Fri Mar 05 19:51:21 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.656416	100.890378	0.000000
-1.282649	96.735748	0.005005
-2.127556	73.875499	0.010010
-3.418497	30.464688	0.015014
-6.516415	-12.435416	0.020019
-11.132824	-28.338834	0.025024
-16.705122	-28.949559	0.030029
-21.681057	-24.557152	0.035034
-25.999949	-33.263527	0.040038
-30.301614	-28.428308	0.045043
-33.738553	-32.345842	0.050048
-37.775998	-28.237151	0.055053
-41.199153	-21.943035	0.060058
-44.531223	-34.007982	0.065062
-48.270938	-20.940867	0.070067
-51.818509	-20.396912	0.075072
-55.754865	-24.477595	0.080077
-59.751186	-26.229026	0.085082
-63.131991	-30.275320	0.090086
-67.119921	-22.230554	0.095091
-70.916568	-34.046306	0.100096
-74.681321	-32.428467	0.105101
-78.649565	-24.125053	0.110106
-82.221152	-25.384394	0.115110
-86.274737	-30.319946	0.120115
-89.652152	-31.089864	0.125120
-93.591582	-31.282838	0.130125
-97.312296	-28.911906	0.135130
-100.795652	-31.314383	0.140134
-104.902197	-24.116374	0.145139
-108.633587	-29.721452	0.150144
-112.431297	-28.276491	0.155149
-116.031768	-18.880530	0.160154
-119.665137	-32.146228	0.165158
-123.426952	-19.346713	0.170163
-126.992953	-22.322589	0.175168
-131.242088	-31.807867	0.180173
-135.426808	-18.018347	0.185178
-138.425199	-30.954828	0.190182
-142.702114	-23.649149	0.195187
-146.941398	-17.748209	0.200192
-150.688929	-15.576341	0.205197
-154.327870	-15.266813	0.210202
-157.532471	-21.656036	0.215206
-161.404823	-21.949488	0.220211
-164.969447	-18.081615	0.225216
-168.677835	-26.437295	0.230221
-172.509860	-23.330980	0.235226
-176.285103	-22.389394	0.240230
-180.100594	-14.461850	0.245235
-183.882058	-19.768665	0.250240
-187.642297	-26.300985	0.255245
-191.410436	-14.545869	0.260250
-195.014953	-37.626172	0.265254
-198.808372	-14.328569	0.270259
-202.717978	-33.883027	0.275264
-206.362358	-20.707903	0.280269
-210.318283	-17.737872	0.285274
-213.902851	-23.498678	0.290278
-218.327484	-23.724399	0.295283
-221.620903	-17.474398	0.300288
-225.062693	-26.233653	0.305293
-229.104594	-15.191722	0.310298
-232.607208	-26.237279	0.315302
-236.298789	-19.045360	0.320307
-240.230960	-23.643637	0.325312
-244.009984	-20.200320	0.330317
-247.787516	-22.546170	0.335322
-251.644159	-20.503387	0.340326
-255.312819	-26.323246	0.345331
-259.017991	-25.872103	0.350336
-262.894381	-20.475162	0.355341
-266.990106	-25.767948	0.360346
-270.612032	-27.949364	0.365350
-274.245663	-17.164918	0.370355
-277.831405	-27.129548	0.375360
-281.550406	-21.989510	0.380365
-285.731103	-23.108744	0.385370
-288.957913	-29.148885	0.390374
-292.777388	-26.258850	0.395379
-296.646509	-26.685062	0.400384
-300.576037	-20.267188	0.405389
-304.235901	-16.448566	0.410394
-307.806823	-27.956179	0.415398
-311.984020	-13.443764	0.420403
-315.787610	-23.775679	0.425408
-319.601942	-18.893175	0.430413
-323.320225	-22.894683	0.435418
-326.645274	-25.005137	0.440422
-330.406312	-20.481205	0.445427
-334.382889	-28.544643	0.450432
-337.826035	-30.789189	0.455437
-341.830267	-29.804480	0.460442
-345.384843	-26.423649	0.465446
-349.526356	-30.985164	0.470451
-353.553547	-32.781635	0.475456
-356.662824	-31.230162	0.480461
-360.954078	-23.481859	0.485466
-364.273922	-27.122717	0.490470
-368.032408	-28.525253	0.495475
-372.218466	-22.280774	0.500480
-375.777202	-38.393284	0.505485
-379.924161	-28.337283	0.510490
-383.153647	-31.741807	0.515494
-386.970894	-26.861891	0.520499
-390.658972	-27.044048	0.525504
-394.641983	-27.513418	0.530509
-398.562171	-19.762796	0.535514
-401.840419	-26.004299	0.540518
-405.917245	-25.123008	0.545523
-409.538562	-28.583201	0.550528
-413.023196	-28.878232	0.555533
-417.302117	-22.289270	0.560538
-420.918405	-25.521594	0.565542
-425.018808	-22.420916	0.570547
-428.533915	-23.836989	0.575552
-432.035074	-25.357784	0.580557
-435.944201	-17.935294	0.585562
-439.651582	-21.184583	0.590566
-443.404943	-20.941501	0.595571
-447.224823	-21.704912	0.600576
-451.153732	-31.530883	0.605581
-454.912290	-21.686588	0.610586
-458.595093	-30.652996	0.615590
-462.442168	-23.932650	0.620595
-465.769812	-29.059164	0.625600
-469.827962	-31.359842	0.630605
-473.880866	-20.538123	0.635610
-477.522170	-28.940278	0.640614
-480.927687	-22.339306	0.645619
-484.735359	-28.890369	0.650624
-488.298905	-26.938176	0.655629
-492.388429	-21.166221	0.660634
-496.191929	-32.303648	0.665638
-500.312758	-24.158131	0.670643
-503.556627	-30.744016	0.675648
-507.106262	-29.446866	0.680653
-511.355738	-22.305788	0.685658
-514.902737	-29.593862	0.690662
-518.605477	-20.524777	0.695667
-522.629504	-27.845456	0.700672
-526.279887	-30.255320	0.705677
-530.356686	-26.005498	0.710682
-533.611129	-30.169061	0.715686
-537.414790	-29.422640	0.720691
-541.299843	-23.027263	0.725696
-544.697348	-27.279922	0.730701
-548.674202	-18.934973	0.735706
-552.649112	-25.627943	0.740710
-556.570107	-19.319838	0.745715
-560.100629	-10.435889	0.750720
-563.911530	-29.459832	0.755725
-567.705149	-15.591750	0.760730
-571.427407	-31.136932	0.765734
-575.043937	-23.865046	0.770739
-579.009199	-19.413766	0.775744
-582.667307	-27.362065	0.780749
-586.462611	-15.023307	0.785754
-589.933355	-24.319842	0.790758
-593.875913	-20.454052	0.795763
-597.628863	-25.170238	0.800768
-601.266228	-30.627115	0.805773
-605.600169	-22.146185	0.810778
-608.935969	-22.882593	0.815782
-612.751600	-23.980725	0.820787
-616.553197	-22.865507	0.825792
-620.259594	-27.199591	0.830797
-624.149782	-17.874903	0.835802
-627.941327	-26.577659	0.840806
-631.740054	-21.779168	0.845811
-635.423415	-27.241259	0.850816
-638.774914	-27.563537	0.855821
-642.767189	-24.627998	0.860826
-646.428605	-22.393433	0.865830
-650.363007	-22.160522	0.870835
-654.454341	-23.126228	0.875840
-657.947056	-28.267087	0.880845
-661.738127	-23.930237	0.885850
-665.206003	-29.619094	0.890854
-669.293761	-25.483982	0.895859
-673.094280	-27.175778	0.900864
-676.733209	-41.776885	0.905869
-680.397894	-31.910996	0.910874
-683.942185	-27.739698	0.915878
-688.301718	-18.000876	0.920883
-692.063315	-26.326693	0.925888
-695.045961	-32.807387	0.930893
-699.058130	-22.855978	0.935898
-702.942785	-39.187090	0.940902
-706.931492	-30.087809	0.945907
-710.702565	-29.365243	0.950912
-714.501585	-37.618803	0.955917
-718.400587	-25.379983	0.960922
-721.859751	-38.294046	0.965926
-725.458792	-31.576665	0.970931
-729.089233	-29.840503	0.975936
-733.129388	-31.047635	0.980941
-737.097484	-24.807411	0.985946
-740.645811	-36.685347	0.990950
-744.360903	-33.505361	0.995955
-748.055223	-34.673120	1.000960
-751.387201	-29.526424	1.005965
-755.730605	-22.412494	1.010970
-759.652551	-21.325121	1.015974
-763.352993	-19.908872	1.020979
-767.013164	-30.333891	1.025984
-770.606501	-37.713497	1.030989
-774.699169	-21.105512	1.035994
-778.434985	-32.830423	1.040998
-782.144947	-29.652776	1.046003
-785.942252	-31.198247	1.051008
-789.548538	-35.309940	1.056013
-793.527250	-27.516235	1.061018
-797.034900	-34.970995	1.066022
-800.811701	-30.167864	1.071027
-804.484533	-27.149077	1.076032
-808.187731	-22.062812	1.081037
-811.895207	-28.708187	1.086042
-815.579021	-39.195570	1.091046
-819.804097	-32.944100	1.096051
-823.632995	-16.788198	1.101056
-827.120019	-37.106039	1.106061
-831.112336	-24.092053	1.111066
-834.632683	-30.355725	1.116070
-838.232991	-23.092358	1.121075
-842.202560	-29.329940	1.126080
-845.741997	-31.925768	1.131085
-850.106591	-28.313790	1.136090
-853.992569	-29.624206	1.141094
-856.986901	-28.651846	1.146099
-860.901222	-23.437135	1.151104
-864.500754	-30.932295	1.156109
-868.703980	-25.974155	1.161114
-871.904126	-38.326999	1.166118
-876.052586	-27.829985	1.171123
-880.253503	-34.369550	1.176128
-883.572786	-32.276051	1.181133
-887.628554	-28.211916	1.186138
-891.101826	-27.557174	1.191142
-894.865633	-32.148133	1.196147
-898.735079	-18.511873	1.201152
-902.136087	-37.536066	1.206157
-906.244149	-29.242116	1.211162
-909.741363	-30.718672	1.216166
-913.736486	-26.717805	1.221171
-917.438814	-16.971699	1.226176
-920.919280	-32.346774	1.231181
-925.058899	-31.629593	1.236186
-928.697937	-35.286406	1.241190
-932.588414	-27.405662	1.246195
-936.506876	-22.224859	1.251200
-939.698644	-30.023213	1.256205
-943.854985	-17.736589	1.261210
-947.506516	-31.024804	1.266214
-951.412658	-24.243794	1.271219
-955.124653	-28.797208	1.276224
-958.490939	-29.640205	1.281229
-962.769361	-34.563491	1.286234
-966.322945	-26.599374	1.291238
-969.875695	-28.314536	1.296243
-973.879258	-28.265565	1.301248
-977.405071	-31.328561	1.306253
-981.623733	-30.420448	1.311258
-985.344948	-25.794648	1.316262
-988.893314	-29.681905	1.321267
-992.954609	-18.323439	1.326272
-996.392533	-28.990193	1.331277
-1000.323984	-31.756476	1.336282
-1003.952677	-38.064051	1.341286
-1007.705858	-32.945838	1.346291
-1011.587499	-21.371652	1.351296
-1015.248546	-30.763229	1.356301
-1019.059695	-21.698150	1.361306
-1022.570592	-28.354115	1.366310
-1026.309155	-24.990169	1.371315
-1030.163017	-30.194116	1.376320
-1033.875706	-33.903636	1.381325
-1038.184725	-25.332901	1.386330
-1041.942233	-23.142283	1.391334
-1045.513622	-33.784455	1.396339
-1049.108907	-37.413381	1.401344
-1052.501175	-36.716164	1.406349
-1056.640394	-19.160447	1.411354
-1060.337552	-22.006681	1.416358
-1064.105052	-17.136816	1.421363
-1068.004942	-29.114102	1.426368
-1071.731647	-41.704110	1.431373
-1075.706812	-23.621111	1.436378
-1079.438495	-23.437255	1.441382
-1082.838806	-24.000244	1.446387
-1086.770004	-30.453262	1.451392
-1090.387359	-34.326169	1.456397
-1094.506466	-25.833022	1.461402
-1097.719741	-36.620697	1.466406
-1101.541613	-32.027503	1.471411
-1105.681179	-32.319241	1.476416
-1109.304846	-35.593455	1.481421
-1113.055733	-26.820143	1.486426
-1116.923635	-36.109072	1.491430
-1120.617913	-32.116565	1.496435
-1124.166498	-29.976586	1.501440
-1127.929744	-27.474261	1.506445
-1131.986694	-17.235878	1.511450
-1135.554131	-26.374156	1.516454
-1139.125316	-27.237725	1.521459
-1143.270848	-33.744659	1.526464
-1146.755182	-37.588295	1.531469
-1150.779425	-25.907508	1.536474
-1154.903800	-22.357058	1.541478
-1158.345685	-24.067590	1.546483
-1161.777222	-25.432851	1.551488
-1165.215359	-27.653318	1.556493
-1169.422998	-27.940359	1.561498
-1173.313473	-29.743095	1.566502
-1176.809916	-34.757976	1.571507
-1181.520138	-19.256889	1.576512
-1184.494613	-28.220307	1.581517
-1188.157347	-28.744306	1.586522
-1191.633307	-37.304200	1.591526
-1195.416680	-28.151837	1.596531
-1199.513467	-20.243965	1.601536
-1203.356043	-24.837579	1.606541
-1207.347926	-28.946833	1.611546
-1211.166671	-25.326921	1.616550
-1214.465847	-30.923655	1.621555
-1218.429122	-31.448400	1.626560
-1222.053240	-34.052172	1.631565
-1226.017335	-17.101361	1.636570
-1229.713953	-29.181843	1.641574
-1233.223501	-25.412682	1.646579
-1237.493373	-28.102325	1.651584
-1240.721248	-34.478388	1.656589
-1244.848491	-24.599152	1.661594
-1248.311415	-31.021167	1.666598
-1251.913944	-33.300347	1.671603
-1256.264643	-30.978192	1.676608
-1259.705029	-35.675492	1.681613
-1263.815284	-24.966330	1.686618
-1267.317774	-25.578927	1.691622
-1270.812839	-25.088863	1.696627
-1274.900962	-24.179036	1.701632
-1278.353505	-34.097114	1.706637
-1282.504084	-23.619582	1.711642
-1286.133027	-31.998729	1.716646
-1289.535344	-29.684796	1.721651
-1293.651083	-27.505829	1.726656
-1297.375248	-33.898569	1.731661
-1301.041618	-32.512162	1.736666
-1304.888313	-24.973718	1.741670
-1308.462702	-30.841646	1.746675
-1312.485764	-29.052786	1.751680
-1315.897348	-29.925857	1.756685
-1320.281226	-24.021824	1.761690
-1323.700546	-23.833957	1.766694
-1327.245583	-22.126314	1.771699
-1331.232825	-22.465685	1.776704
-1334.477341	-28.056798	1.781709
-1338.577907	-25.911718	1.786714
-1342.607398	-25.126272	1.791718
-1346.210722	-29.447284	1.796723
-1350.353673	-22.274497	1.801728
-1353.819184	-32.589338	1.806733
-1357.296080	-21.850521	1.811738
-1361.036328	-24.200523	1.816742
-1364.840469	-27.145826	1.821747
-1368.914173	-19.080518	1.826752
-1372.478683	-39.605778	1.831757
-1376.386644	-33.506602	1.836762
-1380.258603	-26.895953	1.841766
-1383.830725	-28.082260	1.846771
-1387.663537	-23.127318	1.851776
-1391.340670	-36.820662	1.856781
-1395.118227	-25.005513	1.861786
-1398.517344	-31.625160	1.866790
-1402.692395	-29.299313	1.871795
-1406.624272	-24.560288	1.876800
-1410.390675	-26.514946	1.881805
-1413.947296	-24.288089	1.886810
-1417.749678	-18.942163	1.891814
-1421.245319	-28.334309	1.896819
-1425.238038	-31.714507	1.901824
-1428.711120	-34.742667	1.906829
-1432.653433	-25.149762	1.911834
-1436.743112	-35.877029	1.916838
-1440.186744	-34.287951	1.921843
-1444.039253	-23.703334	1.926848
-1447.555671	-35.851707	1.931853
-1451.902985	-21.127297	1.936858
-1455.841942	-20.392419	1.941862
-1459.118227	-26.602721	1.946867
-1462.947572	-24.642773	1.951872
-1466.689559	-28.127700	1.956877
-1470.254536	-23.013666	1.961882
-1473.693532	-35.585967	1.966886
-1477.579924	-29.379694	1.971891
-1481.840472	-25.131950	1.976896
-1485.554652	-32.122046	1.981901
-1489.068847	-27.593267	1.986906
-1492.902407	-28.828999	1.991910
-1496.381197	-30.116806	1.996915
-1500.774786	-26.157622	2.006912
-1501.764287	-29.054191	2.016909
-1498.948354	-30.134915	2.026906
-1496.175918	-29.872893	2.036902
-1494.111519	-26.633302	2.046899
-1491.906285	-31.773553	2.056896
-1490.318834	-28.012324	2.066893
-1488.542007	-35.433419	2.076890
-1486.591125	-33.250898	2.086886
-1484.709384	-28.747324	2.096883
-1482.202407	-33.299573	2.106880
-1480.877749	-33.806743	2.116877
-1479.128615	-29.569296	2.126874
-1476.797450	-32.337614	2.136870
-1475.051158	-24.927632	2.146867
-1473.194670	-28.264143	2.156864
-1471.522889	-34.781046	2.166861
-1469.362576	-34.708341	2.176858
-1467.435461	-24.128388	2.186854
-1465.751592	-26.881469	2.196851
-1463.768372	-28.008812	2.206848
-1461.799487	-32.997507	2.216845
-1459.998150	-29.354187	2.226842
-1458.090500	-29.332593	2.236838
-1455.782385	-23.432013	2.246835
-1454.434150	-28.733427	2.256832
-1452.420020	-33.711991	2.266829
-1450.557085	-31.666933	2.276826
-1448.656409	-28.184772	2.286822
-1446.678080	-30.037626	2.296819
-1444.899894	-26.381113	2.306816
-1443.226623	-27.263023	2.316813
-1441.332202	-26.340884	2.326810
-1438.912020	-32.330232	2.336806
-1437.295258	-31.685735	2.346803
-1435.543378	-29.468148	2.356800
-1433.583713	-24.699113	2.366797
-1431.517353	-26.532892	2.376794
-1429.729862	-30.546738	2.386790
-1428.172121	-31.842768	2.396787
-1426.009634	-32.716151	2.406784
-1424.315333	-32.125112	2.416781
-1422.293269	-31.307077	2.426778
-1420.495709	-34.509376	2.436774
-1418.542447	-29.448780	2.446771
-1416.710301	-32.484510	2.456768
-1414.823819	-23.810090	2.466765
-1412.886778	-23.336852	2.476762
-1411.325358	-23.788730	2.486758
-1408.918686	-26.745912	2.496755
-1406.979236	-28.564088	2.506752
-1405.303666	-26.062683	2.516749
-1403.608098	-18.423466	2.526746
-1401.398098	-22.279147	2.536742
-1399.798577	-21.641337	2.546739
-1398.194027	-22.490108	2.556736
-1395.943924	-25.917997	2.566733
-1394.159555	-32.983397	2.576730
-1392.318071	-27.653831	2.586726
-1390.150859	-27.427420	2.596723
-1388.349253	-26.297747	2.606720
-1386.599399	-26.083465	2.616717
-1384.712456	-29.633203	2.626714
-1382.942183	-23.648023	2.636710
-1381.097726	-26.237280	2.646707
-1378.944689	-27.440684	2.656704
-1376.807207	-20.895339	2.666701
-1375.566325	-23.446390	2.676698
-1373.602646	-30.669954	2.686694
-1371.469478	-27.220207	2.696691
-1369.977583	-27.795138	2.706688
-1367.759146	-24.002197	2.716685
-1365.974332	-26.255055	2.726682
-1363.940264	-27.551505	2.736678
-1362.115084	-31.042391	2.746675
-1360.357119	-29.132032	2.756672
-1358.284883	-33.164565	2.766669
-1356.621702	-28.008530	2.776666
-1354.587169	-29.781884	2.786662
-1352.965960	-28.130679	2.796659
-1351.218149	-27.740781	2.806656
-1348.950701	-32.974545	2.816653
-1347.038286	-29.075757	2.826650
-1345.507802	-27.833178	2.836646
-1343.263602	-28.223779	2.846643
-1341.429843	-28.382891	2.856640
-1339.671854	-26.071470	2.866637
-1337.839350	-27.913523	2.876634
-1335.795988	-27.948287	2.886630
-1334.057447	-30.253714	2.896627
-1332.172949	-25.246768	2.906624
-1330.012526	-33.933884	2.916621
-1328.308979	-33.181623	2.926618
-1326.578736	-31.309433	2.936614
-1324.899589	-36.273746	2.946611
-1322.775218	-36.570937	2.956608
-1320.656479	-33.167780	2.966605
-1319.166398	-34.970799	2.976602
-1316.948326	-35.379298	2.986598
-1315.239116	-31.945323	2.996595
-1313.434296	-32.845038	3.006592
-1311.433467	-30.146151	3.016589
-1309.443324	-24.646098	3.026586
-1307.930725	-27.379550	3.036582
-1305.524033	-32.269248	3.046579
-1303.823024	-28.393428	3.056576
-1302.441599	-28.988528	3.066573
-1300.571724	-31.656001	3.076570
-1298.342341	-29.159471	3.086566
-1296.404741	-31.711466	3.096563
-1294.524217	-33.270646	3.106560
-1292.708762	-27.842093	3.116557
-1290.654475	-27.439622	3.126554
-1289.074656	-27.818574	3.136550
-1286.979933	-25.051008	3.146547
-1285.146095	-35.091071	3.156544
-1283.403817	-34.673394	3.166541
-1281.390347	-32.075977	3.176538
-1279.671527	-32.698220	3.186534
-1277.579011	-39.793906	3.196531
-1276.157731	-34.351203	3.206528
-1274.004472	-31.960887	3.216525
-1272.112772	-25.508736	3.226522
-1270.039569	-22.707710	3.236518
-1268.251245	-19.635302	3.246515
-1266.477207	-25.432655	3.256512
-1264.799882	-26.430350	3.266509
-1262.574013	-28.654243	3.276506
-1260.466224	-32.798170	3.286502
-1258.771329	-27.295032	3.296499
-1257.122541	-30.124457	3.306496
-1255.292615	-26.250282	3.316493
-1253.467317	-27.547963	3.326490
-1251.501569	-28.929697	3.336486
-1249.475817	-24.616332	3.346483
-1247.673090	-27.036178	3.356480
-1245.984819	-22.239331	3.366477
-1243.887741	-30.516768	3.376474
-1242.039261	-27.573967	3.386470
-1240.096571	-31.644089	3.396467
-1238.422278	-29.964981	3.406464
-1236.446060	-24.852630	3.416461
-1234.479599	-25.691309	3.426458
-1232.473798	-29.856788	3.436454
-1230.798334	-23.685784	3.446451
-1228.846873	-26.115206	3.456448
-1227.195144	-30.366126	3.466445
-1224.970606	-29.574000	3.476442
-1223.097436	-28.168282	3.486438
-1221.570368	-29.258743	3.496435
-1219.626027	-32.912273	3.506432
-1217.663665	-27.145587	3.516429
-1215.828165	-28.410135	3.526426
-1213.859682	-29.383330	3.536422
-1212.100673	-24.709881	3.546419
-1210.113374	-24.760827	3.556416
-1208.084579	-28.945754	3.566413
-1206.365042	-32.819091	3.576410
-1204.501892	-23.150751	3.586406
-1202.862288	-26.892876	3.596403
-1200.987559	-27.353693	3.606400
-1198.698487	-25.820293	3.616397
-1196.880715	-26.710939	3.626394
-1195.177197	-21.979649	3.636390
-1192.953219	-32.941018	3.646387
-1191.310059	-27.172182	3.656384
-1189.527150	-20.326760	3.666381
-1187.840438	-26.669030	3.676378
-1185.534075	-28.962572	3.686374
-1184.074872	-32.941080	3.696371
-1182.381925	-27.830725	3.706368
-1179.844950	-23.496461	3.716365
-1178.267252	-23.462895	3.726362
-1176.199328	-26.239329	3.736358
-1174.479640	-26.018480	3.746355
-1172.655594	-27.328530	3.756352
-1170.776777	-19.855809	3.766349
-1168.732748	-27.827859	3.776346
-1166.886521	-24.704635	3.786342
-1165.168039	-26.135157	3.796339
-1163.083545	-29.231596	3.806336
-1161.509190	-23.818040	3.816333
-1159.541291	-25.080043	3.826330
-1157.455476	-33.707710	3.836326
-1155.474339	-30.467116	3.846323
-1153.786339	-33.187482	3.856320
-1152.284516	-29.017573	3.866317
-1150.420851	-22.597142	3.876314
-1147.966687	-21.494312	3.886310
-1146.441652	-26.702273	3.896307
-1144.349315	-24.090507	3.906304
-1142.629669	-25.601725	3.916301
-1140.527886	-22.527258	3.926298
-1138.911884	-25.962409	3.936294
-1137.016302	-29.677547	3.946291
-1135.140480	-22.984313	3.956288
-1133.138715	-27.228012	3.966285
-1131.352281	-31.827258	3.976282
-1129.471887	-28.264209	3.986278
-1127.660235	-26.949623	3.996275
-1125.743140	-25.077170	4.006272
-1123.988767	-29.884439	4.016269
-1121.741369	-36.521620	4.026266
-1119.884673	-28.652165	4.036262
-1118.067052	-27.608525	4.046259
-1116.291596	-23.820256	4.056256
-1114.271343	-23.813234	4.066253
-1112.602876	-24.255195	4.076250
-1110.724221	-26.203930	4.086246
-1108.628471	-24.203727	4.096243
-1107.099131	-27.880781	4.106240
-1105.282192	-24.305981	4.116237
-1102.883092	-25.340074	4.126234
-1101.286694	-25.274711	4.136230
-1099.708119	-26.319649	4.146227
-1097.641474	-22.780050	4.156224
-1095.350540	-23.698939	4.166221
-1094.111220	-25.835915	4.176218
-1092.000830	-27.246970	4.186214
-1089.892285	-25.809320	4.196211
-1088.099623	-26.691128	4.206208
-1086.453433	-24.682150	4.216205
-1084.296983	-27.150561	4.226202
-1082.414727	-30.252476	4.236198
-1080.740324	-25.595387	4.246195
-1078.675296	-26.482861	4.256192
-1077.000068	-29.119026	4.266189
-1075.036012	-27.479831	4.276186
-1073.134382	-27.905376	4.286182
-1071.161859	-34.108547	4.296179
-1069.248308	-31.700220	4.306176
-1067.708595	-30.796824	4.316173
-1065.533791	-36.113402	4.326170
-1063.693400	-34.122840	4.336166
-1061.992235	-32.916846	4.346163
-1060.235258	-32.998718	4.356160
-1057.905662	-29.049566	4.366157
-1055.962416	-30.935957	4.376154
-1054.500030	-31.373336	4.386150
-1052.602318	-36.418216	4.396147
-1050.561328	-35.699196	4.406144
-1049.128238	-28.382447	4.416141
-1046.841052	-38.221700	4.426138
-1044.960053	-37.360244	4.436134
-1043.121900	-33.979841	4.446131
-1041.175566	-35.307769	4.456128
-1039.210236	-31.090337	4.466125
-1037.338206	-34.836367	4.476122
-1035.623170	-29.628379	4.486118
-1033.768990	-28.287362	4.496115
-1032.025294	-35.821268	4.506112
-1030.214675	-32.070135	4.516109
-1027.992334	-36.206920	4.526106
-1026.089673	-33.462080	4.536102
-1024.222076	-28.976373	4.546099
-1022.977991	-25.046204	4.556096
-1020.586310	-22.295883	4.566093
-1018.588971	-24.464053	4.576090
-1016.905417	-29.953077	4.586086
-1014.815827	-29.758111	4.596083
-1013.089691	-31.113958	4.606080
-1011.118250	-31.828511	4.616077
-1009.483517	-28.102915	4.626074
-1007.679027	-30.502338	4.636070
-1005.555803	-27.154860	4.646067
-1003.737162	-31.317063	4.656064
-1001.790632	-29.586581	4.666061
-999.768244	-30.072431	4.676058
-998.178579	-35.001691	4.686054
-996.608621	-28.412581	4.696051
-994.321085	-26.341891	4.706048
-992.525313	-28.681487	4.716045
-990.438859	-28.031263	4.726042
-988.529474	-27.281668	4.736038
-986.771258	-21.589492	4.746035
-985.153293	-27.506953	4.756032
-983.199222	-22.076620	4.766029
-980.990788	-24.730094	4.776026
-979.388501	-26.381900	4.786022
-977.359791	-26.114008	4.796019
-975.495000	-30.997251	4.806016
-973.547646	-31.090555	4.816013
-972.113913	-27.113316	4.826010
-970.066132	-23.715845	4.836006
-968.051500	-22.717801	4.846003
-966.462626	-19.728520	4.856000
-964.334633	-27.472258	4.865997
-962.309233	-30.402759	4.875994
-960.342815	-27.224375	4.885990
-958.527777	-24.958094	4.895987
-956.904722	-29.474249	4.905984
-954.986785	-31.124407	4.915981
-952.644793	-27.126601	4.925978
-950.849600	-27.707132	4.935974
-949.279803	-31.021086	4.945971
-947.779991	-29.961230	4.955968
-945.797504	-28.738554	4.965965
-943.901865	-25.757257	4.975962
-941.707183	-21.255884	4.985958
-939.828613	-29.079718	4.995955
-937.896270	-23.988502	5.005952
-936.114212	-26.411127	5.015949
-934.274064	-20.010431	5.025946
-932.402488	-28.101563	5.035942
-930.731268	-22.997009	5.045939
-928.826233	-14.309318	5.055936
-926.801916	-23.329605	5.065933
-924.674201	-23.532233	5.075930
-922.812349	-21.581302	5.085926
-921.163370	-23.028957	5.095923
-919.296544	-23.635128	5.105920
-917.716300	-22.588112	5.115917
-915.741111	-20.634771	5.125914
-913.582113	-23.839225	5.135910
-911.519503	-26.786687	5.145907
-909.995220	-25.369141	5.155904
-908.161704	-25.510505	5.165901
-905.982932	-20.488660	5.175898
-904.040749	-25.857909	5.185894
-902.295019	-24.005238	5.195891
-900.547072	-18.121875	5.205888
-898.814518	-23.198659	5.215885
-896.531515	-20.198726	5.225882
-894.925801	-20.546817	5.235878
-893.073959	-26.065824	5.245875
-891.213558	-18.773068	5.255872
-889.453259	-25.246909	5.265869
-887.551410	-24.287606	5.275866
-885.474215	-27.864218	5.285862
-883.444436	-18.388013	5.295859
-881.652348	-26.284823	5.305856
-880.036539	-24.485575	5.315853
-877.953756	-19.184671	5.325850
-876.055222	-21.526401	5.335846
-874.191716	-23.467793	5.345843
-872.198260	-17.530499	5.355840
-870.685069	-13.313261	5.365837
-868.519656	-22.641850	5.375834
-866.829915	-21.047043	5.385830
-864.930888	-17.756746	5.395827
-863.113806	-21.451232	5.405824
-860.825861	-24.979411	5.415821
-859.365115	-22.016939	5.425818
-857.458518	-20.223108	5.435814
-855.436245	-26.903016	5.445811
-853.786801	-27.749121	5.455808
-851.512528	-18.896179	5.465805
-849.647061	-23.271020	5.475802
-847.821767	-26.819964	5.485798
-846.129299	-32.624510	5.495795
-844.645367	-28.980475	5.505792
-842.269723	-25.101617	5.515789
-840.730905	-28.524234	5.525786
-838.565610	-27.104899	5.535782
-836.775560	-26.067683	5.545779
-835.088221	-28.786145	5.555776
-833.039068	-27.839291	5.565773
-830.832233	-29.072901	5.575770
-828.970651	-27.110799	5.585766
-827.278177	-30.096918	5.595763
-825.585057	-29.123146	5.605760
-823.591520	-25.849503	5.615757
-821.476155	-23.154278	5.625754
-819.994682	-27.617715	5.635750
-818.009539	-22.533254	5.645747
-815.969146	-29.978656	5.655744
-814.405272	-25.510538	5.665741
-812.393726	-22.277657	5.675738
-810.397257	-21.911309	5.685734
-808.685305	-22.151586	5.695731
-806.612629	-27.999512	5.705728
-804.734358	-22.582167	5.715725
-803.204598	-27.550681	5.725722
-800.923985	-23.269747	5.735718
-798.917714	-26.446530	5.745715
-797.672394	-25.985372	5.755712
-795.455050	-23.827475	5.765709
-793.436927	-22.752468	5.775706
-791.607131	-27.014195	5.785702
-789.791357	-18.577377	5.795699
-788.331797	-18.733087	5.805696
-785.937382	-23.323477	5.815693
-784.211274	-18.761265	5.825690
-782.203878	-19.568217	5.835686
-780.455037	-24.838576	5.845683
-778.775323	-25.932625	5.855680
-776.696370	-22.164171	5.865677
-774.755752	-30.806224	5.875674
-772.811100	-17.299469	5.885670
-771.151724	-21.781839	5.895667
-769.293712	-29.057530	5.905664
-767.436149	-20.889478	5.915661
-765.046755	-25.875359	5.925658
-763.120516	-24.738273	5.935654
-761.958900	-24.536876	5.945651
-760.148211	-26.169739	5.955648
-757.836349	-28.820592	5.965645
-756.089485	-23.233783	5.975642
-754.186327	-33.551411	5.985638
-752.094622	-31.326026	5.995635
-750.520765	-27.314194	6.005632
-748.644934	-25.554830	6.015629
-746.553916	-23.379855	6.025626
-744.672881	-29.418156	6.035622
-742.938474	-30.459342	6.045619
-740.952899	-27.915406	6.055616
-739.179244	-25.760758	6.065613
-737.151684	-27.837209	6.075610
-735.396186	-36.137015	6.085606
-733.592401	-25.519292	6.095603
-731.596939	-21.784822	6.105600
-729.810007	-28.505969	6.115597
-727.938214	-26.311732	6.125594
-726.160695	-23.603481	6.135590
-724.232324	-26.049334	6.145587
-722.006096	-28.081732	6.155584
-720.660030	-25.724528	6.165581
-718.596098	-26.011514	6.175578
-716.580049	-34.708209	6.185574
-714.773903	-26.042423	6.195571
-713.093370	-23.407085	6.205568
-710.691254	-21.603895	6.215565
-709.077797	-31.414147	6.225562
-707.414710	-25.554966	6.235558
-705.439265	-30.162009	6.245555
-703.397906	-20.431692	6.255552
-701.723291	-27.019609	6.265549
-699.761485	-29.243416	6.275546
-697.693656	-25.111534	6.285542
-696.011121	-25.173345	6.295539
-694.298066	-27.251609	6.305536
-692.157077	-22.120886	6.315533
-690.232101	-26.021959	6.325530
-688.377435	-30.158110	6.335526
-686.576549	-21.521457	6.345523
-684.676373	-22.098036	6.355520
-682.806792	-25.385515	6.365517
-681.440290	-23.911027	6.375514
-679.069558	-22.780159	6.385510
-677.303068	-23.220108	6.395507
-675.345721	-27.952132	6.405504
-673.553269	-29.589910	6.415501
-671.423385	-25.532656	6.425498
-669.468158	-23.234861	6.435494
-668.019131	-22.569341	6.445491
-665.981691	-21.970995	6.455488
-664.040275	-25.637833	6.465485
-662.221965	-25.696050	6.475482
-660.455238	-24.920235	6.485478
-658.481624	-25.672738	6.495475
-656.412052	-25.641623	6.505472
-654.757719	-25.144688	6.515469
-653.311950	-19.294950	6.525466
-650.972653	-20.107453	6.535462
-648.795338	-27.179867	6.545459
-647.058616	-27.332405	6.555456
-645.388102	-20.470150	6.565453
-643.494669	-27.111939	6.575450
-641.569728	-26.186124	6.585446
-639.840288	-26.212757	6.595443
-637.807475	-24.075752	6.605440
-635.722534	-28.409709	6.615437
-633.984814	-34.723451	6.625434
-632.527616	-26.189739	6.635430
-630.380109	-29.392108	6.645427
-628.504867	-32.707291	6.655424
-626.595366	-26.475311	6.665421
-624.613175	-23.477575	6.675418
-622.816247	-23.470767	6.685414
-621.157605	-28.854501	6.695411
-619.182355	-22.585648	6.705408
-617.058230	-21.963214	6.715405
-614.970202	-29.243966	6.725402
-613.427750	-21.807016	6.735398
-611.733119	-21.348067	6.745395
-609.690966	-17.957264	6.755392
-608.072791	-21.968735	6.765389
-605.929505	-26.763568	6.775386
-603.720340	-23.217863	6.785382
-602.383490	-22.239118	6.795379
-600.364929	-17.278219	6.805376
-598.453064	-25.059765	6.815373
-596.507958	-21.737132	6.825370
-594.734445	-27.434463	6.835366
-592.767426	-22.830063	6.845363
-590.941855	-23.783071	6.855360
-589.265247	-22.602805	6.865357
-587.037850	-16.765781	6.875354
-585.294392	-20.963041	6.885350
-583.186169	-21.212775	6.895347
-582.002946	-21.824741	6.905344
-579.771215	-23.594204	6.915341
-577.501525	-23.841305	6.925338
-575.838488	-23.955178	6.935334
-574.082336	-21.355501	6.945331
-572.297430	-26.653584	6.955328
-570.212265	-26.056463	6.965325
-568.610410	-20.574235	6.975322
-566.129508	-25.964545	6.985318
-564.473187	-20.599962	6.995315
-562.833523	-23.143255	7.005312
-561.038593	-15.130803	7.015309
-559.065185	-16.977404	7.025306
-557.126631	-17.585276	7.035302
-555.040809	-26.217210	7.045299
-553.477935	-28.983494	7.055296
-551.522812	-20.158203	7.065293
-549.788678	-20.572363	7.075290
-547.836392	-19.655576	7.085286
-546.187810	-24.333444	7.095283
-544.035556	-26.431232	7.105280
-542.047225	-27.148095	7.115277
-540.157218	-26.331881	7.125274
-538.369623	-23.940883	7.135270
-536.619652	-18.588078	7.145267
-534.646565	-21.847769	7.155264
-532.812893	-21.554656	7.165261
-530.893905	-23.883595	7.175258
-528.960856	-19.204238	7.185254
-527.135786	-19.277643	7.195251
-525.505066	-14.935256	7.205248
-523.256974	-19.137287	7.215245
-521.565917	-22.552447	7.225242
-519.826908	-19.916831	7.235238
-517.703033	-18.926373	7.245235
-516.087375	-14.941574	7.255232
-513.937392	-23.913727	7.265229
-511.944831	-20.511758	7.275226
-510.249156	-19.639218	7.285222
-508.358894	-17.283540	7.295219
-506.256666	-18.864883	7.305216
-504.779370	-18.942726	7.315213
-502.727737	-20.002826	7.325210
-500.917734	-22.510125	7.335206
-498.771632	-20.307407	7.345203
-496.828296	-13.281763	7.355200
-495.203592	-17.695260	7.365197
-493.465829	-18.788908	7.375194
-491.603379	-24.337743	7.385190
-489.433106	-21.638349	7.395187
-487.728413	-22.922501	7.405184
-485.825551	-17.033545	7.415181
-484.203982	-26.327072	7.425178
-481.883151	-21.621185	7.435174
-480.211933	-23.681567	7.445171
-478.492761	-20.899067	7.455168
-476.479404	-18.676707	7.465165
-474.564388	-26.035508	7.475162
-472.630160	-20.650500	7.485158
-470.920064	-22.412347	7.495155
-469.130601	-31.255831	7.505152
-467.248218	-24.672011	7.515149
-465.159230	-23.641197	7.525146
-463.378843	-21.073726	7.535142
-461.463109	-24.313146	7.545139
-459.564368	-26.359322	7.555136
-457.777737	-28.218645	7.565133
-455.788598	-26.946087	7.575130
-453.696760	-26.266246	7.585126
-452.021333	-25.551483	7.595123
-450.203533	-21.594183	7.605120
-448.283082	-24.310135	7.615117
-446.439145	-25.438073	7.625114
-444.429456	-26.751952	7.635110
-442.591551	-27.267869	7.645107
-440.861004	-26.212953	7.655104
-439.192927	-32.562815	7.665101
-437.014471	-24.957299	7.675098
-435.276595	-28.744615	7.685094
-433.438374	-25.856356	7.695091
-431.391742	-25.028749	7.705088
-429.443369	-26.579141	7.715085
-427.514293	-23.451173	7.725082
-425.765107	-23.272382	7.735078
-424.051684	-20.539450	7.745075
-422.058217	-26.279682	7.755072
-420.231130	-23.463845	7.765069
-418.191481	-28.966709	7.775066
-416.140037	-25.228270	7.785062
-414.569761	-17.018771	7.795059
-412.951179	-16.767010	7.805056
-411.187657	-20.792092	7.815053
-408.830470	-24.923017	7.825050
-406.806562	-29.684409	7.835046
-405.129222	-27.270966	7.845043
-403.203235	-23.842484	7.855040
-401.296997	-26.129813	7.865037
-399.896487	-15.120554	7.875034
-397.813331	-19.624559	7.885030
-395.791061	-22.877783	7.895027
-393.806264	-22.217113	7.905024
-391.765361	-21.619084	7.915021
-389.965706	-24.588862	7.925018
-388.172610	-23.736526	7.935014
-386.790076	-25.884962	7.945011
-384.641240	-22.534677	7.955008
-382.700833	-23.272179	7.965005
-380.776882	-22.413887	7.975002
-378.919179	-28.198725	7.984998
-377.023799	-28.269030	7.994995
-375.023524	-22.327640	8.004992
-373.255208	-18.079744	8.014989
-371.099638	-23.365816	8.024986
-369.581099	-24.558586	8.034982
-367.815175	-23.959266	8.044979
-365.838201	-18.190987	8.054976
-363.853158	-15.987693	8.064973
-361.722766	-18.583939	8.074970
-359.992605	-21.485759	8.084966
-358.505551	-24.010869	8.094963
-356.714189	-21.113487	8.104960
-354.393978	-23.128976	8.114957
-352.633477	-21.390353	8.124954
-350.808730	-23.413579	8.134950
-348.778991	-25.815321	8.144947
-347.014218	-23.049478	8.154944
-345.161739	-23.891333	8.164941
-343.176309	-24.264936	8.174938
-341.381806	-23.349631	8.184934
-339.372575	-24.000190	8.194931
-337.644712	-24.206354	8.204928
-335.791024	-21.757855	8.214925
-333.733171	-24.550917	8.224922
-332.165345	-25.907848	8.234918
-330.348807	-23.682363	8.244915
-328.137630	-18.600390	8.254912
-326.296372	-24.199408	8.264909
-324.492700	-22.053969	8.274906
-322.599440	-16.494921	8.284902
-320.700306	-23.489496	8.294899
-318.848579	-16.477492	8.304896
-316.942621	-20.185771	8.314893
-314.947646	-24.528787	8.324890
-313.302972	-21.326901	8.334886
-311.403753	-23.322513	8.344883
-309.533369	-23.448775	8.354880
-307.631881	-23.875266	8.364877
-305.758028	-18.096789	8.374874
-304.065878	-23.858305	8.384870
-302.165012	-23.223634	8.394867
-299.991160	-24.899917	8.404864
-298.169113	-31.582166	8.414861
-296.239957	-23.196185	8.424858
-294.336904	-29.398729	8.434854
-292.489774	-23.478608	8.444851
-290.763366	-18.088689	8.454848
-289.165026	-21.806265	8.464845
-286.686605	-26.531167	8.474842
-284.950995	-32.504869	8.484838
-283.259672	-21.834060	8.494835
-281.224764	-25.567631	8.504832
-279.415320	-25.077824	8.514829
-277.719212	-27.707308	8.524826
-275.909837	-25.809060	8.534822
-274.154404	-23.425356	8.544819
-272.088211	-21.391254	8.554816
-269.596758	-18.280286	8.564813
-268.219650	-27.570984	8.574810
-266.350605	-24.742775	8.584807
-264.404987	-24.582588	8.594803
-262.595329	-21.605948	8.604800
-260.716467	-26.141968	8.614797
-258.649494	-26.203253	8.624794
-257.014970	-22.571810	8.634791
-254.860300	-23.622883	8.644787
-253.103058	-26.020527	8.654784
-251.483462	-21.840379	8.664781
-249.831742	-24.420128	8.674778
-247.471457	-22.721893	8.684775
-245.492521	-19.653836	8.694771
-244.034269	-17.240044	8.704768
-241.878919	-11.610650	8.714765
-239.881861	-14.932358	8.724762
-238.180199	-22.744836	8.734759
-236.222759	-22.622829	8.744755
-234.603739	-24.647872	8.754752
-232.558238	-22.357800	8.764749
-230.565121	-28.118355	8.774746
-228.832066	-26.645261	8.784743
-227.060006	-20.171521	8.794739
-225.171136	-25.557012	8.804736
-222.794434	-35.746169	8.814733
-220.952905	-30.912997	8.824730
-219.402824	-29.232272	8.834727
-217.524100	-32.632968	8.844723
-215.646628	-31.631336	8.854720
-213.910235	-32.456143	8.864717
-211.842238	-30.498068	8.874714
-209.954909	-35.684350	8.884711
-208.440627	-28.855248	8.894707
-206.627629	-26.082784	8.904704
-204.151867	-29.368751	8.914701
-201.911116	-28.927191	8.924698
-200.890964	-31.109272	8.934695
-198.907049	-32.066729	8.944691
-196.869789	-28.777412	8.954688
-195.206833	-31.332075	8.964685
-193.363252	-32.725029	8.974682
-191.187796	-30.430398	8.984679
-189.233618	-40.335777	8.994675
-187.687676	-28.124318	9.004672
-185.639922	-28.150894	9.014669
-183.592606	-29.930039	9.024666
-181.891879	-27.840696	9.034663
-180.018719	-34.332071	9.044659
-178.273273	-34.610401	9.054656
-176.343127	-26.303420	9.064653
-174.154982	-35.417175	9.074650
-172.392191	-34.743000	9.084647
-170.732795	-33.905481	9.094643
-168.760376	-31.553167	9.104640
-167.170344	-32.782482	9.114637
-165.202532	-30.765747	9.124634
-162.901087	-25.145385	9.134631
-161.048603	-27.022897	9.144627
-159.454780	-28.925449	9.154624
-157.850283	-22.319126	9.164621
-155.500423	-33.160788	9.174618
-153.713277	-29.567838	9.184615
-151.894504	-24.549396	9.194611
-150.099066	-26.051479	9.204608
-148.383341	-28.778743	9.214605
-146.233140	-27.782679	9.224602
-144.058271	-25.893702	9.234599
-142.372584	-26.138786	9.244595
-140.859634	-21.052589	9.254592
-138.915414	-28.313176	9.264589
-136.955166	-26.528895	9.274586
-135.091945	-31.798121	9.284583
-133.027733	-24.710920	9.294579
-131.253100	-26.358091	9.304576
-128.972334	-31.667093	9.314573
-127.644847	-25.218657	9.324570
-125.487353	-23.667945	9.334567
-123.905983	-20.853720	9.344563
-121.841082	-24.410369	9.354560
-120.061005	-29.149999	9.364557
-117.820883	-31.771437	9.374554
-116.318233	-34.082574	9.384551
-114.336442	-31.142758	9.394547
-112.784747	-22.623756	9.404544
-110.570016	-30.980647	9.414541
-108.498395	-28.375686	9.424538
-106.898543	-29.829163	9.434535
-104.705313	-28.890454	9.444531
-103.538916	-19.695755	9.454528
-101.163666	-28.095619	9.464525
-99.293436	-28.428537	9.474522
-97.449272	-26.224648	9.484519
-95.492524	-21.911862	9.494515
-93.730651	-20.733794	9.504512
-91.911465	-32.363901	9.514509
-90.033447	-31.966997	9.524506
-88.056022	-34.153337	9.534503
-86.149435	-23.928819	9.544499
-84.353944	-27.867195	9.554496
-82.730461	-26.453881	9.564493
-80.435503	-29.808776	9.574490
-78.450738	-31.798910	9.584487
-76.901251	-19.298974	9.594483
-75.041314	-24.488687	9.604480
-72.986188	-33.058507	9.614477
-71.051472	-28.121657	9.624474
-69.236872	-29.869897	9.634471
-67.680714	-27.315299	9.644467
-65.610262	-30.563311	9.654464
-63.690428	-27.586725	9.664461
-61.911391	-28.342438	9.674458
-59.893886	-24.012473	9.684455
-58.108731	-27.791286	9.694451
-56.409677	-25.671583	9.704448
-54.223680	-24.851675	9.714445
-52.166310	-28.934438	9.724442
-50.592145	-27.454813	9.734439
-48.719389	-26.839142	9.744435
-46.879195	-24.961423	9.754432
-44.844252	-29.436921	9.764429
-42.946462	-27.151543	9.774426
-41.426364	-23.779589	9.784423
-39.300783	-21.110541	9.794419
-37.373418	-21.569370	9.804416
-35.628485	-19.471181	9.814413
-33.506847	-29.196328	9.824410
-31.982150	-28.927756	9.834407
-29.854732	-33.749573	9.844403
-28.436975	-24.384928	9.854400
-26.146941	-25.035811	9.864397
-24.085306	-25.054991	9.874394
-22.451682	-21.854292	9.884391
-20.509513	-20.930721	9.894387
-18.530053	-23.406281	9.904384
-16.866890	-22.905574	9.914381
-15.161865	-21.633117	9.924378
-12.979982	-24.662017	9.934375
-10.769189	-22.080748	9.944371
-9.444343	-22.182918	9.954368
-7.896945	-7.767307	9.964365
-6.285195	0.492733	9.974362
-4.537122	31.768125	9.984359
-3.061214	73.140300	9.994355
-1.470914	117.691772	10.004352
0.000000	144.676742	10.009357
0.547580	183.698137	10.014362
1.733870	184.316427	10.019367
1.948343	211.620581	10.024371
2.416092	218.774891	10.029376
2.782062	232.234388	10.034381
2.754976	236.051923	10.039386
2.917912	235.444136	10.044391
2.920444	238.758625	10.049395
3.022077	247.220306	10.054400
3.342291	244.964731	10.059405
3.164753	246.249998	10.064410
3.131479	237.257221	10.069415
3.117473	255.768456	10.074419
3.174467	238.190446	10.079424
3.136922	246.762637	10.084429
3.001642	260.439308	10.089434
3.525490	256.555355	10.094439
3.316858	249.487638	10.099443
3.065353	242.054597	10.104448
3.550511	245.024022	10.109453
3.189726	268.816664	10.114458
3.491042	259.450380	10.119463
3.352542	269.379113	10.124467
3.742392	270.080289	10.129472
3.718311	265.646634	10.134477
3.426938	276.711521	10.139482
3.753735	275.576119	10.144487
3.904438	272.552783	10.149491
3.735300	269.738160	10.154496
3.568958	272.548153	10.159501
3.585732	276.469090	10.164506
3.970934	276.819343	10.169511
3.702206	276.990044	10.174515
3.901508	275.518582	10.179520
4.120418	278.847453	10.184525
3.873022	286.141098	10.189530
4.359102	282.786718	10.194535
4.189721	287.735575	10.199539
4.195231	291.467499	10.204544
4.657730	286.866338	10.209549
3.976074	291.471124	10.214554
4.258737	288.183882	10.219559
4.416815	299.869389	10.224563
4.171657	303.770611	10.229568
4.479099	288.823990	10.234573
4.399044	297.710502	10.239578
4.276763	297.853114	10.244583
4.309437	294.938487	10.249587
4.140486	299.235988	10.254592
4.611207	292.039390	10.259597
4.459343	301.260637	10.264602
4.911077	304.344217	10.269607
4.555904	306.070991	10.274611
4.688344	320.857786	10.279616
5.087428	318.668468	10.284621
5.370709	337.867261	10.289626
5.024823	314.427130	10.294631
4.795744	314.917943	10.299635
4.623543	317.974887	10.304640
5.149606	327.999513	10.309645
5.024754	332.037674	10.314650
5.486980	338.948494	10.319655
5.149569	329.783394	10.324659
5.356525	338.903276	10.329664
5.560120	340.790091	10.334669
5.323647	338.924498	10.339674
5.301324	341.687878	10.344679
5.341253	341.339408	10.349683
5.681030	347.661049	10.354688
5.514135	343.909327	10.359693
5.589057	350.938701	10.364698
5.814402	345.755596	10.369703
5.590967	342.623184	10.374707
5.419344	352.199282	10.379712
5.702936	338.880705	10.384717
5.334347	353.536135	10.389722
5.761842	341.580769	10.394727
5.720422	354.789965	10.399731
5.704499	342.925826	10.404736
5.624701	353.886060	10.409741
5.712025	351.984589	10.414746
6.266115	360.225932	10.419751
5.867078	358.151295	10.424755
6.196773	380.982417	10.429760
6.691135	387.280996	10.434765
6.593670	375.704232	10.439770
6.361397	363.775234	10.444775
5.967571	363.663109	10.449779
6.378496	360.795371	10.454784
6.157478	360.162088	10.459789
6.119123	373.656245	10.464794
6.743646	377.488157	10.469799
6.605668	376.761202	10.474803
6.646244	388.992236	10.479808
6.803502	385.901597	10.484813
6.822478	395.114578	10.489818
7.152127	383.507529	10.494823
6.752845	368.239881	10.499827
6.263391	366.340517	10.504832
6.838719	373.222275	10.509837
6.845293	395.062572	10.514842
6.972500	398.060738	10.519847
7.079375	399.819482	10.524851
7.000849	392.827138	10.529856
7.352756	396.800311	10.534861
7.184200	399.260590	10.539866
7.208753	390.163876	10.544871
7.026705	389.647380	10.549875
7.058855	397.388511	10.554880
7.041388	394.026112	10.559885
6.890995	396.084516	10.564890
7.437429	406.072831	10.569895
7.267629	404.253366	10.574899
7.174022	410.251491	10.579904
7.368695	393.613296	10.584909
6.704991	412.904886	10.589914
7.470109	409.562742	10.594919
7.649819	431.619911	10.599923
7.926431	438.744894	10.604928
8.088254	441.065749	10.609933
7.642859	438.963801	10.614938
7.778224	432.068212	10.619943
7.817820	430.992801	10.624947
7.895912	436.919395	10.629952
8.186526	433.922596	10.634957
7.920368	430.188261	10.639962
8.230662	434.352590	10.644967
7.940593	432.333103	10.649971
8.010412	437.235973	10.654976
8.103720	433.665081	10.659981
7.810679	448.475716	10.664986
8.313462	435.860122	10.669991
8.262122	429.585685	10.674995
8.080316	437.327847	10.680000
8.070778	434.277996	10.685005
7.866472	441.599538	10.690010
8.137712	439.607218	10.695015
8.315816	453.006998	10.700019
8.443992	466.865774	10.705024
8.662553	470.735655	10.710029
8.306803	474.553634	10.715034
8.784764	474.898559	10.720039
8.508263	476.972358	10.725043
8.537239	478.429715	10.730048
9.136544	476.113819	10.735053
8.729647	488.400540	10.740058
8.986924	482.915818	10.745063
8.535847	480.787960	10.750067
8.483567	479.635734	10.755072
9.050863	478.979212	10.760077
8.590011	486.732792	10.765082
8.934855	477.994955	10.770087
9.309000	493.888273	10.775091
9.071858	512.747671	10.780096
9.540231	498.040103	10.785101
9.350988	514.583140	10.790106
9.445240	507.120046	10.795111
9.571874	513.455256	10.800115
9.453049	500.959254	10.805120
9.633828	494.283480	10.810125
9.138319	486.750456	10.815130
9.522327	498.795914	10.820135
9.502929	509.451733	10.825139
9.699117	523.803567	10.830144
9.977797	513.009604	10.835149
10.177446	522.118941	10.840154
9.345828	498.744159	10.845159
9.362625	496.469130	10.850163
9.640620	512.597008	10.855168
9.945104	512.012367	10.860173
9.751401	519.288101	10.865178
9.696572	515.832282	10.870183
10.142511	522.793888	10.875187
10.165200	523.916351	10.880192
10.185977	521.773152	10.885197
10.085209	523.826813	10.890202
9.748021	527.865778	10.895207
9.993748	525.092170	10.900211
10.118662	526.638311	10.905216
10.604374	538.669157	10.910221
10.445660	539.770092	10.915226
10.674420	538.052624	10.920231
10.869322	519.842766	10.925235
10.610325	520.041880	10.930240
10.649844	527.713306	10.935245
10.540890	532.307244	10.940250
10.479161	519.585282	10.945255
10.488886	518.162958	10.950259
10.241211	534.489037	10.955264
11.028800	543.970615	10.960269
10.972724	564.591098	10.965274
10.883042	562.173765	10.970279
11.110085	551.965981	10.975283
11.096057	554.485220	10.980288
11.150813	546.466992	10.985293
10.915769	539.955296	10.990298
11.117225	552.490400	10.995303
11.155617	553.241342	11.000307
11.159069	561.324617	11.005312
11.394420	558.253026	11.010317
11.258629	566.528829	11.015322
11.170363	557.035253	11.020327
11.262331	564.126669	11.025331
11.078617	553.799890	11.030336
11.426299	555.562824	11.035341
11.213071	565.300244	11.040346
11.337754	558.571884	11.045351
11.411148	569.153021	11.050355
11.409170	558.346229	11.055360
11.772515	557.332715	11.060365
11.411243	562.108838	11.065370
11.782568	563.797036	11.070375
11.685855	558.471252	11.075379
11.631541	566.562166	11.080384
11.851503	578.178102	11.085389
11.820425	575.715149	11.090394
11.814472	583.257446	11.095399
11.886089	579.275225	11.100403
11.729845	585.259757	11.105408
12.661903	579.247887	11.110413
12.172015	582.902778	11.115418
11.946527	591.494111	11.120423
12.333009	576.381619	11.125427
12.344759	589.148871	11.130432
12.494288	579.289334	11.135437
12.073511	583.007322	11.140442
12.431820	580.997941	11.145447
12.292412	587.358271	11.150451
12.134037	586.708676	11.155456
12.352647	580.654478	11.160461
12.399894	584.012377	11.165466
12.566508	585.245935	11.170471
12.495237	596.840526	11.175475
12.404176	589.115201	11.180480
12.571817	602.351202	11.185485
12.457777	615.881312	11.190490
12.938291	619.777263	11.195495
13.141971	610.457868	11.200499
12.814476	623.219332	11.205504
13.266375	611.304011	11.210509
13.296443	612.341723	11.215514
13.048454	619.274492	11.220519
13.274167	622.181297	11.225523
13.059669	621.513843	11.230528
13.224231	614.763327	11.235533
13.112801	618.174930	11.240538
13.257445	630.510999	11.245543
13.597061	618.618312	11.250547
12.826711	620.714127	11.255552
13.348790	622.032921	11.260557
13.166149	621.169569	11.265562
13.266978	623.467065	11.270567
13.282530	611.984053	11.275571
13.258285	610.261199	11.280576
13.735272	623.201866	11.285581
13.472438	629.204994	11.290586
13.649371	636.994126	11.295591
13.933199	645.531063	11.300595
13.747440	649.391361	11.305600
13.967806	651.772302	11.310605
13.928642	660.327648	11.315610
13.962730	654.041066	11.320615
14.250316	649.489771	11.325619
14.016359	659.812478	11.330624
14.199586	651.903016	11.335629
14.051856	663.472007	11.340634
14.031837	660.277118	11.345639
14.079516	650.656137	11.350643
14.069880	648.986143	11.355648
14.135421	652.978254	11.360653
14.300953	658.320113	11.365658
14.224261	652.240443	11.370663
14.399990	654.459763	11.375667
14.254299	653.077985	11.380672
14.084681	657.134415	11.385677
14.301537	654.974115	11.390682
14.288729	661.807889	11.395687
14.586101	667.082989	11.400691
14.561851	681.392077	11.405696
14.969579	683.407235	11.410701
15.123886	678.639059	11.415706
15.185046	659.687870	11.420711
15.009538	648.012944	11.425715
14.973284	647.227170	11.430720
15.104036	648.564228	11.435725
15.121460	642.873265	11.440730
14.949021	652.435497	11.445735
15.138213	646.583090	11.450739
14.872584	651.886480	11.455744
15.081427	647.076498	11.460749
15.045516	655.632900	11.465754
15.158827	663.673477	11.470759
15.617828	668.129559	11.475763
15.711710	671.093672	11.480768
15.592452	651.847981	11.485773
15.011854	662.263828	11.490778
15.077673	667.069639	11.495783
15.365118	678.760051	11.500787
15.582172	677.534887	11.505792
15.858674	678.689422	11.510797
15.623916	676.661077	11.515802
15.619830	683.838838	11.520807
15.845191	672.494209	11.525811
15.390086	677.668550	11.530816
15.683353	681.771010	11.535821
15.656331	679.324739	11.540826
15.596240	681.373511	11.545831
15.968794	682.449645	11.550835
15.592998	687.026267	11.555840
15.609038	687.131049	11.560845
15.850582	706.735975	11.565850
16.429140	705.088858	11.570855
16.527073	705.614259	11.575859
16.235511	710.760950	11.580864
16.497669	701.599334	11.585869
15.923634	709.462550	11.590874
16.177901	707.326238	11.595879
16.364456	709.170087	11.600883
16.396131	712.703973	11.605888
16.369534	709.612627	11.610893
16.871520	710.579807	11.615898
16.840077	709.900499	11.620903
17.079845	706.314065	11.625907
16.749633	714.548419	11.630912
16.670635	699.634628	11.635917
16.711070	704.687361	11.640922
16.766127	701.147737	11.645927
17.026010	701.598420	11.650931
16.684393	706.156979	11.655936
16.452950	700.338524	11.660941
16.550008	702.188762	11.665946
16.994822	712.122534	11.670951
16.886471	713.330570	11.675955
16.686104	713.430444	11.680960
17.249067	707.065792	11.685965
16.764961	704.400672	11.690970
16.712663	722.992730	11.695975
17.446805	732.154939	11.700979
17.404684	734.093614	11.705984
17.592886	738.376858	11.710989
17.365085	738.131009	11.715994
17.500570	734.764637	11.720999
17.524399	732.930016	11.726003
17.360001	745.096268	11.731008
17.628616	727.387715	11.736013
17.676401	732.399860	11.741018
17.535694	741.952358	11.746023
18.083657	737.364237	11.751027
17.361267	739.483958	11.756032
17.845606	742.540357	11.761037
17.732410	739.994275	11.766042
17.539186	745.295611	11.771047
17.619490	740.482446	11.776051
17.876272	745.634734	11.781056
18.020320	741.623568	11.786061
17.841016	734.461044	11.791066
17.735148	743.000269	11.796071
18.174943	751.914534	11.801075
18.243779	765.710519	11.806080
18.573885	754.686603	11.811085
18.128716	749.722270	11.816090
18.089496	758.359687	11.821095
18.360844	771.028921	11.826099
18.219236	764.688309	11.831104
18.592388	768.566731	11.836109
18.894361	760.721852	11.841114
18.482565	761.896286	11.846119
18.816096	756.776209	11.851123
18.709104	765.785580	11.856128
18.956127	752.444072	11.861133
18.614627	754.353226	11.866138
18.532416	750.468037	11.871143
18.874428	767.014940	11.876147
18.624534	771.888488	11.881152
18.681011	760.032961	11.886157
19.081061	771.235535	11.891162
18.764405	772.481531	11.896167
19.032214	757.231655	11.901171
18.865620	766.559630	11.906176
19.038382	774.515089	11.911181
18.846113	772.202397	11.916186
18.954937	768.556405	11.921191
18.951177	764.144588	11.926195
18.931282	776.786159	11.931200
19.186125	786.111586	11.936205
19.387648	793.636671	11.941210
19.343599	798.496321	11.946215
19.616728	794.910853	11.951219
19.660236	792.844417	11.956224
19.916563	790.062760	11.961229
19.784707	792.365856	11.966234
19.769151	791.034274	11.971239
20.092105	782.222473	11.976243
19.805716	778.286260	11.981248
19.651123	773.127332	11.986253
19.826356	767.478962	11.991258
19.407145	770.020284	11.996263
19.523797	784.098833	12.001267
19.935803	793.216262	12.006272
19.799908	795.474269	12.011277
20.058796	798.673877	12.016282
19.796371	808.969690	12.021287
20.278987	797.393111	12.026291
19.740226	803.558597	12.031296
19.996130	800.185620	12.036301
19.922572	790.585461	12.041306
19.824445	805.884213	12.046311
19.970219	800.494431	12.051315
19.993867	796.467760	12.056320
20.064322	788.088909	12.061325
20.320785	802.361229	12.066330
19.827298	805.264504	12.071335
20.255365	794.977177	12.076339
19.999729	803.616022	12.081344
20.039335	807.462495	12.086349
20.433606	801.539468	12.091354
20.251316	789.034415	12.096359
20.148580	774.335655	12.101363
19.747646	763.975560	12.106368
20.034951	766.032015	12.111373
19.882416	770.081020	12.116378
19.670535	791.318061	12.121383
20.347562	792.124858	12.126387
19.987130	790.662194	12.131392
19.978487	783.787830	12.136397
20.282218	778.215161	12.141402
20.003019	776.944555	12.146407
20.175524	772.965114	12.151411
19.925191	769.871593	12.156416
20.049574	771.003087	12.161421
19.950259	764.680962	12.166426
19.609173	763.492771	12.171431
20.124663	758.810471	12.176435
19.946544	764.640863	12.181440
19.958634	765.801307	12.186445
19.919434	765.779277	12.191450
19.946253	771.740995	12.196455
19.949184	768.286943	12.201459
20.047461	768.295027	12.206464
20.206572	764.885454	12.211469
20.444577	768.910018	12.216474
19.884158	774.607415	12.221479
20.262644	767.947294	12.226483
19.914643	772.305032	12.231488
19.993389	778.483986	12.236493
20.063400	770.777030	12.241498
19.708325	767.362731	12.246503
20.036526	767.859293	12.251507
19.915613	770.838762	12.256512
20.175264	765.487603	12.261517
19.980973	772.399264	12.266522
19.979665	780.298907	12.271527
19.893588	781.038173	12.276531
20.091064	782.367755	12.281536
19.809750	780.603877	12.286541
20.260172	782.057126	12.291546
20.013030	782.755846	12.296551
20.138984	777.810802	12.301555
20.060815	783.825543	12.306560
20.050558	784.328778	12.311565
20.206144	783.794686	12.316570
20.231327	786.072733	12.321575
20.362716	779.056184	12.326579
20.155422	781.014901	12.331584
20.066665	782.117311	12.336589
20.313133	784.412106	12.341594
19.830076	766.582109	12.346599
20.129536	752.686587	12.351603
20.259855	765.782028	12.356608
19.744100	761.745201	12.361613
20.004896	749.727778	12.366618
19.702388	757.888349	12.371623
20.171673	757.878261	12.376627
20.010902	755.915378	12.381632
20.018755	756.098741	12.386637
20.062664	753.425092	12.391642
19.729560	752.470606	12.396647
19.999689	746.034367	12.401651
20.074864	755.159763	12.406656
19.940423	758.912552	12.411661
20.255853	751.639570	12.416666
20.178177	754.441820	12.421671
20.260385	751.676903	12.426675
20.133442	751.465432	12.431680
20.024265	756.387497	12.436685
20.555348	752.734087	12.441690
20.160685	758.759871	12.446695
20.075465	756.967873	12.451699
19.781933	755.224871	12.456704
20.115716	755.892438	12.461709
20.051201	757.244880	12.466714
19.839717	763.088478	12.471719
20.023644	760.293143	12.476723
20.337078	754.810402	12.481728
20.246942	755.536121	12.486733
20.431603	754.095334	12.491738
19.979836	735.697386	12.496743
20.160338	719.600420	12.501747
19.852763	728.040915	12.506752
20.096031	721.624741	12.511757
20.132613	715.260460	12.516762
19.798942	732.422894	12.521767
19.879814	729.216629	12.526771
19.980157	728.558880	12.531776
19.842756	731.867414	12.536781
20.105878	723.721233	12.541786
19.915785	730.436653	12.546791
20.114226	724.141174	12.551795
20.183207	727.856779	12.556800
19.684181	728.059484	12.561805
19.832755	727.054983	12.566810
19.925382	728.226234	12.571815
19.822212	727.744454	12.576819
19.910866	734.937412	12.581824
20.099267	752.481822	12.586829
20.117233	757.065050	12.591834
19.740466	754.467959	12.596839
20.125093	760.691163	12.601843
20.149778	753.860386	12.606848
19.935798	741.297348	12.611853
20.155108	726.802748	12.616858
19.698799	732.546605	12.621863
19.746948	746.871020	12.626867
19.967695	754.853510	12.631872
20.121494	760.725582	12.636877
20.411260	751.657307	12.641882
20.102175	745.127362	12.646887
20.321778	730.189569	12.651891
19.992187	741.169435	12.656896
19.969616	740.606988	12.661901
19.937057	730.522490	12.666906
19.771780	731.689143	12.671911
19.933536	730.434946	12.676915
19.717698	729.315095	12.681920
19.764039	737.749612	12.686925
19.942511	751.848233	12.691930
20.004122	759.334111	12.696935
20.202350	757.060068	12.701939
19.922913	749.986050	12.706944
19.855798	747.882068	12.711949
20.166262	739.504390	12.716954
19.485859	745.788642	12.721959
20.074218	747.804963	12.726963
20.255349	771.434718	12.731968
20.172602	757.267399	12.736973
20.471859	749.844026	12.741978
19.825300	740.597077	12.746983
20.073281	728.272619	12.751987
19.908812	730.680260	12.756992
19.907500	737.352957	12.761997
20.100530	738.022472	12.767002
19.660498	736.362765	12.772007
19.921413	742.654580	12.777011
19.757999	739.766408	12.782016
19.820346	737.507732	12.787021
20.227421	752.863052	12.792026
19.755714	757.283096	12.797031
20.053328	754.813421	12.802035
20.140834	761.279566	12.807040
19.726565	750.169366	12.812045
20.401511	751.662498	12.817050
19.921171	742.042092	12.822055
19.934299	737.930378	12.827059
19.866545	734.329905	12.832064
19.839250	739.691511	12.837069
20.013438	746.721015	12.842074
19.876182	771.997501	12.847079
19.934675	773.114273	12.852083
20.020680	778.155032	12.857088
20.079185	779.254455	12.862093
20.455326	758.888769	12.867098
20.163613	765.483212	12.872103
19.944457	749.667587	12.877107
20.058735	746.388177	12.882112
19.745389	738.919009	12.887117
20.018729	726.385494	12.892122
19.800226	736.699483	12.897127
20.132899	739.048333	12.902131
19.863673	747.321866	12.907136
19.825401	750.824338	12.912141
19.949191	739.295575	12.917146
19.974124	746.883496	12.922151
19.822677	744.352976	12.927155
19.838826	757.852991	12.932160
19.977411	771.983225	12.937165
20.482629	760.677474	12.942170
20.053770	769.206726	12.947175
20.204697	751.076923	12.952179
20.060617	757.106897	12.957184
20.030525	754.380392	12.962189
20.176615	750.976054	12.967194
20.152195	748.283340	12.972199
20.049428	750.889310	12.977203
20.419775	750.396662	12.982208
20.312016	750.702549	12.987213
20.179898	742.307146	12.992218
19.833844	756.043134	12.997223
20.160359	750.463686	13.002227
20.299970	753.179238	13.007232
20.089260	755.382936	13.012237
20.190949	760.083705	13.017242
20.222303	749.312456	13.022247
20.198227	741.167916	13.027251
20.115746	731.528216	13.032256
20.046280	728.054180	13.037261
20.049909	722.310190	13.042266
19.847664	733.878470	13.047271
19.930487	725.251667	13.052275
19.718185	722.472226	13.057280
19.854321	726.752732	13.062285
19.955533	724.779609	13.067290
19.814073	731.771137	13.072295
20.065772	729.838668	13.077299
19.996606	727.143634	13.082304
19.918563	729.270972	13.087309
20.093204	720.820346	13.092314
19.851138	729.855970	13.097319
19.989428	728.408389	13.102323
20.000572	729.767686	13.107328
20.009763	730.389248	13.112333
19.963261	730.335264	13.117338
19.951739	733.988014	13.122343
20.002575	738.077116	13.127347
19.990850	732.174715	13.132352
19.870313	723.490458	13.137357
20.042845	734.262494	13.142362
19.628566	744.123567	13.147367
20.180206	748.768336	13.152371
20.265291	752.740011	13.157376
19.959999	745.394140	13.162381
20.072059	738.077904	13.167386
19.924144	736.358989	13.172391
19.892987	727.849716	13.177395
20.002631	731.590377	13.182400
19.916745	736.970789	13.187405
20.019497	726.500420	13.192410
19.786934	729.765782	13.197415
19.775569	755.369105	13.202419
20.320656	756.383033	13.207424
19.846783	748.059483	13.212429
19.869828	748.645719	13.217434
19.905711	759.365447	13.222439
20.149493	757.101486	13.227443
19.888585	768.797427	13.232448
19.895870	768.607125	13.237453
20.401385	764.246551	13.242458
19.869576	763.577659	13.247463
19.867557	749.134109	13.252467
20.224646	755.167728	13.257472
19.985339	755.090878	13.262477
19.775659	752.038187	13.267482
19.678048	751.762110	13.272487
19.948430	762.200000	13.277491
20.066634	757.902780	13.282496
19.888917	761.892718	13.287501
20.034590	767.748742	13.292506
20.261817	779.474073	13.297511
20.270172	771.499393	13.302515
20.197441	756.948837	13.307520
19.982604	745.682246	13.312525
20.191360	741.015758	13.317530
19.969303	746.853151	13.322535
19.960245	741.841340	13.327539
19.936953	741.138652	13.332544
19.695314	748.292830	13.337549
20.149925	732.303524	13.342554
19.850287	748.441792	13.347559
20.080233	736.323640	13.352563
19.714677	742.627063	13.357568
19.897445	744.052032	13.362573
20.132041	737.214592	13.367578
20.002555	753.183794	13.372583
20.138108	738.625268	13.377587
20.072565	737.837852	13.382592
19.978088	750.071807	13.387597
20.184592	743.887002	13.392602
19.785064	740.027194	13.397607
20.070552	749.767199	13.402611
20.074662	749.457550	13.407616
20.138382	745.118559	13.412621
20.048188	744.699367	13.417626
19.893281	749.877894	13.422631
19.527771	751.180568	13.427635
19.785525	746.236591	13.432640
19.742207	747.524148	13.437645
20.221709	754.222672	13.442650
20.130901	755.965679	13.447655
20.121561	748.916394	13.452659
20.371902	746.575690	13.457664
20.089107	751.987514	13.462669
20.329514	743.742438	13.467674
19.898528	748.099212	13.472679
19.825190	741.864420	13.477683
20.077435	740.335581	13.482688
19.906050	745.825832	13.487693
20.337965	735.872262	13.492698
20.053995	739.365031	13.497703
20.047480	746.525863	13.502707
19.885025	747.114876	13.507712
20.037955	750.604198	13.512717
19.845032	754.211766	13.517722
19.970237	747.935842	13.522727
19.875989	749.960108	13.527731
20.449512	748.570845	13.532736
19.870844	753.566215	13.537741
20.083137	747.238553	13.542746
19.826891	756.801604	13.547751
19.767791	759.812214	13.552755
20.035853	757.739931	13.557760
19.747258	758.380603	13.562765
20.037850	743.128685	13.567770
19.974584	752.451210	13.572775
19.951749	754.752681	13.577779
20.186447	750.227138	13.582784
19.985325	761.326885	13.587789
20.070625	753.876131	13.592794
20.004937	754.541177	13.597799
19.779950	753.723995	13.602803
19.486344	758.259143	13.607808
19.853209	761.807391	13.612813
20.253666	750.207682	13.617818
19.835645	759.575754	13.622823
19.646164	754.269426	13.627827
20.331892	752.985274	13.632832
19.935292	759.481321	13.637837
20.122393	758.040145	13.642842
