Fri Mar 05 19:47:48 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.659416	98.570554	0.000000
0.236316	88.476244	0.005005
-0.528216	57.144430	0.010010
-2.156937	12.842971	0.015014
-6.049721	-14.667062	0.020019
-11.092622	-8.614493	0.025024
-16.942226	-2.390649	0.030029
-21.351355	-20.731932	0.035034
-25.648940	-15.638739	0.040038
-29.610766	-17.584945	0.045043
-32.781019	-12.479190	0.050048
-36.569586	-11.723341	0.055053
-40.026817	-21.246800	0.060058
-43.659893	-9.371510	0.065062
-47.741956	-9.428254	0.070067
-50.969613	-17.714155	0.075072
-54.898181	-4.851849	0.080077
-58.569928	-16.305928	0.085082
-62.683556	-14.654516	0.090086
-66.364868	-7.595356	0.095091
-70.194422	-7.343844	0.100096
-73.878780	-10.135332	0.105101
-77.752438	-14.169201	0.110106
-81.563237	-4.887952	0.115110
-85.316133	-11.740146	0.120115
-88.945044	-20.318360	0.125120
-92.881345	-11.288307	0.130125
-96.325814	-12.068012	0.135130
-100.065462	-0.185096	0.140134
-104.080297	-7.124777	0.145139
-107.451631	-20.995268	0.150144
-111.563006	-16.773724	0.155149
-115.366356	-21.007980	0.160154
-119.297060	-25.431641	0.165158
-123.389846	-22.965023	0.170163
-126.852765	-17.985916	0.175168
-130.588401	-18.269684	0.180173
-134.356873	-20.352223	0.185178
-138.089821	-14.541543	0.190182
-142.025187	-19.499006	0.195187
-145.263878	-14.981426	0.200192
-149.581363	-3.227007	0.205197
-152.794016	-16.955596	0.210202
-156.480487	-13.076169	0.215206
-160.409113	-8.956244	0.220211
-163.792508	-17.149323	0.225216
-168.146474	-4.597429	0.230221
-171.780944	-22.243595	0.235226
-175.426646	-19.028230	0.240230
-179.354060	-12.202445	0.245235
-183.149728	-25.131472	0.250240
-186.803177	-14.626250	0.255245
-190.604587	-16.071093	0.260250
-194.410162	-12.268794	0.265254
-198.410839	-9.260090	0.270259
-201.703042	-21.253891	0.275264
-205.478845	-23.932806	0.280269
-209.485978	-26.631564	0.285274
-212.970949	-16.828125	0.290278
-216.896218	-15.258555	0.295283
-220.542754	-22.433424	0.300288
-224.508438	-12.192124	0.305293
-228.281161	-17.322056	0.310298
-231.834353	-16.590855	0.315302
-235.886563	-6.370416	0.320307
-239.445628	-14.883848	0.325312
-243.539196	-15.457236	0.330317
-246.986194	-16.318322	0.335322
-250.673549	-18.202315	0.340326
-254.480631	-13.191751	0.345331
-257.882525	-17.999206	0.350336
-262.016072	-17.402403	0.355341
-265.750521	-18.632312	0.360346
-269.957755	-17.935425	0.365350
-273.823915	-14.810878	0.370355
-277.035301	-22.190734	0.375360
-281.448206	-16.775921	0.380365
-284.962844	-21.872841	0.385370
-288.373380	-25.921940	0.390374
-292.217995	-17.734113	0.395379
-295.483072	-20.552760	0.400384
-299.806775	-11.640318	0.405389
-303.312520	-18.402298	0.410394
-307.113506	-17.871122	0.415398
-311.038281	-6.666402	0.420403
-314.598164	-18.241992	0.425408
-318.333610	-13.247497	0.430413
-322.136117	-13.443022	0.435418
-326.251324	-16.684142	0.440422
-330.274061	-16.003989	0.445427
-333.433645	-22.338643	0.450432
-337.307535	-14.518228	0.455437
-340.888154	-19.412143	0.460442
-344.573644	-20.143549	0.465446
-348.505553	-18.564821	0.470451
-352.205402	-20.571239	0.475456
-356.368874	-27.920395	0.480461
-360.203497	-15.892649	0.485466
-363.877573	-22.036308	0.490470
-367.378790	-20.781778	0.495475
-370.905055	-21.991146	0.500480
-374.763590	-22.248603	0.505485
-378.787861	-18.226601	0.510490
-382.535154	-24.473654	0.515494
-386.511840	-16.001247	0.520499
-389.983478	-21.787685	0.525504
-394.054304	-19.018194	0.530509
-397.665179	-23.645418	0.535514
-401.207633	-19.981009	0.540518
-405.279251	-15.484631	0.545523
-408.798653	-28.007954	0.550528
-412.456247	-15.290895	0.555533
-416.279517	-13.076554	0.560538
-419.930064	-24.235373	0.565542
-423.588156	-16.438248	0.570547
-427.574976	-23.899063	0.575552
-431.770960	-21.358679	0.580557
-435.312999	-18.157905	0.585562
-438.823909	-18.986429	0.590566
-442.637142	-20.987213	0.595571
-446.406417	-20.640651	0.600576
-450.241524	-17.415131	0.605581
-453.886715	-14.374472	0.610586
-457.525250	-21.266392	0.615590
-461.356323	-18.746386	0.620595
-464.980536	-15.092481	0.625600
-469.044479	-5.718191	0.630605
-472.690415	-27.772685	0.635610
-476.723373	-12.179187	0.640614
-480.691884	-15.457657	0.645619
-483.754366	-25.899747	0.650624
-487.621305	-10.849979	0.655629
-491.343562	-17.162356	0.660634
-494.965378	-10.973082	0.665638
-499.452214	-11.382296	0.670643
-503.007244	-26.239945	0.675648
-506.952746	-12.836534	0.680653
-510.545320	-25.745394	0.685658
-514.018554	-30.266686	0.690662
-518.056859	-15.694125	0.695667
-521.488024	-27.189009	0.700672
-525.451073	-13.360150	0.705677
-529.182883	-26.885395	0.710682
-532.742882	-26.848088	0.715686
-536.686706	-14.629176	0.720691
-540.363250	-29.169310	0.725696
-544.286873	-12.844133	0.730701
-548.385786	-15.483501	0.735706
-551.728859	-20.558534	0.740710
-555.578446	-9.124185	0.745715
-559.184154	-18.508007	0.750720
-563.138019	-16.863922	0.755725
-566.764501	-18.998416	0.760730
-570.151989	-26.007526	0.765734
-574.132805	-12.473794	0.770739
-578.119066	-19.954936	0.775744
-581.972733	-10.976753	0.780749
-585.868609	-11.489674	0.785754
-589.472051	-21.807350	0.790758
-593.387392	-14.571268	0.795763
-596.978705	-25.775524	0.800768
-600.833264	-13.373659	0.805773
-604.653388	-16.171007	0.810778
-608.028098	-23.871221	0.815782
-611.699638	-14.721823	0.820787
-615.622079	-20.249816	0.825792
-619.353755	-20.244874	0.830797
-623.243983	-16.579772	0.835802
-626.912669	-18.464582	0.840806
-630.957706	-14.164461	0.845811
-634.265870	-16.177824	0.850816
-638.317498	-16.262078	0.855821
-642.245946	-17.602320	0.860826
-645.760938	-13.626558	0.865830
-649.750083	-9.731144	0.870835
-653.213121	-17.945451	0.875840
-657.022132	-21.758453	0.880845
-660.948851	-21.182971	0.885850
-664.786857	-15.053522	0.890854
-668.531300	-13.184109	0.895859
-672.295953	-17.314830	0.900864
-675.991438	-8.374394	0.905869
-679.144262	-17.191734	0.910874
-683.164991	-16.607501	0.915878
-687.434579	-21.283549	0.920883
-691.064846	-23.462974	0.925888
-694.527271	-24.803482	0.930893
-698.748790	-20.834587	0.935898
-702.441270	-23.888709	0.940902
-706.286648	-16.988478	0.945907
-709.218599	-22.255134	0.950912
-713.213619	-26.115585	0.955917
-717.138673	-21.807689	0.960922
-721.177220	-20.630773	0.965926
-725.179113	-18.420512	0.970931
-728.504743	-29.550317	0.975936
-732.289211	-20.625546	0.980941
-736.120635	-16.370429	0.985946
-739.526057	-21.370567	0.990950
-743.539830	-26.036932	0.995955
-747.195084	-29.637816	1.000960
-751.453780	-26.784084	1.005965
-755.410846	-16.330457	1.010970
-758.914432	-24.992269	1.015974
-762.443316	-18.457922	1.020979
-766.086511	-22.368207	1.025984
-769.777415	-27.346322	1.030989
-773.712883	-15.688193	1.035994
-777.590315	-21.950065	1.040998
-781.272607	-21.102797	1.046003
-784.526684	-19.623814	1.051008
-788.755052	-17.984364	1.056013
-792.576872	-11.046762	1.061018
-796.203582	-21.495996	1.066022
-800.323613	-15.609834	1.071027
-803.885652	-9.800241	1.076032
-807.841334	-10.038311	1.081037
-811.512456	-18.684302	1.086042
-814.783260	-21.324688	1.091046
-818.817571	-14.597503	1.096051
-822.481979	-20.694658	1.101056
-826.647700	-6.769860	1.106061
-830.366917	-12.760475	1.111066
-833.528778	-10.747396	1.116070
-837.742141	-14.714653	1.121075
-841.108197	-20.194010	1.126080
-845.239057	-10.422071	1.131085
-849.081043	-12.029673	1.136090
-852.521884	-20.069024	1.141094
-856.592614	-6.572518	1.146099
-860.083541	-21.674786	1.151104
-863.898793	-22.714212	1.156109
-867.840976	-13.680442	1.161114
-871.381472	-29.116951	1.166118
-875.501212	-6.567342	1.171123
-878.793910	-22.540195	1.176128
-882.821025	-11.439665	1.181133
-886.804461	-17.365864	1.186138
-890.180434	-21.785445	1.191142
-894.352263	-19.774808	1.196147
-897.810603	-17.823049	1.201152
-901.692372	-15.522891	1.206157
-905.065916	-20.583070	1.211162
-908.623551	-24.404307	1.216166
-913.151463	-20.458586	1.221171
-916.428035	-25.132136	1.226176
-920.582348	-15.327942	1.231181
-924.315670	-14.185291	1.236186
-927.884165	-19.099149	1.241190
-931.575347	-21.523919	1.246195
-935.515632	-30.579234	1.251200
-939.126255	-20.133411	1.256205
-943.239518	-27.366515	1.261210
-946.845176	-19.222206	1.266214
-950.465762	-21.339696	1.271219
-953.948974	-27.128147	1.276224
-958.046376	-22.193070	1.281229
-961.723934	-21.923432	1.286234
-965.417918	-29.635119	1.291238
-969.696795	-25.650271	1.296243
-972.931976	-24.789052	1.301248
-976.492114	-21.964631	1.306253
-980.746952	-19.592067	1.311258
-984.478340	-16.279785	1.316262
-988.324020	-13.318218	1.321267
-991.744030	-19.127760	1.326272
-995.772575	-15.176590	1.331277
-999.542253	-19.230274	1.336282
-1002.938769	-22.268171	1.341286
-1006.894116	-10.064037	1.346291
-1010.674506	-24.295025	1.351296
-1014.528381	-12.614879	1.356301
-1018.147687	-19.885851	1.361306
-1021.750582	-29.855973	1.366310
-1025.880999	-10.740547	1.371315
-1029.464200	-17.206739	1.376320
-1033.034301	-15.244792	1.381325
-1037.007723	-25.598744	1.386330
-1040.544422	-34.803574	1.391334
-1044.812693	-19.852803	1.396339
-1048.440609	-10.332859	1.401344
-1052.076343	-8.369846	1.406349
-1056.099460	-7.320979	1.411354
-1059.126203	-20.686857	1.416358
-1063.337757	-21.055450	1.421363
-1067.286972	-28.762411	1.426368
-1070.937348	-9.912932	1.431373
-1075.001502	-14.233195	1.436378
-1078.098234	-27.212537	1.441382
-1082.255553	-13.471597	1.446387
-1085.622943	-18.196606	1.451392
-1089.394854	-27.067275	1.456397
-1093.829785	-4.000144	1.461402
-1097.247124	-16.906102	1.466406
-1100.813237	-18.114302	1.471411
-1104.331323	-11.287882	1.476416
-1108.117342	-12.605969	1.481421
-1112.333409	-17.127361	1.486426
-1116.005422	-13.644603	1.491430
-1120.270467	-15.650841	1.496435
-1123.822811	-7.420182	1.501440
-1127.157700	-19.404165	1.506445
-1130.982770	-13.061594	1.511450
-1134.721137	-18.182908	1.516454
-1138.600751	-8.263025	1.521459
-1142.193872	-16.883099	1.526464
-1145.955968	-3.877047	1.531469
-1149.796895	-11.743119	1.536474
-1153.465845	-13.709053	1.541478
-1157.713841	-13.991221	1.546483
-1161.231873	-12.193526	1.551488
-1165.059888	-8.387693	1.556493
-1168.960985	-15.815179	1.561498
-1172.036094	-11.670919	1.566502
-1175.971371	-15.839737	1.571507
-1179.666940	-25.178196	1.576512
-1183.509627	-21.504027	1.581517
-1187.543524	-11.262922	1.586522
-1191.425855	-20.432711	1.591526
-1195.311705	-5.771521	1.596531
-1198.771461	-13.764730	1.601536
-1202.122290	-31.577482	1.606541
-1206.313963	-25.595594	1.611546
-1209.695859	-22.895538	1.616550
-1213.829151	-12.196949	1.621555
-1217.724777	-18.314803	1.626560
-1221.534155	-24.295065	1.631565
-1225.350557	-14.574397	1.636570
-1229.018419	-24.644166	1.641574
-1232.652551	-11.191703	1.646579
-1235.836630	-12.949676	1.651584
-1239.915032	-9.665036	1.656589
-1244.067032	-16.736852	1.661594
-1247.706844	-13.553927	1.666598
-1251.766405	-16.266150	1.671603
-1255.165151	-14.272944	1.676608
-1258.786637	-9.082363	1.681613
-1262.885278	-14.287728	1.686618
-1266.279574	-16.144476	1.691622
-1270.470024	-16.123417	1.696627
-1273.870082	-19.923571	1.701632
-1277.601997	-13.792792	1.706637
-1281.581108	-14.914112	1.711642
-1285.245868	-19.887686	1.716646
-1289.154286	-13.052141	1.721651
-1292.631665	-27.059891	1.726656
-1296.442850	-20.780783	1.731661
-1300.490237	-22.484062	1.736666
-1303.913129	-22.185261	1.741670
-1307.841487	-12.323544	1.746675
-1311.494047	-7.788638	1.751680
-1315.097836	-14.768303	1.756685
-1319.348311	-12.843670	1.761690
-1322.747679	-23.013027	1.766694
-1326.668480	-16.396210	1.771699
-1330.378260	-14.606991	1.776704
-1334.244039	-21.468991	1.781709
-1338.034117	-11.115287	1.786714
-1341.594733	-12.834915	1.791718
-1345.558963	-23.688080	1.796723
-1349.225007	-22.680099	1.801728
-1352.910159	-15.733540	1.806733
-1356.632409	-21.929364	1.811738
-1360.404172	-24.892461	1.816742
-1364.214422	-8.394975	1.821747
-1368.074505	-22.314530	1.826752
-1371.577711	-21.931810	1.831757
-1375.801241	-7.952709	1.836762
-1379.021614	-16.316683	1.841766
-1382.990203	-5.365060	1.846771
-1386.913784	-12.429026	1.851776
-1390.415124	-17.736089	1.856781
-1394.353694	-22.463801	1.861786
-1397.843874	-18.763720	1.866790
-1401.817283	-5.707690	1.871795
-1405.692628	-14.255338	1.876800
-1409.410683	-12.250208	1.881805
-1413.116776	-11.136368	1.886810
-1416.827993	-15.501483	1.891814
-1420.718534	-8.856239	1.896819
-1424.703306	-9.181639	1.901824
-1428.162716	-16.698308	1.906829
-1431.856876	-14.542431	1.911834
-1435.557379	-13.582410	1.916838
-1439.238045	-9.605767	1.921843
-1443.226144	-13.749891	1.926848
-1446.956654	-18.001482	1.931853
-1450.963120	-13.444387	1.936858
-1454.420362	-25.584871	1.941862
-1458.201119	-16.568125	1.946867
-1461.924987	-20.459640	1.951872
-1465.494286	-18.330012	1.956877
-1469.826214	-19.331430	1.961882
-1473.230781	-26.418422	1.966886
-1477.208398	-13.128222	1.971891
-1480.691752	-17.501336	1.976896
-1484.601929	-28.060129	1.981901
-1488.487951	-9.243303	1.986906
-1491.838107	-26.125311	1.991910
-1496.125555	-16.391866	1.996915
-1500.076756	-22.946422	2.006912
-1500.468997	-24.740264	2.016909
-1498.128019	-19.377154	2.026906
-1495.083226	-20.330381	2.036902
-1493.384708	-17.246989	2.046899
-1491.691142	-16.384361	2.056896
-1489.653507	-17.146291	2.066893
-1487.430987	-18.635715	2.076890
-1485.732175	-12.179762	2.086886
-1483.971488	-16.486252	2.096883
-1481.873444	-8.553188	2.106880
-1479.734050	-15.639246	2.116877
-1478.055639	-9.835275	2.126874
-1476.077862	-14.725994	2.136870
-1474.519462	-13.672762	2.146867
-1472.400526	-12.753500	2.156864
-1470.533551	-10.672846	2.166861
-1468.583180	-8.022917	2.176858
-1466.760675	-14.121912	2.186854
-1464.798406	-17.210153	2.196851
-1462.801403	-10.651931	2.206848
-1460.773154	-9.902872	2.216845
-1459.375421	-11.596510	2.226842
-1457.221256	-18.520704	2.236838
-1455.033147	-14.590424	2.246835
-1453.603876	-15.163328	2.256832
-1451.749666	-15.283228	2.266829
-1449.681883	-13.152606	2.276826
-1447.944770	-24.904704	2.286822
-1446.032297	-24.094463	2.296819
-1443.784356	-16.559574	2.306816
-1442.256315	-23.814545	2.316813
-1440.489014	-16.474268	2.326810
-1438.108725	-15.279457	2.336806
-1436.354093	-14.282882	2.346803
-1434.643842	-15.567076	2.356800
-1432.961516	-9.896327	2.366797
-1431.022791	-13.124454	2.376794
-1429.300142	-9.894876	2.386790
-1427.172236	-11.646987	2.396787
-1425.237638	-19.470726	2.406784
-1423.343661	-14.523854	2.416781
-1421.407498	-12.424237	2.426778
-1419.549173	-9.516372	2.436774
-1417.592409	-12.910006	2.446771
-1416.049920	-15.943628	2.456768
-1414.046346	-15.724257	2.466765
-1412.031686	-9.061445	2.476762
-1410.050588	-14.971056	2.486758
-1408.447523	-10.773375	2.496755
-1406.589464	-15.715922	2.506752
-1404.686158	-15.932065	2.516749
-1402.583383	-14.376998	2.526746
-1400.744157	-15.067610	2.536742
-1398.779181	-8.488410	2.546739
-1396.832168	-5.165254	2.556736
-1395.287043	-11.807153	2.566733
-1393.297858	-14.921750	2.576730
-1391.347032	-12.364985	2.586726
-1389.660078	-16.490657	2.596723
-1387.578284	-12.064870	2.606720
-1385.886471	-19.814974	2.616717
-1384.224288	-14.377804	2.626714
-1382.295993	-11.654792	2.636710
-1379.681650	-11.793697	2.646707
-1378.326107	-14.129476	2.656704
-1376.332433	-15.092688	2.666701
-1374.472841	-13.094455	2.676698
-1372.556425	-21.450502	2.686694
-1370.831536	-16.738618	2.696691
-1368.798052	-16.790836	2.706688
-1366.918593	-15.419457	2.716685
-1365.218515	-18.178277	2.726682
-1363.329729	-17.427331	2.736678
-1361.383257	-21.000849	2.746675
-1359.613435	-18.197187	2.756672
-1357.801650	-15.436557	2.766669
-1355.666982	-18.277572	2.776666
-1353.980895	-10.597377	2.786662
-1351.641063	-11.570194	2.796659
-1349.980095	-6.049115	2.806656
-1348.006997	-10.574249	2.816653
-1346.495020	-19.822370	2.826650
-1344.480918	-11.896259	2.836646
-1342.402854	-16.564504	2.846643
-1340.971286	-11.352485	2.856640
-1338.513348	-8.932113	2.866637
-1337.252349	-12.687988	2.876634
-1335.247935	-9.399230	2.886630
-1333.422502	-13.352822	2.896627
-1331.087167	-8.154414	2.906624
-1329.282509	-11.075211	2.916621
-1327.572866	-16.565517	2.926618
-1325.711112	-13.088126	2.936614
-1323.609525	-16.285394	2.946611
-1321.887455	-14.838259	2.956608
-1320.169620	-8.157848	2.966605
-1318.177212	-16.807072	2.976602
-1316.270770	-14.865237	2.986598
-1314.383862	-15.045523	2.996595
-1312.482209	-20.421289	3.006592
-1310.951396	-14.811456	3.016589
-1308.747811	-18.257140	3.026586
-1306.978884	-16.642232	3.036582
-1305.005826	-17.647873	3.046579
-1302.938425	-19.837025	3.056576
-1301.266768	-20.988630	3.066573
-1299.674411	-15.571796	3.076570
-1297.640829	-14.035556	3.086566
-1295.489733	-15.792839	3.096563
-1293.853079	-11.407819	3.106560
-1291.963429	-16.456388	3.116557
-1289.738255	-14.235549	3.126554
-1288.060135	-16.362382	3.136550
-1286.541140	-9.503278	3.146547
-1284.526822	-17.557565	3.156544
-1282.603137	-16.535824	3.166541
-1280.718723	-12.174660	3.176538
-1278.808738	-14.745964	3.186534
-1276.754022	-10.508368	3.196531
-1274.852488	-9.961493	3.206528
-1272.972133	-17.604333	3.216525
-1271.473120	-10.743599	3.226522
-1269.490447	-20.589639	3.236518
-1267.283318	-19.758513	3.246515
-1265.591546	-22.566457	3.256512
-1263.665681	-20.746108	3.266509
-1261.886175	-13.429737	3.276506
-1260.198375	-16.221254	3.286502
-1258.087220	-22.491027	3.296499
-1256.097567	-21.820873	3.306496
-1254.173880	-20.148587	3.316493
-1252.689396	-12.933412	3.326490
-1250.660300	-16.900589	3.336486
-1248.789382	-14.591436	3.346483
-1246.593271	-20.963217	3.356480
-1244.963510	-16.174430	3.366477
-1243.227649	-16.887849	3.376474
-1241.412620	-15.289741	3.386470
-1239.016043	-17.190468	3.396467
-1237.761700	-20.362598	3.406464
-1235.950544	-11.556015	3.416461
-1233.529666	-9.783277	3.426458
-1231.791189	-16.667598	3.436454
-1229.877087	-7.245906	3.446451
-1228.013974	-10.982820	3.456448
-1226.348224	-13.909732	3.466445
-1224.315948	-11.053225	3.476442
-1222.321432	-12.059072	3.486438
-1220.604593	-15.264154	3.496435
-1218.648847	-7.560685	3.506432
-1216.818725	-8.737588	3.516429
-1215.051902	-8.101212	3.526426
-1213.206543	-10.281598	3.536422
-1211.466397	-8.270432	3.546419
-1209.177926	-3.228602	3.556416
-1207.282186	-8.257558	3.566413
-1205.719212	-2.985946	3.576410
-1203.581467	-12.716232	3.586406
-1201.743702	-9.250687	3.596403
-1199.878396	-12.016882	3.606400
-1198.102182	-11.801994	3.616397
-1196.532899	-9.806107	3.626394
-1194.482952	-6.099772	3.636390
-1192.224544	-6.397825	3.646387
-1190.570365	-8.200235	3.656384
-1188.707988	-11.171216	3.666381
-1186.771678	-11.179304	3.676378
-1185.056414	-11.272020	3.686374
-1183.142098	-8.440811	3.696371
-1180.969264	-14.510393	3.706368
-1179.301597	-13.294443	3.716365
-1177.438860	-9.223403	3.726362
-1175.499330	-7.735162	3.736358
-1173.513593	-2.837486	3.746355
-1171.904661	-9.089992	3.756352
-1170.130100	-7.002195	3.766349
-1168.020689	-1.025359	3.776346
-1165.842870	0.418449	3.786342
-1164.336244	-3.555063	3.796339
-1162.552064	-6.096673	3.806336
-1160.529934	-2.218487	3.816333
-1158.667920	-6.419382	3.826330
-1156.896911	-8.453619	3.836326
-1154.685566	-9.817785	3.846323
-1153.146635	-7.498065	3.856320
-1151.333507	-12.076393	3.866317
-1149.161708	-7.195834	3.876314
-1147.384692	-10.792597	3.886310
-1145.397240	-6.604115	3.896307
-1143.365299	-9.839031	3.906304
-1141.893201	-7.576505	3.916301
-1139.887811	-3.525097	3.926298
-1137.863784	-3.199811	3.936294
-1136.341141	-5.251139	3.946291
-1134.484690	-2.934837	3.956288
-1132.395220	-11.109980	3.966285
-1130.541469	-9.508504	3.976282
-1128.516412	-11.741258	3.986278
-1126.847426	-12.702839	3.996275
-1124.993228	-10.433538	4.006272
-1122.879761	-9.467288	4.016269
-1120.905218	-5.936716	4.026266
-1119.177648	-9.871336	4.036262
-1117.548502	-7.788655	4.046259
-1115.585952	-10.431397	4.056256
-1113.351733	-12.332864	4.066253
-1111.843221	-14.554020	4.076250
-1110.269770	-7.469814	4.086246
-1108.139096	-6.509460	4.096243
-1105.939481	-12.066949	4.106240
-1104.136096	-16.773156	4.116237
-1102.286466	-10.751544	4.126234
-1100.550110	-15.380710	4.136230
-1098.660002	-9.428727	4.146227
-1096.674648	-11.921944	4.156224
-1094.637833	-15.247598	4.166221
-1093.010747	-7.118806	4.176218
-1091.054827	-18.725692	4.186214
-1089.050437	-20.511423	4.196211
-1087.305373	-14.810965	4.206208
-1085.660126	-10.806109	4.216205
-1083.760127	-8.491996	4.226202
-1081.851689	-10.355530	4.236198
-1079.692439	-20.153888	4.246195
-1077.946350	-19.482512	4.256192
-1076.238542	-17.072914	4.266189
-1074.203730	-14.421939	4.276186
-1072.029097	-13.064376	4.286182
-1070.468706	-13.596442	4.296179
-1068.624800	-14.071228	4.306176
-1066.823757	-16.880725	4.316173
-1064.655090	-8.740648	4.326170
-1062.847656	-15.026415	4.336166
-1060.974332	-12.172755	4.346163
-1059.368462	-14.087347	4.356160
-1057.540028	-11.687555	4.366157
-1055.394166	-3.027503	4.376154
-1053.288910	-14.801936	4.386150
-1051.685235	-9.573040	4.396147
-1049.990945	-11.853873	4.406144
-1047.874667	-12.039052	4.416141
-1045.933349	-12.717295	4.426138
-1044.170796	-6.913808	4.436134
-1042.506227	-11.755662	4.446131
-1040.484387	-11.895730	4.456128
-1038.405569	-13.846481	4.466125
-1036.554400	-11.159783	4.476122
-1035.022276	-14.728347	4.486118
-1033.115624	-11.557890	4.496115
-1030.933534	-17.990400	4.506112
-1029.198711	-11.482996	4.516109
-1027.465748	-9.468960	4.526106
-1025.456419	-13.554368	4.536102
-1023.535717	-8.194579	4.546099
-1021.439312	-11.888123	4.556096
-1019.809904	-15.655394	4.566093
-1017.915111	-10.090931	4.576090
-1016.156671	-6.040967	4.586086
-1014.048484	-12.709538	4.596083
-1012.223618	-10.042297	4.606080
-1010.357046	-12.975917	4.616077
-1008.576635	-5.323157	4.626074
-1006.787147	-7.710764	4.636070
-1004.888254	-6.841140	4.646067
-1002.992477	-8.554167	4.656064
-1000.872594	-19.146688	4.666061
-999.114326	-12.030380	4.676058
-997.250956	-13.498219	4.686054
-995.513999	-15.654785	4.696051
-993.453084	-10.192657	4.706048
-991.720344	-12.005916	4.716045
-989.849693	-12.094918	4.726042
-987.852169	-9.647901	4.736038
-985.925599	-14.771618	4.746035
-984.085960	-8.160938	4.756032
-982.417424	-14.156015	4.766029
-980.539520	-14.006171	4.776026
-978.650718	-10.730182	4.786022
-976.360284	-4.769480	4.796019
-974.851174	-12.797999	4.806016
-973.092575	-10.540128	4.816013
-971.047964	-12.900613	4.826010
-969.013673	-13.047346	4.836006
-967.187901	-12.004946	4.846003
-965.317578	-11.054932	4.856000
-963.400780	-8.209721	4.865997
-961.562198	-8.081994	4.875994
-959.462915	-2.351231	4.885990
-957.875361	-6.435454	4.895987
-956.139853	-10.489651	4.905984
-954.328844	-10.076457	4.915981
-952.333861	-11.516361	4.925978
-950.258634	-11.985413	4.935974
-948.544085	-18.429928	4.945971
-946.773543	-11.669222	4.955968
-944.513048	-9.712638	4.965965
-942.849129	-12.834853	4.975962
-941.191991	-13.001780	4.985958
-939.025321	-10.854924	4.995955
-937.317995	-8.579352	5.005952
-935.224535	-9.351306	5.015949
-933.469555	-17.941746	5.025946
-931.479055	-5.970947	5.035942
-929.940629	-11.062557	5.045939
-927.840587	-13.049764	5.055936
-926.091709	-12.239772	5.065933
-924.104097	-11.649531	5.075930
-922.305463	-12.633278	5.085926
-920.295094	-13.350880	5.095923
-918.275276	-7.504741	5.105920
-916.607397	-7.535999	5.115917
-914.882291	-7.240092	5.125914
-912.824563	-10.914728	5.135910
-910.859932	-11.956587	5.145907
-909.174534	-11.425379	5.155904
-907.270485	-6.375454	5.165901
-905.097810	-10.008463	5.175898
-903.643838	-7.986041	5.185894
-901.592924	-9.641687	5.195891
-899.767269	-11.872366	5.205888
-897.187390	-13.383637	5.215885
-895.181595	-13.928381	5.225882
-893.773021	-6.681861	5.235878
-891.993983	-12.874548	5.245875
-890.465520	-11.959814	5.255872
-888.626201	-12.591620	5.265869
-886.908330	-14.247689	5.275866
-884.783781	-11.854048	5.285862
-882.498678	-16.112905	5.295859
-880.907565	-14.346079	5.305856
-879.113505	-17.290110	5.315853
-877.300608	-4.610336	5.325850
-875.370233	-10.538261	5.335846
-873.526655	-6.264954	5.345843
-871.655320	-12.137647	5.355840
-869.667554	-10.505280	5.365837
-867.815426	-10.482277	5.375834
-865.924281	-8.242355	5.385830
-863.937625	-15.827686	5.395827
-861.952541	-11.177521	5.405824
-860.187132	-7.089074	5.415821
-858.613356	-9.284191	5.425818
-856.787038	-10.370209	5.435814
-854.535393	-15.899478	5.445811
-852.687948	-9.676776	5.455808
-850.719686	-11.153376	5.465805
-849.413859	-10.548812	5.475802
-847.137599	-10.268334	5.485798
-845.042723	-15.867270	5.495795
-843.573684	-13.575639	5.505792
-841.681875	-6.898967	5.515789
-839.528303	-9.339918	5.525786
-837.717691	-7.063414	5.535782
-835.718243	-6.399200	5.545779
-834.141738	-8.599474	5.555776
-831.968816	-11.965616	5.565773
-830.348956	-13.571240	5.575770
-828.261374	-8.934271	5.585766
-826.607812	-12.482647	5.595763
-824.595214	-14.313680	5.605760
-822.978009	-10.531513	5.615757
-821.227433	-15.041181	5.625754
-818.992475	-13.969338	5.635750
-816.906333	-11.776337	5.645747
-815.232226	-15.575882	5.655744
-813.511622	-16.212337	5.665741
-811.604357	-5.303376	5.675738
-809.455030	-17.722560	5.685734
-807.736460	-18.838684	5.695731
-805.870614	-19.856771	5.705728
-804.086298	-17.493933	5.715725
-802.117847	-16.906841	5.725722
-799.998284	-14.652852	5.735718
-798.385678	-13.246245	5.745715
-796.565807	-19.218023	5.755712
-794.794693	-16.283068	5.765709
-792.805850	-14.488177	5.775706
-790.937422	-15.411928	5.785702
-789.070753	-19.761708	5.795699
-786.881597	-14.686202	5.805696
-785.470770	-12.734176	5.815693
-783.588339	-16.314368	5.825690
-781.220163	-19.834830	5.835686
-779.539066	-20.032314	5.845683
-777.714834	-16.262680	5.855680
-776.119554	-15.170656	5.865677
-773.821859	-13.513535	5.875674
-772.016454	-19.126141	5.885670
-770.299427	-26.965141	5.895667
-768.469077	-17.547012	5.905664
-766.721258	-19.217255	5.915661
-764.486452	-16.484284	5.925658
-762.855290	-17.985880	5.935654
-760.680519	-26.019615	5.945651
-758.922868	-17.889329	5.955648
-757.020335	-19.443767	5.965645
-755.292469	-17.640290	5.975642
-753.589258	-17.707080	5.985638
-751.167063	-17.582465	5.995635
-749.678378	-21.353910	6.005632
-747.731413	-31.129115	6.015629
-745.834068	-23.346411	6.025626
-743.974216	-21.290862	6.035622
-742.218178	-22.643454	6.045619
-740.101697	-19.139971	6.055616
-738.207024	-18.182613	6.065613
-736.560145	-22.134069	6.075610
-734.582215	-14.719492	6.085606
-732.741694	-21.169787	6.095603
-730.770744	-20.270404	6.105600
-729.148776	-26.831029	6.115597
-727.058940	-15.766438	6.125594
-725.316579	-16.911569	6.135590
-723.217284	-21.311109	6.145587
-721.279332	-18.056971	6.155584
-719.752907	-13.445485	6.165581
-717.757567	-16.064724	6.175578
-716.032072	-20.919257	6.185574
-713.946296	-14.428211	6.195571
-711.755576	-13.475511	6.205568
-710.149788	-18.481437	6.215565
-708.354520	-13.529222	6.225562
-706.603656	-17.358330	6.235558
-704.507369	-19.196321	6.245555
-702.510606	-22.388932	6.255552
-701.192040	-21.634742	6.265549
-698.976715	-19.585437	6.275546
-696.915957	-21.414586	6.285542
-695.200005	-22.438633	6.295539
-693.002795	-19.792743	6.305536
-691.180420	-21.181162	6.315533
-689.908474	-22.041095	6.325530
-687.856645	-16.261442	6.335526
-685.685549	-20.506634	6.345523
-683.738191	-18.378178	6.355520
-682.306392	-18.264177	6.365517
-680.155036	-14.557789	6.375514
-678.433094	-16.956465	6.385510
-676.546886	-16.539284	6.395507
-674.491271	-25.997065	6.405504
-672.654027	-17.601531	6.415501
-670.778450	-10.770538	6.425498
-668.963545	-12.647221	6.435494
-666.971889	-14.640567	6.445491
-665.122469	-13.481708	6.455488
-663.368435	-18.774977	6.465485
-661.750873	-6.336954	6.475482
-659.403501	-13.027663	6.485478
-657.654393	-14.424877	6.495475
-655.556491	-12.603082	6.505472
-653.851203	-13.832238	6.515469
-652.103504	-11.752377	6.525466
-650.338554	-17.358435	6.535462
-648.536523	-16.485675	6.545459
-646.979462	-18.929038	6.555456
-645.049833	-16.072978	6.565453
-642.554664	-11.699909	6.575450
-640.429821	-22.084518	6.585446
-638.896859	-22.251918	6.595443
-637.072291	-22.129593	6.605440
-635.119190	-22.684646	6.615437
-633.157749	-22.323661	6.625434
-631.237427	-19.792946	6.635430
-629.660304	-22.845818	6.645427
-627.512946	-21.584532	6.655424
-625.833650	-19.719514	6.665421
-624.035693	-21.986613	6.675418
-622.289908	-22.541690	6.685414
-620.125590	-25.914161	6.695411
-618.087177	-22.699672	6.705408
-616.204558	-26.571870	6.715405
-614.709435	-20.561101	6.725402
-612.537685	-15.353169	6.735398
-610.840587	-18.058882	6.745395
-608.884361	-23.981259	6.755392
-607.194629	-22.825263	6.765389
-605.331083	-15.985978	6.775386
-603.015178	-29.964765	6.785382
-601.186829	-20.069328	6.795379
-599.210428	-26.860183	6.805376
-597.784407	-15.353093	6.815373
-596.089931	-19.937327	6.825370
-593.685193	-14.708177	6.835366
-591.841896	-18.664078	6.845363
-590.058945	-15.910854	6.855360
-588.028284	-11.292989	6.865357
-586.426571	-11.499760	6.875354
-584.837912	-10.326021	6.885350
-582.737272	-15.786714	6.895347
-580.665794	-18.782742	6.905344
-578.978964	-16.361523	6.915341
-577.058657	-17.509711	6.925338
-574.888411	-13.984662	6.935334
-573.282295	-13.246336	6.945331
-571.434043	-21.815124	6.955328
-569.393244	-16.145704	6.965325
-567.526214	-16.222741	6.975322
-565.777464	-23.809312	6.985318
-563.605293	-14.314552	6.995315
-561.984890	-16.581664	7.005312
-560.149023	-20.890038	7.015309
-558.426108	-16.216671	7.025306
-556.618924	-13.852556	7.035302
-554.219741	-12.620378	7.045299
-552.624634	-18.162921	7.055296
-550.911759	-14.102155	7.065293
-548.589990	-18.301824	7.075290
-546.926071	-16.175344	7.085286
-544.994213	-16.906930	7.095283
-543.188840	-9.058820	7.105280
-541.347910	-13.265360	7.115277
-539.361888	-14.828227	7.125274
-537.469389	-7.371397	7.135270
-535.646194	-16.537742	7.145267
-533.975031	-7.929237	7.155264
-532.218973	-9.933788	7.165261
-530.254683	-2.939997	7.175258
-528.109845	-6.440334	7.185254
-526.134525	-6.233056	7.195251
-524.409279	-13.013743	7.205248
-522.873020	-16.110548	7.215245
-520.426485	-9.477992	7.225242
-518.747434	-12.526551	7.235238
-517.170506	-4.621401	7.245235
-515.191339	-6.304733	7.255232
-512.996244	-11.827826	7.265229
-511.213443	-9.672938	7.275226
-509.478824	-8.230355	7.285222
-507.423889	-16.363166	7.295219
-505.808797	-15.676755	7.305216
-504.153537	-11.895698	7.315213
-501.917770	-9.922099	7.325210
-499.795091	-13.567293	7.335206
-498.128675	-11.823281	7.345203
-496.281232	-8.955547	7.355200
-494.533412	-14.921923	7.365197
-492.588908	-11.513897	7.375194
-490.726495	-13.996458	7.385190
-488.734023	-8.186611	7.395187
-486.773762	-2.701615	7.405184
-485.124421	-6.801726	7.415181
-483.256570	-5.069349	7.425178
-481.328178	-12.648245	7.435174
-479.394708	-10.667398	7.445171
-477.608279	-7.167796	7.455168
-475.686168	-10.023040	7.465165
-473.981766	-10.037714	7.475162
-471.844688	-10.222542	7.485158
-469.907476	-16.157569	7.495155
-467.925502	-13.633405	7.505152
-466.199255	-8.475757	7.515149
-464.300723	-7.323003	7.525146
-462.668804	-10.420840	7.535142
-460.769892	-6.077081	7.545139
-458.525430	-10.006954	7.555136
-456.643662	-5.422031	7.565133
-455.065243	-9.706586	7.575130
-453.231517	-18.337713	7.585126
-451.383312	-13.204270	7.595123
-449.516188	-17.020187	7.605120
-447.300364	-16.622304	7.615117
-445.688063	-21.651211	7.625114
-443.860891	-16.463877	7.635110
-441.663790	-25.678813	7.645107
-440.033412	-21.094788	7.655104
-438.180682	-18.846803	7.665101
-436.526295	-13.677658	7.675098
-434.328319	-16.652713	7.685094
-432.530287	-19.961792	7.695091
-430.434340	-20.762122	7.705088
-428.668294	-19.807658	7.715085
-426.719850	-15.965995	7.725082
-424.897947	-17.155191	7.735078
-423.324510	-24.385252	7.745075
-421.564211	-18.268271	7.755072
-419.201755	-19.139571	7.765069
-417.396527	-18.278197	7.775066
-415.574827	-18.965247	7.785062
-413.725900	-20.270855	7.795059
-411.824121	-19.197526	7.805056
-409.869094	-17.570591	7.815053
-408.460113	-14.007508	7.825050
-406.064267	-15.905708	7.835046
-404.385817	-21.976208	7.845043
-402.488393	-16.560057	7.855040
-400.723925	-17.566379	7.865037
-398.680739	-20.085630	7.875034
-396.910592	-17.314423	7.885030
-394.993300	-16.001977	7.895027
-393.082597	-12.043732	7.905024
-391.045037	-20.622099	7.915021
-389.507270	-16.256934	7.925018
-387.463886	-16.350936	7.935014
-385.529714	-18.257505	7.945011
-383.559539	-24.224571	7.955008
-381.902455	-14.715277	7.965005
-379.994212	-21.507718	7.975002
-378.136078	-11.397360	7.984998
-375.948883	-18.706447	7.994995
-374.664211	-18.200873	8.004992
-372.275573	-16.859457	8.014989
-370.498937	-14.768215	8.024986
-368.854883	-9.878422	8.034982
-366.892474	-14.775287	8.044979
-364.638115	-12.814000	8.054976
-362.997454	-14.976847	8.064973
-361.421508	-16.275147	8.074970
-359.320937	-17.440892	8.084966
-357.402636	-19.286483	8.094963
-355.451524	-17.886247	8.104960
-354.063478	-11.255037	8.114957
-351.948758	-12.759352	8.124954
-349.774640	-9.443128	8.134950
-347.758899	-11.026374	8.144947
-346.100422	-10.326253	8.154944
-344.359883	-10.853449	8.164941
-342.645494	-11.111204	8.174938
-340.631781	-11.917275	8.184934
-338.694089	-13.192788	8.194931
-336.900519	-15.147924	8.204928
-334.862642	-16.737851	8.214925
-333.093835	-20.482722	8.224922
-331.151694	-13.561011	8.234918
-329.299028	-18.735589	8.244915
-327.406348	-13.105457	8.254912
-325.611928	-17.347047	8.264909
-323.654768	-18.240390	8.274906
-321.960424	-19.724936	8.284902
-319.581298	-24.680394	8.294899
-317.865953	-19.741948	8.304896
-316.411580	-16.985004	8.314893
-314.601878	-17.071639	8.324890
-312.531105	-18.739430	8.334886
-310.176396	-18.450434	8.344883
-308.693808	-21.380645	8.354880
-306.945712	-21.530071	8.364877
-304.775548	-14.791582	8.374874
-303.078371	-18.970262	8.384870
-301.308158	-19.276374	8.394867
-299.129725	-13.844993	8.404864
-297.319685	-17.778002	8.414861
-295.714714	-20.003002	8.424858
-293.562393	-16.730616	8.434854
-291.773323	-7.243893	8.444851
-289.881814	-18.723097	8.454848
-288.012338	-18.940833	8.464845
-286.131475	-11.744035	8.474842
-284.179042	-18.134514	8.484838
-282.485653	-18.635191	8.494835
-280.710749	-21.935733	8.504832
-278.725176	-16.847760	8.514829
-276.593102	-12.032644	8.524826
-274.734904	-19.505446	8.534822
-273.144740	-16.119621	8.544819
-271.037973	-14.693635	8.554816
-269.065433	-17.960980	8.564813
-267.430321	-19.769193	8.574810
-265.488112	-20.102732	8.584807
-263.682048	-16.083465	8.594803
-261.883278	-24.374143	8.604800
-260.129205	-10.473368	8.614797
-258.091009	-18.142261	8.624794
-256.112684	-18.798928	8.634791
-253.966156	-19.318230	8.644787
-252.119029	-19.390265	8.654784
-250.453467	-18.983316	8.664781
-248.692509	-17.746851	8.674778
-247.064206	-16.246052	8.684775
-245.230500	-19.240164	8.694771
-242.721427	-15.759409	8.704768
-241.275719	-10.934180	8.714765
-239.099827	-12.468688	8.724762
-237.402957	-16.137274	8.734759
-235.304518	-16.010986	8.744755
-233.951102	-19.043695	8.754752
-231.926681	-16.319261	8.764749
-229.701078	-10.407444	8.774746
-227.790309	-12.771210	8.784743
-226.151347	-20.872148	8.794739
-224.479278	-13.814079	8.804736
-222.299621	-13.242845	8.814733
-220.441167	-15.025094	8.824730
-218.575083	-18.471200	8.834727
-216.671859	-17.784788	8.844723
-214.704878	-15.100119	8.854720
-212.891789	-16.976175	8.864717
-211.120369	-12.354491	8.874714
-209.351800	-14.465020	8.884711
-206.901669	-24.140152	8.894707
-205.465905	-24.599658	8.904704
-203.786513	-25.776997	8.914701
-201.790176	-20.461727	8.924698
-199.565298	-31.163536	8.934695
-198.276252	-22.364314	8.944691
-195.954528	-20.765724	8.954688
-194.151170	-25.993915	8.964685
-192.388950	-27.999205	8.974682
-190.538297	-25.951219	8.984679
-188.401634	-23.468873	8.994675
-186.768452	-24.540931	9.004672
-184.960333	-20.774564	9.014669
-183.022030	-24.446905	9.024666
-181.031968	-19.007456	9.034663
-179.171496	-24.202119	9.044659
-177.351729	-24.372363	9.054656
-175.508924	-19.973626	9.064653
-173.668954	-22.332366	9.074650
-171.545219	-22.033216	9.084647
-169.844755	-22.444943	9.094643
-168.041821	-21.564067	9.104640
-166.263033	-27.195687	9.114637
-164.162772	-24.426456	9.124634
-162.154098	-25.804736	9.134631
-160.196077	-20.642789	9.144627
-158.779668	-24.290250	9.154624
-156.784055	-24.243801	9.164621
-154.727235	-21.985527	9.174618
-153.019932	-23.805184	9.184615
-151.079176	-20.628379	9.194611
-149.448098	-20.282173	9.204608
-147.458735	-16.718383	9.214605
-145.325293	-21.861844	9.224602
-143.169264	-6.940361	9.234599
-141.851790	-16.960491	9.244595
-139.702035	-19.566009	9.254592
-137.774881	-21.371790	9.264589
-135.907735	-22.203251	9.274586
-134.284392	-20.951058	9.284583
-132.237683	-22.567489	9.294579
-130.351915	-28.074049	9.304576
-128.642775	-29.737665	9.314573
-126.670004	-23.984357	9.324570
-124.990072	-29.401226	9.334567
-122.985128	-29.163606	9.344563
-120.999774	-26.320738	9.354560
-119.087882	-25.550369	9.364557
-117.398261	-22.079253	9.374554
-115.558017	-23.634305	9.384551
-113.294699	-25.053176	9.394547
-111.534111	-29.126582	9.404544
-109.795118	-26.337554	9.414541
-107.883236	-16.677645	9.424538
-106.005491	-14.438122	9.434535
-104.262418	-20.187164	9.444531
-102.139438	-18.296243	9.454528
-100.530483	-19.280693	9.464525
-98.504772	-12.956325	9.474522
-96.886283	-17.221790	9.484519
-94.705599	-18.731671	9.494515
-92.845801	-19.846139	9.504512
-91.138797	-17.543047	9.514509
-89.162081	-14.457191	9.524506
-87.357412	-18.247088	9.534503
-85.612687	-15.031057	9.544499
-83.462559	-16.826581	9.554496
-81.642192	-13.453666	9.564493
-79.338723	-15.636812	9.574490
-77.965649	-15.219394	9.584487
-76.131673	-18.786589	9.594483
-73.842462	-22.655361	9.604480
-72.398807	-20.561294	9.614477
-70.391114	-19.589853	9.624474
-68.558184	-20.180539	9.634471
-66.819714	-18.214031	9.644467
-64.851865	-19.647298	9.654464
-62.801954	-20.798389	9.664461
-61.103374	-13.783898	9.674458
-59.125270	-18.291450	9.684455
-57.051593	-15.849461	9.694451
-55.487542	-18.279360	9.704448
-53.409301	-17.732847	9.714445
-51.870340	-19.088207	9.724442
-49.885414	-21.391034	9.734439
-47.910407	-18.488030	9.744435
-45.559397	-23.977173	9.754432
-44.091587	-18.542708	9.764429
-42.741370	-11.316310	9.774426
-40.523693	-20.657365	9.784423
-38.201131	-21.089296	9.794419
-36.503193	-13.858366	9.804416
-34.817294	-11.793446	9.814413
-33.125870	-13.133642	9.824410
-31.075208	-13.451137	9.834407
-28.945936	-9.457980	9.844403
-26.812294	-14.500324	9.854400
-25.448420	-16.596691	9.864397
-23.874543	-11.145972	9.874394
-21.563840	-17.846043	9.884391
-19.545674	-11.842507	9.894387
-17.817616	-11.639577	9.904384
-16.001312	-19.258679	9.914381
-14.334491	-15.040158	9.924378
-12.454509	-12.958814	9.934375
-10.279177	-11.673008	9.944371
-8.301046	-13.848402	9.954368
-6.564906	-19.501536	9.964365
-5.030287	-9.759245	9.974362
-3.442706	9.841539	9.984359
-2.184434	41.013433	9.994355
-0.958612	100.390990	10.004352
0.000000	147.002378	10.009357
1.139748	173.378235	10.014362
1.785707	219.576511	10.019367
2.472996	230.272340	10.024371
2.782072	259.431741	10.029376
2.832221	263.113936	10.034381
3.182904	267.438907	10.039386
3.370498	273.616027	10.044391
3.334434	297.005224	10.049395
3.757829	302.081863	10.054400
3.666523	309.344290	10.059405
3.550036	315.322348	10.064410
3.807586	310.403761	10.069415
3.960080	318.002624	10.074419
3.822940	313.370925	10.079424
3.607466	322.668541	10.084429
4.000863	330.063401	10.089434
3.953160	319.325568	10.094439
3.801248	333.377100	10.099443
4.078456	315.927863	10.104448
4.033342	329.613845	10.109453
4.365042	322.035680	10.114458
4.160429	333.362718	10.119463
3.842263	328.179561	10.124467
4.178207	337.586352	10.129472
4.081293	348.415243	10.134477
4.570481	361.031991	10.139482
4.894549	363.787409	10.144487
4.559137	353.918628	10.149491
4.516156	352.047383	10.154496
4.190397	357.134729	10.159501
4.720367	365.884526	10.164506
4.862906	377.476351	10.169511
4.903057	369.195600	10.174515
5.016510	363.233941	10.179520
4.739309	369.925221	10.184525
4.842800	347.014181	10.189530
4.548508	358.650439	10.194535
4.633085	381.651514	10.199539
5.174015	375.031871	10.204544
4.869842	388.079550	10.209549
5.129717	374.712667	10.214554
4.968165	392.276159	10.219559
5.271136	388.793242	10.224563
5.176149	390.538429	10.229568
4.814661	384.438050	10.234573
5.431625	392.022789	10.239578
5.260912	393.888867	10.244583
5.086756	394.807727	10.249587
5.232552	386.675698	10.254592
5.080344	398.708801	10.259597
5.113939	390.501625	10.264602
5.340394	398.192814	10.269607
5.742907	427.523733	10.274611
5.792818	435.265180	10.279616
5.964803	436.753317	10.284621
5.859262	431.072572	10.289626
5.595565	422.229964	10.294631
5.629045	437.612966	10.299635
5.864444	432.986460	10.304640
5.997661	451.310423	10.309645
6.020115	439.030052	10.314650
6.241537	450.653508	10.319655
6.100179	447.478001	10.324659
5.959636	441.834375	10.329664
6.027586	449.358481	10.334669
6.027629	448.852344	10.339674
6.038186	453.365669	10.344679
5.909366	450.913578	10.349683
6.362641	457.562497	10.354688
6.079977	463.899868	10.359693
6.159783	454.693357	10.364698
6.301550	455.132885	10.369703
6.264007	458.578377	10.374707
6.282158	447.888292	10.379712
6.167045	466.570438	10.384717
6.351114	471.932900	10.389722
6.616995	491.374342	10.394727
6.552020	494.480432	10.399731
6.941763	492.634765	10.404736
6.524492	495.866438	10.409741
6.798906	494.985365	10.414746
6.830170	486.611345	10.419751
6.612353	508.080707	10.424755
6.981827	501.204496	10.429760
6.868985	507.817581	10.434765
6.745866	510.281649	10.439770
7.019386	505.825664	10.444775
6.930839	507.672343	10.449779
7.293697	492.335025	10.454784
6.725407	509.933575	10.459789
7.289238	532.715726	10.464794
7.620330	528.536776	10.469799
7.437116	530.850368	10.474803
7.627453	516.859705	10.479808
7.152147	521.747028	10.484813
7.492509	534.333261	10.489818
7.655652	534.430327	10.494823
7.361526	550.734632	10.499827
7.722704	555.199947	10.504832
7.578560	552.545272	10.509837
8.199058	546.168335	10.514842
7.693700	538.660498	10.519847
7.375088	536.602953	10.524851
7.687504	539.768707	10.529856
7.606488	553.621480	10.534861
7.815251	552.383434	10.539866
7.844591	549.391995	10.544871
7.774039	565.875127	10.549875
7.801125	558.903689	10.554880
7.641048	564.368390	10.559885
7.814415	556.370646	10.564890
7.863540	569.000999	10.569895
7.813655	581.286021	10.574899
8.312417	588.046021	10.579904
8.264102	586.860018	10.584909
8.271548	601.017281	10.589914
8.498764	589.077872	10.594919
8.484284	604.411929	10.599923
8.484445	585.238736	10.604928
8.366932	598.927057	10.609933
8.557356	592.202371	10.614938
8.479411	591.539928	10.619943
8.312563	603.564496	10.624947
9.069126	604.254483	10.629952
8.669034	615.955131	10.634957
8.859192	610.865837	10.639962
8.790990	612.696667	10.644967
8.584886	611.483789	10.649971
8.890847	591.156327	10.654976
8.818965	610.888357	10.659981
8.900384	602.936793	10.664986
9.038788	620.801233	10.669991
9.208047	638.750664	10.674995
9.429819	622.735521	10.680000
8.915160	616.987493	10.685005
9.100573	633.877744	10.690010
9.193121	638.644564	10.695015
9.285572	633.698585	10.700019
9.415248	638.905777	10.705024
9.204366	649.860308	10.710029
9.376845	643.211004	10.715034
9.446576	638.178758	10.720039
9.275226	652.093344	10.725043
9.550630	642.325638	10.730048
9.205271	648.742477	10.735053
9.442202	654.129693	10.740058
9.345539	655.946144	10.745063
9.264188	657.979358	10.750067
9.598055	663.160296	10.755072
9.497886	688.776054	10.760077
9.891579	683.424025	10.765082
10.075035	677.399030	10.770087
9.935351	695.098176	10.775091
10.034526	681.196804	10.780096
10.009289	688.180789	10.785101
9.937289	690.835438	10.790106
9.971976	689.601491	10.795111
9.706158	706.144316	10.800115
9.812407	691.385485	10.805120
9.777216	699.892885	10.810125
10.045037	717.639026	10.815130
10.357124	725.009210	10.820135
10.257354	715.509466	10.825139
10.695264	718.349301	10.830144
10.289198	732.932212	10.835149
10.485511	723.449892	10.840154
10.892604	721.216637	10.845159
10.343637	735.396548	10.850163
10.702223	719.151310	10.855168
10.344524	731.936587	10.860173
10.411479	729.879016	10.865178
10.786120	727.515312	10.870183
10.471880	736.078283	10.875187
10.724468	748.558062	10.880192
10.731812	759.173500	10.885197
10.786214	768.742180	10.890202
10.885016	768.964635	10.895207
10.782106	762.990013	10.900211
11.227386	770.687498	10.905216
10.979184	762.999746	10.910221
10.752614	765.675910	10.915226
11.076899	761.962414	10.920231
11.266402	771.427541	10.925235
11.010536	769.191212	10.930240
11.346112	787.811343	10.935245
11.845974	816.342161	10.940250
11.830026	815.414340	10.945255
11.680738	813.151541	10.950259
11.565013	790.848809	10.955264
11.166120	785.932265	10.960269
10.878171	792.866737	10.965274
11.278356	792.474966	10.970279
11.373916	809.934868	10.975283
11.506538	808.216912	10.980288
11.495007	803.060370	10.985293
11.718351	805.622196	10.990298
11.722443	796.515860	10.995303
11.701662	827.559949	11.000307
12.106197	827.976500	11.005312
11.946022	834.813336	11.010317
11.982624	840.538520	11.015322
12.493603	838.671896	11.020327
12.341538	845.546869	11.025331
12.201201	840.813003	11.030336
12.271720	845.682758	11.035341
12.304360	832.761731	11.040346
12.303952	844.031360	11.045351
12.106571	846.847969	11.050355
12.420905	847.124359	11.055360
12.469361	845.982826	11.060365
12.513437	855.174722	11.065370
12.504103	849.155175	11.070375
12.339518	846.650370	11.075379
12.581262	841.056003	11.080384
12.460782	853.073381	11.085389
12.355178	842.549411	11.090394
12.111683	851.145321	11.095399
12.442897	864.054227	11.100403
12.744996	876.707578	11.105408
13.116154	878.398970	11.110413
13.183912	896.081042	11.115418
13.185376	877.397715	11.120423
12.735567	889.226367	11.125427
12.813140	888.337243	11.130432
12.994150	881.095080	11.135437
13.047276	893.830739	11.140442
13.009582	882.712403	11.145447
12.773510	898.545764	11.150451
12.915842	888.280274	11.155456
12.988644	906.947204	11.160461
13.364022	929.360259	11.165466
13.774188	916.322166	11.170471
13.601734	928.204385	11.175475
13.553983	917.532353	11.180480
13.430820	928.682848	11.185485
13.269008	930.602771	11.190490
13.399666	917.073066	11.195495
13.525192	931.038341	11.200499
13.694780	926.313362	11.205504
13.635024	933.831280	11.210509
13.596391	930.297063	11.215514
13.580430	931.853079	11.220519
13.392209	933.113279	11.225523
13.586309	950.409390	11.230528
13.751555	960.889396	11.235533
14.005068	967.048414	11.240538
14.399003	989.698314	11.245543
14.267493	1002.402014	11.250547
14.409660	999.783594	11.255552
14.787595	999.841673	11.260557
14.612768	1005.455557	11.265562
14.469012	983.713700	11.270567
14.441662	971.712076	11.275571
14.155804	939.723219	11.280576
14.081032	944.109951	11.285581
14.127857	965.160859	11.290586
14.736072	974.975672	11.295591
14.444224	974.247977	11.300595
14.571637	976.728935	11.305600
14.290899	970.260590	11.310605
14.302586	973.062800	11.315610
14.359139	965.816791	11.320615
14.375980	973.136420	11.325619
14.398572	977.905047	11.330624
14.337165	981.761347	11.335629
14.511549	996.885908	11.340634
14.908654	978.992528	11.345639
14.837741	996.018710	11.350643
14.690522	975.826080	11.355648
14.794534	997.740022	11.360653
15.153035	1011.221907	11.365658
15.191504	1012.887530	11.370663
15.265197	1027.741160	11.375667
15.441990	1024.428041	11.380672
15.513554	1028.949162	11.385677
15.257473	1030.723274	11.390682
15.737171	1018.341094	11.395687
15.281362	1018.294026	11.400691
15.111792	1023.337762	11.405696
15.514794	1019.930211	11.410701
15.359230	1027.170127	11.415706
15.578201	1022.809425	11.420711
15.557198	1034.470441	11.425715
15.561055	1028.183771	11.430720
15.446469	1017.708419	11.435725
15.233293	1025.960529	11.440730
15.320573	1027.623099	11.445735
15.499370	1052.087906	11.450739
15.815571	1053.245579	11.455744
15.698965	1060.619655	11.460749
15.578987	1069.405741	11.465754
15.794990	1058.451822	11.470759
15.729290	1073.740923	11.475763
16.102593	1067.265988	11.480768
15.932705	1080.184048	11.485773
15.971288	1086.607650	11.490778
16.758956	1087.073493	11.495783
16.485608	1098.981406	11.500787
16.521664	1101.839682	11.505792
16.677299	1096.074437	11.510797
16.284168	1079.937662	11.515802
16.644005	1082.774254	11.520807
16.560665	1100.140030	11.525811
16.709178	1099.003019	11.530816
16.792386	1092.046029	11.535821
16.492208	1094.071627	11.540826
17.058314	1092.519477	11.545831
16.756475	1087.200969	11.550835
16.771588	1093.440647	11.555840
16.846174	1093.384676	11.560845
16.703119	1103.855610	11.565850
17.012672	1092.905668	11.570855
16.669682	1104.331074	11.575859
16.885788	1106.780560	11.580864
17.109478	1096.508255	11.585869
16.773207	1102.684129	11.590874
17.024735	1101.999073	11.595879
16.789897	1101.162922	11.600883
16.728670	1104.744817	11.605888
16.929702	1114.009619	11.610893
17.198916	1130.901276	11.615898
17.445238	1134.407311	11.620903
17.285184	1134.888696	11.625907
17.295970	1127.965320	11.630912
17.639432	1134.662035	11.635917
17.614745	1134.647131	11.640922
17.678960	1120.724107	11.645927
17.926419	1139.765628	11.650931
17.643577	1126.613944	11.655936
18.062817	1134.358359	11.660941
18.209834	1125.629593	11.665946
18.087497	1118.266953	11.670951
17.948575	1128.636313	11.675955
17.657565	1121.696419	11.680960
17.561675	1123.564848	11.685965
17.698883	1132.163281	11.690970
17.949503	1126.693555	11.695975
18.239382	1141.858196	11.700979
18.020733	1134.979299	11.705984
17.904520	1131.894254	11.710989
17.823116	1135.233352	11.715994
18.140297	1132.449789	11.720999
17.826338	1144.256976	11.726003
18.023302	1148.597272	11.731008
18.328388	1156.744711	11.736013
18.159174	1166.172689	11.741018
18.442685	1162.637498	11.746023
18.134720	1161.664763	11.751027
18.680666	1167.250481	11.756032
18.621450	1164.086947	11.761037
18.544903	1166.228283	11.766042
18.659613	1153.450010	11.771047
18.570362	1168.676730	11.776051
18.647162	1164.034289	11.781056
18.529094	1161.294912	11.786061
18.478593	1178.206079	11.791066
19.161515	1177.165184	11.796071
19.275295	1199.076294	11.801075
19.406226	1182.674451	11.806080
19.131310	1188.323295	11.811085
19.025852	1175.105423	11.816090
19.128064	1172.635283	11.821095
19.156353	1167.541651	11.826099
19.115956	1177.770743	11.831104
19.236419	1164.904804	11.836109
19.095636	1189.185834	11.841114
19.174686	1197.159600	11.846119
19.436828	1201.352310	11.851123
19.395194	1206.061865	11.856128
19.267793	1200.206096	11.861133
19.111345	1205.080632	11.866138
19.583920	1198.581920	11.871143
19.381136	1205.870460	11.876147
19.672527	1207.656624	11.881152
19.461266	1208.068902	11.886157
19.396308	1203.742395	11.891162
19.448180	1210.987165	11.896167
19.797245	1223.996055	11.901171
20.012362	1231.648492	11.906176
20.222666	1237.967494	11.911181
19.626107	1239.149337	11.916186
20.031836	1237.793079	11.921191
20.073074	1242.661329	11.926195
20.182597	1243.907182	11.931200
20.569867	1228.614089	11.936205
20.440601	1236.676302	11.941210
20.203336	1222.250868	11.946215
20.083911	1225.263289	11.951219
19.999676	1232.889352	11.956224
20.467170	1241.488789	11.961229
20.138286	1238.924960	11.966234
20.561387	1227.273933	11.971239
20.141248	1238.483073	11.976243
20.312163	1232.991325	11.981248
20.461440	1236.866130	11.986253
20.240985	1243.810551	11.991258
20.203632	1237.102976	11.996263
20.536458	1243.902371	12.001267
20.550248	1257.079895	12.006272
20.819864	1265.977435	12.011277
20.971656	1278.368083	12.016282
21.243417	1265.528390	12.021287
20.958617	1267.657222	12.026291
20.574930	1251.983988	12.031296
21.043742	1247.496629	12.036301
20.738674	1253.218122	12.041306
20.619271	1248.800930	12.046311
20.789798	1257.457206	12.051315
20.642211	1261.229547	12.056320
20.784886	1266.480627	12.061325
20.954197	1278.212415	12.066330
21.039820	1258.971082	12.071335
20.761273	1254.091955	12.076339
20.930124	1261.590926	12.081344
20.738388	1257.066988	12.086349
20.775207	1263.700701	12.091354
20.942002	1243.498617	12.096359
20.948290	1249.553675	12.101363
20.786535	1251.374273	12.106368
20.626758	1251.429806	12.111373
20.520485	1253.003417	12.116378
20.865646	1246.045575	12.121383
20.791210	1256.079862	12.126387
20.767931	1260.094170	12.131392
20.994638	1253.886984	12.136397
20.490897	1259.876730	12.141402
20.852347	1250.426080	12.146407
20.636221	1255.740695	12.151411
20.924211	1258.986206	12.156416
20.837480	1256.833216	12.161421
20.665592	1255.518623	12.166426
20.963634	1247.230934	12.171431
21.122020	1252.096272	12.176435
20.837530	1247.593440	12.181440
21.205678	1246.484468	12.186445
20.806559	1249.260786	12.191450
20.854066	1244.630878	12.196455
20.672800	1251.362454	12.201459
20.892199	1251.297578	12.206464
21.005908	1247.434608	12.211469
20.433074	1258.270695	12.216474
20.606075	1252.084692	12.221479
20.786814	1253.896397	12.226483
20.873192	1248.303000	12.231488
21.013797	1261.619586	12.236493
20.823790	1259.407370	12.241498
21.040531	1259.672527	12.246503
20.993405	1262.840593	12.251507
21.139177	1259.701117	12.256512
21.378687	1253.818344	12.261517
21.275038	1267.438844	12.266522
21.195675	1244.262222	12.271527
21.102581	1240.657762	12.276531
20.643444	1235.763288	12.281536
21.109818	1222.644989	12.286541
20.493726	1225.066374	12.291546
20.544385	1232.916945	12.296551
20.314579	1230.610148	12.301555
20.399217	1231.350574	12.306560
21.003787	1244.268261	12.311565
21.070804	1255.683585	12.316570
21.431630	1239.785946	12.321575
21.260237	1237.719009	12.326579
20.726735	1243.193060	12.331584
20.760871	1235.403248	12.336589
21.016517	1233.419596	12.341594
21.042877	1230.016876	12.346599
21.128122	1234.767709	12.351603
20.876807	1239.165341	12.356608
21.154572	1230.786271	12.361613
21.124667	1234.978261	12.366618
21.137061	1223.153031	12.371623
20.912191	1215.830351	12.376627
20.737532	1217.481103	12.381632
20.645850	1201.876473	12.386637
20.601767	1204.132494	12.391642
20.884878	1211.072277	12.396647
20.651151	1203.612234	12.401651
20.493487	1210.327411	12.406656
21.021910	1217.825780	12.411661
20.793830	1222.762214	12.416666
20.747056	1210.605784	12.421671
20.888792	1208.651344	12.426675
21.019730	1208.266238	12.431680
21.099027	1207.238038	12.436685
20.685510	1210.877728	12.441690
20.974392	1202.910094	12.446695
20.720353	1206.503843	12.451699
20.642988	1206.185081	12.456704
20.980316	1203.701089	12.461709
20.725395	1212.328998	12.466714
20.654561	1210.742804	12.471719
20.778279	1212.667685	12.476723
20.719156	1209.362190	12.481728
20.749961	1207.851254	12.486733
20.680186	1213.289178	12.491738
20.708000	1207.681482	12.496743
20.816731	1215.059121	12.501747
20.483842	1218.561363	12.506752
21.421144	1219.146859	12.511757
20.971143	1222.595236	12.516762
20.691944	1207.611913	12.521767
20.899646	1209.245834	12.526771
20.734797	1215.753985	12.531776
20.900328	1207.328170	12.536781
20.750391	1207.265430	12.541786
20.724238	1209.471279	12.546791
20.779600	1208.964177	12.551795
20.746161	1222.209132	12.556800
21.275265	1217.582845	12.561805
20.962994	1215.729208	12.566810
21.006083	1209.164945	12.571815
21.065257	1225.068271	12.576819
20.740562	1218.621019	12.581824
20.826116	1219.205167	12.586829
20.819672	1218.666918	12.591834
20.721764	1211.262484	12.596839
20.948718	1210.844716	12.601843
20.791644	1212.967361	12.606848
20.968570	1213.161591	12.611853
20.516171	1220.245507	12.616858
20.608835	1216.221886	12.621863
20.809136	1217.975269	12.626867
20.774276	1222.280018	12.631872
20.795647	1214.110600	12.636877
20.721393	1220.170608	12.641882
20.950265	1219.310952	12.646887
20.702623	1216.910801	12.651891
20.788836	1225.126309	12.656896
21.310384	1213.459590	12.661901
20.915451	1224.685201	12.666906
21.288345	1218.850557	12.671911
21.066430	1221.841475	12.676915
20.586370	1206.741946	12.681920
20.757590	1209.417823	12.686925
20.740047	1215.834664	12.691930
20.911470	1210.806502	12.696935
21.016398	1210.387695	12.701939
20.546769	1204.135468	12.706944
20.954301	1191.424006	12.711949
20.415396	1195.225628	12.716954
20.579051	1201.968402	12.721959
20.764757	1212.276580	12.726963
20.582067	1219.932534	12.731968
20.971972	1219.137086	12.736973
20.542588	1222.165827	12.741978
20.820110	1222.782439	12.746983
20.955119	1219.926984	12.751987
20.899397	1236.118328	12.756992
20.957446	1232.772058	12.761997
21.004152	1233.053297	12.767002
20.547466	1223.214303	12.772007
20.890519	1231.776809	12.777011
20.812739	1233.320639	12.782016
20.992950	1221.140611	12.787021
20.641067	1226.304968	12.792026
20.662593	1231.457078	12.797031
20.645724	1229.456965	12.802035
20.559655	1233.698917	12.807040
20.601759	1231.091686	12.812045
20.568595	1232.827112	12.817050
20.950544	1228.061855	12.822055
20.704606	1235.406183	12.827059
20.877556	1234.227414	12.832064
21.086645	1227.597238	12.837069
20.891503	1234.398834	12.842074
20.942848	1230.116851	12.847079
21.032410	1228.326862	12.852083
20.678265	1240.615236	12.857088
21.054551	1237.036842	12.862093
20.784764	1233.675049	12.867098
20.656676	1233.788611	12.872103
20.760698	1239.671945	12.877107
20.598440	1244.720900	12.882112
20.856300	1236.917480	12.887117
20.850885	1244.679223	12.892122
20.920471	1238.643773	12.897127
21.289486	1232.524292	12.902131
20.582087	1221.681265	12.907136
20.945041	1207.486563	12.912141
20.792500	1215.066737	12.917146
20.722431	1207.391339	12.922151
20.434723	1211.463582	12.927155
20.743064	1228.246602	12.932160
20.672646	1227.262782	12.937165
20.778488	1239.015702	12.942170
21.038147	1238.348269	12.947175
20.986544	1247.068358	12.952179
20.690423	1238.001745	12.957184
20.803767	1227.295905	12.962189
20.684631	1227.403307	12.967194
21.045869	1235.530795	12.972199
20.467175	1230.593887	12.977203
20.482658	1232.577039	12.982208
20.844368	1225.197065	12.987213
20.656012	1245.136204	12.992218
20.819539	1239.746565	12.997223
21.139496	1233.999213	13.002227
20.982535	1242.114735	13.007232
21.011288	1237.549326	13.012237
20.688360	1233.355428	13.017242
20.833200	1210.672996	13.022247
20.459372	1220.739243	13.027251
20.105776	1238.361196	13.032256
21.051225	1233.993373	13.037261
20.828504	1243.136599	13.042266
20.802760	1241.024351	13.047271
20.802995	1240.226396	13.052275
20.793181	1249.723628	13.057280
20.799687	1249.284245	13.062285
20.806443	1243.536380	13.067290
20.870671	1248.083973	13.072295
20.838552	1248.235847	13.077299
20.629953	1253.240153	13.082304
21.007742	1242.452695	13.087309
20.789271	1246.389314	13.092314
20.661641	1248.273861	13.097319
21.083552	1240.893740	13.102323
20.800318	1249.278585	13.107328
20.905728	1249.361211	13.112333
20.716388	1259.697702	13.117338
20.806283	1247.543098	13.122343
20.837473	1252.843496	13.127347
20.865401	1260.623585	13.132352
20.859184	1249.878447	13.137357
20.939267	1253.822646	13.142362
20.605207	1240.611213	13.147367
20.888961	1226.854936	13.152371
20.737693	1241.135916	13.157376
20.885863	1246.687334	13.162381
20.866717	1250.603201	13.167386
21.129552	1229.100499	13.172391
21.056161	1227.689766	13.177395
20.636882	1217.873197	13.182400
20.566969	1218.589384	13.187405
20.397377	1226.121818	13.192410
20.568534	1238.752213	13.197415
20.822187	1254.580392	13.202419
20.933763	1258.879142	13.207424
21.117745	1250.846206	13.212429
20.824270	1250.096676	13.217434
20.804373	1230.498444	13.222439
20.930291	1235.253829	13.227443
20.625732	1229.112467	13.232448
20.913992	1225.784678	13.237453
20.697598	1225.343000	13.242458
20.793880	1218.301857	13.247463
21.093539	1223.587810	13.252467
20.700617	1221.906321	13.257472
20.849060	1228.277767	13.262477
20.821338	1234.093797	13.267482
20.779377	1233.133826	13.272487
20.884549	1218.786250	13.277491
20.656402	1232.453385	13.282496
20.635062	1234.762558	13.287501
20.885625	1230.620700	13.292506
20.711367	1232.895912	13.297511
20.596987	1234.426655	13.302515
20.850970	1230.031920	13.307520
20.937791	1229.929838	13.312525
20.603640	1226.717097	13.317530
20.946494	1233.115887	13.322535
21.069562	1229.863335	13.327539
20.794151	1238.721626	13.332544
20.942823	1229.956262	13.337549
20.869714	1229.351370	13.342554
20.702576	1230.699702	13.347559
20.846796	1227.445353	13.352563
20.804299	1235.925844	13.357568
20.753117	1235.378960	13.362573
20.710568	1232.845160	13.367578
20.903852	1226.742672	13.372583
21.140259	1229.258333	13.377587
20.690877	1240.399593	13.382592
21.027854	1229.818942	13.387597
20.539252	1238.755397	13.392602
20.734397	1232.297767	13.397607
21.134551	1228.299220	13.402611
20.747914	1236.817256	13.407616
21.102132	1216.137424	13.412621
20.854456	1232.277373	13.417626
20.872896	1233.477824	13.422631
21.118534	1228.169716	13.427635
20.937238	1233.713752	13.432640
21.073222	1239.240300	13.437645
21.187161	1230.098823	13.442650
20.684970	1233.740046	13.447655
20.849864	1217.649738	13.452659
20.581538	1226.868043	13.457664
20.819920	1225.158403	13.462669
20.947690	1238.201027	13.467674
20.779411	1226.486620	13.472679
20.988176	1220.346969	13.477683
20.695128	1220.184044	13.482688
20.678327	1204.521732	13.487693
20.648262	1211.421576	13.492698
20.604280	1236.944174	13.497703
20.880696	1235.537573	13.502707
20.909354	1243.443702	13.507712
21.312908	1230.597211	13.512717
20.739533	1221.297267	13.517722
20.588372	1214.462764	13.522727
20.833967	1211.684296	13.527731
20.715721	1206.746498	13.532736
20.976538	1217.881702	13.537741
20.926232	1217.240055	13.542746
20.848576	1211.199714	13.547751
20.787635	1208.183114	13.552755
20.737968	1206.573042	13.557760
20.832380	1204.829593	13.562765
20.605302	1218.110162	13.567770
20.682844	1208.648050	13.572775
20.977025	1202.513708	13.577779
20.633261	1217.563439	13.582784
20.774090	1213.282959	13.587789
21.014307	1202.631022	13.592794
20.800832	1206.393356	13.597799
20.579579	1203.452793	13.602803
20.858236	1209.745110	13.607808
20.942252	1206.497214	13.612813
20.374718	1213.003358	13.617818
20.650815	1233.033990	13.622823
21.238053	1230.303535	13.627827
