Fri Mar 05 19:57:44 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.093870	97.605282	0.000000
-0.430766	89.487302	0.005005
-1.285687	66.338492	0.010010
-2.886993	17.973615	0.015014
-7.106405	2.333210	0.020019
-12.482427	4.059634	0.025024
-16.989075	2.607060	0.030029
-21.493444	9.023057	0.035034
-25.702737	8.521271	0.040038
-29.610365	4.628262	0.045043
-32.794794	-3.078019	0.050048
-36.637727	2.524451	0.055053
-40.415949	2.660397	0.060058
-44.195203	3.290095	0.065062
-47.763106	10.362573	0.070067
-51.635861	1.428873	0.075072
-55.359024	0.100545	0.080077
-59.512249	4.968811	0.085082
-62.760119	-0.393441	0.090086
-66.784304	0.258019	0.095091
-70.463422	-0.640499	0.100096
-73.714192	4.954292	0.105101
-77.588930	12.488920	0.110106
-81.549003	-0.789457	0.115110
-85.782618	2.708702	0.120115
-89.339252	-0.681966	0.125120
-93.311373	1.128165	0.130125
-96.902326	2.005445	0.135130
-100.557453	-4.424019	0.140134
-104.392737	-2.528469	0.145139
-108.163116	2.181026	0.150144
-111.932608	2.012919	0.155149
-115.448444	5.596881	0.160154
-119.112340	-4.014991	0.165158
-123.224931	-4.752806	0.170163
-127.034949	-8.132950	0.175168
-130.430987	0.476538	0.180173
-134.551990	-1.761159	0.185178
-137.866732	-3.990300	0.190182
-141.961048	-1.990284	0.195187
-145.827685	-9.879284	0.200192
-149.204803	-2.122761	0.205197
-153.417086	0.630950	0.210202
-157.128885	-12.371509	0.215206
-161.449975	2.970907	0.220211
-165.008654	4.514913	0.225216
-168.670455	-2.504731	0.230221
-172.315271	-1.869477	0.235226
-175.930028	-9.699272	0.240230
-179.688452	5.818316	0.245235
-183.060483	-5.139422	0.250240
-187.236500	2.140672	0.255245
-190.979576	5.964429	0.260250
-194.355724	-4.473823	0.265254
-198.249843	6.978031	0.270259
-202.091087	12.329754	0.275264
-205.974857	-0.170533	0.280269
-209.827585	1.999199	0.285274
-213.286362	-5.571583	0.290278
-217.380296	5.527414	0.295283
-221.009829	-1.429488	0.300288
-224.787177	-9.449298	0.305293
-228.968310	2.650792	0.310298
-232.416907	2.562546	0.315302
-235.807199	-3.298697	0.320307
-239.414871	1.681492	0.325312
-243.711004	-0.742529	0.330317
-247.253666	-6.588897	0.335322
-250.980686	-1.151257	0.340326
-254.835580	5.054268	0.345331
-258.905585	6.445057	0.350336
-262.087248	-6.960384	0.355341
-266.378872	4.583400	0.360346
-269.697753	0.089048	0.365350
-273.591087	10.012842	0.370355
-277.225041	2.254073	0.375360
-281.261679	-10.199595	0.380365
-285.408327	4.006595	0.385370
-288.843786	-8.839483	0.390374
-292.222129	-1.092037	0.395379
-296.071250	-5.501711	0.400384
-300.058570	-8.179923	0.405389
-304.234235	4.154379	0.410394
-307.517532	-8.542496	0.415398
-311.638827	0.468424	0.420403
-315.246656	-3.476695	0.425408
-318.904165	2.831458	0.430413
-322.571202	-2.091359	0.435418
-326.147355	-5.626784	0.440422
-330.092214	1.279182	0.445427
-333.737650	-2.705636	0.450432
-337.455433	-11.256732	0.455437
-341.428042	2.554337	0.460442
-344.783350	-4.122873	0.465446
-348.902507	-0.276687	0.470451
-352.705862	3.465475	0.475456