20.160441	755.618177	13.647847
19.890926	754.467460	13.652851
19.842172	752.896738	13.657856
19.939337	761.985513	13.662861
19.909730	747.428088	13.667866
19.737413	756.796395	13.672871
19.551772	756.767758	13.677875
20.035161	757.575474	13.682880
19.744090	763.199943	13.687885
20.060601	765.382634	13.692890
20.031361	774.923683	13.697895
20.314378	772.382212	13.702899
20.241933	768.492306	13.707904
19.705615	766.027899	13.712909
20.057358	756.739991	13.717914
20.347797	754.047522	13.722919
20.115111	756.265765	13.727923
20.312829	755.996203	13.732928
20.116678	765.727878	13.737933
20.156374	753.411388	13.742938
19.766382	756.060016	13.747943
20.127012	760.427734	13.752947
20.426898	760.679642	13.757952
20.238960	759.198931	13.762957
20.420087	763.111133	13.767962
20.002400	762.110210	13.772967
19.893252	748.497493	13.777971
20.032099	748.671002	13.782976
19.950483	754.978030	13.787981
19.975760	755.880892	13.792986
19.859828	756.244856	13.797991
20.007531	761.490244	13.802995
20.224078	756.114423	13.808000
20.189570	753.913773	13.813005
20.138496	733.668303	13.818010
19.739745	734.794920	13.823015
19.975352	728.892497	13.828019
19.834287	730.354922	13.833024
19.562409	732.786002	13.838029
19.810185	749.123978	13.843034
19.861037	759.350865	13.848039
20.185933	768.553139	13.853043
20.273110	771.819554	13.858048
19.809726	772.257860	13.863053
20.038608	759.285110	13.868058
20.149457	768.597221	13.873063
19.800400	773.322575	13.878067
20.105869	768.814125	13.883072
19.925276	768.532359	13.888077
19.949202	770.249183	13.893082
19.892084	773.953372	13.898087
20.197507	769.514318	13.903091
20.414282	761.328198	13.908096
20.059664	759.686405	13.913101
19.925710	738.047441	13.918106
19.984822	739.459015	13.923111
19.725351	740.348943	13.928115
19.659567	749.788567	13.933120
19.670885	768.143445	13.938125
20.078706	763.875726	13.943130
20.338638	769.193108	13.948135
19.981345	775.302829	13.953139
20.333723	758.889810	13.958144
19.572454	752.102387	13.963149
19.999023	753.944231	13.968154
20.161818	767.141732	13.973159
19.945557	774.058474	13.978163
20.046471	758.977148	13.983168
19.894866	754.221469	13.988173
19.999879	747.720097	13.993178
19.940706	761.935482	13.998183
19.969362	763.881797	14.003187
20.201063	761.430518	14.008192
19.879214	753.055453	14.013210
19.890647	756.394790	14.018227
20.025522	755.906200	14.023245
19.587578	767.548738	14.028263
20.284658	767.324404	14.033280
20.129680	770.740622	14.038298
20.398896	773.272795	14.043315
20.328987	767.064392	14.048333
19.954691	759.732654	14.053351
19.994807	757.728646	14.058368
19.918137	772.830800	14.063386
20.253613	770.875635	14.068403
20.220332	775.567027	14.073421
20.165066	776.683341	14.078439
20.506150	776.067480	14.083456
20.223699	783.271380	14.088474
20.369745	775.694621	14.093491
20.216537	780.117283	14.098509
20.526770	770.916165	14.103527
20.627719	749.287110	14.108544
20.423939	751.641467	14.113562
20.171378	746.755213	14.118579
20.269743	751.172346	14.123597
20.185062	746.443357	14.128615
20.327683	750.203782	14.133632
20.297619	767.234862	14.138650
20.365003	773.100962	14.143667
20.599998	777.071600	14.148685
20.333963	780.304190	14.153703
20.775119	773.155410	14.158720
20.597562	777.583528	14.163738
20.432787	777.399130	14.168755
20.600359	772.864276	14.173773
20.071958	778.930795	14.178791
20.170804	778.930864	14.183808
20.119490	788.812907	14.188826
20.396243	783.615704	14.193843
20.263653	780.160614	14.198861
20.363884	782.980860	14.203879
20.855226	793.240391	14.208896
20.749736	802.825921	14.213914
20.899096	806.212483	14.218931
20.659757	794.816572	14.223949
20.469050	800.725420	14.228967
20.662630	801.050149	14.233984
20.582743	806.271222	14.239002
20.756501	799.742373	14.244019
20.846755	799.235731	14.249037
20.947032	809.364167	14.254055
20.984476	805.263759	14.259072
20.708309	816.468405	14.264090
20.902363	812.387061	14.269107
21.200696	801.545602	14.274125
21.021311	808.740940	14.279143
21.062478	811.293763	14.284160
21.099401	807.981514	14.289178
20.782289	804.991573	14.294195
21.111418	802.820341	14.299213
20.851221	809.501612	14.304231
21.225270	806.895356	14.309248
21.086182	809.596477	14.314266
21.047846	810.879978	14.319283
20.961573	809.792737	14.324301
20.691920	813.587475	14.329319
20.928704	805.013098	14.334336
21.193174	809.820603	14.339354
20.898910	806.639829	14.344371
20.910589	802.228930	14.349389
20.523184	817.215526	14.354407
20.957426	815.625270	14.359424
21.109375	829.844740	14.364442
21.378684	851.912141	14.369459
21.744042	841.574337	14.374477
21.458128	836.806629	14.379495
21.418702	820.068328	14.384512
21.200698	824.299992	14.389530
21.251610	830.532107	14.394547
21.745695	819.425034	14.399565
21.092256	823.122113	14.404583
21.337395	831.398050	14.409600
21.753968	839.369798	14.414618
21.255582	834.379578	14.419635
21.710695	838.057152	14.424653
21.360675	840.659788	14.429671
21.850484	836.034194	14.434688
21.344432	816.836201	14.439706
21.334623	824.081578	14.444723
21.660478	836.708173	14.449741
21.637940	843.565483	14.454759
21.931776	830.933059	14.459776
21.777664	828.115314	14.464794
21.620097	812.089563	14.469811
21.566886	807.632384	14.474829
21.663723	825.432942	14.479847
21.819196	828.165735	14.484864
21.656556	840.730249	14.489882
21.530410	848.412614	14.494899
21.605668	834.970342	14.499917
21.603568	842.831118	14.504935
21.578683	839.719056	14.509952
21.579393	833.485204	14.514970
21.594147	852.695720	14.519987
21.867485	833.003738	14.525005
21.674182	839.153687	14.530023
21.846352	843.639300	14.535040
21.544252	843.722195	14.540058
22.040588	843.962456	14.545075
22.158068	847.701749	14.550093
21.777748	849.488107	14.555111
21.938466	843.044688	14.560128
22.254563	832.341944	14.565146
21.672288	845.020582	14.570163
22.174861	848.107001	14.575181
22.227506	857.862400	14.580199
22.088693	849.078918	14.585216
22.192953	844.566724	14.590234
22.246574	847.924522	14.595251
22.538030	835.210677	14.600269
21.995739	850.014373	14.605287
22.123503	851.696098	14.610304
22.299403	844.383527	14.615322
22.186227	845.940088	14.620339
22.230859	844.473319	14.625357
22.141293	839.765527	14.630375
22.140451	848.179806	14.635392
22.042323	855.215917	14.640410
22.109323	864.122749	14.645427
22.334099	862.679155	14.650445
22.459679	868.900950	14.655463
22.876116	874.623328	14.660480
22.847243	867.716211	14.665498
22.534177	854.900568	14.670515
22.417414	836.069892	14.675533
22.341556	836.414001	14.680551
22.098701	845.096538	14.685568
22.128033	859.434694	14.690586
22.515853	872.856821	14.695603
22.535780	863.327571	14.700621
22.479763	876.645887	14.705639
22.451457	877.487350	14.710656
22.859819	865.934594	14.715674
22.399757	877.876474	14.720691
22.519910	878.794931	14.725709
22.648777	876.347319	14.730727
22.667261	871.463409	14.735744
22.866743	873.915487	14.740762
22.869881	875.069684	14.745779
23.062482	864.586386	14.750797
22.962253	872.346427	14.755815
23.112505	865.778826	14.760832
23.161138	853.331782	14.765850
22.781446	871.376713	14.770867
22.926652	865.075757	14.775885
23.198820	870.522272	14.780903
23.038467	868.551796	14.785920
23.110653	858.536018	14.790938
22.697648	852.050395	14.795955
23.014475	851.310987	14.800973
22.963187	863.610797	14.805991
23.175255	865.439526	14.811008
23.325744	858.513243	14.816026
23.019962	843.266143	14.821043
22.796987	837.810428	14.826061
23.002521	849.537587	14.831079
22.844071	860.670009	14.836096
23.227802	860.616774	14.841114
23.170704	863.276514	14.846131
23.177312	848.105425	14.851149
23.183439	866.862736	14.856167
22.961535	867.160927	14.861184
23.236781	866.714438	14.866202
23.146174	868.501781	14.871219
22.719294	864.594964	14.876237
22.915328	868.584426	14.881255
23.060073	867.900778	14.886272
23.048446	854.538412	14.891290
23.044134	873.127511	14.896307
23.670661	874.081606	14.901325
23.355230	877.142772	14.906343
23.344444	878.489524	14.911360
23.521715	881.398175	14.916378
23.559843	895.934738	14.921395
23.358672	879.574521	14.926413
23.750340	892.089995	14.931431
23.537266	887.615818	14.936448
23.778650	872.076925	14.941466
23.524508	857.280894	14.946483
23.348535	861.762267	14.951501
23.687400	878.047227	14.956519
23.687875	885.695259	14.961536
23.566007	875.826823	14.966554
23.785808	883.153583	14.971571
24.341186	876.332600	14.976589
24.065477	873.307725	14.981607
23.878314	866.462034	14.986624
23.800294	865.162688	14.991642
23.557106	862.050833	14.996659
24.058270	858.675540	15.001677
24.096491	866.923152	15.006695
23.642307	871.183061	15.011712
23.823225	853.810258	15.016730
23.754495	869.175512	15.021747
23.682131	859.307057	15.026765
23.840388	861.514026	15.031783
23.781481	859.536809	15.036800
23.860184	861.780062	15.041818
23.984931	865.576402	15.046835
24.237762	874.502365	15.051853
24.119205	866.994502	15.056871
23.786117	868.526366	15.061888
24.110512	868.619448	15.066906
24.231180	893.351711	15.071923
24.313746	889.742730	15.076941
24.201045	864.754582	15.081959
23.949961	871.144992	15.086976
24.475952	883.028705	15.091994
24.068063	886.000800	15.097011
23.978899	888.060047	15.102029
24.469100	885.312557	15.107047
24.231691	893.116511	15.112064
24.331911	894.728703	15.117082
24.331904	887.120125	15.122099
24.296116	891.920493	15.127117
24.572350	894.899878	15.132135
24.189056	893.803375	15.137152
24.759821	885.804889	15.142170
24.380229	895.083415	15.147187
24.459756	885.012965	15.152205
24.547476	893.268428	15.157223
24.257585	895.746653	15.162240
24.502458	889.679899	15.167258
24.502450	890.682017	15.172275
24.427663	888.172503	15.177293
24.451706	890.850766	15.182311
24.788011	879.048372	15.187328
24.624744	883.949293	15.192346
24.490004	882.517421	15.197363
24.648726	884.021181	15.202381
24.547923	887.730806	15.207399
24.622639	884.948911	15.212416
25.030450	880.388291	15.217434
24.954549	888.174347	15.222451
24.760621	887.887633	15.227469
24.857101	882.870157	15.232487
24.833681	881.227049	15.237504
24.878211	883.604743	15.242522
24.843257	878.534300	15.247539
24.648160	880.018987	15.252557
25.003498	882.416322	15.257575
24.694094	888.636718	15.262592
24.633945	886.080825	15.267610
24.923726	884.519896	15.272627
24.601997	887.281622	15.277645
25.043067	880.283814	15.282663
24.847205	885.386561	15.287680
25.134732	900.765813	15.292698
25.443022	908.051731	15.297715
25.156892	893.762558	15.302733
25.476683	882.390656	15.307751
25.088236	895.247634	15.312768
24.726110	890.358356	15.317786
24.902806	897.830425	15.322803
25.049939	910.746712	15.327821
25.331537	908.059230	15.332839
25.301394	917.831019	15.337856
25.604640	918.004553	15.342874
25.583676	908.950555	15.347891
25.226718	924.509702	15.352909
25.348500	911.896785	15.357927
25.494865	921.059980	15.362944
25.465032	919.295195	15.367962
25.612667	911.777886	15.372979
25.451783	911.838257	15.377997
25.608409	906.683765	15.383015
25.544573	917.091708	15.388032
25.184264	910.676305	15.393050
25.522843	911.416782	15.398067
25.391500	914.671963	15.403085
25.796249	911.066645	15.408103
25.535766	923.086841	15.413120
25.573388	919.945915	15.418138
25.904445	914.870564	15.423155
25.829200	922.890915	15.428173
25.800807	907.877929	15.433191
25.721032	916.613149	15.438208
25.798593	911.982497	15.443226
25.721606	918.952346	15.448243
25.311079	919.766685	15.453261
26.074618	917.260310	15.458279
25.765119	918.703474	15.463296
25.648568	915.530510	15.468314
25.882962	914.278858	15.473331
25.366306	916.042924	15.478349
25.590717	917.619581	15.483367
25.666260	920.964462	15.488384
26.038599	936.954714	15.493402
26.000191	939.575307	15.498419
25.782801	942.864667	15.503437
26.017077	943.020887	15.508455
26.254982	941.367552	15.513472
25.977698	945.643313	15.518490
26.204961	933.062317	15.523507
26.100711	944.451999	15.528525
26.696790	933.769019	15.533543
26.362153	941.327384	15.538560
26.542900	945.122678	15.543578
26.624881	939.942328	15.548595
26.245218	933.336519	15.553613
26.276522	915.177400	15.558631
26.190209	920.292574	15.563648
26.160067	921.456802	15.568666
26.617919	935.764439	15.573683
26.366911	940.803642	15.578701
26.485923	945.915965	15.583719
26.372427	943.031944	15.588736
26.335626	939.530078	15.593754
26.507499	948.163832	15.598771
26.251691	951.868308	15.603789
26.419485	943.319010	15.608807
26.734874	943.542517	15.613824
26.601841	939.519599	15.618842
26.645330	939.786473	15.623859
26.614602	944.296614	15.628877
26.682726	935.519400	15.633895
26.645068	940.692888	15.638912
26.438676	948.219791	15.643930
26.509111	947.008444	15.648947
26.617625	952.040646	15.653965
26.996162	946.348952	15.658983
26.879943	948.819936	15.664000
26.648146	945.654335	15.669018
26.882572	950.504433	15.674035
26.630874	954.129602	15.679053
26.653747	947.514641	15.684071
26.696756	950.968536	15.689088
26.892971	969.447124	15.694106
27.490098	973.166577	15.699123
27.017188	966.432480	15.704141
27.110620	948.821834	15.709159
26.855386	949.196127	15.714176
26.831469	964.290067	15.719194
27.191941	971.213764	15.724211
26.860316	977.895492	15.729229
27.162926	974.117686	15.734247
26.801690	983.857384	15.739264
26.871154	975.509368	15.744282
27.258593	973.544316	15.749299
27.173386	974.523848	15.754317
27.215098	977.484027	15.759335
27.282871	974.157383	15.764352
26.966367	982.519839	15.769370
27.241567	976.006192	15.774387
26.930823	980.561006	15.779405
27.711717	1003.416927	15.784423
27.718748	992.524260	15.789440
27.358497	979.865469	15.794458
27.508277	970.331169	15.799475
27.458214	970.935434	15.804493
27.463107	979.267077	15.809511
28.003560	984.014894	15.814528
27.920932	982.316723	15.819546
27.609963	971.223107	15.824563
27.454681	973.857627	15.829581
27.547574	971.820004	15.834599
27.597347	971.173522	15.839616
27.441498	990.652104	15.844634
28.180320	985.036640	15.849651
27.972441	976.369489	15.854669
27.886314	973.824016	15.859687
28.053117	961.861400	15.864704
27.838908	962.784428	15.869722
27.980584	964.300354	15.874739
27.809435	971.300977	15.879757
27.816015	967.240053	15.884775
27.901405	960.583653	15.889792
27.843916	969.982313	15.894810
28.099191	978.904805	15.899827
28.033434	992.221634	15.904845
28.332378	989.084632	15.909863
28.034748	976.223948	15.914880
28.218830	971.282132	15.919898
27.805198	965.723069	15.924915
27.769349	989.058445	15.929933
28.247521	998.409441	15.934951
28.147459	993.613610	15.939968
28.361658	1005.751648	15.944986
28.793324	984.738032	15.950003
28.554846	995.379952	15.955021
28.368696	977.151618	15.960039
28.558504	959.844910	15.965056
28.162964	963.762011	15.970074
28.353062	970.607489	15.975091
28.403193	960.812236	15.980109
28.442412	963.860899	15.985127
28.253074	963.990302	15.990144
28.401296	980.181515	15.995162
28.866527	985.779753	16.000179
28.452984	981.312351	16.005197
28.435333	985.681993	16.010215
28.510604	989.440639	16.015232
28.496879	1000.159974	16.020250
28.615362	998.697140	16.025267
28.455039	994.212942	16.030285
28.983040	1001.847685	16.035303
28.918045	996.794576	16.040320
28.363202	1007.216402	16.045338
28.902538	992.757721	16.050355
29.004525	996.615927	16.055373
28.962236	996.509518	16.060391
28.884764	994.374795	16.065408
28.666782	996.094379	16.070426
28.687847	997.138761	16.075443
28.817222	1006.226068	16.080461
29.087463	988.786948	16.085479
29.395944	997.026136	16.090496
28.967783	996.260824	16.095514
29.238694	995.022218	16.100531
29.018814	992.238525	16.105549
28.893447	999.961745	16.110567
29.298733	994.327115	16.115584
28.890292	1001.801327	16.120602
29.273131	990.829846	16.125619
29.075424	987.652507	16.130637
28.944053	1000.781608	16.135655
29.157057	997.516738	16.140672
28.883245	998.980958	16.145690
29.177348	1004.411442	16.150707
29.159810	1001.232105	16.155725
28.968278	1013.291715	16.160743
29.349548	1014.535051	16.165760
29.462206	1021.899420	16.170778
29.508397	1022.993279	16.175795
29.814757	1017.232846	16.180813
29.782518	1015.422814	16.185831
29.812028	1004.900934	16.190848
29.501308	1000.802518	16.195866
29.491431	989.704910	16.200883
29.696882	1001.573778	16.205901
29.618470	1002.092904	16.210919
29.140152	999.853798	16.215936
29.442949	1003.178182	16.220954
29.708109	1009.424967	16.225971
29.867879	1017.958447	16.230989
29.827288	1021.427266	16.236007
30.142430	1007.279609	16.241024
30.103860	1021.210329	16.246042
29.994235	1014.916919	16.251059
30.039361	1011.475900	16.256077
29.583958	996.647332	16.261095
29.839781	1005.975595	16.266112
30.018899	1011.017006	16.271130
29.805104	1011.309186	16.276147
30.074621	1017.103819	16.281165
29.865547	1024.999279	16.286183
30.180615	1010.963315	16.291200
30.010642	1007.570762	16.296218
30.079802	1019.360709	16.301235
30.104880	1014.323115	16.306253
29.497526	1018.223676	16.311271
30.046113	1010.659671	16.316288
29.864203	1016.746528	16.321306
29.913846	1022.447244	16.326323
30.385938	1027.495416	16.331341
30.308168	1049.174880	16.336359
30.536097	1042.973912	16.341376
30.128269	1039.677490	16.346394
30.272195	1036.557337	16.351411
30.688763	1045.806504	16.356429
30.475231	1044.468980	16.361447
30.539998	1035.862128	16.366464
30.606432	1048.092982	16.371482
30.433750	1045.116133	16.376499
31.095634	1044.197413	16.381517
30.585739	1038.147158	16.386535
30.800494	1021.166736	16.391552
30.651363	1014.475357	16.396570
30.348621	1029.027094	16.401587
30.972652	1021.518691	16.406605
30.691414	1040.377115	16.411623
30.838883	1040.498418	16.416640
30.621008	1038.362486	16.421658
30.907698	1034.126306	16.426675
31.020941	1030.770374	16.431693
30.702073	1047.619756	16.436711
30.925378	1038.589639	16.441728
30.882146	1039.908548	16.446746
30.604639	1048.197182	16.451763
30.983801	1039.113891	16.456781
30.821561	1043.678073	16.461799
30.780346	1037.022955	16.466816
30.760145	1044.027852	16.471834
31.047711	1044.612878	16.476851
31.171924	1038.161038	16.481869
30.978683	1044.197803	16.486887
31.015691	1048.138747	16.491904
31.130479	1058.427066	16.496922
31.028425	1064.024577	16.501939
31.772990	1053.424795	16.506957
31.599201	1066.878473	16.511975
31.463445	1042.381337	16.516992
31.423553	1039.869378	16.522010
31.581446	1031.576439	16.527027
31.415991	1028.713272	16.532045
31.196537	1033.887474	16.537063
31.655235	1032.183184	16.542080
31.445880	1030.662523	16.547098
31.501441	1028.627701	16.552115
31.758326	1035.121210	16.557133
31.547269	1049.705535	16.562151
31.839253	1050.977273	16.567168
31.411707	1030.822652	16.572186
31.788681	1047.192961	16.577203
32.235771	1047.095017	16.582221
31.408325	1043.834058	16.587239
31.927264	1040.624205	16.592256
31.597374	1033.591984	16.597274
31.954425	1061.703461	16.602291
32.387138	1051.417689	16.607309
31.818139	1043.917082	16.612327
32.012396	1033.401938	16.617344
31.720629	1038.699361	16.622362
31.833655	1059.036500	16.627379
32.146980	1052.567075	16.632397
31.938346	1064.709680	16.637415
32.179377	1050.957621	16.642432
32.350344	1062.205972	16.647450
31.959571	1067.490881	16.652467
32.165929	1052.168169	16.657485
32.099071	1052.394442	16.662503
32.195984	1051.647629	16.667520
32.393191	1055.109990	16.672538
32.126097	1059.912697	16.677555
32.432380	1055.506645	16.682573
32.072165	1066.136571	16.687591
32.135741	1056.877087	16.692608
32.380219	1061.266293	16.697626
32.256263	1064.386620	16.702643
32.474882	1056.310499	16.707661
32.314024	1057.549069	16.712679
32.505286	1060.180244	16.717696
32.521822	1052.101750	16.722714
32.651028	1057.763048	16.727731
32.852176	1054.025001	16.732749
32.686991	1055.668530	16.737767
32.508740	1058.665381	16.742784
32.667521	1057.634991	16.747802
32.276062	1068.877095	16.752819
32.689771	1067.711663	16.757837
33.001567	1084.466794	16.762855
33.195958	1079.900826	16.767872
33.202709	1063.282295	16.772890
33.019141	1060.807404	16.777907
33.088204	1054.301431	16.782925
32.827126	1064.742512	16.787943
32.889108	1057.897891	16.792960
33.137147	1049.516632	16.797978
32.674071	1067.203868	16.802995
32.688368	1056.368196	16.808013
33.073683	1077.321035	16.813031
33.380285	1085.961698	16.818048
33.012806	1084.230295	16.823066
33.024482	1090.893501	16.828083
33.287415	1086.997725	16.833101
33.066784	1092.721125	16.838119
33.256795	1086.183264	16.843136
33.552411	1083.188346	16.848154
33.370109	1094.779359	16.853171
33.705096	1083.777687	16.858189
33.503022	1089.666442	16.863207
33.646818	1090.437996	16.868224
33.641910	1086.566063	16.873242
33.354843	1095.804790	16.878259
33.800041	1078.905525	16.883277
33.509533	1087.207265	16.888295
33.969969	1090.261134	16.893312
33.753241	1065.474849	16.898330
33.057178	1064.804171	16.903347
33.591164	1070.775298	16.908365
33.485825	1078.888624	16.913383
33.516529	1088.693296	16.918400
33.901203	1083.568438	16.923418
33.655781	1096.108622	16.928435
33.957623	1083.680771	16.933453
33.742246	1083.900845	16.938471
33.639342	1082.176008	16.943488
33.950655	1077.531618	16.948506
33.954811	1083.291523	16.953523
33.715542	1080.361466	16.958541
33.908762	1084.949193	16.963559
33.480684	1092.643662	16.968576
33.953039	1094.852482	16.973594
34.387101	1102.208104	16.978611
34.245369	1099.056418	16.983629
34.090499	1103.515622	16.988647
34.266805	1112.826749	16.993664
34.358612	1105.061839	16.998682
34.035779	1107.002654	17.003699
34.478513	1103.679099	17.008717
34.519919	1108.335091	17.013735
34.395147	1109.000041	17.018752
34.716006	1104.651425	17.023770
34.265573	1110.551484	17.028787
34.076520	1107.777009	17.033805
34.117334	1101.033273	17.038823
34.169302	1117.969883	17.043840
34.488097	1101.992105	17.048858
34.202464	1116.432660	17.053875
34.340711	1129.301795	17.058893
34.549586	1129.845892	17.063911
34.811562	1134.784468	17.068928
34.828878	1135.360690	17.073946
34.600019	1142.480712	17.078963
34.862743	1132.758403	17.083981
34.967158	1135.405016	17.088999
35.158994	1134.713846	17.094016
35.295461	1118.308947	17.099034
35.084222	1127.013350	17.104051
35.234551	1120.348094	17.109069
35.173752	1121.229360	17.114087
34.884221	1098.534192	17.119104
34.788223	1096.182182	17.124122
34.816304	1118.568466	17.129139
35.189804	1119.311251	17.134157
35.338600	1123.577309	17.139175
35.287355	1123.510081	17.144192
35.550009	1113.896335	17.149210
35.289368	1126.129084	17.154227
35.173069	1131.170462	17.159245
35.573028	1118.879518	17.164263
35.183774	1118.158330	17.169280
35.481086	1121.206761	17.174298
35.352136	1115.904259	17.179315
35.244089	1117.049466	17.184333
35.468620	1112.321378	17.189351
35.021155	1119.869515	17.194368
35.241255	1116.933826	17.199386
35.507167	1115.909941	17.204403
35.457713	1116.817713	17.209421
35.603293	1116.119763	17.214439
35.353743	1123.843978	17.219456
35.777893	1137.616066	17.224474
35.810742	1146.630767	17.229491
35.992273	1151.717461	17.234509
35.922451	1146.594282	17.239527
36.033149	1149.559224	17.244544
36.195115	1132.642148	17.249562
36.088251	1122.157663	17.254579
35.904028	1121.899283	17.259597
35.739025	1118.342314	17.264615
35.907175	1130.176339	17.269632
36.119157	1135.855927	17.274650
36.326208	1147.774998	17.279667
36.012095	1152.484560	17.284685
36.273809	1138.148667	17.289703
35.852460	1151.621458	17.294720
36.276837	1150.295442	17.299738
36.411350	1145.462148	17.304755
36.179500	1150.959269	17.309773
36.026096	1149.503604	17.314791
35.973427	1152.823369	17.319808
36.345738	1145.535951	17.324826
36.407628	1148.670701	17.329843
36.306146	1139.868503	17.334861
36.759326	1136.713163	17.339879
36.270555	1146.583422	17.344896
36.791076	1136.085383	17.349914
36.254736	1146.707278	17.354931
36.266214	1146.291841	17.359949
36.651992	1157.951178	17.364967
36.978297	1172.413741	17.369984
36.919745	1166.200209	17.375002
36.642541	1153.104871	17.380019
36.296668	1166.582941	17.385037
36.825065	1171.205328	17.390055
36.591131	1181.090022	17.395072
36.951201	1177.594015	17.400090
37.019926	1174.062677	17.405107
36.750335	1181.404722	17.410125
36.815405	1169.884457	17.415143
36.865190	1176.602972	17.420160
37.148738	1174.687499	17.425178
37.172797	1174.885116	17.430195
37.241352	1170.381663	17.435213
37.695462	1170.741929	17.440231
37.258386	1172.375351	17.445248
37.306198	1182.084548	17.450266
37.460643	1187.633332	17.455283
37.254013	1186.889305	17.460301
37.417760	1170.964495	17.465319
37.420649	1176.185083	17.470336
37.308102	1166.931596	17.475354
37.304935	1171.489323	17.480371
37.221974	1172.745366	17.485389
37.542382	1181.387031	17.490407
37.437310	1180.483660	17.495424
37.461437	1178.118771	17.500442
37.608847	1183.259683	17.505459
37.695771	1195.194806	17.510477
38.069273	1204.554767	17.515495
37.863308	1200.342056	17.520512
37.936789	1190.833938	17.525530
37.849409	1186.489059	17.530547
37.652381	1194.560443	17.535565
38.226181	1199.263688	17.540583
38.077936	1191.217690	17.545600
38.173427	1190.172217	17.550618
37.801415	1179.302109	17.555635
37.760592	1197.875425	17.560653
37.965860	1202.662618	17.565671
38.125645	1197.661679	17.570688
37.880209	1199.146561	17.575706
38.181186	1194.190746	17.580723
38.227852	1209.325593	17.585741
38.281613	1201.412541	17.590759
38.156647	1198.676592	17.595776
38.389079	1205.348687	17.600794
38.450089	1202.439928	17.605811
37.928830	1209.877182	17.610829
38.185584	1200.602526	17.615847
38.328801	1193.650503	17.620864
38.073115	1200.826742	17.625882
38.256719	1208.925518	17.630899
38.188023	1219.310856	17.635917
38.582037	1225.878537	17.640935
38.663130	1224.514455	17.645952
38.738039	1223.911144	17.650970
39.088217	1221.885936	17.655987
39.065514	1228.988851	17.661005
38.994689	1229.072611	17.666023
38.925217	1230.795278	17.671040
39.126365	1222.152407	17.676058
39.031154	1224.750649	17.681075
38.777260	1225.519571	17.686093
38.992303	1221.648701	17.691111
39.142971	1225.543250	17.696128
38.824334	1223.569655	17.701146
39.138790	1219.100901	17.706163
38.781620	1227.550208	17.711181
39.056389	1225.415901	17.716199
39.110814	1227.565554	17.721216
39.109572	1223.057486	17.726234
39.331255	1225.112822	17.731251
38.829728	1226.012475	17.736269
39.325549	1229.589277	17.741287
38.946107	1223.823309	17.746304
38.904853	1230.749854	17.751322
39.436868	1239.744777	17.756339
39.364345	1248.549827	17.761357
39.397735	1248.137184	17.766375
39.309161	1250.517291	17.771392
39.510714	1254.789132	17.776410
39.709975	1242.858862	17.781427
39.282442	1260.767182	17.786445
39.369189	1247.146514	17.791463
39.597606	1253.756349	17.796480
39.600196	1268.037826	17.801498
40.288643	1272.441234	17.806515
40.277512	1269.389807	17.811533
40.500157	1256.463197	17.816551
40.025296	1248.927017	17.821568
40.067379	1243.952700	17.826586
40.147693	1240.079718	17.831603
40.416168	1249.945679	17.836621
40.506248	1241.114441	17.841639
40.313305	1242.990511	17.846656
40.006183	1246.929764	17.851674
40.269609	1244.768949	17.856691
40.395045	1243.855552	17.861709
40.140532	1245.558967	17.866727
40.350834	1248.874566	17.871744
40.111255	1242.707177	17.876762
40.284807	1243.905011	17.881779
39.957205	1253.051200	17.886797
40.091866	1247.997621	17.891815
40.621890	1262.476549	17.896832
40.033950	1281.160826	17.901850
40.687644	1277.965612	17.906867
40.651340	1281.081444	17.911885
40.852331	1275.139509	17.916903
41.059211	1282.411905	17.921920
41.086713	1276.164151	17.926938
41.060433	1257.942999	17.931955
40.707585	1243.849740	17.936973
40.906559	1232.356833	17.941991
41.043573	1238.496739	17.947008
40.478387	1241.149491	17.952026
40.792101	1256.255954	17.957043
40.762880	1269.546760	17.962061
40.695596	1270.411766	17.967079
41.046165	1273.950397	17.972096
41.198329	1279.271486	17.977114
41.404418	1268.066860	17.982131
41.204382	1272.080278	17.987149
41.085995	1271.669818	17.992167
41.165196	1273.173719	17.997184
41.154847	1280.005695	18.002202
41.214462	1275.522512	18.007219
41.071717	1271.434980	18.012237
41.354379	1279.483390	18.017255
41.520702	1287.948343	18.022272
41.418416	1302.493550	18.027290
41.811315	1291.089222	18.032307
41.543699	1292.966196	18.037325
41.579038	1293.291007	18.042343
41.798887	1296.900830	18.047360
41.734020	1303.941291	18.052378
41.700668	1301.355882	18.057395
41.643188	1303.351930	18.062413
41.916188	1298.987294	18.067431
42.206784	1298.706665	18.072448
41.772782	1295.659754	18.077466
42.204959	1293.612020	18.082483
42.005954	1297.291792	18.087501
41.867206	1290.836160	18.092519
41.750078	1288.517378	18.097536
41.621031	1296.878430	18.102554
42.054639	1284.053433	18.107571
41.957554	1293.177039	18.112589
41.960485	1293.415781	18.117607
42.248165	1297.552772	18.122624
42.136309	1322.908033	18.127642
42.510252	1310.713888	18.132659
42.645296	1316.152556	18.137677
42.605989	1318.899205	18.142695
42.328038	1308.146136	18.147712
42.387602	1322.188912	18.152730
42.587327	1318.169446	18.157747
42.606062	1322.745750	18.162765
42.543113	1319.501225	18.167783
42.706221	1311.934052	18.172800
42.672531	1317.237605	18.177818
42.711035	1318.916319	18.182835
42.516402	1323.347324	18.187853
42.310280	1321.822969	18.192871
42.773586	1318.113831	18.197888
42.410986	1324.937513	18.202906
42.493564	1322.556986	18.207923
42.735244	1328.755744	18.212941
42.703389	1343.576057	18.217959
43.269623	1345.018020	18.222976
43.010780	1356.964376	18.227994
43.450847	1349.115478	18.233011
43.568772	1347.289321	18.238029
43.305828	1342.082040	18.243047
43.945830	1331.371319	18.248064
43.409189	1327.648622	18.253082
43.602340	1307.765862	18.258099
43.318893	1307.797015	18.263117
43.403862	1314.091549	18.268135
43.396918	1310.845959	18.273152
43.457632	1320.685328	18.278170
44.031361	1329.223758	18.283187
43.637656	1314.304795	18.288205
43.464407	1312.160131	18.293223
43.825584	1321.772251	18.298240
43.793623	1333.064189	18.303258
43.687794	1330.839554	18.308275
43.848920	1338.573891	18.313293
43.942283	1345.678801	18.318311
43.991603	1334.659579	18.323328
43.733985	1339.827390	18.328346
43.939388	1340.735428	18.333363
44.087402	1331.444999	18.338381
44.213477	1340.636866	18.343399
43.922886	1330.584237	18.348416
43.916951	1341.794951	18.353434
43.978277	1335.952347	18.358451
44.310939	1337.120094	18.363469
44.070282	1337.495216	18.368487
44.126712	1326.772176	18.373504
43.737552	1335.709578	18.378522
44.139867	1354.320960	18.383539
44.428026	1367.578542	18.388557
44.603050	1366.554979	18.393575
44.803981	1364.402541	18.398592
44.888978	1368.195915	18.403610
44.595668	1368.409544	18.408627
44.899768	1362.435399	18.413645
44.923447	1366.900814	18.418663
44.968777	1358.238668	18.423680
44.615632	1353.187344	18.428698
44.919398	1351.408628	18.433715
44.872640	1345.765734	18.438733
44.748906	1357.141542	18.443751
45.042641	1359.492155	18.448768
45.091493	1356.561708	18.453786
45.198757	1365.972101	18.458803
45.427921	1353.017624	18.463821
44.881680	1349.074649	18.468839
44.912524	1340.224483	18.473856
45.020087	1360.248303	18.478874
44.902019	1360.578705	18.483891
45.240485	1357.875782	18.488909
44.964656	1363.578203	18.493927
45.084653	1356.154739	18.498944
45.243645	1370.814077	18.503962
44.905063	1355.994821	18.508979
45.300951	1374.511297	18.513997
45.471283	1383.059039	18.519015
45.772908	1382.065623	18.524032
45.773009	1389.051718	18.529050
45.811343	1386.071031	18.534067
45.964278	1387.772403	18.539085
46.007319	1391.188645	18.544103
45.909468	1376.873683	18.549120
45.879054	1368.602721	18.554138
45.594367	1370.506023	18.559155
46.003698	1372.347404	18.564173
46.111066	1382.830625	18.569191
46.060321	1380.768662	18.574208
46.062767	1378.051684	18.579226
45.868167	1388.575204	18.584243
46.273344	1372.116152	18.589261
46.347224	1381.686040	18.594279
46.554267	1372.736965	18.599296
46.582176	1376.943725	18.604314
46.506654	1385.367080	18.609331
46.498912	1379.639297	18.614349
46.300911	1381.786759	18.619367
46.453909	1372.327190	18.624384
46.364097	1383.954019	18.629402
46.131809	1379.021841	18.634419
46.307787	1371.636633	18.639437
45.984896	1378.542098	18.644455
45.995435	1378.321865	18.649472
46.091748	1401.864921	18.654490
46.106264	1407.915894	18.659507
46.319773	1417.454098	18.664525
46.858696	1419.716851	18.669543
46.754231	1430.180406	18.674560
47.358014	1439.935603	18.679578
47.081255	1427.362206	18.684595
47.364501	1433.316059	18.689613
47.069671	1437.054408	18.694631
47.252222	1427.092211	18.699648
46.882967	1421.843652	18.704666
46.903055	1428.062064	18.709683
47.445657	1429.672978	18.714701
47.134545	1445.783023	18.719719
47.209490	1431.604835	18.724736
47.682201	1437.036887	18.729754
47.387805	1437.658116	18.734771
47.427766	1422.374139	18.739789
47.636975	1424.902629	18.744807
47.510223	1426.088597	18.749824
47.576543	1422.519829	18.754842
47.594173	1433.691461	18.759859
47.661337	1436.221371	18.764877
47.787250	1437.055574	18.769895
48.188086	1428.410622	18.774912
47.997388	1424.410135	18.779930
47.525038	1426.554953	18.784947
47.905932	1432.136931	18.789965
47.456749	1438.537158	18.794983
47.437990	1427.364338	18.800000
47.647338	1445.670762	18.805018
47.790767	1460.548971	18.810035
48.123165	1453.524180	18.815053
47.891369	1465.058883	18.820071
48.386475	1459.930442	18.825088
48.519520	1453.648475	18.830106
48.327478	1460.291642	18.835123
48.632224	1455.810209	18.840141
48.727186	1465.416117	18.845159
48.385351	1460.432167	18.850176
48.643603	1461.214590	18.855194
48.777938	1461.588113	18.860211
48.848608	1460.036902	18.865229
48.676293	1462.616022	18.870247
48.551044	1457.834279	18.875264
48.916370	1458.723112	18.880282
48.637824	1456.230265	18.885299
48.697069	1454.772902	18.890317
48.868160	1456.027778	18.895335
48.660496	1465.431832	18.900352
48.878756	1473.927151	18.905370
48.667852	1487.011170	18.910387
48.906327	1471.026922	18.915405
48.981899	1474.346757	18.920423
48.995624	1468.069657	18.925440
49.444944	1470.828858	18.930458
49.351750	1476.509273	18.935475
49.355750	1467.749043	18.940493
49.367762	1465.295588	18.945511
49.588984	1470.534946	18.950528
49.567091	1471.491041	18.955546
49.393626	1473.349876	18.960563
49.535483	1469.707699	18.965581
48.983498	1481.819677	18.970599
49.462674	1492.224015	18.975616
50.323645	1483.733743	18.980634
50.030243	1492.677991	18.985651
50.096763	1482.657181	18.990669
50.252037	1457.456166	18.995687
50.119309	1460.313699	19.000704
50.063921	1460.365896	19.005722
50.152108	1456.872286	19.010739
50.141911	1454.863622	19.015757
50.202436	1450.237090	19.020775
49.973088	1464.208100	19.025792
49.939088	1451.530682	19.030810
49.891382	1463.310527	19.035827
50.131580	1468.085946	19.040845
50.394630	1488.660106	19.045863
50.609861	1495.600930	19.050880
50.563018	1492.544141	19.055898
50.145886	1494.642407	19.060915
50.579245	1489.613469	19.065933
50.585477	1488.539737	19.070951
50.421859	1490.236549	19.075968
50.628162	1486.107446	19.080986
50.458690	1489.294113	19.086003
50.475682	1484.215959	19.091021
50.505453	1483.141620	19.096039
50.445902	1490.731116	19.101056
50.672255	1495.577181	19.106074
50.878379	1515.086828	19.111091
51.122651	1511.233245	19.116109
50.915331	1517.651564	19.121127
50.931798	1519.517867	19.126144
51.167514	1520.018373	19.131162
51.202319	1527.305751	19.136179
51.232353	1518.454032	19.141197
51.591626	1512.537098	19.146215
51.471193	1512.752258	19.151232
51.686263	1512.559967	19.156250
51.593458	1504.121119	19.161267
51.720448	1508.247619	19.166285
51.881278	1504.147786	19.171303
51.527142	1511.638764	19.176320
51.967016	1505.355820	19.181338
51.678834	1510.074730	19.186355
51.760586	1508.953559	19.191373
51.722090	1505.546997	19.196391
51.577179	1514.564321	19.201408
51.896388	1514.006983	19.206426
51.581044	1508.227529	19.211443
51.784897	1501.663679	19.216461
51.760745	1510.959054	19.221479
51.701812	1510.232354	19.226496
51.866281	1523.986451	19.231514
52.027526	1535.244586	19.236531
51.974409	1541.693381	19.241549
52.012831	1534.892407	19.246567
52.198806	1544.348568	19.251584
52.604073	1541.307756	19.256602
52.490400	1547.268329	19.261619
52.602344	1533.607979	19.266637
52.659598	1535.169679	19.271655
52.566578	1535.664410	19.276672
52.686034	1532.760422	19.281690
52.493932	1540.714802	19.286707
52.251443	1545.073278	19.291725
52.650864	1534.901808	19.296743
52.523317	1568.033409	19.301760
52.900575	1563.156545	19.306778
52.907924	1561.620141	19.311795
53.082226	1564.168382	19.316813
53.160934	1567.659205	19.321831
53.121049	1570.046542	19.326848
53.366069	1562.606181	19.331866
53.097010	1558.024312	19.336883
52.909088	1557.184468	19.341901
53.234876	1558.963691	19.346919
53.288616	1564.619920	19.351936
53.256649	1567.308814	19.356954
53.054624	1557.090885	19.361971
53.249211	1562.109573	19.366989
53.766861	1574.507233	19.372007
53.733928	1587.269577	19.377024
53.890496	1578.561243	19.382042
53.976349	1563.849482	19.387059
53.571670	1563.052073	19.392077
53.713564	1561.818268	19.397095
53.535136	1588.407686	19.402112
53.971048	1579.528954	19.407130
53.566395	1582.381899	19.412147
53.731858	1582.332804	19.417165
54.193242	1584.056583	19.422183
53.828371	1585.665947	19.427200
54.000876	1572.489067	19.432218
53.918085	1577.161084	19.437235
54.035130	1601.279268	19.442253
54.497973	1604.483885	19.447271
54.665288	1607.781254	19.452288
54.740522	1615.307631	19.457306
54.825515	1601.898492	19.462323
54.809450	1600.172328	19.467341
55.093119	1582.141234	19.472359
54.766897	1581.763911	19.477376
54.830809	1574.468049	19.482394
54.610680	1578.148113	19.487411
54.391622	1578.975991	19.492429
55.008523	1584.897146	19.497447
54.773270	1593.042488	19.502464
55.026343	1604.152320	19.507482
55.007193	1600.949512	19.512499
54.999716	1607.118125	19.517517
54.933249	1601.814917	19.522535
54.668236	1612.006892	19.527552
54.843409	1604.627988	19.532570
54.945466	1605.951305	19.537587
54.677383	1610.954918	19.542605
55.291727	1617.063693	19.547623
55.378258	1625.922259	19.552640
55.281471	1630.891481	19.557658
55.561549	1633.063412	19.562675
55.689258	1641.025833	19.567693
55.751465	1628.935413	19.572711
55.511668	1637.814568	19.577728
55.598402	1640.217905	19.582746
56.144142	1624.828669	19.587763
56.158029	1628.145006	19.592781
56.238985	1634.382901	19.597799
56.004174	1629.557223	19.602816
56.048261	1635.082879	19.607834
56.255105	1639.984803	19.612851
55.879138	1641.180645	19.617869
56.205341	1636.190770	19.622887
56.358094	1636.957781	19.627904
56.369568	1637.780359	19.632922
56.412369	1637.875102	19.637939
56.218539	1636.140316	19.642957
56.310840	1632.568926	19.647975
56.319965	1635.721636	19.652992
56.343459	1640.471108	19.658010
56.283583	1636.249128	19.663027
56.287650	1642.145342	19.668045
56.778039	1649.130451	19.673063
56.431036	1660.553115	19.678080
56.567455	1663.930146	19.683098
56.713715	1662.236291	19.688115
56.525455	1661.902247	19.693133
56.602100	1661.143692	19.698151
56.725546	1669.416709	19.703168
57.096551	1680.183732	19.708186
57.035393	1688.973077	19.713203
56.973575	1687.693882	19.718221
57.490343	1683.002379	19.723239
57.487152	1686.367073	19.728256
57.537557	1692.158384	19.733274
57.880893	1684.585085	19.738291
57.644064	1686.502031	19.743309
57.776839	1685.563841	19.748327
57.784116	1680.446267	19.753344
57.659907	1688.835088	19.758362
57.765610	1685.866406	19.763379
57.597084	1685.146950	19.768397
57.747411	1676.063582	19.773415
57.735669	1682.544381	19.778432
57.384182	1678.619805	19.783450
57.958801	1682.210115	19.788467
57.675253	1683.579206	19.793485
58.046598	1697.523069	19.798503
58.294656	1697.791154	19.803520
58.502532	1691.297367	19.808538
58.545322	1693.868964	19.813555
58.439077	1695.945206	19.818573
58.858346	1687.708530	19.823591
58.467170	1668.889073	19.828608
58.198374	1665.122780	19.833626
58.393512	1668.088521	19.838643
58.264315	1695.102885	19.843661
58.617101	1681.823219	19.848679
58.640581	1689.053493	19.853696
58.569212	1701.014278	19.858714
59.062945	1688.187206	19.863731
58.409663	1701.210613	19.868749
59.095466	1687.628495	19.873767
59.085734	1695.984119	19.878784
58.551970	1695.188410	19.883802
58.841443	1689.284897	19.888819
58.831724	1707.459840	19.893837
59.282700	1720.058605	19.898855
59.251292	1723.128917	19.903872
59.125910	1728.371734	19.908890
59.187503	1727.053190	19.913907
59.431437	1728.654356	19.918925
59.260579	1730.235153	19.923943
59.417575	1727.036474	19.928960
59.136688	1731.748785	19.933978
59.675897	1734.885408	19.938995
59.671924	1740.664960	19.944013
59.589017	1754.117363	19.949031
59.752380	1754.804033	19.954048
59.916338	1753.357470	19.959066
60.224857	1751.808411	19.964083
60.132385	1744.085135	19.969101
60.114426	1743.997650	19.974119
60.310510	1740.613400	19.979136
60.306401	1746.599840	19.984154
60.108802	1738.267236	19.989171
60.231718	1742.430634	19.994189
60.289082	1740.139795	19.999207
60.275794	1744.044903	20.004224
60.270516	1746.880592	20.009242
60.446280	1739.848396	20.014259
60.459627	1750.132934	20.019277
60.614099	1760.601051	20.024295
60.908170	1766.186782	20.029312
60.692031	1774.875047	20.034330
60.908968	1768.187075	20.039347
61.100918	1775.988307	20.044365
60.901663	1775.084186	20.049383
60.906324	1767.781946	20.054400
61.128719	1774.962449	20.059418
61.127458	1758.183157	20.064435
61.076180	1771.679298	20.069453
61.501572	1773.856392	20.074471
61.680144	1762.571614	20.079488
61.638152	1774.296527	20.084506
61.493656	1766.679856	20.089523
61.422196	1772.626709	20.094541
61.323970	1766.240698	20.099559
61.557612	1764.991458	20.104576
61.587253	1764.117691	20.109594
61.565124	1770.348488	20.114611
61.647795	1766.612638	20.119629
61.509021	1767.545706	20.124647
61.894654	1767.237330	20.129664
61.645535	1780.385912	20.134682
61.914146	1787.651077	20.139699
62.036819	1802.024046	20.144717
61.816159	1794.191405	20.149735
61.790895	1791.641586	20.154752
61.636138	1790.961616	20.159770
62.143623	1797.902384	20.164787
62.208274	1817.780300	20.169805
62.489096	1827.456701	20.174823
62.606066	1825.872898	20.179840
62.397178	1833.410092	20.184858
62.595802	1823.723504	20.189875
62.892010	1815.006918	20.194893
62.852245	1822.128574	20.199911
62.776954	1826.499796	20.204928
62.833396	1826.837772	20.209946
62.950500	1812.751596	20.214963
62.902988	1830.380556	20.219981
62.779089	1819.843224	20.224999
63.039090	1821.707695	20.230016
62.885516	1825.383498	20.235034
63.036316	1830.350271	20.240051
63.294060	1829.485742	20.245069
63.550641	1840.224726	20.250087
63.539384	1833.670651	20.255104
63.313266	1841.482746	20.260122
63.849317	1833.442095	20.265139
63.680338	1840.776288	20.270157
63.643873	1850.276776	20.275175
63.894237	1832.308104	20.280192
63.806164	1842.514495	20.285210
63.869848	1833.110560	20.290227
64.018221	1839.296890	20.295245
63.956035	1836.109546	20.300263
63.966925	1831.669358	20.305280
63.854491	1835.738175	20.310298
64.119953	1831.791462	20.315315
63.895674	1835.587089	20.320333
63.959550	1839.420923	20.325351
64.225905	1841.502261	20.330368
64.045754	1865.764242	20.335386
64.321172	1876.254055	20.340403
64.025767	1866.047653	20.345421
64.146893	1883.998230	20.350439
64.066741	1877.282865	20.355456
64.320868	1878.213059	20.360474
64.507780	1882.585742	20.365491
64.736494	1886.352400	20.370509
64.895773	1889.544929	20.375527
65.278448	1882.663722	20.380544
64.769868	1890.412345	20.385562
64.840505	1888.924806	20.390579
65.079134	1882.588062	20.395597
65.179826	1881.072134	20.400615
65.160911	1882.431288	20.405632
65.118470	1887.455642	20.410650
65.574471	1901.083374	20.415667
65.819012	1907.931628	20.420685
65.456502	1910.836905	20.425703
65.910751	1900.061011	20.430720
65.814417	1889.573505	20.435738
65.581699	1888.929560	20.440755
65.931799	1899.428717	20.445773
65.868814	1919.590626	20.450791
66.004283	1908.432168	20.455808
66.036786	1913.063881	20.460826
66.192246	1914.665807	20.465843
66.390974	1909.750444	20.470861
65.764499	1914.082957	20.475879
66.244510	1911.015994	20.480896
66.280664	1905.196054	20.485914
65.995381	1914.085777	20.490931
66.298062	1916.484610	20.495949
66.345056	1906.539773	20.500967
66.367471	1909.237362	20.505984
66.335670	1910.439688	20.511002
66.726331	1919.755692	20.516019
66.623590	1916.513446	20.521037
66.348010	1932.840956	20.526055
66.723521	1930.671608	20.531072
66.755956	1935.406379	20.536090
66.587317	1944.681026	20.541107
67.038597	1934.720462	20.546125
66.744399	1938.666488	20.551143
67.147084	1940.835431	20.556160
67.231711	1963.661554	20.561178
67.593137	1961.926272	20.566195
67.878391	1959.983687	20.571213
67.781837	1964.586445	20.576231
67.455796	1945.436107	20.581248
67.629082	1952.012582	20.586266
67.857845	1956.941795	20.591283
68.130058	1955.079946	20.596301
67.818984	1952.611076	20.601319
68.115002	1941.740828	20.606336
67.622561	1934.859937	20.611354
67.729621	1943.377986	20.616371
68.121893	1937.958235	20.621389
67.792269	1958.674776	20.626407
67.901630	1953.866465	20.631424
68.041065	1946.542641	20.636442
67.767431	1959.917105	20.641459
68.223852	1963.082714	20.646477
68.419215	1975.570660	20.651495
68.635463	1982.244124	20.656512
68.581983	1988.002567	20.661530
68.560691	1984.352460	20.666547
68.889405	1971.915638	20.671565
68.731883	1980.332750	20.676583
68.783290	1978.462850	20.681600
68.952143	1983.147566	20.686618
68.796039	1983.265380	20.691635
69.100848	1975.069609	20.696653
69.000135	1974.902504	20.701671
68.745312	1974.531872	20.706688
69.018318	1978.850740	20.711706
68.706185	1984.133656	20.716723
69.381535	1986.469137	20.721741
69.227130	2008.612168	20.726759
69.854607	2002.305389	20.731776
69.866617	2004.778123	20.736794
69.713103	1996.050561	20.741811
69.836935	1995.148387	20.746829
69.949026	2002.196360	20.751847
70.038442	1998.089688	20.756864
70.202547	2002.591110	20.761882
69.841804	1997.878993	20.766899
69.803079	2003.421929	20.771917
69.732155	1996.249613	20.776935
70.065288	2001.721447	20.781952
69.975399	2001.144387	20.786970
69.921195	2003.079442	20.791987
70.036761	2008.552153	20.797005
70.084132	2022.639239	20.802023
70.136698	2021.474703	20.807040
70.524531	2026.481612	20.812058
70.315644	2035.230227	20.817075
70.663040	2027.704086	20.822093
70.580114	2047.325831	20.827111
70.930187	2052.965669	20.832128
71.026917	2058.689173	20.837146
70.946017	2060.480618	20.842163
71.047546	2057.702091	20.847181
71.000401	2060.012009	20.852199
70.975524	2058.103138	20.857216
71.046951	2051.731634	20.862234
70.823249	2052.175644	20.867251
71.647378	2054.200311	20.872269
71.779650	2070.035037	20.877287
71.277400	2073.075896	20.882304
71.429233	2075.262055	20.887322
71.873548	2075.878766	20.892339
71.701934	2067.510365	20.897357
71.668176	2082.747831	20.902375
71.930111	2078.018975	20.907392
71.921673	2067.191682	20.912410
71.880030	2084.535274	20.917427
72.096676	2075.854033	20.922445
71.724396	2078.775845	20.927463
72.216324	2079.825444	20.932480
72.362064	2081.404555	20.937498
72.233377	2085.487044	20.942515
72.399981	2103.427494	20.947533
72.430649	2107.151069	20.952551
72.319582	2115.287908	20.957568
72.671408	2112.128080	20.962586
72.564458	2105.416097	20.967603
72.969339	2100.595219	20.972621
72.975368	2103.520417	20.977639
72.969926	2104.145142	20.982656
73.051498	2093.475735	20.987674
73.268581	2098.895322	20.992691
73.687694	2098.344845	20.997709
73.478534	2100.118993	21.002727
73.467080	2098.781388	21.007744
73.674191	2091.021164	21.012762
73.387968	2096.392016	21.017779
73.617417	2096.607233	21.022797
73.588811	2083.126098	21.027815
73.624136	2082.254552	21.032832
73.921792	2084.912212	21.037850
73.772155	2088.754206	21.042867
73.871328	2084.627863	21.047885
73.760768	2091.995339	21.052903
73.698238	2090.551828	21.057920
73.982604	2094.895663	21.062938
73.957873	2112.444247	21.067955
74.389546	2113.778759	21.072973
74.326419	2109.548507	21.077991
74.677231	2125.154157	21.083008
74.365220	2106.861882	21.088026
74.383482	2123.233200	21.093043
74.514525	2112.642413	21.098061
74.665809	2114.436951	21.103079
74.218690	2122.493668	21.108096
74.623299	2110.710856	21.113114
74.415506	2139.932334	21.118131
74.979497	2140.057230	21.123149
75.034672	2132.483249	21.128167
75.022869	2146.435162	21.133184
75.169085	2142.378385	21.138202
75.089745	2144.262406	21.143219
75.074472	2141.331803	21.148237
75.224280	2150.283640	21.153255
75.245905	2159.100182	21.158272
75.853227	2161.231020	21.163290
75.458806	2176.771513	21.168307
75.762128	2172.080862	21.173325
75.968033	2173.533975	21.178343
75.466516	2180.359752	21.183360
75.620990	2176.091632	21.188378
75.833267	2180.189779	21.193395
76.022603	2178.454387	21.198413
75.516815	2181.911932	21.203431
75.896919	2196.192322	21.208448
76.722689	2203.161188	21.213466
76.301727	2207.247847	21.218483
76.256565	2209.010013	21.223501
76.501847	2211.075102	21.228519
76.106315	2202.464669	21.233536
76.479332	2210.265577	21.238554
76.068509	2198.991079	21.243571
76.584007	2203.715761	21.248589
76.753948	2210.457283	21.253607
76.852675	2218.081695	21.258624
77.021516	2220.339889	21.263642
76.874705	2222.354241	21.268659
77.143954	2215.170044	21.273677
77.574925	2212.661448	21.278695
77.110645	2225.794400	21.283712
77.405896	2212.425894	21.288730
77.467695	2220.647705	21.293747
77.937913	2182.048523	21.298765
78.481933	2196.464022	21.303783
78.475515	2188.726000	21.308800
78.619387	2178.384824	21.313818
78.271217	2184.110895	21.318835
78.275632	2168.570659	21.323853
78.367807	2171.362573	21.328871
78.327758	2164.145922	21.333888
78.515256	2166.431809	21.338906
78.622335	2163.863967	21.343923
78.604589	2158.528401	21.348941
78.347457	2155.479050	21.353959
78.305937	2166.482911	21.358976
78.487022	2156.342687	21.363994
78.115322	2164.508532	21.369011
78.249838	2169.573195	21.374029
78.561697	2166.717843	21.379047
78.261160	2181.459151	21.384064
78.717302	2187.562727	21.389082
78.576741	2192.405402	21.394099
78.889136	2196.120254	21.399117
79.301124	2216.231999	21.404135
79.170201	2213.851553	21.409152
79.141808	2217.266796	21.414170
79.079860	2218.628911	21.419187
78.736537	2231.770895	21.424205
79.044138	2223.067197	21.429223
79.335084	2243.290312	21.434240
79.583636	2235.490366	21.439258
79.869352	2243.958077	21.444275
79.638242	2251.911197	21.449293
79.690239	2246.694264	21.454311
79.468080	2252.157212	21.459328
79.781450	2258.088514	21.464346
80.076345	2263.719930	21.469363
80.225467	2257.728451	21.474381
80.566183	2261.592975	21.479399
80.692253	2269.615784	21.484416
80.539302	2269.856590	21.489434
80.600176	2263.490609	21.494451
80.603061	2266.260598	21.499469
80.636876	2260.298519	21.504487
80.647978	2266.609179	21.509504
80.970388	2263.768645	21.514522
81.044589	2264.273701	21.519539
80.674803	2268.298727	21.524557
81.006754	2273.143160	21.529575
80.983512	2267.522902	21.534592
81.122529	2265.772714	21.539610
81.261166	2269.518442	21.544627
81.298416	2291.566052	21.549645
81.704472	2287.464651	21.554663
81.628425	2299.115185	21.559680
81.909174	2296.663569	21.564698
81.735918	2289.532598	21.569715
81.784274	2289.833332	21.574733
81.948436	2284.427808	21.579751
81.761636	2292.898536	21.584768
81.794229	2291.249482	21.589786
81.718092	2291.965720	21.594803
81.832701	2292.753796	21.599821
82.170966	2311.408090	21.604839
82.237252	2331.288807	21.609856
82.112256	2322.383452	21.614874
82.209623	2329.614060	21.619891
81.863018	2346.486663	21.624909
82.314347	2334.068525	21.629927
82.308191	2356.686351	21.634944
82.279948	2358.643270	21.639962
82.910584	2359.943719	21.644979
82.928921	2358.982834	21.649997
83.231427	2351.863274	21.655015
82.864222	2372.880576	21.660032
83.088268	2382.538086	21.665050
83.533904	2383.672179	21.670067
83.434498	2385.199173	21.675085
83.678080	2383.709176	21.680103
83.489473	2388.762517	21.685120
83.605175	2387.897013	21.690138
83.764961	2385.436355	21.695155
83.427850	2387.916847	21.700173
83.849479	2381.142467	21.705191
83.725772	2391.194459	21.710208
83.920778	2405.488056	21.715226
84.180162	2399.740871	21.720243
83.992804	2405.361150	21.725261
84.318209	2411.525000	21.730279
84.278961	2404.323047	21.735296
84.156708	2398.639082	21.740314
84.220862	2399.608260	21.745331
84.364399	2424.227789	21.750349
84.718515	2428.718707	21.755367
84.776018	2433.614041	21.760384
84.852320	2439.550186	21.765402
85.121960	2428.107214	21.770419
84.947389	2430.342333	21.775437
85.277543	2431.775659	21.780455
85.295000	2428.458282	21.785472
85.451006	2431.727754	21.790490
85.480197	2426.622943	21.795507
85.382183	2437.109787	21.800525
85.562228	2423.639900	21.805543
85.277025	2431.117203	21.810560
85.526999	2428.558777	21.815578
85.735505	2433.473293	21.820595
85.693066	2453.248806	21.825613
85.845699	2454.248714	21.830631
86.383734	2442.106124	21.835648
86.652298	2434.758319	21.840666
86.974332	2432.508544	21.845683
86.715723	2425.520118	21.850701
86.686154	2403.651418	21.855719
86.701388	2398.782460	21.860736
86.628692	2401.662064	21.865754
86.973861	2401.263384	21.870771
86.539641	2395.865146	21.875789
86.897599	2395.772770	21.880807
86.953208	2408.461146	21.885824
87.020164	2419.947385	21.890842
87.503626	2422.838987	21.895859
87.128591	2428.638656	21.900877
87.405803	2427.872462	21.905895
87.206404	2439.428723	21.910912
87.082785	2434.581108	21.915930
87.507583	2431.632970	21.920947
87.126098	2439.824125	21.925965
87.161175	2429.493043	21.930983
87.438633	2441.886494	21.936000
87.674850	2462.638580	21.941018
87.602383	2463.940254	21.946035
87.528721	2473.202448	21.951053
87.600722	2469.665556	21.956071
87.660632	2479.527076	21.961088
87.249120	2501.228098	21.966106
87.860663	2494.587779	21.971123
87.727538	2513.982965	21.976141
88.342547	2509.475337	21.981159
88.358311	2519.794643	21.986176
88.225067	2525.838967	21.991194
88.792834	2515.410290	21.996211
88.914679	2542.150209	22.001229
88.830136	2539.603419	22.006247
89.060088	2545.249235	22.011264
89.123655	2550.800451	22.016282
89.588441	2538.943986	22.021299
89.521157	2550.843461	22.026317
89.529333	2540.675482	22.031335
89.610002	2539.998834	22.036352
89.817980	2542.032951	22.041370
89.955846	2538.350244	22.046387
89.719014	2540.185491	22.051405
89.661415	2543.562206	22.056423
89.718503	2540.477609	22.061440
89.556809	2550.258099	22.066458
90.100403	2535.867236	22.071475
89.901870	2544.874079	22.076493
89.708033	2544.307280	22.081511
90.107284	2557.935245	22.086528
90.292844	2569.333467	22.091546
90.422558	2563.238768	22.096563
90.201413	2573.290691	22.101581
90.464100	2571.167563	22.106599
90.530582	2566.153508	22.111616
90.233164	2583.510950	22.116634
90.759041	2579.975593	22.121651
90.786615	2584.703485	22.126669
90.842558	2579.665148	22.131687
91.094324	2585.478980	22.136704
91.459752	2603.612522	22.141722
91.446613	2596.214380	22.146739
91.839379	2598.763365	22.151757
91.886182	2602.653614	22.156775
91.873476	2597.059079	22.161792
91.970128	2609.074833	22.166810
92.164111	2604.024701	22.171827
92.492090	2603.859232	22.176845
92.386427	2596.403478	22.181863
92.294866	2574.960518	22.186880
91.742910	2579.382806	22.191898
92.071517	2585.645332	22.196915
92.080410	2602.686506	22.201933
92.565182	2597.469654	22.206951
92.656395	2591.893160	22.211968
92.101885	2598.952546	22.216986
92.577070	2607.030779	22.222003
92.411127	2620.784331	22.227021
92.552121	2624.666644	22.232039
92.757906	2630.031597	22.237056
92.519126	2634.810633	22.242074
92.875132	2643.851029	22.247091
93.126401	2660.266813	22.252109
93.164915	2663.183010	22.257127
93.647125	2661.854730	22.262144
93.493342	2667.022964	22.267162
93.600728	2661.546909	22.272179
93.779220	2670.130295	22.277197
93.747369	2680.011303	22.282215
94.073386	2685.284736	22.287232
93.502660	2697.220562	22.292250
94.035174	2688.568823	22.297267
93.954761	2690.832229	22.302285
94.042484	2689.314355	22.307303
94.405379	2690.383795	22.312320
94.084118	2698.335800	22.317338
94.373994	2700.548025	22.322355
94.552613	2718.781508	22.327373
94.896632	2722.618886	22.332391
95.005068	2705.710885	22.337408
94.716382	2717.204515	22.342426
94.958999	2717.209193	22.347443
94.840251	2719.732004	22.352461
94.753225	2718.481909	22.357479
95.327446	2732.763338	22.362496
95.300268	2747.865938	22.367514
95.392843	2751.300560	22.372531
95.829673	2742.465036	22.377549
95.681651	2738.902597	22.382567
96.103454	2731.921152	22.387584
96.538258	2724.928984	22.392602
96.373710	2721.798672	22.397619
96.403592	2718.110329	22.402637
96.216826	2724.038198	22.407655
96.726562	2715.467164	22.412672
96.313752	2723.101833	22.417690
96.672990	2716.187795	22.422707
96.633520	2715.466581	22.427725
96.354670	2716.973455	22.432743
96.635851	2715.143909	22.437760
96.955049	2724.609488	22.442778
97.007416	2715.150940	22.447795
96.794881	2715.831528	22.452813
96.597249	2724.688095	22.457831
97.013067	2740.313147	22.462848
97.162252	2744.097434	22.467866
97.335291	2743.723836	22.472883
97.648533	2751.144413	22.477901
97.172334	2746.552717	22.482919
97.496369	2747.460811	22.487936
97.278656	2763.367048	22.492954
97.856515	2769.692953	22.497971
97.912398	2778.283369	22.502989
97.551123	2795.176918	22.508007
97.746058	2783.774687	22.513024
98.127067	2805.396188	22.518042
98.131578	2810.622610	22.523059
98.267225	2809.083709	22.528077
98.217455	2816.586592	22.533095
98.504421	2815.839276	22.538112
98.264599	2828.334424	22.543130
98.778757	2831.529569	22.548147
99.186445	2838.568568	22.553165
98.735836	2846.868510	22.558183
99.032192	2838.047464	22.563200
99.067837	2844.083078	22.568218
99.105328	2839.940402	22.573235
99.302910	2830.682808	22.578253
99.287009	2850.843214	22.583271
99.530857	2863.758404	22.588288
99.508901	2854.955070	22.593306
99.553664	2870.550544	22.598323
99.894833	2870.113162	22.603341
99.594124	2870.281571	22.608359
99.896808	2861.719085	22.613376
100.007696	2881.701992	22.618394
100.446908	2893.886754	22.623411
100.785969	2894.185194	22.628429
100.518679	2891.696589	22.633447
100.590359	2891.118112	22.638464
100.543611	2885.427422	22.643482
100.946376	2883.940311	22.648499
101.112917	2883.577972	22.653517
100.978470	2893.886885	22.658535
101.080378	2890.568522	22.663552
100.759278	2890.869188	22.668570
100.681411	2901.571045	22.673587
101.339390	2908.327101	22.678605
101.119709	2923.515643	22.683623
101.552050	2921.510150	22.688640
101.596103	2920.958889	22.693658
101.462700	2917.381489	22.698675
101.754600	2916.552361	22.703693
101.568626	2940.953137	22.708711
101.713481	2943.923228	22.713728
102.016316	2944.981028	22.718746
102.058578	2944.682557	22.723763
102.214720	2939.164013	22.728781
102.266521	2968.706021	22.733799
102.669744	2972.684270	22.738816
102.673656	2982.510222	22.743834
102.701024	2980.172843	22.748851
102.695643	2961.017228	22.753869
102.626384	2982.052392	22.758887
102.744009	2968.455087	22.763904
103.153100	2983.231136	22.768922
102.683452	3001.901089	22.773939
102.716940	3006.285994	22.778957
103.195061	2997.671854	22.783975
103.547666	3019.291910	22.788992
103.522425	3026.536909	22.794010
103.565162	3024.290681	22.799027
104.055280	3020.878918	22.804045
103.862636	3024.623392	22.809063
104.017424	3015.008300	22.814080
104.326712	3025.982826	22.819098
104.146786	3035.063304	22.824115
104.572010	3041.395577	22.829133
104.596293	3043.732804	22.834151
104.813610	3039.035144	22.839168
105.140494	3038.116262	22.844186
104.718094	3036.863767	22.849203
105.358094	3024.137286	22.854221
105.374413	3039.772876	22.859239
105.255119	3041.879704	22.864256
105.406071	3031.925391	22.869274
105.303817	3041.433997	22.874291
105.580447	3030.533787	22.879309
105.594615	3032.203208	22.884327
105.373132	3030.425462	22.889344
105.361716	3026.565850	22.894362
105.109294	3032.295070	22.899379
105.763970	3039.167349	22.904397
105.696071	3065.520785	22.909415
105.916045	3061.722594	22.914432
106.036267	3054.037075	22.919450
106.161063	3062.799953	22.924467
105.993244	3059.685821	22.929485
106.337256	3073.420622	22.934503
106.318762	3077.823277	22.939520
106.452568	3085.238813	22.944538
106.564415	3086.553628	22.949555
106.654763	3089.682687	22.954573
107.094354	3119.783024	22.959591
106.969805	3123.697589	22.964608
106.955317	3117.108840	22.969626
107.319429	3117.618828	22.974643
107.382111	3110.991818	22.979661
107.567964	3139.209350	22.984679
107.930565	3148.164054	22.989696
107.893869	3154.308088	22.994714
107.733596	3158.211839	22.999731
107.862120	3142.871820	23.004749
107.415505	3152.458222	23.009767
107.671397	3163.142447	23.014784
108.357255	3176.926669	23.019802
108.443005	3189.485055	23.024819
108.536227	3184.571147	23.029837
108.797486	3187.127051	23.034855
108.685336	3169.792724	23.039872
108.704626	3176.004929	23.044890
108.855913	3187.697794	23.049907
109.638398	3191.659679	23.054925
109.732492	3194.038502	23.059943
109.689684	3197.137686	23.064960
109.942118	3189.691390	23.069978
109.602087	3178.040627	23.074995
109.702537	3181.861905	23.080013
109.782989	3186.454912	23.085031
109.755398	3189.875761	23.090048
109.918242	3195.132923	23.095066
109.692240	3200.190931	23.100083
110.190854	3191.324836	23.105101
109.990751	3189.131465	23.110119
109.864380	3204.415546	23.115136
110.175663	3219.769875	23.120154
110.162183	3221.498005	23.125171
110.565783	3211.406527	23.130189
110.450904	3225.273643	23.135207
110.672188	3241.647666	23.140224
111.258192	3244.335869	23.145242
111.053937	3254.582222	23.150259
111.190511	3252.889733	23.155277
111.421810	3250.400224	23.160295
111.199953	3256.557306	23.165312
111.603203	3244.540177	23.170330
111.465124	3251.723044	23.175347
111.497793	3263.504109	23.180365
111.649194	3272.568085	23.185383
111.507288	3270.783126	23.190400
112.121547	3270.038665	23.195418
111.708283	3273.366065	23.200435
112.181980	3293.651175	23.205453
112.130475	3303.774875	23.210471
112.214969	3305.937349	23.215488
112.624816	3296.233417	23.220506
112.282141	3314.416254	23.225523
112.615420	3322.291753	23.230541
112.783363	3334.593299	23.235559
112.587420	3337.166284	23.240576
113.331387	3330.616971	23.245594
113.386590	3352.553188	23.250611
113.821877	3339.992023	23.255629
114.368356	3349.678213	23.260647
114.175343	3340.424372	23.265664
113.831375	3322.416493	23.270682
114.414175	3326.289116	23.275699
114.274623	3318.472608	23.280717
114.455510	3321.008314	23.285735
114.267881	3322.053102	23.290752
