465.624860	333106.142704	38.775066
2468.158715	333546.408301	38.780084
2470.449941	334012.889309	38.785101
2472.759957	334466.007789	38.790119
2475.726960	334921.304469	38.795136
2478.104894	335386.340432	38.800154
2481.257942	335816.234950	38.805172
2483.474099	336275.272526	38.810189
2486.056225	336723.178229	38.815207
2488.852366	337170.259852	38.820224
2491.548112	337620.401281	38.825242
2493.855701	338060.266953	38.830260
2496.323149	338511.174717	38.835277
2498.611412	338958.527622	38.840295
2501.701569	339396.762090	38.845312
2503.891334	339828.052290	38.850330
2506.606353	340235.084875	38.855348
2508.952288	340642.985769	38.860365
2511.255272	341049.595908	38.865383
2513.733964	341458.308262	38.870400
2515.907692	341875.368577	38.875418
2518.694544	342284.280480	38.880436
2520.904531	342694.804372	38.885453
2523.022735	343120.344891	38.890471
2525.583153	343551.017020	38.895488
2528.056517	343986.422104	38.900506
2530.412442	344413.667518	38.905524
2532.486930	344839.253404	38.910541
2534.983107	345286.069941	38.915559
2537.715149	345734.800530	38.920576
2539.829967	346187.865151	38.925594
2542.810284	346631.091063	38.930612
2545.249385	347089.479289	38.935629
2547.744475	347553.389300	38.940647
2550.681182	348005.928382	38.945664
2553.183526	348471.555944	38.950682
2555.830658	348922.280230	38.955700
2558.541100	349383.754548	38.960717
2561.324701	349837.927613	38.965735
2564.325855	350297.393437	38.970752
2566.707459	350746.367737	38.975770
2569.559847	351195.669874	38.980788
2572.011110	351661.532113	38.985805
2574.769588	352112.846824	38.990823
2577.496163	352574.341993	38.995840
2579.507941	353039.119402	39.000858
2582.434295	353508.494641	39.005876
2584.822642	353969.117234	39.010893
2587.246043	354421.226597	39.015911
2589.936299	354902.430014	39.020928
2592.245039	355382.927829	39.025946
2595.340988	355850.427176	39.030964
2597.695725	356328.497325	39.035981
2599.994684	356814.008845	39.040999
2602.830175	357290.089943	39.046016
2605.288375	357769.678194	39.051034
2607.928358	358251.771161	39.056052
2610.669257	358742.244698	39.061069
2613.307038	359220.952688	39.066087
2616.063628	359709.789553	39.071104
2618.286549	360204.416667	39.076122
2621.630826	360681.805309	39.081140
2624.169629	361154.646768	39.086157
2626.661892	361637.236810	39.091175
2629.550144	362119.632276	39.096192
2631.688741	362610.669027	39.101210
2634.472885	363091.015194	39.106228
2636.912234	363578.821649	39.111245
2639.692152	364072.025410	39.116263
2642.439847	364563.960034	39.121280
2645.304270	365035.974362	39.126298
2648.197679	365493.031583	39.131316
2650.947447	365935.057958	39.136333
2653.499296	366368.990543	39.141351
2657.153821	366789.345105	39.146368
2659.577515	367218.112758	39.151386
2661.917912	367647.041701	39.156404
2664.249944	368089.341166	39.161421
2666.973243	368538.755647	39.166439
2669.543436	368969.868327	39.171456
2671.905942	369423.949210	39.176474
2674.134898	369884.035054	39.181492
2676.884210	370352.102838	39.186509
2679.051452	370825.510267	39.191527
2681.379692	371291.629805	39.196544
2683.729004	371781.744916	39.201562
2686.055403	372264.600995	39.206580
2689.232237	372769.391901	39.211597
2691.714389	373264.949315	39.216615
2694.493081	373767.558291	39.221632
2696.791724	374282.745918	39.226650
2699.386097	374786.132814	39.231668
2702.089029	375291.449959	39.236685
2704.727735	375819.478721	39.241703
2708.250143	376330.539366	39.246720
2710.512076	376859.070852	39.251738
2713.039327	377384.889401	39.256756
2716.217637	377906.081954	39.261773
2718.965473	378440.604373	39.266791
2722.025816	378964.998249	39.271808
2724.261909	379494.792467	39.276826
2727.080660	380023.218758	39.281844
2729.878649	380556.207500	39.286861
2732.249137	381107.978424	39.291879
2735.171349	381642.530644	39.296896
2737.819700	382197.235282	39.301914
2740.803889	382741.680993	39.306932
2743.711857	383280.550207	39.311949
2746.250352	383823.681045	39.316967
2749.242262	384367.417082	39.321984
2751.884081	384933.750795	39.327002
2754.823489	385469.970719	39.332020
2757.766177	386013.259162	39.337037
2760.900911	386568.963188	39.342055
2763.809728	387108.537476	39.347072
2766.485744	387653.061199	39.352090
2769.154127	388201.078085	39.357108
2772.160142	388745.025779	39.362125
2775.049077	389291.900453	39.367143
2778.039643	389833.728886	39.372160
2780.853984	390372.000897	39.377178
2783.912370	390909.262308	39.382196
2786.866654	391446.100835	39.387213
2789.489677	391981.259025	39.392231
2792.852295	392504.448565	39.397248
2795.108214	393020.070607	39.402266
2798.043849	393514.604874	39.407284
2800.919146	394011.474621	39.412301
2803.376039	394501.708627	39.417319
2806.231387	394985.025668	39.422336
2808.813697	395483.264315	39.427354
2811.596665	395978.446254	39.432372
2814.519572	396467.107230	39.437389
2817.290320	396976.603328	39.442407
2819.964264	397462.626662	39.447424
2822.615663	397968.449740	39.452442
2825.346399	398481.681804	39.457460
2827.814923	398998.395732	39.462477
2830.644821	399516.109219	39.467495
2833.323361	400039.593979	39.472512
2836.102281	400573.170784	39.477530
2838.504415	401098.457016	39.482548
2841.553944	401629.336728	39.487565
2844.113745	402177.905552	39.492583
2846.942623	402726.016721	39.497600
2849.754215	403280.940915	39.502618
2852.249026	403844.677229	39.507636
2855.361786	404397.151089	39.512653
2858.035195	404966.948679	39.517671
2861.148258	405526.728952	39.522688
2864.061950	406103.413740	39.527706
2866.972278	406675.246593	39.532724
2870.234394	407228.229592	39.537741
2872.984246	407810.282391	39.542759
2875.954941	408376.446660	39.547776
2879.574812	408933.879481	39.552794
2882.625991	409497.754188	39.557812
2885.804864	410054.932000	39.562829
2888.308233	410627.591508	39.567847
2891.860887	411187.477195	39.572864
2894.814266	411740.350581	39.577882
2897.354527	412308.942083	39.582900
2900.836356	412860.874542	39.587917
2904.155865	413408.716665	39.592935
2907.390179	413949.998136	39.597952
2910.542687	414499.062765	39.602970
2913.245312	415044.057447	39.607988
2916.243670	415584.256150	39.613005
2919.148658	416137.789082	39.618023
2922.209333	416685.002184	39.623040
2924.735438	417223.116222	39.628058
2927.256494	417777.134378	39.633076
2930.270394	418325.742458	39.638093
2933.080036	418886.560256	39.643111
2936.261167	419450.475408	39.648128
2938.820834	420002.948857	39.653146
2941.732922	420564.781136	39.658164
2944.512834	421131.437019	39.663181
2947.280175	421700.262256	39.668199
2950.227780	422263.296030	39.673216
2952.921183	422816.072387	39.678234
2955.690850	423360.287706	39.683252
2958.862841	423891.153331	39.688269
2961.346145	424433.036490	39.693287
2963.849643	424972.701639	39.698304
2966.645310	425513.120433	39.703322
2969.195024	426067.829404	39.708340
2972.189930	426631.069263	39.713357
2974.774877	427204.899932	39.718375
2977.775193	427766.443122	39.723392
2980.533190	428351.848445	39.728410
2983.363264	428940.724883	39.733428
2986.736894	429521.270214	39.738445
2989.462740	430110.415569	39.743463
2992.123882	430705.231328	39.748480
2995.301545	431293.721252	39.753498
2998.421600	431909.863694	39.758516
3001.262155	432512.435566	39.763533
3004.104932	433126.212173	39.768551
3007.313968	433746.905794	39.773568
3010.129240	434367.975853	39.778586
3013.495914	434992.893979	39.783604
3016.931996	435595.830648	39.788621
3020.390751	436224.324958	39.793639
3023.468176	436833.062265	39.798656
3026.591512	437451.627442	39.803674
3029.652814	438073.706648	39.808692
3033.093351	438680.644932	39.813709
3036.015668	439300.259334	39.818727
3039.081802	439919.784773	39.823744
3042.575705	440524.289280	39.828762
3045.540176	441145.825267	39.833780
3048.576877	441773.815061	39.838797
3051.439751	442392.196018	39.843815
3054.606905	443018.462068	39.848832
3057.856503	443638.876409	39.853850
3060.561451	444270.954755	39.858868
3063.605148	444904.025969	39.863885
3066.476384	445543.638343	39.868903
3069.546168	446174.545348	39.873920
3072.474865	446809.760784	39.878938
3075.581355	447462.699076	39.883956
3079.278539	448088.697156	39.888973
3082.305066	448735.285132	39.893991
3085.099579	449380.423975	39.899008
3088.040148	450015.854161	39.904026
3091.094807	450666.736849	39.909044
3094.443286	451313.809304	39.914061
3097.177366	451970.374465	39.919079
3099.852911	452620.047067	39.924096
3103.270672	453279.604230	39.929114
3106.353624	453940.460372	39.934132
3109.481814	454600.885196	39.939149
3112.769175	455259.494329	39.944167
3115.757931	455925.569968	39.949184
3118.830303	456570.208232	39.954202
3121.746405	457200.532829	39.959220
3125.114829	457818.674964	39.964237
3127.991107	458450.387063	39.969255
3130.755025	459052.854630	39.974272
3133.905277	459668.854386	39.979290
3136.709271	460311.553920	39.984308
3139.619187	460951.283482	39.989325
3142.906100	461579.703677	39.994343
3145.858573	462242.710273	39.999360
3149.217936	462878.113027	40.004378
3152.351497	463519.501779	40.009396
3155.612791	464175.925050	40.014413
3158.824045	464823.281882	40.019431
3161.765925	465484.672436	40.024448
3165.327741	466151.558566	40.029466
3168.679951	466813.095616	40.034484
3171.638008	467489.391761	40.039501
3174.823540	468146.766010	40.044519
3177.980531	468818.537267	40.049536
3181.150499	469487.149428	40.054554
3184.207400	470167.843985	40.059572
3187.072168	470844.349440	40.064589
3190.334174	471543.322235	40.069607
3193.522996	472224.180877	40.074624
3197.060329	472910.675309	40.079642
3200.209246	473612.578529	40.084660
3204.017050	474278.254185	40.089677
3207.667270	474966.784803	40.094695
3210.778234	475654.163891	40.099712
3214.370295	476345.437154	40.104730
3217.531129	477027.453191	40.109748
3220.482556	477703.665765	40.114765
3223.817745	478390.157158	40.119783
3226.969419	479093.991405	40.124800
3230.547013	479768.214889	40.129818
3233.602009	480470.094635	40.134836
3236.961373	481162.096095	40.139853
3240.111846	481855.672849	40.144871
3242.972632	482564.836435	40.149888
3246.312850	483261.668586	40.154906
3249.436640	483972.103608	40.159924
3252.613648	484666.940077	40.164941
3255.837339	485389.485342	40.169959
3258.865878	486095.258716	40.174976
3262.318864	486812.863208	40.179994
3265.405129	487531.003884	40.185012
3268.724440	488254.789608	40.190029
3271.932601	488963.712013	40.195047
3275.283972	489694.661936	40.200064
3278.497011	490412.218233	40.205082
3281.778228	491139.435139	40.210100
3285.312549	491859.612829	40.215117
3288.571530	492594.959508	40.220135
3291.765402	493321.296636	40.225152
3295.410347	494032.533185	40.230170
3299.005202	494709.507500	40.235188
3302.484004	495378.394588	40.240205
3305.986069	496032.355495	40.245223
3308.818539	496692.913292	40.250240
3312.202463	497369.165765	40.255258
3315.263819	498028.022796	40.260276
3318.362296	498703.260568	40.265293
3321.558423	499378.205098	40.270311
3324.485787	500064.527091	40.275328
3327.764662	500748.646644	40.280346
3330.475792	501454.488456	40.285364
3333.726453	502160.166441	40.290381
3337.009847	502880.703477	40.295399
3339.890000	503600.669096	40.300416
3343.433938	504325.245277	40.305434
3346.601299	505064.337744	40.310452
3349.971640	505792.413993	40.315469
3353.398074	506527.718918	40.320487
3356.408253	507282.741751	40.325504
3359.750738	508022.538836	40.330522
3363.023662	508792.190724	40.335540
3366.399329	509563.356275	40.340557
3369.887323	510330.987568	40.345575
3373.062340	511104.335656	40.350592
3376.446174	511886.899546	40.355610
3379.557455	512663.415956	40.360628
3382.980814	513461.440637	40.365645
3386.241443	514258.898305	40.370663
3389.457501	515052.743426	40.375680
3392.960226	515861.537981	40.380698
3396.455619	516674.027163	40.385716
3399.670207	517481.880585	40.390733
3403.575751	518292.762896	40.395751
3406.789735	519096.149513	40.400768
3410.602486	519893.400824	40.405786
3414.872873	520712.931721	40.410804
3418.597927	521495.796825	40.415821
3422.556227	522290.134650	40.420839
3425.753699	523099.125844	40.425856
3429.700262	523879.420656	40.430874
3433.371196	524666.729250	40.435892
3436.634617	525455.122385	40.440909
3440.134951	526227.357749	40.445927
3443.522166	527022.207637	40.450944
3447.115137	527794.806088	40.455962
3450.475425	528588.472899	40.460980
3453.789908	529388.256182	40.465997
3457.236946	530173.210806	40.471015
3460.621033	530969.122740	40.476032
3463.960994	531760.717646	40.481050
3467.352545	532551.609150	40.486068
3470.442310	533360.900303	40.491085
3474.163614	534155.840317	40.496103
3477.647548	534960.904194	40.501120
3481.085190	535744.949694	40.506125
3484.185853	536492.199180	40.511130
3487.409930	537176.311086	40.516135
3490.764333	537808.656038	40.521140
3493.493700	538396.379533	40.526144
3496.740217	538906.986170	40.531149
3499.055980	539369.648201	40.536154
3501.439803	539772.294812	40.541159
3503.946388	540117.497427	40.546164
3505.719545	540422.967556	40.551168
3507.557029	540647.782236	40.556173
3509.814595	540845.715101	40.561178
3511.081171	540996.893986	40.566183
3512.667176	541099.295464	40.571188
3514.126589	541167.229913	40.576192
3515.649225	541191.932617	40.581197
3516.535465	541183.259404	40.586202
3517.380585	541143.842737	40.591207
3518.327266	541076.840875	40.596212
3518.989612	540988.676566	40.601216
3519.676816	540867.283128	40.606221
3520.251469	540739.493773	40.611226
3520.166006	540589.539633	40.616231
3521.069502	540408.524776	40.621236
3521.457644	540237.637828	40.626240
3521.334966	540033.603156	40.631245
3521.910362	539813.851834	40.636250
3521.545193	539608.486331	40.641255
3521.978082	539374.864284	40.646260
3521.932251	539146.818715	40.651264
3522.097598	538899.495828	40.656269
3522.134159	538643.149605	40.661274
3522.023808	538394.801556	40.666279
3522.269859	538135.030043	40.671284
3522.250934	537870.649659	40.676288
3521.852856	537607.536717	40.681293
3521.670844	537342.112354	40.686298
3521.466163	537076.535443	40.691303
3521.273404	536806.507421	40.696308
3521.137008	536551.416056	40.701312
3521.087034	536283.124015	40.706317
3520.859835	536019.704213	40.711322
3520.591153	535759.317075	40.716327
3520.870520	535500.657319	40.721332
3520.350154	535232.623321	40.726336
3519.949261	534964.616289	40.731341
3519.740989	534709.556232	40.736346
3519.746558	534453.649929	40.741351
3519.649246	534184.924689	40.746356
3518.915537	533952.768218	40.751360
3518.800884	533699.242702	40.756365
3518.661645	533452.587375	40.761370
3518.046025	533213.379157	40.766375
3518.249116	532967.419799	40.771380
3517.405693	532745.164420	40.776384
3517.222837	532513.960285	40.781389
3517.315651	532280.637756	40.786394
3517.424615	532055.443312	40.791399
3516.989090	531831.392661	40.796404
3516.754607	531625.243023	40.801408
3516.571080	531405.188345	40.806413
3516.460799	531190.626256	40.811418
3516.256989	530976.934951	40.816423
3515.934129	530762.905860	40.821428
3515.630338	530551.953005	40.826432
3515.356466	530370.046195	40.831437
3515.112808	530168.628468	40.836442
3514.971059	529974.215621	40.841447
3514.738339	529773.953283	40.846452
3514.627556	529593.072837	40.851456
3514.649793	529403.073702	40.856461
3514.523900	529224.515845	40.861466
3513.852512	529039.472991	40.866471
3513.935655	528856.885891	40.871476
3513.726197	528682.782004	40.876480
3513.535461	528510.694598	40.881485
3513.489876	528342.119793	40.886490
3513.051597	528177.344848	40.891495
3513.303968	528009.578511	40.896500
3512.540127	527852.280360	40.901504
3512.437817	527681.989276	40.906509
3512.332058	527536.864373	40.911514
3512.190022	527376.127786	40.916519
3511.985141	527239.405062	40.921524
3511.734891	527098.948491	40.926528
3511.775741	526953.542402	40.931533
3511.521302	526815.004466	40.936538
3511.407972	526677.554898	40.941543
3511.133937	526548.771915	40.946548
3510.951007	526413.605380	40.951552
3511.186668	526286.660269	40.956557
3510.978293	526155.235602	40.961562
3510.762874	526029.421108	40.966567
3510.770729	525901.093769	40.971572
3510.645839	525781.479709	40.976576
3510.517492	525643.366563	40.981581
3510.699703	525529.362901	40.986586
3510.269949	525406.761621	40.991591
3510.061253	525294.182750	40.996596
3509.611363	525190.385402	41.001600
3509.634056	525076.605911	41.006605
3509.803899	524967.098696	41.011610
3509.668700	524872.600408	41.016615
3509.502801	524755.310265	41.021620
3509.288427	524655.768631	41.026624
3509.147241	524549.138310	41.031629
3509.473933	524448.195670	41.036634
3508.956678	524358.809423	41.041639
3509.116494	524246.771535	41.046644
3508.887134	524155.064022	41.051648
3508.943214	524056.840728	41.056653
3509.160502	523960.259452	41.061658
3508.758028	523874.188563	41.066663
3508.784343	523788.150543	41.071668
3508.486878	523694.884161	41.076672
3508.420620	523593.088389	41.081677
3508.916750	523522.139533	41.086682
3508.408864	523427.742222	41.091687
3508.349408	523346.972606	41.096692
3508.104270	523263.350555	41.101696
3508.050181	523169.385518	41.106701
3508.038804	523088.556462	41.111706
3507.948662	523018.203567	41.116711
3508.067885	522930.326452	41.121716
3507.963005	522860.784027	41.126720
3507.702810	522781.307109	41.131725
3507.667330	522701.238210	41.136730
3507.492892	522632.969607	41.141735
3507.823909	522549.202255	41.146740
3507.663714	522484.671678	41.151744
3507.405413	522416.567078	41.156749
3507.642746	522347.524450	41.161754
3507.323805	522283.321482	41.166759
3507.318356	522209.969035	41.171764
3507.244744	522139.255838	41.176768
3507.270026	522065.544003	41.181773
3507.265494	521998.711952	41.186778
3506.961370	521942.442341	41.191783
3506.922697	521873.542432	41.196788
3506.901352	521804.336163	41.201792
3507.030182	521744.306919	41.206797
3506.869508	521698.225944	41.211802
3506.433042	521640.257321	41.216807
3506.696896	521579.447796	41.221812
3506.845094	521527.099162	41.226816
3506.735057	521474.235058	41.231821
3506.832854	521396.666472	41.236826
3506.551395	521358.591521	41.241831
3506.853048	521296.207717	41.246836
3506.592395	521243.063327	41.251840
3506.587209	521178.806412	41.256845
3506.553057	521134.068884	41.261850
3506.576399	521064.245723	41.266855
3506.464562	521022.654723	41.271860
3505.997991	520977.075073	41.276864
3506.179497	520928.056056	41.281869
3506.068037	520878.931521	41.286874
3505.996580	520834.704648	41.291879
3506.464414	520781.291943	41.296884
3506.274569	520737.639659	41.301888
3506.454521	520679.266843	41.306893
3506.128534	520627.647532	41.311898
3506.415529	520588.419208	41.316903
3506.473021	520535.525585	41.321908
3506.260945	520485.050677	41.326912
3505.906592	520433.688032	41.331917
3505.427484	520396.349905	41.336922
3505.439721	520358.226203	41.341927
3506.199205	520319.883190	41.346932
3506.000623	520277.444489	41.351936
3505.665275	520246.656069	41.356941
3506.073660	520183.947794	41.361946
3506.010240	520155.391427	41.366951
3506.020232	520093.453615	41.371956
3505.510932	520060.720484	41.376960
3505.843888	520010.714135	41.381965
3506.085361	519978.114983	41.386970
3505.833352	519931.183927	41.391975
3506.021614	519885.851664	41.396980
3506.080298	519846.657650	41.401984
3505.742802	519805.200343	41.406989
3505.687801	519754.394989	41.411994
3505.446825	519728.090641	41.416999
3505.505956	519683.789459	41.422004
3505.656417	519646.046747	41.427008
3505.339287	519615.507070	41.432013
3505.682521	519585.368584	41.437018
3505.607620	519554.588261	41.442023
3505.824161	519513.244898	41.447028
3505.615730	519479.401248	41.452032
3505.804614	519437.556444	41.457037
3505.772453	519400.246531	41.462042
3505.387982	519354.649386	41.467047
3505.636719	519316.738698	41.472052
3505.599508	519275.687658	41.477056
3505.601796	519246.310318	41.482061
3505.838747	519202.839305	41.487066
3505.338164	519159.434182	41.492071
3505.572711	519128.149084	41.497076
3505.470300	519090.950699	41.502080
3505.393003	519053.040370	41.507085
3505.783203	519022.943996	41.512090
3505.683200	518978.615502	41.517095
3505.905592	518949.607356	41.522100
3505.603551	518907.282592	41.527104
3505.611381	518862.228846	41.532109
3505.450523	518824.027813	41.537114
3505.381122	518784.598691	41.542119
3505.601188	518760.697581	41.547124
3505.582998	518722.473763	41.552128
3505.335900	518677.914886	41.557133
3505.544863	518646.784612	41.562138
3505.337847	518603.837272	41.567143
3505.434144	518568.730029	41.572148
3505.373146	518544.417942	41.577152
3505.382569	518505.177954	41.582157
3505.775226	518465.978434	41.587162
3505.324608	518438.643285	41.592167
3505.286921	518395.466378	41.597172
3505.687726	518358.793594	41.602176
3505.062663	518335.328835	41.607181
3505.404118	518296.490966	41.612186
3505.327019	518272.838380	41.617191
3505.194974	518226.743121	41.622196
3505.473868	518211.175319	41.627200
3505.403238	518170.126807	41.632205
3505.669163	518113.450549	41.637210
3505.144900	518101.498666	41.642215
3505.218112	518066.242304	41.647220
3505.363085	518027.637124	41.652224
3505.338686	518007.363797	41.657229
3505.232394	517953.577558	41.662234
3504.916101	517927.787906	41.667239
3505.460606	517900.597986	41.672244
3505.208618	517878.641191	41.677248
3505.059890	517844.531911	41.682253
3505.710131	517806.503732	41.687258
3505.493128	517777.107869	41.692263
3505.348012	517736.575728	41.697268
3505.316770	517694.710730	41.702272
3504.996338	517675.191732	41.707277
3505.179869	517645.884033	41.712282
3505.099440	517613.988469	41.717287
3505.167896	517566.949459	41.722292
3505.097759	517553.003815	41.727296
3505.111234	517531.358578	41.732301
3504.933039	517497.910628	41.737306
3504.713825	517470.284459	41.742311
3504.791050	517447.617670	41.747316
3505.302001	517412.088457	41.752320
3505.182984	517395.621977	41.757325
3505.209986	517363.607814	41.762330
3504.950587	517330.728617	41.767335
3505.124216	517299.651963	41.772340
3505.167522	517280.277285	41.777344
3505.063398	517239.029483	41.782349
3505.269106	517210.931170	41.787354
3505.106503	517178.542064	41.792359
3504.956034	517159.096732	41.797364
3504.779748	517129.086451	41.802368
3504.544250	517101.765657	41.807373
3504.907109	517071.316073	41.812378
3504.952502	517049.412315	41.817383
3505.154288	517018.077836	41.822388
3505.170082	517000.831111	41.827392
3504.841702	516977.216389	41.832397
3505.281923	516927.335464	41.837402
3504.916240	516916.571338	41.842407
3504.870050	516872.987246	41.847412
3505.124410	516855.348672	41.852416
3505.203990	516829.747592	41.857421
3505.048769	516812.123137	41.862426
3505.088075	516774.442009	41.867431
3505.472976	516745.404318	41.872436
3505.033871	516708.860637	41.877440
3504.709993	516680.642847	41.882445
3505.213401	516657.806480	41.887450
3504.914698	516632.264884	41.892455
3505.024232	516597.353656	41.897460
3505.120417	516576.654953	41.902464
3505.108394	516545.859089	41.907469
3504.993302	516505.723766	41.912474
3504.786071	516497.918032	41.917479
3505.159714	516454.923917	41.922484
3504.981787	516440.690945	41.927488
3504.807873	516429.238763	41.932493
3505.112260	516374.725068	41.937498
3504.620296	516351.185882	41.942503
3504.786657	516331.436647	41.947508
3504.994614	516305.308751	41.952512
3504.826751	516275.194453	41.957517
3504.709694	516241.835454	41.962522
3504.491165	516232.160211	41.967527
3504.672253	516197.691986	41.972532
3504.769728	516180.734935	41.977536
3504.527657	516174.451724	41.982541
3504.809974	516148.311830	41.987546
3504.576603	516123.467140	41.992551
3504.778609	516106.038339	41.997556
3504.675113	516073.334302	42.002560
3504.848307	516051.459605	42.007565
3505.180287	516023.491049	42.012570
3504.978041	516001.169897	42.017575
3504.747621	515978.499157	42.022580
3504.841511	515950.517537	42.027584
3504.756072	515940.770517	42.032589
3504.759351	515890.904977	42.037594
3504.748606	515880.640385	42.042599
3504.848669	515849.319786	42.047604
3504.779410	515824.549859	42.052608
3504.742889	515801.443646	42.057613
3504.776275	515778.427498	42.062618
3504.464081	515763.203697	42.067623
3504.641596	515742.693399	42.072628
3504.801446	515719.202020	42.077632
3504.504988	515686.780591	42.082637
3504.555049	515660.019183	42.087642
3504.465004	515647.440581	42.092647
3504.461345	515625.492131	42.097652
3504.312243	515619.800904	42.102656
3504.527620	515596.351149	42.107661
3504.810368	515564.495403	42.112666
3504.512932	515551.595488	42.117671
3504.443162	515534.563065	42.122676
3504.847000	515512.904081	42.127680
3504.757429	515497.391980	42.132685
3504.977570	515473.688429	42.137690
3504.801495	515453.486534	42.142695
3505.077463	515428.105136	42.147700
3504.922780	515388.782575	42.152704
3504.823027	515377.621397	42.157709
3505.116021	515337.519913	42.162714
3504.788355	515324.220002	42.167719
3504.680488	515299.404823	42.172724
3504.665050	515268.404841	42.177728
3504.655126	515248.985640	42.182733
3504.946970	515224.865803	42.187738
3504.892440	515196.451202	42.192743
3504.506234	515165.206178	42.197748
3504.692456	515157.135327	42.202752
3504.866279	515126.712075	42.207757
3504.990588	515105.804802	42.212762
3504.752657	515080.908705	42.217767
3504.781529	515054.604858	42.222772
3504.920221	515026.462884	42.227776
3504.716302	514999.083075	42.232781
3504.727990	514986.791352	42.237786
3504.575413	514959.150483	42.242791
3504.828747	514933.569610	42.247796
3504.722501	514906.932854	42.252800
3504.567646	514882.427941	42.257805
3505.147746	514852.243436	42.262810
3504.821233	514837.830275	42.267815
3504.526783	514815.977299	42.272820
3505.101396	514789.991393	42.277824
3504.759919	514785.594700	42.282829
3504.817623	514744.719762	42.287834
3504.913031	514722.349856	42.292839
3504.729088	514692.235245	42.297844
3505.127185	514669.463391	42.302848
3504.851228	514652.816697	42.307853
3504.894551	514608.099852	42.312858
3504.605235	514593.023099	42.317863
3504.235300	514574.469250	42.322868
3504.630513	514539.609728	42.327872
3504.543395	514529.558687	42.332877
3504.645905	514507.187372	42.337882
3504.424293	514494.274656	42.342887
3504.568132	514467.193056	42.347892
3504.721046	514453.260142	42.352896
3504.717036	514429.944587	42.357901
3504.685455	514409.162240	42.362906
3504.618970	514380.191790	42.367911
3504.594010	514364.567272	42.372916
3504.656330	514326.826411	42.377920
3504.534270	514314.656491	42.382925
3504.723114	514282.357950	42.387930
3504.718041	514280.588590	42.392935
3504.606568	514246.364902	42.397940
3504.947758	514222.792187	42.402944
3504.356207	514209.330783	42.407949
3504.958082	514182.226909	42.412954
3504.514221	514165.555690	42.417959
3504.188776	514144.465413	42.422964
3504.363253	514117.479564	42.427968
3504.172402	514099.099198	42.432973
3504.313557	514092.855789	42.437978
3504.091536	514078.981824	42.442983
3504.173521	514074.416856	42.447988
3504.364092	514050.260762	42.452992
3504.196719	514043.459153	42.457997
3504.585265	514009.206532	42.463002
3504.461639	513992.130475	42.468007
3504.449757	513977.262213	42.473012
3504.496268	513951.763114	42.478016
3504.584249	513942.543890	42.483021
3504.574882	513915.637354	42.488026
3504.039079	513903.785425	42.493031
3504.501866	513889.954807	42.498036
3504.570118	513865.059091	42.503040
3504.470082	513852.430141	42.508045
3504.848515	513823.691889	42.513050
3504.434960	513807.622477	42.518055
3504.660887	513779.262309	42.523060
3505.007311	513761.049554	42.528064
3504.852090	513737.099402	42.533069
3504.756947	513707.879425	42.538074
3504.697114	513692.563273	42.543079
3504.367414	513666.212766	42.548084
3504.530361	513638.975074	42.553088
3504.247814	513621.873179	42.558093
3504.588318	513598.704340	42.563098
3504.627285	513584.636977	42.568103
3504.562259	513562.948429	42.573108
3504.816776	513532.408378	42.578112
3504.840429	513518.444541	42.583117
3504.873439	513493.149203	42.588122
3504.548777	513480.049672	42.593127
3504.408036	513454.731158	42.598132
3504.473138	513429.228330	42.603136
3504.182118	513409.143301	42.608141
3504.624037	513400.980616	42.613146
3504.622169	513380.748691	42.618151
3504.326557	513365.722411	42.623156
3504.759488	513336.367746	42.628160
3504.457793	513320.431931	42.633165
3504.764959	513295.244708	42.638170
3504.470970	513284.719809	42.643175
3504.377630	513263.844647	42.648180
3504.626241	513234.974169	42.653184
3504.479432	513219.165521	42.658189
3504.529770	513204.640813	42.663194
3504.582020	513187.536142	42.668199
3504.357565	513153.935067	42.673204
3504.774970	513145.573808	42.678208
3504.714769	513117.207169	42.683213
3504.733221	513097.831580	42.688218
3504.531748	513073.078489	42.693223
3504.613245	513063.556320	42.698228
3504.750795	513025.750073	42.703232
3504.018106	513022.982782	42.708237
3504.448655	512993.122080	42.713242
3504.299460	512969.220467	42.718247
3504.160909	512969.697673	42.723252
3504.319453	512941.852569	42.728256
3504.012308	512946.200659	42.733261
3504.318381	512925.514861	42.738266
3504.169352	512898.831106	42.743271
3504.178647	512891.748197	42.748276
3504.459878	512867.879575	42.753280
3504.201699	512854.364391	42.758285
3504.218068	512843.840746	42.763290
3504.515590	512816.175799	42.768295
3504.531934	512804.741649	42.773300
3504.480290	512789.676295	42.778304
3504.124631	512761.204009	42.783309
3504.662369	512746.146629	42.788314
3504.375744	512725.099020	42.793319
3504.539663	512715.057801	42.798324
3504.529951	512696.900189	42.803329
3504.193048	512679.249517	42.808333
3504.299808	512664.361347	42.813338
3504.339354	512653.530423	42.818343
3504.202916	512626.439583	42.823348
3504.145740	512622.604381	42.828353
3503.921990	512605.340411	42.833357
3504.390324	512594.492261	42.838362
3504.457643	512585.882561	42.843367
3504.467783	512554.418289	42.848372
3504.313227	512546.551801	42.853377
3504.274746	512536.542466	42.858381
3504.388691	512508.551949	42.863386
3504.456097	512491.899429	42.868391
3504.175351	512464.477055	42.873396
3504.482389	512449.607626	42.878401
3504.056598	512432.780081	42.883405
3504.481379	512411.973728	42.888410
3504.444686	512416.026289	42.893415
3503.880987	512383.792475	42.898420
3504.280856	512353.581410	42.903425
3503.938016	512367.394462	42.908429
3504.486918	512343.331045	42.913434
3504.228159	512324.048967	42.918439
3504.098163	512324.221335	42.923444
3504.179147	512308.831087	42.928449
3503.884146	512290.667547	42.933453
3504.063262	512265.195528	42.938458
3504.156512	512266.344293	42.943463
3504.117656	512242.980639	42.948468
3504.073258	512230.544019	42.953473
3504.248886	512227.127189	42.958477
3504.302430	512207.745034	42.963482
3504.181411	512186.721165	42.968487
3504.178546	512174.328523	42.973492
3504.194413	512160.769470	42.978497
3503.773707	512150.162721	42.983501
3504.252250	512139.666760	42.988506
3503.950803	512128.737641	42.993511
3503.824868	512101.239625	42.998516
3504.237909	512092.524447	43.003521
3504.124153	512088.343974	43.008525
3503.983170	512074.152042	43.013530
3504.010105	512056.797307	43.018535
3504.037734	512055.477808	43.023540
3504.268000	512046.487986	43.028545
3504.159820	512032.594344	43.033549
3504.411889	512016.519189	43.038554
3504.275862	512005.260336	43.043559
3503.723286	511987.187765	43.048564
3504.384281	511970.491501	43.053569
3504.140777	511974.930949	43.058573
3504.329041	511947.939460	43.063578
3504.050561	511935.438450	43.068583
3504.191633	511932.482288	43.073588
3504.392404	511904.578222	43.078593
3504.005025	511905.499466	43.083597
3503.887226	511888.774456	43.088602
3504.166968	511875.072299	43.093607
3503.732849	511856.626769	43.098612
3504.214683	511846.838301	43.103617
3504.036343	511842.415048	43.108621
3504.060397	511827.842728	43.113626
3504.127498	511817.664525	43.118631
3504.190823	511793.272393	43.123636
3504.411157	511787.622648	43.128641
3504.101426	511768.044480	43.133645
3504.108633	511762.226069	43.138650
3504.323768	511752.429114	43.143655
3504.094421	511734.153428	43.148660
3504.312148	511713.783633	43.153665
3504.145238	511709.763224	43.158669
3504.261954	511689.915222	43.163674
3504.113318	511674.661864	43.168679
3504.091413	511663.587090	43.173684
3504.181832	511637.065845	43.178689
3504.302585	511634.517531	43.183693
3504.353670	511611.897583	43.188698
3504.354181	511585.845742	43.193703
3504.019944	511578.715409	43.198708
3504.195618	511567.002311	43.203713
3504.390962	511546.686440	43.208717
3504.385008	511538.340720	43.213722
3504.217031	511509.988425	43.218727
3504.239358	511498.350104	43.223732
3504.552149	511478.875556	43.228737
3504.157058	511464.267999	43.233741
3504.163028	511444.184282	43.238746
3504.320868	511439.556029	43.243751
3503.962944	511430.658848	43.248756
3504.063009	511398.065315	43.253761
3504.329560	511401.817256	43.258765
3504.252925	511381.898281	43.263770
3504.221216	511365.108563	43.268775
3504.030947	511362.305846	43.273780
3504.375569	511340.802639	43.278785
3504.227389	511319.478467	43.283789
3504.195108	511309.568602	43.288794
3504.581385	511296.152663	43.293799
3504.310116	511282.537119	43.298804
3504.222057	511273.597202	43.303809
3503.941630	511256.138468	43.308813
3504.243895	511239.953472	43.313818
3504.118696	511241.086247	43.318823