-356.566851	-6.100352	0.480461
-360.612509	0.030133	0.485466
-364.238905	0.435657	0.490470
-367.874338	3.624338	0.495475
-371.411255	-9.560221	0.500480
-375.003719	-2.347754	0.505485
-379.053890	-5.730149	0.510490
-382.940496	-3.575235	0.515494
-386.677663	2.146499	0.520499
-390.304584	-2.935577	0.525504
-393.767636	-10.374514	0.530509
-397.804255	-6.379002	0.535514
-401.480345	-10.226355	0.540518
-405.382880	-3.822187	0.545523
-409.162752	-1.239579	0.550528
-413.005475	0.895760	0.555533
-416.922972	0.999342	0.560538
-420.432808	-4.522423	0.565542
-424.201670	1.691700	0.570547
-427.833930	3.812381	0.575552
-431.390148	1.437709	0.580557
-435.905351	7.495063	0.585562
-439.164159	-7.834270	0.590566
-442.943740	9.292381	0.595571
-446.785353	-1.039623	0.600576
-450.121522	0.530769	0.605581
-454.195278	9.371910	0.610586
-457.722478	-5.178111	0.615590
-462.031644	-7.776269	0.620595
-465.598496	3.683644	0.625600
-468.951653	-3.900462	0.630605
-473.140974	1.614492	0.635610
-476.631786	-8.342974	0.640614
-480.872333	-9.578550	0.645619
-484.525732	1.158782	0.650624
-488.069954	8.727982	0.655629
-492.019448	-0.689442	0.660634
-495.404801	-6.353971	0.665638
-499.600475	-2.211465	0.670643
-503.363795	3.962470	0.675648
-506.872765	-7.956905	0.680653
-510.824337	-2.314282	0.685658
-514.339812	-5.300875	0.690662
-518.315930	-0.184168	0.695667
-521.872667	8.088812	0.700672
-525.603974	-2.580790	0.705677
-529.800926	-2.400851	0.710682
-533.361401	-2.721526	0.715686
-536.911259	-0.568112	0.720691
-540.890939	-3.747024	0.725696
-544.352500	-6.180796	0.730701
-548.306726	3.970752	0.735706
-551.741537	4.262381	0.740710
-555.563738	0.049105	0.745715
-559.217346	-5.378520	0.750720
-563.019761	-4.873617	0.755725
-567.100046	-1.686122	0.760730
-570.861476	-1.569371	0.765734
-574.649288	-5.496375	0.770739
-578.655990	-1.574727	0.775744
-582.434763	-5.354931	0.780749
-586.095527	1.201709	0.785754
-589.687943	-4.842760	0.790758
-593.353427	-4.323414	0.795763
-597.398354	-4.191295	0.800768
-600.834984	-2.864840	0.805773
-604.851038	-3.186745	0.810778
-608.342982	-4.861798	0.815782
-612.059330	-6.226611	0.820787
-616.147443	-6.027637	0.825792
-619.753154	-7.845344	0.830797
-623.884481	2.992192	0.835802
-627.452748	-7.392626	0.840806
-630.949655	-0.630291	0.845811
-634.860896	-6.248443	0.850816
-638.373883	-5.485313	0.855821
-642.405483	-6.255672	0.860826
-646.373841	-3.308273	0.865830
-650.105891	-1.311662	0.870835
-653.928455	3.079000	0.875840
-657.162785	-7.961509	0.880845
-661.074689	-0.341210	0.885850
-664.261577	-2.053881	0.890854
-668.406124	-5.838579	0.895859
-672.612017	2.591945	0.900864
-675.999500	-0.093163	0.905869
-680.472612	1.581940	0.910874
-683.956572	-7.887447	0.915878
-687.502144	-3.561493	0.920883
-691.232550	0.185308	0.925888
-694.810893	2.969545	0.930893
-698.668723	2.710824	0.935898
-702.100261	-4.529253	0.940902
-706.554805	3.477445	0.945907
-710.424056	1.437064	0.950912
-713.341366	-2.346545	0.955917
-717.596219	-2.114445	0.960922
