Fri Mar 05 19:44:17 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.068612	96.210503	0.000000
-0.588922	88.433845	0.005005
-1.221554	60.192296	0.010010
-2.624440	16.759947	0.015014
-6.750850	8.363376	0.020019
-11.387972	1.057521	0.025024
-16.655817	14.046607	0.030029
-21.204442	1.368203	0.035034
-24.906099	-1.385972	0.040038
-28.867724	6.583531	0.045043
-32.592756	9.987901	0.050048
-36.200250	5.542432	0.055053
-39.974206	9.437162	0.060058
-43.570389	4.177774	0.065062
-47.972567	16.241943	0.070067
-51.131422	7.992306	0.075072
-54.889417	-1.800188	0.080077
-58.846688	5.846970	0.085082
-62.340089	8.284038	0.090086
-66.096229	10.945951	0.095091
-69.590499	13.755327	0.100096
-73.475366	19.553826	0.105101
-77.460270	10.762648	0.110106
-81.405285	3.316558	0.115110
-85.484373	19.314180	0.120115
-88.462077	0.355070	0.125120
-92.441001	6.589642	0.130125
-96.554824	16.594136	0.135130
-100.171494	2.803696	0.140134
-103.979683	16.958835	0.145139
-107.771590	9.070469	0.150144
-111.355239	14.691659	0.155149
-114.841412	15.650055	0.160154
-118.602364	11.830008	0.165158
-122.509858	9.734869	0.170163
-126.240997	2.948586	0.175168
-130.548098	9.327042	0.180173
-134.524968	6.963874	0.185178
-137.526074	5.425881	0.190182
-141.421333	7.801025	0.195187
-145.032144	5.456737	0.200192
-148.646362	8.424134	0.205197
-152.772893	9.524183	0.210202
-156.467967	-2.596284	0.215206
-160.716869	3.277776	0.220211
-164.562945	9.734114	0.225216
-168.340905	12.883785	0.230221
-172.196589	15.763592	0.235226
-175.745474	15.659762	0.240230
-179.310733	12.193360	0.245235
-182.771404	-0.629938	0.250240
-186.588066	13.931940	0.255245
-190.294578	14.414676	0.260250
-194.065961	14.863615	0.265254
-198.122054	9.854474	0.270259
-201.415690	5.654061	0.275264
-205.563234	4.147718	0.280269
-209.411393	8.341549	0.285274
-212.722403	9.965985	0.290278
-216.742862	5.987240	0.295283
-220.469816	-0.665517	0.300288
-224.034126	9.789215	0.305293
-228.390049	5.099212	0.310298
-231.822403	0.542517	0.315302
-235.821974	22.403351	0.320307
-239.347853	13.402002	0.325312
-242.952067	10.020760	0.330317
-246.636160	10.916317	0.335322
-250.268983	1.963599	0.340326
-254.532995	18.049336	0.345331
-258.384513	9.798576	0.350336
-262.196363	12.975877	0.355341
-265.622441	15.003524	0.360346
-269.311061	8.950268	0.365350
-273.087905	16.157385	0.370355
-276.875034	10.816870	0.375360
-280.605744	7.501609	0.380365
-284.606204	12.019485	0.385370
-288.092504	5.300038	0.390374
-292.253814	9.081939	0.395379
-295.838721	19.226252	0.400384
-299.288561	14.293977	0.405389
-303.366094	20.825323	0.410394
-307.152836	6.373247	0.415398
-311.027467	19.478009	0.420403
-314.594562	20.621496	0.425408
-318.237993	15.816345	0.430413
-322.335230	23.571418	0.435418
-325.580569	19.748240	0.440422
-329.666608	19.490690	0.445427
-333.421233	10.399851	0.450432
-337.204821	10.923502	0.455437
-340.913592	13.841621	0.460442
-344.415513	17.059459	0.465446
-348.547123	11.728323	0.470451
-352.259438	10.660528	0.475456
-355.763024	11.940591	0.480461
-359.718437	16.815670	0.485466
-363.314904	10.361503	0.490470
-367.128464	13.338968	0.495475
-371.036686	8.697601	0.500480
-375.105192	9.825035	0.505485
-378.834104	10.453561	0.510490
-382.234261	8.522276	0.515494
-386.419597	6.492431	0.520499
-390.039459	5.860938	0.525504
-393.349373	12.678296	0.530509
-397.294314	2.167174	0.535514
-400.886756	7.149941	0.540518
-404.968474	3.883038	0.545523
-408.800513	2.273058	0.550528
-412.666464	10.429731	0.555533
-416.540738	10.475982	0.560538
-419.563454	3.443022	0.565542
-423.437901	7.747038	0.570547
-427.125004	6.088714	0.575552
-430.934438	-1.758462	0.580557
-435.182944	8.258611	0.585562
-438.873614	7.589614	0.590566
-442.700257	16.503296	0.595571
-446.168569	8.530707	0.600576
-449.846367	12.171012	0.605581
-454.102780	8.064775	0.610586
-457.422281	6.048180	0.615590
-461.160240	9.177720	0.620595
-465.159373	7.698592	0.625600
-468.826397	9.332921	0.630605
-472.542871	11.112346	0.635610
-476.057229	7.770731	0.640614
-480.303725	16.951789	0.645619
-483.877608	7.076987	0.650624
-487.627782	8.976933	0.655629
-491.566355	16.449899	0.660634
-495.139434	4.595935	0.665638
-499.263271	9.406671	0.670643
-503.092397	10.011972	0.675648
-506.169111	16.588811	0.680653
-510.169750	12.102784	0.685658
-513.870810	3.356930	0.690662
-517.457932	13.703748	0.695667
-521.344596	10.196161	0.700672
-525.025865	13.692056	0.705677
-529.174730	14.872007	0.710682
-532.752442	5.456785	0.715686
-536.683894	11.563058	0.720691
-540.461797	3.742566	0.725696
-544.144434	15.038222	0.730701
-547.846042	22.083927	0.735706
-551.488988	10.386288	0.740710
-555.427358	15.549114	0.745715
-559.080642	1.421514	0.750720
-562.481623	6.589974	0.755725
-566.474204	9.692538	0.760730
-570.365313	4.080539	0.765734
-574.361601	9.482877	0.770739
-578.064474	9.923053	0.775744
-581.940671	6.789206	0.780749
-586.163259	8.263304	0.785754
-589.164725	4.426774	0.790758
-592.947253	10.827887	0.795763
-596.486725	3.803598	0.800768
-600.437075	-2.734004	0.805773
-604.315086	6.478276	0.810778
-607.710274	-1.482085	0.815782
-611.803691	4.336369	0.820787
-615.389451	5.640975	0.825792
-619.408922	7.765494	0.830797
-623.378744	13.378147	0.835802
-626.672551	4.707765	0.840806
-630.972247	14.783809	0.845811
-634.526417	7.058615	0.850816
-637.914938	4.912956	0.855821
-641.776836	11.027206	0.860826
-645.778846	18.597282	0.865830
-649.456096	12.730476	0.870835
-653.374898	9.896864	0.875840
-656.872842	13.590746	0.880845
-660.820255	18.873456	0.885850
-664.044444	6.741677	0.890854
-668.179073	17.579879	0.895859
-671.995133	7.116456	0.900864
-675.765477	4.828435	0.905869
-679.437218	9.070505	0.910874
-683.441566	4.766721	0.915878
-687.085534	8.953904	0.920883
-690.880225	13.559409	0.925888
-694.415951	9.803651	0.930893
-698.324813	11.131625	0.935898
-701.881186	-1.498937	0.940902
-706.229248	15.723726	0.945907
-709.580772	17.984512	0.950912
-713.095544	12.681618	0.955917
-716.916299	12.560536	0.960922
-720.644276	6.908532	0.965926
-724.461777	9.551301	0.970931
-728.173550	7.875315	0.975936
-732.430762	10.149977	0.980941
-736.313030	14.600816	0.985946
-739.698445	6.867744	0.990950
-743.823640	8.280825	0.995955
-747.093216	9.207099	1.000960
-750.556027	7.619094	1.005965
-754.802636	7.200282	1.010970
-758.573399	7.965397	1.015974
-762.482494	10.124555	1.020979
-765.700456	5.875007	1.025984
-769.463942	8.353099	1.030989
-773.569685	11.142936	1.035994
-777.037736	-2.266428	1.040998
-781.066736	7.161064	1.046003
-785.045626	7.030674	1.051008
-788.736657	3.517502	1.056013
-792.754208	15.756428	1.061018
-796.029740	1.846396	1.066022
-799.775782	9.863075	1.071027
-803.592902	6.882580	1.076032
-807.483472	2.636520	1.081037
-811.388343	14.111578	1.086042
-814.918171	-0.948358	1.091046
-818.994456	2.275233	1.096051
-822.367977	0.628909	1.101056
-826.164564	5.528234	1.106061
-830.107091	12.433093	1.111066
-833.435143	6.034538	1.116070
-837.480112	6.793148	1.121075
-841.182711	12.052784	1.126080
-844.966522	7.005988	1.131085
-849.048695	9.560378	1.136090
-852.399152	17.029787	1.141094
-856.176999	12.018324	1.146099
-859.967821	2.339660	1.151104
-863.654281	9.842294	1.156109
-867.689857	14.948621	1.161114
-871.110496	13.142745	1.166118
-874.869624	16.115462	1.171123
-878.845997	11.649852	1.176128
-882.767389	11.010549	1.181133
-886.599592	17.459477	1.186138
-890.133221	8.837287	1.191142
-893.827948	5.681259	1.196147
-898.067718	9.380547	1.201152
-901.587296	10.555156	1.206157
-905.386316	12.875143	1.211162
-908.699540	11.444804	1.216166
-912.520298	7.843762	1.221171
-916.410974	2.617056	1.226176
-919.833893	5.003087	1.231181
-924.076826	14.791442	1.236186
-927.849239	9.630999	1.241190
-931.461090	7.404783	1.246195
-935.229769	14.053361	1.251200
-939.402506	7.603941	1.256205
-942.791467	14.545049	1.261210
-946.356553	3.296091	1.266214
-950.390742	7.777870	1.271219
-954.265891	2.794747	1.276224
-957.592687	5.479271	1.281229
-961.785893	12.788694	1.286234
-965.088817	12.640407	1.291238
-969.210403	10.927835	1.296243
-972.669626	4.370694	1.301248
-976.201333	4.989122	1.306253
-980.814320	5.627499	1.311258
-984.153012	6.576191	1.316262
-988.190178	2.685036	1.321267
-991.597015	4.399982	1.326272
-995.188022	-2.219624	1.331277
-999.461761	6.624471	1.336282
-1003.004689	8.236621	1.341286
-1006.881857	0.156831	1.346291
-1010.409504	5.839743	1.351296
-1014.137216	0.408953	1.356301
-1018.115359	17.391630	1.361306
-1022.031198	9.882585	1.366310
-1025.530891	4.421653	1.371315
-1029.449254	8.421425	1.376320
-1032.714855	4.511030	1.381325
-1036.705983	11.461839	1.386330
-1040.689469	5.799189	1.391334
-1044.626976	18.716406	1.396339
-1048.377692	8.069725	1.401344
-1051.749644	2.156327	1.406349
-1055.723922	12.602090	1.411354
-1059.350050	-0.444071	1.416358
-1063.307700	12.067967	1.421363
-1067.028132	13.839488	1.426368
-1070.130732	13.858001	1.431373
-1074.591809	20.546580	1.436378
-1078.052688	8.587321	1.441382
-1082.104259	9.002060	1.446387
-1086.174196	10.542515	1.451392
-1089.646554	17.673780	1.456397
-1093.390740	17.477987	1.461402
-1096.650777	8.836019	1.466406
-1100.571173	10.658502	1.471411
-1104.449111	7.008581	1.476416
-1108.498866	8.386577	1.481421
-1112.415713	17.605861	1.486426
-1116.007219	11.995755	1.491430
-1119.475824	15.892191	1.496435
-1123.394687	14.008695	1.501440
-1127.018391	5.096951	1.506445
-1130.731808	13.719181	1.511450
-1134.336982	7.601946	1.516454
-1138.542813	23.249313	1.521459
-1142.267772	10.758401	1.526464
-1146.123620	6.113134	1.531469
-1149.520986	2.294949	1.536474
-1152.856742	5.468448	1.541478
-1156.911106	8.826302	1.546483
-1161.274530	15.111493	1.551488
-1164.957435	15.669242	1.556493
-1168.807727	13.421622	1.561498
-1172.143136	9.502096	1.566502
-1175.845780	3.791600	1.571507
-1179.495648	12.351697	1.576512
-1183.523128	10.469913	1.581517
-1187.697003	20.468441	1.586522
-1191.197058	7.783941	1.591526
-1194.817705	6.940931	1.596531
-1198.431784	8.517450	1.601536
-1202.362770	5.476993	1.606541
-1206.057669	19.902602	1.611546
-1209.577219	4.545217	1.616550
-1213.521286	10.854862	1.621555
-1217.374526	6.754915	1.626560
-1220.982934	5.596180	1.631565
-1224.912305	9.716302	1.636570
-1228.587229	11.964911	1.641574
-1232.381285	4.368946	1.646579
-1236.310171	9.509278	1.651584
-1239.765295	7.714199	1.656589
-1243.974619	4.615853	1.661594
-1247.470025	8.001109	1.666598
-1251.152552	3.222634	1.671603
-1254.892722	12.685099	1.676608
-1258.677253	11.385876	1.681613
-1262.679145	6.283218	1.686618
-1266.058937	9.862885	1.691622
-1269.950026	4.485471	1.696627
-1273.914695	14.330815	1.701632
-1277.764134	10.914745	1.706637
-1281.535987	15.856560	1.711642
-1285.097122	12.977823	1.716646
-1288.772852	10.544778	1.721651
-1292.638370	12.645798	1.726656
-1296.012993	5.941583	1.731661
-1299.969446	17.998074	1.736666
-1303.688395	7.252138	1.741670
-1307.727231	4.139240	1.746675
-1311.700877	12.289315	1.751680
-1315.368037	10.246017	1.756685
-1318.974670	17.949443	1.761690
-1322.688478	2.702189	1.766694
-1326.311408	4.904782	1.771699
-1330.291966	8.547580	1.776704
-1333.862650	13.676471	1.781709
-1337.833790	14.391012	1.786714
-1341.520367	5.092304	1.791718
-1345.019153	10.356356	1.796723
-1348.807899	19.527127	1.801728
-1352.804798	9.961147	1.806733
-1356.626705	16.049628	1.811738
-1360.451206	5.503610	1.816742
-1363.945999	7.952249	1.821747
-1368.212165	20.384849	1.826752
-1371.592140	7.772888	1.831757
-1375.541498	18.757636	1.836762
-1379.104354	11.522294	1.841766
-1382.682685	7.151546	1.846771
-1386.741532	12.571544	1.851776
-1390.253919	6.189142	1.856781
-1394.332909	15.666636	1.861786
-1397.791612	14.857943	1.866790
-1401.542144	12.432324	1.871795
-1405.583425	10.450641	1.876800
-1408.788643	-2.009460	1.881805
-1413.211933	12.990356	1.886810
-1416.880723	3.253700	1.891814
-1420.275773	4.491152	1.896819
-1424.628301	12.872376	1.901824
-1428.140790	10.686229	1.906829
-1431.908077	14.288747	1.911834
-1435.265831	9.619422	1.916838
-1439.085924	6.990542	1.921843
-1442.911735	10.763293	1.926848
-1446.540700	6.615215	1.931853
-1450.564124	10.244580	1.936858
-1454.281895	10.545025	1.941862
-1458.068339	10.227281	1.946867
-1462.081720	19.921462	1.951872
-1465.503672	5.256919	1.956877
-1469.433121	11.252414	1.961882
-1473.497254	15.509643	1.966886
-1476.855993	12.799069	1.971891
-1480.773464	17.028096	1.976896
-1484.131051	16.523457	1.981901
-1488.505883	14.511754	1.986906
-1491.908832	13.585468	1.991910
-1495.558956	11.957616	1.996915
-1499.692053	16.386107	2.006912
-1500.372478	7.916853	2.016909
-1498.255842	11.389613	2.026906
-1495.553128	12.799594	2.036902
-1492.831387	4.995020	2.046899
-1490.813501	6.966242	2.056896
-1489.592851	3.955689	2.066893
-1487.562730	10.655446	2.076890
-1485.229414	4.656223	2.086886
-1483.674166	8.523623	2.096883
-1481.845381	12.891959	2.106880
-1479.760458	9.970386	2.116877
-1477.899933	6.606329	2.126874
-1475.892807	8.159291	2.136870
-1474.080003	7.622858	2.146867
-1472.109812	2.987572	2.156864
-1470.031421	10.206981	2.166861
-1468.502985	9.826610	2.176858
-1466.619331	14.388277	2.186854
-1464.830120	7.083571	2.196851
-1462.751319	6.540872	2.206848
-1460.971977	6.947695	2.216845
-1459.104861	8.665193	2.226842
-1457.223671	6.189943	2.236838
-1454.991597	6.745334	2.246835
-1453.079142	13.140283	2.256832
-1451.470106	6.911269	2.266829
-1449.621777	1.908673	2.276826
-1447.807870	6.377311	2.286822
-1445.666828	12.055146	2.296819
-1443.938273	1.886503	2.306816
-1441.924974	7.115849	2.316813
-1440.180456	5.797749	2.326810
-1438.117313	0.298141	2.336806
-1436.615771	8.290459	2.346803
-1434.725333	6.961633	2.356800
-1432.288030	7.261558	2.366797
-1430.593390	7.246179	2.376794
-1428.818306	3.805841	2.386790
-1427.060426	0.830887	2.396787
-1424.921613	0.654401	2.406784
-1423.432061	6.297612	2.416781
-1421.584632	5.722519	2.426778
-1419.437901	8.341068	2.436774
-1417.143515	3.409188	2.446771
-1415.607637	6.157114	2.456768
-1413.958520	3.415895	2.466765
-1412.122097	8.738322	2.476762
-1410.206276	7.358084	2.486758
-1407.930276	9.780687	2.496755
-1406.160249	9.601679	2.506752
-1404.373289	8.224707	2.516749
-1402.772512	13.008556	2.526746
-1400.447165	10.471718	2.536742
-1398.979896	6.354367	2.546739
-1396.900921	1.089100	2.556736
-1394.919912	1.428953	2.566733
-1393.177708	7.045950	2.576730
-1391.287996	0.475205	2.586726
-1389.334594	2.475787	2.596723
-1387.540999	8.506139	2.606720
-1385.748613	4.193067	2.616717
-1383.791692	13.205155	2.626714
-1381.674033	9.552116	2.636710
-1379.822700	3.988567	2.646707
-1378.101061	3.217331	2.656704
-1376.463714	11.724795	2.666701
-1374.236922	2.908536	2.676698
-1372.366654	-0.644891	2.686694
-1370.623935	14.436196	2.696691
-1368.594379	6.581507	2.706688
-1366.977182	5.497000	2.716685
-1365.033892	9.952892	2.726682
-1363.144931	6.379110	2.736678
-1361.162076	8.389214	2.746675
-1359.145404	5.627092	2.756672
-1357.602616	6.303965	2.766669
-1355.694175	8.809140	2.776666
-1353.617618	7.065326	2.786662
-1351.741705	8.858873	2.796659
-1349.954870	11.282466	2.806656
-1348.493754	11.266633	2.816653
-1346.133605	5.159036	2.826650
-1344.053633	11.917267	2.836646
-1342.503967	9.782538	2.846643
-1340.661426	12.299854	2.856640
-1338.722268	13.855922	2.866637
-1336.764337	10.226910	2.876634
-1334.792759	12.846734	2.886630
-1332.922237	4.905424	2.896627
-1331.124441	7.008332	2.906624
-1329.432043	8.782324	2.916621
-1327.445747	8.824549	2.926618
-1325.429304	8.446690	2.936614
-1323.988258	11.165648	2.946611
-1321.609339	4.191391	2.956608
-1319.726363	5.780151	2.966605
-1318.104049	6.442743	2.976602
-1316.451046	-0.259008	2.986598
-1314.180590	9.459273	2.996595
-1312.245085	8.611224	3.006592
-1310.459682	7.940357	3.016589
-1308.524972	9.606110	3.026586
-1306.828159	5.148919	3.036582
-1305.092980	1.257166	3.046579
-1302.886958	5.033171	3.056576
-1301.072913	2.717211	3.066573
-1299.161533	2.062507	3.076570
-1297.475458	4.287531	3.086566
-1295.257010	8.994710	3.096563
-1293.787261	2.966509	3.106560
-1292.006119	14.034173	3.116557
-1290.042469	6.499566	3.126554
-1287.953314	12.965858	3.136550
-1285.843495	8.954159	3.146547
-1284.026416	7.299301	3.156544
-1282.300785	11.011684	3.166541
-1280.737765	9.345383	3.176538
-1278.336224	13.326966	3.186534
-1276.767503	14.097637	3.196531
-1274.859299	9.031903	3.206528
-1273.022135	10.187510	3.216525
-1271.101307	10.527628	3.226522
-1269.308146	13.649744	3.236518
-1267.512860	7.477881	3.246515
-1265.575036	9.086330	3.256512
-1263.666065	11.668867	3.266509
-1261.713293	9.055999	3.276506
-1259.608668	9.906711	3.286502
-1257.711732	12.522758	3.296499
-1255.964279	6.942766	3.306496
-1254.410153	10.685774	3.316493
-1252.394779	13.687082	3.326490
-1250.332011	8.503475	3.336486
-1248.802677	5.899958	3.346483
-1246.769530	10.229472	3.356480
-1244.853400	9.730367	3.366477
-1243.017775	11.430979	3.376474
-1241.099194	13.418316	3.386470
-1239.095552	5.171563	3.396467
-1237.235067	10.903971	3.406464
-1235.503585	12.831253	3.416461
-1233.480438	10.623987	3.426458
-1231.909525	7.691724	3.436454
-1229.630422	12.722420	3.446451
-1227.790105	11.316517	3.456448
-1226.062403	11.828101	3.466445
-1224.140719	14.392849	3.476442
-1222.655879	13.646985	3.486438
-1220.356793	5.774549	3.496435
-1218.705031	15.107200	3.506432
-1216.567508	7.549564	3.516429
-1214.801696	8.028216	3.526426
-1212.906589	14.430894	3.536422
-1211.103820	4.241049	3.546419
-1209.131669	11.401924	3.556416
-1207.370640	10.722405	3.566413
-1205.408080	11.711160	3.576410
-1203.619242	8.114048	3.586406
-1201.649336	9.066895	3.596403
-1199.712849	13.001394	3.606400
-1197.651470	8.770155	3.616397
-1196.176896	2.030714	3.626394
-1194.080395	5.827509	3.636390
-1192.418315	7.385402	3.646387
-1190.137579	1.230662	3.656384
-1188.449683	6.562832	3.666381
-1186.795228	5.107751	3.676378
-1184.662240	7.676618	3.686374
-1182.727293	-0.341204	3.696371
-1181.120985	8.877168	3.706368
-1179.101722	4.079528	3.716365
-1177.274368	8.742030	3.726362
-1175.393740	7.348665	3.736358
-1173.647134	12.103038	3.746355
-1171.735202	6.177842	3.756352
-1169.811984	6.438715	3.766349
-1168.005025	6.726083	3.776346
-1166.157462	9.149581	3.786342
-1164.046624	7.877289	3.796339
-1162.045992	13.366290	3.806336
-1160.306205	9.154953	3.816333
-1158.426213	15.222205	3.826330
-1156.707457	8.693191	3.836326
-1154.878933	2.280829	3.846323
-1152.832790	12.444119	3.856320
-1151.016993	11.942195	3.866317
-1149.077027	11.772512	3.876314
-1147.129539	7.594272	3.886310
-1145.245383	7.646678	3.896307
-1143.403080	3.854742	3.906304
-1141.813329	5.877399	3.916301
-1140.052432	12.926873	3.926298
-1137.685824	11.462109	3.936294
-1135.681783	3.848528	3.946291
-1134.002236	0.898949	3.956288
-1132.382322	11.240970	3.966285
-1130.418411	7.038011	3.976282
-1128.221238	4.348260	3.986278
-1126.547129	2.444816	3.996275
-1124.798116	4.568324	4.006272
-1122.995322	-0.106220	4.016269
-1120.810124	8.198545	4.026266
-1118.801734	6.633209	4.036262
-1117.036301	3.620956	4.046259
-1115.927973	4.905909	4.056256
-1113.590397	8.942111	4.066253
-1111.721569	3.595435	4.076250
-1109.684902	4.689259	4.086246
-1107.624134	6.033439	4.096243
-1105.916162	7.086688	4.106240
-1104.056633	8.654114	4.116237
-1102.178273	9.883794	4.126234
-1100.409983	11.459503	4.136230
-1098.497965	4.615405	4.146227
-1096.322928	10.591303	4.156224
-1094.612512	14.290479	4.166221
-1092.801956	10.742078	4.176218
-1091.004845	8.016880	4.186214
-1089.222913	12.415144	4.196211
-1087.663122	4.542660	4.206208
-1084.851427	7.149902	4.216205
-1083.272775	5.058072	4.226202
-1081.693716	9.724054	4.236198
-1079.869226	12.272892	4.246195
-1077.653679	5.097629	4.256192
-1075.870105	13.411420	4.266189
-1074.026327	8.899301	4.276186
-1072.268037	-0.718074	4.286182
-1070.138812	4.335179	4.296179
-1068.382488	6.347035	4.306176
-1066.715515	10.320021	4.316173
-1065.038530	8.951420	4.326170
-1062.637884	8.220232	4.336166
-1060.875853	0.517524	4.346163
-1059.219843	0.434385	4.356160
-1057.077937	11.092451	4.366157
-1055.159822	9.459502	4.376154
-1053.292132	1.005690	4.386150
-1051.551153	2.127910	4.396147
-1049.548085	1.701902	4.406144
-1047.700291	2.699673	4.416141
-1045.985080	3.794440	4.426138
-1043.946911	4.199663	4.436134
-1041.921578	3.283786	4.446131
-1040.798621	6.656957	4.456128
-1038.681112	6.989496	4.466125
-1036.628538	5.339794	4.476122
-1034.110390	2.508796	4.486118
-1032.741553	0.846871	4.496115
-1031.068801	6.566849	4.506112
-1029.170859	6.694511	4.516109
-1027.139955	12.388795	4.526106
-1025.320382	1.522177	4.536102
-1023.048765	0.227456	4.546099
-1021.308412	2.920847	4.556096
-1019.862847	7.691907	4.566093
-1017.859122	4.572142	4.576090
-1015.701846	6.467812	4.586086
-1014.229963	-0.368991	4.596083
-1012.304198	5.751063	4.606080
-1010.474610	2.076524	4.616077
-1008.129452	11.020561	4.626074
-1006.379339	4.134529	4.636070
-1004.451768	8.921674	4.646067
-1002.890701	10.473755	4.656064
-1000.659058	2.973881	4.666061
-999.086213	12.475644	4.676058
-997.098520	8.412672	4.686054
-995.336848	3.839532	4.696051
-993.279976	4.079177	4.706048
-991.432445	7.930188	4.716045
-989.665118	10.832449	4.726042
-987.975958	4.794596	4.736038
-986.135897	0.477348	4.746035
-983.986873	2.208578	4.756032
-982.004146	3.573245	4.766029
-980.050082	1.855661	4.776026
-978.238346	1.419257	4.786022
-976.275993	5.608760	4.796019
-974.818172	10.958943	4.806016
-972.904210	5.229362	4.816013
-970.771777	10.376937	4.826010
-968.968585	7.156646	4.836006
-967.136147	8.674832	4.846003
-965.381684	10.745487	4.856000
-963.277558	13.634968	4.865997
-961.594438	16.048613	4.875994
-959.492082	15.586279	4.885990
-957.821889	11.927789	4.895987
-955.953925	10.102412	4.905984
-953.766784	11.214946	4.915981
-952.148524	5.475820	4.925978
-949.949978	7.788111	4.935974
-948.537621	5.271380	4.945971
-946.327368	5.871805	4.955968
-944.437525	6.687672	4.965965
-942.704647	13.744949	4.975962
-940.969894	13.093513	4.985958
-939.010285	7.596658	4.995955
-936.943993	9.636424	5.005952
-935.542958	7.331511	5.015949
-933.325260	11.696543	5.025946
-931.367127	8.610980	5.035942
-929.522764	6.356767	5.045939
-927.690599	7.914501	5.055936
-925.716208	2.388453	5.065933
-923.904159	7.541507	5.075930
-922.205528	12.974803	5.085926
-919.995939	5.461155	5.095923
-918.231950	5.103483	5.105920
-916.528279	3.015459	5.115917
-914.402887	0.637379	5.125914
-912.668586	3.699716	5.135910
-910.798506	7.015084	5.145907
-909.221425	5.643619	5.155904
-907.072469	10.651245	5.165901
-905.053283	7.608048	5.175898
-903.399579	9.161176	5.185894
-901.571461	3.928531	5.195891
-899.487300	8.002313	5.205888
-897.774143	5.401206	5.215885
-895.635347	7.702575	5.225882
-893.958240	4.630392	5.235878
-892.027925	6.592463	5.245875
-890.013449	0.008456	5.255872
-888.402483	5.304212	5.265869
-886.132931	3.447847	5.275866
-884.726300	5.762065	5.285862
-882.756067	3.852502	5.295859
-880.806331	6.070424	5.305856
-879.052671	8.689168	5.315853
-876.989673	3.690571	5.325850
-875.113653	9.826597	5.335846
-873.272113	10.615508	5.345843
-871.163547	5.382262	5.355840
-869.608192	10.683766	5.365837
-867.736139	10.732014	5.375834
-865.677891	4.619448	5.385830
-863.761480	2.536926	5.395827
-861.887993	6.672842	5.405824
-860.377658	5.550499	5.415821
-858.571633	5.282468	5.425818
-856.455130	6.782174	5.435814
-854.450420	2.343965	5.445811
-852.571527	3.398500	5.455808
-850.766994	5.557554	5.465805
-848.963056	6.202495	5.475802
-846.924959	6.544743	5.485798
-844.984364	3.809422	5.495795
-843.359024	9.031863	5.505792
-841.449228	1.529890	5.515789
-839.419431	6.041892	5.525786
-837.606338	4.094326	5.535782
-835.548852	3.541380	5.545779
-833.901768	0.529301	5.555776
-832.221731	1.590375	5.565773
-830.277063	7.739150	5.575770
-828.236185	12.899918	5.585766
-826.060712	4.311804	5.595763
-824.510381	5.783617	5.605760
-822.876291	6.725727	5.615757
-820.708540	7.519379	5.625754
-818.586872	7.039873	5.635750
-816.939284	-0.088590	5.645747
-815.189317	8.213424	5.655744
-813.293138	8.477333	5.665741
-811.420510	6.436586	5.675738
-809.342000	-2.030223	5.685734
-807.626061	5.233551	5.695731
-805.662954	6.086768	5.705728
-804.148835	1.453856	5.715725
-802.050916	-0.663945	5.725722
-800.113944	8.017140	5.735718
-798.035478	-0.107023	5.745715
-796.334261	5.150693	5.755712
-794.443098	9.752789	5.765709
-792.551238	5.978456	5.775706
-790.752386	4.516359	5.785702
-788.858524	3.926447	5.795699
-786.934918	11.073366	5.805696
-785.114097	3.438811	5.815693
-783.335491	13.176278	5.825690
-781.325965	10.519990	5.835686
-779.090894	2.400811	5.845683
-777.732464	5.886484	5.855680
-776.166329	6.378435	5.865677
-773.759389	4.279165	5.875674
-771.785559	5.617013	5.885670
-770.040718	-3.156437	5.895667
-768.328121	1.370006	5.905664
-766.197301	4.279085	5.915661
-764.520743	8.261820	5.925658
-762.513228	5.411658	5.935654
-760.732164	3.306637	5.945651
-758.930651	0.936243	5.955648
-756.778473	-4.962295	5.965645
-755.029205	-1.728545	5.975642
-753.242755	4.115583	5.985638
-751.469064	3.555958	5.995635
-749.541388	7.833309	6.005632
-747.503716	3.828866	6.015629
-745.676012	11.150621	6.025626
-743.820680	3.654264	6.035622
-741.690533	-0.398109	6.045619
-740.021534	3.243218	6.055616
-738.310467	0.869926	6.065613
-736.484199	1.972437	6.075610
-734.426973	3.020674	6.085606
-732.468015	0.794088	6.095603
-730.600268	1.779449	6.105600
-728.737937	2.418309	6.115597
-727.067521	6.621526	6.125594
-725.132949	2.227788	6.135590
-723.213002	1.622707	6.145587
-721.250642	-1.818625	6.155584
-719.402775	-1.160079	6.165581
-717.327958	0.654310	6.175578
-715.390158	0.183751	6.185574
-713.739700	4.192799	6.195571
-712.052046	2.214845	6.205568
-710.168214	1.372387	6.215565
-708.351481	5.244343	6.225562
-706.370743	3.762718	6.235558
-704.168837	7.328393	6.245555
-702.441916	0.065744	6.255552
-700.665724	1.679970	6.265549
-698.976468	7.353358	6.275546
-696.991978	4.086929	6.285542
-695.144854	2.711927	6.295539
-692.921802	3.995809	6.305536
-691.250912	4.494762	6.315533
-689.528333	6.526512	6.325530
-687.334360	5.353464	6.335526
-685.548105	6.767147	6.345523
-683.842068	8.188912	6.355520
-681.973955	8.451095	6.365517
-680.032261	7.790469	6.375514
-678.232800	8.998363	6.385510
-676.242057	1.649366	6.395507
-674.336740	7.111408	6.405504
-672.740554	6.946520	6.415501
-670.659966	13.427407	6.425498
-668.692357	3.233685	6.435494
-666.739927	1.344510	6.445491
-664.869112	4.025226	6.455488
-663.211574	5.650545	6.465485
-661.451722	7.040044	6.475482
-659.074307	3.764550	6.485478
-657.374603	3.025763	6.495475
-655.452708	8.354121	6.505472
-654.028338	8.470908	6.515469
-651.861763	5.497528	6.525466
-650.019018	10.497484	6.535462
-647.860146	3.326910	6.545459
-646.390328	3.496439	6.555456
-644.711472	2.658361	6.565453
-642.924432	8.684066	6.575450
-640.301495	14.726228	6.585446
-638.386418	6.198817	6.595443
-636.990037	7.237455	6.605440
-634.964471	7.046625	6.615437
-633.087272	4.432126	6.625434
-631.180075	4.318631	6.635430
-629.462191	-1.300418	6.645427
-627.560187	2.848506	6.655424
-625.628222	8.328439	6.665421
-623.728827	7.916196	6.675418
-621.613537	1.093660	6.685414
-619.738532	2.093740	6.695411
-618.288623	3.422260	6.705408
-616.326619	1.686333	6.715405
-614.287851	2.865520	6.725402
-612.480215	2.891103	6.735398
-610.672574	1.718263	6.745395
-608.537523	4.593656	6.755392
-607.026623	0.940323	6.765389
-605.004972	0.012773	6.775386
-602.949140	2.637141	6.785382
-601.139262	3.191323	6.795379
-599.244109	-2.542866	6.805376
-597.722414	7.101587	6.815373
-595.583270	9.011599	6.825370
-593.677474	2.020446	6.835366
-591.811554	5.106215	6.845363
-589.924251	6.555935	6.855360
-588.099679	9.697261	6.865357
-586.421066	9.133999	6.875354
-584.044173	7.492876	6.885350
-582.336304	6.923365	6.895347
-580.414153	1.252770	6.905344
-579.016128	4.429081	6.915341
-576.825955	11.830449	6.925338
-574.841996	6.041036	6.935334
-573.050026	7.278629	6.945331
-571.172562	5.609927	6.955328
-569.248724	7.464355	6.965325
-567.371052	6.793521	6.975322
-565.807752	4.358687	6.985318
-563.670941	1.991721	6.995315
-561.862436	4.219841	7.005312
-559.941499	-0.384751	7.015309
-558.125038	-1.528960	7.025306
-556.161048	-1.217255	7.035302
-554.549560	0.979182	7.045299
-552.258424	-0.150842	7.055296
-550.542953	-1.774705	7.065293
-548.838258	1.898957	7.075290
-546.748784	2.834839	7.085286
-544.745734	-1.688119	7.095283
-542.955574	-2.000746	7.105280
-541.131967	2.367616	7.115277
-539.317582	-0.151515	7.125274
-537.573023	-2.563175	7.135270
-535.669396	-1.302336	7.145267
-533.635234	8.764000	7.155264
-531.895959	5.866869	7.165261
-529.987832	4.123827	7.175258
-527.848310	8.370691	7.185254
-526.136978	2.436965	7.195251
-524.489099	2.925501	7.205248
-522.455069	8.536065	7.215245
-520.485655	5.128500	7.225242
-518.520401	3.150553	7.235238
-516.506623	1.469596	7.245235
-514.906909	2.572148	7.255232
-512.978120	-1.822083	7.265229
-511.354694	-0.922263	7.275226
-509.558870	-0.517346	7.285222
-507.611783	-0.543955	7.295219
-505.222766	-7.320109	7.305216
-503.568599	-4.895189	7.315213
-501.775329	-0.458794	7.325210
-499.769080	-1.409058	7.335206
-498.075555	-3.173064	7.345203
-496.202194	-5.605265	7.355200
-494.044986	3.426187	7.365197
-492.302059	1.940085	7.375194
-490.637577	2.512836	7.385190
-488.529337	5.937360	7.395187
-486.873466	-2.507490	7.405184
-485.168535	6.984625	7.415181
-482.929078	2.362380	7.425178
-481.113681	4.448937	7.435174
-478.944878	1.210090	7.445171
-477.358391	-1.552075	7.455168
-475.745559	1.307362	7.465165
-473.457580	-0.330505	7.475162
-471.856513	10.588215	7.485158
-469.780979	0.064768	7.495155
-468.008814	1.507709	7.505152
-466.123269	4.636237	7.515149
-464.162595	5.910130	7.525146
-462.352244	4.965916	7.535142
-460.431351	3.863524	7.545139
-458.372975	6.078667	7.555136
-456.786753	1.634970	7.565133
-454.963912	4.061412	7.575130
-452.947148	5.485833	7.585126
-451.460920	-3.587173	7.595123
-449.111116	-2.302774	7.605120
-447.232281	1.562632	7.615117
-445.681032	1.101912	7.625114
-443.588971	6.760124	7.635110
-441.494393	1.273678	7.645107
-439.719280	4.980391	7.655104
-438.413653	4.025210	7.665101
-435.947072	4.665710	7.675098
-434.044123	0.577244	7.685094
-432.116435	2.110643	7.695091
-430.363230	2.291898	7.705088
-428.758439	-0.245790	7.715085
-426.784925	-0.355501	7.725082
-424.934476	5.167622	7.735078
-423.053396	0.004232	7.745075
-421.207253	3.518036	7.755072
-419.359377	4.445240	7.765069
-417.074606	7.923749	7.775066
-415.427394	2.882968	7.785062
-413.688424	0.358603	7.795059
-411.675132	1.849928	7.805056
-409.807995	0.869845	7.815053
-408.042954	6.949780	7.825050
-406.038628	7.389380	7.835046
-404.353713	2.041006	7.845043
-402.218183	4.367037	7.855040
-400.580242	7.501995	7.865037
-398.455569	2.988153	7.875034
-396.495436	1.688493	7.885030
-394.901194	7.143600	7.895027
-393.144257	4.883223	7.905024
-390.878572	-0.183656	7.915021
-389.292239	-1.103101	7.925018
-387.314990	1.409268	7.935014
-385.315859	0.351287	7.945011
-383.466266	-0.558081	7.955008
-381.563360	3.950909	7.965005
-379.805338	0.316677	7.975002
-378.133626	3.169942	7.984998
-376.326510	-2.158449	7.994995
-374.099770	-1.939069	8.004992
-372.334592	3.427184	8.014989
-370.485124	1.752053	8.024986
-368.533019	-3.987902	8.034982
-366.537698	-1.303138	8.044979
-364.675845	0.536091	8.054976
-362.915525	2.377321	8.064973
-361.218579	0.560757	8.074970
-359.229148	2.488570	8.084966
-357.068726	1.447494	8.094963
-355.404560	-1.061731	8.104960
-353.486872	1.363860	8.114957
-351.562220	1.896751	8.124954
-349.938935	-2.585953	8.134950
-347.922332	-2.171949	8.144947
-346.168068	3.027119	8.154944
-344.240948	-0.016712	8.164941
-342.288554	7.936008	8.174938
-340.449315	1.465665	8.184934
-338.171782	5.673306	8.194931
-336.489417	-4.349902	8.204928
-334.892927	1.262783	8.214925
-333.043116	3.555541	8.224922
-331.207068	4.577860	8.234918
-328.950612	11.409944	8.244915
-327.205112	8.106169	8.254912
-325.242580	6.007231	8.264909
-323.442735	5.402694	8.274906
-321.840719	10.270822	8.284902
-320.033198	11.651390	8.294899
-317.838674	4.244868	8.304896
-316.077453	5.665987	8.314893
-314.238811	4.346313	8.324890
-312.038179	5.070447	8.334886
-310.390971	8.177148	8.344883
-308.369675	8.552542	8.354880
-306.567689	8.746628	8.364877
-304.650566	13.103415	8.374874
-303.022702	6.249992	8.384870
-300.983369	10.257272	8.394867
-298.889077	4.936777	8.404864
-297.520461	10.416919	8.414861
-295.562271	11.869772	8.424858
-293.460506	7.673885	8.434854
-291.432430	9.252955	8.444851
-289.783518	4.009875	8.454848
-287.979985	1.011078	8.464845
-285.936032	3.296569	8.474842
-284.173243	11.609610	8.484838
-282.338762	8.643770	8.494835
-280.072097	9.897398	8.504832
-278.314365	11.208576	8.514829
-276.811481	10.667262	8.524826
-274.757285	13.709030	8.534822
-272.568900	14.274102	8.544819
-271.163726	10.356786	8.554816
-269.386581	7.071685	8.564813
-267.364922	2.918606	8.574810
-265.290472	11.219813	8.584807
-263.246623	11.730594	8.594803
-261.762538	7.900163	8.604800
-259.659698	10.278912	8.614797
-257.861209	6.920938	8.624794
-255.904817	4.594086	8.634791
-254.208139	0.336570	8.644787
-252.221472	10.126546	8.654784
-250.296517	11.202633	8.664781
-248.349270	8.117767	8.674778
-246.462739	10.821580	8.684775
-244.702912	5.938196	8.694771
-242.865966	2.528306	8.704768
-240.377554	-3.420306	8.714765
-239.074165	-0.463947	8.724762
-237.400184	-3.276240	8.734759
-235.382969	1.274628	8.744755
-233.353373	6.829321	8.754752
-231.502022	4.012407	8.764749
-230.104288	2.166316	8.774746
-227.619904	-4.711647	8.784743
-225.674175	4.863829	8.794739
-224.099860	2.975350	8.804736
-222.345214	7.623400	8.814733
-220.276225	5.553345	8.824730
-218.475926	6.421981	8.834727
-216.500999	-3.390477	8.844723
-214.790468	1.701988	8.854720
-213.005591	0.169915	8.864717
-210.981306	6.895483	8.874714
-209.157930	9.964670	8.884711
-206.940162	3.392958	8.894707
-205.324993	5.262207	8.904704
-203.426054	3.651938	8.914701
-201.428401	-3.280958	8.924698
-199.791067	5.780068	8.934695
-197.846667	1.967797	8.944691
-195.952639	5.494670	8.954688
-194.234567	-0.436759	8.964685
-192.251663	5.325949	8.974682
-190.194271	-0.651730	8.984679
-188.389975	0.942611	8.994675
-186.533529	3.681272	9.004672
-184.858165	3.474073	9.014669
-182.823203	-1.626856	9.024666
-180.688771	4.091154	9.034663
-179.130165	-0.308491	9.044659
-177.110399	10.349436	9.054656
-175.256706	6.403234	9.064653
-173.605294	2.021940	9.074650
-171.475776	1.848071	9.084647
-169.536684	4.238818	9.094643
-167.828262	6.047423	9.104640
-165.909891	0.463002	9.114637
-164.114665	5.202516	9.124634
-162.059378	1.839950	9.134631
-160.070494	0.504313	9.144627
-158.499351	2.132722	9.154624
-157.008729	2.498183	9.164621
-154.740218	2.966892	9.174618
-152.601109	3.516251	9.184615
-150.806877	-4.761001	9.194611
-149.133940	6.789139	9.204608
-147.093330	6.286843	9.214605
-145.222768	9.473289	9.224602
-143.365846	1.307616	9.234599
-141.443368	2.363659	9.244595
-139.797001	1.327427	9.254592
-137.800758	1.675382	9.264589
-135.886359	10.161724	9.274586
-133.877779	6.705579	9.284583
-132.331981	0.343779	9.294579
-130.552715	7.755887	9.304576
-128.471054	7.146004	9.314573
-126.311797	6.171634	9.324570
-124.409365	9.608804	9.334567
-122.947893	10.321570	9.344563
-120.772281	6.900366	9.354560
-119.122247	8.096212	9.364557
-117.138563	3.276674	9.374554
-115.223247	4.657567	9.384551
-113.325046	7.346994	9.394547
-111.406831	1.952111	9.404544
-109.527652	7.643020	9.414541
-107.821475	10.320456	9.424538
-106.041624	13.642987	9.434535
-103.982374	13.033542	9.444531
-102.095607	4.919975	9.454528
-100.511193	7.212628	9.464525
-98.473424	9.676114	9.474522
-96.518287	-0.764688	9.484519
-94.534922	8.977012	9.494515
-92.721010	9.068302	9.504512
-90.802934	5.565051	9.514509
-89.260422	13.572340	9.524506
-87.119894	12.330989	9.534503
-84.964085	6.492427	9.544499
-83.293429	4.252348	9.554496
-81.905259	10.618461	9.564493
-79.626452	1.127094	9.574490
-77.643505	9.416234	9.584487
-75.729079	5.602521	9.594483
-73.920299	6.455703	9.604480
-72.115071	2.856783	9.614477
-70.203724	2.596228	9.624474
-68.594519	8.614452	9.634471
-66.458407	5.929076	9.644467
-64.243026	7.802147	9.654464
-62.921495	17.968413	9.664461
-60.717907	10.656970	9.674458
-58.993187	8.394072	9.684455
-57.212230	7.326951	9.694451
-55.188602	11.242217	9.704448
-53.163756	9.656189	9.714445
-51.409203	10.461196	9.724442
-49.586742	13.295390	9.734439
-47.985687	11.061699	9.744435
-45.900681	11.037147	9.754432
-44.141235	13.211918	9.764429
-42.155171	13.875790	9.774426
-40.284217	12.530638	9.784423
-38.123993	7.316679	9.794419
-36.202199	6.770270	9.804416
-34.651512	7.052014	9.814413
-32.772271	6.885031	9.824410
-30.830370	8.077014	9.834407
-28.869398	3.865908	9.844403
-27.052774	7.368950	9.854400
-25.324671	5.574487	9.864397
-23.569403	3.382531	9.874394
-21.468973	6.481883	9.884391
-19.550202	3.474369	9.894387
-17.646829	1.621954	9.904384
-15.665307	4.827121	9.914381
-13.979199	12.577873	9.924378
-12.149776	8.103549	9.934375
-10.011111	10.320490	9.944371
-8.460353	14.657015	9.954368
-6.215513	10.381699	9.964365
-4.574810	9.344882	9.974362
-3.478589	35.917826	9.984359
-2.270701	68.593091	9.994355
-0.976016	126.540272	10.004352
0.000000	184.853607	10.009357
0.951074	216.507772	10.014362
1.540578	247.399652	10.019367
1.695935	274.068326	10.024371
2.458804	299.952591	10.029376
2.773946	321.227845	10.034381
3.031527	332.325028	10.039386
3.247506	364.539895	10.044391
3.010803	368.824535	10.049395
3.361278	372.320073	10.054400
3.423960	391.468923	10.059405
3.617000	398.031582	10.064410
3.792219	416.802964	10.069415
3.616930	422.962324	10.074419
4.119076	414.869633	10.079424
3.998397	424.585852	10.084429
4.005074	416.403448	10.089434
4.104574	431.547239	10.094439
4.154569	430.468564	10.099443
4.577951	434.460279	10.104448
4.125882	433.417525	10.109453
4.377476	427.700310	10.114458
4.532393	431.618147	10.119463
4.469137	439.396560	10.124467
4.499373	444.830850	10.129472
4.220589	447.531042	10.134477
4.713522	447.236446	10.139482
4.270497	453.449561	10.144487
4.727293	447.497755	10.149491
5.044674	451.828088	10.154496
4.921778	452.574756	10.159501
4.931877	454.000397	10.164506
4.980182	456.716230	10.169511
4.942849	449.873385	10.174515
5.072961	459.320964	10.179520
4.632635	461.442935	10.184525
4.841996	458.074278	10.189530
4.785558	460.451995	10.194535
4.796566	482.692228	10.199539
5.144829	488.313936	10.204544
4.873198	502.365789	10.209549
5.047601	500.183869	10.214554
5.147088	500.554439	10.219559
4.903777	501.285621	10.224563
5.116002	498.509449	10.229568
4.942103	501.328543	10.234573
5.355642	501.743642	10.239578
5.071305	514.088069	10.244583
5.487805	532.210030	10.249587
5.604516	528.675568	10.254592
5.538584	534.343644	10.259597
5.901430	531.433052	10.264602
5.703280	540.172926	10.269607
5.649829	540.492194	10.274611
5.894156	545.789871	10.279616
5.878157	549.772848	10.284621
6.110288	540.261274	10.289626
6.031869	548.821202	10.294631
6.015668	554.343367	10.299635
6.180720	542.907508	10.304640
5.889777	550.463668	10.309645
5.967853	552.454081	10.314650
5.939916	549.867596	10.319655
5.984260	547.490364	10.324659
6.515307	557.263578	10.329664
6.009516	557.473638	10.334669
6.020940	554.426697	10.339674
5.653914	557.672433	10.344679
5.808132	566.349813	10.349683
6.266529	571.542390	10.354688
6.258913	589.947329	10.359693
6.522705	587.945110	10.364698
6.409591	586.196979	10.369703
6.493658	591.439805	10.374707
6.391215	595.714136	10.379712
6.324568	604.929832	10.384717
6.672851	595.734021	10.389722
6.565166	598.086817	10.394727
6.491097	614.849684	10.399731
7.099180	629.961453	10.404736
6.986561	638.556851	10.409741
7.051587	636.897000	10.414746
7.301105	635.567281	10.419751
6.998963	635.429458	10.424755
7.040329	635.098070	10.429760
6.919636	642.366916	10.434765
7.383963	634.880977	10.439770
7.072755	644.782279	10.444775
7.259371	651.223070	10.449779
7.389325	651.051024	10.454784
7.286088	660.226857	10.459789
7.555135	649.032958	10.464794
7.161173	657.331029	10.469799
7.070821	651.915857	10.474803
7.328983	657.214522	10.479808
7.177515	667.960873	10.484813
7.389192	659.856026	10.489818
7.435844	667.542912	10.494823
7.388376	684.684830	10.499827
8.062061	683.008323	10.504832
7.802748	689.482407	10.509837
7.981275	689.688982	10.514842
7.767969	689.331977	10.519847
7.702323	699.496936	10.524851
7.755309	698.819904	10.529856
7.796782	702.025749	10.534861
7.665851	702.612855	10.539866
7.795805	692.578138	10.544871
7.639335	704.736744	10.549875
7.975522	707.707920	10.554880
8.044250	726.331100	10.559885
8.361002	730.395101	10.564890
8.327284	742.731289	10.569895
8.374807	735.537292	10.574899
8.237058	742.755289	10.579904
7.985402	752.421651	10.584909
8.023949	741.567234	10.589914
8.439517	738.924172	10.594919
8.109864	745.945687	10.599923
8.379281	750.222257	10.604928
8.268518	774.497793	10.609933
8.478814	779.583354	10.614938
8.646178	776.978295	10.619943
8.848973	772.472001	10.624947
8.887958	772.049522	10.629952
8.737551	781.185643	10.634957
9.137028	781.967289	10.639962
8.880994	783.470103	10.644967
8.937416	782.519693	10.649971
9.062838	786.751428	10.654976
8.747212	792.242588	10.659981
8.688004	790.186199	10.664986
9.072075	801.981116	10.669991
8.960665	818.606662	10.674995
9.387114	822.905519	10.680000
9.362759	825.987843	10.685005
9.316493	816.649809	10.690010
9.035316	822.960273	10.695015
9.303193	827.106218	10.700019
9.549633	821.815471	10.705024
9.265206	840.446235	10.710029
9.518447	831.016265	10.715034
9.336625	829.802637	10.720039
9.363256	828.372826	10.725043
9.756766	844.362755	10.730048
9.884700	863.282612	10.735053
9.734980	852.882362	10.740058
9.890059	855.332069	10.745063
9.822430	861.100685	10.750067
9.897574	853.976345	10.755072
9.662681	861.665658	10.760077
9.775810	851.234525	10.765082
9.951319	857.251381	10.770087
9.794665	870.917801	10.775091
9.968776	861.792183	10.780096
10.031581	864.732874	10.785101
10.069182	866.408071	10.790106
10.156009	885.966905	10.795111
10.053152	892.097563	10.800115
10.861926	892.889632	10.805120
10.545204	901.268567	10.810125
10.561127	896.337852	10.815130
10.395141	909.348171	10.820135
10.386300	901.251552	10.825139
10.621933	903.708921	10.830144
10.615129	911.019663	10.835149
10.595201	908.625813	10.840154
10.525209	908.111896	10.845159
10.548551	915.364213	10.850163
10.589126	906.370259	10.855168
10.343007	907.641256	10.860173
10.916510	908.595437	10.865178
10.789855	911.329798	10.870183
10.701726	930.899250	10.875187
10.946961	938.534104	10.880192
11.165778	944.279145	10.885197
10.832249	942.367417	10.890202
10.891497	945.766035	10.895207
10.954149	952.638341	10.900211
11.093041	940.162339	10.905216
11.060141	950.025767	10.910221
11.381452	942.261267	10.915226
11.159429	946.474343	10.920231
11.198036	966.351654	10.925235
11.553971	965.307727	10.930240
11.483970	978.369034	10.935245
11.758467	984.822768	10.940250
11.520123	987.871443	10.945255
11.485965	994.708744	10.950259
11.481525	991.039730	10.955264
11.348821	990.609934	10.960269
11.451943	990.412199	10.965274
11.587413	1001.614532	10.970279
11.367419	1002.753630	10.975283
11.563211	1000.232312	10.980288
12.012259	1014.690141	10.985293
11.969711	1020.677184	10.990298
12.201407	1024.171325	10.995303
12.103769	1026.090475	11.000307
12.501986	1023.864895	11.005312
12.086908	1023.448593	11.010317
12.116164	1025.440550	11.015322
12.154669	1040.542662	11.020327
11.899508	1034.549621	11.025331
12.308983	1022.662791	11.030336
12.264036	1031.052073	11.035341
12.257114	1036.076169	11.040346
12.196722	1033.344954	11.045351
12.128575	1033.732813	11.050355
12.300694	1032.560494	11.055360
12.515908	1057.328594	11.060365
12.761898	1068.757795	11.065370
12.837217	1066.301416	11.070375
12.703301	1078.802113	11.075379
12.807748	1072.899944	11.080384
12.840556	1079.373343	11.085389
13.022903	1072.567712	11.090394
12.840349	1074.923063	11.095399
12.564756	1082.623714	11.100403
12.992419	1075.239601	11.105408
12.695823	1085.173565	11.110413
12.826514	1078.961259	11.115418
12.996643	1074.639866	11.120423
13.079833	1081.218779	11.125427
13.056653	1083.752153	11.130432
13.068137	1094.176340	11.135437
13.029748	1109.890071	11.140442
13.328305	1115.649272	11.145447
13.255494	1109.540378	11.150451
13.430200	1115.546430	11.155456
13.374920	1122.330385	11.160461
13.467331	1121.102958	11.165466
13.476619	1118.827425	11.170471
13.090895	1125.712974	11.175475
13.477232	1122.998808	11.180480
13.550494	1122.427339	11.185485
13.663031	1138.790436	11.190490
13.934605	1150.912685	11.195495
13.890562	1155.464890	11.200499
13.883680	1151.797803	11.205504
14.025415	1158.444690	11.210509
13.840562	1158.114675	11.215514
14.135820	1154.079253	11.220519
14.049412	1163.640677	11.225523
14.243321	1154.115875	11.230528
14.247518	1163.252810	11.235533
14.053788	1159.112438	11.240538
13.789897	1157.710006	11.245543
14.148222	1164.152027	11.250547
14.419569	1154.425626	11.255552
14.399746	1162.968683	11.260557
14.303761	1162.381626	11.265562
14.352136	1161.296847	11.270567
14.346126	1166.171020	11.275571
14.456348	1157.686236	11.280576
14.353456	1160.166100	11.285581
14.549965	1168.895447	11.290586
14.381136	1171.411063	11.295591
14.337975	1183.257083	11.300595
14.528530	1184.980467	11.305600
14.694212	1200.962969	11.310605
14.786976	1196.735888	11.315610
14.898583	1192.316554	11.320615
14.458569	1202.546305	11.325619
14.791655	1196.680165	11.330624
15.101022	1198.395641	11.335629
14.786218	1195.222388	11.340634
15.012625	1198.108666	11.345639
14.915642	1219.991906	11.350643
15.256887	1212.862799	11.355648
15.103253	1229.342572	11.360653
15.205937	1232.278554	11.365658
15.339537	1227.827315	11.370663
15.227606	1234.137772	11.375667
15.369960	1225.053266	11.380672
15.567254	1233.828262	11.385677
15.620698	1228.763707	11.390682
15.632606	1229.916301	11.395687
15.806100	1235.298074	11.400691
15.972063	1223.733794	11.405696
16.023364	1240.409570	11.410701
15.788944	1231.337840	11.415706
16.106304	1233.275990	11.420711
16.076804	1236.751913	11.425715
15.996376	1228.620795	11.430720
15.751339	1225.770748	11.435725
15.554761	1229.640776	11.440730
16.104568	1232.011820	11.445735
15.792636	1231.880281	11.450739
16.029074	1226.967905	11.455744
15.813389	1231.429229	11.460749
16.150810	1231.329752	11.465754
16.270617	1237.913935	11.470759
15.961871	1234.189308	11.475763
16.251456	1230.124806	11.480768
16.317875	1237.458729	11.485773
15.933146	1241.592176	11.490778
16.185040	1241.618311	11.495783
16.123325	1266.781047	11.500787
16.313006	1258.734576	11.505792
16.323207	1268.638657	11.510797
16.326288	1272.068388	11.515802
16.972999	1264.478919	11.520807
16.482479	1276.011558	11.525811
16.895822	1273.081729	11.530816
16.727541	1271.063169	11.535821
16.665021	1261.689592	11.540826
16.996329	1269.623155	11.545831
16.497244	1271.939128	11.550835
17.122927	1259.222775	11.555840
16.931593	1265.008126	11.560845
16.794810	1260.885452	11.565850
17.142083	1269.289592	11.570855
17.153866	1290.359165	11.575859
17.541657	1287.923881	11.580864
17.653863	1271.504417	11.585869
17.693547	1252.765617	11.590874
17.476774	1251.473941	11.595879
17.217764	1258.694185	11.600883
17.759482	1252.370515	11.605888
17.770536	1249.886505	11.610893
17.510552	1262.279722	11.615898
17.684760	1260.419445	11.620903
17.677039	1260.488565	11.625907
17.316254	1259.161506	11.630912
17.147920	1264.621464	11.635917
17.308844	1259.460903	11.640922
17.864856	1270.935443	11.645927
17.429933	1290.696317	11.650931
17.879847	1281.679427	11.655936
18.084162	1287.220320	11.660941
17.625795	1287.019087	11.665946
17.959192	1293.023559	11.670951
18.054441	1292.432806	11.675955
18.255044	1288.803561	11.680960
18.058301	1292.918079	11.685965
18.230507	1291.625868	11.690970
18.231599	1291.904911	11.695975
18.299153	1291.354848	11.700979
18.370338	1295.167993	11.705984
18.344639	1289.185561	11.710989
18.330531	1295.232842	11.715994
18.538586	1287.711746	11.720999
18.281112	1292.600835	11.726003
18.355977	1298.236501	11.731008
18.396672	1302.625415	11.736013
18.624108	1299.028161	11.741018
18.928336	1290.048695	11.746023
18.597652	1296.127542	11.751027
18.795514	1300.351028	11.756032
18.658197	1297.034318	11.761037
18.499651	1304.923015	11.766042
18.421079	1302.606268	11.771047
18.509965	1296.861045	11.776051
18.939615	1317.319918	11.781056
19.081846	1328.155541	11.786061
18.836803	1330.237024	11.791066
19.042656	1322.353532	11.796071
18.846107	1327.406395	11.801075
18.704030	1326.369327	11.806080
18.948490	1335.201522	11.811085
18.808508	1326.059473	11.816090
19.382278	1322.968418	11.821095
18.867612	1334.082295	11.826099
19.393327	1338.452215	11.831104
19.305586	1356.192755	11.836109
19.322845	1360.336244	11.841114
19.808781	1351.001302	11.846119
19.841312	1359.129236	11.851123
19.772391	1353.286147	11.856128
19.746735	1360.801989	11.861133
19.822325	1356.708499	11.866138
19.949010	1338.081880	11.871143
19.978328	1331.351003	11.876147
20.115074	1319.673025	11.881152
20.021765	1327.355771	11.886157
20.038963	1316.794514	11.891162
19.949498	1322.350734	11.896167
20.020763	1332.208847	11.901171
19.904654	1326.348061	11.906176
20.108102	1323.344457	11.911181
20.145681	1329.989109	11.916186
20.027593	1325.894976	11.921191
19.971985	1333.171133	11.926195
20.257460	1345.212473	11.931200
20.558189	1352.636829	11.936205
20.427414	1357.901581	11.941210
20.389695	1352.868871	11.946215
20.621664	1363.370060	11.951219
20.759898	1344.506604	11.956224
20.142742	1343.214117	11.961229
20.098446	1351.846351	11.966234
20.551063	1353.542153	11.971239
20.731841	1365.160201	11.976243
20.940506	1356.719530	11.981248
20.827256	1363.788834	11.986253
20.594965	1366.273600	11.991258
20.848160	1360.642507	11.996263
20.762883	1363.551719	12.001267
21.152053	1359.043907	12.006272
20.783929	1357.725894	12.011277
21.016254	1354.124693	12.016282
21.193628	1351.172554	12.021287
21.002533	1362.752131	12.026291
21.077067	1363.959408	12.031296
20.882185	1366.480789	12.036301
20.938301	1362.302086	12.041306
21.138083	1361.155294	12.046311
20.904556	1363.045694	12.051315
20.861442	1367.421184	12.056320
20.950960	1369.351533	12.061325
20.993306	1363.842385	12.066330
20.949976	1367.311082	12.071335
20.536589	1374.157001	12.076339
20.770477	1365.721763	12.081344
20.988665	1365.046740	12.086349
20.917843	1367.013701	12.091354
21.186203	1365.534244	12.096359
20.986589	1369.060987	12.101363
21.179985	1364.026108	12.106368
21.098311	1362.709721	12.111373
21.132162	1361.441147	12.116378
21.260913	1360.646336	12.121383
21.150180	1362.668551	12.126387
21.050012	1351.148192	12.131392
21.182325	1342.491028	12.136397
20.684840	1337.427564	12.141402
20.990134	1324.372714	12.146407
20.998676	1330.626149	12.151411
21.009822	1332.934877	12.156416
20.774351	1335.305017	12.161421
20.905765	1335.407145	12.166426
21.106559	1330.260702	12.171431
20.696219	1336.186675	12.176435
20.946563	1345.973654	12.181440
21.152216	1354.427242	12.186445
20.958792	1348.574047	12.191450
21.011561	1334.671562	12.196455
20.885436	1342.753822	12.201459
21.169452	1348.376653	12.206464
20.920092	1342.198039	12.211469
21.095528	1343.416031	12.216474
21.216570	1335.806278	12.221479
20.886669	1344.387857	12.226483
20.894143	1337.463324	12.231488
20.763765	1339.658996	12.236493
20.989903	1338.034876	12.241498
21.138263	1339.586798	12.246503
21.087122	1336.396695	12.251507
21.146383	1343.481056	12.256512
21.025891	1336.863963	12.261517
20.969492	1341.638990	12.266522
21.181506	1337.987411	12.271527
21.151827	1341.734647	12.276531
21.271539	1332.440778	12.281536
21.137821	1337.231290	12.286541
21.075636	1347.074423	12.291546
21.480952	1337.832779	12.296551
21.143522	1345.491387	12.301555
21.198248	1336.020207	12.306560
21.186870	1316.970896	12.311565
21.038345	1313.370517	12.316570
21.157088	1311.709907	12.321575
20.891502	1323.951093	12.326579
20.747627	1317.004973	12.331584
20.614058	1309.240283	12.336589
20.673108	1311.713270	12.341594
21.026296	1324.732626	12.346599
21.034149	1333.263484	12.351603
21.123921	1329.877429	12.356608
20.889059	1315.295378	12.361613
20.759395	1315.175771	12.366618
21.174004	1320.211589	12.371623
20.769815	1329.148812	12.376627
20.760611	1326.532390	12.381632
21.018303	1328.885381	12.386637
20.616555	1347.686904	12.391642
20.947136	1340.707683	12.396647
21.216488	1351.288064	12.401651
21.336386	1340.480155	12.406656
20.870972	1332.443499	12.411661
20.669214	1331.821260	12.416666
20.951493	1332.678407	12.421671
21.020013	1345.462462	12.426675
20.942058	1344.675385	12.431680
21.103741	1353.167527	12.436685
20.860353	1347.804890	12.441690
20.874182	1343.580893	12.446695
20.949658	1349.525592	12.451699
21.013580	1348.315306	12.456704
21.034787	1360.039231	12.461709
20.976499	1354.114014	12.466714
21.230458	1346.095093	12.471719
20.740519	1335.762952	12.476723
20.942422	1331.401721	12.481728
20.964287	1329.799142	12.486733
20.916602	1333.700648	12.491738
20.853547	1333.765976	12.496743
20.829937	1344.345763	12.501747
21.211487	1353.850025	12.506752
20.957612	1347.113840	12.511757
20.616288	1342.180022	12.516762
21.171896	1349.355550	12.521767
20.646671	1359.196841	12.526771
20.758799	1362.626550	12.531776
21.050319	1361.812086	12.536781
20.852707	1361.072480	12.541786
20.963597	1362.679271	12.546791
20.798012	1366.432418	12.551795
21.069995	1361.927525	12.556800
21.028002	1368.302586	12.561805
20.865665	1362.203133	12.566810
21.252264	1354.193017	12.571815
21.003856	1361.369039	12.576819
21.044501	1352.272288	12.581824
21.273942	1360.439786	12.586829
21.113457	1352.767683	12.591834
20.843095	1329.089902	12.596839
20.934275	1327.269670	12.601843
20.753451	1325.753039	12.606848
20.882535	1333.084902	12.611853
20.901482	1349.464740	12.616858
21.248042	1355.266849	12.621863
20.840987	1342.652052	12.626867
20.809192	1347.139281	12.631872
21.518330	1359.665045	12.636877
21.055503	1342.777346	12.641882
20.941460	1327.620878	12.646887
20.922031	1329.399850	12.651891
20.824734	1322.162423	12.656896
20.704555	1327.400241	12.661901
20.766842	1347.162323	12.666906
21.118070	1344.657161	12.671911
21.263104	1350.016706	12.676915
20.918240	1330.716187	12.681920
21.020761	1327.741296	12.686925
20.811752	1336.871340	12.691930
20.713741	1330.715905	12.696935
20.572754	1342.822106	12.701939
20.877330	1345.651789	12.706944
20.903249	1356.400319	12.711949
21.008631	1368.818939	12.716954
21.102664	1362.675443	12.721959
21.404834	1359.288625	12.726963
21.070675	1349.661821	12.731968
21.094488	1337.710079	12.736973
20.659805	1333.666438	12.741978
21.048618	1329.698056	12.746983
20.946339	1336.174189	12.751987
21.247936	1329.955021	12.756992
20.814068	1330.841223	12.761997
20.716843	1340.756179	12.767002
20.770833	1325.003585	12.772007
20.600981	1346.319846	12.777011
21.080721	1359.942000	12.782016
20.982597	1361.355025	12.787021
20.906835	1364.642798	12.792026
21.305338	1364.489420	12.797031
20.961044	1365.287215	12.802035
21.174140	1357.531870	12.807040
21.045889	1350.338794	12.812045
20.751252	1343.714776	12.817050
20.989436	1338.634913	12.822055
20.774186	1342.425939	12.827059
20.844720	1354.624582	12.832064
20.942845	1355.843866	12.837069
21.129654	1373.121133	12.842074
21.150527	1360.690405	12.847079
21.091341	1351.193225	12.852083
21.178301	1347.135775	12.857088
20.960103	1341.829052	12.862093
20.820856	1351.298092	12.867098
20.740878	1344.945793	12.872103
20.824741	1349.278947	12.877107
20.783412	1343.551320	12.882112
21.152821	1355.421574	12.887117
21.098172	1360.011808	12.892122
20.953618	1346.695919	12.897127
20.831026	1350.658266	12.902131
20.937120	1349.666778	12.907136
21.138537	1341.110566	12.912141
20.863735	1343.889139	12.917146
21.075366	1348.216108	12.922151
21.164637	1345.588709	12.927155
20.822179	1352.237208	12.932160
20.820033	1346.325119	12.937165
20.598599	1355.786769	12.942170
21.415410	1356.829923	12.947175
20.965155	1355.417767	12.952179
21.080654	1350.040472	12.957184
20.945943	1347.704284	12.962189
20.687327	1353.085626	12.967194
20.843099	1340.940933	12.972199
21.070670	1351.941174	12.977203
20.699107	1349.667995	12.982208
21.079411	1351.195542	12.987213
20.909273	1349.517918	12.992218
21.234177	1347.441191	12.997223
21.007098	1355.591604	13.002227
20.946010	1348.976070	13.007232
21.173228	1349.414608	13.012237
21.064551	1349.555028	13.017242
21.189942	1342.753624	13.022247
21.195992	1347.851459	13.027251
20.973622	1352.564643	13.032256
21.044525	1346.943704	13.037261
21.035308	1359.142454	13.042266
21.338710	1345.258338	13.047271
21.338948	1361.626980	13.052275
20.962395	1349.652342	13.057280
21.238994	1350.483585	13.062285
21.179458	1353.847623	13.067290
21.117869	1347.990749	13.072295
20.939334	1334.375913	13.077299
20.814024	1325.193673	13.082304
21.087364	1323.565181	13.087309
20.795480	1338.663521	13.092314
21.166720	1334.196427	13.097319
20.609797	1335.346704	13.102323
20.959697	1343.483941	13.107328
21.148753	1341.326371	13.112333
21.208738	1342.382989	13.117338
20.917314	1324.725166	13.122343
20.980083	1325.262477	13.127347
20.939779	1319.214548	13.132352
21.114002	1316.103633	13.137357
20.759560	1317.481834	13.142362
20.913517	1315.485997	13.147367
21.000694	1317.263735	13.152371
20.788279	1327.856275	13.157376
21.139389	1330.462472	13.162381
20.806288	1327.864590	13.167386
20.990585	1330.451657	13.172391
20.848876	1321.456554	13.177395
20.793620	1340.529262	13.182400
20.747980	1353.662721	13.187405
20.959523	1356.890476	13.192410
21.048752	1356.792732	13.197415
20.894277	1358.509660	13.202419
20.624502	1358.603227	13.207424
21.166022	1359.997821	13.212429
21.011982	1361.055457	13.217434
21.125167	1354.252840	13.222439
21.143534	1364.114679	13.227443
21.000845	1360.303605	13.232448
21.055854	1349.171696	13.237453
20.884452	1354.340416	13.242458
20.967928	1348.163914	13.247463
21.097414	1352.418823	13.252467
20.692434	1350.225096	13.257472
20.834027	1346.001224	13.262477
21.045789	1361.227436	13.267482
21.084526	1357.486784	13.272487
21.147294	1354.327399	13.277491
21.058423	1344.186775	13.282496
21.173754	1331.666883	13.287501
21.090664	1331.262281	13.292506
20.818969	1331.799316	13.297511
21.148376	1327.830947	13.302515
21.015149	1328.178726	13.307520
21.299180	1330.081201	13.312525
20.895812	1336.540695	13.317530
20.854733	1326.734688	13.322535
21.090190	1330.718778	13.327539
20.882603	1341.394144	13.332544
21.250629	1328.233082	13.337549
20.847929	1339.846390	13.342554
20.883218	1333.933067	13.347559
21.015230	1328.196725	13.352563
20.846660	1327.842029	13.357568
20.878688	1330.568508	13.362573
20.955998	1339.898915	13.367578
21.257729	1332.244574	13.372583
21.024066	1331.875027	13.377587
21.121729	1333.794609	13.382592
21.180638	1334.015543	13.387597
20.808852	1337.011448	13.392602
20.926327	1337.271930	13.397607
20.917995	1337.033616	13.402611
20.898405	1346.455182	13.407616
20.974247	1335.816743	13.412621
20.893348	1340.723421	13.417626
21.056740	1336.761026	13.422631
20.986412	1342.913495	13.427635
20.817786	1336.479135	13.432640
21.206937	1336.931274	13.437645
20.643054	1346.162081	13.442650
20.920711	1335.526151	13.447655
20.852305	1331.367318	13.452659
20.799146	1338.632047	13.457664
21.049548	1340.932582	13.462669
21.029742	1342.050815	13.467674
20.858119	1337.690804	13.472679
20.814360	1339.344336	13.477683
20.961429	1335.453936	13.482688
21.227088	1336.832595	13.487693
20.932780	1342.039838	13.492698
21.124851	1335.314542	13.497703
21.073871	1330.646685	13.502707
21.013225	1334.458787	13.507712
21.244883	1326.937061	13.512717
21.081513	1333.498637	13.517722
21.698960	1332.059710	13.522727
21.529824	1326.395055	13.527731
20.710640	1326.650370	13.532736
21.081236	1309.595091	13.537741
20.848893	1314.623694	13.542746
20.994561	1311.624576	13.547751
21.082398	1311.169057	13.552755
20.887754	1318.262360	13.557760
20.951488	1308.706176	13.562765
20.753762	1313.071613	13.567770
20.980052	1302.585837	13.572775
21.066922	1315.926805	13.577779
21.163654	1308.160080	13.582784
21.373718	1297.599619	13.587789
20.969803	1309.820273	13.592794
20.912345	1311.267812	13.597799
21.122548	1312.827215	13.602803
20.858680	1318.767671	13.607808
21.151070	1308.003244	13.612813
20.842303	1314.157457	13.617818
21.299548	1311.310513	13.622823
21.059025	1315.170224	13.627827
20.789828	1313.155136	13.632832
21.215879	1310.718478	13.637837
20.887010	1315.272003	13.642842
20.905054	1315.758095	13.647847
21.319672	1309.683349	13.652851
20.752439	1310.425227	13.657856
20.887820	1308.214716	13.662861
20.888885	1312.234607	13.667866
21.146568	1313.368511	13.672871
21.071520	1313.107719	13.677875
20.902486	1317.156318	13.682880
21.066322	1305.123918	13.687885
21.133611	1314.840716	13.692890
20.997167	1320.062200	13.697895
21.043636	1312.005421	13.702899
21.114188	1311.847574	13.707904
21.128200	1303.647730	13.712909
20.787014	1304.668972	13.717914
21.135969	1304.375251	13.722919
21.033633	1314.636386	13.727923
20.647189	1300.386056	13.732928
20.878868	1294.064504	13.737933
21.159695	1313.151389	13.742938
20.952044	1309.126743	13.747943
21.070513	1302.949410	13.752947
20.987305	1301.489759	13.757952
20.941143	1289.522406	13.762957
20.605358	1292.225533	13.767962
20.975993	1305.936006	13.772967
21.200755	1312.561836	13.777971
20.676241	1316.392718	13.782976
20.855375	1312.006736	13.787981
20.909294	1317.322449	13.792986
20.695404	1315.353738	13.797991
21.171670	1324.376057	13.802995
21.110564	1319.020632	13.808000
21.436597	1317.700730	13.813005
21.114734	1305.472958	13.818010
21.005458	1289.259123	13.823015
21.144267	1288.019551	13.828019
20.981799	1284.585420	13.833024
21.085628	1275.929684	13.838029
21.233317	1285.895434	13.843034
20.854585	1283.388424	13.848039
20.817963	1276.693321	13.853043
20.625797	1287.430848	13.858048