3504.268123	511208.383376	43.323828
3504.453397	511198.894346	43.328833
3504.110391	511196.823964	43.333837
3503.992901	511162.544398	43.338842
3504.237115	511160.583549	43.343847
3503.937551	511152.182871	43.348852
3504.103529	511133.641707	43.353857
3503.992170	511126.779482	43.358861
3504.323892	511105.834480	43.363866
3504.158507	511094.124376	43.368871
3503.908641	511075.294760	43.373876
3504.511046	511067.307946	43.378881
3504.223710	511051.772425	43.383885
3504.417138	511040.056160	43.388890
3504.337569	511018.569003	43.393895
3504.208223	510997.190863	43.398900
3504.639791	510983.818109	43.403905
3504.307059	510976.940224	43.408909
3504.282631	510936.777294	43.413914
3504.121960	510942.923911	43.418919
3504.043985	510916.175218	43.423924
3504.423524	510897.144751	43.428929
3504.049274	510885.771044	43.433933
3504.080665	510874.636745	43.438938
3504.057665	510846.867490	43.443943
3503.953643	510840.914579	43.448948
3504.180128	510838.602378	43.453953
3504.094745	510817.065298	43.458957
3503.996476	510790.370204	43.463962
3504.312240	510799.932175	43.468967
3503.759020	510791.065525	43.473972
3504.097366	510767.994346	43.478977
3504.183605	510751.286557	43.483981
3504.082102	510754.489751	43.488986
3504.243978	510736.151158	43.493991
3504.140248	510715.830978	43.498996
3504.441761	510715.024563	43.504001
3504.028363	510694.298002	43.509005
3503.925934	510666.945718	43.514010
3504.197904	510667.863990	43.519015
3503.886861	510658.503694	43.524020
3504.506688	510639.940852	43.529025
3504.326441	510629.548089	43.534029
3504.183132	510621.729519	43.539034
3504.471112	510593.961290	43.544039
3504.114875	510595.484747	43.549044
3504.279173	510576.639710	43.554049
3503.932934	510558.583592	43.559053
3503.900840	510552.821569	43.564058
3503.579269	510541.692251	43.569063
3503.828510	510536.543416	43.574068
3504.080516	510498.409922	43.579073
3503.851561	510503.909827	43.584077
3503.875292	510493.940046	43.589082
3504.078789	510487.533693	43.594087
3503.746135	510467.249398	43.599092
3503.952349	510448.498774	43.604097
3503.815483	510455.603003	43.609101
3504.110807	510443.920814	43.614106
3504.077862	510441.346026	43.619111
3503.929547	510430.037483	43.624116
3504.207898	510411.477775	43.629121
3504.108564	510406.333405	43.634125
3504.327933	510394.865546	43.639130
3504.377615	510370.574714	43.644135
3504.242650	510354.862705	43.649140
3504.318842	510329.960548	43.654145
3504.067485	510317.504650	43.659149
3504.233603	510311.407678	43.664154
3504.555578	510280.547584	43.669159
3503.996716	510281.496013	43.674164
3504.158974	510260.677941	43.679169
3504.207816	510257.280758	43.684173
3504.242497	510241.794782	43.689178
3504.217305	510222.726354	43.694183
3504.060170	510215.921586	43.699188
3504.251618	510190.748060	43.704193
3504.430451	510181.208894	43.709197
3504.198741	510160.503558	43.714202
3504.281197	510147.944186	43.719207
3504.032055	510136.246661	43.724212
3504.175655	510110.473494	43.729217
3504.265660	510105.147336	43.734221
3503.998619	510088.292375	43.739226
3504.125703	510068.238486	43.744231
3504.341470	510069.823353	43.749236
3504.628104	510039.980224	43.754241
3504.229245	510034.883082	43.759245
3503.996669	510019.287374	43.764250
3504.458359	509996.347433	43.769255
3504.104022	509987.398337	43.774260
3504.079260	509974.956966	43.779265
3503.948743	509966.427801	43.784269
3503.806457	509946.618709	43.789274
3503.952589	509939.158807	43.794279
3503.883683	509934.110667	43.799284
3504.099825	509919.303993	43.804289
3503.909659	509918.878800	43.809293
3504.155588	509906.091049	43.814298
3504.061258	509900.642189	43.819303
3504.414341	509891.631824	43.824308
3504.446588	509871.289148	43.829313
3504.062817	509861.686952	43.834317
3504.189449	509839.153897	43.839322
3504.473239	509819.631454	43.844327
3503.858723	509812.190537	43.849332
3504.275827	509783.388759	43.854337
3504.175043	509771.262804	43.859341
3504.031166	509759.244834	43.864346
3504.423062	509743.954907	43.869351
3504.028846	509731.824710	43.874356
3504.154304	509717.082786	43.879361
3503.967594	509712.053200	43.884365
3504.107205	509680.613749	43.889370
3504.257658	509675.783822	43.894375
3504.247803	509667.336621	43.899380
3504.391082	509635.087038	43.904385
3504.330281	509629.784568	43.909389
3504.108428	509604.270769	43.914394
3504.055300	509588.292161	43.919399
3504.041433	509577.062987	43.924404
3503.877912	509562.214828	43.929409
3503.945431	509568.174094	43.934413
3503.931624	509542.930874	43.939418
3504.248171	509535.798008	43.944423
3504.040779	509539.321717	43.949428
3504.058959	509506.433966	43.954433
3503.918917	509493.352766	43.959437
3503.722670	509497.077092	43.964442
3504.390046	509485.891964	43.969447
3504.088196	509477.794374	43.974452
3503.973481	509457.980359	43.979457
3504.377586	509447.292148	43.984461
3503.963810	509431.572765	43.989466
3504.208394	509403.101172	43.994471
3504.103173	509405.293353	43.999476
3504.262611	509390.646963	44.004481
3504.148063	509369.315041	44.009485
3504.158416	509356.513522	44.014490
3504.254890	509354.677006	44.019495
3504.162898	509329.547014	44.024500
3504.090001	509311.244004	44.029505
3503.836135	509322.212250	44.034509
3503.807292	509284.626374	44.039514
3504.088850	509265.002468	44.044519
3503.669095	509269.419878	44.049524
3503.835035	509262.007145	44.054529
3503.655239	509262.642748	44.059533
3503.648478	509259.001191	44.064538
3503.749363	509224.531445	44.069543
3503.957017	509228.596736	44.074548
3503.848013	509215.004487	44.079553
3503.816543	509221.586637	44.084557
3503.959674	509212.659694	44.089562
3504.090069	509196.449342	44.094567
3503.882734	509195.773877	44.099572
3503.865827	509184.089589	44.104577
3504.325346	509184.371183	44.109581
3504.092045	509152.787333	44.114586
3504.378840	509146.114348	44.119591
3503.961341	509135.404021	44.124596
3504.087226	509122.229914	44.129601
3503.926803	509103.636956	44.134605
3503.839464	509091.710769	44.139610
3504.035181	509082.218919	44.144615
3504.282883	509074.337841	44.149620
3504.179992	509056.545235	44.154625
3504.404211	509036.778351	44.159629
3503.950651	509023.746345	44.164634
3504.013664	509006.787559	44.169639
3504.325040	509002.741508	44.174644
3504.233822	508986.565986	44.179649
3504.031150	508970.914001	44.184653
3504.284157	508962.273126	44.189658
3504.258284	508948.667527	44.194663
3504.261237	508921.447581	44.199668
3504.393050	508917.328703	44.204673
3504.128451	508900.573375	44.209677
3503.626220	508876.165282	44.214682
3504.123965	508867.890431	44.219687
3504.165976	508872.943275	44.224692
3504.085633	508849.783912	44.229697
3504.161528	508831.659251	44.234701
3503.998233	508833.557117	44.239706
3504.214294	508824.567853	44.244711
3503.833494	508802.872554	44.249716
3503.726675	508781.538680	44.254721
3503.850479	508783.542959	44.259725
3503.810859	508782.537402	44.264730
3504.055781	508762.412771	44.269735
3504.131634	508760.174696	44.274740
3504.109971	508745.252814	44.279745
3504.126830	508742.214548	44.284749
3504.070706	508714.953018	44.289754
3504.448083	508688.432444	44.294759
3504.183867	508702.741969	44.299764
3504.009965	508660.269974	44.304769
3504.148690	508660.551687	44.309773
3504.117506	508653.726391	44.314778
3504.129390	508625.948024	44.319783
3503.940863	508609.433362	44.324788
3503.906421	508601.849637	44.329793
3503.839385	508608.842402	44.334797
3504.027555	508594.646149	44.339802
3504.290932	508572.191010	44.344807
3504.106695	508564.681539	44.349812
3504.179671	508555.411179	44.354817
3504.016188	508531.960958	44.359821
3503.841784	508521.262420	44.364826
3504.006087	508513.799029	44.369831
3504.029867	508516.729862	44.374836
3503.906232	508500.306029	44.379841
3503.898276	508494.994856	44.384845
3503.526261	508479.925738	44.389850
3504.205003	508467.017916	44.394855
3503.967822	508459.668553	44.399860
3503.680728	508448.835995	44.404865
3503.920408	508440.449942	44.409869
3503.993819	508433.051478	44.414874
3504.211600	508422.088510	44.419879
3503.773475	508413.202427	44.424884
3504.112583	508397.514886	44.429889
3504.028133	508399.248552	44.434893
3503.685483	508378.609194	44.439898
3504.164605	508351.717853	44.444903
3503.774271	508345.100987	44.449908
3504.097053	508345.606592	44.454913
3504.060421	508335.645099	44.459917
3504.049961	508317.988907	44.464922
3504.134932	508305.731367	44.469927
3504.028581	508299.828536	44.474932
3504.323568	508284.856208	44.479937
3504.059270	508267.644851	44.484941
3504.001086	508265.023130	44.489946
3504.207226	508247.332632	44.494951
3504.014860	508220.496621	44.499956
3503.764213	508217.095775	44.504961
3504.170298	508211.314305	44.509965
3504.051619	508196.559070	44.514970
3504.248057	508175.530688	44.519975
3504.014093	508168.686653	44.524980
3503.968354	508159.232459	44.529985
3503.995430	508153.055508	44.534989
3503.928812	508142.643276	44.539994
3503.838990	508125.303008	44.544999
3503.430414	508127.340912	44.550004
3503.765553	508131.588700	44.555009
3503.845122	508106.632191	44.560013
3503.826289	508085.840109	44.565018
3503.827331	508079.869633	44.570023
3503.573103	508082.844479	44.575028
3503.749156	508082.260162	44.580033
3504.062963	508080.540951	44.585037
3503.684329	508060.311670	44.590042
3503.701429	508034.757773	44.595047
3503.716906	508025.900990	44.600052
3503.701462	508034.150749	44.605057
3503.996986	508027.222971	44.610061
3504.018357	508026.207731	44.615066
3503.978069	508005.014169	44.620071
3503.773869	507986.932890	44.625076
3504.108082	507992.901148	44.630081
3504.129241	507984.296429	44.635085
3503.704922	507961.139641	44.640090
3503.895914	507961.969670	44.645095
3503.822187	507952.519786	44.650100
3503.725543	507943.933666	44.655105
3504.044961	507934.978200	44.660109
3503.585754	507915.318050	44.665114
3503.698644	507895.567455	44.670119
3503.507805	507899.645448	44.675124
3503.758725	507898.593920	44.680129
3504.087150	507890.547753	44.685133
3503.633514	507905.798622	44.690138
3503.989891	507871.538774	44.695143
3503.884466	507862.650419	44.700148
3504.068211	507855.790837	44.705153
3504.000228	507856.307623	44.710157
3503.922998	507843.620017	44.715162
3504.280242	507821.655040	44.720167
3503.738948	507819.413190	44.725172
3503.499398	507816.921261	44.730177
3503.905230	507809.621781	44.735181
3503.887681	507802.389215	44.740186
3503.887811	507772.486246	44.745191
3503.583832	507780.275756	44.750196
3503.842402	507772.695952	44.755201
3503.999430	507770.242529	44.760205
3504.018850	507757.944364	44.765210
3504.266527	507734.276281	44.770215
3503.755131	507723.124534	44.775220
3504.007271	507722.123400	44.780225
3504.004370	507698.393677	44.785229
3503.776557	507692.358043	44.790234
3504.009416	507677.850388	44.795239
3503.666618	507678.005834	44.800244
3503.680220	507679.268695	44.805249
3503.985078	507676.235320	44.810253
3503.762746	507652.084837	44.815258
3504.282535	507636.671637	44.820263
3503.847723	507652.830512	44.825268
3503.972025	507631.610479	44.830273
3504.185890	507607.593382	44.835277
3503.978653	507597.911417	44.840282
3504.335577	507591.935121	44.845287
3504.162388	507567.371969	44.850292
3504.071944	507560.150823	44.855297
3503.935435	507542.665556	44.860301
3503.748194	507539.709935	44.865306
3503.995968	507508.300025	44.870311
3503.793742	507513.493067	44.875316
3504.020339	507506.575977	44.880321
3504.156328	507501.191149	44.885325
3503.824771	507492.540736	44.890330
3503.992173	507462.661392	44.895335
3503.770687	507463.809631	44.900340
3503.990967	507456.336937	44.905345
3504.277419	507453.660621	44.910349
3503.643630	507431.446999	44.915354
3503.789965	507411.336378	44.920359
3503.617185	507425.075923	44.925364
3503.752667	507406.535562	44.930369
3504.162309	507399.791891	44.935373
3504.051199	507381.796462	44.940378
3504.145889	507372.218445	44.945383
3503.997716	507372.090139	44.950388
3504.056703	507335.599301	44.955393
3503.854207	507336.137362	44.960397
3503.681880	507334.950302	44.965402
3503.821370	507309.072397	44.970407
3503.894957	507325.454815	44.975412
3503.780689	507305.284062	44.980417
3503.999289	507276.307082	44.985421
3503.951906	507270.293380	44.990426
3503.713873	507278.477483	44.995431
3503.844851	507279.418229	45.000436
3503.765455	507257.673346	45.005441
3503.928623	507253.194925	45.010445
3503.540679	507239.797002	45.015450
3503.850021	507232.816126	45.020455
3503.782300	507241.479317	45.025460
3503.732012	507239.868169	45.030465
3503.879968	507200.529445	45.035469
3503.612483	507186.252258	45.040474
3503.827001	507186.876211	45.045479
3503.930563	507197.080923	45.050484
3503.725594	507196.303805	45.055489
3503.956710	507189.183477	45.060493
3503.540390	507165.619565	45.065498
3503.908500	507160.096746	45.070503
3503.998412	507155.225085	45.075508
3503.667664	507160.539744	45.080513
3504.005901	507141.106867	45.085517
3503.624382	507128.416231	45.090522
3503.824329	507108.397983	45.095527
3503.648643	507105.339263	45.100532
3503.814636	507084.870961	45.105537
3504.072639	507100.617251	45.110541
3503.718262	507102.494907	45.115546
3503.863571	507065.585063	45.120551
3504.098792	507065.851552	45.125556
3503.808848	507068.832215	45.130561
3503.956850	507061.067180	45.135565
3503.996953	507058.885135	45.140570
3503.805115	507029.669017	45.145575
3503.955249	507025.951591	45.150580
3503.850099	507014.431580	45.155585
3504.011730	507011.015931	45.160589
3503.625540	506996.858548	45.165594
3504.077517	506971.537946	45.170599
3504.030046	506974.834500	45.175604
3504.041392	506976.350767	45.180609
3504.287598	506951.113258	45.185613
3504.001898	506932.790759	45.190618
3504.159694	506927.908305	45.195623
3503.823700	506914.906718	45.200628
3503.795354	506898.719301	45.205633
3504.084809	506885.163438	45.210637
3503.924491	506888.882643	45.215642
3503.683544	506882.494601	45.220647
3503.865593	506854.787693	45.225652
3503.853631	506839.407233	45.230657
3503.908523	506843.294833	45.235661
3503.572499	506834.138796	45.240666
3504.047735	506831.483148	45.245671
3503.851322	506832.931064	45.250676
3503.753484	506801.473300	45.255681
3504.178355	506791.589776	45.260685
3503.898502	506790.672673	45.265690
3503.945572	506788.691894	45.270695
3504.129558	506758.049712	45.275700
3503.646286	506764.097003	45.280705
3503.870581	506750.854935	45.285709
3503.708961	506759.077805	45.290714
3503.780980	506737.966143	45.295719
3503.837907	506731.176762	45.300724
3503.464189	506709.831914	45.305729
3504.041920	506705.034827	45.310733
3503.768922	506712.718716	45.315738
3504.072255	506701.235135	45.320743
3503.935401	506693.767961	45.325748
3503.806324	506685.591146	45.330753
3503.799868	506669.147053	45.335757
3503.870425	506670.502187	45.340762
3504.117300	506667.983809	45.345767
3503.713262	506646.694275	45.350772
3503.793358	506621.887348	45.355777
3503.791401	506614.449419	45.360781
3503.546183	506622.128957	45.365786
3503.813533	506616.115885	45.370791
3504.111199	506621.128981	45.375796
3503.709795	506581.926285	45.380801
3503.751601	506578.428289	45.385805
3503.652979	506571.258624	45.390810
3503.780434	506579.435889	45.395815
3503.665220	506575.254298	45.400820
3503.463079	506580.953613	45.405825
3504.054482	506564.617330	45.410829
3503.800100	506555.802447	45.415834
3503.617167	506541.258360	45.420839
3503.617814	506529.873108	45.425844
3503.799171	506529.793913	45.430849
3503.864072	506533.072789	45.435853
3503.797381	506522.457190	45.440858
3503.876316	506499.724913	45.445863
3503.748216	506486.588943	45.450868
3503.620389	506488.228453	45.455873
3504.093119	506488.103205	45.460877
3503.920270	506475.682715	45.465882
3503.997620	506457.251731	45.470887
3504.109570	506447.468071	45.475892
3503.987648	506444.906748	45.480897
3503.880230	506444.417784	45.485901
3503.749936	506416.253532	45.490906
3504.063395	506405.881385	45.495911
3503.857454	506396.451549	45.500916
3503.911483	506393.103388	45.505921
3504.157117	506379.807065	45.510925
3504.011523	506371.025495	45.515930
3504.138463	506361.947839	45.520935
3504.309684	506356.658292	45.525940
3503.825796	506324.400455	45.530945
3504.022963	506308.278048	45.535949
3503.636729	506306.213895	45.540954
3503.944559	506302.471391	45.545959
3503.682727	506297.351475	45.550964
3503.596445	506267.054755	45.555969
3504.067298	506252.052880	45.560973
3503.740639	506264.147804	45.565978
3503.913549	506264.525359	45.570983
3504.140371	506258.214959	45.575988
3504.164524	506234.630764	45.580993
3504.227085	506213.924776	45.585997
3504.048551	506211.068754	45.591002
3504.311876	506184.258768	45.596007
3504.055935	506184.451096	45.601012
3503.998216	506172.265203	45.606017
3504.534209	506150.016852	45.611021
3504.071972	506148.875530	45.616026
3503.886420	506122.794223	45.621031
3503.965177	506113.622849	45.626036
3504.038078	506084.211491	45.631041
3504.197068	506080.998487	45.636045
3504.019553	506077.231441	45.641050
3504.052932	506058.655178	45.646055
3503.993707	506039.891122	45.651060
3503.726730	506038.769533	45.656065
3503.717562	506029.915626	45.661069
3503.936540	506030.741327	45.666074
3503.836811	506011.325810	45.671079
3504.060179	505997.273677	45.676084
3503.887137	506002.867376	45.681089
3504.016455	505989.234921	45.686093
3503.920651	505964.505461	45.691098
3503.840458	505954.094060	45.696103
3503.785850	505951.117203	45.701108
3503.715267	505944.499477	45.706113
3503.934368	505938.493798	45.711117
3503.914385	505941.280176	45.716122
3503.863887	505914.671184	45.721127
3503.938051	505911.825776	45.726132
3503.904530	505906.011822	45.731137
3504.200436	505896.603601	45.736141
3503.505922	505873.689137	45.741146
3503.960118	505868.101702	45.746151
3504.162209	505862.554112	45.751156
3504.242009	505848.322140	45.756161
3504.200741	505838.106928	45.761165
3504.029164	505827.558086	45.766170
3504.230757	505807.892304	45.771175
3503.748631	505788.789994	45.776180
3504.075180	505773.456294	45.781185
3504.246785	505769.482192	45.786189
3503.924166	505770.393508	45.791194
3503.997495	505742.550205	45.796199
3504.093406	505738.082027	45.801204
3503.971883	505731.118048	45.806209
3504.035798	505707.729269	45.811213
3503.956331	505693.370532	45.816218
3504.210478	505679.515693	45.821223
3504.057136	505686.270259	45.826228
3504.004314	505676.157986	45.831233
3503.997164	505656.018991	45.836237
3503.897435	505661.601212	45.841242
3503.874322	505649.510690	45.846247
3504.071749	505639.004618	45.851252
3503.953295	505613.468582	45.856257
3503.920547	505595.408314	45.861261
3503.871555	505597.845105	45.866266
3503.947998	505589.331669	45.871271
3503.743824	505562.037976	45.876276
3503.905676	505546.578298	45.881281
3504.112013	505547.254209	45.886285
3503.878942	505551.086405	45.891290
3503.962826	505533.513677	45.896295
3503.871996	505517.385455	45.901300
3503.954820	505501.735812	45.906305
3503.921944	505501.589266	45.911309
3503.906929	505499.061510	45.916314
3503.904183	505480.793965	45.921319
3503.647759	505481.087584	45.926324
3503.510629	505469.925832	45.931329
3504.023855	505452.740599	45.936333
3503.792189	505462.037837	45.941338
3503.688333	505441.913880	45.946343
3503.784247	505420.037783	45.951348
3503.436716	505421.357887	45.956353
3503.768883	505422.823583	45.961357
3503.717057	505418.479882	45.966362
3503.423778	505406.583706	45.971367
3503.780412	505420.342365	45.976372
3503.684473	505415.752614	45.981377
3503.798744	505399.288241	45.986381
3503.443737	505380.924455	45.991386
3503.584378	505375.133401	45.996391
3503.926720	505370.676784	46.001396
3503.724012	505378.501962	46.006401
3503.871519	505368.003617	46.011405
3503.708730	505376.733366	46.016410
3503.730847	505357.500280	46.021415
3503.962006	505331.959179	46.026420
3503.589627	505331.056620	46.031425
3503.970650	505321.786451	46.036429
3503.539097	505328.585127	46.041434
3503.290660	505324.373687	46.046439
3503.481523	505325.709911	46.051444
3503.972864	505323.962375	46.056449
3503.822348	505305.869816	46.061453
3503.769646	505306.333657	46.066458
3503.877885	505290.781017	46.071463
3504.069516	505284.627642	46.076468
3503.690300	505275.730631	46.081473
3504.048388	505239.188124	46.086477
3503.910184	505238.197943	46.091482
3503.459278	505233.816063	46.096487
3504.037890	505223.249493	46.101492
3503.914049	505228.025986	46.106497
3503.436836	505202.748472	46.111501
3503.546522	505194.178985	46.116506
3503.864216	505184.665729	46.121511
3503.842327	505186.541640	46.126516
3503.759007	505193.841981	46.131521
3504.077635	505177.851149	46.136525
3503.647954	505159.347118	46.141530
3503.721301	505138.435729	46.146535
3503.690128	505133.177802	46.151540
3503.528019	505151.320092	46.156545
3504.152957	505140.493126	46.161549
3503.904424	505150.349849	46.166554
3504.147405	505124.300528	46.171559
3503.950720	505107.176557	46.176564
3503.598528	505109.863758	46.181569
3503.867373	505106.329583	46.186573
3503.860202	505097.930334	46.191578
3503.959355	505068.614327	46.196583
3504.001691	505050.389812	46.201588
3503.702890	505041.479971	46.206593
3503.799766	505050.421867	46.211597
3503.966240	505044.727832	46.216602
3504.063681	505017.689249	46.221607
3503.785934	505011.053306	46.226612
3503.787706	505012.520653	46.231617
3503.921546	505005.009969	46.236621
3503.747788	504989.855870	46.241626
3503.720363	504974.172575	46.246631
3504.044406	504963.899113	46.251636
3504.049418	504960.457214	46.256641
3504.032138	504954.083715	46.261645
3504.026954	504939.510196	46.266650
3503.992597	504931.165769	46.271655
3503.743056	504926.094111	46.276660
3503.524424	504934.630483	46.281665
3503.906025	504906.129857	46.286669
3503.871735	504897.684193	46.291674
3503.515765	504895.969325	46.296679
3503.619596	504889.627266	46.301684
3503.634238	504878.238724	46.306689
3503.887202	504879.463957	46.311693
3503.397752	504886.018925	46.316698
3503.573574	504877.236407	46.321703
3504.070761	504870.427323	46.326708
3503.511559	504857.358263	46.331713
3503.748158	504835.914652	46.336717
3504.115816	504839.297814	46.341722
3503.660225	504837.902321	46.346727
3503.789760	504822.042263	46.351732
3503.732589	504797.001408	46.356737
3503.827711	504781.703420	46.361741
3503.650469	504792.713015	46.366746
3504.049706	504787.488169	46.371751
3504.021481	504779.345124	46.376756
3503.400865	504767.247218	46.381761
3503.560819	504749.914711	46.386765
3503.430610	504747.253235	46.391770
3503.072675	504736.176518	46.396775
3503.742933	504744.015822	46.401780
3503.709258	504755.205175	46.406785
3503.916188	504729.667026	46.411789
3503.777622	504746.945707	46.416794
3503.876149	504746.424143	46.421799
3503.625117	504723.994738	46.426804
3503.535450	504709.586199	46.431809
3503.947792	504694.946485	46.436813
3503.940426	504704.562916	46.441818
3504.086671	504689.965255	46.446823
3503.800062	504688.846679	46.451828
3503.748466	504670.231764	46.456833
3503.905988	504650.571649	46.461837
3503.970431	504662.454043	46.466842
3503.395267	504657.433773	46.471847
3503.552784	504650.121620	46.476852
3503.326873	504647.222223	46.481857
3503.627778	504657.447840	46.486861
3503.606085	504642.573044	46.491866
3503.614861	504626.782503	46.496871
3503.749510	504613.299955	46.501876
3503.543764	504604.527002	46.506881
3503.935623	504598.139314	46.511885
3503.552304	504608.118859	46.516890
3503.573323	504604.471933	46.521895
3504.042511	504591.037706	46.526900
3503.557159	504584.738053	46.531905
3503.499156	504568.553161	46.536909
3503.776087	504561.626952	46.541914
3503.485729	504564.608102	46.546919
3503.438318	504572.560914	46.551924
3503.309813	504564.787867	46.556929
3503.743151	504556.622374	46.561933
3503.526325	504568.751714	46.566938
3503.613872	504562.715751	46.571943
3503.896812	504560.292586	46.576948
3503.334831	504552.385619	46.581953
3503.365251	504525.002622	46.586957
3503.445656	504526.305760	46.591962
3503.685137	504503.343084	46.596967
3503.731289	504507.181981	46.601972
3503.644811	504511.041840	46.606977
3503.429142	504505.914098	46.611981
3503.700101	504508.351078	46.616986
3503.488294	504511.927104	46.621991
3503.731506	504506.726835	46.626996
3503.584969	504521.527261	46.632001
3503.644978	504512.914686	46.637005
3503.814756	504490.823327	46.642010
3503.381178	504479.809011	46.647015
3503.645901	504467.014288	46.652020
3503.680692	504476.674788	46.657025
3503.863624	504468.194583	46.662029
3503.703642	504473.938525	46.667034
3503.503587	504469.516803	46.672039
3503.879975	504472.645621	46.677044
3503.889064	504439.294240	46.682049
3503.887658	504430.387689	46.687053
3503.903011	504422.035163	46.692058
3504.152986	504427.157647	46.697063
3503.795290	504408.439014	46.702068
3503.704068	504388.160027	46.707073
3504.094907	504381.418172	46.712077
3503.884551	504377.099268	46.717082
3503.694281	504376.522124	46.722087
3504.088873	504347.006394	46.727092
3503.783944	504350.546564	46.732097
3503.891072	504333.829283	46.737101
3503.904758	504338.128814	46.742106
3503.650871	504321.924048	46.747111
3503.899417	504301.996119	46.752116
3503.770319	504297.967997	46.757121
3503.822390	504283.030631	46.762125
3503.935596	504284.632248	46.767130
3503.878416	504280.491540	46.772135
3503.946443	504264.792524	46.777140
3503.977085	504254.160161	46.782145
3503.975738	504247.379027	46.787149
3503.689364	504245.906131	46.792154
3503.786234	504237.135772	46.797159
3503.690494	504223.385693	46.802164
3503.489481	504227.061286	46.807169
3503.901421	504211.763334	46.812173
3503.545745	504209.289234	46.817178
3503.497622	504210.410280	46.822183
3503.796200	504202.012884	46.827188
3503.819405	504218.153146	46.832193
3503.822832	504194.012791	46.837197
3503.497053	504175.035825	46.842202
3503.833176	504166.075792	46.847207
3503.819969	504174.731887	46.852212
3504.030875	504175.761387	46.857217
3504.114050	504158.946510	46.862221
3504.228412	504139.495076	46.867226
3503.901414	504126.793631	46.872231
3503.858962	504120.271983	46.877236
3503.535812	504123.258391	46.882241
3503.533012	504089.250320	46.887245
3503.644678	504080.528153	46.892250
3503.681179	504077.789617	46.897255
3504.051065	504074.947779	46.902260
3503.712167	504079.961007	46.907265
3504.128814	504076.200833	46.912269
3503.934771	504056.342579	46.917274
3503.821436	504044.568859	46.922279
3504.061223	504038.862911	46.927284
3503.901354	504032.410398	46.932289
3503.969530	504008.259554	46.937293
3503.884909	503992.533812	46.942298
3503.742220	503995.491718	46.947303
3503.963922	503971.620208	46.952308
3503.611652	503990.249228	46.957313
3503.971473	503965.951013	46.962317
3503.815480	503956.157704	46.967322
3503.651853	503954.766599	46.972327
3503.744420	503941.442012	46.977332
3503.600011	503948.904352	46.982337
3503.665083	503938.316965	46.987341
3503.856180	503941.829426	46.992346
3503.514902	503917.540739	46.997351
3503.622456	503902.391846	47.002356
3503.571014	503894.302669	47.007361
3503.838548	503897.499405	47.012365
3503.887840	503895.315514	47.017370
3503.615311	503898.496392	47.022375
3503.797206	503886.524078	47.027380
3503.862788	503876.746311	47.032385
3503.933780	503856.238637	47.037389
3503.699539	503852.986162	47.042394
3503.793046	503858.487805	47.047399
3504.003066	503857.695549	47.052404
3503.686049	503832.087083	47.057409
3503.705495	503816.901433	47.062413
3503.631639	503813.977863	47.067418
3503.630093	503812.561130	47.072423
3504.101922	503807.780001	47.077428
3503.504001	503803.066732	47.082433
3503.867412	503800.225874	47.087437
3503.701532	503775.352570	47.092442
3503.559533	503763.026493	47.097447
3504.024285	503757.892206	47.102452
3503.666950	503769.639433	47.107457
3503.632558	503752.488486	47.112461
3503.895428	503749.461075	47.117466
3503.688541	503745.900603	47.122471
3503.735446	503724.232574	47.127476
3503.315598	503717.416163	47.132481
3503.721065	503713.505853	47.137485
3503.789179	503707.169013	47.142490
3503.349050	503718.423268	47.147495
3503.881072	503708.824731	47.152500
3503.651553	503710.126306	47.157505
3503.863367	503702.501524	47.162509
3503.981989	503678.494082	47.167514
3503.536063	503664.039774	47.172519
3504.084531	503666.230574	47.177524
3503.519505	503668.951631	47.182529
3503.759849	503658.285764	47.187533
3503.753944	503631.514428	47.192538
3503.628223	503629.965478	47.197543
3504.127177	503616.677633	47.202548
3503.722110	503620.689260	47.207553
3503.541282	503621.628880	47.212557
3503.689843	503616.493918	47.217562
3503.317652	503615.945502	47.222567
3503.731781	503606.821028	47.227572
3503.635757	503590.337588	47.232577
3503.779973	503584.191114	47.237581
3503.733885	503568.307075	47.242586
3503.727219	503573.065496	47.247591
3504.006874	503568.972602	47.252596
3503.712288	503570.132642	47.257601
3503.758677	503549.881548	47.262605
3503.947521	503533.707297	47.267610
3503.784371	503530.645964	47.272615
3504.167689	503523.904972	47.277620
3504.310229	503523.781294	47.282625
3504.062520	503486.824797	47.287629
3503.973469	503494.582238	47.292634
3503.377216	503502.217402	47.297639
3503.545081	503481.440932	47.302644
3503.681730	503484.860871	47.307649
3503.827522	503465.251895	47.312653
3504.098252	503450.633531	47.317658
3503.742508	503444.464810	47.322663
3503.963180	503443.670853	47.327668
3503.608901	503446.358634	47.332673
3503.896404	503424.044889	47.337677
3503.815260	503408.115636	47.342682
3503.697785	503407.678784	47.347687
3504.374971	503401.852888	47.352692
3503.953718	503393.366441	47.357697
3503.816637	503370.107535	47.362701
3503.706162	503364.760392	47.367706
3503.648003	503355.457385	47.372711
3503.921860	503353.187324	47.377716
3503.281429	503365.738715	47.382721
3503.550171	503357.295024	47.387725
3503.976523	503348.320316	47.392730
3503.381602	503336.217357	47.397735
3503.768526	503316.418273	47.402740
3503.345773	503319.066285	47.407745
3503.794075	503317.021699	47.412749
3503.306187	503309.507338	47.417754
3503.324378	503321.853442	47.422759
3503.766877	503303.918140	47.427764
3503.634725	503314.010547	47.432769
3504.120281	503313.427770	47.437773
3504.039060	503290.969695	47.442778
3503.378098	503288.746157	47.447783
3504.241994	503254.751321	47.452788
3503.768397	503267.984959	47.457793
3503.670705	503265.419338	47.462797
3503.748324	503247.845313	47.467802
3503.478573	503226.884658	47.472807
3503.907256	503220.389433	47.477812
3503.673096	503237.583483	47.482817
3503.725443	503222.543953	47.487821
3504.152338	503211.797721	47.492826
3503.580085	503206.169242	47.497831
3503.666149	503186.873061	47.502836
3503.728198	503182.763860	47.507841
3503.735651	503185.748781	47.512845
3503.906151	503178.383356	47.517850
3504.014327	503175.582741	47.522855
3504.150920	503151.875406	47.527860
3503.807942	503140.289209	47.532865
3503.596843	503132.984078	47.537869
3503.996846	503131.655656	47.542874
3503.773351	503131.741661	47.547879
3503.935594	503112.838245	47.552884
3504.043181	503093.842227	47.557889
3504.031699	503083.114593	47.562893
3503.923588	503077.665767	47.567898
3503.832287	503070.797175	47.572903
3504.045459	503046.875152	47.577908
3503.770573	503044.135060	47.582913
3503.708557	503043.841266	47.587917
3503.806234	503024.036961	47.592922
3503.507368	503042.759761	47.597927
3503.722410	503012.207345	47.602932
3503.779602	502997.419912	47.607937
3504.018554	502999.305440	47.612941
3504.028886	502989.384081	47.617946
3503.511624	502985.872510	47.622951
3503.596574	502984.087760	47.627956
3503.420189	502974.499572	47.632961
3503.343123	502962.516949	47.637965
3503.803760	502945.894312	47.642970
3503.319350	502947.033784	47.647975
3503.691851	502951.934889	47.652980
3503.737482	502945.803775	47.657985
3503.541274	502948.213590	47.662989
3503.753991	502944.282965	47.667994
3503.711249	502947.377083	47.672999
3504.056494	502938.516210	47.678004
3504.084633	502905.411970	47.683009
3503.850285	502902.007500	47.688013
3503.871278	502893.653358	47.693018
3503.579934	502887.373039	47.698023
3503.877459	502888.793817	47.703028
3503.497451	502862.434723	47.708033
3503.499939	502854.589603	47.713037
3503.696739	502847.877835	47.718042
3503.514744	502858.180826	47.723047
3503.666544	502840.544060	47.728052
3503.585380	502846.478520	47.733057
3503.412139	502851.111629	47.738061
3503.662802	502844.745628	47.743066
3503.624080	502853.457016	47.748071
3503.875342	502838.588166	47.753076
3503.720175	502815.837504	47.758081
3503.698016	502804.200378	47.763085
3503.901617	502801.738904	47.768090
3503.484438	502805.752627	47.773095
3503.804837	502799.729870	47.778100
3503.679604	502813.263069	47.783105
3503.958745	502796.972649	47.788109
3503.719166	502789.469430	47.793114
3503.672570	502781.632035	47.798119
3503.880639	502764.492418	47.803124
3503.619201	502780.932045	47.808129
3503.919155	502773.292932	47.813133
3503.894177	502744.093896	47.818138
3503.850990	502737.420017	47.823143
3504.161504	502722.642929	47.828148
3503.810225	502723.002192	47.833153
3503.781106	502710.202029	47.838157
3503.658504	502681.777500	47.843162
3503.630900	502680.921527	47.848167
3503.580796	502675.868305	47.853172
3503.618818	502676.520323	47.858177
3503.858420	502674.255590	47.863181
3503.853317	502681.392774	47.868186