-721.050989	-0.360725	0.965926
-724.978152	-3.483059	0.970931
-728.806430	-0.578409	0.975936
-732.454322	-3.612896	0.980941
-736.839143	-2.839607	0.985946
-740.424845	-1.706744	0.990950
-743.838487	-8.646846	0.995955
-747.894830	1.172830	1.000960
-751.794153	-6.129606	1.005965
-755.133985	7.905815	1.010970
-758.663916	-4.844000	1.015974
-762.650525	-9.298732	1.020979
-766.351572	-9.998706	1.025984
-770.008805	-5.851903	1.030989
-774.223313	-2.661530	1.035994
-777.570551	-9.612192	1.040998
-781.587925	-8.227354	1.046003
-785.392623	-0.534109	1.051008
-788.902634	6.796662	1.056013
-792.963255	8.082778	1.061018
-796.185369	-10.072984	1.066022
-800.436856	-8.365273	1.071027
-804.110768	0.462983	1.076032
-808.062712	-2.939096	1.081037
-812.122539	-0.717957	1.086042
-815.646275	-5.792198	1.091046
-819.334807	-1.105740	1.096051
-822.861988	-3.110725	1.101056
-826.102957	1.087897	1.106061
-829.918314	1.194757	1.111066
-833.666484	-9.693968	1.116070
-838.040623	-12.558583	1.121075
-841.625534	5.100466	1.126080
-845.369060	-14.758521	1.131085
-849.283598	-6.790585	1.136090
-853.313341	-5.327956	1.141094
-857.125287	1.852482	1.146099
-860.389959	-3.263103	1.151104
-864.095488	-14.967550	1.156109
-868.200606	-10.020463	1.161114
-871.606825	-3.493058	1.166118
-875.521841	-3.390693	1.171123
-879.427471	-1.413283	1.176128
-882.977756	-16.115014	1.181133
-887.216214	-4.104044	1.186138
-890.674442	-8.605178	1.191142
-894.557466	-7.131243	1.196147
-897.928969	5.386112	1.201152
-901.524813	-4.388314	1.206157
-905.475023	-5.890310	1.211162
-908.825598	-5.066015	1.216166
-913.392684	-7.923294	1.221171
-917.398947	-3.499696	1.226176
-920.767086	-14.758104	1.231181
-924.721058	5.024251	1.236186
-928.031077	-9.556557	1.241190
-931.947201	-0.279389	1.246195
-935.724390	-5.522650	1.251200
-939.482241	-3.185578	1.256205
-943.600270	1.716396	1.261210
-947.225650	-5.419771	1.266214
-950.636572	-16.742251	1.271219
-954.193053	-0.713411	1.276224
-957.718652	-15.420541	1.281229
-962.349452	-5.975437	1.286234
-965.999199	-4.751570	1.291238
-969.551639	-16.224853	1.296243
-973.590413	-0.260788	1.301248
-977.126633	-12.745885	1.306253
-980.874024	-4.847045	1.311258
-984.488679	-4.614337	1.316262
-988.275968	-5.666014	1.321267
-992.186510	-2.063406	1.326272
-995.926827	-7.886460	1.331277
-999.619417	-5.127654	1.336282
-1003.103872	-20.341166	1.341286
-1007.006838	-11.630529	1.346291
-1011.134899	-6.591222	1.351296
-1014.834700	-5.695159	1.356301
-1019.052747	1.541012	1.361306
-1022.328175	-3.049080	1.366310
-1025.884733	-10.803237	1.371315
-1030.063917	-0.755308	1.376320
-1033.415478	0.379975	1.381325
-1037.559161	2.253794	1.386330
-1041.124078	1.694906	1.391334
-1044.778408	-6.299047	1.396339
-1048.606825	-2.244290	1.401344
-1051.918719	-11.567148	1.406349
-1056.214996	-4.990171	1.411354
-1059.872166	-10.471609	1.416358
-1063.516896	-5.301365	1.421363
-1067.338178	-0.203798	1.426368
-1071.070724	-12.023416	1.431373
-1075.081749	-6.368799	1.436378