21.153303	1281.699261	13.863053
20.404358	1288.970849	13.868058
20.685046	1294.703008	13.873063
21.253693	1308.014442	13.878067
20.812651	1298.810029	13.883072
21.258183	1289.049450	13.888077
20.824115	1301.336413	13.893082
20.929847	1292.262437	13.898087
20.918437	1290.523231	13.903091
20.767087	1293.670067	13.908096
21.274138	1307.835064	13.913101
21.039356	1298.063124	13.918106
20.654589	1299.767885	13.923111
21.140590	1308.835954	13.928115
20.617463	1298.237875	13.933120
21.299421	1314.951936	13.938125
21.231116	1308.175133	13.943130
21.126896	1299.096788	13.948135
21.086437	1294.515580	13.953139
21.053254	1294.940450	13.958144
21.036775	1297.182610	13.963149
20.888886	1293.851816	13.968154
21.000862	1301.211624	13.973159
20.951225	1287.111034	13.978163
20.876170	1301.657471	13.983168
21.076482	1296.008027	13.988173
21.155657	1297.582019	13.993178
21.032450	1292.610276	13.998183
20.913142	1302.694322	14.003187
20.827482	1300.019130	14.008192
20.932911	1295.667646	14.013210
20.690590	1300.716563	14.018227
20.794592	1300.031500	14.023245
20.820461	1294.745113	14.028263
20.778181	1298.014456	14.033280
20.959480	1300.738469	14.038298
21.018809	1314.856740	14.043315
21.153863	1322.467771	14.048333
21.106511	1327.273238	14.053351
21.057833	1330.398887	14.058368
21.071058	1329.511217	14.063386
20.708565	1330.929805	14.068403
21.117027	1325.219010	14.073421
21.197524	1317.101829	14.078439
21.110140	1325.989484	14.083456
21.407728	1317.320141	14.088474
21.017598	1318.796619	14.093491
21.009489	1320.717123	14.098509
20.907293	1327.448900	14.103527
21.036667	1333.825988	14.108544
21.079934	1325.546422	14.113562
20.972163	1333.345628	14.118579
20.973866	1338.848008	14.123597
21.035497	1351.937164	14.128615
21.077792	1368.496455	14.133632
21.472450	1364.024278	14.138650
21.477623	1361.808648	14.143667
21.396258	1362.804866	14.148685
21.427067	1361.102687	14.153703
21.279755	1363.630578	14.158720
21.525975	1362.690015	14.163738
21.487798	1364.662512	14.168755
21.488865	1369.897583	14.173773
21.694696	1355.131486	14.178791
21.247363	1367.026074	14.183808
21.658160	1370.078449	14.188826
21.554057	1364.940185	14.193843
21.225547	1362.832832	14.198861
21.610351	1363.452672	14.203879
21.281178	1375.877421	14.208896
21.752112	1372.673554	14.213914
21.718141	1374.422005	14.218931
21.593725	1377.924695	14.223949
21.523968	1373.631980	14.228967
21.581063	1378.836096	14.233984
21.796389	1391.499642	14.239002
22.295117	1406.449291	14.244019
21.976369	1394.466210	14.249037
22.091028	1376.406466	14.254055
22.031080	1370.779799	14.259072
21.943976	1371.861878	14.264090
21.900498	1378.176889	14.269107
21.928353	1372.341157	14.274125
21.789951	1371.207100	14.279143
21.971930	1367.983250	14.284160
21.674274	1369.550380	14.289178
21.653565	1367.194156	14.294195
21.499346	1375.266640	14.299213
22.200507	1390.964229	14.304231
22.099459	1403.335315	14.309248
22.152776	1393.356764	14.314266
21.990690	1394.900701	14.319283
22.066918	1400.633471	14.324301
22.227769	1397.446019	14.329319
22.160768	1404.965046	14.334336
22.396816	1396.071084	14.339354
22.213115	1382.400593	14.344371
21.944989	1378.578401	14.349389
22.179715	1372.917320	14.354407
21.740390	1375.136272	14.359424
21.875462	1387.641150	14.364442
22.012780	1407.811257	14.369459
22.070594	1410.696562	14.374477
22.174934	1400.892345	14.379495
22.433143	1402.696449	14.384512
22.456972	1404.190286	14.389530
22.404467	1406.964194	14.394547
22.340757	1405.807210	14.399565
22.694598	1401.690753	14.404583
22.176136	1406.974090	14.409600
22.729463	1403.154588	14.414618
22.524158	1411.147148	14.419635
22.066186	1410.871042	14.424653
22.422226	1405.881179	14.429671
22.577783	1415.634658	14.434688
22.591225	1410.729322	14.439706
22.405143	1414.193091	14.444723
22.298801	1411.218142	14.449741
22.368701	1406.860670	14.454759
22.308507	1411.444837	14.459776
22.427699	1411.114433	14.464794
22.567071	1407.264995	14.469811
22.718154	1417.649204	14.474829
22.865862	1406.089596	14.479847
22.637868	1415.252210	14.484864
22.327273	1411.823758	14.489882
22.476562	1407.707675	14.494899
22.585769	1428.653885	14.499917
22.989690	1431.061624	14.504935
22.977615	1437.761775	14.509952
22.830672	1440.956604	14.514970
23.190100	1430.836394	14.519987
22.998933	1435.855963	14.525005
23.029846	1418.006945	14.530023
22.833783	1410.765976	14.535040
22.848781	1404.732501	14.540058
22.942602	1407.176322	14.545075
22.487877	1416.736904	14.550093
23.024805	1429.156489	14.555111
22.704967	1436.041796	14.560128
22.645805	1432.913022	14.565146
23.107808	1433.409650	14.570163
22.956251	1442.365028	14.575181
23.014801	1425.689041	14.580199
23.100944	1439.766189	14.585216
23.052036	1438.320542	14.590234
23.339656	1432.460660	14.595251
23.034397	1435.703547	14.600269
23.065639	1432.115961	14.605287
23.128577	1432.157122	14.610304
22.773224	1439.968342	14.615322
23.079763	1439.879413	14.620339
23.223578	1440.368586	14.625357
23.289118	1436.468779	14.630375
23.401781	1438.651616	14.635392
23.171670	1436.262709	14.640410
23.244727	1439.421664	14.645427
23.276612	1448.387902	14.650445
23.433238	1434.386222	14.655463
23.265516	1442.006279	14.660480
23.078278	1432.462482	14.665498
23.641744	1437.883956	14.670515
23.530808	1440.637300	14.675533
23.282345	1438.996171	14.680551
23.749955	1434.690095	14.685568
23.558696	1433.696601	14.690586
23.504837	1426.222938	14.695603
23.146581	1445.809086	14.700621
23.369696	1439.294864	14.705639
23.458568	1449.239119	14.710656
23.088048	1464.040377	14.715674
23.655757	1469.181178	14.720691
23.521463	1477.808197	14.725709
23.755038	1471.436230	14.730727
24.081943	1470.010082	14.735744
23.744814	1477.263119	14.740762
24.225438	1476.608432	14.745779
23.713421	1469.657719	14.750797
24.122403	1458.253035	14.755815
24.038325	1454.748332	14.760832
23.592647	1438.296685	14.765850
23.977998	1434.408008	14.770867
23.920388	1441.226325	14.775885
23.525214	1435.576017	14.780903
23.745002	1441.483328	14.785920
23.711707	1450.816264	14.790938
24.079987	1462.954454	14.795955
23.865180	1484.111301	14.800973
24.081708	1475.280968	14.805991
23.964209	1473.219385	14.811008
23.680493	1472.105350	14.816026
24.254340	1470.410148	14.821043
24.031936	1472.331028	14.826061
24.012906	1476.038737	14.831079
24.182275	1473.477568	14.836096
23.721345	1478.904344	14.841114
23.975685	1466.898230	14.846131
23.834597	1478.438888	14.851149
24.172212	1470.626691	14.856167
24.156217	1475.884972	14.861184
24.306968	1480.625860	14.866202
24.455141	1472.053404	14.871219
24.260453	1483.634076	14.876237
24.033193	1480.611542	14.881255
24.331422	1475.900658	14.886272
24.178491	1483.247021	14.891290
24.165632	1468.997050	14.896307
24.187935	1478.951942	14.901325
24.112562	1468.408679	14.906343
24.239008	1479.226312	14.911360
24.016118	1479.422388	14.916378
24.128790	1484.054516	14.921395
24.547014	1502.923848	14.926413
24.501682	1502.206748	14.931431
24.479601	1504.388276	14.936448
24.730928	1503.097666	14.941466
24.665413	1507.134492	14.946483
24.570752	1513.514356	14.951501
25.011950	1504.957283	14.956519
24.690091	1478.000468	14.961536
24.062839	1479.611525	14.966554
24.510008	1492.751007	14.971571
24.603461	1498.215217	14.976589
24.859025	1502.804111	14.981607
24.964763	1500.724224	14.986624
24.710813	1503.702530	14.991642
24.685316	1504.910865	14.996659
24.740246	1499.869103	15.001677
24.600314	1499.818346	15.006695
24.764144	1508.109962	15.011712
24.669564	1514.367900	15.016730
24.803875	1502.201569	15.021747
25.044135	1504.151700	15.026765
25.007955	1504.328224	15.031783
24.789311	1503.008745	15.036800
24.807559	1506.809621	15.041818
24.896567	1496.870927	15.046835
24.973104	1503.367419	15.051853
24.899695	1502.145118	15.056871
25.011096	1501.323580	15.061888
24.845123	1500.141998	15.066906
25.016166	1496.276474	15.071923
25.048102	1494.096670	15.076941
24.828919	1503.432545	15.081959
25.014632	1498.248011	15.086976
24.802401	1506.890624	15.091994
25.312508	1526.754466	15.097011
25.356484	1541.999375	15.102029
25.242873	1543.884035	15.107047
25.650486	1535.790856	15.112064
25.396867	1528.426081	15.117082
25.129661	1510.902146	15.122099
25.165918	1512.015685	15.127117
25.218053	1516.128135	15.132135
25.395321	1536.037995	15.137152
25.271904	1536.791597	15.142170
25.400420	1529.717460	15.147187
25.569822	1533.259060	15.152205
25.406366	1534.411532	15.157223
25.841758	1528.505234	15.162240
25.423683	1524.338030	15.167258
25.641157	1520.226772	15.172275
25.719607	1511.526195	15.177293
25.204127	1502.435839	15.182311
25.676593	1512.919089	15.187328
25.512226	1531.441699	15.192346
25.871393	1525.418567	15.197363
25.633332	1520.309477	15.202381
25.413790	1525.268319	15.207399
25.876765	1527.994644	15.212416
25.578594	1535.248575	15.217434
25.940565	1534.815738	15.222451
25.976447	1535.267070	15.227469
25.430718	1530.189743	15.232487
25.631935	1526.112538	15.237504
25.705071	1537.762227	15.242522
25.899530	1534.087235	15.247539
25.794981	1540.688919	15.252557
25.613070	1539.056827	15.257575
25.809125	1531.732809	15.262592
25.699414	1530.167070	15.267610
25.809264	1535.386425	15.272627
26.209806	1533.089623	15.277645
26.042642	1534.939563	15.282663
26.091005	1532.470045	15.287680
25.856488	1544.128693	15.292698
25.757198	1536.613453	15.297715
26.095645	1533.696534	15.302733
25.833444	1539.333891	15.307751
25.799535	1531.149104	15.312768
26.079365	1543.251128	15.317786
26.131770	1561.714035	15.322803
26.434859	1554.566424	15.327821
26.315919	1558.375036	15.332839
26.477437	1559.104432	15.337856
26.354589	1557.764164	15.342874
26.503955	1552.307758	15.347891
26.369877	1544.614011	15.352909
25.945463	1538.980124	15.357927
26.628159	1543.334161	15.362944
26.644453	1552.555430	15.367962
26.551062	1545.941411	15.372979
26.472697	1536.237817	15.377997
26.169488	1535.133178	15.383015
26.453942	1537.771569	15.388032
26.548493	1553.872048	15.393050
26.274010	1553.520267	15.398067
26.754762	1547.765609	15.403085
26.407802	1557.604049	15.408103
26.584926	1550.677099	15.413120
26.398383	1557.291868	15.418138
26.516487	1557.384795	15.423155
26.728391	1549.417207	15.428173
26.481151	1555.753781	15.433191
26.887061	1555.165279	15.438208
26.799109	1552.608169	15.443226
26.629453	1548.394258	15.448243
26.944371	1550.382827	15.453261
26.545939	1552.114705	15.458279
26.792739	1547.850105	15.463296
26.731973	1554.528974	15.468314
26.621360	1558.018493	15.473331
26.705666	1553.975658	15.478349
26.463870	1553.293035	15.483367
26.774326	1560.812506	15.488384
26.988336	1576.712267	15.493402
27.047277	1577.892983	15.498419
27.231473	1581.160877	15.503437
26.972441	1586.913369	15.508455
27.110965	1588.046785	15.513472
27.278563	1584.483821	15.518490
26.992433	1583.328474	15.523507
27.219185	1579.922824	15.528525
26.815492	1593.314509	15.533543
27.036512	1582.605123	15.538560
27.006367	1589.623631	15.543578
26.795717	1590.946449	15.548595
27.248499	1583.295944	15.553613
27.077487	1584.825594	15.558631
27.186955	1583.246130	15.563648
27.105198	1581.141863	15.568666
26.803784	1581.005171	15.573683
27.603065	1594.440174	15.578701
27.537839	1606.645263	15.583719
27.649904	1590.062017	15.588736
27.603729	1584.472397	15.593754
27.446158	1590.233878	15.598771
27.530855	1583.139962	15.603789
26.922847	1591.240892	15.608807
27.275200	1599.235854	15.613824
27.761685	1610.629333	15.618842
27.856151	1614.561233	15.623859
28.031131	1608.425864	15.628877
27.848769	1598.863089	15.633895
27.963499	1588.080985	15.638912
27.740266	1578.947904	15.643930
27.704079	1580.363238	15.648947
28.114304	1573.241791	15.653965
27.810019	1579.912317	15.658983
27.890000	1579.963345	15.664000
28.244070	1575.522747	15.669018
27.921299	1586.832120	15.674035
28.099842	1577.758449	15.679053
28.012210	1571.024731	15.684071
28.419268	1566.243763	15.689088
28.132540	1573.370041	15.694106
28.103529	1581.130862	15.699123
28.152986	1567.164237	15.704141
27.819384	1583.815973	15.709159
27.860997	1581.734504	15.714176
27.879748	1568.785845	15.719194
27.584907	1573.446027	15.724211
28.041071	1563.136472	15.729229
27.883945	1571.912699	15.734247
28.403796	1570.882863	15.739264
28.361753	1572.559477	15.744282
27.931786	1569.179914	15.749299
28.170411	1567.465804	15.754317
28.191703	1575.264218	15.759335
28.170598	1577.197053	15.764352
28.387377	1574.145367	15.769370
28.179643	1574.736232	15.774387
28.362917	1567.103549	15.779405
28.051216	1576.399955	15.784423
28.105320	1584.910470	15.789440
28.666690	1599.689088	15.794458
28.450464	1608.225427	15.799475
28.559278	1600.258522	15.804493
28.551811	1611.044912	15.809511
28.657691	1601.374814	15.814528
28.885156	1600.581953	15.819546
28.557232	1591.409715	15.824563
28.618318	1575.813078	15.829581
28.457886	1585.908090	15.834599
28.727279	1595.383975	15.839616
28.838744	1599.390242	15.844634
28.682220	1602.334152	15.849651
28.851847	1603.080348	15.854669
28.750650	1605.831384	15.859687
28.845704	1603.953756	15.864704
28.978487	1602.718225	15.869722
29.019255	1604.376915	15.874739
28.735346	1593.700072	15.879757
28.730675	1602.710777	15.884775
28.813834	1602.866695	15.889792
28.885294	1607.219132	15.894810
28.836177	1609.776237	15.899827
29.024606	1601.714046	15.904845
29.022817	1605.126444	15.909863
28.755375	1608.858074	15.914880
28.934603	1606.127776	15.919898
28.878736	1611.530897	15.924915
28.726148	1613.430435	15.929933
28.802082	1611.004486	15.934951
28.950588	1606.856224	15.939968
29.179835	1623.043055	15.944986
28.985586	1637.638615	15.950003
29.336992	1628.627796	15.955021
29.400963	1634.490034	15.960039
29.128541	1632.235262	15.965056
29.380288	1629.092254	15.970074
29.419903	1636.188538	15.975091
29.496864	1637.126488	15.980109
29.646947	1633.047970	15.985127
29.110541	1640.881094	15.990144
29.717401	1633.479708	15.995162
29.240710	1639.389636	16.000179
29.423944	1628.129367	16.005197
29.358692	1630.534100	16.010215
29.201992	1636.203433	16.015232
29.427305	1627.605212	16.020250
29.310529	1629.360608	16.025267
29.531362	1631.239133	16.030285
29.513918	1637.462797	16.035303
29.511865	1635.125578	16.040320
29.442370	1632.890354	16.045338
29.466535	1637.566535	16.050355
30.035573	1645.655172	16.055373
29.892925	1654.631283	16.060391
29.665596	1654.158715	16.065408
29.903003	1660.444782	16.070426
29.879309	1660.149746	16.075443
29.805032	1657.779208	16.080461
29.999230	1658.196643	16.085479
29.934482	1665.986805	16.090496
30.404591	1654.239510	16.095514
30.239476	1661.587118	16.100531
30.172687	1651.559902	16.105549
30.245490	1629.280394	16.110567
30.101435	1635.468406	16.115584
30.237638	1631.513230	16.120602
30.118892	1621.492749	16.125619
30.142856	1627.704299	16.130637
30.109853	1627.983355	16.135655
30.364140	1627.144528	16.140672
30.338573	1623.536853	16.145690
30.081957	1628.079266	16.150707
30.207091	1633.515665	16.155725
30.381596	1650.242963	16.160743
30.260775	1660.586551	16.165760
30.507076	1653.398397	16.170778
30.253466	1658.305298	16.175795
30.275923	1652.041646	16.180813
30.451846	1659.241263	16.185831
30.292774	1653.743558	16.190848
30.280830	1652.863029	16.195866
30.153287	1663.550626	16.200883
30.155517	1663.334830	16.205901
30.585535	1652.065073	16.210919
30.362083	1664.165665	16.215936
30.333079	1670.686143	16.220954
30.368436	1679.314540	16.225971
30.728289	1691.949006	16.230989
30.870056	1691.864333	16.236007
30.892899	1689.934500	16.241024
31.034025	1679.750617	16.246042
30.782785	1699.515887	16.251059
30.787437	1695.629655	16.256077
30.823656	1691.881541	16.261095
30.623324	1691.090833	16.266112
31.151316	1688.811435	16.271130
30.972721	1693.214004	16.276147
30.844729	1694.741523	16.281165
30.887464	1694.650620	16.286183
30.759958	1700.362516	16.291200
31.168587	1688.294646	16.296218
30.953879	1699.444506	16.301235
30.912297	1699.192436	16.306253
31.097085	1690.502322	16.311271
31.058060	1697.445216	16.316288
30.966877	1697.320612	16.321306
30.908056	1696.129003	16.326323
31.183253	1707.888969	16.331341
31.622421	1711.047798	16.336359
31.195737	1718.666825	16.341376
31.518844	1714.413604	16.346394
31.457678	1709.395791	16.351411
31.331576	1706.829794	16.356429
31.413959	1711.854595	16.361447
31.337243	1720.556736	16.366464
31.821716	1719.032286	16.371482
31.816270	1723.066671	16.376499
31.620642	1697.925916	16.381517
31.538341	1690.492835	16.386535
31.326409	1699.896108	16.391552
31.840143	1706.923891	16.396570
31.832351	1714.513076	16.401587
31.657854	1706.554329	16.406605
31.560285	1701.344114	16.411623
31.505841	1718.119802	16.416640
31.646035	1715.499534	16.421658
31.794402	1718.945429	16.426675
31.749890	1719.441838	16.431693
32.329857	1712.216171	16.436711
31.948184	1715.590861	16.441728
32.242027	1708.941752	16.446746
32.437033	1711.830407	16.451763
31.849232	1700.351688	16.456781
32.011446	1680.357719	16.461799
31.917038	1686.347489	16.466816
31.953864	1691.520341	16.471834
32.321903	1706.517888	16.476851
32.153029	1699.878868	16.481869
32.514379	1694.263540	16.486887
32.129385	1687.909904	16.491904
32.271465	1676.283336	16.496922
32.071108	1674.297076	16.501939
32.137294	1696.483845	16.506957
32.575395	1698.805165	16.511975
32.075702	1696.501682	16.516992
32.331019	1703.948221	16.522010
32.314015	1703.354014	16.527027
32.222792	1705.748743	16.532045
32.577286	1704.370873	16.537063
32.234783	1703.744417	16.542080
32.426892	1703.642276	16.547098
32.534700	1705.814917	16.552115
32.311837	1719.479125	16.557133
32.639513	1705.847114	16.562151
32.550130	1707.911985	16.567168
32.556068	1708.228092	16.572186
32.590082	1705.362838	16.577203
32.603338	1709.348617	16.582221
32.842473	1704.415053	16.587239
32.525405	1710.757324	16.592256
32.418310	1706.450015	16.597274
32.767692	1706.670447	16.602291
32.137079	1714.546163	16.607309
32.674147	1723.123673	16.612327
32.572328	1735.422013	16.617344
32.483631	1741.367634	16.622362
32.962763	1736.870862	16.627379
32.910979	1737.316518	16.632397
32.986081	1739.845183	16.637415
33.140196	1743.193420	16.642432
32.955285	1735.021589	16.647450
33.309755	1739.833111	16.652467
33.209513	1742.362212	16.657485
33.226027	1741.412641	16.662503
33.314133	1737.767144	16.667520
33.328636	1746.015069	16.672538
33.075272	1739.472881	16.677555
33.189654	1739.064582	16.682573
33.481302	1734.514337	16.687591
33.454070	1737.119100	16.692608
33.019453	1741.988826	16.697626
33.501621	1737.814843	16.702643
33.174167	1746.361136	16.707661
33.590548	1739.778991	16.712679
33.325030	1751.650397	16.717696
33.304439	1760.182367	16.722714
33.718993	1756.367606	16.727731
33.620785	1766.882277	16.732749
33.800594	1766.971658	16.737767
34.023925	1768.766428	16.742784
33.703511	1767.874523	16.747802
33.882421	1750.876931	16.752819
33.430127	1755.467107	16.757837
33.798487	1758.916467	16.762855
34.194392	1773.520295	16.767872
34.001854	1764.602436	16.772890
34.032837	1752.800033	16.777907
33.965098	1746.669495	16.782925
34.010308	1732.992054	16.787943
33.982389	1748.936094	16.792960
33.944240	1743.480420	16.797978
34.078507	1733.854473	16.802995
33.667593	1726.178039	16.808013
33.912437	1737.196430	16.813031
34.117095	1753.753862	16.818048
34.148992	1762.706921	16.823066
34.350036	1756.451710	16.828083
34.126950	1767.989156	16.833101
34.396625	1765.985338	16.838119
34.364331	1761.499334	16.843136
34.285595	1774.490127	16.848154
34.428160	1763.361302	16.853171
34.278049	1760.268200	16.858189
34.117331	1759.718148	16.863207
34.581518	1763.113684	16.868224
34.657272	1765.886082	16.873242
34.533311	1766.220548	16.878259
34.639797	1772.857897	16.883277
34.718859	1757.088303	16.888295
34.490050	1760.076022	16.893312
34.077060	1766.612163	16.898330
34.553272	1759.169415	16.903347
34.233635	1764.478586	16.908365
34.482259	1767.310721	16.913383
34.574345	1765.016671	16.918400
34.800538	1762.477853	16.923418
34.543233	1766.821419	16.928435
34.499686	1772.005546	16.933453
34.863992	1777.910397	16.938471
34.706058	1779.290108	16.943488
34.712410	1794.967595	16.948506
35.313999	1789.440552	16.953523
34.817420	1798.394542	16.958541
35.243265	1798.389624	16.963559
34.866840	1797.490133	16.968576
34.744349	1800.516749	16.973594
35.104418	1795.622859	16.978611
35.126862	1797.990036	16.983629
34.880038	1792.602233	16.988647
34.975956	1786.963131	16.993664
34.798051	1797.691894	16.998682
34.930725	1788.020545	17.003699
34.898973	1808.541447	17.008717
35.026800	1818.514350	17.013735
35.196201	1823.305863	17.018752
35.206164	1832.282913	17.023770
35.642012	1822.043275	17.028787
35.721393	1829.160054	17.033805
35.638844	1817.178280	17.038823
35.679137	1814.640784	17.043840
35.725347	1828.966152	17.048858
35.674318	1819.656794	17.053875
35.741875	1817.628572	17.058893
35.636586	1825.341910	17.063911
35.780496	1815.866964	17.068928
35.497167	1826.428506	17.073946
35.878857	1825.679468	17.078963
35.716600	1822.536376	17.083981
35.928936	1823.776024	17.088999
35.789453	1820.567949	17.094016
35.776859	1820.671497	17.099034
35.653201	1815.626646	17.104051
35.757861	1827.491775	17.109069
35.674957	1817.277455	17.114087
35.388858	1818.506927	17.119104
35.398675	1825.243879	17.124122
35.842483	1844.765568	17.129139
36.060346	1847.470483	17.134157
36.295688	1848.293520	17.139175
36.310247	1849.075471	17.144192
36.044095	1855.751051	17.149210
36.579404	1842.416941	17.154227
36.523365	1850.536168	17.159245
36.258550	1849.034459	17.164263
36.305921	1843.152952	17.169280
36.183891	1852.859755	17.174298
36.506794	1840.324059	17.179315
36.219587	1848.149010	17.184333
36.482274	1846.899820	17.189351
36.655687	1840.695387	17.194368
36.366575	1847.717565	17.199386
36.625106	1840.465231	17.204403
36.387238	1848.563902	17.209421
36.258505	1851.206897	17.214439
36.574475	1843.025912	17.219456
36.228158	1849.391785	17.224474
36.856199	1850.536034	17.229491
36.810798	1865.908014	17.234509
36.848673	1874.414209	17.239527
36.968349	1874.600489	17.244544
36.821343	1879.097967	17.249562
37.157143	1864.244558	17.254579
37.382235	1854.770011	17.259597
36.755166	1853.553390	17.264615
37.094588	1847.971390	17.269632
36.940682	1848.163547	17.274650
36.934500	1850.853068	17.279667
37.122841	1863.851686	17.284685
37.074237	1870.546063	17.289703
37.279823	1867.255415	17.294720
37.042098	1866.525719	17.299738
37.500614	1867.460251	17.304755
37.660561	1864.440380	17.309773
37.337321	1873.967703	17.314791
37.529493	1863.942301	17.319808
37.151004	1864.929306	17.324826
37.233499	1866.099997	17.329843
37.525000	1866.706427	17.334861
37.486524	1864.205082	17.339879
37.527278	1863.429400	17.344896
37.334903	1869.017992	17.349914
37.645219	1868.176509	17.354931
37.705295	1868.875693	17.359949
37.764128	1871.458888	17.364967
37.985589	1871.177449	17.369984
37.502825	1864.103107	17.375002
37.878428	1866.435209	17.380019
37.952591	1869.160686	17.385037
37.701325	1871.724906	17.390055
37.850699	1853.975232	17.395072
37.747582	1859.624308	17.400090
37.810428	1863.506260	17.405107
38.078806	1862.249869	17.410125
37.712816	1866.437755	17.415143
37.815599	1859.008892	17.420160
37.961387	1868.831879	17.425178
37.839774	1858.224916	17.430195
37.800906	1863.697783	17.435213
37.463618	1860.069760	17.440231
38.168858	1875.864763	17.445248
38.053928	1887.112903	17.450266
38.001025	1894.170582	17.455283
38.017525	1887.092114	17.460301
38.012237	1893.346984	17.465319
37.904237	1889.174267	17.470336
38.143579	1903.621500	17.475354
38.354878	1915.048096	17.480371
38.785474	1916.471608	17.485389
38.576219	1931.642473	17.490407
38.848225	1923.660377	17.495424
38.842951	1915.134158	17.500442
38.156712	1916.227666	17.505459
38.923671	1911.087937	17.510477
38.676458	1927.189062	17.515495
38.920306	1923.740492	17.520512
38.656595	1925.479242	17.525530
38.837129	1931.859446	17.530547
38.870851	1931.898190	17.535565
38.541621	1938.196877	17.540583
39.159202	1925.684903	17.545600
38.886672	1929.714746	17.550618
38.917182	1933.391074	17.555635
39.498953	1928.399645	17.560653
39.208023	1936.936291	17.565671
39.130012	1934.063688	17.570688
38.872809	1932.091177	17.575706
39.157140	1928.806048	17.580723
39.329841	1927.376136	17.585741
39.289860	1935.765000	17.590759
39.175048	1923.460286	17.595776
38.956343	1925.887966	17.600794
39.040820	1925.287791	17.605811
39.306264	1929.710068	17.610829
39.026994	1934.109886	17.615847
39.189570	1927.109568	17.620864
39.417964	1934.777612	17.625882
39.489297	1928.262998	17.630899
39.475860	1925.953504	17.635917
39.380628	1939.333277	17.640935
39.831199	1944.938130	17.645952
39.509631	1953.154034	17.650970
39.698204	1955.965894	17.655987
39.931220	1955.402594	17.661005
40.215028	1950.453171	17.666023
39.907714	1937.070876	17.671040
39.516301	1937.949828	17.676058
39.857963	1943.745093	17.681075
40.171882	1942.374460	17.686093
39.857868	1955.133145	17.691111
39.986349	1961.662460	17.696128
40.085480	1956.080200	17.701146
40.231111	1957.535005	17.706163
40.187531	1948.006498	17.711181
40.236828	1953.968740	17.716199
40.203993	1956.449371	17.721216
40.386213	1954.127546	17.726234
40.398147	1940.439487	17.731251
40.308871	1925.113438	17.736269
39.999239	1938.613139	17.741287
40.103676	1940.982207	17.746304
40.181167	1948.507574	17.751322
39.956122	1954.388504	17.756339
40.267123	1946.369501	17.761357
40.179700	1955.297660	17.766375
40.283288	1957.722713	17.771392
40.409444	1962.855459	17.776410
40.373130	1971.837615	17.781427
40.850499	1974.974681	17.786445
40.634007	1991.266046	17.791463
40.874706	1975.372904	17.796480
41.033068	1983.371488	17.801498
40.526935	1980.937627	17.806515
40.761314	1972.161568	17.811533
40.803335	1978.076999	17.816551
40.941433	1974.957550	17.821568
41.153510	1979.061928	17.826586
40.874807	1983.827424	17.831603
41.152442	1975.934071	17.836621
40.910390	1985.440652	17.841639
41.083516	1983.369614	17.846656
41.109258	1984.429808	17.851674
40.916911	1977.667767	17.856691
40.959318	1975.619151	17.861709
41.089285	1976.208087	17.866727
40.955192	1975.895255	17.871744
41.237785	1986.321038	17.876762
40.963290	2001.931059	17.881779
41.546822	1997.974449	17.886797
41.477842	2008.479127	17.891815
41.721792	2001.193644	17.896832
41.999541	2001.740134	17.901850
41.664616	2001.895090	17.906867
41.626140	1983.401235	17.911885
41.576339	1985.756367	17.916903
41.533772	1989.452230	17.921920
41.757651	1992.897159	17.926938
41.763605	2001.799443	17.931955
42.006133	1994.209788	17.936973
42.280384	1997.597132	17.941991
41.817998	1985.455557	17.947008
41.911729	1970.836500	17.952026
41.754694	1973.300760	17.957043
41.756293	1981.421093	17.962061
42.023584	1985.512734	17.967079
42.031820	1994.647473	17.972096
42.114895	1996.174398	17.977114
41.705924	2005.194770	17.982131
42.111522	1995.309073	17.987149
41.962600	1997.782269	17.992167
41.695127	2002.751274	17.997184
41.850959	1999.823273	18.002202
41.968318	2017.056432	18.007219
42.324070	2024.882764	18.012237
42.185506	2028.881830	18.017255
42.217276	2031.880746	18.022272
42.481428	2025.970099	18.027290
42.218639	2033.680348	18.032307
42.330735	2025.676505	18.037325
42.365081	2029.692830	18.042343
42.281518	2029.079335	18.047360
42.846800	2035.562619	18.052378
42.812827	2059.448387	18.057395
42.995583	2055.090028	18.062413
42.785449	2050.671625	18.067431
42.757350	2052.126616	18.072448
43.086897	2050.459304	18.077466
43.074812	2060.862131	18.082483
42.993565	2054.278979	18.087501
42.783327	2051.249676	18.092519
42.951574	2061.493959	18.097536
43.345708	2056.682647	18.102554
42.961664	2052.531096	18.107571
43.329270	2053.472275	18.112589
42.891725	2060.270456	18.117607
42.954631	2054.224353	18.122624
43.387990	2050.253924	18.127642
43.064132	2061.926444	18.132659
43.300790	2060.773418	18.137677
43.443323	2057.088486	18.142695
43.274773	2057.316803	18.147712
43.636671	2061.986453	18.152730
43.383305	2059.107182	18.157747
43.629313	2058.549672	18.162765
43.878097	2061.165533	18.167783
43.406435	2056.920194	18.172800
43.646125	2049.944489	18.177818
43.327927	2064.111110	18.182835
43.351922	2062.898397	18.187853
43.517316	2078.697128	18.192871
43.526646	2098.475654	18.197888
44.005536	2084.565900	18.202906
44.020521	2092.084791	18.207923
44.133970	2085.724637	18.212941
44.047181	2085.077045	18.217959
43.977708	2080.335729	18.222976
44.311195	2071.473013	18.227994
43.679460	2089.576899	18.233011
44.223851	2083.440625	18.238029
44.352411	2080.015124	18.243047
44.376405	2082.496153	18.248064
44.120131	2077.869579	18.253082
44.230693	2079.573827	18.258099
44.489828	2081.269325	18.263117
44.351351	2082.673491	18.268135
44.308279	2082.213210	18.273152
44.847618	2076.353044	18.278170
44.475974	2081.698152	18.283187
44.114787	2079.812995	18.288205
44.686800	2081.029127	18.293223
44.643508	2090.741622	18.298240
44.745422	2093.248768	18.303258
44.451609	2103.676892	18.308275
44.843167	2105.234074	18.313293
44.715536	2112.345464	18.318311
44.523893	2118.040221	18.323328
45.022229	2100.502817	18.328346
44.817657	2111.023687	18.333363
44.681618	2111.192546	18.338381
44.940985	2114.999962	18.343399
44.919018	2114.542607	18.348416
44.925646	2108.893237	18.353434
45.271800	2107.903657	18.358451
44.939029	2122.003440	18.363469
45.458643	2120.201981	18.368487
45.468438	2135.585893	18.373504
45.366368	2116.267455	18.378522
45.156678	2122.241966	18.383539
45.276462	2134.576093	18.388557
45.363642	2131.116278	18.393575
45.442722	2141.158530	18.398592
45.529549	2129.623005	18.403610
45.279572	2144.973631	18.408627
45.634311	2135.899045	18.413645
45.567623	2139.236968	18.418663
45.711904	2147.666572	18.423680
45.785996	2134.515874	18.428698
45.694798	2141.777210	18.433715
45.468776	2145.434724	18.438733
45.788408	2137.887759	18.443751
45.222487	2144.829945	18.448768
45.844329	2155.431425	18.453786
45.908495	2165.929927	18.458803
46.238253	2168.875056	18.463821
46.069052	2161.473684	18.468839
46.179554	2174.341050	18.473856
46.363689	2170.360781	18.478874
46.119989	2168.819487	18.483891
45.892718	2179.287393	18.488909
46.357117	2170.125292	18.493927
46.344443	2169.118995	18.498944
46.404534	2167.341261	18.503962
46.374572	2164.235989	18.508979
46.331148	2159.388238	18.513997
46.601224	2161.734859	18.519015
46.370999	2169.296829	18.524032
46.595036	2156.524139	18.529050
46.641432	2165.654473	18.534067
46.622341	2165.760633	18.539085
47.064974	2162.518639	18.544103
46.808149	2168.560465	18.549120
46.929147	2164.295300	18.554138
46.824623	2165.915087	18.559155
46.781338	2168.236173	18.564173
46.542294	2163.328375	18.569191
46.555488	2184.633147	18.574208
46.944844	2185.846956	18.579226
46.957660	2195.423934	18.584243
46.907539	2199.492319	18.589261
46.940087	2189.011553	18.594279
47.062048	2194.358999	18.599296
47.182900	2189.086244	18.604314
47.091247	2198.267718	18.609331
47.402618	2194.632123	18.614349
47.504221	2189.002972	18.619367
47.083581	2209.529037	18.624384
47.512727	2211.963566	18.629402
47.714636	2213.037370	18.634419
47.367130	2219.931386	18.639437
48.060031	2221.291860	18.644455
47.583506	2221.930334	18.649472
47.897722	2216.447392	18.654490
47.736443	2225.333221	18.659507
47.707426	2234.326960	18.664525
47.903465	2224.614541	18.669543
47.820347	2235.623475	18.674560
48.136789	2225.538680	18.679578
48.182030	2224.120414	18.684595
47.861903	2230.122806	18.689613
47.885754	2224.208714	18.694631
47.814627	2226.890570	18.699648
47.924877	2229.072339	18.704666
47.872586	2222.895874	18.709683
48.116886	2226.169276	18.714701
48.132522	2221.632223	18.719719
47.911005	2236.908401	18.724736
48.292089	2237.130869	18.729754
48.599641	2246.667956	18.734771
48.284175	2246.836327	18.739789
48.859321	2242.103063	18.744807
48.539115	2250.683101	18.749824
48.795789	2243.819437	18.754842
48.843860	2243.033129	18.759859
48.719648	2247.418537	18.764877
48.846870	2234.957760	18.769895
48.737179	2239.484007	18.774912
49.207873	2240.478765	18.779930
48.917751	2237.919165	18.784947
48.842203	2243.608041	18.789965
49.011586	2239.843270	18.794983
48.881172	2245.013887	18.800000
48.734458	2246.590070	18.805018
48.989247	2240.123931	18.810035
49.096822	2238.978892	18.815053
48.948305	2232.215248	18.820071
49.040122	2243.875109	18.825088
49.041443	2231.505205	18.830106
49.252020	2239.131417	18.835123
48.909531	2238.418408	18.840141
49.319254	2259.217993	18.845159
49.550985	2268.008134	18.850176
49.534908	2267.235989	18.855194
49.193546	2275.884702	18.860211
49.144565	2281.915452	18.865229
49.504389	2271.300629	18.870247
49.510407	2277.645891	18.875264
49.494877	2274.815958	18.880282
49.458241	2275.672170	18.885299
49.576329	2300.423707	18.890317
49.833978	2290.855589	18.895335
50.024943	2301.136534	18.900352
50.068147	2299.116063	18.905370
50.167031	2298.838435	18.910387
50.103639	2298.408918	18.915405
50.140902	2296.777967	18.920423
50.246164	2297.909666	18.925440
50.059915	2304.028390	18.930458
50.437673	2292.078218	18.935475
50.121147	2304.917838	18.940493
50.359423	2296.411549	18.945511
50.471480	2304.468823	18.950528
50.421892	2296.656588	18.955546
50.716119	2296.866952	18.960563
50.468911	2298.167344	18.965581
50.708249	2292.973979	18.970599
50.504379	2297.498745	18.975616
50.631757	2292.182437	18.980634
50.719723	2286.307650	18.985651
50.582615	2302.848633	18.990669
50.646500	2295.325069	18.995687
50.628894	2309.171831	19.000704
50.524711	2320.111822	19.005722
50.785487	2329.181325	19.010739
50.787495	2330.531646	19.015757
51.134546	2330.665940	19.020775
50.849114	2334.524115	19.025792
50.696745	2339.744675	19.030810
51.007735	2321.939556	19.035827
50.933318	2330.832833	19.040845
51.346339	2342.955975	19.045863
51.584498	2355.542783	19.050880
51.203223	2363.151752	19.055898
51.616339	2357.908626	19.060915
51.484952	2360.860477	19.065933
51.744024	2358.983340	19.070951
52.091893	2368.953780	19.075968
51.641838	2354.067098	19.080986
51.929353	2333.698289	19.086003
51.392254	2333.835146	19.091021
51.473724	2345.183677	19.096039
51.781627	2348.048950	19.101056
51.885538	2349.998132	19.106074
51.919898	2351.536009	19.111091
51.696095	2360.426385	19.116109
51.974671	2357.291531	19.121127
52.025976	2357.757735	19.126144
51.818078	2358.541368	19.131162
52.132157	2356.970881	19.136179
51.950788	2360.614247	19.141197
52.179535	2365.320176	19.146215
52.310338	2379.421001	19.151232
52.136260	2389.237930	19.156250
52.440263	2384.484150	19.161267
52.217522	2394.223891	19.166285
52.192535	2390.959673	19.171303
52.489097	2391.329344	19.176320
52.316236	2391.920970	19.181338
52.535361	2386.605728	19.186355
52.506186	2398.298379	19.191373
52.152746	2399.401769	19.196391
52.435751	2403.090650	19.201408
52.695903	2410.650839	19.206426
52.883987	2406.852366	19.211443
52.653653	2412.102690	19.216461
52.842745	2405.547059	19.221479
53.002899	2408.391858	19.226496
53.015831	2407.951739	19.231514
53.145586	2412.571214	19.236531
53.142116	2436.983683	19.241549
53.061646	2440.285328	19.246567
53.135213	2435.314998	19.251584
53.172989	2436.598271	19.256602
53.418337	2423.536417	19.261619
53.894699	2428.271312	19.266637
53.925332	2428.076145	19.271655
54.089899	2431.617951	19.276672
54.157033	2425.324031	19.281690
54.217452	2400.911299	19.286707
54.030924	2397.605195	19.291725
53.744182	2397.287593	19.296743
53.763330	2392.351127	19.301760
53.801222	2397.148858	19.306778
53.858477	2393.522277	19.311795
53.621544	2398.928608	19.316813
53.656644	2394.426154	19.321831
53.779877	2407.697576	19.326848
53.679978	2431.824937	19.331866
54.013264	2430.684004	19.336883
53.910489	2428.415422	19.341901
53.716842	2430.973694	19.346919
53.978100	2429.481630	19.351936
54.260527	2448.813557	19.356954
54.590312	2448.059398	19.361971
54.267085	2451.353351	19.366989
54.673727	2458.396224	19.372007
54.936322	2442.579316	19.377024
54.654894	2460.040993	19.382042
54.934996	2458.294211	19.387059
54.818087	2457.756809	19.392077
54.620587	2457.541389	19.397095
54.821413	2450.431679	19.402112
54.649362	2457.172756	19.407130
55.177964	2451.652391	19.412147
54.998151	2455.392283	19.417165
54.757667	2455.104273	19.422183
55.113210	2452.228499	19.427200
54.897057	2459.360467	19.432218
54.761101	2455.697824	19.437235
54.830558	2455.726937	19.442253
54.872965	2473.367458	19.447271
55.467155	2484.108886	19.452288
55.363122	2492.355685	19.457306
55.676042	2488.864506	19.462323
55.595334	2493.755122	19.467341
55.648747	2489.798761	19.472359
55.650318	2478.280490	19.477376
55.190281	2482.190146	19.482394
55.390996	2485.092206	19.487411
55.734415	2484.596234	19.492429
55.544827	2483.462383	19.497447
55.560037	2499.254058	19.502464
55.392754	2523.373438	19.507482
55.854945	2510.224224	19.512499
55.947245	2517.469855	19.517517
55.791206	2522.091679	19.522535
56.142505	2514.578802	19.527552
56.014868	2530.294179	19.532570
56.018518	2523.006644	19.537587
56.407986	2514.251151	19.542605
56.089578	2523.770257	19.547623
56.402582	2537.376514	19.552640
56.400875	2552.966429	19.557658
56.589971	2548.871211	19.562675
56.492339	2548.649302	19.567693
56.449730	2562.243073	19.572711
56.909645	2548.857422	19.577728
56.614730	2544.922773	19.582746
56.864189	2547.784034	19.587763
56.846422	2543.421328	19.592781
56.905958	2549.873017	19.597799
56.960708	2543.892513	19.602816
56.738549	2545.358049	19.607834
56.613851	2544.318463	19.612851
56.868491	2536.868972	19.617869
56.924814	2540.807993	19.622887
57.238570	2547.125534	19.627904
56.939941	2559.888582	19.632922
57.072694	2564.892274	19.637939
57.428040	2569.704723	19.642957
57.368887	2566.538732	19.647975
57.332235	2561.265005	19.652992
57.434600	2569.254751	19.658010
57.439611	2563.594451	19.663027
57.489116	2558.179555	19.668045
57.343138	2562.316816	19.673063
57.621741	2560.389344	19.678080
57.735515	2583.078015	19.683098
57.790555	2584.039975	19.688115
57.851210	2592.486320	19.693133
57.831464	2592.352675	19.698151
58.133717	2585.348648	19.703168
58.065794	2589.318508	19.708186
58.539478	2587.064161	19.713203
58.819427	2584.331780	19.718221
58.281224	2589.788585	19.723239
58.412070	2589.071651	19.728256
58.521213	2576.950918	19.733274
58.509765	2586.387287	19.738291
58.900687	2584.051747	19.743309
58.674121	2584.809264	19.748327
58.788998	2577.533068	19.753344
58.666668	2572.903066	19.758362
58.805113	2576.665388	19.763379
58.895206	2578.645909	19.768397
58.567013	2585.758835	19.773415
58.894792	2580.678695	19.778432
58.792586	2584.922252	19.783450
58.711233	2580.945668	19.788467
58.835232	2583.222050	19.793485
58.641906	2581.594804	19.798503
58.987693	2583.674564	19.803520
59.189326	2586.424684	19.808538
58.858768	2578.665757	19.813555
58.940356	2584.922015	19.818573
58.606342	2618.077065	19.823591
59.077864	2614.182209	19.828608
59.246203	2615.708973	19.833626
58.795802	2618.531619	19.838643
59.213016	2631.720179	19.843661
59.282302	2643.084256	19.848679
59.405866	2638.638414	19.853696
59.539200	2646.455717	19.858714
59.772375	2646.933830	19.863731
60.161567	2641.074578	19.868749
59.895239	2647.944047	19.873767
60.137475	2642.075980	19.878784
60.161058	2640.262321	19.883802
59.988368	2654.112116	19.888819
60.025532	2658.786552	19.893837
60.121429	2645.823849	19.898855
60.033575	2648.004236	19.903872
59.851271	2653.047190	19.908890
60.024549	2670.466494	19.913907
60.598284	2672.869393	19.918925
60.321175	2681.309086	19.923943
60.382083	2685.683981	19.928960
60.641476	2674.735631	19.933978
60.422667	2682.189065	19.938995
60.526153	2672.490324	19.944013
60.462811	2679.359688	19.949031
60.948319	2682.577422	19.954048
60.718764	2697.698827	19.959066
60.689061	2707.729713	19.964083
61.200834	2696.989666	19.969101
61.134411	2712.216434	19.974119
61.236743	2705.498306	19.979136
61.206260	2703.177248	19.984154
61.241129	2707.638109	19.989171
61.363107	2696.988542	19.994189
61.535844	2710.308194	19.999207
61.407102	2703.086519	20.004224
61.469964	2700.811144	20.009242
61.441510	2699.106462	20.014259
61.636098	2701.464425	20.019277
61.496206	2703.755379	20.024295
61.792347	2706.023994	20.029312
61.827546	2702.603799	20.034330
61.398502	2705.040764	20.039347
61.633925	2698.427271	20.044365
61.780769	2722.684883	20.049383
61.732890	2725.808342	20.054400
62.030391	2727.248446	20.059418
62.081704	2728.938621	20.064435
62.215338	2715.390896	20.069453
62.153779	2728.169772	20.074471
62.238207	2725.204247	20.079488
62.230306	2728.035792	20.084506
62.175713	2729.029404	20.089523
62.400292	2727.775996	20.094541
62.284384	2728.172126	20.099559
62.394913	2720.107586	20.104576
62.502349	2741.333639	20.109594
62.193429	2764.749964	20.114611
62.622175	2750.640701	20.119629
62.487775	2756.911025	20.124647
62.571072	2760.581504	20.129664
62.966554	2759.965523	20.134682
62.701934	2767.930522	20.139699
63.520701	2743.559898	20.144717
63.508856	2744.985621	20.149735
63.597696	2739.027132	20.154752
63.680416	2743.572406	20.159770
63.386910	2746.091595	20.164787
63.889055	2742.572541	20.169805
63.668671	2749.942880	20.174823
63.681145	2744.046910	20.179840
63.700627	2745.988372	20.184858
63.492298	2741.244600	20.189875
63.722529	2743.734542	20.194893
63.572180	2752.022697	20.199911
64.064171	2742.976194	20.204928
63.959963	2746.556219	20.209946
63.833013	2752.609036	20.214963
63.995531	2739.590003	20.219981
63.841547	2744.774780	20.224999
63.597644	2750.872205	20.230016
64.021517	2747.844676	20.235034
63.491296	2748.557019	20.240051
63.975239	2761.544697	20.245069
64.208500	2774.207377	20.250087
64.409140	2771.091945	20.255104
64.603135	2769.434374	20.260122
64.164961	2775.848330	20.265139
64.623826	2770.245363	20.270157
64.864053	2776.045343	20.275175
64.246834	2775.701772	20.280192
64.607591	2776.036046	20.285210
64.731578	2798.024127	20.290227
65.012755	2794.680316	20.295245
65.004505	2807.883397	20.300263
65.324413	2799.988368	20.305280
65.218036	2810.545996	20.310298
64.979530	2808.462614	20.315315
65.248757	2798.620153	20.320333
65.272617	2802.540824	20.325351
64.917475	2802.480328	20.330368
65.390691	2807.124604	20.335386
65.460168	2797.288827	20.340403
65.463288	2793.264103	20.345421
65.572363	2810.781915	20.350439
65.380208	2807.364128	20.355456
65.769898	2804.464751	20.360474
65.397472	2809.676520	20.365491
65.387320	2803.615800	20.370509
65.325759	2818.855276	20.375527
65.441051	2825.722179	20.380544
65.839718	2827.675551	20.385562
65.378515	2828.378464	20.390579
65.711540	2842.440409	20.395597
65.974733	2855.275374	20.400615
65.817557	2870.214718	20.405632
66.128610	2852.364897	20.410650
66.034650	2855.179513	20.415667
66.433749	2862.632825	20.420685
66.276491	2854.319082	20.425703
66.196499	2871.649225	20.430720
66.587538	2872.861256	20.435738
66.599653	2889.654419	20.440755
66.789134	2893.611632	20.445773
66.877147	2890.139707	20.450791
66.834148	2890.787730	20.455808
67.071806	2884.492377	20.460826
66.721643	2891.645138	20.465843
66.817651	2880.982274	20.470861
67.378357	2879.794817	20.475879
67.141345	2884.052878	20.480896
67.102050	2885.239928	20.485914
66.986756	2887.160424	20.490931
66.945133	2898.026368	20.495949
67.320736	2904.176093	20.500967
67.188532	2912.031951	20.505984
67.210647	2909.984868	20.511002
67.275071	2916.418634	20.516019
67.186936	2912.866241	20.521037
68.112386	2923.743173	20.526055
68.110031	2936.625277	20.531072
68.292988	2935.705722	20.536090
68.071850	2944.207435	20.541107
68.021750	2933.468719	20.546125
68.423248	2936.065895	20.551143
68.306260	2943.011586	20.556160
68.322325	2930.446805	20.561178
68.283686	2928.177356	20.566195
67.911704	2935.167641	20.571213
68.193021	2931.622403	20.576231
68.269007	2931.611932	20.581248
68.407879	2933.512354	20.586266
68.530071	2939.770155	20.591283
68.433453	2933.077357	20.596301
68.558267	2939.053917	20.601319
68.285624	2971.461343	20.606336
68.874295	2961.129685	20.611354
68.474964	2967.723957	20.616371
68.484028	2971.916843	20.621389
69.166825	2966.608473	20.626407
68.931154	2966.370813	20.631424
69.200251	2980.114279	20.636442
69.177072	2991.328969	20.641459
69.285305	2981.830642	20.646477
69.571677	2991.545440	20.651495
69.732667	2995.614991	20.656512
70.347469	2972.768737	20.661530
70.038924	2970.983616	20.666547
70.100268	2967.323204	20.671565
70.018585	2940.459888	20.676583
69.638649	2955.802981	20.681600
70.004908	2945.363637	20.686618
70.046588	2934.587472	20.691635
70.054580	2949.017574	20.696653
70.188566	2942.329688	20.701671
70.038668	2936.391886	20.706688
70.070379	2937.028783	20.711706
70.338318	2942.687539	20.716723
70.347871	2938.757717	20.721741
70.584284	2936.818834	20.726759
70.290900	2944.050666	20.731776
70.777624	2961.475397	20.736794
70.949081	2974.295205	20.741811
70.634241	2966.052938	20.746829
70.701208	2971.096365	20.751847
70.886127	2974.591795	20.756864
70.988572	2966.481999	20.761882
70.860101	2969.907838	20.766899
70.439180	2974.757686	20.771917
70.904084	2974.800828	20.776935
70.858025	2971.470618	20.781952
70.858254	2968.134600	20.786970
70.861350	2988.752289	20.791987
71.217693	3003.185103	20.797005
71.379756	2990.867586	20.802023
71.214999	3004.979965	20.807040
71.337652	3003.163049	20.812058
71.452294	3006.101752	20.817075
71.663093	3007.296127	20.822093
71.436922	3003.730327	20.827111
71.520665	3021.496283	20.832128
71.620811	3026.713789	20.837146
71.770553	3021.993845	20.842163
71.874001	3028.360081	20.847181
72.023662	3029.913468	20.852199
72.151760	3028.459100	20.857216
72.254796	3025.607753	20.862234
72.234027	3035.632719	20.867251
72.331093	3059.050848	20.872269
72.813724	3051.930520	20.877287
72.847949	3063.523918	20.882304
72.829092	3049.735896	20.887322
72.875152	3054.469610	20.892339
72.806150	3052.681677	20.897357
73.076356	3037.688872	20.902375
72.846596	3044.477964	20.907392
72.747948	3053.158435	20.912410
73.052654	3052.331160	20.917427
72.873311	3059.012318	20.922445
72.940199	3056.796816	20.927463
72.869682	3062.224833	20.932480
73.073652	3052.854359	20.937498
73.441785	3050.663188	20.942515
73.097421	3051.464684	20.947533
72.934780	3053.756172	20.952551
73.118432	3083.781553	20.957568
73.152213	3076.362290	20.962586
73.362137	3081.347561	20.967603
73.139124	3085.295876	20.972621
73.777294	3098.426814	20.977639
73.697790	3112.548513	20.982656
73.966359	3119.724642	20.987674
73.908695	3122.903237	20.992691
73.762159	3125.397478	20.997709
74.280882	3123.887101	21.002727
73.738789	3122.840877	21.007744
73.865612	3131.933031	21.012762
74.721067	3143.123358	21.017779
74.502744	3149.805266	21.022797
74.506650	3148.281016	21.027815
74.831963	3151.916933	21.032832
74.996351	3147.156855	21.037850
74.910925	3151.796720	21.042867
74.907411	3143.058687	21.047885
74.968815	3144.232060	21.052903
74.727410	3142.822445	21.057920
74.722348	3146.274270	21.062938
75.082408	3140.325858	21.067955
74.939852	3141.710321	21.072973
75.103032	3140.010426	21.077991
75.015290	3153.080968	21.083008
75.405077	3159.920775	21.088026
75.865950	3172.250158	21.093043
75.442959	3174.058499	21.098061
75.712046	3165.690750	21.103079
75.628887	3174.277573	21.108096
75.495420	3165.579916	21.113114
75.938188	3172.121013	21.118131
75.585980	3178.646507	21.123149
75.699947	3178.921820	21.128167
75.842411	3187.696862	21.133184
75.941303	3193.588771	21.138202
75.835933	3198.916201	21.143219
75.787306	3208.086725	21.148237
76.062702	3204.925457	21.153255
76.131861	3218.955901	21.158272
76.139125	3235.721130	21.163290
76.507751	3236.486026	21.168307
76.681592	3240.784080	21.173325
76.651464	3235.458724	21.178343
76.358399	3239.726612	21.183360
76.589279	3232.653425	21.188378
76.904192	3238.521916	21.193395
76.598904	3263.768955	21.198413
77.024637	3257.985445	21.203431
77.402917	3256.430588	21.208448
77.283956	3257.742074	21.213466
77.726752	3248.254727	21.218483
77.607814	3249.530810	21.223501
77.701794	3243.181914	21.228519
77.605860	3248.974332	21.233536
77.294700	3248.666894	21.238554
77.642306	3248.064824	21.243571
77.556042	3255.202422	21.248589
78.113770	3248.752039	21.253607
78.018214	3253.973302	21.258624
77.909992	3252.545585	21.263642
78.294673	3238.836201	21.268659
78.176243	3244.264060	21.273677
78.480092	3242.292358	21.278695
78.500731	3251.096305	21.283712
78.239109	3245.858205	21.288730
78.291908	3233.003332	21.293747
78.215529	3249.770115	21.298765
78.560173	3252.429908	21.303783
78.286971	3263.507684	21.308800
77.966687	3280.712222	21.313818
78.568330	3274.168294	21.318835
78.708627	3278.847721	21.323853
78.873134	3280.067594	21.328871
79.168512	3292.164667	21.333888
79.112297	3305.446642	21.338906
79.052538	3299.491958	21.343923
79.131665	3307.036644	21.348941
79.123038	3307.275658	21.353959
79.667107	3309.227937	21.358976
79.220421	3310.008004	21.363994
79.280682	3300.612304	21.369011
79.572211	3306.238334	21.374029
79.487578	3313.363114	21.379047
79.529400	3328.213766	21.384064
79.361193	3337.696070	21.389082
79.849644	3336.560222	21.394099
79.967453	3337.173181	21.399117
79.805695	3338.112339	21.404135
79.983582	3341.207792	21.409152
79.903590	3356.065312	21.414170
80.045450	3359.609393	21.419187
80.182704	3366.441584	21.424205
80.172414	3363.048942	21.429223
80.483901	3366.738250	21.434240
80.395052	3376.558766	21.439258
80.735573	3392.856470	21.444275
80.392686	3403.695312	21.449293
80.882457	3384.571090	21.454311
81.105119	3391.191438	21.459328
80.826090	3393.864181	21.464346
81.224944	3388.223355	21.469363
81.215594	3389.557493	21.474381
81.337728	3391.000459	21.479399
81.670478	3382.164609	21.484416
81.477508	3379.944872	21.489434
81.962959	3380.906687	21.494451
81.725198	3385.031282	21.499469
81.399489	3382.142826	21.504487
81.849601	3378.818358	21.509504
81.558008	3384.528754	21.514522
81.832997	3375.850008	21.519539
81.795832	3393.490168	21.524557
81.763392	3410.122691	21.529575
82.155117	3409.134419	21.534592
81.792542	3415.347798	21.539610
82.195311	3411.160845	21.544627
82.151697	3418.884063	21.549645
82.004343	3413.992684	21.554663
82.397786	3420.245195	21.559680
82.388928	3439.290562	21.564698
82.414362	3454.365003	21.569715
82.385721	3456.629678	21.574733
82.670543	3447.819525	21.579751
82.775663	3450.434952	21.584768
82.220253	3460.899456	21.589786
82.635691	3468.280465	21.594803
82.799683	3481.361501	21.599821
82.640351	3486.003031	21.604839
83.451316	3497.015080	21.609856
83.277936	3508.175452	21.614874
83.541611	3501.878835	21.619891
83.857570	3504.957027	21.624909
83.437368	3511.114343	21.629927
83.646568	3509.838152	21.634944
83.541531	3510.961790	21.639962
83.619840	3503.753113	21.644979
83.519921	3508.195593	21.649997
83.376271	3532.141372	21.655015
83.806487	3526.980070	21.660032
83.944796	3542.064134	21.665050
84.105309	3535.809126	21.670067
84.313609	3548.202704	21.675085
84.156505	3566.692115	21.680103
84.466757	3568.575519	21.685120
84.294864	3575.020513	21.690138
84.624289	3561.388867	21.695155
84.910187	3558.339915	21.700173
85.111695	3557.647855	21.705191
85.330183	3554.607292	21.710208
85.297562	3555.518004	21.715226
85.315745	3553.279515	21.720243
85.382181	3552.987374	21.725261
85.440229	3561.713956	21.730279
85.754381	3549.079872	21.735296
85.342796	3552.016855	21.740314
85.550495	3556.710010	21.745331
85.798338	3546.108983	21.750349
85.652386	3551.390307	21.755367
86.062954	3541.557066	21.760384
85.932624	3546.546409	21.765402
85.789879	3545.738542	21.770419
85.925605	3541.360501	21.775437
85.892482	3545.491053	21.780455
86.230414	3564.503309	21.785472
86.177862	3580.846598	21.790490
86.316915	3586.193404	21.795507
86.180970	3573.851336	21.800525
86.180061	3575.930677	21.805543
86.394478	3567.987557	21.810560
86.389948	3584.166649	21.815578
86.318935	3581.722903	21.820595
86.476849	3591.715036	21.825613
86.485899	3605.775102	21.830631
87.083554	3609.024726	21.835648
86.979493	3604.972818	21.840666
87.113677	3607.854248	21.845683
87.166495	3596.204995	21.850701
87.146638	3620.842314	21.855719
87.822357	3628.863929	21.860736
87.749865	3627.429691	21.865754
87.679852	3624.699436	21.870771
87.962963	3632.033977	21.875789
87.717613	3629.183790	21.880807
87.867673	3625.238459	21.885824
87.895725	3630.197068	21.890842
87.642349	3630.893616	21.895859
88.134276	3622.077080	21.900877
87.859267	3638.324536	21.905895
88.003513	3625.962129	21.910912
88.081378	3640.347157	21.915930
88.129720	3656.399899	21.920947
88.281194	3663.848273	21.925965
88.381616	3662.514683	21.930983
88.294729	3664.433109	21.936000
88.488562	3672.916268	21.941018
88.512867	3682.321682	21.946035
88.774581	3692.546702	21.951053
88.471679	3699.372930	21.956071
88.782516	3693.003420	21.961088
89.144751	3708.427183	21.966106
89.034947	3715.536505	21.971123
89.703015	3716.708370	21.976141
89.499712	3721.514317	21.981159
89.797838	3714.717307	21.986176
89.768443	3716.890890	21.991194
89.851678	3714.529511	21.996211
89.916548	3705.538734	22.001229
89.790763	3717.172323	22.006247
89.657261	3704.814022	22.011264
90.186564	3724.282911	22.016282
90.052085	3733.093002	22.021299
90.571374	3734.512792	22.026317
90.682692	3738.822538	22.031335
90.684636	3723.044246	22.036352
90.461941	3712.930342	22.041370
90.423410	3717.872065	22.046387
90.973744	3720.245055	22.051405
90.786360	3730.460690	22.056423
91.070264	3730.452465	22.061440
91.500949	3729.540561	22.066458
91.188589	3729.769016	22.071475
91.213129	3731.436044	22.076493
91.233153	3731.331446	22.081511
91.150884	3727.480561	22.086528
91.193139	3731.836717	22.091546
91.450659	3734.890451	22.096563
91.298954	3719.347489	22.101581
91.272718	3725.346886	22.106599
91.429798	3723.076782	22.111616
91.645128	3739.602517	22.116634
91.567191	3753.798528	22.121651
91.854240	3752.717582	22.126669
91.696422	3758.741907	22.131687
91.919474	3751.263803	22.136704
91.784387	3773.296234	22.141722
92.101374	3787.152397	22.146739
92.393712	3781.751035	22.151757
92.267918	3783.551388	22.156775
92.625628	3777.544885	22.161792
92.785871	3785.250736	22.166810
92.442479	3799.268855	22.171827
92.714466	3807.477670	22.176845
92.746259	3815.382592	22.181863
93.066815	3817.680533	22.186880
93.017706	3822.651511	22.191898
92.886006	3822.324093	22.196915
93.398896	3829.765267	22.201933
93.315544	3842.318882	22.206951
93.335910	3841.696602	22.211968
93.650913	3843.797979	22.216986
93.520440	3855.145291	22.222003
93.846931	3848.455405	22.227021
93.794823	3848.123947	22.232039
94.253388	3848.052472	22.237056
93.944521	3849.132332	22.242074
93.737377	3862.208384	22.247091
94.346311	3865.644282	22.252109
94.354424	3877.435221	22.257127
94.523799	3876.230644	22.262144
94.627332	3871.420251	22.267162
94.350290	3879.653721	22.272179
94.713210	3873.143668	22.277197
94.512625	3876.281495	22.282215
94.594236	3884.999005	22.287232
94.893048	3894.407982	22.292250
94.864433	3907.702621	22.297267
95.192718	3894.606572	22.302285
95.274358	3900.820119	22.307303
95.206081	3906.528145	22.312320
95.051361	3901.699136	22.317338
95.173918	3906.213247	22.322355
95.342946	3923.992658	22.327373
95.298878	3931.168695	22.332391
95.416105	3932.683299	22.337408
95.522593	3933.242236	22.342426
95.331173	3944.641029	22.347443
95.770884	3953.455666	22.352461
96.001765	3966.118974	22.357479
95.918047	3970.611716	22.362496
96.005651	3973.942757	22.367514
95.907119	3988.574950	22.372531
96.336807	3996.580936	22.377549
96.295646	3998.120803	22.382567
96.612082	3998.061765	22.387584
96.895769	3998.400500	22.392602
96.755128	4016.535419	22.397619
97.263016	4018.042805	22.402637
97.073904	4019.787202	22.407655
97.041523	4028.943847	22.412672
97.485367	4024.121619	22.417690
97.293797	4029.589750	22.422707
97.306565	4024.483043	22.427725
97.399581	4028.227812	22.432743
97.484265	4039.675480	22.437760
97.873245	4049.070965	22.442778
97.349634	4060.481125	22.447795
97.724872	4055.010591	22.452813
97.893090	4059.257077	22.457831
97.719025	4060.353217	22.462848
98.443574	4074.460121	22.467866
98.219747	4086.961609	22.472883
98.438469	4090.983715	22.477901
98.137131	4088.023575	22.482919
98.682749	4082.825588	22.487936
98.699636	4088.705760	22.492954
98.351757	4094.733782	22.497971
98.561344	4105.213634	22.502989
98.931352	4117.515828	22.508007
98.768700	4122.236754	22.513024
98.905439	4118.803972	22.518042
98.927702	4123.922580	22.523059
99.390274	4128.882871	22.528077
99.441928	4141.153247	22.533095
99.810429	4134.823914	22.538112
99.741552	4141.438385	22.543130
99.589556	4139.857076	22.548147
99.815000	4133.696878	22.553165
100.016246	4139.589367	22.558183
99.821098	4141.860245	22.563200
100.013956	4155.539093	22.568218
99.931692	4168.900737	22.573235
99.858956	4172.747495	22.578253
100.151546	4168.222319	22.583271
100.074449	4165.140658	22.588288
100.525618	4181.229649	22.593306
100.431694	4191.337870	22.598323
100.610062	4197.438569	22.603341
100.829107	4200.977629	22.608359
100.791640	4204.301132	22.613376
100.744845	4208.221645	22.618394
100.983548	4226.278239	22.623411
101.255532	4228.365292	22.628429
101.745390	4223.989582	22.633447
101.269582	4225.709703	22.638464
101.967670	4222.102425	22.643482
101.600766	4224.946663	22.648499
101.805017	4225.058918	22.653517
102.143874	4218.122234	22.658535
101.722130	4226.529228	22.663552
102.019314	4229.815895	22.668570
102.051313	4253.410723	22.673587
102.471466	4248.820341	22.678605
102.632312	4245.786470	22.683623
102.371770	4248.684555	22.688640
102.972415	4237.667260	22.693658
102.541162	4255.555378	22.698675
102.724066	4244.943753	22.703693
103.087722	4231.199829	22.708711
103.034728	4240.820892	22.713728
103.693705	4253.413825	22.718746
103.827451	4248.370353	22.723763
103.469227	4233.132758	22.728781
103.565286	4224.890337	22.733799
103.552557	4235.035203	22.738816
104.083148	4237.870069	22.743834
103.902176	4249.418476	22.748851
103.618822	4257.340847	22.753869
104.279615	4257.340970	22.758887
104.013015	4265.721674	22.763904
104.006623	4262.572076	22.768922
103.775218	4265.620496	22.773939
104.028285	4268.073235	22.778957
104.127379	4265.079102	22.783975
104.362527	4284.837945	22.788992
104.616358	4284.905320	22.794010
104.385478	4298.232564	22.799027
104.547927	4303.849671	22.804045
104.712198	4305.474029	22.809063
104.871847	4327.639657	22.814080
104.887548	4334.088109	22.819098
104.837263	4337.141491	22.824115
104.991794	4328.913289	22.829133
104.996803	4342.947170	22.834151
105.170008	4360.571465	22.839168
105.400719	4353.830543	22.844186
105.675903	4356.005215	22.849203
105.918852	4361.487570	22.854221
105.787158	4361.131817	22.859239
106.043616	4383.065751	22.864256
106.216498	4382.723579	22.869274
106.357705	4390.992125	22.874291
106.242098	4390.875321	22.879309
106.449978	4381.808619	22.884327
106.340417	4394.681562	22.889344
106.625181	4381.113712	22.894362
106.501963	4386.373614	22.899379
106.433162	4400.250966	22.904397
107.027922	4405.562383	22.909415
107.150044	4414.444461	22.914432
107.071925	4415.367201	22.919450
106.747797	4422.294695	22.924467
107.055848	4417.747312	22.929485
107.198668	4443.264769	22.934503
107.413637	4446.843087	22.939520
107.762244	4449.766804	22.944538
107.594624	4444.769745	22.949555
107.600106	4450.703016	22.954573
108.199726	4451.120406	22.959591
108.058448	4471.435143	22.964608
108.100344	4472.653429	22.969626
108.125306	4476.147193	22.974643
108.207138	4474.696917	22.979661
108.420118	4468.983840	22.984679
107.984814	4489.291990	22.989696
108.773527	4494.876179	22.994714
108.963010	4492.768360	22.999731
108.751070	4500.769944	23.004749
109.066740	4495.763462	23.009767
109.019353	4507.961826	23.014784
109.344410	4517.037392	23.019802
109.287237	4519.449173	23.024819
109.314165	4532.271363	23.029837
109.482423	4516.788250	23.034855
109.713085	4529.822617	23.039872
109.648808	4530.691233	23.044890
109.864773	4537.688429	23.049907
109.675921	4559.933578	23.054925
110.020888	4565.921329	23.059943
110.359876	4568.662514	23.064960
109.928630	4574.197383	23.069978
110.447035	4572.152751	23.074995
110.444512	4585.292793	23.080013
111.116224	4579.877853	23.085031
110.707604	4589.278141	23.090048
110.931652	4595.107389	23.095066
111.209195	4571.572943	23.100083
110.972584	4588.644507	23.105101
111.319390	4578.314110	23.110119
111.097931	4592.118433	23.115136
111.148222	4588.001519	23.120154
111.639751	4610.688163	23.125171
111.586349	4620.921597	23.130189
111.544232	4617.749299	23.135207
111.437392	4621.570930	23.140224
111.289296	4618.981173	23.145242
111.827796	4634.495815	23.150259
111.641780	4640.133213	23.155277
111.682201	4641.127536	23.160295
111.969588	4656.830929	23.165312
112.336396	4670.348780	23.170330
112.124063	4677.707779	23.175347
112.475354	4683.969133	23.180365
112.535503	4678.454995	23.185383
112.582718	4695.000744	23.190400
112.840360	4705.316808	23.195418
113.196733	4703.881736	23.200435
112.799769	4707.918007	23.205453
113.140195	4720.798940	23.210471
113.681778	4739.037590	23.215488
113.507204	4743.334215	23.220506
113.742376	4739.701504	23.225523
113.647317	4736.745314	23.230541
113.903573	4739.320353	23.235559
113.932789	4740.061574	23.240576
113.881735	4752.890097	23.245594
113.949686	4760.170616	23.250611
114.023414	4768.543753	23.255629
114.072089	4770.570514	23.260647
114.652532	4787.781084	23.265664
114.414022	4799.104652	23.270682
114.612267	4815.733449	23.275699
114.690236	4809.065452	23.280717
115.151664	4804.767273	23.285735
115.158607	4804.796135	23.290752
115.317462	4826.954775	23.295770
115.843998	4826.161271	23.300787
115.300013	4838.797836	23.305805
115.577738	4829.769287	23.310823
115.668663	4833.011095	23.315840
115.668883	4829.688030	23.320858
115.865958	4837.015656	23.325875
115.918179	4855.823395	23.330893
116.108295	4851.540929	23.335911
115.938186	4869.990775	23.340928
116.134246	4872.701312	23.345946
116.466984	4872.630236	23.350963
116.397549	4892.384178	23.355981
116.921263	4888.489074	23.360999
117.106638	4893.854147	23.366016
116.837609	4899.721229	23.371034
117.205642	4896.634522	23.376051
116.790063	4891.935680	23.381069
117.068473	4920.028529	23.386087
117.129024	4921.293441	23.391104
117.328626	4932.179066	23.396122
117.711593	4927.391433	23.401139
117.464398	4929.712424	23.406157
117.403953	4946.922311	23.411175