114.446216	3308.769896	23.295770
114.188057	3333.008201	23.300787
114.731760	3337.058548	23.305805
114.849081	3344.856007	23.310823
114.817840	3341.502136	23.315840
114.720851	3330.717133	23.320858
114.621054	3341.413368	23.325875
115.036454	3350.377871	23.330893
115.251309	3359.279175	23.335911
115.282850	3374.001762	23.340928
115.693150	3368.547941	23.345946
115.404197	3382.840218	23.350963
115.657249	3369.551336	23.355981
115.949723	3367.900053	23.360999
115.618394	3379.954007	23.366016
115.606694	3383.904925	23.371034
115.618182	3394.559067	23.376051
115.752064	3396.951245	23.381069
115.978652	3417.608681	23.386087
116.187083	3426.401707	23.391104
116.375512	3418.745240	23.396122
116.651873	3425.513623	23.401139
116.535796	3430.112872	23.406157
116.925733	3441.983428	23.411175
116.830247	3457.218794	23.416192
117.266111	3453.644885	23.421210
117.308147	3451.235867	23.426227
117.564967	3455.622267	23.431245
117.474588	3454.507945	23.436263
117.174706	3473.048372	23.441280
117.597685	3452.085319	23.446298
117.459764	3477.475219	23.451315
117.723208	3484.130837	23.456333
117.904251	3488.899055	23.461351
117.661297	3485.169067	23.466368
118.105295	3497.573835	23.471386
118.299218	3506.206386	23.476403
118.457798	3513.018763	23.481421
118.626176	3504.984710	23.486439
118.753916	3509.304391	23.491456
118.575054	3509.362122	23.496474
118.685151	3518.266068	23.501491
118.893394	3533.504214	23.506509
119.091803	3539.031944	23.511527
119.062245	3542.970019	23.516544
119.517778	3541.597150	23.521562
119.597476	3565.800057	23.526579
119.562937	3568.671445	23.531597
120.023575	3570.641035	23.536615
119.830107	3571.907034	23.541632
120.370875	3568.135440	23.546650
120.184255	3572.561119	23.551667
120.418999	3571.029151	23.556685
120.676893	3568.875969	23.561703
120.720189	3565.790211	23.566720
120.564363	3577.698343	23.571738
120.838743	3586.251246	23.576755
120.881166	3593.102636	23.581773
121.002944	3585.540096	23.586791
121.064116	3603.359179	23.591808
121.349198	3593.237568	23.596826
121.052156	3600.079371	23.601843
121.126452	3614.010300	23.606861
121.737712	3614.186692	23.611879
121.508809	3623.609670	23.616896
121.977224	3617.498287	23.621914
121.992194	3621.646399	23.626931
122.106455	3629.167594	23.631949
122.020185	3642.740266	23.636967
122.059511	3659.205917	23.641984
122.170708	3655.372214	23.647002
122.212742	3652.969457	23.652019
122.167122	3680.012702	23.657037
122.660579	3679.030251	23.662055
122.628570	3690.372003	23.667072
122.545593	3691.571621	23.672090
122.781039	3702.517525	23.677107
122.818782	3715.230336	23.682125
123.089062	3712.773868	23.687143
123.272393	3731.313874	23.692160
123.270781	3735.976780	23.697178
123.876481	3739.670439	23.702195
123.819816	3748.992874	23.707213
124.410544	3733.536059	23.712231
124.035953	3745.888274	23.717248
124.227572	3721.110233	23.722266
124.678987	3719.851285	23.727283
124.672199	3720.050710	23.732301
125.006051	3716.030449	23.737319
124.742682	3717.371326	23.742336
125.013002	3737.010594	23.747354
125.219811	3744.592611	23.752371
125.258750	3756.723924	23.757389
125.605369	3751.822129	23.762407
125.423868	3759.554964	23.767424
125.499187	3751.020352	23.772442
125.968651	3749.492633	23.777459
125.589863	3744.817428	23.782477
125.649977	3747.016895	23.787495
125.649571	3760.926836	23.792512
125.705407	3775.759232	23.797530
125.956907	3775.925339	23.802547
125.946435	3781.706735	23.807565
126.118777	3783.678272	23.812583
126.065743	3801.034367	23.817600
126.125745	3816.938365	23.822618
126.687948	3816.413797	23.827635
126.702926	3826.704257	23.832653
126.712940	3824.826564	23.837671
127.044453	3832.973236	23.842688
126.979648	3844.782110	23.847706
127.196314	3855.893178	23.852723
127.596007	3867.795566	23.857741
127.732080	3853.351979	23.862759
128.017836	3861.918964	23.867776
127.836442	3873.176903	23.872794
128.158364	3886.014470	23.877811
128.150431	3896.561939	23.882829
128.347839	3890.093243	23.887847
128.238481	3893.111145	23.892864
128.274451	3902.359118	23.897882
128.873471	3913.747531	23.902899
128.607515	3928.839860	23.907917
128.825154	3915.099865	23.912935
129.055478	3919.056388	23.917952
129.046608	3916.257356	23.922970
129.041988	3941.474973	23.927987
129.159845	3948.479702	23.933005
129.540871	3943.144407	23.938023
129.429195	3961.977974	23.943040
129.622715	3976.170292	23.948058
130.147036	3969.075949	23.953075
129.734758	3984.359228	23.958093
130.185008	3976.279974	23.963111
130.378231	3978.617947	23.968128
130.309655	3997.369952	23.973146
130.593131	3998.323933	23.978163
130.522262	4007.013949	23.983181
130.710681	4016.631024	23.988199
130.752006	4021.458669	23.993216
130.754665	4025.802381	23.998234
131.233301	4030.095372	24.003251
131.164677	4051.380556	24.008269
131.417268	4051.141354	24.013287
131.511275	4048.753846	24.018304
131.592505	4062.032725	24.023322
132.352772	4070.329075	24.028339
132.340314	4074.195336	24.033357
132.624987	4062.268827	24.038375
132.399480	4062.826457	24.043392
132.503647	4062.274223	24.048410
132.596191	4057.181556	24.053427
132.691526	4056.474968	24.058445
133.028491	4060.075468	24.063463
133.181005	4063.798993	24.068480
132.922400	4086.200924	24.073498
133.126692	4081.616721	24.078515
133.272418	4094.395243	24.083533
133.364077	4090.644785	24.088551
133.532279	4087.828499	24.093568
133.435012	4116.822310	24.098586
134.016918	4111.104066	24.103603
133.957892	4120.305963	24.108621
133.830325	4121.372695	24.113639
133.990993	4127.510839	24.118656
134.308772	4142.957146	24.123674
134.631461	4139.888865	24.128691
134.844709	4152.505629	24.133709
134.728655	4145.971161	24.138727
134.800416	4145.297435	24.143744
135.047794	4167.732880	24.148762
135.450177	4169.445159	24.153779
135.406937	4180.571168	24.158797
135.046348	4176.585204	24.163815
135.748862	4180.118007	24.168832
135.479149	4198.421674	24.173850
135.674782	4195.888135	24.178867
135.826089	4210.060663	24.183885
136.276152	4201.064828	24.188903
136.153366	4204.727657	24.193920
136.125887	4233.815987	24.198938
136.848484	4234.002962	24.203955
136.202429	4237.963213	24.208973
136.588784	4240.583535	24.213991
136.847336	4252.247561	24.219008
136.833513	4265.566955	24.224026
136.694833	4274.850877	24.229043
136.988621	4278.663642	24.234061
137.327773	4286.349922	24.239079
137.783600	4279.706114	24.244096
137.382405	4292.929960	24.249114
137.558913	4287.381706	24.254131
137.732860	4293.096922	24.259149
138.120055	4311.680679	24.264167
138.715818	4310.843152	24.269184
138.742384	4299.885903	24.274202
139.099441	4306.295685	24.279219
139.307763	4299.312147	24.284237
139.599952	4301.863319	24.289255
139.913178	4291.001187	24.294272
139.349051	4280.335598	24.299290
139.360770	4279.567596	24.304307
139.437159	4285.421876	24.309325
139.337670	4287.009652	24.314343
139.731318	4289.669729	24.319360
139.768248	4298.699099	24.324378
139.502755	4290.906873	24.329395
139.872100	4321.774535	24.334413
140.119600	4325.581319	24.339431
140.147051	4323.130430	24.344448
139.884469	4334.308050	24.349466
140.267957	4348.671046	24.354483
140.596178	4348.320659	24.359501
140.658531	4356.981772	24.364519
140.866482	4369.025279	24.369536
141.107199	4385.573703	24.374554
140.964721	4383.377254	24.379571
141.292890	4389.261445	24.384589
141.494379	4417.249228	24.389607
142.062743	4405.028613	24.394624
141.851821	4413.000129	24.399642
142.069354	4417.913093	24.404659
141.832830	4415.448423	24.409677
142.145668	4433.487995	24.414695
142.717984	4438.666157	24.419712
142.230357	4453.603198	24.424730
142.261894	4435.114764	24.429747
142.735878	4458.828310	24.434765
143.115682	4466.479095	24.439783
143.359697	4460.807515	24.444800
143.203758	4464.233390	24.449818
143.519562	4470.399651	24.454835
144.123645	4464.377218	24.459853
143.924362	4486.707361	24.464871
144.316890	4488.624221	24.469888
144.127680	4499.384327	24.474906
144.163727	4494.984950	24.479923
144.431362	4485.527129	24.484941
143.817657	4495.797933	24.489959
144.547901	4494.308806	24.494976
144.361013	4518.779999	24.499994
144.704115	4525.435194	24.505011
144.902321	4520.255505	24.510029
144.748781	4528.658488	24.515047
145.090298	4537.716537	24.520064
145.212769	4563.597028	24.525082
145.216914	4553.383457	24.530099
145.465391	4560.649292	24.535117
145.423082	4586.359420	24.540135
146.104415	4578.993516	24.545152
145.831593	4589.669468	24.550170
145.667522	4594.336521	24.555187
145.970794	4607.191855	24.560205
146.497471	4626.162859	24.565223
146.261003	4624.831793	24.570240
146.505191	4645.982207	24.575258
146.726302	4647.947661	24.580275
146.766551	4658.104865	24.585293
146.958164	4667.841439	24.590311
147.172777	4678.421642	24.595328
147.449378	4692.311110	24.600346
147.417861	4690.592551	24.605363
147.677572	4702.995475	24.610381
147.881729	4720.805700	24.615399
148.253472	4718.539011	24.620416
148.423321	4724.332935	24.625434
148.344156	4719.732367	24.630451
148.690224	4729.293306	24.635469
148.947156	4731.142133	24.640487
149.078023	4720.923975	24.645504
149.107108	4728.306692	24.650522
149.061478	4728.279456	24.655539
149.462067	4737.696393	24.660557
149.491085	4755.026367	24.665575
150.199666	4753.177209	24.670592
150.158250	4754.149218	24.675610
149.933153	4758.962941	24.680627
149.977149	4752.369641	24.685645
150.042738	4749.981044	24.690663
150.608499	4778.682416	24.695680
150.639370	4778.436076	24.700698
150.680014	4787.997761	24.705715
151.150192	4787.986623	24.710733
150.669340	4783.996064	24.715751
151.037272	4791.209138	24.720768
151.004604	4812.156905	24.725786
151.097749	4818.479970	24.730803
151.434050	4814.542419	24.735821
151.538997	4849.755130	24.740839
151.574767	4847.009380	24.745856
151.289297	4852.215893	24.750874
151.444777	4867.478786	24.755891
152.198047	4881.627575	24.760909
152.252487	4897.364483	24.765927
152.302406	4902.721299	24.770944
152.711345	4913.041750	24.775962
152.550240	4915.662946	24.780979
152.921999	4918.316403	24.785997
153.193951	4946.651918	24.791015
153.440591	4950.569145	24.796032
153.161590	4947.199340	24.801050
153.450857	4950.533100	24.806067
153.798699	4964.811125	24.811085
153.907912	4980.024080	24.816103
153.974209	4970.413172	24.821120
153.813282	4972.762142	24.826138
154.194669	4986.680025	24.831155
154.730102	4991.204989	24.836173
154.508705	5006.401453	24.841191
154.863064	4994.810031	24.846208
155.235178	4999.398014	24.851226
155.402210	4998.395155	24.856243
155.559760	5004.374458	24.861261
155.419946	5016.579367	24.866279
155.859094	5015.606286	24.871296
156.299899	5026.895710	24.876314
155.893667	5011.973370	24.881331
156.300728	5009.155804	24.886349
156.253820	5023.368588	24.891367
156.425147	5034.323352	24.896384
156.605087	5040.845091	24.901402
156.723038	5041.590305	24.906419
156.898339	5048.987634	24.911437
156.840851	5052.152486	24.916455
157.427705	5067.401880	24.921472
157.240550	5077.483914	24.926490
157.452022	5085.463970	24.931507
157.458981	5079.601012	24.936525
157.575693	5094.535173	24.941543
157.531403	5106.012144	24.946560
157.738157	5110.064012	24.951578
157.644179	5132.822059	24.956595
158.280576	5139.477976	24.961613
158.256971	5156.539880	24.966631
158.327896	5168.228256	24.971648
158.554363	5173.184895	24.976666
158.482960	5190.046759	24.981683
158.657739	5203.161485	24.986701
158.765540	5210.673507	24.991719
159.435164	5228.537584	24.996736
159.393954	5235.347214	25.001754
159.652077	5241.578071	25.006771
160.060789	5255.969405	25.011789
160.327501	5255.342434	25.016807
160.744789	5261.668294	25.021824
160.906909	5261.964328	25.026842
160.724411	5262.519861	25.031859
160.708339	5266.936158	25.036877
160.744519	5284.496914	25.041895
161.280241	5294.778539	25.046912
161.195630	5291.033066	25.051930
161.007933	5288.387377	25.056947
161.365525	5294.079212	25.061965
161.577723	5315.739992	25.066983
161.603110	5316.422091	25.072000
161.873507	5326.218135	25.077018
161.850806	5355.448740	25.082035
162.408453	5346.056639	25.087053
162.123204	5353.355252	25.092071
162.329227	5365.912057	25.097088
162.822842	5375.995898	25.102106
162.919867	5386.301114	25.107123
163.261510	5391.547082	25.112141
163.090855	5403.695860	25.117159
162.961793	5411.906620	25.122176
163.471994	5417.789741	25.127194
163.311521	5436.666010	25.132211
163.816937	5432.567586	25.137229
163.810923	5447.592480	25.142247
164.261332	5466.527953	25.147264
164.190411	5472.809010	25.152282
164.227688	5482.554996	25.157299
164.679439	5487.150105	25.162317
164.950184	5507.506833	25.167335
164.742341	5516.913493	25.172352
165.145004	5510.953443	25.177370
165.427715	5526.720713	25.182387
165.524623	5535.975732	25.187405
165.955566	5540.099760	25.192423
166.004220	5536.303868	25.197440
166.147263	5540.896288	25.202458
166.118040	5561.544025	25.207475
166.208838	5566.516133	25.212493
166.483078	5575.428199	25.217511
166.547257	5598.576367	25.222528
166.797354	5599.756077	25.227546
166.762330	5611.960503	25.232563
167.110003	5605.625243	25.237581
167.848539	5625.003561	25.242599
168.064365	5621.490191	25.247616
168.433796	5604.349219	25.252634
168.199910	5617.509801	25.257651
168.580276	5610.882158	25.262669
168.690842	5608.063763	25.267687
168.916875	5608.781547	25.272704
169.299239	5601.591842	25.277722
168.999035	5606.908751	25.282739
169.456516	5612.693358	25.287757
169.547797	5625.553486	25.292775
169.782754	5637.371860	25.297792
170.196612	5624.320459	25.302810
169.928331	5634.197085	25.307827
169.974653	5632.705182	25.312845
169.884728	5630.846341	25.317863
170.012717	5633.633996	25.322880
170.152525	5635.750232	25.327898
170.089408	5649.896967	25.332915
170.388828	5655.136387	25.337933
170.659281	5647.641930	25.342951
170.748009	5668.064878	25.347968
171.126423	5670.560849	25.352986
171.049090	5679.165546	25.358003
171.121586	5686.023342	25.363021
171.370661	5692.458033	25.368039
171.520904	5709.539276	25.373056
171.602451	5717.455420	25.378074
172.092806	5732.532067	25.383091
172.141141	5739.068019	25.388109
172.262723	5747.875498	25.393127
172.133921	5758.141449	25.398144
172.488977	5760.336680	25.403162
173.024977	5772.732648	25.408179
172.676830	5775.586802	25.413197
173.005049	5791.363622	25.418215
173.062776	5805.829550	25.423232
173.456017	5800.641925	25.428250
173.102545	5831.259785	25.433267
173.638222	5830.608007	25.438285
173.911823	5856.513876	25.443303
173.862977	5866.270698	25.448320
174.287437	5870.410018	25.453338
174.623576	5895.121887	25.458355
174.490040	5896.553185	25.463373
174.715932	5908.580145	25.468391
174.693819	5928.301222	25.473408
174.963469	5930.654863	25.478426
175.069852	5956.338944	25.483443
175.447903	5966.790948	25.488461
175.807107	5967.637794	25.493479
175.994410	5996.280715	25.498496
176.309465	6006.165293	25.503514
176.163045	6009.882687	25.508531
176.162182	6012.179548	25.513549
176.437731	6019.140452	25.518567
177.003066	6033.893102	25.523584
177.366501	6039.415925	25.528602
177.102109	6053.225344	25.533619
177.158855	6055.639700	25.538637
177.494211	6070.469178	25.543655
177.617607	6090.076004	25.548672
177.873355	6091.343761	25.553690
178.170224	6102.937845	25.558707
178.225367	6118.860048	25.563725
178.354093	6126.698864	25.568743
178.485498	6139.096704	25.573760
179.127672	6145.773408	25.578778
178.952485	6162.295722	25.583795
179.050908	6156.960640	25.588813
179.573419	6165.214277	25.593831
179.606679	6181.055850	25.598848
179.979578	6185.791214	25.603866
180.045586	6187.714730	25.608883
179.801292	6194.455681	25.613901
180.233712	6203.799249	25.618919
179.912360	6221.425199	25.623936
180.365880	6217.264816	25.628954
180.627300	6240.722436	25.633971
180.704962	6249.610389	25.638989
180.875016	6249.003513	25.644007
180.843839	6272.608543	25.649024
181.519936	6269.760443	25.654042
182.030946	6276.988420	25.659059
181.872454	6282.984011	25.664077
183.719880	6247.379724	25.669095
184.025726	6233.082205	25.674112
184.361182	6226.857210	25.679130
184.168119	6206.439318	25.684148
183.967711	6199.612109	25.689165
184.134528	6187.909613	25.694183
184.179615	6187.065382	25.699200
183.989560	6179.323852	25.704218
184.525429	6179.678340	25.709236
183.907602	6173.754839	25.714253
184.369436	6175.485426	25.719271
183.900957	6179.647604	25.724288
184.215372	6185.606313	25.729306
184.558853	6180.765599	25.734324
184.429520	6201.668587	25.739341
184.639924	6205.178863	25.744359
184.436883	6231.886019	25.749376
184.894425	6240.121732	25.754394
184.942058	6252.654190	25.759412
185.061486	6272.130496	25.764429
185.464503	6282.961915	25.769447
184.982763	6289.975231	25.774464
185.523960	6313.041385	25.779482
185.775173	6337.206546	25.784500
185.708633	6354.068171	25.789517
186.228811	6363.434830	25.794535
186.376159	6378.774542	25.799552
186.745257	6391.760207	25.804570
186.733292	6408.416493	25.809588
187.098784	6418.249245	25.814605
187.478845	6440.481310	25.819623
187.210241	6455.719040	25.824640
187.572211	6470.890873	25.829658
188.032777	6481.949305	25.834676
188.001056	6496.530093	25.839693
188.626640	6491.479075	25.844711
188.593183	6517.306804	25.849728
188.622134	6517.521026	25.854746
189.006627	6525.658393	25.859764
189.023714	6542.616267	25.864781
189.404642	6547.539304	25.869799
189.264735	6577.069534	25.874816
189.759539	6580.581768	25.879834
190.081402	6585.127122	25.884852
189.826140	6586.297786	25.889869
190.077603	6594.092892	25.894887
190.027142	6607.518585	25.899904
190.353490	6627.429736	25.904922
190.512627	6635.994926	25.909940
190.382956	6651.245325	25.914957
191.148093	6668.685998	25.919975
190.849358	6685.245111	25.924992
191.515785	6698.355170	25.930010
191.661144	6699.481643	25.935028
191.744178	6705.165871	25.940045
191.750457	6716.339394	25.945063
191.920427	6729.423195	25.950080
192.657899	6749.397217	25.955098
192.968860	6761.853503	25.960116
193.648416	6746.470684	25.965133
193.946442	6739.130224	25.970151
194.470715	6734.954487	25.975168
194.667919	6722.786436	25.980186
195.124617	6723.737385	25.985204
194.886581	6729.573522	25.990221
195.166982	6725.548395	25.995239
195.316747	6712.618405	26.000256
195.158417	6701.107396	26.005274
195.107723	6696.415122	26.010292
194.997294	6713.285726	26.015309
195.091940	6717.384238	26.020327
195.538132	6728.099735	26.025344
195.360580	6740.788102	26.030362
195.635388	6751.394030	26.035380
195.599432	6760.077733	26.040397
196.354423	6762.156642	26.045415
196.452721	6782.885675	26.050432
196.195117	6790.048393	26.055450
196.629534	6797.679892	26.060468
196.765795	6817.525612	26.065485
196.980755	6810.469027	26.070503
197.268465	6822.463271	26.075520
196.871234	6852.806162	26.080538
197.186838	6847.160820	26.085556
197.242355	6882.229666	26.090573
198.072518	6886.161395	26.095591
198.247008	6899.796981	26.100608
198.169123	6921.528390	26.105626
198.495092	6926.039363	26.110644
198.767243	6940.681510	26.115661
199.023387	6954.954839	26.120679
199.010157	6952.596554	26.125696
199.096658	6989.970855	26.130714
199.627370	6978.533901	26.135732
199.139777	7002.954839	26.140749
199.514725	7014.519881	26.145767
199.833442	7041.104390	26.150784
199.888195	7062.558350	26.155802
200.302633	7051.231152	26.160820
200.419112	7083.818508	26.165837
200.722306	7078.519694	26.170855
201.231087	7092.933853	26.175872
201.316365	7108.770482	26.180890
201.754937	7110.132719	26.185908
201.740018	7128.801842	26.190925
201.882742	7126.550069	26.195943
202.395395	7141.261084	26.200960
201.954976	7155.754238	26.205978
202.044681	7158.727687	26.210996
202.458358	7183.039070	26.216013
202.462749	7197.075010	26.221031
202.907397	7202.781251	26.226048
202.834026	7218.900588	26.231066
203.399958	7234.155568	26.236084
203.703319	7255.702363	26.241101
203.151850	7270.993099	26.246119
203.706475	7283.680869	26.251136
203.923021	7302.558412	26.256154
204.401339	7315.127756	26.261172
204.333459	7329.083281	26.266189
205.052391	7330.466153	26.271207
205.110627	7345.416627	26.276224
205.207184	7376.182298	26.281242
205.714480	7370.709998	26.286260
205.951393	7388.283732	26.291277
206.131503	7402.040845	26.296295
206.544226	7393.340977	26.301312
206.592291	7404.002406	26.306330
206.817903	7398.068265	26.311348
206.997621	7419.808905	26.316365
207.242233	7424.491159	26.321383
207.387544	7430.640999	26.326400
207.014574	7450.036040	26.331418
207.682387	7448.861127	26.336436
207.453734	7473.690847	26.341453
207.573643	7497.398057	26.346471
208.122743	7501.247293	26.351488
208.332682	7528.915427	26.356506
208.585656	7536.938980	26.361524
208.766699	7557.906909	26.366541
208.955039	7556.736034	26.371559
209.507843	7569.757971	26.376576
209.473622	7583.196118	26.381594
209.649906	7595.367697	26.386612
209.669220	7604.033637	26.391629
209.440806	7622.340437	26.396647
209.842578	7637.636954	26.401664
210.038781	7655.339458	26.406682
210.339147	7666.673757	26.411700
210.809351	7694.035531	26.416717
211.306841	7703.453088	26.421735
211.853788	7717.977442	26.426752
211.728128	7729.582718	26.431770
212.149708	7719.804807	26.436788
212.294077	7729.853092	26.441805
212.131953	7735.139295	26.446823
212.584068	7736.970773	26.451840
212.338895	7765.887489	26.456858
212.469679	7771.892640	26.461876
212.758943	7781.585800	26.466893
213.194928	7793.083491	26.471911
213.347785	7808.744060	26.476928
213.455621	7824.893392	26.481946
213.573459	7833.277006	26.486964
213.887886	7855.335164	26.491981
214.153906	7863.309601	26.496999
214.492639	7865.782380	26.502016
214.461930	7886.209318	26.507034
214.612650	7901.417081	26.512052
214.931006	7915.062137	26.517069
215.171995	7925.256462	26.522087
215.498678	7939.832672	26.527104
215.209746	7959.928680	26.532122
215.897175	7964.804907	26.537140
216.126896	7985.917154	26.542157
216.050033	7993.772813	26.547175
216.436551	8005.121571	26.552192
216.333603	8026.639434	26.557210
216.951280	8038.698126	26.562228
217.624318	8049.385894	26.567245
217.655925	8060.361630	26.572263
218.317208	8074.087117	26.577280
218.096549	8091.705117	26.582298
218.301290	8087.869922	26.587316
218.583311	8097.475917	26.592333
218.576191	8117.872657	26.597351
218.782937	8112.232395	26.602368
219.200703	8137.820636	26.607386
219.373914	8142.355941	26.612404
219.405449	8146.053362	26.617421
219.406120	8168.191509	26.622439
219.983502	8166.208657	26.627456
220.136325	8186.858555	26.632474
220.357667	8193.587550	26.637492
220.833306	8204.151880	26.642509
220.981595	8219.359961	26.647527
221.251446	8224.014445	26.652544
221.304458	8229.652893	26.657562
221.388486	8242.479852	26.662580
221.627511	8260.593306	26.667597
221.817060	8274.860420	26.672615
222.332875	8282.438007	26.677632
222.208447	8308.171598	26.682650
222.434306	8311.756245	26.687668
222.767038	8325.815266	26.692685
222.684394	8336.266453	26.697703
223.010121	8354.784834	26.702720
223.083880	8363.468502	26.707738
223.464496	8385.024682	26.712756
223.649565	8403.620630	26.717773
223.852167	8407.965620	26.722791
224.151301	8421.214456	26.727808
224.163451	8440.739027	26.732826
224.544851	8459.881340	26.737844
224.870268	8464.097388	26.742861
224.919498	8482.856339	26.747879
224.963429	8494.866401	26.752896
225.072504	8510.385565	26.757914
225.397401	8528.939312	26.762932
225.693996	8546.041797	26.767949
226.241021	8563.002475	26.772967
226.932924	8563.651657	26.777984
227.318070	8572.203968	26.783002
227.379023	8587.980337	26.788020
228.089777	8581.011895	26.793037
228.116082	8595.100346	26.798055
227.991695	8583.820120	26.803072
228.291592	8586.076122	26.808090
228.309712	8585.472525	26.813108
229.117137	8589.674332	26.818125
229.189460	8598.076649	26.823143
229.415595	8582.787850	26.828160
229.277091	8596.590168	26.833178
229.518530	8602.449354	26.838196
229.571304	8612.147704	26.843213
229.802821	8629.344860	26.848231
230.214246	8630.113122	26.853248
230.407914	8649.242718	26.858266
230.404948	8658.419992	26.863284
230.762363	8669.594873	26.868301
230.929012	8695.180427	26.873319
231.152579	8691.177219	26.878336
231.107770	8710.796603	26.883354
230.984887	8728.022432	26.888372
231.439283	8746.200902	26.893389
231.797431	8769.817068	26.898407
231.890228	8786.610790	26.903424
232.365281	8785.810798	26.908442
232.319528	8824.102361	26.913460
232.457379	8832.978326	26.918477
232.698651	8851.415568	26.923495
233.099332	8859.855399	26.928512
233.344988	8882.735006	26.933530
233.497442	8905.202593	26.938548
233.580947	8924.991848	26.943565
233.953269	8934.531264	26.948583
234.330119	8951.990495	26.953600
234.711908	8971.820007	26.958618
234.844024	8996.778094	26.963636
235.128211	9000.693175	26.968653
235.594158	9019.867191	26.973671
235.823450	9028.137703	26.978688
236.205415	9041.550555	26.983706
236.004796	9064.476791	26.988724
236.589568	9071.111657	26.993741
236.487692	9086.058704	26.998759
236.765650	9098.185005	27.003776
237.149820	9104.566596	27.008794
237.527047	9104.225627	27.013812
238.066055	9102.621004	27.018829
238.032436	9112.674197	27.023847
238.431430	9112.610699	27.028864
238.758603	9121.608538	27.033882
238.514902	9146.992714	27.038900
238.995838	9137.315780	27.043917
238.853990	9153.706626	27.048935
239.439308	9159.533643	27.053952
239.513961	9171.805733	27.058970
239.683406	9194.404826	27.063988
239.824990	9208.720612	27.069005
239.965830	9216.776326	27.074023
240.256914	9231.195395	27.079040
240.956095	9234.477386	27.084058
240.553108	9259.799791	27.089076
241.324381	9258.542555	27.094093
241.434774	9285.634872	27.099111
241.812930	9307.307278	27.104128
242.212707	9323.317649	27.109146
242.080060	9331.921066	27.114164
242.396979	9337.993973	27.119181
242.395636	9348.408115	27.124199
242.562875	9371.891976	27.129216
242.678831	9377.010873	27.134234
242.547293	9408.564694	27.139252
243.200080	9427.966394	27.144269
243.219499	9451.263036	27.149287
243.405494	9479.585480	27.154304
243.776555	9498.467926	27.159322
243.862322	9519.769368	27.164340
244.548372	9536.817989	27.169357
244.873557	9556.240992	27.174375
244.885567	9580.910310	27.179392
245.334615	9596.182416	27.184410
245.069828	9614.085459	27.189428
245.752565	9630.003835	27.194445
246.009511	9651.827878	27.199463
246.197029	9675.386104	27.204480
246.450493	9679.084728	27.209498
246.669786	9706.231271	27.214516
247.111771	9717.433986	27.219533
247.214679	9748.487223	27.224551
247.547123	9756.922308	27.229568
247.860470	9779.514296	27.234586
247.994446	9801.676886	27.239604
248.134854	9819.021750	27.244621
248.275478	9836.040001	27.249639
248.398390	9858.956009	27.254656
248.978832	9878.395403	27.259674
249.391768	9894.209508	27.264692
249.684357	9898.991535	27.269709
249.458134	9922.500412	27.274727
249.821366	9928.638187	27.279744
250.805923	9947.954231	27.284762
250.230788	9976.635821	27.289780
250.547342	9982.061748	27.294797
251.051326	9999.116309	27.299815
251.348308	10007.101913	27.304832
252.141451	10013.452545	27.309850
252.247801	10019.588808	27.314868
252.954647	10011.354465	27.319885
253.233708	10005.851893	27.324903
253.278358	10006.935653	27.329920
253.862116	10027.543005	27.334938
253.711519	10036.227990	27.339956
253.991559	10028.012484	27.344973
253.932921	10032.856442	27.349991
254.322117	10039.089287	27.355008
254.602799	10060.698046	27.360026
254.520932	10076.102097	27.365044
254.255694	10070.026367	27.370061
254.911369	10094.996476	27.375079
254.707544	10112.884883	27.380096
255.168296	10127.720456	27.385114
255.422926	10155.547261	27.390132
255.651839	10175.532590	27.395149
256.365732	10191.137701	27.400167
256.333142	10208.248125	27.405184
256.690342	10207.541226	27.410202
256.781544	10239.098663	27.415220
256.924250	10243.122802	27.420237
257.259650	10258.204357	27.425255
257.661135	10285.250499	27.430272
257.854032	10293.294165	27.435290
257.962027	10315.422302	27.440308
258.081812	10338.163642	27.445325
258.580669	10350.714967	27.450343
258.522816	10379.002420	27.455360
259.296336	10394.208667	27.460378
259.451152	10399.597568	27.465396
260.154750	10416.052366	27.470413
260.402575	10425.873083	27.475431
260.221534	10446.183046	27.480448
260.724266	10460.265379	27.485466
261.033481	10481.776146	27.490484
261.012078	10491.790535	27.495501
261.443396	10500.752536	27.500519
261.293785	10525.176065	27.505536
261.539335	10532.288291	27.510554
261.929645	10563.967940	27.515572
262.043094	10579.069848	27.520589
262.611236	10587.675606	27.525607
262.305962	10626.222071	27.530624
262.772508	10642.174020	27.535642
262.959850	10672.197289	27.540660
263.053727	10681.233254	27.545677
263.442080	10698.639956	27.550695
263.635315	10727.127295	27.555712
263.850945	10738.928009	27.560730
263.924959	10764.509419	27.565748
264.652512	10776.734627	27.570765
265.093757	10799.007900	27.575783
265.425997	10816.446113	27.580800
265.951960	10831.084674	27.585818
265.978653	10842.135238	27.590836
266.119639	10864.796469	27.595853
266.477471	10866.867687	27.600871
266.973014	10888.183269	27.605888
267.041718	10902.104203	27.610906
267.307449	10924.234850	27.615924
267.690141	10932.991966	27.620941
267.985635	10950.681749	27.625959
267.939670	10975.736040	27.630976
268.439161	10977.528905	27.635994
268.679681	10994.746618	27.641012
268.736449	11019.361963	27.646029
269.215570	11031.079588	27.651047
269.588020	11045.509468	27.656064
269.706896	11056.096091	27.661082
269.939080	11081.020039	27.666100
270.232068	11100.050741	27.671117
270.584650	11102.702099	27.676135
270.505047	11140.533103	27.681152
271.250525	11147.828811	27.686170
271.410704	11169.752725	27.691188
271.520774	11171.509698	27.696205
272.334601	11193.519534	27.701223
272.534258	11199.977872	27.706240
273.041165	11206.575346	27.711258
273.336066	11225.183252	27.716276
273.602278	11221.966331	27.721293
274.122742	11222.812204	27.726311
274.572995	11232.719243	27.731328
275.419754	11234.426488	27.736346
275.588620	11228.413320	27.741364
275.261860	11235.409318	27.746381
275.758742	11220.254149	27.751399
275.827950	11234.649904	27.756416
276.032397	11228.930934	27.761434
275.693186	11228.921353	27.766452
275.796102	11250.145768	27.771469
276.021326	11252.370798	27.776487
276.021645	11278.747554	27.781504
276.448371	11294.742749	27.786522
276.808808	11321.245565	27.791540
276.717511	11337.367842	27.796557
277.218312	11365.561011	27.801575
277.471667	11396.619633	27.806592
278.009211	11404.874004	27.811610
278.304019	11407.623171	27.816628
278.020114	11428.523632	27.821645
278.831045	11440.200496	27.826663
278.622973	11458.310758	27.831680
278.840861	11477.817491	27.836698
279.080790	11497.193230	27.841716
279.124209	11524.794918	27.846733
279.379937	11539.945158	27.851751
279.735734	11568.562438	27.856768
280.281261	11586.910856	27.861786
280.192184	11614.450788	27.866804
280.790804	11639.830426	27.871821
281.218657	11660.302337	27.876839
281.462568	11685.971565	27.881856
281.847108	11708.010044	27.886874
282.205177	11715.947075	27.891892
282.378945	11739.479626	27.896909
282.256004	11755.492672	27.901927
283.089113	11784.119878	27.906944
283.080577	11812.826387	27.911962
283.427760	11828.638841	27.916980
283.561847	11855.623965	27.921997
283.970079	11871.342318	27.927015
284.274814	11900.960493	27.932032
284.501764	11917.840610	27.937050
285.012789	11947.839220	27.942068
285.487237	11966.729931	27.947085
285.747765	11980.787556	27.952103
286.277311	11992.587033	27.957120
286.471022	12014.249052	27.962138
286.977682	12026.231072	27.967156
286.823970	12039.578894	27.972173
287.579734	12051.145783	27.977191
287.906275	12072.379390	27.982208
288.072271	12083.057609	27.987226
288.606533	12090.190280	27.992244
288.966484	12111.322983	27.997261
289.223377	12112.416751	28.002279
289.422386	12119.898624	28.007296
289.477948	12136.500906	28.012314
289.657259	12156.580000	28.017332
289.605152	12173.683159	28.022349
290.117382	12183.404241	28.027367
290.272658	12211.562362	28.032384
290.185789	12229.587712	28.037402
290.889936	12240.535649	28.042420
291.031948	12264.150032	28.047437
291.192180	12281.105731	28.052455
291.443168	12312.098520	28.057472
291.761960	12325.375612	28.062490
292.254239	12350.553591	28.067508
292.216742	12388.643298	28.072525
293.070240	12392.636585	28.077543
293.257508	12424.077199	28.082560
293.494889	12439.961907	28.087578
294.038347	12449.213391	28.092596
294.335315	12463.531900	28.097613
294.565057	12477.440421	28.102631
294.657626	12492.190803	28.107648
294.936223	12506.005964	28.112666
295.289081	12515.734755	28.117684
295.110341	12538.649968	28.122701
295.861254	12549.014108	28.127719
295.849695	12572.446826	28.132736
295.918736	12590.810619	28.137754
296.493731	12607.739933	28.142772
296.760056	12636.459680	28.147789
297.202524	12658.281721	28.152807
297.169303	12682.497714	28.157824
297.467178	12705.310253	28.162842
298.339581	12715.211595	28.167860
298.542659	12744.889337	28.172877
298.974375	12759.599502	28.177895
299.178195	12769.671789	28.182912
299.258229	12797.257947	28.187930
299.474377	12802.206186	28.192948
299.904236	12820.968109	28.197965
300.275691	12846.897029	28.202983
300.854823	12874.839463	28.208000
300.705708	12888.592082	28.213018
301.132847	12906.552053	28.218036
301.199523	12935.897397	28.223053
301.575193	12945.589474	28.228071
301.993732	12979.049416	28.233088
301.964952	13001.465197	28.238106
302.279873	13020.646049	28.243124
302.362938	13049.805988	28.248141
302.754424	13073.737855	28.253159
302.801771	13097.869149	28.258176
303.292876	13128.588693	28.263194
303.967611	13154.636777	28.268212
304.449324	13179.877837	28.273229
304.796780	13207.688273	28.278247
305.513239	13219.820130	28.283264
305.427632	13245.777019	28.288282
305.748743	13250.664792	28.293300
306.057312	13278.252688	28.298317
306.165905	13306.936284	28.303335
306.541298	13318.302943	28.308352
306.695826	13356.253175	28.313370
307.468317	13366.064212	28.318388
307.573508	13386.350188	28.323405
307.976686	13402.449269	28.328423
308.403125	13407.953092	28.333440
308.714289	13434.083510	28.338458
309.209057	13439.572224	28.343476
309.404212	13462.798415	28.348493
309.769603	13472.081465	28.353511
310.477890	13486.776694	28.358528
310.344061	13504.463988	28.363546
310.414202	13500.225196	28.368564
310.648759	13522.903917	28.373581
311.175194	13535.876219	28.378599
311.263509	13553.393263	28.383616
311.148107	13573.966837	28.388634
311.800756	13596.572540	28.393652
312.116510	13610.831771	28.398669
312.279537	13628.522572	28.403687
312.636848	13653.757186	28.408704
312.546493	13684.438669	28.413722
313.170466	13695.050050	28.418740
313.499734	13725.808990	28.423757
313.587371	13756.680107	28.428775
313.914163	13766.545514	28.433792
314.226683	13798.036501	28.438810
314.992388	13813.268911	28.443828
315.020315	13836.025604	28.448845
315.373450	13858.973054	28.453863
315.822909	13888.785855	28.458880
316.013323	13913.049630	28.463898
316.541254	13923.787964	28.468916
317.023910	13942.744380	28.473933
316.903602	13959.652785	28.478951
317.446669	13972.110935	28.483968
317.826767	13998.579570	28.488986
318.316693	14012.689502	28.494004
318.856930	14031.908732	28.499021
319.517292	14039.190400	28.504039
319.561588	14049.472081	28.509056
319.684653	14077.198833	28.514074
320.009192	14090.501546	28.519092
320.390941	14103.390137	28.524109
320.528338	14121.727436	28.529127
321.038704	14135.692528	28.534144
321.004058	14165.760637	28.539162
321.301254	14187.222980	28.544180
321.974310	14209.796822	28.549197
321.663228	14227.371402	28.554215
322.083340	14248.691438	28.559232
322.449017	14278.545709	28.564250
323.252012	14294.041493	28.569268
323.023270	14316.257069	28.574285
323.204598	14344.445184	28.579303
323.694135	14365.337880	28.584320
323.818558	14400.872049	28.589338
324.017991	14429.976024	28.594356
324.482579	14451.703038	28.599373
325.068445	14475.772626	28.604391
325.299275	14500.441921	28.609408
325.418186	14533.241075	28.614426
325.787530	14561.251724	28.619444
326.108918	14591.676532	28.624461
326.082719	14621.270470	28.629479
326.347519	14643.770776	28.634496
326.631871	14681.015955	28.639514
327.034376	14711.784592	28.644532
327.369650	14745.824845	28.649549
327.675374	14766.713926	28.654567
328.291183	14792.270370	28.659584
328.467545	14827.995142	28.664602
328.997658	14845.365416	28.669620
329.454631	14867.565498	28.674637
329.497559	14908.271462	28.679655
329.871192	14917.478704	28.684672
330.366981	14952.354787	28.689690
330.728510	14983.602948	28.694708
331.268391	15005.906433	28.699725
331.612167	15022.152592	28.704743
331.774326	15047.359791	28.709760
332.109480	15074.207558	28.714778
332.583028	15087.332992	28.719796
332.879886	15110.581884	28.724813
332.702561	15139.909423	28.729831
333.526940	15155.148886	28.734848
333.617773	15198.457453	28.739866
334.222452	15218.737303	28.744884
334.363958	15238.266730	28.749901
334.656833	15263.860173	28.754919
335.138264	15287.241602	28.759936
335.538892	15312.268934	28.764954
335.661055	15337.691019	28.769972
336.320682	15357.309257	28.774989
336.294435	15402.997883	28.780007
336.548332	15418.634282	28.785024
336.858895	15448.247784	28.790042
337.272988	15486.160052	28.795060
337.724431	15515.551460	28.800077
337.947619	15546.907545	28.805095
338.449653	15564.975228	28.810112
338.909304	15599.192304	28.815130
339.044892	15622.768413	28.820148
339.894957	15644.755129	28.825165
340.126615	15668.214242	28.830183
340.637094	15683.360678	28.835200
341.124346	15705.351765	28.840218
341.273176	15716.263183	28.845236
341.869191	15741.097206	28.850253
342.300380	15759.293911	28.855271
342.490064	15776.099405	28.860288
342.950740	15798.924666	28.865306
343.157513	15812.025825	28.870324
343.330283	15828.576430	28.875341
343.512638	15857.721652	28.880359
343.788858	15875.302333	28.885376
344.324323	15894.519647	28.890394
344.191109	15930.948590	28.895412
344.770422	15957.689117	28.900429
345.403264	15983.450221	28.905447
345.661474	15998.741488	28.910464
345.687980	16024.899840	28.915482
345.864298	16049.637684	28.920500
346.385423	16067.176997	28.925517
346.279665	16092.817828	28.930535
347.027856	16121.316552	28.935552
347.376012	16144.549976	28.940570
347.380461	16175.162170	28.945588
347.759620	16196.413989	28.950605
348.089906	16228.236622	28.955623
348.413555	16242.998272	28.960640
348.580056	16281.384781	28.965658
348.593086	16328.577991	28.970676
349.586361	16345.692417	28.975693
349.629734	16385.124092	28.980711
350.328171	16417.544679	28.985728
350.788212	16442.609161	28.990746
351.594653	16455.002766	28.995764
351.992314	16466.114802	29.000781
352.267641	16494.321499	29.005799
352.640304	16505.716261	29.010816
353.083894	16529.833202	29.015834
353.155439	16558.015408	29.020852
353.626388	16570.883989	29.025869
353.805201	16599.256048	29.030887
354.335526	16634.337904	29.035904
354.460581	16651.711100	29.040922
354.731067	16681.714823	29.045940
355.043701	16707.644299	29.050957
355.206613	16730.528038	29.055975
355.705698	16751.316862	29.060992
356.311437	16783.093199	29.066010
356.639802	16800.604426	29.071028
357.258593	16816.309678	29.076045
357.403083	16862.793264	29.081063
357.887585	16887.818354	29.086080
358.517489	16908.266683	29.091098
358.697235	16931.538168	29.096116
359.183495	16950.207790	29.101133
359.300901	16974.862611	29.106151
359.639549	16984.201468	29.111168
360.237172	17009.812039	29.116186
360.295466	17036.505979	29.121204
361.196651	17045.972540	29.126221
361.199776	17075.512575	29.131239
361.377703	17101.545080	29.136256
362.099401	17118.543816	29.141274
362.055765	17137.570730	29.146292
362.355052	17162.794670	29.151309
362.862035	17199.397201	29.156327
363.305100	17223.747976	29.161344
363.734290	17240.768658	29.166362
363.870716	17270.515765	29.171380
365.061610	17261.450110	29.176397
365.399699	17269.192843	29.181415
365.875855	17279.785502	29.186432
366.289376	17300.836527	29.191450
366.268038	17321.210843	29.196468
366.877348	17315.600691	29.201485
366.764571	17332.128728	29.206503
366.968196	17350.058669	29.211520
367.458465	17362.084514	29.216538
367.334319	17395.839769	29.221556
367.810731	17412.220068	29.226573
368.021582	17438.929366	29.231591
367.989108	17463.231891	29.236608
368.549912	17498.457306	29.241626
368.764150	17531.749103	29.246644
369.392892	17547.875356	29.251661
369.674060	17586.400958	29.256679
370.124540	17619.895058	29.261696
370.505379	17650.417314	29.266714
370.248001	17686.929417	29.271732
370.936257	17710.289541	29.276749
371.209372	17751.775452	29.281767
371.142261	17797.121162	29.286784
371.590277	17826.958263	29.291802
372.149888	17869.563786	29.296820
373.174307	17893.396601	29.301837
373.862239	17915.422840	29.306855
374.609166	17939.301125	29.311872
375.460401	17942.612827	29.316890
375.401368	17969.552657	29.321908
375.977047	17982.905535	29.326925
376.392525	18009.054466	29.331943
376.164883	18023.920826	29.336960
376.606682	18048.412078	29.341978
376.684166	18078.717373	29.346996
377.169409	18104.578967	29.352013
377.736390	18134.206757	29.357031
377.681922	18153.611841	29.362048
378.349928	18174.425073	29.367066
378.115663	18219.049030	29.372084
378.471033	18241.345660	29.377101
378.614129	18282.589133	29.382119
379.095515	18321.088195	29.387136
379.528233	18350.722437	29.392154
379.904058	18398.748600	29.397172
380.349133	18435.556832	29.402189
380.955610	18465.778192	29.407207
381.326883	18500.364406	29.412224
381.807254	18527.471225	29.417242
381.910468	18576.747326	29.422260
382.285765	18600.309456	29.427277
383.100012	18641.861124	29.432295
383.177903	18664.775830	29.437312
383.540343	18711.523928	29.442330
383.672935	18751.430486	29.447348
384.166287	18777.993125	29.452365
384.728092	18824.758223	29.457383
384.932969	18856.249914	29.462400
385.417231	18886.113196	29.467418
385.861312	18926.922987	29.472436
386.443947	18944.605386	29.477453
386.778716	18979.041776	29.482471
387.222793	19005.069706	29.487488
387.729584	19014.990520	29.492506
388.090955	19051.048532	29.497524
388.428404	19072.799957	29.502541
388.942207	19099.847718	29.507559
388.989519	19133.958967	29.512576
389.777490	19152.505802	29.517594
389.718077	19184.328872	29.522612
390.480470	19201.562809	29.527629
390.876137	19222.043254	29.532647
391.211726	19266.968406	29.537664
391.578442	19277.064478	29.542682
391.605978	19318.330282	29.547700
392.276426	19350.969758	29.552717
392.648886	19380.727383	29.557735
392.782768	19413.146553	29.562752
393.766054	19434.199849	29.567770
393.915632	19475.515525	29.572788
394.063650	19512.413794	29.577805
394.489602	19531.416445	29.582823
394.811359	19564.638754	29.587840
395.240496	19600.399017	29.592858
395.674196	19636.028699	29.597876
395.931015	19659.750694	29.602893
396.643597	19711.203599	29.607911
396.869125	19739.796603	29.612928
397.558459	19760.509734	29.617946
398.052529	19801.481975	29.622964
398.219558	19830.547513	29.627981
398.625185	19850.155438	29.632999
399.021594	19889.898044	29.638016
399.651642	19918.453694	29.643034
400.262849	19935.482980	29.648052
400.415071	19953.692253	29.653069
401.062273	19990.178601	29.658087
401.379589	20014.124989	29.663104
401.815336	20040.520588	29.668122
402.157920	20071.194645	29.673140
402.687135	20105.189092	29.678157
403.011680	20129.286493	29.683175
403.442098	20150.200869	29.688192
403.724418	20177.853604	29.693210
403.972959	20206.128393	29.698228
404.175573	20244.796321	29.703245
404.527597	20277.208902	29.708263
404.508080	20311.469602	29.713280
404.969172	20360.522613	29.718298
405.197058	20391.734550	29.723316
405.686313	20434.499650	29.728333
406.184071	20465.617544	29.733351
406.722988	20516.999176	29.738368
407.602363	20548.904601	29.743386
407.797699	20578.880158	29.748404
408.071621	20607.557206	29.753421
408.660116	20625.763505	29.758439
408.853071	20672.297572	29.763456
409.064757	20697.235230	29.768474
409.771065	20721.310515	29.773492
410.154227	20765.147150	29.778509
410.563604	20782.214244	29.783527
411.204699	20818.166783	29.788544
411.762620	20851.272284	29.793562
412.207501	20865.733332	29.798580
412.456720	20888.074281	29.803597
413.256302	20918.228276	29.808615
413.312007	20937.793299	29.813632
413.802908	20972.562806	29.818650
414.357636	20994.490591	29.823668
414.586937	21025.434218	29.828685
415.007336	21054.189549	29.833703
415.380669	21083.344637	29.838720
415.567323	21113.543113	29.843738
416.159663	21151.875529	29.848756
416.402198	21188.672894	29.853773
416.723820	21214.787017	29.858791
416.955643	21254.249788	29.863808
417.838640	21291.873103	29.868826
418.308472	21327.143707	29.873844
418.169697	21362.653124	29.878861
418.858564	21391.647460	29.883879
418.960315	21426.548493	29.888896
419.656899	21461.740741	29.893914
420.518007	21477.059077	29.898932
421.116327	21516.849238	29.903949
422.096299	21533.385980	29.908967
422.028062	21560.063693	29.913984
422.383216	21587.194586	29.919002
422.881602	21616.229138	29.924020
423.408141	21627.892978	29.929037
423.904361	21654.046956	29.934055
424.257413	21694.238146	29.939072
424.352917	21712.711703	29.944090
424.888817	21747.818356	29.949108
425.166617	21771.295650	29.954125
425.825272	21794.938338	29.959143
425.818985	21827.037095	29.964160
426.108616	21872.059718	29.969178
426.883579	21899.559015	29.974196
426.989051	21943.635348	29.979213
427.305806	21971.614966	29.984231
427.682792	22002.075443	29.989248
428.124019	22048.674828	29.994266
428.492170	22074.641193	29.999284
428.645472	22126.421100	30.004301
429.246590	22164.498609	30.009319
429.500536	22218.580726	30.014336
429.879825	22256.663082	30.019354
430.462119	22285.650843	30.024372
430.514854	22333.781874	30.029389
431.111209	22377.238531	30.034407
431.489285	22404.215952	30.039424
432.099227	22441.894185	30.044442
432.764153	22475.825664	30.049460
433.027827	22522.583117	30.054477
433.732556	22546.169183	30.059495
434.094381	22583.595074	30.064512
434.568987	22625.910841	30.069530
435.178882	22643.949882	30.074548
435.401442	22683.317667	30.079565
435.692348	22713.491563	30.084583
436.254585	22756.875148	30.089600
436.256477	22801.252344	30.094618
436.846855	22845.173586	30.099636
437.269020	22888.019042	30.104653
437.690438	22936.932008	30.109671
438.237467	22971.916733	30.114688
438.150484	23017.737495	30.119706
439.110543	23058.475802	30.124724
439.427061	23105.365968	30.129741
439.835196	23141.727184	30.134759
440.508374	23176.788358	30.139776
440.924103	23215.834464	30.144794
441.669153	23251.790168	30.149812
441.951302	23295.255294	30.154829
442.608109	23336.634960	30.159847
442.863530	23377.425701	30.164864
443.419296	23423.879340	30.169882
443.671286	23449.519102	30.174900
443.863589	23495.898528	30.179917
444.701469	23523.835671	30.184935
445.260632	23565.155084	30.189952
445.917198	23606.307850	30.194970
446.193752	23639.145802	30.199988
446.249187	23677.032681	30.205005
446.835228	23706.009844	30.210023
447.387673	23755.054901	30.215040
447.821966	23787.597851	30.220058
448.430513	23820.111529	30.225076
448.834524	23862.150392	30.230093
449.070910	23910.831955	30.235111
449.502229	23939.256022	30.240128
449.923155	24000.699146	30.245146
450.375976	24026.154238	30.250164
450.589056	24075.611968	30.255181
451.114940	24118.666350	30.260199
451.640114	24169.584689	30.265216
451.693663	24212.801224	30.270234
452.410016	24255.325432	30.275252
452.347760	24321.651052	30.280269
453.225033	24357.839477	30.285287
453.694305	24405.265265	30.290304
453.968166	24451.463540	30.295322
454.674678	24485.478555	30.300340
455.181645	24540.567269	30.305357
455.883057	24568.134127	30.310375
456.251664	24612.655661	30.315392
456.374819	24650.957862	30.320410
457.147636	24675.206616	30.325428
457.598699	24724.955352	30.330445
458.155453	24768.161754	30.335463
458.640014	24802.939104	30.340480
458.716427	24846.680710	30.345498
459.299422	24883.445790	30.350516
459.601638	24926.179559	30.355533
460.294382	24960.748419	30.360551
460.661116	25008.128524	30.365568
461.208239	25052.996239	30.370586
461.708726	25093.269430	30.375604
462.286161	25131.694984	30.380621
462.725136	25175.113463	30.385639
463.111068	25212.540117	30.390656
463.372268	25260.683006	30.395674
463.716156	25301.980557	30.400692
464.649346	25342.394987	30.405709
465.411401	25376.239985	30.410727
466.541647	25397.551231	30.415744
466.968782	25427.469869	30.420762
467.582692	25452.615614	30.425780
467.795550	25486.420719	30.430797
468.226239	25514.662565	30.435815
468.979210	25548.733106	30.440832
469.036660	25573.101132	30.445850
469.696628	25592.633912	30.450868
469.676453	25625.424746	30.455885
470.732117	25646.901827	30.460903
470.989394	25678.188016	30.465920
471.179814	25715.153837	30.470938
471.783211	25740.835831	30.475956
472.252447	25777.937782	30.480973
472.267706	25816.264683	30.485991
473.250615	25849.301888	30.491008
473.130702	25902.426407	30.496026
473.541315	25940.756009	30.501044
473.811885	25979.672865	30.506061
474.316390	26028.125141	30.511079
474.946860	26070.801002	30.516096
474.939406	26126.885463	30.521114
475.498979	26170.875131	30.526132
475.885681	26228.788687	30.531149
476.363389	26267.885163	30.536167
476.867228	26313.044550	30.541184
477.110851	26371.207515	30.546202
478.014373	26411.687671	30.551220
478.171912	26460.240641	30.556237
479.018585	26515.918588	30.561255
479.718757	26565.305612	30.566272
479.647763	26613.400693	30.571290
480.063195	26648.781571	30.576308
480.537663	26700.832392	30.581325
481.317579	26744.162196	30.586343
481.638649	26786.176251	30.591360
481.984182	26834.932025	30.596378
482.594905	26867.485433	30.601396
483.421723	26919.976384	30.606413
483.397991	26972.964626	30.611431
484.301369	27006.944185	30.616448
484.799048	27055.316340	30.621466
484.898389	27098.900482	30.626484
485.676940	27135.701813	30.631501
486.126314	27185.087358	30.636519
486.727619	27236.259358	30.641536
487.344900	27277.419946	30.646554
487.950419	27324.683749	30.651572
488.218915	27368.643483	30.656589
488.131932	27420.600128	30.661607
488.940907	27461.929193	30.666624
489.107828	27513.566782	30.671642
489.803127	27569.808239	30.676660
490.202103	27619.685322	30.681677
490.454186	27677.415944	30.686695
491.297227	27733.171159	30.691712
491.728903	27792.744024	30.696730
492.750720	27828.145135	30.701748
493.080236	27886.409387	30.706765
493.346139	27938.634513	30.711783
493.902456	27975.961658	30.716800
494.526104	28035.914545	30.721818
495.100404	28075.002376	30.726836
495.812230	28114.274826	30.731853
496.514062	28158.823211	30.736871
497.118436	28202.955470	30.741888
497.390268	28249.296548	30.746906
497.786560	28294.640919	30.751924
498.652803	28335.063298	30.756941
498.422678	28384.229818	30.761959
499.077165	28427.725948	30.766976
499.465393	28480.978115	30.771994
499.775325	28538.708889	30.777012
500.673503	28581.980663	30.782029
501.025348	28626.193697	30.787047
501.529736	28663.886843	30.792064
502.211378	28726.118043	30.797082
502.734549	28776.086058	30.802100
503.064910	28823.858223	30.807117
503.371314	28874.608036	30.812135
503.766368	28915.070674	30.817152
504.440419	28981.418702	30.822170
505.202522	29026.664295	30.827188
505.558275	29077.318629	30.832205
506.231356	29132.807886	30.837223
506.901032	29173.715953	30.842240
507.163388	29225.194067	30.847258
507.694330	29270.209255	30.852276
508.706974	29303.659339	30.857293
509.050125	29339.483899	30.862311
509.430027	29369.608844	30.867328
509.715432	29417.643637	30.872346
510.201606	29454.602404	30.877364
510.934257	29491.457380	30.882381
511.481324	29545.387447	30.887399
511.900757	29576.103761	30.892416
512.075613	29631.201294	30.897434
512.257888	29675.674278	30.902452
513.189839	29725.917348	30.907469
513.309374	29783.996480	30.912487
514.141786	29832.641940	30.917504
515.012858	29877.644025	30.922522
514.966208	29931.419360	30.927540
515.386723	29979.645466	30.932557
516.093128	30028.541677	30.937575
516.343357	30084.232337	30.942592
516.713282	30139.382462	30.947610
517.108404	30195.236388	30.952628
517.728900	30248.419506	30.957645
518.263418	30320.175724	30.962663
518.818285	30372.212898	30.967680
519.527200	30437.084555	30.972698
519.729706	30499.059994	30.977716
520.678959	30546.625144	30.982733
521.324722	30591.792746	30.987751
522.288883	30635.302182	30.992768
522.876048	30676.077437	30.997786
523.485969	30724.961155	31.002804
524.203140	30774.896508	31.007821
524.617952	30815.765758	31.012839
525.060304	30859.346300	31.017856
525.506197	30911.142493	31.022874
525.590507	30957.812704	31.027892
526.496301	31005.253719	31.032909
526.725336	31067.170339	31.037927
527.217607	31117.829737	31.042944
527.263422	31164.196174	31.047962
528.127287	31225.810531	31.052980
528.790585	31284.585385	31.057997
529.035798	31340.512797	31.063015
529.833495	31394.393272	31.068032
530.544036	31444.555530	31.073050
530.873713	31508.911817	31.078068
531.058957	31562.512125	31.083085
531.734459	31620.100976	31.088103
532.249819	31672.838921	31.093120
532.882397	31734.990092	31.098138
533.051600	31790.680530	31.103156
533.863497	31847.157746	31.108173
534.284656	31908.087039	31.113191
534.709472	31976.439786	31.118208
535.222166	32025.213613	31.123226
535.846970	32078.797599	31.128244
536.655693	32132.087663	31.133261
537.342718	32185.844926	31.138279
538.010693	32224.030911	31.143296
538.432503	32269.799929	31.148314
538.926368	32318.733668	31.153332
539.935335	32356.901901	31.158349
540.464522	32406.642027	31.163367
540.859890	32458.540982	31.168384
541.107707	32494.513715	31.173402
541.531049	32554.644323	31.178420
542.029012	32599.856749	31.183437
542.276864	32659.235450	31.188455
543.187261	32706.059601	31.193472
543.666701	32769.471690	31.198490
543.953057	32828.539071	31.203508
544.450424	32863.558628	31.208525
545.165826	32929.939687	31.213543
545.741166	32989.412428	31.218560
546.592605	33024.374353	31.223578
547.155002	33091.124060	31.228596
548.037608	33131.962379	31.233613
548.431805	33181.969087	31.238631
548.914997	33237.876054	31.243648
549.403742	33281.668412	31.248666
549.734181	33337.544873	31.253684
550.458430	33380.691528	31.258701
550.645342	33450.949889	31.263719
551.129447	33503.017685	31.268736
551.757688	33567.567728	31.273754
552.413944	33619.305814	31.278772
552.795923	33671.797101	31.283789
553.425835	33741.853721	31.288807
553.989314	33792.814221	31.293824
554.629659	33850.775857	31.298842
554.916129	33909.713078	31.303860
555.867305	33957.856849	31.308877
556.560647	34028.749511	31.313895
557.037488	34077.661208	31.318912
557.979521	34135.977765	31.323930
558.097957	34198.273677	31.328948
558.872794	34239.541755	31.333965
559.497029	34299.728664	31.338983
559.773402	34357.313373	31.344000
560.590065	34408.687866	31.349018
560.823827	34462.315048	31.354036
561.600974	34516.160107	31.359053
562.178339	34580.091616	31.364071
562.958853	34639.342111	31.369088
563.981975	34663.763768	31.374106
564.487722	34722.014719	31.379124
565.400542	34760.474966	31.384141
565.588127	34806.294595	31.389159
566.188744	34848.607167	31.394176
566.829912	34882.577082	31.399194
566.960923	34933.244216	31.404212
567.684449	34966.524883	31.409229
568.244820	35010.564200	31.414247
568.786956	35049.516107	31.419264
569.323748	35091.010235	31.424282
569.797802	35134.343177	31.429300
570.456700	35178.518587	31.434317
571.030821	35213.474123	31.439335
571.136114	35264.838437	31.444352
571.954284	35315.893885	31.449370
572.151555	35377.924671	31.454388
572.873194	35415.961273	31.459405
573.366418	35473.486917	31.464423
573.371396	35534.847362	31.469440
573.862575	35598.561597	31.474458
574.477683	35670.222546	31.479476
575.010426	35735.177717	31.484493
575.599100	35796.890742	31.489511
576.174415	35863.413020	31.494528
577.245182	35909.033523	31.499546
577.324079	35984.350532	31.504564
578.329703	36037.927628	31.509581
578.957575	36091.519338	31.514599
579.137649	36167.894700	31.519616
580.236343	36224.341132	31.524634
580.805336	36287.509554	31.529652
581.190773	36351.569844	31.534669
581.553322	36415.736503	31.539687
582.045483	36478.014485	31.544704
583.291519	36523.034864	31.549722
583.839118	36588.385124	31.554740
584.896227	36633.189937	31.559757
585.260397	36693.064257	31.564775
585.863960	36758.842993	31.569792
586.597477	36808.024512	31.574810
586.911750	36868.796628	31.579828
587.274484	36927.768594	31.584845
587.864510	36983.201242	31.589863
587.971975	37046.121226	31.594880
589.495784	37092.711821	31.599898
589.983215	37154.795979	31.604916
590.826763	37202.784934	31.609933
591.586440	37250.040038	31.614951
591.603688	37305.785703	31.619968
592.500120	37360.111263	31.624986
593.093764	37426.772404	31.630004
593.407564	37475.937577	31.635021
594.312657	37531.979339	31.640039
594.297650	37593.992189	31.645056
595.100428	37643.899868	31.650074
595.474781	37703.831340	31.655092
595.939053	37773.254793	31.660109
596.521519	37825.385017	31.665127
597.270930	37896.275651	31.670144
597.615083	37966.777020	31.675162
598.210211	38017.642847	31.680180
598.879095	38081.499009	31.685197
599.418806	38134.825870	31.690215
599.858275	38204.802180	31.695232
600.611890	38250.829596	31.700250
601.287030	38316.959357	31.705268
601.829761	38381.782809	31.710285
602.661770	38419.587887	31.715303
603.077196	38495.751813	31.720320
603.539768	38551.739711	31.725338
604.065618	38604.486842	31.730356
605.093804	38665.582191	31.735373
606.293318	38714.121097	31.740391
607.179947	38768.022278	31.745408
607.906274	38809.761881	31.750426
608.414190	38868.711188	31.755444
608.705623	38915.392712	31.760461
609.087130	38963.931726	31.765479
609.655645	39021.856430	31.770496
610.239629	39070.549573	31.775514
610.942473	39135.544360	31.780532
610.972886	39191.735645	31.785549
611.587561	39246.432240	31.790567
611.748098	39328.411814	31.795584
612.377320	39390.716542	31.800602
613.413979	39458.839969	31.805620
614.266557	39515.003889	31.810637
615.684839	39566.328302	31.815655
616.196067	39617.838317	31.820672
617.165287	39670.228003	31.825690
617.349633	39713.677195	31.830708
617.864021	39768.440323	31.835725
618.743307	39815.062239	31.840743
618.907103	39881.621713	31.845760
619.955352	39928.560803	31.850778
620.318321	39989.803120	31.855796
620.842447	40061.946606	31.860813
621.606799	40109.190022	31.865831
621.905984	40173.204384	31.870848
622.281256	40224.461915	31.875866
622.752398	40297.223536	31.880884
623.494320	40362.410748	31.885901
623.890391	40430.955467	31.890919
624.191703	40509.049974	31.895936
624.707610	40570.820384	31.900954
625.840216	40651.842520	31.905972
625.974904	40725.463806	31.910989
626.899278	40797.742207	31.916007
627.527954	40877.669211	31.921024
627.682446	40956.495640	31.926042
628.432466	41029.225424	31.931060
628.518391	41103.852781	31.936077
629.583392	41181.122225	31.941095
630.339529	41272.398099	31.946112
631.044861	41344.300498	31.951130
631.877580	41417.148077	31.956148
632.137918	41490.648548	31.961165
633.331317	41548.845042	31.966183
633.866217	41613.401300	31.971200
634.515201	41674.968399	31.976218
635.166661	41735.261033	31.981236
635.366182	41807.649653	31.986253
636.262766	41863.459436	31.991271
636.797772	41944.551299	31.996288
637.451294	42014.092773	32.001306
638.413444	42079.916990	32.006324
638.685468	42154.266927	32.011341
639.443112	42227.902690	32.016359
639.983496	42302.721526	32.021376
640.583462	42362.012028	32.026394
642.195028	42416.205153	32.031412
643.215470	42475.302918	32.036429
644.297709	42516.146393	32.041447
644.752525	42577.949519	32.046464
645.216617	42631.878127	32.051482
646.069759	42681.341466	32.056500
646.229735	42735.224191	32.061517
646.787650	42795.264157	32.066535
647.052868	42858.953253	32.071552
647.574064	42929.538360	32.076570
648.364238	42988.564147	32.081588
648.791584	43073.479530	32.086605
649.730551	43122.671804	32.091623
650.144395	43201.489279	32.096640
650.927077	43270.037367	32.101658
651.687466	43335.923742	32.106676
652.003814	43408.647458	32.111693
652.829664	43477.293592	32.116711
653.148146	43553.585320	32.121728
653.762707	43630.398055	32.126746
654.312185	43703.275156	32.131764
654.719000	43784.118460	32.136781
655.537211	43856.953415	32.141799
655.954571	43936.653794	32.146816
656.206604	44029.620736	32.151834
657.154526	44112.281632	32.156852
657.491694	44207.851149	32.161869
657.887353	44300.055325	32.166887
659.107652	44385.210491	32.171904
659.658436	44478.387786	32.176922
660.798115	44564.010940	32.181940
661.219321	44653.357912	32.186957
662.273720	44729.206371	32.191975
662.972854	44805.840475	32.196992
663.548434	44887.425478	32.202010
664.642670	44961.637595	32.207028
665.044159	45041.957584	32.212045
665.730750	45113.525293	32.217063
666.486925	45189.644077	32.222080
666.989302	45272.192133	32.227098
667.912813	45343.158345	32.232116
668.195151	45420.527183	32.237133
668.924909	45484.177160	32.242151
669.426565	45556.094770	32.247168
669.901586	45633.771442	32.252186
671.189633	45691.837457	32.257204
671.789805	45770.823026	32.262221
672.329820	45838.394520	32.267239
673.384534	45915.144084	32.272256
673.660972	45974.905414	32.277274
674.422763	46048.768095	32.282292
675.261696	46131.187739	32.287309
676.115540	46189.169947	32.292327
676.888189	46261.435369	32.297344
677.426963	46329.684125	32.302362
678.628018	46384.970948	32.307380
678.761218	46457.872192	32.312397
679.434031	46523.245045	32.317415
680.579168	46584.810496	32.322432
680.998006	46654.376343	32.327450
681.812577	46717.547191	32.332468
682.208274	46792.521936	32.337485
683.161293	46859.116621	32.342503
683.769198	46931.420496	32.347520
684.111162	47009.342143	32.352538
685.197006	47069.356939	32.357556
685.797546	47136.150777	32.362573
686.784454	47203.347163	32.367591
687.654557	47269.565363	32.372608
688.412911	47335.173720	32.377626
689.201822	47387.241605	32.382644
689.456355	47464.800560	32.387661
690.189876	47526.649403	32.392679
690.810368	47598.474415	32.397696
691.497816	47666.493282	32.402714
692.455619	47729.654423	32.407732
693.236356	47797.236135	32.412749
693.591207	47856.912486	32.417767
694.571542	47919.947665	32.422784
695.132144	47989.234316	32.427802
696.064654	48049.355749	32.432820