-1078.841393	-6.123792	1.441382
-1082.518985	-1.683106	1.446387
-1086.373652	5.964982	1.451392
-1089.759013	-6.676526	1.456397
-1093.616675	7.063692	1.461402
-1097.396978	-0.897412	1.466406
-1101.298259	-3.827705	1.471411
-1105.393451	6.129651	1.476416
-1108.543754	-0.143983	1.481421
-1112.331959	-0.348506	1.486426
-1116.340429	-1.490747	1.491430
-1119.897876	-0.257753	1.496435
-1123.860882	2.173930	1.501440
-1127.611548	-4.117173	1.506445
-1131.276149	4.763691	1.511450
-1134.850695	4.433563	1.516454
-1138.810598	-2.019587	1.521459
-1142.962170	-7.443875	1.526464
-1146.746142	-1.514808	1.531469
-1150.296978	3.205319	1.536474
-1153.498432	-6.958207	1.541478
-1157.462343	-10.122805	1.546483
-1161.156023	-2.303244	1.551488
-1165.058324	-4.391191	1.556493
-1169.262307	6.151366	1.561498
-1173.112819	5.368719	1.566502
-1176.406526	6.378258	1.571507
-1180.291286	10.178898	1.576512
-1183.700730	1.176185	1.581517
-1187.692003	1.813234	1.586522
-1191.463117	-2.397690	1.591526
-1195.205464	2.491914	1.596531
-1199.421249	8.001313	1.601536
-1202.800826	4.595065	1.606541
-1206.754132	2.346619	1.611546
-1210.167040	-2.771546	1.616550
-1213.650912	-7.687543	1.621555
-1217.946172	-0.500174	1.626560
-1221.414000	-4.980343	1.631565
-1225.755171	8.675020	1.636570
-1229.341436	-2.839740	1.641574
-1232.383028	-1.900426	1.646579
-1236.233006	6.734297	1.651584
-1240.467752	-7.019971	1.656589
-1244.123221	0.273219	1.661594
-1247.758939	-0.225137	1.666598
-1251.859935	0.027466	1.671603
-1255.891907	-6.443903	1.676608
-1259.129607	-10.134535	1.681613
-1263.097583	3.962625	1.686618
-1266.709252	2.028610	1.691622
-1270.294480	-1.973815	1.696627
-1274.098097	0.407382	1.701632
-1277.932710	-2.555355	1.706637
-1282.178311	9.577279	1.711642
-1285.657855	2.326861	1.716646
-1288.922631	0.540787	1.721651
-1292.922418	4.451479	1.726656
-1296.944762	3.680771	1.731661
-1300.845386	11.484784	1.736666
-1304.519198	-3.262709	1.741670
-1308.213923	-4.462715	1.746675
-1311.920719	6.689622	1.751680
-1315.445871	-2.204478	1.756685
-1319.099930	5.009754	1.761690
-1323.102768	-3.311148	1.766694
-1326.852384	-2.261542	1.771699
-1330.503992	4.178050	1.776704
-1334.305367	-6.292874	1.781709
-1338.428642	-4.629944	1.786714
-1342.197528	0.688327	1.791718
-1345.679399	3.131677	1.796723
-1349.729023	1.107049	1.801728
-1352.981136	-6.376776	1.806733
-1357.063611	3.916419	1.811738
-1360.694988	-0.677702	1.816742
-1364.448814	-7.412587	1.821747
-1368.480938	2.771643	1.826752
-1371.766272	-2.428196	1.831757
-1375.678620	1.027103	1.836762
-1379.747147	7.153473	1.841766
-1383.455427	-0.659399	1.846771
-1387.083405	0.506447	1.851776
-1390.795333	-7.548670	1.856781
-1394.821423	-7.670495	1.861786
-1398.277703	-2.782217	1.866790
-1401.844416	-2.348382	1.871795
-1405.990243	10.006604	1.876800
-1409.655840	-1.561383	1.881805
-1413.456781	-0.531805	1.886810
-1417.215187	-7.694787	1.891814
-1420.717169	-9.434811	1.896819
-1424.750088	-5.073903	1.901824
-1428.539708	-4.657955	1.906829