117.651397	4955.473977	23.416192
117.711214	4961.543547	23.421210
118.650198	4957.379236	23.426227
118.656327	4952.488042	23.431245
118.772807	4942.858902	23.436263
118.571332	4937.443028	23.441280
118.699622	4949.303775	23.446298
118.858978	4944.864121	23.451315
119.279823	4971.307409	23.456333
119.295900	4972.265513	23.461351
119.591187	4973.564593	23.466368
119.518357	4972.614899	23.471386
119.247646	4974.869628	23.476403
119.372818	4965.610422	23.481421
119.521693	4972.129179	23.486439
119.524174	4966.610754	23.491456
119.417124	4974.433803	23.496474
119.674241	4981.873870	23.501491
119.559839	4994.681235	23.506509
120.126465	5007.018125	23.511527
120.058640	4998.485140	23.516544
120.058229	5023.194868	23.521562
120.350993	5038.164580	23.526579
120.322780	5043.460704	23.531597
120.309226	5040.083143	23.536615
120.612700	5043.749771	23.541632
120.355845	5059.469569	23.546650
120.884621	5061.467022	23.551667
121.034976	5074.361264	23.556685
121.323731	5094.178732	23.561703
121.426468	5091.837628	23.566720
121.207536	5093.173080	23.571738
121.498651	5092.183443	23.576755
121.303305	5121.784071	23.581773
121.668097	5133.473512	23.586791
121.905609	5126.316545	23.591808
121.723928	5137.671433	23.596826
122.105440	5153.568835	23.601843
121.966008	5164.913074	23.606861
122.104765	5163.382061	23.611879
122.497812	5186.419661	23.616896
122.601336	5185.348999	23.621914
122.578575	5193.459257	23.626931
122.621049	5199.962823	23.631949
123.316896	5206.075841	23.636967
123.698677	5208.033028	23.641984
123.686157	5215.398196	23.647002
123.877865	5212.412707	23.652019
123.766161	5210.049131	23.657037
123.893311	5217.491946	23.662055
124.071421	5205.572048	23.667072
123.911261	5213.854493	23.672090
124.334488	5204.713615	23.677107
124.263095	5213.889803	23.682125
124.361315	5206.087066	23.687143
124.684906	5223.598728	23.692160
124.560692	5245.112373	23.697178
124.804264	5236.165337	23.702195
124.974568	5238.535457	23.707213
124.985824	5233.260997	23.712231
124.906120	5234.106152	23.717248
124.728653	5239.071323	23.722266
125.217377	5248.855276	23.727283
125.339652	5271.070767	23.732301
125.614485	5278.764639	23.737319
125.634699	5273.456480	23.742336
125.281001	5268.500611	23.747354
125.566847	5290.278583	23.752371
125.798969	5293.760752	23.757389
125.771542	5301.555543	23.762407
126.103434	5312.648512	23.767424
126.193444	5327.134742	23.772442
126.586175	5319.899435	23.777459
126.755138	5335.380905	23.782477
126.699752	5326.458668	23.787495
127.009255	5323.474831	23.792512
126.838368	5328.312316	23.797530
127.218263	5349.144660	23.802547
127.168731	5349.814286	23.807565
127.321184	5348.463596	23.812583
127.707541	5350.891335	23.817600
127.702360	5349.597249	23.822618
127.779725	5352.472350	23.827635
128.005386	5369.441996	23.832653
128.292108	5375.131749	23.837671
128.505055	5376.902670	23.842688
128.465327	5383.640501	23.847706
128.152686	5376.778050	23.852723
128.862087	5382.092005	23.857741
128.386299	5378.709394	23.862759
129.018952	5382.148177	23.867776
128.986830	5395.825501	23.872794
129.059390	5409.673394	23.877811
128.914376	5403.616584	23.882829
128.721895	5405.472608	23.887847
129.351263	5412.660001	23.892864
129.348524	5422.436676	23.897882
129.593122	5434.104610	23.902899
129.878827	5436.416238	23.907917
129.585284	5437.537819	23.912935
129.803992	5455.200227	23.917952
129.956548	5468.468958	23.922970
129.817205	5474.742007	23.927987
130.273365	5484.658765	23.933005
130.225828	5500.767355	23.938023
130.727402	5499.727614	23.943040
130.624098	5515.400595	23.948058
130.771057	5511.303415	23.953075
130.981047	5515.098361	23.958093
131.410902	5529.182070	23.963111
131.541168	5526.992286	23.968128
131.272328	5525.143075	23.973146
131.344518	5526.015953	23.978163
131.886760	5524.909146	23.983181
131.610903	5528.768187	23.988199
131.862234	5542.549935	23.993216
131.630478	5563.288924	23.998234
131.966102	5558.902806	24.003251
132.167961	5563.942926	24.008269
131.969000	5581.765705	24.013287
132.312191	5596.687820	24.018304
132.477523	5605.375693	24.023322
132.544009	5600.120619	24.028339
132.726368	5612.550761	24.033357
132.533460	5629.817179	24.038375
133.341832	5621.842774	24.043392
133.422708	5642.790084	24.048410
133.167149	5652.816502	24.053427
133.655118	5650.251814	24.058445
133.497140	5651.519375	24.063463
134.134241	5648.255080	24.068480
134.076975	5671.716922	24.073498
134.069604	5683.588089	24.078515
134.225727	5686.536455	24.083533
134.104067	5699.244879	24.088551
134.412394	5689.453275	24.093568
134.604879	5713.625937	24.098586
134.564049	5719.570249	24.103603
135.052957	5722.976173	24.108621
134.575269	5722.437946	24.113639
134.999780	5738.482544	24.118656
135.110184	5752.850285	24.123674
135.350149	5753.092188	24.128691
135.899112	5751.674308	24.133709
135.549138	5768.114646	24.138727
136.132394	5768.899759	24.143744
136.124324	5783.060616	24.148762
136.042421	5783.534796	24.153779
136.052877	5773.318568	24.158797
135.833743	5789.694797	24.163815
136.219667	5807.587452	24.168832
136.218316	5817.721362	24.173850
136.855130	5833.377379	24.178867
136.945670	5843.379426	24.183885
136.969489	5848.613253	24.188903
137.066292	5845.432702	24.193920
137.371143	5858.151149	24.198938
137.332227	5862.424892	24.203955
137.632853	5868.005618	24.208973
137.612662	5889.453258	24.213991
137.692034	5870.831866	24.219008
137.876285	5890.255584	24.224026
137.752537	5904.892118	24.229043
137.905820	5912.150945	24.234061
138.013064	5916.539085	24.239079
138.300681	5923.368949	24.244096
138.267845	5941.818697	24.249114
138.359669	5942.490202	24.254131
138.500649	5957.313531	24.259149
138.936604	5973.271588	24.264167
139.093153	5970.659768	24.269184
138.766347	5981.525458	24.274202
139.459954	5996.086837	24.279219
139.776162	6002.685586	24.284237
139.795571	6012.139686	24.289255
139.869507	6001.757397	24.294272
140.143394	6004.776744	24.299290
140.401142	6013.786078	24.304307
140.383404	6016.744922	24.309325
140.457436	6027.142329	24.314343
140.736655	6028.241080	24.319360
140.463261	6036.955884	24.324378
140.176206	6031.902582	24.329395
140.635484	6039.613079	24.334413
140.592463	6056.260498	24.339431
140.907495	6060.952295	24.344448
141.185353	6077.654007	24.349466
141.045489	6088.391621	24.354483
141.290500	6109.315781	24.359501
141.593524	6121.124432	24.364519
141.821697	6124.478397	24.369536
141.955003	6133.700408	24.374554
141.830523	6142.053998	24.379571
142.385138	6150.578628	24.384589
142.190893	6153.848886	24.389607
142.393241	6168.019834	24.394624
142.781995	6171.807692	24.399642
142.919133	6185.071656	24.404659
143.203777	6195.192483	24.409677
142.924135	6198.594385	24.414695
143.408933	6199.658798	24.419712
143.384570	6220.040691	24.424730
143.219756	6221.799561	24.429747
143.741364	6236.029037	24.434765
143.788349	6252.942425	24.439783
143.856246	6261.562031	24.444800
144.156451	6256.724230	24.449818
144.132266	6271.912530	24.454835
144.271533	6286.878873	24.459853
144.462231	6287.930387	24.464871
144.516620	6283.778517	24.469888
144.890883	6304.608387	24.474906
144.717065	6327.392745	24.479923
144.851082	6312.152406	24.484941
145.061665	6337.242180	24.489959
145.107987	6356.394236	24.494976
145.527692	6348.996774	24.499994
145.438735	6365.074352	24.505011
145.897051	6376.733347	24.510029
145.905894	6393.581378	24.515047
145.689557	6384.766779	24.520064
146.091915	6401.195656	24.525082
145.875125	6421.380331	24.530099
146.243124	6418.469567	24.535117
146.541086	6436.735792	24.540135
146.847110	6450.173702	24.545152
147.066863	6457.681845	24.550170
147.011973	6455.377461	24.555187
147.281690	6457.352689	24.560205
147.444716	6469.562394	24.565223
147.732610	6474.774010	24.570240
148.024111	6473.289324	24.575258
147.828626	6478.425369	24.580275
148.387714	6470.364377	24.585293
148.270205	6486.612655	24.590311
148.460810	6505.049508	24.595328
148.755169	6506.622689	24.600346
148.873403	6514.072301	24.605363
148.983110	6508.588136	24.610381
148.842030	6507.613816	24.615399
148.794603	6507.544345	24.620416
149.080530	6515.739080	24.625434
148.969366	6526.067226	24.630451
149.431799	6532.737317	24.635469
149.862084	6546.262509	24.640487
149.974742	6552.313292	24.645504
150.277673	6556.908040	24.650522
150.217416	6559.040538	24.655539
150.365380	6544.837114	24.660557
150.498275	6559.618274	24.665575
150.818964	6558.237508	24.670592
151.199046	6580.126672	24.675610
150.962072	6584.101739	24.680627
151.006949	6575.900006	24.685645
151.169284	6583.009013	24.690663
151.353208	6582.030080	24.695680
151.566818	6587.777596	24.700698
151.687514	6600.117688	24.705715
151.746769	6610.756265	24.710733
151.913644	6608.526654	24.715751
151.721973	6612.798214	24.720768
152.374647	6624.237583	24.725786
152.209575	6638.681576	24.730803
152.663612	6644.548145	24.735821
152.830588	6639.705498	24.740839
152.665807	6647.552006	24.745856
153.031563	6657.915934	24.750874
153.113372	6667.623299	24.755891
153.441738	6668.161919	24.760909
153.159422	6669.426571	24.765927
153.325149	6689.867711	24.770944
153.604877	6695.159388	24.775962
153.497571	6714.408787	24.780979
153.588914	6713.364351	24.785997
154.034925	6735.092952	24.791015
153.944471	6752.198774	24.796032
154.380422	6737.465357	24.801050
153.824656	6751.708951	24.806067
154.322547	6755.156965	24.811085
154.561564	6770.428128	24.816103
154.598240	6791.890035	24.821120
154.727954	6799.187676	24.826138
154.725420	6812.347791	24.831155
155.473905	6832.530195	24.836173
156.056591	6824.465252	24.841191
156.101577	6832.106098	24.846208
155.874535	6833.330478	24.851226
156.163611	6838.009353	24.856243
156.327938	6844.572897	24.861261
156.738820	6856.754420	24.866279
156.479400	6871.330917	24.871296
156.816424	6859.996512	24.876314
156.992246	6866.379624	24.881331
157.010570	6876.253039	24.886349
156.968508	6881.590580	24.891367
156.868480	6903.351406	24.896384
157.428794	6893.491302	24.901402
157.635342	6902.566780	24.906419
158.016977	6915.978109	24.911437
158.333770	6914.372112	24.916455
158.088170	6930.166050	24.921472
158.055129	6921.836494	24.926490
158.142638	6951.228074	24.931507
158.043504	6958.091754	24.936525
158.589088	6963.169613	24.941543
158.633218	6989.343744	24.946560
159.055687	6993.829085	24.951578
158.922110	7002.400199	24.956595
159.148976	7000.393082	24.961613
159.269775	7013.820120	24.966631
159.195400	7032.412393	24.971648
159.688473	7033.341792	24.976666
159.807004	7053.899541	24.981683
159.418905	7057.834305	24.986701
159.738335	7070.704905	24.991719
159.668195	7095.192362	24.996736
160.439407	7104.375434	25.001754
160.764006	7118.036813	25.006771
160.822000	7118.282577	25.011789
161.179945	7138.054772	25.016807
161.305586	7155.226927	25.021824
161.443107	7150.707483	25.026842
161.679412	7144.255543	25.031859
161.621537	7161.239401	25.036877
161.825729	7172.663361	25.041895
161.865803	7187.750290	25.046912
162.278171	7187.856938	25.051930
162.436226	7196.548479	25.056947
162.530978	7202.660610	25.061965
162.723061	7216.428185	25.066983
162.505822	7220.018652	25.072000
162.752786	7220.811048	25.077018
162.770824	7244.661510	25.082035
162.906483	7249.121840	25.087053
163.186594	7248.940344	25.092071
163.143829	7265.190142	25.097088
163.463715	7274.922108	25.102106
163.682434	7285.272150	25.107123
164.156544	7296.491081	25.112141
164.205508	7314.113525	25.117159
164.116826	7323.600642	25.122176
164.295031	7317.770849	25.127194
164.595990	7336.486210	25.132211
164.611309	7347.219659	25.137229
164.824894	7351.807656	25.142247
165.058554	7366.608962	25.147264
165.345817	7382.685097	25.152282
165.467960	7381.771044	25.157299
165.616818	7409.328243	25.162317
165.822564	7403.634873	25.167335
165.643461	7422.075941	25.172352
166.200233	7426.256734	25.177370
166.257997	7434.242069	25.182387
166.234879	7460.121661	25.187405
166.696808	7455.336379	25.192423
166.553686	7477.127731	25.197440
166.871543	7483.790618	25.202458
167.175652	7481.734928	25.207475
167.119534	7507.135157	25.212493
167.284079	7510.928423	25.217511
167.503746	7527.237386	25.222528
167.756118	7532.163114	25.227546
168.205529	7543.891336	25.232563
167.864732	7536.448511	25.237581
168.264212	7551.187369	25.242599
168.242762	7577.001587	25.247616
168.351939	7566.189257	25.252634
168.662796	7589.621400	25.257651
168.737470	7597.842547	25.262669
169.280505	7594.538550	25.267687
169.185736	7621.862728	25.272704
169.618394	7634.356167	25.277722
169.901115	7626.547929	25.282739
169.751588	7651.882248	25.287757
169.971812	7647.654775	25.292775
170.048365	7662.880366	25.297792
170.385436	7668.763633	25.302810
170.669728	7668.428028	25.307827
170.887563	7697.373031	25.312845
170.918798	7698.767969	25.317863
171.181269	7704.408985	25.322880
171.146920	7706.672857	25.327898
171.769292	7700.148113	25.332915
171.488422	7722.555084	25.337933
172.006029	7725.783011	25.342951
171.799401	7728.047599	25.347968
171.969031	7716.758120	25.352986
172.175389	7728.619663	25.358003
172.323658	7747.232412	25.363021
172.752082	7751.381042	25.368039
172.161274	7774.276579	25.373056
172.567476	7759.149531	25.378074
172.737175	7779.768581	25.383091
172.566732	7797.388806	25.388109
172.792830	7811.356097	25.393127
173.241418	7826.819983	25.398144
173.150062	7836.657225	25.403162
173.753064	7850.874495	25.408179
173.815446	7858.023654	25.413197
174.436993	7861.386122	25.418215
174.213766	7890.026474	25.423232
174.335128	7898.928866	25.428250
174.554038	7899.166301	25.433267
174.582618	7910.742365	25.438285
174.522681	7924.686118	25.443303
175.057115	7934.451198	25.448320
175.333475	7957.230797	25.453338
175.198762	7963.805528	25.458355
175.048777	7995.981293	25.463373
175.546037	7999.276656	25.468391
175.838491	8018.604856	25.473408
175.968397	8036.727907	25.478426
176.239565	8029.206156	25.483443
176.711848	8046.958307	25.488461
176.970735	8053.122129	25.493479
176.895743	8057.861401	25.498496
177.347965	8061.684094	25.503514
177.206259	8077.619662	25.508531
177.734127	8089.962175	25.513549
177.907480	8071.810138	25.518567
178.181223	8087.481581	25.523584
177.711840	8099.979548	25.528602
178.679558	8102.183267	25.533619
178.431013	8114.995026	25.538637
178.527022	8113.062921	25.543655
178.689962	8125.466790	25.548672
178.932416	8142.989726	25.553690
179.234491	8146.522014	25.558707
179.720768	8151.706925	25.563725
180.272454	8146.445998	25.568743
180.148955	8153.260600	25.573760
180.122336	8156.122135	25.578778
180.465378	8156.692315	25.583795
180.241365	8149.568928	25.588813
180.353177	8164.329075	25.593831
180.688106	8167.341894	25.598848
180.648862	8185.638456	25.603866
181.206735	8189.479356	25.608883
181.231540	8204.316366	25.613901
181.510633	8195.886369	25.618919
181.415234	8194.601303	25.623936
181.437150	8211.351729	25.628954
181.884674	8211.233636	25.633971
181.715404	8227.058870	25.638989
181.983241	8225.834716	25.644007
182.345653	8248.780848	25.649024
182.357193	8256.625269	25.654042
182.697691	8254.901256	25.659059
182.616822	8271.003597	25.664077
182.909374	8277.894357	25.669095
182.986202	8286.559746	25.674112
182.903391	8304.371978	25.679130
183.061935	8317.288194	25.684148
183.321455	8332.362541	25.689165
183.538215	8337.112441	25.694183
183.628174	8355.434646	25.699200
183.469196	8376.596375	25.704218
184.068885	8387.287378	25.709236
184.257739	8409.692493	25.714253
184.454432	8412.832846	25.719271
184.601605	8428.203373	25.724288
184.671158	8451.587206	25.729306
185.129037	8454.268079	25.734324
185.449893	8490.935110	25.739341
185.747327	8483.051688	25.744359
186.055583	8472.316741	25.749376
186.323403	8492.064579	25.754394
186.418779	8515.729652	25.759412
186.490231	8523.922707	25.764429
186.549557	8519.703329	25.769447
186.677244	8530.123047	25.774464
186.932232	8544.687230	25.779482
187.252260	8543.211574	25.784500
187.317382	8556.070493	25.789517
187.541156	8574.831193	25.794535
187.838299	8577.247342	25.799552
188.051571	8597.143299	25.804570
188.341611	8596.777252	25.809588
188.565645	8612.684592	25.814605
188.769521	8614.802028	25.819623
188.825613	8614.253726	25.824640
188.693197	8638.261813	25.829658
188.761822	8647.046363	25.834676
188.906022	8655.846413	25.839693
188.606762	8678.973842	25.844711
189.271742	8690.520665	25.849728
189.069433	8704.672768	25.854746
189.623865	8712.550098	25.859764
189.803789	8727.564743	25.864781
189.866136	8753.252346	25.869799
190.298712	8772.132277	25.874816
190.454211	8789.675736	25.879834
190.744522	8797.527148	25.884852
190.711993	8800.721046	25.889869
191.034459	8815.268046	25.894887
191.452957	8835.781608	25.899904
191.368387	8839.013319	25.904922
191.596054	8840.803567	25.909940
191.817718	8866.467540	25.914957
192.021642	8879.603251	25.919975
192.357316	8865.523122	25.924992
192.322731	8907.543502	25.930010
192.763913	8910.936151	25.935028
192.990508	8906.964246	25.940045
192.945739	8936.092013	25.945063
193.280479	8936.976752	25.950080
193.129569	8952.055773	25.955098
193.682659	8966.919884	25.960116
194.295308	8959.277524	25.965133
195.092114	8955.856452	25.970151
195.361732	8944.584343	25.975168
195.064164	8961.432967	25.980186
195.518174	8952.791307	25.985204
195.913965	8951.082406	25.990221
195.668250	8957.096080	25.995239
195.948411	8945.861636	26.000256
195.843068	8958.396316	26.005274
195.966308	8944.779253	26.010292
196.039142	8966.897974	26.015309
196.208096	8972.685407	26.020327
196.760064	8975.722814	26.025344
196.386480	8982.129498	26.030362
196.856138	8994.118872	26.035380
196.876364	9009.741201	26.040397
197.000909	9023.706144	26.045415
197.069435	9019.101919	26.050432
196.952369	9032.155549	26.055450
197.238310	9044.185662	26.060468
197.406283	9058.853143	26.065485
197.047875	9081.670333	26.070503
197.754225	9106.954478	26.075520
197.623700	9120.695760	26.080538
198.048339	9140.559138	26.085556
198.368508	9161.078592	26.090573
198.566471	9185.725826	26.095591
198.683708	9191.060042	26.100608
198.785454	9223.561879	26.105626
199.150372	9230.469089	26.110644
199.689208	9250.959709	26.115661
199.755445	9257.214945	26.120679
200.187793	9276.491387	26.125696
200.493789	9277.852510	26.130714
200.691930	9288.688841	26.135732
200.969764	9300.700778	26.140749
200.724953	9307.792577	26.145767
201.183359	9324.538799	26.150784
201.187379	9327.771445	26.155802
201.376139	9350.360556	26.160820
201.733769	9347.385184	26.165837
201.076939	9358.048193	26.170855
201.503477	9368.893028	26.175872
201.878162	9384.412810	26.180890
202.326984	9410.761178	26.185908
202.432676	9416.351897	26.190925
202.653284	9432.561667	26.195943
203.494736	9433.002478	26.200960
203.130950	9449.165741	26.205978
203.729145	9458.563596	26.210996
203.879888	9477.182037	26.216013
203.857025	9489.125591	26.221031
204.472691	9475.751418	26.226048
204.394570	9491.367103	26.231066
204.416127	9498.818274	26.236084
205.026104	9501.457783	26.241101
204.958976	9515.196008	26.246119
205.872323	9520.032376	26.251136
205.825899	9519.642432	26.256154
206.122433	9519.348521	26.261172
206.451692	9521.198599	26.266189
206.468769	9523.122053	26.271207
207.010289	9507.570329	26.276224
207.195757	9511.760158	26.281242
206.825777	9510.198061	26.286260
207.138347	9521.327958	26.291277
207.073738	9538.636273	26.296295
207.304636	9539.266887	26.301312
207.082529	9555.048034	26.306330
207.381984	9567.575352	26.311348
207.679743	9578.978764	26.316365
207.732857	9595.270893	26.321383
207.877333	9609.842714	26.326400
208.125599	9630.962142	26.331418
208.162076	9641.671434	26.336436
208.640587	9662.481910	26.341453
208.669804	9678.033460	26.346471
209.523737	9673.168473	26.351488
209.400520	9699.221347	26.356506
209.948494	9694.846621	26.361524
210.123891	9700.754110	26.366541
210.268954	9715.672603	26.371559
210.508067	9713.717876	26.376576
210.795113	9722.890059	26.381594
210.901932	9730.478852	26.386612
211.316011	9735.618385	26.391629
211.171768	9766.429258	26.396647
211.290224	9762.545590	26.401664
211.167769	9780.051098	26.406682
211.237383	9798.441662	26.411700
211.576394	9797.852939	26.416717
211.780641	9836.412507	26.421735
212.057604	9847.318131	26.426752
212.320574	9862.182559	26.431770
212.428031	9871.269741	26.436788
212.555625	9885.564747	26.441805
212.773428	9903.588296	26.446823
212.973361	9915.433320	26.451840
213.605315	9935.332780	26.456858
213.529980	9940.561812	26.461876
214.134743	9947.471653	26.466893
213.927779	9966.156773	26.471911
214.275603	9962.077912	26.476928
214.353087	9984.559011	26.481946
214.623722	9995.206437	26.486964
214.976959	10001.404428	26.491981
215.111466	10028.631116	26.496999
215.315427	10026.989275	26.502016
215.487358	10046.780420	26.507034
215.645542	10060.304576	26.512052
215.756464	10069.072986	26.517069
215.953404	10097.776876	26.522087
216.416017	10104.537491	26.527104
216.695927	10127.004635	26.532122
216.830250	10131.110318	26.537140
217.234342	10145.250921	26.542157
217.239068	10167.121767	26.547175
217.607218	10166.747568	26.552192
217.908599	10199.796169	26.557210
217.549180	10196.967206	26.562228
218.183376	10224.589550	26.567245
218.097113	10232.824026	26.572263
218.313947	10247.403031	26.577280
218.694780	10272.158654	26.582298
219.093162	10288.801803	26.587316
219.349373	10299.148353	26.592333
219.306694	10314.016305	26.597351
219.871738	10331.876801	26.602368
219.998451	10335.202647	26.607386
220.096051	10361.698786	26.612404
220.608890	10368.748612	26.617421
220.609182	10382.557154	26.622439
220.390810	10403.731591	26.627456
220.615790	10405.974205	26.632474
220.822555	10439.511606	26.637492
221.003907	10445.040279	26.642509
221.483554	10467.897539	26.647527
221.689950	10487.215887	26.652544
221.890022	10503.798411	26.657562
221.833198	10537.634419	26.662580
222.193026	10540.034998	26.667597
222.256358	10575.344128	26.672615
222.472708	10586.971812	26.677632
223.202832	10608.475030	26.682650
223.484918	10615.351227	26.687668
223.576568	10632.390335	26.692685
223.358923	10652.456086	26.697703
224.122186	10657.013756	26.702720
224.149915	10669.900514	26.707738
224.378985	10686.896135	26.712756
225.139896	10698.720430	26.717773
225.373362	10700.436788	26.722791
225.590319	10704.994198	26.727808
225.773885	10710.874418	26.732826
226.011057	10727.917590	26.737844
226.123252	10719.989342	26.742861
226.506670	10739.631991	26.747879
226.797391	10726.045259	26.752896
226.968901	10751.426491	26.757914
226.961433	10754.822222	26.762932
227.728891	10744.432351	26.767949
227.926785	10761.865500	26.772967
227.841938	10754.394428	26.777984
228.347778	10762.241245	26.783002
228.225777	10781.500560	26.788020
228.411095	10784.732165	26.793037
228.605659	10796.126981	26.798055
228.707070	10804.542384	26.803072
229.069122	10814.687465	26.808090
229.121978	10822.763141	26.813108
229.308345	10833.030291	26.818125
229.686982	10851.307555	26.823143
229.336954	10862.533051	26.828160
229.923067	10876.869635	26.833178
229.920539	10882.634378	26.838196
229.963253	10907.309573	26.843213
230.140727	10918.733966	26.848231
230.353185	10952.293046	26.853248
230.798470	10966.908346	26.858266
230.791308	10994.476932	26.863284
231.578601	11002.108616	26.868301
231.835733	11022.184570	26.873319
231.704734	11029.204722	26.878336
232.121575	11052.433349	26.883354
232.376349	11057.606211	26.888372
232.665255	11087.438543	26.893389
232.839121	11101.870963	26.898407
232.880534	11111.273616	26.903424
232.998753	11121.328302	26.908442
233.263937	11145.223086	26.913460
233.566469	11170.427513	26.918477
234.030545	11184.921579	26.923495
234.258673	11200.908927	26.928512
234.481352	11220.224438	26.933530
234.715129	11231.348881	26.938548
235.308399	11244.735880	26.943565
235.558749	11261.548128	26.948583
235.637059	11258.162783	26.953600
236.018860	11267.979968	26.958618
235.923809	11294.440764	26.963636
236.280817	11291.316957	26.968653
236.223395	11319.892334	26.973671
236.239320	11334.654745	26.978688
236.825494	11345.251651	26.983706
236.858606	11369.697537	26.988724
237.130205	11383.884628	26.993741
237.216021	11403.620838	26.998759
237.324034	11419.290109	27.003776
237.663307	11425.797873	27.008794
237.766579	11448.652667	27.013812
238.146360	11461.540651	27.018829
238.785268	11478.484036	27.023847
238.828128	11496.783335	27.028864
239.472272	11502.102860	27.033882
239.547966	11529.787111	27.038900
239.545194	11524.833995	27.043917
239.703791	11547.634076	27.048935
239.492769	11573.640813	27.053952
240.362472	11579.682167	27.058970
240.409364	11607.888063	27.063988
240.461460	11628.209818	27.069005
240.854695	11634.277163	27.074023
241.110419	11666.370509	27.079040
241.233622	11679.973317	27.084058
241.485483	11700.674379	27.089076
241.924812	11705.894591	27.094093
242.381468	11735.373446	27.099111
242.155806	11750.293619	27.104128
242.734959	11759.251262	27.109146
242.894209	11782.299720	27.114164
243.158297	11794.335324	27.119181
243.991430	11790.528681	27.124199
243.782633	11823.012023	27.129216
243.966187	11836.340498	27.134234
244.205073	11850.838435	27.139252
244.260933	11872.852355	27.144269
244.568897	11882.476477	27.149287
244.685547	11912.171225	27.154304
245.087944	11921.623098	27.159322
244.995790	11953.540704	27.164340
245.472935	11968.007466	27.169357
245.829784	11978.717328	27.174375
245.908381	12011.865617	27.179392
246.099355	12013.956476	27.184410
246.201926	12039.115907	27.189428
246.642792	12060.511071	27.194445
247.132546	12071.897578	27.199463
247.367280	12093.928958	27.204480
247.583344	12117.143999	27.209498
247.685876	12120.188377	27.214516
247.845976	12160.438224	27.219533
248.508325	12153.027215	27.224551
248.604517	12184.158482	27.229568
248.750372	12194.251586	27.234586
249.256131	12204.809182	27.239604
249.535960	12201.640036	27.244621
250.136134	12223.149158	27.249639
250.187457	12243.417352	27.254656
250.578229	12238.477033	27.259674
250.668979	12243.360425	27.264692
250.622146	12262.044885	27.269709
250.865079	12272.894132	27.274727
250.866007	12291.902979	27.279744
250.928668	12303.617091	27.284762
251.061464	12318.716031	27.289780
251.609537	12340.328078	27.294797
252.084866	12352.655927	27.299815
252.673732	12359.285082	27.304832
252.716962	12372.105092	27.309850
253.040668	12377.619853	27.314868
253.133024	12407.178154	27.319885
253.562538	12396.527373	27.324903
253.318027	12425.195651	27.329920
253.698570	12434.534049	27.334938
253.757718	12461.431188	27.339956
254.269175	12476.937084	27.344973
254.475867	12490.961607	27.349991
254.483673	12509.405853	27.355008
254.821782	12537.458434	27.360026
255.020619	12538.745247	27.365044
255.454825	12580.134382	27.370061
255.169038	12581.395725	27.375079
255.499341	12621.278837	27.380096
255.542336	12643.082217	27.385114
255.993481	12671.129424	27.390132
255.893214	12688.223866	27.395149
256.540974	12728.853238	27.400167
256.872442	12738.638867	27.405184
257.242674	12768.546555	27.410202
257.520524	12784.417844	27.415220
257.763387	12813.874821	27.420237
258.111257	12839.472893	27.425255
258.264168	12849.979737	27.430272
258.420450	12881.252802	27.435290
258.991983	12889.546611	27.440308
259.333394	12916.311403	27.445325
259.628583	12925.633404	27.450343
259.741849	12961.712709	27.455360
260.067569	12969.131767	27.460378
260.414262	12995.290146	27.465396
260.918876	13000.260129	27.470413
261.061325	13021.696147	27.475431
261.434291	13049.943954	27.480448
261.666808	13054.428162	27.485466
262.373315	13055.376312	27.490484
262.426174	13064.701110	27.495501
263.047416	13064.239091	27.500519
262.997363	13087.797345	27.505536
262.989447	13096.797212	27.510554
263.356167	13103.714387	27.515572
263.076125	13124.585314	27.520589
263.822682	13136.326059	27.525607
263.959833	13158.401299	27.530624
263.805012	13166.968563	27.535642
264.365516	13195.703321	27.540660
264.315891	13198.899294	27.545677
264.909350	13220.831837	27.550695
264.803239	13236.915145	27.555712
265.000530	13266.442152	27.560730
265.259958	13269.591833	27.565748
265.573766	13296.312002	27.570765
265.755382	13310.162985	27.575783
265.821166	13330.711264	27.580800
265.892789	13357.198275	27.585818
266.509618	13385.626865	27.590836
266.484762	13423.990022	27.595853
267.115894	13429.520127	27.600871
267.025812	13466.903824	27.605888
267.072733	13487.695186	27.610906
267.746514	13511.164994	27.615924
267.692324	13548.382684	27.620941
268.167128	13566.525493	27.625959
268.471444	13605.175617	27.630976
268.510314	13620.914953	27.635994
269.423085	13640.856908	27.641012
269.863122	13663.630259	27.646029
270.239756	13685.128674	27.651047
270.442653	13702.479387	27.656064
270.540573	13721.165094	27.661082
271.023010	13726.527526	27.666100
271.439556	13756.561430	27.671117
271.735773	13768.064588	27.676135
272.226976	13778.633871	27.681152
272.432102	13788.915581	27.686170
272.223250	13800.471122	27.691188
272.355430	13816.538411	27.696205
273.150109	13826.917368	27.701223
273.179037	13856.490850	27.706240
273.412742	13865.369806	27.711258
274.315813	13866.791080	27.716276
274.645602	13886.584118	27.721293
274.748461	13892.862001	27.726311
274.902643	13907.636357	27.731328
275.008635	13916.561873	27.736346
275.309165	13931.400207	27.741364
275.342206	13949.812651	27.746381
275.927798	13957.867075	27.751399
276.091196	13978.394837	27.756416
276.129084	14003.019338	27.761434
276.874538	13999.295718	27.766452
277.039178	14029.033386	27.771469
277.222910	14038.471351	27.776487
277.044027	14061.290806	27.781504
277.018869	14076.698678	27.786522
277.582529	14101.974787	27.791540
277.465052	14122.943079	27.796557
277.844180	14149.323090	27.801575
278.255775	14169.640332	27.806592
278.140886	14191.615833	27.811610
278.831240	14222.103347	27.816628
278.786691	14239.781148	27.821645
278.996947	14269.414988	27.826663
279.352488	14289.642528	27.831680
279.698577	14313.102136	27.836698
280.431099	14331.468007	27.841716
280.738788	14355.195156	27.846733
280.995912	14356.954714	27.851751
281.551165	14386.368086	27.856768
281.560350	14399.032466	27.861786
282.164360	14405.100696	27.866804
282.241986	14413.883222	27.871821
282.503798	14431.958672	27.876839
282.940009	14443.345365	27.881856
283.063116	14458.389909	27.886874
283.798192	14461.824382	27.891892
283.533051	14478.537056	27.896909
284.067169	14495.627956	27.901927
284.309316	14510.229954	27.906944
284.369904	14539.900866	27.911962
285.084172	14544.065089	27.916980
285.213831	14560.275359	27.921997
285.578274	14573.202680	27.927015
285.611364	14596.477917	27.932032
285.789211	14607.456107	27.937050
286.103543	14622.370750	27.942068
286.215013	14657.516945	27.947085
286.640664	14668.903621	27.952103
286.596216	14691.353841	27.957120
286.500078	14721.879238	27.962138
287.471627	14740.455192	27.967156
287.477592	14772.786380	27.972173
287.765168	14783.883007	27.977191
288.021579	14821.249322	27.982208
287.913061	14839.720920	27.987226
288.315918	14872.096617	27.992244
288.616744	14902.555465	27.997261
289.247497	14921.146002	28.002279
290.007673	14934.665547	28.007296
289.992870	14967.656330	28.012314
290.369102	14984.926062	28.017332
290.212614	15005.831316	28.022349
290.644780	15025.852281	28.027367
291.013992	15047.599714	28.032384
291.162200	15085.011469	28.037402
291.625884	15100.417738	28.042420
291.678746	15140.568335	28.047437
291.736728	15154.475824	28.052455
292.320361	15177.934423	28.057472
292.806503	15220.941140	28.062490
293.077741	15235.858033	28.067508
293.488365	15266.350488	28.072525
293.296924	15288.449087	28.077543
293.883576	15308.575994	28.082560
294.165446	15349.291321	28.087578
294.495534	15348.992076	28.092596
294.797664	15376.266368	28.097613
295.116179	15391.039778	28.102631
295.536625	15411.589504	28.107648
295.717212	15422.136416	28.112666
296.218539	15452.013898	28.117684
296.655277	15463.907782	28.122701
296.611098	15492.109969	28.127719
297.295289	15497.578259	28.132736
297.757522	15511.519167	28.137754
297.847163	15518.134613	28.142772
298.191130	15535.027392	28.147789
298.358728	15540.609717	28.152807
298.954855	15568.602336	28.157824
298.773836	15583.524235	28.162842
299.301369	15597.132423	28.167860
299.581628	15604.565035	28.172877
299.771930	15634.910095	28.177895
300.240529	15641.683866	28.182912
300.378642	15677.154867	28.187930
300.876373	15676.767197	28.192948
300.782450	15713.782913	28.197965
300.934438	15728.233633	28.202983
301.345638	15749.264547	28.208000
301.488879	15775.735658	28.213018
301.783170	15798.890879	28.218036
302.248770	15821.312828	28.223053
302.350568	15851.417928	28.228071
302.709653	15872.537422	28.233088
302.818796	15908.769966	28.238106
303.203169	15933.483856	28.243124
303.335021	15958.726746	28.248141
303.489379	15983.148085	28.253159
304.174838	16022.493755	28.258176
304.302990	16041.021088	28.263194
304.983941	16068.716686	28.268212
305.559081	16090.344893	28.273229
306.460941	16096.404620	28.278247
306.726188	16109.352197	28.283264
306.724564	16133.467374	28.288282
307.262081	16140.624629	28.293300
307.449822	16148.985725	28.298317
307.423105	16176.610069	28.303335
307.878207	16180.458223	28.308352
308.100609	16209.022731	28.313370
308.252409	16221.307261	28.318388
308.489365	16241.379523	28.323405
308.510382	16271.866583	28.328423
309.128770	16290.852643	28.333440
309.219043	16328.568940	28.338458
309.394632	16344.253944	28.343476
309.211585	16368.390921	28.348493
309.629870	16402.147259	28.353511
310.259604	16428.602581	28.358528
310.289609	16468.890776	28.363546
310.612688	16491.599579	28.368564
311.127613	16515.756443	28.373581
311.411467	16543.666168	28.378599
311.930616	16562.659718	28.383616
311.813452	16596.670894	28.388634
312.261622	16617.208169	28.393652
312.768192	16636.776600	28.398669
313.196274	16668.033747	28.403687
313.400568	16688.306465	28.408704
313.732988	16705.502345	28.413722
314.004044	16728.159753	28.418740
314.378034	16753.865116	28.423757
315.113880	16771.194005	28.428775
315.473100	16782.919195	28.433792
315.802567	16810.144624	28.438810
315.969355	16823.154355	28.443828
316.596007	16850.012635	28.448845
316.576418	16862.521431	28.453863
316.998680	16874.266956	28.458880
316.747748	16903.251070	28.463898
317.122969	16928.335310	28.468916
317.617970	16958.067718	28.473933
317.930864	16981.444176	28.478951
318.248065	16997.681254	28.483968
318.484627	17044.266177	28.488986
318.785749	17068.843194	28.494004
319.295004	17081.919227	28.499021
319.310920	17117.674213	28.504039
319.251618	17137.965316	28.509056
319.771672	17173.510174	28.514074
320.098721	17198.869839	28.519092
320.722308	17224.857059	28.524109
320.944899	17261.185708	28.529127
321.035551	17280.470862	28.534144
321.162683	17311.663497	28.539162
321.947108	17338.652398	28.544180
321.836916	17375.648497	28.549197
322.221726	17410.265094	28.554215
322.784573	17432.765226	28.559232
323.564353	17459.411783	28.564250
323.882299	17481.320326	28.569268
324.256014	17497.626086	28.574285
324.848620	17524.359276	28.579303
325.153532	17537.052525	28.584320
325.245367	17570.575650	28.589338
325.639952	17577.455185	28.594356
325.904823	17605.209223	28.599373
326.323913	17624.888516	28.604391
326.946240	17644.817724	28.609408
326.931199	17665.228444	28.614426
326.817827	17682.382086	28.619444
327.239460	17711.155801	28.624461
327.393274	17743.229681	28.629479
328.104225	17766.339758	28.634496
328.162196	17807.413182	28.639514
328.141354	17814.422412	28.644532
328.828088	17828.003467	28.649549
328.781607	17873.860205	28.654567
328.881829	17886.667068	28.659584
329.443708	17914.993223	28.664602
329.437152	17946.585995	28.669620
330.208324	17978.939931	28.674637
330.507576	18006.393537	28.679655
331.218348	18033.499721	28.684672
331.198118	18064.852785	28.689690
331.355386	18089.236233	28.694708
331.679451	18122.861730	28.699725
331.794143	18149.498929	28.704743
332.597621	18177.922891	28.709760
332.917625	18210.926382	28.714778
333.043647	18245.055365	28.719796
333.489680	18274.493176	28.724813
333.753364	18310.235434	28.729831
334.080692	18332.147226	28.734848
334.416736	18365.509128	28.739866
334.678634	18396.564349	28.744884
335.399763	18414.179134	28.749901
335.531309	18455.351599	28.754919
336.022069	18478.059626	28.759936
336.575674	18502.943572	28.764954
336.594109	18526.876584	28.769972
337.289924	18556.972001	28.774989
337.289365	18579.478933	28.780007
338.103090	18606.608691	28.785024
338.330276	18626.161562	28.790042
338.123904	18658.460875	28.795060
338.672691	18681.412718	28.800077
338.862040	18718.228831	28.805095
339.226152	18750.384270	28.810112
339.681978	18766.250306	28.815130
340.047153	18798.033215	28.820148
340.457187	18822.874013	28.825165
340.881517	18856.262663	28.830183
341.077573	18889.087726	28.835200
341.665175	18911.192730	28.840218
342.181597	18939.438621	28.845236
342.555238	18952.240588	28.850253
342.963991	18987.049018	28.855271
343.273225	19003.123708	28.860288
343.823993	19015.095085	28.865306
343.862911	19039.434308	28.870324
344.377858	19066.846356	28.875341
344.505482	19078.840328	28.880359
344.708127	19114.635105	28.885376
345.171105	19138.188742	28.890394
345.585242	19159.305130	28.895412
346.044410	19180.622654	28.900429
346.487701	19202.571134	28.905447
346.468015	19220.772643	28.910464
346.727190	19247.362706	28.915482
346.825953	19274.731590	28.920500
347.384233	19288.906103	28.925517
347.579440	19322.416128	28.930535
347.667901	19343.202739	28.935552
347.938116	19378.344383	28.940570
348.290563	19410.338067	28.945588
348.778433	19429.486198	28.950605
349.027509	19472.001796	28.955623
349.231326	19495.553172	28.960640
349.635471	19526.280858	28.965658
349.665564	19565.229278	28.970676
350.006503	19591.855722	28.975693
350.355825	19632.908388	28.980711
350.886320	19660.847012	28.985728
351.640212	19699.854462	28.990746
351.511787	19734.854502	28.995764
351.950551	19766.774916	29.000781
352.798732	19796.709458	29.005799
353.050505	19824.670740	29.010816
353.298471	19858.401485	29.015834
353.349953	19898.235619	29.020852
353.834929	19919.331116	29.025869
354.429684	19960.897569	29.030887
354.727104	19993.683597	29.035904
355.554223	20019.184341	29.040922
355.546026	20052.033366	29.045940
356.174227	20076.845334	29.050957
356.430650	20100.238429	29.055975
356.910179	20128.371863	29.060992
357.306784	20165.630861	29.066010
357.609342	20181.393610	29.071028
358.268116	20206.752959	29.076045
358.266530	20228.353239	29.081063
358.480627	20259.163836	29.086080
359.108178	20278.816419	29.091098
358.905784	20317.989607	29.096116
359.373507	20347.997645	29.101133
360.059641	20373.222176	29.106151
359.826720	20421.040002	29.111168
360.243905	20448.708674	29.116186
360.463491	20480.456775	29.121204
360.888521	20523.987511	29.126221
361.318901	20560.030449	29.131239
362.002146	20598.280797	29.136256
362.662409	20628.200412	29.141274
362.348791	20660.791450	29.146292
363.058664	20699.396919	29.151309
363.508425	20738.146310	29.156327
363.430439	20771.927019	29.161344
364.253419	20798.236138	29.166362
364.343435	20838.266944	29.171380
365.070221	20856.812115	29.176397
365.324106	20895.176494	29.181415
365.593624	20914.171832	29.186432
366.324296	20940.406119	29.191450
366.093280	20985.937520	29.196468
366.409921	21005.056981	29.201485
366.971345	21031.245933	29.206503
367.306371	21078.619279	29.211520
367.963454	21102.302062	29.216538
368.389210	21121.958720	29.221556
368.628086	21146.082300	29.226573
368.906723	21184.567087	29.231591
369.129656	21207.567086	29.236608
369.837561	21228.250005	29.241626
369.623284	21270.608035	29.246644
370.077410	21296.614485	29.251661
370.602529	21329.125233	29.256679
370.903736	21358.700220	29.261696
371.235113	21397.437809	29.266714
371.925507	21433.572055	29.271732
371.790895	21456.956234	29.276749
372.298812	21490.261570	29.281767
372.570448	21535.051319	29.286784
373.041942	21557.573540	29.291802
373.136730	21601.482786	29.296820
373.499381	21640.323887	29.301837
373.932237	21675.149015	29.306855
374.192836	21724.335009	29.311872
374.731368	21770.462755	29.316890
374.876585	21810.726659	29.321908
375.384989	21845.162865	29.326925
375.895898	21886.290967	29.331943
376.159995	21930.799503	29.336960
376.898940	21962.472559	29.341978
377.160806	22003.582366	29.346996
377.605752	22038.607996	29.352013
378.091413	22070.524042	29.357031
378.630318	22098.231353	29.362048
379.187234	22128.249841	29.367066
379.586215	22174.351383	29.372084
380.134315	22189.985660	29.377101
380.550933	22206.901873	29.382119
381.003833	22237.909847	29.387136
381.541676	22251.212903	29.392154
382.052900	22278.951721	29.397172
382.071461	22303.944687	29.402189
382.463133	22322.286651	29.407207
383.027838	22352.245253	29.412224
383.445125	22383.578174	29.417242
383.854145	22400.308352	29.422260
384.047875	22430.599518	29.427277
384.092332	22448.422774	29.432295
384.282092	22484.113065	29.437312
384.863785	22513.009905	29.442330
385.244724	22556.259493	29.447348
385.376372	22573.321534	29.452365
385.868419	22598.075693	29.457383
386.222831	22637.739697	29.462400
386.691742	22667.336882	29.467418
387.020588	22700.726078	29.472436
387.203054	22737.609011	29.477453
387.665315	22759.403490	29.482471
387.602019	22790.644448	29.487488
388.456916	22825.564756	29.492506
388.876591	22860.091352	29.497524
388.607989	22904.552815	29.502541
389.205496	22929.869611	29.507559
389.611223	22968.266813	29.512576
389.969166	22999.515103	29.517594
390.214797	23038.751630	29.522612
390.469554	23077.727661	29.527629
391.745622	23111.566991	29.532647
391.670578	23156.904914	29.537664
392.268767	23180.593907	29.542682
392.497459	23221.452231	29.547700
393.019007	23258.283921	29.552717
393.361662	23287.428207	29.557735
393.712036	23325.227801	29.562752
393.873571	23359.305895	29.567770
394.218956	23407.751071	29.572788
394.606619	23445.175590	29.577805
395.556960	23478.013695	29.582823
395.219558	23532.343289	29.587840
395.859413	23553.982173	29.592858
396.849636	23586.844081	29.597876
398.020385	23608.292903	29.602893
398.658639	23626.827883	29.607911
398.650571	23657.021998	29.612928
399.330021	23661.246087	29.617946
399.540335	23695.433707	29.622964
399.548292	23713.682460	29.627981
400.260214	23729.768715	29.632999
400.209683	23777.430545	29.638016
400.856586	23789.044467	29.643034
401.165592	23821.716867	29.648052
401.506821	23853.672124	29.653069
401.762197	23878.796038	29.658087
401.708514	23916.432196	29.663104
402.197116	23949.585885	29.668122
402.636276	23983.646288	29.673140
402.941890	24016.530733	29.678157
403.471778	24052.510640	29.683175
403.602702	24099.069301	29.688192
403.944980	24141.164343	29.693210
404.586830	24171.563876	29.698228
404.381468	24208.972822	29.703245
404.981424	24260.296145	29.708263
405.080508	24303.910482	29.713280
405.466858	24343.993507	29.718298
405.971839	24399.842894	29.723316
406.329587	24459.831012	29.728333
406.906502	24502.289786	29.733351
407.392295	24549.599065	29.738368
407.771275	24594.693068	29.743386
408.225743	24617.925802	29.748404
408.899060	24654.957110	29.753421
409.156982	24688.581555	29.758439
409.452837	24716.542493	29.763456
409.756611	24765.193782	29.768474
410.619150	24788.765071	29.773492
411.152929	24843.569239	29.778509
411.725993	24853.659607	29.783527
411.836613	24894.607988	29.788544
412.252052	24930.122070	29.793562
412.965947	24953.195797	29.798580
413.198820	24997.650144	29.803597
413.882955	25018.330791	29.808615
414.104486	25062.085235	29.813632
414.323496	25089.305975	29.818650
414.736301	25126.973852	29.823668
414.760102	25164.394206	29.828685
415.504937	25197.972869	29.833703
415.555824	25227.661903	29.838720
416.010960	25282.614812	29.843738
416.523203	25328.762591	29.848756
417.709514	25345.409846	29.853773
418.743349	25353.160710	29.858791
419.371189	25392.566646	29.863808
419.834639	25405.954323	29.868826
420.358261	25425.632243	29.873844
420.610951	25445.633012	29.878861
421.107456	25466.924725	29.883879
421.296782	25493.496240	29.888896
421.867664	25514.977838	29.893914
421.946619	25526.199828	29.898932
422.224456	25557.450928	29.903949
422.522015	25573.007148	29.908967
422.847297	25616.262092	29.913984
423.057848	25637.200972	29.919002
423.368002	25667.602635	29.924020
423.568900	25714.889849	29.929037
423.818593	25736.975157	29.934055
424.161747	25783.380431	29.939072
424.529396	25830.917935	29.944090
425.184023	25866.173829	29.949108
425.198619	25916.930830	29.954125
425.466337	25957.356644	29.959143
425.655248	26004.923138	29.964160
426.070979	26064.741013	29.969178
426.781394	26109.242891	29.974196
426.640259	26171.425855	29.979213
427.455485	26212.574161	29.984231
427.991703	26273.048768	29.989248
428.297883	26315.043405	29.994266
429.076207	26353.518588	29.999284
429.145338	26408.625873	30.004301
429.860955	26458.227455	30.009319
430.273018	26511.287263	30.014336
430.961485	26550.219203	30.019354
431.990391	26573.618516	30.024372
432.092851	26614.626940	30.029389
433.071894	26640.798794	30.034407
433.293918	26664.123529	30.039424
433.629365	26700.039525	30.044442
434.197340	26729.712765	30.049460
434.274643	26758.255688	30.054477
434.273048	26796.537112	30.059495
435.040744	26826.496211	30.064512
435.400139	26865.617639	30.069530
435.980809	26898.892764	30.074548
436.237114	26933.822114	30.079565
436.868798	26973.090294	30.084583
437.429769	26998.591913	30.089600
437.798183	27046.266030	30.094618
438.408283	27075.681872	30.099636
439.008832	27116.488525	30.104653
438.918901	27147.342772	30.109671
439.542685	27183.795348	30.114688
439.806091	27218.464977	30.119706
440.368530	27263.354464	30.124724
440.850375	27313.146405	30.129741
441.565766	27337.281437	30.134759
442.094630	27361.491919	30.139776
442.511698	27402.096892	30.144794
442.995751	27446.704714	30.149812
443.156318	27472.485174	30.154829
443.554239	27508.175563	30.159847
443.886025	27527.472991	30.164864
444.563606	27567.587789	30.169882
444.956057	27610.956356	30.174900
444.907690	27649.776706	30.179917
445.496203	27687.276042	30.184935
446.226016	27725.999389	30.189952
446.242699	27766.818763	30.194970
446.944535	27806.602529	30.199988
447.066074	27855.742867	30.205005
447.629864	27896.166552	30.210023
448.317134	27929.652947	30.215040
448.910421	27979.068329	30.220058
449.207314	28028.428654	30.225076
449.567180	28060.112762	30.230093
450.535817	28094.235420	30.235111
451.435174	28122.902707	30.240128
451.411740	28168.365512	30.245146
451.832041	28199.184598	30.250164
452.291908	28231.752902	30.255181
452.686501	28274.999993	30.260199
453.002334	28303.697527	30.265216
453.341062	28350.151070	30.270234
453.596333	28390.406099	30.275252
453.634666	28435.445367	30.280269
454.183647	28482.929486	30.285287
454.785275	28530.238316	30.290304
454.985142	28576.705173	30.295322
455.394509	28619.790092	30.300340
455.813711	28668.954807	30.305357
456.103607	28712.902090	30.310375
456.484748	28769.144084	30.315392
456.974043	28808.363764	30.320410
457.652177	28865.025235	30.325428
457.764473	28910.911314	30.330445
458.231621	28955.311660	30.335463
458.871787	29006.577525	30.340480
458.865335	29068.883307	30.345498
459.243199	29116.532064	30.350516
460.076689	29171.669592	30.355533
460.679485	29214.785157	30.360551
461.257072	29267.718100	30.365568
461.754729	29318.359946	30.370586
462.602425	29356.934458	30.375604
462.763685	29412.556539	30.380621
463.069434	29467.679859	30.385639
463.985342	29502.258300	30.390656
464.179495	29552.470137	30.395674
465.043411	29596.728652	30.400692
465.711109	29639.035994	30.405709
466.312911	29671.975410	30.410727
466.827311	29721.961821	30.415744
466.851834	29760.168843	30.420762
467.685802	29795.531609	30.425780
467.736914	29844.050898	30.430797
468.410898	29892.281988	30.435815
468.946839	29919.516319	30.440832
469.458962	29955.691903	30.445850
470.130818	29995.436955	30.450868
470.661901	30035.595376	30.455885
470.815242	30066.829310	30.460903
471.126589	30110.417616	30.465920
471.338094	30164.593788	30.470938
471.647198	30206.029881	30.475956
472.219178	30261.367205	30.480973
472.530746	30313.266347	30.485991
473.267714	30357.432101	30.491008
473.769107	30407.424257	30.496026
474.117232	30463.177746	30.501044
474.933255	30514.078337	30.506061
475.262416	30559.696516	30.511079
475.918924	30606.700032	30.516096
476.057481	30656.640425	30.521114
476.800344	30703.014224	30.526132
477.054248	30749.120888	30.531149
477.478335	30797.170655	30.536167
478.020735	30841.212680	30.541184
478.458221	30904.754989	30.546202
479.134279	30949.316607	30.551220
479.708859	31002.001898	30.556237
480.272001	31044.868557	30.561255
480.224740	31090.644317	30.566272
480.622757	31149.205520	30.571290
481.084853	31184.732981	30.576308
481.767957	31235.918622	30.581325
481.996406	31286.051501	30.586343
482.642021	31321.228497	30.591360
483.064881	31365.610923	30.596378
484.034260	31397.149256	30.601396
484.858692	31436.025548	30.606413
485.274416	31472.719474	30.611431
485.814319	31504.551815	30.616448
486.091149	31556.064810	30.621466
486.437055	31595.488972	30.626484
487.054163	31628.841267	30.631501
487.750390	31652.787177	30.636519
488.352956	31700.776482	30.641536
488.602452	31732.617697	30.646554
488.818417	31781.322925	30.651572
489.287182	31823.453246	30.656589
489.887405	31865.130864	30.661607
490.392469	31902.259149	30.666624
490.735106	31957.145383	30.671642
491.014058	31994.354027	30.676660
491.421857	32045.554520	30.681677
491.847793	32093.964001	30.686695
492.523317	32151.787890	30.691712
493.124583	32196.845547	30.696730
493.085323	32254.564564	30.701748
493.847418	32295.405740	30.706765
494.469747	32351.144019	30.711783
495.268897	32392.015785	30.716800
495.915663	32444.684741	30.721818
496.999032	32471.531904	30.726836
497.756793	32509.716785	30.731853
498.023553	32526.540042	30.736871
498.458056	32570.028560	30.741888
499.022093	32598.708278	30.746906
499.342632	32638.356497	30.751924
499.752205	32675.186486	30.756941
499.800855	32726.849821	30.761959
500.413294	32763.055021	30.766976
500.866323	32811.197480	30.771994
501.121997	32860.257375	30.777012
501.817546	32909.419163	30.782029
501.564115	32964.521910	30.787047
502.206887	33007.243859	30.792064
502.980009	33070.963313	30.797082
503.479521	33117.201412	30.802100
503.714087	33167.392625	30.807117
503.834864	33225.811476	30.812135
504.682904	33280.344170	30.817152
505.074738	33337.288954	30.822170
505.688058	33393.185084	30.827188
506.432126	33440.471211	30.832205
506.689959	33507.882618	30.837223
507.397187	33554.210227	30.842240
507.711613	33589.577233	30.847258
509.071126	33653.080992	30.852276
509.706696	33691.343239	30.857293
509.947371	33731.061966	30.862311
510.774430	33774.856833	30.867328
510.969299	33800.654393	30.872346
511.078214	33840.643433	30.877364
511.714316	33875.028182	30.882381
512.054630	33926.123863	30.887399
512.899792	33977.694169	30.892416
513.403685	34018.591768	30.897434
513.227357	34067.329948	30.902452
514.220631	34109.926400	30.907469
514.614065	34160.174127	30.912487
515.217962	34208.815244	30.917504
515.605042	34262.522896	30.922522
516.001141	34317.998007	30.927540
516.486376	34358.172691	30.932557
516.685024	34418.382007	30.937575
517.378267	34480.429684	30.942592
517.949680	34528.310770	30.947610
518.218831	34586.638250	30.952628
519.117555	34635.514258	30.957645
519.255733	34707.103479	30.962663
519.859939	34759.015688	30.967680
520.370703	34811.769002	30.972698
520.704082	34878.964258	30.977716
521.727367	34932.353606	30.982733
521.964038	35005.955747	30.987751
522.547395	35050.587332	30.992768
523.315269	35113.810985	30.997786
523.435010	35163.960294	31.002804
524.419113	35214.400884	31.007821
524.725240	35290.189259	31.012839
525.126346	35335.038236	31.017856
525.661892	35400.280059	31.022874
526.172287	35463.506633	31.027892
526.681160	35509.904389	31.032909
527.293782	35575.049485	31.037927
527.650654	35652.363795	31.042944
528.585597	35699.556574	31.047962
528.932230	35763.374762	31.052980
529.450315	35816.823759	31.057997
530.339363	35866.901512	31.063015
531.123719	35918.809127	31.068032
532.050583	35969.021477	31.073050
532.566045	36017.820688	31.078068
533.162569	36048.752523	31.083085
533.912991	36098.391116	31.088103
534.173531	36142.660819	31.093120
534.237511	36187.181090	31.098138
534.571597	36239.785741	31.103156
535.211965	36287.028673	31.108173
535.540680	36354.566404	31.113191
536.393347	36409.207932	31.118208
537.199872	36446.104435	31.123226
537.273892	36497.024934	31.128244
538.210201	36532.379531	31.133261
538.582315	36572.451425	31.138279
539.143682	36610.390064	31.143296
540.248467	36646.714492	31.148314
540.531764	36684.923046	31.153332
541.361849	36717.649377	31.158349
541.557678	36762.441847	31.163367
542.288763	36807.499198	31.168384
542.347024	36847.728948	31.173402
542.747975	36900.927295	31.178420
543.192416	36938.245180	31.183437
543.872404	36997.143119	31.188455
543.979417	37038.213798	31.193472
544.595159	37097.529099	31.198490
544.712769	37162.057580	31.203508
545.411412	37212.461362	31.208525
545.964157	37280.799612	31.213543
546.463484	37337.464979	31.218560
546.790214	37393.241968	31.223578
547.636572	37444.594160	31.228596
549.353394	37479.227299	31.233613
549.759271	37537.965816	31.238631
550.111931	37581.016873	31.243648
551.218740	37622.445323	31.248666
551.945631	37657.271183	31.253684
552.066965	37692.091073	31.258701
552.967201	37734.722625	31.263719
553.453783	37770.608709	31.268736
553.902863	37817.008169	31.273754
554.513085	37853.272073	31.278772
555.032799	37897.006861	31.283789
555.351827	37947.817032	31.288807
555.761668	37980.820886	31.293824
555.720343	38045.371745	31.298842
556.370273	38099.904415	31.303860
556.933843	38150.680978	31.308877
557.279334	38210.801655	31.313895
557.666311	38272.901096	31.318912
558.526802	38330.737426	31.323930
558.957064	38397.650641	31.328948
559.435627	38446.339776	31.333965
559.963109	38507.359673	31.338983
560.315942	38559.456112	31.344000
561.421645	38628.012910	31.349018
561.657237	38692.884794	31.354036
562.092106	38758.393759	31.359053
562.396066	38813.538866	31.364071
562.729210	38899.802964	31.369088
563.623386	38952.350515	31.374106
563.922546	39021.567173	31.379124
564.668918	39082.565314	31.384141
565.342186	39147.504836	31.389159
565.799967	39213.516499	31.394176
566.193431	39281.268483	31.399194
566.570311	39353.771341	31.404212
567.120282	39407.934648	31.409229
568.117218	39474.653050	31.414247
568.333355	39549.880392	31.419264
569.202688	39592.583046	31.424282
569.854255	39668.826470	31.429300
570.247035	39712.316503	31.434317
570.961186	39765.997499	31.439335
571.671419	39847.850916	31.444352
572.631564	39898.115394	31.449370
572.545121	39964.333329	31.454388
573.323266	40021.116220	31.459405
573.928604	40095.184858	31.464423
574.142942	40154.631552	31.469440
574.621958	40215.693677	31.474458
575.244938	40292.685609	31.479476
575.951290	40350.816715	31.484493
576.496833	40427.193953	31.489511
576.856245	40493.483281	31.494528
577.439545	40562.683016	31.499546
578.192937	40630.461883	31.504564
578.862041	40699.355186	31.509581
579.575897	40764.674458	31.514599
580.313113	40841.543431	31.519616
580.951926	40892.120641	31.524634
581.727266	40964.350825	31.529652
581.951263	41026.478366	31.534669
582.384352	41091.092931	31.539687
582.721975	41152.751802	31.544704
583.843816	41223.101685	31.549722
584.434277	41286.442905	31.554740
585.589278	41351.659467	31.559757
586.077785	41411.380691	31.564775
587.124263	41460.705553	31.569792
588.413079	41499.230034	31.574810
589.166654	41547.068878	31.579828
590.097060	41580.834235	31.584845
590.542499	41609.488293	31.589863
591.067738	41648.790777	31.594880
591.277560	41691.660487	31.599898
591.880908	41723.793880	31.604916
592.424743	41764.576133	31.609933
593.064220	41804.977366	31.614951
593.568789	41858.319803	31.619968
594.274104	41894.093003	31.624986
594.673203	41936.157244	31.630004
595.029616	41982.988117	31.635021
595.413854	42038.309051	31.640039
595.733599	42083.259801	31.645056
596.154993	42158.257720	31.650074
596.707458	42208.846255	31.655092
597.116984	42264.154424	31.660109
597.834329	42324.350217	31.665127
598.272373	42382.161886	31.670144
598.980937	42436.524011	31.675162
599.812160	42504.553384	31.680180
599.661100	42562.421617	31.685197
600.862752	42599.167638	31.690215
601.132123	42667.343904	31.695232
602.352571	42704.046150	31.700250
602.769853	42760.603803	31.705268
603.138426	42812.519839	31.710285
603.774347	42874.452812	31.715303
603.727216	42938.535677	31.720320
604.335197	42981.036055	31.725338
605.374663	43041.214598	31.730356
606.482878	43088.042310	31.735373
607.496479	43126.901331	31.740391
607.946658	43191.707168	31.745408
608.328565	43244.445689	31.750426
608.812520	43295.761228	31.755444
609.419847	43353.498718	31.760461
610.164941	43402.025436	31.765479
610.344979	43478.338776	31.770496
611.067496	43535.755699	31.775514
611.808777	43594.400088	31.780532
612.019721	43658.482372	31.785549
612.409287	43709.520794	31.790567
613.266208	43777.667805	31.795584
613.609236	43843.010486	31.800602
614.188428	43913.760612	31.805620
614.897074	43989.758585	31.810637
615.725969	44059.005808	31.815655
615.938972	44139.749027	31.820672
616.656500	44202.304676	31.825690
617.354090	44263.570320	31.830708
618.330822	44326.299656	31.835725
619.666437	44361.113228	31.840743
621.134454	44404.145783	31.845760
621.946969	44440.203731	31.850778
622.848000	44486.714900	31.855796
623.315556	44520.338899	31.860813
623.899586	44557.881478	31.865831
624.413922	44591.677984	31.870848
624.711581	44634.376950	31.875866
625.488516	44666.923532	31.880884
625.762512	44717.062140	31.885901
626.458488	44749.959325	31.890919
626.846693	44800.042128	31.895936
627.614965	44850.058246	31.900954
628.027170	44901.468824	31.905972
628.441583	44946.446629	31.910989
629.182078	45000.877970	31.916007
629.218900	45060.084305	31.921024
629.998074	45115.229136	31.926042
630.327137	45172.149410	31.931060
630.508375	45239.901821	31.936077
631.611458	45310.283959	31.941095
632.310934	45362.022421	31.946112
632.890166	45426.052562	31.951130
633.313270	45484.454280	31.956148
633.563389	45556.588521	31.961165
634.287311	45612.081291	31.966183
634.724498	45688.076264	31.971200
635.134480	45748.452765	31.976218
635.659062	45805.101037	31.981236
635.910249	45888.600510	31.986253
636.611217	45967.154360	31.991271
636.728087	46045.953006	31.996288
637.847336	46133.322229	32.001306
638.499217	46210.891167	32.006324
638.887435	46298.084198	32.011341
639.931494	46365.949664	32.016359
640.440809	46448.852260	32.021376
640.975315	46529.425961	32.026394
642.448946	46589.658079	32.031412
643.636938	46674.283611	32.036429
644.505076	46730.706639	32.041447
644.754293	46800.539765	32.046464
645.603703	46861.253977	32.051482
646.094969	46918.400190	32.056500
646.543794	46987.953021	32.061517
647.400449	47051.301274	32.066535
647.770600	47135.021203	32.071552
648.013647	47203.090016	32.076570
649.124094	47269.967146	32.081588
649.326240	47353.670691	32.086605
650.214019	47426.739668	32.091623
650.900785	47505.312118	32.096640
651.344444	47580.866197	32.101658
652.097597	47641.046258	32.106676
652.269793	47728.116688	32.111693
653.394063	47800.679424	32.116711
654.179391	47877.628644	32.121728
654.627184	47964.239855	32.126746
655.620545	48039.295023	32.131764
656.215143	48109.258184	32.136781
656.857389	48189.216489	32.141799
657.572705	48259.195730	32.146816
658.472641	48331.856320	32.151834
658.838570	48400.399257	32.156852
659.465155	48476.918828	32.161869
660.232452	48547.878574	32.166887
660.773761	48626.315081	32.171904
661.362879	48705.855037	32.176922
662.541130	48778.324838	32.181940
662.915612	48863.592115	32.186957
663.592491	48933.772624	32.191975
664.884787	48993.536962	32.196992
665.913888	49043.611841	32.202010
666.828764	49095.582577	32.207028
667.276893	49170.634685	32.212045
667.962426	49221.559961	32.217063
668.869767	49278.171065	32.222080
669.183836	49341.292047	32.227098
670.057127	49393.270276	32.232116
670.477077	49444.292121	32.237133
670.609743	49501.077765	32.242151
671.303391	49553.331199	32.247168
671.659865	49629.463268	32.252186
672.756706	49665.978959	32.257204
673.359965	49724.182992	32.262221
674.094966	49786.111974	32.267239
674.616734	49838.011779	32.272256
675.222903	49907.270162	32.277274
675.795382	49973.192328	32.282292
676.193628	50049.095484	32.287309
676.981266	50109.171137	32.292327
677.556248	50192.326940	32.297344
677.939192	50261.139413	32.302362
678.892170	50335.241910	32.307380
679.214218	50415.980711	32.312397
679.756938	50486.848248	32.317415
680.527417	50568.630323	32.322432
681.109224	50648.271631	32.327450
681.641408	50726.463214	32.332468
682.253319	50818.597450	32.337485
683.170804	50898.937512	32.342503
683.747502	50994.991488	32.347520
684.573779	51068.293518	32.352538
685.508062	51139.896574	32.357556
686.011597	51236.802953	32.362573
686.579245	51313.214684	32.367591
687.383095	51406.927735	32.372608
688.168299	51479.455317	32.377626
689.417959	51557.227011	32.382644
690.124439	51632.847947	32.387661
691.157278	51696.733845	32.392679
692.642229	51741.324932	32.397696
693.378619	51813.069484	32.402714
694.127297	51859.403418	32.407732
694.491158	51933.104512	32.412749
695.246710	51989.432772	32.417767
696.091974	52044.591820	32.422784
696.611041	52111.234145	32.427802
697.474214	52167.706788	32.432820
697.813627	52220.980691	32.437837
698.641141	52287.606122	32.442855
699.081875	52348.703955	32.447872
699.395848	52422.604356	32.452890
700.026601	52482.621410	32.457908
700.533267	52569.933595	32.462925
701.351602	52645.550444	32.467943
701.755662	52720.195191	32.472960
702.507712	52804.767782	32.477978
703.196697	52871.158616	32.482996
703.633835	52958.130252	32.488013
704.298039	53039.823702	32.493031
704.975357	53126.379164	32.498048
705.139205	53205.224048	32.503066
705.821778	53282.588475	32.508084
706.611079	53370.724336	32.513101
706.959553	53443.073684	32.518119