20.795021	1223.195436	13.632832
20.678087	1212.572073	13.637837
20.766214	1217.887033	13.642842
20.877858	1218.385012	13.647847
20.732698	1202.457725	13.652851
20.594528	1226.475030	13.657856
20.938698	1225.948671	13.662861
20.875394	1232.675617	13.667866
21.049208	1231.421011	13.672871
20.992213	1215.030181	13.677875
20.690378	1223.249232	13.682880
20.954664	1211.872727	13.687885
20.723651	1207.697294	13.692890
20.859134	1218.913996	13.697895
21.072987	1206.298073	13.702899
20.669828	1215.197229	13.707904
20.927029	1212.090455	13.712909
20.982951	1211.966492	13.717914
20.654911	1210.586917	13.722919
21.170164	1215.852672	13.727923
21.080777	1207.864941	13.732928
20.756423	1218.156701	13.737933
20.763717	1210.360143	13.742938
20.835263	1214.914444	13.747943
21.219661	1219.997631	13.752947
20.873496	1216.498203	13.757952
20.920997	1215.574429	13.762957
20.845097	1209.338252	13.767962
20.817348	1225.055154	13.772967
21.286884	1215.773381	13.777971
20.754739	1200.704245	13.782976
20.609079	1190.463977	13.787981
20.758003	1193.641761	13.792986
20.927448	1210.099959	13.797991
20.841825	1197.642206	13.802995
20.683296	1198.271594	13.808000
20.820449	1199.563502	13.813005
20.883065	1206.552647	13.818010
20.630861	1208.600573	13.823015
20.739174	1201.819313	13.828019
20.893296	1220.539912	13.833024
20.910218	1212.946837	13.838029
20.647695	1207.208819	13.843034
20.649667	1216.104861	13.848039
20.690511	1206.779500	13.853043
20.511571	1228.475551	13.858048
20.679680	1223.537807	13.863053
20.900768	1223.379614	13.868058
21.036585	1221.763611	13.873063
20.954036	1218.206364	13.878067
21.043880	1224.617120	13.883072
21.030334	1210.187556	13.888077
20.764132	1192.767173	13.893082
20.682063	1188.482827	13.898087
20.713118	1192.756552	13.903091
20.747949	1196.237985	13.908096
20.742779	1206.095597	13.913101
20.929447	1217.411375	13.918106
20.482959	1213.076330	13.923111
20.662493	1214.247930	13.928115
20.945542	1213.885874	13.933120
20.622028	1219.208141	13.938125
20.719742	1223.554828	13.943130
20.632897	1221.576917	13.948135
20.842362	1225.468930	13.953139
20.586270	1234.639553	13.958144
20.784790	1227.998446	13.963149
20.736955	1219.915764	13.968154
20.687120	1230.886046	13.973159
20.704370	1225.261103	13.978163
20.701712	1233.776242	13.983168
20.914676	1226.205512	13.988173
20.958447	1222.306392	13.993178
20.639269	1228.452781	13.998183
21.110169	1224.499725	14.003187
20.577552	1229.867966	14.008192
20.925403	1222.103469	14.013210
21.049283	1226.993289	14.018227
20.352888	1234.211503	14.023245
20.723961	1222.334055	14.028263
20.737953	1221.597292	14.033280
20.739653	1219.814836	14.038298
20.951382	1224.379178	14.043315
20.694731	1235.367072	14.048333
20.819608	1225.221497	14.053351
20.546480	1237.814961	14.058368
20.949684	1230.121424	14.063386
20.955021	1224.056539	14.068403
20.760525	1229.390405	14.073421
20.890168	1226.777419	14.078439
21.190198	1256.152046	14.083456
21.225236	1248.117668	14.088474
21.310708	1243.581587	14.093491
20.978141	1235.582255	14.098509
21.326939	1227.950881	14.103527
21.028228	1236.274441	14.108544
21.049165	1234.850718	14.113562
21.030790	1225.371371	14.118579
20.991409	1239.112060	14.123597
21.312385	1246.586437	14.128615
21.260399	1257.296306	14.133632
21.257677	1256.066694	14.138650
21.064467	1250.843591	14.143667
21.104341	1256.382334	14.148685
21.477705	1253.330913	14.153703
21.197439	1259.526347	14.158720
21.155959	1267.841930	14.163738
21.365613	1260.797460	14.168755
21.270545	1261.786429	14.173773
21.141391	1257.866608	14.178791
21.233558	1261.628898	14.183808
21.233990	1261.765768	14.188826
21.277007	1269.918434	14.193843
21.135819	1269.478559	14.198861
21.464255	1266.881050	14.203879
21.689484	1270.664590	14.208896
21.305804	1262.651372	14.213914
21.463335	1262.045871	14.218931
21.209121	1265.651049	14.223949
21.396495	1276.382528	14.228967
21.371525	1296.565792	14.233984
21.203631	1302.164434	14.239002
21.717324	1302.878550	14.244019
21.763984	1301.823532	14.249037
21.832892	1305.172682	14.254055
21.782205	1299.160748	14.259072
21.533961	1299.865832	14.264090
21.664553	1299.505304	14.269107
21.750492	1307.786429	14.274125
21.720517	1307.275329	14.279143
21.520304	1301.598710	14.284160
21.634206	1304.394831	14.289178
21.852976	1304.440246	14.294195
21.586048	1312.555855	14.299213
21.937685	1295.705855	14.304231
21.841083	1301.477174	14.309248
21.873632	1307.050139	14.314266
21.953531	1307.270291	14.319283
22.067096	1295.823977	14.324301
22.150234	1302.202142	14.329319
21.969366	1301.638031	14.334336
22.096688	1301.312633	14.339354
22.200837	1299.216518	14.344371
22.028372	1304.362849	14.349389
21.918921	1292.717723	14.354407
21.932793	1298.310967	14.359424
21.763894	1300.513533	14.364442
22.018208	1295.882863	14.369459
22.175199	1299.784264	14.374477
22.058498	1291.748895	14.379495
22.115062	1292.899301	14.384512
22.079649	1290.793988	14.389530
22.168690	1299.291695	14.394547
21.942457	1305.989774	14.399565
22.511900	1297.236186	14.404583
22.338209	1301.780229	14.409600
22.119067	1303.880695	14.414618
22.260391	1298.324211	14.419635
22.359438	1296.581276	14.424653
22.318405	1302.988686	14.429671
22.328812	1303.997014	14.434688
21.968366	1301.350499	14.439706
22.152974	1305.209743	14.444723
22.026980	1310.024613	14.449741
22.447566	1322.719863	14.454759
22.811062	1326.020456	14.459776
22.495111	1328.493452	14.464794
22.476436	1310.862486	14.469811
22.308620	1307.733776	14.474829
22.303520	1318.713070	14.479847
22.487449	1323.601209	14.484864
22.637395	1327.112048	14.489882
22.555132	1325.910848	14.494899
22.481180	1350.229716	14.499917
22.726588	1335.737337	14.504935
23.070514	1325.657429	14.509952
22.548668	1327.809327	14.514970
22.921242	1322.272578	14.519987
22.560662	1307.532383	14.525005
22.549003	1307.548483	14.530023
22.846168	1308.075335	14.535040
22.916309	1325.539377	14.540058
22.988639	1315.098520	14.545075
22.527075	1308.286934	14.550093
22.761593	1310.294591	14.555111
22.887582	1311.990788	14.560128
22.820812	1318.051518	14.565146
22.844483	1317.404443	14.570163
22.901805	1324.784058	14.575181
22.900850	1313.499145	14.580199
23.046978	1309.272700	14.585216
22.979976	1308.306600	14.590234
23.109807	1290.658262	14.595251
23.046278	1296.726331	14.600269
23.215069	1290.127249	14.605287
23.294902	1280.613325	14.610304
22.899246	1299.345583	14.615322
22.886220	1289.138587	14.620339
22.784484	1287.934204	14.625357
22.960702	1284.835569	14.630375
23.132293	1293.664606	14.635392
22.953196	1318.693912	14.640410
23.461634	1317.543216	14.645427
23.311303	1306.363933	14.650445
23.065486	1305.846362	14.655463
23.586266	1293.373957	14.660480
23.144405	1297.279639	14.665498
22.957761	1287.023257	14.670515
23.030613	1296.692328	14.675533
23.093531	1310.347553	14.680551
23.372262	1309.299564	14.685568
23.315305	1320.162859	14.690586
23.402714	1318.841786	14.695603
23.184149	1327.442057	14.700621
23.262395	1326.479530	14.705639
23.602475	1314.852349	14.710656
23.366832	1316.132737	14.715674
23.305568	1319.998168	14.720691
23.625752	1310.239816	14.725709
23.616654	1311.292156	14.730727
23.534432	1310.028028	14.735744
23.515515	1324.729821	14.740762
23.878368	1316.712332	14.745779
23.897127	1313.671841	14.750797
23.336281	1310.977062	14.755815
23.739142	1317.338845	14.760832
23.454381	1321.730720	14.765850
23.622300	1327.519633	14.770867
23.653012	1319.891756	14.775885
23.325182	1321.919896	14.780903
23.358915	1319.550286	14.785920
23.408044	1324.590491	14.790938
23.617896	1320.940631	14.795955
23.622803	1324.134822	14.800973
23.475973	1327.321755	14.805991
24.014281	1326.406972	14.811008
23.819932	1327.823924	14.816026
23.664453	1337.966753	14.821043
23.922963	1349.114813	14.826061
23.853840	1361.199205	14.831079
24.439557	1351.159366	14.836096
23.696889	1336.251992	14.841114
23.920653	1342.260098	14.846131
24.073296	1345.375672	14.851149
23.779230	1351.570199	14.856167
24.004861	1354.751214	14.861184
23.845553	1354.712212	14.866202
23.908726	1358.145661	14.871219
24.024928	1355.001527	14.876237
23.963435	1359.213079	14.881255
24.097840	1356.766056	14.886272
24.122578	1359.420676	14.891290
24.181620	1375.261570	14.896307
24.298332	1382.409938	14.901325
24.004324	1393.433797	14.906343
24.584314	1383.465638	14.911360
24.612793	1365.698092	14.916378
24.045044	1351.325960	14.921395
24.273019	1362.021139	14.926413
24.296463	1353.110781	14.931431
24.223851	1359.416285	14.936448
24.209493	1357.373672	14.941466
24.358044	1355.624407	14.946483
24.479291	1353.442185	14.951501
23.945095	1352.166773	14.956519
24.444127	1354.209325	14.961536
24.352887	1354.312053	14.966554
23.954434	1357.606769	14.971571
24.105058	1362.552145	14.976589
24.216332	1370.563416	14.981607
24.748467	1376.547519	14.986624
24.397895	1382.291736	14.991642
24.456980	1387.001604	14.996659
24.535710	1386.536085	15.001677
24.450854	1397.867943	15.006695
24.774435	1385.425341	15.011712
24.645437	1388.640905	15.016730
24.330116	1380.317835	15.021747
24.629147	1378.022306	15.026765
24.661950	1391.817695	15.031783
25.045128	1380.059316	15.036800
24.944038	1381.562074	15.041818
25.003832	1388.886269	15.046835
25.153325	1383.252942	15.051853
24.737692	1386.753331	15.056871
25.043215	1385.690053	15.061888
25.037598	1380.238774	15.066906
24.995888	1387.671971	15.071923
25.369017	1384.993378	15.076941
24.771358	1381.510058	15.081959
25.216456	1373.062556	15.086976
24.951149	1386.087494	15.091994
25.163380	1384.984039	15.097011
25.239533	1376.129755	15.102029
24.886556	1384.285871	15.107047
24.903632	1386.254287	15.112064
25.124073	1383.776232	15.117082
24.838883	1385.125879	15.122099
24.887465	1381.160371	15.127117
25.029448	1385.676113	15.132135
25.302276	1381.281570	15.137152
25.372250	1378.100758	15.142170
25.217168	1374.115826	15.147187
25.509591	1383.065647	15.152205
25.019228	1380.532651	15.157223
24.998953	1378.848065	15.162240
25.282643	1377.668717	15.167258
25.090334	1374.760982	15.172275
25.084501	1378.244769	15.177293
25.411849	1384.686269	15.182311
25.208691	1383.461874	15.187328
25.001488	1399.433353	15.192346
25.331208	1417.035431	15.197363
26.146096	1413.870294	15.202381
25.554325	1419.902330	15.207399
25.843733	1413.750370	15.212416
25.661236	1392.285901	15.217434
25.463195	1386.997451	15.222451
25.772096	1382.046579	15.227469
25.469796	1385.958339	15.232487
25.808369	1383.999432	15.237504
25.686088	1393.020125	15.242522
25.619885	1393.301336	15.247539
25.767583	1390.388131	15.252557
25.694887	1394.359227	15.257575
25.914466	1405.485226	15.262592
25.856245	1402.279238	15.267610
25.777745	1390.454486	15.272627
25.713098	1385.920282	15.277645
25.656913	1405.447986	15.282663
25.960941	1407.881884	15.287680
25.847801	1412.887439	15.292698
25.768659	1427.856139	15.297715
26.078434	1414.204448	15.302733
26.035851	1422.959969	15.307751
26.160440	1414.488059	15.312768
26.209282	1422.423584	15.317786
26.357914	1414.407963	15.322803
26.086344	1392.657244	15.327821
25.735406	1395.261677	15.332839
26.068343	1406.762864	15.337856
26.343767	1415.650920	15.342874
26.172198	1423.121365	15.347891
26.107211	1410.493747	15.352909
26.097845	1418.100343	15.357927
25.859162	1419.061891	15.362944
26.603890	1416.467958	15.367962
26.343154	1422.564388	15.372979
26.249379	1417.899536	15.377997
26.109588	1412.875500	15.383015
26.618359	1417.387805	15.388032
26.330378	1414.354532	15.393050
26.126836	1416.168586	15.398067
26.435552	1417.647668	15.403085
26.361472	1413.881047	15.408103
26.285273	1405.947698	15.413120
26.522309	1415.214695	15.418138
26.017591	1414.754145	15.423155
26.278132	1417.913875	15.428173
26.334197	1428.431237	15.433191
26.186970	1421.149449	15.438208
26.400402	1414.540045	15.443226
25.984662	1428.034980	15.448243
26.526921	1439.591684	15.453261
26.528898	1434.930431	15.458279
26.413954	1442.668715	15.463296
26.608279	1445.338774	15.468314
26.692153	1446.917432	15.473331
26.876612	1444.864332	15.478349
26.850756	1449.176408	15.483367
26.857847	1450.289885	15.488384
26.890379	1446.053991	15.493402
27.056749	1452.966378	15.498419
27.116605	1454.051776	15.503437
26.698476	1449.031222	15.508455
26.659326	1455.042770	15.513472
27.162569	1450.719997	15.518490
26.867904	1450.435947	15.523507
26.885382	1444.417800	15.528525
26.528713	1442.178082	15.533543
26.715263	1444.333413	15.538560
26.707067	1451.396342	15.543578
26.541557	1452.143294	15.548595
26.924781	1466.142418	15.553613
27.261638	1474.167317	15.558631
27.010232	1473.501974	15.563648
27.381807	1480.562548	15.568666
27.273501	1485.620055	15.573683
27.570368	1479.237208	15.578701
27.411488	1481.002459	15.583719
27.524294	1467.024260	15.588736
27.343687	1451.299567	15.593754
27.066560	1447.802071	15.598771
27.374365	1465.417929	15.603789
27.589865	1475.352239	15.608807
27.513207	1471.799952	15.613824
27.441828	1449.185060	15.618842
27.108297	1462.295668	15.623859
27.524738	1456.707040	15.628877
27.520114	1481.717449	15.633895
27.308863	1475.538350	15.638912
27.890818	1468.761599	15.643930
27.516924	1480.322100	15.648947
27.616322	1475.593383	15.653965
27.671394	1480.237851	15.658983
27.497959	1475.777602	15.664000
27.605715	1475.599258	15.669018
27.337707	1479.184664	15.674035
27.600460	1477.768753	15.679053
27.759152	1480.332814	15.684071
27.682360	1474.524752	15.689088
27.960274	1466.121954	15.694106
27.447311	1483.064904	15.699123
27.624953	1475.358452	15.704141
27.595939	1473.388949	15.709159
27.818774	1479.586816	15.714176
27.968840	1473.088956	15.719194
27.479257	1476.737232	15.724211
27.561396	1487.093957	15.729229
28.153356	1490.980302	15.734247
28.114857	1496.004655	15.739264
28.127686	1497.032274	15.744282
28.001913	1481.831289	15.749299
27.974132	1482.913364	15.754317
27.998984	1486.624312	15.759335
28.223050	1499.563429	15.764352
28.271559	1499.399254	15.769370
28.333761	1506.766384	15.774387
28.514500	1501.747036	15.779405
28.369716	1476.004725	15.784423
28.146459	1481.867105	15.789440
28.399866	1472.482679	15.794458
27.966545	1478.177995	15.799475
27.984893	1480.678708	15.804493
28.481650	1493.568033	15.809511
28.324302	1505.305594	15.814528
28.560713	1493.395135	15.819546
28.343071	1507.961276	15.824563
28.382887	1498.836638	15.829581
28.406285	1498.604106	15.834599
28.387326	1501.072233	15.839616
28.537162	1494.924411	15.844634
28.463773	1502.403618	15.849651
28.621991	1503.227930	15.854669
28.837156	1495.229182	15.859687
28.579147	1500.874521	15.864704
28.408785	1504.051874	15.869722
28.449766	1509.145355	15.874739
28.444232	1506.027685	15.879757
28.644737	1496.878990	15.884775
28.253791	1502.304066	15.889792
28.607479	1494.669415	15.894810
28.817384	1525.377204	15.899827
28.820592	1534.833377	15.904845
29.056981	1526.645602	15.909863
28.875407	1536.973636	15.914880
28.870513	1530.427318	15.919898
28.772514	1526.011652	15.924915
28.981146	1538.977649	15.929933
29.134281	1538.898249	15.934951
28.991458	1542.152232	15.939968
29.143140	1534.436518	15.944986
29.140482	1546.633163	15.950003
28.945738	1533.882197	15.955021
29.332476	1531.502654	15.960039
29.039438	1527.516087	15.965056
29.256545	1537.476926	15.970074
29.166859	1537.680085	15.975091
29.109763	1529.078992	15.980109
29.214696	1529.490217	15.985127
28.976040	1539.009353	15.990144
29.457723	1521.873286	15.995162
29.585494	1524.568920	16.000179
29.207546	1537.345320	16.005197
29.137379	1523.958630	16.010215
29.161235	1524.260873	16.015232
29.444451	1517.665461	16.020250
29.538957	1530.187167	16.025267
29.399020	1529.068297	16.030285
29.437818	1520.256065	16.035303
29.161874	1533.403171	16.040320
29.372895	1515.699925	16.045338
29.586128	1520.466263	16.050355
29.528502	1520.043726	16.055373
29.400313	1510.960821	16.060391
29.487033	1524.213674	16.065408
29.420742	1532.003236	16.070426
29.685077	1542.950736	16.075443
29.554810	1551.769085	16.080461
29.799441	1548.309472	16.085479
29.676948	1558.873499	16.090496
29.844155	1544.850367	16.095514
29.707968	1542.967952	16.100531
29.810858	1552.622963	16.105549
30.208177	1540.362745	16.110567
30.035794	1546.597723	16.115584
30.094688	1542.995482	16.120602
30.030655	1549.821964	16.125619
30.005841	1561.161676	16.130637
30.568888	1560.920150	16.135655
30.218825	1549.885013	16.140672
30.276730	1549.009876	16.145690
30.632658	1547.824499	16.150707
30.025917	1535.934440	16.155725
30.065304	1518.853193	16.160743
30.278123	1532.855965	16.165760
30.066605	1536.910593	16.170778
30.137642	1539.498870	16.175795
30.217202	1551.305651	16.180813
30.427737	1545.408472	16.185831
30.549844	1552.997315	16.190848
30.711411	1546.292300	16.195866
30.508549	1548.296605	16.200883
30.122837	1537.175925	16.205901
30.312821	1546.431634	16.210919
30.573258	1553.451766	16.215936
30.570516	1551.021080	16.220954
30.317977	1555.751604	16.225971
30.448691	1546.610865	16.230989
30.571084	1547.620225	16.236007
30.596028	1561.029262	16.241024
30.283406	1554.742024	16.246042
30.373742	1547.762854	16.251059
30.220060	1556.402464	16.256077
30.474461	1561.502036	16.261095
30.418791	1556.886906	16.266112
30.471588	1571.127606	16.271130
30.930773	1573.333856	16.276147
30.691300	1584.085667	16.281165
30.967475	1582.015559	16.286183
30.995904	1579.079654	16.291200
30.917016	1580.132919	16.296218
30.884907	1590.231076	16.301235
30.794719	1592.421917	16.306253
31.112291	1579.269858	16.311271
30.897191	1587.520504	16.316288
31.108125	1581.019966	16.321306
31.276092	1585.520614	16.326323
31.089673	1588.430762	16.331341
31.283593	1589.265115	16.336359
31.218696	1592.482297	16.341376
31.028197	1594.195973	16.346394
31.184569	1587.984932	16.351411
31.225602	1593.002139	16.356429
31.606276	1587.524564	16.361447
31.440155	1590.417316	16.366464
31.324131	1588.719663	16.371482
31.387120	1597.355412	16.376499
31.404929	1593.297224	16.381517
31.638505	1586.918919	16.386535
31.227135	1592.537630	16.391552
31.007481	1594.163144	16.396570
31.169024	1587.493508	16.401587
31.007655	1591.794993	16.406605
31.263037	1596.639580	16.411623
31.437232	1594.162575	16.416640
31.629559	1597.412666	16.421658
31.645673	1604.528424	16.426675
31.632394	1614.375045	16.431693
31.680454	1611.203971	16.436711
31.700083	1617.911743	16.441728
31.882993	1620.675682	16.446746
32.273155	1610.661353	16.451763
31.864187	1596.654564	16.456781
31.649820	1593.954804	16.461799
31.879580	1599.507438	16.466816
31.855566	1608.404833	16.471834
32.197884	1613.091621	16.476851
31.909820	1610.166077	16.481869
32.044416	1612.360395	16.486887
32.111532	1606.136053	16.491904
32.109291	1618.932041	16.496922
32.162606	1599.192307	16.501939
31.921794	1600.903784	16.506957
31.894704	1612.002429	16.511975
32.062680	1618.950034	16.516992
31.776432	1619.421296	16.522010
31.981518	1616.863851	16.527027
31.604098	1618.994326	16.532045
31.732028	1622.681789	16.537063
32.124477	1625.185782	16.542080
32.170175	1641.577318	16.547098
32.186618	1640.817332	16.552115
32.199886	1639.950096	16.557133
32.637331	1649.283597	16.562151
32.422783	1643.168662	16.567168
32.786730	1650.744939	16.572186
32.857282	1656.530637	16.577203
32.474888	1655.127157	16.582221
32.489750	1651.844960	16.587239
32.773342	1652.067237	16.592256
32.437348	1655.364641	16.597274
32.946150	1652.488174	16.602291
32.946438	1645.466689	16.607309
32.614619	1633.830801	16.612327
32.694576	1629.054797	16.617344
32.534680	1639.727100	16.622362
33.136712	1640.681988	16.627379
32.711574	1642.563662	16.632397
32.887956	1636.777291	16.637415
33.183424	1636.220564	16.642432
32.726317	1652.111837	16.647450
32.853129	1636.591965	16.652467
32.684849	1640.295216	16.657485
32.753650	1640.127016	16.662503
33.232343	1637.377270	16.667520
32.861921	1641.194564	16.672538
33.213620	1637.820890	16.677555
33.070014	1647.172345	16.682573
33.077623	1640.125312	16.687591
33.412342	1635.429013	16.692608
33.032003	1655.500348	16.697626
33.460555	1629.129892	16.702643
32.861172	1634.352297	16.707661
33.175654	1643.102911	16.712679
33.416472	1633.132837	16.717696
33.300500	1638.731191	16.722714
33.182085	1627.128914	16.727731
32.925686	1647.535989	16.732749
33.067457	1652.386131	16.737767
33.368888	1661.238729	16.742784
33.478633	1672.808762	16.747802
33.306137	1666.912849	16.752819
33.455037	1672.028502	16.757837
33.468354	1674.775454	16.762855
34.075032	1669.927223	16.767872
33.473343	1672.489110	16.772890
33.632076	1662.706723	16.777907
33.517192	1661.738011	16.782925
33.513194	1669.817386	16.787943
34.051699	1653.910131	16.792960
33.785304	1663.640635	16.797978
33.830456	1668.565184	16.802995
33.943227	1662.025209	16.808013
33.655033	1658.060643	16.813031
33.887988	1666.153348	16.818048
33.828413	1673.601338	16.823066
34.357048	1686.176637	16.828083
33.983325	1676.547597	16.833101
33.895059	1674.594596	16.838119
34.291577	1686.927474	16.843136
34.162283	1694.265465	16.848154
34.186908	1684.798624	16.853171
34.167083	1678.740710	16.858189
34.193224	1696.486721	16.863207
34.390623	1692.056138	16.868224
34.506602	1702.788309	16.873242
34.628574	1690.915607	16.878259
34.506943	1674.346734	16.883277
34.433584	1663.332660	16.888295
34.433818	1658.851733	16.893312
34.288264	1660.087891	16.898330
34.313191	1656.310135	16.903347
34.502482	1670.312860	16.908365
34.358665	1683.671059	16.913383
34.388614	1691.958973	16.918400
34.513652	1695.112061	16.923418
34.798053	1685.508613	16.928435
34.905613	1704.079324	16.933453
34.732527	1707.682680	16.938471
34.930656	1693.541997	16.943488
34.734708	1703.503548	16.948506
35.008409	1697.817255	16.953523
34.825646	1691.490366	16.958541
34.822157	1695.109929	16.963559
34.884889	1689.384139	16.968576
34.598086	1700.522702	16.973594
34.774219	1692.657493	16.978611
34.811717	1698.113408	16.983629
34.528066	1693.411109	16.988647
34.914014	1693.481775	16.993664
34.390686	1702.727082	16.998682
35.007094	1713.881264	17.003699
35.121852	1724.005641	17.008717
35.215714	1722.754292	17.013735
35.389722	1725.487423	17.018752
35.143871	1729.907034	17.023770
35.291500	1718.506868	17.028787
35.384329	1721.281261	17.033805
35.467803	1724.704481	17.038823
35.690696	1718.537833	17.043840
35.345797	1727.938750	17.048858
35.695633	1724.937393	17.053875
35.660984	1705.682691	17.058893
35.102066	1703.679693	17.063911
35.452403	1706.066928	17.068928
35.682405	1718.639548	17.073946
35.534305	1726.189778	17.078963
35.787952	1720.151152	17.083981
35.190386	1728.751545	17.088999
35.594526	1722.164284	17.094016
35.381319	1725.076371	17.099034
35.347950	1718.636762	17.104051
35.623798	1726.913792	17.109069
35.700936	1727.640932	17.114087
35.764101	1724.947221	17.119104
35.261264	1725.272911	17.124122
35.638222	1741.427671	17.129139
36.045695	1743.318922	17.134157
35.964924	1754.598493	17.139175
36.097916	1745.704244	17.144192
36.033848	1761.186862	17.149210
35.843812	1764.647422	17.154227
36.163980	1753.728610	17.159245
35.789174	1758.028005	17.164263
35.877598	1751.491873	17.169280
35.891401	1751.043779	17.174298
35.480553	1754.622931	17.179315
35.800589	1773.411538	17.184333
35.973787	1789.670428	17.189351
36.390560	1788.537466	17.194368
36.482538	1779.076339	17.199386
36.570569	1780.514364	17.204403
36.699452	1780.304330	17.209421
36.605003	1788.946428	17.214439
36.587897	1788.606301	17.219456
36.382840	1781.626154	17.224474
36.401801	1789.348770	17.229491
36.664194	1777.437869	17.234509
36.492696	1783.550103	17.239527
36.727832	1783.427735	17.244544
36.634037	1781.242781	17.249562
36.441366	1785.005804	17.254579
36.810073	1770.631762	17.259597
36.802357	1779.425983	17.264615
37.025557	1777.716675	17.269632
36.990944	1782.997711	17.274650
36.881100	1781.766263	17.279667
36.987364	1782.630340	17.284685
36.863014	1791.080569	17.289703
37.021597	1776.611826	17.294720
36.726408	1779.546439	17.299738
36.886632	1782.265261	17.304755
37.055342	1801.635709	17.309773
37.390055	1804.341650	17.314791
36.993555	1802.157780	17.319808
37.098334	1820.027473	17.324826
36.950596	1809.812496	17.329843
37.410284	1802.682267	17.334861
37.212637	1813.983671	17.339879
37.506876	1815.303862	17.344896
37.799538	1806.719183	17.349914
37.533973	1806.572849	17.354931
37.582667	1801.214217	17.359949
37.575776	1807.529095	17.364967
37.886718	1801.988627	17.369984
37.936719	1787.272123	17.375002
37.350216	1784.013449	17.380019
37.945947	1768.726188	17.385037
37.362449	1774.440851	17.390055
37.386246	1783.443205	17.395072
37.954373	1789.078017	17.400090
37.525931	1805.778970	17.405107
37.652921	1805.980608	17.410125
37.913874	1808.550441	17.415143
37.705332	1801.930297	17.420160
37.857288	1808.569858	17.425178
37.842637	1805.739098	17.430195
38.167163	1796.830787	17.435213
37.777506	1801.491232	17.440231
37.949830	1801.862615	17.445248
38.047619	1797.123826	17.450266
38.180434	1811.863261	17.455283
37.948158	1803.083868	17.460301
38.032431	1796.691532	17.465319
37.994181	1796.416916	17.470336
38.357789	1792.233514	17.475354
38.326267	1802.669944	17.480371
38.174448	1801.094385	17.485389
37.951579	1810.033059	17.490407
38.203996	1826.767020	17.495424
38.528346	1831.652599	17.500442
38.524252	1832.500460	17.505459
38.599575	1829.832320	17.510477
38.490386	1832.523332	17.515495
38.430538	1831.773932	17.520512
38.787054	1823.582563	17.525530
38.324758	1839.931070	17.530547
38.803895	1818.096160	17.535565
38.654036	1835.683998	17.540583
38.474928	1833.648718	17.545600
38.782380	1822.330738	17.550618
38.771537	1835.862933	17.555635
38.839141	1832.594307	17.560653
38.583263	1830.063155	17.565671
38.661943	1830.915904	17.570688
38.505134	1835.671363	17.575706
38.545860	1850.994208	17.580723
38.676997	1855.979829	17.585741
38.868507	1860.483887	17.590759
38.898086	1854.577692	17.595776
39.318603	1857.623122	17.600794
38.947608	1859.824182	17.605811
38.946468	1863.573194	17.610829
39.115576	1872.508379	17.615847
39.044661	1863.933675	17.620864
39.335634	1866.519968	17.625882
39.091963	1881.151984	17.630899
39.577169	1880.865453	17.635917
39.337763	1896.413148	17.640935
39.483857	1902.099587	17.645952
39.780743	1889.581373	17.650970
39.346900	1889.864598	17.655987
39.630894	1900.566972	17.661005
39.398591	1900.432636	17.666023
39.930091	1891.485750	17.671040
40.185503	1882.785050	17.676058
39.889689	1889.116943	17.681075
39.982985	1881.350581	17.686093
39.681693	1865.241182	17.691111
39.538007	1855.030246	17.696128
40.002328	1871.635288	17.701146
39.902501	1881.044407	17.706163
40.199988	1881.140983	17.711181
40.274783	1875.584666	17.716199
39.897987	1870.586473	17.721216
40.253196	1855.774027	17.726234
39.850497	1859.281900	17.731251
39.970062	1871.965081	17.736269
40.008138	1879.008253	17.741287
40.004627	1881.431505	17.746304
40.371431	1877.331732	17.751322
39.865811	1885.536854	17.756339
39.831910	1883.590885	17.761357
39.853668	1878.467770	17.766375
39.792712	1884.315435	17.771392
40.224961	1899.100800	17.776410
40.105258	1907.883857	17.781427
40.359357	1908.549746	17.786445
40.342202	1905.824766	17.791463
40.288776	1917.476078	17.796480
40.520311	1917.901731	17.801498
40.584665	1917.098695	17.806515
40.380453	1916.207924	17.811533
40.749655	1918.314530	17.816551
40.518525	1928.695578	17.821568
41.322633	1928.480100	17.826586
40.800817	1934.166108	17.831603
40.723320	1925.726134	17.836621
41.277140	1938.303142	17.841639
40.860515	1935.855029	17.846656
41.026609	1927.227542	17.851674
41.002117	1934.388479	17.856691
41.035121	1935.589101	17.861709
41.241778	1935.592406	17.866727
41.194147	1942.152956	17.871744
41.475821	1935.472654	17.876762
41.372263	1945.613916	17.881779
41.304388	1925.054592	17.886797
41.305702	1916.476990	17.891815
41.448248	1920.166131	17.896832
41.109252	1909.534820	17.901850
41.521500	1916.512825	17.906867
41.561595	1934.021718	17.911885
41.189647	1931.509060	17.916903
41.362141	1940.236880	17.921920
41.270057	1935.454394	17.926938
41.253587	1948.905002	17.931955
41.432270	1944.566210	17.936973
41.401774	1942.379788	17.941991
41.418877	1944.309733	17.947008
42.004658	1944.125932	17.952026
41.712857	1944.369984	17.957043
41.834730	1942.493550	17.962061
41.918846	1937.572053	17.967079
41.700580	1944.445343	17.972096
42.028788	1931.201604	17.977114
41.996170	1942.066986	17.982131
41.719109	1940.881072	17.987149
42.100944	1959.512977	17.992167
41.871154	1972.778965	17.997184
42.011071	1976.763503	18.002202
42.277358	1970.035299	18.007219
42.320220	1971.057375	18.012237
42.866243	1967.175975	18.017255
42.433290	1971.015124	18.022272
42.853296	1953.948170	18.027290
42.612578	1937.043251	18.032307
42.440579	1935.296278	18.037325
42.551184	1927.129129	18.042343
42.257976	1928.274021	18.047360
42.314668	1936.623095	18.052378
42.614417	1936.989889	18.057395
42.457560	1950.418842	18.062413
42.688198	1962.046120	18.067431
42.493640	1971.115666	18.072448
42.619387	1954.762652	18.077466
42.613029	1963.958703	18.082483
42.614607	1973.427218	18.087501
42.733749	1962.162763	18.092519
42.476312	1974.279270	18.097536
42.694101	1970.944971	18.102554
42.769823	1968.905209	18.107571
42.669071	1968.646064	18.112589
43.007570	1981.622420	18.117607
42.980642	1990.013964	18.122624
42.898618	1990.890780	18.127642
43.359600	1991.667619	18.132659
43.426372	1994.582297	18.137677
43.432782	1988.121280	18.142695
43.111914	1995.512788	18.147712
43.515949	1991.579303	18.152730
43.053112	1991.507692	18.157747
43.235124	1994.426014	18.162765
43.661130	1996.554248	18.167783
43.354467	1998.406843	18.172800
43.328627	1992.853161	18.177818
43.287490	1999.409554	18.182835
43.464681	1998.566492	18.187853
43.619740	1994.366743	18.192871
43.385643	1996.940058	18.197888
43.715510	1987.337027	18.202906
43.705950	1987.859343	18.207923
43.662155	1997.213193	18.212941
43.872403	2007.766948	18.217959
43.824360	2022.328575	18.222976
44.052256	2017.210288	18.227994
44.245518	2019.071245	18.233011
44.138268	2022.506864	18.238029
44.406402	1988.394766	18.243047
44.031798	1988.663824	18.248064
44.383995	1983.350319	18.253082
44.287810	1992.154846	18.258099
44.334010	1984.430549	18.263117
44.236598	1977.879122	18.268135
44.197157	1983.095715	18.273152
44.301742	1976.674104	18.278170
44.408211	1978.466309	18.283187
44.168956	1997.459250	18.288205
45.026487	2004.869682	18.293223
44.622262	2008.207147	18.298240
44.454650	1993.660433	18.303258
44.546700	1989.017672	18.308275
44.609789	2012.267294	18.313293
44.748370	2013.362202	18.318311
44.430514	2019.873858	18.323328
44.583729	2013.550661	18.328346
44.720932	2013.044335	18.333363
44.629079	2009.136451	18.338381
44.588881	2005.662381	18.343399
44.847054	2011.236599	18.348416
44.710525	2013.536361	18.353434
45.021276	2005.850088	18.358451
44.945777	2010.364530	18.363469
44.713992	1999.594136	18.368487
44.924526	2017.094822	18.373504
45.316008	2029.730838	18.378522
45.298912	2028.143992	18.383539
45.075433	2035.530212	18.388557
45.214109	2025.413344	18.393575
45.382288	2032.080309	18.398592
45.161337	2019.649297	18.403610
45.272775	2031.128889	18.408627
45.306628	2032.274325	18.413645
45.480070	2026.048577	18.418663
45.322844	2031.423196	18.423680
45.246148	2030.372857	18.428698
45.755557	2016.813043	18.433715
45.439300	2029.506880	18.438733
45.730149	2042.140081	18.443751
45.773307	2052.551406	18.448768
45.532331	2055.704744	18.453786
45.982566	2051.874783	18.458803
45.975762	2050.678791	18.463821
46.198812	2049.219606	18.468839
46.139523	2054.995496	18.473856
46.221204	2056.226906	18.478874
46.295142	2032.299527	18.483891
46.053565	2026.523819	18.488909
46.012723	2030.174593	18.493927
46.287060	2033.395185	18.498944
46.213190	2041.589737	18.503962
46.115700	2047.451160	18.508979
46.072852	2051.681175	18.513997
46.492777	2049.509420	18.519015
46.343524	2051.410853	18.524032
46.399703	2045.783502	18.529050
46.657438	2044.648359	18.534067
46.319865	2062.581824	18.539085
46.671224	2049.939160	18.544103
46.383025	2054.547320	18.549120
46.450534	2060.035554	18.554138
46.409694	2052.615348	18.559155
46.313474	2055.322423	18.564173
46.185125	2055.062958	18.569191
46.303450	2078.242523	18.574208
46.358825	2086.130960	18.579226
46.440957	2085.448571	18.584243
46.580751	2100.693738	18.589261
46.697804	2113.504956	18.594279
47.283451	2107.410860	18.599296
47.064563	2121.361136	18.604314
47.578113	2112.605758	18.609331
47.285626	2122.479163	18.614349
47.421611	2113.983793	18.619367
47.516096	2108.113551	18.624384
47.309934	2122.455872	18.629402
47.623550	2107.977807	18.634419
47.429335	2114.058406	18.639437
47.491126	2117.143017	18.644455
47.724657	2110.874614	18.649472
47.168653	2116.676264	18.654490
47.402388	2112.557535	18.659507
47.340762	2118.184373	18.664525
47.621165	2123.287863	18.669543
47.643606	2122.050232	18.674560
47.705197	2120.520044	18.679578
47.617360	2116.672843	18.684595
47.596282	2112.510592	18.689613
47.746871	2113.862376	18.694631
47.998707	2113.060103	18.699648
47.928783	2111.585500	18.704666
48.091726	2123.731045	18.709683
48.100710	2141.654168	18.714701
48.410028	2130.001360	18.719719
48.371347	2126.686693	18.724736
48.353374	2122.738679	18.729754
48.419386	2112.051275	18.734771
48.136335	2123.610378	18.739789
48.262832	2114.736605	18.744807
48.401058	2101.618189	18.749824
48.111582	2116.763513	18.754842
48.480705	2119.022758	18.759859
48.289471	2137.798993	18.764877
48.806157	2142.743672	18.769895
48.863471	2128.019366	18.774912
48.726049	2143.963223	18.779930
48.903772	2136.176967	18.784947
48.942980	2137.817886	18.789965
48.727390	2138.159905	18.794983
48.724536	2138.357874	18.800000
48.576112	2150.066212	18.805018
48.778514	2140.547910	18.810035
48.717692	2144.957012	18.815053
48.643383	2142.746084	18.820071
48.904641	2139.969575	18.825088
48.813348	2151.195284	18.830106
49.125559	2156.067179	18.835123
49.127620	2162.343814	18.840141
49.089477	2163.131838	18.845159
49.297995	2165.253098	18.850176
49.086265	2176.962115	18.855194
49.251587	2163.371309	18.860211
49.343335	2167.796986	18.865229
49.264118	2171.793716	18.870247
49.234672	2166.783281	18.875264
49.323394	2175.794400	18.880282
49.586812	2178.353682	18.885299
49.657862	2188.317813	18.890317
49.877606	2206.632939	18.895335
49.948919	2200.212604	18.900352
49.724297	2205.629499	18.905370
50.050081	2197.317759	18.910387
49.942475	2197.596935	18.915405
50.018344	2195.340023	18.920423
50.030245	2189.169075	18.925440
49.571209	2204.207027	18.930458
50.029605	2196.641051	18.935475
50.204802	2195.143077	18.940493
49.987917	2197.444671	18.945511
50.292771	2195.021452	18.950528
50.306149	2196.450188	18.955546
50.211863	2196.222256	18.960563
50.215084	2206.890980	18.965581
49.800333	2199.101651	18.970599
50.330061	2211.347658	18.975616
50.276175	2222.462053	18.980634
50.477729	2226.529645	18.985651
50.426078	2230.568404	18.990669
50.644522	2226.260943	18.995687
50.718803	2223.952366	19.000704
50.821401	2226.696981	19.005722
50.822872	2228.949596	19.010739
50.711154	2219.472690	19.015757
50.486550	2222.400850	19.020775
51.058688	2222.043032	19.025792
50.916052	2226.207995	19.030810
50.988671	2214.119350	19.035827
51.227386	2229.519563	19.040845
51.127090	2222.410014	19.045863
51.184385	2218.784265	19.050880
51.023249	2230.073874	19.055898
51.283097	2241.736834	19.060915
51.299997	2252.585896	19.065933
51.124275	2254.001536	19.070951
51.732951	2246.247957	19.075968
51.584956	2251.153168	19.080986
51.601769	2254.754686	19.086003
51.466331	2256.620905	19.091021
51.447559	2255.112172	19.096039
51.926238	2245.108467	19.101056
51.478445	2245.562248	19.106074
51.728127	2244.347357	19.111091
51.806468	2244.494622	19.116109
51.582088	2248.310014	19.121127
51.887832	2249.463230	19.126144
51.629900	2246.317225	19.131162
51.796879	2247.436725	19.136179
51.768945	2249.972482	19.141197
51.718495	2280.474044	19.146215
52.065234	2281.000897	19.151232
51.741967	2293.224130	19.156250
51.915007	2281.471016	19.161267
52.172437	2282.044363	19.166285
52.003606	2281.626167	19.171303
52.200995	2289.549486	19.176320
52.481071	2305.000603	19.181338
52.329132	2308.501622	19.186355
52.699639	2303.762436	19.191373
52.647640	2308.326709	19.196391
52.838484	2302.802063	19.201408
52.636741	2307.978584	19.206426
52.821644	2304.078395	19.211443
52.956593	2300.850052	19.216461
52.925983	2304.979865	19.221479
53.338387	2303.169529	19.226496
53.008823	2308.943790	19.231514
52.945042	2314.143146	19.236531
52.975671	2302.960978	19.241549
52.867135	2310.793875	19.246567
52.953805	2302.013652	19.251584
52.812044	2308.539038	19.256602
53.149101	2307.752266	19.261619
53.248443	2299.447481	19.266637
53.074277	2309.571152	19.271655
53.143512	2314.908969	19.276672
53.434582	2330.921555	19.281690
53.253939	2334.870793	19.286707
53.492298	2333.601067	19.291725
53.549841	2330.829483	19.296743
53.677396	2335.116567	19.301760
53.278001	2339.705580	19.306778
53.678014	2330.845474	19.311795
53.888978	2330.501996	19.316813
53.594771	2340.500102	19.321831
53.846567	2334.858746	19.326848
53.844792	2330.960793	19.331866
53.751091	2332.303578	19.336883
54.245953	2345.751658	19.341901
54.159790	2354.119035	19.346919
54.219504	2352.977695	19.351936
54.343453	2361.500347	19.356954
54.557149	2359.477855	19.361971
54.680829	2346.272656	19.366989
54.288541	2338.858802	19.372007
54.403440	2335.267886	19.377024
54.150941	2326.342737	19.382042
54.276293	2340.117971	19.387059
54.415069	2349.539678	19.392077
54.228093	2352.015081	19.397095
54.191289	2347.083629	19.402112
54.121428	2346.736958	19.407130
54.496268	2366.183831	19.412147
54.622103	2375.538399	19.417165
54.860960	2391.962113	19.422183
54.936608	2378.976924	19.427200
55.352890	2387.287783	19.432218
55.184826	2389.389692	19.437235
55.410249	2379.440446	19.442253
55.490084	2384.706592	19.447271
55.498228	2381.768255	19.452288
55.124252	2379.808812	19.457306
55.298052	2385.355728	19.462323
55.774449	2377.601154	19.467341
55.424707	2380.734939	19.472359
55.104874	2375.445884	19.477376
55.572797	2381.758436	19.482394
55.402479	2386.046633	19.487411
55.491022	2381.808614	19.492429
55.586137	2382.369311	19.497447
55.701740	2377.714805	19.502464
55.719574	2383.458858	19.507482
55.552994	2375.935048	19.512499
55.719908	2372.239864	19.517517
55.758071	2387.766621	19.522535
55.716978	2401.629813	19.527552
55.881280	2405.583836	19.532570
56.018717	2408.429119	19.537587
55.871309	2408.747684	19.542605
56.385480	2413.858830	19.547623
56.347477	2409.512771	19.552640
56.107828	2408.167465	19.557658
56.360369	2412.471607	19.562675
56.481667	2415.174733	19.567693
55.827286	2412.566234	19.572711
56.060153	2409.784765	19.577728
56.621664	2412.037758	19.582746
56.752662	2424.640152	19.587763
56.608471	2437.301392	19.592781
56.921648	2433.358686	19.597799
56.860906	2445.019452	19.602816
57.144759	2435.086807	19.607834
56.716460	2418.276532	19.612851
56.915663	2419.771617	19.617869
57.117866	2433.938203	19.622887
57.085884	2442.605333	19.627904
57.285224	2440.205983	19.632922
56.867961	2444.796305	19.637939
56.934329	2437.263627	19.642957
57.081848	2437.133206	19.647975
57.138516	2439.379410	19.652992
57.412603	2439.325553	19.658010
57.376673	2440.446754	19.663027
57.600802	2438.611370	19.668045
57.321925	2445.047775	19.673063
57.365157	2439.366491	19.678080
57.606845	2433.062827	19.683098
57.612599	2442.353211	19.688115
57.755057	2458.500549	19.693133
57.790521	2469.508851	19.698151
57.744399	2452.868054	19.703168
57.646147	2456.181990	19.708186
57.403398	2460.759429	19.713203
57.856326	2452.909448	19.718221
57.745985	2459.783070	19.723239
57.534431	2467.516065	19.728256
58.079669	2479.676448	19.733274
57.699655	2494.234069	19.738291
57.671005	2486.784168	19.743309
58.029764	2491.259389	19.748327
57.844479	2499.773233	19.753344
58.455311	2509.704196	19.758362
58.109885	2523.505131	19.763379
58.541550	2518.362038	19.768397
58.717059	2507.798469	19.773415
58.501301	2516.979496	19.778432
58.952471	2514.259942	19.783450
58.634448	2516.053842	19.788467
58.901260	2506.120721	19.793485
59.430103	2511.157195	19.798503
59.307428	2504.740921	19.803520
59.666473	2502.639381	19.808538
59.311642	2507.319662	19.813555
59.416516	2501.707968	19.818573
59.224608	2493.198600	19.823591
59.410401	2501.489650	19.828608
59.684492	2498.976898	19.833626
59.548088	2502.295355	19.838643
59.780328	2496.784486	19.843661
59.394617	2486.761159	19.848679
59.305008	2504.034206	19.853696
59.428767	2498.093065	19.858714
59.547339	2508.620903	19.863731
59.502766	2501.930238	19.868749
59.619429	2509.201092	19.873767
59.366042	2515.133188	19.878784
59.622968	2507.883147	19.883802
59.343756	2509.902116	19.888819
59.594284	2517.264894	19.893837
59.688924	2534.537696	19.898855
59.825663	2539.677619	19.903872
59.949164	2531.669329	19.908890
59.984314	2545.614103	19.913907
60.128742	2541.562201	19.918925
60.201186	2528.516822	19.923943
60.195935	2543.414313	19.928960
60.490215	2558.277419	19.933978
60.667144	2564.015049	19.938995
60.857670	2567.598378	19.944013
60.816298	2572.043836	19.949031
60.514837	2569.644104	19.954048
61.107288	2565.630865	19.959066
60.933420	2570.367256	19.964083
60.709005	2566.834334	19.969101
60.906971	2560.373976	19.974119
60.460989	2561.728130	19.979136
60.859345	2564.020542	19.984154
60.924162	2561.300457	19.989171
61.084059	2568.249020	19.994189
60.946254	2560.158107	19.999207
60.848086	2559.652332	20.004224
61.554030	2566.926770	20.009242
61.279173	2570.947732	20.014259
60.979743	2575.307706	20.019277
61.449212	2582.999794	20.024295
61.540157	2582.506334	20.029312
61.666958	2575.650648	20.034330
61.876976	2584.137678	20.039347
61.785079	2580.277629	20.044365
62.123432	2591.091408	20.049383
61.919696	2588.197047	20.054400
62.080422	2575.444321	20.059418
62.188150	2576.578804	20.064435
62.015263	2579.827584	20.069453
62.229132	2576.331735	20.074471
62.230011	2581.940917	20.079488
62.415574	2563.530952	20.084506
62.492104	2572.582018	20.089523
62.303997	2580.444268	20.094541
62.483277	2575.243083	20.099559
62.156156	2577.280714	20.104576
62.435463	2576.713163	20.109594
62.440967	2582.695242	20.114611
62.437236	2591.600227	20.119629
62.660470	2581.294864	20.124647
62.332104	2593.826720	20.129664
62.586908	2583.650829	20.134682
62.434022	2578.731520	20.139699
62.715653	2600.469991	20.144717
62.847962	2604.946754	20.149735
62.526062	2611.371215	20.154752
62.550891	2602.830362	20.159770
62.748827	2607.488589	20.164787
62.457873	2618.678065	20.169805
63.151682	2629.592501	20.174823
63.120423	2642.082520	20.179840
63.225546	2639.787050	20.184858
63.231261	2642.989267	20.189875
63.013123	2645.926704	20.194893
63.291203	2641.070790	20.199911
63.114286	2666.411190	20.204928
63.292892	2670.842046	20.209946
63.695411	2672.989077	20.214963
63.656947	2674.258581	20.219981
63.850400	2666.034544	20.224999
63.688217	2672.737974	20.230016
63.982970	2673.369888	20.235034
64.216568	2669.502740	20.240051
63.964327	2671.224812	20.245069
64.015669	2666.787341	20.250087
64.050626	2688.404817	20.255104
64.291112	2688.859747	20.260122
64.284031	2697.921866	20.265139
64.398107	2695.590349	20.270157
64.622738	2685.633943	20.275175
64.325628	2696.305300	20.280192
64.562347	2688.941190	20.285210
64.829761	2696.561732	20.290227
64.653474	2692.656904	20.295245
65.045724	2690.692418	20.300263
64.728066	2699.289630	20.305280
64.933381	2694.003231	20.310298
65.154082	2691.230730	20.315315
64.971468	2700.603236	20.320333
65.365442	2693.566442	20.325351
64.787416	2690.808842	20.330368
65.010345	2699.418951	20.335386
65.363997	2710.431749	20.340403
65.375795	2709.337355	20.345421
65.566977	2714.396290	20.350439
65.262011	2724.669325	20.355456
65.471956	2723.437922	20.360474
65.620636	2720.331581	20.365491
65.385814	2726.405537	20.370509
65.578166	2713.703496	20.375527
65.310065	2723.464075	20.380544
65.456260	2713.056063	20.385562
65.699756	2712.643674	20.390579
65.729720	2731.988719	20.395597
66.011037	2739.454465	20.400615
66.038537	2747.774834	20.405632
66.358989	2752.521334	20.410650
66.355470	2748.806827	20.415667
66.275304	2746.846883	20.420685
66.432708	2739.132770	20.425703
66.392585	2749.063886	20.430720
66.306780	2751.957427	20.435738
66.548540	2745.568665	20.440755
66.454234	2747.813822	20.445773
66.545241	2736.163888	20.450791
66.304663	2746.035725	20.455808
66.382045	2745.190449	20.460826
66.658111	2740.936578	20.465843
66.615486	2768.186859	20.470861
66.729098	2771.482022	20.475879
66.576899	2774.122642	20.480896
66.544827	2771.854539	20.485914
67.239089	2767.357764	20.490931
66.963303	2787.528029	20.495949
67.320523	2796.832593	20.500967
67.406264	2796.850466	20.505984
67.421561	2800.293465	20.511002
67.545293	2799.324376	20.516019
67.443454	2798.224500	20.521037
67.709120	2804.812558	20.526055
67.752136	2799.463906	20.531072
67.643171	2811.619566	20.536090
67.906692	2809.159578	20.541107
67.745221	2804.939285	20.546125
67.581969	2799.727362	20.551143
67.540216	2805.976650	20.556160
67.673956	2819.361626	20.561178
67.900778	2831.920772	20.566195
68.049010	2834.417521	20.571213
68.217711	2834.188540	20.576231
68.390156	2833.206960	20.581248
68.270183	2838.673471	20.586266
68.406279	2833.731586	20.591283
68.478228	2831.280122	20.596301
68.278474	2834.637862	20.601319
68.489737	2846.174544	20.606336
68.712488	2859.984292	20.611354
69.103608	2862.208685	20.616371
69.085781	2862.953389	20.621389
69.191752	2856.920547	20.626407
69.240379	2861.519287	20.631424
69.226947	2866.675411	20.636442
69.220988	2862.966770	20.641459
69.049902	2865.932144	20.646477
69.495749	2856.572781	20.651495
69.351259	2859.828106	20.656512
69.485250	2869.146293	20.661530
69.673671	2853.799372	20.666547
69.179545	2864.098739	20.671565
69.522993	2857.382998	20.676583
69.646376	2856.945712	20.681600
69.491532	2857.440099	20.686618
69.636736	2853.457997	20.691635
69.519809	2860.457141	20.696653
69.813658	2860.017840	20.701671
69.416082	2859.316741	20.706688
69.293039	2866.973687	20.711706
70.066797	2878.569357	20.716723
69.795667	2878.147005	20.721741
69.799655	2885.196886	20.726759
69.841958	2889.537061	20.731776
69.872381	2895.890509	20.736794
70.213434	2913.713635	20.741811
70.298616	2910.892697	20.746829
70.174768	2912.388226	20.751847
70.434246	2907.451810	20.756864
70.383910	2924.246332	20.761882
71.050412	2933.552789	20.766899
71.132107	2938.475873	20.771917
71.061523	2934.290604	20.776935
71.047679	2932.691341	20.781952
70.871015	2941.644571	20.786970
71.165364	2941.681092	20.791987
71.157193	2941.325354	20.797005
71.134647	2934.461068	20.802023
71.089428	2942.272405	20.807040
70.884959	2945.387856	20.812058
71.391219	2933.056403	20.817075
71.459397	2942.471662	20.822093
71.724578	2953.496394	20.827111
72.013795	2956.392309	20.832128
71.731721	2960.246976	20.837146
71.875539	2962.060093	20.842163
71.944864	2961.127202	20.847181
72.072427	2966.660477	20.852199
72.143127	2968.564705	20.857216
71.902079	2965.604636	20.862234
72.185101	2958.208621	20.867251
72.148171	2965.759064	20.872269
72.002865	2967.785842	20.877287
72.186314	2963.667818	20.882304
71.963363	2970.185994	20.887322
72.583077	2969.219601	20.892339
72.463734	2974.955873	20.897357
72.463065	2976.760571	20.902375
72.379716	2993.146674	20.907392
72.456430	2995.778358	20.912410
72.871452	2985.173888	20.917427
72.744816	2992.118793	20.922445
72.746903	2989.750027	20.927463
73.171708	2982.771896	20.932480
73.070965	2982.463172	20.937498
73.010011	2983.365791	20.942515
73.131781	2997.677119	20.947533
73.445579	3002.693001	20.952551
73.807412	3007.494342	20.957568
73.681099	3007.799328	20.962586
73.754512	2996.985025	20.967603
73.987472	2997.799867	20.972621
74.067201	2988.485437	20.977639
73.966392	2978.436784	20.982656
73.866080	2973.785060	20.987674
73.927909	2966.993044	20.992691
74.063813	2970.959616	20.997709
73.902012	2973.376830	21.002727
74.097440	2976.942174	21.007744
74.277977	2994.459832	21.012762
74.682509	2994.837481	21.017779
74.583447	3000.589408	21.022797
74.145939	2977.964459	21.027815
74.457707	2983.598942	21.032832
74.531573	2991.777544	21.037850
74.362322	2990.723016	21.042867
74.635503	3000.705809	21.047885
74.467190	2998.228919	21.052903
74.527294	2996.510875	21.057920
74.297637	3004.573486	21.062938
74.673650	3014.954439	21.067955
74.591648	3031.756495	21.072973
74.661554	3029.946422	21.077991
75.022557	3028.631121	21.083008
74.950459	3037.806866	21.088026
75.329895	3046.693498	21.093043
75.427405	3051.026489	21.098061
75.442869	3057.908646	21.103079
75.753234	3055.832886	21.108096
75.581862	3059.219975	21.113114
75.805922	3051.384941	21.118131
75.956179	3050.826943	21.123149
75.525058	3052.957525	21.128167
76.041598	3050.905522	21.133184
75.808752	3058.876636	21.138202
75.877593	3053.761333	21.143219
76.220098	3052.189394	21.148237
76.053106	3048.938246	21.153255
76.230698	3056.161898	21.158272
76.133396	3077.696422	21.163290
76.135282	3073.170746	21.168307
76.501669	3071.085264	21.173325
76.349825	3081.780143	21.178343
76.242914	3078.514686	21.183360
76.477848	3076.344759	21.188378
76.471334	3084.547244	21.193395
76.370595	3101.448336	21.198413
76.227331	3115.133415	21.203431
76.432518	3116.217786	21.208448
76.483642	3121.956821	21.213466
76.812546	3136.075566	21.218483
77.009859	3144.170848	21.223501
76.902253	3148.105508	21.228519
76.965183	3151.946894	21.233536
77.192444	3157.716063	21.238554
77.622908	3171.705370	21.243571
77.733909	3172.821286	21.248589
77.948488	3183.047180	21.253607
77.927763	3175.881997	21.258624
77.707571	3185.584897	21.263642
77.574442	3186.372392	21.268659
77.882201	3174.723726	21.273677
78.416092	3162.386103	21.278695
79.105581	3145.535167	21.283712
79.215275	3143.713228	21.288730
78.813052	3119.260599	21.293747
78.902823	3114.414896	21.298765
79.061522	3118.292132	21.303783
78.900389	3092.629021	21.308800
78.662828	3107.735620	21.313818
78.471174	3106.178068	21.318835
78.869876	3105.567073	21.323853
78.697081	3102.494616	21.328871
78.930383	3105.264965	21.333888
79.092864	3102.179942	21.338906
78.814387	3105.482648	21.343923
79.145519	3100.243688	21.348941
79.075148	3101.880953	21.353959
79.168797	3104.689307	21.358976
78.982238	3111.399184	21.363994
79.493918	3131.492319	21.369011
79.586018	3136.647440	21.374029
79.320890	3140.631605	21.379047
79.660600	3144.538190	21.384064
79.268203	3139.636435	21.389082
79.549351	3147.402911	21.394099
79.818122	3134.564819	21.399117
79.714795	3144.314344	21.404135
79.694722	3161.989271	21.409152
79.910662	3166.469389	21.414170
79.730410	3169.771389	21.419187
79.816208	3169.716098	21.424205
79.650670	3190.085656	21.429223
79.987968	3207.488107	21.434240
80.104294	3207.918019	21.439258
80.064065	3211.853750	21.444275
80.475088	3228.253310	21.449293
80.405978	3241.506617	21.454311
80.615578	3238.374720	21.459328
80.845284	3235.528312	21.464346
80.787168	3245.655358	21.469363
81.341709	3236.486880	21.474381
81.120513	3239.093748	21.479399
81.533633	3232.640475	21.484416
81.679257	3229.272566	21.489434
81.462472	3219.044012	21.494451
81.781347	3221.316957	21.499469
81.736387	3227.499285	21.504487
81.649911	3221.554409	21.509504
81.657149	3221.219805	21.514522
81.467390	3230.313747	21.519539
81.743663	3231.945301	21.524557
81.828155	3224.030171	21.529575
82.028359	3221.606960	21.534592
81.919792	3217.153133	21.539610
81.714917	3220.858681	21.544627
82.249883	3235.205035	21.549645
82.284297	3252.736868	21.554663
82.136094	3255.446160	21.559680
82.589506	3248.219485	21.564698
82.617005	3256.548011	21.569715
82.652204	3251.979209	21.574733
82.398484	3260.810407	21.579751
82.461238	3250.162025	21.584768
82.483495	3262.743153	21.589786
82.401320	3269.960355	21.594803
82.623827	3273.106897	21.599821
82.501625	3280.700993	21.604839
82.815211	3283.611180	21.609856
82.942784	3306.364076	21.614874
83.024205	3319.094718	21.619891
83.257018	3306.626424	21.624909
83.224906	3315.482884	21.629927
83.365685	3320.688518	21.634944
83.571983	3313.954326	21.639962
83.413222	3337.579691	21.644979
83.734399	3343.751663	21.649997
83.864423	3341.883192	21.655015
84.008849	3348.943939	21.660032
84.138883	3342.140872	21.665050
83.830456	3348.983568	21.670067
84.326947	3333.078061	21.675085
84.061728	3348.255395	21.680103
84.091269	3343.650495	21.685120
84.276569	3355.202735	21.690138
84.026708	3370.483052	21.695155
84.542691	3374.245165	21.700173
84.458729	3382.939234	21.705191
84.545258	3380.551432	21.710208
84.850670	3381.093577	21.715226
84.755785	3397.726618	21.720243
85.262860	3397.770123	21.725261
85.060863	3403.257005	21.730279
85.247077	3397.436910	21.735296
85.507540	3400.894444	21.740314
85.039765	3400.700882	21.745331
85.398181	3388.587717	21.750349
85.285555	3393.969092	21.755367
85.331118	3392.148697	21.760384
85.601494	3392.886011	21.765402
85.668909	3407.159211	21.770419
85.753627	3428.427654	21.775437
85.703736	3428.548184	21.780455
85.786460	3435.617239	21.785472
85.837633	3432.678122	21.790490
85.789961	3428.207439	21.795507
86.170410	3426.995202	21.800525
85.973694	3433.090115	21.805543
86.147622	3454.497765	21.810560
86.365676	3453.328730	21.815578
86.308531	3470.591445	21.820595
86.473324	3455.408928	21.825613
86.550556	3460.959071	21.830631
86.356481	3463.050332	21.835648
87.116048	3476.620085	21.840666
87.087355	3496.284646	21.845683
87.556000	3483.224793	21.850701
87.284745	3495.238558	21.855719
87.078784	3498.118368	21.860736
87.274073	3499.462368	21.865754
87.024018	3496.576784	21.870771
87.101961	3494.899103	21.875789
87.285399	3500.669891	21.880807
87.225333	3523.588352	21.885824
87.262100	3519.104961	21.890842
87.412685	3518.070185	21.895859
87.656439	3525.939585	21.900877
87.418896	3543.456923	21.905895
87.689612	3562.136923	21.910912
88.268232	3550.971035	21.915930
88.318493	3550.645296	21.920947
88.271169	3548.106537	21.925965
88.299869	3547.235940	21.930983
88.433953	3568.744510	21.936000
88.578364	3575.836047	21.941018
88.552378	3586.479755	21.946035
88.741285	3566.746423	21.951053
89.260771	3570.149317	21.956071
89.111340	3582.088658	21.961088
89.086972	3569.368522	21.966106
89.150027	3571.800318	21.971123
89.101024	3571.803497	21.976141
89.163402	3574.030085	21.981159
89.214783	3568.317172	21.986176
89.411562	3594.471975	21.991194
89.598808	3599.398116	21.996211
89.654607	3600.522869	22.001229
89.879624	3592.504106	22.006247
89.615625	3605.817141	22.011264
90.129067	3591.322272	22.016282
90.099213	3607.824821	22.021299
90.181219	3596.304652	22.026317
90.217775	3598.293072	22.031335
90.164675	3598.354330	22.036352
90.084662	3597.368910	22.041370
90.062067	3609.025303	22.046387
90.326906	3618.166557	22.051405
90.440372	3618.022681	22.056423
90.095172	3628.898257	22.061440
90.574460	3620.639905	22.066458
90.291684	3632.879815	22.071475
90.356490	3644.958893	22.076493
90.599180	3644.607184	22.081511
90.609837	3657.545283	22.086528
90.942672	3665.761627	22.091546
91.098386	3682.793981	22.096563
91.363575	3686.489187	22.101581
91.482085	3683.625028	22.106599
91.426129	3697.853678	22.111616
91.786933	3679.687340	22.116634
91.776683	3681.249001	22.121651
91.733090	3690.276650	22.126669
92.106683	3678.567530	22.131687
91.957240	3679.448116	22.136704
91.956716	3688.416189	22.141722
91.975535	3716.049402	22.146739
92.171046	3717.068497	22.151757
92.387350	3707.496621	22.156775
92.237923	3726.805508	22.161792
92.595407	3722.283496	22.166810
92.820242	3709.628123	22.171827
92.611616	3714.070705	22.176845
92.646806	3714.439627	22.181863
92.704892	3721.942266	22.186880
92.953902	3728.011844	22.191898
92.869644	3729.767032	22.196915
92.955882	3725.367729	22.201933
92.948003	3722.105214	22.206951
92.707038	3746.025183	22.211968
93.008659	3763.409599	22.216986
93.388481	3768.100553	22.222003
93.445464	3762.513324	22.227021
93.369283	3775.401655	22.232039
93.219522	3779.222846	22.237056
93.737942	3792.879339	22.242074
93.630320	3796.818894	22.247091
93.817918	3807.372060	22.252109
94.160132	3810.002457	22.257127
94.131096	3831.415492	22.262144
94.402786	3827.729196	22.267162
94.436867	3826.089939	22.272179
94.429517	3834.327590	22.277197
94.856017	3827.346435	22.282215
94.813264	3830.179828	22.287232
95.069161	3820.901284	22.292250
94.939307	3825.310884	22.297267
95.039705	3821.601560	22.302285
95.410245	3819.451595	22.307303
95.386977	3822.285026	22.312320
95.622708	3818.960040	22.317338
95.357426	3821.898932	22.322355
95.175942	3809.814096	22.327373
95.287221	3822.832267	22.332391
95.472737	3834.083558	22.337408
95.734142	3847.214689	22.342426
95.517331	3859.131960	22.347443
95.462146	3847.587846	22.352461
96.063793	3849.559344	22.357479
95.787253	3852.333264	22.362496
95.895411	3861.469764	22.367514
96.235026	3870.505638	22.372531
96.130946	3878.916860	22.377549
95.964556	3875.945483	22.382567
96.031059	3886.689513	22.387584
96.072811	3898.029859	22.392602
96.257682	3912.719061	22.397619
96.278412	3920.237985	22.402637
96.227099	3927.428560	22.407655
96.606326	3941.646259	22.412672
96.889596	3945.024766	22.417690
97.881490	3925.289554	22.422707
97.635168	3926.556913	22.427725
97.839074	3917.330654	22.432743
97.989068	3924.590605	22.437760
98.052049	3914.838510	22.442778
98.353840	3924.604974	22.447795
98.328653	3930.344695	22.452813
98.384115	3914.762992	22.457831
98.192786	3927.430671	22.462848
98.274592	3919.909719	22.467866
98.858788	3923.738981	22.472883
98.556993	3922.942308	22.477901
98.808910	3916.014126	22.482919
98.662751	3931.591581	22.487936
98.732253	3916.879268	22.492954
98.765103	3920.797241	22.497971
98.570075	3913.234692	22.502989
99.181992	3920.579885	22.508007
99.046764	3920.824161	22.513024
98.886427	3917.286981	22.518042
99.013583	3922.245628	22.523059
98.630918	3928.343651	22.528077
98.940145	3924.384665	22.533095
98.788880	3941.546514	22.538112
99.176808	3943.823511	22.543130
99.351957	3949.877428	22.548147
99.148869	3975.438234	22.553165
99.538992	3970.698540	22.558183
99.484339	3989.098997	22.563200
99.770715	3987.781358	22.568218
99.934668	3989.887184	22.573235
99.646131	4014.516101	22.578253
100.210958	4014.486685	22.583271
100.161457	4018.930729	22.588288
100.388591	4011.420381	22.593306
100.754840	4008.415171	22.598323
100.633115	4015.261440	22.603341
100.670938	4015.334159	22.608359
100.821156	4033.332261	22.613376
100.645157	4044.910409	22.618394
101.277609	4039.610483	22.623411
100.874069	4047.802086	22.628429
101.184394	4038.497419	22.633447
101.054518	4042.930688	22.638464
101.245712	4057.893578	22.643482
101.735934	4065.115075	22.648499
101.481996	4070.530245	22.653517
101.608068	4073.446897	22.658535
101.662771	4067.627058	22.663552
101.659155	4073.899124	22.668570
101.869633	4085.477820	22.673587
101.853586	4097.052528	22.678605
102.279303	4090.064295	22.683623
101.977673	4118.530540	22.688640
102.331283	4105.155718	22.693658
102.476099	4105.506381	22.698675
102.401835	4108.101768	22.703693
102.882340	4121.441290	22.708711
103.147952	4128.221123	22.713728
103.033115	4133.240459	22.718746
103.160249	4132.089019	22.723763
103.380201	4125.626832	22.728781
103.734223	4127.626847	22.733799
103.664442	4127.118848	22.738816
103.778680	4128.283884	22.743834
103.786729	4114.420563	22.748851
104.009247	4116.375466	22.753869
104.026946	4117.415867	22.758887
104.300517	4117.060011	22.763904
104.072291	4116.727536	22.768922
104.109106	4119.560096	22.773939
104.280933	4119.585486	22.778957
104.030007	4120.429573	22.783975
104.180551	4119.486018	22.788992
103.998167	4128.429866	22.794010
104.324245	4139.555135	22.799027
104.396791	4147.300343	22.804045
104.349082	4156.408389	22.809063
104.663080	4152.621652	22.814080
104.627892	4174.743396	22.819098
104.774450	4171.228802	22.824115
104.759787	4181.935643	22.829133
104.912299	4181.701360	22.834151
105.003867	4207.375277	22.839168
104.867776	4217.528800	22.844186
105.154272	4216.047492	22.849203
105.106396	4224.176968	22.854221
105.458481	4246.341690	22.859239
105.266989	4242.017991	22.864256
105.134896	4249.804541	22.869274
105.566424	4272.165106	22.874291
105.847269	4273.096685	22.879309
105.698838	4283.492949	22.884327
105.968705	4285.065072	22.889344
106.333928	4304.551467	22.894362
106.846206	4306.679674	22.899379
106.851499	4299.452365	22.904397
107.063376	4299.083530	22.909415
107.167427	4308.307500	22.914432
107.265952	4303.758954	22.919450
107.393217	4306.105111	22.924467
107.491813	4302.678377	22.929485
107.260010	4294.223880	22.934503
107.496031	4296.642375	22.939520
107.317579	4302.081779	22.944538
107.669007	4294.495612	22.949555
107.515473	4315.081151	22.954573
107.742943	4325.535503	22.959591
107.814315	4336.293245	22.964608
107.511586	4324.578971	22.969626
108.104853	4329.489387	22.974643
108.104527	4340.617298	22.979661
108.247417	4359.889839	22.984679
108.464558	4361.390136	22.989696
108.303421	4365.198344	22.994714
108.664388	4365.308431	22.999731
108.463728	4372.407395	23.004749
108.744703	4382.993288	23.009767
108.961220	4394.052045	23.014784
108.764858	4402.019636	23.019802
109.198179	4392.155461	23.024819
109.029303	4402.767476	23.029837
109.077669	4411.474877	23.034855
109.578653	4422.120904	23.039872
109.339262	4430.077279	23.044890
109.346080	4416.848736	23.049907
109.709606	4437.691058	23.054925
109.674204	4453.983819	23.059943
110.202727	4452.433212	23.064960
110.060462	4460.861868	23.069978
110.255022	4447.369709	23.074995
110.386039	4452.648107	23.080013
110.459670	4459.985797	23.085031
110.686610	4468.789053	23.090048
110.556272	4478.830914	23.095066
110.626691	4487.344461	23.100083
110.614680	4485.419828	23.105101
110.954428	4491.852086	23.110119
110.917419	4497.047942	23.115136
110.996310	4521.021217	23.120154
111.192083	4520.456697	23.125171
111.249707	4529.902978	23.130189
111.788978	4516.997736	23.135207
111.724827	4516.565923	23.140224
111.626936	4516.812120	23.145242
111.957039	4519.407605	23.150259
112.086814	4526.571168	23.155277
112.018074	4542.933066	23.160295
111.710199	4530.387902	23.165312
111.821811	4546.614839	23.170330
112.001512	4549.488419	23.175347
112.372615	4566.244359	23.180365
112.375279	4580.224568	23.185383
112.199372	4570.725693	23.190400
112.318197	4589.557884	23.195418
113.197349	4601.791888	23.200435
113.182748	4611.173429	23.205453
113.073350	4612.860352	23.210471
113.114682	4613.773506	23.215488
113.411864	4607.200456	23.220506
113.392720	4611.163093	23.225523