-1432.240937	2.188693	1.911834
-1435.873843	-0.457573	1.916838
-1439.580402	-3.490998	1.921843
-1443.469450	-4.112484	1.926848
-1447.119394	-9.704829	1.931853
-1451.187181	-9.733148	1.936858
-1455.040496	-9.105113	1.941862
-1458.378607	-5.254355	1.946867
-1462.633526	2.154067	1.951872
-1465.920318	-5.637843	1.956877
-1469.684900	1.375121	1.961882
-1473.746005	3.296411	1.966886
-1477.775732	2.962430	1.971891
-1481.477047	-1.268644	1.976896
-1485.080134	-3.069648	1.981901
-1488.290724	6.167968	1.986906
-1492.371412	8.212273	1.991910
-1496.154601	-4.117305	1.996915
-1500.253580	0.735955	2.006912
-1501.092560	5.114542	2.016909
-1498.614960	0.630016	2.026906
-1495.553144	-6.935394	2.036902
-1493.447787	-3.557228	2.046899
-1491.821018	-2.106088	2.056896
-1489.595401	3.374910	2.066893
-1487.799712	-4.592481	2.076890
-1485.988354	-0.881444	2.086886
-1483.985133	1.322573	2.096883
-1482.359915	-2.011774	2.106880
-1480.171017	-2.865877	2.116877
-1478.369935	-6.599428	2.126874
-1476.324319	-4.999030	2.136870
-1474.638824	-5.559366	2.146867
-1472.589248	2.335602	2.156864
-1470.949163	-2.556365	2.166861
-1468.860419	-3.887047	2.176858
-1466.941541	-0.379524	2.186854
-1464.953667	-0.086699	2.196851
-1463.273236	1.155345	2.206848
-1461.492585	-5.423316	2.216845
-1459.437133	-0.005042	2.226842
-1457.244812	-2.999124	2.236838
-1455.664653	0.224751	2.246835
-1454.084899	1.651868	2.256832
-1452.011224	5.273567	2.266829
-1450.185509	2.660291	2.276826
-1447.963803	0.542556	2.286822
-1446.234754	-3.190492	2.296819
-1444.465984	2.494749	2.306816
-1442.399798	0.616654	2.316813
-1440.441248	-1.670517	2.326810
-1438.717239	-2.492780	2.336806
-1436.886103	-3.262721	2.346803
-1434.709878	-0.802152	2.356800
-1433.400854	-1.327446	2.366797
-1431.449558	-0.954526	2.376794
-1429.013613	-0.056045	2.386790
-1427.160320	-4.888961	2.396787
-1425.702726	-0.922290	2.406784
-1423.457804	1.502029	2.416781
-1421.847885	3.001707	2.426778
-1420.120421	-3.888935	2.436774
-1418.056489	-4.187714	2.446771
-1416.125499	-0.764190	2.456768
-1414.373634	-5.445069	2.466765
-1412.529776	-10.304882	2.476762
-1410.640929	-8.823011	2.486758
-1408.540971	0.009733	2.496755
-1406.685953	-9.421294	2.506752
-1404.939274	-1.161984	2.516749
-1403.131183	-1.675579	2.526746
-1400.881654	-4.402454	2.536742
-1399.271677	-6.213792	2.546739
-1397.238210	-2.566660	2.556736
-1395.654006	-7.991204	2.566733
-1393.613935	-8.156669	2.576730
-1391.532451	-6.309308	2.586726
-1390.049025	-6.668288	2.596723
-1388.217060	-5.180449	2.606720
-1386.136799	-6.228649	2.616717
-1384.115591	-4.442683	2.626714
-1381.628395	-0.438700	2.636710
-1379.404365	-1.802012	2.646707
-1378.155599	-2.958676	2.656704
-1376.902761	5.608661	2.666701
-1376.141462	0.639537	2.676698
-1373.560171	6.407928	2.686694
-1370.890666	4.378055	2.696691
-1369.143057	3.435224	2.706688
-1367.240324	3.182820	2.716685
-1365.479825	-1.339936	2.726682
-1363.545169	-1.027452	2.736678
-1361.941628	-4.577719	2.746675
-1359.859506	-0.459923	2.756672