707.656985	53539.977339	32.523136
707.992166	53626.908443	32.528154
709.121033	53718.618528	32.533172
709.651163	53814.950584	32.538189
710.378237	53900.968398	32.543207
710.989748	53986.518936	32.548224
711.820438	54091.124790	32.553242
712.903518	54181.787115	32.558260
713.197974	54275.425683	32.563277
714.075537	54378.895732	32.568295
714.984865	54468.248816	32.573312
715.615477	54549.622976	32.578330
716.756599	54634.618776	32.583348
717.229636	54732.811315	32.588365
717.966528	54822.569210	32.593383
719.003961	54910.142733	32.598400
719.308355	55011.624309	32.603418
720.234189	55101.994277	32.608436
720.661318	55183.211103	32.613453
721.501291	55268.911211	32.618471
722.865678	55367.498724	32.623488
723.360090	55456.837470	32.628506
723.809251	55549.823458	32.633524
724.643753	55642.609681	32.638541
725.446869	55721.748783	32.643559
726.381999	55810.469834	32.648576
726.943611	55922.907077	32.653594
727.817705	55996.543408	32.658612
728.707308	56096.773002	32.663629
729.136667	56182.697430	32.668647
730.018787	56268.928994	32.673664
730.448898	56367.942100	32.678682
731.141598	56456.771159	32.683700
731.866988	56564.706767	32.688717
732.129282	56650.271684	32.693735
733.062887	56737.674745	32.698752
733.678669	56856.504829	32.703770
734.561095	56963.347597	32.708788
735.218993	57054.240205	32.713805
735.802666	57171.653670	32.718823
736.736108	57258.727752	32.723840
737.895003	57358.523572	32.728858
738.978385	57450.935189	32.733876
740.117960	57546.024912	32.738893
740.853452	57634.410854	32.743911
741.609736	57711.087723	32.748928
742.506062	57806.852068	32.753946
743.833776	57858.712800	32.758964
744.870282	57923.289243	32.763981
745.437211	58003.072426	32.768999
746.274077	58065.294409	32.774016
746.785031	58140.853469	32.779034
747.290357	58208.865126	32.784052
747.943743	58268.360858	32.789069
748.608141	58336.530773	32.794087
749.487679	58408.957225	32.799104
749.809748	58490.593672	32.804122
750.535108	58564.737501	32.809140
751.397711	58623.885355	32.814157
751.239022	58714.755085	32.819175
752.345175	58780.264267	32.824192
752.965008	58875.797155	32.829210
753.830229	58947.700734	32.834228
754.714907	59024.763564	32.839245
755.123650	59119.191542	32.844263
756.022699	59200.467734	32.849280
756.605523	59299.538503	32.854298
757.249796	59392.089678	32.859316
758.288320	59476.041199	32.864333
758.813124	59568.419671	32.869351
759.501993	59658.972801	32.874368
760.726567	59748.635973	32.879386
761.104163	59843.906115	32.884404
761.950096	59936.462619	32.889421
762.270893	60034.925416	32.894439
763.355498	60133.851273	32.899456
763.769061	60234.630527	32.904474
764.615912	60335.720248	32.909492
765.604372	60419.551364	32.914509
765.867077	60534.305926	32.919527
766.988116	60644.873487	32.924544
767.688375	60746.692880	32.929562
768.359927	60844.390494	32.934580
769.274739	60947.701915	32.939597
769.934488	61044.123636	32.944615
770.833553	61143.479047	32.949632
771.642148	61246.944795	32.954650
772.394440	61342.333409	32.959668
773.635108	61441.825479	32.964685
774.232521	61550.470300	32.969703
775.109837	61643.244945	32.974720
775.828796	61734.122221	32.979738
776.615180	61833.562362	32.984756
777.854059	61921.604271	32.989773
778.600127	62029.574541	32.994791
779.562942	62104.187194	32.999808
780.293946	62214.586068	33.004826
780.807044	62293.306674	33.009844
781.925508	62379.532058	33.014861
782.277538	62480.247857	33.019879
783.453163	62570.813320	33.024896
784.362534	62659.037426	33.029914
784.843621	62762.162560	33.034932
785.861259	62853.992403	33.039949
786.230922	62955.225808	33.044967
787.283733	63032.752004	33.049984
787.851455	63135.767483	33.055002
788.277879	63205.445604	33.060020
789.475740	63310.038592	33.065037
789.915117	63391.030262	33.070055
790.401338	63486.412031	33.075072
791.153946	63573.458992	33.080090
791.746611	63674.591255	33.085108
792.684670	63770.786774	33.090125
793.396407	63850.499102	33.095143
794.625044	63951.222122	33.100160
795.298728	64051.490815	33.105178
795.727278	64150.775830	33.110196
796.774097	64239.977036	33.115213
797.234727	64355.001149	33.120231
798.412701	64455.835957	33.125248
799.132946	64553.020687	33.130266
799.984395	64663.610411	33.135284
800.571802	64761.022622	33.140301
801.070302	64864.472173	33.145319
801.939248	64971.460536	33.150336
803.079190	65069.980184	33.155354
803.512824	65182.641725	33.160372
804.439208	65288.005686	33.165389
805.344123	65396.831971	33.170407
806.667286	65509.183304	33.175424
807.370232	65599.866818	33.180442
808.112378	65719.013818	33.185460
808.949580	65810.453910	33.190477
809.753035	65932.618184	33.195495
810.537585	66020.331290	33.200512
811.512564	66131.339348	33.205530
812.118620	66233.376811	33.210548
813.329698	66335.005835	33.215565
813.752204	66446.027831	33.220583
814.594223	66554.358998	33.225600
815.421429	66658.539705	33.230618
815.928222	66766.846453	33.235636
816.927911	66873.894070	33.240653
817.366959	66988.334078	33.245671
818.618986	67101.628314	33.250688
819.212851	67213.530791	33.255706
819.593393	67329.390854	33.260724
821.006994	67446.022148	33.265741
821.424347	67563.659216	33.270759
822.513899	67676.313037	33.275776
823.152582	67790.258519	33.280794
824.154754	67909.105980	33.285812
825.218199	68007.520137	33.290829
826.223930	68135.231778	33.295847
826.983440	68235.060032	33.300864
828.247275	68341.132396	33.305882
829.017002	68455.199901	33.310900
829.997510	68540.116651	33.315917
830.663121	68654.783113	33.320935
831.237190	68759.028008	33.325952
832.416830	68872.072426	33.330970
833.039592	68963.195090	33.335988
833.833534	69044.334126	33.341005
834.432000	69158.047607	33.346023
835.500225	69245.025705	33.351040
836.586320	69338.357118	33.356058
837.059525	69437.055640	33.361076
838.301175	69540.389767	33.366093
838.865279	69635.037662	33.371111
839.572585	69735.494731	33.376128
840.456910	69827.653850	33.381146
840.961146	69933.817836	33.386164
842.128747	70031.827580	33.391181
842.545992	70150.371082	33.396199
843.534060	70249.990017	33.401216
844.170152	70356.280617	33.406234
844.875036	70469.119164	33.411252
845.820491	70577.017098	33.416269
846.868496	70684.880349	33.421287
847.989533	70784.834655	33.426304
848.860400	70898.097844	33.431322
849.310021	71019.611052	33.436340
849.860306	71114.855871	33.441357
850.550424	71240.837210	33.446375
851.761571	71358.414952	33.451392
852.725310	71465.923088	33.456410
853.518006	71586.279433	33.461428
854.417872	71707.036484	33.466445
855.256780	71824.233927	33.471463
855.980862	71943.364901	33.476480
857.180970	72055.470228	33.481498
858.005903	72181.492960	33.486516
859.022718	72293.451874	33.491533
860.183067	72399.000226	33.496551
861.094274	72503.268140	33.501568
862.257006	72594.094172	33.506586
863.375129	72699.296980	33.511604
864.759744	72786.341451	33.516621
865.560416	72895.974860	33.521639
865.915582	73001.016319	33.526656
866.902128	73097.660923	33.531674
867.619995	73200.320296	33.536692
869.001923	73295.841334	33.541709
869.647954	73395.947580	33.546727
870.474184	73478.666841	33.551744
871.413910	73572.648181	33.556762
871.723946	73676.771446	33.561780
872.616582	73786.407746	33.566797
873.416582	73894.043525	33.571815
873.936275	74004.865205	33.576832
874.711133	74107.280027	33.581850
875.089636	74234.574803	33.586868
876.090880	74353.012514	33.591885
876.906351	74467.575037	33.596903
877.746177	74592.909143	33.601920
878.881353	74705.918101	33.606938
879.464942	74828.911972	33.611956
880.108880	74941.564369	33.616973
880.986647	75045.351595	33.621991
881.705202	75176.813441	33.627008
882.235188	75290.667707	33.632026
883.168132	75417.970209	33.637044
884.365306	75546.691349	33.642061
885.326618	75659.512124	33.647079
885.918065	75804.080410	33.652096
887.158681	75910.354949	33.657114
887.679447	76037.600539	33.662132
888.251581	76172.448067	33.667149
889.435274	76284.529096	33.672167
890.475865	76425.250943	33.677184
891.242834	76544.117991	33.682202
892.182563	76681.678632	33.687220
893.022984	76803.183666	33.692237
894.079976	76940.152255	33.697255
894.746772	77080.204962	33.702272
895.913210	77212.335570	33.707290
896.534347	77353.484519	33.712308
896.840860	77482.252207	33.717325
898.022184	77624.672787	33.722343
898.895839	77766.467021	33.727360
900.207010	77896.676551	33.732378
901.327288	78024.534418	33.737396
902.754996	78156.522111	33.742413
904.033746	78277.719671	33.747431
904.747406	78401.340208	33.752448
906.090751	78523.142051	33.757466
908.961559	78596.733129	33.762484
910.124410	78689.305817	33.767501
910.945945	78785.751017	33.772519
911.892390	78860.742747	33.777536
912.384623	78951.520743	33.782554
912.874029	79047.204620	33.787572
913.548439	79151.120985	33.792589
914.125065	79247.164849	33.797607
914.676161	79367.037116	33.802624
915.674414	79457.073119	33.807642
916.320599	79580.250043	33.812660
916.839344	79700.856320	33.817677
917.974602	79817.395522	33.822695
918.594247	79942.411961	33.827712
919.442646	80067.595038	33.832730
920.265959	80196.739977	33.837748
920.958309	80311.930152	33.842765
921.841613	80447.413698	33.847783
922.241077	80584.694529	33.852800
923.652371	80714.058886	33.857818
924.287729	80859.281640	33.862836
925.336053	80996.803314	33.867853
926.719854	81125.770034	33.872871
927.084467	81255.196828	33.877888
927.946985	81389.425504	33.882906
928.544775	81526.586168	33.887924
929.766963	81646.579767	33.892941
930.726902	81775.662202	33.897959
932.223320	81890.764796	33.902976
933.428120	81985.760479	33.907994
934.245253	82107.079214	33.913012
935.293459	82228.191197	33.918029
936.544750	82341.350204	33.923047
938.303625	82431.714303	33.928064
939.510534	82528.558128	33.933082
940.245021	82625.287905	33.938100
940.906847	82722.497518	33.943117
942.484851	82820.073904	33.948135
942.961572	82935.173789	33.953152
943.705443	83034.439119	33.958170
944.606717	83139.856624	33.963188
945.106853	83248.600729	33.968205
945.884690	83373.220580	33.973223
946.401840	83494.595065	33.978240
947.124497	83613.029294	33.983258
947.921269	83738.710439	33.988276
948.861896	83870.641244	33.993293
949.989114	84001.057418	33.998311
950.844892	84136.461745	34.003328
951.598774	84256.557421	34.008346
952.678241	84393.091141	34.013364
953.727991	84522.018091	34.018381
954.592450	84657.936500	34.023399
955.352905	84794.744852	34.028416
956.533349	84929.464007	34.033434
957.528797	85056.480747	34.038452
958.008819	85210.654360	34.043469
959.359471	85339.000966	34.048487
960.170012	85497.834574	34.053504
961.002932	85640.112435	34.058522
962.023737	85778.940640	34.063540
962.809055	85918.414220	34.068557
963.708066	86060.930969	34.073575
964.759257	86215.077880	34.078592
965.931263	86359.627158	34.083610
966.636389	86511.624493	34.088628
967.818344	86667.764627	34.093645
968.960834	86800.092494	34.098663
969.627053	86954.698014	34.103680
970.230671	87106.285726	34.108698
971.589868	87255.964787	34.113716
972.178625	87410.263413	34.118733
973.217795	87564.776045	34.123751
974.692896	87714.825591	34.128768
975.528742	87872.034972	34.133786
976.387998	88008.652118	34.138804
977.673117	88165.362158	34.143821
978.782161	88300.189761	34.148839
979.994828	88437.240319	34.153856
981.195263	88574.255749	34.158874
982.372963	88702.371746	34.163892
982.962319	88833.547977	34.168909
984.298609	88954.342523	34.173927
984.993426	89089.917593	34.178944
986.084976	89203.030957	34.183962
986.789440	89350.027170	34.188980
987.353291	89483.329919	34.193997
988.743497	89610.481512	34.199015
989.352532	89749.065620	34.204032
990.187718	89880.177434	34.209050
991.491133	90023.642576	34.214068
992.335511	90168.111346	34.219085
993.163997	90301.351696	34.224103
993.863531	90466.418330	34.229120
994.992777	90601.845149	34.234138
996.058178	90746.662040	34.239156
997.041938	90898.709059	34.244173
998.662666	91042.313813	34.249191
999.381823	91190.711451	34.254208
1000.169551	91337.454795	34.259226
1001.493777	91481.153857	34.264244
1002.232110	91633.984984	34.269261
1003.046269	91782.226030	34.274279
1004.006000	91950.943393	34.279296
1005.322754	92092.396023	34.284314
1006.263135	92236.553207	34.289332
1007.092726	92396.155305	34.294349
1008.563186	92537.757108	34.299367
1009.527330	92701.096998	34.304384
1010.505104	92845.037148	34.309402
1011.377163	93012.840454	34.314420
1012.300306	93155.924780	34.319437
1013.721727	93314.914366	34.324455
1014.685769	93476.615442	34.329472
1015.616732	93624.002656	34.334490
1016.806704	93760.685259	34.339508
1017.583521	93937.777193	34.344525
1018.688811	94075.139350	34.349543
1019.766104	94239.446637	34.354560
1020.228323	94391.278000	34.359578
1021.898153	94536.561198	34.364596
1022.906180	94701.749488	34.369613
1023.756508	94849.328399	34.374631
1024.859526	95013.150202	34.379648
1025.723489	95172.317588	34.384666
1027.053141	95319.380549	34.389684
1027.734599	95480.552765	34.394701
1028.868237	95643.279936	34.399719
1029.753596	95797.343429	34.404736
1030.713268	95965.869757	34.409754
1031.699161	96119.470321	34.414772
1032.780894	96280.331543	34.419789
1034.020147	96439.290029	34.424807
1035.017178	96615.102820	34.429824
1035.983339	96767.667122	34.434842
1037.231539	96910.641440	34.439860
1037.855480	97062.370171	34.444877
1039.521446	97197.144375	34.449895
1040.474833	97334.411395	34.454912
1040.969004	97498.708653	34.459930
1042.625806	97631.936949	34.464948
1043.697466	97775.982311	34.469965
1044.787630	97915.559186	34.474983
1045.553063	98062.470321	34.480000
1046.448576	98211.259661	34.485018
1047.418837	98363.334209	34.490036
1048.251614	98525.383356	34.495053
1049.174716	98683.231052	34.500071
1050.561466	98842.113258	34.505088
1051.324200	99006.188826	34.510106
1052.379261	99169.308015	34.515124
1053.161624	99331.554347	34.520141
1053.913527	99500.911726	34.525159
1054.980648	99673.067320	34.530176
1055.825576	99850.264157	34.535194
1057.133497	100016.506275	34.540212
1058.316130	100190.355644	34.545229
1059.376106	100370.919893	34.550247
1060.665676	100538.990889	34.555264
1061.348817	100725.204700	34.560282
1062.999462	100893.600470	34.565300
1064.682085	101047.673740	34.570317
1066.290925	101202.607628	34.575335
1067.211127	101364.447665	34.580352
1068.278166	101530.093555	34.585370
1069.533749	101659.916249	34.590388
1070.210979	101828.511572	34.595405
1071.402826	101966.900880	34.600423
1072.658022	102123.396762	34.605440
1073.653170	102283.972067	34.610458
1074.843953	102442.005280	34.615476
1075.698827	102603.117622	34.620493
1077.070470	102748.158680	34.625511
1078.693997	102892.869498	34.630528
1079.642288	103037.720237	34.635546
1080.894283	103189.895521	34.640564
1081.743461	103352.886956	34.645581
1082.534182	103502.777316	34.650599
1083.778949	103657.892938	34.655616
1084.311573	103809.496880	34.660634
1085.707099	103964.381714	34.665652
1086.377202	104122.844408	34.670669
1087.446594	104278.991838	34.675687
1088.664287	104447.304811	34.680704
1089.318382	104605.868202	34.685722
1090.386866	104769.011705	34.690740
1091.095287	104948.825445	34.695757
1091.961990	105113.281722	34.700775
1093.683533	105290.222047	34.705792
1094.639618	105460.033001	34.710810
1095.540588	105620.354840	34.715828
1096.679314	105781.329755	34.720845
1097.871995	105930.639912	34.725863
1099.053433	106093.901088	34.730880
1099.956486	106254.840725	34.735898
1101.024067	106412.059307	34.740916
1101.900857	106581.188338	34.745933
1102.858905	106752.470088	34.750951
1104.414523	106906.962528	34.755968
1105.217120	107091.808817	34.760986
1106.389229	107266.838534	34.766004
1107.516558	107430.978132	34.771021
1108.510448	107602.595660	34.776039
1109.457070	107767.709308	34.781056
1110.482796	107956.849487	34.786074
1111.982311	108123.940932	34.791092
1112.729938	108306.577382	34.796109
1113.722361	108488.549679	34.801127
1115.291263	108666.539140	34.806144
1116.268438	108849.320382	34.811162
1117.688645	109013.272211	34.816180
1118.664594	109196.701852	34.821197
1120.305311	109359.006932	34.826215
1122.494453	109512.149343	34.831232
1123.675095	109670.788911	34.836250
1124.881075	109833.229572	34.841268
1126.180909	109976.907975	34.846285
1127.084424	110139.949447	34.851303
1128.257645	110291.916400	34.856320
1129.238333	110447.833033	34.861338
1130.139881	110616.992535	34.866356
1131.137002	110773.465641	34.871373
1132.102345	110955.770751	34.876391
1133.055258	111099.859027	34.881408
1134.214969	111266.184098	34.886426
1135.514785	111419.346898	34.891444
1136.719466	111592.003355	34.896461
1137.690351	111765.983202	34.901479
1139.281882	111925.667064	34.906496
1140.099181	112098.540571	34.911514
1141.029488	112275.119485	34.916532
1141.885870	112450.825168	34.921549
1142.927865	112625.059262	34.926567
1144.416579	112803.547178	34.931584
1145.045831	112984.122804	34.936602
1146.036220	113168.358285	34.941620
1146.977228	113357.331863	34.946637
1148.397631	113549.452887	34.951655
1149.807460	113724.123601	34.956672
1150.584600	113913.918752	34.961690
1151.588365	114105.255643	34.966708
1152.595710	114298.625586	34.971725
1153.765226	114485.748059	34.976743
1155.108888	114675.161315	34.981760
1156.101295	114874.463710	34.986778
1157.228539	115043.180492	34.991796
1158.679336	115227.902299	34.996813
1159.464714	115400.347785	35.001831
1160.510152	115585.738100	35.006848
1161.867316	115769.079570	35.011866
1162.824841	115948.737864	35.016884
1164.339430	116132.449453	35.021901
1164.966890	116320.880915	35.026919
1166.029570	116503.179187	35.031936
1167.211989	116715.008084	35.036954
1168.174189	116895.716969	35.041972
1169.219928	117096.281889	35.046989
1170.494596	117302.402681	35.052007
1171.959310	117493.584138	35.057024
1173.256560	117687.870794	35.062042
1174.889471	117889.811141	35.067060
1175.985566	118075.597665	35.072077
1176.759129	118281.641347	35.077095
1178.126440	118464.785206	35.082112
1179.262214	118676.124787	35.087130
1180.417227	118862.053223	35.092148
1181.739952	119073.727236	35.097165
1182.156781	119271.831957	35.102183
1183.823928	119472.968717	35.107200
1185.253516	119685.979441	35.112218
1186.052960	119891.379570	35.117236
1187.380112	120104.511309	35.122253
1188.480295	120313.450946	35.127271
1189.906652	120504.762006	35.132288
1190.679511	120722.571465	35.137306
1192.421229	120943.078255	35.142324
1194.314189	121125.593643	35.147341
1195.403257	121329.135243	35.152359
1196.935730	121520.512813	35.157376
1198.460950	121713.602717	35.162394
1199.559927	121902.189659	35.167412
1201.013235	122105.616005	35.172429
1202.229170	122283.966171	35.177447
1203.667938	122463.548656	35.182464
1204.709261	122656.405729	35.187482
1205.898655	122845.238309	35.192500
1207.324432	123038.366334	35.197517
1208.211584	123227.794304	35.202535
1209.342064	123410.370664	35.207552
1210.367367	123597.790742	35.212570
1211.325954	123796.938887	35.217588
1212.616580	123985.168122	35.222605
1213.674674	124194.943008	35.227623
1215.046940	124379.919460	35.232640
1216.393854	124571.677776	35.237658
1217.277936	124768.970329	35.242676
1218.955777	124975.752125	35.247693
1219.975264	125159.700679	35.252711
1221.023630	125360.733458	35.257728
1222.146442	125550.152982	35.262746
1223.549168	125744.368130	35.267764
1224.470625	125924.841363	35.272781
1225.387072	126117.882445	35.277799
1226.954628	126302.004953	35.282816
1228.254153	126488.185429	35.287834
1229.095659	126677.505513	35.292852
1230.790506	126860.636162	35.297869
1231.374785	127053.635326	35.302887
1232.830895	127244.723767	35.307904
1234.108097	127436.893410	35.312922
1235.239071	127642.692963	35.317940
1236.687860	127837.498388	35.322957
1237.578508	128057.983449	35.327975
1238.814743	128240.917512	35.332992
1239.717800	128464.355529	35.338010
1240.783483	128665.498495	35.343028
1242.833319	128855.439575	35.348045
1244.518041	129066.001050	35.353063
1245.698767	129260.517060	35.358080
1247.114593	129460.761328	35.363098
1248.059055	129651.985756	35.368116
1249.055667	129871.606900	35.373133
1250.369179	130077.319492	35.378151
1251.887555	130277.477301	35.383168
1252.776674	130483.703762	35.388186
1253.594221	130708.985057	35.393204
1254.997760	130908.747538	35.398221
1256.398915	131122.080827	35.403239
1257.336842	131335.121949	35.408256
1258.974271	131539.425437	35.413274
1260.220011	131768.524047	35.418292
1261.859602	131965.266417	35.423309
1262.960738	132194.340777	35.428327
1264.406670	132404.547138	35.433344
1265.474598	132618.780898	35.438362
1266.710047	132831.291826	35.443380
1268.296311	133038.186294	35.448397
1269.172201	133260.311004	35.453415
1270.332928	133473.091991	35.458432
1271.712183	133699.397387	35.463450
1272.760042	133922.412174	35.468468
1274.230445	134137.328222	35.473485
1275.321344	134374.024153	35.478503
1276.710122	134590.337685	35.483520
1277.822256	134818.493619	35.488538
1279.128461	135049.433512	35.493556
1280.276560	135275.914730	35.498573
1281.669259	135497.556367	35.503591
1282.904738	135738.231956	35.508608
1283.735887	135970.572516	35.513626
1285.354618	136203.765459	35.518644
1286.660409	136432.980366	35.523661
1287.905340	136665.628160	35.528679
1289.116948	136907.178854	35.533696
1290.626418	137120.970257	35.538714
1291.435159	137351.335797	35.543732
1293.111996	137571.173857	35.548749
1294.198376	137789.536029	35.553767
1295.401905	138015.484691	35.558784
1296.664022	138230.932855	35.563802
1298.007042	138444.304078	35.568820
1300.272671	138646.618932	35.573837
1302.270803	138844.390109	35.578855
1303.742089	139057.910094	35.583872
1305.154866	139245.828717	35.588890
1306.338200	139444.785246	35.593908
1307.721606	139629.428613	35.598925
1309.403562	139843.098146	35.603943
1310.402139	140025.790069	35.608960
1311.548157	140227.330408	35.613978
1312.625261	140437.653128	35.618996
1313.887610	140644.335891	35.624013
1315.140208	140853.391599	35.629031
1315.966746	141058.929788	35.634048
1317.612683	141268.965099	35.639066
1318.345986	141482.873062	35.644084
1319.850956	141696.596510	35.649101
1321.270707	141923.934359	35.654119
1322.296029	142164.403735	35.659136
1323.874958	142377.334396	35.664154
1325.298492	142590.316586	35.669172
1326.903425	142809.253794	35.674189
1328.075181	143039.136220	35.679207
1328.728903	143263.158263	35.684224
1330.656955	143484.583864	35.689242
1331.676279	143715.015223	35.694260
1333.049663	143950.702843	35.699277
1334.226148	144185.320818	35.704295
1335.188620	144409.378138	35.709312
1336.540027	144648.610921	35.714330
1337.693543	144902.555063	35.719348
1339.115774	145131.437196	35.724365
1340.288405	145391.872113	35.729383
1341.824635	145638.181416	35.734400
1343.365836	145868.292241	35.739418
1344.585055	146124.682266	35.744436
1346.039873	146365.204659	35.749453
1347.290977	146604.392246	35.754471
1348.403207	146854.581259	35.759488
1350.429639	147095.183150	35.764506
1351.569100	147353.243718	35.769524
1353.874471	147571.418459	35.774541
1355.448799	147806.253746	35.779559
1357.089260	148039.090020	35.784576
1358.859378	148243.891856	35.789594
1359.723507	148478.718180	35.794612
1361.198519	148696.386050	35.799629
1362.683501	148916.373694	35.804647
1364.198633	149134.824126	35.809664
1365.491307	149349.850532	35.814682
1366.507768	149553.411346	35.819700
1367.790579	149761.672421	35.824717
1369.159338	149975.816159	35.829735
1370.353361	150171.378559	35.834752
1371.833107	150371.511353	35.839770
1372.697619	150595.348876	35.844788
1373.682852	150814.630127	35.849805
1374.997205	151026.799015	35.854823
1375.984881	151264.161423	35.859840
1377.515228	151489.648794	35.864858
1378.575193	151730.616305	35.869876
1379.719994	151971.698876	35.874893
1380.731081	152212.183221	35.879911
1381.966945	152466.960120	35.884928
1383.371323	152719.987929	35.889946
1385.384708	152954.537013	35.894964
1387.409401	153187.539163	35.899981
1389.218317	153429.325542	35.904999
1391.075127	153655.764713	35.910016
1392.117917	153878.822720	35.915034
1393.641545	154126.618546	35.920052
1395.278515	154360.578007	35.925069
1396.525392	154582.124800	35.930087
1397.448584	154829.222421	35.935104
1399.261122	155044.621686	35.940122
1400.492222	155295.109875	35.945140
1401.937873	155524.479808	35.950157
1403.286553	155769.031482	35.955175
1404.217655	156004.230263	35.960192
1405.611711	156255.282886	35.965210
1407.108024	156502.466423	35.970228
1408.484284	156748.833942	35.975245
1410.023842	157007.007761	35.980263
1411.222772	157260.419187	35.985280
1413.037071	157487.765585	35.990298
1414.303695	157730.036465	35.995316
1415.592075	157992.822474	36.000333
1417.125278	158238.389492	36.005351
1418.727912	158489.437904	36.010368
1420.472928	158726.821092	36.015386
1422.073806	158979.356946	36.020404
1423.794507	159213.868770	36.025421
1425.183885	159464.285978	36.030439
1426.580737	159706.511837	36.035456
1427.803223	159945.013455	36.040474
1429.287853	160187.951495	36.045492
1430.169453	160425.128263	36.050509
1431.932329	160673.009161	36.055527
1433.044117	160924.520687	36.060544
1434.658086	161171.781965	36.065562
1435.952942	161426.349557	36.070580
1436.924177	161683.227726	36.075597
1438.693012	161931.560276	36.080615
1440.085208	162191.659787	36.085632
1441.374581	162432.247234	36.090650
1442.809265	162674.652097	36.095668
1443.913564	162926.483198	36.100685
1445.375821	163159.489438	36.105703
1446.749636	163404.039465	36.110720
1448.660178	163649.292166	36.115738
1449.767073	163890.438246	36.120756
1451.115517	164138.687832	36.125773
1452.566670	164373.111351	36.130791
1453.949874	164648.956363	36.135808
1455.347070	164892.434575	36.140826
1456.991950	165148.672120	36.145844
1458.550499	165383.402071	36.150861
1460.024456	165638.756986	36.155879
1461.600280	165890.279829	36.160896
1463.167953	166131.177083	36.165914
1464.641264	166391.953019	36.170932
1466.262346	166635.939780	36.175949
1468.301614	166878.162097	36.180967
1469.374993	167136.799815	36.185984
1470.972957	167381.086807	36.191002
1472.127822	167641.922002	36.196020
1473.405130	167895.116535	36.201037
1475.387817	168140.539588	36.206055
1476.569618	168406.030759	36.211072
1477.907752	168658.561138	36.216090
1479.225490	168922.118996	36.221108
1480.679547	169180.037868	36.226125
1482.460652	169451.821274	36.231143
1483.484010	169717.422800	36.236160
1485.309528	169971.114765	36.241178
1487.313362	170243.883125	36.246196
1488.578655	170495.637982	36.251213
1490.120842	170762.014113	36.256231
1491.438477	171025.319936	36.261248
1493.455692	171283.569252	36.266266
1494.688643	171560.794865	36.271284
1495.920048	171821.722255	36.276301
1497.689784	172089.314396	36.281319
1498.747105	172372.091689	36.286336
1500.098941	172626.028326	36.291354
1501.962223	172891.936553	36.296372
1502.871387	173178.434594	36.301389
1504.874723	173442.459462	36.306407
1506.143772	173719.922758	36.311424
1507.804850	173996.247396	36.316442
1509.678889	174275.901871	36.321460
1511.147630	174536.416043	36.326477
1512.747059	174799.879676	36.331495
1514.105162	175079.405997	36.336512
1515.584232	175358.572491	36.341530
1517.347970	175620.150450	36.346548
1518.603145	175910.761307	36.351565
1520.127289	176173.979351	36.356583
1521.323396	176453.972128	36.361600
1522.804594	176725.078894	36.366618
1524.437963	177000.197656	36.371636
1525.966869	177255.073931	36.376653
1527.793900	177503.116906	36.381671
1529.196023	177769.726501	36.386688
1530.425192	178019.681754	36.391706
1532.386389	178268.621426	36.396724
1533.861367	178539.411101	36.401741
1535.840818	178780.066134	36.406759
1537.384390	179035.965886	36.411776
1538.880217	179295.173508	36.416794
1540.354749	179541.876178	36.421812
1541.612625	179812.606969	36.426829
1543.877578	180052.081972	36.431847
1545.303050	180311.611446	36.436864
1546.897766	180558.034442	36.441882
1548.569652	180815.129811	36.446900
1549.597595	181075.957759	36.451917
1550.876452	181339.944814	36.456935
1552.463833	181603.821025	36.461952
1553.993758	181873.265402	36.466970
1555.513168	182149.336402	36.471988
1556.875669	182420.485596	36.477005
1558.486682	182695.974507	36.482023
1559.802925	182967.565824	36.487040
1561.556499	183257.373642	36.492058
1563.100157	183533.576342	36.497076
1564.951995	183805.887108	36.502093
1566.552884	184078.214018	36.507111
1568.002271	184364.169183	36.512128
1569.885072	184642.583500	36.517146
1571.454906	184916.633444	36.522164
1572.430053	185204.255400	36.527181
1574.439417	185480.218456	36.532199
1575.875442	185778.480572	36.537216
1577.331340	186056.616078	36.542234
1578.858042	186343.891146	36.547252
1580.447916	186633.200998	36.552269
1582.272332	186921.955140	36.557287
1583.706372	187222.752190	36.562304
1585.489050	187515.691584	36.567322
1587.179015	187815.322430	36.572340
1588.376763	188108.853358	36.577357
1590.136532	188397.398505	36.582375
1591.807385	188685.629601	36.587392
1593.562399	188975.854144	36.592410
1595.308803	189268.581820	36.597428
1596.923035	189547.474424	36.602445
1598.691871	189820.608032	36.607463
1600.306563	190118.171519	36.612480
1602.053395	190394.218021	36.617498
1604.153173	190671.529881	36.622516
1605.376926	190960.175682	36.627533
1607.016119	191235.698390	36.632551
1608.513781	191518.390097	36.637568
1609.951327	191795.077482	36.642586
1611.794452	192056.180910	36.647604
1613.284362	192335.147410	36.652621
1615.070756	192579.561166	36.657639
1616.545351	192849.420764	36.662656
1618.403570	193110.222789	36.667674
1619.794379	193358.916719	36.672692
1620.989786	193638.470360	36.677709
1622.619527	193891.913662	36.682727
1624.218829	194159.133405	36.687744
1625.843757	194436.123040	36.692762
1627.378880	194715.349500	36.697780
1629.075805	194989.792394	36.702797
1630.760845	195256.750480	36.707815
1632.352857	195546.392451	36.712832
1633.877867	195821.146335	36.717850
1635.617740	196089.813468	36.722868
1636.897990	196388.647952	36.727885
1638.331173	196661.897841	36.732903
1640.071836	196958.111362	36.737920
1641.696787	197249.103015	36.742938
1643.492163	197542.201542	36.747956
1644.977546	197839.856750	36.752973
1646.667175	198135.704248	36.757991
1648.099673	198433.840820	36.763008
1649.745257	198723.009588	36.768026
1651.898006	199035.923649	36.773044
1653.425436	199341.653162	36.778061
1654.991276	199629.075181	36.783079
1656.900106	199933.681284	36.788096
1658.726317	200233.973897	36.793114
1660.815412	200510.299957	36.798132
1662.423970	200819.718603	36.803149
1664.312117	201096.676109	36.808167
1665.724421	201404.567942	36.813184
1667.448804	201699.287001	36.818202
1669.497469	201972.326542	36.823220
1671.177821	202265.951266	36.828237
1673.114599	202560.996570	36.833255
1674.512259	202853.869564	36.838272
1676.009093	203144.126124	36.843290
1677.570496	203444.960503	36.848308
1679.252210	203746.665935	36.853325
1681.030185	204042.086896	36.858343
1683.181374	204318.980429	36.863360
1684.964693	204598.294790	36.868378
1686.781957	204879.788489	36.873396
1688.429552	205188.539400	36.878413
1689.908936	205470.622758	36.883431
1692.372234	205727.746681	36.888448
1694.053367	206016.947495	36.893466
1696.004614	206297.487358	36.898484
1697.723615	206581.099394	36.903501
1699.522982	206845.150507	36.908519
1700.960741	207126.347059	36.913536
1702.374602	207393.940106	36.918554
1704.255353	207643.814636	36.923572
1705.307253	207909.779050	36.928589
1706.814734	208178.274721	36.933607
1708.452894	208433.218146	36.938624
1710.021242	208714.845651	36.943642
1711.684325	208973.837034	36.948660
1712.671174	209251.243040	36.953677
1714.768395	209516.058241	36.958695
1716.733788	209806.209528	36.963712
1717.536915	210096.000802	36.968730
1719.356578	210387.079274	36.973748
1720.807957	210678.547638	36.978765
1722.761799	210970.775461	36.983783
1724.198959	211278.867035	36.988800
1725.759200	211581.202205	36.993818
1727.682585	211888.546653	36.998836
1729.102348	212206.890720	37.003853
1730.916094	212516.553458	37.008871
1732.754436	212824.512537	37.013888
1733.792970	213153.509961	37.018906
1735.768801	213465.093898	37.023924
1737.552865	213797.454822	37.028941
1739.168110	214133.881518	37.033959
1741.492932	214445.909783	37.038976
1743.156044	214779.069239	37.043994
1744.917451	215091.088366	37.049012
1746.717516	215436.811175	37.054029
1748.739382	215758.745824	37.059047
1750.548676	216086.213230	37.064064
1751.975713	216417.031232	37.069082
1753.876583	216751.038567	37.074100
1755.422510	217060.091754	37.079117
1757.242552	217410.074549	37.084135
1759.355471	217738.923503	37.089152
1761.355211	218071.651733	37.094170
1763.758679	218382.974218	37.099188
1765.698316	218703.411793	37.104205
1767.415679	219024.089221	37.109223
1769.174346	219345.802650	37.114240
1770.758963	219677.575713	37.119258
1772.552681	219975.555737	37.124276
1774.441799	220301.696584	37.129293
1776.080417	220637.160215	37.134311
1778.178632	220946.408916	37.139328
1779.721425	221258.210315	37.144346
1781.400348	221640.562856	37.149364
1783.046142	221977.148647	37.154381
1784.693209	222299.374957	37.159399
1786.398010	222623.307599	37.164416
1788.154122	222954.318649	37.169434
1790.322632	223274.586994	37.174452
1792.253901	223605.877727	37.179469
1793.768228	223941.146906	37.184487
1795.865998	224260.897163	37.189504
1797.816704	224572.228030	37.194522
1799.953629	224878.273645	37.199540
1801.669362	225164.159595	37.204557
1803.605851	225452.906624	37.209575
1805.796036	225737.017743	37.214592
1807.169897	226037.855678	37.219610
1809.241687	226311.905363	37.224628
1811.750744	226592.514930	37.229645
1812.992101	226882.850237	37.234663
1815.068611	227159.873293	37.239680
1816.853256	227451.419519	37.244698
1818.562847	227728.274092	37.249716
1820.165070	228028.790791	37.254733
1821.870896	228318.904857	37.259751
1823.780428	228607.209783	37.264768
1824.897018	228915.298648	37.269786
1826.526828	229215.307101	37.274804
1828.563095	229516.242534	37.279821
1829.906966	229836.743035	37.284839
1832.062768	230152.468122	37.289856
1833.883481	230470.203080	37.294874
1835.600252	230781.453920	37.299892
1837.571923	231109.402258	37.304909
1839.557626	231422.999930	37.309927
1841.538733	231736.751769	37.314944
1842.906332	232067.059727	37.319962
1844.914268	232385.152464	37.324980
1846.954330	232703.266559	37.329997
1848.817254	233034.108789	37.335015
1850.665573	233360.306625	37.340032
1852.681265	233678.072209	37.345050
1854.563736	234002.514287	37.350068
1856.569587	234320.943850	37.355085
1858.340998	234655.945963	37.360103
1860.454478	234973.573161	37.365120
1862.447793	235294.928605	37.370138
1864.162218	235617.853233	37.375156
1866.626353	235929.560664	37.380173
1868.064479	236260.760311	37.385191
1870.081099	236574.445592	37.390208
1871.935027	236893.897773	37.395226
1873.964965	237213.703959	37.400244
1875.748071	237533.880455	37.405261
1877.748308	237863.852897	37.410279
1879.569854	238176.405437	37.415296
1881.344765	238501.640498	37.420314
1883.042685	238833.771949	37.425332
1884.815686	239156.367679	37.430349
1886.706963	239486.336807	37.435367
1888.382581	239829.294890	37.440384
1890.236280	240154.522173	37.445402
1892.120032	240481.675970	37.450420
1894.107649	240826.822638	37.455437
1895.509458	241166.780099	37.460455
1897.558530	241497.517227	37.465472
1899.413383	241824.958675	37.470490
1901.312616	242140.735325	37.475508
1903.934897	242450.454409	37.480525
1905.724899	242762.744752	37.485543
1908.017178	243070.307916	37.490560
1909.812010	243370.381469	37.495578
1911.716518	243664.062825	37.500596
1913.527498	243971.577517	37.505613
1915.381554	244289.373290	37.510631
1917.248944	244583.265795	37.515648
1919.088638	244899.820676	37.520666
1921.152511	245209.990558	37.525684
1923.121590	245517.813920	37.530701
1924.946207	245829.267801	37.535719
1927.386831	246153.502849	37.540736
1928.904810	246470.340983	37.545754
1930.617801	246771.324088	37.550772
1932.708606	247083.424308	37.555789
1934.511479	247414.316859	37.560807
1937.147854	247715.612611	37.565824
1939.119200	248032.255190	37.570842
1941.233650	248339.959901	37.575860
1943.466066	248654.352448	37.580877
1945.205620	248967.833187	37.585895
1947.228734	249282.387220	37.590912
1948.963617	249595.539732	37.595930
1950.776593	249920.238129	37.600948
1952.541422	250234.911217	37.605965
1954.194573	250567.155106	37.610983
1956.469800	250886.955769	37.616000
1958.328310	251210.252381	37.621018
1960.148167	251545.342129	37.626036
1962.401611	251874.597529	37.631053
1964.266088	252213.339329	37.636071
1966.327321	252544.912633	37.641088
1968.320971	252865.320432	37.646106
1970.186105	253191.972654	37.651124
1972.240019	253526.673327	37.656141
1974.240774	253860.189129	37.661159
1976.317829	254184.904286	37.666176
1978.421634	254511.597103	37.671194
1980.169910	254843.859133	37.676212
1982.510055	255181.540081	37.681229
1984.337523	255501.292738	37.686247
1986.134028	255834.285382	37.691264
1988.291122	256163.538002	37.696282
1990.555853	256501.461653	37.701300
1992.888090	256828.325072	37.706317
1994.308786	257172.099190	37.711335
1996.358858	257500.761115	37.716352
1998.619175	257832.489254	37.721370
2000.172133	258175.786625	37.726388
2002.293747	258502.355580	37.731405
2004.183463	258846.895997	37.736423
2006.183942	259184.763821	37.741440
2008.101277	259518.149005	37.746458
2010.110357	259835.592563	37.751476
2012.350141	260143.245247	37.756493
2014.207602	260460.713591	37.761511
2015.871512	260772.980026	37.766528
2017.582711	261090.446877	37.771546
2019.356358	261420.122933	37.776564
2021.280327	261748.149720	37.781581
2023.158982	262086.802457	37.786599
2025.135833	262423.483956	37.791616
2027.269180	262763.544974	37.796634
2028.859695	263098.611858	37.801652
2031.016285	263441.032349	37.806669
2033.138204	263789.199758	37.811687
2035.141149	264132.813826	37.816704
2037.502653	264488.463191	37.821722
2039.216493	264844.876107	37.826740
2041.294059	265198.005444	37.831757
2043.320503	265564.937096	37.836775
2045.397047	265910.979715	37.841792
2047.482756	266271.297735	37.846810
2049.846106	266632.638926	37.851828
2052.086201	266997.149937	37.856845
2054.184138	267358.482953	37.861863
2056.197031	267710.049454	37.866880
2058.443491	268071.969062	37.871898
2060.152589	268439.156403	37.876916
2062.290884	268803.278291	37.881933
2064.743434	269165.470689	37.886951
2066.700409	269521.441861	37.891968
2068.730818	269883.650776	37.896986
2070.769044	270252.184050	37.902004
2072.592426	270615.797907	37.907021
2074.762720	270988.629109	37.912039
2077.074403	271358.465827	37.917056
2079.574075	271724.690974	37.922074
2081.335151	272101.067722	37.927092
2083.252681	272465.988227	37.932109
2085.534112	272843.171746	37.937127
2087.626306	273222.849487	37.942144
2090.302189	273586.100319	37.947162
2091.873806	273956.105833	37.952180
2094.129278	274321.633528	37.957197
2096.098226	274705.192310	37.962215
2097.902332	275081.740503	37.967232
2100.526770	275437.048345	37.972250
2102.419816	275822.041752	37.977268
2104.710701	276197.953820	37.982285
2107.012476	276565.557207	37.987303
2108.965516	276932.301332	37.992320
2111.298095	277317.097821	37.997338
2113.286944	277687.189373	38.002356
2115.343471	278054.780569	38.007373
2117.723786	278434.310708	38.012391
2119.849731	278806.209253	38.017408
2122.085726	279153.296535	38.022426
2123.978275	279512.072901	38.027444
2125.781485	279859.380985	38.032461
2128.188963	280198.692655	38.037479
2130.089733	280553.910810	38.042496
2132.420017	280900.931617	38.047514
2134.321930	281246.394378	38.052532
2136.107220	281599.217001	38.057549
2138.149470	281952.786173	38.062567
2139.943410	282312.592905	38.067584
2141.827817	282671.013285	38.072602
2143.909186	283047.971937	38.077620
2146.203961	283424.820257	38.082637
2148.457238	283792.097870	38.087655
2150.231461	284171.390647	38.092672
2152.883291	284556.920111	38.097690
2154.593136	284945.088119	38.102708
2157.047735	285319.521601	38.107725
2159.091756	285702.834703	38.112743
2161.325103	286094.424189	38.117760
2163.521747	286479.795343	38.122778
2165.739018	286874.612717	38.127796
2167.908552	287263.670740	38.132813
2170.490987	287653.018473	38.137831
2172.569673	288033.554612	38.142848
2175.250801	288428.575994	38.147866
2177.506826	288813.147508	38.152884
2180.034468	289192.036032	38.157901
2182.217505	289567.904972	38.162919
2184.247537	289965.567801	38.167936
2186.661034	290338.782670	38.172954
2188.837147	290724.075513	38.177972
2191.028609	291110.559275	38.182989
2193.199097	291491.990663	38.188007
2195.160643	291874.267478	38.193024
2197.517815	292269.995078	38.198042
2199.783544	292656.134394	38.203060
2202.225871	293032.414334	38.208077
2204.947575	293415.101549	38.213095
2207.314275	293803.559918	38.218112
2209.478556	294179.831198	38.223130
2211.261239	294561.471386	38.228148
2213.273040	294938.730775	38.233165
2215.775846	295320.102966	38.238183
2218.012586	295703.777408	38.243200
2220.021726	296084.616764	38.248218
2222.015306	296480.953045	38.253236
2224.281048	296869.650172	38.258253
2226.787481	297251.500626	38.263271
2228.758270	297646.263134	38.268288
2231.693456	298026.646882	38.273306
2233.605864	298418.038511	38.278324
2235.954040	298793.509538	38.283341
2238.273268	299169.746383	38.288359
2240.864717	299550.206688	38.293376
2243.430654	299920.611183	38.298394
2245.366382	300276.331131	38.303412
2247.532492	300621.472201	38.308429
2250.169022	300955.818585	38.313447
2251.895823	301297.319242	38.318464
2254.234375	301642.862555	38.323482
2256.411118	301992.774340	38.328500
2258.379857	302347.595303	38.333517
2260.589227	302703.240907	38.338535
2262.532093	303067.335625	38.343552
2264.414829	303416.223827	38.348570
2266.075210	303796.110054	38.353588
2268.654221	304175.036800	38.358605
2271.124105	304547.324839	38.363623
2272.741020	304937.527543	38.368640
2274.701233	305334.456653	38.373658
2277.202514	305727.564944	38.378676
2279.160111	306114.179562	38.383693
2281.373935	306526.228945	38.388711
2283.720311	306933.988764	38.393728
2286.109233	307341.181735	38.398746
2288.505717	307760.767432	38.403764
2290.668356	308165.529794	38.408781
2293.067178	308583.588334	38.413799
2295.057777	308999.449569	38.418816
2297.707807	309426.279108	38.423834
2300.239122	309844.693251	38.428852
2302.685663	310247.066826	38.433869
2304.930059	310672.914749	38.438887
2307.670990	311084.382534	38.443904
2310.078713	311501.362488	38.448922
2312.652021	311914.123776	38.453940
2315.076445	312319.719185	38.458957
2317.683456	312737.907443	38.463975
2320.046040	313149.097340	38.468992
2322.619762	313556.543965	38.474010
2324.831567	313961.608119	38.479028
2327.213936	314364.941964	38.484045
2329.795236	314777.411564	38.489063
2331.870027	315183.076831	38.494080
2334.292378	315585.510600	38.499098
2336.785764	316000.579796	38.504116
2339.075149	316409.939633	38.509133
2341.564694	316800.928705	38.514151
2343.705816	317220.340863	38.519168
2346.142915	317627.081601	38.524186
2348.303637	318040.086844	38.529204
2350.803933	318462.027193	38.534221
2352.917873	318872.166289	38.539239
2355.113180	319294.938542	38.544256
2357.478012	319698.202336	38.549274
2359.646250	320129.559285	38.554292
2361.494456	320555.631542	38.559309
2364.122794	320966.187638	38.564327
2366.342084	321409.289072	38.569344
2368.747146	321827.698742	38.574362
2371.441856	322225.590939	38.579380
2373.703625	322623.321357	38.584397
2375.845885	323014.338868	38.589415
2377.801700	323417.396496	38.594432
2380.100341	323815.801186	38.599450
2382.624907	324230.777074	38.604468
2384.522666	324639.933018	38.609485
2387.351546	325048.609210	38.614503
2389.842306	325456.168750	38.619520
2391.885427	325874.463235	38.624538
2394.818985	326288.246436	38.629556
2396.805338	326699.993627	38.634573
2399.724855	327114.561988	38.639591
2402.198880	327527.192567	38.644608
2404.347505	327945.662514	38.649626
2407.076888	328359.848049	38.654644
2409.421715	328793.087307	38.659661
2412.157567	329205.159484	38.664679
2414.235723	329631.706715	38.669696
2416.463485	330056.501010	38.674714
2419.092868	330477.293177	38.679732
2421.308559	330912.368964	38.684749
2424.349064	331346.828968	38.689767
2426.560923	331775.958107	38.694784
2429.205002	332204.254391	38.699802
2431.655146	332625.164058	38.704820
2433.588774	333073.882150	38.709837
2436.667124	333494.687075	38.714855
2439.047660	333930.454721	38.719872
2441.540241	334362.545356	38.724890
2443.921604	334802.217801	38.729908
2446.415642	335234.759763	38.734925
2448.829332	335664.442403	38.739943
2450.721664	336116.016467	38.744960
2453.990074	336554.622825	38.749978
2456.043820	336990.447958	38.754996
2458.713349	337441.305833	38.760013
2461.584580	337884.892169	38.765031
2464.057667	338314.014945	38.770048
2466.125430	338755.183533	38.775066
2468.843567	339199.775314	38.780084
2471.053587	339652.366307	38.785101
2473.741027	340101.653845	38.790119
2475.884384	340548.231468	38.795136
2478.641578	340985.365152	38.800154
2481.145033	341439.191582	38.805172
2483.383985	341887.775554	38.810189
2486.109017	342339.427480	38.815207
2488.464332	342794.841430	38.820224
2490.977203	343248.500522	38.825242
2493.702884	343703.188777	38.830260
2496.086955	344147.848428	38.835277
2499.223104	344581.214691	38.840295
2501.366626	345030.120249	38.845312
2504.043134	345456.875759	38.850330
2506.547728	345865.274605	38.855348
2508.807899	346277.415870	38.860365
2511.357987	346692.250073	38.865383
2513.740373	347104.264451	38.870400
2516.153519	347514.874665	38.875418
2518.634094	347931.208629	38.880436
2520.933041	348350.132323	38.885453
2523.314280	348768.557480	38.890471
2525.664534	349203.282372	38.895488
2527.590836	349636.623986	38.900506
2530.823286	350065.084225	38.905524
2532.814159	350517.321080	38.910541
2535.288427	350959.399535	38.915559
2537.545460	351399.681028	38.920576
2540.314477	351847.340977	38.925594
2543.242070	352297.459739	38.930612
2545.871740	352747.038011	38.935629
2548.676055	353193.538634	38.940647
2551.161483	353654.935688	38.945664
2553.493015	354105.057164	38.950682
2556.172289	354551.921269	38.955700
2558.451086	355018.136376	38.960717
2560.779423	355485.227781	38.965735
2563.391345	355960.392521	38.970752
2565.673959	356437.965541	38.975770
2568.377403	356908.817115	38.980788
2570.748692	357397.662131	38.985805
2573.381521	357875.343552	38.990823
2576.069431	358369.992024	38.995840
2578.624414	358856.052210	39.000858
2581.444204	359343.588462	39.005876
2584.118723	359838.731732	39.010893
2586.574470	360311.721771	39.015911
2589.588463	360803.197226	39.020928
2592.090510	361295.890802	39.025946
2595.026673	361780.058939	39.030964
2597.679640	362261.272136	39.035981
2600.611076	362740.888117	39.040999
2603.410590	363223.540164	39.046016
2605.870281	363716.240291	39.051034
2608.741158	364189.429953	39.056052
2611.455120	364677.790467	39.061069
2614.017699	365153.480652	39.066087
2617.132845	365621.312682	39.071104
2619.693670	366100.469916	39.076122
2622.672228	366569.709450	39.081140
2624.974153	367042.959275	39.086157
2627.576279	367515.623577	39.091175
2630.171900	367980.036472	39.096192
2632.748156	368459.444865	39.101210
2635.822058	368931.511640	39.106228
2638.413705	369405.349829	39.111245
2640.633744	369871.375299	39.116263
2643.493900	370340.085588	39.121280
2645.557065	370808.028846	39.126298
2648.390160	371255.799097	39.131316
2650.567373	371706.053675	39.136333
2653.311731	372148.525281	39.141351
2655.574704	372606.394212	39.146368
2657.811412	373064.592134	39.151386
2660.634639	373513.938353	39.156404
2663.003749	373980.630571	39.161421
2665.506897	374452.015575	39.166439
2668.284185	374915.384821	39.171456
2670.411831	375413.053197	39.176474
2673.023608	375888.895223	39.181492
2675.784192	376371.558358	39.186509
2678.274733	376854.918108	39.191527
2681.188411	377364.996572	39.196544
2683.406122	377862.747181	39.201562
2685.833897	378377.430897	39.206580
2688.635105	378873.046749	39.211597
2691.070528	379403.292885	39.216615
2694.112038	379923.516493	39.221632
2696.325337	380455.939833	39.226650
2699.305089	380973.901276	39.231668
2702.238284	381496.606944	39.236685
2705.134377	382022.279367	39.241703
2708.039293	382560.423889	39.246720
2710.288448	383090.394947	39.251738
2713.383594	383612.944337	39.256756
2716.080956	384169.565674	39.261773
2718.499692	384702.099810	39.266791
2721.557751	385242.236200	39.271808
2724.754816	385774.022884	39.276826
2727.513490	386302.802141	39.281844
2730.427285	386857.192669	39.286861
2733.157764	387379.289927	39.291879
2736.100812	387924.097257	39.296896
2738.293934	388473.859494	39.301914
2741.829572	388994.994217	39.306932
2744.718784	389540.064511	39.311949
2747.400463	390074.431098	39.316967
2750.454172	390605.306855	39.321984
2753.298529	391147.696474	39.327002
2756.057542	391674.443453	39.332020
2758.766977	392218.004428	39.337037
2761.933892	392750.478108	39.342055
2764.282144	393281.957369	39.347072
2767.102557	393820.302148	39.352090
2770.001764	394346.123966	39.357108
2772.760389	394884.715340	39.362125
2775.416562	395414.717931	39.367143
2778.295326	395956.113360	39.372160
2780.950394	396496.140827	39.377178
2783.667008	397026.539515	39.382196
2786.735192	397572.037369	39.387213
2789.520098	398092.747355	39.392231
2792.240126	398630.828147	39.397248
2795.051154	399154.864184	39.402266
2797.563145	399663.497973	39.407284
2800.485979	400161.536611	39.412301
2802.818138	400665.796854	39.417319
2806.025326	401150.920666	39.422336
2808.488917	401657.223632	39.427354
2811.190559	402169.160008	39.432372
2813.728717	402679.491496	39.437389
2816.094837	403197.397008	39.442407
2819.070587	403708.910293	39.447424
2821.359383	404251.782328	39.452442
2824.096018	404779.617025	39.457460
2827.019289	405318.795668	39.462477
2829.516427	405867.285230	39.467495
2832.391396	406416.389730	39.472512
2835.258133	406979.326431	39.477530
2838.014164	407536.059931	39.482548
2840.776728	408096.812657	39.487565
2843.748703	408659.575101	39.492583
2846.681261	409224.361151	39.497600
2849.570706	409792.996203	39.502618
2852.012149	410371.297712	39.507636
2855.447991	410934.831448	39.512653
2858.186722	411508.425642	39.517671
2861.576672	412084.566905	39.522688
2864.187269	412669.640180	39.527706
2867.340970	413248.279910	39.532724
2870.443462	413819.161270	39.537741
2873.145068	414393.592265	39.542759
2876.388291	414970.815234	39.547776
2879.196753	415557.015878	39.552794
2882.036350	416131.339937	39.557812
2884.940171	416707.137477	39.562829
2887.848907	417297.594730	39.567847
2891.074483	417872.608338	39.572864
2893.892287	418453.350859	39.577882
2896.859349	419031.194554	39.582900
2899.898937	419625.611486	39.587917
2902.542757	420201.860643	39.592935
2906.051351	420787.437162	39.597952
2908.749522	421368.923747	39.602970
2911.644626	421955.763566	39.607988
2914.906586	422526.900780	39.613005
2917.587746	423123.149116	39.618023
2920.617537	423701.139110	39.623040
2923.574393	424285.385900	39.628058
2926.878852	424866.803770	39.633076
2929.742376	425448.709598	39.638093
2932.596533	426030.452357	39.643111
2935.444847	426610.460879	39.648128
2938.530960	427196.853332	39.653146
2941.395147	427771.261255	39.658164
2944.995942	428356.533457	39.663181
2947.453140	428943.518798	39.668199
2950.486709	429519.432380	39.673216
2953.746684	430073.768287	39.678234
2956.690744	430613.857468	39.683252
2959.623911	431160.496985	39.688269
2962.030310	431695.988539	39.693287
2965.174295	432214.586213	39.698304
2967.784535	432745.794237	39.703322
2970.554967	433296.010593	39.708340
2973.844825	433837.319899	39.713357
2976.650400	434387.329932	39.718375
2979.560034	434934.500672	39.723392
2982.131534	435480.219041	39.728410
2985.101249	436039.714070	39.733428
2988.510529	436596.291033	39.738445
2990.784965	437176.609512	39.743463
2993.832148	437735.421414	39.748480
2996.808828	438314.361577	39.753498
2999.168743	438901.918570	39.758516
3002.536850	439474.920814	39.763533
3005.437705	440080.998994	39.768551
3008.314054	440667.064968	39.773568
3011.207948	441267.544963	39.778586
3014.412092	441869.277532	39.783604
3016.967579	442474.996490	39.788621
3019.758781	443094.232015	39.793639
3023.004440	443710.797619	39.798656
3025.952046	444342.431090	39.803674
3028.719436	444970.380645	39.808692
3031.836731	445587.373822	39.813709
3034.990162	446246.008851	39.818727
3038.314136	446880.451554	39.823744
3041.224543	447521.827100	39.828762
3044.488545	448157.409124	39.833780
3047.662562	448787.875635	39.838797
3050.705604	449443.856844	39.843815
3054.263521	450072.506794	39.848832
3057.327761	450703.546018	39.853850
3060.547191	451343.754961	39.858868
3063.730842	451979.143609	39.863885
3066.984185	452613.541982	39.868903
3070.565996	453252.020638	39.873920
3073.278931	453884.748353	39.878938
3076.626207	454510.020156	39.883956
3079.922381	455141.102213	39.888973
3082.963258	455770.132199	39.893991
3086.244012	456404.065515	39.899008
3089.315963	457050.461486	39.904026
3092.125204	457675.780550	39.909044
3095.075255	458315.732892	39.914061
3097.766849	458962.133228	39.919079
3101.002353	459608.580295	39.924096
3103.894286	460254.455524	39.929114
3106.477864	460904.913641	39.934132
3109.666143	461554.649569	39.939149
3112.468708	462224.814097	39.944167
3115.345830	462894.187235	39.949184
3118.353073	463549.102214	39.954202
3121.273883	464196.575076	39.959220
3124.607091	464808.656783	39.964237
3127.848469	465444.154257	39.969255
3130.938739	466080.162392	39.974272
3133.995246	466718.331577	39.979290
3136.619635	467345.119608	39.984308
3140.027646	467974.850028	39.989325
3142.699895	468640.786998	39.994343
3145.854588	469291.859570	39.999360
3148.727922	469931.679198	40.004378
3151.441930	470605.182690	40.009396
3155.288528	471267.562700	40.014413
3158.767698	471924.417362	40.019431
3161.714113	472600.094224	40.024448
3164.972377	473256.233208	40.029466
3167.962453	473928.977142	40.034484
3171.917935	474597.855323	40.039501
3174.938657	475281.116189	40.044519
3177.825075	475957.600787	40.049536
3181.350963	476635.983587	40.054554
3184.108239	477321.289408	40.059572
3187.910169	477990.533853	40.064589
3191.071448	478683.816841	40.069607
3194.158023	479363.793733	40.074624
3197.195887	480045.877780	40.079642
3200.449202	480744.987543	40.084660
3203.751314	481441.487077	40.089677
3206.509662	482143.607085	40.094695
3209.836258	482851.777452	40.099712
3213.189633	483557.946860	40.104730
3216.085401	484279.019706	40.109748
3219.419338	484975.842154	40.114765
3222.756514	485702.552442	40.119783
3226.039064	486410.093714	40.124800
3229.646782	487124.782527	40.129818
3232.620677	487856.015544	40.134836
3236.273977	488564.327408	40.139853
3239.373783	489280.227735	40.144871
3242.769522	489999.085112	40.149888
3245.851093	490720.187323	40.154906
3248.974715	491450.802268	40.159924
3252.457857	492171.885865	40.164941
3255.673568	492897.479154	40.169959
3258.981449	493631.666335	40.174976
3262.279723	494366.684388	40.179994
3265.150177	495110.932467	40.185012
3268.500358	495823.661957	40.190029
3271.820089	496577.627199	40.195047
3275.192360	497293.729659	40.200064
3278.670274	498032.712411	40.205082
3281.916059	498759.835479	40.210100
3285.206310	499504.190441	40.215117
3288.230174	500257.038945	40.220135
3291.830220	500976.089185	40.225152
3295.177192	501708.680628	40.230170
3298.111185	502416.519573	40.235188
3301.637730	503097.329664	40.240205
3304.663268	503787.127644	40.245223
3307.345511	504482.707333	40.250240
3310.775450	505182.936415	40.255258
3313.891067	505882.884289	40.260276
3317.101656	506594.801325	40.265293
3320.167478	507305.500787	40.270311
3323.365585	508031.542796	40.275328
3326.942663	508756.081299	40.280346
3329.790534	509500.385286	40.285364
3333.061007	510218.703554	40.290381
3336.302131	510959.551472	40.295399
3339.543715	511701.729430	40.300416
3343.154529	512443.362477	40.305434
3346.212611	513196.452651	40.310452
3349.553227	513956.123952	40.315469
3352.941786	514727.810374	40.320487
3356.021908	515490.782955	40.325504
3359.946175	516250.207535	40.330522
3362.880846	517031.998334	40.335540
3366.162967	517819.195163	40.340557
3369.501818	518597.216629	40.345575
3372.619262	519388.197820	40.350592
3375.988510	520191.406328	40.355610
3379.241197	521002.309445	40.360628
3382.842802	521799.451609	40.365645
3385.966114	522612.362499	40.370663
3389.388454	523416.462486	40.375680
3393.350914	524226.285619	40.380698
3397.105426	525035.294221	40.385716
3400.942702	525840.215856	40.390733
3404.495063	526642.923920	40.395751
3407.846574	527452.932531	40.400768
3411.385632	528252.133732	40.405786
3414.756129	529071.532976	40.410804
3418.097846	529875.370798	40.415821
3421.427635	530705.628437	40.420839
3424.790141	531524.951518	40.425856
3428.445418	532319.845614	40.430874
3431.839715	533146.838972	40.435892
3435.270654	533960.429780	40.440909
3439.195340	534775.814382	40.445927
3442.435067	535597.964962	40.450944
3445.917904	536409.755718	40.455962
3449.835661	537222.593379	40.460980
3453.564504	538028.365239	40.465997
3457.276404	538836.313466	40.471015
3460.612424	539653.445202	40.476032
3464.404458	540458.977246	40.481050
3467.641371	541265.611615	40.486068
3470.827012	542062.642258	40.491085
3474.800467	542872.800512	40.496103
3477.808030	543677.326967	40.501120
3481.476222	544463.148605	40.506125
3484.654474	545218.283663	40.511130
3487.973661	545904.003344	40.516135
3490.936083	546547.147286	40.521140
3493.780699	547135.014686	40.526144
3496.864340	547641.866230	40.531149
3498.797695	548101.592684	40.536154
3501.539311	548517.270264	40.541159
3504.001862	548865.910509	40.546164
3505.947526	549174.857531	40.551168
3507.965824	549417.476414	40.556173
3509.755577	549610.773899	40.561178
3511.550253	549761.830370	40.566183
3513.366113	549863.731160	40.571188
3514.705413	549921.097607	40.576192
3515.993503	549947.185149	40.581197
3516.783753	549946.707097	40.586202
3517.742687	549898.616086	40.591207
3518.937254	549825.558975	40.596212
3519.639088	549730.526906	40.601216
3520.055778	549597.792409	40.606221
3520.886205	549463.982035	40.611226
3521.088420	549306.753135	40.616231
3521.822119	549125.467488	40.621236
3521.825679	548937.179263	40.626240
3522.392839	548719.226009	40.631245
3522.696714	548491.217595	40.636250
3522.681379	548261.287808	40.641255
3522.919084	548022.431839	40.646260
3522.796896	547779.036078	40.651264
3523.159269	547508.608211	40.656269
3523.108615	547252.423245	40.661274
3523.110779	546983.001597	40.666279
3523.067242	546700.206695	40.671284
3522.395560	546428.711022	40.676288
3522.732454	546148.772951	40.681293
3522.349122	545869.296730	40.686298
3522.252274	545602.389336	40.691303
3522.286720	545325.209251	40.696308
3521.901748	545042.840400	40.701312
3521.813215	544777.582647	40.706317
3521.550988	544486.501184	40.711322
3521.489285	544207.498080	40.716327
3521.454264	543933.331913	40.721332
3521.011210	543659.528087	40.726336
3521.080693	543375.793639	40.731341
3520.845744	543105.430221	40.736346
3520.571176	542830.524345	40.741351
3520.410663	542559.432467	40.746356
3520.122550	542301.886828	40.751360
3519.914607	542037.457505	40.756365
3519.834339	541780.576916	40.761370
3519.086050	541517.587068	40.766375
3519.004957	541258.476059	40.771380
3518.956684	541010.413387	40.776384
3518.844551	540755.287573	40.781389
3518.777851	540509.188823	40.786394
3517.880024	540277.810618	40.791399
3518.143611	540028.218133	40.796404
3517.695957	539794.337553	40.801408
3517.596459	539556.156509	40.806413
3517.203754	539332.713177	40.811418
3517.120644	539099.774229	40.816423
3516.907305	538877.406828	40.821428
3516.570289	538661.065325	40.826432
3516.634250	538427.486810	40.831437
3516.444634	538231.215551	40.836442
3516.118657	538014.610596	40.841447
3515.983098	537794.992745	40.846452
3515.735185	537604.126523	40.851456
3515.528778	537391.837202	40.856461
3515.065594	537197.969615	40.861466
3514.846640	536989.818161	40.866471
3514.656682	536793.124406	40.871476
3514.503190	536613.342443	40.876480
3514.237417	536426.757497	40.881485
3514.297316	536241.432042	40.886490
3513.792223	536061.699177	40.891495
3514.174560	535881.268347	40.896500
3513.592038	535725.485548	40.901504
3513.765403	535540.739835	40.906509
3513.099011	535370.874063	40.911514
3512.992544	535207.838111	40.916519
3513.125872	535045.772795	40.921524
3512.580847	534888.258157	40.926528
3512.714979	534735.736476	40.931533
3512.524446	534585.184143	40.936538
3512.119672	534431.027133	40.941543
3512.078986	534266.758486	40.946548
3511.848930	534125.452232	40.951552
3512.186933	533978.952764	40.956557
3512.060061	533840.507032	40.961562
3511.649553	533695.992303	40.966567
3511.404009	533554.733806	40.971572
3511.215509	533424.528481	40.976576
3511.454259	533295.163874	40.981581
3511.088708	533156.598201	40.986586
3510.933087	533027.849404	40.991591
3510.717204	532885.014022	40.996596
3510.793090	532771.685592	41.001600
3510.653237	532646.265479	41.006605
3510.511037	532520.288995	41.011610
3510.323540	532401.543220	41.016615
3510.220532	532275.053343	41.021620
3510.027118	532170.654946	41.026624
3510.268853	532050.373515	41.031629
3510.170175	531939.794843	41.036634
3509.640303	531828.980394	41.041639
3509.771183	531718.414398	41.046644
3509.134467	531610.293036	41.051648
3509.638727	531519.825694	41.056653
3509.225959	531410.404448	41.061658
3509.235548	531305.109262	41.066663
3509.434106	531204.987611	41.071668
3508.818304	531120.252761	41.076672
3509.109052	531017.488011	41.081677
3509.133995	530924.061425	41.086682
3508.853486	530825.983588	41.091687
3508.983294	530728.749774	41.096692
3508.564615	530646.962294	41.101696
3508.897742	530557.526987	41.106701
3508.865317	530460.822427	41.111706
3508.841089	530381.447081	41.116711
3508.812036	530288.176827	41.121716
3508.464685	530209.407490	41.126720
3508.614322	530104.284224	41.131725
3508.513179	530009.154140	41.136730