697.015380	48104.754103	32.437837
697.809659	48161.748902	32.442855
698.767412	48219.497231	32.447872
699.159778	48282.920766	32.452890
699.836655	48344.778338	32.457908
700.371969	48400.505655	32.462925
700.833048	48469.832120	32.467943
701.276253	48528.543736	32.472960
702.158006	48601.366201	32.477978
702.533568	48669.874031	32.482996
703.138552	48751.077841	32.488013
703.691491	48835.742389	32.493031
704.063317	48910.537432	32.498048
704.590037	48987.965055	32.503066
705.735233	49055.970025	32.508084
706.479911	49123.310099	32.513101
706.757830	49189.601371	32.518119
708.090635	49257.678223	32.523136
708.403070	49339.044895	32.528154
708.672897	49402.769627	32.533172
709.531241	49482.093588	32.538189
710.315377	49564.468555	32.543207
710.906763	49626.779676	32.548224
711.411676	49725.552204	32.553242
712.406866	49800.286452	32.558260
712.643915	49879.698475	32.563277
713.276330	49964.535608	32.568295
714.073456	50053.843769	32.573312
714.551591	50147.472820	32.578330
715.416784	50230.080945	32.583348
716.164341	50328.379531	32.588365
716.389594	50426.294759	32.593383
717.505010	50513.626382	32.598400
717.715315	50618.124805	32.603418
718.625023	50704.401364	32.608436
719.283248	50807.046553	32.613453
720.383358	50910.193185	32.618471
721.195873	51006.544315	32.623488
721.787272	51102.912228	32.628506
722.703025	51198.001382	32.633524
723.475714	51294.142640	32.638541
724.021975	51384.747111	32.643559
724.925397	51481.237799	32.648576
725.412980	51592.145317	32.653594
726.117320	51683.701316	32.658612
726.900173	51778.076201	32.663629
727.579111	51892.060591	32.668647
728.529816	51983.092867	32.673664
729.167576	52077.271496	32.678682
730.297335	52165.921788	32.683700
730.901070	52261.596453	32.688717
731.701768	52369.160811	32.693735
733.007699	52449.310355	32.698752
733.562850	52532.076267	32.703770
734.127978	52622.601898	32.708788
735.110632	52707.339416	32.713805
736.052773	52805.254452	32.718823
736.886079	52883.865211	32.723840
737.706224	52967.588283	32.728858
738.620315	53036.942362	32.733876
739.169474	53116.464167	32.738893
739.827498	53209.698607	32.743911
740.950836	53279.790427	32.748928
741.499250	53364.164590	32.753946
741.897678	53448.297895	32.758964
743.170983	53526.730932	32.763981
743.697663	53613.142364	32.768999
744.270901	53690.216715	32.774016
744.994369	53772.743715	32.779034
745.385953	53843.153053	32.784052
746.249944	53936.573069	32.789069
746.788220	54023.982018	32.794087
747.549643	54091.063435	32.799104
748.078113	54180.974557	32.804122
748.958878	54250.243890	32.809140
749.650686	54328.851873	32.814157
750.441727	54416.617022	32.819175
751.142349	54500.429319	32.824192
751.538572	54591.663980	32.829210
752.230844	54681.336855	32.834228
753.118714	54772.036462	32.839245
753.747283	54864.886354	32.844263
754.666507	54955.086306	32.849280
755.515278	55051.263804	32.854298
756.527504	55139.063506	32.859316
757.201965	55225.471682	32.864333
757.862447	55323.173648	32.869351
758.773420	55396.861769	32.874368
759.794321	55490.106934	32.879386
760.426452	55570.194436	32.884404
761.894237	55647.324057	32.889421
762.329198	55739.896701	32.894439
763.272774	55818.029079	32.899456
764.097302	55910.221744	32.904474
764.226189	55999.113196	32.909492
765.172672	56067.299363	32.914509
765.872915	56165.419332	32.919527
766.631126	56249.296764	32.924544
767.145348	56352.270872	32.929562
767.839307	56446.327412	32.934580
768.677017	56544.566421	32.939597
769.097379	56651.260080	32.944615
769.975687	56740.559850	32.949632
770.247681	56839.566048	32.954650
771.370489	56936.849434	32.959668
772.484027	57042.011261	32.964685
773.133811	57151.105257	32.969703
773.939808	57252.311114	32.974720
774.501127	57356.943879	32.979738
775.277024	57458.010434	32.984756
776.404687	57548.628762	32.989773
777.191085	57645.552712	32.994791
778.675974	57719.948039	32.999808
779.786455	57811.290189	33.004826
780.630737	57894.750991	33.009844
781.840130	57960.550323	33.014861
782.633063	58055.047606	33.019879
783.075407	58125.424243	33.024896
783.852943	58212.341475	33.029914
784.573290	58288.827659	33.034932
785.485985	58365.772896	33.039949
785.676900	58452.254230	33.044967
786.425553	58532.250804	33.049984
787.037202	58623.796333	33.055002
787.438096	58708.145919	33.060020
788.102853	58790.351197	33.065037
788.864273	58878.855865	33.070055
789.645442	58969.602597	33.075072
790.169454	59056.046344	33.080090
791.184289	59150.842231	33.085108
792.004846	59243.778321	33.090125
792.743932	59338.947413	33.095143
793.950968	59425.195750	33.100160
794.727932	59511.231941	33.105178
795.450629	59599.098945	33.110196
796.606678	59669.250997	33.115213
797.673750	59763.527040	33.120231
798.484536	59831.751840	33.125248
799.104569	59916.255136	33.130266
799.765596	59999.880847	33.135284
800.836545	60090.798454	33.140301
801.046724	60180.296899	33.145319
801.784604	60272.430336	33.150336
802.568382	60363.063443	33.155354
802.824736	60464.866828	33.160372
803.623685	60565.921328	33.165389
804.318768	60672.824825	33.170407
805.281127	60780.510504	33.175424
805.769166	60891.259335	33.180442
806.386656	61007.507638	33.185460
807.318346	61112.206726	33.190477
807.541972	61227.742313	33.195495
808.311887	61349.333234	33.200512
809.548203	61459.489506	33.205530
810.377428	61587.728835	33.210548
811.680266	61698.564288	33.215565
812.317917	61813.387081	33.220583
813.154310	61918.424744	33.225600
814.088956	62035.424650	33.230618
814.633196	62154.479963	33.235636
815.917035	62260.771414	33.240653
816.547997	62374.629243	33.245671
817.492642	62484.563193	33.250688
818.483185	62588.676909	33.255706
819.706120	62692.046853	33.260724
820.806148	62783.092835	33.265741
821.633316	62889.207871	33.270759
822.467043	62977.969816	33.275776
823.734597	63075.034749	33.280794
824.488156	63169.608276	33.285812
825.481105	63260.885176	33.290829
826.156271	63356.716340	33.295847
826.761976	63448.921056	33.300864
827.783078	63539.016887	33.305882
828.135738	63640.992572	33.310900
829.050412	63740.179244	33.315917
829.960766	63845.304233	33.320935
830.524867	63942.425553	33.325952
831.586571	64031.058229	33.330970
831.911296	64128.979690	33.335988
832.964691	64212.899513	33.341005
833.465982	64311.175937	33.346023
834.117586	64398.852362	33.351040
835.384148	64502.553651	33.356058
835.635080	64610.841733	33.361076
836.392925	64723.780708	33.366093
837.304780	64816.818123	33.371111
838.165817	64927.471132	33.376128
838.930728	65024.161733	33.381146
839.325859	65133.607838	33.386164
840.163250	65242.371476	33.391181
840.795838	65366.340740	33.396199
841.710209	65491.500858	33.401216
842.587177	65597.863052	33.406234
843.382955	65719.597794	33.411252
844.080079	65843.566179	33.416269
845.037940	65969.073061	33.421287
845.865694	66083.837613	33.426304
847.393552	66204.501912	33.431322
847.818108	66324.477142	33.436340
849.154104	66417.236872	33.441357
850.556771	66542.029209	33.446375
851.022053	66654.763929	33.451392
852.223927	66756.510461	33.456410
852.970839	66868.854172	33.461428
853.917423	66979.379016	33.466445
854.711282	67084.957206	33.471463
855.638096	67185.239973	33.476480
856.486241	67310.678274	33.481498
857.273170	67411.932058	33.486516
858.168135	67517.186967	33.491533
859.019717	67625.690135	33.496551
859.579394	67739.629065	33.501568
860.461437	67851.495795	33.506586
861.266054	67974.873209	33.511604
861.926695	68095.500949	33.516621
862.468637	68215.295463	33.521639
863.536050	68337.161371	33.526656
864.769158	68464.788583	33.531674
865.147210	68590.973298	33.536692
866.152244	68715.189018	33.541709
866.935472	68833.287380	33.546727
867.708239	68962.911690	33.551744
868.576606	69086.311259	33.556762
869.545569	69217.573930	33.561780
870.272298	69342.103272	33.566797
871.163260	69465.331050	33.571815
872.117859	69587.450153	33.576832
873.300801	69710.772004	33.581850
873.927561	69838.902709	33.586868
874.950727	69956.799073	33.591885
876.045029	70083.890308	33.596903
876.697101	70207.110214	33.601920
877.967178	70319.156763	33.606938
878.871079	70440.196188	33.611956
879.647503	70549.548906	33.616973
880.470599	70660.600743	33.621991
881.116528	70762.222861	33.627008
882.467343	70868.358371	33.632026
883.254824	70975.228575	33.637044
884.033814	71081.355133	33.642061
885.050735	71195.847956	33.647079
885.774698	71308.005986	33.652096
886.593589	71413.736232	33.657114
887.369296	71537.867277	33.662132
888.012793	71649.420825	33.667149
888.981461	71765.283122	33.672167
889.861568	71895.889047	33.677184
890.990312	72006.899805	33.682202
891.774909	72133.080427	33.687220
892.679557	72246.958995	33.692237
893.473583	72357.633213	33.697255
894.089533	72486.218794	33.702272
895.181444	72614.723147	33.707290
896.257096	72733.834630	33.712308
896.969040	72852.549734	33.717325
897.819449	72996.677621	33.722343
898.526353	73125.518251	33.727360
899.989281	73232.912394	33.732378
900.889173	73360.283072	33.737396
901.784942	73490.195533	33.742413
902.681109	73612.089668	33.747431
903.578555	73743.197839	33.752448
904.648937	73853.078062	33.757466
905.337291	73989.662042	33.762484
906.437489	74100.196088	33.767501
907.345105	74231.413264	33.772519
908.037439	74365.085910	33.777536
909.094705	74488.090920	33.782554
909.818550	74615.510224	33.787572
910.926399	74754.750059	33.792589
912.047036	74872.154497	33.797607
912.846715	75010.983808	33.802624
913.497603	75141.268218	33.807642
914.562510	75268.864893	33.812660
915.323822	75390.949268	33.817677
916.270636	75524.165682	33.822695
916.981999	75658.185143	33.827712
918.490887	75783.565668	33.832730
919.307341	75916.236615	33.837748
920.055720	76046.821025	33.842765
921.152214	76168.742998	33.847783
922.064410	76301.243230	33.852800
922.730630	76426.951423	33.857818
923.773759	76558.572966	33.862836
924.781052	76693.120993	33.867853
925.462880	76823.683066	33.872871
926.033173	76952.993348	33.877888
926.976648	77087.067472	33.882906
928.484546	77210.421831	33.887924
929.445626	77324.042054	33.892941
930.687543	77441.208227	33.897959
931.834719	77553.972145	33.902976
932.492651	77661.366263	33.907994
933.655046	77763.478886	33.913012
934.787421	77871.468595	33.918029
935.929271	77980.595075	33.923047
936.561047	78080.600463	33.928064
937.491676	78190.924667	33.933082
938.654621	78307.754419	33.938100
939.169263	78425.516004	33.943117
940.599602	78512.438948	33.948135
941.502238	78627.453637	33.953152
942.057034	78738.264077	33.958170
943.012501	78857.456035	33.963188
944.032059	78977.384354	33.968205
944.723633	79092.732310	33.973223
945.633265	79204.626573	33.978240
946.887277	79317.338949	33.983258
947.254677	79444.010804	33.988276
948.059955	79569.773062	33.993293
949.142344	79692.400969	33.998311
949.967924	79832.004850	34.003328
950.597741	79954.908598	34.008346
951.579217	80080.620646	34.013364
952.822599	80223.156959	34.018381
953.910281	80355.788228	34.023399
954.735450	80494.827724	34.028416
955.577273	80625.363213	34.033434
956.933674	80749.673211	34.038452
957.533723	80897.304131	34.043469
958.663371	81015.336633	34.048487
959.147542	81169.499089	34.053504
959.598693	81308.053554	34.058522
960.747366	81459.836655	34.063540
961.370411	81606.716666	34.068557
962.357323	81741.667584	34.073575
963.219970	81898.948728	34.078592
964.431078	82055.271592	34.083610
965.656250	82210.739934	34.088628
966.527756	82359.589740	34.093645
967.598376	82505.260583	34.098663
968.748780	82662.590190	34.103680
969.564846	82811.869280	34.108698
970.592326	82962.873342	34.113716
971.777165	83108.947462	34.118733
972.940907	83246.750199	34.123751
973.859418	83390.112167	34.128768
974.581068	83540.675897	34.133786
976.123000	83672.813390	34.138804
977.572547	83807.463744	34.143821
979.044140	83924.838653	34.148839
980.396653	84052.342733	34.153856
981.131714	84175.836207	34.158874
982.244334	84280.366038	34.163892
982.916214	84401.126912	34.168909
984.248026	84513.608395	34.173927
984.795306	84620.019133	34.178944
985.715538	84730.562982	34.183962
986.968794	84832.044621	34.188980
987.580834	84949.985585	34.193997
988.829369	85062.363099	34.199015
989.535230	85187.441472	34.204032
990.130643	85312.632994	34.209050
991.041004	85430.763109	34.214068
991.841834	85558.149036	34.219085
992.877451	85689.684148	34.224103
993.632033	85822.124704	34.229120
994.228244	85969.058307	34.234138
995.430917	86091.565362	34.239156
996.023234	86245.033185	34.244173
997.046268	86383.922003	34.249191
997.867606	86539.144945	34.254208
998.641898	86687.610652	34.259226
999.791258	86842.644498	34.264244
1000.492708	87000.526652	34.269261
1001.965209	87150.395757	34.274279
1002.530477	87313.309969	34.279296
1003.589818	87464.176528	34.284314
1004.745422	87625.310828	34.289332
1005.797230	87791.338295	34.294349
1007.152439	87942.470990	34.299367
1008.026175	88096.470058	34.304384
1008.813691	88254.739773	34.309402
1010.342591	88418.432289	34.314420
1011.010711	88575.496540	34.319437
1012.149633	88722.368930	34.324455
1013.333344	88880.694022	34.329472
1013.986848	89048.780191	34.334490
1015.385709	89211.354755	34.339508
1016.441343	89366.775773	34.344525
1017.365843	89521.409283	34.349543
1018.543775	89673.081847	34.354560
1019.768686	89834.752775	34.359578
1021.101923	89989.058971	34.364596
1021.783761	90150.217828	34.369613
1022.742530	90293.885154	34.374631
1023.869709	90432.701186	34.379648
1024.981494	90593.617836	34.384666
1026.336119	90744.725840	34.389684
1027.862399	90880.508759	34.394701
1028.604097	91022.286440	34.399719
1029.669180	91164.810485	34.404736
1030.406886	91324.425904	34.409754
1031.913287	91463.763676	34.414772
1032.516078	91616.534154	34.419789
1033.434364	91757.852084	34.424807
1034.599586	91917.871826	34.429824
1035.334579	92058.101358	34.434842
1036.331993	92201.009708	34.439860
1036.943144	92347.965085	34.444877
1038.145544	92500.039108	34.449895
1039.449266	92644.849673	34.454912
1040.245143	92782.727558	34.459930
1041.490725	92915.278675	34.464948
1042.477681	93064.816562	34.469965
1043.948646	93197.966024	34.474983
1045.123076	93337.994605	34.480000
1045.835743	93478.692085	34.485018
1046.984191	93609.162834	34.490036
1048.287910	93757.839043	34.495053
1049.328388	93897.013237	34.500071
1050.553463	94039.707452	34.505088
1051.440041	94185.283867	34.510106
1052.119830	94316.984523	34.515124
1052.803263	94472.298311	34.520141
1053.904947	94616.091161	34.525159
1055.007551	94775.856790	34.530176
1055.895179	94919.894380	34.535194
1057.276231	95074.873659	34.540212
1057.917585	95238.214020	34.545229
1058.608699	95403.635140	34.550247
1059.819067	95564.420329	34.555264
1060.511842	95737.877368	34.560282
1061.663807	95895.460693	34.565300
1062.792829	96067.370624	34.570317
1064.250444	96234.757147	34.575335
1065.340110	96400.020963	34.580352
1066.386027	96573.327029	34.585370
1067.756675	96725.662368	34.590388
1068.946161	96894.057980	34.595405
1069.887534	97060.950716	34.600423
1071.175626	97212.612902	34.605440
1072.140819	97381.870216	34.610458
1072.925629	97533.760095	34.615476
1074.287492	97711.914839	34.620493
1075.043409	97870.416285	34.625511
1077.029680	98029.165996	34.630528
1077.585626	98205.561165	34.635546
1078.934339	98359.093983	34.640564
1079.918071	98517.715521	34.645581
1080.952338	98682.840227	34.650599
1081.846618	98840.655763	34.655616
1082.874379	99012.566078	34.660634
1084.084873	99166.721002	34.665652
1085.185927	99338.565157	34.670669
1086.627440	99497.911509	34.675687
1088.034925	99659.251024	34.680704
1088.726342	99830.695810	34.685722
1090.223894	99978.344369	34.690740
1091.160502	100134.744796	34.695757
1092.102960	100299.648943	34.700775
1093.054715	100446.760919	34.705792
1094.462330	100606.778336	34.710810
1095.349977	100753.725295	34.715828
1096.505627	100898.801988	34.720845
1097.743969	101049.409137	34.725863
1099.191588	101178.034499	34.730880
1100.061975	101313.990871	34.735898
1101.331142	101459.483271	34.740916
1101.970994	101603.792196	34.745933
1103.012599	101750.037601	34.750951
1104.632529	101886.118548	34.755968
1105.289884	102040.513443	34.760986
1106.442452	102186.066883	34.766004
1107.641291	102340.263743	34.771021
1108.813491	102474.704535	34.776039
1110.591467	102611.372027	34.781056
1111.458707	102767.105116	34.786074
1112.402607	102909.614623	34.791092
1113.285511	103061.474567	34.796109
1113.902990	103213.124587	34.801127
1115.160631	103365.762176	34.806144
1116.150960	103535.313587	34.811162
1117.116921	103696.536116	34.816180
1118.284733	103856.987264	34.821197
1119.086421	104026.565873	34.826215
1120.503856	104179.607294	34.831232
1121.327066	104353.184195	34.836250
1122.402604	104527.019665	34.841268
1123.822798	104689.581585	34.846285
1124.806733	104860.871120	34.851303
1125.829156	105039.585257	34.856320
1126.801977	105212.239685	34.861338
1127.861349	105385.223335	34.866356
1129.120551	105565.485872	34.871373
1130.138226	105748.971437	34.876391
1131.531960	105923.241135	34.881408
1132.410939	106106.074336	34.886426
1133.737606	106278.446037	34.891444
1135.189350	106456.659490	34.896461
1135.623566	106642.466065	34.901479
1137.351869	106812.201916	34.906496
1138.200211	106996.875800	34.911514
1139.464667	107169.966294	34.916532
1140.900844	107345.207887	34.921549
1141.868840	107531.569328	34.926567
1143.322102	107711.975341	34.931584
1144.514644	107888.683659	34.936602
1145.729353	108061.592250	34.941620
1147.491210	108225.357991	34.946637
1148.311770	108402.008949	34.951655
1149.318078	108571.966917	34.956672
1150.302059	108744.138558	34.961690
1151.558708	108918.090917	34.966708
1152.473899	109096.529409	34.971725
1153.305452	109276.425623	34.976743
1154.704551	109443.599208	34.981760
1155.518866	109632.893780	34.986778
1156.842634	109803.847894	34.991796
1157.846297	109962.422681	34.996813
1158.509800	110142.092462	35.001831
1159.824785	110317.102552	35.006848
1161.170605	110490.070796	35.011866
1162.277357	110662.451620	35.016884
1163.273375	110836.402075	35.021901
1164.355061	111018.258857	35.026919
1165.561000	111202.287387	35.031936
1166.752661	111391.218984	35.036954
1167.116237	111575.719728	35.041972
1168.597530	111765.608275	35.046989
1169.765055	111970.689902	35.052007
1170.892595	112153.877064	35.057024
1172.012230	112354.639615	35.062042
1173.573129	112537.520144	35.067060
1175.063769	112722.673123	35.072077
1175.809513	112925.525435	35.077095
1177.138834	113107.643007	35.082112
1178.635449	113301.801225	35.087130
1179.894965	113499.163922	35.092148
1181.318020	113683.245907	35.097165
1182.345340	113877.635140	35.102183
1183.549680	114064.989658	35.107200
1184.936504	114248.201578	35.112218
1185.811940	114441.998908	35.117236
1187.240981	114632.626587	35.122253
1188.239842	114823.070870	35.127271
1189.722232	115007.355688	35.132288
1190.875665	115201.855360	35.137306
1192.008495	115403.393564	35.142324
1193.472766	115582.943515	35.147341
1194.607375	115776.861798	35.152359
1195.972497	115962.754981	35.157376
1196.814267	116162.401814	35.162394
1198.068714	116352.854918	35.167412
1199.052229	116547.461538	35.172429
1199.909148	116752.112302	35.177447
1201.275337	116951.992157	35.182464
1202.408303	117156.583266	35.187482
1203.222871	117368.362239	35.192500
1204.470758	117570.722347	35.197517
1205.591379	117777.935297	35.202535
1207.109148	117982.161543	35.207552
1208.647726	118194.598326	35.212570
1209.950174	118402.483871	35.217588
1211.017252	118609.002846	35.222605
1211.949172	118818.666565	35.227623
1213.165661	119024.690205	35.232640
1214.223329	119232.482020	35.237658
1215.658703	119441.963079	35.242676
1217.259746	119646.176534	35.247693
1218.499890	119864.841867	35.252711
1219.913660	120061.217524	35.257728
1221.279684	120248.053272	35.262746
1222.593386	120442.206096	35.267764
1223.677538	120621.173999	35.272781
1224.923782	120805.259216	35.277799
1226.209955	120984.716730	35.282816
1227.413467	121164.707871	35.287834
1228.628451	121352.778656	35.292852
1229.538628	121537.897626	35.297869
1230.687767	121731.440211	35.302887
1231.803848	121912.412901	35.307904
1233.389451	122101.253331	35.312922
1234.425250	122306.470226	35.317940
1235.682528	122495.732960	35.322957
1237.020851	122688.201217	35.327975
1238.413110	122873.442855	35.332992
1239.661248	123071.653109	35.338010
1240.881952	123268.007316	35.343028
1242.072722	123460.086631	35.348045
1243.581606	123659.868374	35.353063
1244.593713	123849.610337	35.358080
1245.818345	124061.194443	35.363098
1246.597395	124267.695852	35.368116
1248.131808	124458.676382	35.373133
1249.247525	124672.727233	35.378151
1250.125556	124877.634265	35.383168
1251.764832	125084.207840	35.388186
1252.714325	125295.693375	35.393204
1253.908343	125505.380987	35.398221
1255.551206	125714.048839	35.403239
1256.575643	125931.202237	35.408256
1258.143197	126137.959916	35.413274
1259.630644	126349.431471	35.418292
1260.932557	126550.926912	35.423309
1262.442521	126756.267019	35.428327
1263.887181	126958.160798	35.433344
1265.404404	127161.247961	35.438362
1266.730544	127362.137475	35.443380
1268.036110	127560.080117	35.448397
1269.404355	127759.293684	35.453415
1270.847740	127946.487437	35.458432
1272.579145	128130.608994	35.463450
1273.296576	128340.748805	35.468468
1274.627398	128519.780668	35.473485
1275.782288	128722.670908	35.478503
1276.886821	128914.967110	35.483520
1278.819180	129111.972447	35.488538
1279.550086	129309.208175	35.493556
1280.975566	129502.610273	35.498573
1282.041384	129702.113926	35.503591
1283.123050	129897.486412	35.508608
1284.507977	130096.524080	35.513626
1285.434572	130313.322111	35.518644
1286.808777	130511.262217	35.523661
1288.114445	130724.911883	35.528679
1289.269795	130924.828098	35.533696
1290.610053	131115.290241	35.538714
1291.545074	131320.641488	35.543732
1292.987125	131511.508222	35.548749
1294.381962	131696.948430	35.553767
1295.984948	131895.482712	35.558784
1297.512879	132078.002869	35.563802
1298.483464	132273.637553	35.568820
1300.137395	132448.462045	35.573837
1301.501959	132640.780421	35.578855
1302.299462	132838.549747	35.583872
1303.769396	133020.895121	35.588890
1304.505863	133221.134843	35.593908
1305.746766	133428.898090	35.598925
1307.139596	133631.887218	35.603943
1308.522882	133840.669806	35.608960
1309.852741	134037.285780	35.613978
1311.015546	134251.694214	35.618996
1312.049969	134456.963538	35.624013
1313.236275	134678.644543	35.629031
1314.049307	134899.588296	35.634048
1315.647969	135109.422881	35.639066
1316.580464	135349.966180	35.644084
1317.637999	135582.394531	35.649101
1319.069572	135818.807513	35.654119
1320.793806	136050.246618	35.659136
1322.000408	136280.439299	35.664154
1323.610160	136523.317606	35.669172
1324.796192	136749.943781	35.674189
1326.461786	136977.205118	35.679207
1327.600923	137205.996515	35.684224
1329.551958	137431.834730	35.689242
1331.129252	137652.006177	35.694260
1332.817793	137867.612177	35.699277
1334.497882	138086.744057	35.704295
1335.593710	138298.050027	35.709312
1336.929558	138521.459817	35.714330
1338.231912	138745.953798	35.719348
1339.596919	138956.283874	35.724365
1340.964459	139171.494133	35.729383
1341.933907	139387.428215	35.734400
1343.426033	139613.913581	35.739418
1344.495554	139846.576347	35.744436
1345.922421	140067.638672	35.749453
1347.196823	140289.918160	35.754471
1348.298667	140528.322142	35.759488
1349.996318	140752.857036	35.764506
1351.296192	140988.166145	35.769524
1352.733914	141204.089522	35.774541
1354.016116	141419.012564	35.779559
1355.255417	141651.129934	35.784576
1356.636739	141889.842401	35.789594
1358.200953	142112.989060	35.794612
1359.490286	142349.501751	35.799629
1360.668479	142575.526837	35.804647
1361.866927	142811.880100	35.809664
1363.555766	143032.047812	35.814682
1364.613755	143265.701845	35.819700
1365.750873	143477.012082	35.824717
1367.092332	143693.069719	35.829735
1368.480714	143922.544203	35.834752
1370.219603	144137.844662	35.839770
1371.279778	144337.841501	35.844788
1372.547161	144568.696235	35.849805
1374.123104	144775.636004	35.854823
1375.182299	145017.554680	35.859840
1376.396947	145248.232693	35.864858
1377.733579	145482.974565	35.869876
1379.121152	145716.974908	35.874893
1380.764339	145952.634930	35.879911
1382.049275	146171.963725	35.884928
1383.348139	146413.702962	35.889946
1384.899534	146646.251789	35.894964
1385.844752	146889.533965	35.899981
1387.816416	147127.812553	35.904999
1389.103102	147363.248191	35.910016
1390.331675	147607.226062	35.915034
1391.862291	147844.680080	35.920052
1393.059629	148084.457947	35.925069
1394.709630	148325.623500	35.930087
1395.846070	148575.074395	35.935104
1397.016646	148826.879712	35.940122
1398.436012	149074.578132	35.945140
1399.823629	149329.395372	35.950157
1401.451247	149580.385989	35.955175
1403.074670	149842.116921	35.960192
1404.512987	150078.613251	35.965210
1406.229030	150328.708185	35.970228
1407.918341	150573.357909	35.975245
1409.203271	150813.040673	35.980263
1410.558243	151062.209742	35.985280
1412.025547	151308.992086	35.990298
1413.597518	151550.092586	35.995316
1415.123785	151796.463524	36.000333
1416.617380	152041.408859	36.005351
1417.775787	152284.013077	36.010368
1419.297953	152526.738768	36.015386
1420.846560	152774.799667	36.020404
1421.994954	153022.697799	36.025421
1423.672238	153261.676710	36.030439
1425.094004	153513.693651	36.035456
1426.634986	153751.670748	36.040474
1427.922407	153997.221110	36.045492
1429.105055	154251.132715	36.050509
1430.666772	154503.768805	36.055527
1431.831397	154768.870162	36.060544
1432.986558	155014.144648	36.065562
1434.317110	155268.420778	36.070580
1435.673392	155532.217032	36.075597
1437.265236	155790.931419	36.080615
1438.996076	156044.198774	36.085632
1440.601669	156298.312094	36.090650
1442.451174	156532.848849	36.095668
1443.825121	156768.781487	36.100685
1445.107259	157000.875597	36.105703
1446.603022	157238.148864	36.110720
1447.762831	157466.664388	36.115738
1449.309937	157693.331960	36.120756
1450.452772	157943.257685	36.125773
1452.248817	158162.673628	36.130791
1453.284121	158409.589158	36.135808
1455.174339	158650.499457	36.140826
1456.549189	158882.185643	36.145844
1458.210856	159132.519324	36.150861
1459.556698	159368.423369	36.155879
1460.892682	159607.475450	36.160896
1462.455534	159852.820968	36.165914
1464.153409	160079.505419	36.170932
1465.447950	160329.208473	36.175949
1467.088083	160569.461501	36.180967
1468.557203	160810.225220	36.185984
1470.093154	161063.534649	36.191002
1471.571130	161307.102933	36.196020
1472.628646	161562.292700	36.201037
1474.179645	161810.912806	36.206055
1475.730741	162063.148951	36.211072
1476.814030	162314.167627	36.216090
1479.435399	162548.368251	36.221108
1480.664312	162807.610549	36.226125
1482.044255	163046.336239	36.231143
1483.512762	163298.264386	36.236160
1484.912318	163552.094907	36.241178
1486.659487	163790.386663	36.246196
1487.646946	164058.046657	36.251213
1489.310203	164310.369368	36.256231
1491.173577	164556.751863	36.261248
1492.544094	164808.084514	36.266266
1494.165860	165061.192616	36.271284
1495.167871	165325.561952	36.276301
1497.124868	165568.905088	36.281319
1498.153620	165836.951911	36.286336
1499.904076	166098.544370	36.291354
1501.911469	166342.759704	36.296372
1503.010907	166609.494456	36.301389
1504.884664	166855.395893	36.306407
1506.064150	167120.916624	36.311424
1507.338895	167376.454703	36.316442
1509.174108	167628.620372	36.321460
1510.715672	167877.967818	36.326477
1512.970293	168118.540489	36.331495
1514.688925	168370.222250	36.336512
1516.009127	168608.650655	36.341530
1517.654832	168853.967086	36.346548
1519.260153	169088.357666	36.351565
1520.774776	169327.723664	36.356583
1522.641104	169565.398989	36.361600
1523.836946	169807.038380	36.366618
1525.672704	170026.417669	36.371636
1526.905655	170257.906323	36.376653
1528.179949	170465.961111	36.381671
1529.145724	170686.179992	36.386688
1530.638325	170915.563690	36.391706
1532.033627	171158.042362	36.396724
1533.236212	171393.969626	36.401741
1534.599502	171638.346421	36.406759
1536.010878	171895.110511	36.411776
1537.287653	172135.635153	36.416794
1539.184448	172377.927510	36.421812
1540.567113	172640.954873	36.426829
1541.999763	172891.721845	36.431847
1543.547446	173145.516660	36.436864
1545.097367	173413.368443	36.441882
1546.538226	173666.714165	36.446900
1547.893705	173931.872864	36.451917
1549.348482	174199.643518	36.456935
1550.573316	174477.410981	36.461952
1552.131758	174746.183669	36.466970
1553.786966	175017.682977	36.471988
1555.232446	175305.252833	36.477005
1556.950818	175573.193658	36.482023
1558.693100	175857.827772	36.487040
1560.389171	176147.190584	36.492058
1562.276660	176411.608543	36.497076
1563.814619	176701.076479	36.502093
1565.064726	176977.499412	36.507111
1567.139216	177257.345559	36.512128
1568.764217	177540.715834	36.517146
1570.451293	177805.352124	36.522164
1571.664388	178080.722540	36.527181
1573.041822	178373.424732	36.532199
1575.266853	178641.304888	36.537216
1576.687272	178926.188730	36.542234
1578.613467	179207.022982	36.547252
1579.894089	179485.373376	36.552269
1582.047154	179753.589180	36.557287
1583.752315	180014.760022	36.562304
1584.904694	180289.621535	36.567322
1586.907331	180552.537377	36.572340
1588.548139	180829.177183	36.577357
1590.288629	181100.435902	36.582375
1591.912893	181364.254189	36.587392
1593.731311	181637.001079	36.592410
1595.285013	181908.852790	36.597428
1597.125115	182163.759872	36.602445
1598.705997	182423.125165	36.607463
1600.490940	182685.136843	36.612480
1601.832939	182956.127783	36.617498
1603.832466	183215.469312	36.622516
1605.160923	183479.651822	36.627533
1606.860254	183735.224771	36.632551
1608.817505	183980.949756	36.637568
1610.147784	184230.011338	36.642586
1611.801466	184464.608272	36.647604
1613.456204	184704.484900	36.652621
1615.280586	184923.259271	36.657639
1617.064510	185162.293026	36.662656
1618.392472	185400.689861	36.667674
1620.037660	185622.186185	36.672692
1621.466601	185862.003291	36.677709
1622.493032	186116.643384	36.682727
1624.144304	186351.415423	36.687744
1625.363191	186609.542676	36.692762
1627.046801	186878.789828	36.697780
1628.423297	187138.443145	36.702797
1629.975122	187397.651308	36.707815
1631.477161	187662.604637	36.712832
1632.786536	187942.488042	36.717850
1634.224919	188206.832761	36.722868
1635.622779	188498.989357	36.727885
1636.881920	188783.466872	36.732903
1638.492754	189072.344518	36.737920
1640.359905	189370.079126	36.742938
1642.159509	189659.387217	36.747956
1643.765134	189955.022339	36.752973
1645.225976	190244.692343	36.757991
1647.056420	190542.173581	36.763008
1648.373110	190843.621597	36.768026
1650.121806	191141.766735	36.773044
1651.880427	191455.420357	36.778061
1653.607173	191763.243226	36.783079
1655.271033	192061.788193	36.788096
1657.116757	192367.489254	36.793114
1658.772655	192676.306311	36.798132
1660.301575	192987.645638	36.803149
1661.997839	193290.787122	36.808167
1664.144155	193588.896642	36.813184
1665.424223	193904.418610	36.818202
1667.391763	194196.404763	36.823220
1669.259725	194505.440596	36.828237
1670.554495	194813.097100	36.833255
1672.869783	195122.560639	36.838272
1674.376195	195418.472670	36.843290
1675.926842	195725.852901	36.848308
1677.690608	196037.287959	36.853325
1679.663868	196332.750362	36.858343
1681.432642	196641.040624	36.863360
1682.801368	196950.195850	36.868378
1684.853134	197249.522133	36.873396
1686.655460	197561.277506	36.878413
1687.857479	197864.664176	36.883431
1689.903834	198181.664533	36.888448
1691.494110	198478.519876	36.893466
1693.008733	198783.537588	36.898484
1694.797750	199088.246922	36.903501
1696.345819	199398.708016	36.908519
1698.498974	199702.969537	36.913536
1699.685920	200007.589275	36.918554
1701.821623	200294.162890	36.923572
1703.559814	200569.580429	36.928589
1705.150222	200851.572493	36.933607
1706.945676	201129.370067	36.938624
1708.923047	201415.606583	36.943642
1710.419962	201689.874869	36.948660
1712.051468	201974.519050	36.953677
1713.675849	202260.650952	36.958695
1715.393439	202536.398886	36.963712
1717.224010	202824.138392	36.968730
1718.906605	203121.220020	36.973748
1720.547280	203407.101284	36.978765
1722.354888	203688.641586	36.983783
1724.032157	203977.084046	36.988800
1726.158175	204270.889712	36.993818
1727.954475	204551.001628	36.998836
1729.605132	204844.999938	37.003853
1731.067873	205139.054960	37.008871
1733.226373	205417.476007	37.013888
1734.840299	205717.400037	37.018906
1736.793647	206005.846825	37.023924
1738.375804	206296.042308	37.028941
1739.821373	206592.608115	37.033959
1741.891677	206888.390707	37.038976
1743.359203	207194.121445	37.043994
1745.230073	207488.123337	37.049012
1746.855717	207779.893246	37.054029
1748.749453	208089.800879	37.059047
1750.850410	208379.251233	37.064064
1752.472834	208690.969572	37.069082
1754.169286	208986.517081	37.074100
1755.878091	209282.076739	37.079117
1757.253243	209590.957114	37.084135
1759.264809	209888.959823	37.089152
1761.249322	210203.078435	37.094170
1762.885056	210506.069475	37.099188
1764.884109	210821.928112	37.104205
1766.380383	211121.313376	37.109223
1768.773923	211415.974549	37.114240
1770.311619	211719.355097	37.119258
1771.966570	212027.073032	37.124276
1774.198555	212325.509204	37.129293
1775.553298	212638.851070	37.134311
1777.284614	212946.269230	37.139328
1779.034863	213255.577495	37.144346
1780.629957	213569.418866	37.149364
1782.497706	213879.016092	37.154381
1784.158827	214193.852903	37.159399
1786.292376	214504.667732	37.164416
1787.989453	214815.591373	37.169434
1789.358742	215134.567045	37.174452
1791.468547	215432.884207	37.179469
1793.117139	215754.433853	37.184487
1795.101478	216065.939704	37.189504
1797.007006	216369.752773	37.194522
1798.749443	216662.674136	37.199540
1800.686487	216951.236338	37.204557
1802.193672	217245.390951	37.209575
1804.122232	217521.336490	37.214592
1806.165571	217815.408365	37.219610
1807.725005	218098.448673	37.224628
1809.842205	218379.192330	37.229645
1811.429240	218670.356418	37.234663
1813.393516	218960.357170	37.239680
1815.272664	219249.102905	37.244698
1817.181612	219539.495652	37.249716
1819.189501	219838.990274	37.254733
1820.529401	220122.644670	37.259751
1822.415312	220419.393048	37.264768
1824.352358	220719.753171	37.269786
1825.978822	221019.427359	37.274804
1827.755490	221342.175164	37.279821
1829.862477	221672.591861	37.284839
1831.628037	221967.994119	37.289856
1833.436312	222269.168044	37.294874
1835.223936	222569.876616	37.299892
1837.203125	222879.025169	37.304909
1838.692634	223186.335341	37.309927
1840.837439	223487.803391	37.314944
1842.619680	223795.590073	37.319962
1844.230528	224109.957155	37.324980
1846.347875	224414.518612	37.329997
1848.049408	224732.479892	37.335015
1850.132223	225054.546790	37.340032
1851.888307	225366.013295	37.345050
1853.690927	225684.330476	37.350068
1856.026597	225990.717064	37.355085
1857.873218	226312.927956	37.360103
1859.446217	226627.590066	37.365120
1861.479131	226953.227721	37.370138
1863.408736	227255.848542	37.375156
1865.588514	227562.367176	37.380173
1867.499976	227880.103959	37.385191
1869.438582	228184.199620	37.390208
1871.532940	228493.706517	37.395226
1873.251375	228809.064639	37.400244
1875.338163	229108.314598	37.405261
1876.872892	229431.424743	37.410279
1878.615303	229733.652109	37.415296
1880.761986	230050.191110	37.420314
1882.439453	230361.091307	37.425332
1884.848117	230663.749376	37.430349
1886.918310	230976.595722	37.435367
1888.600121	231286.660246	37.440384
1890.480812	231592.325855	37.445402
1892.525618	231901.369698	37.450420
1894.788836	232187.674320	37.455437
1896.419579	232494.195240	37.460455
1898.669785	232790.967633	37.465472
1900.780126	233084.512197	37.470490
1902.394294	233370.110609	37.475508
1904.224826	233637.947640	37.480525
1905.885503	233909.291904	37.485543
1907.575960	234186.702364	37.490560
1909.792087	234461.185562	37.495578
1911.192615	234752.511080	37.500596
1913.310016	235023.836679	37.505613
1915.184419	235317.780852	37.510631
1916.640253	235606.509381	37.515648
1918.351065	235890.118519	37.520666
1920.389296	236191.125404	37.525684
1922.149391	236493.726616	37.530701
1924.223023	236788.608475	37.535719
1925.755161	237086.675752	37.540736
1927.826812	237391.515976	37.545754
1929.520792	237707.110010	37.550772
1931.290970	238013.980948	37.555789
1933.358668	238331.193817	37.560807
1934.923989	238657.783462	37.565824
1937.323684	238973.726306	37.570842
1939.396019	239297.799009	37.575860
1941.301729	239619.181323	37.580877
1943.198152	239934.089108	37.585895
1944.902183	240254.133609	37.590912
1947.396553	240583.553074	37.595930
1949.087151	240912.186605	37.600948
1951.232302	241229.826962	37.605965
1953.015676	241554.637547	37.610983
1955.016595	241886.856681	37.616000
1957.391549	242209.060529	37.621018
1959.172091	242535.804558	37.626036
1961.274061	242864.225648	37.631053
1963.484245	243192.249414	37.636071
1965.493422	243514.717839	37.641088
1967.338562	243834.266649	37.646106
1969.091759	244168.969505	37.651124
1971.102800	244485.013709	37.656141
1973.435786	244822.598077	37.661159
1975.738383	245148.249806	37.666176
1978.023312	245458.918695	37.671194
1979.562883	245791.729015	37.676212
1981.881360	246113.468784	37.681229
1983.867925	246438.208452	37.686247
1985.483765	246757.317870	37.691264
1987.800149	247086.147028	37.696282
1989.374534	247411.970325	37.701300
1991.845756	247729.777701	37.706317
1993.883935	248057.713322	37.711335
1995.439968	248387.123219	37.716352
1997.786690	248713.969850	37.721370
1999.595604	249043.595040	37.726388
2001.634392	249367.062718	37.731405
2003.853107	249685.777841	37.736423
2005.559148	250016.589834	37.741440
2007.847989	250336.539784	37.746458
2009.601161	250652.841309	37.751476
2011.706560	250942.441245	37.756493
2013.912452	251240.281275	37.761511
2015.461427	251543.331788	37.766528
2017.541420	251842.234301	37.771546
2019.997001	252134.651081	37.776564
2022.351837	252418.701720	37.781581
2024.677058	252713.350087	37.786599
2026.316656	253006.050147	37.791616
2028.198376	253297.823190	37.796634
2030.091424	253594.954709	37.801652
2032.194647	253892.129556	37.806669
2034.230190	254198.866777	37.811687
2035.539919	254513.264053	37.816704
2037.522744	254820.036005	37.821722
2039.695995	255154.923845	37.826740
2041.115991	255482.184047	37.831757
2043.326054	255811.351605	37.836775
2045.083097	256138.813380	37.841792
2047.009109	256466.960111	37.846810
2049.324478	256816.586792	37.851828
2051.259420	257150.042216	37.856845
2053.071261	257492.078286	37.861863
2054.958579	257850.944745	37.866880
2057.275763	258191.809360	37.871898
2059.473577	258547.477690	37.876916
2061.233133	258897.729089	37.881933
2063.778852	259259.744701	37.886951
2065.539637	259611.978288	37.891968
2067.713811	259961.225455	37.896986
2070.128216	260314.423196	37.902004
2072.381039	260660.178601	37.907021
2074.917269	261003.196773	37.912039
2076.874872	261348.542586	37.917056
2079.545173	261691.565697	37.922074
2081.415569	262040.482536	37.927092
2083.489361	262384.845778	37.932109
2086.133875	262719.059289	37.937127
2088.220240	263065.732922	37.942144
2090.194013	263393.778964	37.947162
2092.147535	263744.437217	37.952180
2094.003541	264084.848445	37.957197
2096.436154	264428.115279	37.962215
2098.055650	264780.885136	37.967232
2100.278068	265118.521027	37.972250
2102.144530	265477.018823	37.977268
2104.327733	265816.084071	37.982285
2106.849616	266155.603923	37.987303
2108.604839	266521.614144	37.992320
2110.480074	266866.393925	37.997338
2112.917359	267219.950522	38.002356
2115.062746	267571.623011	38.007373
2117.442939	267914.977019	38.012391
2119.390197	268268.307180	38.017408
2121.561376	268599.196328	38.022426
2123.646766	268937.034357	38.027444
2125.235468	269256.432318	38.032461
2127.667739	269575.544208	38.037479
2130.082305	269891.559836	38.042496
2132.835487	270188.240745	38.047514
2134.972851	270495.739646	38.052532
2137.031686	270806.045477	38.057549
2139.316867	271123.403050	38.062567
2141.195479	271450.046628	38.067584
2143.249527	271759.642207	38.072602
2145.221794	272076.338380	38.077620
2147.115056	272404.046825	38.082637
2149.116910	272729.756652	38.087655
2151.184799	273064.829921	38.092672
2153.605263	273393.852124	38.097690
2155.387034	273738.192307	38.102708
2157.155125	274082.052032	38.107725
2159.424055	274427.102525	38.112743
2161.616839	274775.086504	38.117760
2163.613588	275119.519699	38.122778
2166.075994	275479.121091	38.127796
2167.965253	275834.647205	38.132813
2170.240386	276188.105228	38.137831
2172.489621	276550.864971	38.142848
2174.566706	276908.241040	38.147866
2176.664069	277268.077963	38.152884
2178.906466	277630.127314	38.157901
2181.534537	277986.729902	38.162919
2183.666910	278353.089695	38.167936
2185.814245	278714.340928	38.172954
2188.366786	279080.583054	38.177972
2190.542235	279443.125150	38.182989
2192.559220	279807.013207	38.188007
2194.367484	280177.742300	38.193024
2196.315451	280540.650247	38.198042
2198.920098	280906.426067	38.203060
2201.125173	281283.137666	38.208077
2203.581730	281646.497852	38.213095
2205.704620	282019.690991	38.218112
2207.920507	282398.965922	38.223130
2210.420235	282769.025020	38.228148
2212.733479	283133.473916	38.233165
2215.425515	283509.928999	38.238183
2217.426890	283883.724360	38.243200
2219.720701	284248.429525	38.248218
2221.820755	284612.885679	38.253236
2223.852824	284984.109527	38.258253
2226.557232	285332.185834	38.263271
2228.437332	285710.545971	38.268288
2230.825624	286075.615576	38.273306
2233.408452	286448.046248	38.278324
2235.382347	286821.411385	38.283341
2237.731677	287175.054704	38.288359
2239.918799	287544.396976	38.293376
2242.317792	287889.216843	38.298394
2244.548511	288240.159706	38.303412
2246.464059	288575.249965	38.308429
2248.821371	288900.235696	38.313447
2250.649856	289242.883642	38.318464
2253.040417	289575.153945	38.323482
2255.214591	289916.374519	38.328500
2257.055540	290270.933108	38.333517
2258.960269	290616.463172	38.338535
2261.104629	290982.378492	38.343552
2263.334067	291337.661519	38.348570
2265.672388	291701.919280	38.353588
2267.410243	292075.314994	38.358605
2269.698080	292447.378205	38.363623
2271.819276	292823.658646	38.368640
2274.356984	293203.835204	38.373658
2276.544037	293591.179368	38.378676
2278.609509	293986.391432	38.383693
2281.330897	294366.232031	38.388711
2283.132667	294760.747802	38.393728
2285.685212	295161.341914	38.398746
2287.966291	295547.295861	38.403764
2289.840362	295953.787635	38.408781
2292.661951	296342.346947	38.413799
2295.269186	296743.589622	38.418816
2297.425193	297144.140919	38.423834
2300.240600	297544.205780	38.428852
2302.340644	297938.337546	38.433869
2304.414616	298328.230485	38.438887
2307.145887	298736.510762	38.443904
2309.704324	299128.941470	38.448922
2312.053987	299520.540713	38.453940
2314.046104	299932.720112	38.458957
2316.893879	300326.245196	38.463975
2318.951398	300727.057779	38.468992
2321.326319	301129.470117	38.474010
2323.760324	301526.283783	38.479028
2326.151051	301932.425512	38.484045
2328.502953	302331.129789	38.489063
2330.892772	302735.034200	38.494080
2333.248552	303135.513770	38.499098
2335.845519	303529.222770	38.504116
2337.998518	303936.692100	38.509133
2340.540659	304320.374281	38.514151
2343.128216	304719.187002	38.519168
2345.310704	305124.108116	38.524186
2348.016818	305515.558946	38.529204
2349.986066	305919.495449	38.534221
2352.389408	306322.955501	38.539239
2354.718580	306716.189748	38.544256
2356.783352	307119.523183	38.549274
2359.676658	307517.542383	38.554292
2361.516370	307921.493135	38.559309
2364.198818	308313.040811	38.564327
2367.151538	308707.058984	38.569344
2369.467418	309092.693288	38.574362
2372.347253	309452.100654	38.579380
2374.576958	309803.812290	38.584397
2377.072150	310160.865498	38.589415
2379.363751	310513.454170	38.594432
2381.621542	310860.992637	38.599450
2384.215046	311212.667721	38.604468
2385.912998	311569.665101	38.609485
2388.200220	311936.651408	38.614503
2390.396685	312284.068190	38.619520
2392.286566	312674.710759	38.624538
2394.798616	313051.842687	38.629556
2397.023540	313438.340162	38.634573
2399.447203	313814.924629	38.639591
2401.660350	314204.367420	38.644608
2403.539632	314606.332348	38.649626
2406.458997	314985.932634	38.654644
2408.845923	315387.153685	38.659661
2411.255836	315789.309234	38.664679
2413.861664	316187.749388	38.669696
2415.919200	316594.199022	38.674714
2418.079043	316992.224046	38.679732
2420.357271	317410.699316	38.684749
2423.005210	317825.787074	38.689767
2425.484593	318251.490532	38.694784
2427.464277	318681.639629	38.699802
2430.160768	319097.298240	38.704820
2432.605454	319525.693512	38.709837
2435.189928	319958.432932	38.714855
2438.051979	320376.523024	38.719872
2440.345520	320818.091795	38.724890
2442.429393	321229.799625	38.729908
2445.342371	321662.427952	38.734925
2448.042482	322084.472133	38.739943
2450.871114	322512.309663	38.744960
2453.138554	322934.291271	38.749978
2456.193149	323345.657443	38.754996
2458.641765	323772.025096	38.760013
2460.994988	324192.666225	38.765031
2463.578906	324606.487998	38.770048
2465.766394	325032.204869	38.775066
2468.799608	325437.596085	38.780084
2471.402521	325864.233188	38.785101
2473.984948	326269.996393	38.790119
2476.370693	326693.184336	38.795136
2478.568993	327116.653663	38.800154
2481.158857	327525.786762	38.805172
2483.708532	327942.644060	38.810189
2486.141138	328364.037882	38.815207
2488.970632	328776.859364	38.820224
2491.059671	329197.058692	38.825242
2493.719277	329616.835140	38.830260
2496.560088	330025.305587	38.835277
2498.978840	330443.642685	38.840295
2501.483409	330847.946483	38.845312
2504.055572	331257.062109	38.850330
2506.510212	331638.794548	38.855348
2508.980569	332020.598653	38.860365
2511.221213	332414.651224	38.865383
2513.705653	332780.273591	38.870400
2515.546511	333169.205134	38.875418
2518.190578	333565.701251	38.880436
2520.301742	333963.803104	38.885453
2522.556449	334371.960720	38.890471
2524.956752	334777.045767	38.895488
2526.965547	335196.943272	38.900506
2529.826658	335604.641942	38.905524
2532.268302	336018.752559	38.910541
2534.171140	336460.242012	38.915559
2537.228844	336896.238731	38.920576
2539.616667	337327.565131	38.925594
2542.161629	337757.797363	38.930612
2544.683045	338194.327441	38.935629
2546.898945	338641.287809	38.940647
2549.571617	339085.100425	38.945664
2551.990698	339547.789834	38.950682
2554.451209	340004.197897	38.955700
2556.810330	340463.233880	38.960717
2559.272586	340925.296926	38.965735
2561.918438	341394.487327	38.970752
2564.454275	341876.868718	38.975770
2567.432691	342347.624049	38.980788
2569.933640	342824.113131	38.985805
2572.644250	343300.235165	38.990823
2575.707915	343773.783989	38.995840
2577.895010	344242.694863	39.000858
2580.492617	344712.247841	39.005876
2583.470155	345194.329345	39.010893
2585.916633	345667.960656	39.015911
2588.965172	346140.477195	39.020928
2591.339528	346625.739587	39.025946
2594.014202	347103.740294	39.030964
2596.352379	347584.405128	39.035981
2599.144644	348064.993914	39.040999
2602.176014	348543.332052	39.046016
2604.758314	349024.326607	39.051034
2607.870718	349488.579682	39.056052
2610.473002	349962.683205	39.061069
2613.213384	350440.847815	39.066087
2616.078507	350908.834245	39.071104
2618.733702	351386.445474	39.076122
2621.341305	351850.961295	39.081140
2623.925657	352310.653617	39.086157
2626.333106	352788.849926	39.091175
2629.230576	353254.703611	39.096192
2631.333284	353738.194060	39.101210
2633.931898	354202.944291	39.106228
2636.631741	354673.715599	39.111245
2639.504888	355152.958566	39.116263
2642.504948	355627.557175	39.121280
2645.094841	356076.401845	39.126298
2647.740464	356517.415800	39.131316
2650.490435	356943.433659	39.136333
2653.053905	357379.249588	39.141351
2655.709826	357804.919591	39.146368
2658.205071	358240.764097	39.151386
2660.513155	358667.928473	39.156404
2663.103276	359101.948169	39.161421
2665.404718	359560.020274	39.166439
2667.919808	360003.739351	39.171456
2670.616658	360459.481353	39.176474
2673.275601	360908.752992	39.181492
2676.707669	361346.146893	39.186509
2679.638883	361789.021997	39.191527
2682.377158	362245.755425	39.196544
2684.899457	362693.508881	39.201562
2687.532048	363154.310851	39.206580
2690.119105	363606.385073	39.211597
2692.367170	364068.304721	39.216615
2695.134812	364533.055939	39.221632
2697.723773	365008.844842	39.226650
2700.518713	365478.226262	39.231668
2703.241073	365944.721229	39.236685
2705.455351	366434.359848	39.241703
2708.431927	366908.062423	39.246720
2711.075705	367399.754061	39.251738
2713.671189	367887.514496	39.256756
2716.343675	368381.068475	39.261773
2718.618759	368892.544485	39.266791
2721.228822	369386.705961	39.271808
2723.892039	369899.580387	39.276826
2726.621464	370408.885688	39.281844
2729.659802	370915.319393	39.286861
2732.067786	371446.130234	39.291879
2735.216301	371946.520410	39.296896
2737.906732	372461.313384	39.301914
2741.044589	372974.938100	39.306932
2744.152427	373484.577627	39.311949
2746.962537	374003.519123	39.316967
2749.726079	374505.233464	39.321984
2752.563830	375018.271305	39.327002
2755.233119	375526.762405	39.332020
2758.335402	376036.573995	39.337037
2760.899788	376554.786094	39.342055
2763.403896	377065.846425	39.347072
2766.318554	377584.015091	39.352090
2769.011274	378102.668798	39.357108
2772.169001	378604.345651	39.362125
2774.501872	379132.860953	39.367143
2777.659854	379643.784376	39.372160
2780.751361	380167.015565	39.377178
2783.323304	380678.271846	39.382196
2786.632540	381178.876752	39.387213
2789.257544	381696.579995	39.392231
2792.314804	382203.071385	39.397248
2794.844803	382701.014620	39.402266
2797.624914	383189.322981	39.407284
2800.427860	383651.290811	39.412301
2802.970306	384126.865175	39.417319
2805.802314	384588.943642	39.422336
2808.506216	385061.842426	39.427354
2811.029174	385535.169653	39.432372
2814.229793	386010.539529	39.437389
2816.817268	386486.152502	39.442407
2819.934569	386961.117374	39.447424
2823.077137	387439.369362	39.452442
2825.428679	387926.034194	39.457460
2828.205393	388401.693529	39.462477
2830.717967	388889.486536	39.467495
2833.620954	389383.171298	39.472512
2836.356534	389886.259763	39.477530
2838.759962	390393.324766	39.482548
2841.505099	390902.839172	39.487565
2844.314151	391424.281187	39.492583
2847.528742	391925.007503	39.497600
2850.375696	392445.768853	39.502618
2852.593817	392970.806333	39.507636
2855.563248	393491.507170	39.512653
2858.293374	394030.623476	39.517671
2860.614991	394571.216042	39.522688
2863.533794	395116.777172	39.527706
2866.324920	395652.333282	39.532724
2869.223324	396213.931573	39.537741
2872.234025	396784.555212	39.542759
2875.334012	397337.506635	39.547776
2878.060581	397896.517429	39.552794
2880.552505	398466.813956	39.557812
2883.797931	399029.704300	39.562829
2886.541844	399598.546737	39.567847
2889.578811	400181.556801	39.572864
2892.730732	400751.379394	39.577882
2895.816370	401321.836275	39.582900
2898.757580	401882.494190	39.587917
2901.815077	402465.028713	39.592935
2904.616533	403029.009851	39.597952
2907.544550	403608.096016	39.602970
2910.423572	404197.421297	39.607988
2913.651475	404762.926472	39.613005
2916.243943	405336.634171	39.618023
2919.397450	405908.873608	39.623040
2922.538454	406489.495174	39.628058
2925.207730	407068.431409	39.633076
2929.080534	407632.311969	39.638093
2932.217659	408203.472112	39.643111
2935.173644	408776.399215	39.648128
2938.618045	409317.224692	39.653146
2941.282761	409891.038625	39.658164
2944.119684	410438.504953	39.663181
2947.664204	410986.432246	39.668199
2950.494861	411544.245767	39.673216
2953.617603	412078.305150	39.678234
2956.541615	412587.928986	39.683252
2959.640325	413098.276692	39.688269
2962.012138	413609.212109	39.693287
2964.958990	414112.824817	39.698304
2967.644873	414629.673671	39.703322
2969.968980	415158.430750	39.708340
2972.955581	415679.445463	39.713357
2975.964669	416211.141233	39.718375
2978.559508	416738.660811	39.723392
2981.271040	417283.130236	39.728410
2983.627896	417840.644741	39.733428
2986.435236	418396.075208	39.738445
2989.237535	418968.675308	39.743463
2991.976127	419539.170778	39.748480
2995.114689	420110.604873	39.753498
2997.780147	420710.986648	39.758516
3000.426025	421302.136017	39.763533
3003.590430	421899.524774	39.768551
3006.266889	422494.849635	39.773568
3009.666026	423097.825118	39.778586
3012.483825	423699.967281	39.783604
3015.850651	424318.197663	39.788621
3018.694109	424941.436801	39.793639
3021.506297	425563.095899	39.798656
3024.993242	426177.718192	39.803674
3028.204176	426816.916399	39.808692
3031.423406	427434.870630	39.813709
3034.663836	428061.090196	39.818727
3037.417482	428691.500746	39.823744
3040.572864	429315.348393	39.828762
3043.301288	429945.808895	39.833780
3046.510844	430581.547610	39.838797
3049.465597	431227.264784	39.843815
3052.443730	431875.418884	39.848832
3055.673614	432518.477006	39.853850
3058.571926	433169.523713	39.858868
3061.681990	433816.949582	39.863885
3065.126192	434471.650164	39.868903
3067.873926	435122.164407	39.873920
3071.347570	435775.940341	39.878938
3074.604884	436429.176457	39.883956
3077.461866	437069.924756	39.888973
3080.501153	437732.201182	39.893991
3083.497948	438389.757161	39.899008
3086.987441	439037.191218	39.904026
3090.129974	439703.247241	39.909044
3093.437745	440352.549091	39.914061
3096.640061	441008.838049	39.919079
3099.994965	441656.224324	39.924096
3103.466483	442296.992704	39.929114
3106.814144	442946.826663	39.934132
3109.950577	443583.259680	39.939149
3113.280924	444214.278559	39.944167
3116.267765	444854.802382	39.949184
3119.797748	445473.150307	39.954202
3122.665532	446079.032064	39.959220
3125.559106	446661.050769	39.964237
3128.659203	447246.262236	39.969255
3131.657337	447841.295649	39.974272
3134.586983	448430.047990	39.979290
3137.592064	449030.516917	39.984308
3140.374327	449628.120439	39.989325
3143.247163	450223.315305	39.994343
3145.804932	450845.218265	39.999360
3148.744127	451461.577921	40.004378
3151.630176	452099.388590	40.009396
3154.503135	452749.582927	40.014413
3157.579224	453398.107095	40.019431
3160.998984	454038.562464	40.024448
3164.398306	454688.719160	40.029466
3167.304176	455332.963864	40.034484
3170.569179	455990.441724	40.039501
3174.303299	456634.973369	40.044519
3177.075484	457320.927743	40.049536
3180.428042	457973.981622	40.054554
3183.555927	458643.900373	40.059572
3186.446918	459314.544543	40.064589
3189.601646	459989.376341	40.069607
3193.017582	460676.035058	40.074624
3196.063202	461372.848727	40.079642
3199.102625	462053.351481	40.084660
3202.078402	462752.307112	40.089677
3204.959840	463447.562249	40.094695
3208.147662	464178.812505	40.099712
3211.285404	464887.182653	40.104730
3214.254861	465622.009269	40.109748
3217.160112	466351.560421	40.114765
3220.709736	467088.823833	40.119783
3224.061798	467817.545496	40.124800
3227.232053	468558.559832	40.129818
3230.465389	469311.219846	40.134836
3233.833105	470044.362121	40.139853
3237.218146	470778.487054	40.144871
3240.256353	471534.889685	40.149888
3243.835447	472263.823816	40.154906
3247.405704	473005.677309	40.159924
3250.651831	473748.616841	40.164941
3254.306590	474488.127716	40.169959
3257.676205	475243.986451	40.174976
3261.231196	475974.307939	40.179994
3264.188673	476718.498308	40.185012
3267.484051	477468.168175	40.190029
3271.151249	478185.197401	40.195047
3274.296719	478942.367253	40.200064
3277.691901	479661.610166	40.205082
3281.303022	480407.985105	40.210100
3284.466530	481140.756235	40.215117
3288.326345	481873.642514	40.220135
3290.997038	482600.877433	40.225152
3294.684777	483306.143309	40.230170
3298.031247	484005.524959	40.235188
3301.245397	484679.888664	40.240205
3304.510571	485355.231263	40.245223
3307.496843	486043.580072	40.250240
3310.672535	486716.716028	40.255258
3313.998296	487402.132606	40.260276
3317.010365	488080.753375	40.265293
3320.351348	488778.041280	40.270311
3323.561604	489473.707436	40.275328
3326.708298	490169.357885	40.280346
3329.825235	490878.070812	40.285364
3333.099705	491582.741318	40.290381
3336.972138	492290.018231	40.295399
3339.974739	493014.124525	40.300416
3342.955232	493736.539172	40.305434
3346.114050	494465.665101	40.310452
3349.041784	495205.202432	40.315469
3352.383663	495952.926707	40.320487
3355.478382	496703.891374	40.325504
3358.866360	497460.232385	40.330522
3362.080901	498227.274287	40.335540
3364.940773	499002.772051	40.340557
3368.078288	499772.638415	40.345575
3371.238583	500580.637819	40.350592
3374.524190	501372.324086	40.355610
3377.801738	502163.118132	40.360628
3381.408413	502988.909984	40.365645
3385.104900	503790.418668	40.370663
3388.464601	504606.027294	40.375680
3391.658234	505419.857572	40.380698
3395.294994	506232.873234	40.385716
3398.686837	507055.731345	40.390733
3402.601047	507870.039637	40.395751
3405.864873	508696.372698	40.400768
3409.350964	509521.974911	40.405786
3413.015492	510339.788646	40.410804
3416.465271	511170.262217	40.415821
3420.257188	511988.430844	40.420839
3423.458954	512816.491708	40.425856
3427.763337	513621.886990	40.430874
3431.523472	514437.015901	40.435892
3434.990214	515262.795717	40.440909
3438.596136	516064.602449	40.445927
3442.137446	516876.771700	40.450944
3445.332799	517690.216875	40.455962
3448.759079	518497.785383	40.460980
3452.278482	519310.796903	40.465997
3455.748203	520123.523892	40.471015
3459.400851	520935.626911	40.476032
3462.747045	521730.744286	40.481050
3466.548330	522540.726740	40.486068
3469.832059	523361.691940	40.491085
3473.315035	524158.584607	40.496103
3476.714325	524973.247994	40.501120
3480.116459	525759.633513	40.506125
3483.550817	526510.137462	40.511130
3486.318315	527223.970366	40.516135
3489.532129	527866.596683	40.521140
3492.483691	528467.547835	40.526144
3494.833126	529000.403281	40.531149
3497.483395	529459.418232	40.536154
3500.030567	529881.397975	40.541159
3502.757636	530249.525332	40.546164
3504.909103	530536.487097	40.551168
3506.896314	530788.858861	40.556173
3508.921738	530985.591490	40.561178
3510.230479	531145.551352	40.566183
3511.915561	531242.243236	40.571188
3513.352961	531309.517647	40.576192
3514.722644	531348.407542	40.581197
3516.328608	531325.821840	40.586202
3516.909976	531297.183467	40.591207
3518.016663	531221.322044	40.596212
3518.692164	531131.078108	40.601216
3519.099172	531003.032205	40.606221
3519.744046	530857.617115	40.611226
3520.102495	530697.138403	40.616231
3520.447171	530520.188274	40.621236
3520.655867	530325.219114	40.626240
3521.137732	530118.885920	40.631245
3521.604960	529899.919969	40.636250
3521.302444	529669.400148	40.641255
3521.539378	529428.483378	40.646260
3521.753849	529201.664836	40.651264
3521.701816	528935.924588	40.656269
3521.879779	528676.763400	40.661274
3521.914617	528407.564272	40.666279
3521.865977	528142.062826	40.671284
3521.661278	527871.881754	40.676288
3521.714170	527607.921936	40.681293
3521.711415	527319.101987	40.686298
3521.262176	527051.725191	40.691303
3521.274442	526761.983063	40.696308
3521.078102	526473.127827	40.701312
3520.856430	526201.455408	40.706317
3521.241306	525930.996604	40.711322
3521.116079	525648.635159	40.716327
3521.187088	525350.265839	40.721332
3520.887626	525076.211053	40.726336
3520.546229	524783.102481	40.731341
3520.490370	524498.485820	40.736346
3519.849463	524223.762808	40.741351
3519.598642	523939.622007	40.746356
3519.420057	523673.561417	40.751360
3519.160100	523400.735594	40.756365
3518.890020	523126.794646	40.761370
3518.252695	522880.205045	40.766375
3518.095810	522617.662273	40.771380
3518.002015	522371.231787	40.776384
3517.524804	522122.229348	40.781389
3517.744223	521865.125325	40.786394
3517.169049	521630.387301	40.791399
3517.096711	521382.775665	40.796404
3516.893532	521141.652259	40.801408
3516.474940	520910.165325	40.806413
3516.449470	520687.106810	40.811418
3516.010759	520455.414380	40.816423
3515.591391	520221.946013	40.821428
3515.719735	520007.904160	40.826432
3515.310128	519797.938877	40.831437
3515.558152	519581.344482	40.836442
3515.163751	519367.326333	40.841447
3514.964575	519154.639751	40.846452
3514.700680	518944.134895	40.851456
3514.150166	518746.111518	40.856461
3514.302034	518543.575586	40.861466
3514.101072	518352.267957	40.866471
3514.023632	518151.634390	40.871476
3513.587853	517965.517156	40.876480
3513.508655	517776.408558	40.881485
3513.279980	517593.237884	40.886490
3512.981556	517399.305097	40.891495
3513.010441	517228.377850	40.896500
3512.792030	517055.920268	40.901504
3512.639167	516892.047464	40.906509
3512.681641	516711.605559	40.911514
3512.370613	516554.176899	40.916519
3512.313481	516371.825346	40.921524
3512.188587	516210.823999	40.926528
3511.886859	516047.219263	40.931533
3512.291059	515888.255232	40.936538
3511.685655	515731.977940	40.941543
3511.541457	515566.371219	40.946548
3511.060788	515411.588439	40.951552
3511.045842	515260.877776	40.956557
3511.189135	515126.072039	40.961562
3510.943694	514978.126338	40.966567
3510.747621	514821.826418	40.971572
3510.701666	514692.155320	40.976576
3510.535134	514558.810140	40.981581
3510.436393	514419.889647	40.986586
3510.289508	514279.559427	40.991591
3510.065110	514144.348713	40.996596
3509.839375	514007.366862	41.001600
3509.809286	513885.931388	41.006605
3509.841284	513764.080588	41.011610
3509.451046	513643.155502	41.016615
3509.591040	513510.815743	41.021620
3509.506138	513395.859686	41.026624
3509.327356	513283.294994	41.031629
3509.264625	513163.225161	41.036634
3508.776893	513055.867084	41.041639
3508.888027	512938.145512	41.046644
3508.946278	512831.256118	41.051648
3508.686033	512720.622682	41.056653
3508.815006	512607.195519	41.061658
3508.747326	512505.382277	41.066663
3508.813294	512390.597870	41.071668