113.631249	4640.555913	23.230541
113.942327	4646.149458	23.235559
113.833582	4634.540890	23.240576
113.847529	4643.729089	23.245594
113.784507	4650.196536	23.250611
114.111695	4644.914397	23.255629
114.139021	4654.747931	23.260647
114.684316	4648.727691	23.265664
114.808244	4649.989563	23.270682
114.766396	4652.671134	23.275699
115.032965	4653.118042	23.280717
114.579520	4653.197515	23.285735
115.250543	4644.923757	23.290752
114.997841	4655.808149	23.295770
115.062072	4668.780289	23.300787
115.191985	4669.587276	23.305805
115.047446	4680.223145	23.310823
115.401044	4680.451631	23.315840
115.681203	4686.146101	23.320858
115.705554	4707.868941	23.325875
115.948994	4718.753720	23.330893
116.044521	4719.988658	23.335911
116.257804	4708.899833	23.340928
116.062221	4720.591772	23.345946
116.286299	4721.444322	23.350963
116.422543	4721.272417	23.355981
116.216576	4742.546634	23.360999
116.483568	4739.895395	23.366016
116.492388	4747.009909	23.371034
116.803772	4747.228607	23.376051
117.101345	4749.917434	23.381069
117.053274	4763.258440	23.386087
117.306921	4758.683445	23.391104
117.275682	4773.588129	23.396122
117.367382	4769.548748	23.401139
117.391371	4767.213965	23.406157
117.395819	4771.109159	23.411175
117.662350	4790.076182	23.416192
117.653107	4801.181474	23.421210
117.903789	4797.409393	23.426227
117.595426	4801.577118	23.431245
117.740588	4817.422952	23.436263
118.224564	4815.748032	23.441280
118.180713	4823.925186	23.446298
118.519431	4828.256430	23.451315
118.868589	4820.464237	23.456333
118.563354	4856.798885	23.461351
118.920512	4852.879214	23.466368
118.889971	4864.264876	23.471386
118.939683	4853.715755	23.476403
119.379163	4849.333741	23.481421
119.314135	4869.909873	23.486439
119.644051	4876.510654	23.491456
119.679455	4880.256969	23.496474
119.605192	4882.835970	23.501491
120.051332	4875.748921	23.506509
119.625421	4883.299437	23.511527
119.839684	4891.651031	23.516544
120.287675	4914.979980	23.521562
120.320573	4908.990208	23.526579
120.489806	4908.056212	23.531597
120.512219	4914.262334	23.536615
120.819325	4896.369767	23.541632
120.766829	4917.642577	23.546650
120.922573	4942.070022	23.551667
121.316137	4932.214190	23.556685
121.342816	4936.877659	23.561703
120.992478	4938.190796	23.566720
121.616563	4944.485079	23.571738
121.500116	4934.694839	23.576755
122.031878	4947.993901	23.581773
121.937989	4961.851405	23.586791
122.236533	4948.323327	23.591808
122.357145	4957.081681	23.596826
121.950693	4964.666111	23.601843
122.419118	4961.968551	23.606861
122.345783	4958.217415	23.611879
122.342704	4957.523310	23.616896
122.503035	4970.081521	23.621914
122.702375	4985.054284	23.626931
122.894373	4981.623513	23.631949
122.773530	4988.334774	23.636967
122.847917	4982.232935	23.641984
122.998849	4996.729591	23.647002
122.935718	5020.581568	23.652019
123.319306	5016.006229	23.657037
123.262616	5016.565276	23.662055
123.370725	5038.116326	23.667072
123.684526	5048.230934	23.672090
123.750253	5052.791446	23.677107
123.997775	5053.824374	23.682125
123.596769	5061.763588	23.687143
124.016497	5086.102759	23.692160
124.291839	5083.128355	23.697178
124.052182	5095.139164	23.702195
124.506514	5085.506413	23.707213
124.809650	5099.481684	23.712231
124.861683	5113.716509	23.717248
124.779445	5116.070242	23.722266
124.791475	5115.861496	23.727283
125.069971	5109.340770	23.732301
125.018205	5144.272294	23.737319
125.456742	5133.967011	23.742336
125.872539	5142.123756	23.747354
125.756280	5144.346026	23.752371
125.905369	5140.722231	23.757389
126.017428	5145.218738	23.762407
125.807795	5156.029755	23.767424
126.306875	5159.813921	23.772442
126.335794	5169.698682	23.777459
126.523265	5165.751705	23.782477
126.911025	5168.407347	23.787495
126.801355	5166.796372	23.792512
127.120727	5169.713889	23.797530
127.031809	5183.417394	23.802547
127.171369	5189.312284	23.807565
127.367395	5190.861667	23.812583
127.505764	5196.099823	23.817600
127.692713	5195.408448	23.822618
127.634073	5202.608679	23.827635
127.628770	5204.054061	23.832653
127.880088	5215.343123	23.837671
127.749058	5221.484940	23.842688
128.401940	5213.728292	23.847706
128.249952	5229.476407	23.852723
128.122420	5215.554211	23.857741
128.311034	5230.796426	23.862759
128.496109	5248.941511	23.867776
128.812560	5252.599835	23.872794
128.650966	5268.136315	23.877811
128.938322	5248.204089	23.882829
128.878802	5273.963748	23.887847
128.769207	5279.620684	23.892864
128.909773	5281.532955	23.897882
128.713798	5307.326232	23.902899
129.300813	5310.782504	23.907917
129.363875	5324.307702	23.912935
129.582517	5335.890803	23.917952
129.738867	5349.574233	23.922970
129.803289	5347.501979	23.927987
130.198471	5352.461641	23.933005
130.441197	5378.006495	23.938023
130.709555	5377.020474	23.943040
130.943533	5381.369372	23.948058
131.027631	5387.631157	23.953075
131.108705	5373.865154	23.958093
131.382159	5382.387754	23.963111
131.471857	5378.934654	23.968128
131.345926	5382.268605	23.973146
131.319375	5387.605508	23.978163
131.550389	5376.758823	23.983181
131.695145	5382.170685	23.988199
131.874504	5397.910200	23.993216
132.320491	5393.577343	23.998234
131.932372	5411.485168	24.003251
132.050996	5399.889306	24.008269
132.185711	5414.363783	24.013287
132.242661	5403.927194	24.018304
132.531419	5416.336280	24.023322
132.698738	5429.400436	24.028339
132.795648	5434.709801	24.033357
132.626824	5436.584885	24.038375
132.783328	5440.195594	24.043392
133.027361	5445.310778	24.048410
132.964887	5454.625747	24.053427
133.204359	5458.037556	24.058445
133.297094	5475.826297	24.063463
133.442022	5492.056043	24.068480
133.632845	5487.967618	24.073498
133.673848	5501.694758	24.078515
133.865167	5514.082486	24.083533
134.162291	5518.741566	24.088551
134.037292	5531.734411	24.093568
134.097207	5543.877980	24.098586
133.951186	5567.803849	24.103603
134.473806	5564.270660	24.108621
134.909660	5578.996247	24.113639
134.911233	5589.710961	24.118656
135.281538	5578.243980	24.123674
135.201328	5586.127597	24.128691
135.126121	5586.432348	24.133709
135.716120	5603.868945	24.138727
135.291842	5618.712844	24.143744
135.592462	5611.927954	24.148762
136.025067	5615.586730	24.153779
135.987761	5637.217702	24.158797
136.326848	5641.061338	24.163815
136.292582	5640.859180	24.168832
136.526047	5646.000509	24.173850
136.372908	5658.557365	24.178867
136.777898	5672.066124	24.183885
136.654163	5685.600983	24.188903
136.695896	5680.996557	24.193920
137.059272	5680.035491	24.198938
137.203537	5707.119791	24.203955
136.869956	5705.128260	24.208973
137.375682	5712.443306	24.213991
137.682087	5732.586909	24.219008
138.133243	5727.836933	24.224026
137.790797	5734.350983	24.229043
138.109403	5738.470919	24.234061
138.612496	5730.093529	24.239079
138.355970	5740.553682	24.244096
138.501528	5732.457531	24.249114
138.467250	5750.730262	24.254131
139.112214	5762.433756	24.259149
139.174942	5766.629119	24.264167
138.846182	5769.630437	24.269184
139.351933	5759.690869	24.274202
139.418557	5769.057833	24.279219
139.378544	5772.639378	24.284237
139.649918	5780.647993	24.289255
139.614623	5798.001210	24.294272
139.570398	5794.428537	24.299290
139.781564	5791.525596	24.304307
139.700489	5811.792461	24.309325
140.036643	5820.094461	24.314343
140.213827	5828.070915	24.319360
140.663054	5839.793094	24.324378
140.985672	5847.688934	24.329395
140.964629	5849.599512	24.334413
141.341582	5857.619658	24.339431
140.942547	5856.339559	24.344448
141.133329	5854.789961	24.349466
141.231596	5867.897773	24.354483
141.230292	5886.663442	24.359501
141.728365	5884.679321	24.364519
141.318048	5889.416706	24.369536
141.772197	5898.610237	24.374554
141.757957	5916.055435	24.379571
142.303642	5908.386335	24.384589
142.501069	5907.847466	24.389607
142.478606	5916.832193	24.394624
143.081786	5935.269437	24.399642
143.085513	5935.336589	24.404659
143.227774	5927.320322	24.409677
143.512041	5931.804559	24.414695
143.481941	5932.670964	24.419712
143.466656	5922.166065	24.424730
143.677519	5927.114403	24.429747
143.698588	5939.055208	24.434765
143.761584	5946.536954	24.439783
143.762176	5959.969627	24.444800
143.996939	5963.163581	24.449818
144.469425	5955.661911	24.454835
144.201658	5970.831321	24.459853
144.515034	5975.515493	24.464871
144.263971	5989.987531	24.469888
144.678881	5995.886833	24.474906
145.054079	5988.122926	24.479923
145.589920	5988.005310	24.484941
146.393450	5995.789929	24.489959
146.028819	5979.278542	24.494976
146.068371	5979.213310	24.499994
146.152750	5975.218829	24.505011
146.085140	5968.926796	24.510029
146.309187	5964.981644	24.515047
146.172812	5965.659647	24.520064
146.394883	5958.555104	24.525082
146.412627	5954.612953	24.530099
146.310777	5966.972278	24.535117
146.332532	5976.643143	24.540135
146.330279	5994.386286	24.545152
146.536899	5995.925413	24.550170
146.736676	6000.449894	24.555187
146.558347	6026.544518	24.560205
147.147664	6031.556858	24.565223
146.899587	6048.880568	24.570240
147.186273	6059.555667	24.575258
147.363393	6059.030260	24.580275
147.456427	6087.457812	24.585293
148.035103	6088.909300	24.590311
148.119713	6099.334980	24.595328
148.062433	6113.076785	24.600346
148.537389	6124.007515	24.605363
148.777318	6123.078696	24.610381
149.003898	6116.533553	24.615399
148.802946	6126.443805	24.620416
149.546687	6139.932812	24.625434
149.495771	6147.723148	24.630451
149.131118	6159.536805	24.635469
149.511825	6149.597249	24.640487
149.890873	6143.403081	24.645504
149.560912	6154.338652	24.650522
149.920610	6165.156397	24.655539
150.004272	6165.945667	24.660557
150.353300	6162.166218	24.665575
150.815592	6163.991114	24.670592
151.480875	6159.768630	24.675610
151.513768	6153.796452	24.680627
151.258718	6152.137736	24.685645
151.824815	6140.675298	24.690663
151.696936	6140.778385	24.695680
151.591533	6144.977061	24.700698
152.071104	6142.781066	24.705715
151.663548	6146.978353	24.710733
152.021919	6143.816622	24.715751
151.833821	6166.243464	24.720768
152.073238	6166.099942	24.725786
152.186243	6180.272570	24.730803
151.951448	6174.997677	24.735821
152.439562	6195.548034	24.740839
152.595530	6206.161470	24.745856
152.588561	6212.589189	24.750874
152.712732	6209.844809	24.755891
152.479192	6234.665343	24.760909
152.796945	6247.515046	24.765927
153.040939	6266.282996	24.770944
153.125115	6279.834026	24.775962
153.216869	6285.595355	24.780979
153.032358	6303.814829	24.785997
153.577564	6306.787050	24.791015
153.733020	6324.330772	24.796032
153.652283	6342.843746	24.801050
154.128181	6352.376352	24.806067
154.334524	6355.584366	24.811085
154.505384	6367.020109	24.816103
154.154929	6380.683807	24.821120
154.692657	6390.071249	24.826138
155.220507	6405.812135	24.831155
154.859789	6419.024305	24.836173
155.339972	6413.455933	24.841191
155.680604	6434.726460	24.846208
155.769147	6445.355538	24.851226
155.868356	6439.824298	24.856243
155.426855	6454.822053	24.861261
156.156472	6457.769622	24.866279
156.355517	6478.194941	24.871296
156.351767	6480.976199	24.876314
156.505910	6486.977076	24.881331
156.718138	6505.888873	24.886349
156.480311	6508.887639	24.891367
156.833696	6519.455659	24.896384
157.077797	6533.150584	24.901402
157.103177	6539.795168	24.906419
157.428496	6551.044342	24.911437
157.537085	6573.146746	24.916455
157.436517	6574.936339	24.921472
157.443791	6595.475012	24.926490
158.155410	6582.634141	24.931507
158.448166	6613.688710	24.936525
159.001783	6606.412973	24.941543
159.428596	6621.425874	24.946560
159.599910	6614.953056	24.951578
159.850875	6614.565352	24.956595
159.791596	6617.790598	24.961613
160.011976	6599.744581	24.966631
160.190652	6596.888367	24.971648
159.976477	6613.271020	24.976666
160.462444	6596.506081	24.981683
160.380952	6605.080478	24.986701
160.286803	6602.064766	24.991719
160.618602	6602.277102	24.996736
160.304364	6596.733831	25.001754
160.538204	6605.063606	25.006771
160.907610	6630.757230	25.011789
160.825575	6648.769591	25.016807
161.093780	6632.109361	25.021824
160.816384	6650.741411	25.026842
161.391165	6652.028349	25.031859
161.299225	6665.356032	25.036877
161.575282	6677.414924	25.041895
161.882386	6689.203718	25.046912
161.718362	6705.903432	25.051930
161.739973	6707.181798	25.056947
162.018599	6714.119691	25.061965
162.104531	6733.634163	25.066983
162.565082	6745.544884	25.072000
162.787844	6752.204514	25.077018
162.901004	6761.234219	25.082035
163.202665	6770.197681	25.087053
163.187773	6783.707529	25.092071
163.030727	6777.523831	25.097088
162.980495	6807.657047	25.102106
163.249702	6811.638815	25.107123
163.597143	6831.239971	25.112141
163.734629	6840.338234	25.117159
163.958269	6841.977812	25.122176
163.798533	6866.945783	25.127194
164.484673	6871.837542	25.132211
164.276225	6889.379369	25.137229
164.410089	6901.504391	25.142247
164.931473	6916.026480	25.147264
165.121741	6922.694514	25.152282
165.197140	6942.170810	25.157299
165.207578	6939.457021	25.162317
165.533088	6962.756022	25.167335
165.738311	6967.688299	25.172352
166.161204	6980.060004	25.177370
166.025818	6985.360542	25.182387
166.341524	6992.748232	25.187405
166.449841	6994.351923	25.192423
166.827205	7004.323194	25.197440
166.723392	7001.170459	25.202458
167.138961	7027.105262	25.207475
167.084535	7032.819373	25.212493
167.164292	7032.157600	25.217511
167.789858	7041.467721	25.222528
167.775146	7055.934581	25.227546
167.826467	7052.817686	25.232563
167.963271	7059.262189	25.237581
167.543306	7080.955489	25.242599
168.275713	7085.934365	25.247616
168.072275	7103.260049	25.252634
168.484138	7107.738467	25.257651
168.516435	7124.829880	25.262669
168.640297	7139.807811	25.267687
169.044223	7150.159711	25.272704
168.974833	7173.623510	25.277722
169.428136	7179.321245	25.282739
169.827962	7199.581779	25.287757
169.823927	7210.180529	25.292775
169.983514	7203.033427	25.297792
170.035203	7232.592591	25.302810
170.225464	7225.742737	25.307827
170.316546	7239.925380	25.312845
170.491142	7249.426350	25.317863
170.702573	7256.043163	25.322880
170.685706	7267.622052	25.327898
171.255157	7284.436012	25.332915
171.497775	7294.266871	25.337933
171.467585	7294.028632	25.342951
171.764726	7282.792331	25.347968
171.647556	7292.487777	25.352986
172.028354	7318.202807	25.358003
172.360169	7320.899244	25.363021
172.310097	7326.167416	25.368039
172.765225	7318.039931	25.373056
172.799099	7325.358630	25.378074
172.896592	7343.370744	25.383091
173.154797	7354.206331	25.388109
173.348842	7352.708781	25.393127
173.659922	7337.591030	25.398144
173.472002	7362.164602	25.403162
173.662102	7364.182556	25.408179
173.623796	7379.932917	25.413197
173.948300	7383.865108	25.418215
174.195686	7393.865234	25.423232
174.363040	7409.422317	25.428250
174.261718	7412.334187	25.433267
174.773155	7419.833304	25.438285
174.465202	7442.872104	25.443303
174.843474	7450.271292	25.448320
175.317660	7463.748629	25.453338
175.229306	7481.475798	25.458355
175.455740	7471.526917	25.463373
175.571891	7482.197974	25.468391
175.953956	7501.087894	25.473408
175.936578	7502.360742	25.478426
176.180109	7516.976508	25.483443
176.859538	7512.441378	25.488461
177.177905	7517.068596	25.493479
177.471921	7515.508665	25.498496
177.452074	7521.754091	25.503514
177.407129	7519.252036	25.508531
177.638704	7526.138013	25.513549
177.720417	7538.522879	25.518567
177.849647	7544.151250	25.523584
178.171086	7542.895395	25.528602
178.489719	7549.585736	25.533619
178.455573	7538.106992	25.538637
178.564965	7565.177423	25.543655
178.698719	7571.337003	25.548672
178.859044	7575.396928	25.553690
178.798856	7573.834451	25.558707
179.376950	7592.377700	25.563725
179.260756	7604.277204	25.568743
179.287619	7613.605246	25.573760
179.610287	7622.801936	25.578778
179.631608	7641.758208	25.583795
179.917311	7633.109120	25.588813
179.871219	7653.268260	25.593831
180.085568	7661.641868	25.598848
180.431018	7670.790891	25.603866
180.439646	7680.666396	25.608883
180.783171	7690.271336	25.613901
180.912902	7698.838650	25.618919
181.113042	7695.506684	25.623936
181.300035	7703.479438	25.628954
181.372529	7733.529647	25.633971
181.716817	7724.749201	25.638989
181.797779	7740.738234	25.644007
181.928305	7764.104989	25.649024
181.946737	7767.743005	25.654042
182.227387	7775.373525	25.659059
182.356377	7786.296127	25.664077
182.388033	7799.441444	25.669095
182.675799	7814.755493	25.674112
182.835228	7846.030612	25.679130
183.033654	7842.839739	25.684148
183.457638	7849.951711	25.689165
183.640816	7876.019474	25.694183
183.855674	7876.245758	25.699200
183.889907	7890.411330	25.704218
184.344417	7899.283435	25.709236
184.385807	7901.373960	25.714253
184.343401	7929.488267	25.719271
184.860167	7931.435332	25.724288
184.946897	7937.456988	25.729306
184.711248	7961.698433	25.734324
185.381624	7957.406191	25.739341
185.341895	7979.002395	25.744359
185.706100	7991.760041	25.749376
186.002172	7989.576915	25.754394
185.854084	7991.935696	25.759412
185.959252	8019.262575	25.764429
186.404703	8024.638088	25.769447
186.981890	8029.836401	25.774464
187.046987	8040.325177	25.779482
187.165324	8048.931492	25.784500
187.597768	8043.244628	25.789517
187.573849	8050.733816	25.794535
187.870089	8063.075079	25.799552
188.160251	8074.777184	25.804570
188.227365	8082.210169	25.809588
188.187496	8074.473989	25.814605
188.129371	8095.628700	25.819623
188.729373	8104.432879	25.824640
188.814595	8105.357745	25.829658
188.478355	8112.118521	25.834676
189.483174	8130.464178	25.839693
189.324593	8145.021130	25.844711
189.272318	8147.464988	25.849728
189.793543	8154.994004	25.854746
189.871295	8169.700581	25.859764
189.702589	8167.592319	25.864781
190.280146	8183.332682	25.869799
190.588867	8195.237303	25.874816
190.827226	8201.728276	25.879834
190.596004	8200.781208	25.884852
191.033857	8207.843142	25.889869
191.015340	8229.306487	25.894887
191.135665	8231.212930	25.899904
191.576360	8224.122821	25.904922
191.490868	8253.503645	25.909940
191.712056	8258.931524	25.914957
191.668859	8271.006808	25.919975
191.724534	8289.620056	25.924992
192.145535	8300.063681	25.930010
192.243730	8309.649512	25.935028
192.915551	8321.691890	25.940045
192.807313	8330.136586	25.945063
192.891006	8348.154868	25.950080
193.246331	8349.780312	25.955098
193.169834	8370.453606	25.960116
194.043528	8391.788314	25.965133
194.123841	8396.462811	25.970151
193.901779	8398.862958	25.975168
194.198388	8409.435873	25.980186
194.173439	8428.332845	25.985204
194.476257	8430.730365	25.990221
194.873592	8456.116189	25.995239
194.606962	8468.180040	26.000256
194.985544	8477.662651	26.005274
195.091638	8502.367486	26.010292
195.347670	8510.409145	26.015309
195.482006	8526.793409	26.020327
196.077061	8534.527643	26.025344
197.353674	8522.793131	26.030362
197.421571	8530.278937	26.035380
197.730810	8529.113478	26.040397
197.977227	8523.416355	26.045415
197.810759	8509.283630	26.050432
197.910586	8491.781393	26.055450
197.956815	8505.013929	26.060468
198.298102	8514.386047	26.065485
198.205118	8526.797618	26.070503
197.975408	8516.152348	26.075520
198.470734	8514.964305	26.080538
198.442148	8528.291022	26.085556
198.476532	8543.466014	26.090573
198.853178	8552.203379	26.095591
198.909890	8564.327105	26.100608
199.239994	8578.335595	26.105626
199.167402	8595.552041	26.110644
199.578431	8606.366931	26.115661
199.642823	8611.778230	26.120679
199.945184	8625.967459	26.125696
200.133274	8636.013681	26.130714
199.950642	8643.904617	26.135732
200.358784	8664.022602	26.140749
200.513712	8691.074042	26.145767
200.816950	8701.474952	26.150784
201.043853	8709.347845	26.155802
200.765800	8731.314425	26.160820
201.364802	8739.261001	26.165837
201.819074	8751.047645	26.170855
201.497652	8761.161411	26.175872
202.205486	8766.726721	26.180890
201.979938	8776.850000	26.185908
202.267222	8788.036508	26.190925
202.834848	8806.597895	26.195943
202.649159	8815.421527	26.200960
202.909016	8822.614827	26.205978
203.138304	8841.653568	26.210996
203.434664	8839.092550	26.216013
204.242266	8854.792622	26.221031
204.261132	8859.010410	26.226048
204.725027	8855.001086	26.231066
204.773653	8868.300450	26.236084
204.952337	8867.985209	26.241101
205.173429	8858.818869	26.246119
205.306875	8871.643571	26.251136
205.372642	8881.132244	26.256154
205.515474	8889.586016	26.261172
205.470293	8891.120348	26.266189
205.646826	8898.989962	26.271207
205.749344	8926.665960	26.276224
206.049315	8935.880855	26.281242
206.588718	8938.130964	26.286260
206.835505	8951.595544	26.291277
207.137656	8948.893117	26.296295
206.958235	8961.754397	26.301312
207.394874	8978.127161	26.306330
207.347321	8990.640076	26.311348
207.508675	8996.888705	26.316365
207.923175	9009.873323	26.321383
207.677799	9019.244857	26.326400
208.117306	9043.588162	26.331418
208.068316	9061.971170	26.336436
208.210966	9075.630313	26.341453
208.571759	9075.190028	26.346471
208.433280	9103.580758	26.351488
208.957428	9126.498924	26.356506
209.062623	9130.424447	26.361524
209.284044	9157.705754	26.366541
209.576296	9178.627889	26.371559
209.562376	9190.661472	26.376576
210.409144	9204.943096	26.381594
210.394316	9223.277179	26.386612
210.396955	9233.614636	26.391629
210.982947	9251.489395	26.396647
210.898943	9267.519738	26.401664
210.988657	9275.202718	26.406682
210.980100	9300.041254	26.411700
211.611933	9321.107371	26.416717
211.706552	9326.285498	26.421735
211.713322	9342.676828	26.426752
212.125404	9363.038690	26.431770
212.729735	9359.296054	26.436788
212.655411	9397.593975	26.441805
213.405432	9388.581832	26.446823
213.542323	9399.893899	26.451840
213.810530	9387.081607	26.456858
213.720886	9412.885873	26.461876
213.900475	9422.298901	26.466893
214.465398	9430.259546	26.471911
213.759138	9427.486827	26.476928
214.016295	9449.886950	26.481946
214.692076	9461.025011	26.486964
214.719895	9473.842671	26.491981
214.765741	9486.434364	26.496999
214.913508	9504.666140	26.502016
215.217488	9527.538176	26.507034
215.156112	9532.673172	26.512052
215.364735	9559.662923	26.517069
215.836677	9560.759172	26.522087
215.898924	9592.828598	26.527104
216.092723	9604.109711	26.532122
216.474960	9614.306642	26.537140
216.289902	9646.771714	26.542157
216.788066	9648.774318	26.547175
217.669180	9657.878518	26.552192
218.211424	9671.904974	26.557210
218.498175	9667.948864	26.562228
218.462307	9670.141669	26.567245
218.668264	9680.246341	26.572263
218.998456	9702.818957	26.577280
218.914294	9705.537691	26.582298
219.574275	9704.946207	26.587316
219.803364	9704.632359	26.592333
219.920428	9713.982349	26.597351
220.034887	9734.667607	26.602368
220.222517	9723.291521	26.607386
220.258510	9742.196563	26.612404
220.116882	9742.097636	26.617421
220.678613	9754.935088	26.622439
220.470906	9768.761287	26.627456
220.843376	9777.768793	26.632474
221.047227	9802.152868	26.637492
221.071416	9806.927651	26.642509
221.484628	9834.242570	26.647527
221.032415	9847.903992	26.652544
221.357248	9865.061681	26.657562
221.859772	9892.502945	26.662580
222.104642	9913.843680	26.667597
222.676351	9925.120271	26.672615
222.640347	9932.442334	26.677632
222.975385	9964.927879	26.682650
223.862372	9965.196580	26.687668
223.946376	9960.614006	26.692685
224.028850	9978.050493	26.697703
224.138318	9981.677288	26.702720
224.557574	9993.693217	26.707738
224.621832	9993.170331	26.712756
224.679682	10014.671271	26.717773
225.149105	10017.172742	26.722791
225.177263	10017.167156	26.727808
225.241257	10030.589837	26.732826
225.761614	10040.887025	26.737844
225.853614	10059.900406	26.742861
225.984258	10048.682688	26.747879
226.116954	10086.074613	26.752896
226.239795	10090.375333	26.757914
226.447907	10098.466018	26.762932
226.824202	10116.480701	26.767949
226.848182	10116.648921	26.772967
226.972402	10145.951216	26.777984
227.352689	10162.845024	26.783002
227.622536	10172.216589	26.788020
227.526218	10184.725284	26.793037
227.752092	10212.698391	26.798055
228.189359	10235.616760	26.803072
228.059863	10255.295695	26.808090
228.555704	10267.043858	26.813108
228.459605	10300.153303	26.818125
229.012257	10310.792600	26.823143
229.178836	10332.563918	26.828160
229.329939	10358.079579	26.833178
229.626525	10366.349122	26.838196
229.863203	10400.125852	26.843213
230.040314	10417.022428	26.848231
230.465766	10430.762658	26.853248
230.470034	10448.485644	26.858266
231.249138	10466.984296	26.863284
231.124141	10473.684505	26.868301
231.985604	10478.230402	26.873319
232.300565	10499.306194	26.878336
232.502965	10498.826198	26.883354
232.981660	10505.792998	26.888372
233.325857	10519.518915	26.893389
233.047251	10523.753111	26.898407
233.414446	10519.872890	26.903424
233.394417	10535.003081	26.908442
233.722758	10544.430483	26.913460
233.867282	10566.378407	26.918477
233.990055	10570.793393	26.923495
234.295527	10587.782243	26.928512
234.493197	10601.861750	26.933530
234.801930	10608.985552	26.938548
234.769862	10630.042475	26.943565
235.018117	10629.052257	26.948583
235.489883	10653.921521	26.953600
235.424201	10661.871993	26.958618
235.961874	10680.475114	26.963636
236.143043	10682.616545	26.968653
236.350842	10698.595594	26.973671
236.776273	10719.788273	26.978688
236.661343	10728.469124	26.983706
237.074404	10732.693069	26.988724
237.258802	10752.110506	26.993741
237.530861	10753.237141	26.998759
237.853072	10742.412975	27.003776
238.174146	10761.637458	27.008794
238.961306	10760.610511	27.013812
238.513393	10775.054389	27.018829
238.863497	10766.306675	27.023847
239.153460	10782.180631	27.028864
239.503183	10794.947312	27.033882
239.600152	10789.207449	27.038900
239.872728	10801.871921	27.043917
239.803860	10819.573553	27.048935
240.248570	10831.276792	27.053952
240.307172	10834.409774	27.058970
240.488001	10848.158886	27.063988
240.553286	10869.491040	27.069005
240.688824	10879.205569	27.074023
240.979209	10891.983366	27.079040
240.957583	10909.533544	27.084058
241.274395	10931.531664	27.089076
241.518442	10956.640000	27.094093
241.935061	10967.811455	27.099111
241.894463	10993.171826	27.104128
242.022952	11009.873368	27.109146
242.460811	11022.115793	27.114164
242.689224	11051.212772	27.119181
242.583878	11071.226167	27.124199
243.347838	11098.001859	27.129216
243.395826	11118.450904	27.134234
243.717277	11132.198715	27.139252
243.978029	11155.403596	27.144269
244.449457	11163.593368	27.149287
245.000425	11184.278323	27.154304
245.027805	11200.237080	27.159322
245.300092	11210.894558	27.164340
245.650384	11240.066131	27.169357
245.561499	11253.609504	27.174375
246.191492	11265.406721	27.179392
246.192457	11275.821008	27.184410
246.642343	11284.641960	27.189428
246.789817	11307.069809	27.194445
247.042069	11317.300232	27.199463
247.531034	11324.799603	27.204480
247.273857	11350.708852	27.209498
248.003146	11361.090918	27.214516
248.125250	11366.540446	27.219533
248.203671	11391.376036	27.224551
248.695070	11405.047026	27.229568
248.464586	11418.835071	27.234586
249.033574	11431.949461	27.239604
249.517557	11454.397279	27.244621
249.896794	11464.363568	27.249639
250.048147	11467.373084	27.254656
249.934518	11483.917765	27.259674
250.354194	11496.657362	27.264692
250.444611	11499.623667	27.269709
250.600584	11511.646185	27.274727
250.852833	11531.744856	27.279744
251.065635	11541.412077	27.284762
251.442550	11557.365076	27.289780
251.444306	11561.655610	27.294797
251.700212	11583.606146	27.299815
252.031856	11597.952114	27.304832
251.606902	11618.187580	27.309850
251.929232	11638.025521	27.314868
252.142010	11658.814821	27.319885
252.649173	11684.341289	27.324903
252.825389	11701.412210	27.329920
253.326219	11726.683958	27.334938
253.595706	11746.537746	27.339956
254.038415	11772.431383	27.344973
254.071392	11797.155835	27.349991
254.579519	11800.295675	27.355008
254.879193	11832.302884	27.360026
255.262470	11837.402018	27.365044
255.420319	11853.979780	27.370061
255.617570	11868.745696	27.375079
256.439412	11881.840439	27.380096
256.268688	11893.742375	27.385114
256.373761	11905.302442	27.390132
256.544625	11929.258179	27.395149
256.931154	11942.987894	27.400167
257.387180	11959.806513	27.405184
257.281614	11980.137159	27.410202
257.590830	11997.696464	27.415220
257.719429	12025.341716	27.420237
257.818677	12044.497328	27.425255
257.908484	12053.324183	27.430272
258.482989	12082.774905	27.435290
258.925761	12104.904399	27.440308
259.184199	12123.042789	27.445325
259.191610	12144.629965	27.450343
259.841467	12154.760187	27.455360
260.107901	12186.650852	27.460378
260.184807	12192.856421	27.465396
260.335359	12209.415270	27.470413
260.504580	12222.320948	27.475431
261.255062	12237.658435	27.480448
261.136363	12258.175532	27.485466
261.440357	12281.198934	27.490484
261.599590	12298.154970	27.495501
261.916864	12318.302763	27.500519
262.416209	12332.330677	27.505536
262.531768	12355.107558	27.510554
262.914343	12369.929429	27.515572
263.553850	12388.379895	27.520589
263.243012	12404.400717	27.525607
263.728081	12424.055930	27.530624
263.577286	12439.005197	27.535642
263.885315	12454.691484	27.540660
264.430148	12470.018500	27.545677
264.489123	12499.701960	27.550695
264.741986	12500.437838	27.555712
264.814533	12524.337180	27.560730
265.281501	12543.096932	27.565748
265.666179	12563.365362	27.570765
265.479587	12577.121678	27.575783
266.011265	12596.377303	27.580800
266.472428	12616.548406	27.585818
266.746061	12640.017195	27.590836
266.725271	12650.138751	27.595853
266.989985	12661.255586	27.600871
267.516801	12680.498515	27.605888
267.552592	12702.198453	27.610906
267.681658	12727.921747	27.615924
268.176501	12736.488046	27.620941
268.247398	12766.587503	27.625959
268.798128	12785.326134	27.630976
269.076615	12806.375929	27.635994
268.979640	12814.908699	27.641012
269.798552	12835.035661	27.646029
269.863216	12857.335741	27.651047
270.551909	12861.673785	27.656064
270.731022	12896.567058	27.661082
270.591761	12902.651520	27.666100
271.579695	12913.058966	27.671117
271.500424	12925.560804	27.676135
271.812481	12943.796219	27.681152
272.074270	12964.288841	27.686170
272.228806	12968.673885	27.691188
272.620349	12995.819393	27.696205
272.538767	13009.357161	27.701223
273.105063	13026.711968	27.706240
273.328119	13044.303634	27.711258
273.486927	13060.695415	27.716276
273.902805	13078.074650	27.721293
273.875180	13103.478094	27.726311
274.339400	13120.292860	27.731328
274.180221	13134.376601	27.736346
274.708514	13152.658778	27.741364
274.877681	13176.763752	27.746381
274.972634	13203.679631	27.751399
275.628440	13213.541593	27.756416
275.799019	13236.740023	27.761434
275.794960	13267.086989	27.766452
276.336600	13275.011487	27.771469
276.432396	13301.885685	27.776487
276.729719	13330.144925	27.781504
277.055207	13348.991985	27.786522
277.463691	13376.360896	27.791540
277.797359	13387.744356	27.796557
277.702669	13419.906226	27.801575
278.139260	13442.880339	27.806592
278.330913	13460.023785	27.811610
278.632349	13490.681155	27.816628
279.233380	13501.027489	27.821645
279.476340	13520.506930	27.826663
279.364476	13533.111381	27.831680
280.220627	13551.118811	27.836698
280.226628	13567.456677	27.841716
280.637288	13575.530225	27.846733
281.041522	13604.428726	27.851751
281.244541	13598.196824	27.856768
281.543598	13616.455880	27.861786
281.630368	13636.071062	27.866804
281.859765	13652.700485	27.871821
282.302076	13670.725610	27.876839
282.463886	13691.209562	27.881856
282.416437	13718.315239	27.886874
282.807249	13737.992196	27.891892
283.078857	13762.120733	27.896909
283.253843	13782.354153	27.901927
283.669357	13796.638749	27.906944
284.549550	13810.293044	27.911962
284.442103	13834.676451	27.916980
284.705710	13849.990258	27.921997
284.913342	13871.273036	27.927015
285.154205	13893.946930	27.932032
285.671228	13913.358884	27.937050
285.916051	13939.890651	27.942068
285.848895	13951.271215	27.947085
286.109548	13972.296731	27.952103
286.573843	14005.080194	27.957120
287.024668	14026.245409	27.962138
286.792444	14057.354436	27.967156
287.296383	14076.890208	27.972173
287.292130	14102.604891	27.977191
287.699937	14126.122578	27.982208
288.462195	14147.266635	27.987226
288.613689	14168.610237	27.992244
288.943339	14181.198081	27.997261
289.221053	14229.359587	28.002279
289.264309	14240.994454	28.007296
289.726111	14261.557405	28.012314
289.833912	14297.362272	28.017332
290.164919	14315.291558	28.022349
290.205931	14345.109781	28.027367
290.431998	14364.347478	28.032384
290.930137	14392.692175	28.037402
291.343783	14419.701685	28.042420
291.876586	14436.185395	28.047437
292.721308	14446.997455	28.052455
293.213040	14461.655380	28.057472
293.797859	14470.797757	28.062490
293.551777	14483.462561	28.067508
293.968282	14499.992331	28.072525
294.312585	14503.951204	28.077543
294.276634	14523.486909	28.082560
294.527371	14522.603809	28.087578
294.560037	14551.518651	28.092596
295.001048	14561.724227	28.097613
295.372719	14574.734540	28.102631
295.618645	14604.552489	28.107648
296.159041	14600.935711	28.112666
296.022978	14628.007525	28.117684
296.395417	14638.625275	28.122701
296.775205	14652.896000	28.127719
296.614527	14675.372905	28.132736
296.969793	14695.996819	28.137754
297.244723	14716.371515	28.142772
297.857945	14730.555903	28.147789
298.121569	14747.118869	28.152807
298.090134	14781.987811	28.157824
298.709907	14787.483826	28.162842
298.819069	14817.545202	28.167860
299.343125	14835.010066	28.172877
299.548830	14849.392366	28.177895
299.870690	14865.202233	28.182912
300.146379	14885.668550	28.187930
300.297171	14909.331241	28.192948
300.772461	14924.303293	28.197965
301.103153	14937.823695	28.202983
301.380747	14960.337341	28.208000
301.432630	14978.622070	28.213018
301.843959	15000.568108	28.218036
302.218132	15022.138676	28.223053
302.546654	15042.650118	28.228071
302.775550	15072.419535	28.233088
303.261445	15087.354335	28.238106
303.378357	15121.696559	28.243124
303.825956	15129.358430	28.248141
304.006661	15145.901192	28.253159
303.909703	15180.246046	28.258176
304.483681	15194.797490	28.263194
305.065023	15225.301340	28.268212
305.197724	15241.884331	28.273229
305.609167	15255.052734	28.278247
305.465115	15283.127684	28.283264
305.993994	15310.575242	28.288282
306.297042	15337.663439	28.293300
306.608821	15353.987634	28.298317
306.827775	15377.885219	28.303335
307.412133	15407.533090	28.308352
307.992856	15414.353254	28.313370
307.738466	15445.727140	28.318388
308.142740	15466.073458	28.323405
308.796124	15488.485470	28.328423
308.513867	15515.258574	28.333440
308.833754	15542.717715	28.338458
309.196463	15568.135750	28.343476
309.600288	15595.330858	28.348493
309.992916	15617.313038	28.353511
310.219871	15651.276950	28.358528
310.453131	15664.599087	28.363546
310.620449	15692.814398	28.368564
310.855571	15732.888695	28.373581
311.553145	15751.209007	28.378599
311.655017	15766.458594	28.383616
312.131715	15791.685233	28.388634
312.278489	15816.529321	28.393652
312.589876	15847.024782	28.398669
312.923086	15866.635028	28.403687
312.907730	15895.621850	28.408704
313.563687	15911.708736	28.413722
313.943611	15935.709664	28.418740
313.938596	15965.048072	28.423757
314.812093	15986.697871	28.428775
315.156154	16007.126541	28.433792
315.528372	16016.932592	28.438810
315.748032	16050.876110	28.443828
316.133290	16058.178647	28.448845
316.342629	16084.349842	28.453863
316.458032	16111.141098	28.458880
316.667879	16125.452681	28.463898
317.274853	16150.477473	28.468916
317.337159	16177.625102	28.473933
317.672082	16208.213972	28.478951
317.669390	16232.800892	28.483968
318.497936	16256.055697	28.488986
318.521218	16286.881576	28.494004
319.046190	16306.779305	28.499021
319.488899	16321.933390	28.504039
319.339106	16354.988135	28.509056
319.958447	16384.707702	28.514074
320.819528	16401.818996	28.519092
320.916566	16428.101576	28.524109
321.404269	16449.029540	28.529127
321.456752	16465.187207	28.534144
322.066854	16489.203094	28.539162
321.970877	16509.723230	28.544180
322.378649	16529.768655	28.549197
322.870975	16544.932964	28.554215
323.248831	16578.269608	28.559232
323.706251	16579.782670	28.564250
323.902471	16614.760009	28.569268
323.781646	16631.028141	28.574285
324.341958	16650.401435	28.579303
324.502769	16674.950401	28.584320
324.901148	16687.058229	28.589338
325.227741	16730.298819	28.594356
325.731368	16759.164785	28.599373
326.332715	16776.760970	28.604391
326.385847	16800.565741	28.609408
326.679253	16811.530445	28.614426
326.971543	16834.046260	28.619444
327.568588	16853.238771	28.624461
328.063822	16871.421818	28.629479
328.138683	16889.415996	28.634496
328.581308	16896.118493	28.639514
328.874386	16923.607790	28.644532
329.071909	16946.765800	28.649549
329.252120	16955.486591	28.654567
329.380689	16975.905419	28.659584
329.467529	16996.701177	28.664602
330.007373	17021.245989	28.669620
329.962123	17052.395123	28.674637
330.577676	17064.517649	28.679655
330.858224	17088.817690	28.684672
331.286931	17115.390094	28.689690
331.623070	17125.708089	28.694708
331.708287	17158.824725	28.699725
332.023658	17183.357541	28.704743
332.084906	17220.749175	28.709760
332.427832	17241.737311	28.714778
333.094286	17269.185038	28.719796
333.012218	17306.823725	28.724813
333.721497	17324.846230	28.729831
333.776945	17358.703834	28.734848
334.547644	17400.749971	28.739866
334.583296	17425.164763	28.744884
334.704630	17461.485233	28.749901
335.349259	17486.278642	28.754919
336.048890	17514.008909	28.759936
336.355706	17542.894320	28.764954
336.648090	17557.908426	28.769972
337.055170	17592.630554	28.774989
337.442387	17605.689482	28.780007
338.153164	17632.571355	28.785024
338.463276	17639.215968	28.790042
338.984636	17657.316842	28.795060
339.374077	17675.640726	28.800077
340.141466	17685.780920	28.805095
339.948133	17710.827527	28.810112
340.328054	17726.325476	28.815130
340.531627	17737.879950	28.820148
340.566199	17750.377495	28.825165
340.709795	17778.860230	28.830183
340.856629	17804.899613	28.835200
341.005488	17830.338722	28.840218
341.243391	17865.058894	28.845236
341.503312	17899.696501	28.850253
342.077141	17930.752276	28.855271
342.218182	17961.875511	28.860288
343.006079	18002.592589	28.865306
343.336792	18015.016379	28.870324
343.639079	18055.722012	28.875341
343.898520	18076.304503	28.880359
344.709929	18119.620128	28.885376
344.847136	18131.907527	28.890394
345.673646	18157.282482	28.895412
345.361105	18189.154057	28.900429
345.789894	18211.980638	28.905447
345.899893	18243.308599	28.910464
346.291473	18267.051443	28.915482
346.981210	18276.587462	28.920500
346.723980	18314.623044	28.925517
347.432646	18342.317134	28.930535
347.637851	18367.439079	28.935552
347.920066	18386.807691	28.940570
348.446839	18414.019860	28.945588
348.861243	18447.565926	28.950605
349.011448	18466.049347	28.955623
349.367971	18493.621869	28.960640
349.747820	18525.295988	28.965658
350.373933	18557.307317	28.970676
350.241763	18591.963280	28.975693
350.719711	18610.587168	28.980711
351.377176	18628.382043	28.985728
351.715481	18655.219534	28.990746
352.369313	18673.594987	28.995764
352.554716	18710.244396	29.000781
352.937452	18716.605052	29.005799
353.601705	18732.759122	29.010816
353.858747	18765.636430	29.015834
354.434675	18788.667587	29.020852
355.782805	18764.595286	29.025869
356.188140	18786.032677	29.030887
356.604843	18792.714741	29.035904
356.616392	18805.590837	29.040922
357.066653	18798.406973	29.045940
357.155524	18814.924493	29.050957
357.262577	18812.521953	29.055975
357.223783	18825.253718	29.060992
357.439983	18844.835795	29.066010
357.537070	18859.998828	29.071028
357.846966	18879.367973	29.076045
358.087603	18909.997282	29.081063
358.304931	18931.569566	29.086080
358.259033	18968.624182	29.091098
358.885879	19000.820179	29.096116
359.193300	19038.737221	29.101133
359.668064	19070.864285	29.106151
360.284199	19106.973116	29.111168
360.094941	19137.515069	29.116186
360.714226	19168.853499	29.121204
360.656444	19199.261225	29.126221
360.957139	19244.293000	29.131239
361.354922	19275.351168	29.136256
361.831211	19311.959571	29.141274
362.151992	19356.763251	29.146292
362.327214	19399.001437	29.151309
362.758018	19431.804814	29.156327
363.209540	19470.201560	29.161344
363.555043	19497.891800	29.166362
364.358707	19540.192831	29.171380
364.660996	19574.812446	29.176397
365.027472	19604.632036	29.181415
365.483697	19642.694563	29.186432
365.709951	19670.485222	29.191450
366.258629	19702.835692	29.196468
366.333628	19723.124517	29.201485
366.361609	19760.414930	29.206503
367.371843	19788.689596	29.211520
367.323286	19819.908962	29.216538
367.900124	19850.899183	29.221556
368.359471	19865.757400	29.226573
368.479895	19905.978667	29.231591
369.162158	19923.937239	29.236608
369.220546	19974.944331	29.241626
369.620724	19986.388424	29.246644
369.686911	20027.429380	29.251661
369.969598	20069.579009	29.256679
370.765542	20100.217443	29.261696
370.909429	20145.573688	29.266714
371.505942	20174.517036	29.271732
371.860469	20202.131483	29.276749
372.070105	20232.929367	29.281767
372.756296	20267.771660	29.286784
373.027740	20301.080672	29.291802
373.281250	20331.360264	29.296820
373.722764	20364.638371	29.301837
374.085694	20401.720213	29.306855
374.740044	20432.429508	29.311872
375.077637	20469.073744	29.316890
375.603387	20496.160555	29.321908
375.924652	20521.179657	29.326925
376.463467	20556.214608	29.331943
376.635479	20576.844254	29.336960
376.702536	20614.108415	29.341978
377.120539	20636.180292	29.346996
377.680003	20673.222793	29.352013
377.880047	20716.104774	29.357031
378.596935	20739.004911	29.362048
378.786189	20779.745098	29.367066
379.417482	20807.826835	29.372084
379.735618	20830.204716	29.377101
379.802327	20867.999551	29.382119
380.147666	20893.543853	29.387136
380.457586	20930.840154	29.392154
381.061077	20954.209155	29.397172
381.566957	20999.727937	29.402189
382.068839	21031.583391	29.407207
382.701083	21046.535282	29.412224
383.004544	21074.516951	29.417242
383.735283	21099.898580	29.422260
383.993024	21133.663599	29.427277
384.166122	21157.596077	29.432295
384.644696	21175.466869	29.437312
384.861035	21214.636615	29.442330
385.352742	21221.858284	29.447348
385.870376	21248.978404	29.452365
386.048032	21290.667628	29.457383
386.375106	21303.226932	29.462400
386.454528	21326.698114	29.467418
386.700881	21363.549567	29.472436
387.444277	21380.265553	29.477453
388.298677	21387.845342	29.482471
388.931811	21403.960680	29.487488
388.887267	21433.406625	29.492506
389.348835	21445.014484	29.497524
389.733765	21463.629036	29.502541
389.611791	21494.499559	29.507559
390.376043	21519.710349	29.512576
390.397222	21537.729260	29.517594
390.741179	21574.043486	29.522612
390.877205	21608.542468	29.527629
391.288307	21634.976917	29.532647
391.777413	21662.206257	29.537664
391.783897	21712.354206	29.542682
392.177894	21740.052488	29.547700
392.811653	21774.978153	29.552717
392.649993	21820.971123	29.557735
393.351659	21856.580020	29.562752
393.512937	21902.141357	29.567770
393.446316	21936.678859	29.572788
394.560234	21986.347195	29.577805
394.917563	22021.530108	29.582823
395.733016	22051.822308	29.587840
396.032998	22091.289643	29.592858
396.441952	22119.773029	29.597876
397.045970	22149.241402	29.602893
397.278695	22197.526791	29.607911
398.371402	22220.200658	29.612928
398.980525	22247.495372	29.617946
398.825396	22270.637515	29.622964
399.300639	22301.036389	29.627981
399.271635	22330.362596	29.632999
399.575567	22348.444491	29.638016
400.167786	22399.511800	29.643034
400.920979	22416.915716	29.648052
401.457171	22443.758480	29.653069
401.568574	22481.059360	29.658087
402.090599	22508.409361	29.663104
402.263842	22550.040387	29.668122
402.346207	22583.250453	29.673140
402.803091	22614.976080	29.678157
402.798044	22653.625449	29.683175
403.353038	22688.983923	29.688192
403.879825	22741.189870	29.693210
404.069103	22782.574782	29.698228
404.640566	22818.268032	29.703245
404.720766	22869.558644	29.708263
405.523936	22895.129329	29.713280
406.001296	22932.840821	29.718298
406.280058	22968.122636	29.723316
407.198360	23006.079890	29.728333
407.761671	23032.565676	29.733351
408.186627	23065.223575	29.738368
408.469111	23092.407964	29.743386
408.338069	23121.580969	29.748404
408.985499	23141.465550	29.753421
409.411057	23186.165361	29.758439
409.640499	23209.869058	29.763456
410.327927	23248.081076	29.768474
410.348785	23274.611168	29.773492
410.903236	23307.144959	29.778509
411.197106	23342.982869	29.783527
411.304968	23379.497965	29.788544
411.756432	23421.951809	29.793562
412.186932	23458.562184	29.798580
412.418303	23502.781050	29.803597
412.792261	23549.225360	29.808615
413.440966	23580.778209	29.813632
413.804471	23619.019891	29.818650
414.112690	23665.805843	29.823668
414.639867	23708.243661	29.828685
414.977256	23741.666783	29.833703
415.741245	23782.923340	29.838720
415.832555	23838.975331	29.843738
416.510764	23875.176979	29.848756
417.367505	23897.384374	29.853773
417.511402	23945.285928	29.858791
417.690011	23978.207875	29.863808
418.518389	24008.255217	29.868826
418.590532	24047.106773	29.873844
419.567805	24081.557433	29.878861
419.676298	24118.363210	29.883879
420.119486	24164.772289	29.888896
420.232873	24190.463640	29.893914
420.457077	24230.766799	29.898932
421.319727	24261.327475	29.903949
421.462803	24307.398808	29.908967
421.843250	24347.753776	29.913984
422.434084	24391.217547	29.919002
422.635055	24429.732842	29.924020
423.268876	24469.731870	29.929037
423.818095	24507.197753	29.934055
424.591379	24543.703229	29.939072
424.742844	24578.303877	29.944090
425.417838	24619.449171	29.949108
426.027963	24634.943656	29.954125
426.585734	24685.369193	29.959143
426.442317	24706.752410	29.964160
427.321263	24747.830879	29.969178
427.689167	24772.070983	29.974196
427.973672	24790.095735	29.979213
428.470566	24829.174555	29.984231
428.923922	24863.308639	29.989248
429.079652	24893.306493	29.994266
429.283170	24937.844933	29.999284
430.049774	24966.639592	30.004301
430.329678	25012.610016	30.009319
430.755853	25050.938889	30.014336
431.383388	25082.642249	30.019354
431.694094	25109.697967	30.024372
431.905477	25153.427514	30.029389
432.048889	25189.760687	30.034407
433.132014	25198.421367	30.039424
434.276157	25218.861985	30.044442
435.154986	25242.934744	30.049460
435.678570	25232.367055	30.054477
435.623687	25263.898275	30.059495
435.628491	25280.845581	30.064512
436.413601	25310.025495	30.069530
436.405821	25330.623010	30.074548
437.044929	25356.549942	30.079565
437.461586	25390.834375	30.084583
437.916418	25404.898554	30.089600
438.161661	25425.709540	30.094618
438.066134	25463.318996	30.099636
438.560019	25490.368230	30.104653
438.911146	25519.724810	30.109671
438.933031	25571.229547	30.114688
439.410315	25608.019379	30.119706
439.730323	25646.295693	30.124724
440.140154	25689.085981	30.129741
440.702904	25743.780710	30.134759
440.782230	25786.576648	30.139776
441.540177	25832.909695	30.144794
441.393244	25892.899320	30.149812
442.061973	25924.557609	30.154829
442.667099	25990.300017	30.159847
442.988506	26040.654038	30.164864
443.511950	26077.217794	30.169882
443.864027	26135.377525	30.174900
444.436966	26183.296193	30.179917
444.785480	26240.074263	30.184935
445.014767	26286.934026	30.189952
445.735306	26326.462220	30.194970
446.201174	26388.607636	30.199988
446.715031	26438.484757	30.205005
447.273975	26484.191982	30.210023
447.229395	26539.577837	30.215040
448.168877	26581.051586	30.220058
448.660170	26629.974894	30.225076
449.532095	26661.576265	30.230093
449.997108	26712.702856	30.235111
450.360612	26756.663847	30.240128
450.698226	26794.829003	30.245146
450.933388	26843.906431	30.250164
451.470096	26893.729323	30.255181
452.111149	26932.246685	30.260199
451.945027	26984.909362	30.265216
452.710046	27027.416566	30.270234
452.822984	27078.508231	30.275252
453.598576	27135.225349	30.280269
453.970479	27188.680641	30.285287
454.678863	27225.118269	30.290304
455.954618	27245.043382	30.295322
456.109367	27287.684744	30.300340
456.709345	27315.076263	30.305357
457.538694	27342.190197	30.310375
457.346024	27374.622815	30.315392
458.043608	27398.462972	30.320410
458.262983	27435.708554	30.325428
458.841950	27461.026840	30.330445
459.127341	27502.489782	30.335463
459.367391	27539.869400	30.340480
459.797043	27576.167867	30.345498
460.028134	27622.805098	30.350516
460.306781	27662.154853	30.355533
461.047025	27703.418206	30.360551
460.995627	27757.413973	30.365568
461.579296	27800.916483	30.370586
462.018664	27857.046786	30.375604
462.575742	27896.434691	30.380621
462.793253	27950.088858	30.385639
463.056101	28005.983067	30.390656
464.061808	28049.688468	30.395674
464.514561	28108.373461	30.400692
464.442699	28165.002292	30.405709
465.142718	28204.951225	30.410727
465.704622	28261.105952	30.415744
466.184511	28308.911022	30.420762
466.648331	28371.197543	30.425780
467.156298	28407.925055	30.430797
467.900979	28476.454824	30.435815
468.392752	28514.286672	30.440832
469.285686	28553.123122	30.445850
469.437919	28603.307217	30.450868
470.303801	28639.964050	30.455885
470.729405	28682.454041	30.460903
471.006501	28735.294467	30.465920
471.709927	28770.138438	30.470938
471.941967	28825.246134	30.475956
472.375678	28862.246524	30.480973
473.014739	28907.030672	30.485991
473.483828	28955.204971	30.491008
473.777151	28981.619111	30.496026
474.032336	29041.144230	30.501044
474.544448	29098.162344	30.506061
475.111545	29134.793829	30.511079
475.157770	29177.202145	30.516096
475.663391	29229.257632	30.521114
476.254258	29284.784067	30.526132
476.611362	29331.160281	30.531149
477.585439	29382.857962	30.536167
477.966267	29435.241295	30.541184
478.640764	29475.730089	30.546202
479.138665	29527.784608	30.551220
479.556742	29561.985474	30.556237
480.107758	29605.127672	30.561255
480.863083	29652.098530	30.566272
481.229462	29681.974002	30.571290
481.650837	29724.144313	30.576308
482.010962	29757.948224	30.581325
482.609910	29787.088684	30.586343
482.704302	29823.765507	30.591360
482.966666	29873.061298	30.596378
483.445324	29909.264189	30.601396
483.709194	29966.149952	30.606413
484.539080	30008.144022	30.611431
484.895777	30071.829952	30.616448
485.232710	30105.006300	30.621466
485.696334	30169.553409	30.626484
486.344830	30212.486258	30.631501
486.892091	30252.109957	30.636519
486.813840	30315.940200	30.641536
487.845771	30364.003777	30.646554
488.404192	30410.172892	30.651572
489.038193	30452.878582	30.656589
489.950130	30481.655215	30.661607
490.797922	30529.278956	30.666624
491.015321	30550.486307	30.671642
491.315850	30596.894039	30.676660
491.867455	30632.436004	30.681677
492.246666	30677.469721	30.686695
492.348555	30729.329529	30.691712
493.157721	30774.424256	30.696730
493.612611	30816.467536	30.701748
493.869579	30859.169732	30.706765
494.532171	30903.635670	30.711783
495.314288	30959.502979	30.716800
495.841346	30995.246653	30.721818
496.680687	31035.993600	30.726836
496.842052	31069.314926	30.731853
497.437523	31113.702290	30.736871
497.741149	31160.377483	30.741888
498.238991	31197.215337	30.746906
498.804124	31235.136375	30.751924
498.901352	31294.069135	30.756941
499.524014	31342.930530	30.761959
499.885742	31383.023106	30.766976
500.165311	31437.159559	30.771994
500.743892	31488.036395	30.777012
500.792926	31552.123832	30.782029
501.556462	31596.717421	30.787047
501.617532	31669.718069	30.792064
502.669818	31699.464313	30.797082
503.880516	31743.413347	30.802100
504.878573	31776.993707	30.807117
505.694675	31814.169982	30.812135
505.817933	31858.354025	30.817152
506.353579	31888.558043	30.822170
506.934625	31919.084306	30.827188
507.007624	31962.294677	30.832205
507.849529	31986.927159	30.837223
507.938859	32039.330574	30.842240
508.584261	32080.339558	30.847258
508.881888	32107.145800	30.852276
509.235905	32160.199382	30.857293
509.548279	32184.410556	30.862311
509.891752	32226.908648	30.867328
510.336340	32275.400825	30.872346
510.478205	32322.253243	30.877364
511.020327	32372.293770	30.882381
511.611038	32427.082174	30.887399
511.805698	32487.737523	30.892416
512.046251	32541.795547	30.897434
512.925036	32595.755233	30.902452
513.229045	32661.656863	30.907469
513.791354	32713.216284	30.912487
514.227863	32783.843385	30.917504
514.729603	32837.707873	30.922522
515.074153	32894.025028	30.927540
515.784883	32959.521005	30.932557
516.098555	33022.519036	30.937575
516.746690	33089.070570	30.942592
516.937303	33150.316944	30.947610
517.808082	33207.821831	30.952628
518.498762	33272.868268	30.957645
518.989179	33324.786257	30.962663
519.906627	33396.759613	30.967680
520.202821	33448.612773	30.972698
520.566417	33513.121135	30.977716
521.170108	33572.999646	30.982733
522.081104	33632.556715	30.987751
522.774371	33678.294207	30.992768
523.272381	33728.607535	30.997786
524.209364	33769.178600	31.002804
524.142998	33833.499751	31.007821
524.754716	33890.498126	31.012839
525.587946	33937.713158	31.017856
525.871066	34000.757601	31.022874
526.326687	34058.542806	31.027892
526.835275	34119.387416	31.032909
527.595884	34168.041298	31.037927
528.227831	34225.890428	31.042944
528.306620	34272.077395	31.047962
529.033784	34322.050196	31.052980
528.975653	34386.851397	31.057997
529.701379	34447.030476	31.063015
530.093017	34504.892055	31.068032
530.699767	34570.697860	31.073050
531.198298	34636.317803	31.078068
531.693593	34701.906992	31.083085
532.323991	34764.604211	31.088103
532.965262	34819.472860	31.093120
533.447023	34888.916206	31.098138
534.264980	34945.166477	31.103156
534.409708	35005.009743	31.108173
535.040822	35064.793089	31.113191
535.766553	35121.935165	31.118208
535.961352	35179.359067	31.123226
536.510726	35219.204021	31.128244
537.058337	35301.220542	31.133261
537.751280	35350.662717	31.138279
538.184857	35409.822938	31.143296
538.711951	35470.478771	31.148314
539.871278	35513.175345	31.153332
540.194379	35571.861864	31.158349
540.722330	35618.887506	31.163367
541.171352	35664.538508	31.168384
541.556369	35716.442903	31.173402
542.123233	35769.942328	31.178420
542.541344	35834.044234	31.183437
543.181595	35883.750202	31.188455
543.948595	35937.688096	31.193472
544.126031	36002.309830	31.198490
544.867436	36053.065944	31.203508
545.343599	36108.844847	31.208525
545.746416	36172.684042	31.213543
546.187741	36234.962835	31.218560
546.544560	36296.287294	31.223578
547.451371	36350.126994	31.228596
547.975123	36418.994539	31.233613
548.714320	36480.537822	31.238631
549.428703	36544.503807	31.243648
549.189533	36602.764784	31.248666
550.287462	36671.357442	31.253684
550.745824	36726.365532	31.258701
551.135991	36796.438372	31.263719
551.763817	36863.186350	31.268736
551.967982	36931.154604	31.273754
552.725546	36991.448127	31.278772
553.157293	37061.490220	31.283789
553.661188	37126.534115	31.288807
554.547768	37198.145639	31.293824
554.697221	37271.861493	31.298842
555.717420	37317.566333	31.303860
556.464479	37385.170871	31.308877
557.141378	37448.594420	31.313895
557.634328	37511.729011	31.318912
558.199368	37563.787024	31.323930
559.035004	37631.154547	31.328948
559.746365	37691.150474	31.333965
559.813555	37751.249216	31.338983
560.473517	37802.709458	31.344000
560.824538	37875.353620	31.349018
561.517683	37931.482415	31.354036
562.386703	37993.366891	31.359053
562.808540	38061.193071	31.364071
563.324007	38115.556432	31.369088
563.894695	38175.762542	31.374106
564.516677	38228.627143	31.379124
564.684169	38292.319476	31.384141
565.276602	38349.837495	31.389159
566.200559	38413.710962	31.394176
566.300363	38485.517907	31.399194
567.018293	38535.006460	31.404212
567.695059	38601.808702	31.409229
568.057596	38650.248857	31.414247
569.150375	38704.058575	31.419264
570.612476	38727.971540	31.424282
571.345466	38763.322220	31.429300
571.803441	38814.101835	31.434317
572.587803	38844.472780	31.439335
573.182320	38874.814097	31.444352
573.344335	38924.600473	31.449370
573.495052	38966.195546	31.454388
574.021004	39010.914598	31.459405
574.507522	39056.737534	31.464423
575.032734	39106.288412	31.469440
575.008773	39166.226920	31.474458
575.760325	39216.090554	31.479476
575.976012	39284.574163	31.484493
576.443601	39360.323583	31.489511
577.273445	39404.553745	31.494528
577.190764	39481.231819	31.499546
578.073643	39546.361835	31.504564
578.839124	39615.278005	31.509581
579.059148	39679.670463	31.514599
579.621391	39742.906398	31.519616
580.219401	39826.657280	31.524634
580.992558	39899.398977	31.529652
581.339254	39955.849839	31.534669
582.008315	40033.213319	31.539687
583.594608	40078.475920	31.544704
584.755626	40134.056515	31.549722
586.016406	40166.918065	31.554740
587.215279	40210.862894	31.559757
587.485460	40240.034592	31.564775
588.104230	40275.102260	31.569792
588.516394	40310.183982	31.574810
589.037557	40350.524941	31.579828
589.303524	40393.496023	31.584845
589.437111	40440.086949	31.589863
590.369010	40477.382313	31.594880
590.410152	40536.235031	31.599898
591.278630	40581.958658	31.604916
591.591093	40630.432922	31.609933
591.780711	40690.921519	31.614951
592.250564	40749.135817	31.619968
592.531256	40813.644313	31.624986
593.294571	40875.483577	31.630004
593.455578	40942.279364	31.635021
593.453147	41016.526080	31.640039
594.746205	41085.819923	31.645056
594.721028	41164.893469	31.650074
595.332628	41242.370922	31.655092
596.123606	41313.571870	31.660109
596.584540	41405.084604	31.665127
597.230516	41475.564943	31.670144
597.700857	41555.302589	31.675162
598.193776	41621.827365	31.680180
598.939183	41694.182109	31.685197
599.698096	41781.277699	31.690215
600.264437	41837.833833	31.695232
600.572504	41915.851564	31.700250
601.249441	41991.940443	31.705268
602.216961	42048.881280	31.710285
602.401293	42128.522034	31.715303
603.033442	42203.328889	31.720320
603.418437	42276.566745	31.725338
604.017434	42350.978925	31.730356
604.735406	42419.880825	31.735373
605.179355	42513.099168	31.740391
606.258000	42586.347733	31.745408
607.080620	42654.177199	31.750426
607.601084	42730.896739	31.755444
608.486217	42805.911957	31.760461
608.995083	42879.836071	31.765479
609.669702	42940.983994	31.770496
610.203786	43009.434908	31.775514
610.843970	43079.541044	31.780532
611.984563	43141.754219	31.785549
612.313017	43219.191017	31.790567
613.175656	43288.199520	31.795584
613.758885	43350.142598	31.800602
614.239362	43414.622700	31.805620
615.359081	43478.250468	31.810637
615.468894	43537.446330	31.815655
616.477787	43597.328852	31.820672
616.797005	43666.548431	31.825690
617.418094	43726.732904	31.830708
618.500088	43790.746374	31.835725
618.915805	43847.774714	31.840743
619.613477	43914.218927	31.845760
620.124221	43982.901379	31.850778
620.750062	44053.821317	31.855796
621.347970	44117.663872	31.860813
621.672907	44181.944462	31.865831
622.573327	44253.714248	31.870848
623.102592	44314.732435	31.875866
623.644406	44383.916267	31.880884
624.506222	44438.853364	31.885901
624.905304	44510.618873	31.890919
625.523744	44585.996581	31.895936
625.966318	44660.424660	31.900954
626.362934	44718.641915	31.905972
627.429677	44799.706534	31.910989
627.657225	44873.229650	31.916007
628.632188	44940.204634	31.921024
628.673469	45021.118109	31.926042
629.462665	45086.085247	31.931060
630.266075	45157.934151	31.936077
630.697845	45246.906959	31.941095
630.970655	45319.800091	31.946112
631.855763	45395.728785	31.951130
632.670139	45460.869980	31.956148
633.587102	45535.491251	31.961165
634.273110	45590.090854	31.966183
634.878811	45649.022466	31.971200
635.713119	45715.492803	31.976218
636.264624	45781.197613	31.981236
636.732188	45843.764261	31.986253
637.024500	45916.161446	31.991271
637.702289	45984.478130	31.996288
638.824361	46039.921479	32.001306
639.052219	46118.570285	32.006324
639.873522	46188.111126	32.011341
640.292037	46253.368790	32.016359
640.677615	46330.854474	32.021376
641.183896	46402.730564	32.026394
641.501741	46480.931268	32.031412
642.258546	46562.365764	32.036429
642.876395	46652.366706	32.041447
643.161284	46736.035226	32.046464
644.361371	46818.504601	32.051482
645.077123	46901.635187	32.056500
646.006431	46973.137043	32.061517
646.638895	47065.112881	32.066535
647.321146	47136.017400	32.071552
647.945577	47209.909897	32.076570
648.548807	47289.983939	32.081588
649.306376	47358.593003	32.086605
649.958136	47446.686862	32.091623
650.655881	47513.293027	32.096640
651.556543	47595.523443	32.101658
652.218667	47670.402613	32.106676
652.842795	47733.055172	32.111693
653.769941	47809.157992	32.116711
654.394502	47870.548857	32.121728
655.015469	47948.509015	32.126746
655.274468	48028.212096	32.131764
656.224204	48092.353877	32.136781
657.082493	48176.455391	32.141799
657.480950	48251.811291	32.146816
658.541299	48318.883388	32.151834
658.933301	48383.023528	32.156852
659.715015	48462.096290	32.161869
660.197435	48525.152867	32.166887
661.213545	48591.952212	32.171904
662.042177	48659.264443	32.176922
662.374496	48742.190222	32.181940
663.460645	48797.417634	32.186957
663.897977	48864.562604	32.191975
664.001721	48944.777311	32.196992
665.358120	48998.293065	32.202010
666.176958	49058.865086	32.207028
666.797320	49127.332460	32.212045
667.401810	49190.816893	32.217063
668.323454	49239.590426	32.222080
669.479352	49297.948050	32.227098
669.682032	49355.536226	32.232116
670.642816	49391.984659	32.237133
671.202672	49461.343357	32.242151
671.264723	49518.247602	32.247168
671.820753	49563.135760	32.252186
672.188448	49632.046070	32.257204
673.133719	49690.791951	32.262221
673.752426	49753.171661	32.267239
674.124501	49829.046504	32.272256
674.887409	49883.009707	32.277274
675.122545	49963.107094	32.282292
676.007606	50034.031938	32.287309
676.158291	50104.928835	32.292327
676.512247	50196.529771	32.297344
677.285869	50273.207226	32.302362
678.083783	50362.513540	32.307380
678.744651	50438.900397	32.312397
679.341348	50527.876666	32.317415
680.146219	50609.751286	32.322432
680.700012	50691.454822	32.327450
681.104432	50788.175756	32.332468
682.079280	50877.592167	32.337485
682.595491	50966.823273	32.342503
683.095538	51066.954571	32.347520
683.867254	51154.615336	32.352538
684.531706	51240.450570	32.357556
685.071932	51329.149463	32.362573
686.151991	51425.415946	32.367591
686.620408	51519.738441	32.372608
687.850040	51604.428185	32.377626