3503.755157	502673.209197	47.873191
3503.866475	502640.648047	47.878196
3503.799970	502632.914958	47.883201
3503.454174	502640.156619	47.888205
3503.560920	502636.040227	47.893210
3503.607095	502629.402795	47.898215
3503.914100	502621.205768	47.903220
3503.952667	502631.474030	47.908225
3503.595553	502612.196657	47.913229
3503.718246	502600.688339	47.918234
3503.584212	502596.863056	47.923239
3503.936600	502585.723323	47.928244
3504.057327	502599.976995	47.933249
3503.707990	502578.724475	47.938253
3503.499805	502555.931245	47.943258
3503.452115	502547.537183	47.948263
3503.626543	502547.509684	47.953268
3504.062587	502545.365723	47.958273
3503.455867	502548.295987	47.963277
3503.741375	502538.179045	47.968282
3503.759123	502549.614733	47.973287
3503.576710	502518.466321	47.978292
3503.617788	502511.323525	47.983297
3503.511248	502503.495482	47.988301
3503.683294	502499.166287	47.993306
3503.822314	502495.196599	47.998311
3503.818987	502487.301623	48.003316
3503.659993	502503.573477	48.008321
3503.691856	502494.255789	48.013325
3503.825566	502465.739789	48.018330
3503.210664	502456.068790	48.023335
3503.646466	502460.302062	48.028340
3503.506759	502452.732302	48.033345
3503.439523	502460.031234	48.038349
3503.666816	502450.783859	48.043354
3503.567330	502452.520487	48.048359
3503.668887	502444.558301	48.053364
3503.489982	502448.281381	48.058369
3503.560246	502456.722675	48.063373
3503.865739	502446.703747	48.068378
3503.347459	502439.041978	48.073383
3503.730462	502413.472647	48.078388
3503.831257	502399.386403	48.083393
3503.676139	502407.255989	48.088397
3503.587795	502399.070733	48.093402
3503.391212	502401.733745	48.098407
3503.611190	502408.633012	48.103412
3503.799745	502408.400829	48.108417
3503.494818	502404.349450	48.113421
3503.758373	502364.526086	48.118426
3503.537444	502368.002759	48.123431
3503.781666	502367.913616	48.128436
3503.772049	502362.904518	48.133441
3503.795157	502361.787450	48.138445
3503.675176	502358.820315	48.143450
3503.547493	502363.092059	48.148455
3503.690763	502346.670862	48.153460
3503.706911	502338.064158	48.158465
3503.577270	502326.949837	48.163469
3503.708886	502313.314172	48.168474
3503.554203	502325.587069	48.173479
3503.611647	502317.378733	48.178484
3503.734635	502315.233612	48.183489
3503.742038	502321.457928	48.188493
3503.668939	502295.555610	48.193498
3503.473196	502284.603550	48.198503
3503.564600	502265.761040	48.203508
3503.656626	502265.594725	48.208513
3503.511431	502263.491986	48.213517
3503.797559	502263.193765	48.218522
3503.423908	502262.645533	48.223527
3503.568929	502272.998404	48.228532
3503.880955	502261.308102	48.233537
3503.661886	502250.258481	48.238541
3503.757485	502237.083969	48.243546
3503.359036	502231.073411	48.248551
3503.853494	502225.225402	48.253556
3503.907346	502218.029856	48.258561
3503.604226	502226.429048	48.263565
3503.747362	502210.210200	48.268570
3503.611702	502220.556851	48.273575
3503.321249	502193.625857	48.278580
3503.905835	502179.058065	48.283585
3503.548323	502171.775678	48.288589
3503.648904	502172.569667	48.293594
3503.319723	502166.345684	48.298599
3503.619746	502168.727785	48.303604
3503.510015	502163.835682	48.308609
3503.696525	502170.183583	48.313613
3503.607823	502165.389384	48.318618
3503.474192	502169.813956	48.323623
3503.687106	502154.191390	48.328628
3503.759706	502147.701442	48.333633
3503.469405	502127.501934	48.338637
3503.597863	502118.016939	48.343642
3503.724520	502126.449478	48.348647
3503.765155	502118.395547	48.353652
3503.707793	502121.492120	48.358657
3503.504027	502133.772907	48.363661
3503.654758	502119.020571	48.368666
3503.456675	502102.754328	48.373671
3503.534487	502084.571752	48.378676
3503.757613	502087.016632	48.383681
3503.593770	502082.791039	48.388685
3503.764354	502080.992664	48.393690
3503.335214	502089.209384	48.398695
3503.740444	502084.387708	48.403700
3503.821532	502077.693938	48.408705
3503.718420	502079.228720	48.413709
3503.811452	502052.540583	48.418714
3503.417447	502042.328303	48.423719
3503.560608	502027.020334	48.428724
3503.493305	502031.889982	48.433729
3503.491418	502040.798404	48.438733
3503.383332	502024.872162	48.443738
3503.080030	502036.713223	48.448743
3503.446526	502024.761086	48.453748
3503.489711	502028.347922	48.458753
3503.162632	502041.407473	48.463757
3503.207502	502031.682574	48.468762
3503.282260	502033.948456	48.473767
3503.295602	502034.655013	48.478772
3503.463187	502035.185349	48.483777
3503.487540	502035.029728	48.488781
3503.726480	502027.754236	48.493786
3503.456890	502047.688194	48.498791
3503.466860	502024.707958	48.503796
3503.647589	502036.016990	48.508801
3503.292278	502042.804872	48.513805
3503.529296	502036.541966	48.518810
3503.455650	502032.352719	48.523815
3503.620444	502030.150342	48.528820
3503.808593	502003.953237	48.533825
3503.694476	501999.061782	48.538829
3503.768689	501994.241787	48.543834
3503.637332	502005.347095	48.548839
3503.580601	501987.236299	48.553844
3503.728561	501990.604126	48.558849
3503.415083	502003.307257	48.563853
3503.429433	501990.145404	48.568858
3503.388554	501991.366673	48.573863
3503.467336	501979.308138	48.578868
3503.514953	501958.143973	48.583873
3503.320867	501954.176200	48.588877
3503.609374	501944.260903	48.593882
3503.226694	501953.280169	48.598887
3503.495836	501948.024439	48.603892
3503.664265	501952.654393	48.608897
3503.321977	501950.785224	48.613901
3503.255265	501948.113286	48.618906
3503.279077	501953.525311	48.623911
3503.473402	501941.701559	48.628916
3503.646117	501946.482680	48.633921
3503.359847	501943.592373	48.638925
3503.671539	501941.265539	48.643930
3503.435784	501956.132829	48.648935
3503.459842	501941.552209	48.653940
3503.581775	501930.246034	48.658945
3503.156596	501941.954578	48.663949
3503.643778	501944.914499	48.668954
3503.493721	501947.013469	48.673959
3503.455923	501936.289300	48.678964
3503.508272	501933.902227	48.683969
3503.340766	501948.201981	48.688973
3503.783714	501931.479963	48.693978
3503.300097	501910.855234	48.698983
3503.565502	501896.388273	48.703988
3503.654443	501882.860252	48.708993
3503.470712	501899.592099	48.713997
3503.705173	501890.242071	48.719002
3503.588644	501891.222232	48.724007
3503.447225	501890.991582	48.729012
3503.580730	501881.455049	48.734017
3503.702793	501893.684504	48.739021
3504.058562	501880.266149	48.744026
3503.536064	501869.821007	48.749031
3503.586256	501857.412607	48.754036
3503.913254	501852.147704	48.759041
3503.544765	501848.207472	48.764045
3503.690500	501835.328425	48.769050
3503.434977	501845.339939	48.774055
3503.901922	501839.091237	48.779060
3503.852070	501839.352259	48.784065
3503.839803	501821.588568	48.789069
3503.809939	501800.740149	48.794074
3503.871832	501808.575701	48.799079
3503.674870	501798.838282	48.804084
3503.730471	501803.233036	48.809089
3503.643990	501786.847634	48.814093
3503.748233	501758.993146	48.819098
3503.725292	501763.096635	48.824103
3503.560772	501753.252835	48.829108
3504.024493	501753.786988	48.834113
3503.833776	501759.587283	48.839117
3503.855586	501737.971402	48.844122
3503.803359	501725.376639	48.849127
3503.529519	501717.574690	48.854132
3503.586246	501714.883207	48.859137
3503.678181	501718.968549	48.864141
3503.571407	501710.229124	48.869146
3503.916253	501718.424912	48.874151
3503.651159	501702.118278	48.879156
3503.707807	501676.447624	48.884161
3503.697915	501680.397224	48.889165
3504.022082	501678.473305	48.894170
3503.723872	501671.839332	48.899175
3503.805821	501668.587090	48.904180
3504.035921	501657.617950	48.909185
3503.914167	501642.149061	48.914189
3503.979697	501621.690275	48.919194
3504.021454	501629.022936	48.924199
3503.698822	501612.877159	48.929204
3504.046802	501579.618660	48.934209
3503.627328	501592.490682	48.939213
3504.341659	501570.562681	48.944218
3503.902484	501575.946767	48.949223
3503.722698	501557.905598	48.954228
3503.910364	501541.932178	48.959233
3503.645572	501531.496719	48.964237
3503.937991	501529.577801	48.969242
3503.703879	501532.145643	48.974247
3503.726293	501523.537554	48.979252
3503.866344	501493.956067	48.984257
3503.783559	501495.386456	48.989261
3503.433491	501481.573208	48.994266
3503.750607	501487.799480	48.999271
3503.714139	501486.135002	49.004276
3503.799545	501471.949224	49.009281
3504.006364	501475.054769	49.014285
3504.216953	501448.397760	49.019290
3503.707240	501450.857326	49.024295
3503.828780	501437.931201	49.029300
3503.921566	501436.296905	49.034305
3503.544913	501411.504204	49.039309
3503.852217	501400.320241	49.044314
3503.917006	501393.325095	49.049319
3503.772848	501397.245364	49.054324
3503.820067	501393.138093	49.059329
3503.826733	501387.822453	49.064333
3503.995107	501358.995502	49.069338
3503.585447	501354.150581	49.074343
3503.843261	501350.870485	49.079348
3503.904139	501343.471011	49.084353
3503.893086	501341.903734	49.089357
3503.987849	501326.197884	49.094362
3503.870557	501312.195865	49.099367
3503.706808	501317.637728	49.104372
3503.830254	501306.887694	49.109377
3503.768857	501315.147877	49.114381
3504.095171	501267.567887	49.119386
3503.965758	501265.918079	49.124391
3503.904426	501257.626794	49.129396
3504.017146	501258.064594	49.134401
3503.803207	501241.142057	49.139405
3503.908915	501223.409738	49.144410
3503.857993	501221.494438	49.149415
3504.025836	501216.254504	49.154420
3504.108571	501211.179869	49.159425
3503.812413	501185.614886	49.164429
3504.002237	501179.662837	49.169434
3503.897102	501176.035145	49.174439
3503.826045	501167.289807	49.179444
3504.127751	501147.501778	49.184449
3503.908459	501140.905749	49.189453
3503.903661	501128.910464	49.194458
3503.951007	501131.889426	49.199463
3503.556318	501118.285413	49.204468
3503.619567	501094.637539	49.209473
3503.541208	501084.931600	49.214477
3503.640167	501077.424763	49.219482
3503.696646	501093.461384	49.224487
3503.386949	501081.767342	49.229492
3503.731040	501084.142626	49.234497
3503.468616	501091.321120	49.239501
3504.024862	501081.717343	49.244506
3503.950144	501062.697348	49.249511
3503.660714	501043.711269	49.254516
3503.661155	501034.853333	49.259521
3503.535395	501040.643593	49.264525
3503.673278	501037.129312	49.269530
3503.698767	501036.517952	49.274535
3503.735201	501033.880190	49.279540
3504.127244	501006.637056	49.284545
3503.713874	500993.491452	49.289549
3503.898601	500990.830245	49.294554
3503.858357	500989.824338	49.299559
3503.561510	500982.076318	49.304564
3503.881498	500982.683833	49.309569
3503.778209	500972.779305	49.314573
3503.885845	500944.214369	49.319578
3503.743619	500957.549198	49.324583
3503.499188	500943.162047	49.329588
3503.612859	500935.197271	49.334593
3503.547452	500943.205175	49.339597
3503.551026	500929.284985	49.344602
3503.536554	500917.392322	49.349607
3503.347989	500901.579028	49.354612
3503.790921	500889.310347	49.359617
3503.378181	500890.084294	49.364621
3503.526483	500893.249807	49.369626
3503.441243	500905.360856	49.374631
3503.265771	500894.708436	49.379636
3503.611807	500886.858764	49.384641
3503.421041	500900.960565	49.389645
3503.455618	500885.314456	49.394650
3503.314494	500890.651639	49.399655
3503.388899	500885.223907	49.404660
3503.398366	500896.864437	49.409665
3503.340436	500900.821803	49.414669
3503.353358	500883.812452	49.419674
3503.397018	500874.340199	49.424679
3503.426011	500897.214668	49.429684
3503.264041	500892.684791	49.434689
3503.432468	500892.253303	49.439693
3503.486590	500894.775678	49.444698
3503.437248	500897.111938	49.449703
3503.189778	500892.393106	49.454708
3503.574128	500891.674403	49.459713
3503.286616	500900.476690	49.464717
3503.459236	500889.263077	49.469722
3503.575064	500893.851005	49.474727
3503.154019	500886.325043	49.479732
3503.853435	500874.015813	49.484737
3503.812154	500868.252040	49.489741
3503.635603	500850.057790	49.494746
3503.694560	500843.670758	49.499751
3503.731321	500849.081072	49.504756
3503.964011	500844.944361	49.509761
3503.497093	500851.547864	49.514765
3503.438398	500824.071989	49.519770
3503.822079	500810.445950	49.524775
3503.560306	500812.208387	49.529780
3503.720202	500799.073266	49.534785
3503.612418	500787.752057	49.539789
3503.556619	500794.493072	49.544794
3503.488656	500800.679215	49.549799
3503.417801	500800.488014	49.554804
3503.875011	500797.277537	49.559809
3503.312200	500804.250536	49.564813
3503.585818	500796.007331	49.569818
3503.282846	500773.176175	49.574823
3503.180763	500782.961562	49.579828
3503.709957	500784.598985	49.584833
3503.565714	500776.624286	49.589837
3503.510825	500777.240442	49.594842
3503.548753	500765.693718	49.599847
3503.566382	500770.347816	49.604852
3503.776237	500751.130658	49.609857
3503.436108	500759.283301	49.614861
3503.761491	500752.347951	49.619866
3503.523085	500746.868383	49.624871
3503.380608	500756.153993	49.629876
3503.797684	500758.062228	49.634881
3503.938045	500733.389335	49.639885
3503.734251	500723.247465	49.644890
3503.578604	500711.984390	49.649895
3503.581144	500713.553208	49.654900
3503.973840	500704.936816	49.659905
3503.649534	500708.733856	49.664909
3503.538685	500706.169942	49.669914
3503.661656	500707.213548	49.674919
3503.356829	500681.497358	49.679924
3503.629351	500665.104799	49.684929
3503.499388	500662.392046	49.689933
3503.598899	500664.806045	49.694938
3503.601849	500669.867432	49.699943
3503.559800	500665.267925	49.704948
3503.827931	500666.288590	49.709953
3503.493172	500662.190907	49.714957
3503.691308	500666.107853	49.719962
3503.870312	500657.879538	49.724967
3503.498682	500635.919562	49.729972
3503.638836	500625.166477	49.734977
3503.680675	500619.085778	49.739981
3503.852345	500622.601973	49.744986
3503.518238	500621.946198	49.749991
3503.449714	500619.173111	49.754996
3503.656881	500619.849088	49.760001
3503.722072	500624.900651	49.765005
3503.574538	500611.155950	49.770010
3503.440128	500593.663429	49.775015
3503.588169	500587.414080	49.780020
3503.748576	500583.946768	49.785025
3503.721591	500587.848694	49.790029
3503.665373	500583.200787	49.795034
3503.560365	500585.394032	49.800039
3503.703963	500590.939392	49.805044
3503.924938	500568.480724	49.810049
3503.534227	500552.648452	49.815053
3503.395549	500541.939388	49.820058
3503.833886	500541.060285	49.825063
3503.759582	500545.779591	49.830068
3503.600602	500534.820640	49.835073
3503.499637	500533.419358	49.840077
3503.649609	500531.522850	49.845082
3503.689018	500540.830441	49.850087
3503.617877	500526.516800	49.855092
3503.740509	500493.899314	49.860097
3503.597087	500491.644228	49.865101
3503.729138	500488.738181	49.870106
3503.632627	500491.031331	49.875111
3504.015557	500485.504095	49.880116
3503.763868	500486.860023	49.885121
3503.740097	500469.754841	49.890125
3503.729108	500447.838868	49.895130
3503.661828	500439.699999	49.900135
3503.807457	500449.446416	49.905140
3503.756375	500436.698704	49.910145
3503.581408	500449.330428	49.915149
3503.525288	500429.345068	49.920154
3503.876721	500426.606811	49.925159
3503.466803	500406.019303	49.930164
3503.487413	500397.613430	49.935169
3503.606597	500390.153726	49.940173
3503.670578	500403.051427	49.945178
3503.748124	500397.926763	49.950183
3503.464389	500409.867046	49.955188
3503.676174	500391.206000	49.960193
3503.197001	500392.648509	49.965197
3503.593456	500394.155094	49.970202
3503.651713	500397.689258	49.975207
3503.512256	500376.451545	49.980212
3503.748838	500360.722430	49.985217
3503.553875	500351.439471	49.990221
3503.795045	500350.591523	49.995226
3503.638807	500345.605032	50.000231
3503.754559	500349.990637	50.005236
3503.660745	500340.286735	50.010241
3503.623952	500347.024915	50.015245
3503.398913	500331.419355	50.020250
3503.588708	500309.370240	50.025255
3503.416464	500314.712513	50.030260
3503.591348	500306.079737	50.035265
3503.353186	500309.407676	50.040269
3503.523316	500297.536041	50.045274
3503.527143	500304.115960	50.050279
3503.406630	500312.082237	50.055284
3503.590144	500302.081387	50.060289
3503.525723	500306.697956	50.065293
3503.594364	500311.900918	50.070298
3503.779491	500303.570236	50.075303
3503.477207	500300.580951	50.080308
3503.507786	500307.764067	50.085313
3503.455025	500293.447334	50.090317
3503.777131	500272.490877	50.095322
3503.757983	500277.808963	50.100327
3503.405889	500269.917508	50.105332
3503.568042	500266.652335	50.110337
3503.574265	500264.221711	50.115341
3503.481146	500264.540213	50.120346
3503.761690	500258.775996	50.125351
3503.477837	500257.606075	50.130356
3503.896599	500258.856051	50.135361
3503.886712	500231.472787	50.140365
3503.772162	500220.911573	50.145370
3503.834295	500219.838822	50.150375
3503.426433	500205.628763	50.155380
3504.017341	500209.635587	50.160385
3503.884421	500214.566721	50.165389
3503.594205	500174.623513	50.170394
3503.967619	500171.173074	50.175399
3503.517200	500165.119406	50.180404
3503.553458	500158.634479	50.185409
3503.440983	500174.040580	50.190413
3503.411424	500164.123949	50.195418
3503.633544	500151.636569	50.200423
3503.709255	500174.605819	50.205428
3503.617937	500150.677409	50.210433
3503.461246	500135.617687	50.215437
3503.767989	500121.800809	50.220442
3503.571749	500111.606778	50.225447
3503.665998	500126.423432	50.230452
3503.591783	500116.766930	50.235457
3503.593171	500120.715093	50.240461
3503.936658	500111.346904	50.245466
3504.072417	500099.024995	50.250471
3503.492755	500093.244828	50.255476
3503.920395	500068.070036	50.260481
3503.754959	500071.639621	50.265485
3503.377610	500073.217918	50.270490
3503.687921	500060.007863	50.275495
3503.610090	500061.842538	50.280500
3503.687737	500066.689812	50.285505
3503.331082	500057.482875	50.290509
3503.477644	500041.767709	50.295514
3503.640130	500035.465265	50.300519
3503.340972	500037.233685	50.305524
3503.827429	500026.729223	50.310529
3503.613604	500031.470716	50.315533
3503.812140	500024.656374	50.320538
3504.052658	500021.631869	50.325543
3503.963205	500013.546929	50.330548
3503.966011	499999.524897	50.335553
3503.978440	499982.312287	50.340557
3503.930143	499982.117511	50.345562
3504.230896	499965.669231	50.350567
3503.722488	499956.030649	50.355572
3503.833694	499947.053426	50.360577
3503.658617	499948.144186	50.365581
3503.772321	499942.659337	50.370586
3504.174173	499937.888242	50.375591
3503.792653	499918.257461	50.380596
3503.585793	499895.359371	50.385601
3503.997845	499885.575267	50.390605
3503.741486	499884.198495	50.395610
3503.969589	499877.835004	50.400615
3503.845749	499867.426910	50.405620
3503.752161	499860.861158	50.410625
3503.643618	499849.741954	50.415629
3503.739343	499844.917979	50.420634
3503.910637	499855.015005	50.425639
3503.686226	499849.532949	50.430644
3503.889497	499825.101962	50.435649
3503.806886	499808.865991	50.440653
3503.655243	499805.144129	50.445658
3503.836559	499792.460467	50.450663
3503.941668	499794.620597	50.455668
3503.662852	499790.564490	50.460673
3503.414721	499769.444474	50.465677
3503.725624	499753.753700	50.470682
3503.693869	499762.667981	50.475687
3503.562662	499764.055540	50.480692
3503.776160	499754.505229	50.485697
3503.893892	499749.880232	50.490701
3503.700651	499737.356973	50.495706
3503.783441	499714.159769	50.500711
3503.442069	499721.351288	50.505716
3503.458334	499714.464396	50.510721
3503.620636	499707.807523	50.515725
3503.537183	499707.719542	50.520730
3503.795176	499684.545228	50.525735
3503.115127	499665.062594	50.530740
3503.479212	499632.709100	50.535745
3503.394996	499597.389154	50.540749
3503.398383	499543.882356	50.545754
3503.344840	499464.618206	50.550759
3503.102563	499398.241383	50.555764
3503.012512	499311.642220	50.560769
3502.851823	499221.004050	50.565773
3502.590555	499107.145724	50.570778
3502.926379	498999.267010	50.575783
3502.281912	498886.328436	50.580788
3502.445818	498759.846235	50.585793
3501.860853	498618.142559	50.590797
3501.429252	498468.414931	50.595802
3501.441168	498321.299053	50.600807
3500.943129	498170.668213	50.605812
3501.015172	498004.910289	50.610817
3500.521874	497831.595702	50.615821
3500.462858	497655.578244	50.620826
3500.107535	497460.215828	50.625831
3499.681338	497282.379582	50.630836
3499.496973	497069.418228	50.635841
3498.841644	496869.185946	50.640845
3498.485514	496669.359826	50.645850
3498.261025	496452.651028	50.650855
3497.923624	496228.565474	50.655860
3497.463189	495994.724838	50.660865
3497.005171	495773.994400	50.665869
3496.751315	495533.128039	50.670874
3496.386145	495285.946984	50.675879
3495.478675	495051.709233	50.680884
3495.370916	494799.265661	50.685889
3494.881412	494552.853876	50.690893
3494.577761	494302.966184	50.695898
3494.257535	494028.519085	50.700903
3493.683181	493770.514486	50.705908
3493.455707	493497.918390	50.710913
3492.916863	493211.745696	50.715917
3492.452850	492926.417611	50.720922
3491.988300	492636.527590	50.725927
3491.002662	492365.756400	50.730932
3490.778367	492070.958026	50.735937
3490.595309	491771.894481	50.740941
3490.003218	491474.359438	50.745946
3489.339162	491171.969175	50.750951
3488.559830	490865.489981	50.755956
3488.166043	490547.194976	50.760961
3487.747959	490240.091322	50.765965
3487.155447	489933.415384	50.770970
3486.632443	489620.139157	50.775975
3485.867523	489303.249199	50.780980
3485.688295	488981.956067	50.785985
3484.997285	488656.230417	50.790989
3484.280513	488336.328180	50.795994
3483.583652	488002.082662	50.800999
3483.047307	487680.266659	50.806004
3482.555264	487340.050617	50.811009
3481.738260	487013.860734	50.816013
3481.365909	486682.124097	50.821018
3480.999011	486348.455853	50.826023
3480.315694	486007.334403	50.831028
3479.693916	485659.662133	50.836033
3479.026095	485318.171333	50.841037
3478.404571	484980.568013	50.846042
3477.852703	484635.500487	50.851047
3476.947669	484282.680560	50.856052
3476.641602	483936.599071	50.861057
3476.168852	483585.876602	50.866061
3475.271125	483230.553740	50.871066
3474.813322	482873.330835	50.876071
3473.838971	482535.740543	50.881076
3473.363625	482184.233130	50.886081
3472.878797	481822.739080	50.891085
3471.859871	481471.102057	50.896090
3471.310537	481113.405317	50.901095
3470.660872	480752.728268	50.906100
3470.328258	480404.206591	50.911105
3469.471093	480047.299161	50.916109
3468.811958	479686.756065	50.921114
3468.614727	479327.349574	50.926119
3467.353168	478971.094694	50.931124
3466.719679	478598.922799	50.936129
3465.892176	478250.897430	50.941133
3465.093901	477899.719238	50.946138
3464.779874	477539.842699	50.951143
3464.033310	477174.858581	50.956148
3463.301089	476808.395752	50.961153
3462.551812	476455.765307	50.966157
3461.823139	476102.922666	50.971162
3461.448645	475732.835769	50.976167
3460.501588	475376.872458	50.981172
3460.171296	475015.736725	50.986177
3459.394500	474669.415114	50.991181
3458.482060	474305.317475	50.996186
3458.022335	473938.505896	51.001191
3457.201947	473589.942408	51.006196
3456.723135	473219.167047	51.011201
3456.204547	472863.750839	51.016205
3455.195602	472503.590157	51.021210
3454.578313	472142.752897	51.026215
3454.010524	471778.403542	51.031220
3453.320600	471417.565007	51.036225
3452.779799	471055.986822	51.041229
3451.639502	470697.538889	51.046234
3451.227687	470336.637464	51.051239
3450.291238	469991.326530	51.056244
3449.382174	469620.351454	51.061249
3448.980380	469265.158859	51.066253
3448.104680	468914.496845	51.071258
3447.851850	468551.206988	51.076263
3447.037705	468205.340046	51.081268
3446.328206	467842.617097	51.086273
3445.678125	467489.816645	51.091277
3444.675890	467124.085253	51.096282
3444.127839	466780.535926	51.101287
3443.331772	466429.464794	51.106292
3442.972825	466056.209886	51.111297
3442.164671	465715.878985	51.116301
3441.261803	465365.364879	51.121306
3440.469086	465013.052695	51.126311
3439.789122	464658.789806	51.131316
3439.242460	464318.243054	51.136321
3438.615681	463966.901596	51.141325
3437.860493	463614.053244	51.146330
3437.271037	463263.100055	51.151335
3436.512367	462917.442329	51.156340
3435.601545	462570.839488	51.161345
3435.311851	462217.945349	51.166349
3434.312536	461876.417090	51.171354
3434.004308	461509.871108	51.176359
3433.255067	461165.147514	51.181364
3432.170542	460820.572897	51.186369
3431.641634	460462.058000	51.191373
3430.743103	460118.406582	51.196378
3430.400614	459770.908339	51.201383
3429.404041	459432.891920	51.206388
3428.741819	459080.969575	51.211393
3428.357164	458747.411092	51.216397
3427.161947	458401.141940	51.221402
3426.849851	458062.641168	51.226407
3426.051141	457711.377982	51.231412
3424.978549	457378.567042	51.236417
3424.587334	457036.004790	51.241421
3423.960657	456701.743514	51.246426
3423.568392	456355.721300	51.251431
3422.196881	456019.893428	51.256436
3421.757755	455668.997732	51.261441
3421.189171	455333.387745	51.266445
3420.084468	455006.938897	51.271450
3419.712860	454679.608386	51.276455
3418.693125	454339.539490	51.281460
3418.193086	454000.651714	51.286465
3417.517479	453676.094471	51.291469
3417.007455	453344.758274	51.296474
3416.349892	453004.256888	51.301479
3415.189732	452670.223016	51.306484
3414.650933	452337.608210	51.311489
3414.234284	452000.148872	51.316493
3413.293286	451686.311518	51.321498
3412.896257	451337.473214	51.326503
3411.923986	451009.068502	51.331508
3411.266306	450673.860449	51.336513
3410.713853	450345.532131	51.341517
3409.479850	450034.002051	51.346522
3409.341215	449695.856012	51.351527
3408.787829	449376.546852	51.356532
3407.724546	449047.621187	51.361537
3407.118248	448714.914016	51.366541
3405.721320	448410.340382	51.371546
3405.561064	448068.926202	51.376551
3405.011007	447749.035978	51.381556
3404.177937	447441.264822	51.386561
3403.767907	447116.624015	51.391565
3402.764609	446798.061284	51.396570
3402.387161	446474.015495	51.401575
3401.638408	446154.236511	51.406580
3400.776045	445833.354575	51.411585
3400.383441	445501.938509	51.416589
3399.295075	445195.345812	51.421594
3398.580030	444860.571161	51.426599
3397.887182	444561.724245	51.431604
3397.139069	444240.396710	51.436609
3396.554333	443932.033153	51.441613
3395.916641	443621.085299	51.446618
3395.238457	443288.668505	51.451623
3394.337441	442977.753965	51.456628
3393.818036	442677.282595	51.461633
3393.276701	442349.348940	51.466637
3392.123569	442049.325297	51.471642
3391.682237	441736.799257	51.476647
3391.119600	441432.309016	51.481652
3390.539823	441115.228163	51.486657
3389.865640	440803.996071	51.491661
3389.048566	440489.888975	51.496666
3388.155611	440185.181581	51.501671
3387.698482	439876.390920	51.506676
3386.765461	439573.611408	51.511681
3386.338343	439257.294658	51.516685
3385.595828	438949.121326	51.521690
3384.999321	438649.856460	51.526695
3384.067794	438330.942223	51.531700
3383.653644	438025.345514	51.536705
3383.128980	437713.974608	51.541709
3382.033752	437420.587086	51.546714
3381.497589	437107.687273	51.551719
3380.434916	436794.079811	51.556724
3379.842970	436493.011254	51.561729
3379.353560	436194.639297	51.566733
3378.707554	435890.779487	51.571738
3377.942718	435585.538475	51.576743
3376.997415	435291.391496	51.581748
3376.606273	434973.745414	51.586753
3375.872014	434690.475078	51.591757
3375.027934	434389.649800	51.596762
3374.422407	434082.029704	51.601767
3373.642940	433780.044490	51.606772
3372.843052	433502.687081	51.611777
3372.146478	433185.117760	51.616781
3371.455418	432904.715239	51.621786
3370.892774	432614.336194	51.626791
3370.114546	432325.054382	51.631796
3369.284418	432036.666224	51.636801
3368.862037	431734.803625	51.641805
3367.929861	431448.075487	51.646810
3367.867866	431160.876488	51.651815
3367.192851	430865.061644	51.656820
3366.128933	430572.529803	51.661825
3365.633249	430275.562628	51.666829
3364.670963	429986.461594	51.671834
3364.163169	429685.731429	51.676839
3363.458972	429400.036639	51.681844
3362.698097	429106.043823	51.686849
3362.116273	428816.361857	51.691853
3361.403264	428532.665203	51.696858
3360.867950	428236.366899	51.701863
3360.288930	427947.512997	51.706868
3359.577115	427650.017074	51.711873
3358.804104	427360.552572	51.716877
3357.918984	427067.140861	51.721882
3357.442491	426783.515097	51.726887
3356.931213	426492.552198	51.731892
3355.628238	426212.225642	51.736897
3355.164256	425919.776027	51.741901
3354.640795	425635.282037	51.746906
3354.332403	425348.541433	51.751911
3353.402028	425061.184992	51.756916
3352.504102	424768.918502	51.761921
3352.011777	424487.836268	51.766925
3351.077703	424201.690422	51.771930
3350.390221	423912.937267	51.776935
3349.812333	423628.786400	51.781940
3349.154929	423336.187085	51.786945
3348.566760	423051.193652	51.791949
3347.822715	422779.277562	51.796954
3347.282611	422490.994095	51.801959
3346.242044	422206.368235	51.806964
3345.790292	421923.271985	51.811969
3345.327718	421628.769423	51.816973
3344.517877	421357.357736	51.821978
3343.668931	421059.887455	51.826983
3343.035949	420793.548027	51.831988
3342.421710	420501.978716	51.836993
3341.634967	420217.724141	51.841997
3340.573366	419942.934544	51.847002
3340.128886	419669.721259	51.852007
3339.562323	419389.995996	51.857012
3338.977292	419121.194356	51.862017
3338.414574	418837.550862	51.867021
3337.330713	418560.515744	51.872026
3336.841768	418278.861886	51.877031
3335.817034	418009.585711	51.882036
3335.196470	417733.358396	51.887041
3334.870777	417460.943320	51.892045
3333.817583	417192.476865	51.897050
3333.228617	416917.684742	51.902055
3332.680848	416638.615313	51.907060
3331.707664	416371.551218	51.912065
3331.295374	416097.028159	51.917069
3330.525200	415817.503205	51.922074
3329.771633	415553.267707	51.927079
3329.045641	415287.704274	51.932084
3328.561084	415015.900894	51.937089
3327.908533	414740.183396	51.942093
3326.991216	414487.117888	51.947098
3326.435918	414215.089535	51.952103
3326.033374	413946.058046	51.957108
3325.196621	413675.847741	51.962113
3324.525512	413401.111442	51.967117
3323.731295	413137.241569	51.972122
3323.391063	412859.754556	51.977127
3322.929328	412591.965053	51.982132
3322.243178	412321.718484	51.987137
3321.418450	412040.285695	51.992141
3320.280932	411768.987434	51.997146
3319.486880	411494.176597	52.002151
3319.003732	411231.688907	52.007156
3318.056343	410980.707085	52.012161
3317.769426	410705.249745	52.017165
3316.906314	410445.381726	52.022170
3316.077138	410182.126390	52.027175
3315.229977	409921.488974	52.032180
3314.875594	409665.497948	52.037185
3314.303701	409397.239780	52.042189
3313.459419	409139.212577	52.047194
3312.673369	408875.735721	52.052199
3312.201377	408610.300968	52.057204
3311.084252	408355.639296	52.062209
3310.801119	408097.234956	52.067213
3310.070596	407843.168603	52.072218
3309.767966	407576.401992	52.077223
3308.884743	407323.727802	52.082228
3307.846842	407065.967807	52.087233
3307.378317	406792.790916	52.092237
3306.352963	406543.207895	52.097242
3306.081645	406286.514621	52.102247
3305.326496	406027.481336	52.107252
3304.594181	405779.980652	52.112257
3303.551177	405526.224179	52.117261
3303.007786	405274.902742	52.122266
3302.398671	405016.397077	52.127271
3302.186981	404767.306496	52.132276
3301.432737	404508.209606	52.137281
3300.602209	404251.613424	52.142285
3299.891931	404001.731466	52.147290
3298.942132	403746.446261	52.152295
3298.610925	403488.926152	52.157300
3297.561233	403240.337266	52.162305
3297.269530	402983.620142	52.167309
3296.453998	402737.837009	52.172314
3295.938636	402477.592737	52.177319
3294.858227	402230.729206	52.182324
3294.366114	401987.075063	52.187329
3293.609984	401729.658752	52.192333
3293.068654	401487.304920	52.197338
3292.474577	401234.535988	52.202343
3292.020647	400986.114937	52.207348
3291.463564	400736.056054	52.212353
3290.602594	400475.799373	52.217357
3289.758255	400225.731138	52.222362
3289.038695	399968.549183	52.227367
3288.279784	399718.565211	52.232372
3287.684758	399471.069978	52.237377
3287.402882	399210.889528	52.242381
3286.602761	398972.828415	52.247386
3285.634364	398720.632952	52.252391
3285.000226	398474.305717	52.257396
3284.440826	398224.660100	52.262401
3283.844811	397969.222370	52.267405
3283.167598	397721.218531	52.272410
3282.327768	397463.146218	52.277415
3281.557940	397210.196011	52.282420
3280.780280	396969.752686	52.287425
3280.416436	396713.785559	52.292429
3279.548567	396471.700477	52.297434
3278.567698	396233.444881	52.302439
3277.966769	395983.611052	52.307444
3277.471420	395732.360412	52.312449
3276.847604	395494.475293	52.317453
3276.218935	395265.843299	52.322458
3275.523254	395010.525837	52.327463
3275.208381	394765.035984	52.332468
3274.030019	394522.884315	52.337473
3273.533460	394276.656958	52.342477
3272.850869	394031.219967	52.347482
3272.059110	393787.603603	52.352487
3271.661388	393546.389355	52.357492
3271.009595	393306.103458	52.362497
3270.279186	393055.454990	52.367501
3269.563727	392812.480684	52.372506
3269.091789	392576.356373	52.377511
3268.421617	392325.413399	52.382516
3267.368145	392078.571893	52.387521
3266.867661	391837.082272	52.392525
3266.278704	391593.850582	52.397530
3265.327285	391357.895526	52.402535
3264.844498	391106.659866	52.407540
3264.105745	390878.194106	52.412545