3508.467378	512287.006276	41.076672
3508.235519	512197.913723	41.081677
3508.742437	512076.936798	41.086682
3508.354864	511974.766250	41.091687
3508.043511	511869.750265	41.096692
3507.979016	511780.831410	41.101696
3507.998893	511688.104817	41.106701
3507.839399	511598.845923	41.111706
3507.519890	511515.682212	41.116711
3507.856262	511424.978201	41.121716
3507.972710	511330.210930	41.126720
3507.650461	511243.606413	41.131725
3508.041094	511139.031422	41.136730
3507.695874	511053.694256	41.141735
3507.032848	510961.678692	41.146740
3507.051631	510880.734869	41.151744
3507.243012	510800.572798	41.156749
3507.464496	510726.375057	41.161754
3507.104171	510650.953639	41.166759
3507.071302	510566.323499	41.171764
3506.986943	510485.039977	41.176768
3506.763866	510415.868911	41.181773
3506.884195	510325.344969	41.186778
3506.837344	510260.951459	41.191783
3506.752096	510188.924647	41.196788
3506.980513	510112.446583	41.201792
3506.601868	510046.435221	41.206797
3506.873573	509968.280178	41.211802
3506.637937	509902.953932	41.216807
3506.405723	509830.544111	41.221812
3506.503711	509746.344553	41.226816
3506.246643	509687.547184	41.231821
3506.295991	509612.815312	41.236826
3506.153013	509561.183535	41.241831
3506.654283	509494.626235	41.246836
3506.484543	509429.439545	41.251840
3506.429123	509364.740466	41.256845
3506.577629	509285.944082	41.261850
3506.180729	509222.917414	41.266855
3506.094610	509155.692743	41.271860
3505.839911	509103.115973	41.276864
3505.996791	509032.513244	41.281869
3506.371328	508969.717874	41.286874
3506.462371	508917.237671	41.291879
3506.125031	508843.069508	41.296884
3505.955022	508789.365320	41.301888
3505.838674	508725.230001	41.306893
3505.768351	508654.003900	41.311898
3505.444967	508610.897704	41.316903
3505.909124	508555.321731	41.321908
3505.940456	508502.191965	41.326912
3505.731870	508445.558277	41.331917
3505.750819	508382.715779	41.336922
3505.711633	508339.614581	41.341927
3505.618942	508268.744593	41.346932
3505.564705	508207.633286	41.351936
3505.304159	508164.870215	41.356941
3505.421901	508113.698847	41.361946
3505.314027	508075.009728	41.366951
3505.040810	508012.212059	41.371956
3505.005998	507981.151278	41.376960
3505.046373	507936.467998	41.381965
3505.430033	507878.828099	41.386970
3505.220482	507849.919777	41.391975
3505.268051	507786.109238	41.396980
3505.438308	507743.327629	41.401984
3505.439013	507704.013349	41.406989
3505.631271	507651.310908	41.411994
3505.205573	507601.235871	41.416999
3505.234485	507549.874483	41.422004
3505.197838	507500.395437	41.427008
3504.925908	507454.950703	41.432013
3504.966359	507412.998367	41.437018
3504.791564	507368.448826	41.442023
3505.239712	507333.009669	41.447028
3505.071841	507287.143259	41.452032
3505.276031	507244.203258	41.457037
3505.219260	507189.464216	41.462042
3504.992356	507147.300498	41.467047
3505.290096	507101.511802	41.472052
3505.117137	507049.118250	41.477056
3504.990455	507018.677457	41.482061
3505.133602	506967.296287	41.487066
3505.004645	506926.381544	41.492071
3505.183303	506872.768088	41.497076
3505.205461	506832.588239	41.502080
3505.200163	506797.624461	41.507085
3505.085932	506749.268739	41.512090
3504.798474	506703.622088	41.517095
3504.925513	506670.003349	41.522100
3504.786549	506627.166660	41.527104
3505.135304	506584.758787	41.532109
3505.170478	506545.740037	41.537114
3504.965468	506493.501677	41.542119
3505.000995	506460.909021	41.547124
3505.206319	506412.451253	41.552128
3505.086566	506359.490596	41.557133
3504.864686	506320.157758	41.562138
3505.153416	506285.804299	41.567143
3504.869781	506223.609014	41.572148
3504.952279	506187.871105	41.577152
3504.710993	506141.557854	41.582157
3504.441151	506110.986290	41.587162
3504.550965	506077.520937	41.592167
3504.912677	506037.943414	41.597172
3504.919575	505998.421883	41.602176
3504.605477	505968.464294	41.607181
3504.853230	505923.743055	41.612186
3504.962418	505891.542513	41.617191
3504.492985	505851.741715	41.622196
3504.868419	505802.445716	41.627200
3504.500969	505780.238511	41.632205
3504.901172	505731.697446	41.637210
3504.577183	505699.008378	41.642215
3504.838361	505656.409675	41.647220
3505.194835	505611.164417	41.652224
3504.752268	505578.746883	41.657229
3504.878764	505541.836809	41.662234
3504.725075	505497.582760	41.667239
3504.629226	505456.811141	41.672244
3504.519854	505419.128422	41.677248
3504.395036	505380.486581	41.682253
3504.671085	505350.788885	41.687258
3504.551741	505318.724616	41.692263
3504.800365	505286.602129	41.697268
3504.597433	505242.608240	41.702272
3504.463103	505212.367915	41.707277
3504.981794	505175.395079	41.712282
3504.651308	505145.590482	41.717287
3504.538152	505105.731670	41.722292
3504.408374	505071.441970	41.727296
3504.616702	505042.159296	41.732301
3504.631438	505005.316360	41.737306
3504.403048	504970.789022	41.742311
3504.417416	504931.972374	41.747316
3504.637084	504886.139597	41.752320
3504.131465	504871.746360	41.757325
3504.483812	504830.851836	41.762330
3504.347405	504808.505664	41.767335
3504.014364	504774.348721	41.772340
3504.141119	504736.728423	41.777344
3504.242007	504715.204931	41.782349
3504.347788	504681.838756	41.787354
3503.946612	504662.013957	41.792359
3504.411613	504624.441170	41.797364
3504.457318	504597.308931	41.802368
3504.146865	504565.627734	41.807373
3504.386193	504534.618685	41.812378
3504.050097	504512.050663	41.817383
3504.231419	504484.137711	41.822388
3504.358176	504451.577494	41.827392
3504.111212	504431.272596	41.832397
3504.191799	504396.847112	41.837402
3504.092907	504373.026847	41.842407
3504.119432	504343.316277	41.847412
3504.094667	504316.650208	41.852416
3504.102222	504293.217869	41.857421
3504.116551	504260.472637	41.862426
3504.213562	504230.902559	41.867431
3504.023476	504204.464880	41.872436
3504.197349	504194.164128	41.877440
3503.918172	504153.064196	41.882445
3504.345183	504124.960017	41.887450
3504.292702	504092.832328	41.892455
3504.243202	504057.768837	41.897460
3504.348758	504030.120180	41.902464
3504.039276	503994.439746	41.907469
3504.244531	503968.546527	41.912474
3504.117989	503941.693542	41.917479
3504.171670	503904.690313	41.922484
3504.263970	503877.195337	41.927488
3504.141132	503868.459552	41.932493
3504.317005	503823.491272	41.937498
3504.076802	503814.774010	41.942503
3504.125455	503779.694451	41.947508
3504.445885	503750.138861	41.952512
3504.242317	503720.716651	41.957517
3504.228962	503682.458323	41.962522
3504.381182	503659.407149	41.967527
3504.152602	503619.158328	41.972532
3503.908244	503583.517377	41.977536
3503.767382	503583.742182	41.982541
3504.134355	503544.411250	41.987546
3503.855933	503516.721258	41.992551
3504.053921	503494.877268	41.997556
3504.244933	503466.202024	42.002560
3504.239559	503448.438907	42.007565
3504.012218	503417.704091	42.012570
3504.040490	503394.520331	42.017575
3504.093437	503362.425255	42.022580
3504.144229	503324.105400	42.027584
3504.155687	503308.363892	42.032589
3504.093266	503272.946607	42.037594
3503.954447	503257.734910	42.042599
3503.911473	503224.490704	42.047604
3504.189167	503188.817051	42.052608
3503.996203	503179.079794	42.057613
3504.086697	503137.868450	42.062618
3503.987441	503123.460157	42.067623
3503.988572	503087.931235	42.072628
3503.960887	503072.651202	42.077632
3503.741660	503055.883099	42.082637
3504.012120	503026.739085	42.087642
3503.830960	503020.947541	42.092647
3503.788296	502991.346848	42.097652
3504.054002	502955.168506	42.102656
3503.755094	502945.549088	42.107661
3503.714551	502915.897322	42.112666
3503.874722	502883.328925	42.117671
3503.929786	502878.714675	42.122676
3504.070677	502836.128150	42.127680
3503.677644	502828.649235	42.132685
3503.632899	502794.291041	42.137690
3503.839341	502777.354171	42.142695
3504.033854	502763.304046	42.147700
3504.487938	502732.460333	42.152704
3503.710841	502701.659325	42.157709
3503.952716	502674.695567	42.162714
3503.842492	502661.402097	42.167719
3503.992372	502626.709143	42.172724
3503.892356	502617.564232	42.177728
3503.822193	502581.539437	42.182733
3504.085319	502557.811335	42.187738
3503.789425	502532.551957	42.192743
3503.591943	502520.486874	42.197748
3503.711259	502493.187923	42.202752
3503.841083	502465.786043	42.207757
3503.851271	502440.579381	42.212762
3503.783031	502423.786814	42.217767
3503.924117	502410.959563	42.222772
3503.735120	502384.772046	42.227776
3503.648304	502377.143313	42.232781
3504.042659	502342.512388	42.237786
3503.976709	502331.742326	42.242791
3504.025890	502303.138226	42.247796
3503.930584	502270.406629	42.252800
3503.866604	502259.180692	42.257805
3504.102005	502219.563932	42.262810
3503.701213	502212.136594	42.267815
3503.975798	502172.311081	42.272820
3503.973332	502148.877479	42.277824
3504.119346	502130.481747	42.282829
3504.314024	502090.871136	42.287834
3504.231491	502070.739982	42.292839
3503.795948	502047.627765	42.297844
3504.101927	502020.349197	42.302848
3503.641124	501997.544592	42.307853
3503.988677	501975.928159	42.312858
3503.910279	501950.481731	42.317863
3504.025610	501918.779090	42.322868
3504.247463	501892.728366	42.327872
3503.641572	501874.299368	42.332877
3503.808619	501853.774219	42.337882
3504.098501	501828.421250	42.342887
3503.964346	501813.106344	42.347892
3503.901734	501773.232003	42.352896
3503.706108	501758.989675	42.357901
3503.817638	501728.299590	42.362906
3503.763959	501723.297308	42.367911
3503.733066	501688.833552	42.372916
3503.895628	501668.460743	42.377920
3503.565338	501655.454376	42.382925
3504.147918	501625.752577	42.387930
3503.960670	501606.092983	42.392935
3503.836296	501583.234669	42.397940
3504.017752	501551.318461	42.402944
3503.832977	501545.628235	42.407949
3503.804072	501510.050280	42.412954
3503.583753	501495.254873	42.417959
3503.741345	501475.135705	42.422964
3504.000645	501446.446400	42.427968
3503.653849	501428.077217	42.432973
3503.727740	501405.693494	42.437978
3503.906766	501376.510607	42.442983
3503.417014	501369.096974	42.447988
3503.815587	501335.981898	42.452992
3503.595962	501326.146602	42.457997
3503.833736	501294.322263	42.463002
3503.496439	501284.657391	42.468007
3503.562779	501264.856105	42.473012
3503.602606	501233.974036	42.478016
3503.799809	501230.399833	42.483021
3503.894107	501200.825120	42.488026
3503.667323	501178.741717	42.493031
3503.448542	501164.148256	42.498036
3503.775253	501135.194713	42.503040
3503.621477	501116.389767	42.508045
3503.853212	501101.623815	42.513050
3503.610123	501091.589631	42.518055
3503.425064	501069.246415	42.523060
3503.643517	501038.538241	42.528064
3503.665727	501030.233677	42.533069
3503.573983	501010.457096	42.538074
3503.505803	500994.523653	42.543079
3503.829038	500972.099976	42.548084
3503.602848	500952.597665	42.553088
3503.758276	500934.806613	42.558093
3503.746748	500920.990068	42.563098
3503.774229	500899.321685	42.568103
3503.596913	500875.053548	42.573108
3504.148628	500854.466449	42.578112
3503.847125	500840.240118	42.583117
3503.440856	500819.601925	42.588122
3503.828536	500784.007293	42.593127
3503.648381	500771.634575	42.598132
3503.769778	500746.559787	42.603136
3503.506868	500733.339623	42.608141
3503.434302	500697.159534	42.613146
3503.528317	500688.894080	42.618151
3503.464656	500671.491719	42.623156
3503.809535	500645.065401	42.628160
3503.885641	500642.421344	42.633165
3503.644499	500618.365417	42.638170
3503.496654	500601.330619	42.643175
3503.266414	500571.198741	42.648180
3503.501113	500552.888598	42.653184
3503.535061	500548.631409	42.658189
3503.559660	500517.092469	42.663194
3503.414806	500505.017696	42.668199
3503.349893	500506.597227	42.673204
3503.623903	500473.652095	42.678208
3503.366882	500467.011193	42.683213
3503.189510	500435.554650	42.688218
3503.425354	500423.419651	42.693223
3503.582469	500415.093479	42.698228
3503.552489	500396.015113	42.703232
3503.213749	500380.630072	42.708237
3503.709553	500376.097368	42.713242
3503.713871	500337.322845	42.718247
3503.474843	500325.566548	42.723252
3503.615787	500315.167515	42.728256
3503.304462	500294.311230	42.733261
3503.420889	500283.409864	42.738266
3503.963062	500260.191406	42.743271
3503.708138	500243.730001	42.748276
3503.495740	500214.404605	42.753280
3503.404715	500211.888138	42.758285
3503.978681	500190.486854	42.763290
3504.005979	500165.932316	42.768295
3503.620168	500148.782840	42.773300
3503.676026	500127.463371	42.778304
3503.773566	500110.693037	42.783309
3503.945157	500080.749916	42.788314
3503.760317	500063.771072	42.793319
3503.441809	500031.020017	42.798324
3503.593553	500018.493078	42.803329
3503.370764	500008.708174	42.808333
3503.427724	499980.655933	42.813338
3503.813525	499964.042379	42.818343
3503.129282	499957.721911	42.823348
3503.758744	499929.427242	42.828353
3503.567005	499928.597112	42.833357
3503.521120	499893.119857	42.838362
3503.745663	499882.606119	42.843367
3503.834223	499860.774963	42.848372
3503.928430	499844.308627	42.853377
3503.744701	499820.900614	42.858381
3504.057262	499783.645400	42.863386
3503.760664	499757.875987	42.868391
3503.653351	499760.424073	42.873396
3504.102494	499727.247406	42.878401
3503.929749	499712.189896	42.883405
3503.757857	499681.287987	42.888410
3503.762485	499670.201436	42.893415
3503.612336	499636.410635	42.898420
3503.899970	499617.939309	42.903425
3503.831056	499600.587357	42.908429
3503.573319	499565.294801	42.913434
3503.474634	499548.757439	42.918439
3503.413297	499532.264781	42.923444
3503.586475	499517.000568	42.928449
3503.511063	499510.128120	42.933453
3503.515381	499496.662318	42.938458
3503.626679	499477.712507	42.943463
3503.573236	499452.106707	42.948468
3503.649642	499435.085975	42.953473
3503.536065	499403.465672	42.958477
3503.589993	499394.244151	42.963482
3504.005764	499380.308257	42.968487
3503.464695	499365.865508	42.973492
3503.655148	499333.285839	42.978497
3503.636220	499311.066031	42.983501
3503.728022	499305.837590	42.988506
3503.693791	499277.697420	42.993511
3503.343567	499267.375412	42.998516
3503.686148	499247.275123	43.003521
3503.263202	499232.611109	43.008525
3503.544779	499211.609228	43.013530
3503.736819	499183.585013	43.018535
3503.458508	499177.250727	43.023540
3503.540712	499168.530842	43.028545
3503.606569	499134.907443	43.033549
3503.658601	499121.281952	43.038554
3503.490135	499097.212492	43.043559
3503.786932	499082.890196	43.048564
3503.613930	499057.150863	43.053569
3503.559050	499041.314824	43.058573
3503.207123	499032.309133	43.063578
3503.900261	499004.661039	43.068583
3503.570937	499000.005297	43.073588
3503.527936	498971.866034	43.078593
3503.580537	498943.458504	43.083597
3503.651539	498943.801743	43.088602
3503.603116	498912.170277	43.093607
3503.441424	498904.096286	43.098612
3503.589100	498882.862072	43.103617
3503.630023	498860.126017	43.108621
3503.628662	498848.938661	43.113626
3503.634769	498820.740777	43.118631
3503.466612	498810.440351	43.123636
3503.489416	498804.716440	43.128641
3503.552952	498768.915931	43.133645
3503.519565	498754.999924	43.138650
3503.731343	498732.186080	43.143655
3503.525873	498719.259088	43.148660
3503.775240	498705.298352	43.153665
3503.628209	498673.428934	43.158669
3503.463510	498669.911426	43.163674
3503.869324	498635.625880	43.168679
3503.239163	498632.789417	43.173684
3503.215474	498609.557022	43.178689
3503.241320	498590.366666	43.183693
3503.186022	498580.858250	43.188698
3503.638804	498578.863085	43.193703
3503.270147	498563.886201	43.198708
3503.817505	498534.387349	43.203713
3503.707595	498524.735664	43.208717
3503.540173	498503.196439	43.213722
3503.735329	498482.156744	43.218727
3503.134890	498460.230293	43.223732
3503.227201	498439.358676	43.228737
3503.209434	498444.170879	43.233741
3503.067691	498415.995730	43.238746
3503.569113	498401.994921	43.243751
3503.291480	498394.951511	43.248756
3503.612960	498383.409093	43.253761
3503.523949	498368.033474	43.258765
3503.271318	498358.859877	43.263770
3503.496312	498312.857444	43.268775
3503.374131	498311.358124	43.273780
3503.709710	498307.558974	43.278785
3503.578175	498270.877067	43.283789
3503.775409	498267.251649	43.288794
3503.880067	498238.429782	43.293799
3503.516205	498237.069905	43.298804
3503.546863	498190.338505	43.303809
3503.462765	498177.645064	43.308813
3503.539196	498169.128107	43.313818
3503.233975	498142.193367	43.318823
3503.066103	498133.360633	43.323828
3503.643888	498128.308163	43.328833
3503.558998	498096.883530	43.333837
3503.369884	498083.852245	43.338842
3503.625256	498066.801934	43.343847
3503.348818	498058.897576	43.348852
3503.515431	498042.823150	43.353857
3503.668143	498038.951597	43.358861
3503.381649	498013.380586	43.363866
3503.417677	497996.162376	43.368871
3503.182313	497980.758935	43.373876
3502.988615	497942.719300	43.378881
3503.243350	497955.740520	43.383885
3503.498881	497943.195735	43.388890
3503.867347	497924.051768	43.393895
3503.521044	497911.905839	43.398900
3503.624148	497887.336209	43.403905
3503.772634	497879.111481	43.408909
3503.257667	497849.171913	43.413914
3503.447267	497826.107301	43.418919
3503.126951	497818.564154	43.423924
3503.367421	497802.579092	43.428929
3503.441623	497795.226708	43.433933
3503.251090	497774.854663	43.438938
3503.577204	497766.095548	43.443943
3503.152692	497746.216086	43.448948
3503.396771	497729.825382	43.453953
3503.260699	497725.645024	43.458957
3503.288466	497706.706555	43.463962
3503.320419	497686.805507	43.468967
3503.079416	497678.996634	43.473972
3503.113296	497678.636998	43.478977
3503.455340	497659.345048	43.483981
3503.230843	497640.446383	43.488986
3503.756013	497623.049252	43.493991
3503.444585	497610.897608	43.498996
3503.204184	497594.583357	43.504001
3503.483830	497580.616968	43.509005
3503.373320	497565.547824	43.514010
3503.431084	497541.339277	43.519015
3502.905315	497537.574856	43.524020
3503.551245	497519.753526	43.529025
3503.120878	497504.633634	43.534029
3503.051832	497490.013514	43.539034
3503.199749	497491.509041	43.544039
3503.031920	497469.006737	43.549044
3503.087745	497452.797418	43.554049
3503.612706	497435.400141	43.559053
3503.045822	497446.475887	43.564058
3503.124902	497425.402684	43.569063
3502.995398	497408.108824	43.574068
3503.430786	497405.255624	43.579073
3503.069983	497397.364310	43.584077
3502.868918	497377.449125	43.589082
3503.052161	497358.637600	43.594087
3502.701341	497355.554269	43.599092
3503.204897	497352.234642	43.604097
3503.220251	497350.207231	43.609101
3503.364433	497345.020572	43.614106
3503.527287	497330.211788	43.619111
3503.505912	497320.241701	43.624116
3503.396722	497306.336559	43.629121
3503.478150	497282.022671	43.634125
3503.241131	497281.148944	43.639130
3503.245451	497265.150107	43.644135
3503.043458	497249.487630	43.649140
3503.012412	497228.229094	43.654145
3503.606081	497240.235337	43.659149
3502.983220	497212.741886	43.664154
3503.305500	497191.123695	43.669159
3503.000454	497193.349001	43.674164
3503.282805	497186.672257	43.679169
3503.369829	497168.432647	43.684173
3503.308276	497156.696851	43.689178
3503.438511	497140.374237	43.694183
3503.257275	497130.277429	43.699188
3503.307021	497094.172017	43.704193
3503.424297	497106.658669	43.709197
3503.741299	497085.446210	43.714202
3503.878042	497061.477678	43.719207
3503.478565	497048.276384	43.724212
3503.641772	497006.988806	43.729217
3503.456291	497008.385185	43.734221
3503.516820	496988.529482	43.739226
3503.418633	496957.003715	43.744231
3503.304872	496952.870279	43.749236
3503.343013	496945.421994	43.754241
3503.164135	496922.262590	43.759245
3503.406299	496918.579173	43.764250
3503.380574	496895.901812	43.769255
3503.004129	496877.228880	43.774260
3503.092213	496863.393475	43.779265
3503.358191	496865.072908	43.784269
3503.061083	496843.248432	43.789274
3503.164237	496830.625706	43.794279
3503.311928	496818.856620	43.799284
3502.960414	496823.468861	43.804289
3503.604278	496810.355629	43.809293
3503.456891	496786.937931	43.814298
3503.344142	496780.323487	43.819303
3503.069304	496758.292874	43.824308
3503.141201	496740.510884	43.829313
3503.592367	496731.782136	43.834317
3503.099329	496722.088787	43.839322
3503.491392	496692.814004	43.844327
3503.259761	496694.217701	43.849332
3503.457487	496681.934328	43.854337
3503.445846	496656.267327	43.859341
3503.343313	496652.840857	43.864346
3503.352328	496632.891649	43.869351
3503.157763	496610.088730	43.874356
3503.235106	496592.913286	43.879361
3503.313617	496587.888679	43.884365
3502.936762	496575.847939	43.889370
3503.083963	496547.421695	43.894375
3503.212192	496539.199562	43.899380
3502.904467	496531.248850	43.904385
3502.921964	496550.333485	43.909389
3503.128261	496534.555228	43.914394
3503.182217	496499.663076	43.919399
3503.135607	496499.771805	43.924404
3502.940498	496488.866760	43.929409
3503.124741	496488.787112	43.934413
3502.828269	496471.063084	43.939418
3503.296342	496454.433307	43.944423
3503.140986	496438.661499	43.949428
3503.097642	496438.567194	43.954433
3503.114447	496441.298645	43.959437
3503.093033	496419.683233	43.964442
3503.209260	496402.754613	43.969447
3503.184686	496396.683020	43.974452
3503.156653	496396.485035	43.979457
3503.199565	496375.163181	43.984461
3502.916098	496362.094940	43.989466
3503.302310	496353.072499	43.994471
3503.198849	496356.430531	43.999476
3502.885196	496328.988127	44.004481
3503.167137	496321.349161	44.009485
3503.252197	496313.994461	44.014490
3503.504244	496298.816330	44.019495
3502.885452	496288.889474	44.024500
3502.880952	496269.802716	44.029505
3502.927229	496258.251818	44.034509
3502.770368	496256.150244	44.039514
3503.059986	496244.155833	44.044519
3503.091843	496252.555522	44.049524
3503.025105	496230.643267	44.054529
3502.964747	496224.374752	44.059533
3502.996982	496219.863661	44.064538
3503.261984	496206.252946	44.069543
3502.732183	496216.513489	44.074548
3502.916629	496193.346359	44.079553
3503.339220	496175.710910	44.084557
3503.007638	496171.004159	44.089562
3503.228818	496170.007324	44.094567
3502.960209	496174.606624	44.099572
3503.152123	496150.881325	44.104577
3503.228439	496130.515885	44.109581
3503.182307	496122.624908	44.114586
3503.398777	496113.578548	44.119591
3503.201080	496092.041240	44.124596
3503.258166	496082.463118	44.129601
3503.101546	496085.373926	44.134605
3503.027348	496075.715290	44.139610
3503.382713	496056.166383	44.144615
3503.159338	496045.063017	44.149620
3502.994032	496040.886890	44.154625
3503.155162	496036.912320	44.159629
3502.909586	496018.319081	44.164634
3503.132056	495994.487487	44.169639
3502.872352	495993.819805	44.174644
3502.814080	496004.005938	44.179649
3503.177412	495994.531258	44.184653
3502.987132	495982.004955	44.189658
3503.132654	495957.071594	44.194663
3503.470695	495945.423750	44.199668
3503.203740	495943.086386	44.204673
3503.048701	495932.529092	44.209677
3502.958283	495910.113883	44.214682
3503.074659	495897.387159	44.219687
3502.949965	495900.647369	44.224692
3503.033836	495905.849230	44.229697
3503.279174	495896.089362	44.234701
3503.147324	495879.503255	44.239706
3503.342018	495869.599484	44.244711
3503.151786	495871.553644	44.249716
3503.372988	495836.988208	44.254721
3503.258060	495823.234732	44.259725
3502.968110	495822.521192	44.264730
3503.214275	495812.457361	44.269735
3503.285763	495794.978303	44.274740
3503.232432	495778.379693	44.279745
3503.758349	495764.271724	44.284749
3503.205171	495757.118942	44.289754
3503.436670	495733.842530	44.294759
3503.042191	495726.360862	44.299764
3503.310850	495720.495855	44.304769
3503.414807	495697.796504	44.309773
3503.089875	495691.873414	44.314778
3503.333167	495682.366915	44.319783
3503.124346	495653.641127	44.324788
3503.222477	495653.372561	44.329793
3503.171801	495643.507450	44.334797
3503.229055	495629.878510	44.339802
3503.061581	495602.411905	44.344807
3502.958873	495600.200432	44.349812
3503.162403	495596.522857	44.354817
3503.228309	495591.297441	44.359821
3503.172605	495574.496492	44.364826
3503.440515	495552.682426	44.369831
3503.144485	495548.526847	44.374836
3503.212713	495544.212429	44.379841
3503.446116	495523.112632	44.384845
3503.170167	495516.371627	44.389850
3503.615076	495502.883849	44.394855
3503.415585	495480.586618	44.399860
3503.265268	495455.598067	44.404865
3503.498425	495457.333453	44.409869
3503.131757	495435.872710	44.414874
3503.475997	495411.666683	44.419879
3503.102575	495410.561259	44.424884
3503.307286	495391.491148	44.429889
3503.425575	495377.447312	44.434893
3503.100520	495365.701378	44.439898
3503.378507	495367.530952	44.444903
3503.088027	495346.108694	44.449908
3503.218880	495328.214744	44.454913
3503.299329	495318.986959	44.459917
3502.991829	495324.301478	44.464922
3503.511425	495289.080249	44.469927
3503.249401	495281.172399	44.474932
3503.156306	495283.060635	44.479937
3503.194652	495255.054647	44.484941
3502.936028	495246.741180	44.489946
3503.081172	495229.655004	44.494951
3502.973553	495226.026535	44.499956
3502.959144	495223.851693	44.504961
3503.266655	495201.828417	44.509965
3502.783737	495194.208609	44.514970
3502.941051	495180.512885	44.519975
3503.054671	495166.267092	44.524980
3502.894978	495168.773465	44.529985
3503.009588	495171.692181	44.534989
3503.001974	495150.680683	44.539994
3503.431354	495136.992558	44.544999
3503.467131	495132.176839	44.550004
3503.356397	495117.763936	44.555009
3503.695351	495089.862082	44.560013
3503.018371	495104.197184	44.565018
3502.979058	495079.646275	44.570023
3503.136691	495055.975609	44.575028
3503.138763	495053.190538	44.580033
3503.180656	495037.842044	44.585037
3503.161184	495046.503569	44.590042
3503.337455	495011.994310	44.595047
3503.089248	495000.235994	44.600052
3503.118275	494999.320103	44.605057
3503.190227	494998.853129	44.610061
3502.987663	494978.682387	44.615066
3503.452854	494952.178117	44.620071
3503.371787	494959.887375	44.625076
3502.824469	494941.644535	44.630081
3503.291247	494915.899469	44.635085
3502.876532	494903.964873	44.640090
3503.034681	494890.268801	44.645095
3502.987326	494902.580450	44.650100
3502.952602	494904.611400	44.655105
3503.296359	494871.645058	44.660109
3502.774404	494878.563257	44.665114
3502.936137	494863.550114	44.670119
3503.220833	494857.429127	44.675124
3503.059185	494863.530871	44.680129
3503.295706	494829.163648	44.685133
3503.088713	494816.335381	44.690138
3503.460798	494811.314519	44.695143
3503.144803	494816.529258	44.700148
3503.202604	494783.405419	44.705153
3503.496146	494777.485544	44.710157
3503.123721	494770.759512	44.715162
3503.113742	494754.912636	44.720167
3503.310132	494740.855968	44.725172
3503.330205	494735.789455	44.730177
3503.166697	494724.777091	44.735181
3503.026482	494693.659131	44.740186
3503.373466	494688.389030	44.745191
3502.883881	494687.706998	44.750196
3502.793810	494691.974641	44.755201
3503.246522	494662.231313	44.760205
3502.904662	494653.171212	44.765210
3502.999848	494634.269530	44.770215
3503.077505	494633.700376	44.775220
3503.024290	494623.885752	44.780225
3503.509033	494612.365781	44.785229
3502.923973	494612.711531	44.790234
3503.048338	494582.817434	44.795239
3503.302241	494596.145004	44.800244
3502.887654	494573.576855	44.805249
3503.188216	494545.629609	44.810253
3503.086269	494541.949473	44.815258
3503.043418	494540.791744	44.820263
3502.893238	494548.815909	44.825268
3503.218213	494534.181774	44.830273
3503.047399	494515.575188	44.835277
3503.084804	494511.771750	44.840282
3503.297374	494495.028678	44.845287
3503.445406	494494.448398	44.850292
3503.188596	494479.906176	44.855297
3503.339222	494455.780126	44.860301
3503.375506	494460.635474	44.865306
3503.379038	494427.165123	44.870311
3503.474837	494432.011071	44.875316
3503.465586	494412.214233	44.880321
3503.648079	494390.108474	44.885325
3502.962017	494381.507725	44.890330
3503.312887	494364.337592	44.895335
3503.227731	494353.565798	44.900340
3503.180407	494332.610275	44.905345
3503.402814	494330.701709	44.910349
3503.130176	494315.149147	44.915354
3502.977017	494310.920067	44.920359
3503.062295	494297.538885	44.925364
3503.291228	494282.261468	44.930369
3503.302623	494275.474586	44.935373
3502.812632	494264.969270	44.940378
3503.063760	494244.219652	44.945383
3502.869863	494241.921156	44.950388
3503.015982	494236.328224	44.955393
3502.997981	494237.698340	44.960397
3503.077546	494225.381360	44.965402
3503.317707	494203.215626	44.970407
3503.280336	494198.816312	44.975412
3503.157835	494182.936092	44.980417
3503.421441	494167.956914	44.985421
3502.851302	494165.312788	44.990426
3502.981296	494141.442768	44.995431
3502.995220	494140.630493	45.000436
3502.739069	494141.228080	45.005441
3503.286940	494137.191973	45.010445
3503.115709	494113.521435	45.015450
3503.106750	494095.496475	45.020455
3503.139860	494102.631048	45.025460
3502.685327	494095.664563	45.030465
3503.179306	494087.231613	45.035469
3503.280931	494070.910781	45.040474
3503.509823	494054.114093	45.045479
3503.267639	494046.202572	45.050484
3502.999179	494026.851379	45.055489
3503.568438	494006.861393	45.060493
3503.358840	493990.387136	45.065498
3503.192887	493976.437792	45.070503
3503.040263	493971.398365	45.075508
3503.071806	493960.658532	45.080513
3503.319346	493958.948502	45.085517
3503.219975	493939.975584	45.090522
3503.006804	493918.792620	45.095527
3503.258992	493902.447842	45.100532
3502.929674	493914.247715	45.105537
3503.389706	493905.364318	45.110541
3503.110229	493887.837642	45.115546
3503.263534	493871.356555	45.120551
3503.119915	493867.227139	45.125556
3503.280535	493859.910149	45.130561
3503.498814	493827.873234	45.135565
3503.480179	493825.141887	45.140570
3503.156146	493809.951479	45.145575
3503.304841	493794.129333	45.150580
3503.104865	493782.058789	45.155585
3503.432052	493775.778817	45.160589
3503.242388	493747.452111	45.165594
3503.026558	493739.789477	45.170599
3503.174340	493733.892308	45.175604
3503.138111	493740.734158	45.180609
3503.533511	493719.049677	45.185613
3503.151049	493709.185330	45.190618
3503.313417	493691.943091	45.195623
3503.422252	493675.772682	45.200628
3503.367099	493667.628886	45.205633
3503.305212	493665.258814	45.210637
3503.363566	493631.930264	45.215642
3503.214746	493614.483951	45.220647
3503.472262	493598.289974	45.225652
3502.804202	493600.066709	45.230657
3503.265441	493571.636851	45.235661
3503.012969	493556.536199	45.240666
3502.912423	493562.122338	45.245671
3502.986726	493548.286608	45.250676
3503.050808	493555.315222	45.255681
3502.975320	493530.210947	45.260685
3502.835111	493518.383972	45.265690
3503.075208	493515.611685	45.270695
3503.322439	493512.787632	45.275700
3502.977846	493513.247303	45.280705
3503.403446	493477.125985	45.285709
3503.088575	493468.618049	45.290714
3503.136766	493459.546344	45.295719
3503.349301	493447.916760	45.300724
3503.016864	493442.297953	45.305729
3503.043539	493422.798200	45.310733
3502.901218	493404.996195	45.315738
3503.191991	493406.115015	45.320743
3503.298276	493398.553241	45.325748
3502.800129	493379.845329	45.330753
3503.122037	493365.109477	45.335757
3503.122554	493367.843962	45.340762
3503.131081	493373.311642	45.345767
3502.994592	493351.103141	45.350772
3502.852846	493336.541827	45.355777
3502.796766	493332.651645	45.360781
3502.933501	493337.795241	45.365786
3503.261582	493324.780083	45.370791
3503.095780	493311.235318	45.375796
3503.032539	493283.394299	45.380801
3503.306993	493275.704618	45.385805
3503.106992	493267.786093	45.390810
3502.923812	493271.714312	45.395815
3502.969296	493261.680807	45.400820
3502.917921	493244.016187	45.405825
3503.257947	493231.252268	45.410829
3503.144062	493235.220180	45.415834
3503.531390	493223.866659	45.420839
3503.378853	493207.939707	45.425844
3502.838908	493191.820781	45.430849
3503.313032	493173.921119	45.435853
3503.614356	493172.658266	45.440858
3503.161165	493151.005969	45.445863
3503.602921	493139.441238	45.450868
3503.396426	493116.686493	45.455873
3503.263943	493103.592059	45.460877
3503.062515	493094.357073	45.465882
3502.946678	493087.994976	45.470887
3503.342762	493067.170486	45.475892
3503.222050	493051.744759	45.480897
3503.325420	493040.689204	45.485901
3502.836965	493048.109179	45.490906
3502.834115	493023.043372	45.495911
3503.173533	493000.759228	45.500916
3502.978291	493002.714481	45.505921
3503.219007	492995.840243	45.510925
3503.171361	492998.784951	45.515930
3503.044653	492976.625093	45.520935
3503.345710	492970.703454	45.525940
3502.858610	492970.375433	45.530945
3503.006833	492967.921422	45.535949
3502.979497	492954.962181	45.540954
3503.248700	492937.195959	45.545959
3502.943673	492918.203857	45.550964
3502.870721	492912.037479	45.555969
3502.947118	492904.834703	45.560973
3502.909409	492917.399351	45.565978
3502.894800	492886.106565	45.570983
3503.126220	492876.549858	45.575988
3503.103058	492873.717807	45.580993
3503.249028	492863.921401	45.585997
3503.223002	492856.886715	45.591002
3502.888723	492842.355443	45.596007
3503.222159	492824.072563	45.601012
3502.878720	492825.949978	45.606017
3502.941746	492814.647466	45.611021
3503.123379	492817.252126	45.616026
3503.132572	492797.349359	45.621031
3502.924905	492786.494733	45.626036
3502.681305	492775.038102	45.631041
3503.025969	492779.288113	45.636045
3503.071015	492781.306688	45.641050
3502.899307	492774.497556	45.646055
3503.132185	492745.646767	45.651060
3503.044032	492733.405942	45.656065
3503.221026	492716.464322	45.661069
3502.883013	492733.532878	45.666074
3503.176537	492719.408678	45.671079
3503.331494	492712.446611	45.676084
3503.490549	492685.987477	45.681089
3503.419752	492678.453398	45.686093
3503.220693	492650.126493	45.691098
3502.976676	492634.871828	45.696103
3503.338800	492629.750673	45.701108
3503.196725	492632.457164	45.706113
3503.609968	492602.716760	45.711117
3503.105311	492601.783823	45.716122
3503.479993	492586.178126	45.721127
3503.349650	492571.108003	45.726132
3503.129749	492550.633497	45.731137
3503.365035	492545.025961	45.736141
3503.180125	492521.203622	45.741146
3503.232369	492502.509106	45.746151
3503.238301	492497.039089	45.751156
3503.182740	492490.464697	45.756161
3503.382981	492472.151884	45.761165
3503.138829	492458.365674	45.766170
3503.112552	492454.875722	45.771175
3503.381252	492441.666768	45.776180
3502.972541	492425.070662	45.781185
3503.045741	492410.373362	45.786189
3502.945370	492422.340560	45.791194
3502.825117	492408.433447	45.796199
3503.119901	492400.942754	45.801204
3502.936694	492383.399432	45.806209
3503.073731	492353.601005	45.811213
3502.830351	492361.742131	45.816218
3502.875306	492362.950511	45.821223
3502.819896	492350.451053	45.826228
3502.757497	492361.196904	45.831233
3503.090281	492340.736091	45.836237
3503.070594	492337.700845	45.841242
3503.149411	492313.228862	45.846247
3503.014794	492318.871402	45.851252
3502.743076	492315.217654	45.856257
3503.300073	492309.052788	45.861261
3503.203253	492285.266862	45.866266
3503.154759	492276.209860	45.871271
3503.433357	492263.505627	45.876276
3503.081845	492253.888813	45.881281
3503.030251	492246.047676	45.886285
3503.063232	492234.395070	45.891290
3503.188887	492223.740636	45.896295
3503.078223	492213.022265	45.901300
3502.826804	492203.288322	45.906305
3503.416660	492175.494334	45.911309
3503.198746	492185.859735	45.916314
3503.139269	492173.512725	45.921319
3502.965678	492151.207365	45.926324
3502.708845	492145.880060	45.931329
3503.233026	492129.642652	45.936333
3503.100999	492133.259175	45.941338
3502.886956	492136.179680	45.946343
3503.136671	492115.984957	45.951348
3503.104407	492104.798357	45.956353
3503.092366	492092.393154	45.961357
3503.128805	492079.929638	45.966362
3502.971293	492083.246348	45.971367
3503.320103	492050.527385	45.976372
3503.012218	492042.827954	45.981377
3503.160442	492036.575684	45.986381
3503.100617	492040.889798	45.991386
3502.967896	492020.249001	45.996391
3503.256355	491990.071564	46.001396
3503.050268	492005.296825	46.006401
3503.234254	491986.935461	46.011405
3503.138046	491985.634079	46.016410
3502.768736	491972.930772	46.021415
3503.239168	491948.598978	46.026420
3502.959805	491953.049097	46.031425
3503.173332	491943.393454	46.036429
3503.009151	491933.088517	46.041434
3503.114840	491906.180928	46.046439
3503.053516	491897.581549	46.051444
3502.795076	491906.079749	46.056449
3502.611032	491896.132427	46.061453
3502.945389	491895.117479	46.066458
3502.879199	491898.318504	46.071463
3502.966262	491869.894540	46.076468
3502.932605	491877.901444	46.081473
3503.174921	491854.365217	46.086477
3502.993642	491869.333456	46.091482
3502.966969	491849.992407	46.096487
3503.336461	491839.400497	46.101492
3502.662440	491826.492040	46.106497
3502.932267	491809.990702	46.111501
3503.043319	491807.542414	46.116506
3502.731105	491809.566921	46.121511
3502.905890	491803.563587	46.126516
3502.647423	491820.012698	46.131521
3502.774775	491802.672952	46.136525
3502.619218	491784.365056	46.141530
3502.786786	491777.907071	46.146535
3502.889446	491767.610508	46.151540
3502.791899	491774.665346	46.156545
3502.949685	491770.690389	46.161549
3503.209945	491765.838312	46.166554
3502.958921	491752.660374	46.171559
3503.352645	491742.368434	46.176564
3503.078809	491727.370948	46.181569
3502.945796	491707.489490	46.186573
3502.970400	491718.019391	46.191578
3502.877242	491711.146808	46.196583
3503.135657	491703.712227	46.201588
3502.813717	491691.051881	46.206593
3502.802258	491687.255586	46.211597
3502.994977	491679.071737	46.216602
3502.911207	491676.958082	46.221607
3502.966044	491675.531519	46.226612
3503.092778	491661.027737	46.231617
3502.939734	491643.023161	46.236621
3502.907468	491639.432717	46.241626
3502.695536	491626.501725	46.246631
3503.134262	491622.684904	46.251636
3502.696938	491627.615855	46.256641
3502.834722	491617.566872	46.261645
3503.104084	491618.537259	46.266650
3502.813999	491587.032610	46.271655
3502.949123	491589.239650	46.276660
3502.826823	491579.383684	46.281665
3503.174456	491568.693790	46.286669
3502.887569	491566.510941	46.291674
3503.094496	491559.894730	46.296679
3503.289705	491528.009417	46.301684
3503.040693	491541.519972	46.306689
3502.832687	491527.068994	46.311693
3503.037882	491528.454675	46.316698
3502.799246	491512.641160	46.321703
3503.020618	491499.641592	46.326708
3502.774903	491497.401584	46.331713
3503.041718	491495.586999	46.336717
3502.752415	491503.077394	46.341722
3502.943781	491493.779525	46.346727
3503.304696	491477.516713	46.351732
3502.797332	491462.657211	46.356737
3502.863158	491445.529432	46.361741
3502.927726	491443.594878	46.366746
3503.048750	491444.386147	46.371751
3503.319879	491433.505694	46.376756
3502.976304	491425.153282	46.381761
3502.985924	491405.552818	46.386765
3502.795996	491410.849870	46.391770
3502.893491	491407.745306	46.396775
3503.353314	491384.933761	46.401780
3503.027752	491388.834236	46.406785
3503.267279	491361.296983	46.411789
3503.085796	491362.338644	46.416794
3503.129234	491351.291557	46.421799
3503.174256	491351.132613	46.426804
3503.025022	491331.152029	46.431809
3503.145574	491319.687584	46.436813
3503.231614	491304.835451	46.441818
3502.965158	491305.232176	46.446823
3503.277297	491274.290180	46.451828
3503.351381	491267.745508	46.456833
3503.197205	491264.427480	46.461837
3503.216229	491250.193623	46.466842
3503.156693	491240.783353	46.471847
3503.295543	491212.350200	46.476852
3503.021617	491220.901804	46.481857
3503.298866	491191.889660	46.486861
3503.307455	491184.291783	46.491866
3503.056283	491165.643882	46.496871
3503.067926	491167.971779	46.501876
3503.087113	491164.879552	46.506881
3503.136993	491148.817549	46.511885
3503.324973	491127.567985	46.516890
3502.921595	491134.215605	46.521895
3503.181253	491105.915128	46.526900
3502.607518	491092.281286	46.531905
3502.937670	491072.325942	46.536909
3502.789505	491080.148709	46.541914
3502.696992	491071.351300	46.546919
3502.999028	491078.495176	46.551924
3502.875388	491082.059932	46.556929
3502.979464	491081.638429	46.561933
3502.883691	491056.584657	46.566938
3502.903840	491049.187475	46.571943
3503.201924	491036.378039	46.576948
3503.023665	491038.229521	46.581953
3502.988573	491043.350270	46.586957
3503.118580	491032.745112	46.591962
3503.072489	491007.075685	46.596967
3503.127874	490989.949138	46.601972
3503.162908	490983.410538	46.606977
3503.233951	490978.942677	46.611981
3503.151951	490954.848840	46.616986
3503.272207	490954.272843	46.621991
3503.045009	490932.835457	46.626996
3503.057323	490949.647693	46.632001
3503.066281	490914.600148	46.637005
3503.318582	490903.773008	46.642010
3503.114990	490903.197551	46.647015
3502.917300	490890.517021	46.652020
3502.958495	490891.726092	46.657025
3502.851530	490865.914158	46.662029
3503.097656	490859.696665	46.667034
3502.964060	490838.801471	46.672039
3503.073153	490846.279803	46.677044
3503.064509	490842.330956	46.682049
3502.968627	490820.923330	46.687053
3503.134851	490812.388774	46.692058
3502.926527	490801.583735	46.697063
3503.069752	490802.270233	46.702068
3503.098962	490801.708621	46.707073
3503.127358	490786.561316	46.712077
3503.051340	490784.091818	46.717082
3502.711854	490767.331351	46.722087
3503.255433	490760.611002	46.727092
3502.926139	490762.891546	46.732097
3502.849157	490745.431179	46.737101
3503.070507	490721.390385	46.742106
3503.069305	490717.237753	46.747111
3502.842497	490706.283645	46.752116
3502.786247	490710.242984	46.757121
3502.855632	490713.979882	46.762125
3503.090700	490706.801823	46.767130
3502.902724	490695.537698	46.772135
3503.337694	490657.231670	46.777140
3502.900821	490667.176712	46.782145
3502.945343	490662.712968	46.787149
3502.860187	490659.535859	46.792154
3502.709254	490653.836866	46.797159
3502.818494	490624.394588	46.802164
3503.043863	490618.939981	46.807169
3502.774529	490611.993548	46.812173
3503.126992	490613.913123	46.817178
3502.725130	490613.520933	46.822183
3503.056552	490613.468651	46.827188
3502.612997	490604.118759	46.832193
3502.704155	490590.683329	46.837197
3502.915322	490569.733341	46.842202
3502.634649	490574.589160	46.847207
3502.991186	490557.363971	46.852212
3503.234950	490570.544109	46.857217
3503.016132	490566.780361	46.862221
3503.090697	490567.730949	46.867226
3503.036986	490551.077056	46.872231
3503.503820	490521.122281	46.877236
3503.119122	490522.246754	46.882241
3503.107617	490507.763927	46.887245
3503.256930	490489.102695	46.892250
3503.099808	490479.808758	46.897255
3503.326156	490471.922943	46.902260
3502.872271	490475.691951	46.907265
3502.728496	490447.758122	46.912269
3502.952939	490437.694808	46.917274
3502.932728	490429.442776	46.922279
3503.205294	490416.383718	46.927284
3502.944598	490428.934644	46.932289
3502.700137	490425.428151	46.937293
3502.940692	490396.015404	46.942298
3502.752920	490399.944951	46.947303
3502.785863	490377.908700	46.952308
3502.898164	490383.056979	46.957313
3502.982381	490371.597696	46.962317
3503.006575	490383.698452	46.967322
3503.101179	490381.809687	46.972327
3503.258190	490350.536159	46.977332
3503.373998	490337.400531	46.982337
3503.127489	490339.212223	46.987341
3503.156387	490323.304767	46.992346
3503.174469	490305.119912	46.997351
3503.096127	490286.241229	47.002356
3503.001440	490285.800478	47.007361
3503.305559	490279.978800	47.012365
3503.330416	490260.070846	47.017370
3502.916935	490239.320514	47.022375
3503.277145	490227.918814	47.027380
3503.203838	490235.578161	47.032385
3503.027977	490216.714821	47.037389
3503.152413	490203.476442	47.042394
3502.976295	490202.086271	47.047399
3502.924000	490197.840307	47.052404
3503.201518	490185.185480	47.057409
3503.098190	490172.844076	47.062413
3503.150586	490153.286184	47.067418
3502.780995	490142.911430	47.072423
3503.142329	490140.879188	47.077428
3503.253383	490133.365983	47.082433
3503.068419	490107.413389	47.087437
3503.031128	490096.884792	47.092442
3502.747851	490098.094553	47.097447
3502.962141	490098.668550	47.102452
3502.947140	490098.974907	47.107457
3502.812174	490078.889434	47.112461
3502.835063	490053.106501	47.117466
3502.714823	490056.265737	47.122471
3503.134471	490045.918123	47.127476
3502.846548	490050.370044	47.132481
3502.846999	490051.940140	47.137485
3502.837527	490050.827501	47.142490
3502.676777	490051.460779	47.147495
3503.026535	490047.353821	47.152500
3502.567491	490026.357218	47.157505
3502.683945	490025.528557	47.162509
3502.877346	490024.535793	47.167514
3502.407997	490020.102470	47.172519
3502.928665	490023.413646	47.177524
3502.738623	490021.924368	47.182529
3502.466783	490020.042840	47.187533
3502.902392	490010.503041	47.192538
3502.627608	490018.143676	47.197543
3502.635829	490011.102501	47.202548
3502.506716	490023.278368	47.207553
3502.953465	490021.536497	47.212557
3502.949197	489997.986262	47.217562
3502.790556	489987.831315	47.222567
3502.963131	489970.938550	47.227572
3503.069063	489967.072703	47.232577
3502.853058	489970.753564	47.237581
3502.851976	489961.991828	47.242586
3502.909333	489963.704879	47.247591
3502.951350	489934.879912	47.252596
3502.779654	489925.841242	47.257601
3502.430745	489919.565546	47.262605
3502.786358	489913.229140	47.267610
3502.738126	489920.226234	47.272615
3503.443671	489917.075964	47.277620
3503.250789	489913.561222	47.282625
3503.136588	489895.548822	47.287629
3503.025253	489875.408748	47.292634
3503.169607	489872.803001	47.297639
3503.275487	489872.178597	47.302644
3502.821298	489845.407183	47.307649
3502.739413	489831.897266	47.312653
3503.114656	489823.025336	47.317658
3502.723366	489833.824625	47.322663
3503.196488	489824.076212	47.327668
3503.121998	489821.505049	47.332673
3502.902467	489808.067518	47.337677
3503.048024	489783.075192	47.342682
3502.768790	489784.486925	47.347687
3503.033725	489780.140076	47.352692
3502.655370	489778.933783	47.357697
3502.947250	489777.418961	47.362701
3503.394555	489765.344791	47.367706
3503.019750	489759.073135	47.372711
3502.999989	489734.005577	47.377716
3503.008774	489738.765210	47.382721
3502.688453	489740.740570	47.387725
3502.768417	489734.143784	47.392730
3502.859433	489721.872661	47.397735
3502.650949	489698.658218	47.402740
3502.706918	489683.809552	47.407745
3502.895121	489688.794081	47.412749
3503.282355	489669.030816	47.417754
3502.411304	489687.655202	47.422759
3502.863351	489677.251617	47.427764
3503.016863	489686.394784	47.432769
3503.289061	489671.359987	47.437773
3502.994954	489662.087296	47.442778
3502.562428	489649.949525	47.447783
3502.884263	489641.643083	47.452788
3502.703208	489641.722452	47.457793
3502.768777	489643.332938	47.462797
3502.897919	489643.211332	47.467802
3502.701879	489645.116409	47.472807
3502.944054	489634.442083	47.477812
3502.879705	489611.761882	47.482817
3502.976760	489601.414365	47.487821
3502.622072	489592.505754	47.492826
3502.642936	489596.047952	47.497831
3503.000286	489588.343654	47.502836
3503.132759	489592.982477	47.507841
3503.028392	489592.340646	47.512845
3503.400378	489563.412306	47.517850
3502.840264	489566.793096	47.522855
3503.023372	489549.442450	47.527860
3503.019998	489548.582061	47.532865
3502.698303	489539.668209	47.537869
3502.912458	489522.413929	47.542874
3503.067004	489513.222196	47.547879
3503.267026	489498.401264	47.552884
3503.101980	489504.910489	47.557889
3502.859468	489500.035998	47.562893
3503.104899	489496.451898	47.567898
3502.869947	489488.030799	47.572903
3502.891279	489470.300461	47.577908
3503.008868	489472.814418	47.582913
3503.128510	489458.613944	47.587917
3503.124851	489458.817221	47.592922
3502.964234	489443.749355	47.597927
3503.130509	489410.142950	47.602932
3502.950114	489410.171566	47.607937
3503.024003	489409.298958	47.612941
3503.049524	489399.773020	47.617946
3502.786866	489371.957678	47.622951
3503.056295	489366.495745	47.627956
3503.156961	489369.974722	47.632961
3502.930480	489359.475615	47.637965
3502.979710	489361.797794	47.642970
3502.980612	489363.317227	47.647975
3503.214577	489332.181788	47.652980
3503.150753	489312.185548	47.657985
3502.943534	489321.537858	47.662989
3503.089279	489307.333145	47.667994
3503.154599	489302.359298	47.672999
3503.293065	489277.671317	47.678004
3503.030346	489275.889570	47.683009
3502.957754	489270.127124	47.688013
3503.222512	489268.262003	47.693018
3502.733752	489244.838052	47.698023
3503.015447	489227.116982	47.703028
3503.177366	489226.686296	47.708033
3502.854538	489229.928340	47.713037
3503.220393	489220.095272	47.718042
3503.011914	489207.314008	47.723047
3502.935400	489191.675502	47.728052
3502.520481	489184.498301	47.733057
3502.968404	489186.352289	47.738061
3503.293087	489179.108834	47.743066
3502.935528	489184.990153	47.748071
3503.223956	489147.261356	47.753076
3503.080648	489126.213839	47.758081
3502.738230	489138.575942	47.763085
3503.215380	489120.823878	47.768090
3502.839061	489125.391288	47.773095
3502.743415	489103.627116	47.778100
3502.964865	489098.729837	47.783105
3502.742717	489094.003971	47.788109
3503.207865	489093.170806	47.793114
3502.680842	489088.493127	47.798119
3502.851694	489095.405250	47.803124
3503.235473	489088.152420	47.808129
3502.695700	489071.472741	47.813133
3502.935950	489050.111264	47.818138
3502.998038	489045.289810	47.823143
3502.781299	489030.787633	47.828148
3503.056874	489047.965163	47.833153
3503.051541	489036.468571	47.838157
3503.280454	489021.845298	47.843162
3502.726521	489011.752303	47.848167
3503.101373	488997.460494	47.853172
3503.141424	488998.821818	47.858177
3503.046496	488994.632970	47.863181
3502.964415	488972.562602	47.868186
3503.285319	488953.011672	47.873191
3503.123536	488950.150286	47.878196
3503.002499	488961.160608	47.883201
3502.929173	488955.246231	47.888205
3502.931557	488926.679235	47.893210
3503.017767	488924.538401	47.898215
3503.008844	488908.990278	47.903220
3503.263519	488911.330691	47.908225
3502.934411	488912.699720	47.913229
3503.193727	488880.799775	47.918234
3503.063166	488860.053848	47.923239
3503.084985	488855.188059	47.928244
3503.099896	488852.248079	47.933249
3502.915378	488846.503195	47.938253
3503.577336	488821.124067	47.943258
3502.805008	488819.878679	47.948263
3502.875579	488803.152942	47.953268
3503.060419	488816.394278	47.958273
3503.234397	488801.171710	47.963277
3503.194770	488766.026533	47.968282
3503.078946	488775.465969	47.973287
3503.164051	488758.231387	47.978292
3503.449390	488756.818820	47.983297
3502.961800	488732.887540	47.988301
3503.338788	488724.217422	47.993306
3503.148736	488728.755485	47.998311
3502.856570	488699.778845	48.003316
3503.054783	488673.459802	48.008321
3502.940564	488681.734058	48.013325
3503.113789	488668.284285	48.018330
3503.005979	488671.593740	48.023335
3503.292930	488650.021826	48.028340
3503.073293	488633.898969	48.033345
3503.135497	488632.065803	48.038349
3503.169629	488624.361550	48.043354
3502.803328	488624.824759	48.048359
3502.710293	488610.809217	48.053364
3503.024793	488584.826228	48.058369
3502.556255	488585.812109	48.063373
3502.871201	488569.908608	48.068378
3502.755713	488576.309017	48.073383
3502.891155	488571.070638	48.078388
3502.601328	488561.644773	48.083393
3502.485444	488575.288369	48.088397
3502.728246	488563.347060	48.093402
3502.558336	488580.392824	48.098407
3502.838260	488562.823365	48.103412
3502.754563	488568.509634	48.108417
3502.593488	488569.953430	48.113421
3502.852859	488546.511662	48.118426
3502.639328	488551.509340	48.123431
3503.121594	488540.239284	48.128436
3503.051875	488536.451560	48.133441
3502.745752	488546.022491	48.138445
3503.021740	488532.201819	48.143450
3502.786723	488543.179749	48.148455
3502.736662	488512.138502	48.153460
3502.734489	488496.487669	48.158465
3502.750230	488485.645880	48.163469
3502.852349	488487.554596	48.168474
3502.600904	488494.634990	48.173479
3502.568001	488480.305938	48.178484
3502.706924	488477.700859	48.183489
3502.515377	488483.556155	48.188493
3502.957653	488483.840912	48.193498
3502.744353	488494.815437	48.198503
3502.598157	488491.748912	48.203508
3502.999915	488489.203593	48.208513
3502.981038	488471.022808	48.213517
3503.247712	488458.976356	48.218522
3502.947752	488451.932658	48.223527
3502.805028	488434.429883	48.228532
3502.994584	488436.729997	48.233537
3502.624320	488447.628057	48.238541
3502.687021	488433.334509	48.243546
3502.720823	488418.539003	48.248551
3502.547550	488409.043987	48.253556
3502.619042	488386.492795	48.258561
3502.463314	488387.429243	48.263565
3502.794024	488384.337971	48.268570
3502.487770	488387.780145	48.273575
3502.610745	488392.572722	48.278580
3502.699717	488376.755428	48.283585
3502.604723	488391.966059	48.288589
3502.775794	488392.850853	48.293594
3502.836450	488396.842852	48.298599
3502.775002	488388.748397	48.303604
3503.097667	488390.571612	48.308609
3502.813700	488388.084014	48.313613
3503.023371	488368.448759	48.318618
3502.770800	488351.925653	48.323623
3502.869365	488345.933263	48.328628
3503.003101	488343.278334	48.333633
3502.418435	488347.169735	48.338637
3502.948653	488334.423075	48.343642
3502.900273	488337.216676	48.348647
3502.833049	488339.456085	48.353652
3502.881747	488316.959065	48.358657
3502.890840	488304.801273	48.363661
3502.988865	488291.717682	48.368666
3503.020186	488295.866294	48.373671
3502.514911	488301.264714	48.378676
3503.040396	488284.618570	48.383681
3502.918470	488288.436843	48.388685
3503.147038	488279.080854	48.393690
3502.975785	488272.219353	48.398695
3503.162919	488253.195364	48.403700
3502.873074	488246.960423	48.408705
3502.811859	488242.310210	48.413709
3503.040001	488251.948800	48.418714
3502.606879	488234.390436	48.423719
3502.847261	488216.624296	48.428724
3503.074002	488202.760516	48.433729
3502.698444	488209.658025	48.438733
3502.939204	488205.871812	48.443738
3502.985879	488205.104755	48.448743
3502.969603	488196.901774	48.453748
3503.339860	488165.844175	48.458753
3502.907304	488170.522006	48.463757
3502.739366	488148.514898	48.468762
3502.896341	488160.950661	48.473767
3502.760902	488159.300645	48.478772
3502.869950	488151.027183	48.483777
3502.723475	488156.926108	48.488781
3502.645361	488136.120443	48.493786
3502.629570	488127.816051	48.498791
3502.816265	488118.314644	48.503796
3503.228150	488110.550475	48.508801
3502.697653	488108.608330	48.513805
3502.797110	488106.009438	48.518810
3502.787554	488105.656484	48.523815
3503.005368	488105.318245	48.528820
3502.863059	488094.146645	48.533825
3502.438584	488075.826979	48.538829
3502.746467	488067.775315	48.543834
3502.698289	488067.732381	48.548839
3502.619577	488058.272894	48.553844
3502.632650	488056.852659	48.558849
3502.434137	488063.772889	48.563853
3503.098339	488054.601196	48.568858
3502.939779	488056.348549	48.573863
3502.897415	488053.822719	48.578868
3503.062332	488051.061515	48.583873
3502.937039	488055.234934	48.588877
3503.093406	488027.148766	48.593882
3502.855109	488014.624669	48.598887
3502.724992	488011.555523	48.603892
3503.019302	488006.038614	48.608897
3502.688557	488012.422584	48.613901
3502.769605	488008.610923	48.618906
3502.911058	488008.183446	48.623911
3502.695583	487990.185232	48.628916
3503.036998	487976.252508	48.633921
3502.761585	487974.725906	48.638925
3502.593165	487965.787080	48.643930
3502.537428	487964.225755	48.648935
3502.711531	487965.262049	48.653940
3503.164725	487962.607226	48.658945
3502.945911	487957.576630	48.663949
3503.050834	487948.594592	48.668954
3502.897809	487936.259576	48.673959
3503.044988	487926.207137	48.678964
3503.131988	487913.378292	48.683969
3502.964753	487923.839337	48.688973
3503.099306	487907.609224	48.693978
3502.852815	487894.529160	48.698983
3502.778530	487869.822314	48.703988
3503.109554	487871.948178	48.708993
3502.828158	487875.690433	48.713997
3502.950398	487880.331297	48.719002
3503.160956	487874.219751	48.724007
3502.902103	487860.888352	48.729012
3503.181330	487832.985089	48.734017
3503.304452	487826.482122	48.739021
3503.004851	487822.376017	48.744026
3503.171606	487816.828562	48.749031
3503.117296	487801.084088	48.754036
3503.231985	487787.744249	48.759041
3502.880331	487798.285166	48.764045
3502.986174	487786.010442	48.769050
3502.941480	487782.269264	48.774055
3502.866545	487769.617877	48.779060
3503.054962	487741.374259	48.784065
3502.804610	487733.511996	48.789069
3503.025613	487736.567028	48.794074
3502.470290	487743.138545	48.799079
3502.952083	487737.642578	48.804084
3502.862377	487733.452624	48.809089
3502.633781	487733.438205	48.814093
3502.644020	487700.562572	48.819098
3502.802125	487687.874296	48.824103
3502.841015	487688.780016	48.829108
3502.972527	487691.393318	48.834113
3502.815578	487694.812017	48.839117
3502.972846	487685.922888	48.844122
3503.212362	487699.207019	48.849127
3503.004895	487668.442535	48.854132
3503.169366	487655.601271	48.859137
3502.759895	487649.030464	48.864141
3502.902637	487642.220412	48.869146
3503.104393	487632.361806	48.874151
3502.696877	487642.759677	48.879156
3502.897987	487637.358700	48.884161
3502.817169	487614.324127	48.889165
3502.782426	487604.047003	48.894170
3502.837148	487613.865291	48.899175
3503.187517	487599.019108	48.904180
3502.945978	487590.142316	48.909185
3503.099235	487586.065888	48.914189
3503.061348	487567.583317	48.919194
3503.215502	487556.769772	48.924199
3503.052177	487548.336483	48.929204
3503.052774	487541.143630	48.934209
3503.015710	487529.955062	48.939213
3503.144484	487509.825165	48.944218
3502.998942	487501.338390	48.949223
3503.037174	487498.495822	48.954228
3503.094193	487490.280950	48.959233
3502.999712	487480.671706	48.964237
3503.049324	487470.077252	48.969242
3503.313989	487449.368616	48.974247
3502.865455	487453.897184	48.979252
3503.050173	487440.748649	48.984257
3503.044415	487428.947222	48.989261
3503.031703	487410.916408	48.994266
3502.892817	487404.049476	48.999271
3502.653059	487410.824500	49.004276
3502.643305	487405.710058	49.009281
3502.768828	487408.223037	49.014285
3502.924579	487410.174040	49.019290
3503.188182	487392.656732	49.024295
3503.068162	487374.288264	49.029300
3502.630722	487361.693902	49.034305
3502.698726	487351.704329	49.039309
3502.984064	487346.492574	49.044314
3502.749916	487357.420397	49.049319
3502.598063	487360.078534	49.054324
3503.022673	487340.306933	49.059329
3502.889194	487345.494892	49.064333
3502.742047	487323.939429	49.069338
3502.627994	487317.727050	49.074343
3502.650384	487309.466919	49.079348
3503.012829	487297.201975	49.084353
3502.869248	487309.787113	49.089357
3503.158452	487307.259430	49.094362
3503.160335	487300.015628	49.099367
3503.003660	487290.365462	49.104372
3502.974058	487273.248970	49.109377
3503.047809	487263.410406	49.114381
3502.746409	487267.409215	49.119386
3503.156120	487259.138497	49.124391
3502.722276	487253.432535	49.129396
3502.713049	487230.436834	49.134401
3502.687898	487232.517759	49.139405
3502.823233	487223.327952	49.144410
3502.970234	487217.023622	49.149415
3502.707737	487229.779573	49.154420
3503.112348	487213.100944	49.159425
3502.736462	487228.407559	49.164429
3502.885306	487211.718700	49.169434
3502.988487	487193.669362	49.174439
3502.904515	487182.690623	49.179444
3503.059268	487176.030470	49.184449
3502.635441	487184.253007	49.189453
3502.801280	487173.133467	49.194458
3502.998903	487175.229841	49.199463
3502.760887	487171.772374	49.204468
3503.005468	487159.981867	49.209473
3502.719237	487144.476126	49.214477
3502.601750	487125.752432	49.219482
3502.759379	487128.969544	49.224487
3502.666471	487132.479531	49.229492
3502.869623	487118.922620	49.234497
3502.533009	487121.863268	49.239501
3502.821216	487124.958432	49.244506
3502.947839	487114.098332	49.249511
3502.529585	487119.888570	49.254516
3503.020299	487112.263501	49.259521
3502.728149	487109.523750	49.264525
3502.786697	487084.440301	49.269530
3502.662111	487079.951784	49.274535
3502.587308	487072.162809	49.279540
3503.076886	487066.260179	49.284545
3502.466136	487073.296582	49.289549
3502.772123	487064.636933	49.294554
3502.728929	487067.480556	49.299559
3502.587604	487081.078593	49.304564
3502.698782	487071.791221	49.309569
3502.742089	487075.178378	49.314573
3502.760118	487067.830625	49.319578
3502.974684	487078.738339	49.324583
3502.785016	487052.326390	49.329588
3502.692885	487038.208230	49.334593
3502.919239	487043.592673	49.339597
3502.925498	487037.310529	49.344602
3502.809974	487033.327122	49.349607
3502.691921	487043.932843	49.354612
3502.861922	487027.139168	49.359617
3502.907084	487029.614243	49.364621
3502.872309	487018.121080	49.369626
3502.903088	487002.210529	49.374631
3502.816587	486987.787510	49.379636
3502.856198	486965.138358	49.384641
3502.601396	486989.645325	49.389645
3502.923270	486981.590992	49.394650
3502.975350	486978.644847	49.399655
3502.667077	486980.719894	49.404660
3502.673895	486975.805339	49.409665
3502.750537	486963.484045	49.414669
3502.654789	486949.467702	49.419674
3502.991137	486942.576142	49.424679
3502.901825	486937.474150	49.429684
3503.259914	486934.023730	49.434689
3502.700940	486944.547231	49.439693
3502.910010	486937.523821	49.444698
3503.290883	486920.747376	49.449703
3502.791983	486910.796521	49.454708
3502.971895	486902.713938	49.459713
3502.611525	486891.981341	49.464717
3502.868531	486886.672629	49.469722
3502.923547	486890.665837	49.474727
3502.663079	486888.326291	49.479732
3503.090270	486884.257071	49.484737
3502.946196	486864.372241	49.489741
3502.847349	486850.305659	49.494746
3503.236908	486836.820395	49.499751
3502.505543	486849.448087	49.504756
3503.088445	486840.389976	49.509761
3502.793721	486841.551091	49.514765
3502.721004	486822.060184	49.519770
3502.946115	486808.448926	49.524775
3502.731514	486800.833904	49.529780
3502.949552	486784.336357	49.534785
3502.904935	486795.031921	49.539789
3502.806194	486786.182837	49.544794
3502.815086	486792.361563	49.549799
3502.638840	486801.608905	49.554804
3502.700398	486788.732667	49.559809
3502.927558	486768.535779	49.564813
3502.781769	486754.729826	49.569818
3502.948962	486760.225013	49.574823