3508.282498	529936.226377	41.141735
3508.398951	529852.581658	41.146740
3508.286691	529771.448607	41.151744
3508.254271	529694.041754	41.156749
3508.463118	529615.990025	41.161754
3508.048439	529520.552827	41.166759
3508.059363	529430.959919	41.171764
3507.855760	529358.783168	41.176768
3507.726615	529283.612962	41.181773
3507.777801	529212.456435	41.186778
3507.386703	529144.906725	41.191783
3507.634528	529069.827518	41.196788
3507.298982	529013.688735	41.201792
3507.498279	528936.494205	41.206797
3507.258782	528870.283740	41.211802
3507.188438	528817.740710	41.216807
3507.647159	528734.541301	41.221812
3507.117140	528675.248454	41.226816
3507.221086	528603.272312	41.231821
3507.246273	528546.822190	41.236826
3507.184074	528491.750097	41.241831
3507.189370	528414.482613	41.246836
3507.068967	528362.148118	41.251840
3506.877415	528286.275549	41.256845
3507.037586	528229.752430	41.261850
3506.957805	528179.482841	41.266855
3506.753663	528111.292745	41.271860
3506.574674	528056.894556	41.276864
3506.693757	527999.012651	41.281869
3506.735992	527949.329476	41.286874
3506.625249	527896.284416	41.291879
3506.723116	527837.950453	41.296884
3506.485847	527784.823945	41.301888
3506.625158	527725.724976	41.306893
3506.650633	527670.737247	41.311898
3506.382712	527627.975067	41.316903
3506.799196	527578.383194	41.321908
3506.216815	527529.757624	41.326912
3506.416830	527480.907178	41.331917
3506.222817	527424.588780	41.336922
3506.427362	527383.115781	41.341927
3506.548093	527325.584926	41.346932
3506.137762	527282.440020	41.351936
3506.400187	527227.009005	41.356941
3506.588126	527183.162821	41.361946
3506.260630	527135.405448	41.366951
3506.332240	527080.458926	41.371956
3506.269788	527033.366897	41.376960
3506.222146	526981.875511	41.381965
3506.471690	526948.177246	41.386970
3506.005129	526888.008525	41.391975
3506.322896	526852.530406	41.396980
3505.951799	526803.111131	41.401984
3506.070416	526765.238401	41.406989
3506.245304	526721.544628	41.411994
3506.120009	526668.396693	41.416999
3506.082580	526624.534050	41.422004
3505.990403	526566.781405	41.427008
3506.026317	526551.361049	41.432013
3506.136438	526501.359383	41.437018
3506.250430	526446.757761	41.442023
3506.389311	526395.588787	41.447028
3505.909706	526365.946705	41.452032
3506.080870	526318.714562	41.457037
3505.999788	526259.341741	41.462042
3505.759370	526228.398072	41.467047
3505.929634	526195.822657	41.472052
3505.581403	526147.206397	41.477056
3506.068949	526101.338772	41.482061
3505.729431	526071.168585	41.487066
3505.359372	526046.764933	41.492071
3505.901210	525997.754840	41.497076
3505.481994	525960.167370	41.502080
3505.652483	525920.919805	41.507085
3505.746527	525883.251037	41.512090
3505.479473	525853.422783	41.517095
3505.436689	525815.775481	41.522100
3505.568992	525782.800884	41.527104
3505.431892	525748.807400	41.532109
3505.531334	525711.187917	41.537114
3505.323566	525675.082644	41.542119
3505.683420	525639.443555	41.547124
3505.251132	525618.182754	41.552128
3505.224762	525582.250776	41.557133
3505.522911	525548.642967	41.562138
3505.415413	525525.814411	41.567143
3505.539839	525487.685020	41.572148
3505.311638	525462.600990	41.577152
3505.614072	525420.601990	41.582157
3505.443081	525393.335428	41.587162
3505.535522	525356.828184	41.592167
3505.584557	525314.565691	41.597172
3505.406057	525290.130609	41.602176
3505.393259	525247.877713	41.607181
3505.544895	525220.104968	41.612186
3505.199735	525192.157967	41.617191
3505.568568	525160.003965	41.622196
3505.447461	525145.769597	41.627200
3505.692977	525091.900738	41.632205
3505.481304	525044.624256	41.637210
3505.314764	525035.299831	41.642215
3505.618714	524989.104228	41.647220
3505.378468	524966.447492	41.652224
3505.652978	524925.614150	41.657229
3505.680686	524874.205161	41.662234
3505.420563	524845.587026	41.667239
3505.486680	524812.570351	41.672244
3505.418868	524799.237075	41.677248
3505.613175	524747.952989	41.682253
3505.742534	524719.121436	41.687258
3505.551898	524683.011222	41.692263
3505.286528	524647.468747	41.697268
3505.348082	524627.695513	41.702272
3505.103652	524584.163276	41.707277
3505.185169	524551.548003	41.712282
3505.097802	524536.195739	41.717287
3505.356722	524496.829623	41.722292
3505.214434	524474.813818	41.727296
3505.017404	524443.960938	41.732301
3505.324357	524407.771465	41.737306
3505.237318	524379.580067	41.742311
3505.639989	524352.170526	41.747316
3505.067635	524329.514831	41.752320
3505.247102	524292.485945	41.757325
3505.448080	524250.398830	41.762330
3505.186844	524225.368635	41.767335
3505.354301	524207.802240	41.772340
3504.924726	524172.941786	41.777344
3505.126580	524137.122150	41.782349
3505.280395	524113.643714	41.787354
3505.189354	524100.060790	41.792359
3505.511597	524062.857168	41.797364
3505.482202	524039.104291	41.802368
3505.053573	523998.379727	41.807373
3505.034005	523974.928492	41.812378
3504.963203	523947.138158	41.817383
3505.282284	523922.319066	41.822388
3505.361300	523886.214996	41.827392
3505.103511	523850.265173	41.832397
3505.330800	523813.884764	41.837402
3505.053789	523795.983776	41.842407
3505.056500	523760.295875	41.847412
3505.047036	523745.587682	41.852416
3504.905439	523720.942187	41.857421
3505.008459	523690.242639	41.862426
3504.889562	523670.446202	41.867431
3505.074916	523644.434636	41.872436
3504.794974	523620.215246	41.877440
3505.242726	523587.792889	41.882445
3505.204574	523563.383552	41.887450
3504.957114	523542.798484	41.892455
3505.219091	523509.242688	41.897460
3504.709119	523481.318761	41.902464
3505.013576	523462.516707	41.907469
3505.167705	523436.661392	41.912474
3504.582176	523419.415346	41.917479
3505.079405	523396.842045	41.922484
3504.794514	523378.537438	41.927488
3505.093952	523331.579549	41.932493
3505.102203	523325.158426	41.937498
3505.057849	523306.664070	41.942503
3505.244336	523269.126225	41.947508
3504.859651	523256.448359	41.952512
3505.085555	523214.253505	41.957517
3505.276154	523185.358982	41.962522
3504.799378	523162.838190	41.967527
3505.144584	523134.829058	41.972532
3505.061217	523115.632937	41.977536
3504.888630	523083.509817	41.982541
3504.926733	523059.390974	41.987546
3504.761932	523040.157083	41.992551
3505.099707	523017.709558	41.997556
3504.896100	522997.774031	42.002560
3505.045293	522973.384745	42.007565
3505.320025	522935.377217	42.012570
3504.700464	522910.199407	42.017575
3505.320362	522886.898287	42.022580
3504.832669	522860.031350	42.027584
3504.735713	522822.183403	42.032589
3504.925565	522806.128505	42.037594
3504.791293	522784.311334	42.042599
3504.888476	522756.441852	42.047604
3504.749163	522740.994985	42.052608
3504.816049	522721.370233	42.057613
3505.179811	522690.880342	42.062618
3504.870277	522669.090715	42.067623
3504.923015	522647.799881	42.072628
3504.864378	522641.136295	42.077632
3504.810369	522601.511708	42.082637
3505.226379	522579.202871	42.087642
3504.721387	522556.079061	42.092647
3504.756607	522530.948832	42.097652
3504.657037	522517.315373	42.102656
3504.604342	522495.636579	42.107661
3504.923628	522467.023756	42.112666
3504.646140	522438.454647	42.117671
3504.781730	522421.700201	42.122676
3504.669415	522414.084495	42.127680
3504.629638	522368.087387	42.132685
3505.121218	522355.017556	42.137690
3504.673709	522350.184678	42.142695
3505.255054	522313.138302	42.147700
3505.118193	522292.079180	42.152704
3504.936393	522261.573601	42.157709
3504.650122	522231.438352	42.162714
3504.844341	522212.247844	42.167719
3504.776809	522184.251750	42.172724
3504.870342	522173.620717	42.177728
3504.592117	522158.195250	42.182733
3504.999403	522119.355999	42.187738
3504.790536	522117.518581	42.192743
3504.810017	522087.435850	42.197748
3504.688426	522069.508386	42.202752
3504.452854	522050.537277	42.207757
3505.051718	522019.857309	42.212762
3504.964116	522008.344816	42.217767
3505.046276	521988.362883	42.222772
3504.705120	521952.775902	42.227776
3504.559115	521944.305872	42.232781
3504.836076	521912.412711	42.237786
3504.708884	521908.034622	42.242791
3504.703170	521867.389517	42.247796
3505.216179	521851.282603	42.252800
3504.849272	521824.647633	42.257805
3505.029777	521810.413211	42.262810
3504.917910	521791.675023	42.267815
3505.084322	521748.474661	42.272820
3504.887721	521729.952015	42.277824
3504.795030	521709.694043	42.282829
3504.836632	521682.488723	42.287834
3504.723424	521658.189492	42.292839
3504.986657	521635.701287	42.297844
3505.069065	521612.179960	42.302848
3505.038576	521586.603656	42.307853
3505.202084	521563.625555	42.312858
3504.926670	521534.447858	42.317863
3504.885949	521504.120785	42.322868
3504.820340	521484.919929	42.327872
3504.697988	521465.930243	42.332877
3504.967661	521432.419498	42.337882
3504.596410	521413.317419	42.342887
3504.824631	521397.356181	42.347892
3504.898122	521372.470896	42.352896
3504.934774	521341.372945	42.357901
3504.797865	521321.020364	42.362906
3504.684869	521307.792465	42.367911
3504.767636	521284.675062	42.372916
3504.747408	521266.022900	42.377920
3504.551522	521234.708713	42.382925
3504.896079	521218.122231	42.387930
3504.631827	521203.047546	42.392935
3504.921770	521185.660751	42.397940
3504.939524	521164.525177	42.402944
3504.603939	521141.069233	42.407949
3504.679205	521111.279226	42.412954
3504.376399	521103.035767	42.417959
3504.920497	521062.605103	42.422964
3504.630086	521058.050352	42.427968
3504.423632	521044.331435	42.432973
3504.661831	521020.531846	42.437978
3504.739279	521001.358369	42.442983
3505.010793	520978.665721	42.447988
3504.800943	520953.319002	42.452992
3504.742922	520942.559446	42.457997
3504.756636	520909.189197	42.463002
3504.647407	520893.735820	42.468007
3504.724109	520880.123688	42.473012
3504.878067	520840.916969	42.478016
3504.664790	520830.889690	42.483021
3504.854440	520796.783593	42.488026
3504.643218	520785.542564	42.493031
3504.746384	520756.202525	42.498036
3504.565002	520747.535228	42.503040
3504.462569	520718.935433	42.508045
3504.523369	520703.151653	42.513050
3504.220311	520692.127308	42.518055
3504.763776	520662.464720	42.523060
3504.596123	520662.744083	42.528064
3504.643111	520630.227503	42.533069
3504.818714	520611.391967	42.538074
3504.593003	520608.495303	42.543079
3504.651831	520584.622311	42.548084
3504.588958	520568.554594	42.553088
3504.402573	520544.366387	42.558093
3504.831929	520517.653993	42.563098
3504.453841	520502.900006	42.568103
3504.709330	520482.332686	42.573108
3504.765024	520474.285045	42.578112
3504.458763	520452.289693	42.583117
3504.438502	520425.142616	42.588122
3504.417524	520399.714627	42.593127
3504.411140	520405.024449	42.598132
3504.410701	520389.300605	42.603136
3504.625092	520363.279207	42.608141
3504.724341	520352.848324	42.613146
3504.440438	520328.624650	42.618151
3504.471682	520311.732851	42.623156
3504.715406	520290.004276	42.628160
3504.385888	520272.866095	42.633165
3504.542045	520252.162506	42.638170
3504.618709	520233.544412	42.643175
3504.908433	520214.589263	42.648180
3504.638546	520193.497894	42.653184
3504.554389	520174.551230	42.658189
3504.710497	520154.555367	42.663194
3504.206053	520135.675082	42.668199
3504.671566	520120.635741	42.673204
3504.954524	520103.703946	42.678208
3504.452639	520087.907383	42.683213
3504.802848	520049.780083	42.688218
3504.568082	520049.210533	42.693223
3504.793444	520014.793801	42.698228
3504.496136	519995.375011	42.703232
3504.131754	519989.921557	42.708237
3504.284364	519964.465459	42.713242
3504.390598	519962.122946	42.718247
3504.768198	519944.518739	42.723252
3504.878782	519912.799657	42.728256
3504.616799	519900.302018	42.733261
3504.839096	519875.593183	42.738266
3504.606874	519868.955898	42.743271
3504.707023	519847.350550	42.748276
3504.750141	519839.051780	42.753280
3504.362345	519806.096668	42.758285
3504.603659	519790.232919	42.763290
3504.469667	519776.855414	42.768295
3503.950295	519749.583855	42.773300
3504.371714	519735.208431	42.778304
3504.415356	519733.078024	42.783309
3504.392166	519709.418967	42.788314
3504.237756	519699.128881	42.793319
3504.422497	519685.751490	42.798324
3504.413963	519670.584414	42.803329
3504.349889	519664.881142	42.808333
3504.710355	519640.959105	42.813338
3504.437681	519623.457327	42.818343
3504.430639	519604.447255	42.823348
3504.991015	519583.021632	42.828353
3504.363842	519570.025276	42.833357
3504.462416	519551.756880	42.838362
3504.209257	519530.004706	42.843367
3504.337319	519514.209152	42.848372
3504.318812	519511.936852	42.853377
3504.106140	519483.908508	42.858381
3504.465808	519474.801090	42.863386
3504.164571	519470.197041	42.868391
3504.636369	519449.745928	42.873396
3504.886261	519420.885935	42.878401
3504.629180	519412.988332	42.883405
3504.558941	519381.499053	42.888410
3504.691733	519375.309503	42.893415
3504.610657	519343.467926	42.898420
3504.740851	519337.733838	42.903425
3504.416092	519314.020748	42.908429
3504.797500	519284.634102	42.913434
3504.657181	519269.133543	42.918439
3504.331899	519249.060972	42.923444
3504.683071	519241.117716	42.928449
3504.201376	519215.305641	42.933453
3504.376473	519200.715866	42.938458
3504.262358	519203.110441	42.943463
3504.426070	519175.072647	42.948468
3504.912019	519168.624952	42.953473
3504.458933	519142.504861	42.958477
3504.564233	519115.942534	42.963482
3504.083256	519125.120031	42.968487
3504.218249	519104.519468	42.973492
3504.310869	519081.346838	42.978497
3504.306617	519079.628424	42.983501
3504.378768	519050.441928	42.988506
3504.303625	519036.194939	42.993511
3504.618813	519032.454052	42.998516
3504.763158	519013.823880	43.003521
3504.247100	518991.657469	43.008525
3504.359340	518988.757668	43.013530
3504.208198	518959.909685	43.018535
3504.073284	518950.779018	43.023540
3504.411316	518938.691455	43.028545
3504.115707	518928.726586	43.033549
3504.244713	518903.272576	43.038554
3504.232702	518905.398237	43.043559
3504.223584	518899.028682	43.048564
3504.448968	518870.272725	43.053569
3504.423386	518851.820919	43.058573
3504.556435	518843.659125	43.063578
3504.198293	518824.956463	43.068583
3503.911204	518820.754509	43.073588
3504.238963	518822.017453	43.078593
3504.171887	518803.774408	43.083597
3504.246031	518769.985744	43.088602
3504.141475	518763.277268	43.093607
3504.346452	518767.340667	43.098612
3504.366051	518742.459910	43.103617
3504.155310	518733.341106	43.108621
3504.033353	518712.173889	43.113626
3504.304527	518713.091832	43.118631
3504.246328	518697.223803	43.123636
3504.344420	518674.302559	43.128641
3504.272722	518680.786250	43.133645
3504.417927	518653.256141	43.138650
3504.232865	518646.054693	43.143655
3504.272889	518634.216266	43.148660
3504.620881	518603.872956	43.153665
3504.221612	518592.103928	43.158669
3504.381297	518591.370853	43.163674
3504.282608	518568.177173	43.168679
3504.410149	518548.740090	43.173684
3504.176878	518544.327299	43.178689
3504.250471	518529.095626	43.183693
3504.648292	518503.952472	43.188698
3504.421226	518505.960477	43.193703
3504.447163	518486.033726	43.198708
3504.751778	518469.197961	43.203713
3504.581288	518462.702045	43.208717
3504.772924	518423.685867	43.213722
3504.686960	518418.238450	43.218727
3504.535949	518386.658904	43.223732
3504.502953	518382.922335	43.228737
3504.747721	518352.645445	43.233741
3504.889476	518324.963636	43.238746
3504.763303	518307.336172	43.243751
3504.676792	518288.792234	43.248756
3504.518138	518267.529113	43.253761
3504.292445	518244.355050	43.258765
3504.361266	518227.809136	43.263770
3504.314830	518219.119175	43.268775
3504.351153	518199.594966	43.273780
3504.622298	518195.810287	43.278785
3504.291424	518169.972733	43.283789
3504.453104	518148.810531	43.288794
3504.118393	518148.408407	43.293799
3504.300496	518129.215040	43.298804
3504.630161	518104.486582	43.303809
3504.372846	518104.223924	43.308813
3504.351980	518078.944030	43.313818
3504.450565	518064.769878	43.318823
3504.518153	518051.359111	43.323828
3504.481175	518033.717258	43.328833
3504.605633	518023.382050	43.333837
3504.781489	517997.514707	43.338842
3504.420941	517977.395591	43.343847
3504.386235	517958.843095	43.348852
3504.515956	517937.685674	43.353857
3504.380603	517922.891001	43.358861
3504.444304	517908.722228	43.363866
3504.403020	517886.529860	43.368871
3504.681034	517874.552141	43.373876
3504.533654	517865.321708	43.378881
3504.613363	517849.683905	43.383885
3504.679619	517823.732478	43.388890
3504.697473	517808.458383	43.393895
3504.325953	517795.470781	43.398900
3504.677111	517763.810678	43.403905
3504.483122	517762.223250	43.408909
3504.311835	517750.923262	43.413914
3504.467419	517723.491100	43.418919
3504.579356	517708.707721	43.423924
3504.409548	517696.750083	43.428929
3504.393646	517681.986884	43.433933
3504.507924	517650.364003	43.438938
3504.381982	517646.945365	43.443943
3503.719768	517635.470048	43.448948
3504.416874	517610.986189	43.453953
3504.273895	517618.189514	43.458957
3504.223586	517584.670937	43.463962
3504.225627	517583.861598	43.468967
3504.411506	517573.819811	43.473972
3504.301696	517548.806005	43.478977
3504.326084	517554.010746	43.483981
3504.537918	517527.429029	43.488986
3504.348368	517508.040840	43.493991
3504.262296	517492.631174	43.498996
3504.602678	517483.626849	43.504001
3504.324349	517462.988429	43.509005
3504.198276	517453.754398	43.514010
3504.214559	517448.138796	43.519015
3504.231165	517429.375323	43.524020
3504.387086	517405.229537	43.529025
3504.267158	517400.292838	43.534029
3504.504251	517384.174604	43.539034
3504.774073	517366.888101	43.544039
3504.207054	517347.255969	43.549044
3504.318345	517319.526726	43.554049
3504.527245	517310.998208	43.559053
3504.598649	517295.917454	43.564058
3504.493379	517283.645903	43.569063
3504.387118	517265.913044	43.574068
3504.479948	517242.737805	43.579073
3504.437573	517234.855790	43.584077
3504.309127	517225.419731	43.589082
3504.133107	517198.190817	43.594087
3504.066218	517170.489487	43.599092
3504.077081	517168.970762	43.604097
3504.174833	517176.945341	43.609101
3504.083639	517160.120234	43.614106
3504.370574	517136.206198	43.619111
3504.380274	517121.893579	43.624116
3504.444140	517104.942771	43.629121
3503.979001	517104.055537	43.634125
3504.201509	517083.135209	43.639130
3504.319219	517076.694337	43.644135
3504.172878	517069.688359	43.649140
3504.497536	517053.808814	43.654145
3504.241426	517052.989680	43.659149
3504.089441	517040.927611	43.664154
3504.067337	517013.724638	43.669159
3504.282669	517003.677852	43.674164
3504.508917	516988.167786	43.679169
3504.304213	516980.665296	43.684173
3504.166008	516961.015502	43.689178
3504.169100	516957.980888	43.694183
3504.147735	516954.343298	43.699188
3504.402276	516921.280900	43.704193
3504.289655	516919.832240	43.709197
3504.355560	516913.399492	43.714202
3504.096383	516901.404834	43.719207
3504.357502	516870.718093	43.724212
3504.519131	516867.354984	43.729217
3504.419422	516851.087183	43.734221
3504.013019	516835.575824	43.739226
3504.115182	516833.385225	43.744231
3504.258583	516814.601017	43.749236
3504.112365	516794.750011	43.754241
3503.811796	516784.076642	43.759245
3504.021110	516781.565679	43.764250
3504.157819	516784.628947	43.769255
3503.942393	516764.889984	43.774260
3504.347328	516735.292817	43.779265
3504.034948	516739.033919	43.784269
3504.181554	516726.469294	43.789274
3504.230434	516723.680254	43.794279
3504.056408	516712.733986	43.799284
3504.222372	516687.928151	43.804289
3504.358939	516690.890317	43.809293
3504.283669	516662.279190	43.814298
3504.280354	516651.862181	43.819303
3504.086531	516646.228943	43.824308
3504.340954	516631.068089	43.829313
3504.153486	516622.450151	43.834317
3504.366619	516601.176702	43.839322
3504.475765	516594.736997	43.844327
3504.196471	516567.017659	43.849332
3504.391090	516547.213632	43.854337
3503.850460	516555.643402	43.859341
3504.383675	516535.482419	43.864346
3504.305284	516510.967797	43.869351
3504.250827	516512.847616	43.874356
3504.681123	516496.091132	43.879361
3504.169363	516476.600947	43.884365
3504.568388	516464.501946	43.889370
3504.389507	516462.810860	43.894375
3504.485618	516426.434800	43.899380
3504.525780	516409.638745	43.904385
3503.938618	516417.367935	43.909389
3504.226613	516381.720025	43.914394
3504.217808	516370.443988	43.919399
3503.947539	516372.408504	43.924404
3504.411425	516357.922301	43.929409
3504.184178	516349.765655	43.934413
3504.222296	516337.015596	43.939418
3504.266146	516333.620423	43.944423
3504.146677	516316.596643	43.949428
3504.239008	516296.707341	43.954433
3504.458414	516303.904531	43.959437
3504.512625	516269.304770	43.964442
3504.336293	516258.055134	43.969447
3504.258081	516248.458864	43.974452
3504.513574	516223.132466	43.979457
3504.301263	516211.332191	43.984461
3504.518262	516196.227429	43.989466
3504.337391	516182.045265	43.994471
3504.101538	516163.825987	43.999476
3504.253595	516144.584505	44.004481
3504.088293	516144.155552	44.009485
3504.280684	516116.967785	44.014490
3504.458087	516113.753749	44.019495
3504.615216	516116.257616	44.024500
3504.432080	516079.874362	44.029505
3504.221604	516062.763561	44.034509
3504.329626	516063.404007	44.039514
3504.307575	516047.831165	44.044519
3504.160731	516026.715022	44.049524
3504.489781	516018.419719	44.054529
3504.449252	515996.983299	44.059533
3504.514941	515991.511116	44.064538
3504.369587	515975.097953	44.069543
3504.088780	515943.028539	44.074548
3504.613943	515926.205917	44.079553
3504.513589	515916.612955	44.084557
3504.372340	515902.525438	44.089562
3504.110523	515889.468428	44.094567
3504.284530	515880.641255	44.099572
3504.461281	515855.630185	44.104577
3504.033701	515843.408511	44.109581
3504.004139	515839.215666	44.114586
3504.017954	515828.795435	44.119591
3503.819335	515822.201781	44.124596
3504.155407	515797.570031	44.129601
3503.868153	515800.902781	44.134605
3504.083084	515792.726549	44.139610
3504.399139	515781.651639	44.144615
3504.226862	515761.095489	44.149620
3504.241624	515754.619804	44.154625
3503.839835	515760.600494	44.159629
3504.021369	515739.735531	44.164634
3504.261746	515725.284106	44.169639
3503.903337	515707.943453	44.174644
3504.070647	515693.756418	44.179649
3503.833388	515714.377523	44.184653
3503.893386	515707.085490	44.189658
3504.047665	515677.829507	44.194663
3504.207263	515664.250553	44.199668
3504.237893	515659.997575	44.204673
3503.977357	515670.001886	44.209677
3503.964338	515653.719214	44.214682
3504.177065	515626.729731	44.219687
3504.041504	515619.215698	44.224692
3504.300078	515614.218646	44.229697
3504.190165	515624.806067	44.234701
3504.160657	515604.075437	44.239706
3504.186898	515573.878601	44.244711
3504.247640	515578.117305	44.249716
3504.244666	515553.892801	44.254721
3504.059452	515530.152233	44.259725
3504.065224	515534.450210	44.264730
3504.203589	515529.623855	44.269735
3504.107935	515513.859851	44.274740
3504.313712	515488.540197	44.279745
3504.356591	515482.818580	44.284749
3504.143536	515479.109816	44.289754
3504.067330	515491.158653	44.294759
3503.876740	515461.956798	44.299764
3504.385474	515444.074224	44.304769
3504.014341	515449.493859	44.309773
3504.386852	515414.589147	44.314778
3504.166999	515404.407881	44.319783
3503.743667	515393.348422	44.324788
3504.290305	515392.402330	44.329793
3504.084885	515386.618774	44.334797
3503.764205	515361.483283	44.339802
3503.981434	515353.306474	44.344807
3503.647909	515357.759272	44.349812
3504.141283	515348.274445	44.354817
3503.851372	515351.203105	44.359821
3504.042836	515346.621180	44.364826
3504.211508	515312.962269	44.369831
3504.099436	515307.517957	44.374836
3503.887504	515307.804400	44.379841
3503.797444	515307.616407	44.384845
3504.242758	515287.720690	44.389850
3504.285505	515273.654137	44.394855
3504.067167	515255.481673	44.399860
3504.675117	515253.413231	44.404865
3503.767624	515235.096788	44.409869
3503.893662	515215.403172	44.414874
3504.162372	515211.820507	44.419879
3503.981219	515208.511242	44.424884
3504.127864	515204.745566	44.429889
3503.867100	515189.462528	44.434893
3504.450570	515167.521820	44.439898
3504.346119	515164.453301	44.444903
3504.003485	515155.808551	44.449908
3504.339372	515129.557434	44.454913
3504.174146	515128.066354	44.459917
3503.975627	515121.320679	44.464922
3504.168707	515111.124547	44.469927
3504.159103	515091.249921	44.474932
3504.328599	515073.117114	44.479937
3504.146285	515081.693293	44.484941
3504.156702	515064.394830	44.489946
3504.381949	515040.588695	44.494951
3503.992805	515038.172056	44.499956
3504.443245	515023.484524	44.504961
3504.197068	515006.985193	44.509965
3503.886247	515001.723921	44.514970
3504.163897	514988.075185	44.519975
3503.947172	514991.194644	44.524980
3504.153802	514966.480978	44.529985
3504.041231	514953.247920	44.534989
3504.150145	514950.954856	44.539994
3503.893453	514939.312423	44.544999
3503.977776	514936.618635	44.550004
3504.093500	514924.006961	44.555009
3503.925033	514923.629051	44.560013
3503.788236	514916.721810	44.565018
3504.373119	514907.829188	44.570023
3503.999985	514895.395907	44.575028
3504.102906	514879.397615	44.580033
3504.057168	514874.397864	44.585037
3504.121622	514860.985025	44.590042
3504.213114	514856.924531	44.595047
3503.802900	514845.609753	44.600052
3504.513863	514810.245681	44.605057
3504.000304	514825.449286	44.610061
3504.156963	514816.320836	44.615066
3504.328072	514798.592090	44.620071
3504.043058	514780.176766	44.625076
3504.127312	514762.714592	44.630081
3504.191008	514772.921075	44.635085
3504.383113	514744.264403	44.640090
3504.112753	514745.419893	44.645095
3504.039222	514736.327781	44.650100
3504.178255	514720.677667	44.655105
3504.124063	514696.207133	44.660109
3504.358321	514688.179040	44.665114
3504.213773	514685.420231	44.670119
3503.878803	514678.139597	44.675124
3504.096441	514658.582581	44.680129
3503.903717	514656.033689	44.685133
3503.836960	514645.220840	44.690138
3504.189189	514640.411006	44.695143
3503.973883	514642.012995	44.700148
3504.048927	514609.075547	44.705153
3504.111843	514594.196002	44.710157
3504.068670	514588.791144	44.715162
3503.881587	514588.770207	44.720167
3504.004884	514591.583115	44.725172
3504.010631	514574.082575	44.730177
3503.951522	514566.555985	44.735181
3504.318397	514549.048921	44.740186
3504.182509	514550.891253	44.745191
3503.917511	514537.277338	44.750196
3504.194221	514505.117051	44.755201
3503.867346	514518.167176	44.760205
3504.074663	514507.917850	44.765210
3504.025733	514502.058677	44.770215
3504.010933	514483.094544	44.775220
3504.215969	514472.188050	44.780225
3504.287642	514469.040989	44.785229
3504.149386	514454.850624	44.790234
3504.276609	514432.728179	44.795239
3503.989539	514424.074268	44.800244
3503.957252	514405.972632	44.805249
3504.392646	514418.194272	44.810253
3504.133459	514398.307693	44.815258
3504.202556	514380.392317	44.820263
3504.158280	514364.315643	44.825268
3504.490424	514360.823929	44.830273
3504.059620	514343.999079	44.835277
3504.014537	514332.626247	44.840282
3504.149118	514330.683088	44.845287
3503.974990	514323.376879	44.850292
3504.082815	514305.961083	44.855297
3504.112664	514283.904410	44.860301
3504.059678	514273.746660	44.865306
3503.930192	514277.914602	44.870311
3503.891032	514276.555256	44.875316
3504.054884	514241.023567	44.880321
3503.566626	514243.528562	44.885325
3503.888389	514225.067306	44.890330
3504.348861	514220.493137	44.895335
3504.458637	514231.451342	44.900340
3504.179967	514203.424512	44.905345
3503.899690	514204.733340	44.910349
3503.948943	514208.974207	44.915354
3503.836743	514198.977506	44.920359
3503.790394	514204.396785	44.925364
3504.343126	514176.491402	44.930369
3503.958120	514162.744414	44.935373
3503.892571	514156.432541	44.940378
3504.405916	514140.419257	44.945383
3503.866115	514132.412081	44.950388
3503.815552	514121.748071	44.955393
3504.315181	514099.616909	44.960397
3504.312012	514091.828371	44.965402
3504.243967	514089.613737	44.970407
3504.105683	514069.454767	44.975412
3504.603744	514049.700987	44.980417
3504.169581	514056.951864	44.985421
3504.105031	514045.329020	44.990426
3504.583829	514009.190699	44.995431
3504.178695	514031.003718	45.000436
3504.230261	513997.562994	45.005441
3504.185500	513969.245911	45.010445
3504.053241	513961.477715	45.015450
3504.120332	513978.562895	45.020455
3504.078335	513970.426385	45.025460
3504.520741	513926.453888	45.030465
3504.240607	513930.392829	45.035469
3504.024225	513909.891957	45.040474
3504.316321	513894.924993	45.045479
3504.308237	513884.456435	45.050484
3504.043795	513875.697506	45.055489
3504.090236	513874.071701	45.060493
3504.046727	513855.566612	45.065498
3504.196903	513835.058294	45.070503
3503.778708	513828.245658	45.075508
3504.065903	513832.094958	45.080513
3504.036399	513824.967991	45.085517
3503.766427	513806.549220	45.090522
3504.089936	513775.948108	45.095527
3503.883004	513790.497227	45.100532
3503.679440	513782.537900	45.105537
3504.053872	513772.565193	45.110541
3503.943811	513761.859779	45.115546
3504.199248	513754.333691	45.120551
3503.715268	513754.157358	45.125556
3504.267082	513729.539059	45.130561
3504.118350	513738.818730	45.135565
3503.834457	513730.416856	45.140570
3503.980922	513707.936360	45.145575
3503.721208	513696.445279	45.150580
3503.821933	513707.506415	45.155585
3503.904868	513702.485979	45.160589
3503.810858	513693.093059	45.165594
3504.101985	513690.669867	45.170599
3503.777566	513678.480882	45.175604
3503.950102	513659.536793	45.180609
3503.930705	513649.120458	45.185613
3503.852107	513657.832709	45.190618
3503.761875	513650.310627	45.195623
3503.689483	513655.633039	45.200628
3504.230969	513642.548474	45.205633
3503.742308	513626.996550	45.210637
3503.601224	513605.067163	45.215642
3504.149830	513604.929950	45.220647
3504.070143	513609.595988	45.225652
3504.225584	513602.945499	45.230657
3504.206441	513597.840004	45.235661
3503.867462	513577.965064	45.240666
3504.025004	513564.334158	45.245671
3503.860132	513566.737560	45.250676
3503.800769	513563.712201	45.255681
3503.638540	513557.364802	45.260685
3503.704439	513566.762386	45.265690
3504.020829	513547.896597	45.270695
3503.705013	513529.636509	45.275700
3503.920582	513515.743491	45.280705
3503.846576	513519.397048	45.285709
3503.801449	513515.054340	45.290714
3503.935992	513519.180741	45.295719
3504.003249	513510.065713	45.300724
3504.026980	513496.961706	45.305729
3503.906831	513493.945941	45.310733
3503.560418	513486.919499	45.315738
3503.892068	513485.754385	45.320743
3503.730199	513492.153181	45.325748
3504.025375	513486.441589	45.330753
3503.828904	513489.254640	45.335757
3503.878773	513467.244314	45.340762
3503.861108	513447.874823	45.345767
3503.763236	513447.182237	45.350772
3504.006810	513442.439818	45.355777
3503.918930	513440.531717	45.360781
3503.832274	513431.390392	45.365786
3504.543368	513432.846078	45.370791
3504.133534	513411.464721	45.375796
3504.153747	513397.046094	45.380801
3504.099353	513392.502496	45.385805
3503.926107	513378.165009	45.390810
3503.896951	513355.003668	45.395815
3503.731582	513350.882245	45.400820
3503.962804	513341.437727	45.405825
3504.048535	513345.470723	45.410829
3503.975080	513348.921906	45.415834
3503.911255	513334.617669	45.420839
3503.579392	513332.444632	45.425844
3503.628045	513304.364571	45.430849
3503.829324	513310.857783	45.435853
3503.516395	513311.008476	45.440858
3503.957597	513293.538945	45.445863
3503.619995	513306.389377	45.450868
3503.719385	513294.790685	45.455873
3503.723661	513300.404578	45.460877
3504.124153	513302.212852	45.465882
3504.307807	513278.764867	45.470887
3504.079365	513263.879614	45.475892
3504.000032	513261.363168	45.480897
3503.872146	513258.045097	45.485901
3504.091919	513257.403462	45.490906
3504.032753	513237.939127	45.495911
3504.023449	513227.419774	45.500916
3504.166919	513212.323952	45.505921
3503.911297	513221.216150	45.510925
3503.961103	513216.706618	45.515930
3504.092342	513191.344706	45.520935
3503.972647	513179.729980	45.525940
3503.971769	513161.824368	45.530945
3504.131344	513164.732945	45.535949
3504.224985	513164.060659	45.540954
3504.293997	513130.767204	45.545959
3504.013753	513129.496449	45.550964
3504.221616	513112.721169	45.555969
3504.189781	513105.644849	45.560973
3504.001456	513094.850217	45.565978
3504.319164	513073.353444	45.570983
3503.871409	513079.999905	45.575988
3504.004969	513075.173608	45.580993
3504.004157	513043.560212	45.585997
3503.885955	513028.100928	45.591002
3503.850158	513020.064143	45.596007
3504.046440	513025.900690	45.601012
3504.224752	513024.152798	45.606017
3504.183650	513003.269046	45.611021
3503.658503	512988.885681	45.616026
3504.153770	512981.270764	45.621031
3503.858522	512982.480886	45.626036
3504.225534	512972.357135	45.631041
3503.949800	512955.708714	45.636045
3503.857504	512946.568018	45.641050
3503.632351	512938.409375	45.646055
3503.472896	512942.734129	45.651060
3503.766450	512923.972417	45.656065
3503.737276	512935.965069	45.661069
3503.670669	512934.104131	45.666074
3503.841798	512935.645203	45.671079
3503.952772	512942.253994	45.676084
3503.822836	512921.788838	45.681089
3503.952291	512913.371809	45.686093
3504.202077	512889.407010	45.691098
3504.156463	512882.636268	45.696103
3503.855558	512883.240303	45.701108
3503.902401	512871.194385	45.706113
3504.055921	512853.213462	45.711117
3503.700415	512842.242762	45.716122
3504.229555	512846.913951	45.721127
3503.788553	512842.380725	45.726132
3503.889013	512844.034140	45.731137
3504.246843	512835.479813	45.736141
3503.735176	512811.432920	45.741146
3504.115564	512789.268308	45.746151
3503.586228	512818.892233	45.751156
3503.916322	512790.969169	45.756161
3503.479438	512783.046244	45.761165
3503.540373	512804.079028	45.766170
3503.780320	512799.134673	45.771175
3503.946703	512800.271847	45.776180
3504.193107	512779.848205	45.781185
3503.851862	512767.205976	45.786189
3503.567973	512773.674909	45.791194
3503.934063	512760.516222	45.796199
3503.738360	512760.901304	45.801204
3503.952611	512763.244899	45.806209
3504.256017	512758.037589	45.811213
3503.596998	512736.998255	45.816218
3503.981640	512716.299774	45.821223
3503.879760	512731.490777	45.826228
3503.874225	512721.274009	45.831233
3504.003924	512716.599968	45.836237
3503.976528	512712.608331	45.841242
3503.957982	512687.926914	45.846247
3503.591766	512690.969256	45.851252
3503.917586	512681.863500	45.856257
3504.068880	512659.026765	45.861261
3503.993275	512683.773833	45.866266
3504.284127	512671.638625	45.871271
3504.064847	512635.911196	45.876276
3504.081567	512633.430058	45.881281
3504.129124	512640.554821	45.886285
3504.137790	512625.277449	45.891290
3504.443739	512597.863713	45.896295
3503.795555	512600.596553	45.901300
3503.823672	512586.226568	45.906305
3504.053398	512589.174740	45.911309
3503.940573	512579.177176	45.916314
3504.012487	512550.029940	45.921319
3504.060841	512548.353123	45.926324
3503.839441	512541.154777	45.931329
3504.238333	512539.371973	45.936333
3504.091199	512526.294218	45.941338
3504.193599	512491.780227	45.946343
3504.044236	512494.737747	45.951348
3504.329624	512497.525388	45.956353
3504.314667	512477.850857	45.961357
3503.992515	512466.975807	45.966362
3504.062911	512453.104862	45.971367
3504.127389	512449.149226	45.976372
3504.221648	512435.830915	45.981377
3504.071262	512419.769158	45.986381
3503.686102	512406.577178	45.991386
3504.301823	512405.063594	45.996391
3503.788899	512412.985207	46.001396
3503.910797	512399.561332	46.006401
3503.985218	512370.413391	46.011405
3503.979164	512371.426097	46.016410
3504.002453	512357.410768	46.021415
3503.975914	512349.271033	46.026420
3504.145801	512342.567182	46.031425
3503.854588	512328.803871	46.036429
3503.968018	512322.513607	46.041434
3504.245113	512305.271332	46.046439
3504.116076	512316.673197	46.051444
3504.392322	512303.882443	46.056449
3504.277623	512276.787592	46.061453
3503.999392	512274.049513	46.066458
3504.038120	512270.502578	46.071463
3503.820090	512255.665374	46.076468
3503.889225	512230.413007	46.081473
3503.969425	512234.598896	46.086477
3503.956137	512224.737143	46.091482
3504.040921	512224.824985	46.096487
3504.193595	512229.960521	46.101492
3504.105371	512212.118294	46.106497
3504.052186	512188.655647	46.111501
3504.218387	512179.625434	46.116506
3504.253320	512174.865053	46.121511
3504.225382	512160.301229	46.126516
3504.250595	512136.724951	46.131521
3504.093038	512144.185847	46.136525
3503.903853	512132.480215	46.141530
3504.113001	512099.516675	46.146535
3504.127347	512094.304264	46.151540
3503.789568	512089.703935	46.156545
3504.054101	512093.708971	46.161549
3503.870622	512092.979273	46.166554
3503.940085	512070.711110	46.171559
3504.054806	512070.693052	46.176564
3504.224526	512051.899363	46.181569
3504.126015	512056.922897	46.186573
3503.820405	512054.846712	46.191578
3504.217724	512023.168487	46.196583
3503.973921	512011.623158	46.201588
3503.913384	512016.387777	46.206593
3503.893480	512022.562349	46.211597
3504.059570	512010.851067	46.216602
3504.294340	511984.004024	46.221607
3504.233569	511974.250800	46.226612
3504.073452	511962.489871	46.231617
3504.319372	511955.773852	46.236621
3504.165757	511932.579649	46.241626
3504.295245	511925.376168	46.246631
3504.173796	511911.990368	46.251636
3503.999494	511904.632551	46.256641
3504.188925	511886.037905	46.261645
3503.950134	511873.227058	46.266650
3504.220629	511870.098676	46.271655
3504.090956	511879.932791	46.276660
3504.168124	511846.939035	46.281665
3504.156019	511830.854864	46.286669
3503.912608	511832.006287	46.291674
3504.298574	511817.528508	46.296679
3504.455259	511809.308970	46.301684
3504.107354	511792.519053	46.306689
3504.305707	511785.405800	46.311693
3504.048649	511767.994474	46.316698
3504.197287	511746.016886	46.321703
3504.015215	511738.407297	46.326708
3504.278747	511730.322591	46.331713
3504.314579	511719.137553	46.336717
3503.980656	511708.061532	46.341722
3504.124271	511696.859443	46.346727
3504.186218	511694.522778	46.351732
3504.173820	511677.932650	46.356737
3504.288214	511648.979496	46.361741
3504.247326	511648.024899	46.366746
3504.314063	511636.531405	46.371751
3504.014767	511615.079717	46.376756
3504.143692	511601.451757	46.381761
3504.611654	511594.700502	46.386765
3504.157637	511579.191798	46.391770
3504.402295	511558.564618	46.396775
3504.478822	511554.708042	46.401780
3504.334830	511527.060175	46.406785
3504.203132	511519.391939	46.411789
3504.064433	511511.573047	46.416794
3504.357640	511499.031940	46.421799
3503.960645	511490.798584	46.426804
3503.702558	511468.935507	46.431809
3504.034664	511453.150682	46.436813
3504.012877	511453.002439	46.441818
3504.258102	511458.730620	46.446823
3504.080391	511436.601865	46.451828
3503.863307	511420.650876	46.456833
3503.903349	511408.149715	46.461837
3504.115169	511413.225564	46.466842
3503.864989	511411.342884	46.471847
3503.938406	511405.867993	46.476852
3503.768784	511384.142584	46.481857
3503.946082	511363.677576	46.486861
3503.815719	511366.328766	46.491866
3503.780534	511372.556576	46.496871
3504.063859	511365.176785	46.501876
3503.966522	511363.674637	46.506881
3503.912261	511341.526248	46.511885
3503.612166	511337.425626	46.516890
3503.838974	511340.678000	46.521895
3503.633821	511339.243477	46.526900
3503.863188	511346.845917	46.531905
3504.167764	511358.534001	46.536909
3503.727818	511339.431188	46.541914
3503.755184	511324.301451	46.546919
3503.589055	511289.372175	46.551924
3503.660002	511274.033157	46.556929
3503.746447	511272.552542	46.561933
3504.069996	511283.023589	46.566938
3504.274338	511273.480998	46.571943
3504.396048	511265.722010	46.576948
3503.908128	511251.584215	46.581953
3504.048090	511236.740127	46.586957
3503.824313	511235.359127	46.591962
3503.821200	511235.713802	46.596967
3503.978350	511254.001592	46.601972
3503.852737	511234.899569	46.606977
3504.181006	511213.854060	46.611981
3503.911977	511197.809897	46.616986
3504.118372	511185.788154	46.621991
3503.923801	511190.473013	46.626996
3503.558836	511185.927321	46.632001
3504.118539	511184.473076	46.637005
3503.671782	511162.082962	46.642010
3503.504821	511160.692975	46.647015
3503.735101	511157.419058	46.652020
3503.875529	511140.601903	46.657025
3504.175351	511140.504002	46.662029
3503.764706	511146.942998	46.667034
3504.020047	511136.076995	46.672039
3503.854305	511118.599983	46.677044
3503.435168	511105.311184	46.682049
3504.299183	511085.496121	46.687053
3503.672138	511093.234029	46.692058
3503.915737	511093.195602	46.697063
3503.886199	511098.461455	46.702068
3503.667013	511086.962193	46.707073
3504.037472	511075.723844	46.712077
3503.665929	511067.536847	46.717082
3503.876434	511053.086152	46.722087
3503.748100	511053.612385	46.727092
3503.440711	511047.590511	46.732097
3503.775576	511049.459994	46.737101
3503.429981	511049.109986	46.742106
3503.586741	511043.621805	46.747111
3503.957931	511052.163130	46.752116
3503.823550	511055.523233	46.757121
3503.930633	511041.442987	46.762125
3503.709458	511043.400352	46.767130
3503.500647	511015.863073	46.772135
3503.667619	511011.992080	46.777140
3503.577717	511007.453454	46.782145
3504.082543	510993.259718	46.787149
3503.722668	511006.317757	46.792154
3503.872541	510996.075389	46.797159
3503.642731	511005.419956	46.802164
3503.905378	511001.837366	46.807169
3503.804249	511001.651071	46.812173
3503.502616	510994.818862	46.817178
3503.630111	510979.875345	46.822183
3503.615907	510960.957758	46.827188
3503.355992	510968.131818	46.832193
3503.851519	510956.317157	46.837197
3503.516254	510959.304323	46.842202
3503.579189	510961.166206	46.847207
3503.497357	510953.894538	46.852212
3503.742110	510955.272393	46.857217
3503.823135	510956.625537	46.862221
3503.504894	510969.575848	46.867226
3503.909825	510954.841401	46.872231
3504.020060	510957.505217	46.877236
3503.761901	510955.370806	46.882241
3503.784781	510955.266087	46.887245
3503.643000	510962.876771	46.892250
3503.821033	510943.827606	46.897255
3503.639341	510924.885862	46.902260
3503.389579	510906.865443	46.907265
3503.645290	510900.501579	46.912269
3503.277997	510913.409097	46.917274
3503.669600	510898.929649	46.922279
3503.770349	510912.167900	46.927284
3503.725344	510914.603317	46.932289
3504.018480	510910.712361	46.937293
3503.934001	510908.398730	46.942298
3504.249191	510897.674882	46.947303
3503.911007	510883.563704	46.952308
3504.115779	510865.774932	46.957313
3504.329666	510862.655314	46.962317
3503.906026	510865.049405	46.967322
3503.928967	510857.255253	46.972327
3504.100290	510834.767021	46.977332
3503.859689	510824.383911	46.982337
3504.262930	510820.121413	46.987341
3503.770641	510817.669870	46.992346
3503.884413	510811.176641	46.997351
3503.820959	510797.578444	47.002356
3503.912694	510783.652177	47.007361
3503.874093	510763.726456	47.012365
3503.675534	510778.883894	47.017370
3503.806709	510769.757294	47.022375
3503.673537	510767.805460	47.027380
3503.793150	510777.145514	47.032385
3503.932010	510780.108365	47.037389
3503.828322	510761.963528	47.042394
3504.095831	510740.572919	47.047399
3503.981005	510736.139338	47.052404
3503.702246	510724.396303	47.057409
3504.091528	510725.144270	47.062413
3503.540204	510741.571624	47.067418
3503.616792	510728.760656	47.072423
3503.744829	510728.184018	47.077428
3503.851082	510721.691943	47.082433
3503.838438	510697.563178	47.087437
3503.938360	510694.967431	47.092442
3503.743114	510689.281827	47.097447
3503.859999	510690.730502	47.102452
3503.469897	510691.045174	47.107457
3503.928399	510673.620811	47.112461
3503.583011	510681.820277	47.117466
3503.464337	510669.293070	47.122471
3504.111256	510676.829817	47.127476
3503.771867	510658.216233	47.132481
3504.179808	510632.907949	47.137485
3503.715917	510642.492065	47.142490
3503.918037	510634.416548	47.147495
3504.145168	510634.330134	47.152500
3503.845874	510626.485628	47.157505
3503.870505	510606.954443	47.162509
3503.567125	510612.263726	47.167514
3503.829989	510607.719828	47.172519
3503.869232	510600.226517	47.177524
3503.368753	510607.337571	47.182529
3503.705086	510606.980952	47.187533
3503.521721	510599.118111	47.192538
3504.079955	510588.810958	47.197543
3504.225537	510598.045828	47.202548
3503.923739	510581.652139	47.207553
3504.075777	510558.003041	47.212557
3503.974607	510558.828531	47.217562
3504.122500	510547.473245	47.222567
3504.300375	510543.853369	47.227572
3504.159191	510529.356637	47.232577
3504.157357	510515.748476	47.237581
3504.208451	510514.981633	47.242586
3504.357744	510496.442406	47.247591
3504.357628	510479.596223	47.252596
3504.032752	510474.436930	47.257601
3504.037007	510459.512436	47.262605
3503.967430	510447.280843	47.267610
3503.961860	510433.319080	47.272615
3504.101148	510424.241603	47.277620
3503.885572	510428.474684	47.282625
3504.063733	510413.977971	47.287629
3503.706666	510411.707355	47.292634
3503.800254	510393.075640	47.297639
3503.678912	510374.781413	47.302644
3503.697031	510378.724622	47.307649
3504.275039	510362.191670	47.312653
3503.998317	510377.108868	47.317658
3503.970676	510384.246462	47.322663
3503.585990	510372.874054	47.327668
3503.744872	510351.196588	47.332673
3503.762488	510337.231082	47.337677
3503.540083	510335.040352	47.342682
3503.849530	510321.939328	47.347687
3503.694245	510340.833967	47.352692
3503.585219	510337.107622	47.357697
3503.880038	510326.234867	47.362701
3504.226797	510322.740022	47.367706
3503.912881	510313.632935	47.372711
3503.602305	510299.466319	47.377716
3503.746282	510294.991719	47.382721
3503.991608	510275.880584	47.387725
3503.768814	510282.189033	47.392730
3503.900742	510275.085651	47.397735
3503.781023	510289.775751	47.402740
3503.565294	510288.545170	47.407745
3503.902791	510277.564458	47.412749
3503.760835	510271.516162	47.417754
3503.698074	510256.551493	47.422759
3503.641892	510249.022519	47.427764
3504.148267	510241.657582	47.432769
3504.154992	510234.068070	47.437773
3503.466697	510242.524301	47.442778
3503.741965	510233.425232	47.447783
3504.005572	510242.945180	47.452788
3503.617685	510229.144856	47.457793
3503.998465	510193.722177	47.462797
3503.721725	510190.629390	47.467802
3503.849158	510199.513212	47.472807
3503.722616	510189.415229	47.477812
3503.867782	510188.835865	47.482817
3503.816870	510191.677041	47.487821
3503.699049	510194.629972	47.492826
3503.846025	510189.092475	47.497831
3503.792951	510179.387597	47.502836
3503.736881	510163.460572	47.507841
3504.038515	510147.325227	47.512845
3504.045233	510143.226413	47.517850
3504.166776	510151.858238	47.522855
3504.108057	510149.439252	47.527860
3503.934032	510124.576329	47.532865
3504.261462	510099.735296	47.537869
3504.000844	510105.442701	47.542874
3504.164458	510104.759238	47.547879
3504.427393	510091.564208	47.552884
3503.719391	510075.133051	47.557889
3504.164654	510064.792849	47.562893
3504.023734	510057.176003	47.567898
3503.820445	510055.133987	47.572903
3503.850261	510028.063307	47.577908
3503.612421	510019.196992	47.582913
3504.164146	510010.205883	47.587917
3503.668554	510014.028004	47.592922
3503.811945	510007.276835	47.597927
3504.237103	509993.853728	47.602932
3503.963665	509993.036972	47.607937
3504.019293	509970.211754	47.612941
3503.948192	509968.199427	47.617946
3504.131501	509956.028696	47.622951
3504.058625	509947.844546	47.627956
3503.976638	509946.188073	47.632961
3504.183951	509916.003111	47.637965
3503.846915	509920.407286	47.642970
3503.804695	509927.800329	47.647975
3504.108480	509918.848359	47.652980
3503.915486	509920.194303	47.657985
3504.124948	509892.133784	47.662989
3504.160708	509887.069088	47.667994
3504.015803	509881.375257	47.672999
3504.107236	509878.983093	47.678004
3503.516254	509867.845317	47.683009
3504.001676	509837.160940	47.688013
3504.065603	509833.407150	47.693018
3503.710816	509827.999430	47.698023
3503.920005	509822.502573	47.703028
3503.759636	509817.772402	47.708033
3503.858687	509828.836332	47.713037
3503.884167	509832.070225	47.718042
3503.580462	509807.176744	47.723047
3503.564037	509772.321887	47.728052
3503.495575	509799.854548	47.733057
3503.837588	509782.346509	47.738061
3503.504562	509798.082574	47.743066
3503.704085	509795.521540	47.748071
3504.042491	509782.213161	47.753076
3504.000301	509783.231732	47.758081
3503.865619	509785.782666	47.763085
3503.888113	509783.097835	47.768090
3504.287386	509751.617456	47.773095
3503.972030	509751.970921	47.778100
3503.651841	509743.825760	47.783105
3504.075095	509732.021681	47.788109
3503.747153	509740.370612	47.793114
3503.849814	509737.420146	47.798119
3504.085530	509714.515532	47.803124
3503.767658	509710.771467	47.808129
3503.792724	509706.720241	47.813133
3503.504797	509703.173808	47.818138
3503.976991	509698.545996	47.823143
3504.099061	509694.985353	47.828148
3503.511664	509699.935071	47.833153
3503.858426	509674.280899	47.838157
3503.898072	509668.709606	47.843162
3503.756972	509652.188442	47.848167
3504.118446	509654.559795	47.853172
3503.962201	509659.087239	47.858177
3504.178588	509645.848631	47.863181
3503.883562	509631.223676	47.868186
3504.100013	509612.824654	47.873191
3504.076735	509606.706773	47.878196
3503.833401	509621.669943	47.883201
3503.994962	509611.121348	47.888205
3503.632241	509609.509213	47.893210
3503.434508	509589.556683	47.898215
3503.700167	509579.193984	47.903220
3503.843906	509568.749365	47.908225
3503.941223	509555.225954	47.913229
3503.851279	509564.043277	47.918234
3503.779107	509558.590805	47.923239
3503.880493	509561.053869	47.928244
3503.541213	509569.809413	47.933249
3503.900530	509553.613801	47.938253
3503.991131	509558.810548	47.943258
3503.797711	509541.184519	47.948263
3503.737201	509517.112247	47.953268
3503.896710	509511.572551	47.958273
3504.008355	509496.276099	47.963277
3503.723872	509511.245868	47.968282
3503.752589	509523.181180	47.973287
3504.208460	509508.791587	47.978292
3504.130741	509489.275303	47.983297
3504.051826	509466.824826	47.988301
3503.944192	509471.749375	47.993306
3503.911042	509472.361796	47.998311
3504.017151	509464.503274	48.003316
3503.773522	509441.623464	48.008321
3503.964449	509425.504938	48.013325
3504.038859	509418.207922	48.018330
3504.032756	509419.929107	48.023335
3504.209512	509419.901244	48.028340
3503.805118	509408.328937	48.033345
3504.210660	509381.906150	48.038349
3504.160466	509368.152942	48.043354
3504.050478	509377.277085	48.048359
3504.073393	509366.041956	48.053364
3503.945944	509345.926256	48.058369
3503.992740	509320.976672	48.063373
3503.887842	509335.361690	48.068378
3504.017044	509340.299438	48.073383
3504.031406	509333.163655	48.078388
3503.633294	509318.402946	48.083393
3503.861525	509299.242833	48.088397
3503.876376	509285.985209	48.093402
3503.982711	509277.468856	48.098407
3503.857161	509277.893516	48.103412
3503.644884	509294.218073	48.108417
3503.957785	509287.591609	48.113421
3503.853057	509274.504654	48.118426
3503.707788	509255.757675	48.123431
3503.920962	509234.727928	48.128436
3503.833626	509231.048507	48.133441
3503.952731	509228.500099	48.138445
3503.679273	509236.891257	48.143450
3503.824283	509243.192548	48.148455
3503.940950	509228.198622	48.153460
3503.968993	509212.358606	48.158465
3504.237284	509201.489332	48.163469
3504.010564	509191.912526	48.168474
3504.061341	509192.258726	48.173479
3504.552564	509178.419796	48.178484
3504.292524	509169.961296	48.183489
3504.078237	509161.799120	48.188493
3504.170233	509149.692844	48.193498
3504.097083	509127.999912	48.198503
3504.074258	509106.956715	48.203508
3503.776093	509114.491747	48.208513
3503.890238	509101.420661	48.213517
3503.949421	509103.586900	48.218522
3503.677804	509098.115210	48.223527
3504.112380	509056.812836	48.228532
3503.631763	509063.263667	48.233537
3503.770969	509058.738906	48.238541
3504.001225	509062.142954	48.243546
3503.859869	509066.263451	48.248551
3504.024584	509062.645344	48.253556
3503.711772	509068.007186	48.258561
3504.056444	509037.293034	48.263565
3504.056697	509019.888828	48.268570
3503.779709	509019.072585	48.273575
3503.959168	509011.151668	48.278580
3503.575557	509020.622809	48.283585
3503.831275	509014.561810	48.288589
3503.725550	509011.846530	48.293594
3503.786762	508993.218412	48.298599
3503.779627	508970.553565	48.303604
3503.468651	508986.742231	48.308609
3503.829246	508971.456559	48.313613
3503.789219	508971.412365	48.318618
3503.828358	508972.620505	48.323623
3503.847651	508968.772393	48.328628
3503.875515	508977.571398	48.333633
3503.750177	508968.180818	48.338637
3503.964900	508952.715810	48.343642
3503.832949	508934.674691	48.348647
3503.875612	508931.177035	48.353652
3503.768642	508928.765502	48.358657
3504.120419	508921.778596	48.363661
3504.033573	508928.116648	48.368666
3503.704615	508907.627531	48.373671
3503.917454	508885.838499	48.378676
3503.960360	508883.555055	48.383681
3504.090458	508878.272774	48.388685
3503.861172	508880.181070	48.393690
3503.942536	508877.537387	48.398695
3504.041960	508867.149940	48.403700
3503.667075	508848.843561	48.408705
3503.407062	508841.295590	48.413709
3503.565609	508834.996915	48.418714
3503.633631	508835.795746	48.423719
3503.734111	508832.035960	48.428724
3503.624116	508843.386537	48.433729
3503.695260	508838.821881	48.438733
3503.994713	508840.545426	48.443738
3503.860133	508828.069979	48.448743
3504.045778	508825.966345	48.453748
3503.678188	508809.581355	48.458753
3503.917289	508789.457665	48.463757
3503.996959	508790.962979	48.468762
3503.812626	508783.301833	48.473767
3503.946413	508785.405727	48.478772
3503.641880	508786.769387	48.483777
3503.742861	508783.515456	48.488781
3503.672357	508787.877793	48.493786
3503.938115	508759.958312	48.498791
3504.041765	508745.067212	48.503796
3503.869913	508749.192604	48.508801
3504.005799	508739.254668	48.513805
3504.071381	508737.422971	48.518810
3503.710234	508724.882070	48.523815
3503.881351	508692.575705	48.528820
3503.814775	508697.949339	48.533825
3504.120081	508693.651204	48.538829
3504.106685	508681.105904	48.543834
3503.700241	508694.476626	48.548839
3503.991559	508686.689666	48.553844
3503.513221	508668.804204	48.558849
3503.550779	508648.358039	48.563853
3504.088931	508653.281946	48.568858
3503.791448	508652.823087	48.573863
3503.858193	508636.571666	48.578868
3503.802320	508643.765040	48.583873
3503.641998	508648.141608	48.588877
3503.770587	508648.627306	48.593882
3503.714585	508648.737420	48.598887
3503.814681	508646.191931	48.603892
3503.612651	508634.334143	48.608897
3503.788808	508605.467270	48.613901
3503.840461	508602.271697	48.618906
3503.359426	508602.398392	48.623911
3503.920281	508596.339615	48.628916
3503.753251	508604.866043	48.633921
3503.679532	508595.112936	48.638925
3503.716328	508605.883924	48.643930
3503.557298	508604.188902	48.648935
3504.183394	508603.078123	48.653940
3503.682683	508589.344900	48.658945
3503.780290	508572.531995	48.663949
3503.880627	508566.141232	48.668954
3503.400557	508558.476131	48.673959
3503.636757	508552.873411	48.678964
3503.769487	508565.754256	48.683969
3503.934831	508551.055618	48.688973
3503.825666	508552.287227	48.693978
3503.770423	508565.804922	48.698983
3503.922944	508555.661871	48.703988
3503.843293	508545.403723	48.708993
3504.014367	508511.579172	48.713997
3504.071268	508509.293466	48.719002
3503.696611	508512.793230	48.724007
3503.980815	508515.784099	48.729012
3503.700432	508505.557652	48.734017
3503.926675	508506.179706	48.739021
3503.952038	508475.413829	48.744026
3503.647423	508480.066222	48.749031
3503.770107	508468.612356	48.754036
3503.544604	508466.371279	48.759041
3503.695365	508461.743345	48.764045
3503.951938	508463.878468	48.769050
3504.027724	508467.155262	48.774055
3503.930739	508464.489109	48.779060
3503.667414	508448.036700	48.784065
3503.598658	508438.991057	48.789069
3503.709905	508430.625296	48.794074
3503.376588	508428.451848	48.799079
3503.772484	508433.094730	48.804084
3503.780407	508432.233428	48.809089
3503.865632	508431.967054	48.814093
3503.926232	508427.555742	48.819098
3503.728899	508434.215011	48.824103
3503.754435	508435.779507	48.829108
3503.553056	508438.442372	48.834113
3503.797808	508424.945367	48.839117
3503.673204	508411.911491	48.844122
3503.673868	508396.732794	48.849127
3503.973384	508375.890735	48.854132
3503.420555	508395.558682	48.859137
3503.744849	508386.855655	48.864141
3503.933508	508381.766349	48.869146
3503.758203	508380.681025	48.874151
3503.964236	508381.862830	48.879156
3504.063642	508385.743054	48.884161
3504.014254	508359.694176	48.889165
3503.931295	508334.510692	48.894170
3503.721665	508348.407129	48.899175
3503.876855	508326.626502	48.904180
3503.710974	508342.590456	48.909185
3503.899421	508331.176702	48.914189
3503.705735	508330.094280	48.919194
3503.638362	508311.991706	48.924199
3504.082034	508282.221883	48.929204
3503.738800	508301.401447	48.934209
3503.795313	508276.600602	48.939213
3503.649772	508281.683270	48.944218
3503.504666	508286.108121	48.949223
3503.811611	508286.919812	48.954228
3503.817496	508286.615379	48.959233
3503.873544	508283.722628	48.964237
3503.798109	508267.392138	48.969242
3503.594553	508260.695119	48.974247
3503.666997	508249.097261	48.979252
3503.624112	508265.092443	48.984257
3503.665121	508244.797042	48.989261
3503.798104	508245.585634	48.994266
3503.714977	508251.670366	48.999271
3503.864391	508244.968151	49.004276
3503.765198	508255.457275	49.009281
3503.592137	508244.960731	49.014285
3503.798130	508252.214072	49.019290
3503.795218	508236.125071	49.024295
3503.580797	508204.435283	49.029300
3503.299727	508225.628952	49.034305
3503.695208	508184.381264	49.039309
3503.585327	508207.268170	49.044314
3503.546416	508197.306952	49.049319
3503.710261	508195.004302	49.054324
3503.778819	508216.193320	49.059329
3503.591534	508197.502425	49.064333
3503.858010	508186.531608	49.069338
3503.304598	508194.107382	49.074343
3503.656345	508199.819824	49.079348
3503.551669	508204.693671	49.084353
3503.781466	508192.969713	49.089357
3503.818699	508192.002574	49.094362
3503.276942	508196.793715	49.099367
3503.582542	508199.325893	49.104372
3503.528838	508199.435646	49.109377
3503.440000	508196.768163	49.114381
3503.680760	508187.420488	49.119386
3503.650030	508201.136980	49.124391
3503.652737	508194.255548	49.129396
3503.600008	508205.546896	49.134401
3503.369145	508193.389784	49.139405
3503.631469	508184.595257	49.144410
3503.425857	508193.988121	49.149415
3503.648255	508191.575024	49.154420
3503.503974	508193.166382	49.159425
3503.286829	508194.718660	49.164429
3503.712461	508183.419110	49.169434
3503.721360	508180.129023	49.174439
3503.354979	508170.776104	49.179444
3503.306116	508178.423930	49.184449
3503.439718	508178.908850	49.189453
3503.543547	508174.187064	49.194458
3503.562448	508208.589551	49.199463
3503.676322	508170.928067	49.204468
3503.378306	508187.419010	49.209473
3503.664608	508157.167882	49.214477
3503.773767	508148.802315	49.219482
3503.517728	508150.107763	49.224487
3503.632325	508142.044910	49.229492
3503.676987	508178.872008	49.234497
3503.414676	508167.529387	49.239501
3503.765148	508143.845605	49.244506
3503.451503	508151.737676	49.249511
3503.575862	508147.872776	49.254516
3503.604102	508160.213879	49.259521
3503.759991	508150.980791	49.264525
3503.543663	508131.990837	49.269530
3503.922338	508153.232112	49.274535
3504.147681	508140.345107	49.279540
3503.799094	508128.712519	49.284545
3503.615140	508124.592764	49.289549
3503.784098	508102.202522	49.294554
3503.671405	508098.020901	49.299559
3503.652674	508111.280200	49.304564
3503.534733	508103.658853	49.309569
3503.557231	508093.687870	49.314573
3503.415302	508120.830058	49.319578
3503.706836	508095.941212	49.324583
3503.664771	508096.453898	49.329588
3503.659027	508098.579930	49.334593
3503.643656	508098.835415	49.339597
3503.836161	508098.046116	49.344602
3503.546344	508104.011778	49.349607
3503.698608	508098.371581	49.354612
3503.664023	508102.424836	49.359617
3503.598519	508097.628599	49.364621
3504.039350	508069.629735	49.369626
3503.726530	508072.158479	49.374631
3503.753500	508063.957651	49.379636
3503.582383	508066.969965	49.384641
3503.632710	508069.896683	49.389645
3503.842931	508059.035869	49.394650
3503.787114	508060.765047	49.399655
3504.047156	508047.518314	49.404660
3504.017650	508051.469585	49.409665
3503.771664	508021.403540	49.414669
3503.901262	508018.144943	49.419674
3503.627778	508020.566284	49.424679
3503.879157	508011.267432	49.429684
3503.936774	508024.666520	49.434689
3503.853364	508016.938485	49.439693
3503.906150	508006.962665	49.444698
3503.868756	507989.006804	49.449703
3504.041763	507978.202418	49.454708
3503.971934	507978.061737	49.459713
3503.862162	507966.290101	49.464717
3504.029690	507958.724766	49.469722
3504.004514	507965.609990	49.474727
3504.016484	507935.199444	49.479732
3504.102878	507933.161986	49.484737
3504.095733	507923.802753	49.489741
3504.254644	507929.292778	49.494746
3503.804187	507906.190629	49.499751
3503.476353	507889.697285	49.504756
3503.840969	507881.291214	49.509761
3503.742617	507884.494448	49.514765
3503.828283	507880.079035	49.519770
3503.450780	507887.576543	49.524775
3503.791372	507871.584702	49.529780
3503.635637	507874.392230	49.534785
3503.695811	507869.677261	49.539789
3503.845550	507878.305773	49.544794
3503.740859	507887.632255	49.549799
3504.068456	507866.329771	49.554804
3503.682023	507840.839350	49.559809
3503.728603	507834.254424	49.564813
3503.967925	507824.552600	49.569818
3503.810557	507837.429242	49.574823
3504.452388	507827.663804	49.579828
3504.169313	507814.553329	49.584833
3503.929814	507791.114100	49.589837
3504.248757	507791.468543	49.594842
3503.943705	507787.924418	49.599847
3503.950713	507778.006298	49.604852
3503.989905	507748.754862	49.609857
3504.129212	507746.607824	49.614861
3504.270248	507742.790795	49.619866
3504.423499	507740.084980	49.624871
3504.274915	507722.247610	49.629876
3504.353259	507711.205032	49.634881