688.571437	51688.669049	32.382644
689.725467	51765.592134	32.387661
690.542606	51848.139520	32.392679
691.162166	51927.281849	32.397696
691.711145	52011.415968	32.402714
692.380985	52086.681707	32.407732
693.296482	52167.296025	32.412749
694.085599	52246.611591	32.417767
694.278775	52326.085513	32.422784
694.898414	52407.609620	32.427802
695.706606	52498.206289	32.432820
696.590019	52581.743812	32.437837
697.206720	52661.558916	32.442855
697.829009	52755.775004	32.447872
698.725982	52821.880052	32.452890
699.690627	52905.961625	32.457908
700.438695	52988.212763	32.462925
700.867972	53068.390903	32.467943
701.792056	53158.956650	32.472960
702.461599	53214.983653	32.477978
703.077234	53300.785965	32.482996
703.887275	53371.978957	32.488013
704.731378	53450.896519	32.493031
704.938246	53539.937100	32.498048
705.600453	53616.375093	32.503066
706.163125	53684.190419	32.508084
707.251687	53753.645624	32.513101
707.985866	53829.201908	32.518119
708.867808	53900.271898	32.523136
709.663207	53964.661297	32.528154
709.921739	54039.710259	32.533172
710.673038	54109.747638	32.538189
711.391979	54176.905490	32.543207
712.198861	54259.149868	32.548224
712.731527	54332.303575	32.553242
713.627311	54412.735330	32.558260
714.190248	54484.530715	32.563277
714.752852	54561.780810	32.568295
715.472631	54633.267728	32.573312
716.129878	54712.365715	32.578330
716.989313	54811.444116	32.583348
717.244942	54881.648605	32.588365
718.062655	54977.824238	32.593383
718.871785	55051.167239	32.598400
720.068986	55141.601525	32.603418
721.131572	55212.278558	32.608436
721.803985	55275.243300	32.613453
722.613033	55356.782050	32.618471
723.151026	55439.860555	32.623488
723.928172	55505.470445	32.628506
724.361602	55593.086586	32.633524
724.860974	55694.518821	32.638541
725.889141	55763.019052	32.643559
726.269356	55860.197038	32.648576
726.869429	55951.222837	32.653594
727.714100	56028.904569	32.658612
728.203450	56119.585808	32.663629
728.953273	56207.482809	32.668647
729.495790	56304.766733	32.673664
730.147119	56392.329897	32.678682
730.460567	56493.032198	32.683700
731.246461	56602.325295	32.688717
732.360204	56690.829600	32.693735
732.674053	56790.933666	32.698752
733.786241	56879.341263	32.703770
734.594773	56972.911773	32.708788
735.047340	57077.954773	32.713805
736.084654	57184.029138	32.718823
736.545519	57291.345010	32.723840
737.293645	57388.693469	32.728858
737.805638	57489.016015	32.733876
738.546702	57598.931446	32.738893
739.630446	57691.574670	32.743911
740.077216	57806.668318	32.748928
740.939695	57912.525292	32.753946
742.013843	58012.322349	32.758964
742.590720	58112.656885	32.763981
743.640215	58220.774727	32.768999
743.765373	58311.344749	32.774016
744.985162	58412.434131	32.779034
745.768868	58504.791374	32.784052
746.286228	58601.368398	32.789069
747.050039	58694.828445	32.794087
747.509067	58793.250069	32.799104
748.274044	58891.137298	32.804122
748.809919	58983.170135	32.809140
749.246508	59085.928587	32.814157
750.338528	59175.452235	32.819175
751.347079	59281.416886	32.824192
753.093475	59360.585588	32.829210
754.069906	59445.393006	32.834228
754.566396	59535.319447	32.839245
755.801718	59599.437516	32.844263
756.354287	59691.575384	32.849280
757.139795	59772.041762	32.854298
757.808865	59853.976256	32.859316
758.412097	59934.282907	32.864333
759.169230	60019.430953	32.869351
759.681054	60113.358157	32.874368
760.580805	60196.343578	32.879386
760.870073	60288.687329	32.884404
761.589124	60382.718664	32.889421
762.607933	60467.719738	32.894439
763.065592	60563.984880	32.899456
763.773953	60669.904150	32.904474
764.516142	60776.510131	32.909492
765.225315	60873.175715	32.914509
766.132931	60977.075746	32.919527
766.351184	61087.391772	32.924544
767.207715	61196.987949	32.929562
768.083676	61298.791838	32.934580
768.407820	61423.030679	32.939597
769.526476	61536.758339	32.944615
770.358684	61644.908473	32.949632
771.287948	61749.456643	32.954650
772.126069	61853.612557	32.959668
772.750601	61956.786260	32.964685
773.835737	62058.295703	32.969703
775.243697	62154.834519	32.974720
775.937433	62252.109605	32.979738
776.618078	62351.294579	32.984756
777.405561	62447.519991	32.989773
778.384560	62548.521610	32.994791
779.343522	62635.992468	32.999808
780.114988	62716.322100	33.004826
780.923902	62808.554415	33.009844
781.732600	62892.466201	33.014861
782.804868	62988.860609	33.019879
783.852453	63074.434122	33.024896
784.344938	63162.584826	33.029914
785.451694	63240.769605	33.034932
785.900827	63329.685889	33.039949
786.801167	63411.456924	33.044967
787.534853	63502.103495	33.049984
787.765437	63583.915566	33.055002
788.410687	63675.612862	33.060020
789.071866	63760.496208	33.065037
790.032650	63851.518837	33.070055
790.189367	63935.804286	33.075072
790.919583	64042.872698	33.080090
791.950914	64124.733319	33.085108
792.489510	64239.542217	33.090125
793.278784	64327.647910	33.095143
793.709646	64439.967617	33.100160
793.995287	64550.930985	33.105178
794.960454	64652.069140	33.110196
795.870186	64764.238728	33.115213
797.089834	64863.862623	33.120231
797.886052	64964.375573	33.125248
798.488718	65078.626616	33.130266
799.595927	65186.004615	33.135284
800.066681	65291.722205	33.140301
800.906911	65409.689434	33.145319
801.848953	65511.934895	33.150336
802.672507	65620.554317	33.155354
803.586337	65724.131895	33.160372
804.421530	65828.739542	33.165389
805.561652	65933.953005	33.170407
806.281105	66037.683230	33.175424
807.126878	66150.411180	33.180442
808.193519	66238.355161	33.185460
808.777402	66358.264065	33.190477
809.777521	66444.352931	33.195495
810.704359	66551.186104	33.200512
811.125194	66662.721292	33.205530
812.403519	66755.314834	33.210548
813.049104	66857.226123	33.215565
813.887938	66966.314997	33.220583
814.643143	67061.722257	33.225600
815.683849	67166.794021	33.230618
816.899583	67261.516200	33.235636
817.278766	67373.106329	33.240653
818.025938	67470.203580	33.245671
818.878402	67573.538678	33.250688
819.370128	67672.345364	33.255706
820.602876	67762.992610	33.260724
821.445122	67879.363673	33.265741
822.201839	67988.635619	33.270759
823.181175	68077.928518	33.275776
823.780271	68192.223804	33.280794
825.002712	68276.905057	33.285812
825.704274	68383.799975	33.290829
826.872429	68485.194405	33.295847
827.751248	68564.157323	33.300864
828.268008	68661.587803	33.305882
829.429580	68760.002781	33.310900
830.091852	68860.898455	33.315917
830.671440	68955.938627	33.320935
831.104712	69061.117305	33.325952
832.198328	69148.716392	33.330970
833.033927	69242.497873	33.335988
833.620920	69352.322530	33.341005
834.186891	69440.802956	33.346023
835.211394	69540.987422	33.351040
835.824044	69648.453067	33.356058
836.602487	69738.556327	33.361076
837.378832	69841.125800	33.366093
838.522374	69934.204503	33.371111
839.388353	70042.030020	33.376128
839.939866	70151.220349	33.381146
840.749599	70252.725210	33.386164
841.208469	70358.153172	33.391181
842.298358	70457.106177	33.396199
843.290296	70578.896826	33.401216
843.579306	70685.585635	33.406234
844.740145	70802.037093	33.411252
845.503594	70910.616610	33.416269
846.059017	71028.776946	33.421287
847.296040	71135.626907	33.426304
847.910085	71265.203071	33.431322
848.764638	71376.835116	33.436340
849.814940	71485.757569	33.441357
850.806161	71603.782476	33.446375
851.650264	71718.286749	33.451392
852.484791	71843.598127	33.456410
853.439705	71950.465794	33.461428
854.569397	72075.276713	33.466445
855.374030	72187.136104	33.471463
856.246725	72288.685631	33.476480
856.824967	72418.136010	33.481498
857.770231	72523.592875	33.486516
858.769686	72634.810846	33.491533
859.944669	72762.847842	33.496551
861.105279	72863.179154	33.501568
861.509042	72977.981928	33.506586
862.574185	73074.487529	33.511604
862.992568	73195.608286	33.516621
863.911929	73311.304061	33.521639
864.970726	73433.543933	33.526656
865.381285	73551.685443	33.531674
866.195867	73664.670039	33.536692
866.999606	73785.429714	33.541709
867.634411	73916.511177	33.546727
868.834393	74030.934184	33.551744
869.811423	74155.851929	33.556762
870.907629	74277.181003	33.561780
871.773596	74394.047986	33.566797
872.423640	74519.405518	33.571815
873.811969	74627.602512	33.576832
874.476580	74748.232132	33.581850
875.215529	74860.812085	33.586868
876.195068	74969.012776	33.591885
877.283493	75106.551691	33.596903
878.463165	75213.527424	33.601920
880.711301	75277.157109	33.606938
881.976061	75348.084834	33.611956
882.966751	75424.617844	33.616973
883.703824	75499.895943	33.621991
884.769140	75564.251958	33.627008
885.349839	75642.551079	33.632026
886.550719	75706.987094	33.637044
887.520036	75783.158314	33.642061
887.985018	75865.382416	33.647079
889.222260	75933.554771	33.652096
889.534695	76002.468604	33.657114
890.111538	76090.357479	33.662132
890.604529	76171.004683	33.667149
891.123002	76270.602005	33.672167
892.156974	76360.884130	33.677184
892.376330	76471.198348	33.682202
893.096940	76573.362558	33.687220
893.883941	76674.581329	33.692237
894.457668	76789.505177	33.697255
895.211446	76898.990883	33.702272
895.892241	77027.468629	33.707290
896.475606	77157.511171	33.712308
897.345251	77279.608517	33.717325
898.306771	77415.381989	33.722343
898.918878	77546.458983	33.727360
899.691967	77688.003227	33.732378
900.568054	77833.798427	33.737396
902.197331	77954.331521	33.742413
902.686916	78094.684858	33.747431
903.950147	78212.831643	33.752448
904.964005	78344.279621	33.757466
906.330237	78464.851261	33.762484
907.241991	78598.769565	33.767501
907.969366	78730.436266	33.772519
909.030440	78852.910746	33.777536
909.793724	78977.228477	33.782554
910.520239	79099.700777	33.787572
911.612818	79232.658936	33.792589
912.621608	79368.172335	33.797607
913.362816	79486.978409	33.802624
914.413212	79626.943230	33.807642
914.873687	79757.634948	33.812660
915.855148	79877.030827	33.817677
916.568758	80029.637423	33.822695
917.852174	80154.562172	33.827712
918.512152	80293.740262	33.832730
919.501731	80418.213976	33.837748
921.042238	80543.637477	33.842765
921.667726	80676.293644	33.847783
922.562063	80819.452068	33.852800
923.472629	80953.505934	33.857818
924.784594	81069.335018	33.862836
926.258110	81186.169458	33.867853
927.044354	81313.633067	33.872871
928.318893	81434.843511	33.877888
928.909975	81545.403912	33.882906
929.447318	81663.723870	33.887924
930.591427	81780.778427	33.892941
931.190604	81884.663570	33.897959
932.159159	82007.721417	33.902976
932.995198	82118.612540	33.907994
933.828527	82247.237578	33.913012
934.642157	82363.620967	33.918029
935.335667	82490.524896	33.923047
936.330303	82615.598873	33.928064
937.185186	82746.891433	33.933082
938.117751	82878.741441	33.938100
938.733145	82996.500165	33.943117
939.961545	83140.752996	33.948135
940.849516	83272.720047	33.953152
941.909500	83411.532831	33.958170
942.740844	83540.166104	33.963188
944.107517	83651.429774	33.968205
944.754729	83803.372718	33.973223
945.715652	83922.067925	33.978240
946.600627	84064.832740	33.983258
947.276667	84208.409426	33.988276
948.385468	84347.024599	33.993293
949.441885	84488.867198	33.998311
950.307641	84628.597720	34.003328
951.084647	84767.211530	34.008346
952.108487	84902.107169	34.013364
953.260526	85049.578140	34.018381
953.693497	85201.761202	34.023399
954.705903	85340.391878	34.028416
956.210559	85483.661989	34.033434
957.087807	85628.967698	34.038452
958.338958	85771.856449	34.043469
959.736581	85894.697966	34.048487
960.944063	86009.053342	34.053504
961.854230	86155.312174	34.058522
962.688085	86280.357511	34.063540
963.936495	86409.529857	34.068557
964.672046	86544.216186	34.073575
965.554591	86674.162858	34.078592
967.132439	86800.243684	34.083610
967.628422	86935.685114	34.088628
968.641123	87067.858231	34.093645
969.478097	87192.585903	34.098663
970.485770	87334.878844	34.103680
971.626391	87452.856909	34.108698
972.549057	87588.354708	34.113716
973.571242	87700.029493	34.118733
974.619004	87838.607485	34.123751
975.471577	87971.349128	34.128768
976.562363	88100.499808	34.133786
977.520066	88235.610358	34.138804
978.126653	88360.223349	34.143821
979.482225	88487.671082	34.148839
980.687686	88614.675490	34.153856
982.011585	88746.183328	34.158874
982.722094	88860.152328	34.163892
983.369789	88970.211113	34.168909
984.369148	89088.119402	34.173927
985.153783	89204.993745	34.178944
986.250489	89324.070406	34.183962
986.958122	89450.488566	34.188980
987.974426	89567.543017	34.193997
988.652559	89702.751451	34.199015
989.401689	89836.305152	34.204032
989.987148	89965.155229	34.209050
990.697618	90108.987205	34.214068
991.807486	90251.554977	34.219085
992.778300	90395.480228	34.224103
993.782061	90550.196829	34.229120
995.001586	90683.984442	34.234138
995.993043	90832.595647	34.239156
996.878146	90977.607186	34.244173
998.012146	91126.438033	34.249191
998.658318	91291.582620	34.254208
999.878176	91418.126719	34.259226
1000.630981	91580.290275	34.264244
1001.965763	91727.853622	34.269261
1003.131709	91881.624070	34.274279
1003.549615	92034.648102	34.279296
1004.769468	92186.052957	34.284314
1005.732441	92354.412379	34.289332
1006.722639	92495.160556	34.294349
1007.697767	92664.949833	34.299367
1008.773847	92820.550042	34.304384
1010.118364	92978.897980	34.309402
1011.037749	93135.935813	34.314420
1012.320264	93286.054228	34.319437
1013.240986	93436.136335	34.324455
1014.185557	93594.077895	34.329472
1015.456505	93753.720749	34.334490
1016.448324	93895.236570	34.339508
1017.572471	94048.750379	34.344525
1018.768937	94205.454382	34.349543
1020.030688	94348.751848	34.354560
1021.137917	94495.117362	34.359578
1021.978207	94650.704610	34.364596
1023.021782	94787.606552	34.369613
1024.325592	94934.772314	34.374631
1025.111638	95098.860241	34.379648
1026.155131	95245.221814	34.384666
1027.218208	95389.803699	34.389684
1028.318362	95523.449708	34.394701
1029.334481	95672.298111	34.399719
1030.352977	95815.700573	34.404736
1031.778916	95955.756003	34.409754
1032.628965	96117.740981	34.414772
1033.683514	96238.778278	34.419789
1034.710981	96376.698274	34.424807
1035.352218	96535.398314	34.429824
1036.988226	96685.635079	34.434842
1037.506916	96817.515049	34.439860
1038.630639	96947.812896	34.444877
1039.608393	97078.716719	34.449895
1040.194910	97217.515400	34.454912
1041.249384	97370.367045	34.459930
1042.371643	97507.892937	34.464948
1043.230696	97646.442113	34.469965
1044.462739	97786.811735	34.474983
1045.036977	97946.114304	34.480000
1046.342539	98079.837612	34.485018
1047.510749	98233.942248	34.490036
1048.320456	98382.252889	34.495053
1049.675575	98527.074029	34.500071
1050.580519	98669.291529	34.505088
1051.719056	98813.889541	34.510106
1052.584130	98970.685575	34.515124
1053.908698	99124.069062	34.520141
1055.488522	99271.820084	34.525159
1056.000029	99432.686696	34.530176
1057.052110	99576.366887	34.535194
1058.078185	99727.859528	34.540212
1059.101497	99892.849015	34.545229
1060.187249	100036.988588	34.550247
1060.901685	100197.170240	34.555264
1061.898524	100359.547872	34.560282
1062.914056	100517.785721	34.565300
1064.098965	100695.795461	34.570317
1065.307696	100847.025944	34.575335
1066.368547	101007.911036	34.580352
1067.449864	101170.027813	34.585370
1068.632071	101332.370112	34.590388
1069.196266	101498.405807	34.595405
1070.583058	101665.627951	34.600423
1071.577599	101842.151827	34.605440
1072.902130	101992.194417	34.610458
1073.509114	102161.606924	34.615476
1074.447910	102342.060213	34.620493
1076.134288	102514.707855	34.625511
1076.863695	102682.111435	34.630528
1077.686282	102853.987773	34.635546
1078.702213	103023.607226	34.640564
1079.511550	103219.920047	34.645581
1080.995390	103395.232441	34.650599
1082.011559	103570.114288	34.655616
1083.294996	103734.254263	34.660634
1084.022249	103924.207373	34.665652
1085.335114	104083.459835	34.670669
1086.710958	104276.236191	34.675687
1087.596975	104449.430314	34.680704
1088.928767	104613.537056	34.685722
1090.068700	104804.311206	34.690740
1090.991554	104965.738947	34.695757
1092.211077	105141.947985	34.700775
1093.525638	105304.967433	34.705792
1095.002091	105469.424123	34.710810
1096.161046	105637.666266	34.715828
1097.240422	105790.746380	34.720845
1098.618214	105931.192448	34.725863
1099.274931	106093.037202	34.730880
1100.121964	106233.702361	34.735898
1101.106282	106394.490787	34.740916
1101.981613	106564.208510	34.745933
1103.213967	106719.909321	34.750951
1104.001713	106894.655713	34.755968
1105.532181	107055.576881	34.760986
1106.610290	107208.849781	34.766004
1107.730184	107383.135510	34.771021
1109.056112	107527.953495	34.776039
1109.925600	107705.996507	34.781056
1110.798955	107878.812376	34.786074
1112.052081	108035.417108	34.791092
1112.562864	108213.913307	34.796109
1113.886544	108392.597996	34.801127
1115.077920	108567.798621	34.806144
1116.284129	108748.441369	34.811162
1117.268097	108933.526046	34.816180
1118.371976	109109.915422	34.821197
1119.622338	109293.770536	34.826215
1120.390017	109473.678227	34.831232
1121.506130	109659.475285	34.836250
1122.881285	109837.820583	34.841268
1123.553954	110037.717447	34.846285
1124.881217	110212.401885	34.851303
1125.947029	110411.239171	34.856320
1126.965845	110593.254589	34.861338
1128.293690	110784.476447	34.866356
1129.357345	110989.730887	34.871373
1130.939422	111162.235704	34.876391
1132.064488	111360.045767	34.881408
1133.143374	111548.477295	34.886426
1134.427413	111736.111689	34.891444
1135.879539	111912.775958	34.896461
1137.128500	112098.418347	34.901479
1138.064274	112283.630832	34.906496
1139.369406	112456.131727	34.911514
1140.587030	112649.006056	34.916532
1141.534041	112832.119163	34.921549
1142.704660	113001.992800	34.926567
1143.791356	113192.385303	34.931584
1144.960412	113380.164317	34.936602
1146.739866	113544.760131	34.941620
1147.868695	113718.500585	34.946637
1148.852435	113896.285271	34.951655
1150.073666	114082.605197	34.956672
1151.565595	114253.202230	34.961690
1152.997642	114434.559598	34.966708
1153.778489	114600.448010	34.971725
1155.679249	114755.707172	34.976743
1156.740525	114935.183527	34.981760
1157.935445	115082.731951	34.986778
1159.054387	115238.745171	34.991796
1159.813250	115392.113268	34.996813
1161.122138	115528.275662	35.001831
1161.892072	115691.558233	35.006848
1163.192549	115839.879332	35.011866
1164.266611	115996.366516	35.016884
1165.248882	116171.008169	35.021901
1166.161169	116328.896993	35.026919
1166.898259	116486.795659	35.031936
1167.680674	116675.882559	35.036954
1168.880962	116852.678512	35.041972
1169.842516	117024.036970	35.046989
1171.119614	117204.191450	35.052007
1172.162197	117405.386112	35.057024
1173.459815	117581.779059	35.062042
1174.700000	117758.378628	35.067060
1175.868859	117968.016629	35.072077
1177.358960	118135.049904	35.077095
1178.134760	118331.171877	35.082112
1178.880583	118531.783009	35.087130
1180.497428	118718.972996	35.092148
1181.607236	118918.307198	35.097165
1182.808387	119103.318241	35.102183
1183.674497	119316.497860	35.107200
1184.694571	119512.273315	35.112218
1185.953257	119713.749161	35.117236
1186.906138	119923.278998	35.122253
1188.322358	120132.990127	35.127271
1189.674853	120337.545971	35.132288
1190.980200	120544.086580	35.137306
1192.518933	120739.459474	35.142324
1193.787159	120935.294772	35.147341
1195.169089	121131.949328	35.152359
1196.410666	121332.845093	35.157376
1197.599699	121537.068982	35.162394
1198.767963	121728.113353	35.167412
1199.878623	121927.666626	35.172429
1201.649364	122123.443507	35.177447
1202.797407	122318.510260	35.182464
1203.901677	122517.258402	35.187482
1205.421564	122709.799132	35.192500
1206.103838	122907.097412	35.197517
1207.595077	123101.520052	35.202535
1208.783410	123288.367418	35.207552
1209.835538	123498.581116	35.212570
1211.366874	123681.336248	35.217588
1212.198906	123890.030089	35.222605
1213.621895	124076.921646	35.227623
1214.668548	124284.330470	35.232640
1215.812097	124481.440342	35.237658
1217.064310	124685.171639	35.242676
1218.777792	124868.197216	35.247693
1220.125653	125066.038875	35.252711
1221.639880	125250.099392	35.257728
1222.717839	125444.934039	35.262746
1223.901463	125613.089321	35.267764
1224.958148	125788.688713	35.272781
1226.100635	125957.156676	35.277799
1227.774645	126134.408216	35.282816
1228.596273	126303.208013	35.287834
1229.875969	126482.259928	35.292852
1230.796319	126662.839573	35.297869
1232.185216	126831.603118	35.302887
1233.710880	127020.905490	35.307904
1234.906803	127196.035771	35.312922
1235.904705	127380.180107	35.317940
1236.970812	127553.458477	35.322957
1237.901822	127737.831198	35.327975
1239.139678	127939.473569	35.332992
1240.483028	128133.335082	35.338010
1241.519929	128327.348022	35.343028
1242.607933	128522.139634	35.348045
1244.126350	128715.800042	35.353063
1245.448768	128920.983280	35.358080
1246.265458	129126.628493	35.363098
1247.722906	129326.472455	35.368116
1248.834932	129524.054385	35.373133
1249.915465	129735.236401	35.378151
1251.102842	129947.150496	35.383168
1252.195319	130145.234019	35.388186
1253.490315	130363.557362	35.393204
1254.905448	130586.690286	35.398221
1256.032670	130790.524678	35.403239
1257.141347	131016.268938	35.408256
1258.231021	131243.513031	35.413274
1259.774207	131446.500529	35.418292
1260.998161	131685.078816	35.423309
1262.419821	131886.048964	35.428327
1263.960129	132113.963261	35.433344
1265.122547	132335.363721	35.438362
1266.530666	132544.512851	35.443380
1267.538492	132760.594407	35.448397
1269.126138	132985.163223	35.453415
1270.357315	133186.882380	35.458432
1271.616293	133424.088605	35.463450
1273.116513	133636.576104	35.468468
1274.186370	133853.733054	35.473485
1275.337103	134072.513320	35.478503
1276.859628	134282.315840	35.483520
1278.019014	134515.340169	35.488538
1279.285464	134732.662555	35.493556
1280.659902	134936.613991	35.498573
1282.311220	135150.647186	35.503591
1283.963530	135369.420892	35.508608
1285.199317	135584.258279	35.513626
1286.925577	135770.508321	35.518644
1288.036196	135988.802577	35.523661
1288.949365	136203.949250	35.528679
1290.505801	136397.402485	35.533696
1291.677988	136602.550878	35.538714
1292.706795	136798.979832	35.543732
1293.992474	137000.450764	35.548749
1295.652968	137197.757718	35.553767
1296.542003	137375.065127	35.558784
1297.843452	137573.812948	35.563802
1299.440620	137767.192693	35.568820
1300.477311	137973.512692	35.573837
1301.630883	138169.766202	35.578855
1303.227683	138350.743380	35.583872
1304.291764	138542.312029	35.588890
1306.062730	138743.819084	35.593908
1307.077589	138941.709189	35.598925
1308.301547	139139.453311	35.603943
1309.619102	139341.936263	35.608960
1310.762697	139554.067161	35.613978
1312.322749	139756.755163	35.618996
1313.773105	139957.408893	35.624013
1315.149227	140170.597094	35.629031
1316.263096	140363.272076	35.634048
1317.553918	140576.590770	35.639066
1318.839091	140784.829727	35.644084
1319.950624	140998.484065	35.649101
1321.221225	141206.487438	35.654119
1322.748792	141421.346012	35.659136
1323.976518	141628.535286	35.664154
1325.581629	141845.805273	35.669172
1326.719399	142056.446441	35.674189
1327.574374	142268.959108	35.679207
1329.419091	142490.276719	35.684224
1330.745861	142712.071166	35.689242
1332.236427	142928.530539	35.694260
1333.396083	143158.276372	35.699277
1334.576221	143364.458311	35.704295
1336.169447	143583.808491	35.709312
1337.331633	143805.434176	35.714330
1338.263465	144033.283467	35.719348
1340.245685	144253.945472	35.724365
1341.083035	144477.173951	35.729383
1342.469306	144696.590251	35.734400
1343.885326	144933.064425	35.739418
1345.434673	145150.772176	35.744436
1346.861084	145377.766815	35.749453
1348.291603	145607.259551	35.754471
1349.724013	145815.902070	35.759488
1350.331369	146060.397591	35.764506
1351.698039	146290.425171	35.769524
1353.451695	146511.152104	35.774541
1354.537879	146750.683925	35.779559
1356.387528	146974.479131	35.784576
1358.015288	147204.066220	35.789594
1359.430038	147413.558732	35.794612
1360.868802	147643.838207	35.799629
1362.172623	147862.440330	35.804647
1363.886770	148083.628153	35.809664
1365.062597	148296.815310	35.814682
1366.218361	148497.558448	35.819700
1367.480408	148711.837542	35.824717
1368.508366	148929.844267	35.829735
1369.810937	149128.729851	35.834752
1371.228005	149331.819949	35.839770
1372.651047	149535.201950	35.844788
1374.305380	149756.550232	35.849805
1374.997382	149966.820805	35.854823
1376.735346	150178.916866	35.859840
1377.541517	150404.461148	35.864858
1378.790031	150647.507902	35.869876
1380.261556	150863.923132	35.874893
1381.337140	151096.300702	35.879911
1382.680202	151329.106491	35.884928
1384.284781	151558.956430	35.889946
1385.717231	151804.239209	35.894964
1386.657753	152039.421408	35.899981
1387.932966	152290.628144	35.904999
1389.522658	152528.854868	35.910016
1390.933585	152785.102453	35.915034
1392.325813	153023.110536	35.920052
1393.701376	153268.996408	35.925069
1394.870962	153520.064397	35.930087
1396.511783	153762.982960	35.935104
1398.236608	154010.999544	35.940122
1399.681206	154261.129175	35.945140
1401.201955	154506.506573	35.950157
1402.485530	154755.232721	35.955175
1404.402484	154995.618499	35.960192
1405.686395	155255.696251	35.965210
1406.885550	155498.190328	35.970228
1408.546033	155746.369353	35.975245
1409.906595	155998.503186	35.980263
1411.126132	156237.525054	35.985280
1412.877370	156491.832082	35.990298
1414.041330	156738.677071	35.995316
1415.617436	156979.384600	36.000333
1417.218351	157231.007459	36.005351
1418.822658	157465.094872	36.010368
1420.197974	157714.322502	36.015386
1421.443658	157965.474583	36.020404
1423.556170	158210.188531	36.025421
1424.796026	158443.503551	36.030439
1426.274698	158691.605874	36.035456
1427.732449	158927.311509	36.040474
1429.175952	159167.852393	36.045492
1430.639229	159407.047606	36.050509
1431.964661	159645.683024	36.055527
1433.439417	159889.292680	36.060544
1435.160701	160123.607583	36.065562
1436.209110	160371.853538	36.070580
1437.851456	160608.986755	36.075597
1438.758298	160845.528268	36.080615
1440.079518	161106.227216	36.085632
1441.555257	161337.938705	36.090650
1442.880172	161584.386428	36.095668
1444.684644	161807.856349	36.100685
1445.675886	162034.703437	36.105703
1447.277379	162266.806764	36.110720
1448.747217	162496.408784	36.115738
1449.683164	162735.608672	36.120756
1451.472122	162980.254761	36.125773
1452.598182	163213.023085	36.130791
1453.921097	163458.342512	36.135808
1455.784759	163701.168005	36.140826
1456.718752	163947.770034	36.145844
1458.380206	164199.901895	36.150861
1459.826438	164439.995760	36.155879
1461.347553	164692.850853	36.160896
1462.739080	164941.289267	36.165914
1464.481016	165201.532236	36.170932
1466.410379	165430.851373	36.175949
1467.762799	165690.145021	36.180967
1469.373197	165935.321126	36.185984
1471.239760	166167.901690	36.191002
1472.499756	166410.650670	36.196020
1474.084354	166655.848287	36.201037
1475.535879	166895.678150	36.206055
1477.153882	167137.575887	36.211072
1478.571190	167387.028494	36.216090
1479.993532	167635.099416	36.221108
1481.268676	167873.695140	36.226125
1482.435379	168141.076772	36.231143
1483.856032	168388.049378	36.236160
1485.526822	168647.756743	36.241178
1486.660616	168909.111347	36.246196
1488.343765	169169.429129	36.251213
1489.943463	169425.652196	36.256231
1491.419729	169684.255888	36.261248
1492.890020	169925.826925	36.266266
1494.175470	170206.231093	36.271284
1495.831986	170471.001500	36.276301
1497.459087	170721.305029	36.281319
1499.252377	170991.575132	36.286336
1500.706468	171260.328056	36.291354
1502.093781	171524.577553	36.296372
1503.977848	171758.153358	36.301389
1505.378253	172039.313513	36.306407
1507.007912	172300.865816	36.311424
1509.199072	172533.801214	36.316442
1510.898855	172795.523237	36.321460
1512.311590	173030.767119	36.326477
1513.987682	173286.787642	36.331495
1515.052262	173527.823662	36.336512
1516.594407	173779.136849	36.341530
1518.082074	174026.578393	36.346548
1519.598135	174277.048883	36.351565
1520.964681	174532.682513	36.356583
1522.193574	174779.852631	36.361600
1523.587225	175031.159142	36.366618
1524.905664	175278.901632	36.371636
1526.229896	175519.756035	36.376653
1527.898440	175763.259359	36.381671
1529.199909	176009.423171	36.386688
1530.501025	176263.606410	36.391706
1531.675989	176508.055243	36.396724
1533.372542	176777.034861	36.401741
1535.009850	177031.321655	36.406759
1536.416828	177285.063001	36.411776
1538.286449	177538.237608	36.416794
1539.501084	177796.097813	36.421812
1541.158319	178060.131345	36.426829
1542.941185	178311.751215	36.431847
1544.357187	178586.800781	36.436864
1546.080690	178841.972990	36.441882
1547.407508	179132.150884	36.446900
1549.343588	179366.383628	36.451917
1550.315205	179649.250047	36.456935
1551.748362	179922.085215	36.461952
1553.488491	180190.178899	36.466970
1554.738467	180470.633920	36.471988
1556.577417	180743.346408	36.477005
1557.923046	181028.852333	36.482023
1559.293508	181305.373050	36.487040
1560.996829	181593.325418	36.492058
1562.407148	181883.546672	36.497076
1564.217328	182162.705572	36.502093
1565.957177	182461.366789	36.507111
1566.959345	182742.967015	36.512128
1568.948506	183034.131691	36.517146
1570.286473	183325.249458	36.522164
1572.060692	183613.660583	36.527181
1573.712663	183902.549792	36.532199
1575.298019	184196.590448	36.537216
1576.993064	184484.994396	36.542234
1578.736619	184788.911199	36.547252
1580.517329	185055.860700	36.552269
1582.975861	185319.404919	36.557287
1584.783078	185606.643495	36.562304
1586.791856	185866.049484	36.567322
1588.567393	186135.417128	36.572340
1589.823965	186405.224093	36.577357
1591.674482	186668.707719	36.582375
1593.005060	186935.333643	36.587392
1594.480745	187212.369009	36.592410
1596.037738	187480.738672	36.597428
1597.588661	187756.470973	36.602445
1599.115496	188035.127418	36.607463
1600.325679	188308.188755	36.612480
1602.027054	188591.909485	36.617498
1603.391597	188873.845348	36.622516
1605.170188	189150.171489	36.627533
1606.697183	189425.625498	36.632551
1608.032100	189718.928929	36.637568
1609.455072	189987.752939	36.642586
1611.100465	190261.898540	36.647604
1612.581653	190511.655046	36.652621
1614.624286	190774.001662	36.657639
1616.159505	191043.410204	36.662656
1617.939672	191291.498840	36.667674
1619.320512	191561.480480	36.672692
1621.030583	191825.598868	36.677709
1622.680828	192087.037686	36.682727
1624.133157	192355.844779	36.687744
1625.386915	192626.157050	36.692762
1627.120788	192899.161235	36.697780
1628.746548	193176.042247	36.702797
1630.327161	193453.515774	36.707815
1631.718217	193744.968842	36.712832
1633.251539	194015.726532	36.717850
1634.980471	194307.598792	36.722868
1636.429192	194604.517755	36.727885
1638.289492	194881.675525	36.732903
1639.922049	195180.865867	36.737920
1641.718216	195466.883197	36.742938
1643.220289	195744.724451	36.747956
1645.488661	196027.522313	36.752973
1647.726653	196302.254390	36.757991
1649.531082	196584.646687	36.763008
1651.491064	196859.248179	36.768026
1653.436138	197130.337725	36.773044
1654.641405	197406.128103	36.778061
1656.500509	197668.095595	36.783079
1657.789139	197947.124828	36.788096
1659.553627	198230.496970	36.793114
1661.751001	198491.830970	36.798132
1663.443947	198765.393249	36.803149
1664.864030	199035.890540	36.808167
1666.453557	199302.465596	36.813184
1668.274116	199577.661819	36.818202
1670.133923	199853.830568	36.823220
1671.122936	200133.147248	36.828237
1673.038331	200412.330942	36.833255
1674.695123	200685.502511	36.838272
1676.782011	200959.609905	36.843290
1678.007817	201243.261103	36.848308
1679.650347	201513.240348	36.853325
1681.877834	201793.016159	36.858343
1683.381962	202069.150987	36.863360
1684.978299	202346.960774	36.868378
1686.586978	202622.294732	36.873396
1687.996451	202913.655642	36.878413
1689.887715	203192.450953	36.883431
1691.354704	203488.895861	36.888448
1692.813591	203765.883967	36.893466
1694.602282	204047.010025	36.898484
1696.282924	204341.178607	36.903501
1697.952952	204637.140230	36.908519
1699.535816	204926.325876	36.913536
1701.112374	205215.755150	36.918554
1702.946976	205484.186762	36.923572
1704.396522	205770.566954	36.928589
1706.139579	206036.400610	36.933607
1707.661352	206303.717758	36.938624
1709.184636	206579.985444	36.943642
1710.617224	206854.186917	36.948660
1712.305297	207140.561238	36.953677
1714.555972	207434.705557	36.958695
1716.022379	207718.807407	36.963712
1717.622151	208007.662634	36.968730
1719.595747	208295.101533	36.973748
1721.428057	208582.386491	36.978765
1723.048206	208862.279959	36.983783
1724.684070	209153.280301	36.988800
1726.525913	209449.911290	36.993818
1728.231728	209737.780291	36.998836
1729.765075	210044.060579	37.003853
1731.589836	210333.678062	37.008871
1732.917260	210645.541781	37.013888
1734.790119	210943.342873	37.018906
1737.128465	211240.474769	37.023924
1738.615681	211540.828179	37.028941
1740.811394	211848.598941	37.033959
1742.312319	212150.679609	37.038976
1744.233629	212450.676334	37.043994
1746.050623	212737.449405	37.049012
1747.506865	213056.870979	37.054029
1749.459108	213347.510141	37.059047
1751.092017	213659.746154	37.064064
1753.046503	213962.029761	37.069082
1755.626451	214243.165511	37.074100
1757.316173	214539.234649	37.079117
1759.438198	214829.574001	37.084135
1761.193108	215111.072893	37.089152
1763.128962	215398.841532	37.094170
1765.256698	215685.666789	37.099188
1766.485431	215968.204966	37.104205
1768.658233	216263.481208	37.109223
1770.177363	216552.234965	37.114240
1771.949239	216848.770806	37.119258
1773.913347	217126.397680	37.124276
1775.602610	217414.835961	37.129293
1777.757430	217700.217805	37.134311
1779.089264	217979.421212	37.139328
1781.077958	218266.710804	37.144346
1783.195011	218550.261018	37.149364
1784.807165	218841.688342	37.154381
1786.670198	219109.498945	37.159399
1788.490387	219394.280396	37.164416
1789.751522	219676.091740	37.169434
1792.015380	219966.163089	37.174452
1793.741445	220237.249981	37.179469
1795.317430	220588.061391	37.184487
1797.122251	220873.892133	37.189504
1798.931474	221152.473159	37.194522
1800.633635	221418.171802	37.199540
1802.186409	221694.598906	37.204557
1804.091119	221951.404544	37.209575
1805.722587	222215.872844	37.214592
1807.401722	222484.194500	37.219610
1809.182872	222752.564377	37.224628
1810.609212	223035.606338	37.229645
1812.326428	223312.406737	37.234663
1813.979001	223606.779154	37.239680
1815.679270	223891.253623	37.244698
1817.966913	224167.217295	37.249716
1819.431588	224463.400379	37.254733
1821.526251	224749.478692	37.259751
1823.326608	225023.973521	37.264768
1824.756379	225317.663793	37.269786
1827.109910	225609.379981	37.274804
1829.030097	225907.540368	37.279821
1830.535983	226191.990250	37.284839
1832.702882	226492.970623	37.289856
1834.452009	226781.752028	37.294874
1836.818044	227073.509446	37.299892
1838.425844	227380.753026	37.304909
1840.004145	227669.132821	37.309927
1842.078072	227964.723719	37.314944
1843.814872	228279.873751	37.319962
1845.802031	228564.255149	37.324980
1847.818917	228865.369243	37.329997
1849.580299	229174.575734	37.335015
1851.097487	229471.606113	37.340032
1853.107509	229774.527561	37.345050
1855.312644	230069.317370	37.350068
1857.071556	230378.071247	37.355085
1858.943816	230671.011048	37.360103
1860.739069	230968.433947	37.365120
1862.631431	231288.369950	37.370138
1864.899993	231585.846690	37.375156
1866.675204	231893.815711	37.380173
1868.492491	232193.575591	37.385191
1870.557532	232489.030262	37.390208
1872.194567	232798.827386	37.395226
1874.583587	233081.812892	37.400244
1875.990757	233391.369016	37.405261
1878.305062	233688.514851	37.410279
1880.382611	233985.851547	37.415296
1882.176041	234291.514063	37.420314
1884.272078	234576.531428	37.425332
1886.335057	234872.399969	37.430349
1888.041571	235162.077920	37.435367
1889.976417	235455.098460	37.440384
1891.955088	235761.599552	37.445402
1893.851735	236038.372684	37.450420
1895.972053	236342.414729	37.455437
1897.581986	236637.674457	37.460455
1899.410148	236924.163143	37.465472
1901.257383	237214.230827	37.470490
1903.409341	237482.382350	37.475508
1905.349249	237746.275740	37.480525
1907.222720	238008.580164	37.485543
1908.878727	238269.192578	37.490560
1910.475159	238542.133713	37.495578
1912.534644	238806.544044	37.500596
1914.185306	239089.713842	37.505613
1916.080963	239369.137144	37.510631
1918.109227	239636.703901	37.515648
1919.639016	239931.578751	37.520666
1921.381616	240209.098010	37.525684
1923.203251	240511.014514	37.530701
1925.014244	240799.776389	37.535719
1927.023653	241088.024880	37.540736
1928.653413	241398.178232	37.545754
1930.448967	241692.989882	37.550772
1932.396135	242008.301410	37.555789
1934.183914	242314.977602	37.560807
1936.725883	242632.583936	37.565824
1938.424797	242949.842253	37.570842
1940.363037	243253.296427	37.575860
1942.457388	243571.712750	37.580877
1944.167727	243882.392868	37.585895
1946.080556	244208.891483	37.590912
1947.858573	244536.910929	37.595930
1949.818300	244851.719434	37.600948
1951.608983	245171.864234	37.605965
1953.453374	245507.394094	37.610983
1955.729962	245832.086257	37.616000
1957.135127	246168.017620	37.621018
1959.532032	246506.459503	37.626036
1960.935595	246846.761675	37.631053
1962.764412	247192.382183	37.636071
1965.118988	247537.716869	37.641088
1966.821757	247893.443246	37.646106
1969.109314	248231.855663	37.651124
1971.397977	248585.509407	37.656141
1973.236546	248930.954554	37.661159
1975.622810	249267.905709	37.666176
1977.336180	249610.298649	37.671194
1979.350665	249948.351691	37.676212
1981.337742	250295.528932	37.681229
1983.566085	250649.806463	37.686247
1985.790585	250981.884333	37.691264
1987.747538	251331.176837	37.696282
1990.066241	251672.309501	37.701300
1991.832771	252013.124015	37.706317
1993.850653	252365.126910	37.711335
1995.889950	252703.460886	37.716352
1997.800120	253042.120800	37.721370
2000.013902	253384.594258	37.726388
2002.051209	253722.981213	37.731405
2003.987293	254058.107962	37.736423
2006.042360	254400.278193	37.741440
2008.046494	254738.519765	37.746458
2010.087545	255047.721354	37.751476
2012.042369	255366.513729	37.756493
2014.184270	255677.834051	37.761511
2016.708730	255973.928968	37.766528
2018.570498	256280.925427	37.771546
2020.355690	256584.124113	37.776564
2022.443281	256899.290572	37.781581
2024.242893	257197.585141	37.786599
2026.303351	257512.756758	37.791616
2027.804392	257837.721311	37.796634
2030.206788	258144.990154	37.801652
2032.406437	258469.819326	37.806669
2034.164687	258786.056668	37.811687
2036.270376	259107.878672	37.816704
2038.254201	259437.696851	37.821722
2040.031034	259762.747174	37.826740
2042.346732	260106.205589	37.831757
2044.274075	260428.717966	37.836775
2046.480497	260757.410123	37.841792
2048.547102	261099.435915	37.846810
2050.871532	261419.295327	37.851828
2053.168292	261744.925922	37.856845
2054.887692	262086.144225	37.861863
2057.426263	262412.702469	37.866880
2059.426254	262740.413408	37.871898
2061.440124	263071.501065	37.876916
2063.781167	263394.662212	37.881933
2065.905220	263716.918168	37.886951
2068.617977	264043.450346	37.891968
2070.663003	264360.664201	37.896986
2072.845816	264687.128589	37.902004
2075.215906	264999.083768	37.907021
2077.062852	265318.666903	37.912039
2079.158849	265633.816030	37.917056
2081.086940	265961.083926	37.922074
2082.993272	266285.764388	37.927092
2084.991917	266606.162695	37.932109
2086.937726	266942.954669	37.937127
2089.258349	267250.321277	37.942144
2090.992372	267594.539613	37.947162
2093.031431	267926.363792	37.952180
2095.402057	268253.715399	37.957197
2097.232025	268592.000150	37.962215
2099.409227	268927.689671	37.967232
2101.405854	269261.553564	37.972250
2103.781186	269595.763996	37.977268
2105.659500	269933.457462	37.982285
2107.680071	270274.303924	37.987303
2109.999197	270617.643500	37.992320
2111.888338	270954.700567	37.997338
2113.858911	271300.864642	38.002356
2116.286417	271640.732520	38.007373
2117.898661	271984.514914	38.012391
2119.940108	272328.407141	38.017408
2122.446543	272673.826107	38.022426
2123.970554	272995.852012	38.027444
2126.145083	273328.825271	38.032461
2127.827495	273658.345558	38.037479
2130.244211	273971.872280	38.042496
2131.676625	274305.369811	38.047514
2134.027680	274644.767669	38.052532
2136.264481	274973.641243	38.057549
2137.840661	275329.369395	38.062567
2140.199803	275664.193360	38.067584
2142.317542	276018.667032	38.072602
2144.302733	276370.316514	38.077620
2146.544639	276717.987711	38.082637
2148.468956	277086.362195	38.087655
2150.748372	277442.308837	38.092672
2152.779031	277804.645706	38.097690
2154.838418	278177.875980	38.102708
2157.238326	278535.175030	38.107725
2159.338314	278907.001458	38.112743
2161.486964	279287.025321	38.117760
2163.932667	279647.009487	38.122778
2165.953949	280020.143538	38.127796
2168.488948	280388.089876	38.132813
2171.042049	280761.190039	38.137831
2173.133357	281124.659185	38.142848
2175.653739	281501.854068	38.147866
2177.526637	281866.348165	38.152884
2180.160655	282238.393114	38.157901
2181.974093	282604.953841	38.162919
2184.321425	282968.965536	38.167936
2186.423897	283341.500474	38.172954
2188.684765	283712.257190	38.177972
2191.110796	284080.370896	38.182989
2193.664783	284444.094671	38.188007
2196.224911	284801.720420	38.193024
2198.778869	285151.268658	38.198042
2200.988947	285517.433929	38.203060
2203.529060	285873.105867	38.208077
2205.636462	286224.298947	38.213095
2207.591740	286575.973067	38.218112
2209.881901	286936.078324	38.223130
2211.871601	287295.722791	38.228148
2213.921045	287654.925545	38.233165
2215.599010	288023.712890	38.238183
2218.003479	288391.546302	38.243200
2220.397298	288756.205607	38.248218
2222.334465	289140.065181	38.253236
2224.799574	289501.257476	38.258253
2226.758621	289885.214189	38.263271
2229.061371	290256.185896	38.268288
2231.405951	290618.869191	38.273306
2233.746647	290996.260716	38.278324
2236.095670	291374.234623	38.283341
2237.827405	291745.828191	38.288359
2239.946457	292123.430976	38.293376
2242.280545	292486.697481	38.298394
2244.389016	292852.310816	38.303412
2246.833198	293201.485800	38.308429
2248.738473	293554.276618	38.313447
2250.933383	293901.661060	38.318464
2253.328621	294257.649949	38.323482
2255.476331	294614.134729	38.328500
2257.331085	294971.757643	38.333517
2259.730764	295335.593257	38.338535
2261.694384	295705.365234	38.343552
2263.825734	296069.978713	38.348570
2265.709678	296458.000557	38.353588
2268.224572	296820.773660	38.358605
2270.429211	297212.121564	38.363623
2272.421282	297600.352512	38.368640
2274.876627	297993.513322	38.373658
2276.831389	298389.597622	38.378676
2279.501216	298783.814936	38.383693
2281.689461	299175.923163	38.388711
2283.401905	299578.393539	38.393728
2286.081250	299970.295037	38.398746
2288.061757	300387.707804	38.403764
2290.580355	300792.485913	38.408781
2293.006615	301203.373934	38.413799
2295.728075	301617.490827	38.418816
2298.516653	302010.081195	38.423834
2300.866309	302416.532916	38.428852
2303.058400	302819.045951	38.433869
2305.453712	303219.645995	38.438887
2308.048877	303627.833506	38.443904
2310.685964	304025.141664	38.448922
2312.631842	304438.713139	38.453940
2315.062855	304831.809755	38.458957
2317.808460	305233.237556	38.463975
2320.015842	305634.952695	38.468992
2322.781511	306019.915444	38.474010
2325.321639	306426.325312	38.479028
2327.545582	306814.419644	38.484045
2330.040603	307211.105892	38.489063
2332.433998	307596.021361	38.494080
2335.352808	307979.658553	38.499098
2337.730986	308363.380262	38.504116
2340.127110	308736.252179	38.509133
2342.430640	309124.326701	38.514151
2344.912356	309519.102639	38.519168
2347.254460	309881.413274	38.524186
2349.333748	310269.621187	38.529204
2351.559804	310642.666455	38.534221
2353.864813	311030.709023	38.539239
2355.433858	311425.496139	38.544256
2358.051688	311815.975545	38.549274
2360.173649	312222.432019	38.554292
2362.711286	312618.153512	38.559309
2365.073396	313027.032625	38.564327
2366.925892	313433.857461	38.569344
2369.497008	313815.371297	38.574362
2371.540049	314197.119847	38.579380
2374.315035	314572.223552	38.584397
2376.211915	314944.569660	38.589415
2378.682772	315319.287070	38.594432
2381.041936	315684.902823	38.599450
2382.965537	316071.387381	38.604468
2385.032781	316461.885961	38.609485
2387.465224	316858.141239	38.614503
2389.779561	317246.235516	38.619520
2392.545805	317635.831268	38.624538
2395.042266	318039.868663	38.629556
2397.263414	318436.023942	38.634573
2399.459368	318845.997748	38.639591
2401.882267	319255.273447	38.644608
2404.110343	319663.663909	38.649626
2406.570209	320086.568341	38.654644
2408.843625	320505.284451	38.659661
2411.541414	320917.226578	38.664679
2413.784067	321344.502367	38.669696
2415.938373	321772.958330	38.674714
2418.585266	322192.750107	38.679732
2421.022562	322618.363435	38.684749
2423.759946	323040.854145	38.689767
2425.961354	323478.995510	38.694784
2428.361409	323898.640243	38.699802
2430.725722	324332.434013	38.704820
2433.321580	324764.284135	38.709837
2435.836782	325200.690572	38.714855
2438.290025	325643.377157	38.719872
2441.081071	326072.827618	38.724890
2443.409408	326514.538776	38.729908
2445.737760	326952.539797	38.734925
2448.524739	327395.925589	38.739943
2450.578330	327838.891795	38.744960
2453.481183	328272.858162	38.749978
2455.616694	328726.497390	38.754996
2458.288464	329173.167075	38.760013
2461.088763	329611.839985	38.765031
2463.233972	330060.390817	38.770048
2465.794421	330500.594742	38.775066
2468.578399	330942.335015	38.780084
2470.730984	331388.057879	38.785101
2473.615013	331825.586997	38.790119
2475.764688	332285.880558	38.795136
2478.835756	332719.590978	38.800154
2481.520699	333163.364723	38.805172
2483.982846	333600.238751	38.810189
2486.565066	334033.180555	38.815207
2488.993596	334479.170305	38.820224
2491.874499	334906.422174	38.825242
2494.558100	335346.398668	38.830260
2496.769638	335770.551762	38.835277
2498.969909	336203.692642	38.840295
2501.578505	336645.399146	38.845312
2504.125099	337062.711369	38.850330
2506.441197	337472.820956	38.855348
2508.301713	337885.285356	38.860365
2511.238781	338280.132967	38.865383
2513.406890	338695.361855	38.870400
2515.582148	339103.579106	38.875418
2517.944265	339518.238697	38.880436
2520.403932	339946.210012	38.885453
2523.116235	340358.066438	38.890471
2525.552824	340782.938095	38.895488
2527.884531	341209.499183	38.900506
2530.335591	341647.057490	38.905524
2532.779849	342083.090380	38.910541
2535.320635	342512.072033	38.915559
2537.715822	342961.816557	38.920576
2540.293567	343400.763912	38.925594
2542.741374	343863.060801	38.930612
2545.041385	344310.576027	38.935629
2547.886668	344763.079109	38.940647
2550.040917	345225.386416	38.945664
2552.379889	345686.162891	38.950682
2555.392762	346157.034753	38.955700
2557.785287	346623.329741	38.960717
2560.595810	347081.938511	38.965735
2563.054196	347562.686071	38.970752
2565.598362	348040.166415	38.975770
2568.261827	348516.252898	38.980788
2570.551489	348993.359198	38.985805
2573.426899	349466.941437	38.990823
2575.751325	349960.484052	38.995840
2578.704571	350434.807136	39.000858
2581.487291	350926.872134	39.005876
2583.734122	351415.971292	39.010893
2586.672956	351902.392450	39.015911
2589.225948	352393.591839	39.020928
2591.823113	352886.911949	39.025946
2594.519783	353371.250989	39.030964
2596.842508	353865.493773	39.035981
2599.802714	354343.842109	39.040999
2601.977691	354847.033987	39.046016
2605.096017	355350.604514	39.051034
2608.255685	355819.870958	39.056052
2610.746948	356327.541619	39.061069
2613.587014	356807.205667	39.066087
2616.260193	357290.876559	39.071104
2618.801849	357773.243694	39.076122
2621.757326	358252.037856	39.081140
2623.929578	358741.789342	39.086157
2626.557143	359222.174206	39.091175
2629.453084	359725.608568	39.096192
2632.155527	360207.494623	39.101210
2634.886109	360683.838402	39.106228
2638.142628	361154.282009	39.111245
2640.944590	361630.554211	39.116263
2644.028561	362092.970308	39.121280
2646.922257	362543.356685	39.126298
2649.206134	362965.664251	39.131316
2652.088205	363397.466511	39.136333
2654.545637	363814.764523	39.141351
2656.885343	364241.772021	39.146368
2659.300393	364668.230645	39.151386
2662.099980	365086.731752	39.156404
2664.361754	365517.241791	39.161421
2666.883537	365946.564532	39.166439
2669.345253	366397.971025	39.171456
2671.718590	366856.010381	39.176474
2673.986320	367309.138616	39.181492
2676.160257	367769.560145	39.186509
2679.000764	368233.297079	39.191527
2681.349001	368717.737810	39.196544
2683.926806	369200.741113	39.201562
2686.825353	369670.924339	39.206580
2689.305320	370171.212989	39.211597
2691.582354	370654.044607	39.216615
2694.518877	371154.807668	39.221632
2696.993242	371649.395917	39.226650
2699.568387	372158.273353	39.231668
2702.270205	372668.570851	39.236685
2705.207459	373184.305471	39.241703
2707.894700	373706.213560	39.246720
2710.753243	374215.908988	39.251738
2713.782062	374726.256174	39.256756
2716.614679	375249.085770	39.261773
2719.449194	375754.706251	39.266791
2722.568700	376278.593484	39.271808
2724.932388	376791.760103	39.276826
2727.814443	377312.880598	39.281844
2730.316201	377839.813596	39.286861
2733.246954	378357.639867	39.291879
2736.225310	378880.018359	39.296896
2738.498604	379399.381095	39.301914
2742.007704	379921.839198	39.306932
2744.591030	380447.405019	39.311949
2746.974887	380972.107375	39.316967
2750.080992	381493.517177	39.321984
2752.857165	382027.833563	39.327002
2755.755719	382557.607665	39.332020
2758.643088	383083.089090	39.337037
2761.397459	383603.028937	39.342055
2764.777876	384126.210789	39.347072
2767.906280	384633.977321	39.352090
2771.205369	385136.256264	39.357108
2774.121754	385646.579045	39.362125
2776.873340	386144.897855	39.367143
2779.405880	386646.212224	39.372160
2782.141592	387150.556600	39.377178
2784.752522	387655.700004	39.382196
2787.403784	388175.794442	39.387213
2790.316510	388670.273876	39.392231
2793.381663	389183.186478	39.397248
2795.392203	389684.135427	39.402266
2797.988218	390169.615161	39.407284
2800.736284	390645.832463	39.412301
2803.253987	391128.318702	39.417319
2806.022367	391610.986853	39.422336
2808.511787	392101.326069	39.427354
2811.310846	392590.442760	39.432372
2813.628724	393099.079832	39.437389
2816.224683	393610.987472	39.442407
2819.005356	394122.579272	39.447424
2821.283047	394630.160266	39.452442
2824.168122	395148.922034	39.457460
2826.896343	395684.994884	39.462477
2829.607684	396218.475396	39.467495
2832.644125	396748.751653	39.472512
2835.486191	397286.606603	39.477530
2838.687304	397813.822373	39.482548
2841.192251	398365.202833	39.487565
2843.979789	398908.719805	39.492583
2846.753782	399463.436905	39.497600
2849.570710	400022.295963	39.502618
2852.487057	400567.565122	39.507636
2855.153774	401133.097009	39.512653
2858.120835	401710.411469	39.517671
2861.016942	402272.210758	39.522688
2863.410768	402854.463100	39.527706
2866.105399	403427.707888	39.532724
2869.085948	404016.412195	39.537741
2871.764889	404605.457459	39.542759
2875.143005	405196.409023	39.547776
2877.998142	405796.406135	39.552794
2880.747605	406383.834963	39.557812
2883.892927	406977.907496	39.562829
2887.010094	407573.291153	39.567847
2890.055926	408175.087622	39.572864
2892.791699	408764.830460	39.577882
2896.058503	409360.687845	39.582900
2899.055040	409957.716869	39.587917
2901.989591	410554.515747	39.592935
2904.983379	411147.136670	39.597952
2908.008114	411751.425045	39.602970
2910.915706	412340.386151	39.607988
2913.634791	412945.458900	39.613005
2916.641850	413537.269603	39.618023
2919.944075	414136.371138	39.623040
2922.560980	414743.222312	39.628058
2925.848887	415331.581609	39.633076
2928.706607	415933.909542	39.638093
2931.315024	416540.090834	39.643111
2934.576911	417133.663030	39.648128
2937.548330	417740.040199	39.653146
2940.528911	418336.419263	39.658164
2943.629439	418932.209327	39.663181
2946.742303	419531.430866	39.668199
2949.635280	420125.733550	39.673216
2952.782555	420708.885634	39.678234
2955.906377	421262.942626	39.683252
2958.364387	421819.424870	39.688269
2961.271665	422367.337328	39.693287
2964.697438	422907.454903	39.698304
2967.639831	423450.171821	39.703322
2970.672198	423994.991800	39.708340
2973.675793	424550.825605	39.713357
2976.422835	425100.000656	39.718375
2979.479288	425653.928793	39.723392
2982.032125	426213.346323	39.728410
2985.081940	426775.029378	39.733428
2987.878140	427347.582476	39.738445
2990.956003	427907.236093	39.743463
2993.560542	428476.096947	39.748480
2996.457877	429063.617694	39.753498
2999.310639	429648.346203	39.758516
3002.320820	430236.152146	39.763533
3004.649105	430844.112346	39.768551
3008.015859	431439.002486	39.773568
3010.562631	432036.212145	39.778586
3013.443929	432664.379362	39.783604
3016.468857	433278.807498	39.788621
3018.993779	433905.000045	39.793639
3022.406073	434536.532131	39.798656
3025.475493	435179.498334	39.803674
3028.226299	435809.685274	39.808692
3031.757305	436435.352258	39.813709
3034.665176	437084.423402	39.818727
3037.749948	437720.333485	39.823744
3040.715982	438374.603292	39.828762
3043.991435	439011.209780	39.833780
3046.972594	439657.898042	39.838797
3050.013724	440311.345108	39.843815
3053.639003	440961.846753	39.848832
3056.859321	441627.787804	39.853850
3059.839809	442268.432369	39.858868
3063.097180	442916.863989	39.863885
3065.942045	443561.900630	39.868903
3069.106582	444222.260386	39.873920
3072.167047	444879.985788	39.878938
3075.273571	445524.674995	39.883956
3078.509656	446186.487787	39.888973
3081.677506	446849.254690	39.893991
3085.115172	447496.622004	39.899008
3088.242710	448155.916208	39.904026
3091.084003	448814.832162	39.909044
3094.329259	449464.655729	39.914061
3097.243182	450115.070291	39.919079
3100.529363	450767.330993	39.924096
3103.654138	451437.718118	39.929114
3106.669098	452090.844585	39.934132
3110.079078	452751.025873	39.939149
3112.933763	453409.960052	39.944167
3115.963616	454059.130853	39.949184
3119.587698	454712.541060	39.954202
3122.368641	455337.525036	39.959220
3125.315707	455940.655582	39.964237
3128.026571	456571.941529	39.969255
3131.265119	457187.490764	39.974272
3134.301281	457803.257342	39.979290
3137.060257	458422.390036	39.984308
3140.450971	459045.706029	39.989325
3143.018400	459682.693806	39.994343
3146.041058	460315.594220	39.999360
3149.237970	460964.739061	40.004378
3152.023961	461625.312189	40.009396
3155.153655	462262.590875	40.014413
3158.229158	462938.659219	40.019431
3161.505964	463603.242271	40.024448
3164.316802	464275.718849	40.029466
3167.456806	464945.087274	40.034484
3170.893067	465622.834668	40.039501
3173.424769	466340.154712	40.044519
3176.397240	467028.855378	40.049536
3179.410656	467734.975446	40.054554
3182.355218	468447.303149	40.059572
3185.918268	469155.260706	40.064589
3188.781217	469895.770792	40.069607
3191.848050	470618.422212	40.074624
3194.984855	471345.385977	40.079642
3198.218344	472076.505614	40.084660
3201.805222	472808.908462	40.089677
3204.670383	473556.112402	40.094695
3208.008423	474308.725024	40.099712
3211.417359	475050.428693	40.104730
3214.675128	475814.727201	40.109748
3218.053967	476560.121119	40.114765
3220.908904	477312.091291	40.119783
3224.418024	478061.301079	40.124800
3227.824242	478814.138326	40.129818
3231.182782	479589.598944	40.134836
3234.677106	480340.898266	40.139853
3238.250327	481099.434394	40.144871
3241.595109	481852.721117	40.149888
3244.886881	482603.308621	40.154906
3248.154078	483364.180336	40.159924
3251.587188	484111.958158	40.164941
3254.623377	484877.860190	40.169959
3257.870401	485624.345394	40.174976
3261.047792	486394.560632	40.179994
3264.074432	487166.486490	40.185012
3267.352094	487920.506382	40.190029
3270.353588	488691.717335	40.195047
3273.932895	489460.936151	40.200064
3277.280210	490235.868663	40.205082
3280.528723	491015.078547	40.210100
3284.035702	491774.615792	40.215117
3287.391572	492548.996242	40.220135
3290.787245	493321.822738	40.225152
3294.081546	494071.298584	40.230170
3297.095241	494804.273064	40.235188
3300.576202	495519.518722	40.240205
3303.752686	496234.885515	40.245223
3306.956485	496963.198175	40.250240
3309.971253	497679.291164	40.255258
3313.039581	498403.224574	40.260276
3316.456344	499137.020955	40.265293
3319.276629	499887.190278	40.270311
3322.253271	500634.425572	40.275328
3325.556949	501393.088837	40.280346
3328.536734	502150.306885	40.285364
3331.642077	502914.085914	40.290381
3335.045062	503687.224639	40.295399
3338.040964	504453.175399	40.300416
3341.723875	505258.910386	40.305434
3344.997542	506041.808467	40.310452
3348.183161	506832.154990	40.315469
3351.401898	507634.875595	40.320487
3354.956692	508430.440485	40.325504
3357.913660	509250.487773	40.330522
3361.334611	510070.069291	40.335540
3365.161949	510870.574595	40.340557
3368.924799	511693.303968	40.345575
3372.279067	512512.879443	40.350592
3376.106263	513317.911180	40.355610
3379.258954	514136.733396	40.360628
3382.814538	514953.181890	40.365645
3386.374951	515780.132726	40.370663
3389.799402	516586.836771	40.375680
3393.157125	517410.913907	40.380698
3396.418688	518233.250391	40.385716
3400.154042	519055.622312	40.390733
3403.749558	519894.516948	40.395751
3406.988466	520714.413107	40.400768
3410.837156	521533.667446	40.405786
3414.116608	522364.971557	40.410804
3417.765968	523190.426504	40.415821
3421.436146	524003.432866	40.420839
3425.174504	524817.395757	40.425856
3429.038830	525636.238062	40.430874
3432.694688	526441.813162	40.435892
3436.893158	527224.124004	40.440909
3440.265976	528030.520423	40.445927
3443.968848	528836.672419	40.450944
3447.635415	529610.935245	40.455962
3450.970858	530405.019160	40.460980
3454.572977	531188.286288	40.465997
3457.958194	531978.553243	40.471015
3461.328356	532753.917056	40.476032
3464.851718	533544.032318	40.481050
3468.373100	534324.685359	40.486068
3472.005895	535106.440162	40.491085
3475.539471	535883.132833	40.496103
3478.713789	536666.946384	40.501120
3482.309771	537419.207092	40.506125
3485.741918	538140.465533	40.511130
3489.024038	538807.930633	40.516135
3491.818567	539413.229524	40.521140
3495.028387	539968.699545	40.526144
3497.595517	540450.174812	40.531149
3499.808762	540892.709730	40.536154
3502.278837	541267.632624	40.541159
3504.747481	541591.954377	40.546164
3506.252540	541863.558268	40.551168
3508.311392	542086.196003	40.556173
3510.116688	542280.445337	40.561178
3511.638064	542403.700043	40.566183
3513.250922	542508.612133	40.571188
3514.280410	542552.273044	40.576192
3515.831006	542558.540990	40.581197
3517.018122	542547.246119	40.586202
3517.825333	542496.428695	40.591207
3518.660718	542417.484676	40.596212
3519.056932	542314.122666	40.601216
3519.811360	542191.719443	40.606221
3520.355775	542047.032041	40.611226
3520.980787	541885.921228	40.616231
3521.664351	541696.221695	40.621236
3521.953956	541496.180803	40.626240
3522.659490	541277.944841	40.631245
3522.616035	541063.257607	40.636250
3522.761564	540806.526713	40.641255
3523.066264	540558.299875	40.646260
3523.109947	540294.810094	40.651264
3523.156925	540030.759735	40.656269
3523.413426	539759.046570	40.661274
3523.295451	539486.074760	40.666279
3523.149125	539199.417262	40.671284
3523.234564	538915.697218	40.676288
3523.382415	538614.943166	40.681293
3522.974524	538336.643389	40.686298
3523.024858	538042.509188	40.691303
3523.163129	537736.335473	40.696308
3522.982283	537440.913101	40.701312
3522.571063	537133.804047	40.706317
3522.329947	536838.884619	40.711322
3522.292556	536541.603948	40.716327
3522.217517	536252.000809	40.721332
3522.006663	535959.332571	40.726336
3522.206992	535650.581842	40.731341
3521.565255	535359.233049	40.736346
3521.294275	535058.626819	40.741351
3521.646692	534763.725281	40.746356
3520.913514	534484.043066	40.751360
3521.167755	534195.814136	40.756365
3520.907716	533920.088185	40.761370
3520.441277	533629.588340	40.766375
3520.345916	533342.308097	40.771380
3519.996658	533068.551318	40.776384
3520.156880	532782.281227	40.781389
3519.573623	532527.345407	40.786394
3519.240107	532262.968871	40.791399
3519.021707	531988.717718	40.796404
3518.737815	531716.240425	40.801408
3518.785989	531462.096819	40.806413
3518.501864	531216.237225	40.811418
3518.064741	530944.629636	40.816423
3517.935143	530709.550259	40.821428
3517.510440	530467.541181	40.826432
3517.612794	530215.794131	40.831437
3517.142081	529985.911739	40.836442
3516.943888	529748.453948	40.841447
3516.938385	529521.219862	40.846452
3516.624453	529286.047277	40.851456
3516.432116	529061.867991	40.856461
3516.331284	528836.054007	40.861466
3516.123501	528607.120615	40.866471
3515.938511	528406.934345	40.871476
3515.565045	528191.412708	40.876480
3515.935234	527976.831851	40.881485
3515.315893	527773.775166	40.886490
3515.140654	527558.820038	40.891495
3515.054455	527358.301698	40.896500
3514.752524	527159.381613	40.901504
3514.936513	526956.389668	40.906509
3514.232941	526763.896022	40.911514
3514.497031	526575.593559	40.916519
3514.057183	526389.472304	40.921524
3513.637506	526203.800561	40.926528
3513.703919	526015.371112	40.931533
3513.568436	525842.386803	40.936538
3513.155099	525673.690150	40.941543
3513.310981	525495.247940	40.946548
3513.179803	525320.488290	40.951552
3513.008504	525154.628929	40.956557
3512.953615	524994.006146	40.961562
3512.570513	524818.421579	40.966567
3512.565363	524655.209719	40.971572
3512.262742	524500.383419	40.976576
3512.349807	524339.832758	40.981581
3512.242253	524178.957422	40.986586
3512.048223	524035.836547	40.991591
3512.115652	523876.244785	40.996596
3511.471201	523736.275907	41.001600
3511.666869	523584.243344	41.006605
3511.114715	523444.914495	41.011610
3511.117652	523289.067821	41.016615
3511.389163	523160.070272	41.021620
3510.779158	523022.971168	41.026624
3510.957423	522890.346516	41.031629
3510.519724	522762.064512	41.036634
3510.420066	522623.718665	41.041639