3502.706545	486754.893891	49.579828
3503.144495	486747.175705	49.584833
3502.920783	486753.999081	49.589837
3503.026148	486744.661813	49.594842
3503.112674	486725.905478	49.599847
3502.699875	486714.573195	49.604852
3502.834109	486699.456537	49.609857
3502.714915	486702.616165	49.614861
3502.786093	486694.145431	49.619866
3502.761011	486691.059468	49.624871
3502.558012	486700.665682	49.629876
3502.971303	486679.375499	49.634881
3502.963075	486695.992148	49.639885
3502.498518	486679.247809	49.644890
3503.062390	486660.112023	49.649895
3503.050357	486654.339208	49.654900
3503.126084	486649.413677	49.659905
3503.006950	486649.635236	49.664909
3502.946591	486637.993918	49.669914
3502.838259	486618.052524	49.674919
3502.469790	486603.775095	49.679924
3503.058224	486604.999258	49.684929
3502.721078	486604.951337	49.689933
3502.707209	486611.133719	49.694938
3502.572205	486597.123322	49.699943
3502.639133	486598.885822	49.704948
3502.585839	486591.093251	49.709953
3502.589352	486596.563699	49.714957
3502.725975	486599.024374	49.719962
3502.959098	486597.315966	49.724967
3502.830728	486594.448940	49.729972
3502.776032	486582.452098	49.734977
3502.700966	486567.469731	49.739981
3502.526858	486563.039576	49.744986
3502.809925	486553.674126	49.749991
3502.727653	486550.242585	49.754996
3502.991530	486550.656889	49.760001
3502.930387	486552.540950	49.765005
3502.726950	486552.370582	49.770010
3502.999504	486554.505838	49.775015
3502.547764	486545.864408	49.780020
3503.020004	486533.328338	49.785025
3502.738007	486522.481831	49.790029
3502.411184	486510.274672	49.795034
3502.622620	486514.851116	49.800039
3502.685146	486501.771904	49.805044
3502.596371	486507.560905	49.810049
3502.561485	486517.748519	49.815053
3502.678437	486504.458079	49.820058
3502.863736	486512.888565	49.825063
3502.712976	486517.370286	49.830068
3503.112295	486494.157152	49.835073
3502.982934	486499.749943	49.840077
3502.733151	486494.825166	49.845082
3503.204753	486471.549922	49.850087
3502.778165	486474.150292	49.855092
3503.107922	486469.336534	49.860097
3502.865362	486466.436880	49.865101
3502.595792	486462.072447	49.870106
3502.986594	486463.783769	49.875111
3502.810623	486458.695346	49.880116
3503.231804	486429.247884	49.885121
3503.179900	486429.154877	49.890125
3502.998647	486414.037203	49.895130
3503.504836	486412.386932	49.900135
3502.954096	486393.984283	49.905140
3503.022051	486382.170556	49.910145
3502.626121	486379.447102	49.915149
3502.962858	486376.709156	49.920154
3503.054716	486369.805378	49.925159
3502.779157	486379.575193	49.930164
3502.588727	486345.462510	49.935169
3502.970449	486331.826158	49.940173
3502.788792	486322.382079	49.945178
3502.753127	486321.729275	49.950183
3502.766637	486330.085680	49.955188
3503.066537	486316.411593	49.960193
3502.705716	486323.763366	49.965197
3502.682145	486322.500764	49.970202
3503.047337	486310.184097	49.975207
3502.666552	486305.077348	49.980212
3502.932535	486285.532358	49.985217
3502.887620	486290.352003	49.990221
3503.015458	486287.140490	49.995226
3503.157057	486277.949239	50.000231
3502.921505	486276.770797	50.005236
3503.066305	486262.411984	50.010241
3502.581998	486241.111217	50.015245
3502.674488	486237.044106	50.020250
3502.997372	486229.039955	50.025255
3502.841340	486238.031088	50.030260
3503.128926	486228.462136	50.035265
3503.336415	486226.048542	50.040269
3502.938746	486209.191901	50.045274
3502.808772	486190.722549	50.050279
3502.647659	486189.380364	50.055284
3502.803365	486180.642754	50.060289
3502.706669	486190.840312	50.065293
3502.910550	486187.566105	50.070298
3503.093702	486180.901117	50.075303
3502.918831	486181.739382	50.080308
3502.884666	486154.136484	50.085313
3502.884981	486142.941193	50.090317
3503.226711	486145.926742	50.095322
3502.961526	486139.028658	50.100327
3502.800254	486138.243729	50.105332
3502.835992	486128.106641	50.110337
3502.581779	486113.760127	50.115341
3502.584871	486095.826886	50.120346
3502.997586	486089.328212	50.125351
3502.830023	486090.165325	50.130356
3502.687755	486086.844499	50.135361
3502.551889	486089.956204	50.140365
3502.547835	486094.870756	50.145370
3502.627251	486080.876746	50.150375
3502.346847	486094.193521	50.155380
3502.892021	486079.973919	50.160385
3502.892375	486089.598955	50.165389
3502.706997	486089.273754	50.170394
3502.885045	486081.799013	50.175399
3502.661887	486084.620569	50.180404
3502.618331	486046.887431	50.185409
3502.416568	486058.418773	50.190413
3502.631618	486035.690130	50.195418
3502.677055	486036.797526	50.200423
3502.781993	486043.923814	50.205428
3502.900474	486030.531488	50.210433
3502.781817	486045.849049	50.215437
3502.654137	486033.711424	50.220442
3502.890073	486033.116997	50.225447
3502.884959	486037.423836	50.230452
3502.903404	486032.608516	50.235457
3502.957334	486022.113891	50.240461
3502.924727	486004.490155	50.245466
3502.879391	486000.140831	50.250471
3502.706373	486002.599868	50.255476
3502.948587	485993.443235	50.260481
3502.955007	485999.571950	50.265485
3502.961606	485999.419036	50.270490
3502.598292	485968.473805	50.275495
3502.606103	485965.534500	50.280500
3502.894745	485948.670467	50.285505
3502.981974	485943.084379	50.290509
3502.794951	485942.404828	50.295514
3503.084493	485946.006557	50.300519
3502.395474	485951.738627	50.305524
3503.119115	485943.924304	50.310529
3502.787977	485940.785280	50.315533
3502.843305	485939.560840	50.320538
3503.066785	485898.999000	50.325543
3502.781511	485911.151530	50.330548
3502.910376	485908.598350	50.335553
3502.757502	485901.733086	50.340557
3502.846060	485910.584395	50.345562
3502.956546	485900.131423	50.350567
3502.498144	485903.800722	50.355572
3502.629948	485903.121433	50.360577
3502.481835	485881.767125	50.365581
3502.434770	485877.823314	50.370586
3502.788422	485871.283244	50.375591
3502.883747	485862.605691	50.380596
3502.918530	485858.344988	50.385601
3502.751213	485852.799108	50.390605
3502.793645	485850.867483	50.395610
3502.683624	485852.151438	50.400615
3502.862869	485855.517325	50.405620
3503.044514	485853.665013	50.410625
3502.843678	485847.972455	50.415629
3502.634203	485832.909439	50.420634
3503.011236	485809.293730	50.425639
3502.583536	485817.061536	50.430644
3502.492227	485814.036558	50.435649
3502.777188	485807.811275	50.440653
3502.869619	485805.415816	50.445658
3502.804812	485788.810142	50.450663
3502.828764	485810.133726	50.455668
3502.678200	485808.941822	50.460673
3502.864591	485788.193099	50.465677
3502.685675	485795.161711	50.470682
3502.772901	485764.904817	50.475687
3502.698071	485762.535789	50.480692
3502.550339	485761.799363	50.485697
3502.639554	485760.164286	50.490701
3502.457092	485742.766630	50.495706
3502.923420	485755.003095	50.500711
3502.850049	485757.699706	50.505716
3502.855774	485749.694828	50.510721
3503.133879	485757.655050	50.515725
3502.600489	485743.656336	50.520730
3502.891654	485723.600205	50.525735
3502.638323	485703.174187	50.530740
3502.998556	485669.581165	50.535745
3502.525978	485615.957417	50.540749
3502.104114	485572.811959	50.545754
3502.369799	485500.884540	50.550759
3501.950872	485433.675082	50.555764
3502.175361	485349.190031	50.560769
3502.461762	485262.009842	50.565773
3501.773292	485163.787430	50.570778
3501.980113	485040.903291	50.575783
3501.745971	484932.881049	50.580788
3501.500551	484801.454509	50.585793
3501.163085	484659.858641	50.590797
3500.922975	484508.367256	50.595802
3500.937318	484353.490741	50.600807
3500.578056	484200.951861	50.605812
3500.117531	484035.761975	50.610817
3500.020670	483846.599925	50.615821
3499.687503	483685.845323	50.620826
3499.752609	483479.681581	50.625831
3499.277496	483284.088735	50.630836
3498.617737	483083.557857	50.635841
3498.505510	482867.383814	50.640845
3498.356154	482657.799923	50.645850
3498.318716	482431.121165	50.650855
3497.253605	482207.034270	50.655860
3496.974279	481976.740357	50.660865
3496.710272	481725.768253	50.665869
3496.248770	481492.811952	50.670874
3495.707766	481239.546570	50.675879
3495.283144	480988.995758	50.680884
3494.957030	480726.163587	50.685889
3494.444071	480482.612981	50.690893
3493.859959	480208.007961	50.695898
3494.007362	479944.533082	50.700903
3492.814626	479676.959173	50.705908
3492.869844	479387.089954	50.710913
3492.211613	479092.261649	50.715917
3491.613543	478813.838721	50.720922
3491.413258	478532.460385	50.725927
3490.759173	478237.061243	50.730932
3490.551628	477929.677557	50.735937
3489.859195	477627.231030	50.740941
3489.662131	477331.492804	50.745946
3489.540172	477012.424915	50.750951
3488.699847	476697.469375	50.755956
3488.019061	476383.091857	50.760961
3487.817156	476051.046447	50.765965
3486.758481	475722.172056	50.770970
3486.531301	475389.207388	50.775975
3485.647169	475063.487830	50.780980
3485.120637	474717.228896	50.785985
3484.748637	474394.306764	50.790989
3483.751599	474061.289842	50.795994
3483.477541	473719.029039	50.800999
3482.789805	473379.818604	50.806004
3482.090935	473042.936078	50.811009
3481.765279	472693.468028	50.816013
3480.823761	472357.981244	50.821018
3480.635434	471999.709739	50.826023
3479.747692	471654.875261	50.831028
3479.498379	471300.453995	50.836033
3478.831609	470949.134407	50.841037
3478.123586	470592.644223	50.846042
3477.715830	470236.658103	50.851047
3476.791256	469881.254548	50.856052
3475.721315	469522.825879	50.861057
3475.801297	469161.623508	50.866061
3475.065278	468805.208421	50.871066
3474.736098	468441.523160	50.876071
3473.793590	468071.590584	50.881076
3473.118207	467703.028967	50.886081
3472.740266	467339.230858	50.891085
3471.530397	466970.233813	50.896090
3471.470209	466588.016843	50.901095
3470.818831	466228.654289	50.906100
3470.022747	465850.089852	50.911105
3469.212248	465481.358619	50.916109
3468.715885	465104.102647	50.921114
3468.067352	464732.239461	50.926119
3467.212768	464359.489534	50.931124
3466.427849	463977.340125	50.936129
3465.857612	463608.944217	50.941133
3465.343483	463247.886794	50.946138
3464.786531	462862.537144	50.951143
3464.007277	462493.343693	50.956148
3463.198470	462105.687347	50.961153
3462.799051	461732.769171	50.966157
3461.932146	461369.910210	50.971162
3461.509867	460985.469475	50.976167
3460.453103	460619.990542	50.981172
3459.996672	460227.223539	50.986177
3459.389946	459852.834959	50.991181
3458.457841	459476.868249	50.996186
3458.086538	459100.603539	51.001191
3457.331943	458724.494431	51.006196
3456.203182	458348.640954	51.011201
3455.628033	457973.251556	51.016205
3455.119165	457599.265697	51.021210
3454.746932	457232.658364	51.026215
3453.769277	456851.784135	51.031220
3453.175793	456468.153924	51.036225
3452.584131	456106.432878	51.041229
3451.786646	455725.815322	51.046234
3451.080425	455335.943405	51.051239
3450.441036	454964.977999	51.056244
3449.537112	454598.310033	51.061249
3449.121855	454217.251345	51.066253
3448.234773	453847.219942	51.071258
3447.738342	453462.051688	51.076263
3446.766843	453092.833108	51.081268
3445.853636	452720.047572	51.086273
3445.599577	452348.369490	51.091277
3444.157179	451981.236933	51.096282
3443.995159	451604.813310	51.101287
3443.307226	451242.978999	51.106292
3442.164787	450876.085772	51.111297
3441.791432	450514.443983	51.116301
3441.298195	450149.161847	51.121306
3440.574384	449779.749245	51.126311
3439.387515	449421.415945	51.131316
3438.877196	449053.581912	51.136321
3438.430457	448688.066424	51.141325
3437.577821	448329.866461	51.146330
3436.950992	447957.415409	51.151335
3436.184333	447595.435132	51.156340
3435.403826	447234.212727	51.161345
3434.742197	446873.727260	51.166349
3433.886854	446517.783899	51.171354
3433.294915	446156.058381	51.176359
3432.443812	445801.930697	51.181364
3431.717351	445445.494042	51.186369
3431.484539	445092.932952	51.191373
3430.439394	444736.282275	51.196378
3429.937783	444381.266085	51.201383
3428.965109	444027.385020	51.206388
3428.316536	443665.529111	51.211393
3427.919500	443320.277128	51.216397
3427.017917	442969.364047	51.221402
3426.314554	442611.511020	51.226407
3425.660115	442259.837900	51.231412
3424.957535	441903.344844	51.236417
3424.710133	441533.728424	51.241421
3423.680061	441195.450020	51.246426
3423.125705	440828.105039	51.251431
3422.289230	440477.247169	51.256436
3421.263406	440129.409417	51.261441
3420.693470	439781.900792	51.266445
3419.652091	439435.527914	51.271450
3419.331145	439082.537914	51.276455
3418.555563	438746.317781	51.281460
3417.986036	438408.334331	51.286465
3417.089311	438053.999142	51.291469
3416.488738	437714.386499	51.296474
3415.504357	437369.600404	51.301479
3414.971096	437039.919222	51.306484
3414.056270	436697.879966	51.311489
3413.804841	436354.664904	51.316493
3412.661008	436015.698992	51.321498
3412.142532	435666.804619	51.326503
3411.520864	435340.872495	51.331508
3410.789208	435000.786872	51.336513
3410.192386	434658.085722	51.341517
3409.319844	434327.280209	51.346522
3408.522272	433990.999835	51.351527
3407.678069	433669.118341	51.356532
3406.951864	433335.357012	51.361537
3406.398484	432997.679288	51.366541
3405.587189	432675.907059	51.371546
3405.087139	432342.782611	51.376551
3404.252615	432025.246215	51.381556
3403.328053	431689.895240	51.386561
3403.095440	431358.061565	51.391565
3402.466551	431041.902539	51.396570
3401.540062	430706.336013	51.401575
3400.773390	430390.978032	51.406580
3400.005702	430060.101157	51.411585
3399.527405	429726.939710	51.416589
3398.705122	429413.686401	51.421594
3398.006311	429080.881737	51.426599
3397.429118	428763.569657	51.431604
3396.714747	428443.608998	51.436609
3396.128407	428119.307061	51.441613
3395.254066	427804.696937	51.446618
3394.617709	427479.074519	51.451623
3393.856036	427160.020098	51.456628
3393.362513	426832.284718	51.461633
3392.641605	426515.324038	51.466637
3391.676259	426203.376049	51.471642
3391.239801	425875.162788	51.476647
3390.480595	425559.365143	51.481652
3389.894083	425258.775173	51.486657
3389.130015	424927.605232	51.491661
3388.193333	424617.158231	51.496666
3387.683851	424286.473565	51.501671
3386.645582	423977.635432	51.506676
3385.898797	423671.516229	51.511681
3385.908045	423356.993793	51.516685
3384.527376	423037.302740	51.521690
3384.304712	422734.747763	51.526695
3383.288833	422421.113285	51.531700
3382.592595	422127.567460	51.536705
3382.006362	421804.510567	51.541709
3381.526340	421501.931947	51.546714
3380.530376	421192.928803	51.551719
3379.839345	420887.100038	51.556724
3379.151899	420573.951532	51.561729
3378.585788	420262.787113	51.566733
3377.780162	419970.074051	51.571738
3377.172949	419652.939718	51.576743
3376.450769	419351.366766	51.581748
3375.492701	419057.702965	51.586753
3374.945296	418757.416996	51.591757
3374.141626	418465.577093	51.596762
3373.216695	418155.233613	51.601767
3372.740287	417862.421193	51.606772
3372.389820	417563.336250	51.611777
3371.614196	417261.266781	51.616781
3370.641477	416970.911753	51.621786
3370.274826	416671.083263	51.626791
3369.612928	416373.051331	51.631796
3368.828071	416081.844599	51.636801
3368.191975	415776.332989	51.641805
3367.205449	415481.036231	51.646810
3366.603072	415190.807915	51.651815
3366.004917	414897.349309	51.656820
3365.079400	414598.121192	51.661825
3364.563009	414302.128307	51.666829
3363.467682	414018.800907	51.671834
3362.998406	413727.901747	51.676839
3362.602581	413437.572478	51.681844
3361.601244	413146.472186	51.686849
3361.206916	412850.724820	51.691853
3360.531792	412582.308390	51.696858
3359.531074	412288.404507	51.701863
3359.058435	412000.105974	51.706868
3358.034197	411709.630375	51.711873
3357.903262	411418.629525	51.716877
3357.012455	411140.857781	51.721882
3356.220534	410847.236957	51.726887
3355.785194	410568.803423	51.731892
3354.714216	410287.901288	51.736897
3354.414324	409996.354269	51.741901
3353.092031	409717.112869	51.746906
3352.688152	409441.586257	51.751911
3352.282923	409147.887683	51.756916
3351.638288	408872.546432	51.761921
3350.869392	408580.754972	51.766925
3349.928663	408312.367692	51.771930
3349.232695	408028.259488	51.776935
3348.745740	407754.153840	51.781940
3347.901021	407474.282615	51.786945
3347.325842	407194.849074	51.791949
3346.406089	406926.954600	51.796954
3345.685005	406640.499424	51.801959
3345.239723	406374.049967	51.806964
3344.241887	406100.645734	51.811969
3343.951070	405818.791203	51.816973
3343.189484	405547.606661	51.821978
3342.403633	405267.070751	51.826983
3342.029788	404992.871886	51.831988
3341.014053	404716.306792	51.836993
3340.466655	404442.232210	51.841997
3339.451891	404183.173881	51.847002
3339.018741	403905.340366	51.852007
3338.140782	403638.046407	51.857012
3337.270171	403366.580656	51.862017
3337.204454	403092.469002	51.867021
3336.244181	402832.399709	51.872026
3335.489285	402554.325627	51.877031
3334.974531	402292.758089	51.882036
3334.369325	402020.400086	51.887041
3333.984620	401747.547369	51.892045
3332.915918	401475.537629	51.897050
3332.629721	401208.231374	51.902055
3331.685020	400929.054779	51.907060
3330.878829	400667.469247	51.912065
3330.212530	400384.736096	51.917069
3329.420166	400127.490704	51.922074
3328.715472	399851.139254	51.927079
3327.980220	399589.508393	51.932084
3327.217154	399331.489480	51.937089
3326.610873	399060.835285	51.942093
3325.716472	398804.714089	51.947098
3325.370495	398534.522795	51.952103
3324.922193	398275.962807	51.957108
3324.018729	398017.803247	51.962113
3323.483221	397745.449249	51.967117
3322.627604	397476.092527	51.972122
3321.980168	397221.089374	51.977127
3321.735403	396952.979158	51.982132
3320.430664	396698.914877	51.987137
3319.957846	396431.421244	51.992141
3319.198260	396173.275455	51.997146
3318.708519	395910.585191	52.002151
3318.047696	395650.004606	52.007156
3317.253589	395391.121008	52.012161
3316.663871	395124.525273	52.017165
3315.960967	394863.919854	52.022170
3315.196889	394608.203451	52.027175
3314.768572	394341.550614	52.032180
3313.578813	394082.694175	52.037185
3313.094611	393817.342703	52.042189
3312.486232	393562.636230	52.047194
3312.006384	393303.331105	52.052199
3311.231812	393037.027958	52.057204
3310.284762	392783.182863	52.062209
3309.640244	392525.143748	52.067213
3308.931972	392275.274342	52.072218
3308.120518	392013.723688	52.077223
3307.578073	391762.756493	52.082228
3306.919008	391515.416416	52.087233
3306.531625	391256.284749	52.092237
3305.661545	391009.686396	52.097242
3304.900867	390753.356085	52.102247
3304.375559	390494.138891	52.107252
3303.433439	390247.444874	52.112257
3302.936267	389994.245719	52.117261
3302.265257	389741.046818	52.122266
3301.371154	389486.686303	52.127271
3300.960717	389237.256707	52.132276
3299.999714	388976.266520	52.137281
3299.513816	388724.963619	52.142285
3298.581865	388486.926694	52.147290
3297.894672	388239.975004	52.152295
3297.397212	387992.940752	52.157300
3296.638982	387747.522622	52.162305
3295.952054	387497.031211	52.167309
3295.104692	387257.828481	52.172314
3294.512778	387011.819615	52.177319
3293.875418	386767.723470	52.182324
3293.023579	386523.329025	52.187329
3292.723819	386270.479264	52.192333
3291.873423	386038.440166	52.197338
3291.172084	385786.464328	52.202343
3290.818848	385543.281410	52.207348
3290.163228	385302.255429	52.212353
3289.308446	385052.892731	52.217357
3288.382190	384810.151634	52.222362
3287.646179	384562.114669	52.227367
3287.459901	384317.981773	52.232372
3286.784458	384082.393228	52.237377
3286.187874	383839.746239	52.242381
3285.269727	383591.706188	52.247386
3284.516168	383347.554942	52.252391
3283.960115	383106.041216	52.257396
3283.031536	382869.416940	52.262401
3282.482378	382624.414849	52.267405
3281.796218	382377.957764	52.272410
3281.177200	382145.349168	52.277415
3280.586561	381902.587030	52.282420
3279.353276	381666.664682	52.287425
3278.785780	381430.533838	52.292429
3278.228002	381188.524946	52.297434
3277.447381	380950.720831	52.302439
3277.238519	380714.325385	52.307444
3276.019277	380486.862884	52.312449
3275.772654	380250.852071	52.317453
3275.014193	380006.654752	52.322458
3274.383646	379771.998871	52.327463
3273.642869	379531.966952	52.332468
3272.891094	379299.133221	52.337473
3272.411836	379061.346134	52.342477
3271.580215	378826.996145	52.347482
3270.545244	378599.544322	52.352487
3270.366191	378355.270455	52.357492
3269.608183	378128.128188	52.362497
3269.051886	377886.480033	52.367501
3268.383201	377649.045025	52.372506
3267.594988	377417.172460	52.377511
3266.935838	377182.353017	52.382516
3265.859366	376948.386709	52.387521
3265.677629	376711.988267	52.392525
3264.795086	376488.569984	52.397530
3264.236545	376252.889772	52.402535
3263.727654	376017.759927	52.407540
3262.887737	375788.506055	52.412545
3262.269370	375550.033164	52.417549
3261.443608	375323.343530	52.422554
3261.002007	375098.677703	52.427559
3260.299577	374853.727565	52.432564
3259.650550	374627.006093	52.437569
3259.158366	374387.438056	52.442573
3258.201242	374161.551298	52.447578
3257.404787	373921.443599	52.452583
3256.810802	373682.701560	52.457588
3256.360228	373457.773771	52.462593
3255.506716	373230.262917	52.467597
3254.809385	372995.323548	52.472602
3254.268699	372763.614201	52.477607
3253.728997	372536.100784	52.482612
3252.641009	372307.782494	52.487617
3252.038696	372067.811428	52.492621
3251.425902	371848.776994	52.497626
3250.629759	371615.219202	52.502631
3250.291810	371387.006218	52.507636
3249.410709	371164.118445	52.512641
3248.782863	370928.138921	52.517645
3248.228336	370709.241998	52.522650
3247.272373	370483.004442	52.527655
3246.573300	370249.525526	52.532660
3245.723932	370027.847899	52.537665
3245.330624	369804.621449	52.542669
3244.878720	369582.420724	52.547674
3243.634608	369356.553520	52.552679
3243.238572	369131.161562	52.557684
3242.600516	368909.444748	52.562689
3241.752143	368682.519234	52.567693
3241.148506	368456.647788	52.572698
3240.630299	368238.343136	52.577703
3240.276003	368016.017176	52.582708
3239.270413	367803.206448	52.587713
3238.771614	367565.610744	52.592717
3238.036161	367337.464629	52.597722
3237.338315	367123.686031	52.602727
3236.804982	366894.869610	52.607732
3235.709196	366672.934020	52.612737
3235.129201	366440.967818	52.617741
3234.628597	366233.285306	52.622746
3233.989852	366001.962171	52.627751
3233.564805	365782.078656	52.632756
3232.430512	365557.930102	52.637761
3231.915524	365326.609350	52.642765
3231.332711	365110.309507	52.647770
3230.199005	364887.200686	52.652775
3229.684169	364658.191811	52.657780
3229.182861	364447.829630	52.662785
3228.312791	364227.423747	52.667789
3227.681605	364016.902017	52.672794
3227.149388	363797.203923	52.677799
3226.586850	363572.319026	52.682804
3225.519034	363361.812469	52.687809
3224.972719	363134.454801	52.692813
3224.552127	362913.564402	52.697818
3223.499474	362707.886866	52.702823
3223.115604	362490.703515	52.707828
3222.689562	362285.026764	52.712833
3221.991958	362049.570899	52.717837
3220.968214	361834.215951	52.722842
3220.285979	361613.996900	52.727847
3219.726308	361401.238271	52.732852
3218.536648	361191.122853	52.737857
3218.176643	360972.529211	52.742861
3217.614751	360763.152280	52.747866
3217.083440	360551.632166	52.752871
3216.466849	360334.246667	52.757876
3215.755159	360122.091595	52.762881
3215.141413	359904.194774	52.767885
3214.277979	359694.733626	52.772890
3213.405824	359468.198635	52.777895
3213.132086	359259.685598	52.782900
3212.138465	359046.781547	52.787905
3211.809597	358826.493730	52.792909
3211.184372	358616.557636	52.797914
3210.237557	358405.348285	52.802919
3209.579537	358187.679757	52.807924
3208.958107	357981.481002	52.812929
3208.321756	357761.287914	52.817933
3207.236134	357553.404954	52.822938
3206.556837	357342.123259	52.827943
3206.296058	357143.040045	52.832948
3205.266931	356935.425469	52.837953
3204.655905	356721.076641	52.842957
3204.261521	356512.367434	52.847962
3203.431473	356306.729105	52.852967
3202.622416	356097.065857	52.857972
3202.034464	355890.064234	52.862977
3201.406806	355680.116070	52.867981
3200.683369	355482.753560	52.872986
3199.802886	355278.467759	52.877991
3199.485602	355065.312364	52.882996
3198.691927	354861.418326	52.888001
3197.729415	354656.481343	52.893005
3197.396285	354450.934998	52.898010
3196.388949	354251.449493	52.903015
3195.970847	354045.278748	52.908020
3194.806602	353846.885348	52.913025
3194.550847	353645.293578	52.918029
3194.203851	353449.416065	52.923034
3193.270191	353253.834216	52.928039
3192.678339	353036.412931	52.933044
3191.701504	352834.321307	52.938049
3191.119300	352634.482379	52.943053
3190.637504	352438.393350	52.948058
3189.917909	352238.472852	52.953063
3189.443925	352028.663659	52.958068
3188.746769	351831.359401	52.963073
3188.215071	351625.069827	52.968077
3187.713614	351416.509608	52.973082
3186.505387	351212.310572	52.978087
3186.188926	351005.551895	52.983092
3185.348089	350810.786169	52.988097
3184.576769	350604.097906	52.993101
3184.337861	350394.066942	52.998106
3183.330993	350189.628557	53.003111
3182.773983	349983.871141	53.008116
3182.106634	349783.118776	53.013121
3181.295951	349576.789131	53.018125
3180.838283	349383.968282	53.023130
3180.134127	349177.162157	53.028135
3179.594504	348964.017307	53.033140
3178.627426	348761.196159	53.038145
3177.970970	348557.230711	53.043149
3177.543259	348361.321914	53.048154
3176.605940	348161.395337	53.053159
3176.024562	347949.703931	53.058164
3175.108367	347755.651906	53.063169
3174.840712	347553.250184	53.068173
3174.324632	347348.647259	53.073178
3173.030162	347152.285957	53.078183
3172.802776	346945.039779	53.083188
3172.116004	346747.308318	53.088193
3171.358238	346548.620209	53.093197
3170.722262	346349.657614	53.098202
3169.789693	346151.453921	53.103207
3169.364442	345951.871194	53.108212
3168.609177	345747.529420	53.113217
3167.865886	345550.922681	53.118221
3167.194373	345356.620130	53.123226
3166.302755	345154.461325	53.128231
3166.194966	344951.541478	53.133236
3165.307111	344763.252640	53.138241
3164.784330	344563.196946	53.143245
3163.907586	344371.341634	53.148250
3163.322163	344164.625718	53.153255
3162.854607	343960.410325	53.158260
3162.098134	343769.323082	53.163265
3161.302933	343566.889012	53.168269
3160.698077	343358.722494	53.173274
3159.710923	343169.527942	53.178279
3159.506381	342975.678171	53.183284
3158.469784	342785.701156	53.188289
3158.255649	342577.368286	53.193293
3157.349695	342381.896696	53.198298
3156.955914	342178.248985	53.203303
3156.294681	341970.366575	53.208308
3155.543149	341774.384961	53.213313
3155.007130	341568.594086	53.218317
3154.283821	341367.719434	53.223322
3153.134128	341176.304364	53.228327
3152.600224	340973.005715	53.233332
3151.993774	340776.794322	53.238337
3151.303428	340582.784704	53.243341
3150.588806	340390.865632	53.248346
3149.982478	340195.746948	53.253351
3149.351259	339993.555059	53.258356
3148.858673	339801.497224	53.263361
3147.944217	339598.203388	53.268365
3147.260983	339394.719580	53.273370
3146.447712	339209.099987	53.278375
3145.887680	339005.697257	53.283380
3144.982197	338819.123802	53.288385
3144.391756	338622.063113	53.293389
3143.693097	338428.735486	53.298394
3142.929205	338249.087397	53.303399
3142.552224	338046.569069	53.308404
3141.790717	337856.380748	53.313409
3140.883965	337659.163511	53.318413
3140.566518	337477.482523	53.323418
3139.789813	337293.939019	53.328423
3139.558611	337107.126651	53.333428
3138.637915	336905.199925	53.338433
3138.001002	336706.689758	53.343437
3137.008300	336513.581161	53.348442
3136.540065	336326.982281	53.353447
3136.151101	336119.317653	53.358452
3135.096841	335934.974215	53.363457
3134.689914	335735.610140	53.368461
3134.438603	335547.116407	53.373466
3133.359570	335358.065774	53.378471
3132.758416	335159.672631	53.383476
3131.864437	334958.983183	53.388481
3131.142834	334765.215685	53.393485
3130.840724	334576.116313	53.398490
3130.307654	334380.561340	53.403495
3129.549613	334188.401785	53.408500
3128.561020	333992.332262	53.413505
3127.714972	333794.763089	53.418509
3127.267580	333594.940917	53.423514
3126.345114	333414.770316	53.428519
3125.900378	333214.717513	53.433524
3125.009092	333030.213164	53.438529
3124.289364	332848.812508	53.443533
3123.791672	332658.364128	53.448538
3122.823778	332471.375555	53.453543
3122.405598	332280.939036	53.458548
3121.924757	332092.726783	53.463553
3121.256860	331916.712673	53.468557
3120.475892	331720.909457	53.473562
3119.790601	331536.572297	53.478567
3119.177358	331335.166108	53.483572
3118.410737	331157.383669	53.488577
3117.788769	330962.902538	53.493581
3117.061783	330778.060873	53.498586
3116.250924	330598.578339	53.503591
3115.858022	330399.527813	53.508596
3114.914294	330232.158323	53.513601
3114.302247	330044.750740	53.518605
3113.498119	329856.991191	53.523610
3112.761548	329675.992578	53.528615
3112.311558	329494.082569	53.533620
3111.445642	329312.925328	53.538625
3110.634721	329128.551087	53.543629
3110.232400	328943.806228	53.548634
3109.625799	328766.476447	53.553639
3109.177373	328579.064763	53.558644
3108.280940	328395.618804	53.563649
3107.531985	328217.037294	53.568653
3107.309668	328032.032600	53.573658
3106.703307	327837.337188	53.578663
3105.851873	327650.699871	53.583668
3105.035614	327469.428547	53.588673
3104.309909	327288.447988	53.593677
3103.750602	327102.577842	53.598682
3102.782362	326919.521636	53.603687
3102.190512	326738.824143	53.608692
3101.632940	326559.801175	53.613697
3100.663468	326382.421506	53.618701
3100.513594	326196.153449	53.623706
3099.708049	326025.824973	53.628711
3099.526599	325838.211683	53.633716
3098.417988	325654.105434	53.638721
3097.995012	325466.045747	53.643725
3097.283142	325282.461457	53.648730
3096.323678	325097.541062	53.653735
3096.043871	324909.508348	53.658740
3095.635158	324726.969637	53.663745
3094.185020	324552.106220	53.668749
3094.087715	324356.837981	53.673754
3092.780154	324175.967927	53.678759
3092.506916	323991.241978	53.683764
3092.146344	323810.195810	53.688769
3091.315470	323629.147290	53.693773
3090.788362	323433.690286	53.698778
3089.826326	323254.011146	53.703783
3089.461960	323063.594287	53.708788
3088.829016	322882.843835	53.713793
3088.021954	322689.084389	53.718797
3087.416087	322500.741387	53.723802
3086.704782	322318.296233	53.728807
3085.829840	322132.821215	53.733812
3085.042216	321949.368900	53.738817
3084.283511	321766.879158	53.743821
3084.168607	321580.646148	53.748826
3083.153955	321403.212081	53.753831
3082.659798	321208.966957	53.758836
3081.662144	321031.020214	53.763841
3081.048183	320851.841153	53.768845
3080.483869	320664.913471	53.773850
3079.768362	320488.270470	53.778855
3079.172536	320296.763863	53.783860
3078.627371	320124.345334	53.788865
3077.865173	319943.431034	53.793869
3077.249408	319755.669356	53.798874
3076.321419	319578.167024	53.803879
3075.970284	319397.415747	53.808884
3075.539118	319212.450043	53.813889
3074.379011	319032.309850	53.818893
3073.997135	318846.444433	53.823898
3073.244790	318655.061002	53.828903
3072.821352	318471.645804	53.833908
3072.152607	318297.995745	53.838913
3071.146049	318116.021644	53.843917
3070.586730	317927.279751	53.848922
3069.976437	317757.769853	53.853927
3069.503652	317572.221855	53.858932
3068.879955	317385.831644	53.863937
3067.886311	317206.400036	53.868941
3067.346471	317020.326864	53.873946
3066.932315	316836.754271	53.878951
3066.165644	316641.931571	53.883956
3065.146835	316471.032674	53.888961
3064.571178	316286.287844	53.893965
3064.004784	316100.751847	53.898970
3062.888635	315926.684525	53.903975
3062.374990	315732.482026	53.908980
3061.873912	315567.789042	53.913985
3061.132496	315385.818800	53.918989
3060.679706	315206.603517	53.923994
3060.060898	315029.273016	53.928999
3059.307164	314833.833614	53.934004
3058.829967	314661.980159	53.939009
3057.688184	314482.694397	53.944013
3057.222718	314296.859016	53.949018
3056.356967	314116.714102	53.954023
3055.824803	313939.902746	53.959028
3055.429257	313759.097137	53.964033
3054.546805	313584.734202	53.969037
3054.282183	313402.888713	53.974042
3053.355989	313229.881694	53.979047
3052.669265	313039.521083	53.984052
3051.973704	312860.034613	53.989057
3051.325833	312685.836793	53.994061
3050.553144	312504.706781	53.999066
3049.968610	312325.965771	54.004071
3049.206700	312147.430788	54.009076
3048.673139	311963.333666	54.014081
3047.946195	311789.197856	54.019085
3047.325102	311614.179237	54.024090
3046.476782	311427.279049	54.029095
3045.972085	311244.856805	54.034100
3045.645292	311068.364755	54.039105
3044.465394	310894.070056	54.044109
3043.951979	310715.417058	54.049114
3043.057812	310539.395945	54.054119
3042.730853	310361.909713	54.059124
3042.133451	310177.514199	54.064129
3041.115996	310005.509708	54.069133
3040.637683	309829.167051	54.074138
3039.861519	309649.000646	54.079143
3039.249567	309467.763924	54.084148
3038.308795	309293.072462	54.089153
3037.563426	309129.936269	54.094157
3036.934322	308941.927840	54.099162
3036.325280	308773.956744	54.104167
3035.887912	308600.534233	54.109172
3035.210683	308421.165189	54.114177
3034.228734	308249.661836	54.119181
3033.767773	308069.137591	54.124186
3033.190054	307906.049610	54.129191
3032.641533	307727.092085	54.134196
3032.257610	307557.810439	54.139201
3031.461401	307385.410679	54.144205
3030.648155	307197.861628	54.149210
3029.835220	307027.501236	54.154215
3029.056320	306847.178335	54.159220
3028.556251	306670.478044	54.164225
3027.829580	306492.973020	54.169229
3027.878629	306320.056060	54.174234
3026.416353	306154.100916	54.179239
3026.074834	305965.354929	54.184244
3025.373996	305794.745981	54.189249
3024.565515	305628.406577	54.194253
3024.057630	305441.519684	54.199258
3023.318854	305267.274499	54.204263
3022.739189	305095.244874	54.209268
3022.176634	304918.093741	54.214273
3021.439622	304738.041444	54.219277
3021.070792	304552.888440	54.224282
3020.098698	304381.760391	54.229287
3019.513201	304200.944906	54.234292
3018.977847	304014.747979	54.239297
3017.868194	303845.347247	54.244301
3017.348775	303658.969066	54.249306
3016.798595	303489.581222	54.254311
3016.017918	303317.759469	54.259316
3015.512711	303142.634276	54.264321
3014.881565	302959.175979	54.269325
3014.121912	302778.207989	54.274330
3013.402238	302611.672663	54.279335
3013.019438	302432.605481	54.284340
3012.497443	302254.578756	54.289345
3011.461390	302076.480385	54.294349
3010.974169	301892.412263	54.299354
3010.138226	301713.008484	54.304359
3009.441507	301538.828489	54.309364
3008.856982	301363.560958	54.314369
3008.083101	301194.129497	54.319373
3007.776461	301000.532819	54.324378
3006.617574	300829.633925	54.329383
3006.147463	300658.116500	54.334388
3005.353658	300472.898299	54.339393
3004.693499	300305.128660	54.344397
3004.522586	300134.658370	54.349402
3003.540167	299956.065222	54.354407
3002.965302	299771.881151	54.359412
3002.189483	299604.816689	54.364417
3001.333135	299431.219913	54.369421
3001.017030	299245.695506	54.374426
3000.113174	299081.706769	54.379431
2999.507584	298901.881379	54.384436
2999.281989	298729.839370	54.389441
2998.339101	298550.652730	54.394445
2998.110103	298365.495574	54.399450
2997.116980	298186.189175	54.404455
2996.248024	297995.835849	54.409460
2995.689598	297829.652042	54.414465
2994.626916	297653.055586	54.419469
2994.305012	297467.530192	54.424474
2993.724031	297304.660152	54.429479
2992.738413	297118.449985	54.434484
2992.315964	296947.277809	54.439489
2991.324629	296774.158169	54.444493
2990.938574	296597.631862	54.449498
2990.268922	296417.279304	54.454503
2989.768536	296239.446479	54.459508
2989.014901	296060.329290	54.464513
2988.141793	295892.741935	54.469517
2987.777306	295702.459201	54.474522
2986.959900	295540.592809	54.479527
2986.315439	295353.613838	54.484532
2985.792873	295179.170678	54.489537
2984.978501	295006.428920	54.494541
2984.209871	294833.068563	54.499546
2983.532130	294659.362598	54.504551
2982.827148	294480.312690	54.509556
2982.378780	294305.627837	54.514561
2981.521347	294135.158747	54.519565
2981.507831	293959.411553	54.524570
2980.389182	293783.380733	54.529575
2979.560888	293599.026940	54.534580
2979.214167	293420.938124	54.539585
2978.419330	293249.541604	54.544589
2977.778385	293081.253077	54.549594
2977.360577	292899.991677	54.554599
2976.695374	292709.244486	54.559604
2975.977946	292534.626277	54.564609
2975.125903	292356.693011	54.569613
2974.555642	292173.952592	54.574618
2973.745390	291996.980202	54.579623
2973.155437	291824.556957	54.584628
2972.331812	291643.919104	54.589633
2971.575412	291460.978398	54.594637
2971.046793	291297.076694	54.599642
2970.485283	291126.940535	54.604647
2970.004977	290945.916748	54.609652
2969.515312	290759.546118	54.614657
2968.851052	290581.301693	54.619661
2968.500243	290386.784643	54.624666
2967.652845	290206.939024	54.629671
2966.696145	290028.282099	54.634676
2966.344909	289841.354084	54.639681
2965.383619	289654.547978	54.644685
2964.817081	289477.586203	54.649690
2964.232244	289301.263905	54.654695
2963.244666	289110.845178	54.659700
2962.819838	288931.492128	54.664705
2961.925876	288754.225185	54.669709
2961.393626	288566.917498	54.674714
2960.765837	288387.035952	54.679719
2959.934651	288206.651672	54.684724
2959.716326	288023.750825	54.689729
2958.840947	287849.230937	54.694733
2958.288819	287657.418028	54.699738
2957.663822	287485.303221	54.704743
2956.897972	287293.523927	54.709748
2956.648962	287106.730822	54.714753
2955.378352	286928.223603	54.719757
2955.044552	286739.508153	54.724762
2954.534898	286546.363544	54.729767
2953.305108	286372.815829	54.734772
2952.953492	286180.868464	54.739777
2951.699249	286005.337938	54.744781
2951.321694	285808.606499	54.749786
2950.657910	285642.405497	54.754791
2950.377460	285468.630667	54.759796
2949.707082	285287.862836	54.764801
2948.886272	285110.149435	54.769805
2948.310329	284918.593495	54.774810
2947.486616	284736.474411	54.779815
2946.743591	284556.201645	54.784820
2946.341380	284372.920550	54.789825
2945.276791	284191.705278	54.794829
2944.935439	284003.779195	54.799834
2944.337324	283834.510889	54.804839
2943.855418	283640.978446	54.809844
2942.997060	283452.191658	54.814849
2942.157049	283280.338224	54.819853
2941.815398	283091.622306	54.824858
2941.178421	282912.605511	54.829863
2940.589668	282725.405728	54.834868
2939.859364	282544.824551	54.839873
2939.019506	282357.027683	54.844877
2938.630299	282166.688992	54.849882
2937.871062	281985.246291	54.854887
2937.001974	281796.409664	54.859892
2936.621173	281608.463471	54.864897
2935.706910	281426.994204	54.869901
2935.006983	281230.668423	54.874906
2934.230526	281051.418439	54.879911
2933.601910	280876.805696	54.884916
2933.238418	280684.068455	54.889921
2932.548417	280497.291494	54.894925
2931.833740	280310.747607	54.899930
2931.029550	280136.391693	54.904935
2930.162622	279950.661338	54.909940
2929.934358	279766.561677	54.914945
2928.809325	279587.723077	54.919949
2928.309464	279396.942697	54.924954
2927.706013	279219.524081	54.929959
2926.933385	279042.106747	54.934964
2926.241712	278852.884722	54.939969
2925.505770	278680.988145	54.944973
2924.984554	278492.987019	54.949978
2924.234496	278312.891811	54.954983
2923.802642	278139.393441	54.959988
2923.536108	277949.696465	54.964993
2922.684342	277779.499006	54.969997
2922.267559	277573.729758	54.975002
2921.239142	277390.316668	54.980007
2920.209291	277204.051328	54.985012
2919.923143	277012.600021	54.990017
2918.846448	276826.163779	54.995021
2918.291621	276643.796247	55.000026
2917.238496	276458.196699	55.005031
2916.839550	276284.005281	55.010036
2916.266048	276096.572457	55.015041
2915.587401	275931.797666	55.020045
2915.111721	275749.188331	55.025050
2914.294655	275562.405284	55.030055
2913.476245	275382.702656	55.035060
2913.165444	275202.817786	55.040065
2912.458196	275022.842868	55.045069
2912.013348	274834.472774	55.050074
2911.071960	274655.986623	55.055079
2910.159094	274475.229270	55.060084
2909.924360	274292.199747	55.065089
2908.900400	274123.608412	55.070093
2908.479558	273924.079379	55.075098
2907.742905	273747.139877	55.080103
2907.263848	273572.222540	55.085108
2906.934130	273376.321089	55.090113
2905.874698	273210.511467	55.095117
2905.294153	273007.391265	55.100122
2904.441537	272835.538389	55.105127
2903.961406	272650.306595	55.110132
2903.349148	272461.250013	55.115137
2902.333792	272283.488822	55.120141
2902.621030	272096.734835	55.125146
2901.730760	271904.513321	55.130151
2900.925941	271711.285039	55.135156
2900.683459	271524.920616	55.140161
2899.618784	271338.177026	55.145165
2899.238670	271139.966201	55.150170
2898.270555	270952.392401	55.155175
2897.223842	270763.022827	55.160180
2896.911887	270564.190080	55.165185
2896.185659	270388.573675	55.170189
2895.473346	270204.474149	55.175194
2894.664579	270011.628830	55.180199
2894.133378	269825.768865	55.185204
2893.663735	269636.053482	55.190209
2893.056834	269463.525510	55.195213
2892.463621	269258.930828	55.200218
2891.851080	269065.367032	55.205223
2891.010773	268881.313551	55.210228
2890.545380	268680.773724	55.215233
2889.501419	268508.748145	55.220237
2888.848163	268320.233727	55.225242
2888.178913	268118.809494	55.230247
2887.343766	267942.090321	55.235252
2887.090972	267748.113408	55.240257
2886.109062	267569.634809	55.245261
2885.737935	267370.481242	55.250266
2884.868745	267182.408872	55.255271
2884.062123	266997.764869	55.260276
2883.283296	266802.496296	55.265281
2882.475609	266623.888557	55.270285
2882.033810	266448.100855	55.275290
2881.445936	266262.582038	55.280295
2880.668409	266076.074596	55.285300
2880.317159	265880.203864	55.290305
2879.468722	265707.969957	55.295309
2879.337239	265510.281820	55.300314
2878.561004	265317.432926	55.305319
2877.665892	265133.465838	55.310324
2877.232575	264941.708884	55.315329
2876.436985	264756.172653	55.320333
2875.929718	264565.038818	55.325338
2874.767982	264367.055922	55.330343
2874.382705	264181.225781	55.335348
2873.822606	263990.202466	55.340353
2873.027588	263806.984186	55.345357
2872.436494	263611.942026	55.350362
2871.712496	263419.340473	55.355367
2870.819923	263229.720000	55.360372
2870.394214	263044.737279	55.365377
2869.406673	262858.009925	55.370381
2869.093604	262678.637982	55.375386
2868.269942	262491.655671	55.380391
2867.803281	262310.194409	55.385396
2867.151102	262108.286442	55.390401
2866.544360	261927.560676	55.395405
2865.956986	261737.638050	55.400410
2865.200623	261542.521391	55.405415
2864.483662	261361.991680	55.410420
2863.886973	261159.133233	55.415425
2863.165966	260974.045659	55.420429
2862.574982	260787.103933	55.425434
2861.944540	260596.373880	55.430439
2861.094036	260409.855508	55.435444
2860.672242	260215.858269	55.440449
2859.735742	260031.238376	55.445453
2859.527169	259839.627071	55.450458
2858.752764	259644.845633	55.455463
2857.968863	259444.946841	55.460468
2857.326341	259248.642219	55.465473
2856.502727	259057.943825	55.470477
2855.878576	258872.842328	55.475482
2855.159120	258687.374042	55.480487
2854.768303	258488.024970	55.485492
2854.248426	258303.569535	55.490497
2853.179515	258106.900363	55.495501
2852.535458	257917.371378	55.500506
2851.905069	257727.280094	55.505511
2851.477424	257538.430230	55.510516
2850.751462	257335.798936	55.515521
2849.640376	257153.984745	55.520525
2849.146932	256958.473307	55.525530
2848.659145	256777.681282	55.530535
2847.881919	256587.919791	55.535540
2847.309208	256395.452006	55.540545
2846.773950	256201.628691	55.545549
2846.007251	256010.414392	55.550554
2845.569735	255818.307716	55.555559
2844.826626	255633.533233	55.560564
2844.063218	255428.541154	55.565569
2843.507884	255243.762745	55.570573
2842.535661	255054.950300	55.575578
2842.101510	254865.950956	55.580583
2841.193953	254671.067442	55.585588
2840.796335	254475.186553	55.590593
2839.536565	254282.778563	55.595597
2839.030904	254098.298935	55.600602
2838.761191	253911.923024	55.605607
2838.108127	253720.438194	55.610612
2837.350199	253524.207834	55.615617
2836.711015	253341.914761	55.620621
2836.391252	253143.272450	55.625626
2835.480574	252951.931052	55.630631
2834.681685	252766.811533	55.635636
2834.172732	252574.770239	55.640641
2833.341002	252385.301473	55.645645
2832.561523	252195.340762	55.650650
2832.081649	252004.568806	55.655655
2831.359124	251814.548545	55.660660
2830.729222	251615.727806	55.665665
2829.751624	251437.743165	55.670669
2829.309602	251237.466969	55.675674
2828.853482	251056.038542	55.680679
2827.989121	250871.389763	55.685684
2827.566587	250672.435403	55.690689
2826.855021	250482.847803	55.695693
2826.247825	250294.975612	55.700698
2825.685781	250097.852149	55.705703
2824.736179	249914.644045	55.710708
2824.128888	249716.866077	55.715713
2823.384943	249531.690388	55.720717
2822.560449	249342.707713	55.725722
2822.200947	249145.196802	55.730727
2821.424424	248963.464885	55.735732
2821.339227	248763.160652	55.740737
2820.265864	248579.999142	55.745741
2819.852944	248386.037452	55.750746
2819.057136	248197.051612	55.755751
2818.578865	247995.766504	55.760756
2817.789185	247797.510511	55.765761
2817.141011	247601.957241	55.770765
2816.687474	247395.932325	55.775770
2815.818312	247203.597827	55.780775
2815.094646	247013.583410	55.785780
2814.579847	246811.669032	55.790785
2813.720051	246613.349330	55.795789
2813.135763	246417.940311	55.800794
2812.548561	246228.210901	55.805799
2811.492687	246034.405038	55.810804
2811.219674	245842.461794	55.815809
2810.302771	245643.872360	55.820813
2809.509812	245443.124461	55.825818
2808.885524	245254.242606	55.830823
2807.991551	245081.345202	55.835828
2807.589932	244876.003272	55.840833
2806.623250	244690.588806	55.845837
2806.230218	244505.593059	55.850842
2805.567086	244319.596255	55.855847
2804.718865	244128.383138	55.860852
2804.660979	243931.417279	55.865857
2803.590966	243742.786384	55.870861
2802.940775	243541.611258	55.875866
2802.437128	243353.094956	55.880871
2801.536401	243179.182478	55.885876
2801.052364	242979.840876	55.890881
2800.365343	242782.899992	55.895885
2799.931484	242583.041758	55.900890
2799.187535	242397.493409	55.905895
2798.315396	242205.472042	55.910900
2797.932883	242008.993443	55.915905
2797.116991	241820.477935	55.920909
2796.305946	241613.932760	55.925914
2795.703936	241432.310442	55.930919
2794.913909	241249.928758	55.935924
2794.292260	241048.371125	55.940929
2794.181598	240855.263610	55.945933
2793.421451	240653.422994	55.950938
2792.923845	240467.151008	55.955943
2792.008815	240272.873120	55.960948
2791.389950	240072.157028	55.965953
2790.575381	239875.419283	55.970957
2789.776991	239673.051644	55.975962
2789.455489	239478.553755	55.980967
2788.418211	239282.692614	55.985972
2787.908628	239088.810852	55.990977
2787.027883	238903.671551	55.995981
2786.602271	238697.070438	56.000986
2786.272256	238513.601592	56.005991
2785.067349	238327.674251	56.010996
2784.669510	238115.493142	56.016001
2783.715084	237931.309287	56.021005
2783.018058	237735.855304	56.026010
2782.699098	237535.656406	56.031015
2782.070936	237351.625563	56.036020
2781.460786	237145.973270	56.041025
2780.991808	236954.787978	56.046029
2780.335176	236751.002665	56.051034
2779.652904	236553.358581	56.056039
2778.876085	236354.914996	56.061044
2778.441185	236153.005492	56.066049
2777.595870	235957.705539	56.071053
2776.613036	235756.265531	56.076058
2776.078125	235558.701826	56.081063
2775.541859	235366.969861	56.086068
2775.264588	235169.697119	56.091073
2774.157750	234960.537397	56.096077
2773.317567	234771.350092	56.101082
2773.020029	234562.648668	56.106087
2772.157310	234378.685648	56.111092
2771.844699	234169.554546	56.116097
2771.119408	233976.785678	56.121101
2770.281352	233764.912226	56.126106
2769.634464	233559.043700	56.131111
2768.730339	233374.325196	56.136116
2768.223807	233160.872749	56.141121
2767.373219	232969.908098	56.146125
2766.938439	232762.861814	56.151130
2766.185283	232569.590859	56.156135
2765.550963	232379.942646	56.161140
2764.806304	232173.812438	56.166145
2763.919509	231979.876342	56.171149
2763.344014	231785.407546	56.176154
2762.930620	231593.790745	56.181159
2761.746072	231400.030306	56.186164
2761.242417	231215.608999	56.191169
2760.812288	231022.315491	56.196173
2760.073786	230822.629248	56.201178
2759.459720	230631.911920	56.206183
2758.677691	230439.693853	56.211188
2758.323863	230235.848532	56.216193
2757.709621	230039.123383	56.221197
2756.986963	229841.881128	56.226202
2756.308757	229641.449507	56.231207
2755.433763	229458.669185	56.236212
2754.931346	229253.551043	56.241217
2754.489303	229053.821723	56.246221
2753.565498	228858.854126	56.251226
2753.040143	228663.976619	56.256231
2752.004901	228478.117356	56.261236
2751.654160	228269.005440	56.266241
2751.146278	228074.712088	56.271245
2750.358545	227876.135034	56.276250
2749.860634	227664.858185	56.281255
2749.122839	227479.310398	56.286260
2748.398890	227271.533063	56.291265
2748.096036	227081.079590	56.296269
2747.109841	226878.207852	56.301274
2746.622872	226671.132818	56.306279
2745.666540	226475.233672	56.311284
2745.145204	226272.442522	56.316289
2744.586400	226072.967724	56.321293
2743.610892	225877.849568	56.326298
2743.237705	225673.865201	56.331303
2742.503056	225481.103147	56.336308
2741.463633	225277.199821	56.341313
2741.159536	225075.459261	56.346317
2740.492255	224890.071516	56.351322
2740.042165	224684.395917	56.356327
2738.915580	224489.330443	56.361332
2738.612228	224281.443020	56.366337
2737.680478	224082.363110	56.371341
2736.957437	223886.535014	56.376346
2736.530919	223688.559959	56.381351
2735.665254	223497.541932	56.386356
2735.225486	223291.982829	56.391361
2734.437911	223102.773782	56.396365
2733.739192	222897.167612	56.401370
2733.219491	222695.136203	56.406375
2732.604336	222512.597225	56.411380
2732.053575	222299.153013	56.416385
2731.273112	222100.461491	56.421389
2730.350835	221892.780223	56.426394
2729.905237	221695.462443	56.431399
2729.324030	221501.132683	56.436404
2728.892392	221295.246591	56.441409
2728.203285	221097.141491	56.446413
2727.374146	220893.012500	56.451418
2726.876855	220681.601067	56.456423
2725.899050	220495.229071	56.461428
2725.424403	220285.991924	56.466433
2724.795714	220078.752838	56.471437
2724.089356	219879.788070	56.476442
2723.085367	219674.646275	56.481447
2722.428077	219489.384407	56.486452
2722.055768	219280.426658	56.491457
2721.253711	219084.381492	56.496461
2720.498111	218893.408490	56.501466
2720.013117	218685.424987	56.506471
2719.118773	218497.186340	56.511476
2718.658040	218285.152240	56.516481
2718.087140	218087.876600	56.521485
2717.211832	217889.682306	56.526490
2716.848396	217686.175815	56.531495
2716.046288	217497.810611	56.536500
2715.442678	217296.672697	56.541505
2714.541500	217094.322317	56.546509
2714.054445	216895.165534	56.551514
2713.537380	216699.985493	56.556519
2712.363298	216498.061924	56.561524
2711.915226	216287.011906	56.566529
2711.575644	216080.718647	56.571533
2710.990714	215887.155459	56.576538
2710.109535	215686.626201	56.581543
2709.074806	215488.642133	56.586548
2709.007467	215298.040769	56.591553
2708.225685	215094.684457	56.596557
2707.660864	214880.742375	56.601562
2706.777135	214680.343753	56.606567
2705.960915	214477.007470	56.611572
2705.248055	214272.993544	56.616577
2704.738823	214071.671867	56.621581
2704.107045	213873.705047	56.626586
2703.434518	213677.756350	56.631591
2702.538659	213481.958161	56.636596
2701.709456	213273.192590	56.641601
2701.328258	213078.459610	56.646605
2700.458568	212881.386225	56.651610
2700.141053	212683.844115	56.656615
2699.346433	212491.864005	56.661620
2698.552375	212291.496551	56.666625
2698.102774	212086.633053	56.671629
2697.284041	211891.603795	56.676634
2696.948216	211693.533006	56.681639
2696.041477	211498.582514	56.686644
2695.453365	211293.628916	56.691649
2694.928968	211099.013633	56.696653
2694.100880	210895.563027	56.701658
2693.514115	210693.614904	56.706663
2692.683449	210500.373653	56.711668
2692.312389	210298.507165	56.716673
2691.601579	210097.815176	56.721677
2690.796443	209895.458723	56.726682
2690.171732	209695.085298	56.731687
2689.377641	209502.414055	56.736692
2689.164942	209304.534849	56.741697
2688.385271	209103.856954	56.746701
2687.459596	208896.215483	56.751706
2686.971748	208688.403531	56.756711
2686.453087	208493.337225	56.761716
2685.535380	208295.649292	56.766721
2685.310783	208094.441293	56.771725
2684.282282	207894.914027	56.776730
2683.790535	207683.606115	56.781735
2682.823476	207486.552254	56.786740
2682.472876	207285.175984	56.791745
2681.989386	207083.999615	56.796749
2681.051958	206879.790443	56.801754
2680.593639	206660.602801	56.806759
2679.785092	206466.683452	56.811764
2679.131510	206257.353400	56.816769
2678.319094	206053.598141	56.821773
2677.696820	205851.531576	56.826778
2677.059223	205646.286445	56.831783
2676.512817	205451.221662	56.836788
2675.982593	205242.957427	56.841793
2675.518886	205030.712693	56.846797
2674.642468	204827.175445	56.851802
2673.909541	204614.287641	56.856807
2673.219368	204413.942142	56.861812
2672.614696	204212.909289	56.866817
2672.119052	204009.480030	56.871821
2671.001044	203799.303319	56.876826
2670.755034	203596.663185	56.881831
2669.867152	203401.124888	56.886836
2669.393299	203188.583099	56.891841
2668.744840	202977.876878	56.896845
2667.382267	202778.788970	56.901850
2667.252649	202576.426726	56.906855
2666.435091	202388.770933	56.911860
2666.040610	202172.898891	56.916865
2665.249574	201965.184189	56.921869
2664.531229	201752.928331	56.926874
2663.618094	201563.674257	56.931879
2662.834934	201359.765583	56.936884
2662.279506	201159.003014	56.941889
2662.069603	200950.716453	56.946893
2661.145931	200750.433654	56.951898
2660.568578	200547.080753	56.956903
2659.717503	200352.463519	56.961908
2658.981204	200153.642104	56.966913
2658.194857	199948.326632	56.971917
2657.937441	199754.228301	56.976922
2657.245382	199543.071183	56.981927
2656.665313	199350.781512	56.986932
2655.795454	199143.191762	56.991937
2655.165703	198932.548895	56.996941
2654.258307	198732.830861	57.001946
2653.818475	198534.846462	57.006951
2653.169363	198333.447458	57.011956
2652.408163	198132.830474	57.016961
2651.785270	197935.080905	57.021965
2651.267018	197742.812667	57.026970
2651.011228	197536.226222	57.031975
2649.976067	197326.531956	57.036980
2649.094541	197122.247668	57.041985
2648.661232	196921.328842	57.046989
2647.532998	196723.231243	57.051994
2647.502475	196520.354165	57.056999
2646.690048	196313.835277	57.062004
2645.852071	196112.105685	57.067009
2645.280765	195916.060649	57.072013
2644.654070	195710.939883	57.077018
2644.452549	195499.453998	57.082023
2643.309967	195306.822854	57.087028
2642.791373	195096.915783	57.092033
2642.201406	194888.954966	57.097037
2641.401118	194683.585879	57.102042
2640.922653	194476.359806	57.107047
2640.144031	194273.368358	57.112052
2639.611905	194066.394220	57.117057
2639.043373	193857.403587	57.122061
2637.636097	193654.323371	57.127066
2637.830739	193451.511852	57.132071
2636.728408	193252.036703	57.137076
2635.856398	193047.321836	57.142081
2635.411657	192839.308290	57.147085
2634.835325	192648.455242	57.152090
2634.032979	192440.003804	57.157095
2633.539739	192237.624303	57.162100
2633.115034	192034.458638	57.167105
2632.131484	191825.364159	57.172109
2631.245439	191620.606526	57.177114
2630.766322	191411.930101	57.182119
2629.866382	191212.532908	57.187124
2629.179781	191010.354508	57.192129
2628.851465	190810.715713	57.197133
2627.893058	190610.706815	57.202138
2627.563982	190400.916763	57.207143
2627.117289	190197.176974	57.212148
2626.380212	190000.507139	57.217153
2625.728790	189793.442631	57.222157
2624.500642	189593.773323	57.227162
2624.031572	189386.261829	57.232167
2623.318870	189191.016413	57.237172
2622.630770	188991.175002	57.242177
2622.227644	188788.057724	57.247181
2621.403874	188588.964695	57.252186
2620.709684	188376.378796	57.257191
2620.227875	188180.655671	57.262196
2619.271407	187982.222355	57.267201
2618.886251	187778.915739	57.272205
2618.037162	187576.128795	57.277210
2617.759317	187367.934310	57.282215
2617.323743	187176.317351	57.287220
2616.372489	186960.598056	57.292225
2615.895606	186754.931395	57.297229
2615.018255	186544.113062	57.302234
2614.609909	186336.389154	57.307239
2613.425746	186131.829651	57.312244
2612.959518	185923.862339	57.317249
2612.229615	185723.380012	57.322253
2611.342753	185528.902663	57.327258
2611.065798	185316.251956	57.332263
2610.331662	185119.691237	57.337268
2609.335645	184919.114675	57.342273
2608.847234	184715.888821	57.347277
2607.859889	184509.104592	57.352282
2607.429546	184305.858659	57.357287
2606.851275	184110.015475	57.362292
2606.802074	183903.479741	57.367297
2605.964700	183698.163871	57.372301
2605.172238	183498.311941	57.377306
2604.628474	183280.357490	57.382311
2603.839155	183084.552237	57.387316
2603.172316	182880.332569	57.392321
2602.711865	182667.456330	57.397325
2601.688362	182462.773544	57.402330
2601.327401	182248.675073	57.407335
2600.386108	182050.112620	57.412340
2599.613516	181840.317382	57.417345
2598.851098	181633.332801	57.422349
2597.871228	181432.947484	57.427354
2597.638795	181224.519757	57.432359
2596.944162	181029.179315	57.437364
2596.466087	180831.744728	57.442369
2596.058078	180626.146185	57.447373
2595.195600	180428.214652	57.452378
2594.573925	180204.016733	57.457383
2593.591059	180000.064131	57.462388
2593.356094	179798.003766	57.467393
2592.529009	179594.219209	57.472397
2591.435743	179396.761481	57.477402
2591.058859	179178.584854	57.482407
2590.604302	178983.877094	57.487412
2589.289401	178783.697116	57.492417
2589.451747	178577.649150	57.497421
2588.493415	178374.908812	57.502426
2587.938738	178162.324088	57.507431
2587.067930	177968.946199	57.512436
2586.161159	177759.090414	57.517441
2585.959435	177551.922235	57.522445
2585.070771	177353.589428	57.527450
2584.781111	177142.735867	57.532455
2583.999781	176938.816962	57.537460
2583.316970	176742.031632	57.542465
2582.875680	176525.392553	57.547469
2582.083569	176327.151091	57.552474
2581.245559	176114.926947	57.557479
2580.555554	175911.481948	57.562484
2579.783481	175704.260732	57.567489
2579.371569	175495.266450	57.572493
2578.551094	175296.703756	57.577498
2578.071328	175085.636440	57.582503
2577.243890	174878.797015	57.587508
2576.726371	174680.977862	57.592513
2576.215035	174472.538746	57.597517
2575.489808	174263.473236	57.602522
2574.785521	174050.322893	57.607527
2574.083108	173843.761454	57.612532
2573.125309	173639.161996	57.617537
2572.888768	173427.021875	57.622541
2572.027362	173228.374052	57.627546
2571.248271	173009.899470	57.632551
2570.556523	172813.592374	57.637556
2569.803434	172612.259673	57.642561
2569.415109	172408.415643	57.647565
2568.288055	172200.950696	57.652570
2567.891488	171995.787440	57.657575
2566.857722	171807.144703	57.662580
2566.475046	171597.898944	57.667585
2566.049145	171392.603573	57.672589
2565.376739	171187.768011	57.677594
2564.768356	170980.761416	57.682599
2563.762865	170787.629850	57.687604
2562.928169	170583.789677	57.692609
2562.594450	170383.915244	57.697613
2562.543400	170182.165774	57.702618
2561.708979	169965.993181	57.707623
2560.807160	169758.378284	57.712628
2560.197986	169549.471867	57.717633
2559.523739	169342.458982	57.722637
2558.739685	169137.295826	57.727642
2558.213491	168930.159958	57.732647
2557.390099	168721.190241	57.737652
2556.716313	168520.412859	57.742657
2556.528835	168321.924734	57.747661
2555.380157	168114.141648	57.752666
2554.971810	167901.791641	57.757671
2554.176071	167696.803365	57.762676
2553.605946	167490.330791	57.767681
2552.851280	167276.500495	57.772685
2552.111089	167075.283475	57.777690
2551.963344	166859.312065	57.782695
2551.472966	166651.966739	57.787700
2550.271862	166445.205675	57.792705
2549.552257	166237.314032	57.797709
2548.831864	166024.973159	57.802714
2548.395476	165809.943623	57.807719
2547.209473	165602.955937	57.812724
2546.614320	165401.813914	57.817729
2546.337925	165188.644504	57.822733
2545.168189	164989.693820	57.827738
2544.596530	164789.390606	57.832743
2544.161346	164581.984456	57.837748
2543.586570	164386.413991	57.842753
2542.919247	164177.864390	57.847757
2541.881714	163979.584815	57.852762
2541.534247	163759.848526	57.857767
2540.806046	163574.491379	57.862772
2540.114585	163305.847298	57.867777
2539.910828	163090.021130	57.872781
2539.157193	162896.127162	57.877786
2538.391394	162682.998984	57.882791
2537.972396	162477.483946	57.887796
2536.997913	162259.089381	57.892801
2536.647624	162063.750068	57.897805
2535.415581	161850.738825	57.902810
2535.226429	161634.779150	57.907815
2534.406263	161438.144560	57.912820
2534.063160	161229.420640	57.917825
2533.547405	161014.203017	57.922829
2532.877100	160805.876699	57.927834
2532.093895	160585.287915	57.932839
2531.168453	160373.660818	57.937844
2530.365988	160168.461333	57.942849
2529.943068	159950.107855	57.947853
2529.128903	159744.442275	57.952858
2528.716727	159537.442834	57.957863
2527.687157	159325.418958	57.962868
2526.778495	159124.208942	57.967873
2526.536662	158903.977089	57.972877
2525.533306	158707.513793	57.977882
2525.004161	158495.072362	57.982887
2524.435471	158288.562753	57.987892
2523.665256	158092.332937	57.992897
2523.282495	157874.074980	57.997901
2522.143770	157661.150446	58.002906
2521.677707	157456.116904	58.007911
2520.880507	157259.997765	58.012916
2520.557109	157059.164558	58.017921
2519.636613	156840.820353	58.022925
2518.840208	156640.382361	58.027930
2518.319326	156429.287067	58.032935
2517.752659	156235.463575	58.037940
2517.133081	156028.276341	58.042945
2516.644046	155822.302745	58.047949
2515.124135	155619.544662	58.052954
2514.685857	155402.595068	58.057959
2514.484195	155210.067006	58.062964
2513.643532	155007.065084	58.067969
2512.991810	154799.026010	58.072973
2512.587415	154603.571683	58.077978