3263.444417	390627.796898	52.417549
3262.706645	390390.911611	52.422554
3262.222524	390148.034710	52.427559
3261.787239	389911.378056	52.432564
3260.783737	389672.292393	52.437569
3260.103832	389420.389353	52.442573
3259.579713	389188.242584	52.447578
3258.838177	388942.575676	52.452583
3257.835629	388702.084812	52.457588
3257.232253	388461.834331	52.462593
3256.518126	388229.609674	52.467597
3255.786679	388005.319937	52.472602
3254.974032	387761.970174	52.477607
3254.542904	387519.067000	52.482612
3253.789489	387285.138740	52.487617
3253.300290	387046.233925	52.492621
3252.272603	386818.016730	52.497626
3251.665836	386584.849070	52.502631
3251.323096	386365.929602	52.507636
3250.453041	386124.358010	52.512641
3249.780040	385891.781287	52.517645
3248.975360	385669.268806	52.522650
3248.312887	385437.806465	52.527655
3247.822575	385194.948041	52.532660
3246.921849	384970.208651	52.537665
3246.521927	384740.073658	52.542669
3245.590785	384519.125520	52.547674
3245.006932	384280.980611	52.552679
3244.629947	384047.048470	52.557684
3243.801339	383824.223510	52.562689
3243.370901	383587.931832	52.567693
3242.533502	383350.024542	52.572698
3241.793234	383122.196823	52.577703
3241.262385	382894.080279	52.582708
3240.231652	382685.802196	52.587713
3239.814086	382450.238868	52.592717
3239.110909	382224.968526	52.597722
3238.495454	381991.824299	52.602727
3237.964500	381751.264344	52.607732
3237.050400	381526.074090	52.612737
3236.484791	381286.254240	52.617741
3235.877534	381076.705003	52.622746
3235.038528	380840.689723	52.627751
3234.821775	380608.415029	52.632756
3233.897585	380372.664687	52.637761
3233.352999	380145.220589	52.642765
3232.891088	379907.435884	52.647770
3232.087801	379672.272566	52.652775
3231.268206	379439.094279	52.657780
3230.369804	379222.408574	52.662785
3230.024690	378981.954557	52.667789
3229.311441	378745.525114	52.672794
3228.411612	378513.345950	52.677799
3227.685598	378278.594417	52.682804
3226.943145	378049.185474	52.687809
3226.348996	377817.335383	52.692813
3225.481111	377604.985374	52.697818
3224.861130	377373.772660	52.702823
3224.376784	377142.893246	52.707828
3223.267943	376930.704928	52.712833
3222.998704	376696.558545	52.717837
3222.455106	376487.279915	52.722842
3221.214454	376258.270122	52.727847
3220.671411	376032.379105	52.732852
3220.170325	375814.899704	52.737857
3219.299134	375590.584316	52.742861
3218.417153	375368.736770	52.747866
3217.969407	375151.270800	52.752871
3217.317449	374932.589549	52.757876
3216.601110	374715.494420	52.762881
3216.007375	374492.579006	52.767885
3215.394025	374276.660813	52.772890
3214.505126	374059.029869	52.777895
3214.000122	373842.481748	52.782900
3213.356108	373631.372766	52.787905
3212.548015	373411.919523	52.792909
3212.074306	373196.584091	52.797914
3211.217383	372970.318783	52.802919
3210.888084	372751.473139	52.807924
3209.819965	372542.180954	52.812929
3209.482020	372320.027390	52.817933
3208.787199	372105.764283	52.822938
3207.927409	371892.721812	52.827943
3207.378989	371666.248003	52.832948
3206.703648	371452.792537	52.837953
3206.274620	371232.301184	52.842957
3205.722752	371024.954927	52.847962
3204.686115	370800.232716	52.852967
3204.154669	370577.108430	52.857972
3203.387968	370362.593453	52.862977
3202.882214	370129.592058	52.867981
3202.251714	369922.100229	52.872986
3201.671461	369699.716848	52.877991
3200.698129	369476.351438	52.882996
3200.118112	369262.462879	52.888001
3199.537989	369036.743336	52.893005
3198.581299	368822.912188	52.898010
3198.118734	368605.312876	52.903015
3197.556989	368380.172152	52.908020
3196.686643	368171.895749	52.913025
3196.374531	367942.871651	52.918029
3195.564681	367737.636575	52.923034
3194.633228	367514.025485	52.928039
3194.306662	367291.131705	52.933044
3193.357594	367079.707795	52.938049
3192.862354	366859.891546	52.943053
3192.094992	366645.867176	52.948058
3191.318385	366428.815610	52.953063
3190.622377	366209.587633	52.958068
3189.739018	366002.804155	52.963073
3189.401396	365792.269651	52.968077
3189.058348	365571.023627	52.973082
3187.887384	365354.385431	52.978087
3187.454282	365142.718061	52.983092
3186.434956	364926.740783	52.988097
3185.881624	364711.044959	52.993101
3185.232665	364502.640033	52.998106
3184.430854	364284.717037	53.003111
3184.262033	364079.770859	53.008116
3183.200396	363873.031285	53.013121
3182.579102	363651.769034	53.018125
3181.886877	363438.887991	53.023130
3181.285700	363228.815849	53.028135
3180.705254	363016.373164	53.033140
3179.674721	362808.631565	53.038145
3179.224283	362590.466841	53.043149
3178.626948	362385.326476	53.048154
3177.916927	362181.144487	53.053159
3177.209295	361967.037781	53.058164
3176.202947	361758.677000	53.063169
3175.954908	361545.029999	53.068173
3175.681211	361337.442016	53.073178
3174.446201	361128.427601	53.078183
3173.913856	360919.530104	53.083188
3173.089695	360707.827967	53.088193
3172.772423	360492.431430	53.093197
3171.912946	360293.226787	53.098202
3171.068510	360090.176626	53.103207
3170.629572	359867.900723	53.108212
3169.560283	359659.693354	53.113217
3168.785469	359453.423290	53.118221
3168.468873	359259.115897	53.123226
3167.422132	359051.487596	53.128231
3166.576879	358839.627872	53.133236
3166.453872	358644.218637	53.138241
3165.596501	358438.109990	53.143245
3165.055852	358243.757641	53.148250
3164.417504	358035.246099	53.153255
3164.222542	357823.279082	53.158260
3163.141770	357628.144549	53.163265
3162.537677	357419.497740	53.168269
3162.100412	357207.999012	53.173274
3161.320841	356998.920141	53.178279
3160.435958	356798.585531	53.183284
3159.609880	356586.153217	53.188289
3159.290102	356373.996165	53.193293
3158.841617	356176.363810	53.198298
3158.006103	355973.829573	53.203303
3157.646576	355752.489497	53.208308
3156.750926	355549.581347	53.213313
3156.002877	355336.342511	53.218317
3155.388765	355134.736911	53.223322
3154.342042	354917.166459	53.228327
3153.627855	354706.286324	53.233332
3153.002793	354504.883551	53.238337
3152.633006	354299.749536	53.243341
3151.927904	354099.732066	53.248346
3150.932233	353894.466417	53.253351
3150.925435	353688.992600	53.258356
3149.996307	353479.464788	53.263361
3149.271844	353270.947168	53.268365
3148.643859	353073.382105	53.273370
3147.983637	352857.777755	53.278375
3147.187165	352652.373884	53.283380
3146.432017	352449.991175	53.288385
3145.899488	352239.072259	53.293389
3145.320748	352036.965448	53.298394
3144.547322	351831.376579	53.303399
3143.839036	351624.275055	53.308404
3143.092420	351429.191243	53.313409
3142.343847	351224.461397	53.318413
3141.813521	351017.176656	53.323418
3141.159921	350818.105647	53.328423
3140.427048	350618.002972	53.333428
3139.584992	350418.018631	53.338433
3138.953411	350213.368223	53.343437
3138.592946	350015.647661	53.348442
3137.669275	349815.674007	53.353447
3137.160048	349611.790950	53.358452
3136.398054	349414.208085	53.363457
3135.807860	349212.499689	53.368461
3135.044120	349010.003570	53.373466
3134.204633	348802.402970	53.378471
3133.873910	348604.443542	53.383476
3132.941505	348415.868411	53.388481
3132.434870	348206.202240	53.393485
3131.775679	348002.438761	53.398490
3131.269559	347812.190679	53.403495
3130.573648	347607.922535	53.408500
3129.689936	347412.489748	53.413505
3129.417662	347209.909315	53.418509
3128.585076	347003.904409	53.423514
3127.454249	346795.527978	53.428519
3127.262670	346602.553555	53.433524
3126.203718	346412.108244	53.438529
3125.805736	346213.260196	53.443533
3125.137857	346016.414011	53.448538
3124.509782	345812.892247	53.453543
3123.971985	345605.079410	53.458548
3123.230985	345403.584837	53.463553
3122.417382	345204.849969	53.468557
3121.735619	345016.452952	53.473562
3121.227327	344813.799576	53.478567
3120.838767	344602.599720	53.483572
3119.982979	344405.981420	53.488577
3119.298027	344198.466829	53.493581
3118.647875	344000.058349	53.498586
3117.650030	343807.991249	53.503591
3117.107973	343606.688091	53.508596
3116.426176	343410.191665	53.513601
3115.573239	343213.721670	53.518605
3115.117901	343013.522754	53.523610
3114.504866	342815.689888	53.528615
3113.913455	342609.071291	53.533620
3113.030766	342428.690409	53.538625
3112.454799	342220.133520	53.543629
3111.888504	342019.007048	53.548634
3111.295553	341831.145876	53.553639
3110.763993	341618.405373	53.558644
3109.674588	341428.279702	53.563649
3109.330201	341223.399127	53.568653
3108.413144	341021.968511	53.573658
3107.612802	340822.860613	53.578663
3107.311882	340625.938537	53.583668
3106.527389	340426.801403	53.588673
3105.837290	340232.892441	53.593677
3105.212728	340031.157775	53.598682
3104.221331	339834.546097	53.603687
3103.944561	339637.006155	53.608692
3102.863292	339442.851182	53.613697
3102.293249	339243.065428	53.618701
3101.597840	339056.612131	53.623706
3100.966836	338858.998536	53.628711
3100.350174	338656.061816	53.633716
3099.736818	338469.568365	53.638721
3098.991306	338270.112797	53.643725
3098.594465	338074.750757	53.648730
3097.494469	337888.230801	53.653735
3096.825548	337700.165643	53.658740
3096.266699	337511.853418	53.663745
3095.650655	337302.344658	53.668749
3094.991258	337105.544787	53.673754
3094.365081	336927.169493	53.678759
3093.955389	336731.754547	53.683764
3092.855683	336540.444884	53.688769
3092.257812	336348.215191	53.693773
3091.944524	336149.295716	53.698778
3091.212171	335953.318572	53.703783
3090.445758	335759.128222	53.708788
3089.661121	335566.696718	53.713793
3089.386444	335373.623915	53.718797
3088.853204	335168.015692	53.723802
3087.961170	334978.119752	53.728807
3087.560452	334779.871947	53.733812
3086.968982	334583.664874	53.738817
3085.984582	334378.583887	53.743821
3085.748405	334179.544583	53.748826
3084.753087	333992.284363	53.753831
3083.721524	333791.205914	53.758836
3083.250137	333587.161525	53.763841
3082.690575	333389.316714	53.768845
3081.989969	333189.482496	53.773850
3081.083340	332996.553931	53.778855
3080.716928	332803.132022	53.783860
3079.977186	332609.004921	53.788865
3078.798869	332410.236945	53.793869
3078.614472	332219.177695	53.798874
3077.852050	332038.621805	53.803879
3077.462439	331834.330275	53.808884
3076.399224	331641.575552	53.813889
3075.965349	331436.246101	53.818893
3075.405555	331248.273219	53.823898
3074.384598	331048.280015	53.828903
3073.976318	330841.391856	53.833908
3073.191605	330649.252344	53.838913
3072.535984	330463.965762	53.843917
3071.817949	330272.349344	53.848922
3071.154900	330097.068329	53.853927
3070.794666	329896.865590	53.858932
3070.072985	329698.807148	53.863937
3069.263318	329499.743740	53.868941
3069.073025	329308.194073	53.873946
3067.919965	329117.992855	53.878951
3067.326426	328909.321013	53.883956
3067.188952	328717.837863	53.888961
3065.702180	328521.857763	53.893965
3065.068628	328329.688356	53.898970
3064.332121	328133.970421	53.903975
3063.906526	327937.617214	53.908980
3063.287580	327746.666095	53.913985
3062.572660	327559.879628	53.918989
3061.829530	327366.655846	53.923994
3060.883656	327182.985656	53.928999
3060.649235	326980.132966	53.934004
3059.778178	326790.950671	53.939009
3059.070755	326607.343236	53.944013
3058.396088	326423.297368	53.949018
3057.678774	326233.249223	53.954023
3057.278083	326037.040063	53.959028
3056.536590	325854.632908	53.964033
3055.898366	325662.686826	53.969037
3055.456090	325456.349607	53.974042
3054.724284	325273.786838	53.979047
3053.989681	325078.442917	53.984052
3053.374721	324882.799525	53.989057
3052.495304	324706.369384	53.994061
3051.980750	324498.589916	53.999066
3051.548612	324309.077714	54.004071
3050.560328	324111.607468	54.009076
3049.948231	323924.898096	54.014081
3049.173863	323731.212225	54.019085
3048.681338	323539.263572	54.024090
3047.751659	323355.811274	54.029095
3047.005949	323150.254673	54.034100
3046.698371	322971.922617	54.039105
3045.699237	322780.867172	54.044109
3045.323822	322592.462408	54.049114
3044.329108	322407.337907	54.054119
3044.001552	322206.957891	54.059124
3043.200643	322023.915190	54.064129
3042.588221	321837.761430	54.069133
3042.220427	321644.133779	54.074138
3041.051281	321461.682864	54.079143
3040.696651	321267.033830	54.084148
3040.056133	321079.966283	54.089153
3039.354594	320890.158124	54.094157
3038.632434	320695.031298	54.099162
3037.921393	320498.196338	54.104167
3037.174613	320299.406031	54.109172
3036.354578	320116.413322	54.114177
3035.918687	319923.862099	54.119181
3035.437942	319730.553703	54.124186
3034.558890	319545.583137	54.129191
3034.055280	319352.252095	54.134196
3033.674750	319167.252792	54.139201
3032.808129	318979.860202	54.144205
3032.127361	318785.130119	54.149210
3031.522982	318593.188404	54.154215
3031.044206	318384.319329	54.159220
3030.381094	318197.529521	54.164225
3029.485459	318014.417292	54.169229
3028.959019	317821.672328	54.174234
3028.153682	317632.892366	54.179239
3027.520230	317430.818741	54.184244
3026.727464	317243.181844	54.189249
3025.992674	317069.208951	54.194253
3025.546669	316875.660008	54.199258
3024.758415	316687.512062	54.204263
3024.198865	316488.862270	54.209268
3023.560162	316302.345010	54.214273
3022.794409	316114.166940	54.219277
3022.496462	315914.430601	54.224282
3021.805164	315729.448373	54.229287
3020.884784	315541.064524	54.234292
3020.365052	315347.677034	54.239297
3019.862736	315151.230818	54.244301
3019.194092	314955.905472	54.249306
3018.171763	314761.272314	54.254311
3017.631185	314558.516080	54.259316
3016.727307	314369.134371	54.264321
3016.134774	314184.592044	54.269325
3015.650770	313983.124370	54.274330
3014.932563	313789.179693	54.279335
3014.093936	313601.823354	54.284340
3013.723024	313420.020147	54.289345
3012.857820	313228.822326	54.294349
3012.358068	313030.436444	54.299354
3011.192248	312837.095610	54.304359
3010.715013	312650.622564	54.309364
3010.411603	312468.679737	54.314369
3009.700035	312280.486127	54.319373
3008.983155	312085.850624	54.324378
3008.075464	311889.742593	54.329383
3007.435013	311700.976524	54.334388
3007.110327	311514.095434	54.339393
3006.249643	311324.319549	54.344397
3005.648312	311135.546330	54.349402
3004.360574	310949.911691	54.354407
3003.983242	310760.873213	54.359412
3003.459705	310575.269793	54.364417
3002.738590	310393.415153	54.369421
3002.075086	310194.871863	54.374426
3001.474667	310010.425602	54.379431
3000.948976	309830.627239	54.384436
3000.235181	309633.924400	54.389441
2999.271122	309452.106740	54.394445
2999.059355	309251.122133	54.399450
2998.102266	309068.844418	54.404455
2997.665434	308879.863235	54.409460
2996.917085	308695.209152	54.414465
2996.060188	308501.073573	54.419469
2995.569521	308313.627917	54.424474
2994.831663	308125.075176	54.429479
2994.031075	307936.404750	54.434484
2993.507028	307765.515776	54.439489
2992.826599	307568.753361	54.444493
2992.172522	307381.230294	54.449498
2991.626079	307203.952358	54.454503
2991.076114	307008.696323	54.459508
2990.075265	306813.409494	54.464513
2989.405599	306628.103253	54.469517
2988.820239	306432.291705	54.474522
2988.272998	306254.987114	54.479527
2987.517812	306067.554520	54.484532
2986.993564	305881.893146	54.489537
2985.966493	305696.769477	54.494541
2985.622803	305507.284650	54.499546
2984.468081	305325.261989	54.504551
2984.134242	305144.178701	54.509556
2983.498741	304956.318146	54.514561
2982.680703	304772.153271	54.519565
2981.854493	304583.991337	54.524570
2981.292895	304409.589653	54.529575
2980.873556	304223.832995	54.534580
2980.092840	304044.907176	54.539585
2979.506284	303876.824277	54.544589
2979.178313	303676.791601	54.549594
2978.196755	303494.026071	54.554599
2977.419689	303309.598122	54.559604
2976.874491	303117.315204	54.564609
2976.374206	302934.498249	54.569613
2975.746551	302742.380681	54.574618
2974.671744	302552.854774	54.579623
2974.228720	302375.299518	54.584628
2973.614489	302195.632001	54.589633
2973.182907	302014.611121	54.594637
2972.620191	301818.025512	54.599642
2971.621733	301640.786501	54.604647
2971.079294	301438.696503	54.609652
2970.494030	301254.235642	54.614657
2969.705024	301072.226105	54.619661
2969.341341	300874.054342	54.624666
2968.635166	300691.954853	54.629671
2967.906093	300491.624879	54.634676
2967.235349	300309.417476	54.639681
2966.275793	300128.758102	54.644685
2965.781463	299924.392037	54.649690
2965.103682	299746.565341	54.654695
2964.261886	299555.751040	54.659700
2963.949486	299369.385759	54.664705
2963.125347	299186.488325	54.669709
2962.793897	298988.665690	54.674714
2962.051731	298811.382987	54.679719
2961.348852	298609.238450	54.684724
2960.580049	298426.331438	54.689729
2959.917319	298237.091706	54.694733
2959.550513	298031.735428	54.699738
2958.502869	297843.498469	54.704743
2957.960209	297655.079507	54.709748
2957.201813	297464.631687	54.714753
2956.539860	297276.766016	54.719757
2956.251191	297083.467556	54.724762
2955.375953	296893.648840	54.729767
2955.222963	296701.449045	54.734772
2954.171516	296510.842891	54.739777
2953.361549	296312.252629	54.744781
2952.982780	296113.721237	54.749786
2952.004434	295932.729451	54.754791
2951.176630	295746.696662	54.759796
2950.745839	295545.091412	54.764801
2950.023863	295361.282606	54.769805
2949.461612	295166.701229	54.774810
2948.400810	294987.198722	54.779815
2947.881230	294790.980332	54.784820
2947.242735	294599.160932	54.789825
2946.657388	294415.024036	54.794829
2946.158855	294219.693124	54.799834
2945.410911	294038.102891	54.804839
2944.728536	293838.445832	54.809844
2944.360909	293652.694838	54.814849
2943.624765	293455.134255	54.819853
2943.061958	293259.557974	54.824858
2942.132242	293058.564121	54.829863
2941.472704	292867.179456	54.834868
2941.054460	292683.167445	54.839873
2940.179009	292486.290214	54.844877
2939.482705	292290.148479	54.849882
2938.524906	292101.509943	54.854887
2937.964144	291914.845803	54.859892
2937.522542	291726.558202	54.864897
2936.569782	291516.449302	54.869901
2936.204062	291329.117147	54.874906
2935.343444	291138.170398	54.879911
2934.748098	290949.753737	54.884916
2934.268922	290775.580401	54.889921
2933.301443	290578.996342	54.894925
2932.963408	290375.563565	54.899930
2932.047840	290194.837338	54.904935
2931.447244	290010.622990	54.909940
2930.871318	289819.273657	54.914945
2930.087022	289628.033580	54.919949
2929.699252	289436.348582	54.924954
2929.237791	289241.669925	54.929959
2928.195581	289044.358020	54.934964
2927.560650	288852.355207	54.939969
2926.695257	288664.336260	54.944973
2926.569882	288471.335690	54.949978
2925.528156	288272.698866	54.954983
2924.969172	288091.634706	54.959988
2924.238301	287886.912541	54.964993
2923.676101	287700.653220	54.969997
2922.988257	287499.413091	54.975002
2922.293771	287313.913056	54.980007
2921.430527	287126.478602	54.985012
2921.102023	286926.938522	54.990017
2920.158550	286740.764483	54.995021
2919.679227	286542.979876	55.000026
2919.301305	286357.225457	55.005031
2918.046111	286164.657062	55.010036
2917.666870	285973.350631	55.015041
2916.926611	285781.668298	55.020045
2916.379703	285578.596514	55.025050
2915.869146	285395.409411	55.030055
2915.041510	285200.709921	55.035060
2914.723273	285001.396374	55.040065
2913.577243	284815.457182	55.045069
2913.231047	284615.052745	55.050074
2912.449846	284424.980725	55.055079
2911.822192	284223.983959	55.060084
2911.006409	284020.189921	55.065089
2910.437195	283836.476585	55.070093
2909.768723	283631.207366	55.075098
2909.063979	283445.630688	55.080103
2908.259433	283250.035278	55.085108
2907.798363	283061.210884	55.090113
2906.961296	282877.743329	55.095117
2906.331433	282683.291578	55.100122
2905.511639	282492.562715	55.105127
2904.955057	282302.352414	55.110132
2904.375265	282109.522493	55.115137
2903.571649	281925.794634	55.120141
2902.991035	281730.443361	55.125146
2902.067066	281547.065524	55.130151
2901.360331	281353.873430	55.135156
2901.035514	281167.751925	55.140161
2900.277858	280983.074181	55.145165
2899.793601	280791.018236	55.150170
2899.224958	280596.454237	55.155175
2898.308431	280399.958735	55.160180
2897.752106	280202.489295	55.165185
2896.921708	280015.326923	55.170189
2896.610783	279816.366840	55.175194
2895.501300	279618.781085	55.180199
2894.787348	279440.997957	55.185204
2894.471354	279233.353841	55.190209
2893.694298	279056.726704	55.195213
2893.239835	278864.920267	55.200218
2892.526339	278678.910651	55.205223
2891.955291	278479.864123	55.210228
2891.383597	278285.580245	55.215233
2890.598973	278091.482856	55.220237
2890.340996	277892.310259	55.225242
2889.517106	277702.930677	55.230247
2888.400008	277505.651361	55.235252
2887.935809	277304.703077	55.240257
2886.911955	277114.158069	55.245261
2886.329718	276921.403778	55.250266
2885.971735	276732.714373	55.255271
2885.403567	276538.175032	55.260276
2884.662798	276346.337184	55.265281
2883.747941	276153.788301	55.270285
2883.489951	275957.187808	55.275290
2882.706160	275756.875762	55.280295
2882.166961	275566.330313	55.285300
2881.196004	275372.542325	55.290305
2880.676224	275185.330149	55.295309
2880.165058	274984.440080	55.300314
2879.303016	274788.750179	55.305319
2878.978413	274592.975187	55.310324
2878.014565	274394.754569	55.315329
2877.411513	274202.130813	55.320333
2876.696405	273996.052028	55.325338
2876.207036	273813.801389	55.330343
2875.262441	273621.078923	55.335348
2874.929145	273424.643171	55.340353
2874.286610	273218.196383	55.345357
2873.527477	273019.663271	55.350362
2872.602366	272823.270332	55.355367
2872.217722	272634.126731	55.360372
2871.566235	272440.008130	55.365377
2870.805281	272249.930886	55.370381
2870.163270	272043.356799	55.375386
2869.569479	271847.471820	55.380391
2868.822607	271656.857588	55.385396
2868.443226	271450.318414	55.390401
2867.763857	271257.554214	55.395405
2867.099304	271062.495550	55.400410
2866.489090	270861.927156	55.405415
2865.593470	270659.977765	55.410420
2865.074327	270455.549314	55.415425
2864.061957	270261.768358	55.420429
2863.785461	270062.446179	55.425434
2863.030897	269865.288142	55.430439
2862.030821	269674.943596	55.435444
2861.366084	269475.810373	55.440449
2860.729080	269285.663119	55.445453
2860.000405	269085.827011	55.450458
2859.324118	268894.769222	55.455463
2858.699783	268708.109271	55.460468
2858.565493	268507.415171	55.465473
2857.525113	268310.200943	55.470477
2856.917599	268109.403620	55.475482
2856.263154	267909.836270	55.480487
2855.553276	267732.562469	55.485492
2855.191334	267521.717447	55.490497
2854.231503	267331.570960	55.495501
2853.565851	267130.121012	55.500506
2852.816633	266943.226714	55.505511
2852.078736	266748.002593	55.510516
2851.760601	266546.981743	55.515521
2850.955718	266361.344415	55.520525
2850.380948	266156.951627	55.525530
2849.843891	265948.936481	55.530535
2848.918439	265770.984389	55.535540
2848.604176	265564.742378	55.540545
2847.753248	265375.878288	55.545549
2847.348979	265165.626757	55.550554
2846.459358	264980.003418	55.555559
2845.876170	264777.700987	55.560564
2845.215572	264571.819918	55.565569
2844.212297	264374.601418	55.570573
2843.398906	264173.609149	55.575578
2843.007932	263977.236214	55.580583
2842.501256	263792.495116	55.585588
2842.070036	263584.082393	55.590593
2841.273264	263390.040678	55.595597
2840.705936	263188.933579	55.600602
2839.713225	262988.989075	55.605607
2839.170868	262785.942691	55.610612
2838.735373	262582.140938	55.615617
2837.853182	262385.362780	55.620621
2837.488152	262178.672244	55.625626
2836.785153	261977.943905	55.630631
2835.907309	261786.564615	55.635636
2835.293814	261584.319749	55.640641
2834.676544	261378.357312	55.645645
2834.147806	261175.488068	55.650650
2833.528618	260973.702932	55.655655
2833.070831	260776.018156	55.660660
2832.209647	260563.218610	55.665665
2831.126896	260361.329031	55.670669
2830.479815	260160.287446	55.675674
2829.776097	259959.458717	55.680679
2829.078743	259770.395197	55.685684
2828.581959	259572.029819	55.690689
2827.730152	259376.547714	55.695693
2827.235182	259174.183925	55.700698
2826.423504	258976.454613	55.705703
2825.615503	258778.826742	55.710708
2825.277062	258574.095620	55.715713
2824.332945	258378.781698	55.720717
2823.637157	258176.068490	55.725722
2823.264823	257988.712072	55.730727
2822.412482	257801.024329	55.735732
2822.192030	257593.779528	55.740737
2821.442271	257401.109701	55.745741
2820.822660	257198.818205	55.750746
2820.054366	256997.110713	55.755751
2819.341567	256799.443924	55.760756
2818.731774	256594.884811	55.765761
2817.886595	256396.398917	55.770765
2817.470541	256194.127020	55.775770
2816.733005	255995.573507	55.780775
2815.863068	255803.153285	55.785780
2815.468421	255608.111247	55.790785
2814.800080	255409.216246	55.795789
2814.368743	255199.282076	55.800794
2813.416964	255000.610618	55.805799
2812.782308	254796.642903	55.810804
2812.161391	254595.780205	55.815809
2811.148872	254402.314241	55.820813
2810.597525	254196.754981	55.825818
2810.191301	254001.665372	55.830823
2809.059846	253800.884326	55.835828
2808.507681	253601.616171	55.840833
2807.906432	253411.269432	55.845837
2807.388738	253209.500465	55.850842
2806.682983	253016.394777	55.855847
2806.013536	252814.854001	55.860852
2805.533875	252610.227367	55.865857
2804.700466	252417.346252	55.870861
2804.138026	252219.838409	55.875866
2803.713907	252023.582214	55.880871
2802.893333	251825.122479	55.885876
2802.184529	251612.765908	55.890881
2801.365643	251423.092372	55.895885
2800.785502	251215.299910	55.900890
2800.319379	251016.632160	55.905895
2799.176057	250820.134677	55.910900
2799.087960	250616.976339	55.915905
2798.355676	250416.950779	55.920909
2797.499052	250218.422206	55.925914
2797.122279	250015.921510	55.930919
2796.263848	249813.853871	55.935924
2795.532538	249614.898719	55.940929
2794.880234	249422.730822	55.945933
2794.136263	249218.430225	55.950938
2793.692294	249022.740927	55.955943
2792.977651	248816.806358	55.960948
2792.500505	248608.466088	55.965953
2791.692554	248412.402267	55.970957
2790.980395	248215.941532	55.975962
2790.616651	248007.584112	55.980967
2789.892659	247795.082120	55.985972
2788.920252	247589.597474	55.990977
2788.371220	247387.636773	55.995981
2787.654477	247184.938925	56.000986
2787.056769	246981.229332	56.005991
2786.193412	246788.003127	56.010996
2785.761567	246573.368413	56.016001
2784.877974	246383.762110	56.021005
2784.250224	246184.693182	56.026010
2783.985856	245982.485621	56.031015
2783.060909	245775.646334	56.036020
2782.855364	245568.005845	56.041025
2781.457962	245374.178562	56.046029
2780.999824	245167.953821	56.051034
2780.586162	244957.265863	56.056039
2779.747299	244760.982687	56.061044
2779.148807	244550.350096	56.066049
2778.757539	244347.273733	56.071053
2777.763192	244151.270724	56.076058
2777.095810	243941.846877	56.081063
2776.304993	243742.017893	56.086068
2775.604132	243534.255246	56.091073
2774.907881	243339.021127	56.096077
2774.613846	243137.764730	56.101082
2773.828631	242933.250494	56.106087
2773.023316	242746.616325	56.111092
2772.449558	242534.429685	56.116097
2771.552006	242337.191764	56.121101
2771.342635	242136.025404	56.126106
2770.659566	241936.589616	56.131111
2769.860894	241733.632825	56.136116
2769.502193	241519.020143	56.141121
2768.463690	241320.838495	56.146125
2767.893306	241118.050288	56.151130
2767.360456	240918.796083	56.156135
2766.369711	240714.343523	56.161140
2765.701035	240490.003290	56.166145
2764.971837	240301.374533	56.171149
2764.538225	240107.810053	56.176154
2763.719196	239903.051585	56.181159
2762.918551	239703.790907	56.186164
2762.543723	239498.555365	56.191169
2761.925656	239303.264385	56.196173
2761.072637	239101.593916	56.201178
2760.492259	238894.507642	56.206183
2759.952481	238700.147475	56.211188
2759.472119	238482.452956	56.216193
2758.582319	238292.503320	56.221197
2757.965091	238084.023840	56.226202
2757.021401	237885.782110	56.231207
2756.356338	237682.480181	56.236212
2755.681436	237478.365337	56.241217
2754.925848	237287.046580	56.246221
2754.282788	237088.173008	56.251226
2754.063702	236889.843784	56.256231
2753.095396	236683.026807	56.261236
2752.734207	236479.831788	56.266241
2751.694679	236285.325881	56.271245
2751.137921	236086.567820	56.276250
2750.632047	235876.139717	56.281255
2749.532275	235677.952244	56.286260
2749.028181	235476.793419	56.291265
2748.376964	235290.961858	56.296269
2747.912294	235091.096178	56.301274
2747.632390	234883.664450	56.306279
2746.587872	234687.354422	56.311284
2745.653706	234472.311757	56.316289
2745.374508	234279.548020	56.321293
2744.519903	234079.847941	56.326298
2743.824250	233881.498095	56.331303
2743.203288	233683.213203	56.336308
2742.882597	233477.216766	56.341313
2741.802008	233290.336524	56.346317
2741.217678	233085.630351	56.351322
2740.795783	232875.729910	56.356327
2740.126763	232674.806523	56.361332
2739.387043	232476.593808	56.366337
2738.661435	232285.941702	56.371341
2737.997644	232078.372954	56.376346
2737.651891	231872.638518	56.381351
2736.673260	231667.845035	56.386356
2736.322548	231453.276778	56.391361
2735.438865	231255.598658	56.396365
2734.732504	231053.436947	56.401370
2734.057519	230855.319220	56.406375
2733.203602	230654.709488	56.411380
2732.747980	230448.791882	56.416385
2731.741850	230257.424460	56.421389
2731.158229	230058.020866	56.426394
2730.261667	229851.614277	56.431399
2729.607749	229661.872817	56.436404
2729.441988	229466.503722	56.441409
2728.724190	229274.812622	56.446413
2727.813797	229070.523353	56.451418
2727.417635	228868.266430	56.456423
2726.697748	228673.470613	56.461428
2726.186955	228467.540808	56.466433
2725.465932	228272.593286	56.471437
2724.662230	228069.587974	56.476442
2724.571041	227873.828653	56.481447
2723.441465	227674.644184	56.486452
2722.813783	227464.712348	56.491457
2722.131541	227265.126970	56.496461
2721.439045	227069.133720	56.501466
2721.021419	226858.559025	56.506471
2720.164034	226661.472537	56.511476
2719.758048	226451.508075	56.516481
2719.075071	226256.839169	56.521485
2718.196069	226046.619648	56.526490
2717.805640	225842.026510	56.531495
2716.824812	225638.940470	56.536500
2716.218688	225434.140623	56.541505
2715.647367	225230.697920	56.546509
2714.781832	225030.930468	56.551514
2714.617618	224821.950249	56.556519
2713.675521	224613.679375	56.561524
2713.050929	224407.331927	56.566529
2712.373914	224215.645772	56.571533
2711.468049	224010.362309	56.576538
2711.028727	223795.623359	56.581543
2709.947111	223600.069151	56.586548
2709.796724	223392.796278	56.591553
2709.058788	223201.631407	56.596557
2708.115048	222994.663466	56.601562
2707.561472	222790.816760	56.606567
2706.923782	222587.391266	56.611572
2706.340389	222382.824738	56.616577
2705.749728	222194.936039	56.621581
2704.918039	221985.508886	56.626586
2704.204687	221774.752387	56.631591
2703.303693	221582.942634	56.636596
2702.814634	221380.107800	56.641601
2702.343177	221184.564840	56.646605
2701.646267	220983.507955	56.651610
2701.304763	220773.433638	56.656615
2700.263736	220575.003738	56.661620
2699.814217	220360.072244	56.666625
2699.203092	220169.289438	56.671629
2698.420223	219970.858433	56.676634
2697.687423	219755.680773	56.681639
2696.969131	219555.000265	56.686644
2696.391131	219356.182029	56.691649
2695.941581	219151.386640	56.696653
2694.731511	218951.982239	56.701658
2694.600271	218739.016270	56.706663
2693.766181	218544.046867	56.711668
2693.113696	218339.273177	56.716673
2692.325309	218149.898454	56.721677
2691.669660	217941.129432	56.726682
2691.260929	217729.852454	56.731687
2690.302070	217537.222242	56.736692
2689.806342	217332.642989	56.741697
2689.068539	217128.280879	56.746701
2688.458406	216919.113042	56.751706
2687.975413	216715.373669	56.756711
2687.195224	216509.861734	56.761716
2686.436102	216307.020126	56.766721
2685.774341	216110.082586	56.771725
2684.907260	215902.956917	56.776730
2684.535844	215699.317395	56.781735
2683.601698	215502.653851	56.786740
2683.273557	215286.267257	56.791745
2682.444212	215103.729808	56.796749
2681.748233	214902.091547	56.801754
2681.199546	214690.425903	56.806759
2680.660436	214500.092402	56.811764
2680.074157	214283.151649	56.816769
2679.278379	214079.342348	56.821773
2678.392670	213881.657548	56.826778
2677.889270	213673.704616	56.831783
2677.073768	213475.284380	56.836788
2676.796460	213261.760095	56.841793
2676.001867	213059.964791	56.846797
2675.133609	212861.656575	56.851802
2674.539223	212650.131914	56.856807
2673.760257	212452.345371	56.861812
2673.467493	212243.396235	56.866817
2672.660962	212039.607651	56.871821
2671.801661	211840.970182	56.876826
2671.236358	211631.302509	56.881831
2670.647298	211428.716009	56.886836
2670.065706	211209.162687	56.891841
2669.327327	210993.936967	56.896845
2668.608840	210796.985946	56.901850
2667.786122	210589.488001	56.906855
2667.328727	210382.951077	56.911860
2666.577388	210176.703220	56.916865
2666.311499	209972.962843	56.921869
2665.070584	209775.512293	56.926874
2664.772035	209569.716526	56.931879
2663.982581	209362.153716	56.936884
2663.437894	209160.292912	56.941889
2662.981581	208953.404155	56.946893
2662.050186	208745.305887	56.951898
2661.462077	208532.559364	56.956903