3510.347637	522497.904464	41.046644
3510.383442	522376.419764	41.051648
3510.500893	522259.369974	41.056653
3510.169595	522142.946363	41.061658
3510.134241	522016.010380	41.066663
3510.162671	521901.904243	41.071668
3509.741021	521783.166815	41.076672
3509.708008	521674.832082	41.081677
3509.561790	521558.627812	41.086682
3509.747226	521452.784867	41.091687
3509.656595	521337.783584	41.096692
3509.292649	521238.244531	41.101696
3509.355323	521114.016093	41.106701
3509.227484	521024.701531	41.111706
3509.413752	520902.727038	41.116711
3509.649902	520802.938807	41.121716
3509.121144	520712.978094	41.126720
3509.020664	520592.967834	41.131725
3508.954374	520491.708742	41.136730
3508.965376	520396.099465	41.141735
3509.081756	520287.630797	41.146740
3508.793905	520193.028206	41.151744
3508.716189	520090.099954	41.156749
3508.637660	520005.170785	41.161754
3508.223599	519909.120244	41.166759
3508.445054	519816.406856	41.171764
3508.220446	519736.403822	41.176768
3508.564010	519651.355545	41.181773
3508.155979	519551.863761	41.186778
3507.949418	519474.890322	41.191783
3508.138602	519378.235705	41.196788
3507.654850	519300.142320	41.201792
3507.604913	519218.086640	41.206797
3507.766097	519142.974919	41.211802
3507.903031	519055.883127	41.216807
3507.731517	518981.177198	41.221812
3507.889065	518903.031130	41.226816
3507.786628	518831.549702	41.231821
3507.660825	518735.042224	41.236826
3507.594208	518674.779781	41.241831
3507.925665	518594.784434	41.246836
3507.415031	518519.776059	41.251840
3507.677674	518453.241242	41.256845
3507.035755	518381.944266	41.261850
3507.151869	518311.841879	41.266855
3507.403744	518232.514712	41.271860
3506.770595	518179.570955	41.276864
3507.298536	518096.103632	41.281869
3507.294495	518034.362532	41.286874
3507.477900	517969.557561	41.291879
3507.396825	517885.325797	41.296884
3507.164485	517818.310424	41.301888
3507.174061	517758.083162	41.306893
3506.944767	517686.768533	41.311898
3506.766312	517628.593229	41.316903
3506.859767	517559.603732	41.321908
3506.653271	517501.836960	41.326912
3506.735687	517438.815766	41.331917
3506.706398	517380.211466	41.336922
3506.570171	517322.281256	41.341927
3506.898409	517261.394995	41.346932
3506.662285	517203.277882	41.351936
3506.446720	517147.230662	41.356941
3506.863353	517085.925232	41.361946
3506.499343	517043.453769	41.366951
3506.606133	516964.699732	41.371956
3506.643056	516923.782831	41.376960
3506.686160	516856.416612	41.381965
3506.717722	516805.588487	41.386970
3506.439923	516743.228433	41.391975
3506.408579	516682.042891	41.396980
3506.239308	516635.898506	41.401984
3506.408386	516565.274655	41.406989
3506.332632	516522.655156	41.411994
3506.073275	516467.472277	41.416999
3506.678622	516404.971366	41.422004
3506.061675	516367.039030	41.427008
3506.315470	516321.180905	41.432013
3506.349521	516267.215284	41.437018
3506.144854	516213.641225	41.442023
3506.482285	516159.071008	41.447028
3506.296979	516115.709197	41.452032
3506.325733	516045.408757	41.457037
3506.300107	516001.819121	41.462042
3506.114801	515957.192576	41.467047
3506.195589	515890.625662	41.472052
3506.304254	515840.035271	41.477056
3506.365060	515798.049789	41.482061
3506.229718	515745.424165	41.487066
3506.113352	515686.827664	41.492071
3506.078517	515636.309911	41.497076
3505.849026	515609.592603	41.502080
3506.099191	515553.415830	41.507085
3505.996446	515503.919896	41.512090
3505.490781	515458.735761	41.517095
3505.861224	515404.764756	41.522100
3505.877743	515364.707024	41.527104
3505.811631	515322.032359	41.532109
3506.385704	515274.957517	41.537114
3505.908795	515222.586534	41.542119
3505.916042	515182.024077	41.547124
3505.884752	515133.729562	41.552128
3506.225724	515091.192267	41.557133
3506.090639	515045.139230	41.562138
3505.773704	514995.574495	41.567143
3505.818160	514946.407676	41.572148
3505.849951	514909.785614	41.577152
3506.041254	514857.054989	41.582157
3506.013841	514824.083594	41.587162
3505.865402	514782.128636	41.592167
3505.831919	514725.134117	41.597172
3505.749500	514690.400967	41.602176
3505.573325	514639.851971	41.607181
3505.613771	514604.037105	41.612186
3505.857289	514551.600730	41.617191
3505.848193	514513.972722	41.622196
3505.932080	514470.867561	41.627200
3505.850246	514422.275521	41.632205
3505.756193	514374.797982	41.637210
3505.835051	514331.086325	41.642215
3506.100271	514292.908683	41.647220
3505.718423	514251.849118	41.652224
3505.724404	514199.600925	41.657229
3505.713069	514161.567854	41.662234
3505.571271	514131.698464	41.667239
3505.700877	514091.771552	41.672244
3505.380419	514039.321564	41.677248
3505.319898	514010.956476	41.682253
3505.554798	513977.587906	41.687258
3505.704208	513935.179122	41.692263
3505.807137	513899.605776	41.697268
3505.341553	513862.351936	41.702272
3505.619148	513817.444207	41.707277
3505.866732	513774.665445	41.712282
3505.554318	513735.970886	41.717287
3505.618888	513696.508535	41.722292
3505.540903	513656.006444	41.727296
3505.771532	513616.770558	41.732301
3505.515296	513568.254196	41.737306
3505.519258	513532.038173	41.742311
3505.841603	513491.775894	41.747316
3505.566481	513458.588072	41.752320
3505.253022	513414.834884	41.757325
3505.656010	513378.302558	41.762330
3505.264804	513342.249749	41.767335
3505.372959	513299.390658	41.772340
3505.487404	513257.440926	41.777344
3505.609458	513232.434607	41.782349
3505.590309	513182.513968	41.787354
3505.403969	513141.673699	41.792359
3505.669107	513106.781183	41.797364
3505.349722	513070.109460	41.802368
3505.539940	513033.255947	41.807373
3505.708478	512989.071398	41.812378
3505.417239	512961.954980	41.817383
3505.591872	512909.170309	41.822388
3505.296593	512870.774549	41.827392
3505.231748	512844.532640	41.832397
3505.256181	512802.292511	41.837402
3504.917959	512778.976913	41.842407
3505.224714	512731.330227	41.847412
3504.985701	512708.605844	41.852416
3504.874186	512677.464520	41.857421
3504.949598	512654.791532	41.862426
3504.839749	512632.198380	41.867431
3505.113750	512598.112743	41.872436
3505.280710	512572.137271	41.877440
3505.019705	512532.116661	41.882445
3504.816541	512501.900000	41.887450
3504.716903	512469.845915	41.892455
3505.358179	512440.203841	41.897460
3504.883280	512421.815961	41.902464
3504.970408	512388.669946	41.907469
3505.306631	512358.064270	41.912474
3505.062288	512330.130084	41.917479
3505.039991	512297.001185	41.922484
3504.941038	512264.541931	41.927488
3505.083403	512229.009419	41.932493
3505.335554	512200.187195	41.937498
3505.019921	512176.816612	41.942503
3505.419898	512134.717797	41.947508
3505.045582	512107.562555	41.952512
3505.064435	512079.788693	41.957517
3505.214332	512038.538523	41.962522
3504.969015	511999.424701	41.967527
3505.192235	511977.739144	41.972532
3504.925391	511952.893575	41.977536
3505.318548	511919.546518	41.982541
3505.245589	511884.401414	41.987546
3505.008833	511858.893344	41.992551
3505.264676	511810.240413	41.997556
3505.252135	511794.915071	42.002560
3505.190394	511758.907981	42.007565
3505.068739	511726.046600	42.012570
3505.100420	511692.756233	42.017575
3504.897371	511674.071642	42.022580
3504.961722	511645.379333	42.027584
3505.252796	511610.732570	42.032589
3505.146799	511569.015846	42.037594
3505.039307	511547.280840	42.042599
3505.240976	511504.149498	42.047604
3505.294266	511471.968183	42.052608
3504.957801	511445.362349	42.057613
3505.093876	511410.183225	42.062618
3505.044158	511377.158039	42.067623
3505.184371	511348.048544	42.072628
3504.978487	511320.056028	42.077632
3504.689004	511283.325124	42.082637
3505.384164	511255.240670	42.087642
3504.840625	511240.251693	42.092647
3505.068640	511202.123551	42.097652
3504.881343	511175.392542	42.102656
3504.639554	511156.561744	42.107661
3504.923264	511129.907978	42.112666
3504.801450	511113.739306	42.117671
3505.057923	511072.672299	42.122676
3504.553681	511044.018260	42.127680
3504.939075	511029.388147	42.132685
3505.027698	510993.659198	42.137690
3504.719942	510964.366914	42.142695
3504.885561	510947.697361	42.147700
3504.817836	510917.911765	42.152704
3504.731593	510890.557278	42.157709
3504.984336	510859.253869	42.162714
3504.877460	510828.361362	42.167719
3505.115937	510798.425983	42.172724
3505.174258	510768.114318	42.177728
3505.039341	510738.895504	42.182733
3505.045088	510707.883800	42.187738
3504.706894	510676.622871	42.192743
3504.685571	510650.876582	42.197748
3505.060622	510628.507654	42.202752
3505.019325	510597.907899	42.207757
3505.084980	510568.505324	42.212762
3505.129358	510534.957742	42.217767
3504.766046	510500.310978	42.222772
3504.977799	510483.026608	42.227776
3504.652461	510453.483277	42.232781
3505.141430	510433.777333	42.237786
3504.872334	510407.918072	42.242791
3504.964233	510377.347458	42.247796
3504.974160	510353.922910	42.252800
3505.023640	510314.859800	42.257805
3504.810888	510295.062251	42.262810
3504.644565	510265.341691	42.267815
3504.705643	510235.281596	42.272820
3504.421276	510202.190043	42.277824
3504.509041	510193.070006	42.282829
3504.897667	510157.089528	42.287834
3504.627823	510136.794916	42.292839
3504.864458	510119.455655	42.297844
3504.834283	510098.263076	42.302848
3504.922548	510062.127512	42.307853
3504.738696	510040.301473	42.312858
3504.804479	510016.715862	42.317863
3505.003363	509986.026457	42.322868
3504.448134	509969.773434	42.327872
3504.644838	509938.274834	42.332877
3504.818571	509906.779806	42.337882
3504.554310	509895.742198	42.342887
3504.793732	509869.751155	42.347892
3504.503597	509844.450870	42.352896
3504.434874	509823.769958	42.357901
3504.374677	509794.284762	42.362906
3504.281250	509783.827177	42.367911
3504.865024	509746.701979	42.372916
3504.614959	509745.476797	42.377920
3504.550311	509722.417313	42.382925
3504.780579	509696.376863	42.387930
3504.586012	509677.182825	42.392935
3504.425185	509666.027536	42.397940
3504.809588	509639.608494	42.402944
3504.439796	509624.590629	42.407949
3504.449760	509586.240391	42.412954
3504.316004	509571.083988	42.417959
3504.611560	509554.949054	42.422964
3504.289077	509532.790135	42.427968
3504.433030	509519.208742	42.432973
3504.474278	509489.454026	42.437978
3504.269818	509482.403495	42.442983
3504.312243	509449.916536	42.447988
3504.475295	509424.796962	42.452992
3504.616389	509406.055491	42.457997
3504.712079	509391.570959	42.463002
3504.496466	509380.221773	42.468007
3504.889860	509336.700511	42.473012
3504.863214	509324.714306	42.478016
3504.519144	509294.767192	42.483021
3504.819710	509272.307085	42.488026
3504.712164	509253.503562	42.493031
3504.488675	509216.757783	42.498036
3504.649943	509201.301455	42.503040
3504.607297	509178.440135	42.508045
3504.624607	509148.890985	42.513050
3504.289057	509142.417561	42.518055
3504.662890	509103.856952	42.523060
3504.608430	509094.151689	42.528064
3504.441399	509062.658382	42.533069
3504.831896	509050.100115	42.538074
3504.830686	509016.657955	42.543079
3504.674751	508994.927359	42.548084
3504.858586	508972.485312	42.553088
3504.589013	508958.108742	42.558093
3504.398409	508917.410799	42.563098
3504.448879	508913.861321	42.568103
3504.675939	508888.882629	42.573108
3504.423506	508871.315848	42.578112
3504.341928	508845.121022	42.583117
3504.665850	508829.031520	42.588122
3504.618745	508807.232891	42.593127
3504.607540	508782.291706	42.598132
3504.665594	508747.321822	42.603136
3504.394845	508735.677356	42.608141
3504.699731	508720.906221	42.613146
3504.527769	508700.999194	42.618151
3504.917323	508667.089832	42.623156
3504.802345	508652.587381	42.628160
3504.702400	508630.493312	42.633165
3504.995927	508587.694271	42.638170
3504.875476	508566.615261	42.643175
3504.750987	508532.989266	42.648180
3504.677297	508516.355178	42.653184
3504.676839	508506.135096	42.658189
3504.979680	508466.622973	42.663194
3504.647876	508442.136732	42.668199
3504.764929	508416.162835	42.673204
3504.849196	508385.134522	42.678208
3504.530118	508375.217702	42.683213
3505.125686	508337.935819	42.688218
3504.574581	508323.350238	42.693223
3504.651887	508283.569770	42.698228
3504.890551	508265.368191	42.703232
3504.776658	508243.528810	42.708237
3504.516734	508230.667987	42.713242
3504.296582	508201.205341	42.718247
3504.491420	508185.186239	42.723252
3504.748734	508161.820792	42.728256
3504.470919	508147.596635	42.733261
3504.578680	508111.656275	42.738266
3504.506520	508097.450168	42.743271
3504.583498	508078.413809	42.748276
3504.483535	508045.592531	42.753280
3504.682666	508032.557808	42.758285
3504.661607	508012.423746	42.763290
3504.521854	507994.332292	42.768295
3504.320614	507966.586546	42.773300
3504.926302	507947.820653	42.778304
3504.757723	507929.430105	42.783309
3504.698413	507895.438386	42.788314
3504.631930	507871.364771	42.793319
3504.655675	507849.148955	42.798324
3504.482953	507829.443429	42.803329
3504.336909	507800.322566	42.808333
3504.622803	507764.656913	42.813338
3504.407154	507766.967965	42.818343
3504.076130	507740.355512	42.823348
3504.423631	507723.654085	42.828353
3504.378500	507708.988008	42.833357
3504.764414	507683.122306	42.838362
3504.340260	507675.498585	42.843367
3504.355372	507638.205747	42.848372
3504.490414	507629.582858	42.853377
3504.510916	507600.890715	42.858381
3504.678481	507581.586502	42.863386
3504.431210	507555.567701	42.868391
3504.596863	507543.904049	42.873396
3504.710760	507519.548442	42.878401
3504.147064	507512.655079	42.883405
3504.356341	507486.462816	42.888410
3504.253106	507462.394439	42.893415
3504.392066	507458.274094	42.898420
3504.303476	507443.968850	42.903425
3504.532632	507414.231450	42.908429
3504.754579	507384.343343	42.913434
3504.621689	507381.480314	42.918439
3504.454855	507353.171561	42.923444
3504.827571	507325.789453	42.928449
3504.543181	507305.392598	42.933453
3504.358171	507274.253058	42.938458
3504.067438	507267.265852	42.943463
3504.275480	507248.005468	42.948468
3504.345433	507226.641732	42.953473
3504.491215	507216.296574	42.958477
3504.552404	507186.382937	42.963482
3504.314434	507171.898682	42.968487
3504.279860	507150.095981	42.973492
3504.520962	507129.464062	42.978497
3504.248748	507126.370015	42.983501
3504.268581	507091.099225	42.988506
3504.381562	507081.416964	42.993511
3504.416942	507054.543143	42.998516
3504.602666	507036.196843	43.003521
3504.418788	507024.537490	43.008525
3504.388988	506981.583184	43.013530
3504.287799	506988.582018	43.018535
3504.061017	506953.349929	43.023540
3504.631503	506935.398104	43.028545
3504.660395	506918.037865	43.033549
3504.713852	506897.941329	43.038554
3504.732803	506877.293624	43.043559
3504.682149	506845.373076	43.048564
3504.407843	506830.894280	43.053569
3504.390469	506809.290832	43.058573
3504.668624	506790.727262	43.063578
3504.766052	506779.934086	43.068583
3504.420598	506765.061677	43.073588
3504.408841	506727.669928	43.078593
3504.640697	506706.178760	43.083597
3504.446183	506679.947903	43.088602
3504.371903	506664.526540	43.093607
3504.576286	506646.379282	43.098612
3504.762786	506620.847123	43.103617
3504.155616	506613.707265	43.108621
3504.536524	506580.554199	43.113626
3504.503798	506562.596134	43.118631
3504.238499	506552.821567	43.123636
3504.457463	506520.807206	43.128641
3504.551618	506512.443231	43.133645
3504.682962	506482.213685	43.138650
3504.309054	506477.870567	43.143655
3504.100475	506450.174152	43.148660
3504.492359	506420.004519	43.153665
3504.321188	506415.983549	43.158669
3504.577752	506396.916959	43.163674
3504.566594	506388.670773	43.168679
3504.556190	506348.596118	43.173684
3504.777481	506333.937369	43.178689
3504.556482	506306.394492	43.183693
3504.848460	506280.490950	43.188698
3504.314291	506257.652857	43.193703
3504.490844	506242.444482	43.198708
3504.432458	506224.135910	43.203713
3504.024709	506197.988632	43.208717
3504.646805	506179.977271	43.213722
3504.536231	506158.488951	43.218727
3504.303416	506146.634334	43.223732
3504.587481	506108.992088	43.228737
3504.454440	506099.398769	43.233741
3504.768485	506072.327577	43.238746
3504.453604	506055.425634	43.243751
3504.563936	506040.581767	43.248756
3504.692829	506029.884357	43.253761
3504.121960	506007.608362	43.258765
3504.342704	505975.744526	43.263770
3504.182299	505963.321710	43.268775
3504.210031	505950.565531	43.273780
3504.555524	505922.983110	43.278785
3504.350617	505914.716721	43.283789
3504.419618	505890.365928	43.288794
3504.138433	505879.986258	43.293799
3503.968831	505859.670766	43.298804
3504.322251	505833.048406	43.303809
3504.002788	505834.161647	43.308813
3504.187710	505818.293740	43.313818
3504.546334	505796.123573	43.318823
3504.311657	505781.081002	43.323828
3504.376038	505753.289730	43.328833
3504.081948	505739.369786	43.333837
3504.288705	505729.014108	43.338842
3504.060076	505719.992326	43.343847
3503.931635	505691.725400	43.348852
3504.232745	505685.200644	43.353857
3504.232338	505675.535524	43.358861
3504.450383	505636.688211	43.363866
3504.332012	505641.564950	43.368871
3504.223107	505607.424780	43.373876
3504.281923	505608.630055	43.378881
3504.150152	505595.848225	43.383885
3504.255226	505559.548782	43.388890
3504.328640	505548.758639	43.393895
3504.214870	505538.757135	43.398900
3504.254535	505505.706569	43.403905
3504.023109	505497.444173	43.408909
3504.233038	505481.015363	43.413914
3504.161774	505465.137025	43.418919
3503.964217	505448.266551	43.423924
3504.104404	505447.029976	43.428929
3504.014179	505432.672730	43.433933
3504.300409	505405.351880	43.438938
3504.212358	505401.621162	43.443943
3504.297356	505385.616844	43.448948
3504.431459	505360.698375	43.453953
3504.117324	505353.106841	43.458957
3504.372566	505329.080059	43.463962
3504.222552	505311.038034	43.468967
3504.194766	505309.321953	43.473972
3504.194132	505292.723830	43.478977
3504.181481	505288.323310	43.483981
3504.495537	505279.266127	43.488986
3504.172946	505251.585827	43.493991
3503.806095	505225.481228	43.498996
3504.347711	505214.566269	43.504001
3504.089740	505204.131922	43.509005
3504.315773	505182.285564	43.514010
3504.352753	505176.713258	43.519015
3503.854940	505151.944978	43.524020
3504.031817	505130.865401	43.529025
3503.635111	505133.863282	43.534029
3504.151785	505120.877399	43.539034
3504.018400	505092.509074	43.544039
3504.068208	505076.358220	43.549044
3504.153752	505075.029045	43.554049
3503.963780	505064.381445	43.559053
3503.818962	505045.427429	43.564058
3504.130453	505035.510235	43.569063
3503.950673	505032.198780	43.574068
3504.226905	505009.585192	43.579073
3503.882184	505003.415292	43.584077
3504.137595	504994.316626	43.589082
3504.032764	504994.181462	43.594087
3503.922074	504968.440833	43.599092
3504.244755	504944.099230	43.604097
3504.179409	504952.155933	43.609101
3503.868096	504929.533899	43.614106
3504.308926	504904.920539	43.619111
3504.108214	504897.260273	43.624116
3504.437772	504892.552534	43.629121
3504.157339	504867.749491	43.634125
3504.230192	504849.266916	43.639130
3503.901368	504850.331091	43.644135
3504.165246	504823.974380	43.649140
3504.486851	504807.274257	43.654145
3504.311012	504797.990623	43.659149
3504.331552	504778.099272	43.664154
3504.474979	504769.423039	43.669159
3504.425456	504744.330292	43.674164
3504.342096	504720.204377	43.679169
3504.179506	504716.788932	43.684173
3504.431548	504684.006883	43.689178
3504.187376	504674.177315	43.694183
3504.243241	504659.290279	43.699188
3504.470174	504627.220583	43.704193
3504.360357	504625.466794	43.709197
3504.326786	504593.286392	43.714202
3504.226757	504585.559469	43.719207
3504.277686	504574.671066	43.724212
3504.061602	504547.276457	43.729217
3503.906087	504542.948937	43.734221
3504.234031	504525.184802	43.739226
3504.248651	504513.947854	43.744231
3504.060809	504499.757092	43.749236
3504.267917	504493.297361	43.754241
3503.977186	504471.126943	43.759245
3503.957240	504445.826666	43.764250
3503.838084	504438.608771	43.769255
3503.734983	504441.864003	43.774260
3504.017180	504433.621133	43.779265
3503.580746	504408.234811	43.784269
3503.879456	504394.270702	43.789274
3504.081969	504389.076839	43.794279
3503.999825	504391.266016	43.799284
3504.187009	504369.121143	43.804289
3503.783185	504358.861166	43.809293
3503.723166	504350.621742	43.814298
3503.890974	504346.445498	43.819303
3504.076339	504339.078215	43.824308
3504.079747	504310.029105	43.829313
3503.938348	504300.132474	43.834317
3503.810621	504290.081853	43.839322
3504.197945	504281.366828	43.844327
3503.848506	504269.377546	43.849332
3504.116428	504255.873662	43.854337
3503.710449	504243.184792	43.859341
3504.029782	504232.456184	43.864346
3503.812531	504218.219235	43.869351
3503.754064	504198.137284	43.874356
3503.995534	504193.392676	43.879361
3503.515662	504198.073916	43.884365
3503.850856	504188.304321	43.889370
3503.845999	504187.596662	43.894375
3503.944027	504165.769273	43.899380
3504.195035	504149.737587	43.904385
3503.999570	504155.639082	43.909389
3504.190622	504138.705920	43.914394
3503.965369	504118.245377	43.919399
3503.931527	504110.204134	43.924404
3504.376426	504100.619583	43.929409
3504.043657	504081.086935	43.934413
3503.865672	504059.556082	43.939418
3504.354472	504049.256049	43.944423
3503.963511	504032.161739	43.949428
3504.266397	504016.931464	43.954433
3504.217763	504012.637528	43.959437
3504.316703	504003.664299	43.964442
3504.068729	503973.338550	43.969447
3504.175036	503958.898423	43.974452
3504.745684	503941.955681	43.979457
3504.238688	503929.839245	43.984461
3504.290092	503917.280278	43.989466
3504.389255	503886.140381	43.994471
3504.269757	503876.594310	43.999476
3504.206453	503851.502465	44.004481
3504.332798	503844.346739	44.009485
3504.214443	503827.057313	44.014490
3504.138261	503818.314105	44.019495
3504.255786	503810.603062	44.024500
3504.427971	503799.796232	44.029505
3504.253427	503783.173560	44.034509
3504.296762	503755.635492	44.039514
3504.380950	503739.275538	44.044519
3503.730072	503716.756220	44.049524
3504.102510	503704.652450	44.054529
3504.112737	503695.642477	44.059533
3504.356452	503675.157900	44.064538
3504.159273	503660.563061	44.069543
3503.996349	503651.327388	44.074548
3504.419373	503646.098452	44.079553
3504.114527	503619.374346	44.084557
3504.276621	503604.874502	44.089562
3504.463856	503583.285337	44.094567
3504.164749	503557.673640	44.099572
3504.508622	503547.092566	44.104577
3504.075105	503532.788026	44.109581
3504.194809	503511.968593	44.114586
3504.220070	503505.486634	44.119591
3503.924280	503486.554797	44.124596
3504.038604	503463.762375	44.129601
3504.115719	503458.436230	44.134605
3504.180055	503452.859053	44.139610
3504.304569	503427.281428	44.144615
3504.037247	503428.487793	44.149620
3504.300139	503404.254732	44.154625
3504.028530	503387.596418	44.159629
3504.311487	503369.028468	44.164634
3504.193701	503362.265405	44.169639
3504.043715	503342.601825	44.174644
3504.160093	503312.267956	44.179649
3504.055707	503323.165754	44.184653
3504.122704	503295.522007	44.189658
3504.125572	503279.629973	44.194663
3503.943237	503266.905046	44.199668
3503.961708	503260.272239	44.204673
3504.031496	503244.217764	44.209677
3504.088974	503232.264676	44.214682
3504.413860	503215.967411	44.219687
3504.128503	503197.995216	44.224692
3504.550973	503171.459133	44.229697
3504.071961	503168.194621	44.234701
3503.966712	503154.141550	44.239706
3504.224593	503133.704717	44.244711
3504.010018	503128.070301	44.249716
3504.345863	503109.088831	44.254721
3503.994787	503090.722027	44.259725
3503.904014	503081.626483	44.264730
3504.169380	503068.830649	44.269735
3503.817128	503055.727539	44.274740
3504.234896	503049.284594	44.279745
3504.147247	503046.211255	44.284749
3504.093650	503024.760696	44.289754
3503.919793	503007.732294	44.294759
3503.593067	502993.916547	44.299764
3504.210846	502988.757858	44.304769
3504.113658	502980.523667	44.309773
3504.176690	502963.002277	44.314778
3504.250864	502948.212123	44.319783
3503.633133	502945.070718	44.324788
3504.162022	502911.988557	44.329793
3503.884217	502900.290685	44.334797
3503.667788	502895.567495	44.339802
3504.062285	502897.175402	44.344807
3503.999669	502891.921784	44.349812
3504.196292	502863.700145	44.354817
3503.936596	502868.853047	44.359821
3504.191470	502850.440826	44.364826
3504.352829	502834.523340	44.369831
3504.060114	502821.056363	44.374836
3504.335954	502803.146897	44.379841
3504.246391	502773.553220	44.384845
3504.023096	502774.803281	44.389850
3504.292437	502761.044971	44.394855
3504.009377	502731.684256	44.399860
3504.177503	502732.720616	44.404865
3503.846826	502728.369723	44.409869
3504.210894	502700.475641	44.414874
3504.099272	502688.801974	44.419879
3503.838123	502671.483373	44.424884
3504.274901	502669.136870	44.429889
3504.416087	502637.279557	44.434893
3504.107085	502623.815004	44.439898
3504.611887	502615.839776	44.444903
3503.991566	502591.947654	44.449908
3504.261241	502572.621782	44.454913
3504.319137	502572.055977	44.459917
3504.116831	502548.148335	44.464922
3504.371588	502526.749658	44.469927
3503.860195	502526.678735	44.474932
3504.027007	502496.487333	44.479937
3504.117728	502491.108133	44.484941
3504.099072	502484.733966	44.489946
3504.370701	502454.222248	44.494951
3504.300626	502443.503495	44.499956
3504.329086	502426.796844	44.504961
3504.287501	502411.822088	44.509965
3504.164654	502394.380129	44.514970
3504.074249	502385.992749	44.519975
3504.063853	502364.888852	44.524980
3503.867236	502352.924720	44.529985
3504.118277	502348.228719	44.534989
3504.167084	502333.593901	44.539994
3504.340387	502319.192458	44.544999
3503.804881	502321.807841	44.550004
3504.278919	502306.346590	44.555009
3503.955885	502271.120296	44.560013
3504.138743	502258.691212	44.565018
3504.256468	502259.533114	44.570023
3504.062850	502243.974886	44.575028
3504.261878	502224.761029	44.580033
3504.218440	502215.758784	44.585037
3503.742905	502192.045688	44.590042
3503.943679	502175.564632	44.595047
3503.956562	502166.958368	44.600052
3504.122975	502163.945945	44.605057
3504.077957	502149.427032	44.610061
3503.839068	502125.271533	44.615066
3503.968127	502120.645367	44.620071
3504.114761	502117.231152	44.625076
3504.284447	502096.604609	44.630081
3504.063131	502073.660993	44.635085
3504.007715	502066.988803	44.640090
3504.347427	502057.014866	44.645095
3503.739838	502048.000479	44.650100
3504.215562	502020.492592	44.655105
3503.830103	502034.927976	44.660109
3503.859499	501997.823329	44.665114
3504.013649	501988.081140	44.670119
3503.611117	501981.565012	44.675124
3503.825481	501966.954337	44.680129
3503.920353	501970.786100	44.685133
3503.984396	501960.906296	44.690138
3503.859562	501942.047008	44.695143
3503.861762	501925.900793	44.700148
3503.830978	501917.655611	44.705153
3504.014529	501927.901382	44.710157
3503.709230	501908.513827	44.715162
3503.845137	501889.714499	44.720167
3503.906858	501890.312198	44.725172
3504.212875	501875.079588	44.730177
3503.944594	501866.669463	44.735181
3504.143347	501848.821833	44.740186
3503.828734	501832.472537	44.745191
3503.715769	501827.580862	44.750196
3504.226065	501820.768548	44.755201
3503.980628	501802.738008	44.760205
3504.043217	501786.835194	44.765210
3504.212836	501778.963189	44.770215
3504.101325	501773.767581	44.775220
3504.019656	501748.979342	44.780225
3504.067821	501740.063606	44.785229
3504.175790	501734.175303	44.790234
3504.102441	501705.640191	44.795239
3503.919724	501702.986564	44.800244
3503.909328	501688.208726	44.805249
3503.988990	501678.073221	44.810253
3503.817232	501670.204511	44.815258
3504.227664	501645.135885	44.820263
3504.183324	501647.623115	44.825268
3504.010312	501618.243159	44.830273
3504.098836	501605.119917	44.835277
3503.997030	501598.505498	44.840282
3504.332724	501586.709786	44.845287
3503.871808	501575.647362	44.850292
3504.178642	501544.622365	44.855297
3504.150498	501532.377971	44.860301
3503.806576	501517.095940	44.865306
3503.990445	501489.532133	44.870311
3503.785610	501487.489355	44.875316
3503.653828	501489.281811	44.880321
3503.647960	501488.523588	44.885325
3503.649993	501472.630065	44.890330
3503.895144	501455.027784	44.895335
3503.515408	501448.457240	44.900340
3503.930007	501440.799442	44.905345
3503.839828	501438.080532	44.910349
3503.775935	501443.304127	44.915354
3503.883235	501438.428145	44.920359
3503.636688	501405.313900	44.925364
3504.108853	501386.359658	44.930369
3503.776217	501395.421932	44.935373
3503.800426	501394.962646	44.940378
3504.027561	501382.829647	44.945383
3503.953035	501367.150594	44.950388
3503.788276	501349.309305	44.955393
3504.020539	501349.019596	44.960397
3503.813500	501351.583200	44.965402
3503.843957	501317.615152	44.970407
3503.922625	501311.832573	44.975412
3503.915237	501298.825497	44.980417
3503.873394	501294.681675	44.985421
3503.841750	501298.179269	44.990426
3504.135121	501264.776956	44.995431
3503.856884	501257.532288	45.000436
3503.881561	501251.302677	45.005441
3503.815923	501248.731708	45.010445
3503.782458	501240.436019	45.015450
3503.961924	501214.795900	45.020455
3503.653135	501208.922681	45.025460
3504.304420	501198.544702	45.030465
3504.205103	501202.711023	45.035469
3504.338874	501178.292867	45.040474
3504.598926	501155.828759	45.045479
3504.137793	501146.993227	45.050484
3504.044282	501121.801053	45.055489
3503.858709	501100.065328	45.060493
3504.104796	501101.291929	45.065498
3504.110529	501087.067825	45.070503
3503.931263	501063.053307	45.075508
3504.205063	501057.087952	45.080513
3504.041783	501049.976879	45.085517
3503.855984	501032.695382	45.090522
3504.473033	501008.706773	45.095527
3504.203007	501003.890314	45.100532
3503.866980	500980.760950	45.105537
3504.126238	500966.142358	45.110541
3503.986880	500968.341000	45.115546
3504.135242	500955.663374	45.120551
3503.821767	500932.530383	45.125556
3504.016886	500923.034222	45.130561
3504.249207	500926.135845	45.135565
3504.049619	500902.225556	45.140570
3503.976338	500881.180455	45.145575
3503.879728	500882.511856	45.150580
3503.970975	500870.956778	45.155585
3503.927671	500850.362458	45.160589
3504.027479	500840.071440	45.165594
3504.179750	500824.001739	45.170599
3503.981932	500823.982472	45.175604
3504.320457	500796.190678	45.180609
3504.126824	500781.289198	45.185613
3504.277933	500782.480217	45.190618
3504.310579	500750.889767	45.195623
3503.826512	500734.414391	45.200628
3503.886855	500738.049407	45.205633
3504.181486	500721.400318	45.210637
3504.091742	500707.899652	45.215642
3503.934485	500700.838104	45.220647
3503.618095	500696.990627	45.225652
3503.876401	500685.712730	45.230657
3504.036172	500666.503398	45.235661
3503.590068	500652.299748	45.240666
3504.046863	500637.649665	45.245671
3503.810641	500639.509331	45.250676
3504.000798	500630.570597	45.255681
3504.216423	500606.138719	45.260685
3503.885700	500606.292313	45.265690
3503.860789	500592.629457	45.270695
3503.873221	500592.931283	45.275700
3504.226880	500567.515791	45.280705
3504.390535	500556.657719	45.285709
3503.604325	500550.657271	45.290714
3504.109163	500535.341474	45.295719
3504.061817	500514.544932	45.300724
3503.763653	500507.758671	45.305729
3504.212263	500500.449425	45.310733
3503.907759	500484.603473	45.315738
3503.895293	500459.043224	45.320743
3503.791225	500447.316270	45.325748
3503.935711	500441.776099	45.330753
3504.084565	500443.220589	45.335757
3503.628873	500427.094772	45.340762
3504.318236	500396.665357	45.345767
3504.407770	500408.900993	45.350772
3504.132040	500395.328250	45.355777
3504.364563	500361.427680	45.360781
3503.816683	500360.653843	45.365786
3503.980806	500351.617847	45.370791
3503.626321	500339.373598	45.375796
3503.781507	500314.140974	45.380801
3503.809484	500307.657418	45.385805
3503.512548	500313.879938	45.390810
3503.765632	500305.133570	45.395815
3503.739359	500312.831875	45.400820
3503.550990	500288.058469	45.405825
3503.760475	500265.651854	45.410829
3503.716445	500260.394519	45.415834
3503.851943	500262.144850	45.420839
3503.725122	500264.645309	45.425844
3503.765778	500254.768257	45.430849
3504.017000	500252.956964	45.435853
3503.711779	500236.301000	45.440858
3503.948134	500213.991312	45.445863
3503.985699	500210.695211	45.450868
3503.792969	500212.143094	45.455873
3503.876081	500204.689022	45.460877
3503.804847	500182.124198	45.465882
3503.655934	500174.757407	45.470887
3503.663606	500171.516644	45.475892
3503.748663	500166.491974	45.480897
3504.117113	500165.168336	45.485901
3503.735041	500139.362335	45.490906
3503.854169	500112.768404	45.495911
3503.926589	500113.921287	45.500916
3503.725907	500110.966543	45.505921
3503.949199	500107.185492	45.510925
3503.592684	500116.049709	45.515930
3503.935844	500072.057834	45.520935
3503.711074	500071.435391	45.525940
3503.622174	500058.237817	45.530945
3503.948727	500049.530331	45.535949
3503.855567	500063.668006	45.540954
3503.912969	500057.837763	45.545959
3503.958963	500029.432963	45.550964
3503.978545	500031.555976	45.555969
3503.978499	500022.292665	45.560973
3503.916010	500022.859441	45.565978
3503.922647	499987.019698	45.570983
3503.985621	499983.820780	45.575988
3503.990186	499970.102170	45.580993
3504.196697	499959.793780	45.585997
3503.880000	499951.036061	45.591002
3504.203914	499936.203930	45.596007
3503.982568	499931.025145	45.601012
3503.983901	499913.662366	45.606017
3503.989744	499908.447665	45.611021
3503.752487	499890.363275	45.616026
3503.859011	499874.958013	45.621031
3503.729033	499887.937384	45.626036
3503.800135	499863.881678	45.631041
3504.198236	499848.632787	45.636045
3503.699963	499850.837675	45.641050
3503.781312	499840.042799	45.646055
3503.795140	499830.321613	45.651060
3503.861581	499806.367807	45.656065
3503.718666	499794.342844	45.661069
3503.947603	499794.661082	45.666074
3503.913020	499778.569357	45.671079
3504.051165	499794.341156	45.676084
3503.864483	499776.501758	45.681089
3504.019211	499740.891218	45.686093
3504.086703	499734.958034	45.691098
3503.929070	499740.804390	45.696103
3503.931146	499718.834839	45.701108
3503.877962	499705.935084	45.706113
3503.955168	499703.948760	45.711117
3503.462885	499707.519474	45.716122
3504.112513	499683.827669	45.721127
3503.837779	499674.759458	45.726132
3503.798711	499652.492605	45.731137
3503.984766	499653.880660	45.736141
3503.746883	499659.840967	45.741146
3504.042340	499639.090465	45.746151
3503.949248	499625.285785	45.751156
3503.969215	499607.211072	45.756161
3504.108447	499601.722093	45.761165
3504.042892	499600.922603	45.766170
3504.169021	499570.682058	45.771175
3504.036004	499557.896056	45.776180
3503.939194	499555.734738	45.781185
3504.403949	499530.603943	45.786189
3504.400387	499521.290307	45.791194
3504.160817	499505.129496	45.796199
3503.968597	499493.466471	45.801204
3503.738426	499463.383305	45.806209
3503.811747	499468.231440	45.811213
3503.652327	499466.029385	45.816218
3503.857293	499455.214738	45.821223
3503.680551	499446.991484	45.826228
3503.700118	499424.461974	45.831233
3504.014719	499411.402631	45.836237
3503.799571	499415.182705	45.841242
3504.249624	499402.203187	45.846247
3504.033208	499380.065272	45.851252
3504.088564	499371.957162	45.856257
3503.855585	499363.844002	45.861261
3503.804947	499372.710858	45.866266
3503.707771	499348.326709	45.871271
3503.876880	499333.316063	45.876276
3503.551005	499327.394301	45.881281
3503.993574	499313.099739	45.886285
3503.547087	499320.358674	45.891290
3503.641183	499307.334109	45.896295
3503.686532	499308.693809	45.901300
3503.853544	499295.910819	45.906305
3503.959900	499289.616993	45.911309
3503.957222	499297.312005	45.916314
3503.878597	499280.568712	45.921319
3504.106256	499278.710425	45.926324
3503.612256	499248.820467	45.931329
3503.949016	499232.872044	45.936333
3503.882893	499226.605459	45.941338
3503.752957	499230.979566	45.946343
3503.748986	499220.704022	45.951348
3503.614342	499201.843389	45.956353
3503.656468	499184.675944	45.961357
3503.748650	499188.154378	45.966362
3503.933068	499180.633246	45.971367
3503.856554	499187.580644	45.976372
3503.711811	499171.050188	45.981377
3504.131812	499151.089391	45.986381
3503.960348	499148.787956	45.991386
3504.130110	499124.563799	45.996391
3503.975634	499135.117718	46.001396
3503.956605	499103.684398	46.006401
3504.141308	499090.037886	46.011405
3503.888548	499101.771673	46.016410
3503.832024	499080.013093	46.021415
3503.792933	499053.037622	46.026420
3503.726202	499037.254048	46.031425
3503.498869	499038.302513	46.036429
3503.678342	499034.477542	46.041434
3503.949658	499033.219800	46.046439
3503.576858	499044.618241	46.051444
3503.582209	499018.951877	46.056449
3504.037233	498990.531403	46.061453
3503.984139	498999.955679	46.066458
3503.939458	498992.521304	46.071463
3504.023630	498979.346202	46.076468
3504.135341	498963.989963	46.081473
3503.724981	498954.790956	46.086477
3503.476409	498945.313258	46.091482
3503.811496	498945.817226	46.096487
3503.640041	498942.553931	46.101492
3503.636076	498955.362188	46.106497
3504.196509	498912.750568	46.111501
3503.853744	498915.335970	46.116506
3503.894601	498905.154406	46.121511
3504.249443	498893.758881	46.126516
3503.904650	498885.815047	46.131521
3503.934357	498857.410967	46.136525
3503.722091	498865.999882	46.141530
3503.856662	498854.284788	46.146535
3503.885072	498859.798284	46.151540
3504.075181	498827.521457	46.156545
3504.090556	498806.915512	46.161549
3503.973082	498811.388997	46.166554
3503.760501	498785.655502	46.171559
3504.087614	498763.127175	46.176564
3503.659296	498766.586715	46.181569
3503.953123	498752.416468	46.186573
3503.571203	498759.918537	46.191578
3504.128265	498751.832093	46.196583
3503.947315	498737.331892	46.201588
3503.604176	498724.983496	46.206593
3503.425539	498713.621558	46.211597
3503.760225	498713.467492	46.216602
3503.651038	498706.650675	46.221607
3503.958070	498704.425421	46.226612
3503.842235	498687.434340	46.231617
3504.110806	498667.243825	46.236621
3503.747311	498662.644000	46.241626
3503.960370	498653.801910	46.246631
3504.136236	498646.585649	46.251636
3504.031502	498625.745364	46.256641
3503.861210	498602.687975	46.261645
3503.975774	498617.806426	46.266650
3503.822011	498604.820531	46.271655
3504.019687	498569.302129	46.276660
3503.814330	498565.841630	46.281665
3504.027631	498558.214426	46.286669
3503.542969	498551.507523	46.291674
3503.546104	498554.190173	46.296679
3503.605387	498534.437581	46.301684
3503.566619	498540.822400	46.306689
3503.905867	498520.468678	46.311693
3503.606209	498533.982084	46.316698
3503.840899	498534.755053	46.321703
3504.254651	498522.995615	46.326708
3504.364894	498498.476281	46.331713
3504.324281	498484.561182	46.336717
3503.873253	498475.925221	46.341722
3504.285829	498449.181198	46.346727
3504.249877	498441.492095	46.351732
3504.102243	498432.504413	46.356737
3504.012035	498405.789172	46.361741
3503.934346	498393.955458	46.366746
3503.977257	498391.417543	46.371751
3503.981521	498384.481423	46.376756
3504.053758	498373.889605	46.381761
3504.247116	498343.332626	46.386765
3503.925960	498343.231598	46.391770
3504.155214	498332.311190	46.396775
3504.247616	498310.781263	46.401780
3503.831694	498301.785298	46.406785
3503.949258	498299.387444	46.411789
3504.182198	498271.810935	46.416794
3503.779517	498251.928555	46.421799
3503.993010	498244.959310	46.426804
3503.888249	498244.722828	46.431809
3504.413340	498224.339398	46.436813
3503.983244	498214.991257	46.441818
3503.834158	498199.979338	46.446823
3503.929789	498198.546810	46.451828
3503.684635	498177.880077	46.456833
3503.898880	498170.404435	46.461837
3504.140529	498160.950087	46.466842
3503.996980	498153.682868	46.471847
3503.846850	498150.061684	46.476852
3503.862392	498122.873685	46.481857
3504.101469	498109.724088	46.486861
3503.935910	498117.141599	46.491866
3503.881049	498098.874699	46.496871
3503.791718	498076.208840	46.501876
3503.769131	498060.923685	46.506881
3503.959304	498051.325541	46.511885
3504.121018	498062.386986	46.516890
3504.160674	498031.246271	46.521895
3504.061445	498013.138173	46.526900
3503.855655	498004.007594	46.531905
3504.047797	498011.672361	46.536909
3503.743190	497991.875442	46.541914
3503.837562	497971.154806	46.546919
3504.122293	497964.123567	46.551924
3503.741543	497963.525701	46.556929
3504.160456	497953.435720	46.561933
3503.926645	497926.337464	46.566938
3503.830230	497913.139503	46.571943
3504.021254	497914.273781	46.576948
3503.706071	497911.134268	46.581953
3504.074193	497894.167195	46.586957
3503.938421	497889.986806	46.591962
3503.672478	497870.133017	46.596967
3503.773713	497867.484559	46.601972
3503.658044	497870.489844	46.606977
3503.951628	497861.432137	46.611981
3503.807889	497843.381530	46.616986
3503.626490	497823.868708	46.621991
3503.697748	497822.034995	46.626996
3503.734585	497830.281272	46.632001
3504.008800	497821.783491	46.637005
3503.663650	497812.168583	46.642010
3503.681531	497786.498485	46.647015
3503.811933	497786.477956	46.652020
3503.312062	497789.847738	46.657025
3503.688710	497781.789381	46.662029
3503.948315	497777.394593	46.667034
3503.626777	497774.711695	46.672039
3504.073001	497765.629813	46.677044
3504.252317	497748.439317	46.682049
3504.401840	497732.417915	46.687053
3503.938543	497731.934340	46.692058
3504.231562	497706.018135	46.697063
3504.081894	497681.133764	46.702068
3503.746146	497689.540250	46.707073
3503.886214	497671.393986	46.712077
3503.520293	497656.871526	46.717082
3503.716296	497642.867751	46.722087
3503.938800	497642.174521	46.727092
3503.619391	497643.541377	46.732097
3503.431016	497633.648461	46.737101
3503.588036	497637.268825	46.742106
3503.461561	497628.176145	46.747111
3504.166617	497622.040238	46.752116
3503.860390	497604.065703	46.757121
3503.884876	497597.176711	46.762125
3503.863614	497599.812732	46.767130
3503.810524	497582.658814	46.772135
3503.938958	497560.312273	46.777140
3503.758592	497554.417550	46.782145
3504.049120	497540.500009	46.787149
3503.841691	497542.709825	46.792154
3503.921662	497533.685719	46.797159
3503.902294	497498.655162	46.802164
3503.761917	497508.094012	46.807169
3504.084217	497495.386456	46.812173
3504.078784	497493.969847	46.817178
3504.205087	497477.698757	46.822183
3504.343393	497460.008201	46.827188
3504.199277	497451.070101	46.832193
3504.383506	497422.639340	46.837197
3504.124879	497411.947375	46.842202
3504.033934	497402.798339	46.847207
3504.099985	497374.689945	46.852212
3503.694531	497365.337466	46.857217
3503.949077	497351.526722	46.862221
3503.712756	497359.867016	46.867226
3503.930811	497339.024852	46.872231
3503.621846	497317.607812	46.877236
3503.219701	497310.836774	46.882241
3503.694799	497296.282344	46.887245
3503.626695	497307.886851	46.892250
3503.611707	497303.231588	46.897255
3503.955946	497306.316153	46.902260
3504.068641	497301.488827	46.907265
3503.824368	497267.151526	46.912269
3503.679968	497261.807925	46.917274
3503.835820	497258.340706	46.922279
3503.898519	497245.117107	46.927284
3503.723304	497259.573714	46.932289
3503.851737	497242.289527	46.937293
3503.833052	497214.447415	46.942298
3503.747226	497218.106249	46.947303
3503.826521	497209.790875	46.952308
3503.638120	497207.846260	46.957313
3503.787808	497200.431052	46.962317
3503.848851	497199.206423	46.967322
3503.844819	497161.185759	46.972327
3504.015864	497152.096440	46.977332
3503.331690	497159.495061	46.982337
3503.762904	497144.998074	46.987341
3503.683527	497146.478909	46.992346
3503.552090	497143.006450	46.997351
3503.902019	497125.130235	47.002356
3503.921477	497117.634322	47.007361
3503.552975	497109.237798	47.012365
3503.613975	497115.354210	47.017370
3503.580480	497099.513061	47.022375
3503.986268	497102.031026	47.027380
3503.564911	497097.794338	47.032385
3504.000571	497070.234586	47.037389
3504.038763	497064.406413	47.042394
3503.790877	497062.116789	47.047399
3504.063778	497060.352383	47.052404
3503.893137	497044.786005	47.057409
3503.604159	497031.364697	47.062413
3503.632276	497037.638218	47.067418
3503.757358	497031.441903	47.072423
3503.824816	497028.089869	47.077428
3503.543278	497028.387593	47.082433
3503.461841	497011.794524	47.087437
3503.529474	497009.758790	47.092442
3503.918180	497010.001201	47.097447
3503.936448	496978.052006	47.102452
3503.681087	496969.688162	47.107457
3504.043016	496970.643602	47.112461
3503.750000	496981.372559	47.117466
3503.849211	496946.676590	47.122471
3503.985929	496930.757761	47.127476
3503.400597	496939.609069	47.132481
3503.614967	496922.766649	47.137485
3504.066560	496917.885653	47.142490
3503.898313	496919.886837	47.147495
3503.667564	496883.724050	47.152500
3503.676723	496878.862348	47.157505
3503.860079	496869.467170	47.162509
3503.738289	496870.043418	47.167514
3503.874193	496876.553099	47.172519
3503.808617	496857.122184	47.177524
3503.640421	496855.883138	47.182529
3503.588845	496832.956612	47.187533
3503.754802	496832.525433	47.192538
3503.311119	496835.228335	47.197543
3503.663887	496824.439384	47.202548
3503.675882	496841.853823	47.207553
3503.812465	496829.934588	47.212557
3503.717234	496838.354077	47.217562
3503.744799	496798.960687	47.222567
3503.901630	496785.468731	47.227572
3503.993484	496787.226302	47.232577
3503.660220	496788.392894	47.237581
3503.963759	496778.168613	47.242586
3503.427669	496762.710385	47.247591
3503.806330	496743.057244	47.252596
3503.522412	496742.849059	47.257601
3503.861105	496742.947493	47.262605
3503.807405	496727.666131	47.267610
3503.766046	496742.405766	47.272615
3504.041690	496722.566370	47.277620
3503.848823	496706.193150	47.282625
3503.699605	496701.508322	47.287629
3503.752356	496687.222680	47.292634
3503.516364	496689.690259	47.297639
3503.672357	496682.526988	47.302644
3503.712478	496681.052486	47.307649
3503.915663	496668.818843	47.312653
3503.851308	496646.906684	47.317658
3503.596488	496653.225059	47.322663
3503.859811	496642.247622	47.327668
3503.720622	496642.927884	47.332673
3503.528548	496635.161432	47.337677
3503.954392	496620.259845	47.342682
3503.563048	496603.766017	47.347687
3503.603354	496596.317223	47.352692
3503.535230	496582.961932	47.357697
3503.678719	496583.040593	47.362701
3503.582779	496580.828149	47.367706
3503.629672	496590.288505	47.372711
3503.775618	496580.949721	47.377716
3503.578038	496583.107466	47.382721
3503.449279	496551.535166	47.387725
3503.640454	496539.151446	47.392730
3503.576412	496540.174241	47.397735
3503.847299	496539.878358	47.402740
3503.593358	496540.121098	47.407745
3503.621561	496531.712230	47.412749
3504.113126	496536.495044	47.417754
3503.696985	496516.764770	47.422759
3503.876118	496490.358537	47.427764
3503.879989	496489.396046	47.432769
3503.761874	496491.996907	47.437773
3503.791671	496488.448208	47.442778
3504.055961	496483.596703	47.447783
3504.076983	496464.556717	47.452788
3503.522240	496461.859853	47.457793
3503.625315	496446.300326	47.462797
3503.958043	496447.209780	47.467802
3503.858612	496448.390063	47.472807
3503.869404	496417.959956	47.477812
3503.501179	496415.790531	47.482817
3503.443663	496398.383043	47.487821
3503.721249	496398.693658	47.492826
3503.788247	496395.088431	47.497831
3503.686737	496395.307078	47.502836
3503.667832	496391.209130	47.507841
3503.996738	496374.499988	47.512845
3504.194462	496359.786135	47.517850
3503.518610	496354.576899	47.522855
3503.670895	496350.502512	47.527860
3503.918537	496355.374559	47.532865
3503.698535	496334.246076	47.537869
3504.113739	496313.320945	47.542874
3503.811839	496307.141245	47.547879
3503.944424	496288.944153	47.552884
3503.957098	496290.461137	47.557889
3503.892257	496276.244390	47.562893
3503.886099	496262.322138	47.567898
3503.599967	496267.683621	47.572903
3504.092394	496260.720158	47.577908
3503.715956	496263.716295	47.582913
3503.796330	496245.223631	47.587917
3503.837842	496219.496952	47.592922
3503.846206	496219.951386	47.597927
3503.943908	496215.379293	47.602932
3503.987142	496223.422767	47.607937
3504.055699	496196.577914	47.612941
3503.920665	496179.891297	47.617946
3503.831131	496184.107859	47.622951
3503.877685	496169.721530	47.627956
3503.996235	496166.462522	47.632961
3503.784453	496143.003514	47.637965
3503.992199	496129.553656	47.642970
3503.805805	496123.305005	47.647975
3503.883688	496111.748993	47.652980
3503.981190	496107.480688	47.657985
3503.802875	496086.142805	47.662989
3503.839113	496078.846334	47.667994
3503.492210	496083.913692	47.672999
3503.895993	496073.014972	47.678004
3503.771498	496066.300841	47.683009
3503.474897	496048.930811	47.688013
3503.523867	496024.873496	47.693018
3503.561640	496025.373916	47.698023
3503.874400	496013.831347	47.703028
3503.352738	496033.457411	47.708033
3503.422085	496022.814047	47.713037
3503.415092	496012.689053	47.718042
3503.283638	496014.937674	47.723047
3503.398804	496012.691792	47.728052
3503.800028	496015.160001	47.733057
3503.626848	496005.972628	47.738061
3503.716118	496021.451662	47.743066
3503.469106	496002.656084	47.748071
3503.799783	495981.997089	47.753076
3503.428677	495977.549670	47.758081
3503.562918	495981.832170	47.763085
3503.870466	495969.328407	47.768090
3503.332596	495972.704525	47.773095
3503.467064	495972.531460	47.778100
3503.713735	495982.669388	47.783105
3503.583995	495976.310470	47.788109
3503.625235	495968.709378	47.793114
3503.620256	495955.849958	47.798119
3503.831971	495932.273107	47.803124
3503.713690	495927.532557	47.808129
3503.493267	495929.187678	47.813133
3503.748219	495921.400893	47.818138
3503.779168	495921.801133	47.823143
3503.685183	495921.056603	47.828148
3503.769606	495911.929727	47.833153
3503.538245	495897.890899	47.838157
3503.744620	495886.516959	47.843162
3503.609084	495878.184303	47.848167
3503.838210	495875.363447	47.853172
3503.853831	495881.588710	47.858177
3503.817921	495879.214798	47.863181
3503.647571	495838.534201	47.868186
3503.729556	495820.445903	47.873191
3503.873928	495831.207662	47.878196
3503.655076	495829.217080	47.883201
3503.496963	495822.508173	47.888205
3503.827168	495824.076268	47.893210
3504.021172	495821.007799	47.898215
3504.043151	495780.904250	47.903220
3503.800386	495781.297126	47.908225
3503.827450	495786.001665	47.913229
3503.754984	495769.102256	47.918234
3503.722792	495761.411422	47.923239
3503.576124	495744.321191	47.928244
3503.838435	495733.292736	47.933249
3503.809526	495720.943249	47.938253
3503.795964	495725.198541	47.943258
3503.553665	495737.540426	47.948263
3503.627181	495721.529268	47.953268
3503.791416	495723.072974	47.958273
3503.734972	495698.981261	47.963277
3503.764363	495679.280919	47.968282
3503.780527	495684.999844	47.973287
3503.616894	495678.747443	47.978292
3503.851062	495684.735701	47.983297
3503.814209	495674.615239	47.988301
3503.549159	495642.657852	47.993306
3503.658045	495639.805334	47.998311
3503.874784	495633.290266	48.003316
3503.764963	495633.763395	48.008321
3503.864888	495622.659277	48.013325
3504.116015	495617.505832	48.018330
3503.437094	495604.297001	48.023335
3503.733026	495581.870925	48.028340
3503.875452	495588.936990	48.033345
3503.932520	495582.345878	48.038349
3503.909053	495584.526850	48.043354
3503.512227	495560.843181	48.048359
3503.723842	495537.417734	48.053364
3503.771589	495532.296412	48.058369
3503.391728	495539.850110	48.063373
3503.780918	495529.864754	48.068378
3503.796583	495530.014258	48.073383
3503.995372	495530.134815	48.078388
3503.845173	495503.526050	48.083393
3503.663165	495497.276490	48.088397
3503.509128	495491.984523	48.093402
3503.715416	495499.091161	48.098407
3503.919769	495492.679265	48.103412
3504.082954	495485.058698	48.108417
3503.942682	495479.156962	48.113421
3504.113983	495443.737884	48.118426
3503.631047	495445.181379	48.123431
3503.665471	495445.378550	48.128436
3503.757592	495446.731149	48.133441
3503.405676	495423.647793	48.138445
3503.535571	495407.627448	48.143450
3503.388942	495404.714016	48.148455
3503.691735	495396.565019	48.153460
3503.798573	495399.029213	48.158465
3503.972391	495388.267701	48.163469
3503.997550	495397.124519	48.168474
3503.733642	495376.406926	48.173479
3503.915513	495361.036550	48.178484
3503.706227	495351.196328	48.183489
3503.698839	495348.311511	48.188493
3503.688126	495351.098089	48.193498
3503.559154	495349.903371	48.198503
3503.757327	495338.935450	48.203508
3504.092673	495319.743321	48.208513
3503.763380	495312.048626	48.213517
3503.995165	495293.176636	48.218522
3503.803195	495310.877941	48.223527
3503.507388	495298.317192	48.228532
3503.692623	495290.186729	48.233537
3503.805713	495273.054999	48.238541
3504.118385	495239.182801	48.243546
3503.794816	495258.879648	48.248551
3503.665286	495248.722966	48.253556
3503.813953	495244.750172	48.258561
3503.264595	495236.432000	48.263565
3503.608987	495209.542096	48.268570
3503.607860	495221.846208	48.273575
3503.671606	495199.760163	48.278580
3503.533200	495213.807507	48.283585
3503.828158	495210.571079	48.288589
3503.784214	495203.286933	48.293594
3503.230327	495203.728998	48.298599
3503.769997	495203.947576	48.303604
3503.918533	495190.050688	48.308609
3503.881123	495174.765450	48.313613
3503.921295	495164.986964	48.318618
3503.759591	495159.291045	48.323623
3504.038464	495149.424187	48.328628
3503.995583	495131.354945	48.333633
3503.907833	495118.001684	48.338637
3504.043954	495117.220750	48.343642
3503.691890	495121.884120	48.348647
3503.920243	495102.202342	48.353652
3504.016554	495081.073042	48.358657
3503.664917	495079.710967	48.363661
3503.862190	495063.780939	48.368666
3503.956909	495063.411615	48.373671
3503.658003	495050.800551	48.378676
3503.850023	495032.390281	48.383681
3503.863392	495026.210945	48.388685
3503.947474	495008.425315	48.393690
3503.862959	495016.742682	48.398695
3503.621098	495010.704951	48.403700
3503.778885	494978.679567	48.408705
3503.725626	494980.764053	48.413709
3503.844343	494972.188260	48.418714
3503.712297	494973.120623	48.423719
3503.748810	494964.456551	48.428724
3503.748973	494965.317383	48.433729
3503.515960	494949.354001	48.438733
3503.993677	494935.252986	48.443738
3503.623808	494933.995050	48.448743
3503.755221	494921.366513	48.453748
3503.999582	494914.441753	48.458753
3503.899180	494923.419915	48.463757
3503.866066	494895.930981	48.468762
3503.613843	494877.438872	48.473767
3503.599491	494870.554988	48.478772
3503.773013	494874.477102	48.483777
3503.653655	494871.052933	48.488781
3503.924390	494870.351979	48.493786
3503.767102	494842.781325	48.498791
3503.750161	494834.125641	48.503796
3503.707660	494833.828636	48.508801
3503.512471	494832.998790	48.513805
3503.821054	494818.924420	48.518810
3503.528233	494825.249431	48.523815
3503.647242	494820.977428	48.528820
3503.851620	494811.679140	48.533825
3503.182678	494791.581882	48.538829
3503.489607	494775.583637	48.543834
3503.470949	494785.662902	48.548839
3503.613860	494787.564499	48.553844
3503.887496	494775.824799	48.558849
3503.637900	494775.813699	48.563853
3504.004606	494764.464355	48.568858
3503.671968	494775.757845	48.573863
3503.906258	494761.948346	48.578868
3504.168776	494754.716850	48.583873
3503.933647	494749.234947	48.588877
3503.718123	494736.509217	48.593882
3503.895892	494726.404941	48.598887
3503.578438	494707.416626	48.603892
3503.753768	494695.945586	48.608897
3503.695748	494698.284030	48.613901
3504.095438	494682.828022	48.618906
3503.571551	494689.695948	48.623911
3503.675469	494675.704454	48.628916
3503.669063	494657.730249	48.633921
3503.319575	494653.430990	48.638925
3503.831737	494636.488760	48.643930
3503.743758	494635.186246	48.648935
3503.931778	494642.448010	48.653940
3503.949891	494639.204607	48.658945
3504.085541	494619.840773	48.663949
3504.168137	494601.143557	48.668954
3503.854605	494595.825905	48.673959
3504.185989	494587.064413	48.678964
3504.017908	494564.457262	48.683969
3503.518355	494561.346306	48.688973
3503.969592	494553.831726	48.693978
3504.075580	494548.093304	48.698983
3503.944516	494528.872802	48.703988
3503.962534	494506.793151	48.708993
3503.875890	494509.794399	48.713997
3503.872078	494504.022683	48.719002
3503.694856	494500.962037	48.724007
3503.586553	494477.940251	48.729012
3503.697987	494471.542687	48.734017
3503.475646	494465.349785	48.739021
3503.695267	494457.314789	48.744026
3503.774535	494451.884372	48.749031
3503.593094	494451.102970	48.754036
3503.770870	494443.834111	48.759041
3503.848351	494439.214137	48.764045
3503.770566	494422.466231	48.769050
3503.307079	494418.488748	48.774055
3503.447129	494402.263379	48.779060
3503.954491	494404.613764	48.784065
3503.300920	494408.362899	48.789069
3503.856319	494399.616544	48.794074
3503.595253	494409.076071	48.799079
3503.806155	494396.535879	48.804084
3504.246502	494390.339475	48.809089
3503.794149	494378.663639	48.814093
3503.781297	494352.740388	48.819098
3503.895358	494358.494889	48.824103
3503.895981	494353.279416	48.829108
3504.229175	494320.263084	48.834113
3503.909380	494314.946340	48.839117
3504.140351	494307.112027	48.844122
3503.851803	494296.524231	48.849127
3503.911567	494267.500606	48.854132
3504.067835	494262.766863	48.859137
3504.056733	494255.072063	48.864141
3504.040669	494246.669142	48.869146
3503.892670	494216.412381	48.874151
3503.973719	494207.335826	48.879156
3504.183616	494205.176023	48.884161
3503.731204	494198.968760	48.889165
3503.974074	494173.106107	48.894170
3503.921461	494164.405110	48.899175
3503.556704	494165.526205	48.904180
3504.019608	494162.161776	48.909185
3503.707557	494152.387788	48.914189
3503.888647	494119.850864	48.919194
3503.765321	494120.224893	48.924199
3503.681370	494114.718903	48.929204
3503.755235	494107.668882	48.934209
3503.501095	494112.013210	48.939213
3503.750831	494113.391631	48.944218
3503.451568	494101.640784	48.949223
3503.622014	494080.802433	48.954228
3503.656783	494070.669764	48.959233
3503.753160	494080.123597	48.964237
3503.870543	494065.977602	48.969242
3503.885989	494068.355149	48.974247
3503.775107	494072.018571	48.979252
3504.132468	494025.477997	48.984257
3503.796557	494034.139364	48.989261
3503.797702	494017.378612	48.994266
3503.602855	494018.877949	48.999271
3503.749842	494020.930892	49.004276
3503.843656	493998.838650	49.009281
3503.801886	493985.730480	49.014285
3503.711334	493985.795512	49.019290
3503.756698	493990.295074	49.024295
3503.352219	493989.599543	49.029300
3503.896536	493972.651621	49.034305
3503.700073	493988.937086	49.039309
3503.650985	493949.904132	49.044314
3503.236222	493930.626574	49.049319
3503.411188	493932.675104	49.054324
3503.355702	493923.265534	49.059329
3503.075327	493932.880267	49.064333
3503.672493	493924.430906	49.069338
3503.534207	493931.339436	49.074343
3503.372259	493937.087060	49.079348
3503.799133	493926.942971	49.084353
3503.445319	493926.036882	49.089357
3503.795923	493934.336598	49.094362
3503.937848	493933.301513	49.099367
3503.482478	493934.740764	49.104372
3503.810900	493909.269311	49.109377
3503.491132	493902.332067	49.114381
3503.731700	493890.394483	49.119386
3503.530849	493891.185865	49.124391
3503.753818	493884.719831	49.129396
3503.858528	493875.538099	49.134401
3503.884755	493886.572861	49.139405
3503.920932	493859.122060	49.144410
3503.675360	493841.944415	49.149415
3503.969524	493832.631441	49.154420
3503.831718	493823.943749	49.159425
3503.527295	493837.410742	49.164429
3503.897609	493823.123308	49.169434
3503.643425	493806.655908	49.174439
3503.338435	493790.297798	49.179444
3503.654690	493781.994048	49.184449
3503.217677	493792.950177	49.189453
3503.620119	493782.809871	49.194458
3503.336323	493781.791433	49.199463
3503.468440	493787.391348	49.204468
3503.923010	493778.306178	49.209473
3503.749081	493796.512461	49.214477
3503.486898	493771.286082	49.219482
3503.655609	493771.107586	49.224487
3503.605295	493756.076392	49.229492
3503.539255	493736.085226	49.234497
3503.124012	493734.935651	49.239501
3503.599078	493721.998785	49.244506
3503.545373	493734.565390	49.249511
3503.494853	493737.561053	49.254516
3503.496598	493722.420329	49.259521
3503.342544	493727.913584	49.264525
3503.551528	493730.615044	49.269530
3503.860076	493716.590476	49.274535
3503.388725	493731.805598	49.279540
3503.528336	493733.961014	49.284545
3503.629958	493717.437293	49.289549
3503.532041	493715.376725	49.294554
3503.653968	493694.343057	49.299559
3503.771640	493690.830564	49.304564
3504.064928	493679.998533	49.309569
3503.362731	493687.198837	49.314573
3503.852623	493674.259595	49.319578
3503.897292	493681.392486	49.324583
3503.602367	493662.753990	49.329588
3503.928184	493632.370738	49.334593
3503.677274	493645.424312	49.339597
3503.864186	493640.128553	49.344602
3503.533884	493641.244232	49.349607
3503.371044	493642.333441	49.354612
3503.949953	493631.810697	49.359617
3503.446822	493617.357339	49.364621
3503.594273	493599.408418	49.369626
3504.133634	493592.183345	49.374631
3503.485748	493583.525528	49.379636
3503.893921	493574.194404	49.384641
3503.701043	493582.833373	49.389645
3504.094142	493569.453619	49.394650
3503.846917	493546.553901	49.399655
3503.660042	493537.873830	49.404660
3503.920871	493533.832301	49.409665
3503.474530	493538.359057	49.414669
3503.528031	493533.692009	49.419674
3503.905174	493527.404032	49.424679
3503.782561	493519.422724	49.429684
3503.788904	493492.887575	49.434689
3503.453164	493494.966241	49.439693
3503.758787	493486.005747	49.444698
3503.333896	493487.136386	49.449703
3503.659118	493487.388890	49.454708
3504.096083	493472.077891	49.459713
3503.767918	493475.016207	49.464717
3503.558204	493451.907890	49.469722
3503.854791	493439.556057	49.474727
3503.647276	493437.158315	49.479732
3503.748359	493434.104138	49.484737
3503.528691	493433.987028	49.489741
3503.541041	493428.718801	49.494746
3503.959283	493428.804689	49.499751
3503.567728	493422.131800	49.504756
3503.996042	493397.150232	49.509761
3503.800236	493397.890199	49.514765
3503.754642	493381.085618	49.519770
3503.870955	493391.650693	49.524775
3503.475646	493372.318836	49.529780
3503.767156	493353.739247	49.534785
3503.434827	493346.854416	49.539789
3503.641160	493333.959758	49.544794
3503.750738	493329.739539	49.549799
3503.573930	493340.604167	49.554804
3504.041279	493327.972077	49.559809
3503.897098	493329.260907	49.564813
3503.864819	493304.301380	49.569818