2511.689817	154393.324108	58.082983
2511.202084	154189.813532	58.087988
2510.649589	153975.204667	58.092993
2510.309469	153770.262261	58.097997
2509.355506	153572.002829	58.103002
2508.614539	153361.126735	58.108007
2508.067124	153148.886626	58.113012
2507.162739	152944.585277	58.118017
2506.445923	152732.921235	58.123021
2506.068713	152535.237509	58.128026
2505.280085	152321.286797	58.133031
2504.679129	152111.108221	58.138036
2503.848503	151910.589326	58.143041
2503.146290	151701.941960	58.148045
2502.331435	151493.237503	58.153050
2501.970280	151289.457640	58.158055
2501.552418	151081.213996	58.163060
2500.564928	150871.727381	58.168065
2500.030949	150653.006205	58.173069
2498.851319	150460.368202	58.178074
2498.656094	150247.480808	58.183079
2497.896449	150042.424596	58.188084
2497.256316	149847.734664	58.193089
2496.709537	149634.627375	58.198093
2496.004429	149439.225732	58.203098
2495.348809	149223.456653	58.208103
2494.730878	149019.629974	58.213108
2493.830831	148810.180892	58.218113
2492.834862	148599.210542	58.223117
2492.314109	148402.565848	58.228122
2491.763905	148193.433894	58.233127
2491.049640	147994.382205	58.238132
2490.340136	147796.284175	58.243137
2489.917035	147584.759456	58.248141
2488.945344	147383.502887	58.253146
2488.720823	147182.408753	58.258151
2488.011520	146978.380763	58.263156
2487.113758	146766.809618	58.268161
2486.537977	146572.624959	58.273165
2486.143608	146370.940160	58.278170
2485.316304	146156.820226	58.283175
2484.488615	145952.080522	58.288180
2483.822578	145750.951071	58.293185
2483.662223	145544.913663	58.298189
2482.612303	145340.518154	58.303194
2482.187449	145133.584971	58.308199
2481.542961	144926.815046	58.313204
2480.775940	144721.196902	58.318209
2479.793265	144505.956438	58.323213
2478.901026	144304.948366	58.328218
2478.546813	144103.970678	58.333223
2477.757533	143901.360451	58.338228
2477.378544	143703.413655	58.343233
2476.928253	143491.755548	58.348237
2475.978291	143297.917350	58.353242
2475.438698	143092.299350	58.358247
2474.905217	142886.211590	58.363252
2474.176571	142680.257799	58.368257
2473.524960	142466.783417	58.373261
2472.768381	142266.770932	58.378266
2472.352885	142053.884628	58.383271
2471.730568	141853.777317	58.388276
2470.768220	141636.101262	58.393281
2470.401993	141422.627043	58.398285
2469.575847	141226.393499	58.403290
2468.688310	141020.272769	58.408295
2468.283618	140806.732730	58.413300
2467.630679	140603.487358	58.418305
2466.867692	140393.793438	58.423309
2465.914066	140193.088863	58.428314
2465.540445	139980.807612	58.433319
2464.963518	139777.250810	58.438324
2463.854868	139579.281221	58.443329
2463.491776	139366.748519	58.448333
2462.712553	139167.268287	58.453338
2462.137174	138963.272066	58.458343
2461.541893	138753.042083	58.463348
2460.713884	138548.440767	58.468353
2460.279448	138346.764176	58.473357
2459.648025	138153.035424	58.478362
2458.848221	137934.585350	58.483367
2458.491936	137723.689500	58.488372
2457.388503	137524.817968	58.493377
2456.938546	137314.054227	58.498381
2455.927997	137113.137990	58.503386
2455.420743	136903.237471	58.508391
2455.011562	136701.606190	58.513396
2454.200653	136500.662484	58.518401
2453.791572	136291.360577	58.523405
2452.859277	136093.017868	58.528410
2452.320014	135880.817570	58.533415
2451.360277	135675.761585	58.538420
2450.748934	135483.063524	58.543425
2450.173640	135267.748233	58.548429
2449.426617	135070.450223	58.553434
2448.765972	134877.179616	58.558439
2448.266087	134663.698872	58.563444
2447.489695	134464.491402	58.568449
2447.171350	134254.529159	58.573453
2446.302343	134045.710105	58.578458
2445.607576	133845.820686	58.583463
2445.245068	133643.809379	58.588468
2444.366838	133425.773834	58.593473
2443.685521	133214.936681	58.598477
2442.715127	133023.633028	58.603482
2442.274368	132820.369636	58.608487
2441.586477	132615.749574	58.613492
2441.195611	132412.811438	58.618497
2440.626524	132195.079230	58.623501
2439.483814	131997.013959	58.628506
2438.855633	131791.666313	58.633511
2438.684180	131585.041042	58.638516
2437.551326	131375.838732	58.643521
2436.925634	131173.010185	58.648525
2436.554247	130962.547040	58.653530
2435.667526	130764.386299	58.658535
2435.356591	130553.929320	58.663540
2434.492890	130354.154698	58.668545
2434.000095	130138.826825	58.673549
2432.787604	129936.811488	58.678554
2432.225110	129722.336157	58.683559
2432.117270	129518.472143	58.688564
2431.173026	129317.815888	58.693569
2430.586333	129101.126457	58.698573
2429.859244	128897.047623	58.703578
2429.294437	128690.493290	58.708583
2428.696614	128488.175086	58.713588
2427.802799	128275.770134	58.718593
2427.396051	128064.991474	58.723597
2426.848305	127862.720701	58.728602
2426.093003	127647.479104	58.733607
2425.385847	127432.066451	58.738612
2424.920650	127231.450957	58.743617
2423.960093	127007.305961	58.748621
2423.553844	126808.970223	58.753626
2422.710543	126591.604538	58.758631
2422.235352	126384.824661	58.763636
2421.355354	126177.285041	58.768641
2420.738458	125963.164985	58.773645
2419.827368	125757.589227	58.778650
2419.226670	125539.012405	58.783655
2419.036758	125329.693515	58.788660
2418.075072	125133.058124	58.793665
2417.684755	124909.995582	58.798669
2416.644340	124704.702281	58.803674
2416.104149	124496.093010	58.808679
2415.644778	124299.891997	58.813684
2414.610556	124080.227384	58.818689
2414.071868	123860.574894	58.823693
2413.296682	123658.041216	58.828698
2412.367057	123448.028774	58.833703
2412.060887	123238.008024	58.838708
2411.086810	123029.504314	58.843713
2410.783511	122822.038719	58.848717
2410.184848	122614.888220	58.853722
2409.431880	122401.313241	58.858727
2408.696342	122194.581346	58.863732
2408.006887	121990.789628	58.868737
2407.445102	121781.100226	58.873741
2406.614215	121584.635195	58.878746
2405.815636	121379.367167	58.883751
2405.496119	121168.907750	58.888756
2404.519453	120960.027074	58.893761
2404.357283	120750.130123	58.898765
2403.743876	120534.643500	58.903770
2402.946891	120333.268657	58.908775
2402.359667	120124.536021	58.913780
2401.468857	119908.539854	58.918785
2401.175996	119687.194262	58.923789
2400.341835	119479.458165	58.928794
2399.310101	119277.570010	58.933799
2399.109803	119053.339370	58.938804
2398.180412	118851.939792	58.943809
2397.357673	118631.950435	58.948813
2396.743063	118429.640887	58.953818
2396.191770	118224.847174	58.958823
2395.647563	118011.204970	58.963828
2394.824642	117804.064489	58.968833
2394.470964	117590.236860	58.973837
2393.813678	117389.275251	58.978842
2392.942085	117175.628389	58.983847
2392.193482	116965.664482	58.988852
2391.437487	116748.721104	58.993857
2391.181115	116538.619171	58.998861
2390.516942	116330.564032	59.003866
2389.708468	116115.392592	59.008871
2389.010487	115892.728225	59.013876
2388.409968	115696.740883	59.018881
2388.328359	115471.449881	59.023885
2387.047566	115263.310788	59.028890
2386.604162	115046.890861	59.033895
2386.055053	114833.231494	59.038900
2385.518231	114619.146725	59.043905
2384.654460	114396.261522	59.048909
2383.784193	114180.094395	59.053914
2382.860378	113969.192844	59.058919
2382.621007	113751.558428	59.063924
2381.686220	113544.755889	59.068929
2381.357482	113328.338846	59.073933
2380.582480	113119.623142	59.078938
2379.629897	112902.813639	59.083943
2379.225165	112675.510761	59.088948
2378.602811	112474.442899	59.093953
2378.010320	112256.978981	59.098957
2377.511824	112033.174680	59.103962
2376.853351	111826.653504	59.108967
2376.235953	111597.407757	59.113972
2375.236155	111399.524451	59.118977
2374.887595	111174.301586	59.123981
2374.376144	110957.610419	59.128986
2373.385690	110734.936589	59.133991
2372.870625	110514.956258	59.138996
2371.924532	110294.062605	59.144001
2371.090719	110076.744916	59.149005
2370.636266	109870.912112	59.154010
2369.901186	109662.022428	59.159015
2369.561722	109426.813089	59.164020
2368.548854	109220.611039	59.169025
2368.302963	108992.859908	59.174029
2367.407695	108797.849166	59.179034
2366.597075	108569.899623	59.184039
2366.279623	108354.025580	59.189044
2365.609055	108133.964360	59.194049
2364.802011	107908.768001	59.199053
2364.330521	107706.223989	59.204058
2363.459712	107489.252449	59.209063
2363.128168	107265.281100	59.214068
2362.166208	107044.736626	59.219073
2361.915760	106823.294561	59.224077
2360.991870	106605.273402	59.229082
2360.152207	106392.564276	59.234087
2359.474988	106165.713884	59.239092
2358.651172	105944.059918	59.244097
2358.081728	105726.967628	59.249101
2357.204187	105503.346684	59.254106
2356.697762	105291.723839	59.259111
2356.557657	105078.039886	59.264116
2355.669367	104871.353970	59.269121
2355.000838	104647.682517	59.274125
2354.473696	104425.462654	59.279130
2353.565170	104212.472959	59.284135
2353.007766	103990.350784	59.289140
2352.138924	103761.764522	59.294145
2351.797681	103529.360079	59.299149
2350.948286	103336.524386	59.304154
2350.293808	103111.672490	59.309159
2349.472461	102881.374310	59.314164
2348.785971	102671.814428	59.319169
2348.480983	102444.680406	59.324173
2347.950990	102224.327756	59.329178
2346.796074	102011.111521	59.334183
2346.380529	101793.523348	59.339188
2345.666629	101571.613720	59.344193
2345.142331	101350.177279	59.349197
2344.560413	101129.538674	59.354202
2343.615216	100915.195404	59.359207
2343.375497	100681.350395	59.364212
2342.602417	100473.289265	59.369217
2342.247244	100243.869257	59.374221
2341.253529	100020.325118	59.379226
2340.630515	99800.555636	59.384231
2340.265491	99571.029672	59.389236
2339.385796	99345.888190	59.394241
2338.765945	99115.075123	59.399245
2338.009871	98896.971831	59.404250
2337.077928	98670.158015	59.409255
2336.445599	98443.229157	59.414260
2335.579757	98229.113862	59.419265
2335.015899	98000.002968	59.424269
2334.630596	97778.673819	59.429274
2334.016931	97557.966539	59.434279
2333.324889	97338.174455	59.439284
2332.449834	97117.373349	59.444289
2332.058278	96886.730452	59.449293
2331.172174	96672.030442	59.454298
2330.389151	96446.578677	59.459303
2330.088523	96218.585544	59.464308
2329.206415	96007.258891	59.469313
2328.775350	95775.073388	59.474317
2328.134935	95556.717321	59.479322
2327.189484	95327.313339	59.484327
2326.714985	95092.630330	59.489332
2325.874064	94871.592027	59.494337
2325.473630	94652.566140	59.499341
2324.686440	94439.761497	59.504346
2323.872062	94216.765846	59.509351
2323.551032	93978.353944	59.514356
2322.593632	93767.117337	59.519361
2321.936368	93550.533690	59.524365
2321.308792	93315.925252	59.529370
2320.219851	93092.179006	59.534375
2319.710265	92870.600618	59.539380
2318.936169	92663.093080	59.544385
2318.671245	92443.116180	59.549389
2317.925439	92229.736327	59.554394
2317.156263	92006.020065	59.559399
2317.023977	91774.361333	59.564404
2316.082807	91562.439262	59.569409
2315.307827	91340.645596	59.574413
2314.846003	91114.429389	59.579418
2314.320980	90882.442829	59.584423
2313.703912	90654.550323	59.589428
2313.070451	90437.714350	59.594433
2312.328632	90203.315549	59.599437
2311.872734	89975.036792	59.604442
2310.753761	89747.429859	59.609447
2310.207915	89521.959847	59.614452
2309.519193	89312.428768	59.619457
2308.737360	89072.266159	59.624461
2308.170651	88853.983413	59.629466
2307.519148	88618.788447	59.634471
2307.063897	88395.832711	59.639476
2306.025451	88172.255344	59.644481
2305.465403	87942.023682	59.649485
2304.925749	87722.885806	59.654490
2304.465867	87500.073158	59.659495
2303.682579	87274.708509	59.664500
2303.074684	87050.567294	59.669505
2302.204299	86814.304554	59.674509
2301.768691	86592.334251	59.679514
2301.046410	86367.311756	59.684519
2300.598554	86132.574343	59.689524
2299.485695	85912.804097	59.694529
2298.999769	85686.255211	59.699533
2298.032056	85457.141731	59.704538
2297.525631	85240.984247	59.709543
2297.158002	85011.298620	59.714548
2296.231031	84785.025752	59.719553
2295.477439	84559.881460	59.724557
2295.086715	84328.229154	59.729562
2294.226967	84116.684008	59.734567
2293.816739	83885.768575	59.739572
2292.765061	83657.372375	59.744577
2292.658670	83428.549835	59.749581
2291.935325	83208.999303	59.754586
2291.211556	82981.325358	59.759591
2290.804753	82749.002013	59.764596
2289.951358	82516.606278	59.769601
2289.257811	82286.399772	59.774605
2288.731290	82055.022110	59.779610
2287.458041	81825.311899	59.784615
2287.110222	81598.258807	59.789620
2286.354734	81367.318006	59.794625
2285.670211	81145.406196	59.799629
2285.039135	80915.204861	59.804634
2284.174529	80691.095566	59.809639
2283.823662	80463.668700	59.814644
2282.848723	80246.971316	59.819649
2282.417934	80020.347827	59.824653
2281.689474	79792.994524	59.829658
2280.845603	79579.490042	59.834663
2280.774874	79342.410987	59.839668
2279.870477	79123.508803	59.844673
2278.981940	78885.601438	59.849677
2278.560053	78664.314558	59.854682
2277.460638	78440.811840	59.859687
2277.120534	78204.637732	59.864692
2276.303412	77990.758904	59.869697
2275.610323	77761.882530	59.874701
2275.046614	77543.735216	59.879706
2274.149305	77326.074025	59.884711
2273.769615	77094.139174	59.889716
2272.850493	76875.085866	59.894721
2272.206149	76647.570234	59.899725
2271.789522	76434.024348	59.904730
2271.066400	76208.097531	59.909735
2270.506742	75975.082429	59.914740
2269.708675	75751.833775	59.919745
2269.156730	75531.577182	59.924750
2268.637213	75306.046289	59.929754
2267.594808	75090.294807	59.934759
2267.234897	74851.615625	59.939764
2266.366983	74639.009214	59.944769
2265.799727	74405.018664	59.949774
2265.140277	74175.404374	59.954778
2264.183709	73967.469470	59.959783
2263.730637	73737.155877	59.964788
2263.106229	73513.980453	59.969793
2262.745803	73291.772965	59.974798
2262.238312	73070.003059	59.979802
2260.902180	72852.725670	59.984807
2260.338240	72617.520058	59.989812
2259.644306	72400.741233	59.994817
2259.165830	72170.741102	59.999822
2258.620529	71953.664823	60.004826
2257.628660	71727.894282	60.009831
2257.556919	71503.063618	60.014836
2256.637213	71280.726507	60.019841
2255.837070	71062.040689	60.024846
2255.265320	70831.823794	60.029850
2254.247272	70613.817281	60.034855
2253.716258	70377.017662	60.039860
2252.836944	70175.590208	60.044865
2252.415717	69944.720001	60.049870
2252.129005	69725.524140	60.054874
2251.208365	69497.785145	60.059879
2250.824770	69271.920839	60.064884
2249.946650	69049.931637	60.069889
2249.523819	68815.249202	60.074894
2248.917903	68600.524939	60.079898
2247.628861	68371.654019	60.084903
2247.567551	68139.816881	60.089908
2246.515242	67914.954674	60.094913
2246.048663	67700.230870	60.099918
2245.591533	67474.949989	60.104922
2244.520406	67249.192762	60.109927
2244.169697	67026.161230	60.114932
2243.540135	66798.458195	60.119937
2242.812180	66579.538595	60.124942
2242.080777	66345.181839	60.129946
2241.168445	66125.033163	60.134951
2240.691526	65887.807540	60.139956
2239.926867	65665.655285	60.144961
2239.044091	65462.760317	60.149966
2238.392845	65222.239454	60.154970
2237.820311	65007.147512	60.159975
2237.201004	64785.264161	60.164980
2236.660220	64569.051212	60.169985
2236.167650	64353.070518	60.174990
2235.663210	64126.895807	60.179994
2234.862556	63901.717434	60.184999
2234.072883	63666.800971	60.190004
2233.479290	63440.439553	60.195009
2232.687820	63226.424975	60.200014
2232.169460	62999.448975	60.205018
2231.142875	62777.178619	60.210023
2230.584061	62557.648018	60.215028
2229.908065	62335.925574	60.220033
2229.020267	62120.726176	60.225038
2228.673328	61893.330964	60.230042
2227.836383	61684.393632	60.235047
2227.247785	61446.139131	60.240052
2226.660914	61231.576413	60.245057
2225.838794	61020.868097	60.250062
2225.599037	60798.936180	60.255066
2224.861249	60576.322963	60.260071
2224.308417	60354.673864	60.265076
2223.523174	60130.079145	60.270081
2222.618823	59914.366229	60.275086
2222.252215	59683.623197	60.280090
2221.134258	59461.542489	60.285095
2220.571744	59242.070051	60.290100
2219.946630	59018.504665	60.295105
2218.690212	58809.612010	60.300110
2218.432108	58587.332495	60.305114
2217.688496	58370.491386	60.310119
2217.100018	58157.825247	60.315124
2216.409437	57948.320741	60.320129
2215.801722	57729.116998	60.325134
2215.685001	57507.429325	60.330138
2214.497263	57299.128284	60.335143
2213.849556	57065.392148	60.340148
2213.411388	56846.694170	60.345153
2212.363504	56634.428537	60.350158
2211.767700	56418.507798	60.355162
2210.881268	56212.744270	60.360167
2210.654092	55983.094766	60.365172
2209.708259	55780.307769	60.370177
2209.365936	55556.685462	60.375182
2208.626187	55345.363713	60.380186
2207.631960	55131.394786	60.385191
2207.313336	54905.064521	60.390196
2206.738512	54701.860321	60.395201
2206.219504	54485.475414	60.400206
2205.386763	54258.544819	60.405210
2204.538114	54038.821950	60.410215
2203.944919	53829.665293	60.415220
2203.185436	53616.996429	60.420225
2202.762594	53398.947827	60.425230
2202.334319	53183.500626	60.430234
2201.333075	52974.617876	60.435239
2200.742725	52753.040583	60.440244
2199.879804	52530.578951	60.445249
2199.278142	52320.520211	60.450254
2198.746553	52102.596192	60.455258
2197.632230	51894.791166	60.460263
2197.239314	51681.529957	60.465268
2196.506409	51463.101364	60.470273
2195.869337	51256.009504	60.475278
2195.280803	51034.234671	60.480282
2194.537404	50829.850788	60.485287
2193.846025	50619.285053	60.490292
2193.160822	50398.115557	60.495297
2192.307639	50191.048099	60.500302
2191.732695	49992.541223	60.505306
2191.121557	49777.505377	60.510311
2190.598899	49554.884162	60.515316
2189.699515	49350.231851	60.520321
2188.776029	49139.536841	60.525326
2188.747230	48933.102951	60.530330
2187.546015	48725.006757	60.535335
2187.092875	48526.053958	60.540340
2186.748860	48314.523859	60.545345
2185.764065	48104.730270	60.550350
2185.153272	47891.732233	60.555354
2184.219285	47687.617004	60.560359
2183.767015	47471.720192	60.565364
2183.080657	47277.446347	60.570369
2181.924236	47073.569610	60.575374
2181.533185	46860.090448	60.580378
2180.848904	46666.449309	60.585383
2180.108308	46464.860725	60.590388
2179.638386	46256.959039	60.595393
2178.918674	46053.790286	60.600398
2178.642067	45850.983758	60.605402
2177.580240	45650.967393	60.610407
2177.136927	45440.955077	60.615412
2176.232387	45249.297055	60.620417
2175.430574	45044.106588	60.625422
2174.896146	44823.798738	60.630426
2174.127457	44636.670903	60.635431
2173.688389	44431.518631	60.640436
2172.866321	44237.641493	60.645441
2172.301246	44034.367253	60.650446
2171.495563	43817.559328	60.655450
2170.931742	43631.178307	60.660455
2170.305377	43428.139086	60.665460
2169.666180	43231.404115	60.670465
2168.797577	43039.223870	60.675470
2168.419582	42824.204240	60.680474
2167.925331	42630.716781	60.685479
2167.054021	42430.141054	60.690484
2166.249835	42229.904865	60.695489
2165.509832	42027.576821	60.700494
2164.906651	41829.523867	60.705498
2164.054363	41640.850922	60.710503
2163.718315	41424.273544	60.715508
2163.067301	41233.612533	60.720513
2162.036226	41044.819531	60.725518
2161.311564	40839.321853	60.730522
2160.784917	40649.906110	60.735527
2160.081734	40450.060355	60.740532
2159.392445	40255.460526	60.745537
2158.656468	40057.120190	60.750542
2158.091582	39861.820523	60.755546
2157.284448	39683.054096	60.760551
2156.628400	39482.554470	60.765556
2156.104593	39290.751852	60.770561
2155.091691	39107.695520	60.775566
2154.845268	38908.095682	60.780570
2154.109144	38728.178682	60.785575
2153.003229	38536.489550	60.790580
2152.415771	38351.652295	60.795585
2151.704757	38166.261234	60.800590
2151.271456	37968.176972	60.805594
2150.360393	37793.613857	60.810599
2149.603364	37612.246602	60.815604
2148.967462	37418.223964	60.820609
2148.127717	37240.152294	60.825614
2147.539034	37058.465504	60.830618
2146.930981	36885.479173	60.835623
2146.086550	36699.512020	60.840628
2145.182113	36526.865653	60.845633
2144.509854	36356.676904	60.850638
2143.790241	36188.149151	60.855642
2142.750319	36016.784532	60.860647
2142.207686	35839.221084	60.865652
2141.510275	35684.013024	60.870657
2140.420191	35524.849301	60.875662
2140.083988	35358.083535	60.880666
2138.597841	35214.514584	60.885671
2137.701582	35060.232110	60.890676
2137.152132	34911.182857	60.895681
2136.551956	34774.537275	60.900686
2135.852241	34622.249117	60.905690
2134.929564	34491.754540	60.910695
2134.060395	34339.023286	60.915700
2133.333830	34197.400316	60.920705
2132.562586	34074.667101	60.925710
2131.918036	33940.835914	60.930714
2131.226721	33810.905773	60.935719
2130.792742	33669.054379	60.940724
2129.859903	33550.262153	60.945729
2129.100694	33417.463230	60.950734
2128.486635	33284.395801	60.955738
2127.470399	33169.963939	60.960743
2126.788991	33035.701800	60.965748
2126.175067	32909.957476	60.970753
2125.597988	32801.605945	60.975758
2125.225871	32681.198062	60.980762
2124.143856	32561.346172	60.985767
2123.621668	32441.802974	60.990772
2123.005761	32328.474910	60.995777
2122.452888	32205.998980	61.000782
2121.693744	32079.433820	61.005786
2121.091224	31961.480764	61.010791
2120.300096	31840.838909	61.015796
2119.713773	31719.005564	61.020801
2118.897782	31614.147740	61.025806
2118.263677	31490.885676	61.030810
2117.341866	31375.553697	61.035815
2116.747038	31264.127386	61.040820
2116.212665	31145.578366	61.045825
2115.696333	31050.380332	61.050830
2115.373389	30923.097490	61.055834
2114.284524	30818.762067	61.060839
2113.643770	30695.601818	61.065844
2113.066965	30585.678349	61.070849
2112.445356	30464.180645	61.075854
2112.157818	30347.088240	61.080858
2111.160708	30249.558346	61.085863
2110.689522	30123.534513	61.090868
2109.893416	30014.918451	61.095873
2109.409897	29894.449047	61.100878
2108.951587	29773.327138	61.105882
2107.990529	29660.005847	61.110887
2107.685196	29544.241310	61.115892
2106.937482	29423.651390	61.120897
2105.964990	29308.281942	61.125902
2105.475249	29201.019374	61.130906
2104.838948	29084.324707	61.135911
2104.287697	28971.412414	61.140916
2103.920318	28850.194437	61.145921
2103.023262	28733.183432	61.150926
2102.641884	28610.658118	61.155930
2102.076301	28484.440706	61.160935
2101.045047	28364.317541	61.165940
2100.521359	28236.573970	61.170945
2099.661848	28124.026118	61.175950
2099.350801	28003.818193	61.180954
2098.623240	27889.685391	61.185959
2097.893536	27768.171177	61.190964
2097.172392	27646.206265	61.195969
2096.059997	27532.721571	61.200974
2095.514756	27406.386078	61.205978
2094.899412	27296.809992	61.210983
2094.235750	27175.363990	61.215988
2093.714228	27065.030510	61.220993
2092.992976	26960.159085	61.225998
2092.366218	26838.493328	61.231002
2091.561935	26726.184959	61.236007
2090.819581	26618.273381	61.241012
2090.198075	26500.552315	61.246017
2089.506196	26394.374272	61.251022
2088.928561	26274.003482	61.256026
2088.029177	26165.066992	61.261031
2087.159142	26052.960933	61.266036
2086.851543	25938.845548	61.271041
2086.067549	25839.641779	61.276046
2085.754199	25722.360075	61.281050
2085.152651	25616.979221	61.286055
2084.586548	25503.566641	61.291060
2084.150163	25391.293702	61.296065
2083.291673	25277.376255	61.301070
2082.657365	25153.466391	61.306074
2081.941153	25036.680889	61.311079
2081.167397	24920.139141	61.316084
2080.858329	24807.024766	61.321089
2079.847591	24691.119355	61.326094
2079.448324	24574.553863	61.331098
2078.356132	24461.352962	61.336103
2077.919087	24342.610694	61.341108
2077.349058	24233.323092	61.346113
2076.547407	24117.806428	61.351118
2076.138169	23992.597558	61.356122
2075.163314	23883.684582	61.361127
2074.720474	23761.856558	61.366132
2074.149777	23647.975319	61.371137
2073.613752	23546.618116	61.376142
2072.957897	23416.653834	61.381146
2072.192238	23305.446743	61.386151
2071.647124	23184.097384	61.391156
2071.052503	23071.459925	61.396161
2070.220761	22951.559513	61.401166
2069.555936	22834.590845	61.406170
2068.805816	22724.265045	61.411175
2068.137755	22607.207751	61.416180
2067.481039	22491.105004	61.421185
2066.671188	22376.227675	61.426190
2066.200108	22265.338822	61.431194
2065.307605	22144.356538	61.436199
2064.702222	22032.436458	61.441204
2064.358719	21912.151351	61.446209
2063.189606	21801.241489	61.451214
2062.768986	21684.596293	61.456218
2062.091044	21576.933554	61.461223
2061.285607	21463.553717	61.466228
2060.578608	21351.769065	61.471233
2059.745399	21249.211905	61.476238
2059.159628	21133.264189	61.481242
2058.483824	21024.892662	61.486247
2057.914112	20920.899046	61.491252
2057.076396	20805.184010	61.496257
2056.076952	20709.364948	61.501262
2055.887005	20594.748803	61.506266
2054.905837	20487.515076	61.511271
2054.173860	20381.110252	61.516276
2053.442915	20278.776093	61.521281
2052.948531	20181.390221	61.526286
2052.716790	20075.071515	61.531290
2051.768208	19977.916889	61.536295
2050.991523	19865.481947	61.541300
2050.495705	19758.401974	61.546305
2049.610880	19657.856118	61.551310
2048.846873	19553.125885	61.556314
2048.233376	19461.758519	61.561319
2047.738926	19358.251596	61.566324
2046.933567	19253.655061	61.571329
2046.054711	19161.614696	61.576334
2045.379978	19055.486487	61.581338
2044.854126	18970.808432	61.586343
2044.038924	18872.399219	61.591348
2043.732340	18765.065077	61.596353
2042.887745	18674.930682	61.601358
2042.243871	18567.098011	61.606362
2041.764847	18466.523038	61.611367
2040.654324	18370.345513	61.616372
2039.905062	18275.251208	61.621377
2039.090074	18187.823121	61.626382
2038.762026	18097.398909	61.631386
2037.920403	18007.188562	61.636391
2037.263006	17908.630518	61.641396
2036.537049	17810.774723	61.646401
2035.957798	17732.648667	61.651406
2035.129706	17641.351264	61.656410
2034.820987	17554.174782	61.661415
2033.846561	17460.115053	61.666420
2033.181032	17365.781892	61.671425
2032.278389	17288.042914	61.676430
2032.112106	17195.798442	61.681434
2031.264538	17117.165093	61.686439
2030.327896	17021.550880	61.691444
2029.886196	16928.903333	61.696449
2028.820192	16858.600345	61.701454
2028.604991	16769.198836	61.706458
2027.822809	16684.075799	61.711463
2027.064606	16586.388929	61.716468
2026.118823	16506.547799	61.721473
2025.407853	16429.228497	61.726478
2025.113078	16348.478341	61.731482
2024.500465	16259.079303	61.736487
2023.892676	16181.758872	61.741492
2023.672579	16089.160897	61.746497
2022.624526	16005.493539	61.751502
2021.954650	15907.208888	61.756506
2021.452408	15830.682125	61.761511
2020.642191	15744.335986	61.766516
2019.737123	15657.900208	61.771521
2018.962382	15583.470921	61.776526
2018.707889	15496.734874	61.781530
2017.785209	15413.244802	61.786535
2016.953937	15342.579758	61.791540
2016.479540	15260.158126	61.796545
2015.704751	15178.328429	61.801550
2015.082187	15079.694450	61.806554
2014.453636	15010.768623	61.811559
2013.510716	14929.231541	61.816564
2012.790320	14850.046822	61.821569
2011.884077	14776.105414	61.826574
2011.682589	14694.738898	61.831578
2010.898687	14636.763993	61.836583
2009.926482	14566.502643	61.841588
2009.692454	14484.426942	61.846593
2008.815809	14410.689380	61.851598
2008.023150	14336.624920	61.856602
2007.199348	14265.988995	61.861607
2006.639261	14189.669480	61.866612
2006.325665	14118.752888	61.871617
2005.415659	14047.456956	61.876622
2005.265209	13968.801922	61.881626
2004.612978	13897.066823	61.886631
2003.964633	13818.824363	61.891636
2003.363241	13742.592648	61.896641
2002.382720	13663.759974	61.901646
2001.793101	13583.456142	61.906650
2001.219816	13519.042503	61.911655
2000.413031	13445.822429	61.916660
2000.219664	13357.185400	61.921665
1999.315590	13290.720640	61.926670
1998.362177	13206.496047	61.931674
1997.619481	13129.971968	61.936679
1996.717847	13061.712626	61.941684
1995.990022	12987.053091	61.946689
1995.488188	12928.198334	61.951694
1994.815026	12845.742104	61.956698
1994.240891	12792.667869	61.961703
1993.555802	12715.167238	61.966708
1992.979993	12639.631624	61.971713
1992.091991	12580.772126	61.976718
1991.613203	12502.025523	61.981722
1990.975633	12446.317232	61.986727
1989.944954	12379.861646	61.991732
1989.853115	12311.832937	61.996737
1989.301145	12241.461425	62.001742
1988.560259	12164.775594	62.006746
1987.516167	12088.042594	62.011751
1986.872730	12021.874917	62.016756
1986.428277	11947.396282	62.021761
1985.319286	11890.256843	62.026766
1984.957368	11823.880419	62.031770
1984.352254	11760.926991	62.036775
1983.542593	11689.724598	62.041780
1983.162416	11619.141285	62.046785
1982.281462	11553.454656	62.051790
1981.466854	11480.391949	62.056794
1980.863903	11411.685728	62.061799
1979.989769	11359.442456	62.066804
1979.597563	11293.349734	62.071809
1978.683425	11236.725317	62.076814
1978.049416	11166.340639	62.081818
1977.570942	11102.827743	62.086823
1976.886846	11041.459512	62.091828
1976.222524	10973.264503	62.096833
1975.672326	10909.674045	62.101838
1975.117018	10841.955492	62.106842
1974.108954	10785.803751	62.111847
1973.668923	10714.695812	62.116852
1973.360963	10649.747902	62.121857
1972.211360	10586.179381	62.126862
1971.871284	10521.144013	62.131866
1971.455722	10449.226636	62.136871
1970.549107	10383.163319	62.141876
1969.864156	10316.273309	62.146881
1968.950512	10258.377003	62.151886
1968.546068	10195.255220	62.156890
1967.977413	10126.554322	62.161895
1967.154853	10073.177230	62.166900
1966.602001	9984.293418	62.171905
1965.671125	9928.164575	62.176910
1964.946772	9859.762014	62.181914
1964.182781	9795.172632	62.186919
1963.492422	9740.277801	62.191924
1963.003223	9679.974574	62.196929
1962.302825	9620.297652	62.201934
1961.753024	9545.574562	62.206938
1961.074627	9486.323893	62.211943
1960.170143	9433.391287	62.216948
1960.046034	9356.802663	62.221953
1959.258103	9304.781436	62.226958
1958.443736	9240.947230	62.231962
1957.599450	9173.080454	62.236967
1956.856789	9104.987592	62.241972
1955.982596	9047.451431	62.246977
1954.949291	8995.391329	62.251982
1954.443843	8934.758358	62.256986
1954.140753	8883.131065	62.261991
1952.950953	8837.597400	62.266996
1952.843763	8775.385080	62.272001
1951.944218	8715.680642	62.277006
1951.545525	8667.051115	62.282010
1951.026459	8604.575101	62.287015
1950.519584	8546.127733	62.292020
1950.252158	8484.848942	62.297025
1949.476245	8428.456143	62.302030
1948.564710	8361.329934	62.307034
1948.139819	8301.167196	62.312039
1947.037606	8244.868700	62.317044
1946.889318	8172.444444	62.322049
1945.721440	8113.792064	62.327054
1944.962398	8063.748781	62.332058
1944.441755	8001.202953	62.337063
1943.855297	7941.518568	62.342068
1943.206147	7881.214034	62.347073
1942.323957	7829.058665	62.352078
1942.014882	7762.797634	62.357082
1941.504507	7707.209924	62.362087
1940.472437	7646.575829	62.367092
1939.887353	7583.587178	62.372097
1939.099580	7525.884188	62.377102
1938.567367	7469.033085	62.382106
1937.958745	7408.601748	62.387111
1937.122659	7342.884185	62.392116
1936.770040	7279.506496	62.397121
1936.048198	7232.540267	62.402126
1935.203318	7160.794744	62.407130
1934.806118	7106.234983	62.412135
1933.898737	7057.964783	62.417140
1933.292523	6989.545132	62.422145
1932.488397	6934.810782	62.427150
1931.823403	6865.481223	62.432154
1931.497568	6817.782517	62.437159
1930.526033	6755.526080	62.442164
1929.996185	6688.271866	62.447169
1929.150883	6647.218188	62.452174
1928.632119	6582.548523	62.457178
1927.900640	6532.754885	62.462183
1927.039396	6465.889540	62.467188
1926.483580	6402.386127	62.472193
1925.694938	6352.995793	62.477198
1925.222575	6301.146341	62.482202
1924.384046	6244.252304	62.487207
1923.731929	6191.715518	62.492212
1923.441918	6133.506636	62.497217
1922.667713	6082.265137	62.502222
1922.195008	6025.950435	62.507226
1921.489908	5974.357571	62.512231
1920.490379	5915.890649	62.517236
1920.221255	5852.288859	62.522241
1919.067661	5800.465688	62.527246
1918.783598	5747.006737	62.532250
1917.907741	5696.123470	62.537255
1917.202686	5633.875976	62.542260
1916.812064	5566.936816	62.547265
1915.967683	5529.611531	62.552270
1915.540044	5465.033231	62.557274
1914.911750	5403.959266	62.562279
1914.003957	5345.273376	62.567284
1913.336866	5289.264459	62.572289
1912.570977	5234.882894	62.577294
1911.703154	5180.012901	62.582298
1911.013037	5130.794786	62.587303
1910.133135	5076.747408	62.592308
1909.986877	5035.688976	62.597313
1909.365098	4992.273625	62.602318
1908.715328	4928.799327	62.607322
1907.990214	4876.403420	62.612327
1907.523919	4822.954649	62.617332
1907.079605	4772.438287	62.622337
1906.231912	4705.865053	62.627342
1905.416631	4657.037518	62.632346
1904.812133	4597.468022	62.637351
1904.095428	4543.608859	62.642356
1903.905598	4477.993846	62.647361
1902.687659	4425.794511	62.652366
1902.146003	4373.484843	62.657370
1901.622888	4314.950203	62.662375
1900.616490	4267.117329	62.667380
1900.347665	4209.377201	62.672385
1899.507087	4155.204708	62.677390
1898.744951	4101.506596	62.682394
1897.970468	4054.653452	62.687399
1897.328536	4009.998827	62.692404
1896.949324	3944.607117	62.697409
1896.146104	3904.455082	62.702414
1895.415320	3852.633946	62.707418
1894.811646	3791.262254	62.712423
1893.691336	3743.687355	62.717428
1893.228401	3683.978409	62.722433
1892.566722	3633.047755	62.727438
1891.927733	3577.728611	62.732442
1891.492220	3534.575066	62.737447
1890.615391	3481.690837	62.742452
1890.241412	3420.893870	62.747457
1889.399157	3379.978935	62.752462
1888.931711	3330.250398	62.757466
1888.132930	3279.071437	62.762471
1887.243784	3227.393584	62.767476
1886.655348	3170.475640	62.772481
1885.891299	3124.786292	62.777486
1885.341241	3075.943197	62.782490
1884.816812	3025.749180	62.787495
1884.221634	2991.557211	62.792500
1883.853055	2926.356828	62.797505
1882.766410	2866.642182	62.802510
1882.080217	2821.077067	62.807514
1881.578416	2772.847192	62.812519
1881.212895	2723.638437	62.817524
1879.982666	2671.010401	62.822529
1879.393740	2618.008662	62.827534
1878.810918	2569.503682	62.832538
1878.145743	2522.107336	62.837543
1877.427891	2478.951251	62.842548
1877.047704	2417.628684	62.847553
1876.006602	2374.563660	62.852558
1875.606135	2321.488122	62.857562
1874.834168	2272.902961	62.862567
1874.289351	2222.434189	62.867572
1873.649861	2174.256538	62.872577
1872.644490	2129.559672	62.877582
1872.324557	2071.276152	62.882586
1871.767059	2031.919061	62.887591
1870.828730	1984.347810	62.892596
1870.487826	1926.617847	62.897601
1869.144751	1880.230209	62.902606
1868.806279	1838.809035	62.907610
1868.220069	1791.137560	62.912615
1867.527308	1747.519909	62.917620
1866.971743	1694.646338	62.922625
1866.334970	1646.777543	62.927630
1865.808814	1594.320766	62.932634
1865.024527	1537.631105	62.937639
1864.193920	1495.545421	62.942644
1863.643947	1449.210665	62.947649
1862.850121	1394.502378	62.952654
1862.165383	1344.393210	62.957658
1861.520229	1306.135479	62.962663
1860.551259	1257.009336	62.967668
1860.045531	1207.985656	62.972673
1859.168286	1170.410958	62.977678
1858.952884	1119.925240	62.982682
1858.306330	1073.820710	62.987687
1857.251356	1040.752720	62.992692
1856.798053	989.757188	62.997697
1855.909173	947.359830	63.002702
1855.093553	907.009046	63.007706
1854.768411	871.051491	63.012711
1853.873951	819.644018	63.017716
1853.276735	782.504501	63.022721
1852.657391	747.671096	63.027726
1851.795143	694.938954	63.032730
1851.450840	659.924886	63.037735
1850.434798	624.777849	63.042740
1849.611585	577.247335	63.047745
1849.418469	544.852655	63.052750
1848.514867	505.477373	63.057754
1847.735934	468.932090	63.062759
1847.013680	433.319382	63.067764
1846.238600	404.064229	63.072769
1845.683099	368.715375	63.077774
1844.805178	330.432518	63.082778
1844.443269	295.269155	63.087783
1843.319901	277.318360	63.092788
1842.862128	239.413749	63.097793
1842.230018	217.126334	63.102798
1841.114864	188.006044	63.107802
1840.710349	153.718715	63.112807
1839.829330	132.667102	63.117812
1838.785943	104.114342	63.122817
1838.331681	85.265899	63.127822
1837.723056	69.264790	63.132826
1837.353447	37.055391	63.137831
1836.244069	28.589800	63.142836
1835.414046	7.743166	63.147841
1834.800171	5.957834	63.152846
1832.977786	11.963843	63.157850
1831.767593	15.809963	63.162855
1830.661323	37.667600	63.167860
1830.526144	38.042412	63.172865
1830.189041	36.534833	63.177870
1829.349802	39.069935	63.182874
1828.901892	40.615637	63.187879
1828.673595	50.959134	63.192884
1828.357109	41.322101	63.197889
1827.470265	40.452179	63.202894
1826.352198	43.394263	63.207898
1825.838601	40.208417	63.212903
1825.059497	56.564093	63.217908
1825.055248	47.131372	63.222913
1824.492030	44.833359	63.227918
1823.935901	56.149872	63.232922
1823.178526	43.969789	63.237927
1822.188422	46.008447	63.242932
1821.355920	42.777044	63.247937
1820.610802	50.130650	63.252942
1819.455530	55.207570	63.257946
1819.574082	45.769543	63.262951
1818.903151	52.491617	63.267956
1818.384280	49.844359	63.272961
1817.903638	50.463265	63.277966
1816.863267	61.913447	63.282970
1816.143480	49.653275	63.287975
1815.136310	52.648720	63.292980
1815.374156	51.631750	63.297985
1815.028229	50.436239	63.302990
1813.758959	50.994289	63.307994
1812.882990	45.019537	63.312999
1812.197521	50.092822	63.318004
1811.974788	43.927608	63.323009
1811.304278	53.811462	63.328014
1810.389326	61.975803	63.333018
1810.068186	55.081876	63.338023
1809.109049	58.408747	63.343028
1808.127417	55.872821	63.348033
1807.478154	54.192458	63.353038
1806.592349	54.438881	63.358042
1806.712457	43.877798	63.363047
1806.130120	56.299207	63.368052
1805.137595	50.945371	63.373057
1804.550200	47.941560	63.378062
1804.325626	51.452990	63.383066
1803.335706	49.038234	63.388071
1802.202443	53.438295	63.393076
1801.903311	48.810152	63.398081
1801.496532	45.597887	63.403086
1800.974624	50.769782	63.408090
1800.311644	44.950451	63.413095
1799.052712	48.145154	63.418100
1798.742673	41.949652	63.423105
1798.017645	49.629660	63.428110
1797.424665	53.882425	63.433114
1796.972247	40.559504	63.438119
1795.961356	50.019585	63.443124
1795.625352	51.339361	63.448129
1794.583131	47.731255	63.453134
1793.848623	55.449043	63.458138
1793.504253	50.099520	63.463143
1792.561191	52.958634	63.468148
1792.031970	55.524946	63.473153
1791.622375	55.372470	63.478158
1790.853271	48.738924	63.483162
1790.166316	39.990222	63.488167
1789.630646	50.469263	63.493172
1789.119715	55.926430	63.498177
1788.112981	50.431352	63.503182
1787.409992	57.259452	63.508186
1786.979215	49.895655	63.513191
1785.736366	57.612169	63.518196
1785.621209	51.434603	63.523201
1784.934068	58.611853	63.528206
1784.090968	64.274740	63.533210
1783.679862	48.344814	63.538215
1783.175798	57.785919	63.543220
1781.871075	53.186581	63.548225
1781.284654	60.086060	63.553230
1780.649960	64.604080	63.558234
1780.373346	48.397326	63.563239
1779.741854	54.312039	63.568244
1779.322963	57.062685	63.573249
1778.536103	56.834502	63.578254
1777.257026	63.374040	63.583258
1776.852473	55.023619	63.588263
1776.538866	62.422256	63.593268
1775.790727	62.219465	63.598273
1774.782281	60.083632	63.603278
1774.079700	65.766785	63.608282
1774.116758	49.926540	63.613287
1772.843885	52.744995	63.618292
1771.877895	57.467018	63.623297
1771.856621	49.494134	63.628302
1771.470249	60.428876	63.633306
1770.461833	55.173773	63.638311
1769.695534	60.688845	63.643316
1769.088936	48.927967	63.648321
1768.427473	60.382643	63.653326
1767.751147	60.658891	63.658330
1767.413834	47.208882	63.663335
1767.069074	58.775691	63.668340
1766.033121	54.098985	63.673345
1765.796925	49.719478	63.678350
1764.193666	53.940300	63.683354
1763.476862	51.294525	63.688359
1763.247459	55.352360	63.693364
1762.275503	56.728981	63.698369
1761.619304	54.013656	63.703374
1761.733309	58.262962	63.708378
1760.710924	48.689159	63.713383
1759.641760	60.076118	63.718388
1758.914033	59.658774	63.723393
1758.244855	50.419968	63.728398
1757.452989	57.326844	63.733402
1757.704277	45.784550	63.738407
1756.775605	57.149195	63.743412
1756.009154	54.268452	63.748417
1755.273845	50.389266	63.753422
1754.997232	47.364498	63.758426
1754.226667	56.346450	63.763431
1753.652407	67.456119	63.768436
1753.106802	55.747058	63.773441
1751.839222	52.698317	63.778446
1750.776369	63.981775	63.783450
1750.616195	46.802466	63.788455
1750.125638	55.296817	63.793460
1749.247639	55.483671	63.798465
1749.070004	52.280754	63.803470
1748.032799	53.442234	63.808474
1747.737032	47.632409	63.813479
1747.279524	56.616685	63.818484
1746.469296	49.623826	63.823489
1745.153807	45.617588	63.828494
1744.129447	60.432096	63.833498
1744.458789	48.533622	63.838503
1743.310017	56.539568	63.843508
1742.275700	55.883911	63.848513
1741.816468	49.407753	63.853518
1741.272164	57.013342	63.858522
1740.759928	52.225085	63.863527
1739.826603	50.212958	63.868532
1739.540087	53.502412	63.873537
1739.073943	50.025192	63.878542
1738.005688	58.403135	63.883546
1737.832301	50.657843	63.888551
1737.512243	53.605690	63.893556
1736.824656	53.692919	63.898561
1735.445567	42.600382	63.903566
1734.652307	48.689029	63.908570
1734.009652	57.466164	63.913575
1733.172794	59.737565	63.918580
1732.991990	60.742535	63.923585
1732.408829	59.882762	63.928590
1731.564021	53.622387	63.933594
1731.514413	49.903967	63.938599
1730.817632	58.973557	63.943604
1729.964610	49.573146	63.948609
1729.042915	53.132220	63.953614
1727.973692	56.227439	63.958618
1727.486942	49.087016	63.963623
1726.864547	49.053506	63.968628
1726.685662	57.146693	63.973633
1726.182744	56.416105	63.978638
1724.895189	59.657968	63.983642
1724.159748	44.990699	63.988647
1723.388999	52.004615	63.993652
1722.772644	55.950442	63.998657
1722.536853	57.929257	64.003662
1721.479896	61.230693	64.008666
1721.383902	44.194167	64.013671
1720.828342	56.491480	64.018676
1720.318620	57.364185	64.023681
1719.404178	47.531980	64.028686
1718.162574	55.489599	64.033690
1717.398201	55.387176	64.038695
1716.932275	56.055803	64.043700
1716.086265	54.875077	64.048705
1715.827782	53.818658	64.053710
1715.299038	57.337403	64.058714
1714.831220	50.275979	64.063719
1714.370430	53.157869	64.068724
1713.348463	50.327186	64.073729
1712.183094	48.293577	64.078734
1711.421111	60.215242	64.083738
1711.048735	50.186554	64.088743
1710.430952	54.504776	64.093748
1709.852071	51.040737	64.098753
1709.622932	44.845016	64.103758
1709.116223	59.307649	64.108762
1708.284848	50.370594	64.113767
1706.745102	53.532670	64.118772
1706.139354	55.240659	64.123777
1705.570901	46.610360	64.128782
1704.801642	50.892716	64.133786
1704.856237	45.270105	64.138791
1704.224233	51.211720	64.143796
1703.695394	55.561549	64.148801
1703.275756	47.301858	64.153806
1701.821183	64.356212	64.158810
1701.467272	45.728481	64.163815
1700.626415	62.455114	64.168820
1699.878760	52.135946	64.173825
1699.341082	49.939564	64.178830
1698.830930	51.580330	64.183834
1697.841458	47.093396	64.188839
1696.570126	56.706842	64.193844
1696.862983	53.142189	64.198849
1696.246171	51.089266	64.203854
1695.098402	56.909377	64.208858
1694.848433	56.734716	64.213863
1694.255384	53.624596	64.218868
1693.731550	57.932631	64.223873
1693.070109	51.159015	64.228878
1691.673362	59.975511	64.233882
1691.134872	55.937347	64.238887
1690.579360	53.989808	64.243892
1689.779717	60.765470	64.248897
1689.302461	55.031789	64.253902
1688.734830	57.733532	64.258906
1688.456015	50.755636	64.263911
1688.082414	61.388726	64.268916
1686.995956	56.125556	64.273921
1686.212547	56.423564	64.278926
1685.399751	56.341458	64.283930
1684.925720	55.101656	64.288935
1684.313092	54.897868	64.293940
1683.206113	53.324936	64.298945
1683.110587	48.721244	64.303950
1681.833478	54.809489	64.308954
1681.534441	49.175240	64.313959
1680.480694	49.315914	64.318964
1680.197013	46.617137	64.323969
1680.188589	38.536570	64.328974
1679.239430	47.389202	64.333978
1678.050950	42.743075	64.338983
1677.294717	40.611378	64.343988
1676.660912	49.464383	64.348993
1676.102125	44.454878	64.353998
1675.431980	48.499144	64.359002
1675.303187	42.538229	64.364007
1674.779195	47.814553	64.369012
1673.799902	51.857464	64.374017
1673.105250	45.022899	64.379022
1671.758389	49.028001	64.384026
1671.591040	44.733768	64.389031
1671.006083	46.973057	64.394036
1670.562959	49.495749	64.399041
1670.127428	44.260083	64.404046
1668.673904	45.885123	64.409050
1668.148449	46.552175	64.414055
1667.509359	50.999947	64.419060
1666.921957	50.107747	64.424065
1666.988530	38.791925	64.429070
1665.783200	52.346800	64.434074
1665.047023	46.119663	64.439079
1663.864921	36.978146	64.444084
1663.431893	42.948083	64.449089
1663.265046	37.907864	64.454094
1662.418927	47.974175	64.459098
1662.211327	47.305500	64.464103
1661.623774	39.815254	64.469108
1660.087881	42.263948	64.474113
1659.686391	39.757357	64.479118
1658.905042	39.030011	64.484122
1658.715437	36.049785	64.489127
1658.366109	47.440690	64.494132
1657.107632	49.329648	64.499137
1656.329492	49.374511	64.504142
1655.427380	45.805713	64.509146
1655.130974	33.773260	64.514151
1654.758776	29.314453	64.519156
1654.067333	35.842685	64.524161
1652.891390	31.227700	64.529166
1651.770061	43.036131	64.534170
1651.417066	40.051898	64.539175
1651.499069	41.516602	64.544180
1650.423975	37.543194	64.549185
1650.219506	37.145264	64.554190
1649.746401	45.280450	64.559194
1648.754833	38.247056	64.564199
1648.064979	34.928400	64.569204
1647.150356	45.404569	64.574209
1646.547491	41.878126	64.579214
1645.788277	44.514113	64.584218
1645.604144	38.882121	64.589223
1644.094062	35.532913	64.594228
1643.373786	38.433955	64.599233
1643.101277	37.625781	64.604238
1642.221204	43.818126	64.609242
1641.996810	35.588943	64.614247
1641.587216	42.319993	64.619252
1640.849562	36.025293	64.624257
1640.250278	42.078414	64.629262
1639.371309	38.518563	64.634266
1638.395093	47.618359	64.639271
1637.736738	45.912678	64.644276
1636.641551	43.855340	64.649281
1636.968716	34.267495	64.654286
1636.749560	48.045763	64.659290
1636.012485	46.524479	64.664295
1634.903135	45.992752	64.669300
1634.069119	48.572816	64.674305
1633.691520	44.274141	64.679310
1631.980259	52.869383	64.684314
1631.514403	40.133710	64.689319
1631.089093	40.792745	64.694324
1630.734771	44.884619	64.699329
1630.124143	38.260655	64.704334
1629.489090	37.470653	64.709338
1629.036869	40.877902	64.714343
1628.493176	36.351724	64.719348
1627.107655	42.203317	64.724353
1626.741912	51.767540	64.729358
1625.936327	42.518917	64.734362
1625.397051	50.647274	64.739367
1625.006997	45.926372	64.744372
1624.466320	53.066189	64.749377
1623.562271	53.358149	64.754382
1622.655443	44.778479	64.759386
1622.237293	45.851123	64.764391
1622.072505	50.234593	64.769396
1621.027298	53.062681	64.774401
1619.840995	50.840050	64.779406
1619.147636	58.032511	64.784410
1618.781559	45.064940	64.789415
1618.404711	46.548922	64.794420
1617.517370	49.640518	64.799425
1617.647019	41.233664	64.804430
1616.460459	48.794638	64.809434
1615.707920	54.028432	64.814439
1615.198575	42.427210	64.819444
1613.867775	39.754446	64.824449
1613.201427	45.341981	64.829454
1612.096099	43.972250	64.834458
1612.153781	51.080085	64.839463
1611.755921	45.149308	64.844468
1610.942503	53.507304	64.849473
1610.614040	49.043128	64.854478
1609.979951	50.665752	64.859482
1608.951034	47.024074	64.864487
1608.301724	45.534588	64.869492
1607.084818	53.057811	64.874497
1607.092215	42.837930	64.879502
1606.417165	59.164488	64.884506
1606.029486	54.663986	64.889511
1604.983685	47.970388	64.894516
1603.955571	45.038226	64.899521
1603.572361	44.998284	64.904526
1602.862440	51.220382	64.909530
1602.337048	50.288383	64.914535
1602.104544	51.326805	64.919540
1601.265482	51.868650	64.924545
1600.489054	47.286409	64.929550
1599.832909	56.210789	64.934554
1598.989983	43.924543	64.939559
1598.749615	49.404980	64.944564
1597.247449	46.034040	64.949569
1596.505232	40.768268	64.954574
1596.037191	50.847068	64.959578
1595.727452	45.493660	64.964583
1595.377281	49.662152	64.969588
1594.911245	49.852994	64.974593
1594.604857	39.425923	64.979598
1593.237996	53.033293	64.984602
1592.515610	48.920292	64.989607
1592.080737	46.166699	64.994612
1590.712747	48.429483	64.999617
1589.946029	48.546670	65.004622
1588.925209	49.686685	65.009626
1588.824120	39.274307	65.014631
1588.790600	44.920578	65.019636
1588.085874	48.992435	65.024641
1587.949534	40.252521	65.029646
1587.086959	42.261540	65.034650
1586.255618	53.054085	65.039655
1585.703702	53.755321	65.044660
1584.137498	51.626181	65.049665
1583.660639	42.088801	65.054670
1583.170027	44.666360	65.059674
1582.411620	48.459737	65.064679
1581.851086	41.048801	65.069684
1581.222216	44.304348	65.074689
1580.801104	41.323065	65.079694
1579.931821	46.080243	65.084698
1579.204922	44.544744	65.089703
1578.701272	38.851561	65.094708
1577.992407	46.775051	65.099713
1577.639246	36.841126	65.104718
1576.283774	51.511149	65.109722
1575.387811	41.884240	65.114727
1574.881570	44.500554	65.119732
1573.998825	50.387412	65.124737
1573.970136	42.486693	65.129742
1573.772490	49.991488	65.134746
1573.134563	42.717432	65.139751
1572.649760	42.780370	65.144756
1571.564268	43.618425	65.149761
1570.818903	42.079555	65.154766
1569.616756	51.406083	65.159770
1568.659907	42.474835	65.164775
1568.575720	42.002606	65.169780
1568.138982	50.911051	65.174785
1567.497436	44.795071	65.179790
1567.068518	46.845582	65.184794
1566.625401	45.482620	65.189799
1565.309791	41.670469	65.194804
1564.543749	49.696089	65.199809
1564.108435	40.260927	65.204814
1563.408155	45.882248	65.209818
1562.849527	40.059031	65.214823
1561.987328	42.973181	65.219828
1561.164856	43.663792	65.224833
1560.747065	40.726140	65.229838
1560.183868	49.944841	65.234842
1559.925092	48.513165	65.239847
1559.109927	36.903786	65.244852
1558.001905	47.106351	65.249857
1557.582106	43.486188	65.254862
1557.042848	50.105384	65.259866
1555.772518	44.504061	65.264871
1554.900303	50.195283	65.269876
1554.296590	52.283032	65.274881
1554.170172	41.026270	65.279886
1553.708065	48.554161	65.284890
1553.047538	36.396658	65.289895
1553.107239	39.161174	65.294900
1551.382265	45.062009	65.299905
1550.986128	39.894230	65.304910
1550.131458	45.219959	65.309914
1549.275494	45.658849	65.314919
1549.136381	33.700779	65.319924
1548.038622	45.295761	65.324929
1547.308320	41.061030	65.329934
1546.834591	44.419669	65.334938
1546.274704	49.327972	65.339943
1546.250999	44.479489	65.344948
1544.697935	47.400916	65.349953
1544.172377	41.436829	65.354958
1543.445451	42.087032	65.359962
1543.203672	46.730320	65.364967
1542.569740	47.321593	65.369972
1541.625343	43.478856	65.374977
1541.056435	45.261451	65.379982
1540.427240	42.428358	65.384986
1539.468707	45.070813	65.389991
1538.948507	44.103309	65.394996
1538.523094	42.220292	65.400001
1537.407166	40.339762	65.405006
1536.456590	45.289645	65.410010
1536.183134	35.633229	65.415015
1535.918293	39.720354	65.420020
1535.319366	43.401667	65.425025
1534.705249	43.308539	65.430030
1533.560555	46.425284	65.435034
1532.841398	48.473033	65.440039
1532.908605	39.850597	65.445044
1531.701107	41.565929	65.450049
1530.764743	38.746955	65.455054
1530.031189	47.051274	65.460058
1529.521304	38.608850	65.465063
1529.365969	45.029846	65.470068
1528.828843	44.840906	65.475073
1528.412844	32.478978	65.480078
1527.190134	44.838151	65.485082
1526.248332	42.827454	65.490087
1526.294008	40.030631	65.495092
1524.632727	41.508987	65.500097
1523.987483	36.932739	65.505102
1523.364117	44.697570	65.510106
1523.049578	48.727939	65.515111
1522.959390	38.697045	65.520116
1522.115295	39.468376	65.525121
1521.869676	35.654962	65.530126
1520.347048	45.198012	65.535130
1519.659119	42.397912	65.540135
1519.180167	42.595551	65.545140
1518.498324	45.534672	65.550145
1517.652771	37.964042	65.555150
1516.889787	48.594346	65.560154
1516.272307	36.272320	65.565159
1515.910394	37.965256	65.570164
1515.091274	44.570579	65.575169
1515.279386	39.656901	65.580174
1513.908555	44.847039	65.585178
1512.895288	37.859733	65.590183
1512.679056	36.269915	65.595188
1512.068774	43.597423	65.600193
1511.675275	42.699679	65.605198
1510.365544	47.571023	65.610202
1509.369191	41.161357	65.615207
1509.281702	45.122530	65.620212
1508.304873	47.144998	65.625217
1508.086151	35.010349	65.630222
1507.885439	36.706055	65.635226
1506.807685	37.156548	65.640231
1506.079790	31.465905	65.645236
1505.134863	47.483679	65.650241
1504.841864	40.744622	65.655246
1503.927158	39.642696	65.660250
1502.896837	47.388621	65.665255
1503.008475	39.333146	65.670260
1502.119007	47.979219	65.675265
1501.919868	41.696762	65.680270
1500.430826	39.298369	65.685274
1499.683062	45.695235	65.690279
1499.100398	39.918434	65.695284
1498.449090	51.559184	65.700289
1498.312011	41.583052	65.705294
1497.874953	45.068336	65.710298
1496.677395	44.632689	65.715303
1496.086970	40.664333	65.720308
1495.431806	41.348878	65.725313
1494.845015	47.458388	65.730318
1494.133451	44.524855	65.735322
1493.313659	36.141153	65.740327
1492.612290	33.969258	65.745332
1492.059516	47.732723	65.750337
1491.830489	36.922795	65.755342
1491.071666	45.194865	65.760346
1489.652729	47.628225	65.765351
1489.538195	43.997411	65.770356
1488.980817	44.820961	65.775361
1488.570565	43.862804	65.780366
1487.203353	42.712945	65.785370
1486.423154	43.541943	65.790375
1486.205802	48.695446	65.795380
1485.559373	44.310209	65.800385
1485.199050	33.746658	65.805390
1484.174073	41.698321	65.810394
1483.326961	39.913869	65.815399
1482.657894	37.459295	65.820404
1482.238825	40.545901	65.825409
1482.101871	31.028659	65.830414
1480.917279	34.817246	65.835418
1479.868437	49.700351	65.840423
1479.537030	38.323214	65.845428
1478.872649	36.271602	65.850433
1478.703058	33.231445	65.855438
1477.972595	40.369895	65.860442
1476.905903	43.089485	65.865447
1476.682212	36.691086	65.870452
1475.867836	41.431682	65.875457
1474.809075	41.500696	65.880462
1473.728151	35.924515	65.885466
1473.523378	35.126097	65.890471
1473.316087	39.388585	65.895476
1472.465032	42.431880	65.900481
1471.537892	33.702545	65.905486
1470.486678	37.957225	65.910490
1470.151370	43.736608	65.915495
1470.126585	31.205291	65.920500
1469.296815	42.510119	65.925505
1468.388855	35.894035	65.930510
1467.491897	38.774313	65.935514
1466.884382	34.105353	65.940519
1466.337002	36.106894	65.945524
1465.811748	36.352902	65.950529
1465.262336	31.476012	65.955534
1464.639324	38.466499	65.960538
1463.746415	39.608310	65.965543
1463.667090	41.828783	65.970548
1462.042742	43.260307	65.975553
1461.237646	38.427204	65.980558
1460.546084	35.337538	65.985562
1460.085728	37.553911	65.990567
1459.605869	33.823465	65.995572
1459.218995	48.642370	66.000577
1458.960388	35.402303	66.005582
1458.022336	41.473024	66.010586
1456.789432	40.918432	66.015591
1456.820277	40.010027	66.020596
1456.082206	47.012498	66.025601
1454.807568	36.852888	66.030606
1454.126954	44.625251	66.035610
1453.748653	42.116588	66.040615
1453.479049	36.212775	66.045620
1452.753382	48.112930	66.050625
1452.013452	37.414171	66.055630
1450.969683	36.211350	66.060634
1450.334207	46.613239	66.065639
1449.937944	41.443923	66.070644
1449.494840	46.218562	66.075649
1448.532534	43.673405	66.080654
1447.574957	35.217004	66.085658
1447.075680	49.762034	66.090663
1446.972592	33.201380	66.095668
1445.932046	45.230428	66.100673
1444.984436	37.267612	66.105678
1444.532893	28.697673	66.110682
1443.553195	43.213395	66.115687
1443.998430	35.909161	66.120692
1442.710299	35.773367	66.125697
1441.884104	32.561600	66.130702
1441.417882	35.039108	66.135706
1440.613691	35.239567	66.140711
1440.406252	25.476491	66.145716
1439.255294	30.513441	66.150721
1438.061266	36.061869	66.155726
1437.872820	39.870350	66.160730
1437.505548	35.040212	66.165735
1436.851893	30.112088	66.170740
1435.708203	31.028834	66.175745
1434.640861	32.723510	66.180750
1434.229206	32.885237	66.185754
1433.951642	40.967284	66.190759
1433.874126	35.490266	66.195764
1433.016965	42.536899	66.200769
1431.867521	41.011832	66.205774
1430.985653	45.039337	66.210778
1430.568187	42.191546	66.215783
1430.400157	35.629765	66.220788
1429.832938	33.657342	66.225793
1428.940435	31.402303	66.230798
1428.488465	32.898248	66.235802
1427.573000	33.691991	66.240807
1426.691553	26.535545	66.245812
1425.686785	38.749719	66.250817
1425.646511	37.871543	66.255822
1425.225774	37.512736	66.260826
1424.283485	41.622386	66.265831
1423.370264	32.208033	66.270836
1422.313923	38.543572	66.275841
1421.905537	35.050936	66.280846
1421.526038	38.224301	66.285850
1421.109480	41.515522	66.290855
1420.232253	35.498555	66.295860
1419.170910	37.618066	66.300865
1418.827037	40.367872	66.305870
1418.369118	42.833026	66.310874
1417.680291	34.671395	66.315879
1416.889538	34.015006	66.320884
1416.310720	44.720134	66.325889
1415.779215	37.284135	66.330894
1414.569750	41.616029	66.335898
1413.575192	48.451117	66.340903
1413.258583	34.193673	66.345908
1412.431928	40.032231	66.350913
1412.214830	35.630819	66.355918
1411.915270	41.617414	66.360922
1411.229533	35.670940	66.365927
1410.637817	33.577835	66.370932
1409.488302	32.434417	66.375937
1409.125284	33.722260	66.380942
1408.569563	37.494500	66.385946
1407.276959	42.131352	66.390951
1406.869855	32.404745	66.395956
1405.803739	36.926748	66.400961
1405.850687	37.752030	66.405966
1405.332731	35.371232	66.410970
1404.004730	33.298966	66.415975
1403.447821	25.204687	66.420980
1403.016110	37.837141	66.425985
1402.660591	34.012827	66.430990
1402.069790	29.965712	66.435994
1400.810338	38.000400	66.440999
1400.471495	26.348505	66.446004
1399.539359	36.490039	66.451009
1399.293549	40.760230	66.456014
1398.279957	41.733586	66.461018
1397.190968	38.678725	66.466023
1397.004708	32.410010	66.471028
1396.106801	34.298545	66.476033
1395.717056	31.935218	66.481038
1395.427530	41.446327	66.486042
1394.433810	37.251942	66.491047
1393.927737	29.381398	66.496052
1393.173085	35.232170	66.501057
1392.539978	35.585223	66.506062
1391.855682	33.200907	66.511066
1390.898971	39.577391	66.516071
1390.628270	26.183152	66.521076
1389.973898	40.098385	66.526081
1388.724332	41.408879	66.531086
1388.083331	25.741160	66.536090
1387.384291	40.748450	66.541095
1387.382048	31.440047	66.546100
1386.825544	41.506110	66.551105
1386.167048	43.645179	66.556110
1385.215232	33.948391	66.561114
1384.319364	32.860862	66.566119
1384.253753	30.553248	66.571124
1382.798193	34.692457	66.576129
1382.279381	36.850324	66.581134
1381.642830	38.139072	66.586138
1381.307923	45.492215	66.591143
1380.941138	34.546513	66.596148
1379.909502	35.670980	66.601153
1379.137982	35.448367	66.606158
1378.784797	27.556679	66.611162
1378.005619	37.700714	66.616167
1377.428243	32.142309	66.621172
1376.466987	44.307006	66.626177
1375.741319	43.105690	66.631182
1375.531755	37.957177	66.636186
1374.490442	36.998427	66.641191
1374.207569	32.135963	66.646196
1373.175732	39.241916	66.651201
1372.480161	33.543026	66.656206
1372.381564	33.919929	66.661210
1371.063405	40.432724	66.666215
1370.255720	42.795788	66.671220
1369.758685	32.566240	66.676225
1369.303548	37.901046	66.681230
1369.065102	30.470519	66.686234
1367.909282	39.392352	66.691239
1367.453004	24.680887	66.696244
1366.486716	29.013566	66.701249
1366.137889	28.260135	66.706254
1365.498540	25.184277	66.711258
1364.212986	32.180749	66.716263
1363.922023	24.670264	66.721268
1363.394114	33.870752	66.726273
1362.942021	35.868204	66.731278
1362.655784	26.180748	66.736282
1361.181691	30.108446	66.741287
1360.617054	37.092824	66.746292
1360.009623	36.104532	66.751297
1359.465602	32.396925	66.756302
1358.538704	26.916168	66.761306
1357.450331	31.482726	66.766311
1357.555801	27.007969	66.771316
1356.763091	26.713036	66.776321
1356.438387	18.074079	66.781326
1355.423180	24.448827	66.786330
1354.495938	28.242287	66.791335
1354.286366	23.776611	66.796340
1353.790832	30.027749	66.801345
1353.033292	25.641298	66.806350
1351.997547	27.077091	66.811354
1351.090929	30.149753	66.816359
1351.059712	29.273293	66.821364
1350.429083	29.269567	66.826369
1349.156234	32.780500	66.831374
1348.641923	23.947752	66.836378
1348.040423	27.741471	66.841383
1348.043225	23.861784	66.846388
1347.022505	33.079114	66.851393
1345.923772	32.318742	66.856398
1345.418377	23.063527	66.861402
1344.784677	26.505970	66.866407
1344.764698	22.916913	66.871412
1343.360940	28.834613	66.876417
1342.338340	27.883942	66.881422
1342.120093	30.366198	66.886426
1341.398828	38.939834	66.891431
1341.292230	30.315085	66.896436
1340.510963	33.356785	66.901441
1339.169703	36.116922	66.906446
1338.558848	32.989231	66.911450
1338.224356	30.531974	66.916455
1337.902874	25.166294	66.921460
1337.429236	35.663889	66.926465
1336.452603	31.089919	66.931470
1335.762281	31.403196	66.936474
1334.756643	40.304320	66.941479
1333.882809	34.938138	66.946484
1333.276600	34.761799	66.951489
1332.785102	32.520316	66.956494
1332.683458	30.089121	66.961498
1331.627071	36.270154	66.966503
1331.604885	27.316594	66.971508
1330.415190	32.648332	66.976513
1329.700557	26.285431	66.981518
1329.369103	21.747672	66.986522
1328.230190	39.141464	66.991527
1327.451826	27.937934	66.996532
1326.782752	38.433486	67.001537
1326.090191	32.877638	67.006542
1326.425500	29.181634	67.011546
1325.378916	46.090820	67.016551
1324.098380	32.969100	67.021556
1323.692829	34.323640	67.026561
1322.993395	38.582372	67.031566
1322.728769	30.496842	67.036570
1321.223953	39.918881	67.041575
1320.827694	25.962719	67.046580
1320.226375	29.038893	67.051585
1319.568132	33.130225	67.056590
1319.829188	34.279438	67.061594
1318.591423	35.446161	67.066599
1317.982069	23.335820	67.071604
1317.375447	29.487928	67.076609
1316.332059	39.789100	67.081614
1315.480132	41.843819	67.086618
1315.034182	39.743333	67.091623
1314.607482	30.876162	67.096628
1314.079095	32.986677	67.101633
1313.331904	33.152881	67.106638
1312.414985	34.166094	67.111642
1311.443865	41.410650	67.116647
1311.252421	35.082846	67.121652
1310.595873	27.337177	67.126657
1310.173348	31.450959	67.131662
1309.162889	18.690028	67.136666
1308.625117	36.918661	67.141671
1307.818773	37.168389	67.146676
1307.718929	29.548679	67.151681
1306.487990	37.952614	67.156686
1306.099957	28.394894	67.161690
1305.149433	36.225961	67.166695