3504.031898	507709.586175	49.639885
3504.294230	507679.894575	49.644890
3503.702570	507671.690139	49.649895
3504.164675	507667.468165	49.654900
3504.310597	507659.096551	49.659905
3504.090265	507655.033030	49.664909
3504.276391	507627.832675	49.669914
3503.976500	507619.632698	49.674919
3504.057703	507612.485638	49.679924
3504.323897	507606.371894	49.684929
3504.220413	507585.390186	49.689933
3503.886569	507581.799970	49.694938
3503.986783	507563.568928	49.699943
3504.160246	507561.568263	49.704948
3503.680949	507540.392907	49.709953
3503.791516	507525.145476	49.714957
3504.109631	507524.538692	49.719962
3503.823365	507530.503989	49.724967
3503.544436	507517.443231	49.729972
3503.990053	507524.911997	49.734977
3503.879918	507522.551365	49.739981
3503.439235	507510.275138	49.744986
3503.742473	507500.563031	49.749991
3503.809533	507480.667402	49.754996
3503.667241	507481.145349	49.760001
3503.753957	507491.909141	49.765005
3503.922444	507480.042597	49.770010
3503.723956	507482.755748	49.775015
3503.888470	507480.705890	49.780020
3503.657729	507459.187560	49.785025
3503.610298	507473.210859	49.790029
3504.060421	507468.788338	49.795034
3503.718751	507450.475222	49.800039
3504.000516	507437.224589	49.805044
3503.700237	507440.055032	49.810049
3503.786179	507435.538266	49.815053
3503.989926	507428.472959	49.820058
3503.910874	507429.649290	49.825063
3503.848685	507420.146689	49.830068
3503.902961	507397.470071	49.835073
3503.855714	507391.911775	49.840077
3503.857953	507385.738474	49.845082
3503.646123	507389.364523	49.850087
3503.926375	507378.087426	49.855092
3503.826064	507370.968955	49.860097
3503.897215	507380.318517	49.865101
3503.856790	507367.270549	49.870106
3503.701294	507343.766838	49.875111
3503.616077	507328.651375	49.880116
3503.740634	507339.358683	49.885121
3503.607670	507329.816620	49.890125
3503.842544	507334.131059	49.895130
3503.538310	507346.120501	49.900135
3503.995085	507324.341547	49.905140
3504.033432	507330.862792	49.910145
3503.691413	507336.179184	49.915149
3503.854950	507295.421426	49.920154
3503.747438	507292.250767	49.925159
3503.796504	507278.733198	49.930164
3503.863345	507290.815827	49.935169
3503.647575	507284.272156	49.940173
3503.897828	507280.791956	49.945178
3504.000994	507287.201775	49.950183
3503.982590	507267.370007	49.955188
3503.791933	507256.319055	49.960193
3503.525751	507254.640835	49.965197
3504.008962	507235.842928	49.970202
3503.524383	507247.354952	49.975207
3503.676710	507234.023424	49.980212
3504.129403	507240.580414	49.985217
3504.014412	507232.604024	49.990221
3504.036895	507224.555304	49.995226
3503.777519	507217.310113	50.000231
3503.873324	507203.228509	50.005236
3503.869875	507200.294381	50.010241
3503.971299	507197.950867	50.015245
3504.048777	507193.283578	50.020250
3504.070013	507180.478719	50.025255
3504.156936	507166.246691	50.030260
3504.001636	507150.990352	50.035265
3503.927397	507153.734516	50.040269
3504.189944	507157.892828	50.045274
3504.009262	507145.018657	50.050279
3503.978556	507114.714614	50.055284
3504.020348	507108.737360	50.060289
3503.753054	507107.160500	50.065293
3504.067582	507100.279949	50.070298
3503.846817	507098.139140	50.075303
3503.912740	507073.638680	50.080308
3503.736974	507067.240402	50.085313
3503.737420	507069.163184	50.090317
3504.109874	507064.702238	50.095322
3503.593722	507057.598762	50.100327
3503.506350	507061.255807	50.105332
3503.878297	507066.105243	50.110337
3503.538228	507057.708951	50.115341
3503.969629	507058.551632	50.120346
3503.496212	507047.140441	50.125351
3503.608640	507024.960139	50.130356
3503.787020	507017.089082	50.135361
3503.927485	507009.072214	50.140365
3504.068779	507003.281597	50.145370
3503.595621	507013.628178	50.150375
3503.843008	507009.743580	50.155380
3503.923832	506995.259378	50.160385
3503.843465	507010.452049	50.165389
3504.113057	507000.137785	50.170394
3503.986948	506980.525111	50.175399
3503.929004	506989.591689	50.180404
3503.962696	506972.787332	50.185409
3503.602456	506980.080102	50.190413
3503.872230	506965.060014	50.195418
3503.654538	506958.263524	50.200423
3503.847067	506937.183646	50.205428
3503.944138	506934.790184	50.210433
3503.746072	506926.421984	50.215437
3503.795519	506924.036048	50.220442
3503.690617	506927.038094	50.225447
3503.774227	506921.307166	50.230452
3503.691673	506920.510688	50.235457
3503.538378	506922.154186	50.240461
3503.961957	506920.923515	50.245466
3503.506996	506908.446717	50.250471
3503.571624	506884.958193	50.255476
3503.747941	506876.733199	50.260481
3503.397616	506877.547641	50.265485
3503.489415	506875.863404	50.270490
3503.416730	506878.151966	50.275495
3503.433924	506868.940116	50.280500
3503.339426	506876.747529	50.285505
3503.509894	506888.459861	50.290509
3503.629496	506881.357031	50.295514
3503.439146	506881.235389	50.300519
3503.873888	506882.077552	50.305524
3503.791874	506873.184984	50.310529
3503.636615	506875.587797	50.315533
3503.679942	506882.159024	50.320538
3503.439176	506879.312950	50.325543
3503.395068	506868.997588	50.330548
3503.562788	506882.025959	50.335553
3503.709556	506882.812436	50.340557
3504.028819	506873.502247	50.345562
3503.997552	506881.704464	50.350567
3503.883465	506878.686568	50.355572
3503.963114	506852.058425	50.360577
3503.817025	506843.732570	50.365581
3503.839790	506828.296003	50.370586
3503.692083	506828.117021	50.375591
3503.718737	506823.558866	50.380596
3503.926443	506834.860547	50.385601
3504.106742	506838.323533	50.390605
3504.236446	506810.220011	50.395610
3503.535739	506803.955202	50.400615
3503.861050	506790.545394	50.405620
3503.896016	506784.467907	50.410625
3503.618692	506792.709056	50.415629
3503.847856	506787.005679	50.420634
3503.853692	506791.204653	50.425639
3503.887383	506770.605079	50.430644
3504.025989	506752.114116	50.435649
3503.598404	506752.586572	50.440653
3504.249510	506732.243574	50.445658
3503.563615	506741.510729	50.450663
3503.982385	506726.365686	50.455668
3503.616413	506732.849858	50.460673
3503.861771	506732.355748	50.465677
3503.562895	506709.329242	50.470682
3503.567576	506708.316565	50.475687
3503.701497	506694.076723	50.480692
3503.611939	506688.069484	50.485697
3503.544860	506689.142771	50.490701
3503.872551	506696.175130	50.495706
3503.641597	506701.878966	50.500711
3503.601308	506691.158091	50.505716
3503.693053	506680.062138	50.510721
3503.667346	506696.612660	50.515725
3504.170259	506680.239865	50.520730
3503.743548	506672.110081	50.525735
3503.996437	506639.635161	50.530740
3504.049830	506598.994377	50.535745
3503.447542	506536.648107	50.540749
3503.532439	506492.257620	50.545754
3503.542577	506428.549140	50.550759
3503.502332	506339.598217	50.555764
3503.170563	506266.733692	50.560769
3502.796431	506186.538264	50.565773
3502.735557	506069.353266	50.570778
3502.620807	505962.600150	50.575783
3502.643204	505835.381084	50.580788
3502.361951	505710.030805	50.585793
3501.965897	505570.022668	50.590797
3501.937172	505415.836767	50.595802
3501.293554	505265.187810	50.600807
3501.101972	505116.945761	50.605812
3501.394406	504941.956806	50.610817
3500.959446	504782.111086	50.615821
3500.725193	504586.503918	50.620826
3500.072110	504391.669265	50.625831
3499.865838	504208.097969	50.630836
3499.457304	504006.641382	50.635841
3498.970664	503801.702814	50.640845
3498.956024	503590.108020	50.645850
3498.655612	503370.711279	50.650855
3498.352090	503163.307052	50.655860
3498.194328	502928.395364	50.660865
3497.711498	502693.329481	50.665869
3497.364342	502448.571988	50.670874
3496.823871	502194.528776	50.675879
3496.154932	501947.183308	50.680884
3496.007942	501684.567406	50.685889
3495.308044	501436.359257	50.690893
3495.200485	501165.580327	50.695898
3494.749221	500893.788642	50.700903
3494.243357	500613.598852	50.705908
3493.922623	500333.577879	50.710913
3493.310771	500054.509684	50.715917
3492.799401	499755.780529	50.720922
3492.398866	499479.605960	50.725927
3491.750165	499176.332945	50.730932
3491.603146	498868.216959	50.735937
3490.609143	498574.606729	50.740941
3490.465267	498260.151867	50.745946
3489.855825	497956.902730	50.750951
3489.467738	497648.601504	50.755956
3488.681942	497331.599372	50.760961
3488.195242	497016.417660	50.765965
3487.437969	496678.996457	50.770970
3487.270049	496366.183270	50.775975
3486.853191	496031.885943	50.780980
3486.128028	495710.694219	50.785985
3485.185321	495367.607270	50.790989
3485.175986	495036.315898	50.795994
3484.439923	494707.614495	50.800999
3483.809501	494371.042005	50.806004
3483.310474	494025.226753	50.811009
3482.639682	493674.216500	50.816013
3482.349859	493328.456372	50.821018
3481.142353	492979.138151	50.826023
3480.647562	492630.409639	50.831028
3480.237941	492282.673923	50.836033
3479.536193	491944.751798	50.841037
3479.024615	491580.661637	50.846042
3478.473876	491221.179159	50.851047
3477.706287	490869.776590	50.856052
3476.810715	490515.196939	50.861057
3476.294867	490161.715427	50.866061
3476.157903	489786.236798	50.871066
3475.155968	489435.604073	50.876071
3474.610376	489080.384838	50.881076
3474.170396	488708.781985	50.886081
3473.211844	488347.181548	50.891085
3472.549118	487982.488263	50.896090
3471.979836	487619.849989	50.901095
3471.384638	487250.927689	50.906100
3471.124229	486885.035308	50.911105
3470.168352	486513.420304	50.916109
3469.695182	486138.682293	50.921114
3468.826063	485777.677369	50.926119
3468.327497	485398.724201	50.931124
3468.171940	485018.240166	50.936129
3466.699959	484648.544973	50.941133
3466.165024	484265.876904	50.946138
3465.552724	483895.727395	50.951143
3465.105149	483521.795573	50.956148
3464.271153	483147.816277	50.961153
3463.634137	482772.430631	50.966157
3463.478824	482391.286820	50.971162
3462.535079	482017.860457	50.976167
3461.512711	481637.041617	50.981172
3461.036221	481245.589592	50.986177
3459.977354	480879.608230	50.991181
3459.382199	480505.692505	50.996186
3458.992399	480140.757069	51.001191
3458.379700	479764.651069	51.006196
3457.662535	479382.980119	51.011201
3456.930512	479004.851485	51.016205
3456.433133	478622.320288	51.021210
3455.452535	478249.486965	51.026215
3454.720494	477872.046224	51.031220
3454.502810	477495.936064	51.036225
3453.724362	477109.112373	51.041229
3453.069711	476721.349345	51.046234
3452.320921	476347.176756	51.051239
3451.474644	475962.571685	51.056244
3450.528645	475581.675023	51.061249
3449.608136	475212.779694	51.066253
3449.087069	474845.335082	51.071258
3448.525064	474470.337782	51.076263
3447.468941	474096.932308	51.081268
3447.302575	473719.019998	51.086273
3446.622694	473349.951315	51.091277
3446.220847	472986.610824	51.096282
3445.030857	472612.388200	51.101287
3444.547987	472239.618437	51.106292
3443.879956	471867.175326	51.111297
3443.243836	471479.917413	51.116301
3442.265180	471110.044440	51.121306
3441.580388	470744.681105	51.126311
3440.607068	470388.888123	51.131316
3440.523797	470007.193325	51.136321
3439.554705	469639.320465	51.141325
3438.858557	469263.995645	51.146330
3438.080859	468897.752523	51.151335
3437.053399	468532.962116	51.156340
3436.714321	468156.191936	51.161345
3435.724051	467810.346081	51.166349
3435.391581	467448.874791	51.171354
3434.438278	467086.886954	51.176359
3433.479736	466718.301833	51.181364
3433.214149	466349.752846	51.186369
3432.192601	465995.058958	51.191373
3431.611796	465645.563228	51.196378
3430.754986	465286.064744	51.201383
3430.067330	464919.484593	51.206388
3429.866566	464565.955560	51.211393
3428.740785	464202.272201	51.216397
3428.423045	463845.098403	51.221402
3427.635981	463490.021424	51.226407
3426.521616	463143.865492	51.231412
3425.936524	462781.949020	51.236417
3425.225816	462419.995607	51.241421
3424.523571	462076.851111	51.246426
3423.866561	461729.687244	51.251431
3423.204313	461374.657123	51.256436
3422.689395	461013.967948	51.261441
3422.163486	460670.570438	51.266445
3421.494850	460305.633253	51.271450
3420.896552	459952.395815	51.276455
3419.930373	459600.022408	51.281460
3419.229350	459238.014499	51.286465
3418.423468	458890.068096	51.291469
3417.737525	458538.749309	51.296474
3416.883367	458194.401095	51.301479
3415.982026	457845.032935	51.306484
3415.544634	457494.064058	51.311489
3414.478578	457154.603092	51.316493
3414.113088	456800.314478	51.321498
3413.704628	456472.559233	51.326503
3412.805621	456133.614322	51.331508
3412.212478	455785.940686	51.336513
3411.498942	455437.925551	51.341517
3410.542262	455081.420157	51.346522
3409.689534	454749.549741	51.351527
3408.848320	454409.098324	51.356532
3408.434036	454062.384454	51.361537
3407.630358	453739.065838	51.366541
3407.448633	453391.594607	51.371546
3406.897847	453060.108289	51.376551
3405.704119	452722.630079	51.381556
3404.834838	452377.332357	51.386561
3404.139553	452049.811899	51.391565
3403.799401	451709.697465	51.396570
3403.043374	451378.422135	51.401575
3402.350877	451046.066378	51.406580
3401.627424	450710.666092	51.411585
3401.086567	450371.781435	51.416589
3400.479508	450038.991691	51.421594
3399.885135	449694.574344	51.426599
3398.711209	449363.894354	51.431604
3398.232408	449015.744154	51.436609
3397.227576	448683.708321	51.441613
3396.720119	448354.329560	51.446618
3395.905456	448031.998161	51.451623
3395.142207	447701.331156	51.456628
3395.039056	447373.346428	51.461633
3393.821693	447054.820834	51.466637
3393.019706	446716.482595	51.471642
3392.523824	446396.159200	51.476647
3391.670189	446079.187019	51.481652
3391.122420	445751.503806	51.486657
3390.356657	445422.175614	51.491661
3390.185285	445098.941095	51.496666
3389.313578	444771.447856	51.501671
3388.224650	444450.633660	51.506676
3387.636216	444116.945036	51.511681
3387.120075	443796.386815	51.516685
3386.458501	443478.689825	51.521690
3385.714182	443163.082878	51.526695
3385.046437	442828.830545	51.531700
3384.592693	442513.016868	51.536705
3383.545596	442187.698869	51.541709
3383.015161	441865.442100	51.546714
3382.001106	441539.399505	51.551719
3381.180044	441227.586710	51.556724
3381.036077	440898.910539	51.561729
3380.112009	440592.080846	51.566733
3379.254149	440273.459138	51.571738
3378.721268	439951.786676	51.576743
3378.061637	439635.663677	51.581748
3377.297899	439322.396084	51.586753
3376.461706	439024.087307	51.591757
3376.077969	438692.678035	51.596762
3375.299370	438377.928511	51.601767
3374.367850	438063.503796	51.606772
3374.171346	437744.287943	51.611777
3372.813071	437445.560404	51.616781
3372.438215	437139.286415	51.621786
3371.528050	436823.522600	51.626791
3370.896678	436511.442589	51.631796
3370.458070	436201.892320	51.636801
3369.435659	435902.610916	51.641805
3368.703651	435588.783633	51.646810
3368.515450	435281.670469	51.651815
3367.602574	434975.759859	51.656820
3367.169168	434667.205488	51.661825
3366.562811	434362.153007	51.666829
3365.756569	434066.014724	51.671834
3365.034692	433743.835329	51.676839
3364.432051	433424.324350	51.681844
3363.916607	433122.517976	51.686849
3363.084751	432817.812780	51.691853
3362.298384	432501.086916	51.696858
3361.803981	432190.176345	51.701863
3360.679204	431882.408674	51.706868
3360.038716	431582.990822	51.711873
3359.318629	431270.175099	51.716877
3358.781322	430967.407466	51.721882
3358.118917	430664.554517	51.726887
3357.245653	430372.726526	51.731892
3356.396607	430060.018221	51.736897
3355.724741	429776.582275	51.741901
3355.251219	429473.279358	51.746906
3354.708123	429159.724728	51.751911
3353.962301	428873.954476	51.756916
3353.227666	428566.187588	51.761921
3352.538661	428265.139562	51.766925
3351.512156	427981.816560	51.771930
3350.998185	427684.213402	51.776935
3350.210087	427379.107704	51.781940
3349.600693	427091.468155	51.786945
3348.708234	426806.714654	51.791949
3347.967455	426512.740557	51.796954
3347.416474	426218.784016	51.801959
3346.816812	425927.803422	51.806964
3346.076001	425640.219859	51.811969
3345.183886	425360.047885	51.816973
3344.547385	425062.333372	51.821978
3343.942942	424793.793112	51.826983
3343.182258	424499.063633	51.831988
3342.955686	424211.027976	51.836993
3341.893752	423930.334693	51.841997
3341.041896	423641.045729	51.847002
3340.537944	423354.899035	51.852007
3339.811430	423073.534312	51.857012
3339.238384	422778.324772	51.862017
3338.603220	422498.870120	51.867021
3337.772350	422218.275148	51.872026
3337.334883	421944.549556	51.877031
3336.336349	421646.880480	51.882036
3335.722268	421357.631489	51.887041
3334.893562	421093.383273	51.892045
3334.169724	420801.707284	51.897050
3333.557241	420525.226545	51.902055
3332.742973	420256.192486	51.907060
3332.630200	419977.163267	51.912065
3331.511381	419702.558047	51.917069
3330.934672	419412.978144	51.922074
3330.368621	419136.323931	51.927079
3329.405360	418865.572661	51.932084
3329.002533	418595.670117	51.937089
3328.462506	418315.625019	51.942093
3327.537061	418024.256911	51.947098
3327.042203	417752.252315	51.952103
3326.208915	417479.257033	51.957108
3325.430737	417193.547830	51.962113
3324.651407	416930.446783	51.967117
3324.083367	416651.177310	51.972122
3323.501224	416380.011832	51.977127
3322.772861	416099.110953	51.982132
3322.099659	415819.951652	51.987137
3321.078744	415551.362984	51.992141
3320.577002	415287.313770	51.997146
3320.274458	415008.342081	52.002151
3319.496249	414740.444314	52.007156
3318.657027	414460.104007	52.012161
3318.188958	414195.607610	52.017165
3317.326517	413913.182272	52.022170
3316.862782	413652.872607	52.027175
3315.760965	413384.352944	52.032180
3315.526873	413109.747954	52.037185
3314.985206	412839.889705	52.042189
3313.826106	412571.625768	52.047194
3313.453527	412295.180214	52.052199
3312.593446	412020.613258	52.057204
3312.040100	411753.313314	52.062209
3311.455729	411485.634718	52.067213
3310.649209	411210.187855	52.072218
3309.872963	410938.164094	52.077223
3309.252110	410670.179021	52.082228
3308.772586	410405.421817	52.087233
3307.755330	410138.434885	52.092237
3306.809298	409877.278970	52.097242
3306.584093	409599.362098	52.102247
3305.759579	409349.973452	52.107252
3305.232509	409065.034875	52.112257
3304.430636	408809.158078	52.117261
3304.067573	408544.264481	52.122266
3303.329628	408272.413910	52.127271
3302.225424	408010.250399	52.132276
3301.893460	407738.686653	52.137281
3301.135996	407491.381471	52.142285
3300.137819	407218.342832	52.147290
3299.838286	406949.460827	52.152295
3299.082152	406695.109355	52.157300
3298.503247	406426.851499	52.162305
3297.414051	406168.558301	52.167309
3296.751855	405904.578744	52.172314
3296.335270	405637.432049	52.177319
3295.747777	405383.475192	52.182324
3294.832293	405112.209373	52.187329
3294.335430	404856.149822	52.192333
3293.381368	404605.446986	52.197338
3293.045506	404343.003807	52.202343
3292.305249	404079.834485	52.207348
3291.448461	403827.712161	52.212353
3290.719425	403565.248429	52.217357
3290.134338	403308.961484	52.222362
3289.596238	403049.716646	52.227367
3288.568322	402798.528201	52.232372
3288.211160	402534.904182	52.237377
3287.607405	402280.391120	52.242381
3286.773083	402028.403454	52.247386
3286.187264	401766.944366	52.252391
3285.140658	401519.485281	52.257396
3284.619829	401259.384371	52.262401
3284.231445	401010.241318	52.267405
3283.344289	400756.854001	52.272410
3283.179479	400495.572193	52.277415
3282.029167	400243.569690	52.282420
3281.682262	399969.501082	52.287425
3281.046391	399705.592940	52.292429
3279.993032	399464.652089	52.297434
3279.559621	399204.800492	52.302439
3278.539377	398953.504625	52.307444
3278.126292	398684.977345	52.312449
3277.362758	398442.712111	52.317453
3276.735262	398183.213594	52.322458
3276.143626	397924.342894	52.327463
3275.071136	397677.087511	52.332468
3274.602538	397424.472516	52.337473
3274.379808	397172.655631	52.342477
3273.368941	396918.597251	52.347482
3272.925488	396658.218773	52.352487
3271.998472	396409.151412	52.357492
3271.374998	396151.822720	52.362497
3270.618619	395900.055224	52.367501
3269.985089	395653.554376	52.372506
3269.360094	395392.864295	52.377511
3268.445591	395147.624496	52.382516
3267.900726	394898.816020	52.387521
3267.052479	394645.426599	52.392525
3266.290719	394401.860632	52.397530
3265.915309	394144.553698	52.402535
3265.190895	393910.105533	52.407540
3264.495953	393660.065957	52.412545
3263.833096	393415.740009	52.417549
3262.889219	393157.600282	52.422554
3262.508658	392908.751327	52.427559
3261.743719	392673.843481	52.432564
3261.214000	392416.039501	52.437569
3260.225117	392180.019583	52.442573
3259.669030	391941.336192	52.447578
3259.302118	391691.408454	52.452583
3258.355042	391448.283151	52.457588
3257.817753	391200.082383	52.462593
3257.004974	390958.763119	52.467597
3256.107455	390713.845028	52.472602
3256.006668	390468.722937	52.477607
3254.812928	390229.899887	52.482612
3254.030703	389985.899293	52.487617
3253.687674	389742.768359	52.492621
3252.736944	389509.673991	52.497626
3252.131460	389261.902631	52.502631
3251.138187	389018.132183	52.507636
3250.917406	388773.576761	52.512641
3250.373808	388546.997533	52.517645
3249.579983	388303.572087	52.522650
3249.093146	388059.842151	52.527655
3247.853601	387829.274490	52.532660
3247.455487	387584.383016	52.537665
3247.043014	387344.832231	52.542669
3246.399109	387107.961094	52.547674
3245.568400	386865.523516	52.552679
3244.780950	386634.597017	52.557684
3244.075251	386390.331011	52.562689
3243.391052	386157.071063	52.567693
3242.820146	385918.883731	52.572698
3242.389679	385678.841673	52.577703
3241.425640	385446.486090	52.582708
3240.901331	385201.496859	52.587713
3240.186189	384962.105487	52.592717
3239.617520	384717.399801	52.597722
3239.103205	384492.647176	52.602727
3237.911116	384247.808122	52.607732
3237.344147	384003.072031	52.612737
3236.520649	383766.233218	52.617741
3236.029369	383536.283176	52.622746
3235.414417	383297.958815	52.627751
3234.594977	383067.625468	52.632756
3234.076485	382837.243109	52.637761
3233.360373	382607.602704	52.642765
3232.377598	382369.025462	52.647770
3231.689720	382133.248514	52.652775
3231.017032	381912.981626	52.657780
3230.383333	381677.218713	52.662785
3229.934891	381450.606343	52.667789
3229.085962	381222.708021	52.672794
3228.805187	380983.909333	52.677799
3227.819600	380765.440220	52.682804
3227.370138	380532.184461	52.687809
3226.620397	380300.526244	52.692813
3226.066677	380063.596253	52.697818
3225.447028	379829.956232	52.702823
3224.518415	379617.397746	52.707828
3224.044173	379378.772348	52.712833
3223.021491	379145.853261	52.717837
3222.255589	378923.574714	52.722842
3221.731616	378688.335770	52.727847
3221.200498	378459.506150	52.732852
3220.660403	378233.550782	52.737857
3219.875984	378000.205680	52.742861
3219.204239	377779.889724	52.747866
3218.402495	377553.870114	52.752871
3217.923834	377323.881021	52.757876
3217.422280	377095.751033	52.762881
3216.567945	376868.616672	52.767885
3215.603459	376645.491910	52.772890
3215.126236	376407.662991	52.777895
3214.449534	376189.221309	52.782900
3213.834129	375964.409613	52.787905
3212.819085	375739.634442	52.792909
3212.296455	375515.695854	52.797914
3211.915420	375284.941965	52.802919
3210.960775	375070.328303	52.807924
3210.519745	374841.463730	52.812929
3209.754463	374626.588840	52.817933
3208.844450	374400.568651	52.822938
3208.479253	374169.831382	52.827943
3207.594763	373942.405559	52.832948
3206.936754	373717.181191	52.837953
3206.213654	373495.883350	52.842957
3205.656328	373272.166910	52.847962
3205.014448	373054.720468	52.852967
3204.373786	372837.959532	52.857972
3203.724342	372601.051482	52.862977
3203.172232	372377.660105	52.867981
3202.382276	372169.314095	52.872986
3201.748056	371937.767478	52.877991
3200.604384	371721.182076	52.882996
3200.245039	371509.406707	52.888001
3199.533818	371286.594358	52.893005
3198.808482	371064.342737	52.898010
3198.483505	370847.852303	52.903015
3197.434762	370630.788382	52.908020
3196.829191	370413.958528	52.913025
3196.570292	370194.579607	52.918029
3195.358368	369969.117473	52.923034
3194.860722	369757.965823	52.928039
3194.434147	369543.927123	52.933044
3193.791017	369312.698346	52.938049
3192.827388	369089.838144	52.943053
3192.195326	368874.047778	52.948058
3191.884930	368644.340125	52.953063
3191.000889	368421.489339	52.958068
3190.406610	368205.282619	52.963073
3189.551155	367984.587583	52.968077
3188.908978	367766.478169	52.973082
3188.358933	367546.394092	52.978087
3187.835839	367333.453778	52.983092
3186.981268	367113.975432	52.988097
3186.165383	366898.382500	52.993101
3185.611214	366670.051503	52.998106
3185.101420	366447.080625	53.003111
3184.081962	366240.752238	53.008116
3183.530325	366021.856630	53.013121
3183.251517	365802.407939	53.018125
3182.419958	365588.515805	53.023130
3181.943070	365371.258974	53.028135
3180.921231	365161.007794	53.033140
3180.528091	364928.597010	53.038145
3179.782752	364714.127342	53.043149
3178.886554	364491.538653	53.048154
3178.315045	364264.292242	53.053159
3177.323814	364055.684923	53.058164
3176.959910	363838.962643	53.063169
3176.358615	363625.304708	53.068173
3175.798821	363408.102506	53.073178
3175.153542	363187.248856	53.078183
3174.188632	362973.518200	53.083188
3173.528460	362756.939475	53.088193
3172.947878	362544.749033	53.093197
3172.335852	362329.712809	53.098202
3171.684405	362107.506434	53.103207
3170.984076	361890.573807	53.108212
3170.290518	361673.486434	53.113217
3169.540413	361465.083755	53.118221
3168.801560	361247.212785	53.123226
3168.070283	361028.601700	53.128231
3167.280627	360818.294029	53.133236
3166.799447	360603.865348	53.138241
3166.354640	360403.755811	53.143245
3165.244113	360198.712507	53.148250
3164.644534	359968.039898	53.153255
3163.836822	359764.931602	53.158260
3163.204943	359559.860731	53.163265
3162.877862	359356.852797	53.168269
3161.916890	359145.521585	53.173274
3161.169204	358920.287439	53.178279
3160.488073	358730.539552	53.183284
3160.070557	358521.308040	53.188289
3159.283299	358314.398880	53.193293
3158.462183	358101.997693	53.198298
3157.888387	357897.953936	53.203303
3157.081214	357685.268823	53.208308
3156.612835	357481.181213	53.213313
3156.183152	357276.526798	53.218317
3155.397007	357069.866698	53.223322
3154.666508	356868.515447	53.228327
3154.081685	356659.124361	53.233332
3153.318833	356443.067830	53.238337
3152.964473	356236.641333	53.243341
3151.792054	356034.694993	53.248346
3151.165988	355820.293696	53.253351
3150.630198	355624.988701	53.258356
3149.958686	355416.980343	53.263361
3149.565758	355209.690503	53.268365
3148.875893	355001.734242	53.273370
3148.277117	354788.291296	53.278375
3147.347110	354573.143910	53.283380
3146.689832	354359.377597	53.288385
3146.125875	354164.504084	53.293389
3145.350868	353961.901312	53.298394
3145.309039	353743.276127	53.303399
3144.227159	353531.736722	53.308404
3143.599959	353327.326642	53.313409
3142.883719	353115.218708	53.318413
3142.081484	352905.948400	53.323418
3141.639679	352686.313177	53.328423
3140.482151	352486.590072	53.333428
3140.093894	352283.639635	53.338433
3139.661359	352077.106999	53.343437
3138.849198	351865.874485	53.348442
3138.213446	351656.801919	53.353447
3137.516541	351441.324777	53.358452
3136.967178	351232.618628	53.363457
3136.315342	351027.109166	53.368461
3135.526842	350814.138117	53.373466
3134.938458	350608.413408	53.378471
3134.142285	350408.345373	53.383476
3133.517303	350197.509316	53.388481
3132.972624	349986.786987	53.393485
3132.239928	349779.529460	53.398490
3131.527424	349570.079163	53.403495
3130.953854	349377.276546	53.408500
3130.206453	349165.819586	53.413505
3129.802570	348953.798437	53.418509
3128.655834	348744.846364	53.423514
3128.119328	348537.553102	53.428519
3127.481151	348337.299783	53.433524
3127.140176	348120.836915	53.438529
3126.521701	347910.932763	53.443533
3125.416535	347712.863582	53.448538
3124.803689	347493.183460	53.453543
3124.070907	347297.497281	53.458548
3123.396044	347091.035008	53.463553
3122.756885	346890.420342	53.468557
3121.984028	346690.487880	53.473562
3121.462291	346476.643421	53.478567
3120.616045	346280.666254	53.483572
3120.119876	346071.626754	53.488577
3119.540527	345864.330435	53.493581
3118.673714	345667.361769	53.498586
3117.919226	345468.032996	53.503591
3117.316585	345258.192897	53.508596
3116.565553	345068.152525	53.513601
3116.035826	344858.884865	53.518605
3115.164254	344660.335437	53.523610
3114.737214	344453.213599	53.528615
3113.833133	344249.679076	53.533620
3113.228697	344052.688887	53.538625
3112.483449	343849.509652	53.543629
3111.629650	343653.092111	53.548634
3111.447787	343462.498320	53.553639
3110.544986	343255.803913	53.558644
3110.212846	343063.272680	53.563649
3109.500984	342860.008422	53.568653
3108.562111	342666.986475	53.573658
3108.381049	342463.204170	53.578663
3107.445824	342260.253225	53.583668
3106.658709	342054.961821	53.588673
3106.313254	341846.036224	53.593677
3105.163142	341650.753565	53.598682
3104.981559	341435.157010	53.603687
3104.018670	341240.097962	53.608692
3103.333880	341040.666987	53.613697
3102.957697	340834.161004	53.618701
3102.177915	340634.209196	53.623706
3101.482618	340422.330438	53.628711
3100.646466	340231.473687	53.633716
3099.523943	340033.585132	53.638721
3099.299047	339831.277440	53.643725
3098.526643	339633.434044	53.648730
3098.131224	339439.068676	53.653735
3097.198341	339247.206024	53.658740
3096.708228	339041.781289	53.663745
3096.266594	338843.017597	53.668749
3095.557972	338641.291756	53.673754
3094.956867	338441.304718	53.678759
3094.190452	338238.848538	53.683764
3093.536566	338038.104921	53.688769
3093.014818	337828.913824	53.693773
3092.082901	337636.282517	53.698778
3091.654009	337438.428894	53.703783
3090.596256	337239.044978	53.708788
3090.282808	337034.069565	53.713793
3089.442436	336837.119294	53.718797
3088.518473	336639.417966	53.723802
3088.458039	336433.967890	53.728807
3087.736222	336237.175268	53.733812
3086.812066	336035.373649	53.738817
3086.272354	335826.331766	53.743821
3085.716602	335640.966671	53.748826
3084.967704	335430.989296	53.753831
3084.294805	335237.062630	53.758836
3083.329416	335023.350604	53.763841
3082.865222	334832.368236	53.768845
3081.977310	334628.061864	53.773850
3081.695881	334426.968366	53.778855
3080.925894	334223.125814	53.783860
3080.378891	334025.178967	53.788865
3079.836468	333824.710529	53.793869
3078.882930	333624.637515	53.798874
3078.653828	333427.529672	53.803879
3077.600706	333226.987577	53.808884
3076.788371	333023.020910	53.813889
3076.365274	332812.703951	53.818893
3075.175986	332627.405527	53.823898
3074.894371	332411.489683	53.828903
3074.469515	332229.709758	53.833908
3073.530889	332022.246965	53.838913
3073.082909	331823.794536	53.843917
3072.432452	331621.834887	53.848922
3071.728247	331425.636780	53.853927
3070.791027	331221.124627	53.858932
3070.286310	331020.362241	53.863937
3069.973279	330818.015991	53.868941
3068.842920	330619.209983	53.873946
3068.381578	330417.700772	53.878951
3067.710046	330225.644042	53.883956
3066.680193	330022.161547	53.888961
3066.028573	329815.716315	53.893965
3065.315616	329628.425420	53.898970
3064.794849	329432.473003	53.903975
3064.082772	329244.493611	53.908980
3063.266208	329038.887027	53.913985
3062.839801	328844.394780	53.918989
3061.815418	328657.914526	53.923994
3061.480777	328458.085757	53.928999
3061.101234	328271.426133	53.934004
3060.285093	328063.321810	53.939009
3059.640848	327864.049674	53.944013
3058.777250	327666.695753	53.949018
3058.082319	327464.146304	53.954023
3057.556695	327279.391417	53.959028
3057.124843	327095.079531	53.964033
3056.513729	326880.320013	53.969037
3055.432795	326686.282336	53.974042
3055.137265	326487.766218	53.979047
3054.521701	326286.703312	53.984052
3053.481008	326090.366392	53.989057
3052.948948	325887.023302	53.994061
3051.832266	325693.599904	53.999066
3051.537121	325491.364034	54.004071
3050.398158	325306.497926	54.009076
3049.803432	325108.585865	54.014081
3049.646517	324916.358130	54.019085
3048.926463	324734.937990	54.024090
3048.232023	324544.984061	54.029095
3047.337130	324348.518000	54.034100
3046.533735	324153.411876	54.039105
3046.319146	323963.457053	54.044109
3045.206800	323766.081971	54.049114
3045.064115	323571.226376	54.054119
3044.087313	323387.297817	54.059124
3043.736228	323190.411972	54.064129
3043.235718	322984.739751	54.069133
3042.458688	322795.762438	54.074138
3041.607411	322591.290531	54.079143
3041.010819	322396.911448	54.084148
3040.318360	322215.379645	54.089153
3039.935748	322004.492283	54.094157
3038.716848	321814.182359	54.099162
3038.179650	321612.433733	54.104167
3037.542021	321434.863627	54.109172
3036.634248	321233.452852	54.114177
3036.731465	321036.414760	54.119181
3035.806868	320851.046674	54.124186
3035.083462	320651.515031	54.129191
3034.614828	320453.724956	54.134196
3033.723527	320246.936873	54.139201
3033.265384	320049.653487	54.144205
3032.145632	319859.909304	54.149210
3031.518830	319663.466555	54.154215
3031.051350	319470.257330	54.159220
3030.558955	319268.776410	54.164225
3030.181546	319074.024361	54.169229
3029.154649	318888.642986	54.174234
3028.391322	318686.618041	54.179239
3027.747909	318485.744953	54.184244
3026.849020	318293.059871	54.189249
3026.654127	318093.515398	54.194253
3025.983381	317902.550329	54.199258
3025.324514	317692.333215	54.204263
3024.751757	317497.914365	54.209268
3023.774698	317304.552154	54.214273
3023.321835	317096.185375	54.219277
3022.319016	316914.131955	54.224282
3021.615007	316718.128144	54.229287
3021.093485	316526.805710	54.234292
3020.273070	316325.625088	54.239297
3019.607860	316139.570025	54.244301
3018.675636	315948.948045	54.249306
3018.551619	315742.283301	54.254311
3017.704797	315558.445728	54.259316
3017.195775	315362.713932	54.264321
3016.618638	315160.499388	54.269325
3016.271444	314974.264514	54.274330
3015.189482	314768.487823	54.279335
3014.523953	314562.161004	54.284340
3013.967738	314362.309672	54.289345
3013.458697	314159.700421	54.294349
3012.585282	313973.979901	54.299354
3012.082892	313768.236810	54.304359
3011.192577	313567.163647	54.309364
3010.439808	313382.110505	54.314369
3010.415716	313181.663427	54.319373
3009.211631	312988.914567	54.324378
3008.822835	312790.739832	54.329383
3008.126135	312588.208201	54.334388
3007.068308	312399.560299	54.339393
3006.281903	312203.739179	54.344397
3005.623167	312013.677852	54.349402
3005.042110	311810.566264	54.354407
3004.404689	311609.653144	54.359412
3003.876982	311429.093678	54.364417
3003.325653	311229.490386	54.369421
3002.474277	311032.557054	54.374426
3001.905524	310844.236528	54.379431
3001.273983	310655.874699	54.384436
3000.764850	310449.719004	54.389441
2999.816683	310245.669585	54.394445
2998.906668	310061.985394	54.399450
2998.488642	309858.997291	54.404455
2997.954721	309671.509664	54.409460
2997.100527	309484.581723	54.414465
2996.213689	309294.806606	54.419469
2995.642349	309100.372133	54.424474
2995.112890	308907.407672	54.429479
2994.465736	308705.574307	54.434484
2993.656652	308523.450572	54.439489
2993.499938	308332.998147	54.444493
2992.554293	308152.321505	54.449498
2991.907467	307951.276250	54.454503
2991.209422	307752.836206	54.459508
2990.456833	307559.522956	54.464513
2990.015671	307368.324648	54.469517
2989.095668	307177.201839	54.474522
2988.371459	306982.508093	54.479527
2987.693676	306793.740094	54.484532
2986.903535	306608.198223	54.489537
2986.666934	306414.648767	54.494541
2985.908981	306229.508701	54.499546
2985.207141	306029.946097	54.504551
2984.339562	305831.300710	54.509556
2984.019258	305654.290421	54.514561
2983.184969	305463.202447	54.519565
2982.630941	305271.636926	54.524570
2981.963369	305076.905911	54.529575
2981.209341	304879.565345	54.534580
2980.583823	304690.455013	54.539585
2979.770461	304494.167371	54.544589
2978.884596	304309.426884	54.549594
2978.118891	304119.726781	54.554599
2977.970892	303933.137335	54.559604
2977.121114	303751.089768	54.564609
2976.735453	303562.856707	54.569613
2976.024422	303371.007814	54.574618
2975.305046	303173.532023	54.579623
2974.690051	302986.174880	54.584628
2973.920604	302798.409020	54.589633
2973.308673	302596.968216	54.594637
2972.467915	302415.172196	54.599642
2972.022308	302214.443059	54.604647
2971.487779	302019.890521	54.609652
2970.743598	301831.686515	54.614657
2970.238180	301639.038839	54.619661
2969.338818	301443.983054	54.624666
2968.580276	301243.531359	54.629671
2968.103241	301060.199102	54.634676
2967.429481	300871.829977	54.639681
2966.788175	300667.691841	54.644685
2965.984114	300476.999969	54.649690
2965.318085	300286.387886	54.654695
2964.884658	300088.047904	54.659700
2964.106388	299896.740068	54.664705
2963.364994	299705.018707	54.669709
2962.766039	299520.557994	54.674714
2962.132770	299318.148607	54.679719
2961.680796	299123.986909	54.684724
2960.883708	298946.101830	54.689729
2960.286540	298743.202172	54.694733
2959.674065	298543.335228	54.699738
2959.227413	298351.209139	54.704743
2958.349249	298159.456742	54.709748
2957.823928	297959.880933	54.714753
2957.018717	297764.729484	54.719757
2956.272735	297569.950448	54.724762
2955.550967	297369.997606	54.729767
2954.819737	297174.935675	54.734772
2954.114243	296988.146194	54.739777
2953.731207	296782.841984	54.744781
2952.900947	296584.102406	54.749786
2952.151728	296394.899894	54.754791
2951.880257	296197.624941	54.759796
2951.075085	296008.150766	54.764801
2950.762563	295803.139939	54.769805
2950.170725	295610.524630	54.774810
2949.299007	295401.552639	54.779815
2948.565565	295208.017072	54.784820
2947.398333	295010.806318	54.789825
2947.175791	294803.055235	54.794829
2946.300218	294613.820081	54.799834
2945.827093	294414.639775	54.804839
2945.146756	294221.324075	54.809844
2944.325221	294021.434532	54.814849
2943.640995	293826.463716	54.819853
2943.257387	293633.431586	54.824858
2942.789651	293434.300447	54.829863
2941.921641	293229.247665	54.834868
2941.197591	293041.718918	54.839873
2940.930657	292835.730204	54.844877
2939.814713	292630.232243	54.849882
2939.092893	292432.413808	54.854887
2938.553137	292230.287853	54.859892
2937.861183	292035.112970	54.864897
2937.117234	291830.523185	54.869901
2936.540976	291647.808743	54.874906
2935.945494	291431.225387	54.879911
2935.286755	291231.740585	54.884916
2934.411993	291049.607772	54.889921
2933.813572	290843.797156	54.894925
2933.216342	290651.305747	54.899930
2932.770755	290455.224722	54.904935
2932.032712	290255.598908	54.909940
2931.192867	290055.250496	54.914945
2930.617796	289852.516994	54.919949
2930.112290	289649.594054	54.924954
2929.427898	289451.232540	54.929959
2928.645695	289254.923788	54.934964
2928.166072	289053.116900	54.939969
2927.648110	288844.516042	54.944973
2926.730252	288642.727308	54.949978
2926.085590	288436.489256	54.954983
2925.536851	288239.888187	54.959988
2924.394695	288046.615348	54.964993
2923.929842	287838.209129	54.969997
2923.268040	287652.296621	54.975002
2922.679403	287448.137410	54.980007
2921.989358	287244.554417	54.985012
2921.149764	287062.209757	54.990017
2920.605556	286851.854437	54.995021
2919.928641	286658.634463	55.000026
2919.256863	286457.009137	55.005031
2918.722167	286262.493031	55.010036
2917.882551	286060.690307	55.015041
2917.399691	285863.236961	55.020045
2916.531404	285662.686491	55.025050
2915.862032	285471.935088	55.030055
2915.211389	285267.300537	55.035060
2914.366171	285078.435947	55.040065
2914.243573	284878.760278	55.045069
2913.175801	284671.848395	55.050074
2912.762756	284480.139090	55.055079
2912.103513	284278.485173	55.060084
2911.731547	284078.084558	55.065089
2910.671207	283879.473727	55.070093
2909.849297	283684.950903	55.075098
2909.318748	283484.855281	55.080103
2908.870281	283290.782536	55.085108
2908.312770	283094.383904	55.090113
2907.401753	282886.249386	55.095117
2906.727599	282690.862322	55.100122
2906.152388	282499.254285	55.105127
2905.895023	282294.683473	55.110132
2904.851267	282096.222114	55.115137
2904.061503	281898.408118	55.120141
2903.149772	281692.667271	55.125146
2902.655014	281490.043873	55.130151
2902.073758	281281.805616	55.135156
2901.026399	281094.525064	55.140161
2900.350590	280896.667238	55.145165
2900.213784	280699.666348	55.150170
2898.932702	280512.575447	55.155175
2898.722937	280314.643675	55.160180
2897.871368	280122.365549	55.165185
2897.527166	279919.030208	55.170189
2896.851522	279722.216242	55.175194
2896.042837	279529.854781	55.180199
2895.345918	279330.650071	55.185204
2894.370476	279135.895435	55.190209
2893.929717	278931.505483	55.195213
2893.491021	278743.516775	55.200218
2892.698493	278550.643193	55.205223
2892.170928	278350.571022	55.210228
2891.100332	278160.848536	55.215233
2890.579820	277947.582573	55.220237
2890.102148	277756.951169	55.225242
2889.510431	277565.930301	55.230247
2889.075254	277367.600672	55.235252
2888.091124	277181.684622	55.240257
2887.459023	276970.626468	55.245261
2886.747738	276783.826725	55.250266
2886.108929	276591.132295	55.255271
2885.383598	276386.583281	55.260276
2884.514046	276188.959017	55.265281
2884.367412	275989.895931	55.270285
2883.617763	275795.130589	55.275290
2883.019845	275606.631907	55.280295
2882.582940	275398.369725	55.285300
2881.581744	275200.613450	55.290305
2881.206653	274993.793171	55.295309
2880.494544	274807.044403	55.300314
2879.831914	274605.159579	55.305319
2879.032833	274403.474639	55.310324
2878.404501	274196.236030	55.315329
2878.116283	273984.384738	55.320333
2876.845836	273790.364028	55.325338
2876.120587	273594.601564	55.330343
2875.990183	273381.681116	55.335348
2875.572588	273181.362066	55.340353
2874.834380	272983.207670	55.345357
2874.009380	272770.473653	55.350362
2873.328345	272565.051758	55.355367
2872.924491	272351.487059	55.360372
2872.128647	272150.642230	55.365377
2871.692364	271938.992849	55.370381
2870.648614	271742.262266	55.375386
2869.979637	271529.936677	55.380391
2869.583788	271321.897502	55.385396
2868.629298	271120.925140	55.390401
2868.125093	270917.130940	55.395405
2867.346227	270711.393738	55.400410
2866.615816	270502.770986	55.405415
2865.992100	270286.134333	55.410420
2865.437726	270090.370775	55.415425
2865.155288	269883.052529	55.420429
2864.173123	269677.475095	55.425434
2863.391682	269466.237440	55.430439
2862.786329	269253.291056	55.435444
2862.053956	269053.353672	55.440449
2861.294606	268844.557655	55.445453
2860.552160	268646.048207	55.450458
2859.805811	268433.939385	55.455463
2859.413204	268229.236824	55.460468
2858.723822	268039.123688	55.465473
2858.284244	267829.411454	55.470477
2857.332199	267621.104784	55.475482
2856.629424	267427.377481	55.480487
2856.127473	267210.187696	55.485492
2855.279431	267012.434097	55.490497
2854.804525	266805.274668	55.495501
2854.131842	266608.792337	55.500506
2853.379374	266398.468033	55.505511
2853.032306	266194.064649	55.510516
2851.929599	265990.595979	55.515521
2851.686266	265785.794327	55.520525
2851.169889	265576.018780	55.525530
2850.009570	265367.949784	55.530535
2849.736855	265162.974797	55.535540
2848.711519	264951.242694	55.540545
2848.253322	264743.368452	55.545549
2847.370688	264535.790735	55.550554
2846.466121	264328.089259	55.555559
2846.133091	264121.341587	55.560564
2845.390650	263924.871529	55.565569
2844.894081	263717.869825	55.570573
2843.970211	263513.635503	55.575578
2843.343733	263313.352681	55.580583
2843.076439	263115.305216	55.585588
2841.869738	262910.275584	55.590593
2841.855519	262695.812398	55.595597
2840.913496	262495.197997	55.600602
2840.101124	262283.866671	55.605607
2839.724959	262073.892614	55.610612
2838.740563	261880.849263	55.615617
2837.995448	261668.361640	55.620621
2837.734707	261454.116590	55.625626
2836.788000	261260.023478	55.630631
2836.458507	261051.749067	55.635636
2835.583622	260849.571558	55.640641
2834.971609	260641.927933	55.645645
2834.227995	260432.242408	55.650650
2833.623852	260233.460608	55.655655
2833.231176	260023.363272	55.660660
2832.105871	259817.915351	55.665665
2831.626619	259599.886131	55.670669
2831.214816	259390.454472	55.675674
2830.216732	259193.085599	55.680679
2829.671042	258975.016479	55.685684
2828.687269	258788.087367	55.690689
2828.371669	258568.250364	55.695693
2827.321862	258374.379370	55.700698
2826.653614	258178.996461	55.705703
2826.318228	257958.933924	55.710708
2825.362540	257762.858307	55.715713
2824.820944	257560.656025	55.720717
2824.180697	257354.343812	55.725722
2823.507585	257160.694292	55.730727
2823.219785	256945.973320	55.735732
2822.247427	256751.276433	55.740737
2821.854996	256538.991816	55.745741
2821.029862	256335.256537	55.750746
2820.508895	256133.306927	55.755751
2820.001789	255920.429848	55.760756
2818.957328	255706.619380	55.765761
2818.499577	255499.541437	55.770765
2817.789535	255288.887305	55.775770
2817.133298	255088.615472	55.780775
2816.572201	254873.226749	55.785780
2815.728096	254669.343273	55.790785
2815.257466	254464.178441	55.795789
2814.452697	254259.245000	55.800794
2813.555274	254051.830673	55.805799
2813.203164	253843.337000	55.810804
2812.067185	253640.519482	55.815809
2811.662615	253430.328273	55.820813
2811.108819	253237.911379	55.825818
2810.337847	253032.795618	55.830823
2809.882846	252825.388961	55.835828
2809.058974	252613.584249	55.840833
2808.474851	252409.865733	55.845837
2807.734254	252209.737574	55.850842
2807.023502	252003.416488	55.855847
2806.726497	251788.880765	55.860852
2805.949751	251582.494217	55.865857
2805.058865	251372.204119	55.870861
2804.604275	251174.909573	55.875866
2803.994075	250968.573781	55.880871
2803.078474	250752.329165	55.885876
2802.304656	250546.580059	55.890881
2801.528545	250339.278111	55.895885
2801.009326	250134.202257	55.900890
2800.030201	249934.318245	55.905895
2799.531806	249720.988477	55.910900
2798.834414	249530.381056	55.915905
2798.208067	249327.793420	55.920909
2797.948228	249130.623262	55.925914
2797.239383	248935.358026	55.930919
2796.756029	248712.477359	55.935924
2796.096500	248522.425411	55.940929
2795.497949	248300.403962	55.945933
2794.979848	248098.717555	55.950938
2794.177350	247891.830430	55.955943
2793.672697	247664.116091	55.960948
2792.920635	247459.488054	55.965953
2792.038606	247251.672161	55.970957
2791.436797	247037.140097	55.975962
2790.677326	246838.727791	55.980967
2790.244349	246617.599392	55.985972
2789.186838	246412.028017	55.990977
2788.676855	246204.383893	55.995981
2788.161956	245985.943352	56.000986
2787.377362	245784.098601	56.005991
2786.841879	245568.539598	56.010996
2785.966557	245363.221018	56.016001
2785.232581	245153.296544	56.021005
2784.862699	244951.132671	56.026010
2783.946183	244731.484424	56.031015
2783.645437	244522.740122	56.036020
2782.677724	244316.495525	56.041025
2782.318413	244108.397780	56.046029
2781.610791	243903.258578	56.051034
2780.616865	243690.194377	56.056039
2780.473875	243472.743052	56.061044
2779.385587	243273.674938	56.066049
2778.399149	243063.768272	56.071053
2778.291425	242849.521031	56.076058
2777.298395	242633.886444	56.081063
2776.752722	242430.073586	56.086068
2776.000656	242230.037110	56.091073
2775.442430	242017.568784	56.096077
2774.971509	241800.554227	56.101082
2774.186174	241601.237051	56.106087
2773.483716	241385.838719	56.111092
2772.717198	241186.340985	56.116097
2771.907373	240974.449072	56.121101
2771.185369	240768.553309	56.126106
2770.405755	240567.530787	56.131111
2770.074709	240361.981244	56.136116
2769.344268	240157.564826	56.141121
2768.652802	239953.244448	56.146125
2767.894402	239737.094012	56.151130
2767.464461	239535.432191	56.156135
2766.912378	239331.345476	56.161140
2766.140772	239123.270514	56.166145
2765.502768	238918.510603	56.171149
2764.902318	238712.853862	56.176154
2764.230783	238501.657542	56.181159
2763.776850	238289.816015	56.186164
2763.058621	238079.544598	56.191169
2762.166140	237872.204088	56.196173
2761.605818	237658.623589	56.201178
2760.950192	237448.521708	56.206183
2760.560490	237243.190808	56.211188
2759.423982	237040.092080	56.216193
2758.698257	236825.495390	56.221197
2758.530953	236617.278503	56.226202
2757.602765	236409.360774	56.231207
2757.166729	236198.131612	56.236212
2756.560289	235995.332877	56.241217
2755.683562	235774.268987	56.246221
2754.836476	235563.666402	56.251226
2754.222133	235357.763599	56.256231
2753.785303	235152.164118	56.261236
2753.025102	234941.421723	56.266241
2752.300959	234725.123035	56.271245
2751.666766	234508.428611	56.276250
2751.149513	234308.318181	56.281255
2750.503823	234101.506201	56.286260
2749.696855	233894.974822	56.291265
2748.990272	233681.043670	56.296269
2748.523153	233460.352807	56.301274
2747.626862	233257.707288	56.306279
2747.263826	233049.172177	56.311284
2746.617661	232833.680058	56.316289
2745.960825	232626.185438	56.321293
2745.228972	232414.094381	56.326298
2744.476642	232200.326495	56.331303
2744.246091	231976.647857	56.336308
2743.090347	231764.574452	56.341313
2742.463400	231547.681734	56.346317
2741.997868	231335.958299	56.351322
2741.333840	231125.565363	56.356327
2740.636808	230916.120237	56.361332
2739.795006	230693.916429	56.366337
2738.842023	230490.470986	56.371341
2738.495354	230278.578360	56.376346
2737.381260	230078.342123	56.381351
2737.194397	229862.096586	56.386356
2736.144683	229658.057228	56.391361
2735.605482	229447.291899	56.396365
2735.371289	229239.865189	56.401370
2734.218527	229044.169591	56.406375
2733.687494	228828.592134	56.411380
2733.117984	228621.627361	56.416385
2732.460127	228408.260725	56.421389
2732.068859	228196.049077	56.426394
2731.322712	227990.666925	56.431399
2730.723327	227772.378499	56.436404
2729.532432	227559.683978	56.441409
2728.799736	227358.476866	56.446413
2728.465677	227137.601884	56.451418
2727.618995	226945.579863	56.456423
2726.994078	226741.480011	56.461428
2726.364799	226530.786911	56.466433
2725.620934	226320.749013	56.471437
2725.259301	226122.172195	56.476442
2724.098665	225917.178943	56.481447
2723.853391	225690.743197	56.486452
2722.955242	225496.250204	56.491457
2722.141354	225288.568390	56.496461
2721.753403	225070.138883	56.501466
2721.085780	224879.226250	56.506471
2719.969389	224668.895095	56.511476
2719.844010	224467.738781	56.516481
2719.191377	224266.080889	56.521485
2718.795805	224060.474621	56.526490
2717.713286	223855.461432	56.531495
2717.524302	223638.735567	56.536500
2716.614867	223431.862914	56.541505
2715.795977	223223.028763	56.546509
2715.291623	223013.088751	56.551514
2714.641112	222802.599601	56.556519
2714.068762	222597.585240	56.561524
2713.363844	222380.868170	56.566529
2712.842240	222173.186337	56.571533
2712.483040	221959.050767	56.576538
2711.472672	221742.918518	56.581543
2710.780554	221529.473366	56.586548
2710.053570	221317.294575	56.591553
2709.590860	221095.870945	56.596557
2709.073383	220885.111359	56.601562
2708.084992	220676.603718	56.606567
2707.597085	220463.816615	56.611572
2706.798096	220251.346710	56.616577
2706.139513	220036.818446	56.621581
2705.809208	219816.676020	56.626586
2704.855541	219601.508363	56.631591
2704.267719	219383.546561	56.636596
2703.233577	219177.137990	56.641601
2702.590691	218979.107572	56.646605
2702.084646	218764.915267	56.651610
2701.589368	218553.280468	56.656615
2700.959472	218335.583043	56.661620
2700.121729	218130.342879	56.666625
2699.554254	217912.407719	56.671629
2698.910684	217692.181307	56.676634
2697.943161	217487.409062	56.681639
2697.663124	217264.720591	56.686644
2696.779044	217053.011789	56.691649
2695.746626	216851.013854	56.696653
2695.398362	216638.648619	56.701658
2694.680907	216436.716544	56.706663
2694.054016	216223.963920	56.711668
2693.478288	216020.470410	56.716673
2692.826687	215803.038790	56.721677
2692.636271	215587.953257	56.726682
2691.377539	215383.080555	56.731687
2691.007722	215165.669954	56.736692
2690.340901	214960.004680	56.741697
2689.358593	214747.567490	56.746701
2689.017101	214530.638112	56.751706
2688.087536	214319.415848	56.756711
2687.741156	214099.841104	56.761716
2686.847690	213896.187875	56.766721
2685.953264	213682.683663	56.771725
2685.738750	213469.556106	56.776730
2685.014868	213269.289119	56.781735
2684.242082	213040.010084	56.786740
2683.647599	212832.952496	56.791745
2682.805222	212634.309960	56.796749
2682.349932	212416.934549	56.801754
2681.530088	212215.604081	56.806759
2681.170747	211991.812661	56.811764
2680.222495	211785.743578	56.816769
2679.390946	211570.734366	56.821773
2678.963157	211353.841820	56.826778
2678.230709	211151.533497	56.831783
2677.504180	210940.264481	56.836788
2676.946544	210734.022343	56.841793
2676.066237	210525.655543	56.846797
2675.808300	210316.121708	56.851802
2675.131218	210104.147616	56.856807
2674.559616	209881.364505	56.861812
2674.076861	209676.743088	56.866817
2673.308234	209451.345380	56.871821
2672.663504	209225.585218	56.876826
2671.791473	209017.934849	56.881831
2670.863637	208803.688496	56.886836
2670.196264	208590.254358	56.891841
2669.466177	208378.803629	56.896845
2668.987171	208177.342940	56.901850
2668.143544	207966.306165	56.906855
2667.868815	207747.047329	56.911860
2667.115573	207546.815793	56.916865
2666.262708	207336.597205	56.921869
2665.960622	207114.163217	56.926874
2664.989000	206912.899306	56.931879
2664.367563	206698.446371	56.936884
2664.026730	206477.522660	56.941889
2663.018305	206268.554238	56.946893
2662.509726	206055.371149	56.951898
2661.477584	205847.782462	56.956903
2660.802728	205629.434723	56.961908
2660.347743	205428.730325	56.966913
2659.493260	205215.388713	56.971917
2659.195588	204999.503435	56.976922
2658.325957	204804.097495	56.981927
2657.622633	204584.281881	56.986932
2656.692292	204379.672999	56.991937
2655.854517	204168.088829	56.996941
2655.273912	203954.084863	57.001946
2655.065728	203756.643265	57.006951
2654.681686	203540.268057	57.011956
2654.258822	203330.542907	57.016961
2652.882066	203127.879961	57.021965
2652.474120	202913.165321	57.026970
2651.865226	202707.480671	57.031975
2651.423562	202498.601492	57.036980
2650.883394	202284.342872	57.041985
2649.912846	202065.940964	57.046989
2649.455197	201841.693823	57.051994
2648.401002	201643.820954	57.056999
2648.038522	201422.474639	57.062004
2647.347710	201209.580213	57.067009
2646.456516	200990.419132	57.072013
2646.227678	200776.536934	57.077018
2645.204733	200566.560876	57.082023
2644.733344	200351.853415	57.087028
2644.247575	200139.452389	57.092033
2643.376853	199918.854360	57.097037
2642.841785	199701.334497	57.102042
2641.766399	199489.780216	57.107047
2641.404632	199280.595138	57.112052
2640.894374	199063.213886	57.117057
2639.886562	198848.610079	57.122061
2639.703470	198630.186181	57.127066
2638.812264	198423.709695	57.132071
2637.977886	198210.964283	57.137076
2637.592802	197996.277967	57.142081
2636.626297	197777.587203	57.147085
2636.120957	197560.962062	57.152090
2635.425758	197349.177876	57.157095
2634.917508	197128.801145	57.162100
2634.131626	196911.128794	57.167105
2633.329701	196698.918776	57.172109
2632.960850	196475.379716	57.177114
2632.086263	196272.090186	57.182119
2631.500063	196059.861321	57.187124
2630.648026	195842.534758	57.192129
2629.865596	195630.364195	57.197133
2629.535758	195408.070555	57.202138
2628.619119	195209.461714	57.207143
2627.947340	194989.921616	57.212148
2627.557231	194769.714348	57.217153
2626.940985	194565.970738	57.222157
2626.237889	194352.418700	57.227162
2625.444606	194141.032215	57.232167
2624.692861	193923.278038	57.237172
2624.114773	193718.933766	57.242177
2623.323018	193497.714134	57.247181
2622.934924	193285.796261	57.252186
2622.217652	193074.911171	57.257191
2621.479532	192849.118077	57.262196
2621.075519	192639.966517	57.267201
2619.893062	192423.801228	57.272205
2619.808253	192211.763537	57.277210
2618.902757	192005.824106	57.282215
2618.042625	191780.805905	57.287220
2617.573633	191566.439855	57.292225
2616.729770	191357.007174	57.297229
2616.452691	191145.971520	57.302234
2615.539539	190931.564119	57.307239
2615.063517	190709.645355	57.312244
2614.365001	190489.276909	57.317249
2613.541177	190280.939879	57.322253
2613.378693	190059.674189	57.327258
2612.211299	189854.116162	57.332263
2611.654267	189614.835742	57.337268
2611.107094	189405.237283	57.342273
2610.359755	189198.559526	57.347277
2609.795844	188970.975645	57.352282
2608.784461	188760.333978	57.357287
2608.024850	188549.653358	57.362292
2607.979312	188334.700269	57.367297
2606.871714	188125.972334	57.372301
2606.664988	187911.441113	57.377306
2605.580903	187692.240834	57.382311
2605.230473	187474.897295	57.387316
2604.507222	187262.575513	57.392321
2603.940975	187046.120559	57.397325
2603.255182	186821.670619	57.402330
2602.414983	186604.345140	57.407335
2601.893453	186381.105351	57.412340
2601.431994	186167.385856	57.417345
2600.569614	185943.477045	57.422349
2600.200816	185723.205892	57.427354
2599.289159	185507.372653	57.432359
2598.588883	185287.321506	57.437364
2597.904315	185067.981345	57.442369
2597.200474	184844.548951	57.447373
2596.658073	184617.161134	57.452378
2595.744070	184402.414850	57.457383
2595.184298	184192.562081	57.462388
2594.458508	183975.396391	57.467393
2593.636339	183759.760855	57.472397
2593.449564	183542.702675	57.477402
2592.560203	183328.988044	57.482407
2591.967274	183104.058361	57.487412
2591.337456	182879.110221	57.492417
2590.319795	182666.932905	57.497421
2589.844107	182437.790114	57.502426
2589.047288	182229.663312	57.507431
2588.593320	182014.741163	57.512436
2587.817806	181789.427322	57.517441
2587.042206	181574.303882	57.522445
2586.662051	181357.503329	57.527450
2585.926596	181148.163489	57.532455
2584.988480	180935.536732	57.537460
2584.427668	180722.952994	57.542465
2583.644615	180504.083515	57.547469
2583.412951	180274.035711	57.552474
2582.293814	180070.600476	57.557479
2581.577718	179853.962443	57.562484
2581.199719	179641.469554	57.567489
2580.440380	179431.938305	57.572493
2579.691396	179213.006407	57.577498
2578.816497	178999.539692	57.582503
2578.694292	178790.877349	57.587508
2577.920546	178579.330130	57.592513
2576.878821	178361.084998	57.597517
2576.754701	178140.253427	57.602522
2576.099946	177942.554929	57.607527
2575.209817	177718.285475	57.612532
2574.427256	177495.005009	57.617537
2573.827436	177280.053395	57.622541
2573.268911	177059.703364	57.627546
2572.351887	176853.605961	57.632551
2571.767500	176642.928848	57.637556
2571.111403	176421.554688	57.642561
2570.305506	176209.808317	57.647565
2570.229960	175991.409752	57.652570
2569.372764	175784.532335	57.657575
2568.566425	175567.193020	57.662580
2567.965665	175349.949467	57.667585
2567.091714	175135.192347	57.672589
2566.592527	174916.078074	57.677594
2565.629246	174714.195861	57.682599
2565.026875	174488.740955	57.687604
2564.487874	174282.227717	57.692609
2563.870781	174078.462354	57.697613
2563.402319	173855.533425	57.702618
2562.306546	173645.270743	57.707623
2561.720190	173433.898265	57.712628
2561.343257	173224.312401	57.717633
2560.474898	173006.818582	57.722637
2559.773110	172798.252996	57.727642
2559.094960	172588.425682	57.732647
2558.658917	172377.340196	57.737652
2557.813506	172156.515309	57.742657
2557.315178	171953.759359	57.747661
2556.588966	171729.471468	57.752666
2555.969975	171527.398141	57.757671
2555.180840	171318.065690	57.762676
2554.752905	171101.631665	57.767681
2554.026439	170880.896807	57.772685
2553.468137	170658.496017	57.777690
2552.485356	170459.957648	57.782695
2552.068629	170242.890734	57.787700
2551.564444	170032.095687	57.792705
2550.733193	169817.538512	57.797709
2550.221012	169594.373470	57.802714
2549.266337	169387.837183	57.807719
2548.691276	169174.540095	57.812724
2548.094066	168955.868526	57.817729
2547.447707	168744.467193	57.822733
2546.881515	168528.425487	57.827738
2545.779375	168318.637436	57.832743
2545.170356	168104.067311	57.837748
2544.977128	167884.422255	57.842753
2544.174535	167665.459982	57.847757
2543.672687	167473.168085	57.852762
2543.393493	167180.295351	57.857767
2542.536624	166965.084264	57.862772
2541.947221	166742.177000	57.867777
2541.007057	166523.815355	57.872781
2540.537606	166291.253100	57.877786
2539.711898	166087.270171	57.882791
2538.976421	165846.436731	57.887796
2538.709073	165637.383227	57.892801
2537.748496	165412.940524	57.897805
2537.186340	165195.264233	57.902810
2536.783436	164989.389283	57.907815
2535.972204	164753.470343	57.912820
2535.264130	164520.143180	57.917825
2534.651237	164317.191604	57.922829
2533.885776	164079.769329	57.927834
2533.295100	163867.661863	57.932839
2532.626317	163643.908422	57.937844
2531.737962	163411.227184	57.942849
2530.623040	163204.712165	57.947853
2530.440920	162976.460948	57.952858
2529.897033	162763.195442	57.957863
2529.025744	162545.507558	57.962868
2528.414946	162319.973023	57.967873
2527.831180	162098.071922	57.972877
2527.094498	161886.825573	57.977882
2526.491187	161672.571482	57.982887
2525.796982	161450.984295	57.987892
2525.290481	161226.953054	57.992897
2524.312208	161011.923202	57.997901
2524.036806	160790.655145	58.002906
2523.008978	160577.886122	58.007911
2522.170817	160356.557380	58.012916
2521.560821	160129.243854	58.017921
2520.542019	159924.181804	58.022925
2520.209865	159710.430489	58.027930
2519.502305	159501.609212	58.032935
2518.690601	159280.422850	58.037940
2518.501660	159066.322190	58.042945
2517.425882	158862.864502	58.047949
2517.094174	158639.038033	58.052954
2516.212227	158433.263754	58.057959
2515.618610	158212.583508	58.062964
2514.935733	157997.804880	58.067969
2514.407192	157793.440349	58.072973
2513.895940	157567.907545	58.077978
2512.670850	157353.409522	58.082983
2512.094074	157144.289208	58.087988
2511.791733	156914.926479	58.092993
2511.060349	156720.312786	58.097997
2510.450778	156501.247727	58.103002
2509.307777	156291.141776	58.108007
2508.940953	156071.596054	58.113012
2508.351429	155857.337139	58.118017
2507.802621	155641.039186	58.123021
2506.941575	155420.037818	58.128026