3503.800323	493291.145669	49.574823
3503.442184	493288.569162	49.579828
3503.595352	493286.316943	49.584833
3503.593366	493290.115222	49.589837
3503.900106	493288.952774	49.594842
3503.579553	493283.838403	49.599847
3503.288380	493264.895081	49.604852
3503.701906	493252.828470	49.609857
3503.800909	493251.344386	49.614861
3503.516255	493241.818776	49.619866
3503.881528	493236.747903	49.624871
3503.717224	493247.965079	49.629876
3503.527620	493233.613777	49.634881
3503.385935	493237.130317	49.639885
3503.804427	493238.735324	49.644890
3503.900761	493227.377135	49.649895
3503.576702	493213.654734	49.654900
3503.667432	493200.980810	49.659905
3503.740030	493212.616309	49.664909
3503.639610	493200.428347	49.669914
3503.599029	493204.182106	49.674919
3503.533385	493201.306160	49.679924
3503.683691	493189.787501	49.684929
3503.353434	493181.028647	49.689933
3503.714576	493167.349822	49.694938
3503.461868	493161.617028	49.699943
3503.416430	493155.648915	49.704948
3503.569141	493141.749821	49.709953
3503.781990	493153.464467	49.714957
3503.600413	493136.124131	49.719962
3503.909633	493137.847697	49.724967
3503.692629	493138.439107	49.729972
3503.587969	493118.757210	49.734977
3503.240105	493111.368357	49.739981
3503.295534	493112.321817	49.744986
3503.340942	493106.946996	49.749991
3503.547755	493107.876528	49.754996
3503.737824	493099.693697	49.760001
3503.565850	493116.836922	49.765005
3503.618737	493102.345911	49.770010
3503.745001	493101.313257	49.775015
3503.731782	493105.366544	49.780020
3503.558072	493093.190096	49.785025
3503.449571	493098.625698	49.790029
3503.669401	493085.526177	49.795034
3503.907985	493063.308654	49.800039
3503.438027	493059.331896	49.805044
3503.642377	493056.717085	49.810049
3503.792152	493057.706275	49.815053
3503.796233	493054.211616	49.820058
3503.777905	493050.821777	49.825063
3503.605681	493039.556561	49.830068
3503.600576	493032.265416	49.835073
3503.223609	493014.246901	49.840077
3503.380990	492999.283540	49.845082
3503.693114	493002.930950	49.850087
3503.362543	493012.047703	49.855092
3503.321230	493008.053818	49.860097
3503.251008	493008.318196	49.865101
3503.389677	493003.992027	49.870106
3503.326220	493006.027709	49.875111
3503.442333	493014.364906	49.880116
3503.655756	493003.697021	49.885121
3503.459686	492995.980293	49.890125
3503.326211	493003.192244	49.895130
3503.685927	493003.692499	49.900135
3503.517868	493002.250608	49.905140
3503.724196	493004.547482	49.910145
3503.664699	493005.012722	49.915149
3503.663374	492979.338913	49.920154
3503.626215	492965.570978	49.925159
3503.348633	492966.526445	49.930164
3503.594173	492946.738370	49.935169
3503.588586	492958.842142	49.940173
3503.607399	492957.066874	49.945178
3503.814174	492947.615352	49.950183
3503.738855	492954.970047	49.955188
3503.884168	492937.729773	49.960193
3503.836227	492920.368111	49.965197
3503.831940	492912.469116	49.970202
3504.162400	492912.062488	49.975207
3504.037742	492901.802459	49.980212
3503.733875	492878.049993	49.985217
3503.419243	492876.935098	49.990221
3503.688893	492865.853129	49.995226
3503.848970	492857.877491	50.000231
3503.574283	492865.516933	50.005236
3503.492530	492856.364168	50.010241
3503.601359	492870.678056	50.015245
3503.450895	492853.332537	50.020250
3503.941792	492851.837116	50.025255
3503.750776	492839.308757	50.030260
3503.903101	492809.863092	50.035265
3503.742080	492817.687146	50.040269
3503.359255	492809.493462	50.045274
3503.614051	492807.630239	50.050279
3503.519596	492818.988553	50.055284
3503.983306	492795.418492	50.060289
3503.957121	492785.902431	50.065293
3503.556415	492772.850134	50.070298
3503.620137	492775.473416	50.075303
3503.496054	492769.720169	50.080308
3503.459406	492749.166250	50.085313
3503.301635	492757.445575	50.090317
3503.592734	492767.325061	50.095322
3503.735538	492760.212989	50.100327
3503.394744	492769.635315	50.105332
3503.696207	492758.750814	50.110337
3503.654073	492738.602869	50.115341
3503.489582	492731.438078	50.120346
3503.684966	492715.202482	50.125351
3503.663193	492723.359045	50.130356
3503.986229	492716.167828	50.135361
3503.918063	492713.950525	50.140365
3503.742154	492709.218250	50.145370
3503.943165	492675.916034	50.150375
3503.689376	492682.893926	50.155380
3503.584937	492680.277232	50.160385
3503.573236	492664.631365	50.165389
3503.614669	492658.953201	50.170394
3503.784190	492655.331036	50.175399
3503.621745	492651.710703	50.180404
3503.699747	492634.278225	50.185409
3503.429166	492631.586504	50.190413
3503.678628	492621.672307	50.195418
3503.784990	492618.212039	50.200423
3503.731934	492612.396875	50.205428
3503.691994	492623.088369	50.210433
3503.578025	492619.409726	50.215437
3503.482916	492614.360815	50.220442
3503.635685	492605.120216	50.225447
3503.156749	492580.584794	50.230452
3503.251953	492575.050027	50.235457
3503.399032	492593.409314	50.240461
3503.425823	492588.087925	50.245466
3503.679897	492574.982631	50.250471
3503.242990	492573.127438	50.255476
3503.512335	492572.629183	50.260481
3503.357867	492567.994764	50.265485
3503.590027	492570.692732	50.270490
3503.278121	492564.817188	50.275495
3503.014544	492572.708196	50.280500
3503.613571	492558.586198	50.285505
3503.578623	492551.907266	50.290509
3503.619764	492567.548739	50.295514
3503.752120	492558.868388	50.300519
3504.040149	492563.279301	50.305524
3503.921120	492552.714346	50.310529
3503.971035	492533.868281	50.315533
3503.651498	492514.878032	50.320538
3504.070521	492522.002839	50.325543
3503.613988	492513.820674	50.330548
3503.764301	492505.137460	50.335553
3503.670304	492496.189015	50.340557
3503.777287	492483.562672	50.345562
3503.857975	492477.878247	50.350567
3503.489891	492472.973726	50.355572
3503.786727	492463.406441	50.360577
3503.728651	492457.288178	50.365581
3503.632388	492457.151554	50.370586
3503.962315	492448.693126	50.375591
3503.595885	492440.648609	50.380596
3503.815964	492431.599847	50.385601
3503.956396	492425.551478	50.390605
3503.666511	492427.116605	50.395610
3504.102442	492425.072791	50.400615
3503.760706	492403.655178	50.405620
3504.079477	492389.324146	50.410625
3504.136742	492392.556194	50.415629
3503.925513	492385.348016	50.420634
3503.858451	492354.569000	50.425639
3503.754888	492353.471351	50.430644
3503.484743	492345.057085	50.435649
3503.794838	492345.767768	50.440653
3503.586968	492336.634681	50.445658
3503.944632	492329.488482	50.450663
3503.852799	492318.210120	50.455668
3503.825417	492291.526655	50.460673
3503.503319	492289.703927	50.465677
3503.510656	492288.234256	50.470682
3503.952349	492288.215163	50.475687
3503.560503	492284.833582	50.480692
3503.600484	492274.395259	50.485697
3503.908453	492264.724829	50.490701
3503.733473	492255.738427	50.495706
3503.763787	492255.835000	50.500711
3503.616727	492252.313439	50.505716
3504.028847	492244.905394	50.510721
3503.827008	492232.327694	50.515725
3503.643728	492216.303439	50.520730
3503.894556	492196.412447	50.525735
3503.865126	492172.514413	50.530740
3503.638891	492135.531289	50.535745
3503.630773	492076.180615	50.540749
3503.499779	492013.202956	50.545754
3503.240796	491951.815219	50.550759
3503.259812	491879.191395	50.555764
3503.685380	491774.851443	50.560769
3503.296666	491685.427325	50.565773
3502.774861	491578.754523	50.570778
3502.877301	491455.016891	50.575783
3502.706335	491333.347405	50.580788
3502.348023	491194.386446	50.585793
3502.112721	491055.050495	50.590797
3501.855425	490909.183787	50.595802
3501.700374	490746.637459	50.600807
3501.187530	490591.287330	50.605812
3501.029570	490423.977952	50.610817
3500.832611	490248.063304	50.615821
3500.571491	490060.862818	50.620826
3500.026779	489866.817198	50.625831
3499.714039	489685.394967	50.630836
3499.637454	489477.039163	50.635841
3499.173516	489262.157862	50.640845
3498.922699	489055.243110	50.645850
3498.822270	488842.528158	50.650855
3498.287366	488614.025691	50.655860
3498.152553	488363.575657	50.660865
3497.805915	488132.302408	50.665869
3497.227912	487887.183970	50.670874
3496.984560	487624.685883	50.675879
3496.544565	487373.865770	50.680884
3496.263149	487117.799802	50.685889
3495.921418	486840.515131	50.690893
3495.654887	486565.696707	50.695898
3494.997405	486267.684400	50.700903
3494.557805	485996.988390	50.705908
3493.790015	485698.478059	50.710913
3493.599313	485404.937819	50.715917
3492.754066	485113.725609	50.720922
3492.873017	484806.499609	50.725927
3492.361254	484510.412724	50.730932
3491.806669	484195.076185	50.735937
3491.588592	483885.456955	50.740941
3490.613492	483562.019694	50.745946
3490.350090	483238.211197	50.750951
3489.387403	482914.963825	50.755956
3489.148885	482586.985895	50.760961
3488.886900	482246.491166	50.765965
3487.751831	481915.603563	50.770970
3487.679674	481577.853931	50.775975
3486.889603	481246.140399	50.780980
3486.401367	480905.607378	50.785985
3485.696208	480556.589785	50.790989
3485.266728	480214.971371	50.795994
3484.801439	479862.457757	50.800999
3483.965213	479517.851098	50.806004
3483.509145	479163.397882	50.811009
3483.196102	478802.885164	50.816013
3482.373234	478454.507776	50.821018
3481.894790	478085.899734	50.826023
3481.212903	477732.672926	50.831028
3480.498674	477365.203756	50.836033
3480.301292	476999.622692	50.841037
3479.531334	476631.844750	50.846042
3478.935399	476255.315021	50.851047
3478.190947	475886.860496	50.856052
3477.764498	475503.396824	50.861057
3477.274675	475124.244193	50.866061
3476.129206	474761.255886	50.871066
3475.822878	474374.811934	50.876071
3475.169030	474000.682279	50.881076
3474.512868	473614.887416	50.886081
3473.826185	473245.615280	50.891085
3473.118036	472862.703758	50.896090
3472.569065	472478.340496	50.901095
3471.941633	472092.056056	50.906100
3471.453981	471709.037393	50.911105
3470.623420	471335.799346	50.916109
3469.777070	470938.425486	50.921114
3469.090298	470551.006150	50.926119
3468.769130	470163.065469	50.931124
3468.077650	469775.835154	50.936129
3467.144161	469390.359681	50.941133
3466.488543	469000.675628	50.946138
3466.230412	468624.763152	50.951143
3465.406944	468231.998436	50.956148
3464.721487	467849.598865	50.961153
3464.250982	467455.851119	50.966157
3463.172643	467054.636891	50.971162
3462.709640	466671.673648	50.976167
3462.177126	466268.177759	50.981172
3461.239710	465888.114944	50.986177
3460.824372	465493.662633	50.991181
3459.991157	465123.965137	50.996186
3459.493675	464713.588193	51.001191
3458.386422	464334.132963	51.006196
3457.731662	463928.076334	51.011201
3457.173635	463546.846760	51.016205
3456.449028	463165.687460	51.021210
3455.615051	462771.910364	51.026215
3454.990550	462378.853707	51.031220
3454.088308	461994.303712	51.036225
3453.487068	461612.184519	51.041229
3452.563902	461223.313029	51.046234
3452.041876	460831.226475	51.051239
3451.423116	460459.233913	51.056244
3450.522108	460079.823425	51.061249
3450.027611	459695.371194	51.066253
3449.140331	459326.800275	51.071258
3448.272666	458938.640178	51.076263
3447.943994	458560.330315	51.081268
3447.320776	458183.125791	51.086273
3446.755575	457793.274446	51.091277
3445.615417	457419.638836	51.096282
3445.289685	457029.939118	51.101287
3444.235272	456658.255589	51.106292
3443.722078	456271.210200	51.111297
3443.285017	455895.915910	51.116301
3442.442045	455532.398801	51.121306
3441.640061	455139.037869	51.126311
3440.795312	454764.955978	51.131316
3440.231745	454385.343986	51.136321
3439.561054	454006.808007	51.141325
3438.534262	453642.376185	51.146330
3437.978834	453264.367675	51.151335
3437.722031	452902.440608	51.156340
3436.757167	452525.144142	51.161345
3435.892261	452150.058210	51.166349
3435.573540	451773.205308	51.171354
3434.718588	451405.818278	51.176359
3433.749235	451026.518860	51.181364
3432.994120	450659.002618	51.186369
3432.258516	450282.800106	51.191373
3431.515513	449928.565396	51.196378
3431.059936	449549.820164	51.201383
3430.432997	449199.311176	51.206388
3429.598464	448811.174873	51.211393
3428.933496	448453.809713	51.216397
3428.157035	448085.190347	51.221402
3427.634785	447725.304765	51.226407
3426.667800	447367.818517	51.231412
3425.956174	447005.312788	51.236417
3425.487639	446635.505434	51.241421
3424.404369	446286.699836	51.246426
3424.078109	445915.031593	51.251431
3423.261247	445556.479086	51.256436
3422.291240	445199.214269	51.261441
3421.987098	444836.407880	51.266445
3421.262827	444491.224365	51.271450
3420.630641	444123.484814	51.276455
3419.573249	443770.323819	51.281460
3419.157232	443407.614976	51.286465
3418.376622	443044.146148	51.291469
3417.471635	442701.604999	51.296474
3417.093458	442341.006086	51.301479
3416.394455	441988.574511	51.306484
3415.495720	441640.382735	51.311489
3415.173480	441279.759210	51.316493
3414.065630	440928.544483	51.321498
3413.562188	440581.391897	51.326503
3412.854805	440227.159389	51.331508
3411.962301	439877.164675	51.336513
3411.390748	439530.185665	51.341517
3410.772536	439183.107610	51.346522
3409.907418	438826.417618	51.351527
3409.222157	438487.387267	51.356532
3408.522088	438133.504298	51.361537
3407.842840	437792.331147	51.366541
3406.974040	437455.168874	51.371546
3406.728034	437102.367208	51.376551
3405.743040	436751.632177	51.381556
3404.504338	436407.304471	51.386561
3404.181030	436072.398308	51.391565
3403.287837	435738.110936	51.396570
3402.755814	435398.963706	51.401575
3402.022779	435057.177940	51.406580
3401.033041	434726.345258	51.411585
3400.689104	434396.802545	51.416589
3399.962698	434063.329921	51.421594
3398.805576	433733.932596	51.426599
3398.411119	433400.043364	51.431604
3397.545874	433071.530783	51.436609
3397.109094	432736.040006	51.441613
3396.441103	432410.179179	51.446618
3396.043737	432068.706606	51.451623
3395.453829	431737.061114	51.456628
3394.280800	431416.676008	51.461633
3393.864423	431071.790773	51.466637
3392.781217	430751.230896	51.471642
3392.220310	430420.554308	51.476647
3391.578504	430096.158437	51.481652
3390.954012	429759.439957	51.486657
3390.198654	429437.085356	51.491661
3389.063397	429118.342046	51.496666
3388.515771	428789.699705	51.501671
3388.053548	428475.768722	51.506676
3387.261686	428150.610731	51.511681
3386.537453	427835.494618	51.516685
3385.581369	427522.798617	51.521690
3385.312998	427190.740055	51.526695
3384.642413	426884.111839	51.531700
3383.936419	426551.505012	51.536705
3383.514033	426239.192114	51.541709
3382.384851	425925.895263	51.546714
3381.902008	425601.546248	51.551719
3381.360581	425273.062752	51.556724
3380.615739	424964.595721	51.561729
3379.769791	424632.368278	51.566733
3379.048508	424324.880773	51.571738
3377.993886	424002.965085	51.576743
3377.585130	423691.534960	51.581748
3376.607824	423383.950318	51.586753
3376.050183	423059.227160	51.591757
3375.198768	422758.727545	51.596762
3374.755975	422454.019761	51.601767
3373.894288	422140.662403	51.606772
3373.281006	421833.282239	51.611777
3372.865774	421529.804537	51.616781
3371.863501	421212.089864	51.621786
3371.205463	420902.394906	51.626791
3370.569936	420599.678524	51.631796
3369.762477	420306.588144	51.636801
3369.366170	419995.317581	51.641805
3368.521629	419693.970777	51.646810
3367.831064	419382.409699	51.651815
3367.142095	419074.757055	51.656820
3366.430853	418779.374593	51.661825
3365.719809	418471.693458	51.666829
3365.014630	418173.458453	51.671834
3364.451425	417880.659843	51.676839
3363.669123	417574.174252	51.681844
3362.823648	417272.420702	51.686849
3362.291684	416962.637095	51.691853
3361.640182	416669.052437	51.696858
3360.764164	416357.995600	51.701863
3360.396795	416075.614759	51.706868
3359.527404	415777.914241	51.711873
3358.820700	415476.373919	51.716877
3358.306492	415185.852038	51.721882
3357.601625	414882.806230	51.726887
3356.873223	414590.152639	51.731892
3355.998679	414288.931400	51.736897
3355.331621	413991.180541	51.741901
3354.433399	413701.212720	51.746906
3353.816751	413409.241045	51.751911
3353.122227	413109.529109	51.756916
3352.254869	412826.535170	51.761921
3351.672157	412543.823820	51.766925
3351.081838	412253.056157	51.771930
3350.508544	411966.196046	51.776935
3350.108482	411680.347575	51.781940
3349.653297	411401.569115	51.786945
3349.115427	411088.852723	51.791949
3348.057546	410795.095476	51.796954
3347.321518	410502.732872	51.801959
3346.490027	410210.331690	51.806964
3345.603494	409913.514768	51.811969
3344.962131	409628.752134	51.816973
3344.095263	409360.286130	51.821978
3343.677646	409061.277476	51.826983
3342.970417	408774.611299	51.831988
3341.939950	408513.965286	51.836993
3341.398593	408223.659083	51.841997
3340.626314	407940.807273	51.847002
3340.208063	407663.004947	51.852007
3339.304284	407375.975503	51.857012
3338.771303	407091.324465	51.862017
3338.000067	406827.141385	51.867021
3337.443663	406537.558603	51.872026
3336.862574	406257.583705	51.877031
3336.398046	405975.376758	51.882036
3335.349248	405704.696387	51.887041
3334.978634	405415.404133	51.892045
3334.132168	405135.740656	51.897050
3333.127676	404857.980426	51.902055
3332.586100	404575.035925	51.907060
3332.010819	404309.682160	51.912065
3331.350026	404026.700739	51.917069
3330.358873	403750.250246	51.922074
3329.795233	403472.331798	51.927079
3329.178055	403190.886409	51.932084
3328.275127	402931.774629	51.937089
3327.689997	402651.691920	51.942093
3327.008889	402383.110713	51.947098
3326.388311	402120.109605	51.952103
3326.103282	401841.446560	51.957108
3325.281138	401568.000536	51.962113
3324.986693	401297.925648	51.967117
3323.881667	401017.224558	51.972122
3323.074880	400742.015192	51.977127
3322.706091	400472.783978	51.982132
3321.432356	400200.744995	51.987137
3321.269028	399921.537730	51.992141
3320.575957	399656.621527	51.997146
3319.865436	399377.724918	52.002151
3319.177083	399108.202493	52.007156
3318.390804	398834.193917	52.012161
3317.983830	398553.996685	52.017165
3317.167806	398293.486677	52.022170
3316.621460	398031.177906	52.027175
3315.590862	397749.013355	52.032180
3314.788958	397479.139657	52.037185
3314.269433	397207.795491	52.042189
3313.495666	396940.785623	52.047194
3312.639108	396676.684831	52.052199
3311.952706	396402.386114	52.057204
3311.480629	396136.237307	52.062209
3310.803407	395875.203377	52.067213
3309.994499	395612.840834	52.072218
3309.379129	395343.378014	52.077223
3308.906514	395086.907204	52.082228
3308.244061	394824.998422	52.087233
3307.428775	394554.645697	52.092237
3306.465965	394294.966770	52.097242
3305.862291	394031.186633	52.102247
3305.270465	393774.724781	52.107252
3304.582087	393518.657646	52.112257
3304.099757	393248.521592	52.117261
3303.121282	392995.572824	52.122266
3302.384377	392739.787236	52.127271
3301.693536	392480.534636	52.132276
3300.915993	392232.023338	52.137281
3300.404647	391964.195541	52.142285
3299.738423	391723.875475	52.147290
3299.122796	391464.374560	52.152295
3298.397182	391209.211562	52.157300
3297.828696	390967.980919	52.162305
3297.253384	390701.729989	52.167309
3296.389208	390452.533210	52.172314
3295.927493	390203.016745	52.177319
3295.685755	389934.723962	52.182324
3294.889122	389667.839127	52.187329
3294.386402	389409.729131	52.192333
3293.218690	389149.967930	52.197338
3292.787651	388887.469252	52.202343
3292.150840	388639.291741	52.207348
3291.130664	388373.907394	52.212353
3290.583263	388116.583393	52.217357
3289.689014	387858.091837	52.222362
3289.292307	387601.070889	52.227367
3288.317645	387340.655759	52.232372
3287.433734	387091.158922	52.237377
3286.869614	386842.779537	52.242381
3286.177459	386586.942444	52.247386
3285.271866	386343.801274	52.252391
3284.793535	386079.128148	52.257396
3284.129022	385850.898299	52.262401
3283.475903	385592.149056	52.267405
3282.879761	385348.748899	52.272410
3282.111504	385094.591828	52.277415
3281.399827	384855.122986	52.282420
3280.749737	384613.913557	52.287425
3280.254245	384357.597527	52.292429
3279.574727	384118.678328	52.297434
3278.833331	383863.643920	52.302439
3277.976938	383614.882111	52.307444
3277.264789	383380.591888	52.312449
3276.807734	383127.948935	52.317453
3275.922161	382895.641371	52.322458
3275.333501	382643.499193	52.327463
3274.592303	382393.261452	52.332468
3273.877003	382154.309991	52.337473
3273.240859	381913.513355	52.342477
3272.767137	381676.682456	52.347482
3272.037834	381426.131273	52.352487
3271.459753	381193.357727	52.357492
3270.692167	380942.733135	52.362497
3270.164453	380696.799591	52.367501
3269.512887	380444.678261	52.372506
3268.466903	380209.251368	52.377511
3267.917863	379974.812663	52.382516
3267.065775	379722.820080	52.387521
3266.204560	379481.509696	52.392525
3265.719749	379247.641432	52.397530
3264.988694	379010.555092	52.402535
3264.488215	378770.760198	52.407540
3263.488011	378543.073578	52.412545
3262.946171	378298.398845	52.417549
3262.488969	378065.027862	52.422554
3261.481635	377829.860302	52.427559
3260.945056	377596.804334	52.432564
3260.293886	377368.165485	52.437569
3259.863916	377121.965082	52.442573
3259.180991	376894.727505	52.447578
3258.518765	376662.652506	52.452583
3258.325750	376417.325977	52.457588
3257.007680	376187.081629	52.462593
3256.330690	375950.248242	52.467597
3255.605098	375720.136433	52.472602
3254.877883	375478.602439	52.477607
3254.211719	375243.696396	52.482612
3253.240775	375019.800602	52.487617
3252.802155	374789.281997	52.492621
3252.147334	374570.039618	52.497626
3251.366876	374327.769528	52.502631
3251.021903	374103.108313	52.507636
3250.317757	373873.389682	52.512641
3249.934110	373632.833373	52.517645
3249.176219	373402.484669	52.522650
3248.324207	373175.227599	52.527655
3247.456977	372949.574309	52.532660
3246.719527	372718.582611	52.537665
3246.426628	372481.337713	52.542669
3245.505344	372255.536581	52.547674
3244.689645	372019.389313	52.552679
3244.458908	371789.609714	52.557684
3243.340532	371562.589513	52.562689
3242.847963	371336.232276	52.567693
3242.139711	371114.080024	52.572698
3241.199856	370883.644480	52.577703
3240.864454	370648.329389	52.582708
3240.143183	370436.453321	52.587713
3239.580018	370199.034826	52.592717
3239.010319	369972.784290	52.597722
3238.015883	369744.284677	52.602727
3237.735979	369513.279417	52.607732
3236.929974	369289.047016	52.612737
3236.178968	369043.358215	52.617741
3235.595332	368832.571858	52.622746
3234.858725	368606.111585	52.627751
3234.574657	368370.699594	52.632756
3233.481195	368146.481318	52.637761
3232.854625	367909.238364	52.642765
3232.171102	367693.908292	52.647770
3231.235213	367466.430535	52.652775
3230.973323	367235.308574	52.657780
3229.984518	367020.481452	52.662785
3229.514572	366782.673372	52.667789
3228.828013	366556.194611	52.672794
3228.243569	366327.128869	52.677799
3227.307005	366095.675179	52.682804
3226.991579	365885.722769	52.687809
3226.078224	365661.412519	52.692813
3225.450485	365435.478511	52.697818
3224.656293	365213.055384	52.702823
3223.972306	364992.827274	52.707828
3223.175756	364777.780864	52.712833
3222.734513	364540.719651	52.717837
3222.168665	364316.983835	52.722842
3221.454018	364096.527237	52.727847
3220.744107	363879.630942	52.732852
3219.773872	363660.790185	52.737857
3219.588432	363431.290447	52.742861
3219.375417	363217.696462	52.747866
3218.152277	362991.997195	52.752871
3217.563695	362755.408058	52.757876
3216.571443	362533.359455	52.762881
3216.141349	362313.536315	52.767885
3215.460125	362096.779781	52.772890
3214.711868	361869.880377	52.777895
3214.170002	361646.484067	52.782900
3213.264714	361425.892250	52.787905
3212.394430	361201.502535	52.792909
3211.847677	360981.742502	52.797914
3211.108985	360766.897328	52.802919
3210.747356	360544.357880	52.807924
3209.966473	360334.123060	52.812929
3209.062637	360113.906592	52.817933
3208.588973	359897.666948	52.822938
3207.821929	359682.897715	52.827943
3207.056170	359462.401953	52.832948
3206.361279	359249.400597	52.837953
3205.732700	359023.028501	52.842957
3205.084789	358820.272686	52.847962
3204.357119	358614.042468	52.852967
3204.056242	358391.636138	52.857972
3203.026254	358187.818482	52.862977
3202.546033	357954.420094	52.867981
3201.916901	357749.748347	52.872986
3200.966659	357537.466979	52.877991
3200.396016	357311.713971	52.882996
3199.695780	357101.197927	52.888001
3199.245568	356887.358719	52.893005
3198.279281	356676.704833	52.898010
3197.239651	356466.748747	52.903015
3197.191393	356252.257928	52.908020
3196.303086	356054.109368	52.913025
3195.712792	355835.452731	52.918029
3195.385254	355626.983695	52.923034
3194.426434	355416.425129	52.928039
3194.020240	355192.723296	52.933044
3192.772892	354997.172218	52.938049
3192.466195	354776.073993	52.943053
3191.650447	354563.962352	52.948058
3190.508962	354361.393727	52.953063
3189.983338	354145.137214	52.958068
3189.433106	353947.868563	52.963073
3188.740593	353741.536377	52.968077
3188.277279	353530.586269	52.973082
3187.484712	353330.096117	52.978087
3186.943678	353117.018892	52.983092
3186.310781	352916.298290	52.988097
3185.725329	352704.906071	52.993101
3185.122379	352497.943999	52.998106
3184.059628	352293.547927	53.003111
3184.079868	352083.202617	53.008116
3182.988495	351871.708944	53.013121
3182.389041	351659.474900	53.018125
3182.132895	351445.760486	53.023130
3181.157296	351249.439730	53.028135
3180.598511	351029.867085	53.033140
3179.813482	350814.884957	53.038145
3179.015352	350602.092785	53.043149
3178.482176	350393.584456	53.048154
3177.327008	350190.492927	53.053159
3176.911128	349984.102321	53.058164
3176.205120	349779.411142	53.063169
3175.550989	349572.471298	53.068173
3174.479960	349370.025118	53.073178
3173.926504	349173.350073	53.078183
3173.669968	348960.898461	53.083188
3172.616701	348764.377384	53.088193
3172.205080	348569.230274	53.093197
3171.938026	348353.163881	53.098202
3170.733285	348153.355898	53.103207
3170.330590	347951.638680	53.108212
3169.668442	347746.805756	53.113217
3168.745323	347543.056902	53.118221
3168.333375	347338.335611	53.123226
3167.314794	347141.701517	53.128231
3166.656570	346932.843574	53.133236
3165.940960	346748.479040	53.138241
3165.400347	346543.138920	53.143245
3164.614517	346332.059147	53.148250
3164.236580	346137.661840	53.153255
3163.437594	345939.588954	53.158260
3162.659807	345743.471890	53.163265
3162.189981	345531.219251	53.168269
3161.509430	345329.740302	53.173274
3160.655517	345136.687570	53.178279
3160.287997	344929.685309	53.183284
3159.415891	344724.467511	53.188289
3158.712607	344522.760285	53.193293
3158.433762	344324.625038	53.198298
3157.581946	344133.477660	53.203303
3156.797562	343931.017631	53.208308
3156.227235	343729.133926	53.213313
3155.586334	343525.046228	53.218317
3154.901476	343327.633675	53.223322
3154.296490	343130.335100	53.228327
3153.615053	342930.273490	53.233332
3152.751928	342728.559993	53.238337
3152.396347	342519.918356	53.243341
3151.630406	342323.635308	53.248346
3150.844900	342127.354719	53.253351
3150.464322	341928.209444	53.258356
3149.354652	341714.644384	53.263361
3148.641356	341514.328588	53.268365
3148.110051	341321.517909	53.273370
3147.528647	341137.750971	53.278375
3147.049416	340921.563381	53.283380
3145.982819	340722.268188	53.288385
3145.278487	340534.267942	53.293389
3145.231122	340332.417463	53.298394
3144.129215	340133.660525	53.303399
3143.546058	339931.766252	53.308404
3143.138580	339741.883875	53.313409
3142.019055	339543.356952	53.318413
3141.444709	339335.070077	53.323418
3140.633997	339144.918786	53.328423
3140.240082	338938.918512	53.333428
3139.267552	338742.274990	53.338433
3138.516077	338546.919584	53.343437
3138.119114	338345.550825	53.348442
3137.486202	338157.277650	53.353447
3136.926584	337955.729762	53.358452
3136.058755	337761.968656	53.363457
3135.472734	337565.744048	53.368461
3134.830895	337374.618924	53.373466
3134.016507	337181.280389	53.378471
3133.646475	336971.935290	53.383476
3132.719541	336780.089850	53.388481
3131.788206	336590.510179	53.393485
3131.459440	336388.666368	53.398490
3130.696103	336195.596887	53.403495
3130.101412	336003.722084	53.408500
3129.268230	335823.772797	53.413505
3128.803365	335616.856824	53.418509
3127.894764	335426.939306	53.423514
3126.983971	335237.199798	53.428519
3126.422270	335043.305927	53.433524
3125.744951	334863.762184	53.438529
3125.141675	334672.954152	53.443533
3124.656710	334480.752170	53.448538
3123.789884	334295.076248	53.453543
3123.072197	334104.819342	53.458548
3122.084223	333929.904647	53.463553
3121.653561	333743.114463	53.468557
3121.154960	333548.264449	53.473562
3120.311202	333371.823525	53.478567
3120.017125	333183.075437	53.483572
3119.148010	332996.505377	53.488577
3118.508758	332819.266964	53.493581
3118.294435	332616.273754	53.498586
3117.380461	332426.425201	53.503591
3116.389445	332234.118893	53.508596
3115.820976	332051.826648	53.513601
3115.172052	331858.370491	53.518605
3114.515500	331673.952727	53.523610
3113.669987	331490.786393	53.528615
3113.192615	331300.407512	53.533620
3112.274174	331115.495133	53.538625
3111.711115	330931.977186	53.543629
3111.229858	330746.867396	53.548634
3110.801726	330560.730382	53.553639
3110.012357	330366.325034	53.558644
3109.427115	330185.532816	53.563649
3108.799548	329988.784113	53.568653
3108.292560	329801.690221	53.573658
3107.685440	329614.331653	53.578663
3106.675998	329424.846796	53.583668
3106.511046	329230.339662	53.588673
3105.481160	329042.206409	53.593677
3104.785950	328854.019726	53.598682
3104.160876	328657.318046	53.603687
3103.442012	328461.470861	53.608692
3102.587895	328275.701076	53.613697
3102.128221	328092.007025	53.618701
3101.613382	327890.372230	53.623706
3100.662405	327711.388667	53.628711
3099.929891	327521.753405	53.633716
3099.256223	327340.077287	53.638721
3098.582056	327153.487069	53.643725
3098.064957	326959.717310	53.648730
3096.929299	326776.203493	53.653735
3096.584130	326589.941771	53.658740
3095.686929	326407.102241	53.663745
3095.349809	326223.155251	53.668749
3094.869895	326033.603722	53.673754
3093.974424	325842.488045	53.678759
3093.600957	325657.501631	53.683764
3093.095811	325479.078954	53.688769
3092.012428	325287.686170	53.693773
3091.495624	325100.455180	53.698778
3090.835909	324916.632633	53.703783
3090.044633	324726.592634	53.708788
3089.473440	324532.876485	53.713793
3088.638509	324350.353429	53.718797
3088.225321	324158.113580	53.723802
3087.107300	323981.439575	53.728807
3086.638929	323800.308568	53.733812
3086.144696	323604.770344	53.738817
3085.577541	323421.362661	53.743821
3084.739821	323231.759426	53.748826
3084.095668	323052.793356	53.753831
3083.364139	322857.418257	53.758836
3082.489556	322679.557237	53.763841
3081.669017	322493.590596	53.768845
3081.453568	322305.694574	53.773850
3080.328620	322132.047705	53.778855
3079.787899	321945.831906	53.783860
3079.218668	321772.554678	53.788865
3078.534051	321593.159125	53.793869
3077.773353	321409.879612	53.798874
3077.000215	321230.955635	53.803879
3076.594162	321048.153940	53.808884
3076.091405	320876.952286	53.813889
3075.276418	320692.101243	53.818893
3074.789209	320508.700197	53.823898
3074.027018	320328.983350	53.828903
3072.930926	320147.027406	53.833908
3072.568064	319959.964494	53.838913
3072.005413	319784.339835	53.843917
3071.368614	319600.018517	53.848922
3070.230884	319420.664845	53.853927
3069.778600	319248.688247	53.858932
3069.392765	319071.862974	53.863937
3068.265894	318886.802988	53.868941
3067.916254	318701.797867	53.873946
3067.352542	318529.710255	53.878951
3066.653728	318354.282659	53.883956
3065.787696	318174.374329	53.888961
3064.949974	317998.866204	53.893965
3064.663431	317819.145577	53.898970
3063.872285	317644.316916	53.903975
3063.281098	317456.521220	53.908980
3062.686279	317272.341447	53.913985
3062.206802	317097.487927	53.918989
3062.070631	316903.024268	53.923994
3060.950640	316723.408031	53.928999
3060.205801	316542.127925	53.934004
3059.293765	316351.936422	53.939009
3058.724955	316177.553726	53.944013
3058.241629	315990.909434	53.949018
3057.328119	315807.388454	53.954023
3056.938642	315633.001883	53.959028
3056.174295	315451.060824	53.964033
3055.249543	315273.880996	53.969037
3054.835545	315086.230978	53.974042
3054.059377	314902.050027	53.979047
3053.618369	314725.072779	53.984052
3052.937726	314546.197927	53.989057
3052.100243	314364.164646	53.994061
3051.449617	314175.124453	53.999066
3050.813423	313991.327136	54.004071
3050.266004	313795.318351	54.009076
3049.578008	313621.943224	54.014081
3048.937725	313446.879652	54.019085
3048.096843	313257.435032	54.024090
3047.344066	313071.923026	54.029095
3046.842890	312900.426940	54.034100
3046.048478	312725.692144	54.039105
3045.536175	312546.481687	54.044109
3044.870804	312353.366347	54.049114
3043.979402	312178.111276	54.054119
3043.756201	311988.872238	54.059124
3043.018824	311807.175244	54.064129
3042.316753	311635.021431	54.069133
3041.712289	311435.376011	54.074138
3040.967589	311266.054903	54.079143
3040.085312	311077.020481	54.084148
3039.781445	310905.388200	54.089153
3038.985273	310720.159205	54.094157
3038.247221	310526.924880	54.099162
3037.421384	310352.624222	54.104167
3036.930027	310168.211882	54.109172
3036.230152	309992.159157	54.114177
3035.108754	309814.415825	54.119181
3034.681062	309635.034550	54.124186
3034.152083	309459.743378	54.129191
3033.325763	309282.436366	54.134196
3032.653920	309098.611133	54.139201
3031.791779	308927.064292	54.144205
3031.343262	308745.851505	54.149210
3030.550589	308584.402710	54.154215
3029.686913	308400.708631	54.159220
3029.275381	308227.128681	54.164225
3028.486718	308057.733497	54.169229
3028.269509	307875.235023	54.174234
3027.289210	307703.144930	54.179239
3026.537700	307531.680479	54.184244
3025.952843	307355.401977	54.189249
3025.460354	307179.719771	54.194253
3024.899770	307007.638689	54.199258
3024.036571	306831.479907	54.204263
3023.163773	306658.531022	54.209268
3022.367629	306477.217161	54.214273
3021.618063	306313.568598	54.219277
3021.119460	306142.138644	54.224282
3020.546928	305968.657471	54.229287
3020.094341	305796.837801	54.234292
3019.980171	305618.954498	54.239297
3018.526994	305441.868601	54.244301
3018.306068	305271.972427	54.249306
3017.736704	305094.975371	54.254311
3016.896645	304917.868136	54.259316
3016.242633	304730.494048	54.264321
3015.673035	304560.168322	54.269325
3015.084857	304379.557195	54.274330
3014.315537	304196.758987	54.279335
3013.756720	304018.307327	54.284340
3013.324308	303834.869607	54.289345
3012.563369	303664.598538	54.294349
3011.669049	303479.017944	54.299354
3011.229297	303302.303678	54.304359
3010.228003	303131.993620	54.309364
3009.939711	302940.688442	54.314369
3008.830475	302773.883883	54.319373
3008.252555	302585.348940	54.324378
3007.554571	302418.045960	54.329383
3006.800786	302236.363303	54.334388
3006.259817	302064.323852	54.339393
3005.335654	301890.638628	54.344397
3005.056903	301698.133430	54.349402
3004.316987	301539.570996	54.354407
3003.391404	301359.238720	54.359412
3003.120584	301183.080919	54.364417
3002.142359	301009.428720	54.369421
3001.798805	300823.757645	54.374426
3001.015995	300647.043625	54.379431
3000.210718	300474.764108	54.384436
2999.455369	300295.524181	54.389441
2998.661996	300126.018240	54.394445
2998.317215	299941.594186	54.399450
2997.734976	299775.441493	54.404455
2996.919594	299600.234002	54.409460
2996.297166	299417.483162	54.414465
2995.590273	299250.560211	54.419469
2995.048798	299066.140847	54.424474
2994.086030	298895.005129	54.429479
2993.737101	298723.823008	54.434484
2992.931126	298541.966139	54.439489
2992.144704	298377.117717	54.444493
2991.969879	298195.440712	54.449498
2991.093770	298034.808168	54.454503
2990.291046	297847.423783	54.459508
2989.481129	297671.576785	54.464513
2988.369037	297508.128842	54.469517
2988.218837	297329.477602	54.474522
2987.654089	297155.806907	54.479527
2987.118219	296985.009231	54.484532
2986.449234	296812.398853	54.489537
2985.570020	296640.152663	54.494541
2985.005036	296456.778457	54.499546
2984.292458	296282.824745	54.504551
2983.764898	296096.311832	54.509556
2983.288754	295932.074230	54.514561
2982.627763	295771.329265	54.519565
2981.707372	295580.243039	54.524570
2980.947334	295412.077080	54.529575
2980.280079	295228.081225	54.534580
2979.697732	295050.896948	54.539585
2978.631730	294896.505767	54.544589
2978.443670	294723.588204	54.549594
2977.536640	294546.327550	54.554599
2976.872313	294365.488384	54.559604
2976.413866	294194.013878	54.564609
2975.450120	294023.332304	54.569613
2975.226261	293844.816889	54.574618
2974.414058	293673.856374	54.579623
2973.825506	293496.671766	54.584628
2973.295891	293324.061804	54.589633
2972.251180	293156.397511	54.594637
2972.278993	292972.671674	54.599642
2971.249079	292797.721103	54.604647
2970.714717	292627.912770	54.609652
2970.074245	292440.599520	54.614657
2968.998869	292259.594489	54.619661
2968.850407	292085.930023	54.624666
2967.774394	291909.687241	54.629671
2966.848028	291746.103456	54.634676
2966.811512	291562.208420	54.639681
2965.761905	291391.971417	54.644685
2965.221968	291209.862135	54.649690
2964.829155	291036.031860	54.654695
2964.069808	290856.911295	54.659700
2963.600087	290676.776986	54.664705
2962.868361	290504.324316	54.669709
2962.070244	290317.823903	54.674714
2961.303919	290137.965385	54.679719
2960.876992	289957.263520	54.684724
2960.427040	289782.473685	54.689729
2959.309003	289605.140858	54.694733
2958.901190	289413.127944	54.699738
2958.002149	289247.933796	54.704743
2957.068997	289069.552652	54.709748
2956.523694	288893.121954	54.714753
2956.026245	288718.517254	54.719757
2955.529691	288530.592646	54.724762
2954.885552	288362.199636	54.729767
2954.146328	288181.036731	54.734772
2953.815934	287996.472709	54.739777
2952.916981	287829.316735	54.744781
2952.283509	287629.035866	54.749786
2951.461233	287459.728257	54.754791
2950.866657	287279.891734	54.759796
2950.427899	287090.097955	54.764801
2949.228503	286912.725498	54.769805
2948.514383	286733.264157	54.774810
2947.723054	286565.606613	54.779815
2947.249150	286385.623172	54.784820
2946.773625	286211.879554	54.789825
2945.889458	286052.004200	54.794829
2945.283221	285867.839230	54.799834
2944.797066	285695.727002	54.804839
2944.113806	285518.679633	54.809844
2943.612535	285347.435554	54.814849
2942.290541	285161.931877	54.819853
2941.993826	284984.975879	54.824858
2941.492686	284808.510592	54.829863
2940.823482	284636.019390	54.834868
2940.189077	284455.525624	54.839873
2939.503123	284289.531299	54.844877
2938.863274	284104.071965	54.849882
2938.520396	283926.537065	54.854887
2937.524482	283743.349679	54.859892
2937.053480	283559.671629	54.864897
2936.391725	283391.049922	54.869901
2935.816260	283203.797261	54.874906
2935.129585	283023.820567	54.879911
2934.153722	282847.455138	54.884916
2933.988738	282655.476608	54.889921
2933.430818	282488.264378	54.894925
2932.681615	282299.765482	54.899930
2932.127684	282115.183181	54.904935
2930.847593	281926.844611	54.909940
2930.502722	281739.147435	54.914945
2929.616959	281573.693210	54.919949
2929.236970	281377.495085	54.924954
2928.445140	281201.354689	54.929959
2927.641657	281013.908177	54.934964
2927.292444	280832.807699	54.939969
2926.478061	280666.297742	54.944973
2925.835410	280474.496011	54.949978
2925.201167	280297.668258	54.954983
2924.570695	280112.613604	54.959988
2923.928641	279936.296371	54.964993
2923.076019	279749.672300	54.969997
2922.520748	279548.305889	54.975002
2921.620312	279364.872844	54.980007
2920.728082	279183.501398	54.985012
2920.501068	278992.983340	54.990017
2919.675049	278825.914550	54.995021
2919.286733	278641.763580	55.000026
2918.264662	278470.752711	55.005031
2917.770828	278281.499249	55.010036
2917.190382	278098.168128	55.015041
2916.133524	277914.403041	55.020045
2915.687036	277740.957854	55.025050
2915.054429	277566.778062	55.030055
2914.066272	277389.776616	55.035060
2913.687568	277203.688324	55.040065
2912.969552	277036.143774	55.045069
2912.267909	276858.281925	55.050074
2911.486246	276678.879157	55.055079
2911.070405	276500.590003	55.060084
2910.364926	276319.112208	55.065089
2909.432800	276156.134865	55.070093
2909.159150	275963.280715	55.075098
2908.500868	275788.391730	55.080103
2907.703861	275617.166681	55.085108
2907.333537	275429.752581	55.090113
2906.596845	275252.787585	55.095117
2905.861110	275070.601415	55.100122
2905.259548	274901.102727	55.105127
2904.500358	274719.837131	55.110132
2904.238267	274535.309282	55.115137
2903.343606	274357.197751	55.120141
2902.799990	274165.405055	55.125146
2902.184291	273980.831332	55.130151
2900.957316	273809.470619	55.135156
2900.627056	273618.688368	55.140161
2899.879068	273444.424845	55.145165
2899.194431	273264.217168	55.150170
2898.579272	273076.969230	55.155175
2898.122033	272904.187812	55.160180
2897.618443	272721.048117	55.165185
2896.925750	272539.848510	55.170189
2895.862382	272359.930092	55.175194
2895.341475	272170.935471	55.180199
2894.417335	271998.559156	55.185204
2894.055488	271816.008362	55.190209
2893.591671	271631.818294	55.195213
2892.825675	271446.504553	55.200218
2892.323102	271253.050198	55.205223
2891.596229	271067.653918	55.210228
2890.879592	270885.643340	55.215233
2890.219676	270712.766946	55.220237
2889.503505	270520.619961	55.225242
2889.174834	270331.900823	55.230247
2888.236548	270143.889486	55.235252
2887.488382	269964.354506	55.240257
2886.998642	269785.491759	55.245261
2886.415592	269592.508917	55.250266
2885.890281	269405.221880	55.255271
2884.978556	269221.077736	55.260276
2884.661788	269020.641606	55.265281
2883.697285	268847.228064	55.270285
2882.932450	268655.853289	55.275290
2882.247995	268469.865114	55.280295
2881.625810	268277.041640	55.285300
2881.324822	268088.598845	55.290305
2880.410349	267905.525171	55.295309
2879.644948	267715.042164	55.300314
2878.971320	267526.531211	55.305319
2878.155519	267346.956709	55.310324
2877.628998	267155.901237	55.315329
2876.870196	266976.852666	55.320333
2876.640921	266791.200455	55.325338
2875.979197	266609.233267	55.330343
2874.767299	266449.434166	55.335348
2874.593329	266276.940435	55.340353
2874.012798	266069.543369	55.345357
2873.124975	265868.842238	55.350362
2872.753097	265671.395824	55.355367
2871.691343	265474.262480	55.360372
2871.288881	265286.651775	55.365377
2870.438455	265104.231171	55.370381
2869.992884	264910.184032	55.375386
2869.460186	264717.220439	55.380391
2868.398264	264526.683798	55.385396
2867.747543	264340.080623	55.390401
2867.081649	264158.216994	55.395405
2866.296488	263968.859270	55.400410
2865.797069	263775.228707	55.405415
2864.998774	263587.528678	55.410420
2864.414452	263407.358856	55.415425
2863.802875	263231.981419	55.420429
2863.034725	263042.061191	55.425434
2862.774338	262834.997144	55.430439
2861.562494	262663.993660	55.435444
2861.338455	262466.067070	55.440449
2860.392501	262284.987321	55.445453
2859.520844	262103.386551	55.450458
2859.177884	261916.965142	55.455463
2858.136711	261731.010954	55.460468
2857.629115	261540.388175	55.465473
2856.754012	261364.671451	55.470477
2856.148517	261188.326377	55.475482
2855.984953	261000.756533	55.480487
2854.852100	260822.839776	55.485492
2854.283900	260629.654930	55.490497
2853.863790	260446.863072	55.495501
2853.135724	260268.067593	55.500506
2852.636070	260078.666960	55.505511
2851.528455	259905.356439	55.510516
2851.530886	259707.981571	55.515521
2850.410073	259530.140134	55.520525
2849.467770	259346.183782	55.525530
2849.677214	259154.252086	55.530535
2848.697584	258973.994712	55.535540
2847.867514	258783.017395	55.540545
2847.326968	258596.451200	55.545549
2846.460395	258399.749751	55.550554
2846.040298	258215.100301	55.555559
2845.225488	258028.094080	55.560564
2844.887789	257838.185560	55.565569
2844.101476	257654.587760	55.570573
2843.038824	257476.840440	55.575578
2842.557383	257278.168859	55.580583
2842.032746	257096.491050	55.585588
2841.500439	256901.265949	55.590593
2840.753622	256716.389267	55.595597
2839.955448	256527.522497	55.600602
2839.342166	256338.575674	55.605607
2838.351661	256159.824734	55.610612
2838.139349	255972.546506	55.615617
2837.405562	255783.695647	55.620621
2836.881697	255593.334613	55.625626
2836.135169	255407.440305	55.630631
2835.453607	255220.033309	55.635636
2835.126259	255030.227411	55.640641
2834.144025	254837.112796	55.645645
2833.335047	254639.514183	55.650650
2832.747714	254455.989433	55.655655
2831.713942	254271.771538	55.660660
2831.517182	254073.541724	55.665665
2830.974210	253891.411160	55.670669
2830.183569	253697.528767	55.675674
2829.620625	253514.204771	55.680679
2828.815236	253333.873510	55.685684
2828.614790	253136.205514	55.690689
2827.748453	252942.514146	55.695693
2826.971376	252755.175561	55.700698
2826.205954	252556.477108	55.705703
2825.462401	252377.512190	55.710708
2824.752290	252175.571107	55.715713
2824.276660	251988.363840	55.720717
2823.424241	251803.839512	55.725722
2823.066364	251611.902647	55.730727
2822.637001	251428.228517	55.735732
2821.832855	251230.989273	55.740737
2821.171187	251032.454359	55.745741
2820.408554	250837.144455	55.750746
2819.987691	250645.014905	55.755751
2818.793241	250455.249138	55.760756
2818.585122	250256.032112	55.765761
2817.670634	250064.312466	55.770765
2817.217530	249875.117554	55.775770
2816.593688	249680.347289	55.780775
2815.712214	249490.227473	55.785780
2815.198363	249290.525246	55.790785
2814.432267	249099.267102	55.795789
2813.535240	248909.456037	55.800794
2813.055025	248711.659184	55.805799
2811.899419	248530.471660	55.810804
2811.749949	248326.103562	55.815809
2811.045595	248140.744972	55.820813
2809.915232	247956.574585	55.825818
2809.383217	247769.966779	55.830823
2808.769257	247589.866032	55.835828
2808.230514	247399.618103	55.840833
2807.506052	247209.527160	55.845837
2806.813573	247025.721493	55.850842
2806.054098	246838.361434	55.855847
2805.598483	246658.083950	55.860852
2804.882495	246457.067766	55.865857
2804.327567	246280.677295	55.870861
2803.277299	246084.094701	55.875866
2802.732584	245894.129814	55.880871
2802.050590	245715.875701	55.885876
2801.613406	245532.235244	55.890881
2800.790794	245351.253569	55.895885
2800.033061	245165.092331	55.900890
2799.549252	244975.984882	55.905895
2799.046277	244788.867045	55.910900
2798.744536	244607.014429	55.915905
2797.886391	244405.667203	55.920909
2797.073171	244218.675688	55.925914
2796.426532	244020.249540	55.930919
2795.794293	243845.937137	55.935924
2795.517909	243647.070930	55.940929
2794.210352	243456.058863	55.945933
2793.651107	243263.018668	55.950938
2793.071041	243075.737203	55.955943
2792.216298	242890.689522	55.960948
2791.697996	242711.751396	55.965953
2790.939332	242516.401113	55.970957
2790.729968	242323.587040	55.975962
2790.091219	242127.734531	55.980967
2789.135497	241938.451574	55.985972
2789.053506	241748.928668	55.990977
2787.986097	241557.142951	55.995981
2787.213215	241365.132634	56.000986
2786.956837	241166.190770	56.005991
2785.737631	240986.143829	56.010996
2785.132670	240780.662419	56.016001
2784.547008	240592.494324	56.021005
2783.740314	240407.086255	56.026010
2783.573153	240210.118093	56.031015
2782.748356	240015.036939	56.036020
2782.260450	239820.310185	56.041025
2781.581344	239634.730340	56.046029
2780.789475	239433.813567	56.051034
2780.429095	239224.527398	56.056039
2779.331398	239031.579206	56.061044
2778.710473	238841.535158	56.066049
2778.356794	238638.462305	56.071053
2777.655450	238449.501154	56.076058
2776.823882	238246.504698	56.081063
2776.033331	238057.481945	56.086068
2775.413141	237865.096732	56.091073
2774.725713	237676.465723	56.096077
2773.581118	237483.578560	56.101082
2773.494212	237283.929041	56.106087
2772.633844	237101.972519	56.111092
2771.896035	236908.563597	56.116097
2771.428002	236710.223233	56.121101
2770.545588	236527.099837	56.126106
2770.180298	236325.942894	56.131111
2769.454383	236134.035853	56.136116
2768.998712	235944.658190	56.141121
2768.064818	235748.990706	56.146125
2767.430378	235558.139703	56.151130
2766.815887	235362.855235	56.156135
2766.191942	235174.982509	56.161140
2765.421932	234987.031407	56.166145
2764.748637	234789.032754	56.171149
2764.135357	234593.825949	56.176154
2763.649535	234396.078465	56.181159
2762.873047	234210.421521	56.186164
2762.145499	234010.370463	56.191169
2761.353581	233817.918018	56.196173
2760.781255	233641.192822	56.201178
2760.486842	233437.738645	56.206183
2759.713471	233238.587606	56.211188
2759.222299	233045.834400	56.216193
2758.460233	232844.034228	56.221197
2757.977976	232645.958656	56.226202
2757.237815	232444.945193	56.231207
2756.415117	232253.901153	56.236212
2756.040560	232040.455738	56.241217
2755.164135	231843.411836	56.246221
2754.254153	231653.197629	56.251226
2753.974144	231444.932942	56.256231
2753.316908	231249.128688	56.261236
2752.689415	231036.565864	56.266241
2751.612845	230852.261485	56.271245
2750.951467	230657.095690	56.276250
2750.667882	230454.893810	56.281255
2749.779696	230259.382848	56.286260
2748.941975	230057.855245	56.291265
2748.624747	229865.131913	56.296269
2747.593201	229665.494613	56.301274
2747.408987	229471.223328	56.306279
2746.694039	229273.624631	56.311284
2745.605221	229068.345182	56.316289
2745.230006	228873.570748	56.321293
2744.428228	228676.750981	56.326298
2743.763035	228471.711353	56.331303
2743.057004	228293.337003	56.336308
2742.526742	228085.730740	56.341313
2742.056168	227888.936661	56.346317
2741.225877	227697.623298	56.351322
2740.825384	227493.384269	56.356327
2739.680247	227293.031952	56.361332
2739.021272	227092.450329	56.366337
2738.529284	226899.201020	56.371341
2737.847006	226706.898894	56.376346
2737.145822	226497.974094	56.381351
2736.175751	226307.220668	56.386356
2735.825161	226107.891040	56.391361
2735.594835	225917.505083	56.396365
2734.354652	225722.276461	56.401370
2734.199510	225516.704832	56.406375
2733.176223	225314.186485	56.411380
2732.765958	225116.001691	56.416385
2732.365816	224914.429509	56.421389
2731.410455	224717.172225	56.426394
2730.719528	224513.521138	56.431399
2729.904613	224320.418092	56.436404
2729.286933	224112.695472	56.441409
2728.745234	223919.384616	56.446413
2727.737036	223719.859440	56.451418
2727.226888	223520.255871	56.456423
2726.283543	223327.493814	56.461428
2725.567718	223125.148665	56.466433
2725.281095	222933.963904	56.471437
2724.298560	222741.502277	56.476442
2724.005324	222540.224660	56.481447
2723.263601	222353.250635	56.486452
2722.431161	222151.575699	56.491457
2722.203858	221956.666813	56.496461
2721.206032	221760.378357	56.501466
2720.940804	221558.806067	56.506471
2720.044743	221362.387942	56.511476
2719.409409	221163.268513	56.516481
2718.872531	220956.445287	56.521485
2717.547229	220762.197105	56.526490
2717.511426	220567.630589	56.531495
2716.492305	220369.719710	56.536500
2716.086178	220168.517136	56.541505
2715.736379	219969.992106	56.546509
2714.699453	219781.479982	56.551514
2714.148752	219574.891891	56.556519
2713.268010	219383.008200	56.561524
2712.799251	219177.388406	56.566529
2712.110889	218984.495120	56.571533
2711.562959	218788.817840	56.576538
2711.195009	218583.871128	56.581543
2710.296829	218382.611362	56.586548
2709.504749	218182.175475	56.591553
2709.087821	217975.379785	56.596557
2707.885540	217785.396978	56.601562
2707.479148	217572.707198	56.606567
2706.813598	217381.138411	56.611572
2706.328823	217176.570637	56.616577
2705.640335	216984.561040	56.621581
2704.606798	216789.169811	56.626586
2704.038171	216580.276480	56.631591
2703.375816	216387.042401	56.636596
2702.704708	216185.701975	56.641601
2702.094720	215989.202122	56.646605
2701.360679	215792.073310	56.651610
2700.990391	215593.245431	56.656615
2700.431650	215400.837782	56.661620
2699.593838	215186.823445	56.666625
2698.786141	214990.052275	56.671629
2698.068226	214794.298465	56.676634
2697.875616	214591.563134	56.681639
2696.780832	214398.555890	56.686644
2696.318866	214197.850056	56.691649
2695.280682	213993.913984	56.696653
2694.618733	213800.776246	56.701658
2694.322151	213602.833509	56.706663
2693.574115	213403.104546	56.711668
2692.935136	213205.980930	56.716673
2692.138589	212996.791039	56.721677
2691.159979	212801.338922	56.726682
2690.990692	212599.751481	56.731687
2690.303607	212407.652771	56.736692
2689.373558	212210.934637	56.741697
2688.686047	212010.067516	56.746701
2687.749049	211819.499313	56.751706
2687.543018	211622.680990	56.756711
2687.226028	211428.668262	56.761716
2686.099989	211227.860316	56.766721
2685.796112	211025.929980	56.771725
2684.671772	210835.139816	56.776730
2684.497342	210638.854072	56.781735
2683.425751	210445.472982	56.786740
2682.636664	210240.172791	56.791745
2682.168294	210045.500958	56.796749
2681.462358	209854.392911	56.801754
2681.081137	209658.422981	56.806759
2680.283324	209463.856053	56.811764
2679.764982	209257.548890	56.816769
2678.976637	209056.821628	56.821773
2678.172388	208865.744913	56.826778
2677.850383	208669.323256	56.831783
2677.162646	208463.885580	56.836788
2676.313562	208266.594161	56.841793
2675.728199	208073.245227	56.846797
2674.632003	207877.674209	56.851802
2674.436576	207681.184756	56.856807
2673.681547	207483.460974	56.861812
2673.059566	207285.907665	56.866817
2672.685524	207080.997673	56.871821
2671.913403	206892.849267	56.876826
2671.094493	206683.213032	56.881831
2670.434843	206484.306540	56.886836
2669.891929	206285.140407	56.891841
2669.142349	206076.068030	56.896845
2668.607738	205881.929029	56.901850
2667.807612	205687.234574	56.906855
2667.179080	205487.092002	56.911860
2666.645368	205291.605771	56.916865
2665.994360	205084.048493	56.921869
2665.328484	204885.199279	56.926874
2664.713960	204668.881817	56.931879
2663.878778	204475.813213	56.936884
2663.203809	204271.278803	56.941889
2662.581884	204073.736229	56.946893
2661.816739	203879.525872	56.951898
2661.102826	203667.402146	56.956903
2660.285520	203478.711899	56.961908
2659.746777	203271.423320	56.966913
2659.395046	203063.584092	56.971917
2658.196065	202872.538351	56.976922
2657.851102	202669.535421	56.981927
2657.111854	202474.473103	56.986932
2656.468125	202286.141102	56.991937
2656.196031	202077.058462	56.996941
2655.509942	201876.250397	57.001946
2654.706305	201666.286338	57.006951
2654.045929	201471.151387	57.011956
2652.987088	201274.604063	57.016961
2652.870298	201067.765787	57.021965
2651.870964	200877.216984	57.026970
2651.036185	200674.260736	57.031975
2650.315810	200475.181138	57.036980
2649.823303	200292.176684	57.041985
2649.341405	200084.305555	57.046989
2648.417404	199878.948549	57.051994
2648.093040	199692.547224	57.056999
2647.368177	199484.589628	57.062004
2646.773912	199291.780694	57.067009
2646.489703	199075.966969	57.072013
2645.203042	198882.251184	57.077018
2644.789653	198679.948233	57.082023
2643.892449	198482.430992	57.087028
2643.370837	198275.082127	57.092033
2642.755359	198072.978920	57.097037
2642.365611	197875.714377	57.102042
2641.354203	197669.043554	57.107047
2640.624408	197471.770770	57.112052
2639.696343	197279.594618	57.117057
2639.298069	197073.274354	57.122061
2638.790292	196877.673741	57.127066
2638.123522	196676.042107	57.132071
2637.420569	196482.115383	57.137076
2636.903957	196273.526594	57.142081
2636.301050	196068.769673	57.147085
2635.496708	195869.517003	57.152090
2634.843400	195665.113227	57.157095
2634.184765	195469.414580	57.162100
2633.506896	195272.078288	57.167105
2632.928200	195064.598517	57.172109
2631.967118	194860.971994	57.177114
2631.371259	194655.634275	57.182119
2630.925380	194457.411854	57.187124
2630.000346	194260.767569	57.192129
2629.656962	194056.791918	57.197133
2628.718280	193858.853509	57.202138
2628.069710	193648.591326	57.207143
2627.589617	193455.111561	57.212148
2626.772912	193248.300419	57.217153
2626.031442	193049.392395	57.222157
2625.417447	192840.171480	57.227162
2624.699665	192643.080818	57.232167
2624.328386	192452.501422	57.237172
2623.368125	192250.259508	57.242177
2622.752689	192044.502991	57.247181
2622.187466	191860.051174	57.252186
2621.541470	191652.863386	57.257191
2621.105160	191448.378770	57.262196
2620.052806	191251.270352	57.267201
2619.546742	191045.055385	57.272205
2619.264725	190853.704658	57.277210
2618.574435	190642.036892	57.282215
2617.814820	190433.014716	57.287220
2617.044020	190240.318875	57.292225
2616.476169	190034.766875	57.297229
2615.705404	189820.672651	57.302234
2615.185871	189619.822255	57.307239
2614.744563	189407.878731	57.312244
2613.674462	189211.366713	57.317249
2613.074458	188994.882698	57.322253
2612.275833	188797.909524	57.327258
2611.815857	188592.283031	57.332263
2611.043044	188388.882557	57.337268
2610.337754	188191.858953	57.342273
2609.780283	187977.548403	57.347277
2609.159937	187789.406009	57.352282
2608.442333	187576.509407	57.357287
2607.763985	187369.472521	57.362292
2607.044001	187174.643756	57.367297
2606.646507	186962.958732	57.372301
2605.905378	186753.695436	57.377306
2605.149119	186551.661605	57.382311
2604.604525	186352.432122	57.387316
2603.613909	186150.589849	57.392321
2603.410998	185941.219511	57.397325
2602.554784	185736.762497	57.402330
2601.866335	185528.755886	57.407335
2601.211376	185329.688275	57.412340
2600.532593	185134.060155	57.417345
2600.114365	184914.258727	57.422349
2599.210111	184712.905270	57.427354
2598.334987	184504.487676	57.432359
2597.422796	184308.900109	57.437364
2597.112590	184109.490640	57.442369
2596.660548	183900.118307	57.447373
2595.657440	183696.584277	57.452378
2595.053012	183489.476951	57.457383
2594.315986	183292.962857	57.462388
2593.513688	183092.974399	57.467393
2593.178086	182887.468293	57.472397
2592.543567	182697.084843	57.477402
2591.859524	182487.526938	57.482407
2591.715867	182287.666723	57.487412
2590.708791	182084.560507	57.492417
2589.860255	181871.762358	57.497421
2589.007189	181672.119124	57.502426
2588.391220	181454.922960	57.507431
2587.681286	181263.908921	57.512436
2587.027074	181066.984583	57.517441
2586.494899	180857.881069	57.522445
2585.809890	180658.012328	57.527450
2585.139379	180455.025737	57.532455
2584.743845	180256.842941	57.537460
2583.663426	180054.419282	57.542465
2583.459420	179845.535790	57.547469
2582.228157	179648.098802	57.552474
2581.771069	179447.105641	57.557479
2581.682000	179234.912431	57.562484
2580.609773	179042.731819	57.567489
2580.009502	178831.346663	57.572493
2579.330710	178634.055782	57.577498
2578.559425	178421.160680	57.582503
2578.123779	178214.713198	57.587508
2577.475846	178021.554170	57.592513
2576.842684	177809.161772	57.597517
2576.018060	177609.914548	57.602522
2575.053729	177399.408307	57.607527
2574.829854	177189.892368	57.612532
2574.120391	177002.700435	57.617537
2573.462032	176794.603578	57.622541
2573.024439	176594.282335	57.627546
2572.360118	176377.018011	57.632551
2571.744194	176170.583760	57.637556
2570.920584	175961.067310	57.642561
2570.225589	175756.390160	57.647565
2569.546779	175549.803640	57.652570
2568.604360	175343.234498	57.657575
2568.222194	175133.067252	57.662580
2567.389124	174933.529010	57.667585
2566.956509	174728.217643	57.672589
2566.179302	174523.178136	57.677594
2565.525078	174309.522508	57.682599
2564.779419	174101.911006	57.687604
2563.847577	173907.010232	57.692609
2563.858936	173700.946921	57.697613
2562.832055	173497.465653	57.702618
2562.026157	173284.449962	57.707623
2561.394284	173075.274110	57.712628
2560.516191	172882.493703	57.717633
2560.216225	172678.443549	57.722637
2559.282961	172473.197581	57.727642
2558.796811	172272.447503	57.732647
2558.173540	172066.594924	57.737652
2557.127337	171873.629847	57.742657
2556.964732	171659.897730	57.747661
2556.205861	171465.490175	57.752666
2555.397644	171255.436193	57.757671
2554.933739	171042.988766	57.762676
2554.303578	170850.751245	57.767681
2553.644760	170647.938438	57.772685
2552.932658	170451.773510	57.777690
2552.453202	170231.511871	57.782695
2552.134136	170021.908394	57.787700
2550.905382	169817.422561	57.792705
2550.659757	169608.318358	57.797709
2549.843485	169405.511549	57.802714
2549.145172	169190.377254	57.807719
2548.445797	168981.882457	57.812724
2547.650407	168779.482569	57.817729
2547.132184	168577.815533	57.822733
2546.513192	168363.703338	57.827738
2545.704176	168146.812121	57.832743
2545.197777	167938.546747	57.837748
2544.326019	167741.390889	57.842753
2543.799329	167524.954405	57.847757
2543.141524	167322.591303	57.852762
2542.328463	167114.379049	57.857767
2541.803000	166904.888906	57.862772
2540.749636	166696.640744	57.867777
2540.455518	166485.717511	57.872781
2539.548501	166288.676547	57.877786
2538.992951	166079.589959	57.882791
2538.400916	165863.008069	57.887796
2537.756872	165671.866897	57.892801
2537.183698	165466.270612	57.897805
2536.689016	165258.526823	57.902810
2535.649401	165046.471031	57.907815
2534.992707	164839.365604	57.912820
2534.264730	164633.544159	57.917825
2533.566991	164429.626347	57.922829
2532.917411	164227.456716	57.927834
2532.333993	164013.567152	57.932839
2532.297053	163806.025997	57.937844
2531.335023	163612.085001	57.942849
2530.794719	163393.780146	57.947853
2529.999662	163197.983949	57.952858
2529.435645	162926.474408	57.957863
2528.983634	162692.431719	57.962868
2528.100771	162495.979343	57.967873
2527.448085	162280.992035	57.972877
2526.927680	162067.726908	57.977882
2526.061626	161854.619537	57.982887
2525.792241	161643.338707	57.987892
2524.434676	161433.579284	57.992897
2524.328920	161222.974269	57.997901
2523.310867	161013.583058	58.002906
2522.631173	160805.665118	58.007911
2522.130888	160585.807081	58.012916
2521.092356	160379.855574	58.017921
2520.534509	160176.918501	58.022925
2519.909456	159974.120376	58.027930
2519.450849	159768.347488	58.032935
2518.764419	159543.681547	58.037940
2517.763837	159345.561536	58.042945
2517.556040	159128.259717	58.047949
2516.765222	158919.912775	58.052954
2516.148904	158713.331968	58.057959
2515.482453	158489.813777	58.062964
2514.575816	158291.888233	58.067969
2514.171759	158076.314871	58.072973
2513.563899	157869.496166	58.077978
2512.648524	157651.565607	58.082983
2512.230923	157433.303266	58.087988
2511.174320	157241.064623	58.092993
2510.258821	157030.257065	58.097997