2660.650147	208325.143592	56.961908
2660.282021	208121.069119	56.966913
2659.614252	207919.028243	56.971917
2658.711077	207719.761673	56.976922
2658.223877	207505.017299	56.981927
2657.407555	207298.636614	56.986932
2656.846995	207090.077971	56.991937
2656.362592	206890.595065	56.996941
2655.367017	206679.879537	57.001946
2654.995065	206472.833120	57.006951
2654.212134	206269.326966	57.011956
2653.532918	206057.659910	57.016961
2652.899302	205858.624077	57.021965
2652.134746	205651.184557	57.026970
2651.707303	205431.436557	57.031975
2650.572939	205237.471016	57.036980
2650.050153	205024.535673	57.041985
2649.599494	204826.148860	57.046989
2648.940272	204618.174520	57.051994
2648.551181	204416.394098	57.056999
2647.566542	204211.845284	57.062004
2647.105179	204000.151154	57.067009
2646.363398	203788.438597	57.072013
2645.403017	203599.961471	57.077018
2644.915633	203378.054548	57.082023
2644.457299	203183.161591	57.087028
2643.749171	202967.628883	57.092033
2642.951010	202758.410677	57.097037
2641.998937	202555.504300	57.102042
2641.392538	202342.363081	57.107047
2640.726605	202138.980186	57.112052
2640.215433	201934.924487	57.117057
2639.489669	201732.328829	57.122061
2638.752599	201538.071110	57.127066
2638.315656	201326.523092	57.132071
2637.802224	201125.283113	57.137076
2636.599919	200919.457229	57.142081
2635.888515	200717.766523	57.147085
2635.566656	200514.131453	57.152090
2634.870513	200305.669829	57.157095
2634.134963	200114.814600	57.162100
2633.546861	199905.446601	57.167105
2633.006058	199695.435644	57.172109
2632.097189	199498.845430	57.177114
2631.798144	199278.261196	57.182119
2631.291547	199084.942782	57.187124
2630.409293	198880.728177	57.192129
2629.573313	198671.773259	57.197133
2628.795317	198463.586202	57.202138
2628.617250	198254.541402	57.207143
2627.723884	198050.229929	57.212148
2627.140582	197846.213691	57.217153
2626.704333	197637.466723	57.222157
2625.783695	197444.334379	57.227162
2625.179132	197219.760556	57.232167
2624.706146	197015.157437	57.237172
2623.687025	196802.217889	57.242177
2623.049612	196599.156687	57.247181
2622.307240	196396.138356	57.252186
2622.111808	196187.664397	57.257191
2620.828774	195986.896504	57.262196
2620.277581	195784.562848	57.267201
2619.886268	195576.275082	57.272205
2619.219900	195366.848374	57.277210
2618.615469	195146.533430	57.282215
2617.922299	194963.273782	57.287220
2617.378977	194762.864270	57.292225
2616.518477	194559.795556	57.297229
2615.542642	194352.394286	57.302234
2615.572057	194128.776843	57.307239
2614.537618	193929.122814	57.312244
2613.873293	193726.077260	57.317249
2613.283777	193518.401901	57.322253
2612.257863	193312.145274	57.327258
2612.068769	193107.932675	57.332263
2611.047798	192901.117116	57.337268
2610.116885	192691.705240	57.342273
2609.685925	192493.284589	57.347277
2609.018927	192299.991563	57.352282
2608.851185	192084.175888	57.357287
2607.721643	191882.305792	57.362292
2607.387801	191680.017811	57.367297
2606.994295	191471.365711	57.372301
2605.863691	191265.477742	57.377306
2605.372812	191049.170718	57.382311
2604.458595	190842.181498	57.387316
2603.945043	190638.246848	57.392321
2603.338962	190432.508315	57.397325
2602.753597	190231.831146	57.402330
2602.394386	190013.344968	57.407335
2601.656619	189800.428792	57.412340
2600.599593	189600.007116	57.417345
2600.233186	189383.013527	57.422349
2599.306466	189181.211620	57.427354
2598.564949	188964.584718	57.432359
2597.687346	188752.471462	57.437364
2597.326516	188561.600337	57.442369
2597.076499	188345.458182	57.447373
2596.063885	188149.437592	57.452378
2595.397485	187924.584832	57.457383
2594.924927	187720.808839	57.462388
2593.967014	187511.678211	57.467393
2593.596876	187295.979759	57.472397
2592.816161	187094.825222	57.477402
2592.260726	186878.420179	57.482407
2591.378965	186673.314173	57.487412
2590.349463	186469.033976	57.492417
2590.129373	186261.611321	57.497421
2589.370442	186057.646290	57.502426
2588.943212	185839.266633	57.507431
2588.155504	185634.939108	57.512436
2587.480571	185435.657878	57.517441
2587.200433	185216.825348	57.522445
2586.258787	185009.535424	57.527450
2585.376608	184788.803059	57.532455
2584.715042	184590.655637	57.537460
2584.122355	184370.451909	57.542465
2583.693644	184163.148196	57.547469
2582.358066	183964.754131	57.552474
2582.115167	183749.204909	57.557479
2581.421103	183540.648552	57.562484
2580.705386	183338.520778	57.567489
2580.115129	183136.030572	57.572493
2579.615312	182923.413739	57.577498
2578.796859	182712.374932	57.582503
2578.047095	182506.579982	57.587508
2577.283707	182300.075784	57.592513
2576.647584	182091.097275	57.597517
2575.864742	181889.584635	57.602522
2575.717497	181675.505948	57.607527
2574.557291	181474.118622	57.612532
2574.077999	181277.559901	57.617537
2573.611415	181065.519213	57.622541
2572.785519	180862.059185	57.627546
2572.302095	180647.275595	57.632551
2571.820421	180441.778617	57.637556
2570.972883	180231.557780	57.642561
2570.580800	180012.819596	57.647565
2569.463331	179817.742413	57.652570
2569.016405	179599.193109	57.657575
2568.359839	179396.768935	57.662580
2567.502944	179185.689749	57.667585
2567.102961	178975.175198	57.672589
2566.643426	178769.466495	57.677594
2565.859764	178552.349660	57.682599
2565.155184	178349.213058	57.687604
2564.214433	178141.484915	57.692609
2564.055365	177915.839267	57.697613
2563.155379	177711.057726	57.702618
2562.367267	177488.159712	57.707623
2561.680653	177284.847333	57.712628
2560.976614	177083.446601	57.717633
2560.111052	176866.745758	57.722637
2559.334653	176661.937058	57.727642
2558.881138	176451.558109	57.732647
2558.021262	176245.111214	57.737652
2557.410048	176044.425800	57.742657
2556.845378	175841.686241	57.747661
2556.022933	175637.589456	57.752666
2555.488244	175424.608524	57.757671
2554.726883	175227.842840	57.762676
2554.096242	175018.936499	57.767681
2553.927315	174818.314180	57.772685
2553.063004	174618.019261	57.777690
2552.393049	174393.325935	57.782695
2551.597837	174189.473728	57.787700
2550.978950	173987.909344	57.792705
2550.656353	173774.560042	57.797709
2549.613979	173569.007732	57.802714
2548.778991	173351.341371	57.807719
2548.373769	173148.259307	57.812724
2547.816542	172951.904754	57.817729
2547.008997	172741.041499	57.822733
2546.325487	172532.550664	57.827738
2545.792306	172321.760609	57.832743
2544.869172	172117.112553	57.837748
2544.215742	171912.053999	57.842753
2544.083960	171696.638007	57.847757
2543.025355	171492.536072	57.852762
2542.463333	171285.278869	57.857767
2542.152618	171073.442815	57.862772
2541.461662	170877.539409	57.867777
2540.484790	170653.259174	57.872781
2539.637847	170451.303766	57.877786
2539.429863	170233.923989	57.882791
2538.439840	170035.248999	57.887796
2537.926212	169828.182606	57.892801
2537.303682	169612.169135	57.897805
2536.154760	169406.223032	57.902810
2535.872410	169197.915255	57.907815
2535.167016	168995.690659	57.912820
2534.284806	168793.228099	57.917825
2533.594667	168576.697045	57.922829
2532.804365	168383.199999	57.927834
2532.325186	168170.452769	57.932839
2531.896167	167966.485799	57.937844
2530.916313	167766.320383	57.942849
2530.745484	167549.827299	57.947853
2529.821201	167345.230040	57.952858
2529.262270	167135.286082	57.957863
2528.645296	166933.541620	57.962868
2527.757959	166721.973488	57.967873
2527.345035	166516.256969	57.972877
2526.492763	166309.975413	57.977882
2525.634036	166100.923978	57.982887
2525.276505	165897.948675	57.987892
2524.307408	165695.389287	57.992897
2523.827848	165479.516524	57.997901
2523.511723	165279.119281	58.002906
2522.582753	165065.392769	58.007911
2522.049866	164849.328671	58.012916
2521.350759	164652.161630	58.017921
2520.673680	164442.976289	58.022925
2519.731020	164234.330114	58.027930
2519.380056	164018.928660	58.032935
2518.750898	163816.897854	58.037940
2518.157800	163614.862447	58.042945
2517.884753	163391.925100	58.047949
2516.736901	163186.546975	58.052954
2516.220966	162951.126778	58.057959
2515.798005	162701.046155	58.062964
2515.202600	162486.836788	58.067969
2514.504298	162270.941260	58.072973
2513.532068	162053.183280	58.077978
2512.890573	161841.019341	58.082983
2512.449713	161629.384279	58.087988
2511.310136	161408.414596	58.092993
2510.813402	161195.430532	58.097997
2510.057024	160990.346130	58.103002
2509.619125	160781.779671	58.108007
2508.817419	160576.323411	58.113012
2508.079649	160367.552625	58.118017
2507.454459	160153.336476	58.123021
2506.914778	159952.088668	58.128026
2506.262277	159726.526167	58.133031
2505.265610	159520.166121	58.138036
2504.493201	159322.480411	58.143041
2504.184601	159107.648315	58.148045
2503.391602	158902.874197	58.153050
2502.602009	158688.553148	58.158055
2502.033248	158467.994425	58.163060
2501.051447	158246.701638	58.168065
2500.291177	158041.342575	58.173069
2499.678577	157842.025348	58.178074
2499.151472	157628.063305	58.183079
2498.414741	157431.005558	58.188084
2497.898844	157234.600412	58.193089
2497.434265	157023.225568	58.198093
2496.528626	156825.969212	58.203098
2495.927374	156613.258306	58.208103
2495.287969	156403.745555	58.213108
2494.986458	156206.473271	58.218113
2494.193395	155999.389957	58.223117
2493.389000	155796.301290	58.228122
2492.817547	155586.808187	58.233127
2492.370261	155368.728840	58.238132
2491.323655	155174.822149	58.243137
2490.989128	154952.265733	58.248141
2490.215742	154743.661515	58.253146
2489.584582	154541.798625	58.258151
2488.747525	154324.219962	58.263156
2488.232133	154121.476849	58.268161
2487.670108	153917.204267	58.273165
2486.830094	153720.451243	58.278170
2486.204855	153499.602948	58.283175
2485.759256	153294.082712	58.288180
2484.878953	153084.323582	58.293185
2484.672820	152873.162389	58.298189
2483.687691	152659.037252	58.303194
2482.778223	152446.414089	58.308199
2482.156831	152241.118866	58.313204
2481.357495	152046.822436	58.318209
2480.918867	151828.891799	58.323213
2479.786067	151628.905487	58.328218
2479.330417	151422.966252	58.333223
2479.042408	151208.460366	58.338228
2478.211183	151012.929460	58.343233
2477.571763	150793.563100	58.348237
2476.969698	150591.045906	58.353242
2475.957763	150374.957056	58.358247
2475.539175	150166.871829	58.363252
2474.820750	149968.062826	58.368257
2474.450978	149758.205795	58.373261
2474.012444	149559.011762	58.378266
2472.935533	149342.241028	58.383271
2472.479440	149124.470964	58.388276
2471.846002	148924.968562	58.393281
2471.205377	148710.001203	58.398285
2470.207962	148500.239100	58.403290
2469.774677	148288.101285	58.408295
2469.092431	148084.748219	58.413300
2468.376654	147882.621827	58.418305
2468.074795	147665.307418	58.423309
2467.259516	147465.830187	58.428314
2466.626145	147248.075516	58.433319
2465.818524	147026.969432	58.438324
2464.918705	146832.593054	58.443329
2464.707224	146618.321529	58.448333
2463.950216	146413.440524	58.453338
2463.150202	146198.413658	58.458343
2462.562334	145985.184623	58.463348
2461.875835	145774.539722	58.468353
2461.182222	145558.992018	58.473357
2460.089789	145357.144743	58.478362
2459.617511	145151.438906	58.483367
2459.180459	144931.902662	58.488372
2457.999421	144725.638451	58.493377
2457.939693	144525.602546	58.498381
2456.980121	144320.818122	58.503386
2456.424143	144105.766913	58.508391
2456.012600	143909.107401	58.513396
2455.062899	143705.710577	58.518401
2454.438108	143489.505465	58.523405
2453.461038	143288.059938	58.528410
2453.078055	143078.897280	58.533415
2452.740133	142866.730036	58.538420
2451.740842	142661.950170	58.543425
2451.081253	142455.199084	58.548429
2450.422796	142249.249738	58.553434
2449.902865	142035.490615	58.558439
2449.207542	141822.027626	58.563444
2448.404905	141616.791546	58.568449
2448.205907	141403.761064	58.573453
2447.013682	141200.190555	58.578458
2446.363179	140996.662600	58.583463
2445.825227	140785.138692	58.588468
2444.956928	140571.495887	58.593473
2444.543602	140373.220248	58.598477
2443.993801	140167.115290	58.603482
2443.511601	139955.855167	58.608487
2442.559574	139741.087984	58.613492
2442.021717	139541.376395	58.618497
2441.414880	139323.190483	58.623501
2440.802850	139119.783435	58.628506
2439.875352	138907.419664	58.633511
2439.636475	138692.724816	58.638516
2438.516742	138483.621674	58.643521
2438.054853	138274.885806	58.648525
2437.110953	138080.508254	58.653530
2436.418032	137847.850343	58.658535
2435.925750	137636.862298	58.663540
2434.831852	137446.400360	58.668545
2434.729682	137229.153460	58.673549
2433.915571	137030.175846	58.678554
2433.090898	136827.758334	58.683559
2432.774467	136620.167181	58.688564
2432.028572	136406.954045	58.693569
2431.621230	136202.835823	58.698573
2430.996481	135999.337876	58.703578
2430.413679	135780.602555	58.708583
2429.666138	135563.635426	58.713588
2428.844147	135353.440158	58.718593
2428.380744	135138.285913	58.723597
2427.386602	134926.672791	58.728602
2426.799320	134712.875218	58.733607
2426.415275	134504.865193	58.738612
2425.342911	134290.703012	58.743617
2424.756641	134081.038543	58.748621
2424.095838	133875.134856	58.753626
2423.629902	133660.716072	58.758631
2423.122542	133445.695708	58.763636
2422.108117	133234.771459	58.768641
2421.743775	133029.563597	58.773645
2420.914394	132815.602528	58.778650
2420.297057	132604.111864	58.783655
2419.774149	132382.560086	58.788660
2418.909020	132176.358023	58.793665
2418.307628	131962.684767	58.798669
2417.583256	131744.624931	58.803674
2416.991312	131536.097798	58.808679
2416.543982	131314.872613	58.813684
2415.322508	131108.455356	58.818689
2415.091294	130905.477250	58.823693
2414.189937	130688.977830	58.828698
2413.379867	130485.370513	58.833703
2412.690639	130274.340484	58.838708
2412.065740	130073.755176	58.843713
2411.370913	129857.419941	58.848717
2410.992464	129652.950047	58.853722
2410.382535	129443.501363	58.858727
2409.784721	129220.093801	58.863732
2409.198383	129010.670028	58.868737
2408.470493	128795.529453	58.873741
2407.614891	128583.814610	58.878746
2407.141682	128375.520759	58.883751
2406.257975	128156.218601	58.888756
2405.707970	127944.472893	58.893761
2404.978805	127735.691011	58.898765
2404.334437	127536.447922	58.903770
2403.192355	127314.704140	58.908775
2402.883653	127108.743302	58.913780
2402.209954	126906.283587	58.918785
2401.866730	126677.357070	58.923789
2401.180832	126480.846005	58.928794
2400.586892	126264.827641	58.933799
2399.936428	126045.378338	58.938804
2399.385374	125833.395077	58.943809
2399.090728	125620.585447	58.948813
2397.784825	125398.108505	58.953818
2396.935158	125178.786664	58.958823
2396.615662	124971.649922	58.963828
2395.692156	124761.346865	58.968833
2395.140210	124546.986367	58.973837
2394.575737	124337.810687	58.978842
2393.691925	124122.591856	58.983847
2393.368050	123902.663662	58.988852
2392.357184	123699.316202	58.993857
2391.986577	123478.065542	58.998861
2391.409009	123273.078008	59.003866
2390.195799	123060.205619	59.008871
2390.212488	122836.752847	59.013876
2389.187443	122630.469784	59.018881
2388.402549	122413.471270	59.023885
2387.861217	122198.772312	59.028890
2387.126330	121988.816636	59.033895
2387.024543	121775.524346	59.038900
2386.048597	121561.381957	59.043905
2385.655607	121343.352343	59.048909
2384.981313	121122.524924	59.053914
2384.108763	120901.654602	59.058919
2383.733951	120684.948051	59.063924
2382.536697	120473.744516	59.068929
2381.925655	120253.701566	59.073933
2381.377593	120036.710404	59.078938
2380.623092	119825.810094	59.083943
2380.112239	119608.899104	59.088948
2379.213974	119397.574311	59.093953
2378.737183	119180.496423	59.098957
2377.990941	118967.773451	59.103962
2377.197786	118754.640681	59.108967
2376.615432	118528.183450	59.113972
2375.982734	118323.446272	59.118977
2375.083714	118106.418904	59.123981
2374.695435	117899.513420	59.128986
2374.220061	117690.357225	59.133991
2373.507933	117467.389414	59.138996
2372.469015	117261.042897	59.144001
2372.317094	117042.852295	59.149005
2371.643709	116828.935648	59.154010
2370.389993	116610.663155	59.159015
2370.235292	116389.793522	59.164020
2369.473215	116174.188921	59.169025
2368.954517	115959.848767	59.174029
2368.108917	115747.891721	59.179034
2367.365914	115523.479473	59.184039
2366.879292	115304.455440	59.189044
2366.072389	115092.840462	59.194049
2365.768326	114873.156483	59.199053
2364.985601	114664.429189	59.204058
2364.342309	114441.990977	59.209063
2363.715105	114219.641028	59.214068
2363.117559	113998.138820	59.219073
2362.561409	113782.902688	59.224077
2361.843337	113569.693311	59.229082
2361.223975	113340.501675	59.234087
2360.513008	113117.793930	59.239092
2359.888145	112901.966955	59.244097
2359.055949	112678.590552	59.249101
2358.471609	112464.087362	59.254106
2357.817333	112238.915998	59.259111
2357.296159	112008.984796	59.264116
2356.389647	111784.739681	59.269121
2355.970608	111568.751979	59.274125
2355.360464	111357.004013	59.279130
2354.832751	111123.832760	59.284135
2353.977576	110895.202331	59.289140
2353.180267	110675.474717	59.294145
2352.601869	110459.547338	59.299149
2351.921452	110221.370077	59.304154
2351.355449	110013.009017	59.309159
2350.845134	109775.456380	59.314164
2350.214790	109566.772974	59.319169
2349.386941	109340.690955	59.324173
2348.433161	109113.552228	59.329178
2347.882809	108893.420646	59.334183
2347.334449	108664.007195	59.339188
2346.245394	108443.717611	59.344193
2345.959378	108221.881310	59.349197
2345.470026	107998.385057	59.354202
2344.583175	107776.483110	59.359207
2343.984744	107557.754505	59.364212
2343.561538	107333.746264	59.369217
2342.657968	107103.344222	59.374221
2341.868352	106887.767451	59.379226
2341.442919	106657.744346	59.384231
2340.790316	106423.939789	59.389236
2339.938916	106218.606880	59.394241
2339.409562	105980.529658	59.399245
2338.879849	105756.794063	59.404250
2337.865366	105534.622090	59.409255
2337.473732	105298.560115	59.414260
2336.775653	105084.793242	59.419265
2336.037991	104868.312748	59.424269
2335.523388	104641.774555	59.429274
2334.724352	104416.102051	59.434279
2334.067929	104186.272547	59.439284
2333.245388	103968.018248	59.444289
2332.610097	103749.444430	59.449293
2332.011940	103523.513824	59.454298
2331.330952	103302.718222	59.459303
2330.958547	103078.316729	59.464308
2330.296871	102860.871867	59.469313
2329.379055	102633.420809	59.474317
2329.056040	102402.534402	59.479322
2328.133283	102178.197037	59.484327
2327.520163	101946.143104	59.489332
2326.798572	101731.116141	59.494337
2326.073276	101496.635780	59.499341
2325.820801	101273.615425	59.504346
2324.905224	101055.371182	59.509351
2324.176270	100836.484074	59.514356
2323.407413	100612.238833	59.519361
2323.090868	100389.763598	59.524365
2322.577375	100158.517253	59.529370
2321.678484	99928.824982	59.534375
2321.206788	99695.071062	59.539380
2320.309545	99476.064895	59.544385
2319.488112	99243.760136	59.549389
2319.204678	99009.380712	59.554394
2318.081641	98793.372655	59.559399
2317.850489	98557.517986	59.564404
2316.918279	98340.132903	59.569409
2316.301846	98109.443527	59.574413
2315.760882	97881.636754	59.579418
2314.704901	97650.590402	59.584423
2314.207536	97425.064595	59.589428
2313.544499	97200.448889	59.594433
2312.517611	96972.994619	59.599437
2312.298001	96751.021231	59.604442
2311.617153	96524.575740	59.609447
2310.879344	96301.071641	59.614452
2310.309447	96082.673918	59.619457
2309.445631	95851.399734	59.624461
2309.060436	95632.101859	59.629466
2307.972056	95415.143653	59.634471
2307.952151	95173.931559	59.639476
2306.867355	94958.454841	59.644481
2306.125298	94736.425517	59.649485
2305.768031	94509.936219	59.654490
2304.884864	94294.249987	59.659495
2304.353801	94060.315985	59.664500
2304.000895	93846.033906	59.669505
2303.026988	93616.169933	59.674509
2302.649876	93386.549778	59.679514
2301.666177	93153.990685	59.684519
2301.373394	92921.964920	59.689524
2300.506144	92701.021964	59.694529
2299.771500	92470.966993	59.699533
2299.377230	92241.665744	59.704538
2298.613277	92022.812051	59.709543
2297.905227	91785.702440	59.714548
2297.173110	91560.621475	59.719553
2296.731806	91329.897755	59.724557
2295.990827	91101.963170	59.729562
2295.146852	90881.548295	59.734567
2294.579641	90642.925895	59.739572
2293.702172	90420.003739	59.744577
2292.717829	90192.935105	59.749581
2292.494816	89962.419372	59.754586
2291.581120	89738.007223	59.759591
2291.165153	89507.165486	59.764596
2290.466578	89295.264842	59.769601
2289.832252	89067.499348	59.774605
2289.220646	88837.279020	59.779610
2288.259565	88620.779289	59.784615
2287.728419	88383.355088	59.789620
2286.884633	88165.262651	59.794625
2286.054863	87942.237805	59.799629
2285.573796	87721.080903	59.804634
2284.816732	87500.718116	59.809639
2284.025048	87270.149932	59.814644
2283.628286	87066.039962	59.819649
2283.028698	86842.736385	59.824653
2282.515991	86613.766573	59.829658
2281.854612	86405.761705	59.834663
2281.333882	86158.876624	59.839668
2280.485172	85951.457390	59.844673
2279.823936	85720.694964	59.849677
2279.243354	85501.218514	59.854682
2278.644512	85271.813946	59.859687
2278.001091	85041.024342	59.864692
2277.204626	84824.048614	59.869697
2276.377594	84596.367316	59.874701
2276.071460	84366.539407	59.879706
2275.347446	84144.462759	59.884711
2274.698557	83909.458396	59.889716
2274.196710	83683.529151	59.894721
2273.022865	83471.273273	59.899725
2272.668150	83240.501832	59.904730
2271.738913	83016.713826	59.909735
2271.243189	82785.291524	59.914740
2270.690116	82561.809975	59.919745
2269.667488	82341.067297	59.924750
2269.122610	82112.702507	59.929754
2268.439009	81895.891062	59.934759
2267.936285	81662.568154	59.939764
2267.412387	81442.535409	59.944769
2266.662467	81219.074039	59.949774
2266.199534	80995.030836	59.954778
2265.537981	80766.775295	59.959783
2264.799092	80533.515133	59.964788
2263.963833	80312.187446	59.969793
2263.096213	80091.025686	59.974798
2262.695924	79861.071894	59.979802
2261.893759	79640.379863	59.984807
2261.455598	79403.903358	59.989812
2260.705931	79183.885956	59.994817
2259.866050	78966.477093	59.999822
2259.579087	78738.399933	60.004826
2258.630064	78517.825569	60.009831
2257.999564	78282.070482	60.014836
2257.513897	78060.584721	60.019841
2256.891185	77833.090467	60.024846
2256.293259	77601.881492	60.029850
2255.455812	77382.093721	60.034855
2254.530242	77154.236821	60.039860
2254.250585	76932.660874	60.044865
2253.656727	76709.724139	60.049870
2253.262073	76470.670224	60.054874
2252.109386	76248.631884	60.059879
2251.711075	76016.382723	60.064884
2251.163107	75790.977645	60.069889
2250.198782	75558.620735	60.074894
2249.470843	75322.097923	60.079898
2248.825341	75101.645387	60.084903
2248.301525	74873.503226	60.089908
2247.964915	74646.157600	60.094913
2247.238465	74421.188903	60.099918
2246.158971	74191.096154	60.104922
2245.420563	73965.469202	60.109927
2245.133499	73723.839407	60.114932
2244.319480	73496.886582	60.119937
2243.499782	73272.281307	60.124942
2243.237537	73040.044809	60.129946
2242.097468	72813.461870	60.134951
2241.091819	72589.964398	60.139956
2240.690215	72373.430889	60.144961
2239.869437	72141.109710	60.149966
2239.314410	71912.093928	60.154970
2238.476276	71691.677739	60.159975
2238.188557	71478.018260	60.164980
2237.398078	71257.453629	60.169985
2236.888888	71027.294190	60.174990
2236.344737	70800.620649	60.179994
2235.489647	70582.753302	60.184999
2234.730477	70352.368979	60.190004
2234.171983	70136.796909	60.195009
2233.538032	69906.511947	60.200014
2233.014598	69676.041124	60.205018
2232.209160	69462.542547	60.210023
2231.744237	69231.757276	60.215028
2230.653589	69007.528305	60.220033
2229.883628	68786.031625	60.225038
2229.604682	68552.235237	60.230042
2228.937131	68336.573539	60.235047
2228.058598	68114.227623	60.240052
2227.395258	67895.333605	60.245057
2226.854474	67676.169261	60.250062
2226.256593	67447.680873	60.255066
2225.396050	67228.806622	60.260071
2224.909369	67002.851855	60.265076
2223.966378	66786.142674	60.270081
2223.444960	66564.600143	60.275086
2223.014403	66326.912094	60.280090
2222.097424	66119.674263	60.285095
2221.229089	65894.492759	60.290100
2220.658826	65676.828095	60.295105
2220.177582	65452.068487	60.300110
2219.537714	65235.271613	60.305114
2218.470720	65021.742943	60.310119
2218.004062	64800.582431	60.315124
2217.281972	64588.124744	60.320129
2216.273730	64367.663050	60.325134
2216.152257	64147.762963	60.330138
2215.330240	63936.408025	60.335143
2214.827905	63716.088885	60.340148
2214.055469	63500.402801	60.345153
2213.293038	63278.961670	60.350158
2212.958659	63059.722084	60.355162
2211.791857	62840.309962	60.360167
2211.210225	62628.054412	60.365172
2211.193028	62404.877935	60.370177
2209.783455	62194.452325	60.375182
2209.452555	61965.578372	60.380186
2208.725031	61748.293623	60.385191
2208.036802	61534.737576	60.390196
2207.474789	61327.862612	60.395201
2206.596848	61112.410334	60.400206
2206.424296	60882.254925	60.405210
2205.396553	60670.829682	60.410215
2204.951742	60456.750219	60.415220
2204.367114	60232.185740	60.420225
2203.408820	60018.901798	60.425230
2202.981894	59791.516092	60.430234
2201.956785	59578.029344	60.435239
2201.577481	59353.651729	60.440244
2200.744634	59143.852452	60.445249
2200.004408	58929.625201	60.450254
2199.838351	58702.179693	60.455258
2198.549762	58497.793488	60.460263
2198.178365	58281.498904	60.465268
2197.577719	58064.983653	60.470273
2196.705570	57854.034008	60.475278
2196.322065	57632.925201	60.480282
2195.597856	57420.156069	60.485287
2194.917317	57196.963152	60.490292
2194.214879	56987.544142	60.495297
2193.442981	56768.773395	60.500302
2192.945344	56549.028078	60.505306
2192.251759	56338.114847	60.510311
2191.846362	56118.894884	60.515316
2191.297445	55892.319950	60.520321
2190.315796	55672.646033	60.525326
2189.837378	55455.116557	60.530330
2188.855642	55237.473288	60.535335
2188.514826	55013.104128	60.540340
2187.707595	54800.970185	60.545345
2186.994091	54589.608648	60.550350
2186.531148	54360.554783	60.555354
2185.842500	54150.368428	60.560359
2184.967534	53918.163998	60.565364
2184.392847	53701.262388	60.570369
2183.437633	53496.109844	60.575374
2182.849107	53268.883821	60.580378
2182.327226	53056.525536	60.585383
2181.600767	52839.177302	60.590388
2181.105565	52632.743280	60.595393
2180.238334	52419.561243	60.600398
2179.622056	52194.963541	60.605402
2179.141880	51985.189985	60.610407
2178.398258	51761.320308	60.615412
2177.833962	51540.006827	60.620417
2177.225701	51323.322503	60.625422
2176.286192	51103.864735	60.630426
2175.207056	50899.368768	60.635431
2174.815930	50686.818246	60.640436
2174.593977	50466.523558	60.645441
2173.437694	50256.222472	60.650446
2173.140684	50043.215373	60.655450
2172.217182	49828.987743	60.660455
2171.561972	49612.113212	60.665460
2171.067079	49394.646416	60.670465
2170.031699	49186.543808	60.675470
2169.431258	48966.223224	60.680474
2168.871016	48757.003098	60.685479
2168.375182	48556.636258	60.690484
2167.600249	48332.118396	60.695489
2166.548172	48134.963753	60.700494
2166.358433	47917.862005	60.705498
2165.406785	47701.918210	60.710503
2164.834696	47494.404073	60.715508
2164.326687	47278.708225	60.720513
2163.659604	47074.892998	60.725518
2162.833371	46861.792823	60.730522
2162.136025	46667.533721	60.735527
2161.484485	46453.338442	60.740532
2160.814495	46240.183032	60.745537
2159.821831	46033.243071	60.750542
2159.453984	45826.219071	60.755546
2158.653283	45615.176416	60.760551
2157.818772	45413.424970	60.765556
2157.205428	45205.881059	60.770561
2156.466425	45006.557763	60.775566
2155.785666	44806.012957	60.780570
2155.299009	44604.364297	60.785575
2154.763866	44404.190024	60.790580
2154.149721	44199.767193	60.795585
2153.118882	43993.793558	60.800590
2152.457386	43792.267410	60.805594
2151.925560	43588.341554	60.810599
2151.095284	43397.156959	60.815604
2150.364025	43196.183262	60.820609
2149.679174	42986.248246	60.825614
2149.438821	42785.182448	60.830618
2148.303425	42599.352223	60.835623
2147.557040	42402.545591	60.840628
2146.858773	42202.950665	60.845633
2145.948748	42011.215291	60.850638
2145.570643	41810.429331	60.855642
2144.957121	41618.916906	60.860647
2144.181916	41427.628318	60.865652
2143.818496	41243.413627	60.870657
2143.006639	41046.952221	60.875662
2142.583655	40849.081129	60.880666
2141.529464	40656.748111	60.885671
2140.727032	40466.062687	60.890676
2140.268490	40278.265511	60.895681
2139.046412	40099.347104	60.900686
2138.405675	39904.686611	60.905690
2137.783295	39716.646494	60.910695
2136.564234	39543.837524	60.915700
2136.078713	39360.642608	60.920705
2134.847275	39190.338633	60.925710
2134.491464	39020.937666	60.930714
2133.592240	38866.821644	60.935719
2132.562347	38705.398833	60.940724
2132.090840	38532.294968	60.945729
2131.218897	38373.801698	60.950734
2130.583358	38207.012590	60.955738
2129.751799	38047.436255	60.960743
2128.591663	37912.529703	60.965748
2128.035127	37752.493596	60.970753
2127.390111	37613.862410	60.975758
2126.544368	37468.925375	60.980762
2125.544042	37321.004376	60.985767
2125.292869	37178.999448	60.990772
2124.718850	37040.472345	60.995777
2123.462016	36909.452405	61.000782
2122.569919	36763.442832	61.005786
2121.925975	36628.240170	61.010791
2121.137898	36510.524649	61.015796
2120.707706	36381.296584	61.020801
2119.913764	36254.954992	61.025806
2119.402177	36119.507799	61.030810
2118.406519	35999.652260	61.035815
2117.973040	35871.041912	61.040820
2117.354738	35744.590933	61.045825
2116.149012	35623.241396	61.050830
2115.663478	35495.909806	61.055834
2115.128139	35378.957133	61.060839
2114.759086	35263.523087	61.065844
2114.105791	35144.433316	61.070849
2112.910641	35022.751375	61.075854
2112.440380	34902.341415	61.080858
2111.904325	34788.373828	61.085863
2111.570352	34664.863548	61.090868
2111.097792	34536.054692	61.095873
2110.188815	34422.646620	61.100878
2109.857828	34293.368318	61.105882
2108.831027	34175.134943	61.110887
2108.273884	34049.338206	61.115892
2107.659314	33927.325579	61.120897
2107.000579	33810.280183	61.125902
2106.455099	33688.729303	61.130906
2105.787208	33568.671655	61.135911
2104.988404	33442.965253	61.140916
2104.835468	33311.774600	61.145921
2103.732322	33199.142118	61.150926
2102.846696	33065.457342	61.155930
2102.306891	32950.355589	61.160935
2101.856145	32839.243451	61.165940
2101.390265	32708.510197	61.170945
2100.311794	32592.955930	61.175950
2100.151298	32467.601275	61.180954
2099.240311	32338.591382	61.185959
2098.589659	32224.389308	61.190964
2098.027486	32093.775740	61.195969
2096.991380	31979.780320	61.200974
2096.557390	31851.445992	61.205978
2095.957378	31728.119835	61.210983
2095.141521	31614.586595	61.215988
2094.463591	31499.199230	61.220993
2093.852199	31376.861963	61.225998
2093.183365	31247.079488	61.231002
2092.417461	31142.360490	61.236007
2091.825953	31014.940970	61.241012
2091.552938	30890.523135	61.246017
2090.575825	30776.079503	61.251022
2089.690904	30652.738658	61.256026
2089.037514	30535.881488	61.261031
2088.207197	30426.182580	61.266036
2088.165473	30312.371157	61.271041
2087.168503	30193.641667	61.276046
2086.546925	30073.031667	61.281050
2085.877484	29961.750824	61.286055
2085.073418	29843.595257	61.291060
2085.010730	29721.507150	61.296065
2083.645670	29604.919644	61.301070
2083.110531	29483.511844	61.306074
2082.473017	29371.438370	61.311079
2081.820568	29266.981940	61.316084
2081.137464	29151.415981	61.321089
2080.519933	29047.873372	61.326094
2080.076054	28921.481567	61.331098
2079.354391	28811.172708	61.336103
2078.962724	28688.893304	61.341108
2078.410244	28562.510453	61.346113
2077.377575	28446.063337	61.351118
2076.815298	28330.155406	61.356122
2076.244198	28220.738248	61.361127
2075.560625	28096.548986	61.366132
2075.182482	27981.952461	61.371137
2074.203274	27859.622433	61.376142
2073.976240	27726.920885	61.381146
2073.015868	27614.228247	61.386151
2072.059690	27493.943183	61.391156
2071.803802	27375.562123	61.396161
2070.838797	27256.152271	61.401166
2070.451165	27137.190381	61.406170
2069.999609	27021.868213	61.411175
2068.979059	26903.431850	61.416180
2068.731525	26776.159869	61.421185
2067.692851	26658.300832	61.426190
2067.236966	26530.159457	61.431194
2066.572336	26414.258557	61.436199
2065.860038	26288.008041	61.441204
2065.349558	26167.527843	61.446209
2064.530258	26040.132026	61.451214
2064.137745	25924.220688	61.456218
2063.319510	25800.229959	61.461223
2062.781558	25679.476592	61.466228
2061.870693	25554.466220	61.471233
2061.055993	25443.285996	61.476238
2060.193815	25315.217173	61.481242
2059.549040	25194.941688	61.486247
2058.946185	25091.853271	61.491252
2058.698177	24964.713340	61.496257
2057.328513	24858.043260	61.501262
2056.816488	24734.957517	61.506266
2056.322672	24624.945913	61.511271
2055.821465	24507.994278	61.516276
2055.207354	24385.084583	61.521281
2054.342514	24268.619656	61.526286
2053.608459	24151.675986	61.531290
2053.114269	24035.996585	61.536295
2052.100637	23916.052216	61.541300
2051.847811	23796.237564	61.546305
2051.005201	23695.544815	61.551310
2050.516362	23574.903749	61.556314
2049.689901	23461.640101	61.561319