-1357.697794	0.360953	2.766669
-1356.015084	1.542713	2.776666
-1354.234732	1.376225	2.786662
-1352.119251	-2.110720	2.796659
-1350.391437	4.125887	2.806656
-1348.497070	-3.786151	2.816653
-1346.659343	-4.006028	2.826650
-1344.904454	-0.814778	2.836646
-1342.638295	0.928860	2.846643
-1340.878429	-4.556926	2.856640
-1339.298273	-8.883427	2.866637
-1337.538275	-8.391388	2.876634
-1335.322673	-0.693386	2.886630
-1333.395021	-3.727096	2.896627
-1331.619129	-2.762337	2.906624
-1329.854041	-2.490578	2.916621
-1328.072493	-2.690395	2.926618
-1325.871033	-6.295287	2.936614
-1324.006240	-0.603212	2.946611
-1321.932212	-2.820348	2.956608
-1320.272812	-1.025362	2.966605
-1318.671016	3.786716	2.976602
-1316.466139	5.025456	2.986598
-1315.045327	-4.192332	2.996595
-1313.196151	8.299570	3.006592
-1310.879856	0.915286	3.016589
-1309.152200	-0.303778	3.026586
-1307.392664	3.968329	3.036582
-1305.042224	-2.451946	3.046579
-1303.394045	0.797468	3.056576
-1301.581588	6.870571	3.066573
-1299.822385	-4.076618	3.076570
-1297.924578	2.273350	3.086566
-1295.904389	-0.809877	3.096563
-1294.181404	5.358077	3.106560
-1291.828823	-2.712517	3.116557
-1290.403758	-5.736809	3.126554
-1288.687348	-6.600376	3.136550
-1286.582782	-6.551860	3.146547
-1284.595120	-4.068863	3.156544
-1282.736449	-5.285191	3.166541
-1281.040782	-1.448102	3.176538
-1279.008062	-3.555959	3.186534
-1277.248525	1.350904	3.196531
-1275.172709	-3.634351	3.206528
-1273.376513	-6.528555	3.216525
-1271.799420	-0.049872	3.226522
-1269.722752	-2.526330	3.236518
-1267.807459	-3.652235	3.246515
-1265.897896	-0.940408	3.256512
-1264.371883	2.409112	3.266509
-1262.315927	0.944914	3.276506
-1260.248330	1.447787	3.286502
-1258.255041	-2.744252	3.296499
-1256.605924	1.229778	3.306496
-1254.501874	0.424202	3.316493
-1252.645771	0.100407	3.326490
-1250.995428	-0.116250	3.336486
-1249.267724	1.052073	3.346483
-1247.047843	-2.718326	3.356480
-1245.092991	1.522576	3.366477
-1243.369468	4.259456	3.376474
-1241.574604	0.397600	3.386470
-1239.625749	0.407918	3.396467
-1237.735797	4.136585	3.406464
-1235.881439	3.162561	3.416461
-1234.262391	7.905628	3.426458
-1232.253194	2.233177	3.436454
-1229.879949	-1.176488	3.446451
-1228.539246	6.086894	3.456448
-1226.667410	4.506926	3.466445
-1224.745890	4.712682	3.476442
-1222.458238	-0.838527	3.486438
-1220.902643	-3.615247	3.496435
-1219.198164	-2.092661	3.506432
-1217.023729	1.435767	3.516429
-1215.284517	2.987535	3.526426
-1213.145302	0.070067	3.536422
-1211.510283	-1.827256	3.546419
-1209.981253	8.949139	3.556416
-1207.855819	3.815474	3.566413
-1205.862935	1.481949	3.576410
-1203.766068	-1.839258	3.586406
-1202.098882	1.512980	3.596403
-1200.423949	5.386609	3.606400
-1198.178285	-1.915217	3.616397
-1196.474322	5.743218	3.626394
-1194.670513	5.230469	3.636390
-1192.590010	-7.256995	3.646387
-1191.065259	4.233775	3.656384
-1189.139944	5.619999	3.666381
-1186.954464	7.870909	3.676378
-1185.190153	3.813456	3.686374
-1183.428123	-1.640988	3.696371