2509.998907	156831.067788	58.103002
2508.904337	156617.926611	58.108007
2508.475191	156423.457390	58.113012
2507.631855	156215.071438	58.118017
2507.131318	156008.895185	58.123021
2506.586967	155810.735742	58.128026
2505.710216	155611.575035	58.133031
2505.160837	155392.799910	58.138036
2504.424290	155202.161801	58.143041
2503.566495	154995.018638	58.148045
2502.910752	154794.314979	58.153050
2502.382458	154594.456701	58.158055
2501.888946	154385.835816	58.163060
2501.254187	154186.619690	58.168065
2500.543827	153987.098938	58.173069
2500.027154	153792.874722	58.178074
2499.476782	153588.831158	58.183079
2498.671599	153372.956972	58.188084
2498.132933	153181.942997	58.193089
2497.145692	152963.265733	58.198093
2496.529833	152756.797103	58.203098
2495.833959	152556.087751	58.208103
2495.132696	152357.274373	58.213108
2494.420247	152149.058024	58.218113
2493.945400	151942.343309	58.223117
2493.367729	151749.589672	58.228122
2492.909862	151547.908114	58.233127
2492.438689	151334.383797	58.238132
2491.400181	151130.076805	58.243137
2490.536705	150925.425583	58.248141
2490.302211	150713.545533	58.253146
2489.512748	150505.339065	58.258151
2488.442257	150294.306005	58.263156
2487.907619	150092.251549	58.268161
2487.217303	149891.366907	58.273165
2486.543191	149691.040167	58.278170
2485.591602	149490.046901	58.283175
2485.470483	149280.242580	58.288180
2484.795659	149086.033009	58.293185
2484.147119	148886.520596	58.298189
2483.458968	148671.726320	58.303194
2482.566356	148467.387499	58.308199
2481.934837	148264.698915	58.313204
2480.921788	148064.639331	58.318209
2480.657632	147859.467630	58.323213
2480.216036	147657.070506	58.328218
2479.084587	147460.096328	58.333223
2478.578984	147256.796845	58.338228
2478.036905	147057.939787	58.343233
2477.269291	146856.298401	58.348237
2476.921911	146659.268436	58.353242
2475.999510	146452.456347	58.358247
2475.507441	146246.873652	58.363252
2474.659737	146044.246164	58.368257
2474.244807	145850.434438	58.373261
2473.792449	145641.799408	58.378266
2472.865509	145433.749314	58.383271
2472.554807	145228.233468	58.388276
2471.617467	145024.660947	58.393281
2470.816128	144808.932217	58.398285
2470.167582	144594.502361	58.403290
2469.776321	144399.996916	58.408295
2469.067473	144189.099426	58.413300
2468.009878	143987.064937	58.418305
2467.512499	143772.019529	58.423309
2466.895074	143570.705834	58.428314
2466.096274	143386.322827	58.433319
2465.924186	143168.472571	58.438324
2465.073512	142966.068850	58.443329
2464.352801	142754.369758	58.448333
2463.621393	142552.610611	58.453338
2462.830576	142348.638514	58.458343
2462.225846	142136.289954	58.463348
2461.470273	141940.421880	58.468353
2461.009764	141729.171466	58.473357
2460.401619	141530.169544	58.478362
2459.450630	141332.379550	58.483367
2459.313645	141123.483555	58.488372
2458.190113	140921.111199	58.493377
2457.653813	140700.490041	58.498381
2456.657534	140506.105146	58.503386
2456.158487	140311.871385	58.508391
2455.759446	140108.538313	58.513396
2454.762021	139905.250646	58.518401
2454.304334	139696.046871	58.523405
2453.615074	139483.234749	58.528410
2452.718392	139286.694683	58.533415
2452.420341	139080.315930	58.538420
2451.557407	138880.965273	58.543425
2451.018811	138682.072741	58.548429
2450.339908	138474.932698	58.553434
2449.780396	138268.842397	58.558439
2449.242680	138065.494350	58.563444
2448.469842	137866.441119	58.568449
2447.442785	137659.844733	58.573453
2447.140110	137456.107867	58.578458
2446.157203	137251.019203	58.583463
2445.559204	137041.170252	58.588468
2444.871870	136845.604094	58.593473
2444.269510	136641.119979	58.598477
2443.583720	136438.835653	58.603482
2443.091097	136233.714464	58.608487
2442.348448	136024.746881	58.613492
2441.608939	135821.065176	58.618497
2441.292904	135623.174281	58.623501
2440.494875	135413.444907	58.628506
2439.706536	135215.390280	58.633511
2439.400160	135003.502496	58.638516
2438.530214	134807.407251	58.643521
2437.786202	134606.199256	58.648525
2437.253812	134395.507762	58.653530
2436.336259	134193.783898	58.658535
2435.918687	133981.019282	58.663540
2435.131026	133789.516467	58.668545
2434.216885	133587.669272	58.673549
2433.888681	133380.026966	58.678554
2432.898447	133174.930069	58.683559
2432.228074	132961.946308	58.688564
2431.497146	132764.191566	58.693569
2431.412915	132575.824524	58.698573
2430.747880	132367.315667	58.703578
2429.851695	132159.645234	58.708583
2429.407207	131942.543082	58.713588
2428.717008	131750.225518	58.718593
2427.783025	131545.906254	58.723597
2427.473215	131328.622317	58.728602
2426.748109	131117.706062	58.733607
2426.112168	130908.441192	58.738612
2425.242139	130718.280363	58.743617
2424.615927	130509.969541	58.748621
2424.129375	130298.932679	58.753626
2423.354362	130093.417482	58.758631
2422.980620	129877.056675	58.763636
2422.100354	129678.610489	58.768641
2421.513976	129476.461164	58.773645
2420.689921	129264.367893	58.778650
2420.080106	129051.327794	58.783655
2419.729579	128837.448058	58.788660
2418.952191	128634.954090	58.793665
2418.479679	128421.503321	58.798669
2417.743222	128216.592774	58.803674
2416.889109	128005.555328	58.808679
2416.585610	127780.652203	58.813684
2415.756014	127569.487196	58.818689
2415.022814	127369.078344	58.823693
2414.308705	127154.177035	58.828698
2413.251330	126941.948040	58.833703
2412.705346	126727.594916	58.838708
2411.857304	126527.489811	58.843713
2411.369656	126321.347435	58.848717
2410.866969	126119.806283	58.853722
2410.021909	125913.952241	58.858727
2409.606456	125703.802712	58.863732
2408.819402	125494.742370	58.868737
2408.164305	125286.450071	58.873741
2407.601125	125075.617658	58.878746
2406.704639	124878.732545	58.883751
2406.078665	124655.811110	58.888756
2405.441243	124464.665984	58.893761
2404.854245	124247.926106	58.898765
2404.151396	124038.647781	58.903770
2403.413768	123835.662410	58.908775
2403.230430	123622.558864	58.913780
2402.493675	123415.754275	58.918785
2401.746287	123205.626009	58.923789
2401.128369	122995.631244	58.928794
2400.323307	122786.988404	58.933799
2399.838143	122573.407739	58.938804
2399.001332	122361.459080	58.943809
2398.626129	122149.350036	58.948813
2397.890554	121938.925128	58.953818
2396.833965	121728.882924	58.958823
2396.587621	121512.187400	58.963828
2395.860933	121304.623058	58.968833
2395.041169	121092.605652	58.973837
2394.703677	120877.313788	58.978842
2393.637261	120671.547807	58.983847
2392.859818	120460.023967	58.988852
2392.202184	120257.611906	58.993857
2391.690424	120049.274262	58.998861
2391.247651	119833.614036	59.003866
2390.048887	119624.626894	59.008871
2389.794731	119418.545161	59.013876
2389.142193	119209.696922	59.018881
2388.170144	118997.733291	59.023885
2387.783481	118784.243901	59.028890
2386.868717	118582.069685	59.033895
2386.411516	118373.882773	59.038900
2385.517249	118170.769010	59.043905
2384.722977	117966.022273	59.048909
2384.442764	117746.773352	59.053914
2383.800774	117541.434528	59.058919
2383.264882	117332.106832	59.063924
2382.491436	117117.778438	59.068929
2381.849016	116918.125831	59.073933
2381.035636	116706.631896	59.078938
2380.296466	116499.336354	59.083943
2379.954140	116281.423706	59.088948
2379.015810	116076.181666	59.093953
2378.609539	115865.499728	59.098957
2378.209195	115650.229475	59.103962
2377.163577	115445.174554	59.108967
2376.622776	115233.306843	59.113972
2375.889780	115016.076283	59.118977
2375.413023	114804.995386	59.123981
2375.040525	114598.342657	59.128986
2374.000321	114381.369353	59.133991
2373.539973	114168.012591	59.138996
2372.513518	113959.069631	59.144001
2372.228706	113746.228089	59.149005
2371.673721	113532.694955	59.154010
2370.421135	113334.106578	59.159015
2370.291959	113104.902931	59.164020
2369.716876	112887.982992	59.169025
2368.795457	112670.421724	59.174029
2368.235152	112459.963964	59.179034
2367.424506	112241.982685	59.184039
2367.243009	112018.083896	59.189044
2365.949683	111808.572896	59.194049
2365.369996	111593.023061	59.199053
2364.921198	111371.634837	59.204058
2364.070273	111162.059145	59.209063
2363.506223	110937.253440	59.214068
2362.711238	110728.199280	59.219073
2361.771954	110512.093954	59.224077
2361.631875	110298.814671	59.229082
2360.722905	110090.082252	59.234087
2360.196584	109871.461195	59.239092
2359.444982	109664.420819	59.244097
2358.642564	109458.526137	59.249101
2358.440034	109239.573805	59.254106
2357.596266	109027.381685	59.259111
2357.374876	108812.560829	59.264116
2356.352003	108594.664461	59.269121
2355.667826	108377.661809	59.274125
2354.648015	108157.655823	59.279130
2354.261236	107943.934878	59.284135
2353.962944	107719.643202	59.289140
2353.239221	107503.029003	59.294145
2352.244685	107281.123384	59.299149
2351.878282	107067.889163	59.304154
2351.028448	106859.327313	59.309159
2350.467992	106635.461617	59.314164
2349.598205	106421.418284	59.319169
2348.960304	106206.458143	59.324173
2348.308725	105983.393384	59.329178
2347.761772	105771.062173	59.334183
2347.224900	105553.490497	59.339188
2346.444699	105336.016486	59.344193
2345.657068	105118.526597	59.349197
2345.121054	104893.404359	59.354202
2344.505756	104683.104870	59.359207
2344.054851	104457.541826	59.364212
2343.362347	104239.492910	59.369217
2342.584059	104013.522855	59.374221
2341.941538	103782.438984	59.379226
2341.167409	103572.123764	59.384231
2340.628841	103343.387737	59.389236
2340.099525	103130.100292	59.394241
2339.086386	102919.016744	59.399245
2338.494319	102691.126591	59.404250
2338.009609	102482.354837	59.409255
2337.185714	102254.093326	59.414260
2336.304819	102036.989105	59.419265
2335.768480	101821.215189	59.424269
2335.549139	101596.492825	59.429274
2334.721960	101375.744953	59.434279
2334.005244	101143.081158	59.439284
2333.056417	100928.034286	59.444289
2332.151278	100716.376206	59.449293
2331.936114	100493.490710	59.454298
2331.238994	100280.680833	59.459303
2330.607891	100065.001633	59.464308
2329.919511	99849.618967	59.469313
2329.069578	99635.209050	59.474317
2328.558974	99408.708161	59.479322
2327.541102	99196.187472	59.484327
2327.181901	98978.464556	59.489332
2326.633097	98767.865119	59.494337
2325.679813	98549.016296	59.499341
2325.292240	98330.422358	59.504346
2324.243602	98109.410934	59.509351
2323.773821	97893.796241	59.514356
2323.027944	97676.603659	59.519361
2322.386253	97465.764522	59.524365
2321.968137	97250.851721	59.529370
2321.316473	97035.705257	59.534375
2320.464649	96822.387455	59.539380
2320.033622	96597.595134	59.544385
2319.278964	96381.215421	59.549389
2318.880460	96153.530280	59.554394
2318.004444	95944.308923	59.559399
2317.390340	95723.683011	59.564404
2316.628183	95503.653511	59.569409
2315.983471	95284.920309	59.574413
2315.183167	95070.691259	59.579418
2314.319131	94856.525090	59.584423
2314.043169	94628.074880	59.589428
2313.589134	94418.762709	59.594433
2312.487527	94204.234567	59.599437
2312.046983	93978.252255	59.604442
2311.565229	93763.325641	59.609447
2310.890967	93540.536538	59.614452
2310.440702	93316.135134	59.619457
2309.391106	93104.317067	59.624461
2308.802303	92876.143620	59.629466
2308.090478	92654.523438	59.634471
2307.767210	92433.864765	59.639476
2306.938417	92210.885198	59.644481
2305.905297	91996.088452	59.649485
2305.771916	91765.336827	59.654490
2305.092394	91546.189225	59.659495
2304.196286	91322.468386	59.664500
2303.606322	91107.381733	59.669505
2302.952037	90895.135322	59.674509
2302.319592	90661.709853	59.679514
2301.167592	90447.264082	59.684519
2300.699801	90224.424885	59.689524
2300.437829	90004.928414	59.694529
2299.420034	89784.552234	59.699533
2298.992117	89561.466187	59.704538
2298.086751	89342.452480	59.709543
2297.533280	89115.364860	59.714548
2296.886845	88897.550890	59.719553
2296.243409	88682.718441	59.724557
2296.109767	88453.022455	59.729562
2294.819359	88234.721303	59.734567
2294.422998	88008.343080	59.739572
2293.685938	87787.517839	59.744577
2293.027629	87567.684038	59.749581
2292.149671	87346.067832	59.754586
2291.450915	87128.007344	59.759591
2291.310428	86905.568671	59.764596
2290.166404	86682.974481	59.769601
2289.571962	86467.909036	59.774605
2289.491924	86235.964964	59.779610
2288.249419	86014.122351	59.784615
2287.752853	85791.124107	59.789620
2287.134505	85570.949391	59.794625
2286.372231	85349.563654	59.799629
2285.745551	85125.109656	59.804634
2285.065454	84901.401808	59.809639
2284.565773	84681.895712	59.814644
2284.021321	84461.936250	59.819649
2283.079090	84240.083489	59.824653
2282.150481	84008.253842	59.829658
2281.446597	83802.455370	59.834663
2280.947888	83574.612650	59.839668
2280.694774	83354.326904	59.844673
2279.705488	83140.536638	59.849677
2279.453236	82912.059828	59.854682
2278.548910	82684.836140	59.859687
2278.049673	82462.830370	59.864692
2277.206704	82236.634919	59.869697
2276.310691	82015.013719	59.874701
2276.174700	81775.166694	59.879706
2274.900754	81555.460988	59.884711
2274.427876	81349.928733	59.889716
2273.806845	81115.154095	59.894721
2272.999393	80887.820452	59.899725
2272.490115	80669.796363	59.904730
2271.732832	80448.531024	59.909735
2271.219682	80230.746639	59.914740
2270.646817	80005.090226	59.919745
2269.737731	79790.206099	59.924750
2269.259021	79555.337773	59.929754
2268.318384	79336.908126	59.934759
2267.849847	79116.707546	59.939764
2267.152359	78892.597611	59.944769
2266.481808	78675.291816	59.949774
2265.870297	78448.093276	59.954778
2265.130992	78230.986848	59.959783
2264.419894	78009.987423	59.964788
2263.795927	77789.153987	59.969793
2262.709293	77575.265292	59.974798
2262.418034	77347.717635	59.979802
2261.805864	77133.460481	59.984807
2261.034977	76909.124039	59.989812
2260.344242	76688.636232	59.994817
2259.433637	76472.431041	59.999822
2259.152845	76253.473345	60.004826
2258.256835	76042.104999	60.009831
2257.675556	75824.302088	60.014836
2257.161325	75598.874903	60.019841
2256.223764	75384.092179	60.024846
2255.968455	75164.749347	60.029850
2255.252938	74950.544256	60.034855
2254.496765	74725.912800	60.039860
2253.653163	74505.979825	60.044865
2253.218850	74287.276807	60.049870
2252.669737	74065.882734	60.054874
2251.537633	73855.917841	60.059879
2251.357122	73634.134272	60.064884
2250.246236	73419.602705	60.069889
2249.485931	73202.540713	60.074894
2249.101276	72981.284562	60.079898
2248.195819	72776.217528	60.084903
2247.672046	72555.304917	60.089908
2247.498256	72342.144026	60.094913
2246.456207	72128.597330	60.099918
2246.135101	71901.267810	60.104922
2245.057693	71682.441852	60.109927
2244.349967	71466.568687	60.114932
2243.729636	71257.956257	60.119937
2242.886832	71041.957104	60.124942
2242.580316	70816.341707	60.129946
2241.781121	70606.307558	60.134951
2241.159186	70391.382676	60.139956
2240.721707	70178.818931	60.144961
2239.277753	69963.053610	60.149966
2238.993901	69741.323488	60.154970
2238.132690	69533.229874	60.159975
2237.540440	69315.949371	60.164980
2237.110709	69107.329436	60.169985
2236.421630	68893.977055	60.174990
2235.725196	68676.118436	60.179994
2235.281557	68461.655070	60.184999
2234.477744	68249.309654	60.190004
2233.850904	68031.865200	60.195009
2233.029798	67820.686251	60.200014
2232.533973	67600.141360	60.205018
2231.670127	67393.616303	60.210023
2231.035182	67175.327673	60.215028
2230.602609	66959.162725	60.220033
2229.638658	66755.915655	60.225038
2229.136810	66540.140025	60.230042
2228.289973	66321.036470	60.235047
2227.913243	66112.962659	60.240052
2227.415793	65903.687971	60.245057
2226.683647	65691.188162	60.250062
2225.904454	65472.951103	60.255066
2225.155792	65262.947440	60.260071
2224.344648	65042.415199	60.265076
2223.958764	64834.461122	60.270081
2222.804430	64623.566233	60.275086
2222.473320	64402.138796	60.280090
2221.893787	64197.043466	60.285095
2221.189414	63980.093812	60.290100
2220.659264	63764.686220	60.295105
2219.823924	63565.840701	60.300110
2219.162826	63344.085254	60.305114
2218.177967	63139.486656	60.310119
2217.349025	62928.470202	60.315124
2217.261534	62712.412231	60.320129
2216.073266	62512.338815	60.325134
2215.487877	62315.546719	60.330138
2215.226712	62101.524090	60.335143
2214.454713	61888.800587	60.340148
2213.838269	61675.206366	60.345153
2212.723104	61482.771279	60.350158
2212.188969	61268.462631	60.355162
2211.517567	61064.273568	60.360167
2210.747809	60860.092821	60.365172
2210.522999	60653.624568	60.370177
2209.143563	60454.657409	60.375182
2208.721204	60236.322471	60.380186
2208.081643	60044.659168	60.385191
2207.489777	59832.705839	60.390196
2206.655576	59639.805025	60.395201
2205.562916	59440.302991	60.400206
2205.254046	59239.754456	60.405210
2204.621975	59049.923400	60.410215
2203.794574	58860.527255	60.415220
2203.488205	58656.198866	60.420225
2202.463640	58465.017977	60.425230
2201.671570	58262.812537	60.430234
2201.185265	58073.797581	60.435239
2200.088001	57885.109358	60.440244
2199.377067	57705.876116	60.445249
2198.486377	57541.058463	60.450254
2198.161217	57367.733490	60.455258
2197.050256	57196.712339	60.460263
2196.211243	57024.997637	60.465268
2195.676884	56844.345786	60.470273
2194.537817	56687.145758	60.475278
2193.940598	56501.579408	60.480282
2192.899020	56342.566015	60.485287
2191.970847	56181.402887	60.490292
2191.519979	56015.769497	60.495297
2190.483420	55867.966078	60.500302
2189.796291	55699.711412	60.505306
2189.071688	55553.183911	60.510311
2188.088876	55400.979883	60.515316
2187.571616	55247.070275	60.520321
2186.802510	55112.902011	60.525326
2185.902823	54970.002017	60.530330
2184.995640	54822.819424	60.535335
2184.472861	54694.820977	60.540340
2183.851077	54546.557339	60.545345
2182.771014	54420.949869	60.550350
2182.459499	54285.249891	60.555354
2181.493105	54147.692818	60.560359
2180.977843	54021.476350	60.565364
2180.242453	53893.254599	60.570369
2179.702499	53764.395171	60.575374
2178.719864	53627.066117	60.580378
2178.146920	53498.748590	60.585383
2177.506788	53368.949043	60.590388
2177.045011	53249.985349	60.595393
2176.018064	53127.871821	60.600398
2175.959542	52991.979957	60.605402
2175.000409	52864.785055	60.610407
2174.274844	52741.139102	60.615412
2173.629544	52613.567090	60.620417
2172.617033	52491.534665	60.625422
2172.192520	52366.843612	60.630426
2171.565496	52242.897486	60.635431
2171.141016	52118.790345	60.640436
2170.667056	51998.295855	60.645441
2169.583541	51877.471720	60.650446
2169.110650	51750.359390	60.655450
2168.460344	51622.905906	60.660455
2168.030841	51504.549734	60.665460
2167.415633	51379.636297	60.670465
2166.788919	51250.878122	60.675470
2166.396666	51121.159788	60.680474
2165.591506	50997.389697	60.685479
2164.907895	50872.857649	60.690484
2164.370306	50734.268172	60.695489
2163.418262	50606.486926	60.700494
2163.036167	50481.425680	60.705498
2162.153718	50351.490106	60.710503
2161.411794	50230.844312	60.715508
2160.599914	50097.903239	60.720513
2159.834555	49975.225399	60.725518
2159.619619	49852.280737	60.730522
2158.958900	49727.541041	60.735527
2158.203367	49610.021036	60.740532
2157.657916	49483.391838	60.745537
2156.555280	49349.781138	60.750542
2156.172357	49234.773386	60.755546
2155.910795	49106.127706	60.760551
2154.801804	48980.290650	60.765556
2154.343159	48851.719202	60.770561
2153.807688	48721.262737	60.775566
2153.136283	48590.860430	60.780570
2152.332040	48478.980377	60.785575
2151.377969	48356.292999	60.790580
2151.152839	48222.535720	60.795585
2150.131058	48104.194780	60.800590
2149.562253	47969.200088	60.805594
2148.845706	47840.891984	60.810599
2148.039006	47727.770678	60.815604
2147.589882	47602.338509	60.820609
2146.839386	47498.576457	60.825614
2146.537767	47363.695826	60.830618
2145.508393	47241.898026	60.835623
2144.924337	47118.780918	60.840628
2144.501120	46998.549340	60.845633
2143.780458	46875.272135	60.850638
2143.239224	46748.617489	60.855642
2142.740369	46619.711169	60.860647
2141.903530	46494.743776	60.865652
2141.379511	46364.549582	60.870657
2140.777056	46247.438784	60.875662
2140.067810	46117.538345	60.880666
2139.500663	45985.114332	60.885671
2138.805173	45860.666739	60.890676
2138.236230	45727.220127	60.895681
2137.339077	45610.454493	60.900686
2136.930840	45471.951991	60.905690
2136.420925	45341.699877	60.910695
2135.201522	45220.094887	60.915700
2134.887374	45090.484121	60.920705
2134.076058	44955.715463	60.925710
2133.448557	44824.046745	60.930714
2132.894335	44706.508434	60.935719
2132.086764	44569.841291	60.940724
2131.513568	44439.760911	60.945729
2130.859054	44317.753131	60.950734
2130.166596	44187.538578	60.955738
2129.326882	44058.926560	60.960743
2128.377912	43936.923890	60.965748
2127.864135	43808.201916	60.970753
2127.553350	43687.921432	60.975758
2127.057080	43554.581083	60.980762
2126.460946	43428.006601	60.985767
2125.596033	43309.458050	60.990772
2125.268242	43166.147623	60.995777
2124.380765	43046.760044	61.000782
2123.749452	42920.947525	61.005786
2123.223031	42785.135295	61.010791
2122.144626	42657.836521	61.015796
2121.542447	42532.325798	61.020801
2120.665547	42399.456353	61.025806
2120.476871	42266.266846	61.030810
2119.769388	42130.127973	61.035815
2118.956871	42027.372766	61.040820
2118.737793	41882.060271	61.045825
2117.747612	41753.173002	61.050830
2116.700951	41625.405619	61.055834
2116.437605	41497.119610	61.060839
2115.615858	41373.970078	61.065844
2115.238777	41240.944866	61.070849
2114.095272	41112.908893	61.075854
2113.690730	40977.701844	61.080858
2113.374869	40848.284301	61.085863
2112.534553	40735.156773	61.090868
2111.950730	40598.804846	61.095873
2110.833864	40468.619232	61.100878
2110.415257	40341.602846	61.105882
2109.991251	40208.378056	61.110887
2109.001821	40078.462930	61.115892
2108.394467	39951.514167	61.120897
2107.654055	39834.098594	61.125902
2107.052794	39701.056072	61.130906
2106.492807	39568.047559	61.135911
2105.328012	39445.491190	61.140916
2105.017325	39315.780863	61.145921
2104.333844	39192.218775	61.150926
2103.641422	39059.687380	61.155930
2103.270740	38938.303407	61.160935
2102.364271	38824.165122	61.165940
2102.007689	38687.055695	61.170945
2100.989475	38561.437679	61.175950
2100.614021	38427.904488	61.180954
2099.980074	38300.651323	61.185959
2098.778194	38181.828057	61.190964
2098.563321	38043.982056	61.195969
2097.765322	37917.570330	61.200974
2097.107322	37786.745914	61.205978
2096.575250	37664.693197	61.210983
2095.824701	37541.479393	61.215988
2095.344135	37410.210827	61.220993
2094.279910	37290.583179	61.225998
2093.760935	37164.970587	61.231002
2093.222459	37031.374677	61.236007
2092.292417	36919.287338	61.241012
2092.104549	36781.210222	61.246017
2091.005408	36663.857685	61.251022
2090.422548	36531.219603	61.256026
2089.963456	36413.117592	61.261031
2089.186906	36282.445345	61.266036
2088.517570	36155.109617	61.271041
2087.842232	36025.613519	61.276046
2087.132614	35903.021626	61.281050
2086.758630	35769.212042	61.286055
2085.661461	35648.945334	61.291060
2085.560598	35524.192201	61.296065
2084.756516	35397.122265	61.301070
2083.701866	35270.009286	61.306074
2083.357149	35140.665115	61.311079
2082.733199	35016.550371	61.316084
2082.205004	34890.602181	61.321089
2081.349004	34771.545784	61.326094
2080.680985	34634.152023	61.331098
2080.224356	34502.369722	61.336103
2079.430095	34378.615477	61.341108
2078.832160	34252.020950	61.346113
2077.880044	34124.758167	61.351118
2077.304224	33999.695072	61.356122
2076.607459	33870.238007	61.361127
2075.553276	33770.673548	61.366132
2075.291950	33634.489384	61.371137
2074.466479	33518.041578	61.376142
2073.774068	33400.776965	61.381146
2073.155369	33280.667896	61.386151
2072.765746	33158.119633	61.391156
2072.052536	33036.733021	61.396161
2071.760481	32902.713722	61.401166
2070.887568	32773.746700	61.406170
2070.124630	32653.290525	61.411175
2069.298170	32521.508321	61.416180
2069.027105	32395.103619	61.421185
2068.297012	32281.817805	61.426190
2067.429259	32144.444698	61.431194
2067.027929	32007.142515	61.436199
2066.254886	31882.646563	61.441204
2065.587180	31758.672106	61.446209
2065.105171	31627.287985	61.451214
2064.336161	31497.952555	61.456218
2063.535381	31369.852559	61.461223
2062.675851	31251.345007	61.466228
2062.221862	31122.558253	61.471233
2061.098649	31000.185055	61.476238
2060.657810	30874.623223	61.481242
2060.218681	30745.848117	61.486247
2059.103808	30617.745357	61.491252
2058.384907	30496.977174	61.496257
2057.535865	30371.390741	61.501262
2057.109534	30263.269067	61.506266
2056.816679	30141.786473	61.511271
2055.778550	30025.660914	61.516276
2055.429378	29908.835906	61.521281
2054.642424	29776.140334	61.526286
2054.022291	29668.991870	61.531290
2053.431485	29536.173893	61.536295
2052.400079	29422.413650	61.541300
2051.979760	29297.083413	61.546305
2051.115452	29177.187005	61.551310
2050.471512	29061.110015	61.556314
2049.815126	28938.881945	61.561319
2049.028221	28823.052109	61.566324
2048.505364	28703.014940	61.571329
2047.675460	28591.062804	61.576334
2046.684210	28472.815869	61.581338
2046.167567	28358.387313	61.586343
2045.584926	28246.404625	61.591348
2045.131672	28127.240645	61.596353
2044.555059	28003.630871	61.601358
2044.069219	27887.570330	61.606362
2043.633261	27762.221201	61.611367
2042.523932	27645.962750	61.616372
2042.117472	27515.324775	61.621377
2041.459461	27393.129114	61.626382
2040.613213	27282.253372	61.631386
2039.958863	27156.398559	61.636391
2039.413528	27039.216094	61.641396
2038.679352	26924.890618	61.646401
2037.924288	26810.954720	61.651406
2036.977640	26699.035746	61.656410
2036.808210	26564.469059	61.661415
2035.732754	26463.888433	61.666420
2035.353942	26338.920378	61.671425
2034.688946	26224.240559	61.676430
2033.896477	26105.112115	61.681434
2033.486789	25982.541757	61.686439
2033.005335	25869.912575	61.691444
2032.555851	25755.120537	61.696449
2031.587675	25630.238874	61.701454
2030.778400	25504.090600	61.706458
2030.326642	25379.001769	61.711463
2029.544658	25270.292913	61.716468
2028.891224	25146.898831	61.721473
2028.132867	25028.041476	61.726478
2027.527570	24911.131988	61.731482
2026.970949	24789.255875	61.736487
2026.124990	24672.469248	61.741492
2025.704807	24553.339026	61.746497
2024.987339	24438.211949	61.751502
2024.244609	24310.723077	61.756506
2023.340522	24185.750088	61.761511
2022.832844	24083.535315	61.766516
2022.294797	23961.061568	61.771521
2021.765060	23833.503209	61.776526
2020.723683	23725.878963	61.781530
2020.123379	23598.336051	61.786535
2019.359633	23493.357486	61.791540
2018.779686	23376.872941	61.796545
2018.376959	23265.723932	61.801550
2017.381684	23161.442116	61.806554
2016.864266	23039.636296	61.811559
2015.791933	22929.586962	61.816564
2015.602403	22808.031740	61.821569
2014.877765	22706.363249	61.826574
2014.094105	22589.717801	61.831578
2013.729486	22475.873148	61.836583
2013.037603	22360.228735	61.841588
2012.001474	22234.762156	61.846593
2011.516139	22125.652553	61.851598
2010.701643	22005.747982	61.856602
2010.079783	21883.437759	61.861607
2009.122503	21784.207037	61.866612
2008.676989	21662.919934	61.871617
2008.115208	21559.002290	61.876622
2007.260688	21452.263160	61.881626
2006.955960	21342.109330	61.886631
2005.951577	21225.510538	61.891636
2005.513899	21114.875633	61.896641
2004.927592	20996.254789	61.901646
2004.240861	20892.886428	61.906650
2003.709646	20765.195035	61.911655
2002.648113	20662.087438	61.916660
2002.067394	20548.149616	61.921665
2001.415055	20434.581653	61.926670
2000.544536	20323.398833	61.931674
1999.977570	20218.019914	61.936679
1999.152284	20109.581401	61.941684
1998.259718	20004.947620	61.946689
1997.290565	19898.840409	61.951694
1996.976635	19797.670613	61.956698
1996.257024	19694.181126	61.961703
1995.640145	19587.570869	61.966708
1995.032077	19487.619022	61.971713
1994.421475	19398.386478	61.976718
1993.396138	19290.563687	61.981722
1992.706620	19180.266179	61.986727
1992.142114	19081.219502	61.991732
1991.363695	18969.360593	61.996737
1990.594372	18871.857631	62.001742
1989.895157	18778.152550	62.006746
1989.214339	18675.957179	62.011751
1988.598578	18589.585559	62.016756
1987.777894	18494.918579	62.021761
1987.085823	18395.414136	62.026766
1986.481269	18309.580297	62.031770
1985.969355	18227.778905	62.036775
1985.264886	18131.448908	62.041780
1984.555196	18041.784724	62.046785
1983.970487	17948.403142	62.051790
1982.999124	17865.190877	62.056794
1982.713757	17768.935929	62.061799
1981.754888	17684.933621	62.066804
1981.195997	17588.708995	62.071809
1980.664408	17494.872921	62.076814
1979.534154	17408.052719	62.081818
1978.981278	17318.980777	62.086823
1977.899721	17227.777837	62.091828
1977.439758	17153.570948	62.096833
1976.827891	17071.390095	62.101838
1976.163029	16995.130147	62.106842
1975.737679	16899.115539	62.111847
1975.088266	16825.083169	62.116852
1974.166785	16745.147049	62.121857
1973.725029	16662.750923	62.126862
1972.829553	16581.553276	62.131866
1972.465998	16495.053594	62.136871
1971.461409	16406.691456	62.141876
1970.915971	16322.653989	62.146881
1970.205762	16250.776496	62.151886
1969.424535	16175.259132	62.156890
1969.317899	16079.497577	62.161895
1968.428752	16005.633079	62.166900
1967.871974	15928.799420	62.171905
1967.161607	15843.437241	62.176910
1966.276750	15763.093885	62.181914
1965.703345	15681.468404	62.186919
1965.030208	15599.088426	62.191924
1964.144028	15522.646507	62.196929
1963.712212	15443.995810	62.201934
1962.801380	15367.421630	62.206938
1962.361073	15285.393322	62.211943
1961.401800	15204.111819	62.216948
1960.953366	15128.780182	62.221953
1960.330022	15053.487038	62.226958
1959.719094	14975.011901	62.231962
1959.162496	14890.465250	62.236967
1958.131274	14821.992579	62.241972
1957.670430	14744.234636	62.246977
1957.116205	14669.229657	62.251982
1956.112414	14596.715976	62.256986
1955.716894	14523.730790	62.261991
1954.882184	14438.769945	62.266996
1954.154138	14378.430414	62.272001
1953.588181	14294.979459	62.277006
1952.775797	14226.205282	62.282010
1952.272386	14154.857210	62.287015
1951.513640	14084.189280	62.292020
1950.852116	13996.201949	62.297025
1950.111786	13921.390677	62.302030
1949.249518	13861.992082	62.307034
1948.922610	13785.692487	62.312039
1948.349885	13721.279746	62.317044
1947.466510	13652.012940	62.322049
1947.238758	13570.458430	62.327054
1946.128804	13498.943539	62.332058
1945.768310	13424.179166	62.337063
1945.090893	13358.444319	62.342068
1944.313064	13278.637767	62.347073
1943.888901	13206.619107	62.352078
1942.883356	13136.292552	62.357082
1942.757446	13060.412130	62.362087
1941.838658	12988.622542	62.367092
1940.891134	12916.640092	62.372097
1940.070342	12841.357001	62.377102
1939.431454	12776.026940	62.382106
1938.798764	12703.809964	62.387111
1938.032270	12637.504735	62.392116
1937.524537	12577.169302	62.397121
1937.228411	12506.766080	62.402126
1936.193586	12442.141785	62.407130
1935.535111	12370.278398	62.412135
1935.277901	12302.777339	62.417140
1934.160071	12228.355963	62.422145
1933.513542	12154.027627	62.427150
1932.667808	12090.364972	62.432154
1932.567672	12015.442176	62.437159
1931.773904	11968.649186	62.442164
1931.039692	11892.233236	62.447169
1930.598727	11803.254198	62.452174
1929.751017	11748.862610	62.457178
1929.245492	11675.235280	62.462183
1928.737877	11606.653373	62.467188
1927.561272	11533.896128	62.472193
1926.873728	11464.283274	62.477198
1926.294346	11390.740856	62.482202
1925.884340	11313.610949	62.487207
1924.831113	11253.264788	62.492212
1924.365980	11192.817616	62.497217
1923.473269	11110.452883	62.502222
1922.977117	11052.028078	62.507226
1922.286149	10987.016093	62.512231
1921.742020	10928.192222	62.517236
1921.035306	10848.936718	62.522241
1920.272353	10779.925452	62.527246
1919.784367	10717.892664	62.532250
1919.201717	10643.728077	62.537255
1918.255546	10592.439305	62.542260
1917.512820	10520.920381	62.547265
1917.239713	10447.579116	62.552270
1916.139683	10392.028189	62.557274
1915.505407	10331.762804	62.562279
1914.828848	10273.093093	62.567284
1914.369478	10210.215946	62.572289
1913.717737	10150.187810	62.577294
1912.557911	10087.197901	62.582298
1912.439428	10018.865381	62.587303
1911.473746	9959.729137	62.592308
1910.777224	9893.854032	62.597313
1910.594407	9835.540410	62.602318
1909.875279	9765.817503	62.607322
1909.333551	9702.811947	62.612327
1908.551365	9636.809545	62.617332
1907.841539	9566.753125	62.622337
1907.122618	9516.106139	62.627342
1906.409855	9445.515023	62.632346
1906.264729	9376.956887	62.637351
1905.536185	9320.912656	62.642356
1904.481814	9257.549310	62.647361
1903.920873	9184.332864	62.652366
1903.165308	9119.899357	62.657370
1902.413192	9050.871408	62.662375
1901.912900	8988.224403	62.667380
1901.536351	8919.248282	62.672385
1900.945429	8858.995717	62.677390
1900.157687	8795.242090	62.682394
1899.454486	8727.086760	62.687399
1898.580488	8654.113527	62.692404
1897.986742	8593.787525	62.697409
1897.397359	8526.855258	62.702414
1896.499182	8462.427494	62.707418
1895.786087	8396.801420	62.712423
1894.962852	8335.651769	62.717428
1894.277909	8283.602013	62.722433
1893.916362	8219.415134	62.727438
1892.862633	8166.463030	62.732442
1892.603671	8095.514314	62.737447
1891.984129	8038.710858	62.742452
1891.391829	7972.491951	62.747457
1890.803540	7903.324546	62.752462
1889.714288	7845.517565	62.757466
1889.487906	7776.435291	62.762471
1888.828106	7723.187516	62.767476
1888.221564	7649.211895	62.772481
1887.471701	7586.897137	62.777486
1886.631191	7524.518931	62.782490
1886.353405	7454.629802	62.787495
1885.496560	7392.653917	62.792500
1884.847390	7327.702009	62.797505
1884.151306	7265.130770	62.802510
1883.396839	7200.458829	62.807514
1882.933529	7138.730756	62.812519
1882.275924	7072.839387	62.817524
1881.643770	7015.857625	62.822529
1880.950544	6938.989962	62.827534
1880.037403	6886.789614	62.832538
1879.832717	6811.096564	62.837543
1879.254529	6746.691269	62.842548
1878.334295	6681.522527	62.847553
1877.778704	6611.620713	62.852558
1876.829025	6549.859497	62.857562
1876.305089	6483.843807	62.862567
1875.583330	6425.894065	62.867572
1874.909635	6356.958009	62.872577
1874.425813	6293.255950	62.877582
1873.499528	6236.681999	62.882586
1872.751655	6163.987260	62.887591
1872.320460	6104.248564	62.892596
1871.558754	6045.652721	62.897601
1870.908711	5979.633263	62.902606
1870.193666	5912.805639	62.907610
1869.495730	5848.165312	62.912615
1868.730669	5784.686779	62.917620
1868.093561	5721.573134	62.922625
1867.572425	5658.864136	62.927630
1866.923539	5597.368333	62.932634
1866.143548	5529.678772	62.937639
1865.698667	5478.845407	62.942644
1864.779218	5414.506384	62.947649
1864.199400	5351.425447	62.952654
1863.562054	5299.948064	62.957658
1862.560184	5238.734598	62.962663
1862.151170	5175.417478	62.967668
1861.549730	5118.886928	62.972673
1861.051721	5056.773900	62.977678
1860.369985	4998.888062	62.982682
1859.597310	4932.664002	62.987687
1859.072664	4860.339324	62.992692
1858.213959	4798.955875	62.997697
1857.768323	4741.815202	63.002702
1857.163876	4683.626493	63.007706
1856.424470	4611.987051	63.012711
1855.715247	4553.944842	63.017716
1854.787197	4498.997087	63.022721
1854.532067	4419.875519	63.027726
1853.751932	4369.377620	63.032730
1853.006348	4308.376556	63.037735
1852.722632	4252.589959	63.042740
1851.602998	4188.841743	63.047745
1851.261453	4121.392671	63.052750
1850.491629	4060.297894	63.057754
1849.923784	3992.913737	63.062759
1849.218120	3940.150587	63.067764
1848.691018	3872.237604	63.072769
1847.750874	3803.219311	63.077774
1846.884374	3743.142841	63.082778
1846.485334	3679.154647	63.087783
1845.515092	3624.542585	63.092788
1844.941596	3565.129343	63.097793
1844.436519	3508.830212	63.102798
1843.551222	3452.917393	63.107802
1843.206339	3393.056858	63.112807
1842.396751	3339.209807	63.117812
1841.490807	3278.384381	63.122817
1840.866532	3210.394456	63.127822
1840.247110	3164.401299	63.132826
1839.494120	3105.374103	63.137831
1838.917671	3044.856164	63.142836
1838.150096	2992.329438	63.147841
1837.767316	2925.600601	63.152846
1837.052520	2877.405820	63.157850
1836.557690	2811.248922	63.162855
1835.623196	2749.412092	63.167860
1834.589902	2691.178701	63.172865
1834.448474	2634.653257	63.177870
1833.367904	2586.877129	63.182874
1832.868781	2525.371947	63.187879
1832.599022	2465.992999	63.192884
1831.683063	2413.577083	63.197889
1831.016499	2349.794887	63.202894
1830.179261	2302.368261	63.207898
1829.571663	2247.277900	63.212903
1829.037928	2187.042987	63.217908
1828.245764	2135.023220	63.222913
1827.918548	2079.052263	63.227918
1827.436779	2022.504364	63.232922
1826.322356	1954.932463	63.237927
1825.865233	1913.495248	63.242932
1824.948876	1850.515097	63.247937
1824.482246	1786.029371	63.252942
1823.523535	1740.412368	63.257946
1822.958072	1677.718699	63.262951
1822.492633	1623.925041	63.267956
1821.549447	1580.404473	63.272961
1821.097993	1519.165646	63.277966
1820.272273	1465.619039	63.282970
1819.689962	1405.375349	63.287975
1818.851517	1360.509289	63.292980
1818.090342	1309.701141	63.297985
1817.407423	1253.326162	63.302990
1816.847468	1212.293661	63.307994
1816.147813	1148.198663	63.312999
1815.795321	1093.117887	63.318004
1814.853648	1040.509125	63.323009
1814.494794	991.950997	63.328014
1813.751399	945.455405	63.333018
1812.703679	895.606545	63.338023
1812.431323	842.726621	63.343028
1811.499233	788.120688	63.348033
1811.078262	733.810710	63.353038
1810.139714	687.130879	63.358042
1809.598584	633.229890	63.363047
1809.039865	577.890482	63.368052
1808.044392	535.705271	63.373057
1807.567056	478.172284	63.378062
1806.782143	437.835314	63.383066
1806.011551	385.170220	63.388071
1805.604396	349.906694	63.393076
1804.719604	306.108640	63.398081
1804.262524	256.605015	63.403086
1803.381425	213.468208	63.408090
1802.499883	166.016160	63.413095
1801.896245	125.722237	63.418100
1801.025171	100.502709	63.423105
1800.544110	48.027834	63.428110
1799.668865	11.038557	63.433114
1798.396329	-26.346433	63.438119
1797.624066	-52.062361	63.443124
1796.511777	-70.053882	63.448129
1792.071644	13.716688	63.453134
1789.484835	70.275894	63.458138
1790.885407	69.922665	63.463143
1791.924809	73.157656	63.468148
1792.196883	71.176421	63.473153
1792.540307	57.837478	63.478158
1792.087760	56.458607	63.483162
1791.379786	62.592033	63.488167
1789.825925	59.588724	63.493172
1788.404961	73.086340	63.498177
1787.631426	71.225424	63.503182
1787.175412	70.129383	63.508186
1786.516905	74.999681	63.513191
1786.596428	68.896832	63.518196
1786.245859	73.440678	63.523201
1785.640799	73.483232	63.528206
1784.756492	69.089930	63.533210
1783.858161	69.724695	63.538215
1783.194168	69.197857	63.543220
1781.631150	75.836094	63.548225
1781.635094	65.656135	63.553230
1781.223494	74.688301	63.558234
1780.335802	68.598706	63.563239
1779.916103	70.557819	63.568244
1779.707626	77.655889	63.573249
1779.388442	77.112139	63.578254
1778.190497	79.895029	63.583258
1777.453230	79.961736	63.588263
1777.043255	79.683146	63.593268
1775.749168	83.372301	63.598273
1775.233640	77.639923	63.603278
1774.165574	75.289612	63.608282
1773.674283	68.417962	63.613287
1773.903387	69.080262	63.618292
1773.097044	73.360596	63.623297
1772.392642	68.605984	63.628302
1771.749044	72.830508	63.633306
1770.840478	74.118197	63.638311
1770.539287	71.929954	63.643316
1769.299287	81.752865	63.648321
1768.430633	68.773571	63.653326
1767.668033	76.093686	63.658330
1767.759775	72.057896	63.663335
1767.777312	70.615410	63.668340
1766.073078	69.925773	63.673345
1765.401852	72.369544	63.678350
1765.266448	69.880577	63.683354
1764.313820	72.463659	63.688359
1764.025056	72.686224	63.693364
1762.923911	74.400323	63.698369
1762.093033	72.887573	63.703374
1761.381092	76.517394	63.708378
1760.629651	83.835743	63.713383
1760.567657	71.221933	63.718388
1760.009494	83.992750	63.723393
1759.245730	71.927218	63.728398
1758.285586	71.606696	63.733402
1758.106899	71.680891	63.738407
1757.482199	67.337834	63.743412
1756.597782	67.117251	63.748417
1755.628656	73.568136	63.753422
1755.155747	65.775770	63.758426
1754.538728	78.519660	63.763431
1754.092958	76.412729	63.768436
1753.204483	82.372984	63.773441
1752.525189	84.652458	63.778446
1752.330177	74.527750	63.783450
1751.369556	82.486461	63.788455
1750.911617	76.992529	63.793460
1749.658308	83.524826	63.798465
1749.134869	68.707145	63.803470
1748.775502	73.613520	63.808474
1747.823682	86.371168	63.813479
1747.358668	71.646710	63.818484
1746.497493	81.231264	63.823489
1746.185631	64.090208	63.828494
1745.384600	70.541206	63.833498
1744.519096	79.214952	63.838503
1743.844083	73.198825	63.843508
1742.919657	83.182942	63.848513
1742.521234	72.414019	63.853518
1741.691262	82.187587	63.858522
1741.178748	83.931210	63.863527
1741.053571	74.716370	63.868532
1740.107194	81.174688	63.873537
1739.480521	78.068300	63.878542
1739.104358	74.767581	63.883546
1738.114710	80.669791	63.888551
1737.925398	68.178712	63.893556
1737.027256	79.576358	63.898561
1736.689490	76.133920	63.903566
1735.863707	70.252133	63.908570
1734.877744	73.723628	63.913575
1734.202864	61.957817	63.918580
1733.160820	74.299272	63.923585
1733.124830	67.227582	63.928590
1732.413224	74.309367	63.933594
1731.245025	77.535414	63.938599
1730.936923	73.466935	63.943604
1730.203694	82.132293	63.948609
1729.524223	78.605354	63.953614
1728.713144	79.205779	63.958618
1728.562951	74.221226	63.963623
1727.555521	75.978802	63.968628
1726.417389	83.620355	63.973633
1726.374470	73.949321	63.978638
1726.248235	72.597481	63.983642
1724.413571	76.867691	63.988647
1724.075240	68.713328	63.993652
1724.177567	78.543825	63.998657
1723.343681	68.826535	64.003662
1722.029427	66.993177	64.008666
1721.050607	73.510268	64.013671
1720.727899	74.761690	64.018676
1720.573572	77.924478	64.023681
1720.292296	68.182495	64.028686
1719.613071	69.343885	64.033690
1718.715742	80.306160	64.038695
1718.270551	71.254121	64.043700
1717.223388	74.680149	64.048705
1716.087270	70.036706	64.053710
1715.545698	68.533214	64.058714
1715.290342	61.955273	64.063719
1714.743805	62.988353	64.068724
1713.245662	69.772440	64.073729
1712.588718	64.049929	64.078734
1712.876750	63.242581	64.083738
1711.957003	74.547465	64.088743
1711.473628	69.108049	64.093748
1710.367740	71.132009	64.098753
1709.769932	68.779574	64.103758
1709.243478	72.477716	64.108762
1708.619224	77.140737	64.113767
1708.295068	60.041075	64.118772
1707.571757	72.566878	64.123777
1707.094881	67.908613	64.128782
1705.895399	66.444970	64.133786
1704.611617	76.697487	64.138791
1704.440362	71.850325	64.143796
1703.842946	75.179689	64.148801
1703.500027	68.435880	64.153806
1702.481452	68.632448	64.158810
1701.663410	69.410608	64.163815
1701.452861	59.854524	64.168820
1700.529533	71.705611	64.173825
1699.652999	70.053476	64.178830
1699.350576	74.326326	64.183834
1698.796639	72.939921	64.188839
1698.474901	64.063828	64.193844
1697.633772	73.034912	64.198849
1697.306311	75.327899	64.203854
1696.020278	71.018943	64.208858
1694.959039	76.057312	64.213863
1694.247338	76.082134	64.218868
1693.756981	70.708487	64.223873
1693.664770	67.749033	64.228878
1693.018444	69.778851	64.233882
1692.082445	70.969996	64.238887
1691.778339	67.836040	64.243892
1691.228741	71.771254	64.248897
1690.707813	63.458246	64.253902
1689.491840	70.348912	64.258906
1688.380245	74.414401	64.263911
1687.842313	54.456528	64.268916
1686.908605	69.067400	64.273921
1686.456804	63.944681	64.278926
1686.141367	64.898479	64.283930
1685.145766	67.272367	64.288935
1685.347573	61.678388	64.293940
1684.406994	68.637276	64.298945
1683.749554	65.116317	64.303950
1683.112218	68.560836	64.308954
1682.514465	64.426413	64.313959
1682.100364	57.712844	64.318964
1680.738389	62.021535	64.323969
1679.830253	61.656511	64.328974
1679.348912	55.171248	64.333978
1678.499163	62.402716	64.338983
1678.425957	56.858733	64.343988
1678.125811	65.232941	64.348993
1677.455084	60.058268	64.353998
1677.130371	62.623636	64.359002
1675.887719	61.463337	64.364007
1675.295845	60.317935	64.369012
1674.413269	66.182649	64.374017
1673.464211	59.902573	64.379022
1673.017480	55.892401	64.384026
1671.846172	67.055897	64.389031
1671.320449	63.619675	64.394036
1671.140202	66.222020	64.399041
1670.340239	63.576851	64.404046
1669.666365	58.237099	64.409050
1668.723668	59.205384	64.414055
1668.178372	63.616165	64.419060
1667.725732	71.079452	64.424065
1667.199491	70.322601	64.429070
1666.572425	67.672045	64.434074
1666.028204	72.336551	64.439079
1665.510389	60.071147	64.444084
1664.333518	62.294061	64.449089
1663.267496	70.567583	64.454094
1662.901749	64.262657	64.459098
1661.885049	73.903471	64.464103
1661.825636	65.558156	64.469108
1660.838036	69.783732	64.474113
1660.736052	77.300131	64.479118
1660.189529	73.014068	64.484122
1659.853639	66.382695	64.489127
1658.949062	62.697573	64.494132
1657.890156	65.239224	64.499137
1657.039699	67.498600	64.504142
1656.579017	67.245432	64.509146
1655.882218	70.546436	64.514151
1655.355624	65.402488	64.519156
1654.778631	63.040453	64.524161
1653.386819	64.933236	64.529166
1652.753333	65.866600	64.534170
1652.032648	70.467676	64.539175
1652.097269	68.129872	64.544180
1651.459248	62.224600	64.549185
1650.857146	74.858892	64.554190
1650.555373	66.452730	64.559194
1649.687933	62.709672	64.564199
1648.486685	64.026550	64.569204
1647.545943	59.126597	64.574209
1646.603716	61.473095	64.579214
1646.624787	53.408321	64.584218
1645.909856	53.080426	64.589223
1645.369796	60.287935	64.594228
1645.009483	65.148734	64.599233
1644.655811	63.691103	64.604238
1643.484726	57.405312	64.609242
1642.668647	62.578215	64.614247
1641.895304	63.488067	64.619252
1641.648385	56.799989	64.624257
1640.763509	62.720271	64.629262
1640.339189	52.969502	64.634266
1639.207924	64.344267	64.639271
1638.515854	59.362235	64.644276
1637.928832	57.334541	64.649281
1637.193106	65.508285	64.654286
1636.596502	59.926028	64.659290
1635.807168	64.538012	64.664295
1635.740468	65.382913	64.669300
1635.619296	66.457244	64.674305
1634.501015	65.698260	64.679310
1633.622201	62.501072	64.684314
1632.931796	62.519374	64.689319
1632.145781	60.885999	64.694324
1631.247570	76.502093	64.699329
1630.114677	66.759806	64.704334
1630.342475	65.936787	64.709338
1629.435981	67.309350	64.714343
1628.740259	58.581001	64.719348
1628.188864	64.356842	64.724353
1627.617680	57.723436	64.729358
1627.341528	67.309684	64.734362
1626.342660	68.392567	64.739367
1625.514804	57.890610	64.744372
1624.625985	54.349659	64.749377
1624.018991	58.978408	64.754382
1623.441589	49.322930	64.759386
1622.853560	55.148744	64.764391
1622.662370	55.718528	64.769396
1621.759051	57.342904	64.774401
1620.582295	57.441631	64.779406
1620.267647	56.173350	64.784410
1618.936421	62.161396	64.789415
1618.986745	52.786240	64.794420
1618.488622	59.572344	64.799425
1617.373187	52.834597	64.804430
1617.462248	54.589898	64.809434
1616.498115	66.737647	64.814439
1615.876580	61.654527	64.819444
1615.099765	61.186659	64.824449
1614.459370	62.870193	64.829454
1614.226742	59.538811	64.834458
1612.566084	65.407310	64.839463
1611.919326	66.150401	64.844468
1611.431798	55.050325	64.849473
1610.727415	67.059035	64.854478
1610.585087	60.322804	64.859482
1609.790444	63.223040	64.864487
1609.540898	56.235760	64.869492
1608.558553	63.018373	64.874497
1607.231468	69.754835	64.879502
1606.707049	63.457784	64.884506
1606.062043	66.573948	64.889511
1605.542457	62.934915	64.894516
1605.360078	63.903852	64.899521
1604.723048	63.672403	64.904526
1604.313073	51.675327	64.909530
1603.201731	55.732918	64.914535
1602.517249	56.349537	64.919540
1601.962594	55.373284	64.924545
1601.131766	52.083330	64.929550
1600.822795	55.368458	64.934554
1599.401923	66.555858	64.939559
1598.737624	64.046857	64.944564
1598.197815	61.169565	64.949569
1597.696536	57.262694	64.954574
1597.440045	61.454132	64.959578
1596.926833	67.529846	64.964583
1596.417234	62.521989	64.969588
1595.569962	65.495247	64.974593
1594.186797	67.001905	64.979598
1593.799730	55.247197	64.984602
1592.991737	66.671543	64.989607
1592.535015	58.860882	64.994612
1592.418865	56.745770	64.999617
1590.992595	67.509825	65.004622
1590.813051	53.616882	65.009626
1589.700368	55.501618	65.014631
1589.543824	57.873115	65.019636
1589.074588	60.313217	65.024641
1587.655226	55.675420	65.029646
1586.954570	54.733407	65.034650
1586.130930	61.875592	65.039655
1585.840494	59.565818	65.044660
1585.405884	55.060145	65.049665
1585.101822	59.062020	65.054670
1584.539276	45.212593	65.059674
1583.387819	59.799726	65.064679
1582.612573	51.612320	65.069684
1582.003728	54.951404	65.074689
1581.331208	55.671785	65.079694
1581.275070	54.263086	65.084698
1579.396725	67.693102	65.089703
1578.842946	49.943992	65.094708
1578.090002	55.370233	65.099713
1577.547572	62.191769	65.104718
1577.889848	49.214148	65.109722
1577.104064	53.300447	65.114727
1576.785688	60.942680	65.119732
1575.628361	57.717227	65.124737
1574.125942	61.335491	65.129742
1574.070956	61.301732	65.134746
1573.178518	61.237031	65.139751
1572.837494	69.553083	65.144756
1572.562172	59.341830	65.149761
1571.601148	67.234414	65.154766
1570.756552	54.535261	65.159770
1569.996510	63.925576	65.164775
1569.417050	56.476629	65.169780
1569.220591	68.254827	65.174785
1568.068767	69.871399	65.179790
1567.319852	56.191932	65.184794
1566.430469	65.273212	65.189799
1566.081921	56.347796	65.194804
1565.736288	55.469228	65.199809
1564.987227	60.103215	65.204814
1564.481551	51.194884	65.209818
1563.112679	60.167843	65.214823
1562.504798	62.793986	65.219828
1562.253831	58.088824	65.224833
1561.390095	65.748329	65.229838
1560.828129	56.150339	65.234842
1560.289038	67.982980	65.239847
1559.901812	56.611511	65.244852
1559.053058	57.172241	65.249857
1557.682679	65.391652	65.254862
1557.683323	54.611422	65.259866
1557.093739	69.432572	65.264871
1556.729361	58.976849	65.269876
1555.815872	58.568565	65.274881
1554.613398	54.836202	65.279886
1553.987894	51.193514	65.284890
1553.732575	63.074102	65.289895
1553.139103	57.639608	65.294900
1552.914198	62.699674	65.299905
1551.554435	61.775668	65.304910
1551.042342	58.925523	65.309914
1550.386657	63.647181	65.314919
1550.044306	61.593246	65.319924
1548.845302	67.008374	65.324929
1547.574646	65.726429	65.329934
1547.203377	53.286395	65.334938
1546.604026	58.046409	65.339943
1546.346767	64.163460	65.344948
1546.152923	51.463419	65.349953
1545.558238	63.490974	65.354958
1544.970754	46.543612	65.359962
1543.411997	57.499046	65.364967
1542.952725	55.041063	65.369972
1542.506192	54.468695	65.374977
1541.652483	59.579793	65.379982
1541.621871	46.934244	65.384986
1540.415963	55.441340	65.389991
1539.415270	66.440570	65.394996
1539.056782	55.230124	65.400001
1538.761708	63.209284	65.405006
1538.319815	63.102964	65.410010
1537.301883	64.729812	65.415015
1536.740594	61.728213	65.420020
1536.272485	58.984625	65.425025
1534.971177	68.800010	65.430030
1534.146153	51.699578	65.435034
1533.034224	68.065587	65.440039
1532.983803	56.777802	65.445044
1532.631707	56.467977	65.450049
1531.901437	59.061534	65.455054
1531.662321	55.172945	65.460058
1530.881155	63.238810	65.465063
1529.727603	62.335665	65.470068
1529.537277	52.440508	65.475073
1528.580709	65.232057	65.480078
1528.075746	47.965653	65.485082
1526.747799	60.253234	65.490087
1526.156923	55.416010	65.495092
1525.443854	50.065188	65.500097
1525.063552	62.615349	65.505102
1524.773025	53.155591	65.510106
1524.216946	64.140941	65.515111
1523.753883	61.913801	65.520116
1522.605213	58.062516	65.525121
1521.591585	66.420796	65.530126
1521.109973	56.176105	65.535130
1520.602381	61.624875	65.540135
1520.471575	64.361297	65.545140
1519.493491	59.382175	65.550145
1518.340537	62.697350	65.555150
1517.916693	61.504783	65.560154
1517.514915	61.146084	65.565159
1516.851044	63.552472	65.570164
1515.742170	60.540124	65.575169
1514.853678	56.918737	65.580174
1514.558442	58.364514	65.585178
1513.994452	63.953137	65.590183
1513.582672	53.224261	65.595188
1513.036344	56.353148	65.600193
1511.929497	65.888475	65.605198
1511.267202	53.486814	65.610202
1510.601754	62.062580	65.615207
1510.019858	61.787700	65.620212
1510.079816	54.585670	65.625217
1508.745433	57.565398	65.630222
1508.135187	58.518757	65.635226
1507.287881	62.960210	65.640231
1506.848618	67.116044	65.645236
1506.729296	54.962415	65.650241
1505.526454	65.498609	65.655246
1504.809349	53.960381	65.660250
1504.273636	58.498975	65.665255
1503.723252	59.729831	65.670260
1502.494923	51.611306	65.675265
1501.433369	68.641109	65.680270
1501.054211	52.767688	65.685274
1500.779425	51.925180	65.690279
1500.119842	51.066552	65.695284
1499.769540	53.145563	65.700289
1498.902043	63.961206	65.705294
1498.363800	49.940786	65.710298
1497.637122	67.289536	65.715303
1496.611274	56.434320	65.720308
1496.534036	49.050667	65.725313
1495.782123	54.194485	65.730318
1494.851684	58.882545	65.735322
1494.133478	57.192706	65.740327
1493.301211	64.509754	65.745332
1492.803510	56.989488	65.750337
1492.178298	62.660384	65.755342
1492.019412	57.529009	65.760346
1490.617446	63.503124	65.765351
1489.821809	60.199731	65.770356
1489.537143	59.410834	65.775361
1488.895480	61.376877	65.780366
1488.500212	62.490043	65.785370
1488.111331	55.174839	65.790375
1486.999298	56.042366	65.795380
1486.430650	59.509123	65.800385
1485.756152	70.139559	65.805390
1485.148158	51.635845	65.810394
1483.963755	63.159454	65.815399
1483.194844	54.919038	65.820404
1483.130629	58.956920	65.825409
1482.257995	67.119337	65.830414
1482.042364	53.312580	65.835418
1481.529621	58.678593	65.840423
1480.364202	57.053525	65.845428
1480.095947	53.227922	65.850433
1479.263033	59.781818	65.855438
1478.727659	46.513169	65.860442
1477.386532	55.172667	65.865447
1476.565113	61.772046	65.870452
1476.480431	51.983114	65.875457
1475.549653	53.638711	65.880462
1475.480379	56.627131	65.885466
1474.143374	53.482324	65.890471
1473.149337	58.212038	65.895476
1472.972959	50.968724	65.900481
1472.261818	59.294711	65.905486
1472.203914	57.514130	65.910490
1471.588915	55.941939	65.915495
1470.468303	56.925955	65.920500
1469.901086	47.114367	65.925505
1469.368046	57.766468	65.930510
1468.494123	59.912934	65.935514
1467.597116	60.300010	65.940519
1466.540226	60.688843	65.945524
1466.383001	56.821941	65.950529
1465.588054	67.001581	65.955534
1465.471645	55.473556	65.960538
1465.193247	65.191048	65.965543
1463.730487	63.414545	65.970548
1462.954776	50.698190	65.975553
1462.113590	58.727874	65.980558
1461.935590	52.095109	65.985562
1461.531841	54.338739	65.990567
1460.626019	55.695481	65.995572
1459.724776	43.270324	66.000577
1459.152678	60.848395	66.005582
1458.805137	49.555809	66.010586
1458.174649	56.594783	66.015591
1457.262053	55.169244	66.020596
1456.577389	44.668267	66.025601
1455.703535	53.679289	66.030606
1455.517173	53.502408	66.035610
1455.010961	50.984094	66.040615
1453.571595	53.775527	66.045620
1453.189890	54.413450	66.050625
1451.813245	56.228231	66.055630
1452.268260	55.061575	66.060634
1451.588310	53.021889	66.065639
1450.910516	58.308482	66.070644
1450.249584	54.239362	66.075649
1449.305576	54.406831	66.080654
1449.042286	64.319043	66.085658
1447.885619	50.461588	66.090663
1446.597880	55.258491	66.095668
1446.434485	56.415234	66.100673
1445.570412	57.549300	66.105678
1445.376487	51.415815	66.110682
1444.859369	55.514641	66.115687
1444.316100	55.030207	66.120692
1443.995754	45.553133	66.125697
1442.710797	55.528375	66.130702
1442.187560	51.478374	66.135706
1441.851514	52.720907	66.140711
1440.560981	60.588625	66.145716
1439.889751	54.139914	66.150721
1439.017593	56.377572	66.155726
1438.654471	56.938425	66.160730
1438.668744	50.423339	66.165735
1437.071689	57.032466	66.170740
1436.863652	56.109969	66.175745
1435.562387	52.289290	66.180750
1435.395267	52.882069	66.185754
1434.914166	56.010064	66.190759
1434.520395	53.838163	66.195764
1433.769459	55.506191	66.200769
1432.794993	54.044762	66.205774
1432.494246	57.249749	66.210778
1431.968952	53.261579	66.215783
1430.450428	60.537904	66.220788
1430.020941	53.975078	66.225793
1429.603768	57.395692	66.230798
1429.000347	50.390575	66.235802
1428.334677	53.033814	66.240807
1427.445199	52.359982	66.245812
1427.068555	51.040080	66.250817
1426.388405	56.336513	66.255822
1426.023826	57.285535	66.260826
1424.908853	62.099144	66.265831
1423.979414	61.614593	66.270836
1423.490565	58.486390	66.275841
1422.746885	63.567417	66.280846
1422.441910	58.891361	66.285850
1421.455408	54.618529	66.290855
1420.623092	59.538600	66.295860
1420.515968	53.924338	66.300865
1419.867940	59.780224	66.305870
1419.117263	58.060876	66.310874
1418.235576	50.648979	66.315879
1417.240954	58.723564	66.320884
1417.213076	50.083111	66.325889
1416.437872	51.305563	66.330894
1415.874421	57.908107	66.335898
1415.100683	59.412606	66.340903
1414.036792	53.568797	66.345908
1413.913383	53.337757	66.350913
1413.352262	58.293572	66.355918
1412.222901	53.931486	66.360922
1411.204261	56.129358	66.365927
1410.612937	63.908027	66.370932
1410.190871	49.306193	66.375937
1409.778165	53.516161	66.380942
1409.480186	47.621576	66.385946
1408.818849	54.419454	66.390951
1407.447196	62.394700	66.395956
1407.048958	50.920948	66.400961
1406.459086	52.169138	66.405966
1405.981184	54.956003	66.410970
1405.253715	54.910870	66.415975
1403.891708	50.812854	66.420980
1403.855245	48.336578	66.425985
1403.263793	61.336624	66.430990
1402.743593	51.039759	66.435994
1402.025399	51.283315	66.440999
1400.871945	54.306876	66.446004
1400.646670	45.969044	66.451009
1400.007993	52.733358	66.456014
1399.047108	55.947086	66.461018
1398.195542	52.263104	66.466023
1397.220633	58.691355	66.471028
1397.067806	47.656422	66.476033
1396.361075	53.606798	66.481038
1396.049343	55.521993	66.486042
1395.832585	51.721334	66.491047
1394.563312	57.885714	66.496052
1394.001153	48.967490	66.501057
1393.545736	50.739942	66.506062
1392.151332	59.797459	66.511066
1391.462969	54.759725	66.516071
1390.753689	47.807719	66.521076
1390.771846	43.495052	66.526081
1389.944331	52.618573	66.531086
1389.590618	55.295811	66.536090
1389.020640	58.255013	66.541095
1387.817680	59.267924	66.546100
1387.557325	49.965830	66.551105
1387.118948	53.336202	66.556110
1385.797881	47.222627	66.561114
1385.195008	50.876194	66.566119
1384.164172	59.399675	66.571124
1383.992017	50.285413	66.576129
1383.653001	56.237265	66.581134
1382.616389	51.743755	66.586138
1381.760037	49.859866	66.591143
1380.941404	49.338794	66.596148
1380.800641	50.550290	66.601153
1380.409291	66.098459	66.606158
1379.025610	60.349655	66.611162
1378.392231	56.742960	66.616167
1377.853512	52.862595	66.621172
1377.427965	54.887349	66.626177
1376.938208	52.134621	66.631182
1376.202589	61.552629	66.636186
1375.652275	55.337033	66.641191
1374.576107	55.476652	66.646196
1374.400590	55.209742	66.651201
1373.125934	57.997113	66.656206
1372.421820	57.672306	66.661210
1372.152007	56.519936	66.666215
1371.330224	58.987730	66.671220
1371.296855	49.348355	66.676225
1370.205877	55.796642	66.681230
1369.166760	57.737584	66.686234
1368.646886	55.229345	66.691239
1368.136589	53.773002	66.696244
1367.930365	55.859086	66.701249
1366.676035	54.073162	66.706254
1366.185422	57.652117	66.711258
1365.495651	53.073515	66.716263
1365.015758	58.464284	66.721268
1364.408061	54.001946	66.726273
1363.237371	52.488160	66.731278
1362.556267	52.224354	66.736282
1362.364354	55.041456	66.741287
1361.784408	56.467853	66.746292
1360.760978	51.537013	66.751297
1359.689652	55.712917	66.756302
1359.052685	62.653592	66.761306
1359.095527	53.915167	66.766311
1358.347702	65.164408	66.771316
1358.069115	57.434302	66.776321
1356.930201	65.725815	66.781326
1356.291448	56.100675	66.786330
1355.622007	55.639472	66.791335
1354.392997	57.348831	66.796340
1353.732935	60.114200	66.801345
1353.137142	56.358033	66.806350
1352.685084	59.460924	66.811354
1352.430704	53.027976	66.816359
1351.622078	58.136689	66.821364
1351.834776	50.897773	66.826369
1350.309355	54.986597	66.831374
1349.574630	55.168140	66.836378
1349.154992	52.103070	66.841383
1348.584889	57.364678	66.846388
1347.432286	59.134433	66.851393
1346.796008	55.157620	66.856398
1346.052910	51.875889	66.861402
1345.951393	54.032061	66.866407
1345.333334	59.794887	66.871412
1344.552051	47.803303	66.876417
1343.742959	53.684807	66.881422
1342.893765	61.223779	66.886426
1342.894648	54.453779	66.891431
1341.777134	55.394779	66.896436
1340.951297	58.050887	66.901441
1340.399648	54.689833	66.906446
1339.512302	64.065738	66.911450
1339.063573	49.747290	66.916455
1337.821107	50.285528	66.921460
1337.827474	47.651057	66.926465
1337.326719	61.147627	66.931470
1336.615602	65.482321	66.936474
1335.782683	50.292962	66.941479
1334.689225	54.068689	66.946484
1334.516366	54.827968	66.951489
1333.857451	55.995687	66.956494
1333.239033	54.916090	66.961498
1332.490747	46.536840	66.966503
1331.388967	57.359800	66.971508
1331.018359	51.639202	66.976513
1330.612716	50.472162	66.981518
1329.936703	53.932362	66.986522
1329.664019	44.187538	66.991527
1328.189455	57.439953	66.996532
1327.999552	47.950051	67.001537
1327.485548	54.820714	67.006542
1326.722494	59.532678	67.011546
1325.866810	56.527474	67.016551
1325.290673	62.985392	67.021556
1324.691552	54.498846	67.026561
1323.784524	56.518154	67.031566
1322.640025	59.379473	67.036570
1322.248846	54.999419	67.041575
1321.636587	56.484579	67.046580
1321.634524	62.889074	67.051585
1321.100459	57.886755	67.056590
1319.855263	56.578801	67.061594
1319.269676	50.640071	67.066599
1318.728913	53.310785	67.071604
1318.265894	52.036173	67.076609
1316.887082	50.408839	67.081614
1316.248817	50.273854	67.086618
1315.760308	48.440317	67.091623
1315.528584	46.975966	67.096628
1314.961102	47.848451	67.101633
1313.958376	56.853189	67.106638
1313.057706	59.295696	67.111642
1312.862326	52.537980	67.116647
1312.168624	64.264330	67.121652
1311.308791	55.238913	67.126657
1310.291760	61.695967	67.131662
1309.622844	61.392390	67.136666
1309.363822	56.515081	67.141671
1308.536796	60.013490	67.146676
1308.687564	58.179238	67.151681
1307.735851	55.276043	67.156686
1306.573137	54.207298	67.161690
1306.524162	47.090414	67.166695
1304.882921	66.292449	67.171700
1304.209573	60.924344	67.176705
1303.449768	62.768862	67.181710