2048.986270	23341.180195	61.566324
2048.641760	23223.928797	61.571329
2047.477803	23117.255077	61.576334
2047.116400	22992.456283	61.581338
2046.559825	22873.762833	61.586343
2045.538856	22766.268835	61.591348
2044.840238	22655.763955	61.596353
2044.053532	22556.134010	61.601358
2043.728087	22425.033267	61.606362
2043.019423	22314.127266	61.611367
2042.419073	22198.616241	61.616372
2041.606102	22085.640578	61.621377
2040.768180	21981.078459	61.626382
2040.526925	21860.664573	61.631386
2040.047046	21748.407547	61.636391
2039.062516	21635.196221	61.641396
2038.651115	21522.396940	61.646401
2037.677154	21404.448729	61.651406
2037.018393	21288.663826	61.656410
2036.474794	21179.781470	61.661415
2035.924950	21079.114128	61.666420
2035.298899	20945.682465	61.671425
2034.576349	20839.632282	61.676430
2033.564619	20731.423440	61.681434
2033.243032	20616.418214	61.686439
2032.625379	20506.560564	61.691444
2032.003193	20392.318439	61.696449
2031.166990	20280.249988	61.701454
2030.496884	20166.700852	61.706458
2029.722267	20055.775376	61.711463
2028.941471	19951.717413	61.716468
2028.693236	19825.661199	61.721473
2027.460747	19727.419796	61.726478
2026.969577	19614.841437	61.731482
2026.258187	19508.843456	61.736487
2025.450786	19403.853833	61.741492
2024.997710	19291.108324	61.746497
2024.614607	19197.426631	61.751502
2023.479464	19079.331163	61.756506
2022.961659	18968.987229	61.761511
2022.077755	18877.379578	61.766516
2021.551998	18748.447898	61.771521
2020.450298	18655.395860	61.776526
2019.573822	18558.189626	61.781530
2019.586373	18459.794506	61.786535
2018.663220	18362.653344	61.791540
2018.063480	18260.165073	61.796545
2016.967029	18166.709737	61.801550
2016.245276	18065.871117	61.806554
2015.857686	17971.527251	61.811559
2014.859715	17875.848021	61.816564
2014.361474	17780.945405	61.821569
2013.825537	17694.381632	61.826574
2013.297552	17595.774216	61.831578
2012.466586	17505.981470	61.836583
2011.725699	17404.783094	61.841588
2011.029744	17321.808569	61.846593
2010.297310	17232.829052	61.851598
2009.619774	17128.838626	61.856602
2008.678720	17039.544023	61.861607
2008.110728	16955.313001	61.866612
2007.403602	16863.032380	61.871617
2006.741683	16781.677898	61.876622
2005.919408	16700.668988	61.881626
2005.652978	16609.771375	61.886631
2004.524159	16516.122125	61.891636
2003.900903	16433.737368	61.896641
2003.255135	16359.831063	61.901646
2002.721061	16273.020946	61.906650
2002.226972	16186.284101	61.911655
2001.290899	16113.288783	61.916660
2000.830461	16026.848228	61.921665
2000.066002	15940.836667	61.926670
1999.253915	15858.213812	61.931674
1998.888640	15773.289870	61.936679
1997.919410	15694.294494	61.941684
1997.505198	15614.744752	61.946689
1996.749990	15531.627811	61.951694
1995.980978	15446.923855	61.956698
1995.571908	15362.094370	61.961703
1994.442577	15289.990010	61.966708
1994.211476	15208.131257	61.971713
1993.619433	15131.055677	61.976718
1992.767866	15041.412315	61.981722
1992.315410	14961.684952	61.986727
1991.527704	14880.337460	61.991732
1990.876936	14792.843548	61.996737
1989.887150	14718.199392	62.001742
1989.283539	14640.550462	62.006746
1988.660464	14559.258847	62.011751
1987.768604	14488.825250	62.016756
1987.159437	14403.978937	62.021761
1986.582930	14325.296244	62.026766
1985.753911	14250.327158	62.031770
1985.161293	14164.805133	62.036775
1984.635927	14103.059282	62.041780
1984.174088	14027.593304	62.046785
1983.482832	13952.111429	62.051790
1982.522473	13871.730143	62.056794
1982.079714	13801.126738	62.061799
1981.205680	13741.265513	62.066804
1980.690376	13652.419771	62.071809
1980.182512	13587.316417	62.076814
1979.438812	13511.304236	62.081818
1978.669525	13439.056038	62.086823
1977.830740	13363.957002	62.091828
1977.657308	13280.425384	62.096833
1976.739933	13220.632663	62.101838
1976.218774	13133.185260	62.106842
1975.714819	13055.308855	62.111847
1974.555710	12981.696258	62.116852
1974.083040	12904.567247	62.121857
1973.355139	12825.302516	62.126862
1972.467674	12760.872567	62.131866
1971.845168	12694.474494	62.136871
1971.303368	12627.080019	62.141876
1970.970314	12554.734706	62.146881
1969.930885	12489.897174	62.151886
1969.451926	12412.947529	62.156890
1968.700177	12332.346614	62.161895
1967.813183	12269.126847	62.166900
1967.254607	12194.045025	62.171905
1966.604078	12134.512012	62.176910
1966.089882	12057.834311	62.181914
1965.599791	11988.396534	62.186919
1964.532811	11914.108977	62.191924
1964.099496	11839.297052	62.196929
1963.220693	11771.840108	62.201934
1962.724443	11705.500684	62.206938
1962.339156	11632.317583	62.211943
1961.397782	11569.668638	62.216948
1960.903288	11500.053482	62.221953
1959.907310	11429.512545	62.226958
1959.503987	11356.791309	62.231962
1959.006819	11289.990058	62.236967
1958.063430	11227.929336	62.241972
1957.279319	11146.456273	62.246977
1956.649929	11080.600946	62.251982
1956.067058	11017.401248	62.256986
1955.581512	10946.762205	62.261991
1954.990809	10885.436172	62.266996
1954.281511	10800.652627	62.272001
1953.824204	10737.244200	62.277006
1952.812868	10664.428494	62.282010
1952.221646	10587.030713	62.287015
1951.515645	10520.402709	62.292020
1950.751256	10450.989473	62.297025
1950.210447	10378.480381	62.302030
1949.219933	10319.162725	62.307034
1948.812398	10237.249931	62.312039
1947.922438	10184.979475	62.317044
1947.054240	10114.747695	62.322049
1946.509992	10055.600497	62.327054
1945.978193	9986.967931	62.332058
1945.590404	9922.032634	62.337063
1944.655228	9856.425871	62.342068
1944.101010	9785.523057	62.347073
1943.299372	9727.611773	62.352078
1942.788960	9672.847580	62.357082
1941.989062	9595.436329	62.362087
1941.367929	9539.059336	62.367092
1940.603542	9475.984258	62.372097
1940.043711	9400.487082	62.377102
1939.241725	9354.390432	62.382106
1938.616246	9279.619499	62.387111
1937.649414	9228.300698	62.392116
1937.247600	9164.654168	62.397121
1936.899675	9108.109975	62.402126
1935.965556	9053.494982	62.407130
1935.299268	8984.955395	62.412135
1934.697778	8925.116390	62.417140
1934.515376	8866.533788	62.422145
1933.751910	8803.374997	62.427150
1933.143079	8735.918949	62.432154
1932.546031	8666.863314	62.437159
1931.495952	8609.250218	62.442164
1931.163740	8532.671968	62.447169
1930.355759	8460.743116	62.452174
1929.647783	8402.289543	62.457178
1929.229184	8330.366564	62.462183
1928.444381	8279.583444	62.467188
1927.710274	8208.867310	62.472193
1926.923883	8144.255423	62.477198
1926.184538	8082.112765	62.482202
1925.556625	8014.251178	62.487207
1924.744643	7959.061449	62.492212
1924.115497	7897.453515	62.497217
1923.583880	7833.689260	62.502222
1922.840694	7776.145049	62.507226
1922.224233	7707.829810	62.512231
1921.132547	7650.889296	62.517236
1920.804174	7592.911132	62.522241
1920.329623	7535.817866	62.527246
1919.385738	7473.057011	62.532250
1919.132133	7409.286721	62.537255
1918.210117	7355.898780	62.542260
1917.653025	7293.900868	62.547265
1917.006682	7230.280466	62.552270
1916.398516	7175.686067	62.557274
1915.984753	7104.627296	62.562279
1915.128330	7049.998615	62.567284
1914.605442	6987.438819	62.572289
1913.495779	6921.586655	62.577294
1913.074807	6860.841363	62.582298
1912.326536	6794.221238	62.587303
1911.514565	6743.513531	62.592308
1911.225147	6677.166208	62.597313
1910.455097	6614.816816	62.602318
1909.735329	6555.647402	62.607322
1908.917073	6488.241058	62.612327
1908.035060	6433.713365	62.617332
1907.663417	6362.615159	62.622337
1906.825631	6316.072505	62.627342
1906.356943	6255.173184	62.632346
1905.736430	6192.493394	62.637351
1904.532623	6145.677289	62.642356
1904.112476	6082.478667	62.647361
1903.829429	6023.376140	62.652366
1902.936788	5970.006658	62.657370
1902.507849	5902.639767	62.662375
1901.768704	5856.026104	62.667380
1901.158298	5785.564898	62.672385
1900.614344	5735.016076	62.677390
1899.669825	5675.929234	62.682394
1899.536040	5604.381201	62.687399
1898.546034	5554.242989	62.692404
1897.947739	5489.822579	62.697409
1897.209475	5436.914034	62.702414
1896.078966	5377.252917	62.707418
1896.010350	5316.937574	62.712423
1895.095488	5264.199662	62.717428
1894.196376	5198.855722	62.722433
1893.882785	5146.705845	62.727438
1893.092213	5085.614756	62.732442
1892.795445	5024.223883	62.737447
1891.654359	4975.022638	62.742452
1891.144189	4912.708558	62.747457
1890.376269	4850.434084	62.752462
1889.405091	4794.364864	62.757466
1889.057381	4734.574969	62.762471
1888.493638	4687.845649	62.767476
1887.843720	4629.863836	62.772481
1887.078516	4570.377508	62.777486
1886.285964	4511.724718	62.782490
1885.782544	4459.832979	62.787495
1885.196203	4408.628946	62.792500
1884.171242	4337.268745	62.797505
1883.834233	4286.901820	62.802510
1882.635257	4242.435852	62.807514
1882.240145	4185.148840	62.812519
1881.516612	4137.543556	62.817524
1881.224347	4078.120578	62.822529
1880.088703	4025.820447	62.827534
1879.716146	3973.104377	62.832538
1879.174278	3915.782559	62.837543
1878.376495	3868.876101	62.842548
1877.857183	3810.498991	62.847553
1877.464115	3755.135371	62.852558
1876.569170	3703.651536	62.857562
1875.800483	3640.170875	62.862567
1874.975715	3586.703810	62.867572
1874.223464	3532.069224	62.872577
1873.773153	3485.989776	62.877582
1873.034409	3432.766722	62.882586
1872.710420	3372.088175	62.887591
1871.542862	3328.272222	62.892596
1871.208026	3274.664626	62.897601
1870.514918	3211.038171	62.902606
1869.555466	3166.158095	62.907610
1869.148183	3110.507356	62.912615
1868.698088	3075.997955	62.917620
1868.193959	3014.664144	62.922625
1867.406795	2956.766710	62.927630
1866.638218	2910.068462	62.932634
1866.242899	2835.679463	62.937639
1865.416187	2789.620954	62.942644
1864.376739	2736.695802	62.947649
1863.885949	2684.537821	62.952654
1863.303825	2632.716287	62.957658
1862.675147	2578.974924	62.962663
1861.902594	2532.720143	62.967668
1861.426722	2468.590822	62.972673
1860.406110	2414.659932	62.977678
1859.495638	2367.511197	62.982682
1859.219308	2306.512465	62.987687
1858.627898	2260.671408	62.992692
1857.690414	2207.621579	62.997697
1857.256343	2162.010570	63.002702
1856.503390	2107.343557	63.007706
1855.631251	2052.126304	63.012711
1854.981919	2010.996065	63.017716
1854.339036	1961.348102	63.022721
1853.774849	1911.770614	63.027726
1852.852852	1882.153306	63.032730
1852.627868	1817.085650	63.037735
1851.790894	1766.089930	63.042740
1851.100808	1722.401714	63.047745
1850.626835	1668.574473	63.052750
1849.767947	1624.568743	63.057754
1849.263662	1563.584858	63.062759
1848.537362	1526.068831	63.067764
1848.035326	1476.674576	63.072769
1847.119448	1428.477789	63.077774
1846.412542	1382.828158	63.082778
1845.683608	1329.339151	63.087783
1845.168376	1282.467099	63.092788
1844.056110	1240.805349	63.097793
1843.628172	1192.215660	63.102798
1842.858977	1152.907142	63.107802
1842.487969	1104.881981	63.112807
1841.637752	1075.923610	63.117812
1841.430255	1021.241092	63.122817
1840.737818	968.704907	63.127822
1839.661507	933.202353	63.132826
1839.310368	888.811490	63.137831
1838.581020	837.257849	63.142836
1837.770514	797.507388	63.147841
1836.988196	748.156167	63.152846
1836.265165	712.656412	63.157850
1835.557778	660.954821	63.162855
1834.725604	624.083234	63.167860
1834.052509	581.640036	63.172865
1833.421236	538.912764	63.177870
1832.727082	503.405782	63.182874
1832.017250	462.306089	63.187879
1831.529198	423.672453	63.192884
1830.827790	387.305855	63.197889
1829.920950	348.697913	63.202894
1829.381375	321.942915	63.207898
1828.759623	279.811005	63.212903
1827.849084	250.577640	63.217908
1827.243404	220.949776	63.222913
1826.790474	173.467419	63.227918
1826.020039	148.673332	63.232922
1825.339343	120.310506	63.237927
1824.180990	84.400435	63.242932
1823.234397	64.876362	63.247937
1822.617643	46.440100	63.252942
1821.957796	24.606007	63.257946
1821.286838	0.253705	63.262951
1819.959900	0.637944	63.267956
1817.795873	19.184677	63.272961
1816.969157	29.159518	63.277966
1815.862770	40.131270	63.282970
1816.190806	43.963354	63.287975
1815.898808	46.816816	63.292980
1815.464861	43.690830	63.297985
1814.968678	40.571573	63.302990
1814.212777	61.294929	63.307994
1813.725008	51.052685	63.312999
1812.684933	54.630497	63.318004
1811.556487	57.238305	63.323009
1811.419578	61.781323	63.328014
1810.776072	73.340355	63.333018
1809.926828	63.183889	63.338023
1809.542713	67.628964	63.343028
1809.346956	72.047286	63.348033
1809.089903	68.181987	63.353038
1807.733062	71.581442	63.358042
1807.056738	70.447822	63.363047
1806.263495	77.252378	63.368052
1805.281021	75.434075	63.373057
1804.854167	78.468233	63.378062
1804.433186	76.351030	63.383066
1804.183438	73.295140	63.388071
1803.529863	76.429956	63.393076
1802.272083	76.549329	63.398081
1801.785507	77.673782	63.403086
1800.735943	83.894559	63.408090
1800.418918	80.384141	63.413095
1800.468870	80.920339	63.418100
1799.675942	81.058938	63.423105
1799.035732	70.219560	63.428110
1798.018663	86.551528	63.433114
1797.502717	76.004656	63.438119
1796.659079	81.823719	63.443124
1795.732008	77.952851	63.448129
1795.539221	71.030617	63.453134
1794.538454	80.806050	63.458138
1793.336035	77.704320	63.463143
1792.694726	74.816268	63.468148
1792.608682	82.235517	63.473153
1792.506444	76.106318	63.478158
1791.497750	87.934671	63.483162
1791.315470	81.334046	63.488167
1790.362789	83.227968	63.493172
1789.348389	85.618980	63.498177
1789.172419	72.583262	63.503182
1788.094166	77.458699	63.508186
1787.514264	81.458623	63.513191
1786.535532	76.660811	63.518196
1785.935595	88.550414	63.523201
1785.445384	90.896035	63.528206
1784.454858	88.381990	63.533210
1784.161266	83.757655	63.538215
1784.046350	84.983944	63.543220
1783.095568	88.443513	63.548225
1781.994543	89.184566	63.553230
1781.359322	92.756454	63.558234
1781.395981	85.953900	63.563239
1780.803567	77.737343	63.568244
1779.375425	94.052598	63.573249
1779.079728	92.010121	63.578254
1778.738561	88.317455	63.583258
1777.616074	84.168536	63.588263
1776.620523	85.604060	63.593268
1776.480221	97.835427	63.598273
1775.807547	82.028970	63.603278
1775.361773	85.143410	63.608282
1774.589234	90.807686	63.613287
1773.569961	87.639032	63.618292
1773.106348	89.076818	63.623297
1772.724213	81.930756	63.628302
1771.702121	86.798861	63.633306
1771.324747	89.300032	63.638311
1769.911173	93.672056	63.643316
1769.774588	92.165719	63.648321
1769.411719	82.059753	63.653326
1768.679772	88.693736	63.658330
1768.177678	81.664500	63.663335
1766.847441	86.537386	63.668340
1766.298067	89.356038	63.673345
1766.317400	87.575777	63.678350
1765.110714	94.417622	63.683354
1764.190710	92.007505	63.688359
1764.269300	92.829319	63.693364
1763.098932	100.849717	63.698369
1762.739917	88.675708	63.703374
1761.753878	90.836718	63.708378
1761.208665	92.997108	63.713383
1760.813427	87.026404	63.718388
1759.617775	89.078775	63.723393
1759.415400	88.644197	63.728398
1758.731121	94.912640	63.733402
1758.044999	90.871051	63.738407
1757.262627	87.227955	63.743412
1756.336233	90.205834	63.748417
1756.025366	81.883068	63.753422
1755.155516	90.331985	63.758426
1755.049888	85.635226	63.763431
1754.131590	86.978064	63.768436
1753.399264	86.187671	63.773441
1752.684774	85.219401	63.778446
1752.098393	88.013970	63.783450
1751.622172	84.317526	63.788455
1750.895747	79.599509	63.793460
1750.481583	85.493885	63.798465
1749.850090	82.378776	63.803470
1749.046284	86.313340	63.808474
1748.437866	93.184760	63.813479
1747.405188	93.755697	63.818484
1746.006071	101.544342	63.823489
1746.548428	84.368499	63.828494
1745.478584	93.213466	63.833498
1744.569613	88.630097	63.838503
1744.074999	91.618256	63.843508
1743.219909	98.409003	63.848513
1743.208880	90.823953	63.853518
1742.157877	96.748510	63.858522
1741.782596	85.584787	63.863527
1741.022127	90.706248	63.868532
1740.393620	93.740904	63.873537
1739.902706	86.150068	63.878542
1739.261101	88.440890	63.883546
1738.538827	94.379473	63.888551
1737.458362	88.823536	63.893556
1736.315336	93.192033	63.898561
1736.730600	90.032109	63.903566
1735.825001	87.913034	63.908570
1734.778443	85.311713	63.913575
1734.303280	91.332477	63.918580
1733.135986	90.693175	63.923585
1733.112317	92.901628	63.928590
1732.159328	98.339105	63.933594
1731.562700	94.319580	63.938599
1731.148058	87.292231	63.943604
1730.184657	96.669090	63.948609
1729.654215	90.984798	63.953614
1728.862473	94.285083	63.958618
1728.430143	96.594712	63.963623
1727.898022	89.095579	63.968628
1727.507437	99.303999	63.973633
1727.407857	89.220879	63.978638
1725.957209	90.506348	63.983642
1724.905483	88.979777	63.988647
1724.429117	92.502792	63.993652
1723.365046	97.841217	63.998657
1722.841725	95.134718	64.003662
1722.562393	90.314158	64.008666
1722.211116	89.037469	64.013671
1721.473592	90.753738	64.018676
1720.730526	89.014139	64.023681
1720.026687	82.762871	64.028686
1718.679565	87.679462	64.033690
1717.774237	84.699319	64.038695
1718.288490	94.970609	64.043700
1717.657409	96.438157	64.048705
1716.711048	91.363987	64.053710
1715.751299	89.736078	64.058714
1715.272810	93.402937	64.063719
1714.911029	89.349272	64.068724
1714.041194	93.780046	64.073729
1713.226949	87.625162	64.078734
1712.202734	91.356620	64.083738
1711.497462	81.722953	64.088743
1711.155570	89.356306	64.093748
1710.903841	93.915993	64.098753
1710.015519	85.834764	64.103758
1709.170107	96.361432	64.108762
1708.833580	90.882894	64.113767
1708.675706	91.146164	64.118772
1707.675975	97.762770	64.123777
1706.599350	85.494596	64.128782
1705.405988	91.621551	64.133786
1705.012390	95.878914	64.138791
1704.646726	85.268771	64.143796
1703.831437	96.375716	64.148801
1703.573456	89.836010	64.153806
1702.995260	82.404131	64.158810
1702.506167	91.593693	64.163815
1702.039224	86.567965	64.168820
1700.806767	83.352777	64.173825
1700.125417	81.235946	64.178830
1698.871577	84.239043	64.183834
1698.466909	82.209156	64.188839
1698.402329	73.410463	64.193844
1697.279215	78.651034	64.198849
1697.523674	82.668273	64.203854
1696.477047	89.953085	64.208858
1695.363900	87.602058	64.213863
1694.879070	71.652269	64.218868
1694.025099	80.931319	64.223873
1693.577467	80.379582	64.228878
1692.404717	92.252946	64.233882
1691.945879	81.859462	64.238887
1691.708503	75.952015	64.243892
1691.234837	84.910460	64.248897
1690.832941	80.585625	64.253902
1689.543352	83.595981	64.258906
1688.277414	88.223720	64.263911
1687.662131	76.560388	64.268916
1686.941290	90.076151	64.273921
1687.148489	86.884613	64.278926
1686.592342	82.954870	64.283930
1686.154213	90.501007	64.288935
1685.417399	88.299947	64.293940
1684.105204	78.844698	64.298945
1683.554429	85.511423	64.303950
1682.669997	89.261689	64.308954
1682.043816	86.661428	64.313959
1681.840513	79.687260	64.318964
1681.201677	86.908877	64.323969
1680.905463	80.340558	64.328974
1679.807509	93.832646	64.333978
1678.678866	88.328545	64.338983
1678.224411	88.829741	64.343988
1677.717385	90.381674	64.348993
1677.042654	79.648744	64.353998
1676.367644	92.427087	64.359002
1675.816167	83.981703	64.364007
1675.616131	87.042930	64.369012
1674.231899	87.057869	64.374017
1673.277049	87.170186	64.379022
1672.446101	87.959849	64.384026
1672.082602	81.058437	64.389031
1671.713313	72.327074	64.394036
1671.262387	83.111205	64.399041
1670.932562	81.337522	64.404046
1670.230768	79.220793	64.409050
1669.552494	85.762690	64.414055
1668.686485	82.315842	64.419060
1667.214214	79.209729	64.424065
1667.081285	75.431967	64.429070
1666.458021	85.357212	64.434074
1665.941464	83.321449	64.439079
1665.715512	89.490295	64.444084
1664.144708	96.617105	64.449089
1663.761978	85.825176	64.454094
1663.188199	86.293288	64.459098
1662.125993	82.626868	64.464103
1661.904765	83.518381	64.469108
1661.019212	84.804009	64.474113
1660.593742	81.394419	64.479118
1660.342383	84.279293	64.484122
1659.107933	88.369023	64.489127
1658.279526	79.194916	64.494132
1657.420607	86.941939	64.499137
1657.472196	81.803892	64.504142
1656.788251	84.554051	64.509146
1656.291242	83.518146	64.514151
1655.622075	74.489061	64.519156
1654.351353	91.807545	64.524161
1653.762546	77.052288	64.529166
1653.000338	89.254692	64.534170
1652.546715	79.262524	64.539175
1652.293502	81.857527	64.544180
1651.590627	79.646357	64.549185
1651.097040	75.946388	64.554190
1649.806177	80.803609	64.559194
1648.826098	83.212875	64.564199
1648.458043	78.941021	64.569204
1647.843703	85.445957	64.574209
1647.410475	81.999755	64.579214
1646.964512	82.258329	64.584218
1646.177151	82.104349	64.589223
1645.243305	79.366889	64.594228
1644.023050	87.094043	64.599233
1643.639754	74.747314	64.604238
1643.032793	80.707018	64.609242
1642.499607	79.670554	64.614247
1642.225368	76.728964	64.619252
1641.678838	80.323059	64.624257
1641.465849	76.887606	64.629262
1640.439385	82.303660	64.634266
1639.363053	80.962388	64.639271
1638.982942	79.401705	64.644276
1638.120246	83.689435	64.649281
1638.153315	76.666687	64.654286
1636.927872	77.377100	64.659290
1635.946140	84.918129	64.664295
1635.325987	70.376027	64.669300
1634.811203	79.544436	64.674305
1634.091002	80.638222	64.679310
1633.962499	89.535535	64.684314
1632.560717	86.812489	64.689319
1631.831222	80.177389	64.694324
1630.988210	80.899594	64.699329
1630.910769	79.164672	64.704334
1629.983856	80.417455	64.709338
1629.556364	75.845960	64.714343
1629.597274	71.908120	64.719348
1628.842377	78.214607	64.724353
1627.638648	81.067847	64.729358
1626.802441	77.753478	64.734362
1626.308337	78.085937	64.739367
1626.103655	70.829721	64.744372
1625.028323	76.244079	64.749377
1624.066699	82.127663	64.754382
1623.556109	81.261082	64.759386
1623.126034	78.139243	64.764391
1622.806851	71.011606	64.769396
1621.423047	86.115055	64.774401
1620.504869	76.097349	64.779406
1619.824744	83.926364	64.784410
1619.062094	80.855783	64.789415
1618.926637	75.987156	64.794420
1618.131702	79.436211	64.799425
1617.941568	74.475344	64.804430
1617.729721	83.083113	64.809434
1616.650860	87.078756	64.814439
1615.907415	70.523519	64.819444
1614.734888	84.883764	64.824449
1614.479638	72.582936	64.829454
1614.365410	83.572205	64.834458
1612.795558	82.623167	64.839463
1612.355417	79.835672	64.844468
1611.655997	81.415027	64.849473
1610.981211	79.349219	64.854478
1610.548328	81.785109	64.859482
1609.754786	86.311024	64.864487
1609.102093	81.961392	64.869492
1608.038770	84.961072	64.874497
1607.557224	86.318154	64.879502
1606.856333	79.561823	64.884506
1605.937481	80.684021	64.889511
1605.954093	78.631378	64.894516
1605.360153	78.195942	64.899521
1605.028112	85.622725	64.904526
1604.254223	79.124001	64.909530
1602.847205	86.022964	64.914535
1602.317494	79.947504	64.919540
1601.880104	83.640964	64.924545
1601.698300	81.681345	64.929550
1600.764298	85.855833	64.934554
1599.473813	91.447893	64.939559
1599.086277	78.852684	64.944564
1598.022351	85.372283	64.949569
1597.982795	79.884437	64.954574
1597.776827	87.109839	64.959578
1596.497884	87.101784	64.964583
1595.647571	79.872446	64.969588
1594.821350	91.638746	64.974593
1594.405579	73.832951	64.979598
1593.941559	87.984446	64.984602
1593.512150	88.976849	64.989607
1593.057985	83.212669	64.994612
1591.719853	88.779184	64.999617
1591.063351	80.973421	65.004622
1590.804098	81.661242	65.009626
1590.048954	84.285531	65.014631
1589.909815	79.428530	65.019636
1588.795011	82.712367	65.024641
1587.934098	81.013611	65.029646
1587.374106	74.145016	65.034650
1586.624146	83.904316	65.039655
1585.837800	85.208901	65.044660
1584.603148	88.704173	65.049665
1584.107694	82.574387	65.054670
1583.879419	83.104320	65.059674
1583.677620	84.043216	65.064679
1583.113508	75.336517	65.069684
1582.604588	85.875975	65.074689
1581.307759	80.132138	65.079694
1580.480842	79.984462	65.084698
1579.729402	82.690168	65.089703
1579.352141	78.298363	65.094708
1578.745856	83.642950	65.099713
1578.585924	81.629395	65.104718
1577.435677	80.146926	65.109722
1576.555104	85.897798	65.114727
1576.556298	79.772687	65.119732
1575.863900	82.199350	65.124737
1574.536726	81.378938	65.129742
1573.799204	78.006331	65.134746
1572.851006	84.638441	65.139751
1572.578555	74.827252	65.144756
1571.940831	79.848822	65.149761
1571.519962	85.455692	65.154766
1571.132034	89.779976	65.159770
1570.518989	87.340087	65.164775
1569.404348	75.021266	65.169780
1568.542423	79.397203	65.174785
1567.955552	83.447161	65.179790
1567.992890	79.908863	65.184794
1567.161525	76.019727	65.189799
1566.283521	65.506807	65.194804
1565.267801	79.769606	65.199809
1564.884491	69.640139	65.204814
1564.400013	78.152447	65.209818
1564.156156	78.651740	65.214823
1563.106637	76.202356	65.219828
1561.978729	82.825174	65.224833
1561.484821	75.719000	65.229838
1561.074680	73.846129	65.234842
1560.300447	88.176226	65.239847
1559.754634	71.832468	65.244852
1558.594961	80.497790	65.249857
1558.254208	70.743192	65.254862
1557.911398	74.079423	65.259866
1557.090750	80.222907	65.264871
1556.590083	77.150145	65.269876
1555.251514	76.413558	65.274881
1554.698295	78.800764	65.279886
1554.567620	78.626052	65.284890
1553.887859	85.128782	65.289895
1553.238807	70.663845	65.294900
1552.084987	83.007332	65.299905
1551.400551	79.782418	65.304910
1551.027580	72.122438	65.309914
1550.291407	83.093827	65.314919
1550.045969	72.936147	65.319924
1548.982552	79.234903	65.324929
1548.160460	80.786455	65.329934
1547.992963	69.719093	65.334938
1547.269382	79.710753	65.339943
1546.786002	74.807528	65.344948
1545.273949	75.912037	65.349953
1544.762796	78.194789	65.354958
1544.144372	80.961371	65.359962
1543.334667	76.874833	65.364967
1543.381953	79.445751	65.369972
1542.589391	84.294808	65.374977
1541.920348	80.878213	65.379982
1540.918422	78.862829	65.384986
1539.901268	76.247460	65.389991
1539.994564	75.792729	65.394996
1539.559306	74.674494	65.400001
1538.729214	83.443577	65.405006
1538.176362	72.905808	65.410010
1536.870609	86.281134	65.415015
1536.836306	73.484737	65.420020
1536.148784	79.409950	65.425025
1535.141973	74.263466	65.430030
1534.359274	76.702909	65.435034
1533.460992	76.030416	65.440039
1533.408137	72.649958	65.445044
1532.843406	80.142101	65.450049
1531.873297	71.772750	65.455054
1531.100151	74.098710	65.460058
1530.267354	78.313908	65.465063
1529.618232	77.832064	65.470068
1529.504438	75.795413	65.475073
1528.780561	80.144695	65.480078
1527.711393	76.077313	65.485082
1527.024695	82.689961	65.490087
1526.541444	75.202052	65.495092
1526.057514	76.846536	65.500097
1525.630300	74.821840	65.505102
1524.410443	78.497715	65.510106
1523.414169	84.309565	65.515111
1522.961145	80.894920	65.520116
1522.550270	81.548492	65.525121
1521.963470	83.283442	65.530126
1521.689405	74.199508	65.535130
1521.135087	89.041877	65.540135
1520.026335	81.473585	65.545140
1519.484891	79.935403	65.550145
1518.866010	79.198017	65.555150
1518.243637	81.884807	65.560154
1516.836630	86.929281	65.565159
1516.705954	83.069170	65.570164
1515.828018	83.519413	65.575169
1515.138444	87.721321	65.580174
1515.210037	85.852333	65.585178
1514.330663	87.871900	65.590183
1513.400308	84.889504	65.595188
1512.485614	86.228697	65.600193
1512.124527	80.659485	65.605198
1511.998978	75.891799	65.610202
1510.444916	82.631240	65.615207
1509.981658	72.976544	65.620212
1509.336488	82.846941	65.625217
1508.740115	94.184068	65.630222
1508.408572	80.004582	65.635226
1507.370183	82.498858	65.640231
1506.860009	81.010905	65.645236
1505.999177	78.069506	65.650241
1505.846277	82.974622	65.655246
1505.236104	71.624368	65.660250
1504.090004	84.070725	65.665255
1503.477259	82.236366	65.670260
1502.807233	72.486795	65.675265
1502.325802	73.582097	65.680270
1501.629946	64.346000	65.685274
1500.323855	78.114052	65.690279
1500.069030	81.688626	65.695284
1499.558333	79.163106	65.700289
1499.146795	71.577076	65.705294
1498.582064	65.565563	65.710298
1497.410414	75.680472	65.715303
1496.712248	69.357420	65.720308
1496.010946	71.530045	65.725313
1495.263613	72.423171	65.730318
1495.353395	66.033255	65.735322
1494.285389	73.670032	65.740327
1493.255990	75.782832	65.745332
1492.868468	77.941866	65.750337
1492.133543	80.619738	65.755342
1491.811861	70.251835	65.760346
1491.132718	78.137485	65.765351
1490.280467	76.046296	65.770356
1489.560280	78.220348	65.775361
1488.662384	81.753611	65.780366
1488.587493	79.389076	65.785370
1487.586931	83.974729	65.790375
1486.763340	72.134839	65.795380
1485.754554	79.855254	65.800385
1485.328164	79.880506	65.805390
1485.305801	72.693111	65.810394
1484.699683	76.515901	65.815399
1484.132133	77.355229	65.820404
1483.015033	78.513706	65.825409
1482.339992	82.115635	65.830414
1481.899629	81.523356	65.835418
1481.145516	78.471965	65.840423
1480.341487	78.166140	65.845428
1479.380105	80.168787	65.850433
1478.572281	85.627423	65.855438
1478.579895	76.008293	65.860442
1477.793533	81.974457	65.865447
1477.433224	76.606983	65.870452
1476.278615	75.492690	65.875457
1475.405224	78.154724	65.880462
1475.549773	75.361073	65.885466
1474.714607	81.164680	65.890471
1473.723383	74.241645	65.895476
1473.066001	75.450072	65.900481
1472.046323	82.377426	65.905486
1471.953384	67.502444	65.910490
1471.422299	80.448743	65.915495
1470.374447	67.786628	65.920500
1469.395112	73.419177	65.925505
1469.085979	77.133272	65.930510
1468.781044	67.013454	65.935514
1468.172307	72.419948	65.940519
1467.361598	68.018203	65.945524
1466.287462	75.916167	65.950529
1465.465949	79.803156	65.955534
1465.177416	69.136673	65.960538
1464.450824	76.846939	65.965543
1464.253183	66.757380	65.970548
1463.331496	76.055127	65.975553
1462.448382	79.242266	65.980558
1462.071936	74.713158	65.985562
1461.369263	72.369548	65.990567
1460.187829	74.722568	65.995572
1459.514414	72.910480	66.000577
1458.735725	82.981879	66.005582
1458.383709	71.973819	66.010586
1458.009173	78.894842	66.015591
1457.982161	77.513042	66.020596
1457.050994	75.073279	66.025601
1456.210915	81.010138	66.030606
1455.790359	75.444082	66.035610
1454.679827	73.215757	66.040615
1453.928950	75.446735	66.045620
1453.322730	75.267180	66.050625
1452.737749	77.167436	66.055630
1452.419345	69.445190	66.060634
1450.909145	79.845739	66.065639
1450.160058	65.691643	66.070644
1449.820692	75.414093	66.075649
1449.356296	74.015073	66.080654
1449.077876	74.860497	66.085658
1448.207591	74.314473	66.090663
1447.220475	65.807517	66.095668
1446.599508	73.067329	66.100673
1445.930703	73.711442	66.105678
1445.812296	66.933562	66.110682
1444.500195	73.137831	66.115687
1443.626855	71.657148	66.120692
1442.956787	71.744790	66.125697
1442.502283	74.076903	66.130702
1442.161856	72.976732	66.135706
1441.670548	75.645860	66.140711
1441.411154	75.091059	66.145716
1440.494598	72.477091	66.150721
1439.605675	75.961632	66.155726
1439.029538	70.153800	66.160730
1437.811437	79.140691	66.165735
1437.145312	77.032556	66.170740
1436.631626	73.774231	66.175745
1436.108206	74.679096	66.180750
1435.814560	74.967115	66.185754
1434.904443	79.467446	66.190759
1433.724079	78.663199	66.195764
1433.065945	73.194834	66.200769
1432.673316	77.111439	66.205774
1432.433669	62.231402	66.210778
1432.079066	70.191635	66.215783
1430.983847	72.444231	66.220788
1430.225925	71.214871	66.225793
1429.271790	64.617132	66.230798
1429.202726	70.286369	66.235802
1427.798773	68.297083	66.240807
1427.484737	67.120179	66.245812
1426.779626	60.632675	66.250817
1425.907228	71.592611	66.255822
1425.950616	65.063413	66.260826
1425.327614	65.580401	66.265831
1424.371632	60.585167	66.270836
1423.760106	77.977130	66.275841
1422.650012	74.841987	66.280846
1422.467063	62.510797	66.285850
1421.086810	78.268192	66.290855
1420.611907	64.909483	66.295860
1420.023884	67.264397	66.300865
1419.155998	77.053506	66.305870
1418.940038	62.437794	66.310874
1418.577309	67.814655	66.315879
1418.129926	65.080394	66.320884
1417.245377	63.393342	66.325889
1416.510740	69.961584	66.330894
1416.357566	57.365467	66.335898
1414.955140	73.180000	66.340903
1414.172612	58.301102	66.345908
1413.595305	69.990009	66.350913
1413.006299	67.652001	66.355918
1412.895384	64.511019	66.360922
1411.353433	64.495972	66.365927
1410.752252	57.578789	66.370932
1410.161770	63.721990	66.375937
1409.927482	60.707852	66.380942
1409.471176	62.816325	66.385946
1408.053339	74.686143	66.390951
1407.563049	67.273507	66.395956
1407.307140	58.418537	66.400961
1406.805640	71.107813	66.405966
1405.964156	68.414117	66.410970
1404.924247	66.868459	66.415975
1404.435824	70.342968	66.420980
1404.154361	69.082040	66.425985
1403.183718	74.686421	66.430990
1402.359311	69.810630	66.435994
1401.809571	70.314402	66.440999
1401.201586	73.145587	66.446004
1400.937557	71.631149	66.451009
1399.768528	70.268445	66.456014
1398.974337	65.717442	66.461018
1398.423582	78.362514	66.466023
1397.945112	66.166610	66.471028
1397.570602	72.663423	66.476033
1396.337921	77.505200	66.481038
1396.035590	68.039430	66.486042
1395.059349	72.247502	66.491047
1394.579539	70.816250	66.496052
1393.632164	63.679704	66.501057
1392.270802	69.913902	66.506062
1392.091146	71.333422	66.511066
1391.793921	74.690809	66.516071
1391.629948	72.895536	66.521076
1391.076620	77.030080	66.526081
1390.163205	72.641534	66.531086
1389.579095	75.483119	66.536090
1388.266410	78.375859	66.541095
1388.012430	68.520776	66.546100