-1181.538212	2.198258	3.706368
-1179.482901	7.413141	3.716365
-1177.597217	6.737307	3.726362
-1175.904848	10.368168	3.736358
-1173.955217	4.613714	3.746355
-1172.152153	4.491100	3.756352
-1170.032129	-1.273241	3.766349
-1168.438521	-6.857042	3.776346
-1166.417621	-4.224523	3.786342
-1164.571592	-2.010863	3.796339
-1163.054952	-3.404480	3.806336
-1160.963735	4.127292	3.816333
-1158.943592	-4.144202	3.826330
-1156.843984	-0.660586	3.836326
-1155.117401	-5.637237	3.846323
-1153.326682	-4.999972	3.856320
-1151.429499	0.731282	3.866317
-1149.721963	-0.964444	3.876314
-1147.825786	-4.635597	3.886310
-1145.760293	-11.575393	3.896307
-1143.714684	-1.792643	3.906304
-1142.037281	1.952740	3.916301
-1140.250156	2.197435	3.926298
-1138.390214	-1.412653	3.936294
-1136.591531	2.196491	3.946291
-1134.552121	-4.098077	3.956288
-1132.657259	-4.211662	3.966285
-1130.722826	-0.619494	3.976282
-1128.832954	-2.874897	3.986278
-1127.279676	-1.631210	3.996275
-1125.053798	0.974873	4.006272
-1123.462938	-0.819011	4.016269
-1121.355144	0.937550	4.026266
-1119.354636	1.340756	4.036262
-1117.526883	-3.203634	4.046259
-1115.828509	2.328930	4.056256
-1114.088020	-0.849928	4.066253
-1112.178350	-2.137438	4.076250
-1110.271130	1.553839	4.086246
-1108.118337	-3.355170	4.096243
-1106.338322	2.265395	4.106240
-1104.764168	4.110491	4.116237
-1102.564135	-3.701842	4.126234
-1100.627694	-4.906783	4.136230
-1099.058818	2.594918	4.146227
-1096.840142	5.846389	4.156224
-1095.278945	-0.646390	4.166221
-1093.373297	-2.755868	4.176218
-1091.191762	-0.603709	4.186214
-1089.414155	-4.439009	4.196211
-1087.663623	-8.827341	4.206208
-1085.831400	-3.548269	4.216205
-1084.158338	-5.532116	4.226202
-1082.003575	-5.415655	4.236198
-1079.919880	-2.824680	4.246195
-1078.345401	-4.649071	4.256192
-1076.303539	-2.232980	4.266189
-1074.460779	-7.774469	4.276186
-1072.707446	-9.976409	4.286182
-1070.770857	-3.375078	4.296179
-1068.673109	-7.109989	4.306176
-1067.080814	-1.443580	4.316173
-1065.286317	-8.328915	4.326170
-1063.198069	-12.224932	4.336166
-1061.545260	-8.780291	4.346163
-1059.728989	-5.693371	4.356160
-1057.686733	-2.198911	4.366157
-1055.799032	-4.423909	4.376154
-1053.652074	-1.549345	4.386150
-1051.998137	-3.299586	4.396147
-1050.259735	-6.896483	4.406144
-1048.308950	-5.372111	4.416141
-1046.370096	-5.312663	4.426138
-1044.433497	-3.017076	4.436134
-1042.300614	-7.910209	4.446131
-1040.667712	-3.278164	4.456128
-1038.895662	-3.752556	4.466125
-1037.154905	1.594871	4.476122
-1035.486537	-8.229204	4.486118
-1033.152244	-3.390382	4.496115
-1031.333727	-5.544297	4.506112
-1029.199688	-0.839232	4.516109
-1027.520872	-4.297111	4.526106
-1025.864078	-8.638829	4.536102
-1023.902906	-6.369260	4.546099
-1022.013888	-0.038168	4.556096
-1020.052290	-0.773385	4.566093
-1018.293417	-0.441974	4.576090
-1016.585915	-1.837600	4.586086
-1014.135661	-6.854097	4.596083
-1012.503952	-4.767091	4.606080
-1010.968073	-3.182649	4.616077
-1009.163788	0.784121	4.626074
-1006.805503	-5.506076	4.636070