1302.895382	58.801118	67.186714
1302.625786	58.766794	67.191719
1302.432325	60.319414	67.196724
1301.970032	58.025966	67.201729
1301.030839	56.126891	67.206734
1300.061005	57.121699	67.211738
1299.908009	52.107685	67.216743
1298.710288	60.015900	67.221748
1298.113161	48.681038	67.226753
1297.451861	58.074625	67.231758
1296.740240	54.767403	67.236762
1296.623924	49.542552	67.241767
1295.257589	62.919705	67.246772
1294.756496	59.115380	67.251777
1294.282014	56.669327	67.256782
1293.621854	64.361186	67.261786
1293.066956	53.142611	67.266791
1291.955541	58.501336	67.271796
1291.486854	58.484476	67.276801
1291.222957	51.714003	67.281806
1290.323056	62.541151	67.286810
1289.433156	56.978823	67.291815
1288.448331	59.038898	67.296820
1288.312971	52.825160	67.301825
1287.751581	53.340287	67.306830
1286.962933	55.482712	67.311834
1285.884406	60.219614	67.316839
1285.330675	57.852397	67.321844
1285.140031	54.552230	67.326849
1284.567047	55.237937	67.331854
1283.663164	62.832930	67.336858
1282.627551	51.720758	67.341863
1282.177867	56.543755	67.346868
1281.499930	54.562146	67.351873
1281.522263	57.586462	67.356878
1280.066154	56.073942	67.361882
1279.723071	49.901120	67.366887
1278.525312	59.368972	67.371892
1278.150157	56.396191	67.376897
1278.078746	53.436615	67.381902
1277.161752	59.191791	67.386906
1276.774657	54.413700	67.391911
1275.782306	64.899158	67.396916
1275.317993	53.361830	67.401921
1274.216674	52.341686	67.406926
1273.196852	57.212762	67.411930
1273.096037	48.434111	67.416935
1272.395653	61.870963	67.421940
1271.765645	58.236954	67.426945
1271.259486	54.774067	67.431950
1270.191515	53.026369	67.436954
1270.146082	51.136581	67.441959
1269.100195	60.096158	67.446964
1268.107116	56.218680	67.451969
1267.670131	52.443594	67.456974
1266.650643	56.258049	67.461978
1266.713226	48.667684	67.466983
1265.891695	54.790885	67.471988
1264.692548	54.723022	67.476993
1264.376759	49.540931	67.481998
1263.457616	53.711595	67.487002
1263.290362	52.328462	67.492007
1262.775485	58.388712	67.497012
1261.627471	62.351342	67.502017
1260.673613	51.364955	67.507022
1260.263620	53.988078	67.512026
1260.117948	47.894257	67.517031
1259.421877	49.917888	67.522036
1258.545680	51.873967	67.527041
1257.771932	45.369082	67.532046
1257.288196	49.670787	67.537050
1256.728182	52.019718	67.542055
1255.434516	56.611066	67.547060
1254.993580	55.771352	67.552065
1254.653265	49.853564	67.557070
1253.938869	61.649443	67.562074
1253.760139	56.530714	67.567079
1252.391800	57.401249	67.572084
1251.869711	57.038070	67.577089
1251.609781	53.077135	67.582094
1250.718852	64.369650	67.587098
1249.788668	53.691742	67.592103
1249.093151	59.306051	67.597108
1248.435208	55.252286	67.602113
1248.047073	49.682729	67.607118
1247.027546	55.637145	67.612122
1246.721666	51.669326	67.617127
1245.842196	56.216891	67.622132
1245.398377	51.086702	67.627137
1244.678340	52.226314	67.632142
1244.225133	56.351279	67.637146
1243.160233	45.287945	67.642151
1242.633671	52.375083	67.647156
1242.277746	58.340672	67.652161
1241.453265	48.629994	67.657166
1240.201796	44.836199	67.662170
1239.744014	52.806541	67.667175
1239.124849	55.972291	67.672180
1238.552151	52.777039	67.677185
1238.473456	48.451392	67.682190
1237.407968	56.997774	67.687194
1236.788445	52.016954	67.692199
1235.895179	51.447872	67.697204
1235.464708	55.985542	67.702209
1235.019697	49.601854	67.707214
1233.851138	55.813365	67.712218
1233.547738	50.618271	67.717223
1233.091025	56.379112	67.722228
1231.903296	52.491603	67.727233
1231.300794	43.518348	67.732238
1230.641091	57.800295	67.737242
1230.158901	56.792102	67.742247
1229.586676	60.396673	67.747252
1228.586980	52.670881	67.752257
1228.431218	50.724522	67.757262
1227.537411	61.624832	67.762266
1227.445166	57.321839	67.767271
1225.984662	52.124672	67.772276
1225.169941	51.396445	67.777281
1224.817472	49.082395	67.782286
1224.251079	61.914466	67.787290
1223.916933	46.762544	67.792295
1222.850433	53.277953	67.797300
1222.052750	54.739006	67.802305
1221.868140	58.591022	67.807310
1220.533998	60.960565	67.812314
1219.902613	59.767940	67.817319
1219.252068	57.146474	67.822324
1218.611791	52.648358	67.827329
1218.463393	54.482402	67.832334
1217.976934	60.005123	67.837338
1217.070466	55.997198	67.842343
1216.020665	65.264926	67.847348
1215.541725	59.407034	67.852353
1215.311279	54.392730	67.857358
1213.966066	58.711595	67.862362
1213.311552	52.820126	67.867367
1212.736169	60.071156	67.872372
1212.425933	62.195869	67.877377
1212.166650	62.339689	67.882382
1210.883288	59.397811	67.887386
1210.310036	52.244460	67.892391
1209.764652	53.845167	67.897396
1208.941814	51.883469	67.902401
1208.040823	45.881391	67.907406
1206.994993	54.207033	67.912410
1206.996718	53.626516	67.917415
1206.512197	53.785657	67.922420
1206.137713	56.305368	67.927425
1205.289746	57.017477	67.932430
1204.057357	51.531730	67.937434
1203.733391	57.083804	67.942439
1203.248526	57.780746	67.947444
1202.175520	57.607695	67.952449
1201.593733	55.982982	67.957454
1200.874068	58.762596	67.962458
1200.438592	56.748758	67.967463
1200.020970	59.385719	67.972468
1198.861689	51.977061	67.977473
1198.514690	47.069608	67.982478
1197.707777	58.374000	67.987482
1197.197556	52.767098	67.992487
1195.914035	50.274691	67.997492
1194.881136	53.440016	68.002497
1195.080615	47.232964	68.007502
1194.347087	58.014748	68.012506
1194.005685	52.724777	68.017511
1193.667290	54.068639	68.022516
1192.795439	48.194397	68.027521
1192.062759	44.657168	68.032526
1191.069887	56.210333	68.037530
1190.573460	45.900297	68.042535
1189.465606	51.438266	68.047540
1188.823187	55.364669	68.052545
1188.380244	58.505557	68.057550
1188.027984	58.501739	68.062554
1187.783292	55.251179	68.067559
1186.476072	57.097634	68.072564
1185.712425	59.508928	68.077569
1185.427713	44.804902	68.082574
1184.466484	53.233791	68.087578
1183.861907	40.879863	68.092583
1183.212023	49.940484	68.097588
1182.586461	55.094243	68.102593
1182.326394	49.673067	68.107598
1180.855560	55.866441	68.112602
1180.236817	56.297671	68.117607
1180.205686	50.806969	68.122612
1179.534890	46.209641	68.127617
1178.767720	47.801472	68.132622
1177.392073	55.878379	68.137626
1176.972991	45.294269	68.142631
1176.360874	49.384589	68.147636
1176.017770	49.847676	68.152641
1176.114011	49.002967	68.157646
1174.653283	54.276940	68.162650
1174.341494	47.695459	68.167655
1173.555170	49.142103	68.172660
1172.163661	47.149437	68.177665
1171.730161	42.897575	68.182670
1170.960969	51.967712	68.187674
1170.769564	45.707711	68.192679
1170.295652	48.005116	68.197684
1169.670560	61.855788	68.202689
1168.824335	50.939061	68.207694
1167.934928	57.607677	68.212698
1167.540877	51.398828	68.217703
1166.311751	49.552227	68.222708
1165.550821	52.984969	68.227713
1165.271173	43.100939	68.232718
1164.499394	51.171692	68.237722
1164.474517	50.503943	68.242727
1163.608295	49.427532	68.247732
1162.308188	59.480990	68.252737
1162.008104	50.741932	68.257742
1161.368370	55.762330	68.262746
1161.170266	50.351803	68.267751
1160.307128	55.196420	68.272756
1159.499526	54.203728	68.277761
1159.360863	50.702918	68.282766
1157.664440	49.834249	68.287770
1157.018766	41.512867	68.292775
1156.634696	45.084366	68.297780
1156.257005	55.770134	68.302785
1156.104367	50.458033	68.307790
1154.927668	53.837058	68.312794
1154.007728	48.489303	68.317799
1153.595998	42.407853	68.322804
1153.203667	49.811122	68.327809
1152.193455	38.340172	68.332814
1150.965650	47.123707	68.337818
1150.762462	41.982078	68.342823
1150.031254	42.139464	68.347828
1149.355398	50.398391	68.352833
1149.408066	42.845884	68.357838
1148.089042	48.206141	68.362842
1147.533039	46.378644	68.367847
1147.187604	45.509567	68.372852
1146.174120	51.489863	68.377857
1145.699623	37.401097	68.382862
1144.867303	50.374811	68.387866
1144.446599	51.717577	68.392871
1143.821319	51.113788	68.397876
1142.194789	53.364294	68.402881
1142.287533	39.764050	68.407886
1141.563993	53.223517	68.412890
1141.057300	40.098668	68.417895
1140.572269	41.997296	68.422900
1139.394424	51.037821	68.427905
1138.862418	42.726750	68.432910
1138.262902	44.131075	68.437914
1138.074334	44.825054	68.442919
1136.726424	45.030074	68.447924
1135.851495	53.057316	68.452929
1135.501232	53.955213	68.457934
1135.021544	48.408128	68.462938
1134.807005	47.453577	68.467943
1133.662638	45.606128	68.472948
1132.828959	52.048265	68.477953
1132.661616	41.097696	68.482958
1131.987330	50.832418	68.487962
1130.989026	46.402318	68.492967
1130.049978	41.046577	68.497972
1129.459705	44.655609	68.502977
1129.448521	39.404595	68.507982
1128.628273	42.930359	68.512986
1127.682927	44.654625	68.517991
1126.788670	41.669827	68.522996
1126.229464	53.521459	68.528001
1126.109359	46.182516	68.533006
1125.074881	56.244197	68.538010
1124.092014	55.214740	68.543015
1123.984743	48.313728	68.548020
1123.559269	50.146116	68.553025
1122.761512	49.465687	68.558030
1121.535324	56.809211	68.563034
1121.011551	55.386604	68.568039
1120.834094	51.084561	68.573044
1119.746108	54.684457	68.578049
1118.738508	48.320901	68.583054
1118.055324	48.030684	68.588058
1117.474499	51.690258	68.593063
1117.337560	33.838783	68.598068
1116.671343	45.123954	68.603073
1116.351572	39.652365	68.608078
1114.844757	40.530807	68.613082
1114.522741	31.013084	68.618087
1114.261943	39.937700	68.623092
1112.696935	42.673604	68.628097
1112.238425	33.112937	68.633102
1111.773300	36.061816	68.638106
1111.090326	40.474080	68.643111
1110.895491	48.855194	68.648116
1110.134668	49.474623	68.653121
1109.571750	45.308016	68.658126
1108.576239	55.525931	68.663130
1108.029747	48.223276	68.668135
1107.378940	45.543537	68.673140
1106.358022	53.904672	68.678145
1105.921727	45.502690	68.683150
1105.324090	54.211236	68.688154
1105.049434	49.372718	68.693159
1103.875853	49.919034	68.698164
1103.256436	56.234056	68.703169
1102.919632	47.423582	68.708174
1101.674876	50.241015	68.713178
1100.891544	49.635571	68.718183
1100.569724	42.975276	68.723188
1100.139088	49.629276	68.728193
1099.916116	43.520965	68.733198
1098.539068	48.056260	68.738202
1097.720251	41.612223	68.743207
1097.206363	43.982232	68.748212
1096.624738	50.846333	68.753217
1096.504722	39.065067	68.758222
1095.423836	50.827797	68.763226
1094.444423	46.744795	68.768231
1094.213070	50.241546	68.773236
1093.502995	51.125723	68.778241
1092.671995	46.416711	68.783246
1091.702455	49.762807	68.788250
1091.459191	50.195830	68.793255
1090.937206	53.067027	68.798260
1090.184945	51.436345	68.803265
1089.578178	44.266289	68.808270
1088.447695	48.029076	68.813274
1088.219981	50.996965	68.818279
1087.950308	40.524735	68.823284
1086.988668	53.068022	68.828289
1086.393945	43.197861	68.833294
1085.978958	45.460674	68.838298
1084.457596	45.895166	68.843303
1083.770678	39.715584	68.848308
1083.303542	51.443761	68.853313
1082.983965	48.900572	68.858318
1082.371175	44.694597	68.863322
1080.964044	50.975658	68.868327
1080.558846	43.399798	68.873332
1079.799611	53.663712	68.878337
1079.860186	48.379204	68.883342
1079.504900	46.541870	68.888346
1078.243618	46.146508	68.893351
1077.545181	43.803942	68.898356
1076.977554	54.423731	68.903361
1076.600873	41.541574	68.908366
1075.085751	50.064916	68.913370
1074.407087	43.250082	68.918375
1074.127039	38.601666	68.923380
1073.785296	47.318389	68.928385
1073.365487	45.144388	68.933390
1072.258454	47.731766	68.938394
1071.178893	45.968654	68.943399
1070.947325	47.986246	68.948404
1070.172302	46.851205	68.953409
1069.849637	41.580360	68.958414
1068.943021	36.768271	68.963418
1068.353280	46.171003	68.968423
1068.084324	41.501899	68.973428
1066.919713	52.525746	68.978433
1065.909058	35.844616	68.983438
1065.402516	44.027732	68.988442
1064.967681	47.891173	68.993447
1064.507959	42.269968	68.998452
1063.754470	58.861339	69.003457
1062.834981	46.912367	69.008462
1062.408556	47.981663	69.013466
1061.791647	51.394674	69.018471
1061.348991	46.634931	69.023476
1059.985560	57.814995	69.028481
1059.435699	47.212298	69.033486
1058.921588	50.131134	69.038490
1058.488249	42.446215	69.043495
1058.337284	40.352451	69.048500
1056.995883	49.245559	69.053505
1056.330513	44.776719	69.058510
1055.656057	44.764253	69.063514
1055.193666	50.685289	69.068519
1054.257501	39.249918	69.073524
1053.479719	49.266047	69.078529
1053.011815	45.543236	69.083534
1052.830392	46.143044	69.088538
1051.998262	52.827808	69.093543
1051.140010	50.043891	69.098548
1050.435679	49.386470	69.103553
1050.212107	39.342157	69.108558
1049.241087	51.585744	69.113562
1048.193962	45.031390	69.118567
1047.908223	47.224760	69.123572
1047.211317	46.517272	69.128577
1046.501605	41.624979	69.133582
1045.310990	49.476960	69.138586
1044.671381	47.661212	69.143591
1044.314744	40.555457	69.148596
1043.716569	52.339178	69.153601
1043.633751	38.287481	69.158606
1042.606036	48.335489	69.163610
1041.658102	51.135689	69.168615
1041.318218	54.671789	69.173620
1040.743348	46.063211	69.178625
1040.270412	40.097183	69.183630
1039.473183	51.754876	69.188634
1038.751909	56.368798	69.193639
1038.130774	49.579514	69.198644
1036.911909	60.607278	69.203649
1036.714588	52.419604	69.208654
1036.072443	56.989399	69.213658
1035.441010	57.750692	69.218663
1034.498871	51.843541	69.223668
1033.718204	62.670702	69.228673
1033.211628	54.937511	69.233678
1032.882929	53.352999	69.238682
1031.795325	54.926467	69.243687
1031.244892	47.223913	69.248692
1030.285683	51.703802	69.253697
1030.171472	44.878025	69.258702
1029.667364	52.671253	69.263706
1028.473714	52.299849	69.268711
1027.927523	48.744041	69.273716
1027.223294	53.076130	69.278721
1027.062271	48.891333	69.283726
1026.388228	52.193592	69.288730
1025.002163	54.724459	69.293735
1024.858840	51.041475	69.298740
1024.302670	53.935469	69.303745
1023.505630	48.062010	69.308750
1022.131024	53.141008	69.313754
1021.929232	47.414118	69.318759
1021.708430	46.900548	69.323764
1020.953857	53.684946	69.328769
1020.012041	43.713912	69.333774
1019.345978	48.632868	69.338778
1018.526310	51.015273	69.343783
1018.107725	52.826080	69.348788
1017.656970	57.444275	69.353793
1017.179733	53.147362	69.358798
1016.088111	47.336546	69.363802
1015.404349	56.132925	69.368807
1015.012093	53.449921	69.373812
1013.524234	55.194315	69.378817
1012.975816	44.550405	69.383822
1012.694945	43.820888	69.388826
1012.030243	60.387100	69.393831
1012.124879	51.252530	69.398836
1010.870699	57.157628	69.403841
1010.188935	48.687492	69.408846
1009.438580	51.656541	69.413850
1009.057759	51.537443	69.418855
1008.240912	49.737289	69.423860
1007.252747	54.256487	69.428865
1006.779206	53.724784	69.433870
1006.726364	53.263339	69.438874
1005.519011	57.192935	69.443879
1004.973106	50.237149	69.448884
1004.212692	54.213904	69.453889
1003.872324	52.412055	69.458894
1002.881154	43.530681	69.463898
1001.916033	54.779856	69.468903
1001.647509	54.619236	69.473908
1001.072120	46.427072	69.478913
1000.508889	44.646492	69.483918
999.402854	47.836141	69.488922
998.639507	45.751510	69.493927
998.212921	39.293990	69.498932
997.875019	50.536403	69.503937
996.964138	39.242118	69.508942
996.491064	43.643088	69.513946
995.383178	50.307087	69.518951
995.504531	48.468043	69.523956
994.149230	55.747005	69.528961
993.511454	50.890589	69.533966
992.983401	52.956939	69.538970
992.129724	53.103896	69.543975
992.215228	44.751382	69.548980
990.717401	51.417505	69.553985
989.998534	37.870728	69.558990
989.345020	48.198257	69.563994
988.875986	54.583987	69.568999
988.777225	46.746498	69.574004
987.578063	53.396640	69.579009
986.749415	59.115766	69.584014
986.379529	45.004095	69.589018
985.811916	53.056592	69.594023
985.647028	56.042877	69.599028
984.195060	58.497519	69.604033
983.507880	54.088939	69.609038
983.141714	52.352700	69.614042
982.591099	51.426409	69.619047
982.135640	42.243759	69.624052
981.086374	59.561876	69.629057
980.710860	54.001405	69.634062
980.060332	52.422379	69.639066
978.468174	56.369063	69.644071
977.883645	53.484847	69.649076
977.363564	60.938425	69.654081
977.019944	56.718031	69.659086
977.197668	55.086060	69.664090
976.066208	59.844117	69.669095
975.253054	56.464843	69.674100
974.462950	59.127988	69.679105
974.128634	44.543879	69.684110
973.526991	50.860823	69.689114
972.317237	60.105190	69.694119
971.915831	52.853604	69.699124
971.601144	60.045838	69.704129
970.383021	44.760266	69.709134
969.563507	52.930121	69.714138
969.015375	53.908412	69.719143
968.950827	49.485918	69.724148
967.929091	51.922569	69.729153
966.699763	54.285022	69.734158
966.314936	45.520069	69.739162
965.719968	52.323236	69.744167
965.577885	48.096008	69.749172
965.014415	51.238758	69.754177
963.921370	50.687372	69.759182
963.342458	50.554070	69.764186
962.389241	52.867856	69.769191
962.204884	46.300833	69.774196
961.052314	52.820567	69.779201
960.123779	57.473797	69.784206
959.832238	52.596988	69.789210
959.302705	58.960811	69.794215
959.340812	48.551592	69.799220
958.071384	57.802305	69.804225
957.494122	53.964450	69.809230
957.083731	56.048354	69.814234
955.912535	56.105500	69.819239
955.289552	45.855100	69.824244
954.560655	52.129220	69.829249
954.044138	57.417059	69.834254
953.662657	42.394182	69.839258
952.215201	52.169968	69.844263
951.907025	47.702665	69.849268
951.382751	61.035838	69.854273
950.727251	53.547145	69.859278
950.377080	50.666643	69.864282
949.358324	56.240988	69.869287
948.947094	49.084013	69.874292
948.077425	55.877282	69.879297
947.459933	57.836448	69.884302
946.850667	42.372001	69.889306
946.194696	52.382961	69.894311
945.855096	43.429467	69.899316
944.594917	50.639695	69.904321
943.560598	63.727605	69.909326
943.241013	53.619735	69.914330
942.743139	59.885482	69.919335
942.251908	54.846486	69.924340
941.733894	56.887595	69.929345
941.001191	54.764988	69.934350
940.256036	45.456561	69.939354
939.378514	51.822145	69.944359
939.047894	54.725994	69.949364
937.984338	53.233209	69.954369
937.061317	49.144454	69.959374
936.590543	49.746162	69.964378
936.313287	53.079915	69.969383
935.924447	43.079270	69.974388
934.960858	50.223379	69.979393
934.365468	45.461163	69.984398
933.825795	47.480487	69.989402
932.678382	41.580822	69.994407
931.825460	51.690936	69.999412
931.235000	47.544529	70.004417
930.890259	45.196181	70.009422
930.519661	41.700766	70.014426
929.745064	50.410687	70.019431
928.818721	48.955995	70.024436
927.948642	48.495298	70.029441
927.567938	52.260256	70.034446
927.584572	51.421901	70.039450
926.276957	56.310512	70.044455
925.805571	44.246144	70.049460
925.323081	51.490312	70.054465
924.249124	52.889764	70.059470
923.100521	42.087511	70.064474
922.185794	44.193333	70.069479
922.321898	40.380737	70.074484
922.251543	47.892054	70.079489
921.540365	47.431303	70.084494
920.527922	48.723194	70.089498
919.517072	48.232864	70.094503
919.058990	46.443454	70.099508
918.532450	47.266930	70.104513
917.291564	47.951778	70.109518
916.758172	51.100789	70.114522
916.070427	56.740739	70.119527
915.745101	46.122858	70.124532
915.330340	52.533074	70.129537
914.263824	53.321061	70.134542
913.820449	49.124442	70.139546
912.852756	49.071949	70.144551
912.785788	48.977033	70.149556
911.592531	43.947273	70.154561
910.709845	49.727056	70.159566
910.541905	52.508823	70.164570
909.794596	59.118625	70.169575
909.863594	45.310869	70.174580
909.264473	53.187041	70.179585
908.436087	53.631200	70.184590
907.841631	55.069465	70.189594
906.811774	60.568321	70.194599
906.166061	42.914557	70.199604
905.116566	49.033128	70.204609
904.449830	48.358726	70.209614
904.100066	51.861717	70.214618
902.684306	52.847218	70.219623
902.556734	45.342334	70.224628
901.990452	48.789898	70.229633
901.369585	58.033608	70.234638
900.771163	43.196662	70.239642
899.679626	52.291349	70.244647
899.321067	51.151583	70.249652
898.744151	58.325630	70.254657
897.633691	50.838402	70.259662
897.054974	53.308652	70.264666
896.303303	59.195325	70.269671
896.053937	46.442765	70.274676
895.367280	46.867526	70.279681
894.821277	46.303223	70.284686
894.021997	48.054788	70.289690
893.189686	47.761558	70.294695
892.749123	51.812016	70.299700
891.784923	49.171178	70.304705
890.766905	54.277067	70.309710
890.690696	48.353588	70.314714
890.137076	56.257216	70.319719
889.752026	48.156219	70.324724
888.587595	51.848797	70.329729
887.571235	55.098337	70.334734
887.089336	57.925344	70.339738
886.613115	61.456351	70.344743
886.310203	52.336175	70.349748
885.250155	44.902435	70.354753
884.613867	50.333925	70.359758
883.970597	48.364261	70.364762
883.687843	53.985490	70.369767
883.113462	54.936436	70.374772
881.902427	54.284016	70.379777
881.284954	59.761401	70.384782
881.093320	51.982859	70.389786
879.658578	46.116335	70.394791
878.971091	47.301328	70.399796
878.646744	43.398013	70.404801
878.209474	46.249455	70.409806
878.023422	49.246995	70.414810
876.594277	52.932825	70.419815
876.121560	49.346438	70.424820
875.593752	52.336872	70.429825
874.301944	56.341469	70.434830
873.776051	45.899025	70.439834
873.100610	57.401751	70.444839
872.711393	50.725418	70.449844
872.458388	50.374684	70.454849
871.933985	49.467900	70.459854
870.852122	47.347274	70.464858
869.924974	52.670520	70.469863
869.343590	56.257690	70.474868
869.362702	49.793912	70.479873
868.097098	52.010795	70.484878
867.536844	50.258159	70.489882
866.971152	57.988669	70.494887
866.241925	53.678284	70.499892
865.074721	52.569461	70.504897
864.514839	51.512206	70.509902
864.191242	45.905653	70.514906
863.812403	52.687051	70.519911
863.340836	48.666819	70.524916
862.584074	50.140389	70.529921
861.631149	51.197325	70.534926
861.249168	41.668698	70.539930
860.165600	49.699255	70.544935
859.499706	46.837485	70.549940
858.984117	41.950626	70.554945
858.429888	47.867378	70.559950
857.951587	50.356345	70.564954
856.850936	47.726203	70.569959
856.422678	48.188693	70.574964
855.862172	55.569869	70.579969
854.723522	54.114304	70.584974
854.250531	46.718024	70.589978
853.612721	61.491695	70.594983
853.532217	46.607020	70.599988
852.267005	53.409656	70.604993
851.219254	60.600308	70.609998
850.923610	49.889406	70.615002
850.640140	46.775953	70.620007
849.670243	51.971968	70.625012
848.981953	45.297516	70.630017
848.156373	45.135694	70.635022
847.852420	44.545489	70.640026
846.987739	55.896989	70.645031
845.763414	46.718487	70.650036
845.066755	44.694254	70.655041
844.568960	50.750261	70.660046
844.431531	52.063752	70.665050
844.004995	46.875713	70.670055
843.870845	45.701812	70.675060
842.969138	48.710766	70.680065
842.132704	47.689653	70.685070
841.121001	40.059007	70.690074
839.765740	43.353046	70.695079
839.493224	40.416050	70.700084
839.044025	46.029079	70.705089
838.306935	48.276966	70.710094
838.180615	42.689480	70.715098
837.252674	45.204291	70.720103
836.477721	46.557760	70.725108
835.857578	49.564475	70.730113
835.239836	53.278865	70.735118
834.394761	51.781310	70.740122
833.647247	54.981768	70.745127
833.071698	47.477238	70.750132
833.020203	41.977190	70.755137
831.499398	48.235465	70.760142
830.963644	39.964510	70.765146
830.050726	48.306959	70.770151
830.047930	43.415751	70.775156
829.625537	40.696580	70.780161
828.512700	46.333248	70.785166
827.918322	37.633231	70.790170
826.806261	44.594423	70.795175
826.855471	42.735319	70.800180
826.206940	41.085056	70.805185
825.063832	43.034876	70.810190
824.647908	41.696095	70.815194
823.922529	44.293784	70.820199
823.271122	46.403456	70.825204
822.263047	49.602814	70.830209
821.619026	46.731265	70.835214
821.361703	48.726166	70.840218
821.064808	51.787085	70.845223
820.237686	46.156614	70.850228
819.271391	50.555699	70.855233
818.418021	48.136947	70.860238
818.339508	45.768316	70.865242
817.029534	48.351834	70.870247
816.325316	46.221579	70.875252
815.759968	50.026980	70.880257
815.433879	58.287063	70.885262
815.055977	49.593584	70.890266
813.638832	55.917372	70.895271
812.861253	51.531124	70.900276
812.852748	44.133456	70.905281
812.189591	51.726521	70.910286
811.903091	45.267243	70.915290
810.721829	53.136752	70.920295
810.132692	50.250160	70.925300
809.625120	53.951749	70.930305
808.617991	54.629400	70.935310
808.157962	45.190480	70.940314
807.460439	49.721826	70.945319
806.876015	47.153032	70.950324
806.241209	40.966825	70.955329
804.901863	50.416384	70.960334
804.980117	41.729144	70.965338
804.346953	40.505374	70.970343
802.932919	47.240256	70.975348
802.311086	47.457602	70.980353
801.366675	46.160378	70.985358
800.940203	46.655708	70.990362
800.349706	51.471218	70.995367
799.741687	44.411842	71.000372
799.395277	50.047938	71.005377
798.992254	45.395487	71.010382
799.172242	46.809837	71.015386
797.798751	54.795109	71.020391
796.715096	55.648951	71.025396
796.328394	41.153663	71.030401
795.139893	55.234403	71.035406
794.515282	46.078733	71.040410
793.816236	49.922769	71.045415
793.330871	49.197446	71.050420
793.211918	46.765868	71.055425
792.434235	59.447104	71.060430
791.483139	49.168570	71.065434
790.811861	49.389060	71.070439
790.328219	47.308854	71.075444
790.159640	48.799195	71.080449
788.986604	55.640801	71.085454
788.288526	40.707804	71.090458
787.768426	46.779984	71.095463
786.729546	48.705344	71.100468
785.940974	43.854077	71.105473
784.964201	49.617335	71.110478
784.600514	43.684442	71.115482
784.180357	50.183838	71.120487
783.761093	46.035450	71.125492
783.416972	43.926727	71.130497
782.155665	45.780265	71.135502
781.924660	38.377024	71.140506
781.187756	42.044160	71.145511
780.288129	46.856846	71.150516
779.679647	46.830797	71.155521
778.829515	52.272698	71.160526
778.723857	45.828791	71.165530
777.747076	50.442449	71.170535
776.978015	43.374026	71.175540
776.491247	38.667105	71.180545
775.579598	48.728254	71.185550
775.300916	42.934795	71.190554
774.475409	40.230926	71.195559
773.312659	50.280014	71.200564
773.427121	45.579876	71.205569
772.426565	45.993143	71.210574
771.558016	40.985880	71.215578
770.817432	40.397389	71.220583
770.391679	42.425416	71.225588
770.282704	47.213155	71.230593
768.933311	51.343663	71.235598
768.516341	45.649491	71.240602
767.840787	50.658321	71.245607
767.386336	54.665275	71.250612
766.687769	45.598660	71.255617
765.422971	56.070856	71.260622
765.181607	49.533436	71.265626
764.517869	46.579887	71.270631
763.715781	55.584384	71.275636
763.098571	51.543207	71.280641
762.259494	55.879481	71.285646
762.081415	39.594255	71.290650
761.390854	50.657849	71.295655
760.130601	50.599954	71.300660
759.578773	49.137741	71.305665
759.180832	57.410841	71.310670
758.952498	50.975427	71.315674
758.192808	52.175101	71.320679
757.013465	47.915917	71.325684
756.344201	50.296532	71.330689
755.770148	54.648960	71.335694
755.824909	49.299157	71.340698
754.489154	51.568264	71.345703
753.886990	52.055305	71.350708
753.758830	40.079853	71.355713
752.410679	49.388909	71.360718
751.696759	43.872907	71.365722
751.126936	47.421988	71.370727
750.828612	54.734627	71.375732
750.462838	45.905194	71.380737
749.133975	47.104027	71.385742
748.518768	43.224965	71.390746
747.920069	50.273189	71.395751
747.190223	49.716111	71.400756
746.450814	46.306258	71.405761
745.538731	46.792181	71.410766
745.032609	34.405402	71.415770
744.641461	41.122531	71.420775
744.260401	43.706421	71.425780
743.887931	38.233832	71.430785
742.865224	47.133104	71.435790
742.319502	42.721008	71.440794
741.414053	46.206832	71.445799
740.376779	48.086222	71.450804
739.940950	37.643681	71.455809
739.392603	43.420741	71.460814
739.023722	46.780134	71.465818
737.808513	45.073463	71.470823
737.080610	47.848197	71.475828
736.817185	39.500794	71.480833
736.197183	44.210624	71.485838
735.868813	45.675946	71.490842
734.424923	49.764746	71.495847
733.923588	51.252877	71.500852
733.487227	47.842085	71.505857
732.969436	45.152315	71.510862
732.114884	40.997552	71.515866
731.398448	46.268365	71.520871
730.698553	45.687600	71.525876
730.710912	48.814405	71.530881
729.345300	48.989344	71.535886
728.338516	46.314354	71.540890
728.034345	45.214841	71.545895
727.563576	49.363169	71.550900
726.986994	46.578681	71.555905
725.764570	46.672476	71.560910
725.198511	47.158506	71.565914
724.845237	45.513298	71.570919
724.256860	51.943291	71.575924
724.119217	45.089743	71.580929
722.724162	50.948008	71.585934
721.881378	43.927615	71.590938
721.781148	41.716990	71.595943
720.777143	39.871042	71.600948
719.878218	41.119705	71.605953
719.045200	45.346213	71.610958
718.758230	49.807478	71.615962
718.254748	52.775143	71.620967
718.003137	51.981077	71.625972
717.252596	39.040283	71.630977
716.328762	49.571745	71.635982
715.801371	37.366557	71.640986
714.925721	47.377833	71.645991
714.198044	47.515860	71.650996
713.447250	37.468832	71.656001
713.032451	47.324727	71.661006
712.850099	40.093523	71.666010
711.970410	38.910609	71.671015
711.085216	44.217759	71.676020
710.603210	36.986962	71.681025
709.231235	41.529525	71.686030
708.169121	45.488162	71.691034
707.895469	40.334160	71.696039
707.637541	42.326012	71.701044
707.370518	35.182411	71.706049
706.641386	43.779480	71.711054
705.854839	39.035155	71.716058
705.234457	43.290886	71.721063
704.434462	40.352745	71.726068
703.572508	32.200006	71.731073
702.426141	40.005645	71.736078
702.069706	37.663930	71.741082
701.614985	30.638530	71.746087
701.516933	46.829093	71.751092
701.098164	35.502328	71.756097
699.804871	45.463414	71.761102
699.281330	43.626126	71.766106
698.600128	37.265993	71.771111
697.121563	44.936876	71.776116
696.974274	37.258545	71.781121
696.522467	45.663223	71.786126
696.228728	44.347586	71.791130
695.090993	49.076788	71.796135
694.042797	45.736622	71.801140
694.046961	37.740860	71.806145
693.097303	47.375994	71.811150
692.749202	41.114209	71.816154
691.717559	43.068415	71.821159
690.818781	43.143807	71.826164
690.725227	37.046495	71.831169
690.090916	40.834513	71.836174
688.981906	36.179391	71.841178
688.378729	42.351544	71.846183
687.937681	40.070613	71.851188
687.659741	37.758978	71.856193
686.587291	43.386114	71.861198
685.572195	49.445668	71.866202
685.048836	36.266865	71.871207
684.403472	41.359212	71.876212
684.234404	41.308946	71.881217
683.128434	48.220336	71.886222
682.452360	49.695301	71.891226
682.029821	50.983236	71.896231
681.304251	52.527585	71.901236
680.699171	46.152179	71.906241
679.651883	43.460006	71.911246
679.166326	39.921444	71.916250
678.979137	43.185677	71.921255
677.755221	52.998535	71.926260
677.193682	48.174232	71.931265
676.302876	40.029249	71.936270
676.187593	42.720635	71.941274
675.820563	49.722517	71.946279
674.524538	49.320276	71.951284
673.915567	43.312925	71.956289
673.619440	38.258703	71.961294
672.658132	41.608363	71.966298
671.871872	45.393775	71.971303
671.322596	51.748164	71.976308
670.639857	44.833193	71.981313
670.413359	45.132697	71.986318
669.543552	35.579305	71.991322
668.852095	43.124858	71.996327
668.002011	42.094941	72.001332
667.503885	41.564066	72.006337
666.403081	43.948767	72.011342
665.811162	38.783954	72.016346
665.535070	39.315284	72.021351
664.917981	43.810197	72.026356
664.550402	31.876050	72.031361
663.563648	37.962632	72.036366
662.890338	37.253074	72.041370
661.801444	39.604340	72.046375
660.592374	50.682713	72.051380
660.208755	43.254909	72.056385
659.825143	46.343842	72.061390
659.762614	51.475847	72.066394
659.517549	45.878904	72.071399
658.473687	49.388375	72.076404
657.444603	46.616041	72.081409
657.113548	46.241489	72.086414
656.081105	39.287598	72.091418
655.245964	38.646392	72.096423
654.317715	42.870737	72.101428
654.172416	33.487405	72.106433
653.577372	42.425829	72.111438
653.310275	36.174808	72.116442
652.372890	42.499540	72.121447
651.286845	43.755948	72.126452
651.203989	42.542353	72.131457
650.391468	42.963569	72.136462
649.258768	43.114076	72.141466
648.758298	44.999478	72.146471
648.066340	45.412534	72.151476
647.882836	35.727779	72.156481
646.633643	45.872676	72.161486
645.813236	44.043253	72.166490
645.753624	36.715244	72.171495
644.991701	41.006144	72.176500
644.822999	36.761114	72.181505
643.276779	48.757358	72.186510
642.844842	38.464036	72.191514
642.550872	31.482436	72.196519
641.971386	39.831755	72.201524
640.678103	38.235339	72.206529
639.955831	45.637573	72.211534
639.391086	41.572310	72.216538
639.471549	33.742600	72.221543
638.264659	48.624253	72.226548
637.735811	39.707281	72.231553
637.048202	39.186088	72.236558
636.352073	43.532745	72.241562
635.781050	34.144676	72.246567
634.590801	36.862179	72.251572
634.238737	36.213432	72.256577
633.820931	36.745257	72.261582
633.152121	39.961615	72.266586
632.837735	42.897600	72.271591
631.788671	44.690601	72.276596
631.543146	35.534545	72.281601
630.360192	40.873370	72.286606
629.371475	47.829184	72.291610
628.670885	36.708172	72.296615
628.217678	45.094156	72.301620
628.104375	33.702995	72.306625
627.160497	41.459068	72.311630
626.152457	45.536857	72.316634
625.826777	40.230306	72.321639
625.120144	45.102188	72.326644
624.946033	33.613480	72.331649
623.737706	41.580405	72.336654
622.938329	42.759630	72.341658
622.651877	44.262444	72.346663
621.497653	55.705839	72.351668
621.016226	43.129080	72.356673
620.078905	47.831124	72.361678
619.453318	43.846519	72.366682
619.478321	42.655171	72.371687
618.739802	47.606251	72.376692
618.400938	42.494189	72.381697
617.086552	42.260484	72.386702
616.530905	38.791446	72.391706
615.821302	36.474454	72.396711
614.715797	45.989351	72.401716
614.004988	46.134182	72.406721
613.722304	45.668353	72.411726
613.301318	44.303607	72.416730
613.011957	37.245583	72.421735
612.090613	46.915654	72.426740
611.547074	36.890853	72.431745
610.886212	38.752921	72.436750
609.929762	39.739547	72.441754
609.012309	48.495942	72.446759
608.119459	45.979477	72.451764
607.957697	37.478715	72.456769
607.594343	40.422501	72.461774
606.959967	33.129270	72.466778
606.125231	40.992545	72.471783
605.614895	43.210687	72.476788
604.501693	41.610840	72.481793
603.586451	39.645149	72.486798
602.936893	41.767194	72.491802
602.569472	36.039941	72.496807
602.369571	37.678782	72.501812
601.805596	32.683005	72.506817
600.408179	37.808416	72.511822
599.795753	44.344759	72.516826
599.635088	39.147549	72.521831
598.688027	43.357562	72.526836
597.810442	45.045994	72.531841
597.026949	39.098004	72.536846
596.345174	38.713089	72.541850
596.572579	38.435678	72.546855
595.608511	38.737546	72.551860
594.549377	41.366376	72.556865
594.245864	36.625583	72.561870
593.690297	41.221097	72.566874
593.010295	39.413485	72.571879
591.566683	46.589998	72.576884
591.181641	39.140362	72.581889
590.922132	32.719410	72.586894
590.242183	37.658011	72.591898
589.497670	38.315997	72.596903
588.436470	37.338658	72.601908
588.128685	34.758978	72.606913
587.563698	41.907510	72.611918
586.648942	35.663464	72.616922
586.095875	37.755951	72.621927
584.801786	40.037430	72.626932
584.878822	39.209956	72.631937
584.216235	45.736946	72.636942
583.693137	49.467851	72.641946
583.130080	39.485590	72.646951
582.460256	48.325553	72.651956
581.911894	41.458597	72.656961
580.652071	45.100266	72.661966
580.089007	46.286020	72.666970
579.758235	42.054195	72.671975
579.114732	44.455980	72.676980
578.158947	41.676739	72.681985
577.383153	43.418350	72.686990
576.769310	49.781459	72.691994
576.605755	44.056430	72.696999
575.573360	51.564847	72.702004
574.830623	44.082300	72.707009
574.148711	45.928807	72.712014
573.525881	44.892687	72.717018
573.324875	42.701278	72.722023
572.059750	51.401099	72.727028
571.364951	42.474309	72.732033
571.043349	36.755534	72.737038
570.494651	36.037192	72.742042
570.048143	37.655391	72.747047
568.685989	47.386227	72.752052
568.440977	39.485358	72.757057
567.908627	41.237080	72.762062
566.649054	45.313956	72.767066
566.239864	36.814765	72.772071
565.665601	45.778280	72.777076
565.137690	38.964843	72.782081
564.315997	44.156265	72.787086
563.231792	44.300663	72.792090
562.815558	40.303230	72.797095
562.233619	46.068323	72.802100
562.139072	40.378036	72.807105
561.245090	43.135114	72.812110
560.317113	46.055304	72.817114
559.909258	36.180796	72.822119
559.343878	43.480783	72.827124
558.506992	40.190601	72.832129
557.711939	34.157737	72.837134
556.814355	40.561312	72.842138
556.576914	31.121712	72.847143
555.268692	38.533717	72.852148
554.901291	31.115976	72.857153
554.493004	41.101726	72.862158
553.978878	34.503718	72.867162
553.726550	34.635459	72.872167
552.261016	35.438270	72.877172
551.715912	33.719570	72.882177
551.089019	40.231416	72.887182
550.459095	40.204108	72.892186
549.811883	36.677134	72.897191
549.048980	43.259532	72.902196
548.663101	40.354828	72.907201
547.929631	36.377971	72.912206
546.953908	39.392502	72.917210
546.363459	35.881719	72.922215
545.459510	43.379143	72.927220
544.981433	41.604034	72.932225
544.681778	36.755402	72.937230
544.078965	45.805469	72.942234
543.185891	36.848777	72.947239
542.265529	48.212361	72.952244
542.018594	43.298559	72.957249
541.559910	42.472843	72.962254
540.180399	48.617305	72.967258
539.776026	41.602844	72.972263
538.903857	46.174687	72.977268
538.555899	44.628011	72.982273
538.032895	46.004511	72.987278
537.455075	48.782198	72.992282
536.746240	37.263566	72.997287
536.304661	37.767655	73.002292
535.420020	41.474158	73.007297
534.558130	42.267553	73.012302
534.145019	41.093957	73.017306
533.776628	38.356782	73.022311
532.175518	46.332700	73.027316
531.532580	38.936776	73.032321
531.331500	35.714054	73.037326
530.842499	41.905894	73.042330
530.682082	29.654932	73.047335
529.362793	37.508682	73.052340
528.597559	36.659263	73.057345
528.326493	39.272966	73.062350
527.356513	46.787223	73.067354
526.487226	28.554252	73.072359
525.827522	33.614220	73.077364
525.235160	35.615207	73.082369
524.811138	35.551951	73.087374
523.954353	40.465122	73.092378
523.288381	36.482250	73.097383
522.539446	46.247882	73.102388
522.291926	44.130119	73.107393
521.711085	36.121911	73.112398
520.510238	34.129211	73.117402
520.188074	28.828432	73.122407
519.458636	36.294905	73.127412
518.638920	38.287958	73.132417
517.842403	30.497039	73.137422
516.980707	40.443058	73.142426
516.815852	39.270917	73.147431
516.374718	37.341696	73.152436
515.967623	35.178394	73.157441
515.029237	35.160811	73.162446
514.044441	41.144630	73.167450
513.701663	33.700897	73.172455
512.748111	32.562940	73.177460
511.835699	41.466787	73.182465
511.405564	36.504907	73.187470
510.838496	42.952037	73.192474
510.735802	39.765682	73.197479
509.457675	48.630026	73.202484
508.839699	33.883097	73.207489
508.162243	39.991420	73.212494
507.468577	44.069632	73.217498
506.726845	31.919168	73.222503
505.716995	36.989192	73.227508
505.386692	38.508464	73.232513
504.836449	38.673478	73.237518
504.003771	42.502600	73.242522
504.319380	33.282408	73.247527
502.876433	41.485455	73.252532
502.189433	33.648708	73.257537
501.920705	35.271712	73.262542
500.609812	37.008706	73.267546
499.980459	30.902159	73.272551
499.394498	41.928623	73.277556
498.714080	37.752518	73.282561
498.594492	29.872687	73.287566
497.823626	36.582519	73.292570
497.200526	37.101341	73.297575
496.326694	38.420201	73.302580
495.886371	42.784483	73.307585
494.846660	41.272327	73.312590
493.780941	44.545645	73.317594
493.430299	33.635444	73.322599
493.353674	37.352002	73.327604
492.733859	39.109788	73.332609
492.034006	39.074712	73.337614
490.709940	47.309291	73.342618
490.528908	42.250956	73.347623
490.000248	43.819179	73.352628
489.356538	33.567529	73.357633
488.886804	41.713305	73.362638
487.782791	46.186481	73.367642
487.154022	35.576058	73.372647
486.156724	40.399662	73.377652
485.618276	43.836560	73.382657
485.359880	35.420600	73.387662
484.014476	40.835830	73.392666
483.555687	31.188658	73.397671
483.074136	37.480240	73.402676
482.437316	35.391391	73.407681
482.199187	32.761206	73.412686
480.808750	35.343515	73.417690
480.333268	23.179036	73.422695
480.118643	28.228026	73.427700
479.256368	36.318068	73.432705
478.475052	30.581092	73.437710
477.262579	41.835109	73.442714
477.316755	32.268638	73.447719
477.016733	33.150730	73.452724
475.868806	37.523672	73.457729
475.136530	36.042968	73.462734
474.120244	41.943509	73.467738
473.876854	29.994361	73.472743
473.195935	31.717732	73.477748
472.210219	34.604571	73.482753
471.900407	34.877942	73.487758
471.307636	42.800472	73.492762
470.877380	31.414107	73.497767
469.899930	31.077913	73.502772
469.004990	30.635533	73.507777
468.510765	21.583799	73.512782
467.773911	27.717358	73.517786
467.592215	30.512367	73.522791
466.675758	31.161514	73.527796
465.707865	38.030480	73.532801
465.444693	32.581538	73.537806
464.638311	35.266343	73.542810
463.658763	27.047293	73.547815
463.050231	37.262069	73.552820
462.379413	42.311208	73.557825
461.986267	36.570737	73.562830
461.554000	41.261747	73.567834
460.639376	36.104258	73.572839
459.942911	25.621333	73.577844
459.360113	40.151286	73.582849
459.096650	32.070455	73.587854
457.823542	35.296403	73.592858
457.446942	23.054676	73.597863
456.598959	35.054867	73.602868
456.007626	37.188169	73.607873
455.045350	33.187875	73.612878
454.273838	42.484028	73.617882
453.945155	32.462897	73.622887
453.723841	26.688745	73.627892
453.161364	34.578061	73.632897
452.065919	24.034132	73.637902
451.387013	37.092329	73.642906
450.879480	29.135545	73.647911
450.078481	32.450277	73.652916
449.035104	32.077287	73.657921
448.607290	30.082880	73.662926
448.284329	23.777724	73.667930
447.980550	33.540242	73.672935
446.908843	30.986109	73.677940
445.897593	36.993087	73.682945
445.691437	35.472718	73.687950
444.776040	40.921954	73.692954
443.948027	32.674034	73.697959
443.128795	35.237890	73.702964
442.597272	36.476995	73.707969
442.558753	38.137440	73.712974
441.617654	43.614427	73.717978
440.737538	32.739720	73.722983
440.075932	25.851434	73.727988
439.595194	33.615764	73.732993
439.380465	33.353594	73.737998
438.057969	37.509939	73.743002
437.431308	35.802684	73.748007
436.934993	33.183681	73.753012
436.003146	35.208819	73.758017
435.218017	36.863649	73.763022
434.109589	34.466760	73.768026
434.100796	30.653593	73.773031
433.753485	28.532822	73.778036
433.201845	30.017983	73.783041
432.621168	30.377097	73.788046
431.365804	38.001508	73.793050
430.985121	35.149616	73.798055
430.810845	28.013369	73.803060
429.380044	33.205687	73.808065
429.240718	21.949603	73.813070
428.461320	40.942123	73.818074
427.669589	30.414463	73.823079
426.818994	33.051130	73.828084
426.038378	37.220485	73.833089
425.668939	30.952698	73.838094
425.165827	38.698520	73.843098
424.308456	28.755333	73.848103
423.282042	25.850219	73.853108
422.690106	27.262956	73.858113
422.786557	29.641485	73.863118
421.587509	31.191963	73.868122
420.544203	26.715742	73.873127
420.050598	28.737285	73.878132
419.538498	30.971510	73.883137
419.483002	27.459100	73.888142
418.792620	24.153513	73.893146
417.456818	29.612973	73.898151
416.866970	32.225440	73.903156
416.529751	38.367875	73.908161
416.174416	24.987363	73.913166
414.656656	34.847132	73.918170
414.018794	32.351615	73.923175
413.843661	32.109947	73.928180
413.135171	32.180348	73.933185
413.028374	27.908138	73.938190
411.793758	35.888795	73.943194
411.214030	25.679024	73.948199
410.589431	29.069736	73.953204
409.279970	38.620352	73.958209
409.015210	27.710685	73.963214
408.163526	32.175219	73.968218
407.815480	36.832313	73.973223
407.698447	34.479308	73.978228
406.336027	38.407065	73.983233
406.054195	31.742122	73.988238
405.124678	34.883382	73.993242
404.823224	29.524130	73.998247
403.727655	31.504405	74.003252
402.951714	30.644118	74.008257
402.682103	27.104328	74.013262
401.968652	33.543258	74.018266
401.052177	24.383788	74.023271
400.741567	23.021995	74.028276
400.023079	34.635709	74.033281
399.290673	25.938916	74.038286
398.007729	29.466080	74.043290
397.686758	30.217478	74.048295
397.659453	29.737788	74.053300
396.863039	34.612988	74.058305
396.237755	26.782218	74.063310
395.113178	31.414822	74.068314
394.805411	25.148256	74.073319
394.047598	33.978609	74.078324
392.742984	32.718448	74.083329
392.178816	25.010405	74.088334
391.858805	32.362773	74.093338
391.369503	29.258540	74.098343
391.120527	34.037042	74.103348
389.820361	29.787848	74.108353
389.390816	28.847133	74.113358
388.648766	28.669000	74.118362
388.112367	37.000449	74.123367
387.230449	35.564120	74.128372
386.371491	36.426484	74.133377
386.138777	36.353265	74.138382
385.525479	37.007747	74.143386
384.607784	31.101729	74.148391
384.036850	33.698574	74.153396
383.273922	32.448289	74.158401
383.077507	29.291075	74.163406
382.111218	24.741098	74.168410
381.018570	32.459446	74.173415
380.566833	26.256826	74.178420
379.916415	34.995951	74.183425
380.003909	33.597527	74.188430
378.646326	35.561220	74.193434
377.609626	33.935096	74.198439
377.310798	35.193901	74.203444
376.752642	38.867347	74.208449
376.189497	32.182586	74.213454
375.117872	37.161575	74.218458
374.281939	31.674617	74.223463
374.272843	35.124944	74.228468
373.665556	34.786568	74.233473
373.468097	38.793618	74.238478
372.180207	34.118275	74.243482
371.545896	30.253410	74.248487
371.405712	30.278988	74.253492
370.034317	40.323616	74.258497
369.669880	25.476424	74.263502
369.356177	36.942057	74.268506
367.963752	41.811326	74.273511
367.117135	29.102053	74.278516
366.459469	38.416348	74.283521
366.072344	36.953213	74.288526
365.623420	36.449252	74.293530
364.830480	37.580223	74.298535
364.264092	33.414375	74.303540
363.360712	41.872124	74.308545
363.112965	34.362817	74.313550
362.229412	41.210490	74.318554
361.337834	39.222200	74.323559
360.723495	34.210863	74.328564
360.396666	37.793830	74.333569
359.894246	29.407326	74.338574
358.797259	39.028181	74.343578
357.778631	45.465300	74.348583
357.573990	31.351153	74.353588
356.873068	45.113046	74.358593
356.640972	28.117454	74.363598
355.588564	35.720589	74.368602
354.956256	30.790967	74.373607
354.719509	39.382170	74.378612
353.704395	41.160411	74.383617
353.246116	34.506251	74.388622
352.513478	39.517957	74.393626
351.737835	36.798411	74.398631
350.722425	35.351832	74.403636
349.896757	44.194592	74.408641
349.502762	45.179985	74.413646
349.215670	38.635737	74.418650
348.812581	42.284476	74.423655
347.979181	30.735318	74.428660
346.983340	40.453598	74.433665
346.841152	36.759465	74.438670
345.374339	39.784528	74.443674
344.512579	35.408716	74.448679
344.491211	37.687747	74.453684
343.900106	39.597111	74.458689
343.325660	36.036525	74.463694
342.064019	43.297701	74.468698
341.394245	48.285201	74.473703
341.290236	31.228195	74.478708
340.816663	51.517136	74.483713
339.994796	31.218783	74.488718
339.007417	34.380326	74.493722
338.192562	45.479561	74.498727
338.017423	36.129420	74.503732
336.995911	40.378194	74.508737
336.116582	35.524216	74.513742
335.524352	40.428393	74.518746
334.858976	32.622955	74.523751
334.746688	34.295157	74.528756
333.973476	31.753426	74.533761
333.389201	29.560051	74.538766
332.388870	30.183192	74.543770
332.043215	34.597060	74.548775
331.407276	34.102412	74.553780
330.072481	36.247003	74.558785
329.804634	33.962195	74.563790
329.498698	37.502410	74.568794
328.814870	32.992591	74.573799
327.736817	26.657996	74.578804
326.838468	34.654478	74.583809
326.544561	28.626988	74.588814
326.261379	33.529216	74.593818
325.148560	34.193942	74.598823
324.649844	33.366766	74.603828
323.866454	40.155908	74.608833
323.561939	29.211595	74.613838
322.825099	40.832982	74.618842
321.895322	38.439211	74.623847
320.963546	40.317722	74.628852
320.618335	37.926974	74.633857
320.250418	36.588518	74.638862
319.290262	35.779696	74.643866
318.494980	39.634451	74.648871
317.915192	38.156300	74.653876
317.325631	37.900268	74.658881
316.371942	33.501274	74.663886
315.673404	32.852605	74.668890
315.078451	35.839645	74.673895
314.848268	30.883789	74.678900
314.425428	34.966186	74.683905
313.324013	29.617761	74.688910
312.531671	38.951954	74.693914
311.636978	35.385651	74.698919
311.709319	36.500147	74.703924
310.860969	39.306805	74.708929
309.918685	31.283739	74.713934
309.328324	33.528881	74.718938
308.719546	31.568076	74.723943
308.441333	28.996342	74.728948
307.208047	28.371408	74.733953
306.974237	28.930729	74.738958
306.484859	36.289599	74.743962
305.556467	39.377098	74.748967
304.720268	33.712013	74.753972
304.021719	36.876417	74.758977
303.654920	35.146702	74.763982
302.716166	36.673095	74.768986
301.925529	44.753346	74.773991
301.796533	29.789795	74.778996
300.789420	34.867339	74.784001
299.945275	28.935443	74.789006
299.235442	24.532284	74.794010
298.516132	25.848657	74.799015
298.197610	32.510088	74.804020
297.778136	40.217363	74.809025
296.914486	36.695003	74.814030
296.030733	36.470099	74.819034
295.500722	41.231903	74.824039
295.389786	35.965303	74.829044
294.240807	41.166389	74.834049
293.271927	29.156307	74.839054
292.859620	33.437300	74.844058
292.074851	32.712496	74.849063
291.786108	28.858805	74.854068
290.023983	35.630496	74.859073
290.084598	35.969424	74.864078
289.623928	33.267503	74.869082
289.083569	33.986076	74.874087
288.613116	36.232610	74.879092
287.603009	37.349336	74.884097
286.910212	29.461554	74.889102
286.236584	27.115279	74.894106
285.547815	37.834877	74.899111
284.841597	26.834759	74.904116
284.252597	37.062214	74.909121
283.805522	33.550728	74.914126
283.431408	40.519069	74.919130
282.108157	43.179086	74.924135
281.763850	34.630205	74.929140
281.157303	34.417890	74.934145
280.337553	31.227584	74.939150
279.421606	28.080999	74.944154
278.559505	33.504441	74.949159
278.500613	33.378294	74.954164
277.831609	32.732813	74.959169
277.259293	28.842325	74.964174
276.624942	33.740609	74.969178
275.670362	39.771729	74.974183
275.311782	35.586973	74.979188
274.328424	39.544260	74.984193
273.520431	32.187354	74.989198
273.017493	35.577628	74.994202
272.244165	39.920905	74.999207
272.216026	27.778222	75.004212
270.837751	43.589323	75.009217
270.292715	44.098912	75.014222
269.859601	34.323129	75.019226
269.276653	40.418013	75.024231
268.588624	37.798070	75.029236
267.533435	37.064342	75.034241
267.104379	34.737431	75.039246
266.967281	30.869032	75.044250
265.619152	35.657173	75.049255
265.091951	28.932025	75.054260
264.169036	37.735110	75.059265
263.944729	28.947911	75.064270
263.009544	32.891213	75.069274
261.959347	39.478474	75.074279
261.519244	31.689191	75.079284
261.282138	38.597846	75.084289
260.941537	33.158127	75.089294
260.152419	39.304802	75.094298
259.025721	38.364857	75.099303
258.766781	25.268645	75.104308
257.892410	37.135891	75.109313
256.867545	35.031694	75.114318
256.287936	32.449666	75.119322
255.803231	36.707513	75.124327
255.630238	35.386880	75.129332
254.481366	40.936471	75.134337
253.787292	38.948277	75.139342
253.082009	40.366506	75.144346
252.561975	32.733470	75.149351
252.771872	27.866741	75.154356
251.440250	37.490342	75.159361
250.579813	40.663221	75.164366
250.205251	41.041559	75.169370
248.896992	39.998098	75.174375
247.977587	36.240218	75.179380
247.266774	41.145969	75.184385
247.307317	44.706653	75.189390
246.526870	37.835796	75.194394
246.447048	45.985672	75.199399
245.800011	39.459400	75.204404
244.671734	46.030732	75.209409
244.405885	40.976490	75.214414
243.435755	40.047862	75.219418
242.209703	45.412645	75.224423
241.850216	37.798170	75.229428
241.376652	38.834111	75.234433
241.082081	36.567767	75.239438
240.301100	37.968106	75.244442
239.534294	47.528484	75.249447
238.999220	40.541242	75.254452
237.496622	40.301474	75.259457
236.864141	41.414790	75.264462
236.323784	28.869645	75.269466
235.469271	38.026109	75.274471
235.716988	31.368241	75.279476
235.011122	37.517419	75.284481
234.529504	37.212660	75.289486
233.652047	25.599621	75.294490
232.866165	39.428685	75.299495
232.435172	31.562264	75.304500
231.231141	43.213994	75.309505
230.600993	34.664963	75.314510
230.163740	30.122176	75.319514
229.486652	34.681931	75.324519
229.294683	31.303253	75.329524
228.094886	34.113925	75.334529
227.593639	29.024677	75.339534
227.094243	27.305076	75.344538
225.616593	37.607980	75.349543
224.869047	34.158602	75.354548
224.401568	40.878481	75.359553
224.106424	38.303149	75.364558
224.122045	30.237797	75.369562
222.878903	38.306625	75.374567
222.229966	31.129387	75.379572
221.665415	31.878639	75.384577
221.281046	36.128379	75.389582
220.322158	40.636871	75.394586
219.220813	47.457809	75.399591
218.911762	40.049762	75.404596
218.421605	41.660786	75.409601
217.575765	39.081787	75.414606
217.097965	34.323116	75.419610
216.256647	43.419137	75.424615
215.911287	34.257006	75.429620
214.516864	38.369735	75.434625
213.794770	32.244950	75.439630
213.408205	33.683340	75.444634
213.072779	34.165830	75.449639
212.908461	28.425206	75.454644
211.844216	34.667794	75.459649
210.942906	38.438558	75.464654
210.600471	28.566337	75.469658
209.647799	37.348950	75.474663
208.881274	24.529218	75.479668
208.137818	34.771845	75.484673
207.606278	32.495979	75.489678
207.356614	32.652561	75.494682
206.366091	38.342504	75.499687
205.497147	37.560186	75.504692
205.017437	43.165538	75.509697
204.463256	40.655162	75.514702
204.158299	32.032218	75.519706
202.772890	37.482346	75.524711
202.328072	40.838136	75.529716
201.947172	39.913353	75.534721
201.003941	39.420424	75.539726
199.941377	32.149867	75.544730
199.303624	43.987292	75.549735
199.091475	29.287757	75.554740
198.377937	36.242410	75.559745
198.064720	42.625462	75.564750
197.155676	33.570554	75.569754
196.454607	38.925770	75.574759
196.028660	29.762302	75.579764
195.179644	39.614912	75.584769
194.516934	36.230866	75.589774
193.905400	35.530513	75.594778
193.321236	39.026791	75.599783
192.728473	41.980394	75.604788
191.506581	47.909085	75.609793
191.065198	38.710227	75.614798
190.700558	31.708445	75.619802
190.115497	39.054200	75.624807
188.975884	37.589646	75.629812
188.459293	41.161884	75.634817
188.012246	34.390860	75.639822
187.329869	27.539088	75.644826
186.058808	37.700263	75.649831
185.586121	27.831470	75.654836
185.017666	33.495125	75.659841
184.471278	31.642678	75.664846
184.281731	37.033033	75.669850
182.823684	35.619254	75.674855
182.281534	34.762763	75.679860
181.950472	37.389212	75.684865
181.567353	42.383080	75.689870
181.487706	41.684658	75.694874
179.957148	39.121806	75.699879
179.709199	34.290226	75.704884
178.306214	47.008179	75.709889
177.498700	43.505298	75.714894
177.501755	33.497572	75.719898
176.647529	44.014916	75.724903
176.006326	39.033149	75.729908
175.397660	36.581930	75.734913
174.412754	37.819262	75.739918
173.845419	31.985206	75.744922
173.388941	43.279644	75.749927
172.813920	31.823411	75.754932
171.971768	37.664751	75.759937
171.083479	43.086096	75.764942
171.079899	35.727126	75.769946
170.403985	46.361121	75.774951
169.354084	43.716905	75.779956
168.391183	35.123181	75.784961
168.279736	43.134592	75.789966
167.644659	30.164604	75.794970
166.422478	41.811366	75.799975
166.167887	38.444255	75.804980
165.696109	38.410753	75.809985
164.511314	42.792860	75.814990
163.614996	38.244435	75.819994
162.777739	40.458015	75.824999
162.788706	35.736540	75.830004
162.331077	36.492411	75.835009
161.657281	31.643581	75.840014
160.695983	29.341635	75.845018
159.673809	41.557325	75.850023
159.608905	34.580295	75.855028
159.164840	33.307625	75.860033
158.356033	45.511374	75.865038
157.719745	30.747015	75.870042
156.864032	36.303516	75.875047
156.306231	39.579556	75.880052
155.261844	31.216453	75.885057
154.455683	39.444290	75.890062
154.057139	39.550500	75.895066
153.576035	41.374556	75.900071
153.176745	30.278241	75.905076
152.071325	32.999782	75.910081
150.740172	40.947058	75.915086
150.879662	40.122232	75.920090
150.377229	49.605782	75.925095
150.046444	39.594517	75.930100
149.054903	41.294963	75.935105
148.364895	36.437682	75.940110
147.899219	37.123876	75.945114
146.423338	42.356649	75.950119
145.832406	34.212979	75.955124
145.340456	38.945082	75.960129
144.908004	44.822028	75.965134
144.811347	40.321140	75.970138
143.463974	44.580947	75.975143
143.055815	40.799935	75.980148
142.490636	36.835804	75.985153
141.285090	38.426875	75.990158
140.848657	35.550811	75.995162
139.860292	35.009910	76.000167
139.457666	27.796580	76.005172
139.547002	28.927281	76.010177
138.754689	33.587432	76.015182
137.745659	32.307084	76.020186
137.185742	42.608772	76.025191
136.952627	33.927078	76.030196
135.590842	40.404798	76.035201
134.689378	40.245855	76.040206
134.379473	39.364957	76.045210
133.607558	39.070239	76.050215
132.966820	37.396851	76.055220
132.229187	32.045702	76.060225
131.551961	32.625285	76.065230
130.970334	36.386097	76.070234
130.564817	38.529264	76.075239
129.792625	34.986077	76.080244
128.738537	41.633931	76.085249
128.338319	40.691741	76.090254
128.034857	33.771680	76.095258
127.000899	43.246947	76.100263
126.495577	36.272342	76.105268
126.050488	41.651411	76.110273
125.416825	41.648463	76.115278
124.506001	31.105234	76.120282
123.337124	43.987725	76.125287
122.984582	39.907690	76.130292
122.859312	38.081142	76.135297
121.694684	34.679387	76.140302
121.318601	29.270587	76.145306
120.110182	37.967854	76.150311
119.892560	40.394872	76.155316
119.603931	39.398619	76.160321
118.503717	38.350439	76.165326
117.996582	30.470959	76.170330
117.159171	35.816396	76.175335
116.623168	39.615668	76.180340
115.395001	37.595993	76.185345
114.660334	45.165893	76.190350
114.505695	32.346391	76.195354
113.997986	45.095066	76.200359
113.642742	32.812177	76.205364
112.699975	38.723195	76.210369
111.650003	47.970790	76.215374
111.413491	35.872392	76.220378
110.651549	36.698878	76.225383
109.977741	38.432248	76.230388
109.200470	34.129790	76.235393
108.457603	40.608172	76.240398
108.305327	36.554551	76.245402
106.985253	41.937540	76.250407
106.209986	42.026564	76.255412
105.747304	40.864105	76.260417
105.399198	44.933036	76.265422
105.101039	32.524353	76.270426
103.706033	36.794928	76.275431
103.126920	34.463595	76.280436
102.773669	32.771178	76.285441
102.152358	42.585922	76.290446
101.884931	31.722480	76.295450
100.758764	34.452082	76.300455
100.058682	34.138035	76.305460
99.209821	37.268115	76.310465
98.038143	39.927708	76.315470
97.793724	33.679478	76.320474
97.286914	40.227449	76.325479
96.758838	35.836370	76.330484
96.540044	37.629642	76.335489
95.126796	42.541796	76.340494
94.695926	35.165821	76.345498
94.242220	40.196185	76.350503
93.504589	40.099439	76.355508
92.613960	35.051822	76.360513
91.643409	49.985849	76.365518
91.826242	38.889748	76.370522
90.785282	44.595662	76.375527
90.107085	37.098282	76.380532
89.421646	39.346021	76.385537
88.479664	39.390675	76.390542
88.584152	40.943158	76.395546
87.996508	39.305470	76.400551
86.942085	38.325695	76.405556
86.174994	40.999616	76.410561
85.319966	36.342138	76.415566
84.786750	32.412351	76.420570
83.777206	36.225649	76.425575
83.165371	36.745931	76.430580
82.985260	39.151199	76.435585
82.578177	40.186028	76.440590
81.798668	39.517224	76.445594
80.808468	39.949616	76.450599
80.242446	33.963991	76.455604
79.490107	36.539367	76.460609
78.321587	34.675779	76.465614
78.115688	30.539251	76.470618
77.283224	39.860972	76.475623
77.024380	28.401660	76.480628
76.794139	29.091319	76.485633
75.379557	37.573903	76.490638
75.115450	36.559553	76.495642
74.725576	37.449713	76.500647
73.956055	32.814873	76.505652
72.894649	29.019791	76.510657
72.311908	33.621305	76.515662
71.636181	24.989719	76.520666
70.632315	35.146172	76.525671
69.665538	40.903339	76.530676
69.449013	33.160450	76.535681
68.639401	35.063722	76.540686
68.797509	35.492750	76.545690
67.883154	39.517953	76.550695
66.863231	45.687298	76.555700
66.298083	32.302498	76.560705
65.552676	41.755417	76.565710
65.041911	39.682852	76.570714
64.266090	40.979920	76.575719
63.479416	41.465013	76.580724
63.351984	38.068175	76.585729
62.389703	40.790581	76.590734
61.563393	28.606496	76.595738
60.711996	32.249499	76.600743
60.432312	33.921598	76.605748
60.369182	29.267142	76.610753
59.150074	35.263250	76.615758
58.412555	30.358386	76.620762
57.948004	35.977107	76.625767
57.286489	36.745015	76.630772
56.282859	34.377324	76.635777
55.431444	38.097603	76.640782
55.054101	39.813665	76.645786
54.643890	42.019092	76.650791
53.527176	39.656822	76.655796
52.941272	30.686062	76.660801
51.983940	42.049352	76.665806
51.933434	35.533659	76.670810
51.559112	37.618245	76.675815
50.687259	39.066251	76.680820
50.117545	36.402274	76.685825
49.463771	47.690345	76.690830
48.763594	33.133338	76.695834
47.608546	40.850724	76.700839
46.941557	38.894542	76.705844
47.031458	32.911542	76.710849
45.508246	33.875238	76.715854
44.944983	30.100065	76.720858
44.465543	42.323840	76.725863
43.654866	41.139628	76.730868
43.633844	28.169523	76.735873
42.461217	42.864549	76.740878
41.813066	34.594422	76.745882
41.148741	37.275619	76.750887
40.925169	31.651700	76.755892
39.877105	30.229388	76.760897
38.771447	39.656193	76.765902
38.331707	28.739828	76.770906
38.154460	34.292225	76.775911
37.701625	30.893676	76.780916
37.215947	29.186123	76.785921
35.893989	36.018658	76.790926
35.599665	27.903412	76.795930
34.300202	32.724907	76.800935
33.639856	42.992163	76.805940
33.425753	24.274925	76.810945
32.503092	41.251347	76.815950
32.438233	29.376329	76.820954
31.226516	39.349907	76.825959
30.349663	37.479244	76.830964
30.287421	32.734761	76.835969
29.261824	38.072393	76.840974
28.416638	36.313374	76.845978
27.750092	32.598833	76.850983
27.144069	34.562685	76.855988
26.943105	28.001611	76.860993
26.051987	36.694035	76.865998
25.467937	32.493252	76.871002
25.024645	36.888030	76.876007
24.175835	33.265641	76.881012
23.312714	32.845158	76.886017
22.210057	41.628098	76.891022
21.997933	29.801802	76.896026
21.357135	38.891114	76.901031
21.125433	34.544244	76.906036
20.318591	33.927129	76.911041
19.259780	35.474353	76.916046
19.029286	28.071170	76.921050
18.145040	36.290993	76.926055
17.380446	28.383226	76.931060
16.663403	28.546570	76.936065
16.054359	40.094008	76.941070
15.992463	34.835386	76.946074
14.743620	44.592547	76.951079
13.759598	40.113367	76.956084
13.483691	31.282407	76.961089
12.980674	35.027549	76.966094
12.279923	32.726682	76.971098
11.241167	39.725368	76.976103
10.270053	44.075034	76.981108
10.121697	31.789137	76.986113
9.792619	38.212575	76.991118
9.447468	34.483043	76.996122
8.504284	33.506060	77.001127
7.660893	39.085870	77.006132
6.687696	33.073754	77.011137
5.635511	39.535268	77.016142
5.045949	30.265489	77.021147
4.601325	35.548302	77.026151
4.207132	38.364613	77.031156
3.669377	28.247636	77.036161