1304.415435	30.782366	67.171700
1303.126523	28.153578	67.176705
1302.413972	33.153997	67.181710
1302.996624	25.383202	67.186714
1302.219762	37.001349	67.191719
1301.893414	26.691071	67.196724
1300.551839	42.302004	67.201729
1299.674877	33.288801	67.206734
1299.268661	32.025680	67.211738
1299.018708	33.503720	67.216743
1298.191216	29.798621	67.221748
1296.992143	30.479803	67.226753
1296.320221	28.711720	67.231758
1295.795940	24.083197	67.236762
1295.552260	37.215619	67.241767
1295.218777	33.386244	67.246772
1293.883934	25.828850	67.251777
1293.353743	28.925260	67.256782
1292.827995	21.559354	67.261786
1291.987931	34.469624	67.266791
1291.435846	28.449903	67.271796
1290.784768	32.462830	67.276801
1289.991680	35.798163	67.281806
1289.773619	30.655746	67.286810
1288.545649	30.442655	67.291815
1287.666343	31.314276	67.296820
1286.933582	32.843850	67.301825
1286.559479	40.827707	67.306830
1286.549708	37.959279	67.311834
1285.817602	37.260490	67.316839
1284.722229	35.241188	67.321844
1284.200944	28.003883	67.326849
1283.283055	34.506690	67.331854
1282.910091	28.961545	67.336858
1281.904290	39.920654	67.341863
1281.116046	40.345711	67.346868
1280.686869	40.363589	67.351873
1280.491453	36.387683	67.356878
1279.909948	30.229138	67.361882
1278.810154	39.952657	67.366887
1278.364253	36.087541	67.371892
1278.068545	35.418717	67.376897
1276.575724	36.091421	67.381902
1275.772422	27.034981	67.386906
1275.557436	42.146672	67.391911
1274.935867	28.924943	67.396916
1274.570736	37.669049	67.401921
1273.465310	31.732582	67.406926
1272.832755	32.684825	67.411930
1271.709835	39.590825	67.416935
1271.532754	29.622677	67.421940
1271.229006	30.582564	67.426945
1270.007036	39.560682	67.431950
1269.569587	31.016934	67.436954
1268.737206	32.494542	67.441959
1268.436705	36.629930	67.446964
1267.963885	40.639753	67.451969
1266.900920	36.372855	67.456974
1266.638815	34.580618	67.461978
1265.609573	37.073558	67.466983
1264.884441	32.814447	67.471988
1264.191756	40.968811	67.476993
1263.366552	29.755409	67.481998
1262.853297	20.424200	67.487002
1262.394133	32.378191	67.492007
1261.838206	34.221856	67.497012
1261.219888	25.497136	67.502017
1260.351802	36.992598	67.507022
1259.825510	19.445878	67.512026
1258.894164	30.405764	67.517031
1258.008229	30.407963	67.522036
1257.656126	27.562431	67.527041
1256.918122	33.541475	67.532046
1256.686838	28.612480	67.537050
1255.724262	40.901993	67.542055
1254.910882	31.126487	67.547060
1254.570519	30.404842	67.552065
1254.002339	36.557159	67.557070
1253.406979	29.170789	67.562074
1252.077553	35.152411	67.567079
1251.398756	34.175495	67.572084
1250.723129	35.863152	67.577089
1250.340617	31.235750	67.582094
1250.358047	21.359685	67.587098
1248.864777	28.755090	67.592103
1248.307728	29.892454	67.597108
1247.643943	33.558901	67.602113
1247.333101	26.068946	67.607118
1246.761487	33.737275	67.612122
1245.614514	45.687105	67.617127
1245.112604	32.946257	67.622132
1244.904598	33.819960	67.627137
1243.804727	44.071790	67.632142
1243.118689	31.118946	67.637146
1241.935728	43.542858	67.642151
1241.942466	35.564002	67.647156
1241.748753	35.929226	67.652161
1240.726555	37.974773	67.657166
1240.064970	37.118126	67.662170
1239.001736	32.956942	67.667175
1238.512347	37.346298	67.672180
1237.468383	36.340718	67.677185
1236.624568	38.018853	67.682190
1236.417094	34.372880	67.687194
1235.749391	43.439496	67.692199
1235.553960	37.716315	67.697204
1235.120710	32.302192	67.702209
1234.030727	39.502593	67.707214
1233.606657	32.623582	67.712218
1232.672424	30.187593	67.717223
1231.839054	24.788213	67.722228
1231.248632	34.310895	67.727233
1230.207641	36.343664	67.732238
1230.037854	37.167136	67.737242
1229.685864	43.583129	67.742247
1228.992831	36.360530	67.747252
1228.166702	36.810551	67.752257
1227.147295	37.884246	67.757262
1227.074905	34.148984	67.762266
1225.469774	41.663120	67.767271
1224.917743	32.850596	67.772276
1224.307342	32.274399	67.777281
1223.980459	36.734110	67.782286
1223.867895	26.099694	67.787290
1222.641288	34.638590	67.792295
1222.046236	33.826562	67.797300
1221.465004	33.217342	67.802305
1220.878737	33.402139	67.807310
1220.291606	29.304027	67.812314
1219.183029	31.276584	67.817319
1218.525880	40.016668	67.822324
1218.548642	32.628208	67.827329
1217.137148	38.487278	67.832334
1216.728106	30.677049	67.837338
1215.598028	36.669565	67.842343
1215.077461	38.062912	67.847348
1214.838415	36.918303	67.852353
1214.264169	41.934598	67.857358
1214.017701	37.115255	67.862362
1212.723606	36.133693	67.867367
1212.165207	35.181796	67.872372
1211.801745	29.827545	67.877377
1210.312822	39.956745	67.882382
1209.998092	34.132691	67.887386
1209.390880	41.256328	67.892391
1209.009145	33.758727	67.897396
1208.530144	30.026627	67.902401
1207.323598	28.889219	67.907406
1207.077569	32.128115	67.912410
1206.154074	41.664348	67.917415
1205.745611	33.024542	67.922420
1204.828694	36.959915	67.927425
1204.169398	44.082375	67.932430
1203.875584	34.563311	67.937434
1202.887824	35.199894	67.942439
1201.781857	38.398926	67.947444
1201.636842	37.174709	67.952449
1200.914615	44.556339	67.957454
1200.384016	36.987793	67.962458
1199.518662	45.529180	67.967463
1198.840128	38.321632	67.972468
1198.232957	28.049730	67.977473
1197.467665	34.815302	67.982478
1197.379694	39.170789	67.987482
1196.021719	50.666911	67.992487
1195.368112	37.420339	67.997492
1195.022044	38.103112	68.002497
1194.241082	49.365544	68.007502
1193.906963	43.759040	68.012506
1192.820898	38.666364	68.017511
1192.153184	44.951218	68.022516
1191.707900	36.219498	68.027521
1190.852258	43.800544	68.032526
1190.716638	42.656836	68.037530
1189.569490	46.857490	68.042535
1189.001262	42.289595	68.047540
1188.756888	39.340207	68.052545
1187.679988	38.447120	68.057550
1186.841209	33.569013	68.062554
1186.153565	43.988694	68.067559
1185.458655	45.531200	68.072564
1185.177314	43.901305	68.077569
1184.226512	39.709648	68.082574
1183.855019	36.689014	68.087578
1183.390094	43.460441	68.092583
1182.747458	41.030135	68.097588
1181.605303	29.684247	68.102593
1180.708706	40.362664	68.107598
1180.256384	29.919482	68.112602
1180.016920	33.848048	68.117607
1179.442341	40.204824	68.122612
1178.559334	34.665120	68.127617
1177.436762	36.586304	68.132622
1177.330695	35.434743	68.137626
1176.785493	30.238713	68.142631
1175.748102	35.506868	68.147636
1174.905008	33.546843	68.152641
1174.229393	44.472396	68.157646
1174.388391	29.548021	68.162650
1173.345671	33.594874	68.167655
1172.502614	42.785584	68.172660
1172.044704	40.228130	68.177665
1171.180160	42.832109	68.182670
1170.116203	43.044003	68.187674
1169.173350	36.906687	68.192679
1168.746948	39.453599	68.197684
1168.338063	26.649102	68.202689
1167.865499	47.557683	68.207694
1167.576368	47.841893	68.212698
1167.271264	38.146434	68.217703
1166.222326	41.128250	68.222708
1165.499146	29.718891	68.227713
1164.197376	37.935448	68.232718
1163.715687	30.428525	68.237722
1162.907236	37.614136	68.242727
1162.539406	38.451763	68.247732
1162.261757	30.056095	68.252737
1161.607681	39.513219	68.257742
1160.576983	36.053377	68.262746
1159.920555	27.956077	68.267751
1159.637621	34.411550	68.272756
1158.525871	33.214933	68.277761
1157.233796	33.676004	68.282766
1156.905927	31.785430	68.287770
1156.362904	33.351094	68.292775
1155.953710	41.578662	68.297780
1155.685787	35.245698	68.302785
1155.195450	38.402028	68.307790
1154.163327	37.172248	68.312794
1153.229811	36.316296	68.317799
1152.970277	37.166662	68.322804
1151.838874	34.134430	68.327809
1150.681199	44.201516	68.332814
1150.625590	35.609682	68.337818
1150.250793	42.702672	68.342823
1149.776064	43.366489	68.347828
1149.038218	41.880170	68.352833
1147.943028	41.819494	68.357838
1147.441318	40.499047	68.362842
1147.161346	41.262777	68.367847
1145.634902	45.271461	68.372852
1145.357838	31.690632	68.377857
1144.688755	36.662097	68.382862
1144.544909	30.651604	68.387866
1143.583731	32.034617	68.392871
1142.562996	32.942975	68.397876
1142.192607	26.553774	68.402881
1141.495086	34.246874	68.407886
1140.562548	34.521457	68.412890
1140.040560	35.382029	68.417895
1139.211472	27.438355	68.422900
1139.095363	26.012425	68.427905
1138.536006	31.926809	68.432910
1137.837386	29.505422	68.437914
1137.136726	37.016096	68.442919
1136.489051	29.494581	68.447924
1135.372151	30.165922	68.452929
1134.439021	33.263371	68.457934
1133.708542	26.330621	68.462938
1133.630448	23.856271	68.467943
1133.103189	36.470812	68.472948
1132.194274	26.513436	68.477953
1131.302031	34.176009	68.482958
1130.665905	27.215636	68.487962
1130.493810	24.883972	68.492967
1129.907866	31.368717	68.497972
1128.658550	36.410397	68.502977
1127.891495	35.234662	68.507982
1127.683269	30.489677	68.512986
1127.177362	32.531995	68.517991
1126.227763	29.600170	68.522996
1125.496230	18.736218	68.528001
1124.574489	24.560007	68.533006
1124.429041	25.357536	68.538010
1124.252057	31.687346	68.543015
1123.035725	32.185273	68.548020
1121.966071	31.019824	68.553025
1121.338542	36.571315	68.558030
1121.120543	30.496925	68.563034
1120.607755	33.059161	68.568039
1119.700920	34.985478	68.573044
1118.923203	30.157611	68.578049
1118.496043	34.082918	68.583054
1118.140858	29.607317	68.588058
1117.098276	32.212821	68.593063
1116.110670	32.918799	68.598068
1116.066695	25.982516	68.603073
1114.500692	34.528130	68.608078
1114.126095	22.823652	68.613082
1113.720273	31.096413	68.618087
1113.212138	39.076368	68.623092
1112.528167	28.318390	68.628097
1111.704865	35.463796	68.633102
1110.916577	24.976307	68.638106
1110.310740	28.799147	68.643111
1109.660901	27.850780	68.648116
1109.550904	29.006950	68.653121
1108.255411	37.194146	68.658126
1107.770750	24.546804	68.663130
1107.244471	27.745127	68.668135
1106.770711	41.450310	68.673140
1105.945144	23.501816	68.678145
1104.805116	36.600186	68.683150
1104.564323	31.554452	68.688154
1103.954598	30.128194	68.693159
1102.992563	31.989179	68.698164
1102.547581	30.066779	68.703169
1101.841786	30.713743	68.708174
1101.060391	26.640259	68.713178
1100.531764	36.541063	68.718183
1099.446653	27.996305	68.723188
1098.839197	31.240659	68.728193
1098.289395	38.449798	68.733198
1097.994380	27.366603	68.738202
1097.738768	31.747176	68.743207
1096.640557	23.206083	68.748212
1095.933529	23.282383	68.753217
1095.267774	29.778251	68.758222
1095.049985	29.660033	68.763226
1093.692103	33.812242	68.768231
1092.957067	30.379518	68.773236
1092.907355	25.314432	68.778241
1092.148433	36.338398	68.783246
1091.301190	30.867160	68.788250
1090.775497	33.272180	68.793255
1089.890968	27.160318	68.798260
1089.552415	24.304776	68.803265
1088.269909	32.970887	68.808270
1087.848754	24.213286	68.813274
1087.195095	29.212269	68.818279
1086.497513	38.029768	68.823284
1086.734389	23.605534	68.828289
1085.482680	27.264612	68.833294
1084.749526	32.227356	68.838298
1084.143019	28.539222	68.843303
1083.091646	30.561084	68.848308
1082.713349	32.668266	68.853313
1081.808374	30.905777	68.858318
1081.032057	26.140781	68.863322
1080.846630	27.953929	68.868327
1079.804608	32.615722	68.873332
1079.399864	21.392294	68.878337
1078.772769	38.375145	68.883342
1078.137669	27.118971	68.888346
1077.191974	35.545428	68.893351
1076.118779	30.340376	68.898356
1075.710251	32.939651	68.903361
1075.141771	40.016147	68.908366
1074.761916	29.610354	68.913370
1075.018467	37.517553	68.918375
1073.573411	34.923188	68.923380
1072.881496	25.319254	68.928385
1072.358005	32.565209	68.933390
1071.225689	26.316154	68.938394
1070.558374	21.070196	68.943399
1069.897338	31.777391	68.948404
1069.683879	27.022209	68.953409
1068.822925	32.595072	68.958414
1068.571111	26.332104	68.963418
1067.535240	27.402172	68.968423
1066.612115	29.067745	68.973428
1066.225375	30.991767	68.978433
1065.633481	35.096254	68.983438
1064.274914	33.886903	68.988442
1064.048561	25.702297	68.993447
1063.654792	28.972588	68.998452
1063.394770	27.708330	69.003457
1062.210851	33.925512	69.008462
1061.198588	27.244198	69.013466
1061.029749	34.394313	69.018471
1060.186272	32.197844	69.023476
1059.566711	33.547044	69.028481
1058.638514	26.208955	69.033486
1058.064978	23.039137	69.038490
1057.663392	29.485103	69.043495
1057.370206	26.321147	69.048500
1056.527193	30.908710	69.053505
1055.303083	42.219583	69.058510
1054.772767	33.201805	69.063514
1054.696943	23.632334	69.068519
1053.541771	28.012511	69.073524
1052.981657	20.683681	69.078529
1051.997208	23.503890	69.083534
1051.606416	16.103970	69.088538
1051.268124	23.550698	69.093543
1049.975457	30.755018	69.098548
1049.702496	22.432749	69.103553
1049.149236	32.687560	69.108558
1048.513331	27.204796	69.113562
1047.508030	21.302981	69.118567
1046.517570	27.079379	69.123572
1046.420399	27.504953	69.128577
1045.866400	28.963574	69.133582
1045.605080	19.160263	69.138586
1045.071739	27.202576	69.143591
1043.817628	31.339877	69.148596
1043.137737	18.026602	69.153601
1041.901590	37.195825	69.158606
1041.227214	22.990684	69.163610
1040.871309	22.389815	69.168615
1040.473885	22.602957	69.173620
1040.324832	24.648441	69.178625
1039.077261	22.046335	69.183630
1038.208854	31.744153	69.188634
1037.671529	28.480268	69.193639
1037.002172	35.885055	69.198644
1037.032898	21.984058	69.203649
1035.897127	28.236167	69.208654
1035.142362	28.458851	69.213658
1034.895602	29.535855	69.218663
1033.467141	38.438103	69.223668
1032.950536	21.814033	69.228673
1032.546515	28.952674	69.233678
1031.941113	30.764832	69.238682
1030.804295	22.521654	69.243687
1029.726156	34.041120	69.248692
1029.633283	20.522493	69.253697
1029.000411	31.069093	69.258702
1028.804122	25.229388	69.263706
1028.611426	22.017911	69.268711
1026.888062	41.985331	69.273716
1026.481567	29.926398	69.278721
1025.831480	31.808745	69.283726
1025.548566	31.809704	69.288730
1024.663965	25.194831	69.293735
1023.792586	28.976356	69.298740
1023.087510	27.894874	69.303745
1022.848791	26.753388	69.308750
1021.955508	24.626360	69.313754
1021.183921	25.618129	69.318759
1020.345487	29.184678	69.323764
1020.370605	25.019177	69.328769
1019.502845	32.671575	69.333774
1018.324881	24.840230	69.338778
1017.561140	33.220406	69.343783
1016.962905	27.376842	69.348788
1016.628436	29.156935	69.353793
1016.365128	33.627048	69.358798
1015.637062	31.428003	69.363802
1014.884603	28.944256	69.368807
1014.069219	31.166720	69.373812
1013.268171	24.713601	69.378817
1012.416901	21.726756	69.383822
1011.655409	19.298065	69.388826
1011.484592	26.429567	69.393831
1010.713441	25.606184	69.398836
1009.695811	26.383212	69.403841
1009.361946	32.239662	69.408846
1008.623023	23.576796	69.413850
1008.499788	26.908131	69.418855
1007.283134	35.005554	69.423860
1006.631271	19.849093	69.428865
1005.656061	31.513038	69.433870
1005.571895	25.314872	69.438874
1005.184490	30.364550	69.443879
1004.139399	34.321955	69.448884
1003.422297	28.643964	69.453889
1002.425951	36.360983	69.458894
1002.370526	31.314157	69.463898
1001.702608	21.274346	69.468903
1000.595086	32.336445	69.473908
1000.226336	24.040465	69.478913
999.910871	24.401423	69.483918
998.971388	24.215112	69.488922
998.152215	23.629611	69.493927
997.232957	31.304401	69.498932
996.990346	23.090855	69.503937
995.881357	25.880437	69.508942
995.200945	23.645432	69.513946
994.828422	24.192090	69.518951
994.218359	38.281662	69.523956
994.204782	17.628855	69.528961
992.572554	30.502791	69.533966
991.531484	22.304326	69.538970
991.722162	21.777347	69.543975
990.996870	34.193169	69.548980
990.567291	24.374061	69.553985
989.571138	22.626115	69.558990
988.781938	32.574695	69.563994
988.542323	22.949292	69.568999
987.466253	38.032381	69.574004
986.498041	21.915427	69.579009
985.995157	22.632639	69.584014
985.444119	19.348873	69.589018
985.532468	16.198341	69.594023
984.026559	24.037438	69.599028
983.445745	13.122759	69.604033
982.917431	12.043127	69.609038
982.334536	29.113557	69.614042
981.922012	23.287765	69.619047
980.978584	28.641960	69.624052
980.487390	20.986793	69.629057
979.735267	29.455013	69.634062
979.102667	24.411719	69.639066
978.214218	20.352160	69.644071
977.487943	21.328847	69.649076
977.034849	24.859325	69.654081
976.582978	25.916930	69.659086
976.047304	22.995000	69.664090
975.201579	20.019903	69.669095
974.276480	27.462236	69.674100
973.816194	23.906987	69.679105
972.504049	23.849369	69.684110
971.727638	31.323240	69.689114
971.681857	20.372312	69.694119
970.871867	25.356768	69.699124
970.879146	20.899217	69.704129
969.664411	24.724353	69.709134
968.801957	22.330664	69.714138
968.593547	15.748574	69.719143
967.794486	21.578119	69.724148
967.300159	10.673340	69.729153
966.335651	26.396264	69.734158
965.728212	22.421306	69.739162
965.418943	22.200960	69.744167
964.672419	28.514161	69.749172
963.791892	21.900244	69.754177
963.088255	35.233571	69.759182
962.380326	32.734869	69.764186
962.292780	27.977012	69.769191
961.067458	39.887356	69.774196
960.458229	30.592005	69.779201
959.963200	35.685623	69.784206
959.258521	36.975850	69.789210
958.404152	30.496541	69.794215
957.404900	35.034877	69.799220
957.197914	30.045288	69.804225
956.839333	30.722197	69.809230
955.741251	36.704990	69.814234
955.033987	25.808855	69.819239
954.163181	30.623222	69.824244
954.267110	22.453890	69.829249
953.498792	27.127366	69.834254
952.338942	26.211312	69.839258
951.882281	24.719735	69.844263
951.204229	29.785706	69.849268
950.953579	23.949932	69.854273
949.850509	31.975684	69.859278
948.899285	33.336685	69.864282
948.654473	34.795012	69.869287
947.819999	33.642678	69.874292
947.678760	30.823569	69.879297
946.497410	31.530479	69.884302
945.639590	28.538392	69.889306
945.736032	26.739604	69.894311
944.699393	28.494245	69.899316
943.792098	26.640714	69.904321
943.045239	21.226104	69.909326
942.355890	32.305256	69.914330
942.435418	23.244092	69.919335
941.453548	38.849948	69.924340
940.912462	31.302075	69.929345
940.110450	26.951229	69.934350
939.463536	37.045915	69.939354
938.570253	34.489983	69.944359
937.576961	30.213730	69.949364
937.412292	26.302362	69.954369
936.710099	28.962579	69.959374
936.210681	34.629336	69.964378
935.684313	30.251973	69.969383
934.597656	34.069362	69.974388
933.779729	37.755677	69.979393
933.549673	31.787314	69.984398
932.785491	35.950781	69.989402
931.781591	25.474025	69.994407
931.097095	36.729029	69.999412
930.926676	21.067051	70.004417
930.518291	32.158264	70.009422
929.716296	39.041704	70.014426
928.686508	30.595464	70.019431
928.208738	29.562992	70.024436
927.585245	22.247440	70.029441
926.694385	30.406587	70.034446
925.784848	28.406762	70.039450
925.526220	29.764787	70.044455
924.709754	28.836678	70.049460
924.403890	26.696632	70.054465
923.612007	26.997797	70.059470
922.594096	31.025024	70.064474
922.209726	31.204567	70.069479
921.635884	34.937198	70.074484
920.837504	19.048726	70.079489
920.118434	32.516977	70.084494
919.364070	25.638570	70.089498
919.137308	24.022104	70.094503
918.290438	20.206689	70.099508
917.268299	26.357179	70.104513
916.879437	23.438708	70.109518
916.327373	24.606886	70.114522
915.958385	20.737499	70.119527
914.680163	24.702074	70.124532
914.402528	20.769263	70.129537
913.661263	25.730182	70.134542
913.060648	29.137489	70.139546
912.140648	25.756338	70.144551
911.035399	28.244160	70.149556
910.784502	30.958720	70.154561
910.414664	24.056970	70.159566
909.984212	22.767813	70.164570
909.263063	11.553794	70.169575
908.213999	23.240550	70.174580
907.920752	29.334971	70.179585
907.194538	13.405064	70.184590
906.139074	21.785952	70.189594
905.970287	21.689914	70.194599
905.315147	24.635964	70.199604
904.374711	23.140962	70.204609
903.202146	24.742209	70.209614
902.670202	22.802150	70.214618
902.747013	18.445501	70.219623
901.808550	30.116239	70.224628
901.149369	16.261986	70.229633
900.194818	23.169704	70.234638
899.937345	19.128031	70.239642
899.358447	28.180560	70.244647
898.321037	29.145284	70.249652
897.576354	27.628593	70.254657
897.120414	17.875212	70.259662
896.490715	25.138089	70.264666
895.981566	24.676748	70.269671
894.815100	31.410038	70.274676
894.268569	28.669629	70.279681
893.829180	30.452242	70.284686
893.312780	27.345913	70.289690
892.391749	23.244264	70.294695
891.586436	24.320286	70.299700
890.962492	27.244029	70.304705
890.629163	24.032872	70.309710
889.588550	30.569515	70.314714
888.993774	20.945464	70.319719
887.997546	27.238498	70.324724
888.026172	22.689243	70.329729
887.433437	24.248678	70.334734
886.890112	30.340323	70.339738
886.218429	18.792005	70.344743
885.382439	23.605579	70.349748
884.478296	22.527434	70.354753
883.666146	21.627038	70.359758
882.871996	30.675982	70.364762
882.806408	18.777312	70.369767
882.269779	25.295246	70.374772
881.235574	24.078529	70.379777
880.308770	19.540987	70.384782
879.868337	22.973268	70.389786
879.501970	17.141732	70.394791
878.162898	29.461286	70.399796
877.440504	22.867969	70.404801
876.639055	28.765730	70.409806
876.049857	27.520767	70.414810
876.316911	23.911281	70.419815
875.758184	23.016286	70.424820
875.198619	21.531641	70.429825
874.529920	14.232766	70.434830
873.760518	24.935154	70.439834
872.443302	20.967533	70.444839
871.044654	24.427743	70.449844
870.857349	20.825917	70.454849
870.727641	24.844261	70.459854
870.318945	26.748149	70.464858
869.914722	17.536904	70.469863
868.606829	29.268024	70.474868
868.258553	19.018119	70.479873
867.564034	18.641481	70.484878
866.274242	21.584471	70.489882
865.652533	10.750462	70.494887
864.963580	19.945086	70.499892
864.875731	23.803802	70.504897
864.517693	16.576911	70.509902
863.257293	24.641923	70.514906
863.055351	17.186759	70.519911
862.105445	15.590780	70.524916
861.528285	7.984029	70.529921
860.828457	13.841959	70.534926
860.118603	17.533166	70.539930
859.910952	13.773732	70.544935
858.892580	16.727141	70.549940
857.903171	17.975979	70.554945
857.400926	17.190270	70.559950
856.711941	24.014733	70.564954
856.348130	14.404399	70.569959
855.099817	19.151142	70.574964
854.391265	20.913522	70.579969
854.292807	19.153640	70.584974
853.728611	22.957285	70.589978
853.227316	12.074151	70.594983
852.128561	24.656661	70.599988
851.518630	16.537882	70.604993
850.945116	16.493651	70.609998
850.191577	29.402843	70.615002
849.594578	18.445051	70.620007
848.867108	25.351336	70.625012
848.237241	23.896810	70.630017
848.086342	18.508804	70.635022
846.788491	21.535088	70.640026
846.210459	17.206977	70.645031
845.622677	23.933331	70.650036
844.505120	20.449613	70.655041
843.879848	12.063620	70.660046
842.924865	17.120071	70.665050
843.008732	8.846713	70.670055
842.380283	20.165336	70.675060
841.661986	13.229184	70.680065
841.499817	18.728727	70.685070
840.079153	21.916489	70.690074
839.909428	13.443795	70.695079
839.335065	22.820460	70.700084
837.948706	17.466678	70.705089
837.701350	15.016134	70.710094
836.897394	18.857945	70.715098
836.548678	16.218530	70.720103
835.069771	18.447311	70.725108
834.281978	20.143462	70.730113
833.874675	21.960400	70.735118
833.341043	29.182767	70.740122
833.245409	16.965612	70.745127
832.801763	14.951592	70.750132
832.259750	28.678675	70.755137
831.442862	18.681566	70.760142
830.471375	30.273999	70.765146
829.981790	21.617248	70.770151
828.663456	21.836659	70.775156
828.160042	26.702968	70.780161
828.190000	14.538365	70.785166
827.069391	20.233047	70.790170
826.449101	18.677654	70.795175
825.480697	29.992053	70.800180
825.098828	29.269191	70.805185
824.878049	15.723658	70.810190
823.461159	27.090519	70.815194
822.882192	18.747622	70.820199
822.403757	21.757027	70.825204
822.003502	22.866366	70.830209
821.569330	11.512086	70.835214
820.141261	19.409837	70.840218
819.775555	14.680504	70.845223
819.016839	19.568528	70.850228
818.854291	24.440503	70.855233
817.961684	23.280122	70.860238
816.949714	24.439527	70.865242
816.689839	24.274415	70.870247
815.888141	22.400971	70.875252
815.079593	19.752753	70.880257
814.759947	10.968036	70.885262
814.214150	31.153372	70.890266
813.540288	12.288338	70.895271
812.456994	21.755480	70.900276
811.617812	23.399893	70.905281
811.352937	16.569771	70.910286
810.507857	27.159639	70.915290
809.523455	13.907554	70.920295
808.925684	19.886448	70.925300
808.491038	17.992425	70.930305
808.328269	14.539667	70.935310
807.177328	21.182206	70.940314
806.593578	14.611004	70.945319
805.710155	18.252583	70.950324
804.978857	21.387398	70.955329
805.098097	20.234687	70.960334
803.712661	23.301743	70.965338
803.039759	21.658537	70.970343
802.353823	23.030976	70.975348
802.160716	17.824738	70.980353
801.924233	17.592826	70.985358
800.498614	22.085543	70.990362
800.120031	22.068641	70.995367
799.313419	18.486561	71.000372
798.650379	26.727746	71.005377
797.685853	19.441294	71.010382
796.844684	29.190025	71.015386
796.445714	23.507198	71.020391
795.881626	21.305775	71.025396
795.726240	23.424817	71.030401
795.486429	18.334824	71.035406
794.008208	17.089478	71.040410
793.621759	16.621242	71.045415
792.890797	15.624374	71.050420
791.808152	24.353404	71.055425
791.406370	16.133700	71.060430
790.668638	22.934396	71.065434
790.125806	17.074200	71.070439
789.082571	20.667109	71.075444
788.377848	17.759522	71.080449
787.882067	19.959559	71.085454
787.572543	19.486963	71.090458
787.157821	19.117846	71.095463
786.313914	20.715711	71.100468
785.601042	22.119250	71.105473
784.989599	13.021444	71.110478
783.977945	19.644972	71.115482
783.269847	19.412446	71.120487
782.670973	19.796470	71.125492
782.119300	21.801978	71.130497
782.235014	14.185873	71.135502
780.841872	28.657160	71.140506
780.045691	22.457249	71.145511
779.596172	17.206677	71.150516
778.858896	23.409636	71.155521
778.224330	28.940231	71.160526
777.295899	25.439052	71.165530
777.310349	23.125032	71.170535
776.518321	20.581432	71.175540
775.102089	27.360837	71.180545
774.794685	15.663110	71.185550
774.089013	24.839914	71.190554
773.945540	18.242784	71.195559
773.050296	16.560866	71.200564
771.974121	24.396315	71.205569
771.635780	16.202786	71.210574
771.071617	20.466913	71.215578
770.680002	16.766737	71.220583
769.435790	24.524858	71.225588
768.898149	20.223454	71.230593
768.806655	16.682081	71.235598
767.726594	27.356677	71.240602
766.680383	20.222015	71.245607
766.196017	21.357369	71.250612
765.611306	25.801389	71.255617
765.319521	27.035396	71.260622
764.238093	28.667928	71.265626
763.706004	17.225169	71.270631
762.944861	22.537796	71.275636
762.506989	31.328195	71.280641
761.514570	20.211034	71.285646
760.568754	20.293904	71.290650
760.350115	22.878758	71.295655
759.780045	27.486029	71.300660
759.263207	25.185629	71.305665
758.376873	24.399588	71.310670
757.459770	30.583875	71.315674
757.269363	26.962054	71.320679
756.841021	19.481448	71.325684
755.664283	18.143974	71.330689
755.507008	23.193307	71.335694
754.358898	21.873353	71.340698
753.537946	19.977764	71.345703
752.679926	25.920831	71.350708
751.891405	26.333478	71.355713
751.429826	17.186590	71.360718
751.251442	26.342531	71.365722
750.970765	17.608391	71.370727
750.154981	28.980512	71.375732
748.999105	30.200700	71.380737
748.880041	21.358827	71.385742
747.318730	22.839107	71.390746
746.517993	11.447015	71.395751
746.153794	9.688447	71.400756
745.325604	19.452463	71.405761
745.246247	11.796454	71.410766
744.973797	17.259939	71.415770
744.615502	11.518612	71.420775
743.550614	12.501965	71.425780
742.634255	18.326586	71.430785
741.832542	13.411219	71.435790
740.965645	11.228060	71.440794
740.411090	14.754221	71.445799
740.086700	18.380935	71.450804
739.467933	15.730915	71.455809
738.684562	9.694566	71.460814
737.660170	21.880491	71.465818
737.149746	16.183885	71.470823
736.823371	12.916456	71.475828
735.529694	18.015828	71.480833
735.132170	7.934655	71.485838
734.071104	20.585312	71.490842
734.000488	15.805861	71.495847
733.765196	13.326601	71.500852
732.784231	13.672122	71.505857
732.155081	13.174728	71.510862
731.084060	20.498434	71.515866
731.152114	5.110791	71.520871
729.800863	13.884178	71.525876
729.032033	21.833133	71.530881
728.677443	16.737770	71.535886
728.188536	15.043215	71.540890
727.461355	13.180015	71.545895
726.635053	6.004060	71.550900
726.004734	14.755707	71.555905
725.844315	20.901525	71.560910
724.594185	16.552723	71.565914
723.936503	8.542518	71.570919
723.537938	15.577808	71.575924
722.638038	12.773858	71.580929
722.266179	14.044271	71.585934
720.983003	17.688023	71.590938
720.418708	20.607035	71.595943
720.014210	19.301166	71.600948
719.795942	14.606726	71.605953
719.280953	7.253473	71.610958
717.996441	20.398606	71.615962
717.828221	17.315733	71.620967
716.614299	12.112768	71.625972
715.676928	18.451678	71.630977
715.052969	10.207447	71.635982
714.260604	19.248251	71.640986
714.218503	20.838324	71.645991
713.720751	20.231703	71.650996
713.331396	17.075230	71.656001
712.621443	13.387905	71.661006
711.710902	20.619834	71.666010
710.403160	20.750887	71.671015
709.738751	16.220524	71.676020
709.140171	24.695889	71.681025
708.628235	16.495322	71.686030
708.177960	20.798097	71.691034
707.999517	16.497864	71.696039
707.041280	22.329166	71.701044
706.251257	22.934455	71.706049
705.836935	13.038888	71.711054
704.806019	15.035563	71.716058
703.903611	17.456478	71.721063
703.345755	11.962978	71.726068
702.741922	16.050505	71.731073
702.868564	6.647552	71.736078
701.863524	13.451401	71.741082
701.174016	19.760311	71.746087
700.469997	11.513063	71.751092
698.863220	22.631090	71.756097
698.358796	14.875609	71.761102
697.479925	19.481596	71.766106
697.025968	20.126418	71.771111
696.927288	15.778793	71.776116
696.266579	24.323976	71.781121
696.426294	16.212011	71.786126
695.336345	17.948429	71.791130
694.628208	11.650958	71.796135
694.166355	15.602339	71.801140
692.856390	10.063019	71.806145
691.863774	8.063900	71.811150
691.562658	15.000097	71.816154
691.134171	17.962144	71.821159
691.116080	10.436737	71.826164
689.717619	19.487322	71.831169
688.946225	9.979779	71.836174
688.488163	15.029696	71.841178
687.915669	14.468098	71.846183
686.786889	16.921910	71.851188
686.349869	13.017670	71.856193
686.077683	-0.327241	71.861198
684.794527	16.184485	71.866202
684.178951	16.511267	71.871207
683.605835	7.010003	71.876212
682.804488	20.023020	71.881217
682.735369	13.016672	71.886222
682.028399	13.102540	71.891226
681.076279	8.080260	71.896231
680.411382	12.557560	71.901236
680.005147	15.919766	71.906241
679.534407	15.450778	71.911246
678.458606	13.912765	71.916250
678.276168	9.532750	71.921255
676.961564	12.490819	71.926260
675.951923	16.023227	71.931265
675.525683	15.034642	71.936270
674.700502	24.596348	71.941274
674.661786	13.642765	71.946279
674.201843	14.802631	71.951284
673.207491	17.495242	71.956289
672.500647	17.462821	71.961294
672.010109	20.400060	71.966298
671.429611	10.395347	71.971303
670.364593	24.819155	71.976308
669.269261	26.972759	71.981313
669.119669	14.335295	71.986318
668.424369	22.236284	71.991322
668.307228	20.501465	71.996327
667.630959	15.053638	72.001332
666.654582	21.547009	72.006337
666.228043	6.812145	72.011342
664.927678	13.141061	72.016346
663.971560	9.403067	72.021351
663.494139	17.901719	72.026356
663.148572	27.259322	72.031361
662.972755	19.069898	72.036366
662.525941	22.069562	72.041370
661.295472	12.956832	72.046375
660.663714	18.144800	72.051380
659.927794	23.254738	72.056385
659.620274	2.844383	72.061390
658.192091	12.208795	72.066394
657.611123	14.152760	72.071399
657.394069	11.486102	72.076404
656.648603	20.558875	72.081409
656.382120	12.289277	72.086414
655.123622	14.768490	72.091418
654.572592	15.334160	72.096423
654.097989	10.324158	72.101428
653.369281	18.181583	72.106433
652.559476	8.360051	72.111438
651.853643	16.865115	72.116442
651.447442	17.827192	72.121447
651.014660	5.195413	72.126452
650.021680	15.971287	72.131457
649.265097	14.084409	72.136462
648.552021	13.775443	72.141466
648.279207	9.550172	72.146471
647.807036	-0.970093	72.151476
646.555274	8.139145	72.156481
646.292077	-8.793175	72.161486
645.758068	13.093367	72.166490
644.720355	15.545311	72.171495
644.067325	11.595055	72.176500
643.401289	14.353663	72.181505
643.363061	6.393075	72.186510
641.802860	14.196834	72.191514
641.379997	14.444051	72.196519
640.919791	11.836617	72.201524
640.005161	17.932231	72.206529
639.871406	7.354916	72.211534
638.773057	22.496821	72.216538
638.003728	11.536593	72.221543
637.795023	6.173592	72.226548
636.868825	18.064782	72.231553
636.156606	18.411697	72.236558
635.542724	16.502098	72.241562
634.773380	17.354852	72.246567
634.769776	5.228741	72.251572
633.298472	17.788638	72.256577
632.610811	13.768206	72.261582
632.382304	19.847596	72.266586
631.539628	21.017959	72.271591
630.999884	18.246574	72.276596
629.943497	14.493022	72.281601
629.606706	13.155886	72.286606
629.147812	24.097453	72.291610
628.262857	23.114120	72.296615
627.435240	26.887219	72.301620
626.640428	24.918125	72.306625
626.538539	19.320490	72.311630
626.109751	16.854712	72.316634
624.901445	19.232906	72.321639
624.375951	17.197269	72.326644
623.695909	26.464637	72.331649
623.268151	16.260570	72.336654
622.233583	22.252289	72.341658
621.257915	20.729894	72.346663
621.194864	13.866088	72.351668
620.319679	17.347141	72.356673
618.992224	11.520490	72.361678
618.326526	21.380083	72.366682
618.211008	12.917715	72.371687
617.764921	20.607136	72.376692
617.311323	19.870501	72.381697
617.021104	16.731373	72.386702
615.805225	20.799698	72.391706
614.854124	18.645764	72.396711
614.904550	14.417904	72.401716
613.641580	26.723864	72.406721
612.792960	21.598393	72.411726
612.142748	22.276062	72.416730
612.012548	24.927265	72.421735
611.486884	15.795355	72.426740
610.405455	18.642206	72.431745
609.862674	16.886870	72.436750
609.258313	18.680030	72.441754
608.201682	18.025244	72.446759
607.713994	7.707730	72.451764
606.772739	27.861424	72.456769
606.315653	15.131018	72.461774
605.777180	13.062760	72.466778
605.303312	27.622675	72.471783
604.410902	22.073671	72.476788
603.473783	20.519912	72.481793
602.999847	19.720287	72.486798
602.772657	23.260570	72.491802
602.022716	5.516364	72.496807
601.467919	11.493176	72.501812
600.584370	8.032235	72.506817
600.087261	11.410500	72.511822
599.139550	12.332673	72.516826
598.093957	14.878930	72.521831
597.803977	10.200661	72.526836
597.016352	21.743364	72.531841
596.964761	13.627210	72.536846
595.954813	14.182404	72.541850
595.012629	25.341296	72.546855
594.820078	19.743911	72.551860
593.835002	18.535262	72.556865
593.161947	20.538063	72.561870
592.354362	14.705898	72.566874
591.809009	20.668596	72.571879
591.927431	21.715861	72.576884
590.617067	29.404169	72.581889
589.957521	9.105091	72.586894
589.360015	14.882127	72.591898
588.705924	23.462545	72.596903
588.292260	21.779689	72.601908
587.261873	22.454837	72.606913
586.952820	13.909757	72.611918
585.921328	24.937795	72.616922
584.574767	33.713665	72.621927
584.320110	30.023249	72.626932
583.701166	28.708980	72.631937
583.653570	33.732964	72.636942
583.264305	24.812723	72.641946
582.067352	32.839365	72.646951
581.562875	29.535670	72.651956
580.465854	35.322889	72.656961
580.048490	24.431197	72.661966
579.216587	26.475072	72.666970
578.379864	23.451379	72.671975
578.032164	20.270949	72.676980
577.677801	26.567508	72.681985
577.205749	29.238468	72.686990
576.376773	22.540811	72.691994
575.467646	25.899553	72.696999
575.141870	17.360291	72.702004
573.596781	29.430505	72.707009
573.117849	22.743327	72.712014
572.533129	32.154797	72.717018
572.288517	35.557511	72.722023
571.957438	34.444976	72.727028
570.532339	34.326713	72.732033
570.096768	31.265934	72.737038
569.623166	17.140986	72.742042
568.948538	25.420327	72.747047
568.315713	21.108904	72.752052
567.366587	31.314854	72.757057
566.881651	21.381682	72.762062
566.463636	33.818010	72.767066
565.096225	31.776136	72.772071
564.797225	30.972308	72.777076
564.087491	35.548246	72.782081
563.732414	37.412099	72.787086
563.067739	31.891491	72.792090
562.078828	38.697560	72.797095
561.710338	31.808285	72.802100
560.831230	33.765069	72.807105
560.422572	22.151328	72.812110
559.383050	19.658262	72.817114
558.440859	36.776487	72.822119
558.556199	27.600833	72.827124
557.711608	25.552959	72.832129
557.042129	26.736760	72.837134
556.233654	26.908219	72.842138
555.433681	19.773865	72.847143
555.302793	21.072151	72.852148
554.176860	27.669807	72.857153
553.388306	24.289943	72.862158
552.920830	23.248024	72.867162
552.449684	26.530702	72.872167
551.909766	14.598832	72.877172
550.507641	27.630303	72.882177
549.946362	20.850593	72.887182
549.547635	18.988747	72.892186
548.860511	27.788901	72.897191
548.693788	18.424792	72.902196
547.755169	24.054325	72.907201
546.973682	16.210556	72.912206
546.262092	17.550878	72.917210
545.926173	19.537836	72.922215
545.700276	28.685570	72.927220
544.499415	27.661124	72.932225
543.898788	18.667331	72.937230
542.824881	18.967806	72.942234
542.050170	21.317973	72.947239
542.014594	11.862017	72.952244
541.346846	18.583809	72.957249
540.676797	20.753302	72.962254
539.906911	21.997255	72.967258
539.146011	22.626343	72.972263
538.774827	17.439044	72.977268
537.089407	21.265230	72.982273
536.572116	31.443402	72.987278
536.429561	26.317453	72.992282
535.796616	29.223784	72.997287
535.743665	16.400639	73.002292
534.469117	21.364594	73.007297
533.884977	17.772404	73.012302
533.453448	14.952267	73.017306
532.495417	32.828376	73.022311
531.602079	23.222044	73.027316
530.761305	21.831162	73.032321
530.431445	25.829352	73.037326
530.196511	16.537615	73.042330
529.221728	22.094066	73.047335
528.173974	11.400587	73.052340
527.368367	19.858492	73.057345
527.177937	19.236071	73.062350
526.742936	24.182989	73.067354
526.040089	28.521293	73.072359
525.249371	20.625385	73.077364
524.428612	21.134702	73.082369
523.994840	18.046841	73.087374
523.681054	16.893714	73.092378
522.335858	20.813946	73.097383
521.846723	23.057126	73.102388
521.215786	17.453892	73.107393
520.823664	17.467575	73.112398
519.557644	22.092710	73.117402
518.751631	28.148984	73.122407
518.627178	12.946572	73.127412
517.948921	25.246154	73.132417
517.604408	16.853394	73.137422
516.926263	16.001160	73.142426
515.902828	17.473169	73.147431
515.333653	19.162973	73.152436
514.875676	16.296590	73.157441
513.864371	13.641356	73.162446
513.186574	19.711896	73.167450
512.539393	15.896366	73.172455
512.369808	14.650883	73.177460
511.461761	17.015991	73.182465
510.411893	19.012607	73.187470
510.086343	19.649622	73.192474
509.543206	17.799749	73.197479
509.105192	12.552141	73.202484
508.092405	20.248270	73.207489
507.385446	22.300648	73.212494
506.926213	19.522776	73.217498
505.822248	23.128621	73.222503
505.201754	16.042969	73.227508
504.510032	23.484527	73.232513
503.958910	18.921989	73.237518
503.733202	19.227708	73.242522
502.614459	26.087589	73.247527
502.026337	15.746677	73.252532
501.299746	23.469757	73.257537
501.070549	27.212217	73.262542
500.769803	9.473768	73.267546
499.340484	19.967539	73.272551
498.850408	17.574628	73.277556
498.038220	18.946758	73.282561
497.512909	25.415636	73.287566
496.826949	9.960484	73.292570
496.180015	21.351483	73.297575
495.679693	22.129883	73.302580
494.479979	25.602753	73.307585
493.865445	20.698658	73.312590
493.499937	15.141458	73.317594
492.776426	19.503560	73.322599
492.544551	18.665394	73.327604
491.725548	19.906148	73.332609
491.102746	17.034489	73.337614
490.224917	17.120823	73.342618
489.871213	19.668863	73.347623
488.506434	16.038623	73.352628
487.943658	24.285966	73.357633
487.302977	16.989069	73.362638
487.260413	16.291056	73.367642
486.432844	19.427097	73.372647
485.606827	18.361888	73.377652
485.022004	29.109063	73.382657
484.614933	22.244881	73.387662
483.596502	22.068188	73.392666
482.765881	19.966077	73.397671
482.321986	14.482869	73.402676
481.690492	20.517654	73.407681
480.737309	18.605381	73.412686
480.034085	20.780173	73.417690
479.230283	21.365651	73.422695
479.087604	25.179483	73.427700
478.536514	20.107590	73.432705
477.740755	21.505495	73.437710
477.245913	19.032924	73.442714
476.331001	24.732819	73.447719
476.098284	25.213122	73.452724
474.649886	28.519040	73.457729
473.887868	17.169783	73.462734
473.611736	22.215976	73.467738
472.906416	27.002541	73.472743
472.804723	13.250464	73.477748
472.188116	25.858776	73.482753
471.224897	20.702734	73.487758
470.611735	18.208014	73.492762
469.487265	19.934258	73.497767
468.857895	15.418889	73.502772
467.991962	19.341640	73.507777
467.363657	18.170821	73.512782
467.274219	19.867783	73.517786
466.728360	17.453805	73.522791
466.071471	16.934090	73.527796
465.203021	9.857997	73.532801
464.484557	17.931447	73.537806
464.168605	12.229164	73.542810
463.007615	24.848515	73.547815
462.401804	11.889541	73.552820
462.223571	23.224795	73.557825
461.018289	22.593756	73.562830
459.975098	21.864354	73.567834
459.342590	22.788400	73.572839
459.015773	15.635474	73.577844
458.933888	17.645046	73.582849
458.381432	11.674516	73.587854
457.339968	15.778200	73.592858
456.575580	15.587852	73.597863
456.024935	0.707258	73.602868
455.275264	13.472380	73.607873
454.320698	7.753576	73.612878
454.037006	10.711509	73.617882
453.477465	16.744296	73.622887
452.463531	11.344033	73.627892
451.362345	16.351367	73.632897
451.083049	17.605492	73.637902
450.907849	11.999058	73.642906
450.178382	16.453582	73.647911
449.263390	10.802590	73.652916
448.593549	16.431905	73.657921
447.812961	14.276104	73.662926
447.486905	14.050614	73.667930
445.971296	27.530718	73.672935
445.518613	16.379770	73.677940
445.245677	22.852598	73.682945
444.747247	15.484167	73.687950
444.799938	11.446762	73.692954
443.489835	17.160744	73.697959
443.010766	8.289550	73.702964
442.256420	14.643535	73.707969
441.005894	16.063446	73.712974
440.383116	17.834347	73.717978
439.868369	24.088660	73.722983
439.777973	13.662161	73.727988
438.659965	20.201825	73.732993
437.736575	15.028415	73.737998
437.453726	6.868704	73.743002
436.619116	21.129704	73.748007
436.378729	14.787758	73.753012
434.995134	13.896561	73.758017
434.271742	21.639645	73.763022
434.141472	16.614256	73.768026
433.726459	22.015316	73.773031
433.074049	12.477882	73.778036
432.078634	13.869766	73.783041
431.857925	15.434679	73.788046
431.072026	15.290345	73.793050
429.670937	15.023258	73.798055
429.352720	20.295354	73.803060
428.997416	13.760409	73.808065
428.138006	21.165621	73.813070
427.676880	9.918258	73.818074
426.349751	15.097219	73.823079
426.018634	15.200544	73.828084
425.548931	9.540114	73.833089
424.871684	22.240092	73.838094
424.299431	6.915093	73.843098
423.180371	19.568771	73.848103
422.506288	15.748093	73.853108
422.315052	7.297821	73.858113
421.808550	12.287680	73.863118
420.634759	9.611069	73.868122
420.170500	19.222553	73.873127
419.711806	8.657626	73.878132
419.164019	16.256035	73.883137
418.022844	14.883097	73.888142
417.386837	17.696900	73.893146
416.797226	23.157322	73.898151
416.605152	12.280251	73.903156
415.686029	13.849219	73.908161
414.657026	11.311966	73.913166
414.428724	3.408498	73.918170
413.390981	9.799760	73.923175
413.370453	5.420787	73.928180
412.139567	7.154549	73.933185
411.440470	16.592140	73.938190
411.446750	3.119347	73.943194
409.839882	12.075532	73.948199
409.050534	12.404840	73.953204
408.863291	4.114785	73.958209
408.212203	16.862631	73.963214
408.210617	2.328228	73.968218
406.941460	19.470176	73.973223
406.266109	19.547930	73.978228
406.131849	11.337739	73.983233
405.331194	10.905604	73.988238
404.219020	10.270797	73.993242
403.545127	16.812245	73.998247
403.201578	16.674703	74.003252
402.745210	21.216610	74.008257
401.162186	18.923761	74.013262
400.823084	13.912729	74.018266
400.179556	21.444398	74.023271
399.818159	17.460361	74.028276
399.267402	24.734398	74.033281
398.312441	18.359666	74.038286
397.768506	15.924898	74.043290
397.038896	10.518779	74.048295
396.687772	7.670090	74.053300
395.634205	14.756162	74.058305
394.632859	10.098243	74.063310
394.314754	11.615601	74.068314
393.784343	22.089184	74.073319
393.562822	12.000556	74.078324
392.476033	13.219357	74.083329
391.432949	18.069223	74.088334
391.232811	5.870384	74.093338
390.791105	16.068054	74.098343
390.065453	5.958840	74.103348
389.429662	12.968879	74.108353
388.586549	15.834614	74.113358
387.608763	11.403177	74.118362
386.922209	11.296642	74.123367
386.531819	8.034743	74.128372
385.910828	11.803368	74.133377
385.082503	15.780075	74.138382
385.173195	13.458646	74.143386
383.811683	16.359682	74.148391
383.133264	16.316507	74.153396
382.933851	12.926403	74.158401
381.837102	17.005809	74.163406
380.992018	8.716507	74.168410
380.138459	15.748637	74.173415
380.122747	7.171054	74.178420
379.270280	12.555095	74.183425
378.033606	14.256680	74.188430
377.854451	6.138805	74.193434
377.529792	7.759711	74.198439
376.873570	19.242090	74.203444
375.807109	14.581938	74.208449
374.620545	17.030900	74.213454
374.785359	11.151097	74.218458
374.193904	16.594471	74.223463
373.830277	1.882802	74.228468
372.500915	10.004732	74.233473
371.585963	25.480186	74.238478
371.303394	17.109127	74.243482
371.033880	12.441827	74.248487
370.156810	15.642561	74.253492
369.018397	11.946358	74.258497
368.295693	11.142269	74.263502
368.025415	9.494953	74.268506
367.650959	14.922671	74.273511
366.914470	17.098063	74.278516
366.255568	8.001661	74.283521
365.256281	16.001611	74.288526
364.959418	3.357725	74.293530
363.504548	4.666735	74.298535
362.965764	3.290867	74.303540
362.693557	13.232868	74.308545
362.300746	8.184674	74.313550
361.723127	5.722168	74.318554
360.873190	19.187685	74.323559
360.424000	13.068262	74.328564
360.002468	16.947033	74.333569
358.554102	20.221469	74.338574
358.043981	6.340545	74.343578
357.469108	16.426976	74.348583
356.853106	15.307841	74.353588
356.059708	8.647189	74.358593
355.160066	17.774552	74.363598
354.878131	10.349570	74.368602
354.280887	16.662770	74.373607
353.693329	12.629630	74.378612
352.943838	14.229933	74.383617
351.987241	17.008109	74.388622
351.729453	6.988351	74.393626
350.784040	21.872573	74.398631
350.112402	19.218472	74.403636
349.501979	14.022032	74.408641
348.817789	24.835518	74.413646
348.532367	14.684542	74.418650
347.196572	19.953233	74.423655
346.765414	20.561367	74.428660
346.722829	15.022120	74.433665
345.530822	15.601699	74.438670
344.693365	18.960132	74.443674
344.066564	26.878655	74.448679
343.638820	12.443707	74.453684
343.276136	16.817725	74.458689
342.195557	22.831068	74.463694
341.647777	13.590806	74.468698
340.944269	22.844613	74.473703
340.475767	7.165645	74.478708
339.674638	8.659064	74.483713
338.424129	15.188341	74.488718
338.319814	14.842371	74.493722
337.726707	12.527419	74.498727
337.006792	7.132393	74.503732
335.827557	18.143045	74.508737
335.372084	9.932017	74.513742
334.809180	10.059679	74.518746
334.518566	16.469094	74.523751
334.066723	11.412966	74.528756
333.168760	20.070138	74.533761
332.482272	19.662410	74.538766
332.291267	11.060728	74.543770
330.766007	16.391160	74.548775
330.056986	15.550209	74.553780
330.026509	15.766481	74.558785
329.029797	15.942783	74.563790
328.610976	7.829996	74.568794
327.609137	17.025693	74.573799
326.792800	7.083920	74.578804
326.615792	15.585188	74.583809
325.571455	16.303667	74.588814
325.011583	3.250701	74.593818
323.783690	18.958960	74.598823
323.563723	14.725316	74.603828
323.188211	13.908484	74.608833
322.621565	19.781576	74.613838
322.500853	10.941611	74.618842
321.112414	14.208092	74.623847
320.592197	16.459414	74.628852
319.823510	8.506469	74.633857
318.884966	10.846540	74.638862
318.205789	13.061696	74.643866
317.715737	21.508781	74.648871
317.285468	14.736649	74.653876
316.933808	17.337998	74.658881
315.996889	23.421494	74.663886
315.315828	16.159478	74.668890
314.814529	20.662826	74.673895
313.855781	14.137351	74.678900
313.327829	12.089564	74.683905
312.459360	19.500980	74.688910
311.819268	13.192800	74.693914
310.820216	25.764314	74.698919
310.304218	19.212426	74.703924
310.025261	17.919737	74.708929
309.491520	27.137033	74.713934
309.037933	14.970715	74.718938
307.783165	14.793918	74.723943
307.076646	18.992507	74.728948
306.906671	19.346131	74.733953
305.465489	26.183361	74.738958
304.977596	19.076640	74.743962
304.583979	18.595432	74.748967
304.073253	22.619315	74.753972
303.669249	16.880633	74.758977
302.470180	12.675314	74.763982
301.685701	13.984742	74.768986
301.227519	17.467240	74.773991
300.756632	13.027589	74.778996
300.558919	10.953978	74.784001
299.223341	22.167760	74.789006
298.835736	17.542946	74.794010
298.198644	12.964207	74.799015
297.066846	11.897338	74.804020
296.407161	10.682681	74.809025
295.675118	16.588447	74.814030
295.427523	7.349243	74.819034
294.908945	15.912837	74.824039
294.303982	13.322243	74.829044
293.271331	9.063597	74.834049
292.680898	19.053170	74.839054
292.618213	7.560994	74.844058
291.236546	13.382646	74.849063
290.381841	12.503426	74.854068
289.835994	-3.048067	74.859073
289.121920	12.737570	74.864078
289.066843	13.187998	74.869082
288.295178	19.902750	74.874087
287.156188	18.742415	74.879092
286.782181	15.799620	74.884097
286.107774	22.147211	74.889102
285.507269	14.096506	74.894106
284.669613	24.492918	74.899111
284.069046	15.311550	74.904116
284.073470	15.771418	74.909121
282.963672	19.837176	74.914126
282.444361	7.350190	74.919130
281.553985	16.143358	74.924135
280.843351	15.666954	74.929140
279.829262	14.316404	74.934145
278.982034	20.743582	74.939150
278.716442	14.120252	74.944154
278.350714	17.193780	74.949159
278.018727	21.015711	74.954164
277.132791	15.714975	74.959169
275.942005	19.077709	74.964174
275.793287	5.807836	74.969178
274.882792	9.335625	74.974183
273.672590	7.566907	74.979188
273.372490	13.727101	74.984193
272.761499	14.240910	74.989198
272.809723	12.553876	74.994202
271.830761	19.818913	74.999207
271.506994	14.915849	75.004212
270.763073	14.323329	75.009217
269.366026	10.442899	75.014222
268.673684	14.456310	75.019226
268.002058	9.316962	75.024231
267.421285	12.244995	75.029236
267.213275	8.559810	75.034241
266.164936	13.566676	75.039246
265.647173	6.243960	75.044250
264.961775	12.115487	75.049255
264.466255	11.849226	75.054260
263.992480	3.336788	75.059265
262.852620	17.389430	75.064270
262.378619	6.757607	75.069274
261.858496	4.267039	75.074279
260.653123	15.117879	75.079284
260.193829	8.146965	75.084289
259.420166	13.198358	75.089294
259.298166	10.103435	75.094298
258.541359	15.554265	75.099303
257.895541	12.137564	75.104308
257.028830	12.483982	75.109313
256.182858	13.519376	75.114318
256.101185	12.304055	75.119322
254.981522	9.437551	75.124327
253.785021	11.877112	75.129332
253.849616	2.662272	75.134337
253.151274	12.183346	75.139342
253.027766	1.505121	75.144346
251.942344	6.066894	75.149351
251.200495	6.202600	75.154356
250.755163	2.820176	75.159361
249.512006	5.628297	75.164366
248.980447	4.489424	75.169370
248.307862	2.187166	75.174375
247.489166	5.194130	75.179380
247.719858	4.838916	75.184385
246.557641	13.460961	75.189390
245.901298	6.324344	75.194394
245.538860	8.250907	75.199399
244.181147	5.669937	75.204404
243.475537	4.054187	75.209409
242.488765	9.891760	75.214414
241.970771	12.935946	75.219418
241.925787	6.764737	75.224423
241.676966	19.290786	75.229428
240.937511	9.712108	75.234433
239.406485	6.816571	75.239438
239.189180	11.107499	75.244442
238.837821	1.213072	75.249447
238.334364	8.179963	75.254452
237.380141	10.438985	75.259457
236.693561	15.848663	75.264462
236.130732	2.903434	75.269466
234.752605	7.939228	75.274471
234.227322	6.021922	75.279476
233.768599	10.669879	75.284481
233.389302	14.732744	75.289486
233.112290	7.031037	75.294490
232.155105	5.192044	75.299495
231.210463	12.754394	75.304500
231.018875	5.259844	75.309505
230.097723	13.045530	75.314510
229.856147	12.156899	75.319514
228.574380	15.731275	75.324519
227.980673	10.119049	75.329524
226.867753	18.378432	75.334529
226.198595	15.988901	75.339534
225.871253	17.903565	75.344538
225.889383	19.815195	75.349543
225.304223	18.553984	75.354548
224.371717	10.269224	75.359553
223.305615	18.002329	75.364558
222.771129	14.049074	75.369562
221.507145	16.705989	75.374567
221.010536	14.627996	75.379572
220.754481	3.606630	75.384577
219.971266	21.002331	75.389582
219.553073	7.519962	75.394586
219.085389	11.007139	75.399591
217.824778	14.776843	75.404596
217.382003	12.627191	75.409601
216.408259	19.998647	75.414606
216.263271	6.122643	75.419610
215.540443	20.941447	75.424615
214.503714	13.901749	75.429620
214.326228	6.062754	75.434625
213.498960	21.134751	75.439630
212.870868	13.408590	75.444634
211.838126	25.047216	75.449639
211.047727	22.546130	75.454644
210.968789	8.588632	75.459649
210.495254	17.280673	75.464654
209.468275	10.340350	75.469658
208.557492	11.277282	75.474663
208.282874	12.372991	75.479668
208.145696	-0.980703	75.484673
206.618333	5.952309	75.489678
206.111411	10.943843	75.494682
205.987331	13.545193	75.499687
205.161001	9.991707	75.504692
204.080744	6.075006	75.509697
203.217232	18.143965	75.514702
202.905985	6.866472	75.519706
202.694410	14.906471	75.524711
201.662379	21.881949	75.529716
201.045223	5.075561	75.534721
200.179842	16.302726	75.539726
199.770415	14.319648	75.544730
198.576222	7.831766	75.549735
197.845108	14.365030	75.554740
197.413835	10.933067	75.559745
197.002085	17.418571	75.564750
196.742390	7.047491	75.569754
195.851900	15.629389	75.574759
194.759534	16.596854	75.579764
194.167196	6.668314	75.584769
193.826635	13.919902	75.589774
193.254552	15.271195	75.594778
192.278636	5.216154	75.599783
191.835824	10.654784	75.604788
191.212474	8.240615	75.609793
189.811711	18.646397	75.614798
189.372100	10.607922	75.619802
188.874749	11.070518	75.624807
188.464205	14.534398	75.629812
188.179805	5.827786	75.634817
186.707775	7.016632	75.639822
186.013141	8.974089	75.644826
185.893508	7.334318	75.649831
184.986395	18.997072	75.654836
185.041262	9.665512	75.659841
183.730092	21.411613	75.664846
183.104883	19.401439	75.669850
182.583184	17.297492	75.674855
181.666402	15.258113	75.679860
180.957846	-3.610524	75.684865
180.507252	17.378045	75.689870
180.255275	20.043942	75.694874
179.160202	20.366873	75.699879
178.388161	11.321693	75.704884
177.951652	14.684059	75.709889
177.135866	17.630658	75.714894
176.101105	12.997089	75.719898
175.665232	10.469454	75.724903
174.807920	17.120617	75.729908
174.535786	4.684148	75.734913
174.349527	10.219070	75.739918
173.401445	11.264464	75.744922
172.622190	2.094286	75.749927
171.691821	15.807626	75.754932
171.358801	9.250262	75.759937
170.301256	10.822463	75.764942
169.697456	18.426685	75.769946
169.359435	15.750986	75.774951
168.744701	10.312440	75.779956
167.926318	11.106922	75.784961
166.795099	13.288534	75.789966
166.470056	15.641230	75.794970
165.960220	14.170906	75.799975
165.434609	23.030530	75.804980
164.372116	14.894254	75.809985
163.529365	16.865872	75.814990
162.925321	10.077334	75.819994
162.794789	5.239677	75.824999
162.227876	16.233184	75.830004
161.939060	6.901232	75.835009
160.896295	14.572289	75.840014
159.932277	20.163415	75.845018
159.196239	7.326253	75.850023
158.149721	14.546903	75.855028
157.838051	9.006423	75.860033
157.349359	18.735364	75.865038
157.103010	9.237369	75.870042
156.115820	14.196680	75.875047
155.456881	17.834211	75.880052
155.009936	7.508766	75.885057
153.801108	10.227881	75.890062
152.939363	6.530253	75.895066
152.562781	11.758056	75.900071
152.138492	18.940998	75.905076
151.973844	12.755759	75.910081
150.804752	15.766583	75.915086
149.887052	5.577703	75.920090
149.409347	17.209843	75.925095
148.611819	17.430151	75.930100
147.654898	14.868908	75.935105
147.090019	19.175839	75.940110
146.847544	22.344847	75.945114
146.619452	17.292509	75.950119
145.741959	20.253688	75.955124
144.916698	14.410326	75.960129
144.159931	15.835231	75.965134
143.592826	11.198073	75.970138
142.398399	8.291506	75.975143
141.447411	14.080831	75.980148
140.930757	9.512900	75.985153
140.551948	15.698267	75.990158
140.263480	14.547465	75.995162
140.260895	7.112677	76.000167
139.065737	11.527991	76.005172
138.141335	7.912899	76.010177
137.714765	11.218491	76.015182
136.892094	16.329771	76.020186
136.252788	15.037793	76.025191
135.410464	17.864058	76.030196
135.206798	11.610926	76.035201
134.350067	15.303654	76.040206
133.145385	12.021836	76.045210
132.995644	12.892637	76.050215
132.111722	20.795421	76.055220
132.083443	7.880108	76.060225
130.850344	11.910393	76.065230
129.970060	19.255934	76.070234
129.827407	11.860826	76.075239
129.065940	14.368271	76.080244
128.149444	16.149810	76.085249
127.568459	15.376812	76.090254
126.715177	17.618203	76.095258
126.547549	13.527627	76.100263
125.435261	19.628107	76.105268
124.667197	9.962576	76.110273
124.110259	19.653518	76.115278
123.683584	18.250367	76.120282
123.743247	13.956392	76.125287
122.191436	14.970342	76.130292
121.479268	11.926960	76.135297
120.903711	15.308353	76.140302
120.415203	13.856716	76.145306
119.523089	9.624627	76.150311
118.785156	12.334902	76.155316
118.535373	11.851290	76.160321
117.994111	15.097905	76.165326
117.156330	5.046106	76.170330
116.470030	8.489312	76.175335
115.529747	9.438867	76.180340
115.111234	9.278627	76.185345
114.262660	10.674027	76.190350
113.006397	14.277508	76.195354
112.976568	7.419499	76.200359
112.480309	23.924215	76.205364
112.428918	10.265115	76.210369
110.962178	21.963513	76.215374
109.658420	17.401255	76.220378
109.814910	9.471171	76.225383
109.023232	17.220479	76.230388
108.923205	15.582316	76.235393
107.949290	13.296612	76.240398
107.247144	14.917821	76.245402
106.591435	10.323188	76.250407
105.784273	13.192739	76.255412
104.777257	5.591700	76.260417
104.069973	18.723860	76.265422
103.737514	9.107145	76.270426
103.342508	9.156047	76.275431
102.903623	17.719571	76.280436
101.967207	15.420004	76.285441
101.364617	14.251491	76.290446
100.737634	9.344774	76.295450
99.648309	20.443676	76.300455
98.882924	20.512218	76.305460
98.687613	5.384284	76.310465
98.181267	17.517733	76.315470
97.140635	15.302596	76.320474
96.593146	14.547919	76.325479
95.403699	9.664668	76.330484
95.079318	10.041352	76.335489
95.032661	15.121932	76.340494
93.935325	14.994255	76.345498
93.136056	9.719202	76.350503
92.208135	8.217797	76.355508
92.299662	2.491609	76.360513
91.622155	7.603403	76.365518
90.581123	13.471759	76.370522
90.423503	2.920425	76.375527
89.424549	10.412630	76.380532
88.676966	8.262728	76.385537
88.084609	11.411841	76.390542
87.449391	9.212481	76.395546
86.169992	0.153640	76.400551
84.887893	6.303288	76.405556
85.054964	4.497954	76.410561
84.549515	15.347626	76.415566
83.894769	11.930825	76.420570
83.858419	10.031775	76.425575
83.319957	1.848250	76.430580
82.138199	0.292714	76.435585
81.597490	1.689489	76.440590
80.753015	11.993986	76.445594
79.644400	4.469087	76.450599
78.617855	15.658904	76.455604
78.767172	1.280262	76.460609
78.231198	7.856546	76.465614
77.949457	15.213879	76.470618
77.061764	5.945915	76.475623
76.038952	7.809082	76.480628
75.744767	8.132067	76.485633
74.499501	7.950720	76.490638
73.747723	11.049567	76.495642
73.274277	3.068563	76.500647
73.069291	10.060416	76.505652
72.296218	7.209691	76.510657
71.375322	3.915765	76.515662
70.534635	9.810522	76.520666
70.457581	0.537863	76.525671
69.818768	8.843112	76.530676
69.085588	9.698154	76.535681
68.182052	9.728815	76.540686
67.616519	5.665438	76.545690
66.756852	0.895191	76.550695
65.644997	9.555002	76.555700
65.547532	7.783971	76.560705
64.598019	3.529522	76.565710
64.048720	5.719297	76.570714
64.012716	-5.326082	76.575719
62.745864	7.635119	76.580724
62.242331	2.144183	76.585729
61.955750	9.488092	76.590734
60.550340	6.774488	76.595738
59.965905	5.508474	76.600743
59.035239	7.281258	76.605748
58.865536	3.999997	76.610753
58.527633	0.340288	76.615758
57.939823	4.199881	76.620762
57.529942	1.098851	76.625767
56.421332	7.422692	76.630772
55.370039	5.825862	76.635777
54.313844	0.571303	76.640782
53.758468	10.799736	76.645786
53.593551	0.277960	76.650791
53.109353	0.066707	76.655796
52.711927	10.172178	76.660801
51.726218	9.116819	76.665806
51.075219	7.664305	76.670810
50.937857	2.247435	76.675815
49.559319	12.009493	76.680820
48.672814	2.462236	76.685825
48.272681	10.525997	76.690830
47.849843	11.074507	76.695834
47.342705	11.131840	76.700839
46.205092	12.210664	76.705844
45.742108	5.789174	76.710849
45.367511	9.693613	76.715854
44.537243	3.747016	76.720858
43.607635	6.546228	76.725863
42.915522	9.504680	76.730868
42.148544	5.080779	76.735873
42.013492	3.575941	76.740878
40.764782	9.087930	76.745882
40.238016	-1.757751	76.750887
39.421445	12.274931	76.755892
39.235111	7.108721	76.760897
38.930617	13.310628	76.765902
37.795872	12.619666	76.770906
37.110874	7.307487	76.775911
36.122844	8.710962	76.780916
36.041582	7.077697	76.785921
34.919825	6.469819	76.790926
34.039190	14.064598	76.795930
34.276948	2.450431	76.800935
33.535255	9.102111	76.805940
32.172849	16.882542	76.810945
31.805210	9.070750	76.815950
31.368588	10.857786	76.820954
30.964863	2.252243	76.825959
29.640477	12.868261	76.830964
29.021725	4.631326	76.835969
28.535952	8.175033	76.840974
27.668674	12.853489	76.845978
27.641181	4.955909	76.850983
26.247037	10.374408	76.855988
25.588933	3.850005	76.860993
25.043369	6.786663	76.865998
24.572741	8.359929	76.871002
24.334314	2.030362	76.876007
23.349138	14.043068	76.881012
22.775519	1.566418	76.886017
22.019408	9.204414	76.891022
21.063144	10.719522	76.896026
20.693478	2.326168	76.901031
20.026300	5.894079	76.906036
19.283603	4.325314	76.911041
18.383478	3.395090	76.916046
17.635772	8.197978	76.921050
17.422869	-2.271981	76.926055
16.512633	4.740896	76.931060
16.103309	2.221677	76.936065
15.205389	1.680609	76.941070
14.300106	1.211677	76.946074
13.968488	-1.938097	76.951079
13.567773	8.394980	76.956084
13.103232	8.202676	76.961089
12.017686	-0.142721	76.966094
11.238823	10.014131	76.971098
11.119225	6.095682	76.976103
10.008503	5.107590	76.981108
8.842980	9.515080	76.986113
8.463315	6.464432	76.991118
7.973497	3.924938	76.996122
7.738591	3.399542	77.001127
6.620676	12.120266	77.006132
5.916182	3.313546	77.011137
5.688961	4.707642	77.016142
5.002528	6.750570	77.021147
4.662301	-0.575153	77.026151
3.015293	13.659383	77.031156
2.912168	8.210248	77.036161