2506.202296	155209.810967	58.133031
2505.354540	155008.246634	58.138036
2505.250385	154785.654860	58.143041
2504.280625	154583.743744	58.148045
2503.490938	154376.466438	58.153050
2503.004967	154159.176463	58.158055
2502.277539	153944.849779	58.163060
2501.986188	153723.375140	58.168065
2500.787958	153511.070671	58.173069
2500.518802	153297.412738	58.178074
2500.145453	153082.158374	58.183079
2499.078593	152872.366641	58.188084
2498.459188	152653.874599	58.193089
2497.767245	152441.077229	58.198093
2497.287347	152227.815449	58.203098
2496.210672	152017.242599	58.208103
2495.628184	151806.249579	58.213108
2495.166950	151586.697227	58.218113
2494.194094	151376.429769	58.223117
2493.645452	151162.512102	58.228122
2493.037816	150941.932292	58.233127
2492.284362	150731.990068	58.238132
2491.961619	150522.349516	58.243137
2491.095731	150310.762791	58.248141
2490.596531	150098.547372	58.253146
2489.649514	149885.603590	58.258151
2489.124577	149668.450922	58.263156
2488.781138	149448.754423	58.268161
2487.751537	149247.965651	58.273165
2487.077824	149023.977696	58.278170
2486.470127	148806.691404	58.283175
2485.793355	148599.279970	58.288180
2485.072927	148383.946214	58.293185
2484.547190	148183.109627	58.298189
2484.139129	147962.798024	58.303194
2483.088908	147743.098075	58.308199
2482.383578	147528.771678	58.313204
2482.332360	147308.903663	58.318209
2481.381251	147108.547923	58.323213
2480.893102	146885.943446	58.328218
2480.320464	146668.322970	58.333223
2479.287380	146448.451315	58.338228
2479.034930	146223.399514	58.343233
2478.209195	146010.767238	58.348237
2477.489190	145784.204135	58.353242
2476.565568	145573.649053	58.358247
2475.979796	145361.529575	58.363252
2475.283908	145126.694447	58.368257
2474.444753	144933.184350	58.373261
2473.995047	144708.250898	58.378266
2473.335189	144500.444223	58.383271
2472.497731	144288.066927	58.388276
2471.886075	144067.497059	58.393281
2471.394402	143869.135044	58.398285
2470.828794	143649.107268	58.403290
2470.416412	143435.435811	58.408295
2469.478463	143215.927592	58.413300
2468.719707	142992.936204	58.418305
2467.925563	142789.050648	58.423309
2467.412801	142560.533976	58.428314
2466.881522	142356.939998	58.433319
2466.225970	142130.126462	58.438324
2465.518836	141918.710514	58.443329
2464.791791	141700.437647	58.448333
2464.190685	141479.020592	58.453338
2463.563829	141275.283780	58.458343
2462.622566	141054.609871	58.463348
2462.278218	140837.705630	58.468353
2461.456586	140622.822625	58.473357
2460.625869	140402.885595	58.478362
2460.010006	140199.471916	58.483367
2459.500737	139981.418302	58.488372
2459.187488	139763.856129	58.493377
2458.295462	139543.325210	58.498381
2457.700706	139326.153878	58.503386
2457.104781	139117.662132	58.508391
2456.192851	138895.309547	58.513396
2455.961132	138666.574393	58.518401
2455.014682	138451.980796	58.523405
2454.096604	138231.438268	58.528410
2453.592854	138008.837016	58.533415
2452.624495	137794.836064	58.538420
2452.303573	137568.855038	58.543425
2451.434395	137378.434196	58.548429
2451.132577	137156.150368	58.553434
2450.084371	136940.160925	58.558439
2449.505256	136718.191147	58.563444
2449.134241	136500.979593	58.568449
2448.259839	136290.900296	58.573453
2447.660055	136068.887883	58.578458
2446.949094	135855.304863	58.583463
2446.352818	135635.518393	58.588468
2445.911933	135421.273241	58.593473
2445.135260	135206.866927	58.598477
2444.273217	134977.485381	58.603482
2443.708195	134763.709377	58.608487
2442.966643	134549.454791	58.613492
2442.651717	134332.644297	58.618497
2441.580206	134118.203844	58.623501
2440.504755	133894.060361	58.628506
2440.324778	133686.150979	58.633511
2439.795310	133466.230632	58.638516
2439.464426	133248.516202	58.643521
2438.358507	133042.333418	58.648525
2437.854663	132813.725277	58.653530
2437.167727	132597.101158	58.658535
2436.214286	132378.920410	58.663540
2435.867792	132152.248811	58.668545
2434.951923	131948.063489	58.673549
2434.245060	131724.640710	58.678554
2433.797610	131495.957987	58.683559
2433.008524	131287.946677	58.688564
2432.590233	131075.330820	58.693569
2431.461992	130864.797891	58.698573
2430.916089	130644.127132	58.703578
2430.387837	130426.833943	58.708583
2429.491223	130212.369767	58.713588
2428.989683	129992.891030	58.718593
2428.322442	129780.400626	58.723597
2427.588240	129567.096866	58.728602
2426.934606	129354.709148	58.733607
2426.182822	129150.492697	58.738612
2425.687042	128921.686164	58.743617
2424.750526	128706.249194	58.748621
2424.399372	128500.513401	58.753626
2424.083111	128272.026679	58.758631
2423.224435	128071.061077	58.763636
2422.639484	127850.647196	58.768641
2422.163719	127635.463023	58.773645
2421.361775	127409.422693	58.778650
2420.396338	127194.573594	58.783655
2419.919591	126974.619471	58.788660
2419.213581	126747.553367	58.793665
2418.314107	126541.957202	58.798669
2417.736598	126324.742040	58.803674
2417.099173	126109.849444	58.808679
2416.572804	125901.112930	58.813684
2416.126698	125671.779432	58.818689
2415.252127	125461.742640	58.823693
2414.110557	125240.307751	58.828698
2413.720215	125022.489135	58.833703
2413.115097	124814.522701	58.838708
2412.625938	124598.374040	58.843713
2412.002501	124388.686724	58.848717
2411.185424	124161.228057	58.853722
2410.780862	123944.271202	58.858727
2410.017867	123727.106249	58.863732
2409.304506	123515.674887	58.868737
2408.831528	123295.115058	58.873741
2407.784868	123078.660640	58.878746
2407.178600	122854.925609	58.883751
2406.929332	122648.621066	58.888756
2406.424319	122423.921241	58.893761
2405.371434	122213.798403	58.898765
2404.622298	121975.694050	58.903770
2404.398792	121764.871881	58.908775
2403.510704	121552.252116	58.913780
2403.001887	121322.051490	58.918785
2402.295442	121101.470667	58.923789
2401.387000	120888.351577	58.928794
2401.092905	120660.916060	58.933799
2400.218292	120453.013638	58.938804
2399.829114	120215.960020	58.943809
2398.934068	120000.141569	58.948813
2398.129014	119779.714432	58.953818
2397.758177	119552.522874	58.958823
2396.795789	119338.396503	58.963828
2396.457362	119109.781655	58.968833
2395.537922	118883.920786	58.973837
2394.548210	118659.786996	58.978842
2394.513904	118450.891251	58.983847
2393.456147	118230.136406	58.988852
2393.136755	117999.046259	58.993857
2392.371629	117792.207796	58.998861
2391.876197	117554.363679	59.003866
2391.025161	117322.773521	59.008871
2390.265568	117112.594375	59.013876
2389.710695	116877.641430	59.018881
2388.901847	116661.189636	59.023885
2388.271613	116444.463797	59.028890
2387.715029	116219.647793	59.033895
2386.874922	115997.893734	59.038900
2386.291553	115769.766240	59.043905
2385.652788	115555.327993	59.048909
2385.066377	115333.076141	59.053914
2384.487727	115106.597774	59.058919
2383.551119	114886.207952	59.063924
2382.945480	114664.256970	59.068929
2382.651272	114442.112576	59.073933
2381.845016	114212.409570	59.078938
2381.165190	113989.981204	59.083943
2380.424731	113781.654425	59.088948
2380.100856	113546.143454	59.093953
2379.242997	113322.530626	59.098957
2378.513275	113095.446879	59.103962
2378.175543	112858.992545	59.108967
2377.221442	112645.124043	59.113972
2376.485410	112416.333883	59.118977
2376.007417	112193.591155	59.123981
2374.982760	111960.592466	59.128986
2374.885475	111740.541415	59.133991
2374.088632	111517.366621	59.138996
2373.650680	111284.147978	59.144001
2372.926409	111062.038285	59.149005
2372.361161	110829.161415	59.154010
2371.278865	110592.611858	59.159015
2370.615599	110372.795953	59.164020
2370.286778	110145.466169	59.169025
2369.646955	109912.717654	59.174029
2368.938434	109677.450257	59.179034
2368.292309	109462.418161	59.184039
2367.377987	109224.160818	59.189044
2367.027513	108988.894026	59.194049
2365.971989	108753.880887	59.199053
2365.349713	108543.504389	59.204058
2364.987869	108301.646688	59.209063
2364.182055	108079.012168	59.214068
2363.556111	107839.720054	59.219073
2362.734953	107624.046619	59.224077
2362.162332	107389.890160	59.229082
2361.658141	107156.784755	59.234087
2360.834650	106935.261254	59.239092
2360.518371	106699.021376	59.244097
2359.515019	106470.969896	59.249101
2358.651067	106243.050753	59.254106
2358.195134	106005.209183	59.259111
2357.678524	105773.394446	59.264116
2357.020348	105540.988957	59.269121
2356.360784	105314.454759	59.274125
2355.693685	105080.532439	59.279130
2354.993642	104847.620072	59.284135
2354.202781	104618.125022	59.289140
2353.537884	104387.159339	59.294145
2352.788298	104159.730447	59.299149
2351.930590	103930.588884	59.304154
2351.505549	103705.561785	59.309159
2350.510616	103479.307596	59.314164
2349.960697	103245.353043	59.319169
2349.295166	103042.352747	59.324173
2348.855976	102806.177258	59.329178
2348.328242	102556.182067	59.334183
2347.469078	102344.977724	59.339188
2346.884555	102102.659757	59.344193
2346.378188	101889.906432	59.349197
2345.514375	101658.808678	59.354202
2345.166513	101421.604959	59.359207
2344.499038	101195.891760	59.364212
2343.670539	100962.727294	59.369217
2343.129698	100742.041488	59.374221
2342.327563	100506.568400	59.379226
2341.654046	100266.839975	59.384231
2340.729431	100053.941362	59.389236
2340.489239	99805.363602	59.394241
2340.031204	99582.760050	59.399245
2338.982738	99354.391278	59.404250
2338.618825	99109.570334	59.409255
2337.530815	98890.352676	59.414260
2337.047500	98644.629538	59.419265
2336.350795	98428.176812	59.424269
2335.723661	98190.961657	59.429274
2335.065289	97955.314206	59.434279
2334.312269	97743.329431	59.439284
2333.937034	97501.901690	59.444289
2333.207341	97276.528439	59.449293
2332.805431	97039.162668	59.454298
2331.949967	96810.636418	59.459303
2331.512157	96576.262071	59.464308
2330.811661	96330.503115	59.469313
2330.374671	96110.568339	59.474317
2329.522925	95855.750204	59.479322
2328.878939	95628.464406	59.484327
2328.112557	95396.044290	59.489332
2327.413315	95145.287866	59.494337
2326.493547	94919.594017	59.499341
2326.204285	94676.476776	59.504346
2325.674898	94437.959913	59.509351
2324.829830	94205.057242	59.514356
2323.999381	93962.553561	59.519361
2323.491737	93728.727205	59.524365
2322.548047	93496.075845	59.529370
2322.316190	93257.530721	59.534375
2321.310037	93024.875157	59.539380
2320.189840	92783.229238	59.544385
2319.709736	92557.857297	59.549389
2318.784704	92326.451729	59.554394
2318.504458	92106.074824	59.559399
2317.731525	91881.193724	59.564404
2317.261240	91634.695204	59.569409
2316.471765	91411.070665	59.574413
2315.576597	91178.340801	59.579418
2315.370189	90951.420041	59.584423
2314.340031	90716.370409	59.589428
2314.269022	90491.170256	59.594433
2313.724705	90250.304023	59.599437
2312.833090	90022.258780	59.604442
2311.950188	89777.888115	59.609447
2311.180342	89545.897509	59.614452
2310.874581	89321.596204	59.619457
2310.120695	89082.988798	59.624461
2309.054145	88851.756384	59.629466
2308.833966	88614.388218	59.634471
2307.951532	88379.391024	59.639476
2307.449355	88138.668225	59.644481
2306.801677	87914.689247	59.649485
2306.059397	87674.840194	59.654490
2305.520074	87446.537857	59.659495
2304.672728	87215.459317	59.664500
2304.398811	86969.273961	59.669505
2303.264422	86745.016608	59.674509
2302.638411	86513.948534	59.679514
2302.023057	86279.901771	59.684519
2301.173172	86047.073855	59.689524
2300.850465	85809.645026	59.694529
2299.815201	85596.338091	59.699533
2299.485554	85355.016846	59.704538
2298.664447	85122.492370	59.709543
2297.709394	84887.969557	59.714548
2297.387180	84656.708561	59.719553
2296.804946	84425.180713	59.724557
2295.882158	84201.968735	59.729562
2295.788973	83955.263310	59.734567
2295.083321	83729.613189	59.739572
2294.374504	83495.605492	59.744577
2293.458687	83258.730212	59.749581
2292.713835	83029.823151	59.754586
2292.321636	82785.549341	59.759591
2291.043251	82557.169369	59.764596
2290.737741	82330.722847	59.769601
2289.974592	82091.339261	59.774605
2289.023854	81874.843019	59.779610
2288.748454	81636.629525	59.784615
2287.950179	81411.006282	59.789620
2287.386813	81184.194741	59.794625
2286.404116	80953.484743	59.799629
2286.103871	80723.473954	59.804634
2285.428417	80498.550920	59.809639
2284.776102	80267.403198	59.814644
2284.208408	80029.628325	59.819649
2283.660894	79798.887470	59.824653
2282.936023	79573.659086	59.829658
2282.394321	79336.002120	59.834663
2281.642714	79106.175893	59.839668
2280.861224	78868.993254	59.844673
2280.134640	78645.765105	59.849677
2279.503768	78416.022477	59.854682
2279.312407	78176.491928	59.859687
2278.392670	77945.761116	59.864692
2277.515887	77701.972402	59.869697
2277.149298	77477.907755	59.874701
2276.051635	77244.190468	59.879706
2275.323844	77005.924600	59.884711
2274.810707	76787.093048	59.889716
2274.397572	76547.718101	59.894721
2273.482519	76324.995012	59.899725
2272.756601	76089.559213	59.904730
2272.278057	75852.800668	59.909735
2271.264069	75630.240279	59.914740
2270.911259	75397.870686	59.919745
2270.507428	75165.106349	59.924750
2269.448683	74933.937485	59.929754
2269.062351	74722.920202	59.934759
2268.297987	74506.934497	59.939764
2267.554977	74270.508844	59.944769
2266.697190	74056.354787	59.949774
2265.959156	73811.779816	59.954778
2265.743388	73585.478790	59.959783
2264.721858	73378.200221	59.964788
2264.426380	73136.705639	59.969793
2263.806268	72901.467650	59.974798
2262.891845	72666.652879	59.979802
2262.185283	72433.961832	59.984807
2261.567929	72219.003734	59.989812
2261.084118	71980.289724	59.994817
2260.245679	71744.422162	59.999822
2259.499744	71523.796917	60.004826
2259.487592	71268.470158	60.009831
2258.510014	71039.176803	60.014836
2257.963969	70786.386098	60.019841
2257.265402	70549.782083	60.024846
2256.318239	70320.802620	60.029850
2255.883398	70088.761085	60.034855
2255.010365	69858.381678	60.039860
2254.379271	69617.945905	60.044865
2253.995747	69396.507819	60.049870
2252.941719	69160.325238	60.054874
2252.609093	68926.938375	60.059879
2251.801646	68691.837105	60.064884
2251.205184	68461.613902	60.069889
2250.878990	68226.638240	60.074894
2250.023269	68008.938957	60.079898
2249.593978	67771.666998	60.084903
2248.722959	67523.910019	60.089908
2248.218106	67284.603918	60.094913
2247.260441	67055.999952	60.099918
2246.324509	66824.551586	60.104922
2245.817907	66580.396809	60.109927
2245.066829	66351.439054	60.114932
2244.331606	66115.382141	60.119937
2243.798630	65886.772109	60.124942
2243.140207	65660.917327	60.129946
2242.533160	65419.874090	60.134951
2241.926279	65204.899435	60.139956
2241.107102	64962.014747	60.144961
2240.434015	64724.574985	60.149966
2239.653460	64510.268902	60.154970
2239.306510	64269.851078	60.159975
2238.141165	64038.418723	60.164980
2237.632807	63820.800180	60.169985
2236.916017	63584.461133	60.174990
2236.373932	63362.825864	60.179994
2235.744748	63130.331656	60.184999
2234.852721	62910.824565	60.190004
2234.240760	62667.283951	60.195009
2233.854217	62456.193029	60.200014
2232.751553	62220.087248	60.205018
2232.903295	62000.273159	60.210023
2231.612333	61770.721318	60.215028
2231.114693	61533.157339	60.220033
2230.503675	61318.293613	60.225038
2229.727749	61085.189268	60.230042
2229.013730	60848.497630	60.235047
2228.326836	60633.982959	60.240052
2227.767263	60401.333929	60.245057
2227.267653	60169.919157	60.250062
2226.305023	59947.877751	60.255066
2226.259166	59706.108845	60.260071
2224.983745	59489.462614	60.265076
2224.524333	59262.310158	60.270081
2224.021005	59038.434063	60.275086
2223.278881	58813.069683	60.280090
2222.767632	58578.029991	60.285095
2221.828363	58345.710449	60.290100
2221.330646	58107.718218	60.295105
2220.647778	57886.559017	60.300110
2219.944525	57657.458082	60.305114
2219.229921	57411.112131	60.310119
2218.339303	57194.070746	60.315124
2217.965975	56960.558343	60.320129
2217.415231	56738.426556	60.325134
2216.444346	56504.603249	60.330138
2215.853617	56281.059092	60.335143
2215.013218	56057.497115	60.340148
2214.458011	55824.616586	60.345153
2214.051918	55600.687445	60.350158
2213.393456	55377.699843	60.355162
2212.943002	55140.194036	60.360167
2211.885379	54915.721504	60.365172
2211.038632	54688.673932	60.370177
2210.590661	54466.841251	60.375182
2209.797468	54235.705353	60.380186
2209.412759	54006.966390	60.385191
2208.154515	53781.504823	60.390196
2207.733797	53553.473437	60.395201
2207.230242	53324.442284	60.400206
2206.124103	53108.429551	60.405210
2205.751492	52877.668189	60.410215
2205.099913	52668.135505	60.415220
2204.523301	52445.227706	60.420225
2203.892382	52215.677007	60.425230
2203.033207	51995.660993	60.430234
2202.654440	51761.095716	60.435239
2202.224198	51536.261623	60.440244
2201.318602	51315.207634	60.445249
2200.500811	51090.136834	60.450254
2199.842819	50869.080685	60.455258
2199.545564	50626.892148	60.460263
2198.704928	50403.266814	60.465268
2198.017750	50185.741909	60.470273
2197.270635	49957.586203	60.475278
2196.656533	49740.827070	60.480282
2195.795594	49511.049967	60.485287
2195.085031	49279.515118	60.490292
2194.290648	49061.011688	60.495297
2193.911315	48835.504205	60.500302
2192.749587	48626.899938	60.505306
2192.406063	48396.618547	60.510311
2191.445505	48185.073968	60.515316
2190.851149	47979.781688	60.520321
2190.157298	47758.671644	60.525326
2189.536123	47540.798424	60.530330
2188.946359	47315.416370	60.535335
2188.105768	47116.275176	60.540340
2187.413694	46901.268022	60.545345
2186.513521	46683.462274	60.550350
2185.887998	46475.968659	60.555354
2185.312192	46259.527460	60.560359
2184.865201	46044.542482	60.565364
2184.156656	45830.104546	60.570369
2183.258554	45627.987566	60.575374
2182.652107	45413.538518	60.580378
2182.379214	45196.527813	60.585383
2181.596185	44979.129449	60.590388
2180.496323	44770.285786	60.595393
2180.051484	44558.336036	60.600398
2179.189462	44352.325145	60.605402
2178.878854	44146.140654	60.610407
2178.133169	43932.936846	60.615412
2177.810674	43728.489174	60.620417
2177.111257	43512.819455	60.625422
2176.210744	43310.065518	60.630426
2175.681061	43079.554377	60.635431
2175.094929	42876.973839	60.640436
2174.087419	42653.530137	60.645441
2173.942102	42444.256197	60.650446
2172.852608	42237.980718	60.655450
2172.511785	42021.260693	60.660455
2171.633166	41804.802626	60.665460
2171.219317	41592.295954	60.670465
2170.496319	41375.483385	60.675470
2169.600646	41168.611253	60.680474
2168.970803	40952.171861	60.685479
2168.325616	40738.950336	60.690484
2167.677717	40524.837020	60.695489
2166.955898	40316.293800	60.700494
2166.038838	40112.444877	60.705498
2165.491537	39898.072048	60.710503
2164.756382	39683.461361	60.715508
2164.189309	39484.032194	60.720513
2163.518112	39275.831941	60.725518
2162.534691	39073.030376	60.730522
2162.205628	38854.206327	60.735527
2161.414492	38670.608924	60.740532
2160.292392	38458.833639	60.745537
2159.867323	38249.005487	60.750542
2158.948855	38042.372393	60.755546
2158.340516	37855.431937	60.760551
2157.712450	37665.831486	60.765556
2157.028487	37468.900997	60.770561
2156.334709	37260.553539	60.775566
2155.556835	37070.076183	60.780570
2154.878997	36872.024617	60.785575
2154.079842	36683.756906	60.790580
2153.392704	36494.175800	60.795585
2153.177059	36302.010377	60.800590
2152.022781	36115.327515	60.805594
2150.978181	35923.994974	60.810599
2150.356941	35732.256038	60.815604
2149.575894	35547.903797	60.820609
2148.510154	35364.847387	60.825614
2147.531345	35201.583367	60.830618
2146.843671	35032.908861	60.835623
2145.848276	34868.504837	60.840628
2144.899674	34704.577056	60.845633
2144.355267	34546.715858	60.850638
2143.173446	34404.400013	60.855642
2142.562328	34263.121703	60.860647
2141.711961	34125.038685	60.865652
2140.918444	33979.074103	60.870657
2140.233117	33829.441300	60.875662
2139.048982	33702.585097	60.880666
2138.725640	33557.851860	60.885671
2138.001797	33418.397074	60.890676
2137.005786	33295.100000	60.895681
2136.546628	33164.618155	60.900686
2135.720273	33046.553833	60.905690
2135.385313	32907.547344	60.910695
2134.648405	32793.552610	60.915700
2133.672071	32653.629123	60.920705
2133.321181	32533.133630	60.925710
2132.303931	32413.909402	60.930714
2131.973850	32283.799592	60.935719
2131.090166	32161.888500	60.940724
2130.280517	32039.223847	60.945729
2129.725344	31912.180417	60.950734
2129.138200	31795.400234	60.955738
2128.496334	31668.276040	60.960743
2127.734248	31561.826637	60.965748
2127.080931	31432.662882	60.970753
2126.445240	31314.351546	60.975758
2125.810834	31209.745603	60.980762
2125.256578	31083.221962	60.985767
2124.609230	30961.309107	60.990772
2123.922078	30850.263690	60.995777
2123.460910	30727.916932	61.000782
2122.621087	30609.116873	61.005786
2122.398835	30482.161212	61.010791
2121.798802	30372.448280	61.015796
2120.905482	30242.093165	61.020801
2120.446168	30118.834207	61.025806
2119.175375	30016.547331	61.030810
2118.772943	29874.082033	61.035815
2118.003991	29759.979064	61.040820
2117.334329	29641.893726	61.045825
2116.755897	29521.397904	61.050830
2116.113697	29408.026199	61.055834
2115.628425	29284.700218	61.060839
2114.684732	29176.914196	61.065844
2114.239906	29058.653620	61.070849
2114.107865	28939.612758	61.075854
2113.245127	28830.598041	61.080858
2112.652094	28703.468529	61.085863
2112.114697	28589.047874	61.090868
2111.276157	28463.417444	61.095873
2110.472532	28328.077207	61.100878
2109.832151	28215.132174	61.105882
2109.282512	28094.248936	61.110887
2108.582157	27973.305197	61.115892
2107.911869	27854.999079	61.120897
2107.592108	27729.396277	61.125902
2106.477125	27618.399632	61.130906
2105.907481	27500.315522	61.135911
2105.027247	27375.970281	61.140916
2104.454560	27268.766797	61.145921
2104.218689	27141.232642	61.150926
2103.271492	27019.491584	61.155930
2102.845641	26898.832994	61.160935
2102.126623	26788.703361	61.165940
2101.148131	26669.973768	61.170945
2100.693659	26539.501260	61.175950
2099.875775	26433.383247	61.180954
2099.326089	26308.263154	61.185959
2098.778734	26197.136440	61.190964
2098.311772	26085.605187	61.195969
2097.394651	25959.037523	61.200974
2096.665480	25846.820518	61.205978
2095.944249	25721.327810	61.210983
2095.409554	25615.447474	61.215988
2094.767109	25498.245703	61.220993
2094.330482	25371.436610	61.225998
2093.627647	25256.889636	61.231002
2092.606315	25139.347017	61.236007
2092.102277	25013.947785	61.241012
2091.288823	24898.702219	61.246017
2090.983726	24780.368585	61.251022
2090.126961	24662.554571	61.256026
2089.420784	24545.598899	61.261031
2088.545280	24430.540292	61.266036
2087.829591	24317.373868	61.271041
2087.722734	24204.665246	61.276046
2086.677895	24093.406156	61.281050
2086.086324	23972.403309	61.286055
2085.535613	23847.684774	61.291060
2085.025574	23737.681884	61.296065
2084.034400	23619.606265	61.301070
2083.304800	23512.541168	61.306074
2082.921775	23396.562928	61.311079
2082.114234	23273.705944	61.316084
2081.488704	23164.146241	61.321089
2081.041774	23042.392294	61.326094
2080.187443	22923.500962	61.331098
2079.418502	22817.891887	61.336103
2079.065512	22698.972430	61.341108
2078.526743	22581.239403	61.346113
2077.609029	22466.436196	61.351118
2076.693040	22350.281667	61.356122
2076.389453	22229.098700	61.361127
2075.302160	22119.746601	61.366132
2074.602815	22008.839714	61.371137
2074.079974	21898.286984	61.376142
2072.855049	21795.414954	61.381146
2072.596361	21686.303118	61.386151
2072.281503	21565.323627	61.391156
2071.436387	21461.342530	61.396161
2070.850024	21346.954406	61.401166
2070.135379	21233.620255	61.406170
2069.468313	21119.523731	61.411175
2068.714037	21013.069236	61.416180
2067.723791	20915.683300	61.421185
2067.532146	20793.847681	61.426190
2066.778272	20684.926346	61.431194
2066.116874	20579.161965	61.436199
2065.598671	20471.025065	61.441204
2064.941207	20362.436486	61.446209
2064.473562	20249.022841	61.451214
2063.609323	20138.438702	61.456218
2063.186078	20019.068916	61.461223
2062.463110	19909.656162	61.466228
2061.678043	19794.869487	61.471233
2061.189424	19681.349968	61.476238
2060.353141	19569.733104	61.481242
2059.715538	19455.495141	61.486247
2058.907798	19339.430476	61.491252
2058.215645	19227.157238	61.496257
2057.593726	19116.073284	61.501262
2056.605089	19022.015469	61.506266
2056.118720	18913.875948	61.511271
2055.527078	18796.344957	61.516276
2054.579301	18694.824493	61.521281
2054.298047	18581.814894	61.526286
2053.393058	18483.039102	61.531290
2052.537386	18373.355381	61.536295
2051.989187	18266.344457	61.541300
2051.485402	18165.231830	61.546305
2050.967277	18058.325319	61.551310
2049.837030	17950.587915	61.556314
2049.541786	17844.406536	61.561319
2048.824643	17748.811039	61.566324
2047.867686	17646.892303	61.571329
2047.268682	17541.828872	61.576334
2046.605298	17446.118159	61.581338
2046.152700	17336.915746	61.586343
2045.033379	17239.587375	61.591348
2044.547790	17141.599764	61.596353
2043.945450	17034.110163	61.601358
2043.083675	16941.280160	61.606362
2042.440493	16834.384141	61.611367
2041.796731	16754.018399	61.616372
2040.893022	16653.440250	61.621377
2040.576355	16546.605106	61.626382
2039.590197	16470.886664	61.631386
2038.857476	16372.085894	61.636391
2037.996292	16275.911763	61.641396
2037.290578	16179.988839	61.646401
2036.923976	16083.779644	61.651406
2036.065544	16003.469822	61.656410
2035.399807	15912.042383	61.661415
2034.805566	15820.496002	61.666420
2033.775775	15737.776743	61.671425
2033.278877	15639.481148	61.676430
2032.461259	15568.671999	61.681434
2031.682547	15483.954604	61.686439
2031.021703	15401.409865	61.691444
2030.348770	15321.550299	61.696449
2029.726322	15246.511623	61.701454
2029.017095	15164.739666	61.706458
2028.149207	15080.699964	61.711463
2027.745196	15002.437926	61.716468
2027.073679	14924.837726	61.721473
2026.765100	14843.958321	61.726478
2025.584244	14763.195967	61.731482
2024.987284	14682.722489	61.736487
2024.364898	14596.371325	61.741492
2023.664468	14525.707907	61.746497
2023.375190	14436.235960	61.751502
2022.258746	14367.372979	61.756506
2021.084532	14293.493778	61.761511
2020.900691	14223.769466	61.766516
2020.128136	14146.715063	61.771521
2019.934608	14067.280582	61.776526
2019.249418	13997.953047	61.781530
2018.508351	13919.483947	61.786535
2017.953945	13840.877033	61.791540
2017.272703	13776.839810	61.796545
2016.859921	13681.278996	61.801550
2016.045822	13607.797873	61.806554
2015.186211	13521.358316	61.811559
2014.615867	13446.910094	61.816564
2013.892429	13372.416195	61.821569
2013.220582	13291.676509	61.826574
2012.365543	13228.354776	61.831578
2012.021800	13155.162530	61.836583
2011.129310	13079.183828	61.841588
2010.216499	13001.487019	61.846593
2010.049319	12925.305879	61.851598
2009.118277	12855.231300	61.856602
2008.816449	12782.330126	61.861607
2008.169939	12702.638333	61.866612
2006.958409	12628.586273	61.871617
2006.663909	12553.346168	61.876622
2005.955610	12468.488861	61.881626
2005.557761	12400.388766	61.886631
2004.909387	12324.796779	61.891636
2003.834472	12253.905888	61.896641
2003.447528	12168.042621	61.901646
2002.631060	12103.282630	61.906650
2001.888762	12030.579048	61.911655
2001.635680	11951.382217	61.916660
2000.652862	11876.057420	61.921665
1999.870360	11804.256951	61.926670
1999.298023	11731.057910	61.931674
1998.978227	11651.028489	61.936679
1998.333675	11577.201686	61.941684
1997.421309	11503.968735	61.946689
1996.834228	11420.611922	61.951694
1995.894570	11354.357842	61.956698
1994.981706	11281.905270	61.961703
1994.646193	11208.199685	61.966708
1993.935125	11143.897748	61.971713
1993.390716	11072.819087	61.976718
1992.674130	11011.885574	61.981722
1992.361748	10937.533157	61.986727
1991.541296	10868.286707	61.991732
1990.759152	10795.403233	61.996737
1990.008533	10709.151238	62.001742
1989.374560	10641.872936	62.006746
1988.759737	10574.345711	62.011751
1987.856896	10498.663549	62.016756
1987.344039	10432.339850	62.021761
1986.472446	10363.097914	62.026766
1985.806580	10298.527872	62.031770
1985.306390	10219.276335	62.036775
1984.617464	10157.141169	62.041780
1983.927095	10093.447967	62.046785
1983.500763	10014.841855	62.051790
1982.407313	9944.792011	62.056794
1981.728949	9884.810308	62.061799
1981.439279	9802.972716	62.066804
1980.657483	9743.410782	62.071809
1980.178229	9661.228482	62.076814
1979.229068	9600.801709	62.081818
1978.680372	9535.065585	62.086823
1978.301206	9465.050567	62.091828
1977.141285	9403.874963	62.096833
1977.073856	9320.433050	62.101838
1976.114857	9261.191103	62.106842
1975.339709	9194.731041	62.111847
1974.997456	9121.317975	62.116852
1973.977276	9058.519982	62.121857
1973.357154	8979.753969	62.126862
1972.817630	8918.915409	62.131866
1972.255314	8850.100777	62.136871
1971.679417	8777.485454	62.141876
1970.713206	8719.853498	62.146881
1970.333342	8644.055838	62.151886
1969.850614	8572.826706	62.156890
1968.851777	8513.386150	62.161895
1968.326992	8440.871639	62.166900
1967.382412	8369.882061	62.171905
1966.675392	8295.298613	62.176910
1965.921965	8237.898636	62.181914
1965.188769	8173.605597	62.186919
1964.739638	8105.889587	62.191924
1963.928342	8043.664641	62.196929
1963.486648	7970.937647	62.201934
1962.806223	7907.352526	62.206938
1961.919646	7845.436590	62.211943
1961.458605	7780.778984	62.216948
1960.762252	7710.086844	62.221953
1960.583884	7651.603432	62.226958
1959.344019	7591.146102	62.231962
1958.892554	7517.619769	62.236967
1958.319482	7454.568996	62.241972
1957.282457	7387.485208	62.246977
1956.763452	7316.289114	62.251982
1955.938381	7257.509144	62.256986
1955.390856	7200.776653	62.261991
1954.984740	7139.201148	62.266996
1954.131748	7077.109913	62.272001
1953.668023	6995.936093	62.277006
1952.918820	6937.874250	62.282010
1952.122540	6874.263405	62.287015
1951.570561	6813.054369	62.292020
1950.746539	6748.359061	62.297025
1950.414895	6679.606941	62.302030
1949.873061	6626.790773	62.307034
1948.902466	6564.168156	62.312039
1948.555185	6485.987263	62.317044
1947.464612	6428.897431	62.322049
1947.234639	6367.376039	62.327054
1946.734528	6298.243019	62.332058
1945.558015	6230.125622	62.337063
1945.210129	6156.001891	62.342068
1944.311813	6093.925901	62.347073
1943.988484	6034.478721	62.352078
1943.299598	5960.118235	62.357082
1942.319649	5898.616074	62.362087
1941.770823	5828.318444	62.367092
1940.661721	5765.636782	62.372097
1940.112304	5695.619897	62.377102
1939.513029	5641.148054	62.382106
1938.941959	5588.946009	62.387111
1938.526834	5520.475955	62.392116
1937.722416	5454.954160	62.397121
1937.186198	5392.459214	62.402126
1936.359670	5331.074670	62.407130
1935.925079	5267.109622	62.412135
1934.846376	5193.443511	62.417140
1934.171879	5140.480952	62.422145
1933.838086	5073.179257	62.427150
1933.221327	5017.116035	62.432154
1932.451549	4949.158454	62.437159
1931.982850	4880.020749	62.442164
1931.004276	4827.812722	62.447169
1930.572508	4756.474648	62.452174
1929.539329	4692.646540	62.457178
1928.902205	4634.972662	62.462183
1928.446000	4580.047422	62.467188
1927.439775	4525.402935	62.472193
1927.279179	4467.570461	62.477198
1926.662107	4408.904429	62.482202
1925.822368	4333.265204	62.487207
1925.269123	4270.396752	62.492212
1924.202551	4202.854899	62.497217
1923.925105	4150.838472	62.502222
1923.208910	4083.646154	62.507226
1922.665026	4020.361634	62.512231
1921.694532	3960.390611	62.517236
1920.775141	3901.744619	62.522241
1920.544085	3838.819764	62.527246
1919.694233	3773.564241	62.532250
1918.867286	3717.980202	62.537255
1918.485745	3653.721117	62.542260
1917.736439	3606.746286	62.547265
1916.959835	3544.896721	62.552270
1916.182418	3490.534441	62.557274
1915.539463	3428.047407	62.562279
1915.225512	3371.379264	62.567284
1914.140564	3327.428739	62.572289
1913.648212	3257.363095	62.577294
1913.113437	3195.960848	62.582298
1912.053894	3149.788323	62.587303
1911.743002	3089.123867	62.592308
1910.928273	3030.726574	62.597313
1910.219341	2980.759140	62.602318
1909.766145	2917.627432	62.607322
1909.340143	2863.285823	62.612327
1908.562997	2804.207600	62.617332
1907.816232	2744.720221	62.622337
1907.234140	2680.061905	62.627342
1906.670815	2624.465397	62.632346
1905.627314	2568.435876	62.637351
1905.292154	2508.948780	62.642356
1904.411800	2457.564011	62.647361
1903.517127	2403.515380	62.652366
1903.016307	2351.340473	62.657370
1902.221004	2292.960388	62.662375
1901.801590	2234.924632	62.667380
1900.968755	2184.684647	62.672385
1900.518953	2128.957652	62.677390
1899.678199	2073.232211	62.682394
1898.775807	2015.306333	62.687399
1898.607453	1965.542021	62.692404
1897.799810	1910.278005	62.697409
1896.977806	1848.664404	62.702414
1896.535411	1797.981302	62.707418
1895.532083	1743.687399	62.712423
1895.067687	1686.358857	62.717428
1894.320820	1631.516813	62.722433
1893.718126	1581.296782	62.727438
1893.068769	1533.051816	62.732442
1892.161790	1490.266948	62.737447
1892.016587	1426.059755	62.742452
1890.770770	1376.839127	62.747457
1890.324725	1315.474056	62.752462
1889.676412	1276.918798	62.757466
1889.024254	1226.076210	62.762471
1888.219703	1168.716175	62.767476
1887.801206	1129.978939	62.772481
1887.077880	1075.144716	62.777486
1886.280696	1019.136457	62.782490
1885.649002	970.426100	62.787495
1884.951169	910.721580	62.792500
1884.182655	871.896298	62.797505
1883.536443	813.959761	62.802510
1883.151709	765.948948	62.807514
1882.309728	724.120389	62.812519
1881.878922	674.073332	62.817524
1880.675527	623.194992	62.822529
1879.935083	586.857744	62.827534
1879.539999	536.427001	62.832538
1878.787477	494.660600	62.837543
1878.310363	451.070135	62.842548
1877.677350	410.040399	62.847553
1876.855052	355.308189	62.852558
1876.233935	316.255982	62.857562
1875.127901	275.369537	62.862567
1874.688880	226.560910	62.867572
1873.743587	195.784552	62.872577
1873.195219	154.604902	62.877582
1872.380271	121.264321	62.882586
1871.325263	85.575953	62.887591
1870.926437	50.225049	62.892596
1869.924250	21.355204	62.897601
1869.695624	-20.109681	62.902606
1869.026945	-47.020121	62.907610
1868.153603	-84.302842	62.912615
1867.410021	-107.034933	62.917620
1866.241723	-129.686941	62.922625
1865.541653	-167.107345	62.927630
1864.697899	-180.470480	62.932634
1863.874079	-180.927816	62.937639
1862.472987	-191.266163	62.942644
1855.303736	-7.901748	62.947649
1853.018125	81.533707	62.952654
1854.705014	110.478028	62.957658
1856.765536	132.406985	62.962663
1858.443050	125.026925	62.967668
1859.398605	135.255029	62.972673
1859.548647	122.878726	62.977678
1859.284531	100.232620	62.982682
1858.596262	81.839207	62.987687
1858.210320	57.632372	62.992692
1856.646058	59.732177	62.997697
1855.085004	48.878154	63.002702
1853.967612	54.185553	63.007706
1852.797283	55.390170	63.012711
1852.633058	53.188043	63.017716
1851.852266	61.971287	63.022721
1851.285479	60.074353	63.027726
1850.878845	49.760878	63.032730
1849.707264	54.772525	63.037735
1849.643853	51.611358	63.042740
1848.444681	57.218755	63.047745
1847.972233	57.314341	63.052750
1847.466287	62.571974	63.057754
1847.028533	66.320649	63.062759
1846.790819	57.424865	63.067764
1845.919183	62.112922	63.072769
1845.115832	61.409477	63.077774
1844.423671	57.761501	63.082778
1843.033355	71.353548	63.087783
1842.721196	63.461503	63.092788
1841.613132	61.026028	63.097793
1841.503870	69.879278	63.102798
1841.204869	75.783738	63.107802
1840.015023	76.109927	63.112807
1839.887824	65.297905	63.117812
1838.762230	76.965012	63.122817
1838.006008	76.115311	63.127822
1838.210008	75.638284	63.132826
1837.520007	80.010499	63.137831
1836.996449	73.284289	63.142836
1835.565260	77.712684	63.147841
1835.291323	78.760790	63.152846
1834.883396	81.716243	63.157850
1833.853110	84.563929	63.162855
1833.371029	74.970486	63.167860
1832.378464	79.389164	63.172865
1831.660314	82.110018	63.177870
1830.982403	78.828792	63.182874
1830.200390	83.392241	63.187879
1829.602591	86.144449	63.192884
1828.839406	79.678641	63.197889
1828.662344	84.477203	63.202894
1828.808664	78.945641	63.207898
1827.576019	87.441098	63.212903
1826.537474	79.773195	63.217908
1825.551733	88.910706	63.222913
1825.571902	79.661723	63.227918
1825.282158	90.325632	63.232922
1824.032448	79.132007	63.237927
1823.746908	84.679514	63.242932
1822.693415	77.845058	63.247937
1822.087995	84.697056	63.252942
1821.436254	84.297557	63.257946
1820.780181	82.346994	63.262951
1819.870658	86.597949	63.267956
1819.451224	93.316340	63.272961
1818.594976	91.798115	63.277966
1817.987252	82.808105	63.282970
1817.309127	88.064705	63.287975
1816.971318	89.771096	63.292980
1816.195198	86.770400	63.297985
1815.155957	94.643787	63.302990
1815.117461	88.726821	63.307994
1814.080789	86.475563	63.312999
1813.647853	80.580230	63.318004
1813.065320	86.532871	63.323009
1812.551797	89.714834	63.328014
1811.704125	85.257330	63.333018
1810.822649	87.687149	63.338023
1810.290648	82.036209	63.343028
1809.344719	87.220214	63.348033
1808.737610	87.348229	63.353038
1808.334976	83.647976	63.358042
1807.122545	92.376781	63.363047
1807.093804	88.541462	63.368052
1806.242854	92.221716	63.373057
1805.500628	93.527115	63.378062
1805.118287	95.934453	63.383066
1804.127128	87.274994	63.388071
1803.476793	84.243291	63.393076
1803.309034	97.472511	63.398081
1802.470823	99.368752	63.403086
1801.964706	84.518309	63.408090
1801.102153	87.714694	63.413095
1800.794064	81.288597	63.418100
1800.206816	88.842627	63.423105
1799.618741	86.414484	63.428110
1798.923298	88.694917	63.433114
1797.512980	94.539307	63.438119
1796.711539	86.977270	63.443124
1796.444475	91.460536	63.448129
1795.933371	91.067097	63.453134
1795.035710	81.328336	63.458138
1794.580115	96.738495	63.463143
1794.047690	89.947464	63.468148
1792.776455	96.171902	63.473153
1792.124658	91.061968	63.478158
1792.241703	87.373815	63.483162
1791.045967	94.112977	63.488167
1790.330978	87.358823	63.493172
1789.958730	85.148729	63.498177
1789.222469	94.401181	63.503182
1788.623238	85.841924	63.508186
1787.762244	86.172688	63.513191
1787.157518	97.812309	63.518196
1786.681898	95.527164	63.523201
1786.030846	92.451422	63.528206
1785.796184	94.696536	63.533210
1785.012004	102.288155	63.538215
1784.658732	96.320247	63.543220
1783.471991	102.635355	63.548225
1782.022518	104.975606	63.553230
1782.314974	100.217208	63.558234
1780.966597	103.607448	63.563239
1780.683566	98.614000	63.568244
1780.148524	100.236597	63.573249
1779.029520	105.115358	63.578254
1778.540308	99.115419	63.583258
1777.831107	100.543317	63.588263
1777.344529	93.055867	63.593268
1776.928393	102.454614	63.598273
1775.918735	100.268468	63.603278
1775.893237	95.276705	63.608282
1774.939287	99.219335	63.613287
1774.713564	96.687923	63.618292
1774.181945	98.152279	63.623297
1772.715497	101.381496	63.628302
1771.676486	93.772034	63.633306
1770.898652	96.234296	63.638311
1770.946664	106.593840	63.643316
1770.238809	101.044947	63.648321
1769.365998	103.840844	63.653326
1769.074432	101.824523	63.658330
1768.224982	97.326312	63.663335
1767.698063	88.585262	63.668340
1767.365967	104.283329	63.673345
1766.748381	93.710026	63.678350
1765.692314	95.778072	63.683354
1764.307049	104.105406	63.688359
1763.584277	97.484960	63.693364
1764.057032	97.906707	63.698369
1763.370308	100.345041	63.703374
1762.491297	90.123924	63.708378
1761.627952	95.501416	63.713383
1760.974046	90.681991	63.718388
1760.514431	96.736552	63.723393
1759.901492	97.269211	63.728398
1758.964802	92.075217	63.733402
1758.031763	96.963875	63.738407
1757.278314	93.800321	63.743412
1756.846986	97.588997	63.748417
1756.193952	98.347225	63.753422
1755.623429	94.566407	63.758426
1755.097150	93.664443	63.763431
1754.875076	91.268076	63.768436
1754.073060	87.435712	63.773441
1753.596769	100.688696	63.778446
1752.465210	101.806776	63.783450
1751.561520	101.614466	63.788455
1750.598638	100.608371	63.793460
1750.206786	95.174886	63.798465
1749.558244	95.413575	63.803470
1749.092646	86.869379	63.808474
1748.330606	95.545604	63.813479
1747.567521	96.449047	63.818484
1747.541346	91.244502	63.823489
1746.676220	89.469087	63.828494
1746.481491	86.857062	63.833498
1745.079916	96.456462	63.838503
1744.203544	93.642024	63.843508
1743.762446	89.823309	63.848513
1742.775214	99.574533	63.853518
1742.596085	92.058766	63.858522
1741.828708	97.638647	63.863527
1741.339458	93.761346	63.868532
1740.925401	86.432705	63.873537
1740.112463	91.778542	63.878542
1738.920285	92.529356	63.883546
1737.916725	95.863275	63.888551
1738.071232	87.777275	63.893556
1737.469684	89.295321	63.898561
1736.449748	93.115975	63.903566
1736.047780	89.961265	63.908570
1735.492303	95.335603	63.913575
1735.040662	94.423367	63.918580
1734.322327	93.788456	63.923585
1732.678632	100.937837	63.928590
1732.131549	87.371279	63.933594
1731.479644	92.205833	63.938599
1731.569845	92.918570	63.943604
1731.164115	96.108660	63.948609
1730.120610	105.748977	63.953614
1729.927108	94.447579	63.958618
1728.855394	88.177462	63.963623
1727.910447	95.176446	63.968628
1726.985511	86.842404	63.973633
1726.425920	97.878764	63.978638
1725.848941	91.577384	63.983642
1725.182005	96.136779	63.988647
1724.980090	95.719480	63.993652
1724.377925	98.879267	63.998657
1723.718632	103.727616	64.003662
1723.140203	102.759822	64.008666
1721.568089	97.751916	64.013671
1721.206792	95.443897	64.018676
1720.514269	90.752045	64.023681
1719.906062	98.725743	64.028686
1719.728978	87.532134	64.033690
1719.064219	101.318110	64.038695
1718.795927	97.891431	64.043700
1717.694038	87.543304	64.048705
1716.566502	94.225930	64.053710
1716.067249	86.913980	64.058714
1715.325754	97.799456	64.063719
1714.785010	92.203543	64.068724
1714.297422	88.444259	64.073729
1713.620810	90.896767	64.078734
1713.035642	93.336329	64.083738
1711.673068	96.128024	64.088743
1711.371356	85.949287	64.093748
1710.736274	91.020874	64.098753
1709.895124	93.814912	64.103758
1709.664007	93.370713	64.108762
1708.970491	97.131649	64.113767
1708.739168	92.010153	64.118772
1708.349714	96.221122	64.123777
1706.969354	98.572513	64.128782
1706.244727	90.209819	64.133786
1705.414380	97.892365	64.138791
1705.257158	87.832608	64.143796
1704.519157	89.763425	64.148801
1702.977075	91.976497	64.153806
1702.694358	84.868284	64.158810
1701.944195	91.519363	64.163815
1701.498453	94.308950	64.168820
1701.177917	90.221932	64.173825
1700.609222	103.346092	64.178830
1700.196220	92.726127	64.183834
1699.335434	98.533747	64.188839
1698.520782	99.342890	64.193844
1697.747506	95.496517	64.198849
1696.657180	99.695804	64.203854
1696.244847	94.943686	64.208858
1695.835523	95.619065	64.213863
1695.291689	101.056218	64.218868
1694.654215	101.122848	64.223873
1693.260282	98.657143	64.228878
1693.134762	99.859890	64.233882
1692.196076	100.844857	64.238887
1691.843072	98.563910	64.243892
1691.108003	100.522652	64.248897
1690.347796	100.645048	64.253902
1690.176464	96.392403	64.258906
1688.879145	94.852814	64.263911
1687.919062	97.104344	64.268916
1687.405322	95.049205	64.273921
1687.076027	96.793684	64.278926
1686.609884	89.385017	64.283930
1685.900307	98.931302	64.288935
1685.541807	93.770083	64.293940
1684.648349	101.172496	64.298945
1683.858093	100.082236	64.303950
1683.248734	96.933667	64.308954
1682.255927	102.030542	64.313959
1681.779396	95.412015	64.318964
1681.582317	92.128576	64.323969
1680.805315	105.295287	64.328974
1679.902153	97.498707	64.333978
1678.874242	99.045064	64.338983
1678.251511	103.086507	64.343988
1678.052841	104.717197	64.348993
1677.250510	97.645785	64.353998
1677.209450	88.811820	64.359002
1676.114117	92.723320	64.364007
1675.241456	89.291719	64.369012
1674.774820	93.294173	64.374017
1674.113245	95.703301	64.379022
1673.914689	94.673604	64.384026
1672.460272	93.070665	64.389031
1671.690855	94.195913	64.394036
1671.179517	89.213519	64.399041
1670.269105	97.484389	64.404046
1670.141328	86.541583	64.409050
1669.606916	107.169888	64.414055
1668.698443	98.169341	64.419060
1667.895017	85.974498	64.424065
1666.928886	96.977665	64.429070
1666.354246	95.607153	64.434074
1665.704140	104.402817	64.439079
1665.010269	95.297222	64.444084
1664.912027	89.517493	64.449089
1664.330362	97.554793	64.454094
1663.838703	85.252082	64.459098
1662.807340	87.213738	64.464103
1662.013157	98.492375	64.469108
1661.472068	91.854146	64.474113
1660.856822	100.264219	64.479118
1660.705181	95.549549	64.484122
1659.296283	98.167276	64.489127
1658.198405	96.160775	64.494132
1657.879659	89.507731	64.499137
1656.875014	100.330938	64.504142
1657.056363	93.242057	64.509146
1656.479222	90.730211	64.514151
1656.253803	88.645051	64.519156
1655.022276	90.808820	64.524161
1653.766151	97.199653	64.529166
1653.423359	95.183601	64.534170
1652.923600	93.340719	64.539175
1652.164190	91.313574	64.544180
1651.866284	94.898138	64.549185
1650.763788	94.985029	64.554190
1650.098512	90.069672	64.559194
1649.614615	96.645351	64.564199
1648.820696	98.279132	64.569204
1648.301727	94.378187	64.574209
1647.255342	93.071577	64.579214
1646.565365	88.806707	64.584218
1645.732111	92.055257	64.589223
1645.196463	94.731398	64.594228
1645.011908	85.022931	64.599233
1644.255594	90.843930	64.604238
1644.032287	81.222047	64.609242
1643.745130	94.118551	64.614247
1642.309940	93.163869	64.619252
1641.462002	91.254871	64.624257
1640.852922	94.193417	64.629262
1640.673999	92.178145	64.634266
1640.016017	94.993571	64.639271
1638.784790	95.667052	64.644276
1638.141800	82.640902	64.649281
1637.515341	94.470072	64.654286
1637.228490	85.093252	64.659290
1636.637294	90.276155	64.664295
1635.631728	96.480534	64.669300
1634.619214	87.652658	64.674305
1633.388002	96.480708	64.679310
1633.438548	92.320560	64.684314
1632.716176	92.334459	64.689319
1632.607686	94.633658	64.694324
1632.429028	89.112716	64.699329
1631.522828	92.618867	64.704334
1630.480806	89.876518	64.709338
1629.694392	95.889965	64.714343
1629.102861	92.896277	64.719348
1628.592785	91.846684	64.724353
1627.970743	100.163222	64.729358
1626.930865	88.597325	64.734362
1626.166692	91.500586	64.739367
1625.716160	95.667649	64.744372
1625.331836	83.089277	64.749377
1624.642059	86.165226	64.754382
1623.889412	84.720499	64.759386
1622.557669	93.216008	64.764391
1621.963842	90.005065	64.769396
1621.553209	84.251314	64.774401
1620.838261	91.816195	64.779406
1620.756132	92.228291	64.784410
1620.228098	88.499109	64.789415
1619.679482	97.247114	64.794420
1618.664326	86.356974	64.799425
1617.672231	95.416707	64.804430
1617.476486	91.492809	64.809434
1617.022419	97.937595	64.814439
1616.076692	95.378654	64.819444
1615.301997	93.109516	64.824449
1614.383705	97.016570	64.829454
1614.134635	92.203841	64.834458
1613.520064	94.283811	64.839463
1612.136401	90.547052	64.844468
1611.820096	88.460566	64.849473
1610.886600	90.493429	64.854478
1610.790304	90.554532	64.859482
1610.219934	92.408281	64.864487
1609.800642	91.721168	64.869492
1608.468623	86.490692	64.874497
1607.463796	95.615529	64.879502
1607.082621	91.437234	64.884506
1606.737803	88.918455	64.889511
1606.136386	95.435537	64.894516
1605.720843	88.461984	64.899521
1604.535197	92.853068	64.904526
1603.592695	91.143613	64.909530
1603.532497	90.143982	64.914535
1602.922738	85.002198	64.919540
1602.586291	82.286546	64.924545
1600.908136	84.063968	64.929550
1600.710103	83.018425	64.934554
1599.804450	85.376456	64.939559
1599.450406	87.511235	64.944564
1599.191838	82.788331	64.949569
1597.715156	91.751584	64.954574
1597.433164	93.841801	64.959578
1596.783365	82.065717	64.964583
1596.042844	98.010008	64.969588
1595.985886	79.634698	64.974593
1594.620760	87.974669	64.979598
1593.538724	84.538515	64.984602
1593.091409	88.973156	64.989607
1592.656122	88.279125	64.994612
1592.258725	89.411525	64.999617
1591.731394	93.505636	65.004622
1591.060973	89.944164	65.009626
1590.306828	94.153158	65.014631
1589.077731	93.493776	65.019636
1589.218358	83.758890	65.024641
1588.160609	94.089067	65.029646
1587.659005	84.164471	65.034650
1586.669862	89.697615	65.039655
1585.877139	91.916283	65.044660
1585.703454	87.679796	65.049665
1584.689904	97.168733	65.054670
1584.422768	86.763754	65.059674
1583.874087	88.334936	65.064679
1582.756494	85.278180	65.069684
1582.197359	87.112802	65.074689
1581.613662	94.368252	65.079694
1581.346775	92.324382	65.084698
1580.122625	93.637021	65.089703
1579.251604	91.723826	65.094708
1578.693229	85.569349	65.099713
1577.988295	95.116489	65.104718
1578.051210	91.514207	65.109722
1577.364452	87.865446	65.114727
1576.153490	93.561572	65.119732
1575.693292	87.050870	65.124737
1574.935833	93.286813	65.129742
1574.365194	90.777108	65.134746
1573.692099	90.767424	65.139751
1572.591446	90.218532	65.144756
1571.858711	92.060237	65.149761
1571.082820	93.836257	65.154766
1571.113779	93.762025	65.159770
1570.685220	93.574716	65.164775
1570.415426	95.965778	65.169780
1569.323734	88.735377	65.174785
1568.463058	93.066960	65.179790
1568.069745	86.865760	65.184794
1566.767987	89.364007	65.189799
1565.669944	93.045740	65.194804
1565.087480	88.560384	65.199809
1564.491494	95.839868	65.204814
1564.737783	90.549468	65.209818
1563.952511	89.143059	65.214823
1563.285963	93.002245	65.219828
1563.063817	92.416284	65.224833
1561.606354	98.380243	65.229838
1560.680733	97.081290	65.234842
1560.436642	97.336192	65.239847
1559.694696	90.163770	65.244852
1559.547733	90.370122	65.249857
1558.585102	94.675329	65.254862
1557.652897	90.914181	65.259866
1557.020593	82.204136	65.264871
1556.473595	88.242636	65.269876
1556.333445	99.325913	65.274881
1555.254964	100.916623	65.279886
1554.301581	96.239460	65.284890
1553.910912	97.312449	65.289895
1553.563031	94.642774	65.294900
1552.676665	98.148953	65.299905
1551.502417	103.386666	65.304910
1550.930846	91.834710	65.309914
1550.695925	95.674207	65.314919
1549.534731	93.001291	65.319924
1549.695985	88.109185	65.324929
1548.488094	98.232994	65.329934
1547.666657	93.167434	65.334938
1547.176832	94.286141	65.339943
1546.508056	91.042970	65.344948
1546.198873	91.475375	65.349953
1545.120030	93.107146	65.354958
1544.408502	87.962625	65.359962
1543.697507	96.972985	65.364967
1543.234938	98.576226	65.369972
1542.948979	90.009849	65.374977
1542.501338	97.671051	65.379982
1541.448516	87.966515	65.384986
1540.912266	93.389868	65.389991
1540.221204	93.417741	65.394996
1539.150456	87.215373	65.400001
1538.295353	98.336552	65.405006
1537.636680	93.562108	65.410010
1537.095215	90.081088	65.415015
1536.672497	96.777949	65.420020
1536.444245	86.808357	65.425025
1535.405291	91.685525	65.430030
1534.494289	94.670489	65.435034
1534.117866	85.459314	65.440039
1533.354152	91.533830	65.445044
1533.053560	80.862943	65.450049
1531.958132	95.308729	65.455054
1531.193076	92.837811	65.460058
1530.452756	85.925345	65.465063
1529.798152	88.128389	65.470068
1529.536074	78.944783	65.475073
1529.226105	83.116329	65.480078
1528.036881	89.524967	65.485082
1527.535537	78.906481	65.490087
1526.539033	85.002216	65.495092
1526.394370	85.515716	65.500097
1525.288244	81.346973	65.505102
1524.214705	85.777045	65.510106
1523.863296	81.084675	65.515111
1523.132140	82.158152	65.520116
1523.053654	81.498905	65.525121
1522.374355	90.009057	65.530126
1521.679061	90.353003	65.535130
1521.033220	86.817609	65.540135
1520.039515	85.001203	65.545140
1519.976814	89.094037	65.550145
1518.865449	89.199740	65.555150
1518.224297	91.042676	65.560154
1517.183135	85.133667	65.565159
1516.517828	89.935699	65.570164
1516.422091	83.636764	65.575169
1515.548508	91.179563	65.580174
1515.037397	89.819493	65.585178
1514.274771	94.398867	65.590183
1513.555295	93.428303	65.595188
1513.074435	90.488025	65.600193
1512.494239	90.995038	65.605198
1511.589773	90.528541	65.610202
1510.681679	86.222678	65.615207
1509.858293	93.785889	65.620212
1509.829942	80.736241	65.625217
1509.197196	86.107119	65.630222
1508.286291	79.228079	65.635226
1507.507189	88.260301	65.640231
1506.566990	90.264301	65.645236
1506.538924	78.652816	65.650241
1505.809394	89.236792	65.655246
1505.357722	93.208506	65.660250
1504.331848	86.710438	65.665255
1503.728503	91.811714	65.670260
1503.251853	85.037136	65.675265
1502.271274	82.837023	65.680270
1501.588232	84.082636	65.685274
1501.040679	83.802282	65.690279
1500.394403	92.906444	65.695284
1500.226747	90.288566	65.700289
1499.094814	88.766950	65.705294
1498.032102	87.059291	65.710298
1497.647543	76.614650	65.715303
1497.034251	84.991310	65.720308
1496.736415	72.132731	65.725313
1495.435138	81.117040	65.730318
1494.514167	87.752725	65.735322
1494.025408	85.040793	65.740327
1493.439298	87.770711	65.745332
1493.502248	77.207648	65.750337
1492.902601	89.860482	65.755342
1492.030607	91.475175	65.760346
1491.225298	83.650519	65.765351
1490.208595	81.479806	65.770356
1490.108341	83.299873	65.775361
1489.221366	96.424156	65.780366
1487.999453	85.573248	65.785370
1487.821560	84.158656	65.790375
1487.044321	98.012990	65.795380
1486.971560	85.594883	65.800385
1486.048743	90.750084	65.805390
1484.943196	87.424950	65.810394
1484.366694	89.361700	65.815399
1483.530504	89.764317	65.820404
1483.645310	80.374169	65.825409
1482.911541	91.326260	65.830414
1481.725227	83.939052	65.835418
1481.470520	84.283959	65.840423
1480.369099	92.829661	65.845428
1479.875044	85.755074	65.850433
1478.697568	79.967097	65.855438
1477.616918	81.370520	65.860442
1478.202799	82.781925	65.865447
1477.397596	83.638520	65.870452
1476.974946	90.499378	65.875457
1476.291550	87.479329	65.880462
1475.264908	92.431833	65.885466
1474.529380	83.063273	65.890471
1474.079596	88.684207	65.895476
1473.741082	82.710868	65.900481
1472.392036	85.268715	65.905486
1471.598903	90.937906	65.910490
1470.938397	85.670182	65.915495
1470.309269	86.442027	65.920500
1470.044757	79.870294	65.925505
1469.760858	85.852803	65.930510
1469.038821	87.858416	65.935514
1467.908312	89.537853	65.940519
1467.100300	86.017208	65.945524
1466.892865	86.417683	65.950529
1466.274861	84.066923	65.955534
1465.179985	89.725720	65.960538
1464.548225	77.081064	65.965543
1464.223577	86.263426	65.970548
1463.714225	81.894216	65.975553
1462.457584	85.997012	65.980558
1461.469026	89.459532	65.985562
1461.131625	83.091774	65.990567
1460.572519	85.601361	65.995572
1460.429756	81.468788	66.000577
1460.056240	91.202976	66.005582
1458.988001	89.589254	66.010586
1457.882313	81.191020	66.015591
1457.004841	75.856858	66.020596
1457.195746	76.965170	66.025601
1456.178498	90.938070	66.030606
1455.064699	87.388754	66.035610
1454.546886	82.185093	66.040615
1453.901281	84.982821	66.045620
1453.898487	79.951206	66.050625
1453.457778	88.738847	66.055630
1452.328152	87.399815	66.060634
1451.558330	80.340679	66.065639
1450.899166	82.525542	66.070644
1450.289534	77.561984	66.075649
1449.296441	73.698596	66.080654
1448.691076	86.571540	66.085658
1448.518709	78.726739	66.090663
1447.614353	91.167804	66.095668
1446.672399	82.101724	66.100673
1445.704192	86.040415	66.105678
1445.546088	85.242434	66.110682
1445.210402	77.579711	66.115687
1444.735953	77.111130	66.120692
1443.787819	73.078171	66.125697
1442.616851	75.946779	66.130702
1442.115875	80.804709	66.135706
1442.034834	70.381236	66.140711
1440.957131	78.953136	66.145716
1440.128397	80.901596	66.150721
1439.420618	80.216206	66.155726
1438.794400	78.035496	66.160730
1438.275383	77.238104	66.165735
1437.821094	83.629321	66.170740
1436.655843	82.892056	66.175745
1436.175855	83.386313	66.180750
1435.496064	81.431740	66.185754
1435.341887	75.946363	66.190759
1434.619299	87.770327	66.195764
1433.799107	82.438107	66.200769
1433.076390	80.143423	66.205774
1432.429581	84.914145	66.210778
1431.708041	82.715469	66.215783
1430.457090	88.588321	66.220788
1429.664401	83.349504	66.225793
1429.663441	77.407684	66.230798
1428.865417	82.749649	66.235802
1428.725803	81.368403	66.240807
1428.113723	82.126510	66.245812
1427.588920	74.585314	66.250817
1426.321543	79.244926	66.255822
1425.769893	86.856430	66.260826
1425.316744	78.502740	66.265831
1423.936944	92.232069	66.270836
1423.715752	79.941649	66.275841
1422.882147	80.082096	66.280846
1422.423243	86.067190	66.285850
1422.301121	78.742694	66.290855
1421.238819	81.642928	66.295860
1420.118491	80.926916	66.300865
1419.627883	81.403940	66.305870
1419.274109	75.086106	66.310874
1418.877906	79.500026	66.315879
1417.619771	85.840809	66.320884
1417.111994	79.339289	66.325889
1416.543331	77.909540	66.330894
1416.225944	73.763726	66.335898
1415.184300	79.059258	66.340903
1413.820867	78.724092	66.345908
1413.760754	78.341052	66.350913
1413.213124	72.462468	66.355918
1412.901812	76.560117	66.360922
1412.278352	74.114044	66.365927
1410.897331	85.523836	66.370932
1410.410921	75.330376	66.375937
1409.931142	77.510391	66.380942
1409.418156	85.793850	66.385946
1408.607588	72.950555	66.390951
1407.416963	78.019028	66.395956
1407.091899	78.685788	66.400961
1406.406616	79.658964	66.405966
1406.104355	93.103493	66.410970
1405.962403	79.732869	66.415975
1404.434018	76.025544	66.420980
1403.934668	82.357693	66.425985
1403.402016	76.260684	66.430990
1402.787371	86.050543	66.435994
1401.786873	80.212400	66.440999
1401.004053	87.037468	66.446004
1400.371429	79.253214	66.451009
1399.926477	86.623831	66.456014
1399.733943	82.653719	66.461018
1398.942159	76.303003	66.466023
1397.867902	83.882455	66.471028
1397.584627	80.417206	66.476033
1397.218178	82.180235	66.481038
1396.166078	82.981479	66.486042
1395.314500	83.824970	66.491047
1394.673817	83.930031	66.496052
1394.153893	81.016491	66.501057
1392.809607	85.598457	66.506062
1392.178431	89.996114	66.511066
1392.195150	78.440605	66.516071
1391.712111	86.274599	66.521076
1391.229288	76.973143	66.526081
1390.329105	84.884479	66.531086
1389.147390	81.043211	66.536090
1388.724997	86.038472	66.541095
1388.113692	84.016256	66.546100
1387.743565	88.897554	66.551105
1386.444440	90.520247	66.556110
1385.503395	93.147329	66.561114
1385.352344	89.236856	66.566119
1384.917765	81.583555	66.571124
1384.599736	89.102736	66.576129
1383.752999	92.055456	66.581134
1382.395720	91.569515	66.586138
1382.115236	80.810310	66.591143
1381.420333	91.560695	66.596148
1381.347860	85.023107	66.601153
1380.273106	90.442190	66.606158
1379.061401	80.493335	66.611162
1379.043820	73.590631	66.616167
1378.378342	85.850230	66.621172
1377.611280	87.049305	66.626177
1376.765834	89.976589	66.631182
1375.953477	86.354163	66.636186
1375.695691	67.995071	66.641191
1375.098063	82.688193	66.646196
1373.975647	78.217757	66.651201
1372.856514	80.614525	66.656206
1372.128963	87.359851	66.661210
1372.219503	87.839126	66.666215
1371.716557	87.340395	66.671220
1371.863173	81.917599	66.676225
1370.976771	85.941084	66.681230
1369.896399	91.275908	66.686234
1369.132603	90.708253	66.691239
1367.807258	90.606757	66.696244
1366.842897	90.152986	66.701249
1366.585074	84.947444	66.706254
1366.069459	86.866655	66.711258
1365.818110	81.816206	66.716263
1365.226032	90.028664	66.721268
1365.048877	92.088043	66.726273
1364.068238	94.536920	66.731278
1363.120726	83.532082	66.736282
1362.648367	89.028882	66.741287
1361.198035	97.868212	66.746292
1360.710426	87.263359	66.751297
1360.313287	82.135159	66.756302
1359.883555	87.175746	66.761306
1359.420136	83.501014	66.766311
1358.396748	94.756212	66.771316
1357.280609	81.598802	66.776321
1357.161885	87.889378	66.781326
1356.732058	82.506174	66.786330
1356.201689	90.025994	66.791335
1354.970508	93.716357	66.796340
1354.320826	80.344449	66.801345
1353.976321	83.885977	66.806350
1352.935344	84.502542	66.811354
1352.269539	80.013148	66.816359
1351.845456	84.623900	66.821364
1350.976453	82.393496	66.826369
1350.656257	83.349652	66.831374
1349.785459	81.982140	66.836378
1349.153772	85.575628	66.841383
1348.227071	90.496518	66.846388
1348.141302	82.346225	66.851393
1347.449397	82.579291	66.856398
1346.190098	79.191931	66.861402
1345.660695	80.329580	66.866407
1345.490864	81.287066	66.871412
1344.636890	79.374402	66.876417
1343.698183	77.011577	66.881422
1342.587715	79.711336	66.886426
1342.289489	83.508863	66.891431
1341.739410	88.609585	66.896436
1341.558139	76.409035	66.901441
1341.098135	77.608194	66.906446
1339.945915	83.227263	66.911450
1339.156865	79.467105	66.916455
1338.495564	93.769811	66.921460
1338.154786	88.610576	66.926465
1337.279747	85.072247	66.931470
1336.405651	85.714329	66.936474
1336.008081	76.987548	66.941479
1335.524854	86.638252	66.946484
1334.289827	81.490289	66.951489
1333.747609	74.103278	66.956494
1332.666390	83.017978	66.961498
1332.590418	74.353617	66.966503
1332.194719	80.856957	66.971508
1331.586611	78.093070	66.976513
1331.042824	84.925887	66.981518
1329.758769	76.325840	66.986522
1329.443295	74.557814	66.991527
1328.709871	80.580249	66.996532
1328.000921	72.554263	67.001537
1327.677991	73.996564	67.006542
1326.597502	71.295160	67.011546
1326.421392	64.375087	67.016551
1325.299960	78.913357	67.021556
1324.097887	77.491283	67.026561
1323.931405	70.301592	67.031566
1323.315521	79.997037	67.036570
1322.830990	84.221581	67.041575
1322.265769	88.107288	67.046580
1321.391195	83.390891	67.051585
1320.568669	78.857036	67.056590
1319.494672	75.112222	67.061594
1319.660855	72.324596	67.066599
1319.186199	85.875371	67.071604
1317.849096	79.404794	67.076609
1317.344828	72.489579	67.081614
1316.598451	78.318530	67.086618
1316.370230	74.453452	67.091623
1315.780783	75.879777	67.096628
1314.495061	80.595972	67.101633
1314.223795	79.103198	67.106638
1313.129906	83.170725	67.111642
1313.057367	73.055005	67.116647
1312.138936	82.604583	67.121652
1311.326677	84.375418	67.126657
1310.727038	81.362605	67.131662
1310.141460	78.828534	67.136666
1310.116580	74.912207	67.141671
1308.683065	82.730154	67.146676
1307.806895	79.937926	67.151681
1307.687778	77.552052	67.156686
1307.044332	84.933733	67.161690
1306.649308	72.475436	67.166695
1305.531416	78.152138	67.171700
1304.734760	78.740918	67.176705
1304.569058	75.384727	67.181710
1303.667969	84.251876	67.186714
1302.682292	78.799357	67.191719
1302.038340	80.138155	67.196724
1301.501293	72.572134	67.201729
1301.441763	73.868482	67.206734
1300.219678	86.274931	67.211738
1299.603120	81.590064	67.216743