1387.749639	61.431537	66.551105
1386.218763	71.199876	66.556110
1385.831900	70.310524	66.561114
1385.185593	74.653815	66.566119
1384.832027	68.143560	66.571124
1384.225982	68.145346	66.576129
1383.010043	77.679123	66.581134
1382.644144	66.829415	66.586138
1381.867617	70.523191	66.591143
1381.728944	77.103946	66.596148
1380.971983	73.572064	66.601153
1379.863943	74.680257	66.606158
1379.386789	66.812949	66.611162
1378.895096	69.770734	66.616167
1378.099986	76.749152	66.621172
1377.356692	68.723873	66.626177
1376.164060	76.027258	66.631182
1376.021433	68.064196	66.636186
1375.563682	71.283096	66.641191
1375.025729	73.382476	66.646196
1374.005968	75.894340	66.651201
1372.718564	72.448356	66.656206
1372.287534	73.169811	66.661210
1372.258172	75.997335	66.666215
1371.684002	69.493764	66.671220
1371.594372	68.390006	66.676225
1370.076614	73.485270	66.681230
1369.521841	67.486403	66.686234
1369.006064	73.993059	66.691239
1367.943393	69.997261	66.696244
1367.253344	63.549961	66.701249
1366.393961	69.034162	66.706254
1366.509286	61.176759	66.711258
1365.670285	65.042897	66.716263
1364.783430	66.723071	66.721268
1364.138009	68.002163	66.726273
1363.116738	66.694837	66.731278
1362.865920	67.679386	66.736282
1362.278143	69.401906	66.741287
1361.539115	68.111217	66.746292
1360.855911	58.810086	66.751297
1360.153219	70.949444	66.756302
1359.770993	62.519843	66.761306
1359.190367	67.119205	66.766311
1358.244252	67.771152	66.771316
1357.608872	67.575755	66.776321
1356.729028	68.046855	66.781326
1356.597190	64.929703	66.786330
1355.235912	66.593833	66.791335
1354.343014	66.325831	66.796340
1353.973055	73.567833	66.801345
1353.539156	70.631165	66.806350
1353.516922	68.266153	66.811354
1352.674102	74.922573	66.816359
1351.637390	76.596613	66.821364
1351.270387	76.257627	66.826369
1350.364315	81.050658	66.831374
1349.117038	66.925340	66.836378
1348.451271	69.262665	66.841383
1347.993661	74.892742	66.846388
1347.646121	68.108720	66.851393
1347.304496	69.169208	66.856398
1347.024763	68.571918	66.861402
1345.693613	75.763293	66.866407
1345.220042	66.376797	66.871412
1344.975918	70.339189	66.876417
1343.303043	71.892009	66.881422
1342.461317	69.513768	66.886426
1341.977091	78.155368	66.891431
1341.223891	79.205592	66.896436
1341.461878	77.783244	66.901441
1340.727896	80.216574	66.906446
1340.348948	73.746632	66.911450
1339.360074	78.382515	66.916455
1338.411863	74.318070	66.921460
1337.782654	69.885942	66.926465
1336.734523	70.976744	66.931470
1336.001322	73.509300	66.936474
1335.610605	72.443947	66.941479
1335.046528	75.768066	66.946484
1334.877965	72.937455	66.951489
1333.992140	78.951005	66.956494
1332.912896	73.081256	66.961498
1332.273552	72.839185	66.966503
1331.709611	74.732967	66.971508
1331.418897	75.261809	66.976513
1330.362605	80.077150	66.981518
1329.422856	70.752152	66.986522
1328.625538	67.180972	66.991527
1328.217168	77.958353	66.996532
1328.145197	68.810795	67.001537
1327.822919	72.367715	67.006542
1326.873947	68.330206	67.011546
1326.125611	70.223341	67.016551
1325.339234	58.193114	67.021556
1324.478602	71.552931	67.026561
1323.345097	73.330680	67.031566
1322.922987	71.344636	67.036570
1322.369412	76.258256	67.041575
1322.038167	71.639988	67.046580
1321.830969	66.385404	67.051585
1320.559400	73.270845	67.056590
1319.973069	67.466246	67.061594
1319.369430	75.444001	67.066599
1318.722825	70.740250	67.071604
1317.864542	65.045121	67.076609
1316.964708	73.153544	67.081614
1316.327566	65.951940	67.086618
1315.855958	71.789251	67.091623
1315.528593	70.649174	67.096628
1314.908362	74.548358	67.101633
1313.980441	75.460784	67.106638
1313.284922	66.502251	67.111642
1313.022492	78.992680	67.116647
1311.562406	74.191175	67.121652
1310.981111	66.412983	67.126657
1310.483486	71.249898	67.131662
1310.143324	71.474362	67.136666
1309.661146	74.690847	67.141671
1309.222128	73.494404	67.146676
1308.092460	78.975863	67.151681
1307.264825	83.567201	67.156686
1306.612065	72.094477	67.161690
1306.443843	72.532883	67.166695
1305.144591	73.035986	67.171700
1305.086187	59.530678	67.176705
1303.925810	81.726637	67.181710
1303.513138	66.148730	67.186714
1302.794166	70.404240	67.191719
1301.859526	75.394217	67.196724
1301.661258	72.833264	67.201729
1300.890704	73.747483	67.206734
1300.328297	67.284642	67.211738
1299.621676	74.625906	67.216743
1298.564668	70.307536	67.221748
1298.122050	63.418793	67.226753
1297.077928	78.168723	67.231758
1296.354209	64.154169	67.236762
1295.416138	66.320332	67.241767
1295.140570	66.411524	67.246772
1294.705813	66.294633	67.251777
1294.252795	66.470809	67.256782
1294.141369	67.359084	67.261786
1293.389670	63.410076	67.266791
1292.109065	78.150296	67.271796
1291.810086	68.305542	67.276801
1290.817183	77.069023	67.281806
1289.921953	69.129435	67.286810
1289.398341	74.255918	67.291815
1288.467864	83.649730	67.296820
1288.571516	71.612043	67.301825
1288.006142	70.962403	67.306830
1287.224327	66.655480	67.311834
1286.680683	65.442560	67.316839
1285.752970	63.208901	67.321844
1284.866821	68.311021	67.326849
1283.505231	69.003822	67.331854
1283.134614	60.722207	67.336858
1282.976660	64.931100	67.341863
1282.292454	62.704459	67.346868
1282.150107	65.665062	67.351873
1281.195483	71.277972	67.356878
1280.339054	65.609371	67.361882
1280.032858	70.471048	67.366887
1278.837021	73.291644	67.371892
1278.208577	72.458066	67.376897
1277.472884	71.758236	67.381902
1277.042830	68.951861	67.386906
1276.473468	68.195623	67.391911
1275.714386	67.488474	67.396916
1274.727583	59.091943	67.401921
1273.999224	76.546642	67.406926
1273.814187	68.306483	67.411930
1273.424908	69.677335	67.416935
1272.868225	65.905487	67.421940
1272.000861	66.306821	67.426945
1271.185223	69.834954	67.431950
1270.167640	70.178171	67.436954
1269.138736	65.290792	67.441959
1268.570196	67.691526	67.446964
1268.416697	68.906617	67.451969
1267.529878	67.723034	67.456974
1267.166640	62.633620	67.461978
1266.895092	69.159803	67.466983
1265.839689	73.976601	67.471988
1265.276425	72.758920	67.476993
1264.336622	80.348584	67.481998
1263.727728	80.472278	67.487002
1262.729573	70.743430	67.492007
1262.196672	73.300928	67.497012
1261.778465	72.520659	67.502017
1261.114527	77.685230	67.507022
1260.727382	70.899637	67.512026
1260.129170	68.547363	67.517031
1259.096966	77.479530	67.522036
1258.783755	73.132799	67.527041
1258.097199	78.999566	67.532046
1257.147524	71.762517	67.537050
1256.470488	78.766345	67.542055
1255.658609	73.625261	67.547060
1255.484509	66.889377	67.552065
1254.680988	75.215895	67.557070
1253.708759	64.866337	67.562074
1253.491561	68.698294	67.567079
1252.955433	66.246262	67.572084
1252.026561	67.349674	67.577089
1250.797814	74.367110	67.582094
1250.196046	71.867167	67.587098
1249.950646	68.056867	67.592103
1249.877541	68.779776	67.597108
1249.133837	64.892590	67.602113
1247.871188	71.689909	67.607118
1247.263501	70.714265	67.612122
1246.725043	62.500347	67.617127
1245.340995	71.032716	67.622132
1244.921355	73.121193	67.627137
1244.313362	72.628152	67.632142
1244.062828	69.771160	67.637146
1243.679407	69.854275	67.642151
1242.575473	79.430221	67.647156
1242.025285	78.442280	67.652161
1241.162424	76.039050	67.657166
1240.653206	67.093498	67.662170
1240.602864	67.541548	67.667175
1239.518431	70.617262	67.672180
1238.680138	68.951305	67.677185
1238.045186	78.872153	67.682190
1237.495758	68.053242	67.687194
1236.349368	68.019557	67.692199
1235.364542	68.244037	67.697204
1235.285543	69.201276	67.702209
1234.776385	64.549815	67.707214
1234.094393	63.056127	67.712218
1234.050634	63.482630	67.717223
1232.920438	73.783428	67.722228
1232.238463	66.680445	67.727233
1231.505543	59.654954	67.732238
1230.777552	60.715391	67.737242
1229.736665	73.797959	67.742247
1229.306921	70.743959	67.747252
1228.772542	58.941788	67.752257
1228.319929	74.371964	67.757262
1227.191247	65.657387	67.762266
1226.393795	50.106016	67.767271
1225.576558	67.648959	67.772276
1225.555182	61.530623	67.777281
1224.817949	67.310833	67.782286
1225.030921	62.451502	67.787290
1223.955382	69.025109	67.792295
1223.152653	73.312881	67.797300
1222.229850	56.190273	67.802305
1221.148289	63.214272	67.807310
1220.531614	61.729126	67.812314
1220.141714	59.911447	67.817319
1219.477275	68.617981	67.822324
1219.232202	61.284679	67.827329
1218.147849	70.707701	67.832334
1217.330015	67.461525	67.837338
1216.842693	65.891153	67.842343
1216.463712	81.123545	67.847348
1215.921688	63.568214	67.852353
1214.722382	69.980154	67.857358
1213.976939	65.277962	67.862362
1213.998510	71.819037	67.867367
1212.934182	67.751033	67.872372
1211.955903	69.494682	67.877377
1211.087438	69.643897	67.882382
1210.827789	73.225561	67.887386
1210.658139	63.563692	67.892391
1210.028506	75.563721	67.897396
1209.475262	63.231536	67.902401
1208.527764	78.688375	67.907406
1207.698792	63.801186	67.912410
1206.769117	70.925621	67.917415
1206.039424	62.322653	67.922420
1205.760737	69.892351	67.927425
1205.180304	75.154040	67.932430
1204.820383	67.149864	67.937434
1203.673527	69.469110	67.942439
1202.689377	72.123610	67.947444
1202.732523	64.003298	67.952449
1201.824376	66.538476	67.957454
1201.028879	64.411559	67.962458
1200.297277	66.207448	67.967463
1199.469132	70.037215	67.972468
1199.210784	66.083899	67.977473
1198.619172	59.723508	67.982478
1197.560472	69.688088	67.987482
1196.938406	63.471312	67.992487
1196.385729	71.499327	67.997492
1196.285623	62.813587	68.002497
1195.314334	70.928673	68.007502
1194.159086	65.563097	68.012506
1194.079394	68.849634	68.017511
1193.161078	69.468835	68.022516
1192.254500	65.367870	68.027521
1191.311201	69.040908	68.032526
1190.663562	68.040092	68.037530
1190.608741	63.489856	68.042535
1190.064444	65.695936	68.047540
1189.602353	70.181860	68.052545
1188.441646	61.346241	68.057550
1187.995851	69.127021	68.062554
1187.418858	59.960452	68.067559
1186.071476	70.393574	68.072564
1185.532349	62.928843	68.077569
1184.770330	65.548022	68.082574
1184.526604	69.945602	68.087578
1184.453413	59.038363	68.092583
1183.428848	65.312136	68.097588
1182.640353	61.438404	68.102593
1182.194667	60.377089	68.107598
1181.279828	62.683099	68.112602
1180.409677	53.862784	68.117607
1179.147648	63.137449	68.122612
1179.079937	64.446135	68.127617
1178.614408	64.249002	68.132622
1178.017710	66.969625	68.137626
1177.826019	60.304362	68.142631
1176.273939	64.600930	68.147636
1175.739288	62.844127	68.152641
1174.895546	64.415003	68.157646
1174.563394	61.080565	68.162650
1174.569302	59.638344	68.167655
1173.075950	70.738090	68.172660
1172.646058	60.091010	68.177665
1172.096064	62.954019	68.182670
1171.520205	63.359490	68.187674
1170.497832	54.643812	68.192679
1169.371582	70.300968	68.197684
1169.419093	60.527300	68.202689
1168.945714	59.218076	68.207694
1168.576284	65.143232	68.212698
1167.534830	66.721900	68.217703
1166.501256	66.941544	68.222708
1166.446062	64.835674	68.227713
1165.066975	75.122461	68.232718
1164.356956	68.120157	68.237722
1164.231068	60.618097	68.242727
1163.072647	71.637772	68.247732
1162.952632	64.560559	68.252737
1162.262931	67.195051	68.257742
1161.411723	68.390223	68.262746
1160.819143	61.252550	68.267751
1160.164795	69.386626	68.272756
1159.854722	64.974759	68.277761
1158.755880	69.068366	68.282766
1157.808543	68.632470	68.287770
1157.635971	65.985444	68.292775
1156.880905	73.216166	68.297780
1156.014801	64.087702	68.302785
1155.220547	67.309688	68.307790
1154.900646	70.345843	68.312794
1154.281725	66.489305	68.317799
1153.472852	79.443534	68.322804
1152.669200	70.197900	68.327809
1151.685089	68.982524	68.332814
1151.372550	60.254883	68.337818
1151.302785	59.102245	68.342823
1150.482890	65.785029	68.347828
1149.565365	63.772155	68.352833
1148.743287	68.805776	68.357838
1148.365010	63.975824	68.362842
1148.097086	67.837930	68.367847
1146.845496	74.784923	68.372852
1146.596238	64.665789	68.377857
1145.582437	70.586200	68.382862
1144.319667	63.430542	68.387866
1144.070801	64.533072	68.392871
1143.172569	67.535053	68.397876
1142.676742	59.352236	68.402881
1142.295243	70.615783	68.407886
1142.017855	59.624331	68.412890
1141.177944	55.075966	68.417895
1139.781784	61.153384	68.422900
1139.550500	56.137629	68.427905
1139.370707	69.436501	68.432910
1138.767673	63.986278	68.437914
1137.975397	63.115715	68.442919
1137.129952	69.474558	68.447924
1136.384653	60.208617	68.452929
1135.353710	61.139069	68.457934
1134.311084	59.275411	68.462938
1134.301824	55.952702	68.467943
1133.571188	69.861163	68.472948
1133.511491	61.547478	68.477953
1132.567170	59.907885	68.482958
1131.838403	66.025816	68.487962
1131.264967	58.038276	68.492967
1130.572389	59.673433	68.497972
1129.505591	58.441256	68.502977
1128.663396	67.411045	68.507982
1128.160707	64.111623	68.512986
1128.143169	55.933163	68.517991
1127.241911	63.672846	68.522996
1126.118330	61.514559	68.528001
1125.974437	58.974940	68.533006
1125.065092	63.453160	68.538010
1124.695032	59.320505	68.543015
1123.553217	59.341337	68.548020
1123.046297	63.722434	68.553025
1122.234814	65.365468	68.558030
1121.566515	66.944726	68.563034
1121.737558	61.997444	68.568039
1120.389140	69.976992	68.573044
1119.526799	63.569798	68.578049
1118.807951	64.702929	68.583054
1118.742305	59.198778	68.588058
1118.348818	57.031601	68.593063
1117.088098	63.298802	68.598068
1116.621669	59.184631	68.603073
1115.927971	66.353558	68.608078
1114.467290	63.069320	68.613082
1114.131528	54.857900	68.618087
1113.583464	55.763592	68.623092
1113.702392	55.818864	68.628097
1113.055422	60.561285	68.633102
1112.186687	62.667596	68.638106
1111.442995	67.947382	68.643111
1110.676517	64.882313	68.648116
1110.247438	65.102022	68.653121
1108.971191	62.073884	68.658126
1107.921318	72.108052	68.663130
1107.824362	59.372164	68.668135
1107.382514	69.011570	68.673140
1107.372922	50.040647	68.678145
1106.012506	61.496168	68.683150
1105.286916	59.902218	68.688154
1105.077111	55.982199	68.693159
1103.784526	55.412004	68.698164
1103.189726	58.223804	68.703169
1102.800118	56.458140	68.708174
1101.798628	67.812420	68.713178
1101.724859	55.367741	68.718183
1100.246825	64.932267	68.723188
1099.822862	66.147809	68.728193
1099.456299	61.789095	68.733198
1098.487528	65.232823	68.738202
1098.628416	61.198672	68.743207
1097.533039	69.465990	68.748212
1096.849665	59.270842	68.753217
1095.827135	60.319820	68.758222
1094.751239	56.499722	68.763226
1094.042958	58.589976	68.768231
1093.339653	65.572776	68.773236
1093.503323	61.804663	68.778241
1093.202038	52.379806	68.783246
1092.541694	60.131638	68.788250
1091.708043	54.005327	68.793255
1090.723246	67.523709	68.798260
1090.145725	64.117926	68.803265
1089.989647	55.866889	68.808270
1088.508281	56.998319	68.813274
1088.341510	56.875106	68.818279
1087.433958	71.431466	68.823284
1086.941795	55.514624	68.828289
1085.691863	57.046061	68.833294
1084.919784	53.362145	68.838298
1084.893313	49.411390	68.843303
1084.287535	67.113103	68.848308
1083.857376	59.151671	68.853313
1082.952806	61.779360	68.858318
1081.929087	61.677345	68.863322
1081.870106	57.906803	68.868327
1080.921697	58.639642	68.873332
1079.524460	59.177369	68.878337
1079.146888	52.943820	68.883342
1078.563183	62.086966	68.888346
1078.323012	60.753279	68.893351
1077.843720	66.383678	68.898356
1077.279181	56.436144	68.903361
1076.219809	60.099296	68.908366
1075.551247	56.197064	68.913370
1075.299801	50.211538	68.918375
1074.135023	55.195610	68.923380
1073.136461	55.589496	68.928385
1072.759667	50.065462	68.933390
1071.971665	63.784353	68.938394
1071.853157	51.441419	68.943399
1071.010491	61.646059	68.948404
1070.300088	60.921768	68.953409
1069.860128	57.315912	68.958414
1068.643496	65.772839	68.963418
1068.518093	59.533868	68.968423
1067.457653	56.840433	68.973428
1066.789395	53.162085	68.978433
1066.354808	62.552750	68.983438
1065.573847	58.201618	68.988442
1065.496545	53.626585	68.993447
1064.569487	60.069389	68.998452
1064.064476	47.592400	69.003457
1063.119326	50.403169	69.008462
1061.754752	58.246534	69.013466
1061.311369	48.066846	69.018471
1060.783127	54.657519	69.023476
1060.479964	47.565307	69.028481
1060.378506	60.340766	69.033486
1059.008768	58.655335	69.038490
1058.134185	44.042003	69.043495
1057.662558	59.902548	69.048500
1057.422270	51.346368	69.053505
1056.343359	48.195404	69.058510
1055.458521	59.081696	69.063514
1055.212969	51.675964	69.068519
1054.589095	47.296695	69.073524
1054.285459	58.954706	69.078529
1053.197599	48.901200	69.083534
1052.363989	54.870242	69.088538
1052.261589	52.309838	69.093543
1050.799776	59.201996	69.098548
1050.092526	55.719092	69.103553
1049.603952	49.473247	69.108558
1049.171340	62.162615	69.113562
1049.175485	52.826374	69.118567
1047.781213	64.880247	69.123572
1047.044021	57.721462	69.128577
1046.514216	61.792393	69.133582
1046.164893	58.232048	69.138586
1045.419998	54.682594	69.143591
1044.557087	55.431806	69.148596
1043.820548	60.350919	69.153601
1043.117822	55.657762	69.158606
1041.963007	62.720286	69.163610
1041.545082	50.085944	69.168615
1040.819867	66.441005	69.173620
1040.438851	56.890068	69.178625
1040.350647	56.434235	69.183630
1039.653642	51.172463	69.188634
1038.706641	50.205121	69.193639
1037.933086	62.814688	69.198644
1037.303531	54.120164	69.203649
1036.527041	50.072687	69.208654
1035.315992	61.687402	69.213658
1035.113644	54.082409	69.218663
1034.649674	59.699335	69.223668
1034.371702	54.892875	69.228673
1034.062597	49.440082	69.233678
1032.609110	58.286364	69.238682
1032.195303	57.466012	69.243687
1031.064488	48.794469	69.248692
1029.992698	53.170825	69.253697
1029.583802	59.204771	69.258702
1029.028082	61.034225	69.263706
1029.042935	59.071761	69.268711
1028.359867	65.691806	69.273716
1027.616026	60.070052	69.278721
1026.970042	59.572070	69.283726
1026.161803	59.626610	69.288730
1025.732551	64.227178	69.293735
1024.540618	68.132218	69.298740
1023.944390	66.162893	69.303745
1023.539738	58.340924	69.308750
1022.448277	64.045069	69.313754
1021.709209	61.795693	69.318759
1021.160773	55.740728	69.323764
1020.695960	61.461870	69.328769
1020.283093	64.238435	69.333774
1019.571923	65.067594	69.338778
1019.070017	63.040687	69.343783
1018.326687	61.066383	69.348788
1017.733158	60.016003	69.353793
1016.763812	50.284287	69.358798
1015.670101	60.719692	69.363802
1015.359872	53.306909	69.368807
1014.860469	48.753305	69.373812
1014.482260	61.137548	69.378817
1013.647775	58.223683	69.383822
1012.446921	60.896956	69.388826
1012.429090	58.780419	69.393831
1011.536267	61.071945	69.398836
1010.724469	67.275654	69.403841
1009.974157	54.214803	69.408846
1009.273510	60.290438	69.413850
1009.023854	58.606604	69.418855
1008.532425	60.011091	69.423860
1007.327356	59.203093	69.428865
1006.621308	58.580630	69.433870
1006.364067	58.460777	69.438874
1005.956339	60.345539	69.443879
1004.932524	58.138319	69.448884
1003.943579	61.474901	69.453889
1003.785293	56.099041	69.458894
1002.859364	62.689920	69.463898
1002.687103	57.380939	69.468903
1001.140686	65.962903	69.473908
1000.661113	63.104538	69.478913
1000.386347	49.819798	69.483918
999.721780	60.283124	69.488922
999.116834	56.164211	69.493927
998.007860	54.542983	69.498932
997.399309	63.967640	69.503937
997.306986	60.481531	69.508942
996.590673	56.241565	69.513946
995.681633	58.423711	69.518951
995.049029	62.709705	69.523956
994.482136	62.429385	69.528961
993.630069	60.261075	69.533966
992.432046	60.148983	69.538970
992.099037	48.217090	69.543975
991.263515	52.044931	69.548980
991.329229	61.174647	69.553985
990.935794	48.919628	69.558990
989.663481	61.449285	69.563994
989.365604	55.277191	69.568999
988.924850	54.505290	69.574004
987.536769	50.633989	69.579009
986.558065	47.331494	69.584014
986.004412	50.012189	69.589018
985.989092	57.133124	69.594023
985.366496	50.668921	69.599028
984.212175	60.186723	69.604033
983.577625	51.358972	69.609038
982.920521	64.913547	69.614042
982.374846	58.632646	69.619047
982.151094	65.575436	69.624052
981.007135	61.294706	69.629057
980.510033	54.682801	69.634062
979.555902	55.194234	69.639066
979.046073	52.976208	69.644071
978.735605	56.603815	69.649076
977.672440	58.452519	69.654081
977.133692	56.604951	69.659086
976.470147	65.686698	69.664090
976.059734	59.355891	69.669095
974.868571	59.630650	69.674100
974.345882	49.608686	69.679105
973.889992	56.944803	69.684110
973.279679	54.919386	69.689114
973.023450	55.843328	69.694119
972.025048	56.469042	69.699124
971.336968	63.654449	69.704129
970.671004	64.026992	69.709134
969.328688	61.234948	69.714138
968.706375	58.180105	69.719143
968.435468	58.388863	69.724148
968.057488	63.783957	69.729153
967.809331	51.871682	69.734158
966.446619	64.507198	69.739162
965.617820	51.551899	69.744167
965.127755	58.570177	69.749172
964.572248	57.360795	69.754177
964.441324	56.530136	69.759182
963.313935	61.505152	69.764186
962.507574	50.582149	69.769191
962.001810	52.230201	69.774196
961.643948	56.964497	69.779201
960.686800	54.174249	69.784206
959.706401	59.931707	69.789210
959.433229	61.116969	69.794215
959.040504	61.580080	69.799220
957.674030	63.905991	69.804225
957.090871	62.431349	69.809230
956.294814	63.884319	69.814234
956.038222	59.199049	69.819239
955.739110	53.145432	69.824244
954.264120	54.840477	69.829249
953.849789	58.889895	69.834254
953.252569	58.262746	69.839258
952.938173	48.688620	69.844263
952.568256	57.447675	69.849268
951.354415	59.492255	69.854273
950.902588	55.818927	69.859278
950.055840	61.512543	69.864282
949.800634	61.572146	69.869287
948.721897	57.557024	69.874292
948.155648	54.725081	69.879297
947.799781	56.489633	69.884302
946.288043	58.132184	69.889306
945.351792	51.768366	69.894311
945.044183	51.178715	69.899316
944.696464	51.159999	69.904321
944.397128	53.552650	69.909326
943.939958	71.043067	69.914330
943.280836	53.801387	69.919335
942.312975	58.124969	69.924340
941.612570	60.001119	69.929345
940.702541	42.502909	69.934350
939.516573	55.223845	69.939354
939.455426	56.071014	69.944359
938.780868	54.801735	69.949364
938.474888	46.180340	69.954369
937.674592	55.457315	69.959374
936.988318	66.367236	69.964378
936.344965	60.037236	69.969383
936.185049	62.215313	69.974388
934.639053	63.205727	69.979393
934.272137	53.837080	69.984398
933.352498	59.040824	69.989402
932.799503	53.596897	69.994407
932.084340	63.013296	69.999412
931.092897	56.642496	70.004417
930.903817	60.197174	70.009422
930.271330	67.233394	70.014426
929.621796	56.662340	70.019431
929.228500	52.533422	70.024436
928.051482	62.390750	70.029441
927.841287	53.884998	70.034446
926.888739	59.371527	70.039450
926.426700	50.193066	70.044455
925.737048	56.997102	70.049460
925.039694	58.721382	70.054465
924.890012	55.340603	70.059470
923.301545	63.782639	70.064474
922.656464	55.822337	70.069479
922.308782	47.146079	70.074484
921.714211	56.983259	70.079489
921.396329	49.697872	70.084494
920.158985	51.774591	70.089498
919.495057	53.777406	70.094503
918.982436	53.020108	70.099508
918.359037	53.193502	70.104513
918.163964	45.998962	70.109518
916.855867	52.937686	70.114522
916.345786	54.551741	70.119527
916.098120	59.413585	70.124532
915.016483	60.809511	70.129537
914.114645	56.608558	70.134542
913.153299	66.879432	70.139546
912.806986	59.888728	70.144551
912.729488	56.985322	70.149556
912.093072	54.585604	70.154561
911.293127	60.457864	70.159566
910.054944	61.459232	70.164570
909.994249	53.574670	70.169575
909.332476	50.524549	70.174580
908.327555	59.238004	70.179585
907.944276	47.468676	70.184590
907.329548	58.777221	70.189594
906.955446	54.203702	70.194599
905.265310	54.439628	70.199604
904.739758	60.944740	70.204609
904.268498	60.887343	70.209614
903.837423	57.647542	70.214618
903.574182	53.258233	70.219623
902.588917	58.310002	70.224628
901.695099	61.312934	70.229633
901.504766	56.279658	70.234638
900.641974	64.399638	70.239642
899.450389	58.847609	70.244647
899.269914	55.634160	70.249652
898.392433	64.316301	70.254657
897.914025	48.444657	70.259662
897.390471	63.132324	70.264666
896.344855	56.082605	70.269671
896.084119	57.224892	70.274676
895.433919	65.899249	70.279681
895.158118	55.128381	70.284686
893.805249	57.641394	70.289690
893.148077	57.664050	70.294695
892.357069	58.844997	70.299700
891.795570	57.849476	70.304705
891.499003	51.875892	70.309710
890.156027	67.372068	70.314714
889.774001	56.263288	70.319719
889.362822	57.688142	70.324724
889.141244	59.697837	70.329729
888.426364	59.715484	70.334734
887.423062	61.240882	70.339738
886.911112	59.646115	70.344743
885.629421	63.620691	70.349748
884.814945	64.442674	70.354753
884.329734	57.709051	70.359758
883.671414	55.815879	70.364762
883.491715	55.180646	70.369767
883.324602	59.050377	70.374772
882.233492	56.574797	70.379777
881.684122	54.014577	70.384782
880.894225	54.230248	70.389786
880.270078	57.035725	70.394791
879.231925	53.143489	70.399796
878.602723	49.971497	70.404801
878.413240	52.384518	70.409806
877.238052	57.015510	70.414810
876.317386	51.937623	70.419815
876.051723	59.983073	70.424820
875.579618	57.011584	70.429825
875.461607	53.491727	70.434830
874.008315	60.198114	70.439834
873.367806	53.104433	70.444839
873.043456	53.928838	70.449844
872.046030	54.161771	70.454849
871.338080	51.877530	70.459854
870.549469	55.817790	70.464858
870.075154	51.879976	70.469863
869.724444	56.058049	70.474868
869.057557	64.150012	70.479873
868.276524	55.386613	70.484878
867.261044	62.556337	70.489882
866.758235	54.048282	70.494887
866.507420	55.130645	70.499892
865.307353	61.012982	70.504897
864.650253	48.104524	70.509902
863.901638	62.832744	70.514906
863.409269	55.270783	70.519911
863.304367	64.159556	70.524916
862.325037	56.309243	70.529921
861.583364	61.158253	70.534926
860.773335	60.416763	70.539930
860.541608	61.125502	70.544935
859.556042	48.486945	70.549940
858.556328	59.156599	70.554945
858.265480	44.627081	70.559950
857.956508	64.382076	70.564954
857.298833	54.878374	70.569959
856.610183	60.680894	70.574964
855.790211	57.682775	70.579969
854.971984	53.908512	70.584974
853.502244	56.090061	70.589978
853.038122	51.062523	70.594983
852.497551	45.269712	70.599988
851.971349	62.362671	70.604993
851.679582	59.171671	70.609998
851.628189	50.260611	70.615002
850.816022	60.909879	70.620007
849.938770	47.378873	70.625012
849.231095	61.595949	70.630017
848.349599	48.928217	70.635022
847.140825	54.597479	70.640026
846.467442	56.568700	70.645031
846.386800	52.285956	70.650036
845.964257	52.517285	70.655041
845.604917	50.016714	70.660046
844.408134	62.980684	70.665050
844.123781	54.160319	70.670055
843.581078	54.131651	70.675060
842.038350	56.692257	70.680065
841.723620	46.153110	70.685070
840.896584	64.533448	70.690074
840.579768	58.399089	70.695079
840.065444	53.221848	70.700084
838.552149	58.999509	70.705089
838.339813	57.049555	70.710094
837.795801	61.518600	70.715098
837.270397	52.679834	70.720103
836.600234	51.086607	70.725108
835.454750	64.578584	70.730113
835.126218	50.789930	70.735118
834.337536	58.248418	70.740122
834.227269	58.553047	70.745127
833.490644	46.677557	70.750132
832.638505	57.277995	70.755137
832.312879	47.778226	70.760142
830.765850	57.666096	70.765146
830.410974	54.663342	70.770151
830.066973	58.129142	70.775156
829.607098	59.189591	70.780161
828.603042	54.438813	70.785166
827.894004	55.379649	70.790170
827.189703	61.552100	70.795175
826.815918	49.387042	70.800180
825.411205	55.809750	70.805185
824.910616	46.030325	70.810190
824.288254	57.054663	70.815194
823.804070	54.048839	70.820199
823.548980	56.145874	70.825204
822.859295	63.148637	70.830209
822.051014	56.381300	70.835214
821.222393	59.358110	70.840218
821.015617	58.326643	70.845223
820.124295	60.201675	70.850228
818.802520	63.215983	70.855233
818.492511	58.007801	70.860238
818.378763	57.404653	70.865242
817.331310	56.525927	70.870247
816.337774	55.812085	70.875252
815.663231	70.929077	70.880257
815.303761	56.344250	70.885262
814.676747	58.360139	70.890266
814.235025	54.316223	70.895271
813.335939	51.899997	70.900276
812.287929	59.981670	70.905281
812.158197	44.543419	70.910286
811.893567	60.506636	70.915290
810.943060	50.459783	70.920295
810.323107	51.727067	70.925300
809.452824	60.272463	70.930305
808.763609	53.648608	70.935310
807.602176	60.650771	70.940314
807.039396	55.296746	70.945319
806.923268	50.876150	70.950324
806.288899	57.272438	70.955329
805.615974	51.410819	70.960334
804.762212	56.668771	70.965338
803.892570	52.513201	70.970343
803.576620	48.917626	70.975348
802.720898	52.822855	70.980353
801.950680	47.464008	70.985358
801.485326	58.827635	70.990362
800.917435	56.915361	70.995367
800.550953	58.594888	71.000372
799.191647	66.059066	71.005377
798.796101	62.182844	71.010382
798.149043	53.762427	71.015386
797.778493	56.656864	71.020391
796.894691	54.184594	71.025396
795.833390	63.993588	71.030401
795.338822	52.076424	71.035406
794.526867	56.700092	71.040410
794.709284	58.103007	71.045415
793.741281	54.287953	71.050420
793.019434	63.748020	71.055425
792.510086	53.161012	71.060430
791.766068	59.027552	71.065434
790.656493	56.485568	71.070439
789.952267	51.671310	71.075444
789.293717	61.966552	71.080449
789.237467	61.073553	71.085454
788.201763	60.703905	71.090458
787.662073	58.921186	71.095463
787.350437	62.484341	71.100468
786.147678	64.181879	71.105473
785.344026	63.127159	71.110478
784.890584	54.664886	71.115482
784.274118	60.124767	71.120487
783.880257	56.860144	71.125492
783.173495	65.858916	71.130497
782.038774	61.848053	71.135502
781.467999	54.509910	71.140506
781.046157	66.997301	71.145511
781.048188	50.333274	71.150516
779.287203	52.379878	71.155521
778.917721	61.170413	71.160526
778.099775	57.661062	71.165530
777.654570	52.252059	71.170535
777.346963	48.503773	71.175540
776.191867	58.701442	71.180545
776.002384	43.348406	71.185550
775.462338	52.095125	71.190554
773.867767	60.591829	71.195559
773.223962	44.942108	71.200564
772.658844	60.699268	71.205569
772.145633	52.981379	71.210574
771.958450	52.128149	71.215578
771.484863	56.281638	71.220583
770.474317	50.227773	71.225588
769.354801	62.387831	71.230593
769.266023	53.768161	71.235598
768.780089	48.748847	71.240602
767.712306	49.489766	71.245607
767.019838	48.731169	71.250612
766.493514	55.334192	71.255617
766.258250	44.905416	71.260622
765.420175	53.414153	71.265626
764.230952	58.444822	71.270631
763.911082	47.909665	71.275636
763.309486	61.971092	71.280641
762.466498	50.678691	71.285646
761.720000	59.306895	71.290650
760.947743	55.525347	71.295655
760.911207	55.151186	71.300660
759.558281	62.833563	71.305665
758.554857	51.081001	71.310670
758.140519	57.880665	71.315674
757.398105	52.298208	71.320679
757.321581	48.055817	71.325684
757.058057	65.594245	71.330689
756.839092	54.666126	71.335694
755.476855	52.965480	71.340698
754.475931	52.964049	71.345703
753.688469	57.407209	71.350708
752.871416	60.828479	71.355713
752.506599	53.361362	71.360718
751.909590	59.926757	71.365722
751.505858	50.067277	71.370727
751.121113	45.528602	71.375732
749.729802	56.356823	71.380737
749.424514	45.470840	71.385742
748.885199	55.745525	71.390746
747.730122	51.398876	71.395751
747.132989	60.662474	71.400756
746.275019	58.586658	71.405761
746.054168	54.261588	71.410766
745.688760	50.194500	71.415770
744.632609	58.990277	71.420775
744.182883	55.020192	71.425780
743.385898	55.388422	71.430785
742.873312	53.707056	71.435790
742.104112	57.227943	71.440794
741.011629	57.282095	71.445799
740.834100	51.161853	71.450804
740.304827	64.243515	71.455809
739.241456	54.914835	71.460814
738.844199	50.174725	71.465818
738.107140	54.608287	71.470823
737.694735	52.994551	71.475828
736.428631	58.368634	71.480833
735.869000	61.080292	71.485838
735.380090	55.791798	71.490842
734.590405	51.994112	71.495847
734.080590	52.360780	71.500852
733.218020	67.912993	71.505857
732.850990	52.102521	71.510862
732.546011	54.439320	71.515866
731.581922	57.749963	71.520871
730.631610	56.305448	71.525876
729.781751	58.826770	71.530881
729.445334	57.375980	71.535886
729.196896	52.134358	71.540890
728.296478	60.632533	71.545895
727.599467	56.523625	71.550900
726.744937	56.855291	71.555905
726.409526	57.608935	71.560910
725.277871	58.336386	71.565914
724.673052	62.660589	71.570919
724.306464	58.609461	71.575924
723.778675	68.917015	71.580929
722.888376	56.559825	71.585934
721.979946	58.049680	71.590938
721.154072	54.672501	71.595943
721.057597	55.905347	71.600948
720.495002	54.526839	71.605953
719.692226	55.201930	71.610958
719.072763	51.389764	71.615962
718.027125	48.282545	71.620967
718.058064	44.209130	71.625972
716.524830	56.810388	71.630977
716.123831	55.981744	71.635982
715.575212	51.426588	71.640986
714.827519	62.865140	71.645991
714.779120	45.786533	71.650996
713.234591	49.533375	71.656001
712.636661	45.977982	71.661006
712.250721	47.752081	71.666010
711.840714	53.155447	71.671015
711.221002	42.959785	71.676020
710.199045	49.290065	71.681025
709.467624	52.227777	71.686030
709.300964	49.529393	71.691034
708.164818	54.176317	71.696039
707.502114	54.622527	71.701044
706.444225	54.100326	71.706049
706.252173	46.511099	71.711054
706.062826	47.834425	71.716058
705.362752	55.971120	71.721063
704.489620	43.187014	71.726068
703.516918	46.212029	71.731073
703.396050	47.250061	71.736078
702.731277	51.484463	71.741082
701.558140	50.307252	71.746087
701.110607	44.466554	71.751092
700.439591	50.124369	71.756097
699.548966	45.924874	71.761102
699.179656	46.720188	71.766106
698.155228	48.876651	71.771111
698.107012	40.204808	71.776116
697.313524	52.406010	71.781121
696.506978	49.085689	71.786126
695.849789	53.031878	71.791130
695.347385	53.537724	71.796135
694.244769	53.399544	71.801140
693.173385	51.176379	71.806145
693.039905	35.404445	71.811150
692.616841	48.907580	71.816154
691.975406	51.933470	71.821159
691.448980	43.634238	71.826164
690.547875	55.403146	71.831169
689.891548	37.022589	71.836174
689.620877	42.036336	71.841178
688.163144	47.888806	71.846183
687.600943	37.445878	71.851188
686.881227	49.466598	71.856193
686.615921	40.785168	71.861198
686.631944	45.674417	71.866202
685.504458	48.634199	71.871207
684.758682	48.120657	71.876212
684.091924	46.208386	71.881217
682.599525	55.116224	71.886222
681.974153	40.688911	71.891226
681.482026	46.761369	71.896231
681.268004	46.497473	71.901236
680.852555	53.470785	71.906241
680.373309	49.324065	71.911246
679.531020	42.084388	71.916250
678.371848	49.160353	71.921255
678.284949	56.989680	71.926260
677.435253	54.177709	71.931265
676.580463	50.418796	71.936270
675.927668	42.275310	71.941274
675.302443	51.210647	71.946279
674.945309	48.520520	71.951284
673.551918	43.219951	71.956289
672.954262	50.660670	71.961294
672.589453	49.698537	71.966298
672.167604	52.162761	71.971303
671.726516	50.949422	71.976308
670.699529	47.380359	71.981313
669.937642	49.722110	71.986318
669.647687	46.229652	71.991322
668.514776	53.902263	71.996327
667.835571	47.429831	72.001332
667.086899	57.644821	72.006337
666.828570	52.078354	72.011342
666.435040	51.300569	72.016346
665.371608	52.843510	72.021351
664.790404	50.893966	72.026356
664.401257	59.589866	72.031361
663.833466	44.755993	72.036366
662.717272	48.850974	72.041370
661.824011	57.068903	72.046375
661.652686	52.236061	72.051380
660.634197	50.770892	72.056385
659.619507	45.419488	72.061390
659.078248	54.830316	72.066394
658.342607	61.474573	72.071399
658.304659	51.514292	72.076404
657.591677	55.420489	72.081409
657.315689	52.482475	72.086414
656.131686	49.156043	72.091418
655.236101	57.863201	72.096423
655.238776	45.190391	72.101428
654.148272	55.057691	72.106433
653.135282	50.298955	72.111438
652.805127	52.650809	72.116442
651.874821	48.350418	72.121447
651.709118	41.830916	72.126452
651.237660	48.955073	72.131457
650.364329	59.292421	72.136462
650.002809	55.915440	72.141466
648.907547	62.525504	72.146471
648.002695	45.709454	72.151476
647.438416	52.908320	72.156481
646.868255	53.541660	72.161486
646.844574	44.884836	72.166490
645.543166	48.037911	72.171495
644.925758	52.148088	72.176500
644.552214	56.482784	72.181505
643.511137	55.374458	72.186510
642.640341	49.558597	72.191514
641.747141	52.307622	72.196519
641.584780	44.459787	72.201524
641.010244	56.093122	72.206529
640.253844	54.084750	72.211534
639.839101	55.220047	72.216538
639.012545	54.244719	72.221543
638.681847	50.038082	72.226548
637.799832	51.359755	72.231553
636.519071	49.986826	72.236558
635.751014	52.674923	72.241562
635.370689	60.509977	72.246567
635.281981	40.775902	72.251572
635.042966	46.907407	72.256577
633.669826	52.405812	72.261582
633.365068	53.501517	72.266586
632.741307	56.792690	72.271591
631.757167	43.239395	72.276596
630.670784	54.574196	72.281601
629.798675	50.871676	72.286606
629.828925	42.862282	72.291610
629.487777	51.427532	72.296615
628.671423	40.042651	72.301620
627.532991	53.494134	72.306625
627.017594	51.772241	72.311630
626.704101	38.261962	72.316634
625.352220	48.826907	72.321639
624.636290	38.881570	72.326644
624.189978	48.911215	72.331649
623.833159	49.043804	72.336654
623.783136	54.919709	72.341658
622.915615	53.001580	72.346663
621.989035	45.840005	72.351668
621.010741	47.694259	72.356673
620.499345	44.902552	72.361678
619.723984	45.169606	72.366682
618.825616	59.688315	72.371687
618.552814	50.804659	72.376692
618.018403	50.700602	72.381697
617.303067	53.534851	72.386702
616.526300	51.625925	72.391706
615.772646	55.568572	72.396711
615.240749	49.813868	72.401716
614.730648	54.999796	72.406721
613.310532	47.776473	72.411726
613.104400	41.909968	72.416730
612.477004	53.944386	72.421735
611.961080	45.058452	72.426740
611.510711	55.104518	72.431745
610.661829	49.209486	72.436750
610.271197	48.000739	72.441754
609.332747	59.573766	72.446759
608.625125	38.407041	72.451764
607.691916	49.484060	72.456769
606.879513	39.740174	72.461774
606.829511	42.496847	72.466778
606.364947	41.883351	72.471783
605.534217	43.822919	72.476788
604.424838	45.116158	72.481793
604.015053	49.428243	72.486798
603.855932	52.219643	72.491802
601.976810	46.007722	72.496807
601.736225	41.603816	72.501812
600.756881	50.220245	72.506817
600.355128	51.665716	72.511822
600.128466	46.600423	72.516826
599.604628	53.491655	72.521831
598.750351	41.644469	72.526836
597.827378	47.837596	72.531841
597.394869	42.655277	72.536846
597.202314	46.588988	72.541850
595.836352	52.308620	72.546855
595.135207	45.579509	72.551860
594.299086	53.313689	72.556865
593.940279	47.288573	72.561870
593.869201	42.367237	72.566874
592.610041	50.362757	72.571879
592.287785	49.631981	72.576884
591.615895	45.651583	72.581889
591.023531	47.468037	72.586894
590.007050	43.755412	72.591898
589.095035	48.290991	72.596903
589.061339	37.494263	72.601908
588.695537	45.185072	72.606913
587.386580	45.753165	72.611918
586.720612	47.693306	72.616922
586.293893	49.887081	72.621927
585.734023	40.263833	72.626932
584.548797	50.870064	72.631937
583.967394	50.361913	72.636942
583.440256	50.584713	72.641946
583.017097	64.111533	72.646951
582.262459	56.823236	72.651956
581.388385	52.852965	72.656961
580.756658	53.715323	72.661966
580.692647	46.141992	72.666970
579.475806	53.339146	72.671975
578.659403	43.720487	72.676980
577.752867	52.449907	72.681985
577.647018	49.467461	72.686990
577.127995	47.954315	72.691994
576.253836	55.303473	72.696999
575.686043	57.128633	72.702004
575.051386	52.566719	72.707009
574.370637	49.139672	72.712014
573.229446	44.546475	72.717018
572.168476	57.687596	72.722023
571.976304	51.809408	72.727028
571.448983	49.903345	72.732033
571.266941	54.674327	72.737038
571.446675	46.696320	72.742042
570.722913	51.523621	72.747047
569.771048	58.451495	72.752052
568.532404	53.646736	72.757057
567.615701	55.598434	72.762062
566.884170	51.184417	72.767066
565.923159	60.250529	72.772071
565.238160	52.810800	72.777076
565.026152	57.197046	72.782081
564.639375	59.627315	72.787086
563.878007	47.837882	72.792090
562.837108	54.194886	72.797095
562.412500	52.682474	72.802100
561.749532	54.593760	72.807105
560.969144	53.697838	72.812110
560.083188	52.463914	72.817114
559.256909	50.558164	72.822119
559.095299	46.676272	72.827124
558.742525	51.458678	72.832129
557.630264	55.217184	72.837134
556.886490	50.866621	72.842138
556.327032	53.800637	72.847143
555.824107	46.585803	72.852148
555.551216	55.979129	72.857153
554.435683	56.070151	72.862158
553.679246	55.460576	72.867162
552.515145	61.088155	72.872167
552.522525	50.576616	72.877172
552.109817	55.218759	72.882177
550.643432	57.819416	72.887182
550.270037	44.987324	72.892186
549.766466	46.212477	72.897191
549.489167	44.354906	72.902196
548.849946	51.843267	72.907201
547.666235	56.300712	72.912206
547.354578	50.192400	72.917210
546.657524	51.257561	72.922215
545.949502	55.331730	72.927220
544.596578	53.825262	72.932225
544.072520	45.897859	72.937230
543.803748	47.227539	72.942234
543.212389	63.924030	72.947239
543.230011	53.983295	72.952244
541.802407	53.045392	72.957249
541.095675	52.727526	72.962254
540.920079	51.505039	72.967258
539.662988	55.244044	72.972263
539.433069	52.174129	72.977268
538.734401	56.983249	72.982273
538.163875	50.808941	72.987278
537.470238	42.435466	72.992282
536.198519	50.440895	72.997287
535.853987	46.536104	73.002292
535.277048	48.241303	73.007297
534.617077	52.616904	73.012302
534.009835	49.501437	73.017306
532.841365	60.144448	73.022311
532.470598	45.261896	73.027316
532.294070	49.800185	73.032321
531.739117	55.961522	73.037326
530.911291	40.571460	73.042330
529.887859	54.875137	73.047335
529.520287	44.445410	73.052340
528.665983	48.776272	73.057345
527.585246	44.741173	73.062350
527.253857	37.043287	73.067354
526.499863	39.767019	73.072359
526.318756	45.685874	73.077364
525.327949	54.540698	73.082369
524.598905	47.320891	73.087374
524.179685	43.393308	73.092378
523.617507	54.982108	73.097383
522.623119	45.160011	73.102388
521.652898	53.800244	73.107393
521.150790	54.823319	73.112398
521.226374	40.587190	73.117402
520.276494	49.977966	73.122407
519.576625	40.667202	73.127412
518.567071	48.301292	73.132417
518.121912	48.436930	73.137422
517.502807	44.847118	73.142426
516.469014	46.538363	73.147431
515.709806	37.454675	73.152436
515.313603	42.622469	73.157441
515.083250	51.409772	73.162446
514.933158	38.818093	73.167450
513.926249	46.827078	73.172455
513.292385	47.685062	73.177460
512.046891	45.374598	73.182465
510.772516	45.386864	73.187470
510.319411	46.465213	73.192474
509.680036	45.800734	73.197479
509.374877	40.497224	73.202484
509.264443	46.400091	73.207489
508.539161	52.788837	73.212494
507.866953	42.492802	73.217498
507.076382	45.118288	73.222503
506.595983	39.932581	73.227508
505.697302	49.233203	73.232513
504.737142	48.376976	73.237518
504.257505	44.525253	73.242522
503.815776	43.865561	73.247527
502.704477	43.749350	73.252532
502.093185	46.986523	73.257537
501.663703	45.104315	73.262542
501.603523	34.881101	73.267546
500.524471	57.693444	73.272551
499.681747	54.032025	73.277556
499.467452	47.807288	73.282561
498.075803	58.657752	73.287566
497.511540	41.398024	73.292570
496.609156	40.314977	73.297575
496.528411	42.078332	73.302580
495.848409	50.484679	73.307585
494.682879	49.741598	73.312590
494.250770	43.832261	73.317594
493.852450	48.590388	73.322599
493.445923	43.515917	73.327604
492.402507	40.886267	73.332609
491.404027	35.136547	73.337614
491.261255	35.621410	73.342618
490.412941	46.702279	73.347623
489.408695	39.195170	73.352628
488.907019	43.455674	73.357633
488.211489	52.559936	73.362638
487.939767	35.018649	73.367642
487.253953	44.873566	73.372647
486.558356	39.865650	73.377652
485.704203	41.898874	73.382657
485.325434	46.144529	73.387662
484.549391	39.326468	73.392666
483.585847	43.204812	73.397671
482.615578	42.438514	73.402676
482.626931	35.185932	73.407681
481.784098	50.413326	73.412686
481.294275	44.178872	73.417690
480.502684	49.819671	73.422695
480.167016	45.069806	73.427700
479.091517	46.671516	73.432705
478.013810	44.208184	73.437710
477.760081	37.786310	73.442714
477.015440	50.255736	73.447719
476.835044	43.442130	73.452724
475.927877	44.247469	73.457729
474.843715	48.509310	73.462734
474.653615	37.847901	73.467738
473.845483	56.239457	73.472743
473.348662	47.044592	73.477748
472.458614	39.263831	73.482753
471.417507	44.513873	73.487758
471.095310	44.126880	73.492762
471.014135	45.327331	73.497767
470.317772	45.315341	73.502772
469.785939	45.275561	73.507777
468.666752	47.634868	73.512782
467.815772	41.937351	73.517786
466.938532	57.482474	73.522791
466.254100	44.991699	73.527796
466.162373	47.958446	73.532801
465.638481	55.702840	73.537806
464.237190	51.376639	73.542810
463.587269	56.504440	73.547815
463.094955	54.144969	73.552820
462.927213	49.215388	73.557825
462.378838	52.636512	73.562830
461.348146	45.931567	73.567834
460.701878	46.782078	73.572839
460.295684	50.629983	73.577844
459.319344	57.457711	73.582849
458.089705	57.226333	73.587854
457.896845	48.309474	73.592858
457.450287	57.050802	73.597863
456.846497	63.451747	73.602868
455.818078	51.510939	73.607873
454.763582	57.449101	73.612878
454.657769	52.085451	73.617882
454.255816	60.666710	73.622887
454.011528	54.232289	73.627892
452.894276	50.762862	73.632897
451.617600	57.573787	73.637902
451.881035	45.608515	73.642906
450.603341	53.356313	73.647911
449.579117	48.736656	73.652916
449.436263	46.319935	73.657921
448.923942	52.707881	73.662926
448.636516	39.914167	73.667930
447.354611	42.338830	73.672935
446.263145	46.262801	73.677940
446.185290	46.783055	73.682945
445.341088	53.909855	73.687950
445.042767	46.504758	73.692954
443.874055	59.898051	73.697959
443.422856	40.491440	73.702964
443.115130	50.435940	73.707969
442.252296	49.955316	73.712974
441.395372	46.095910	73.717978
440.521225	49.788139	73.722983
440.323553	52.530493	73.727988
440.141974	52.531109	73.732993
438.851708	47.958577	73.737998
438.394495	50.056306	73.743002
437.675140	47.416048	73.748007
436.353494	49.612083	73.753012
435.513613	56.468539	73.758017
434.591193	47.409305	73.763022
434.379292	57.502545	73.768026
433.887928	49.533694	73.773031
433.441982	42.007043	73.778036
432.716253	49.681095	73.783041
432.661992	50.328478	73.788046
432.621550	46.113480	73.793050
431.098551	50.489415	73.798055
430.790845	47.458717	73.803060
430.037042	45.134611	73.808065
429.089535	48.174633	73.813070
428.608608	44.208016	73.818074
427.371966	53.770667	73.823079
426.869456	44.799075	73.828084
426.697449	42.071610	73.833089
425.676079	58.751461	73.838094
425.038661	50.777498	73.843098
424.109853	51.505879	73.848103
423.878770	50.497247	73.853108
423.657505	49.452358	73.858113
422.119882	47.696268	73.863118
421.691606	44.369392	73.868122
421.240314	53.658678	73.873127
420.059036	54.865682	73.878132
419.184930	50.047078	73.883137
418.287882	56.504216	73.888142
418.156149	45.325732	73.893146
417.736342	48.969230	73.898151
417.226761	47.675390	73.903156
416.841495	44.739054	73.908161
415.881332	41.746089	73.913166
415.299781	41.313696	73.918170
414.654101	50.878383	73.923175
413.547075	54.661345	73.928180
412.960944	43.873812	73.933185
412.169750	56.929414	73.938190
412.030234	44.569455	73.943194
411.041735	47.467781	73.948199
410.111234	55.850983	73.953204
409.688229	52.013911	73.958209
409.073251	45.392563	73.963214
408.747891	48.167879	73.968218
407.921010	52.275212	73.973223
407.050554	45.754497	73.978228
406.631878	45.263038	73.983233
405.910267	51.241213	73.988238
405.223692	41.849526	73.993242
404.487279	53.574909	73.998247
403.624098	51.518975	74.003252
403.512826	48.925337	74.008257
402.294898	53.350449	74.013262
401.485850	52.750882	74.018266
400.987973	51.125596	74.023271
400.262158	48.062178	74.028276
399.973002	53.506244	74.033281
399.431571	55.442358	74.038286
398.927924	42.788764	74.043290
397.957869	55.592170	74.048295
397.217292	51.430389	74.053300
396.671828	49.604529	74.058305
395.380191	54.533400	74.063310
395.119139	56.972042	74.068314
394.381434	44.157048	74.073319
393.889247	46.310820	74.078324
393.737093	49.421238	74.083329
392.379578	52.832537	74.088334
391.921150	55.770986	74.093338
391.353467	46.227892	74.098343
390.921789	53.147045	74.103348
390.175027	55.325615	74.108353
389.466994	58.169798	74.113358
388.962474	51.839936	74.118362
387.868646	58.812565	74.123367
386.807924	53.962209	74.128372
386.622291	42.289274	74.133377
385.287034	53.496650	74.138382
384.438716	45.177842	74.143386
383.707727	46.999084	74.148391
383.544467	52.736904	74.153396
383.431700	44.398657	74.158401
383.090129	45.249519	74.163406
382.716883	39.702993	74.168410
381.519358	52.435415	74.173415
380.740726	50.441710	74.178420
380.370417	45.397763	74.183425
378.764859	44.713818	74.188430
378.476821	38.024615	74.193434
377.678388	46.279542	74.198439
377.308297	49.572923	74.203444
377.333995	47.772747	74.208449
376.353591	49.912858	74.213454
375.677896	39.098613	74.218458
375.645521	48.029407	74.223463
374.180300	49.264333	74.228468
373.324800	41.426071	74.233473
372.489087	43.789130	74.238478
372.079012	44.643026	74.243482
370.996080	46.436777	74.248487
370.196851	41.131601	74.253492
369.967709	39.176493	74.258497
369.234441	51.366581	74.263502
369.133400	43.204664	74.268506
368.784214	51.321774	74.273511
367.503265	50.346410	74.278516
367.288326	37.383473	74.283521
366.420539	46.373277	74.288526
365.763279	47.875269	74.293530
364.635780	45.580773	74.298535
363.980983	47.689501	74.303540
363.810812	52.810255	74.308545
362.749734	45.075719	74.313550
361.983883	39.329988	74.318554
361.284275	52.497156	74.323559
360.677661	52.696399	74.328564
360.622399	44.396300	74.333569
359.555499	51.083947	74.338574
358.898202	44.040428	74.343578
358.172381	46.890605	74.348583
357.945324	42.424654	74.353588
357.507558	40.807147	74.358593
356.073744	49.751540	74.363598
355.714998	43.359036	74.368602
355.287663	42.015834	74.373607
354.160347	46.374486	74.378612
353.539573	39.648426	74.383617
352.789819	42.962889	74.388622
352.544157	52.485915	74.393626
351.326282	42.690062	74.398631
350.269541	54.488581	74.403636
349.899562	48.454258	74.408641
349.356940	45.082542	74.413646
349.604387	40.365932	74.418650
348.814375	42.297515	74.423655
347.690995	46.953587	74.428660
347.028885	45.434911	74.433665
346.451509	50.246821	74.438670
346.026138	45.353582	74.443674
344.570169	49.121217	74.448679
344.294540	52.166159	74.453684
344.073797	45.582929	74.458689
343.435981	56.717024	74.463694
342.578470	48.513238	74.468698
341.541974	51.365623	74.473703
340.961175	42.862275	74.478708
340.778538	41.577849	74.483713
339.784098	50.553154	74.488718
338.970178	49.251063	74.493722
338.339365	52.898237	74.498727
337.666668	52.043573	74.503732
337.552536	37.183269	74.508737
336.275206	46.618395	74.513742
335.660695	41.651224	74.518746
335.211027	49.525728	74.523751
334.570404	57.559979	74.528756
334.032545	46.446235	74.533761
332.917270	45.802454	74.538766
332.623034	35.678066	74.543770
332.245129	46.671385	74.548775
331.139190	49.821847	74.553780
330.753961	44.113236	74.558785
330.091252	49.189484	74.563790
329.329704	41.530232	74.568794
328.470280	49.336000	74.573799
327.411396	46.112799	74.578804
327.280601	46.010713	74.583809
326.368433	55.285149	74.588814
326.171711	50.041658	74.593818
325.327441	62.101219	74.598823
324.794938	63.316834	74.603828
324.316928	49.315608	74.608833
322.663952	55.992597	74.613838
322.296793	51.979486	74.618842
321.964451	53.907523	74.623847
321.346097	53.626098	74.628852
321.033439	56.006739	74.633857
319.980845	57.551249	74.638862
319.207818	53.779443	74.643866
318.870472	57.122807	74.648871
317.825463	60.791846	74.653876
317.033993	48.532655	74.658881
316.258764	56.153123	74.663886
315.879965	52.504568	74.668890
315.645718	46.066997	74.673895
314.739160	57.461548	74.678900
314.014065	52.155612	74.683905
313.104732	48.003411	74.688910
312.873760	42.789037	74.693914
312.521902	50.228485	74.698919
310.970800	52.268767	74.703924
310.537875	40.457066	74.708929
309.991292	47.651582	74.713934
309.584037	41.430823	74.718938
308.574115	50.115292	74.723943
307.410231	52.398213	74.728948
307.596860	49.523713	74.733953
306.766162	56.019193	74.738958
306.977497	46.597971	74.743962
305.566449	49.036981	74.748967
304.546149	54.958707	74.753972
304.331772	39.448911	74.758977
303.234728	51.706451	74.763982
302.251008	46.708247	74.768986
301.858407	45.499867	74.773991
301.307382	52.062735	74.778996
301.255848	46.805570	74.784001
300.278647	49.246397	74.789006
299.553708	37.645248	74.794010
298.773289	52.045866	74.799015
298.226949	45.352113	74.804020
297.934674	46.581483	74.809025
296.790508	50.010865	74.814030
296.326850	51.478864	74.819034
295.722727	43.401872	74.824039
294.702690	49.038129	74.829044
293.696453	44.893497	74.834049
292.921575	50.949573	74.839054
292.648851	38.631374	74.844058
292.380189	46.104870	74.849063
291.851406	44.968660	74.854068
291.374347	47.001767	74.859073
290.001313	48.914331	74.864078
289.524803	43.948832	74.869082
289.246353	48.965419	74.874087
287.985763	52.254090	74.879092
287.691491	42.952883	74.884097
286.897136	51.393265	74.889102
286.440632	39.602677	74.894106
285.622586	48.124104	74.899111
284.572737	43.456572	74.904116
284.428084	37.238119	74.909121
284.124590	41.921228	74.914126
283.014374	37.324821	74.919130
282.222620	46.805576	74.924135
281.548897	45.457504	74.929140
281.214380	40.332181	74.934145
280.131318	42.804080	74.939150
279.099811	38.821180	74.944154
278.530258	39.009804	74.949159
278.319225	46.909354	74.954164
278.086767	47.744415	74.959169
277.613363	49.253394	74.964174
276.518278	41.574787	74.969178
276.084271	38.985294	74.974183
274.987557	49.851916	74.979188
274.235949	43.044233	74.984193
273.260075	51.182392	74.989198
273.143652	44.205654	74.994202
272.891198	48.177309	74.999207
271.724521	46.508846	75.004212
271.143883	36.367045	75.009217
270.111454	42.530408	75.014222
270.071790	40.303836	75.019226
269.017658	38.603243	75.024231
267.774391	45.572922	75.029236
267.286938	42.484170	75.034241
267.021484	51.346453	75.039246
266.347546	45.497795	75.044250
266.570349	45.782473	75.049255
265.455936	52.703232	75.054260
264.707379	37.649180	75.059265
264.034817	49.495293	75.064270
263.070460	42.764104	75.069274
262.328712	43.349187	75.074279
262.229760	44.500436	75.079284
262.367163	38.306413	75.084289
261.232045	47.009273	75.089294
260.246096	42.147064	75.094298
259.487743	39.508350	75.099303
258.790360	48.243938	75.104308
257.419151	42.952708	75.109313
256.376099	50.549646	75.114318
255.901566	46.473240	75.119322
256.123309	49.571370	75.124327
255.695946	50.599928	75.129332
255.195053	42.005024	75.134337
253.823684	50.597315	75.139342
253.395682	46.429915	75.144346
252.973126	47.598055	75.149351
251.606329	49.296758	75.154356
250.967475	43.513476	75.159361
250.245529	52.481643	75.164366
249.861378	46.108980	75.169370
249.655792	47.058031	75.174375
248.621604	53.663234	75.179380
248.031562	50.511990	75.184385
247.001370	42.438278	75.189390
246.684180	45.770549	75.194394
246.476009	46.937632	75.199399
245.423079	49.868368	75.204404
244.824870	40.588814	75.209409
244.047041	44.126978	75.214414
243.291622	51.999768	75.219418
242.452408	44.826016	75.224423
241.781823	48.903750	75.229428
241.582178	47.043302	75.234433
240.959400	52.786564	75.239438
239.612647	52.701698	75.244442
239.153128	40.785448	75.249447
238.516366	45.505918	75.254452
238.509619	44.049960	75.259457
237.636021	50.738376	75.264462
236.793882	50.519454	75.269466
236.051749	51.907275	75.274471
235.316140	58.234653	75.279476
234.888287	42.817249	75.284481
234.089882	46.746627	75.289486
232.921301	50.941596	75.294490
232.650614	41.901571	75.299495
232.032841	51.236333	75.304500
231.914776	51.744080	75.309505
230.776171	52.532785	75.314510
230.033066	50.503506	75.319514
229.855958	47.863606	75.324519
228.376323	51.717080	75.329524
228.031692	48.534605	75.334529
227.169629	61.308228	75.339534
226.670584	53.780629	75.344538
227.023130	53.715037	75.349543
225.563067	55.124270	75.354548
224.834557	59.425711	75.359553
224.248109	57.160147	75.364558
223.619596	60.600401	75.369562
222.701725	57.958740	75.374567
222.036012	56.036974	75.379572
221.675191	47.777715	75.384577
221.381298	55.411357	75.389582
220.298821	56.487587	75.394586
219.647731	46.010099	75.399591
219.070017	54.004377	75.404596
218.483716	50.319535	75.409601
217.166384	47.978103	75.414606
216.635829	47.504512	75.419610
215.921688	51.095610	75.424615
215.345794	53.887233	75.429620
215.337608	38.563787	75.434625
214.347783	45.023153	75.439630
213.526216	41.016276	75.444634
213.213715	38.598236	75.449639
212.419393	51.350016	75.454644
211.511853	46.752870	75.459649
210.384944	52.305271	75.464654
210.200593	55.739372	75.469658
210.243485	49.450025	75.474663
209.357497	56.665551	75.479668
208.351415	53.252637	75.484673
207.581855	66.803152	75.489678
207.137099	58.614043	75.494682
206.200154	41.831744	75.499687
205.068591	48.329481	75.504692
204.948668	46.749641	75.509697
204.209190	46.848678	75.514702
204.223769	45.184317	75.519706
203.443407	43.037985	75.524711
202.503702	51.465289	75.529716
202.068898	50.443426	75.534721
201.211625	41.394422	75.539726
200.365338	44.101420	75.544730
199.683550	43.246667	75.549735
199.110219	49.666449	75.554740
198.335238	51.758108	75.559745
197.327326	52.477108	75.564750
197.055457	50.276518	75.569754
196.943195	48.209755	75.574759
195.961025	56.853568	75.579764
195.096387	51.614077	75.584769
194.382794	47.142137	75.589774
193.809665	48.351639	75.594778
193.413493	49.329502	75.599783
192.311067	55.048318	75.604788
191.548955	48.808465	75.609793
190.911544	51.147852	75.614798
190.589019	46.714491	75.619802
190.257939	39.196402	75.624807
188.861372	61.039140	75.629812
188.681646	47.635382	75.634817
188.066561	58.136671	75.639822
187.157781	50.729602	75.644826
186.199983	53.413384	75.649831
185.301409	57.718293	75.654836
185.297812	51.496282	75.659841
184.821511	54.182146	75.664846
184.135374	53.864255	75.669850
183.340708	51.348048	75.674855
182.604785	53.647950	75.679860
182.317894	48.330546	75.684865
181.112912	52.810463	75.689870
180.376073	55.280823	75.694874
179.644550	53.407409	75.699879
179.293929	58.257316	75.704884
179.031455	46.814290	75.709889
177.749358	53.386503	75.714894
176.873463	45.633577	75.719898
176.497396	40.910713	75.724903
176.099424	54.565980	75.729908
176.198912	50.147339	75.734913
175.116389	50.608584	75.739918
174.119014	40.561641	75.744922
173.007575	41.661431	75.749927
171.788456	44.235493	75.754932
171.698049	46.115511	75.759937
171.155754	45.188064	75.764942
170.581668	45.528823	75.769946
170.264954	39.771479	75.774951
169.754738	48.258047	75.779956
168.729999	42.705051	75.784961
168.078558	30.672776	75.789966
167.690419	40.574900	75.794970
166.866862	37.549223	75.799975
165.810372	46.813591	75.804980
165.495241	39.907975	75.809985
165.086133	47.036438	75.814990
163.789126	40.607492	75.819994
163.130478	39.531442	75.824999
162.575725	46.422928	75.830004
162.649549	47.551365	75.835009
161.802332	43.394055	75.840014
160.417420	50.488868	75.845018
160.200917	44.736046	75.850023
159.420004	47.513059	75.855028
159.037532	42.696601	75.860033
157.716535	46.788171	75.865038
157.274227	47.483237	75.870042
156.781723	46.484776	75.875047
156.459726	46.313837	75.880052
156.032868	45.820572	75.885057
154.550527	43.891838	75.890062
154.101839	44.397111	75.895066
153.784172	47.546540	75.900071
152.721607	45.191332	75.905076
152.101569	46.167049	75.910081
151.630404	47.420227	75.915086
151.078695	42.367405	75.920090
150.462137	43.017715	75.925095
149.283144	50.510209	75.930100
148.847015	41.884510	75.935105
147.919571	48.351300	75.940110
147.462638	41.637031	75.945114
147.099857	42.824042	75.950119
146.182901	56.864837	75.955124
145.669255	41.068484	75.960129
145.226805	48.208573	75.965134
143.919046	50.959208	75.970138
143.650683	39.908219	75.975143
142.899507	52.072815	75.980148
142.607863	38.045102	75.985153
141.467986	45.605475	75.990158
140.443347	46.399704	75.995162
140.324402	49.596297	76.000167
139.658181	52.763459	76.005172
139.480095	44.383622	76.010177
138.495680	49.654709	76.015182
137.556260	49.695761	76.020186
137.278383	39.507306	76.025191
136.307443	36.725913	76.030196
135.558859	40.087556	76.035201
134.938958	50.848234	76.040206
134.616112	44.637711	76.045210
133.849119	42.590196	76.050215
132.730490	55.086199	76.055220
132.320091	40.873995	76.060225
131.944337	43.271021	76.065230
131.124749	44.434680	76.070234
130.642926	32.334372	76.075239
129.445969	45.096746	76.080244
129.079152	38.899546	76.085249
128.598310	45.064893	76.090254
127.607910	41.018738	76.095258
126.900327	42.789011	76.100263
125.946420	48.862636	76.105268
126.180590	40.210487	76.110273
125.445574	40.373491	76.115278
124.210917	48.634959	76.120282
123.688741	42.189719	76.125287
122.744909	44.136436	76.130292
122.571819	47.962981	76.135297
122.436278	49.184724	76.140302
121.105082	50.765856	76.145306
120.591235	39.123237	76.150311
119.869080	40.821719	76.155316
119.275864	39.634322	76.160321
117.981023	44.168017	76.165326
117.449711	44.200770	76.170330
117.194220	42.106391	76.175335
116.862135	42.558384	76.180340
115.990749	37.212773	76.185345
114.955621	45.557544	76.190350
114.489415	40.727641	76.195354
114.400485	31.792705	76.200359
113.314311	45.940905	76.205364
112.519369	35.842794	76.210369
111.880238	41.352141	76.215374
111.429748	36.168075	76.220378
110.652340	37.764983	76.225383
109.511872	44.161673	76.230388
109.201655	31.248688	76.235393
108.775969	37.842054	76.240398
108.280387	41.776793	76.245402
107.494818	39.729096	76.250407
106.693613	41.640459	76.255412
106.345694	41.448429	76.260417
104.639384	40.441688	76.265422
104.269701	43.626224	76.270426
104.029947	41.165061	76.275431
103.089561	39.334442	76.280436
103.037274	36.573727	76.285441
101.818236	37.517242	76.290446
101.177388	45.706104	76.295450
100.786893	37.262378	76.300455
100.245642	51.222766	76.305460
99.648525	43.742387	76.310465
98.775577	37.233244	76.315470
97.876983	39.983307	76.320474
97.765779	35.208763	76.325479
96.401907	49.661451	76.330484
95.778979	40.606664	76.335489
95.213413	44.563605	76.340494
94.545498	40.767236	76.345498
94.565651	41.741801	76.350503
93.493421	48.573895	76.355508
92.649647	46.030860	76.360513
91.978194	47.614032	76.365518
91.560442	45.969730	76.370522
90.954754	31.798153	76.375527
90.137296	43.681585	76.380532
89.415573	37.572529	76.385537
88.664577	38.816726	76.390542
87.620026	44.486926	76.395546
87.049764	44.508551	76.400551
86.657950	45.526736	76.405556
86.415963	41.563098	76.410561
86.108977	44.807025	76.415566
85.101173	36.767675	76.420570
84.382411	31.147006	76.425575
83.704970	40.631647	76.430580
82.536335	41.948756	76.435585
81.769436	41.443500	76.440590
80.981341	38.524162	76.445594
81.045839	35.211816	76.450599
80.359935	35.343348	76.455604
79.716149	32.104532	76.460609
78.974456	42.769517	76.465614
78.156310	39.771394	76.470618
77.243147	35.202014	76.475623
76.575543	43.404608	76.480628
75.872895	43.040495	76.485633
74.997695	35.244931	76.490638
74.288826	50.485725	76.495642
74.158513	38.925460	76.500647
73.527416	46.106678	76.505652
73.065147	42.930377	76.510657
72.634977	36.757486	76.515662
71.789426	40.806389	76.520666
71.234111	39.250262	76.525671
70.449004	45.464141	76.530676
70.014017	35.502610	76.535681
68.688915	37.272031	76.540686
68.114604	38.617366	76.545690
67.585224	32.321528	76.550695
67.011164	43.160055	76.555700
66.069774	40.777678	76.560705
65.647366	37.677024	76.565710
64.796180	40.463692	76.570714
64.472734	32.955455	76.575719
63.876082	37.346287	76.580724
63.097252	41.515440	76.585729
62.132985	40.537044	76.590734
62.069214	40.402205	76.595738
61.258571	39.758854	76.600743
60.451163	45.318704	76.605748
60.125588	41.053011	76.610753
59.224365	44.478442	76.615758
58.048918	46.572508	76.620762
57.645027	38.886287	76.625767
56.976173	44.196961	76.630772
57.191262	37.145306	76.635777
56.203739	49.270337	76.640782
55.434989	50.566261	76.645786
54.986364	40.378248	76.650791
53.460712	46.571466	76.655796
52.691146	39.260533	76.660801
52.627512	40.158574	76.665806
51.798590	46.332138	76.670810
51.049213	45.442476	76.675815
50.157324	53.314997	76.680820
49.808520	47.288402	76.685825
49.338170	45.382839	76.690830
48.437017	52.510941	76.695834
47.873704	39.791294	76.700839
47.128052	46.855170	76.705844
46.760944	45.142876	76.710849
46.023916	45.315686	76.715854
44.914249	51.499336	76.720858
44.456790	44.884524	76.725863
43.601643	52.643954	76.730868
43.648816	44.728100	76.735873
42.756557	40.906027	76.740878
41.717544	43.658005	76.745882
41.583333	34.354985	76.750887
40.499284	47.403736	76.755892
39.659794	47.507735	76.760897
39.284309	43.723090	76.765902
38.616970	50.575784	76.770906
38.534039	46.195700	76.775911
37.088829	50.393874	76.780916
36.099312	44.802207	76.785921
36.025387	36.643899	76.790926
35.381135	44.298728	76.795930
34.934095	41.676670	76.800935
33.607593	39.926584	76.805940
33.071823	42.287643	76.810945
32.733976	43.153726	76.815950
32.098914	46.771681	76.820954
31.418219	35.691869	76.825959
29.909198	45.449503	76.830964
29.174021	39.259037	76.835969
29.090817	41.467490	76.840974
28.263851	44.896857	76.845978
27.845013	42.733925	76.850983
27.715067	39.321705	76.855988
27.393641	36.288531	76.860993
26.379702	40.684426	76.865998
25.548567	40.593133	76.871002
24.669514	37.902788	76.876007
23.545309	42.956513	76.881012
23.278380	43.670938	76.886017
22.795856	41.858785	76.891022
22.461953	44.186072	76.896026
21.485803	38.232739	76.901031
20.606832	53.953258	76.906036
20.252268	49.373650	76.911041
19.533120	47.332734	76.916046
18.330083	42.442183	76.921050
17.700470	37.908026	76.926055
17.265039	44.908235	76.931060
16.812435	43.413009	76.936065
16.686481	43.830560	76.941070
15.682983	53.487075	76.946074
15.353839	38.768366	76.951079
14.334033	48.492135	76.956084
13.252508	48.185318	76.961089
12.815253	51.807997	76.966094
12.476845	41.272834	76.971098
12.075367	41.237593	76.976103
10.954785	45.891778	76.981108
10.154152	49.042563	76.986113
10.049871	48.685530	76.991118
8.473710	49.583552	76.996122
7.553788	32.557389	77.001127
6.705091	46.924785	77.006132
6.321875	45.133065	77.011137
5.949035	43.647196	77.016142
5.381752	49.544075	77.021147
5.381607	38.108141	77.026151
4.597842	41.637856	77.031156
3.410652	48.690169	77.036161