1299.248570	88.728696	67.221748
1298.350498	89.965968	67.226753
1297.469287	78.731425	67.231758
1296.656248	86.168456	67.236762
1296.198492	72.360784	67.241767
1295.646751	82.736750	67.246772
1295.256812	78.179862	67.251777
1294.597378	78.761022	67.256782
1293.341933	80.203348	67.261786
1292.971401	78.604931	67.266791
1292.316213	77.745639	67.271796
1291.975591	75.008624	67.276801
1290.993399	77.465656	67.281806
1289.941499	78.536574	67.286810
1289.597372	72.408047	67.291815
1289.209443	72.917657	67.296820
1288.708650	80.803367	67.301825
1287.981455	67.751332	67.306830
1287.018463	76.002264	67.311834
1286.623215	68.946722	67.316839
1285.604248	77.406830	67.321844
1284.692181	80.071915	67.326849
1284.181873	72.533188	67.331854
1283.353023	82.265652	67.336858
1283.339804	74.997981	67.341863
1282.691888	84.342130	67.346868
1282.128943	81.910125	67.351873
1281.297856	82.606890	67.356878
1280.639959	85.313569	67.361882
1279.786146	74.418462	67.366887
1278.761923	75.361979	67.371892
1278.026924	81.056665	67.376897
1277.734285	73.483332	67.381902
1277.315735	88.710974	67.386906
1276.961979	71.089421	67.391911
1276.057685	75.746566	67.396916
1275.085873	86.906848	67.401921
1274.568750	77.927850	67.406926
1274.164053	84.621863	67.411930
1273.189337	75.316647	67.416935
1272.366979	75.931601	67.421940
1271.667696	82.306593	67.426945
1271.524128	74.711136	67.431950
1270.308854	78.430543	67.436954
1269.534756	68.158291	67.441959
1268.897441	79.576049	67.446964
1268.313449	77.391825	67.451969
1268.182394	74.481144	67.456974
1267.688956	75.688784	67.461978
1266.721635	74.532193	67.466983
1265.930410	75.310935	67.471988
1265.366579	73.702256	67.476993
1265.080842	69.396894	67.481998
1263.745166	79.582110	67.487002
1262.896763	70.599021	67.492007
1262.630694	81.912023	67.497012
1262.115675	84.744225	67.502017
1261.566961	72.072255	67.507022
1260.110821	75.102978	67.512026
1259.865347	73.259176	67.517031
1259.113522	76.603698	67.522036
1258.633906	81.798884	67.527041
1258.368266	72.568594	67.532046
1257.424875	79.416068	67.537050
1256.826352	75.682417	67.542055
1256.121313	81.563158	67.547060
1255.244699	81.805117	67.552065
1254.302912	75.057256	67.557070
1253.511713	74.657999	67.562074
1253.528174	69.700609	67.567079
1253.078809	67.654259	67.572084
1252.474254	73.088507	67.577089
1251.786610	70.062896	67.582094
1250.894756	80.995998	67.587098
1250.447781	70.365807	67.592103
1248.901779	67.285865	67.597108
1248.130449	77.879677	67.602113
1248.028587	70.574065	67.607118
1247.583240	86.725340	67.612122
1247.368934	76.875022	67.617127
1246.467810	69.552992	67.622132
1245.367475	74.227124	67.627137
1245.006122	67.620371	67.632142
1244.114533	75.727496	67.637146
1243.213525	70.125925	67.642151
1242.440206	72.586033	67.647156
1242.128927	73.465088	67.652161
1241.609965	73.055664	67.657166
1241.038132	75.009067	67.662170
1240.221208	75.760363	67.667175
1239.383721	66.002835	67.672180
1238.835734	69.158829	67.677185
1238.389614	62.267511	67.682190
1237.523500	70.400546	67.687194
1236.935352	64.758695	67.692199
1236.088082	76.695547	67.697204
1235.620101	71.843572	67.702209
1235.141154	76.144510	67.707214
1233.963363	68.946903	67.712218
1233.342944	71.176117	67.717223
1232.811449	72.389815	67.722228
1232.495546	78.442075	67.727233
1232.087609	65.970089	67.732238
1230.689741	70.727807	67.737242
1230.078029	71.601018	67.742247
1229.480504	63.423314	67.747252
1229.285144	70.932449	67.752257
1228.613405	66.991250	67.757262
1227.448701	69.277050	67.762266
1227.281390	62.278323	67.767271
1226.312247	64.301211	67.772276
1225.501189	67.487999	67.777281
1225.058183	63.406351	67.782286
1224.245333	68.075777	67.787290
1223.735856	68.940618	67.792295
1222.849394	66.373991	67.797300
1221.804959	72.450632	67.802305
1221.712894	68.988123	67.807310
1220.825856	71.043690	67.812314
1220.431945	71.576339	67.817319
1220.186751	66.304163	67.822324
1218.884361	68.984025	67.827329
1218.809617	59.802245	67.832334
1217.760790	63.250773	67.837338
1217.157842	59.636113	67.842343
1216.147775	74.024234	67.847348
1215.219578	68.225146	67.852353
1214.800989	65.752859	67.857358
1214.470134	67.779911	67.862362
1214.155659	66.754497	67.867367
1213.128574	67.160748	67.872372
1212.096057	69.589539	67.877377
1211.711800	67.346761	67.882382
1211.369767	70.153038	67.887386
1210.788151	70.948928	67.892391
1209.677422	72.514939	67.897396
1208.862457	77.413369	67.902401
1208.925580	64.554244	67.907406
1207.739637	73.149736	67.912410
1206.926786	68.023024	67.917415
1206.299002	67.910036	67.922420
1205.825356	76.766004	67.927425
1205.482471	70.936923	67.932430
1204.818362	73.018548	67.937434
1203.967395	66.595320	67.942439
1203.341794	66.926691	67.947444
1202.805592	64.252334	67.952449
1201.868782	68.528311	67.957454
1200.642608	74.126075	67.962458
1200.489149	64.220367	67.967463
1199.972746	70.736600	67.972468
1199.405265	76.300583	67.977473
1198.600204	75.610230	67.982478
1197.923169	80.537193	67.987482
1197.372586	74.190778	67.992487
1196.885138	69.805538	67.997492
1195.428606	75.063041	68.002497
1195.049163	63.108515	68.007502
1194.279017	68.621145	68.012506
1194.045550	71.142074	68.017511
1193.801981	74.670719	68.022516
1192.731650	78.649387	68.027521
1191.862127	71.230890	68.032526
1191.756696	73.750382	68.037530
1190.672822	67.186000	68.042535
1189.558111	76.270073	68.047540
1188.726440	69.351766	68.052545
1188.945764	65.399767	68.057550
1188.376904	67.524596	68.062554
1187.864312	57.142990	68.067559
1186.690644	61.707375	68.072564
1186.082819	75.011237	68.077569
1185.389704	65.224467	68.082574
1184.449629	72.758992	68.087578
1183.755115	63.238954	68.092583
1183.577037	64.552578	68.097588
1182.919793	69.444853	68.102593
1182.264452	67.106418	68.107598
1180.978734	71.168227	68.112602
1180.501684	70.387870	68.117607
1180.296167	72.249913	68.122612
1179.397837	79.375676	68.127617
1178.909130	57.721240	68.132622
1177.647388	72.750218	68.137626
1177.099594	74.732926	68.142631
1176.986655	66.886608	68.147636
1176.315624	74.685859	68.152641
1175.990133	64.992018	68.157646
1174.985949	69.665077	68.162650
1174.484562	72.842057	68.167655
1173.403265	64.440104	68.172660
1172.030315	62.785081	68.177665
1171.718822	67.332210	68.182670
1170.977863	66.735753	68.187674
1170.853601	67.350106	68.192679
1170.512877	64.592629	68.197684
1169.922260	78.038839	68.202689
1169.036429	65.704376	68.207694
1168.123202	79.348552	68.212698
1167.475196	70.352559	68.217703
1167.155587	69.805789	68.222708
1165.866741	73.221546	68.227713
1165.275023	74.066362	68.232718
1164.609985	73.490949	68.237722
1164.179846	71.961958	68.242727
1164.091927	66.007182	68.247732
1162.968813	71.356756	68.252737
1162.826366	69.696857	68.257742
1161.630683	66.906614	68.262746
1160.711767	68.106245	68.267751
1160.013889	63.863294	68.272756
1159.118515	74.787510	68.277761
1159.210466	71.056040	68.282766
1158.866112	70.733983	68.287770
1157.731129	77.347025	68.292775
1157.074000	71.058569	68.297780
1156.396878	72.689684	68.302785
1155.777953	65.091000	68.307790
1154.489553	64.879660	68.312794
1153.688038	75.987649	68.317799
1153.441693	72.637992	68.322804
1152.737183	70.417772	68.327809
1152.499274	66.098515	68.332814
1152.447439	75.098716	68.337818
1151.348524	71.894114	68.342823
1150.581197	77.226534	68.347828
1149.673555	72.020299	68.352833
1148.924376	66.028765	68.357838
1147.895297	72.664390	68.362842
1147.044208	75.652562	68.367847
1146.926032	70.185151	68.372852
1146.556928	71.980172	68.377857
1146.468014	65.684930	68.382862
1144.959912	80.877689	68.387866
1144.576572	76.901685	68.392871
1144.086843	69.416497	68.397876
1142.892111	75.993314	68.402881
1142.284982	65.528980	68.407886
1141.303415	78.562705	68.412890
1140.883038	79.132691	68.417895
1140.825175	72.411457	68.422900
1139.999297	73.314021	68.427905
1139.246679	73.854846	68.432910
1138.251612	80.027746	68.437914
1138.122581	71.751900	68.442919
1137.085593	62.521318	68.447924
1136.037491	70.763749	68.452929
1135.617149	63.224953	68.457934
1135.079943	74.894887	68.462938
1134.628290	68.188978	68.467943
1134.174959	66.513870	68.472948
1132.774007	71.199586	68.477953
1132.439257	73.205190	68.482958
1131.984090	71.214980	68.487962
1131.389286	73.845424	68.492967
1130.490212	65.789829	68.497972
1129.634844	77.907765	68.502977
1129.033333	70.826717	68.507982
1128.722616	65.019346	68.512986
1128.049748	71.598321	68.517991
1127.402901	71.694968	68.522996
1126.337434	75.904702	68.528001
1125.968932	65.061794	68.533006
1125.375037	67.595899	68.538010
1124.643341	70.114074	68.543015
1123.979571	68.530787	68.548020
1123.130223	75.937358	68.553025
1123.026500	66.624576	68.558030
1122.000397	77.115428	68.563034
1120.985703	82.138692	68.568039
1120.771067	71.846902	68.573044
1119.914108	69.685633	68.578049
1119.686621	69.546845	68.583054
1118.377896	76.397273	68.588058
1117.643185	77.946094	68.593063
1117.299673	70.289422	68.598068
1117.001250	82.558479	68.603073
1116.281875	75.174478	68.608078
1115.165872	77.162419	68.613082
1114.840494	75.596274	68.618087
1114.545308	67.432018	68.623092
1113.152713	70.315515	68.628097
1112.038312	63.079510	68.633102
1111.667873	69.522074	68.638106
1111.213308	71.072070	68.643111
1111.036260	64.749849	68.648116
1110.383694	70.522921	68.653121
1109.836442	66.487842	68.658126
1109.022576	76.807743	68.663130
1108.357472	83.571576	68.668135
1107.221633	80.912189	68.673140
1106.389588	84.003003	68.678145
1106.400988	71.781322	68.683150
1105.670710	71.057028	68.688154
1104.623787	68.545930	68.693159
1103.890433	68.148558	68.698164
1103.153951	75.601838	68.703169
1102.985399	68.228004	68.708174
1102.214002	68.940562	68.713178
1101.435826	69.368768	68.718183
1100.725098	67.023395	68.723188
1099.910703	76.982257	68.728193
1099.930875	63.273683	68.733198
1098.811889	73.085447	68.738202
1097.874656	73.458528	68.743207
1097.537257	61.584076	68.748212
1097.148144	70.904426	68.753217
1096.310842	65.273861	68.758222
1095.297874	68.584267	68.763226
1094.615103	71.769610	68.768231
1094.175507	66.876886	68.773236
1093.726917	70.023403	68.778241
1093.541882	68.381322	68.783246
1092.064845	72.774806	68.788250
1091.542017	74.091232	68.793255
1091.461809	56.525597	68.798260
1090.091048	70.165286	68.803265
1089.380044	66.462191	68.808270
1088.612992	71.266296	68.813274
1088.255291	76.519382	68.818279
1087.822930	71.258073	68.823284
1086.770390	66.276766	68.828289
1086.278576	67.228711	68.833294
1085.682391	69.137132	68.838298
1085.125234	67.831790	68.843303
1084.638168	67.190242	68.848308
1083.500868	77.597867	68.853313
1082.884122	69.674003	68.858318
1082.445662	72.435707	68.863322
1081.565498	62.921585	68.868327
1080.876945	62.543902	68.873332
1080.160020	80.930355	68.878337
1079.511708	71.776744	68.883342
1079.270662	68.673839	68.888346
1078.549525	67.361467	68.893351
1077.997286	58.025424	68.898356
1076.748184	70.176033	68.903361
1076.324154	62.907500	68.908366
1075.792026	71.570928	68.913370
1074.661339	68.961202	68.918375
1074.128343	67.767139	68.923380
1073.495068	65.691732	68.928385
1073.410073	60.987037	68.933390
1072.984978	62.802012	68.938394
1071.889935	71.449326	68.943399
1070.987019	59.857232	68.948404
1070.423283	64.881312	68.953409
1069.995255	61.213636	68.958414
1069.039877	63.281700	68.963418
1068.334666	67.735347	68.968423
1067.824312	59.605333	68.973428
1067.256824	70.332328	68.978433
1066.414276	58.014690	68.983438
1065.232029	63.446246	68.988442
1064.463213	69.259896	68.993447
1064.326098	63.401267	68.998452
1063.821866	66.515638	69.003457
1063.753917	62.705527	69.008462
1062.844834	58.053078	69.013466
1062.013927	69.134216	69.018471
1061.804611	60.241949	69.023476
1060.257613	59.955098	69.028481
1059.889629	56.049213	69.033486
1059.250346	67.524072	69.038490
1058.586779	64.239223	69.043495
1058.433661	66.485601	69.048500
1056.855963	69.911088	69.053505
1056.676844	60.621352	69.058510
1056.043180	65.467324	69.063514
1055.303408	63.997072	69.068519
1054.233263	59.974226	69.073524
1053.588240	60.307147	69.078529
1053.406024	64.412668	69.083534
1052.831599	64.620816	69.088538
1051.965057	66.428748	69.093543
1051.103111	68.735848	69.098548
1050.450585	68.656797	69.103553
1050.086291	66.033977	69.108558
1049.644546	68.337310	69.113562
1048.505316	67.812131	69.118567
1048.167109	61.074008	69.123572
1047.051188	68.728007	69.128577
1046.969744	66.743019	69.133582
1045.714380	68.302144	69.138586
1045.017749	68.629084	69.143591
1044.847482	64.584513	69.148596
1044.055909	75.235198	69.153601
1043.583206	61.743815	69.158606
1042.447020	70.966969	69.163610
1041.848506	66.749249	69.168615
1041.523928	56.154852	69.173620
1041.203199	73.888486	69.178625
1040.132563	64.562379	69.183630
1039.855064	69.592971	69.188634
1038.796331	64.606365	69.193639
1037.578670	68.152783	69.198644
1036.580890	66.482307	69.203649
1036.679759	67.058015	69.208654
1036.063521	63.647370	69.213658
1035.508832	71.324056	69.218663
1035.362256	62.454927	69.223668
1033.937548	71.711369	69.228673
1033.283150	73.348362	69.233678
1032.813793	72.232493	69.238682
1032.232640	69.100121	69.243687
1032.111598	61.294538	69.248692
1030.614891	72.251368	69.253697
1030.015865	65.160498	69.258702
1029.598974	73.996412	69.263706
1028.779842	70.640124	69.268711
1027.947717	60.892878	69.273716
1027.180052	73.345388	69.278721
1026.914687	69.344333	69.283726
1026.632172	73.320733	69.288730
1025.373924	69.589600	69.293735
1024.645339	66.942737	69.298740
1023.731422	68.758214	69.303745
1023.492439	68.266447	69.308750
1023.327294	69.541752	69.313754
1022.781172	72.386825	69.318759
1022.176974	62.005650	69.323764
1020.581197	68.602160	69.328769
1019.532853	64.862869	69.333774
1019.144646	70.027770	69.338778
1018.438138	73.101790	69.343783
1018.365047	62.833240	69.348788
1018.019947	77.207084	69.353793
1017.540895	66.020667	69.358798
1016.615598	72.108386	69.363802
1015.763738	71.261534	69.368807
1015.488386	69.386245	69.373812
1014.364489	72.130850	69.378817
1013.739557	62.793774	69.383822
1013.104988	62.473754	69.388826
1011.966222	67.906301	69.393831
1011.176555	61.665791	69.398836
1010.475776	76.611888	69.403841
1010.178548	63.810118	69.408846
1009.735665	64.304857	69.413850
1009.391548	73.495050	69.418855
1009.076556	58.428431	69.423860
1007.675340	66.646655	69.428865
1007.419789	70.808002	69.433870
1006.600520	69.719423	69.438874
1005.416526	77.319616	69.443879
1004.495020	67.851527	69.448884
1004.132589	77.489342	69.453889
1003.955187	69.429372	69.458894
1003.614625	68.288287	69.463898
1002.005308	71.504370	69.468903
1001.730351	60.999856	69.473908
1001.007508	66.604355	69.478913
1000.701663	69.994682	69.483918
999.486546	69.566756	69.488922
998.721349	72.304761	69.493927
998.518629	62.880016	69.498932
997.782412	67.042142	69.503937
997.240767	66.980157	69.508942
996.296313	63.181770	69.513946
995.745699	63.677881	69.518951
995.558225	64.687079	69.523956
994.847887	71.261003	69.528961
993.709934	74.444673	69.533966
993.063675	68.381626	69.538970
992.340799	67.274562	69.543975
992.505117	60.525883	69.548980
991.144991	73.790182	69.553985
990.460510	64.192926	69.558990
989.907764	59.263037	69.563994
989.263914	63.235425	69.568999
988.442537	60.535529	69.574004
987.357131	69.857856	69.579009
986.820097	65.354401	69.584014
986.456446	62.009240	69.589018
986.187616	70.206581	69.594023
985.484280	63.138629	69.599028
984.254773	69.815658	69.604033
983.689829	66.642873	69.609038
983.365671	64.933051	69.614042
983.007948	75.590413	69.619047
982.502611	65.302331	69.624052
981.404232	72.622402	69.629057
980.941542	63.532338	69.634062
979.698032	69.757431	69.639066
978.813769	71.166079	69.644071
978.503844	61.567583	69.649076
977.649753	70.660720	69.654081
977.436418	59.364233	69.659086
976.836896	67.030711	69.664090
975.828607	70.767774	69.669095
975.369889	61.896280	69.674100
974.884176	70.337865	69.679105
974.330095	61.317540	69.684110
973.525409	57.050644	69.689114
972.360098	62.219343	69.694119
972.123288	64.155763	69.699124
971.328038	67.338531	69.704129
970.481139	70.568941	69.709134
970.157985	57.452765	69.714138
969.435631	70.011614	69.719143
968.952639	56.980795	69.724148
967.670419	65.530189	69.729153
967.283849	57.259083	69.734158
967.005234	60.473189	69.739162
966.167520	70.930952	69.744167
965.860824	61.448641	69.749172
964.426769	66.073474	69.754177
964.172975	70.174618	69.759182
963.808213	66.741327	69.764186
962.719322	71.700752	69.769191
961.970984	56.028160	69.774196
961.277132	59.606383	69.779201
960.885224	68.760024	69.784206
960.251336	63.428310	69.789210
959.060034	70.901947	69.794215
958.730795	59.598674	69.799220
958.063757	70.989654	69.804225
957.688497	65.484323	69.809230
957.406890	66.432807	69.814234
955.842292	77.184434	69.819239
955.312319	68.994490	69.824244
954.712001	66.838177	69.829249
954.430456	68.942567	69.834254
953.560279	68.492894	69.839258
952.560635	76.765523	69.844263
952.006869	62.438661	69.849268
951.425437	61.480992	69.854273
951.325209	56.387647	69.859278
950.529046	62.375985	69.864282
949.218116	73.095134	69.869287
949.008230	64.089434	69.874292
948.491979	66.180708	69.879297
947.507733	62.970573	69.884302
946.825612	76.193239	69.889306
946.118256	75.518961	69.894311
945.921060	64.051174	69.899316
945.017377	69.140408	69.904321
943.839696	75.413391	69.909326
943.510503	72.163678	69.914330
942.680606	66.024212	69.919335
942.753888	65.545843	69.924340
941.948003	62.753611	69.929345
940.828980	65.216770	69.934350
940.231591	68.647186	69.939354
939.608763	72.146305	69.944359
939.129641	63.962470	69.949364
937.668223	69.501581	69.954369
937.319758	65.064328	69.959374
937.193817	61.088412	69.964378
936.521995	68.089883	69.969383
936.413524	62.471141	69.974388
935.542860	68.515496	69.979393
934.585058	66.337225	69.984398
933.603934	66.614847	69.989402
932.123566	69.922417	69.994407
932.125995	63.219999	69.999412
931.119503	69.066771	70.004417
930.787394	70.281916	70.009422
930.848053	60.373724	70.014426
930.201181	65.612909	70.019431
929.701639	68.559397	70.024436
928.805193	70.290126	70.029441
927.850126	75.207770	70.034446
927.128871	67.814679	70.039450
925.922748	69.624649	70.044455
925.907223	65.301576	70.049460
925.106548	62.830222	70.054465
924.815477	60.842328	70.059470
923.811874	66.116204	70.064474
923.333735	73.280826	70.069479
922.738886	64.908828	70.074484
921.799305	71.869333	70.079489
920.949817	65.204710	70.084494
920.525546	62.749154	70.089498
919.832256	68.270120	70.094503
919.483132	60.556042	70.099508
918.498370	72.090629	70.104513
917.482106	68.071887	70.109518
917.284945	58.475963	70.114522
916.767659	65.416574	70.119527
916.178299	65.526204	70.124532
915.258988	71.625616	70.129537
914.399245	61.322992	70.134542
914.302076	63.428008	70.139546
913.040394	78.848156	70.144551
912.323520	62.451476	70.149556
911.910665	68.180132	70.154561
911.427563	69.275804	70.159566
910.721696	62.895839	70.164570
909.391549	66.687297	70.169575
908.894088	63.491178	70.174580
908.430573	72.774493	70.179585
908.266443	69.616791	70.184590
908.253148	60.056263	70.189594
906.817629	66.556370	70.194599
906.132014	66.135690	70.199604
905.222728	68.316328	70.204609
904.073605	61.609509	70.209614
903.373166	59.472298	70.214618
902.992669	69.573459	70.219623
902.575556	68.766273	70.224628
902.145469	65.901634	70.229633
901.751093	69.116822	70.234638
900.940796	62.821289	70.239642
899.897812	66.598593	70.244647
899.362462	65.020164	70.249652
899.026458	69.148587	70.254657
897.987257	70.938314	70.259662
897.461567	69.626431	70.264666
896.671382	65.779880	70.269671
896.372991	68.768480	70.274676
895.223260	74.262743	70.279681
894.552304	69.089913	70.284686
894.331580	62.984411	70.289690
893.465198	69.762962	70.294695
892.886870	62.612071	70.299700
891.955450	64.957085	70.304705
891.340495	72.364259	70.309710
890.934809	61.741802	70.314714
890.083323	72.660672	70.319719
889.045052	67.557338	70.324724
888.530031	65.641359	70.329729
887.877089	72.929999	70.334734
887.890139	57.580973	70.339738
887.136978	69.066093	70.344743
886.220974	66.723492	70.349748
885.536157	69.590663	70.354753
884.704657	68.267527	70.359758
884.519018	69.825224	70.364762
883.375302	68.214306	70.369767
883.008001	62.747149	70.374772
882.370508	72.102308	70.379777
881.600747	69.700165	70.384782
880.582186	63.368398	70.389786
879.817720	69.708107	70.394791
879.365188	60.014057	70.399796
879.108569	56.221372	70.404801
878.515341	68.016932	70.409806
877.937474	61.503067	70.414810
876.841802	64.106041	70.419815
876.666921	67.368301	70.424820
875.297968	62.211947	70.429825
874.755958	65.906376	70.434830
874.270192	66.890513	70.439834
873.627725	60.889983	70.444839
873.479349	61.221179	70.449844
872.351062	68.008301	70.454849
871.719929	68.421059	70.459854
871.308370	58.720492	70.464858
870.004504	71.649450	70.469863
869.570791	55.201425	70.474868
868.823946	59.127151	70.479873
868.139771	68.595396	70.484878
867.936868	65.327174	70.489882
866.899706	63.759231	70.494887
866.051251	68.445458	70.499892
865.722247	68.292888	70.504897
865.544664	66.367366	70.509902
864.768158	59.438839	70.514906
863.909620	65.776175	70.519911
863.282218	62.455666	70.524916
862.061526	64.228559	70.529921
860.999495	69.393484	70.534926
860.831279	57.626215	70.539930
859.995842	68.695499	70.544935
859.924424	65.955136	70.549940
859.667728	64.816495	70.554945
858.668478	69.167176	70.559950
858.221940	69.725601	70.564954
857.444162	71.610933	70.569959
856.679260	65.156803	70.574964
855.700411	71.503830	70.579969
854.709335	71.576485	70.584974
854.357644	64.282301	70.589978
854.003775	73.934525	70.594983
852.919444	69.562366	70.599988
852.006995	76.441304	70.604993
851.461291	75.946331	70.609998
851.344746	70.259494	70.615002
850.757040	85.029925	70.620007
850.074502	69.823141	70.625012
849.226357	73.574186	70.630017
848.246934	77.768752	70.635022
847.919351	68.704529	70.640026
847.297518	80.624505	70.645031
846.119959	80.518684	70.650036
845.864599	66.229519	70.655041
845.039179	75.281857	70.660046
845.399547	72.035951	70.665050
843.761429	71.419957	70.670055
843.436437	72.091504	70.675060
842.937280	71.204345	70.680065
841.421381	76.473057	70.685070
840.822255	65.193843	70.690074
840.140341	71.443152	70.695079
839.576649	71.605485	70.700084
839.402417	65.273393	70.705089
839.261967	68.534905	70.710094
838.453858	66.301308	70.715098
837.328479	69.733779	70.720103
836.813470	63.129496	70.725108
836.162871	67.233879	70.730113
834.710525	70.585928	70.735118
834.472090	61.695182	70.740122
834.141780	70.455825	70.745127
833.640520	68.465127	70.750132
832.679089	67.891248	70.755137
831.592528	69.012021	70.760142
831.470753	65.074874	70.765146
831.064562	66.029007	70.770151
830.128021	64.356754	70.775156
829.391469	61.070975	70.780161
828.722375	65.963631	70.785166
828.383906	68.504451	70.790170
827.070358	66.942669	70.795175
826.300822	63.425596	70.800180
825.878957	63.347737	70.805185
825.311255	66.571597	70.810190
825.236580	62.593839	70.815194
824.062320	67.076468	70.820199
823.211938	61.435479	70.825204
822.620357	62.411237	70.830209
822.177049	63.212006	70.835214
822.007743	64.953187	70.840218
820.779203	67.384943	70.845223
820.195508	63.248507	70.850228
819.455477	62.212035	70.855233
818.353256	61.174867	70.860238
817.740003	58.432443	70.865242
817.229427	65.685815	70.870247
817.023164	62.662564	70.875252
816.962033	58.632189	70.880257
815.742325	70.693057	70.885262
814.951564	65.326433	70.890266
814.137153	64.796969	70.895271
813.475935	62.830161	70.900276
812.607766	53.855156	70.905281
811.667674	65.194997	70.910286
811.530212	65.830390	70.915290
810.901559	74.685834	70.920295
810.315191	62.882627	70.925300
809.472788	63.262796	70.930305
808.573090	70.474031	70.935310
808.564099	64.336416	70.940314
807.991566	61.347814	70.945319
806.857172	67.032058	70.950324
806.363071	66.123601	70.955329
805.645370	74.769292	70.960334
805.017694	59.862891	70.965338
803.648446	76.069753	70.970343
802.995628	71.371884	70.975348
802.835429	59.969204	70.980353
802.073196	67.912346	70.985358
802.191891	63.616801	70.990362
801.187018	71.533913	70.995367
800.409023	66.171570	71.000372
799.659089	64.799210	71.005377
798.962472	72.552137	71.010382
798.727711	68.109425	71.015386
797.039348	79.360231	71.020391
796.834520	69.248298	71.025396
796.524754	67.476287	71.030401
796.058086	76.518840	71.035406
795.043361	73.390891	71.040410
794.273650	76.609069	71.045415
793.765173	67.171528	71.050420
793.320229	72.452717	71.055425
791.932684	71.916720	71.060430
791.560612	61.030318	71.065434
791.079916	75.233349	71.070439
790.741781	71.206065	71.075444
789.869633	62.898754	71.080449
788.806554	77.306457	71.085454
788.463336	64.250289	71.090458
787.875979	67.109854	71.095463
787.245828	69.717609	71.100468
786.635539	77.571917	71.105473
785.499840	82.398514	71.110478
785.475306	64.477144	71.115482
784.861179	73.819138	71.120487
783.639470	70.120166	71.125492
783.034465	65.033069	71.130497
782.535118	67.864433	71.135502
781.544905	64.942325	71.140506
780.681167	68.158127	71.145511
780.233020	70.295361	71.150516
779.826447	68.956659	71.155521
779.317043	75.883422	71.160526
779.078877	73.551232	71.165530
777.707864	68.641269	71.170535
776.974496	73.351780	71.175540
776.775184	67.947789	71.180545
775.856327	69.795678	71.185550
775.118914	62.053556	71.190554
774.301181	61.332244	71.195559
773.662923	69.498509	71.200564
773.670210	65.977641	71.205569
772.563461	71.731617	71.210574
771.849955	58.168275	71.215578
771.138586	64.307165	71.220583
770.628459	71.137848	71.225588
770.357464	72.078354	71.230593
768.826799	68.688773	71.235598
768.733189	64.933230	71.240602
768.183831	67.991755	71.245607
767.491724	69.149110	71.250612
766.539233	58.825050	71.255617
765.712013	73.176284	71.260622
765.689203	58.228805	71.265626
764.675269	64.158818	71.270631
763.478755	62.844946	71.275636
762.908525	59.130587	71.280641
761.996302	63.462716	71.285646
761.891626	56.646476	71.290650
761.679300	70.374693	71.295655
761.316739	61.937386	71.300660
760.182442	64.333666	71.305665
759.380830	72.172701	71.310670
758.908154	61.374864	71.315674
757.667345	58.451661	71.320679
757.049163	65.446203	71.325684
756.631009	69.362211	71.330689
755.933141	73.136668	71.335694
755.807299	67.407168	71.340698
754.730450	61.545215	71.345703
754.093927	68.457522	71.350708
753.730565	60.025076	71.355713
752.709460	75.712906	71.360718
751.760754	69.726471	71.365722
751.259319	74.031056	71.370727
750.465361	66.632259	71.375732
750.590166	62.931834	71.380737
749.742428	75.045476	71.385742
748.815229	57.575334	71.390746
748.129510	69.033971	71.395751
747.656965	71.110439	71.400756
746.677811	62.348671	71.405761
746.013814	80.575335	71.410766
745.131509	66.395469	71.415770
744.410903	66.284758	71.420775
744.303669	65.224839	71.425780
744.135051	62.968315	71.430785
742.860803	71.868200	71.435790
742.089502	55.004030	71.440794
741.748194	61.546060	71.445799
740.675128	68.710796	71.450804
740.146471	58.546357	71.455809
739.467376	69.327424	71.460814
739.413183	60.418404	71.465818
738.520662	65.499615	71.470823
737.444906	68.722375	71.475828
736.919240	65.819370	71.480833
736.241686	65.615075	71.485838
735.471759	66.556168	71.490842
734.803159	66.429295	71.495847
733.818323	65.796102	71.500852
733.805982	58.547270	71.505857
733.019754	66.856947	71.510862
732.055099	61.691507	71.515866
731.550452	59.818068	71.520871
730.714683	67.605775	71.525876
730.640476	58.660519	71.530881
729.844876	61.986913	71.535886
728.887733	58.487127	71.540890
728.071261	64.947114	71.545895
727.625885	64.384156	71.550900
727.397443	62.327971	71.555905
725.900685	65.914231	71.560910
725.420991	62.827290	71.565914
724.982892	70.461801	71.570919
724.498478	61.517197	71.575924
724.116700	58.181279	71.580929
722.533225	71.139039	71.585934
722.415841	61.935726	71.590938
721.939659	64.080587	71.595943
721.074599	59.328229	71.600948
720.266551	58.051880	71.605953
719.267095	66.094309	71.610958
719.245488	58.635640	71.615962
718.900519	59.035991	71.620967
717.950743	65.558205	71.625972
717.361941	61.764812	71.630977
716.405408	66.767912	71.635982
715.950928	59.608398	71.640986
714.842015	63.763699	71.645991
713.954991	66.333519	71.650996
713.829426	52.809065	71.656001
713.083489	60.965672	71.661006
712.405803	58.041146	71.666010
711.573235	54.956776	71.671015
710.658069	59.923327	71.676020
710.397124	61.925109	71.681025
709.864444	58.654220	71.686030
709.790131	50.506931	71.691034
708.577703	49.864253	71.696039
707.544072	60.867348	71.701044
707.277446	52.277589	71.706049
707.041235	62.043542	71.711054
706.041936	59.460385	71.716058
705.263313	61.442089	71.721063
704.643689	60.441675	71.726068
703.500735	50.636835	71.731073
702.610759	59.649012	71.736078
702.379443	62.628524	71.741082
701.780578	54.358171	71.746087
701.218046	59.812630	71.751092
700.942361	55.676075	71.756097
699.859569	62.566403	71.761102
699.236593	56.149663	71.766106
698.822371	64.284999	71.771111
698.026273	50.055177	71.776116
697.259197	50.098536	71.781121
696.451355	69.166535	71.786126
696.024393	56.347662	71.791130
695.492238	59.179531	71.796135
694.659498	57.131258	71.801140
694.028161	56.602646	71.806145
693.246420	59.695030	71.811150
693.050328	61.989265	71.816154
692.156526	65.747623	71.821159
691.163832	61.993315	71.826164
690.788514	60.780540	71.831169
689.694027	63.829681	71.836174
688.790811	58.343817	71.841178
688.171945	61.263611	71.846183
687.670336	56.888639	71.851188
687.721748	54.032536	71.856193
687.033142	63.504668	71.861198
686.122848	55.760148	71.866202
685.376131	64.085621	71.871207
684.495409	64.828326	71.876212
684.245130	54.460310	71.881217
683.997166	62.887719	71.886222
683.057420	62.010823	71.891226
682.067002	63.579976	71.896231
681.038033	60.384962	71.901236
680.525709	54.939365	71.906241
679.435210	57.644097	71.911246
678.995166	56.673443	71.916250
678.682515	59.675370	71.921255
678.290002	62.265810	71.926260
678.154700	50.539074	71.931265
676.834994	60.474394	71.936270
676.252513	60.999303	71.941274
675.425196	59.584110	71.946279
674.814149	61.277364	71.951284
674.275677	55.840663	71.956289
673.322185	64.739961	71.961294
672.644646	57.552899	71.966298
672.436626	56.904849	71.971303
671.283648	63.314351	71.976308
670.990584	60.823760	71.981313
670.008201	63.358315	71.986318
669.928787	61.117557	71.991322
669.121050	62.302811	71.996327
667.576692	71.452318	72.001332
667.401503	55.138243	72.006337
667.079971	64.821589	72.011342
666.382947	68.622740	72.016346
665.740874	68.453815	72.021351
664.485092	65.332770	72.026356
664.234606	57.812781	72.031361
663.860156	68.403423	72.036366
663.140862	58.896995	72.041370
662.055392	59.145606	72.046375
661.463369	64.313032	72.051380
661.216140	59.919636	72.056385
660.400648	62.402390	72.061390
659.708116	68.738580	72.066394
659.146256	64.762716	72.071399
658.236474	68.291817	72.076404
657.263109	62.875483	72.081409
656.488418	65.509436	72.086414
655.844484	62.656823	72.091418
655.677643	57.253990	72.096423
655.196130	59.152127	72.101428
654.968799	53.118682	72.106433
653.579646	61.464458	72.111438
653.199974	56.475563	72.116442
652.674427	56.357473	72.121447
651.674070	59.073093	72.126452
651.102578	53.638503	72.131457
650.284958	65.010922	72.136462
649.867022	51.742774	72.141466
649.209423	64.685593	72.146471
648.231882	66.932380	72.151476
648.151820	61.976200	72.156481
647.504755	62.068273	72.161486
646.573001	59.367152	72.166490
645.855597	59.522466	72.171495
644.910586	65.777438	72.176500
643.915360	57.087669	72.181505
643.334643	66.917946	72.186510
642.411845	60.599429	72.191514
642.116453	60.490423	72.196519
641.748955	63.734477	72.201524
641.637943	61.090320	72.206529
640.892146	67.146412	72.211534
639.904467	60.070249	72.216538
639.188881	56.904198	72.221543
638.668906	70.720822	72.226548
637.873406	59.215914	72.231553
637.201065	68.571925	72.236558
636.646046	64.279586	72.241562
636.216734	60.260545	72.246567
635.052642	65.391341	72.251572
634.271894	65.626131	72.256577
633.633625	71.067435	72.261582
632.898147	60.934388	72.266586
632.767247	69.855671	72.271591
631.497319	73.144088	72.276596
631.088338	63.734911	72.281601
630.365113	67.877712	72.286606
630.116778	65.865707	72.291610
629.724610	60.093480	72.296615
628.505082	70.038105	72.301620
627.921401	54.733691	72.306625
627.296593	70.166046	72.311630
626.783324	59.645953	72.316634
625.689640	62.866880	72.321639
624.746979	75.678488	72.326644
624.625903	64.154491	72.331649
624.125914	65.727568	72.336654
623.321436	60.524053	72.341658
622.814141	60.790994	72.346663
621.681983	58.575962	72.351668
621.764046	53.207614	72.356673
620.788439	64.583120	72.361678
619.766577	64.938315	72.366682
619.262620	60.166339	72.371687
618.854935	64.329855	72.376692
618.374940	64.743838	72.381697
617.253073	59.994572	72.386702
616.374292	55.361137	72.391706
616.267234	60.378798	72.396711
615.431469	67.357552	72.401716
614.501477	57.982470	72.406721
613.576203	71.810024	72.411726
613.207011	66.589229	72.416730
612.978163	55.531837	72.421735
612.471892	64.210119	72.426740
611.462118	54.393582	72.431745
610.575010	56.860945	72.436750
610.390525	62.177944	72.441754
609.583216	61.387218	72.446759
608.234798	66.905350	72.451764
607.616452	57.819686	72.456769
607.304302	65.880426	72.461774
606.943510	57.865502	72.466778
606.632701	62.656990	72.471783
605.397623	58.085033	72.476788
604.828186	58.499070	72.481793
604.285967	63.491416	72.486798
603.638347	61.022607	72.491802
602.823943	66.088264	72.496807
601.981941	74.591362	72.501812
601.928763	64.234545	72.506817
600.843631	70.895048	72.511822
599.501242	64.930380	72.516826
599.514586	64.605051	72.521831
598.548077	66.768097	72.526836
598.598182	66.463723	72.531841
597.705565	71.212255	72.536846
596.660799	72.481013	72.541850
596.304440	63.982832	72.546855
595.657526	71.645880	72.551860
595.018075	66.766176	72.556865
593.903291	64.575197	72.561870
593.242985	60.973001	72.566874
592.915790	65.874334	72.571879
592.438404	69.902299	72.576884
591.595268	66.598879	72.581889
590.983088	63.145137	72.586894
590.384255	62.377986	72.591898
589.824404	65.695259	72.596903
588.778820	72.007268	72.601908
588.161965	57.703213	72.606913
587.466209	60.187418	72.611918
586.918448	61.299754	72.616922
586.548675	53.355654	72.621927
585.579139	68.909145	72.626932
585.033966	61.160134	72.631937
584.251162	64.941849	72.636942
583.978554	65.168267	72.641946
582.957683	62.579136	72.646951
581.835752	69.508859	72.651956
581.452809	62.352179	72.656961
580.702605	71.244361	72.661966
580.718293	74.793251	72.666970
580.286871	65.572164	72.671975
578.865223	63.628763	72.676980
578.577490	60.788828	72.681985
577.768823	65.434107	72.686990
577.112990	57.029363	72.691994
576.416916	61.937408	72.696999
575.765365	61.908788	72.702004
575.345272	63.402918	72.707009
574.016937	66.855205	72.712014
573.375612	68.062871	72.717018
572.998473	67.003370	72.722023
572.440367	72.116527	72.727028
572.314957	63.520067	72.732033
571.090053	66.285675	72.737038
570.306667	57.451815	72.742042
570.089546	57.210502	72.747047
569.020234	69.372083	72.752052
568.417858	53.692202	72.757057
567.467231	59.976474	72.762062
567.054300	64.274874	72.767066
567.162709	56.077996	72.772071
565.638008	64.409133	72.777076
564.768673	60.201570	72.782081
564.264383	63.051102	72.787086
563.799997	63.005291	72.792090
563.762809	55.681585	72.797095
562.473290	62.385691	72.802100
561.828197	66.290559	72.807105
561.313619	64.939136	72.812110
561.028325	63.410844	72.817114
559.755750	59.335318	72.822119
559.066281	66.746526	72.827124
558.586386	56.184872	72.832129
558.159565	63.000733	72.837134
557.034311	70.320504	72.842138
556.691515	60.618531	72.847143
555.965909	62.771607	72.852148
555.480193	54.238852	72.857153
554.636690	69.786469	72.862158
553.868067	64.722348	72.867162
553.282824	58.462072	72.872167
552.731468	60.278310	72.877172
551.589310	57.382082	72.882177
550.937098	64.724278	72.887182
550.327435	61.445190	72.892186
550.420716	58.822116	72.897191
549.618433	66.423184	72.902196
549.001488	50.669940	72.907201
547.830235	60.341972	72.912206
547.503204	58.970141	72.917210
546.651949	64.675620	72.922215
545.600062	75.467214	72.927220
545.115602	65.086058	72.932225
544.799527	56.408012	72.937230
544.202887	68.095341	72.942234
543.671571	56.930022	72.947239
542.830166	64.456896	72.952244
542.131823	56.355404	72.957249
541.520677	55.383645	72.962254
540.426148	62.151320	72.967258
539.728889	57.378615	72.972263
539.149572	66.366586	72.977268
539.092502	60.093148	72.982273
538.266841	55.566402	72.987278
537.472606	56.030453	72.992282
536.802354	59.247048	72.997287
536.134969	70.500946	73.002292
536.107547	57.057085	73.007297
534.915452	62.581890	73.012302
534.008414	68.149602	73.017306
533.836724	60.421542	73.022311
532.295165	66.389945	73.027316
531.616216	59.926981	73.032321
531.251079	61.896489	73.037326
530.519704	63.713022	73.042330
530.259696	59.861002	73.047335
529.747170	70.431065	73.052340
529.222961	59.721934	73.057345
528.260712	58.038126	73.062350
527.472838	65.658980	73.067354
527.022854	55.739125	73.072359
525.601419	73.493509	73.077364
525.423346	62.459582	73.082369
524.868131	56.678658	73.087374
524.379172	61.891192	73.092378
523.813397	57.266284	73.097383
522.612482	70.130087	73.102388
522.298724	66.682445	73.107393
521.834427	61.148813	73.112398
520.751429	66.151621	73.117402
519.809933	61.575522	73.122407
519.288983	62.693063	73.127412
519.141772	58.124485	73.132417
518.578043	62.188289	73.137422
517.620474	70.231995	73.142426
517.025477	61.664615	73.147431
516.353904	62.083902	73.152436
515.662282	61.949718	73.157441
515.277909	65.286361	73.162446
513.955779	66.405369	73.167450
513.301221	64.579512	73.172455
512.803060	76.371013	73.177460
512.591789	63.073132	73.182465
512.143628	61.602330	73.187470
510.822821	61.382291	73.192474
510.675135	58.784987	73.197479
509.920590	61.226537	73.202484
509.062285	53.838094	73.207489
508.458270	55.277951	73.212494
507.345022	66.058824	73.217498
507.277796	56.634668	73.222503
506.285114	52.418394	73.227508
505.267275	57.251552	73.232513
505.195680	55.686074	73.237518
504.423544	61.935626	73.242522
504.252723	60.993082	73.247527
502.932144	63.635189	73.252532
502.292062	57.897752	73.257537
501.742055	55.504888	73.262542
501.174190	62.851002	73.267546
500.279559	49.956885	73.272551
499.546495	64.480815	73.277556
499.223648	60.039566	73.282561
499.002811	53.226094	73.287566
497.719781	55.349710	73.292570
497.247473	50.328299	73.297575
496.594583	64.036787	73.302580
495.696854	49.077352	73.307585
494.928643	55.028233	73.312590
494.009165	62.521824	73.317594
493.541937	57.245712	73.322599
493.040847	58.118819	73.327604
493.098004	52.019580	73.332609
492.196819	54.705269	73.337614
491.143590	52.693770	73.342618
490.856623	54.542019	73.347623
489.672848	59.811627	73.352628
488.718016	59.064943	73.357633
488.216095	60.605237	73.362638
487.583560	70.754451	73.367642
487.663078	55.517909	73.372647
487.293432	59.547646	73.377652
485.912355	52.652502	73.382657
485.044485	60.604652	73.387662
484.410689	64.646510	73.392666
484.318241	54.485207	73.397671
482.893832	66.279177	73.402676
482.151144	63.976935	73.407681
481.741373	62.019052	73.412686
481.364888	64.062914	73.417690
481.011167	60.691033	73.422695
479.786159	66.706808	73.427700
479.078509	60.210587	73.432705
478.765755	56.013740	73.437710
478.145852	64.408940	73.442714
477.600275	56.071824	73.447719
476.514754	64.189539	73.452724
475.943190	56.266572	73.457729
475.765683	52.519690	73.462734
474.409180	64.856357	73.467738
473.934546	56.058507	73.472743
473.099780	62.832133	73.477748
472.885616	54.014866	73.482753
472.385311	59.997192	73.487758
471.388253	58.467186	73.492762
470.941788	53.395931	73.497767
470.092079	54.386083	73.502772
468.894241	55.256654	73.507777
468.168390	47.971709	73.512782
467.764642	54.887979	73.517786
467.446157	51.993037	73.522791
466.905019	59.878947	73.527796
466.607664	54.041191	73.532801
465.937672	52.440159	73.537806
464.922614	49.184681	73.542810
464.594757	48.129964	73.547815
463.401297	59.139667	73.552820
462.588326	51.542172	73.557825
462.522715	60.736893	73.562830
461.346496	66.060504	73.567834
460.395268	55.206541	73.572839
459.752130	53.165992	73.577844
459.464093	56.734875	73.582849
459.173700	57.691116	73.587854
458.135207	62.188538	73.592858
457.331594	57.158415	73.597863
456.769709	60.670002	73.602868
456.236584	54.004060	73.607873
455.595564	48.784034	73.612878
454.660068	59.301633	73.617882
454.286421	56.540060	73.622887
453.565646	58.999900	73.627892
452.860933	60.011112	73.632897
451.950160	56.597098	73.637902
451.373033	65.300879	73.642906
450.847685	52.450453	73.647911
450.428811	61.335601	73.652916
449.983788	59.749193	73.657921
448.965138	57.169230	73.662926
448.386346	62.848674	73.667930
447.771315	56.648370	73.672935
446.641266	62.092364	73.677940
446.026777	58.795151	73.682945
445.585254	58.110206	73.687950
444.990502	57.072781	73.692954
444.725676	52.731110	73.697959
443.344442	60.334552	73.702964
442.626441	59.914430	73.707969
442.406571	62.909482	73.712974
441.759884	57.717167	73.717978
441.245394	47.643617	73.722983
440.182963	63.262396	73.727988
439.439422	58.897646	73.732993
439.007204	55.278082	73.737998
438.393866	59.564270	73.743002
437.460781	54.239392	73.748007
436.684651	65.263044	73.753012
436.261081	55.974520	73.758017
436.228052	58.485640	73.763022
435.354166	64.281488	73.768026
434.660341	52.028769	73.773031
433.925825	60.623585	73.778036
432.962297	57.568067	73.783041
432.265191	52.779606	73.788046
431.024085	67.151104	73.793050
431.084094	59.170101	73.798055
430.699568	64.332894	73.803060
430.147540	52.456555	73.808065
429.063199	54.409776	73.813070
428.264489	57.670517	73.818074
428.031016	57.195279	73.823079
426.929620	55.954730	73.828084
425.890099	56.815866	73.833089
425.881140	55.014907	73.838094
425.048752	54.918945	73.843098
424.950874	56.140985	73.848103
423.895639	54.866274	73.853108
423.175723	51.939105	73.858113
422.584794	62.568972	73.863118
422.199311	65.509988	73.868122
421.332790	62.136242	73.873127
420.424921	54.642193	73.878132
419.929180	56.473251	73.883137
419.757718	55.426737	73.888142
418.214096	62.758022	73.893146
417.834014	58.770608	73.898151
416.988802	63.959496	73.903156
416.714782	64.356468	73.908161
415.934802	60.369693	73.913166
414.557309	69.546359	73.918170
414.456955	58.457496	73.923175
414.041811	59.384734	73.928180
413.438546	59.089843	73.933185
412.447269	56.254798	73.938190
411.311274	66.205118	73.943194
411.108011	57.095964	73.948199
410.535869	60.979778	73.953204
410.240988	63.329193	73.958209
409.854522	57.918807	73.963214
408.720452	69.311737	73.968218
408.445378	58.966652	73.973223
407.033523	57.879657	73.978228
405.549875	56.783603	73.983233
405.464997	55.023126	73.988238
404.586530	59.402028	73.993242
404.780912	59.859986	73.998247
404.344990	60.784228	74.003252
403.729384	65.032940	74.008257
403.100086	68.394430	74.013262
402.073624	59.017474	74.018266
401.765291	60.757173	74.023271
400.849764	64.448123	74.028276
399.995602	63.575046	74.033281
399.577125	56.636962	74.038286
398.771450	62.057674	74.043290
397.653743	65.487527	74.048295
396.935272	57.490221	74.053300
396.336867	54.892205	74.058305
396.604938	51.246222	74.063310
395.712873	62.095964	74.068314
394.859314	52.320881	74.073319
393.853441	55.116323	74.078324
393.308258	61.534743	74.083329
393.188461	53.967174	74.088334
392.135759	56.025756	74.093338
391.518206	41.673023	74.098343
390.955312	58.249848	74.103348
389.873211	64.698630	74.108353
389.318316	53.712165	74.113358
388.087846	51.322101	74.118362
387.850224	55.384427	74.123367
387.745003	59.118150	74.128372
387.252395	49.583601	74.133377
386.472864	48.881564	74.138382
385.522083	56.074242	74.143386
384.896058	54.603423	74.148391
384.448708	62.431823	74.153396
383.308322	62.695613	74.158401
382.707646	56.212345	74.163406
381.632139	63.896412	74.168410
381.533004	60.889259	74.173415
380.746703	59.986452	74.178420
380.371030	55.659299	74.183425
379.727379	56.206638	74.188430
378.987812	62.392683	74.193434
378.371173	59.108447	74.198439
377.318893	44.632601	74.203444
376.575086	57.262755	74.208449
376.509145	55.269026	74.213454
375.813052	58.658511	74.218458
375.251028	56.087819	74.223463
374.369939	58.552726	74.228468
373.605604	60.898102	74.233473
373.341343	60.240118	74.238478
372.241013	59.909327	74.243482
371.271201	57.148151	74.248487
370.751841	62.278818	74.253492
370.331077	56.471783	74.258497
370.147274	55.676399	74.263502
368.742388	66.883836	74.268506
368.115300	61.578034	74.273511
367.675058	59.336445	74.278516
366.945869	58.550698	74.283521
366.914075	62.924004	74.288526
365.711766	64.527044	74.293530
364.924065	59.087565	74.298535
364.712425	62.161734	74.303540
363.591806	61.775832	74.308545
362.907828	58.650566	74.313550
362.100279	59.821693	74.318554
361.829073	60.450035	74.323559
361.223747	70.426197	74.328564
360.353095	52.888923	74.333569
359.383780	58.774114	74.338574
358.907045	69.226525	74.343578
358.680184	61.385857	74.348583
357.947158	65.249589	74.353588
356.883628	62.498621	74.358593
356.244077	57.002422	74.363598
355.840607	62.141432	74.368602
355.596724	54.144209	74.373607
354.460868	52.855568	74.378612
353.750570	59.398077	74.383617
353.443969	58.679033	74.388622
352.561747	63.692486	74.393626
351.647515	45.529812	74.398631
351.247349	57.423964	74.403636
350.406347	64.274309	74.408641
350.328233	53.554078	74.413646
348.889004	60.252173	74.418650
348.462580	54.472854	74.423655
347.722394	56.292418	74.428660
347.169404	64.929288	74.433665
346.527275	55.374421	74.438670
345.304752	63.778943	74.443674
345.287842	53.023728	74.448679
344.664555	55.718796	74.453684
344.193025	67.012470	74.458689
343.217938	54.627991	74.463694
342.494820	60.907617	74.468698
341.913767	63.280566	74.473703
341.416094	54.257768	74.478708
340.496269	61.368258	74.483713
339.706636	46.719689	74.488718
338.835146	65.886176	74.493722
338.697901	55.787226	74.498727
338.239732	53.047029	74.503732
337.310279	64.273330	74.508737
336.662468	59.073343	74.513742
336.178108	54.009736	74.518746
335.421699	58.265128	74.523751
334.241657	52.504989	74.528756
333.296889	54.227849	74.533761
333.251167	49.438117	74.538766
332.908727	66.635834	74.543770
332.490570	52.114142	74.548775
331.786743	58.911090	74.553780
330.886044	63.093286	74.558785
330.517317	55.866593	74.563790
329.229166	65.063751	74.568794
328.533990	58.778485	74.573799
328.135686	61.775171	74.578804
327.543459	63.869206	74.583809
326.605547	67.631557	74.588814
325.798031	59.812471	74.593818
325.327282	60.753316	74.598823
325.248226	54.573290	74.603828
323.898465	60.807708	74.608833
323.457335	53.952103	74.613838
322.488549	58.815356	74.618842
321.995295	55.565090	74.623847
321.703390	56.784939	74.628852
320.744946	57.735699	74.633857
320.027526	54.328771	74.638862
319.754229	53.309534	74.643866
318.959694	56.158056	74.648871
317.882656	63.216338	74.653876
317.155806	62.381348	74.658881
316.912898	54.868102	74.663886
316.319474	58.849942	74.668890
315.489235	54.044891	74.673895
314.620796	60.171065	74.678900
313.951104	65.431357	74.683905
313.941568	58.956399	74.688910
312.737178	62.570412	74.693914
311.783808	63.343748	74.698919
311.308221	51.918894	74.703924
310.738760	61.640182	74.708929
310.544136	55.740350	74.713934
309.918058	70.937967	74.718938
308.891161	62.059445	74.723943
308.089952	65.848900	74.728948
307.576534	62.341652	74.733953
307.419287	59.124570	74.738958
306.100848	62.031363	74.743962
305.721438	55.651627	74.748967
305.135161	56.292343	74.753972
303.891809	55.427712	74.758977
303.468381	56.444597	74.763982
302.682006	51.399172	74.768986
302.374656	65.580890	74.773991
302.223831	56.348282	74.778996
300.789472	52.114184	74.784001
300.482584	55.719199	74.789006
299.670188	54.295453	74.794010
299.201155	49.066988	74.799015
298.403530	54.926411	74.804020
297.343239	51.064783	74.809025
297.247727	49.458971	74.814030
296.278032	51.658904	74.819034
295.255419	46.331014	74.824039
294.782446	44.624514	74.829044
294.143333	56.206667	74.834049
294.006777	50.078389	74.839054
293.407613	56.732506	74.844058
292.388246	55.166708	74.849063
291.642665	51.415772	74.854068
291.285895	61.446939	74.859073
290.440516	45.839029	74.864078
289.427141	57.466642	74.869082
288.809039	57.018028	74.874087
288.576247	47.227635	74.879092
288.123751	56.534465	74.884097
287.244770	47.395845	74.889102
286.404827	54.476269	74.894106
285.991350	49.145912	74.899111
285.294950	57.408252	74.904116
284.092344	54.379865	74.909121
283.744411	49.814923	74.914126
282.930043	58.944466	74.919130
282.645537	58.346490	74.924135
282.015725	58.391753	74.929140
280.930574	60.274204	74.934145
280.551860	50.477106	74.939150
280.048664	58.815885	74.944154
278.944483	58.673408	74.949159
278.263366	54.950047	74.954164
277.570311	64.380381	74.959169
277.081586	53.280906	74.964174
276.986554	54.675961	74.969178
276.077527	50.408610	74.974183
275.422381	46.886116	74.979188
274.354391	43.847320	74.984193
274.178722	53.777076	74.989198
272.864669	60.411104	74.994202
272.296104	50.489728	74.999207
271.726079	47.724798	75.004212
271.385341	52.071646	75.009217
271.007805	46.707180	75.014222
269.583688	64.512540	75.019226
269.047285	55.290933	75.024231
268.464595	50.736604	75.029236
267.963480	59.696373	75.034241
267.498546	47.189625	75.039246
266.431583	55.041100	75.044250
265.976041	60.426539	75.049255
265.865709	47.959465	75.054260
264.720528	65.646250	75.059265
264.193401	52.280511	75.064270
263.145245	58.848506	75.069274
262.815401	56.603535	75.074279
262.034883	51.688079	75.079284
261.099301	55.694505	75.084289
260.721819	53.998023	75.089294
260.256912	63.719999	75.094298
259.263589	56.420993	75.099303
258.267907	55.177864	75.104308
257.650557	57.510883	75.109313
257.471373	57.979488	75.114318
256.775654	55.548409	75.119322
255.946144	55.751667	75.124327
255.257390	52.660313	75.129332
254.443198	59.310866	75.134337
254.466311	49.692576	75.139342
253.781017	51.251103	75.144346
252.800134	60.993824	75.149351
252.153777	55.441973	75.154356
251.465325	66.743422	75.159361
250.859520	55.337764	75.164366
249.610974	59.392505	75.169370
249.263848	62.387351	75.174375
249.239803	53.823673	75.179380
248.069727	58.805770	75.184385
247.768868	60.864416	75.189390
246.479074	58.299377	75.194394
246.035059	64.846774	75.199399
245.787834	52.340020	75.204404
244.869548	53.774839	75.209409
244.342432	47.921712	75.214414
243.587018	60.706705	75.219418
242.868154	51.463731	75.224423
242.134674	47.083257	75.229428
241.212698	52.910477	75.234433
241.170864	55.247955	75.239438
240.342711	54.776066	75.244442
239.557413	56.065110	75.249447
238.454607	55.575502	75.254452
237.557808	62.811663	75.259457
237.487910	57.040193	75.264462
237.190037	57.081441	75.269466
236.404454	52.655657	75.274471
235.228016	48.921382	75.279476
234.525632	56.763638	75.284481
234.456902	54.164812	75.289486
234.097985	55.324389	75.294490
232.870396	55.028139	75.299495
232.202862	64.419720	75.304500
231.384698	60.010167	75.309505
230.987084	49.426043	75.314510
230.386475	48.810653	75.319514
229.267097	51.315168	75.324519
228.961398	54.596724	75.329524
228.358744	63.266757	75.334529
227.943583	60.761000	75.339534
226.994653	56.946306	75.344538
225.992021	55.480371	75.349543
225.716300	46.693468	75.354548
225.234993	48.104368	75.359553
224.391302	55.270562	75.364558
223.499262	54.201737	75.369562
222.777415	54.581809	75.374567
222.714306	49.649776	75.379572
221.776632	52.297216	75.384577
221.020896	53.411243	75.389582
220.253326	51.472600	75.394586
219.747761	60.034115	75.399591
219.420896	49.730451	75.404596
218.423629	63.681525	75.409601
217.574891	57.567436	75.414606
217.197155	53.970774	75.419610
216.597824	61.389755	75.424615
215.718925	55.305706	75.429620
214.838512	61.403855	75.434625
214.505786	59.999866	75.439630
213.904071	47.589058	75.444634
213.081283	50.353804	75.449639
212.363862	61.396522	75.454644
211.452289	62.882325	75.459649
211.370596	54.014027	75.464654
210.970952	51.535764	75.469658
209.455715	52.785063	75.474663
208.858373	44.894682	75.479668
208.376181	56.380868	75.484673
207.944997	44.909550	75.489678
207.406964	54.583258	75.494682
206.132749	61.100580	75.499687
205.722211	47.989092	75.504692
205.074683	49.494303	75.509697
204.995504	51.639037	75.514702
203.942478	63.809164	75.519706
203.071604	51.865465	75.524711
202.374882	56.319534	75.529716
201.912018	58.307817	75.534721
201.425460	57.928141	75.539726
200.244064	59.699813	75.544730
199.774310	64.732713	75.549735
199.474823	51.294438	75.554740
198.658634	55.305507	75.559745
197.883897	54.541266	75.564750
196.894136	56.123115	75.569754
196.521597	58.320926	75.574759
196.561140	44.786032	75.579764
195.266932	55.824507	75.584769
194.670576	60.117499	75.589774
194.046674	56.768243	75.594778
193.269427	69.723889	75.599783
192.776874	58.721242	75.604788
191.630354	57.145796	75.609793
191.448969	63.548827	75.614798
191.094460	52.030592	75.619802
190.062050	70.163049	75.624807
189.625035	58.976506	75.629812
188.932921	61.490195	75.634817
188.080837	57.024566	75.639822
187.125298	52.540740	75.644826
186.277515	53.920186	75.649831
186.296431	55.587236	75.654836
185.752944	53.901462	75.659841
184.718376	49.442853	75.664846
184.026050	43.674430	75.669850
183.351190	55.888345	75.674855
183.103866	44.945964	75.679860
181.456724	55.190735	75.684865
181.048812	53.030763	75.689870
180.581027	47.775321	75.694874
179.973418	58.105100	75.699879
179.912113	39.361851	75.704884
178.894001	59.412742	75.709889
178.201451	50.328026	75.714894
177.646956	57.963790	75.719898
176.842474	45.670480	75.724903
175.584308	46.822044	75.729908
175.015706	54.865332	75.734913
174.803331	41.602419	75.739918
174.301756	60.419788	75.744922
173.736517	51.032501	75.749927
172.854329	51.592692	75.754932
171.951519	53.782007	75.759937
171.498493	57.069710	75.764942
171.220878	46.386049	75.769946
170.199290	63.162176	75.774951
169.700121	53.674469	75.779956
168.852495	51.278676	75.784961
168.531103	53.857842	75.789966
167.509109	50.296098	75.794970
166.664302	52.291664	75.799975
166.363031	41.671702	75.804980
165.523996	62.086709	75.809985
164.291925	55.950180	75.814990
163.686145	51.278137	75.819994
163.008798	60.007395	75.824999
162.820617	44.674818	75.830004
162.136227	66.550662	75.835009
162.034763	44.488022	75.840014
161.545460	53.422261	75.845018
160.334537	49.857526	75.850023
159.946390	51.171583	75.855028
158.857682	50.055291	75.860033
158.249737	47.465171	75.865038
157.735586	48.403503	75.870042
157.072734	59.899576	75.875047
156.637827	51.854000	75.880052
155.746656	50.149552	75.885057
155.060036	50.773185	75.890062
154.549454	46.322510	75.895066
153.094894	55.330226	75.900071
152.731652	42.389415	75.905076
151.969005	49.624705	75.910081
151.764594	52.737154	75.915086
151.280161	46.943480	75.920090
150.664589	46.089223	75.925095
149.794590	49.389794	75.930100
148.896271	51.179432	75.935105
148.583717	44.142527	75.940110
147.505516	51.926448	75.945114
146.812105	48.094705	75.950119
146.680329	47.298929	75.955124
145.894935	53.262097	75.960129
145.031344	51.837106	75.965134
144.174860	42.119381	75.970138
143.405534	48.441107	75.975143
143.220326	47.158688	75.980148
142.753331	54.480884	75.985153
141.910381	37.853963	75.990158
141.213518	51.637299	75.995162
140.447162	46.079390	76.000167
140.316616	52.067457	76.005172
139.125717	53.006465	76.010177
138.320595	53.141219	76.015182
137.774265	49.886845	76.020186
137.174467	49.906860	76.025191
136.570373	49.035007	76.030196
135.479375	57.844416	76.035201
135.026759	54.526214	76.040206
134.529189	45.282695	76.045210
134.210032	55.705258	76.050215
133.528128	50.584892	76.055220
132.435632	56.765765	76.060225
131.523838	54.468526	76.065230
131.505261	48.764579	76.070234
130.505116	43.374839	76.075239
129.795198	53.580586	76.080244
129.067651	52.252180	76.085249
128.687833	49.720310	76.090254
128.181539	38.924893	76.095258
127.251845	56.389689	76.100263
126.850788	37.922978	76.105268
126.084581	55.708634	76.110273
125.103861	51.794975	76.115278
124.521849	39.759534	76.120282
123.888006	54.434841	76.125287
123.592567	41.297149	76.130292
122.530268	47.500015	76.135297
121.502968	47.572430	76.140302
120.921073	36.617185	76.145306
120.428358	57.114163	76.150311
120.488630	40.524579	76.155316
119.726716	49.391901	76.160321
118.586156	50.833823	76.165326
118.042548	52.215253	76.170330
117.505643	45.911139	76.175335
116.488378	49.345589	76.180340
115.298480	46.619618	76.185345
115.079680	55.578539	76.190350
114.508877	46.365626	76.195354
114.180321	48.890747	76.200359
114.044151	43.697563	76.205364
112.854021	43.822754	76.210369
112.415983	61.715362	76.215374
111.678208	56.285366	76.220378
110.256035	56.401828	76.225383
110.050575	50.095325	76.230388
109.202211	46.922237	76.235393
108.535054	60.363382	76.240398
108.461217	48.330486	76.245402
107.185867	59.214605	76.250407
106.656386	52.832036	76.255412
106.241685	53.901178	76.260417
105.677429	59.501090	76.265422
105.069776	44.497190	76.270426
104.033446	54.753415	76.275431
103.778294	42.328392	76.280436
102.905540	50.260916	76.285441
101.952974	47.126523	76.290446
101.513076	45.682872	76.295450
100.985189	54.191186	76.300455
100.599612	49.403625	76.305460
99.573159	52.147266	76.310465
98.722479	64.920669	76.315470
98.402702	56.670668	76.320474
97.301067	46.287157	76.325479
96.595674	48.667367	76.330484
95.933850	45.488192	76.335489
95.542607	54.241221	76.340494
94.939044	51.615726	76.345498
94.151570	52.551925	76.350503
93.745053	33.876368	76.355508
93.050422	48.351631	76.360513
92.394656	45.889003	76.365518
91.620343	51.577605	76.370522
90.691829	47.896911	76.375527
90.290803	56.692503	76.380532
89.915605	59.663457	76.385537
88.885458	48.391765	76.390542
88.236761	54.986007	76.395546
87.295409	57.220921	76.400551
86.976768	49.759221	76.405556
86.648303	48.548537	76.410561
85.658437	53.995549	76.415566
85.077729	47.646389	76.420570
84.305584	47.648169	76.425575
83.885562	50.716157	76.430580
82.388574	51.152070	76.435585
81.841885	47.553994	76.440590
81.584847	51.621008	76.445594
81.187128	52.980757	76.450599
80.776040	47.460833	76.455604
79.822409	51.112231	76.460609
78.534217	53.493922	76.465614
78.186057	46.383860	76.470618
77.694092	59.808109	76.475623
77.597141	48.288259	76.480628
76.312933	58.233941	76.485633
75.776228	48.181397	76.490638
75.210955	41.948053	76.495642
74.435530	49.470826	76.500647
73.640393	48.631032	76.505652
72.880687	47.153231	76.510657
72.376909	50.136806	76.515662
72.378123	45.297031	76.520666
71.029563	50.449589	76.525671
70.600519	49.981921	76.530676
69.962719	46.365261	76.535681
68.994075	35.878564	76.540686
68.145556	48.134376	76.545690
67.617635	39.624272	76.550695
67.161476	45.722609	76.555700
66.873428	53.648632	76.560705
65.745187	46.972058	76.565710
65.148322	44.268234	76.570714
64.130937	53.417585	76.575719
63.807263	45.032602	76.580724
63.389778	48.052879	76.585729
62.505507	49.165372	76.590734
61.615374	53.002192	76.595738
61.073096	63.818311	76.600743
61.238304	52.231421	76.605748
59.839854	54.212814	76.610753
59.219898	52.003103	76.615758
58.961609	43.230804	76.620762
57.773503	60.763637	76.625767
57.025049	52.239814	76.630772
56.421266	51.443625	76.635777
55.791520	60.392392	76.640782
55.563465	55.150786	76.645786
54.589257	59.418909	76.650791
53.798362	53.565323	76.655796
53.452710	47.686464	76.660801
52.847515	57.687869	76.665806
52.104034	54.002912	76.670810
50.766631	62.290256	76.675815
50.752654	55.803412	76.680820
50.450116	51.207621	76.685825
49.362197	61.338054	76.690830
48.579244	50.897436	76.695834
47.649294	60.942752	76.700839
47.468910	61.184482	76.705844
47.189027	66.668092	76.710849
45.843958	64.447870	76.715854
45.366917	43.104329	76.720858
44.469400	64.466963	76.725863
44.290493	56.312779	76.730868
43.055205	53.042151	76.735873
42.349944	56.887341	76.740878
42.021956	56.353098	76.745882
41.141769	56.422586	76.750887
41.139896	57.495283	76.755892
40.012805	58.037810	76.760897
39.000993	63.963003	76.765902
38.814874	51.949600	76.770906
38.403699	57.857845	76.775911
37.778579	45.127565	76.780916
36.711980	53.937846	76.785921
35.901456	54.556041	76.790926
35.771890	54.277159	76.795930
34.526624	55.146040	76.800935
33.618324	58.429105	76.805940
33.403478	61.593688	76.810945
33.038796	57.502971	76.815950
32.784280	62.821686	76.820954
31.175396	57.336686	76.825959
30.736860	51.717071	76.830964
30.147260	59.203915	76.835969
29.612995	67.932459	76.840974
28.891422	53.443489	76.845978
27.794555	66.300327	76.850983
27.519761	53.037932	76.855988
27.031561	64.733252	76.860993
26.300476	62.211690	76.865998
25.654667	50.090259	76.871002
24.568351	58.096294	76.876007
24.244512	50.108734	76.881012
23.809728	59.799115	76.886017
22.990685	59.880934	76.891022
22.001344	47.981453	76.896026
21.424981	66.293518	76.901031
21.306486	54.193638	76.906036
20.136871	54.072752	76.911041
19.373231	60.248527	76.916046
18.843034	60.412011	76.921050
18.345453	59.244080	76.926055
17.804442	65.936282	76.931060
16.638726	57.488485	76.936065
15.686970	62.688172	76.941070
15.622556	56.190452	76.946074
15.230158	62.111476	76.951079
14.572401	50.914469	76.956084
13.881896	48.656100	76.961089
12.964856	62.927165	76.966094
12.724755	56.325003	76.971098
11.619742	66.928109	76.976103
10.999298	53.468536	76.981108
10.761201	52.465800	76.986113
9.676130	61.233309	76.991118
8.830487	57.367542	76.996122
8.148670	64.181551	77.001127
7.681861	54.666655	77.006132
7.253193	53.937165	77.011137
5.971929	67.835822	77.016142
5.533673	52.055886	77.021147
4.981040	65.338433	77.026151
4.893968	54.963457	77.031156
3.842040	56.733492	77.036161