-1004.898765	-2.371999	4.646067
-1003.401015	-5.336697	4.656064
-1001.248169	-0.252509	4.666061
-999.374389	5.179466	4.676058
-997.522929	-3.293874	4.686054
-995.716060	3.168799	4.696051
-993.844144	-1.924140	4.706048
-992.083874	-4.390815	4.716045
-990.419470	-1.197446	4.726042
-987.963942	2.475727	4.736038
-985.970583	0.952305	4.746035
-984.465372	0.492204	4.756032
-982.984850	-0.507104	4.766029
-980.732692	-4.509790	4.776026
-978.702124	-10.793343	4.786022
-976.815918	-1.638619	4.796019
-975.175257	-3.819313	4.806016
-972.975696	-0.196772	4.816013
-971.275915	-6.129007	4.826010
-969.465425	-0.915834	4.836006
-967.505320	6.730251	4.846003
-965.796746	-3.839158	4.856000
-963.745186	4.982827	4.865997
-961.995733	1.155277	4.875994
-960.207742	-3.445798	4.885990
-958.333380	-0.435977	4.895987
-956.211587	1.391128	4.905984
-954.467461	-1.560830	4.915981
-952.448071	-0.080504	4.925978
-950.645621	-1.884422	4.935974
-948.778189	-4.090306	4.945971
-947.044832	2.076269	4.955968
-944.928459	-4.756241	4.965965
-942.964818	-1.898050	4.975962
-941.313905	-5.479303	4.985958
-939.620653	-4.561027	4.995955
-937.533303	-0.317354	5.005952
-935.653999	0.607493	5.015949
-933.661585	-0.702576	5.025946
-932.090992	-7.395705	5.035942
-930.156900	-6.034352	5.045939
-928.042380	-5.961841	5.055936
-926.282231	-11.778959	5.065933
-924.387760	-10.300742	5.075930
-922.250386	-3.046119	5.085926
-920.690689	-12.625380	5.095923
-918.927464	-4.568832	5.105920
-916.826351	-4.737324	5.115917
-914.803522	-5.119087	5.125914
-913.119583	-1.816679	5.135910
-911.420797	-1.366633	5.145907
-909.497558	-1.473523	5.155904
-907.483534	0.629804	5.165901
-905.862138	3.239589	5.175898
-903.807467	0.223806	5.185894
-901.892928	-4.913773	5.195891
-900.020622	-3.627780	5.205888
-898.121488	-0.047135	5.215885
-896.144350	1.831574	5.225882
-894.207947	-5.617908	5.235878
-892.875896	-5.623953	5.245875
-890.793058	0.478899	5.255872
-888.766332	0.941270	5.265869
-886.859127	-3.778285	5.275866
-884.695644	-2.038305	5.285862
-882.979966	-3.323038	5.295859
-881.439589	-3.750801	5.305856
-879.440304	0.510163	5.315853
-877.367733	0.431532	5.325850
-875.646247	1.528499	5.335846
-873.715580	-4.118478	5.345843
-871.749606	0.531501	5.355840
-870.032797	-4.658129	5.365837
-868.158024	-5.180393	5.375834
-866.371939	3.662020	5.385830
-864.170549	3.660703	5.395827
-862.479366	-1.780615	5.405824
-860.552507	-1.360676	5.415821
-858.898742	-6.437588	5.425818
-856.800509	-6.886618	5.435814
-854.992964	0.332378	5.445811
-853.396320	0.986688	5.455808
-851.513783	2.555296	5.465805
-849.418308	-8.247993	5.475802
-847.284042	-11.560659	5.485798
-845.417693	-9.853671	5.495795
-843.679744	-3.624592	5.505792
-841.731244	-6.138614	5.515789
-840.333068	-8.637297	5.525786
-837.863215	-6.377827	5.535782
-836.170669	-12.136710	5.545779
-834.419565	-10.935500	5.555776
-832.357799	-2.129234	5.565773
-830.599309	-2.230250	5.575770
-828.658383	-6.457783	5.585766
-827.001948	-5.149857	5.595763
-824.969631	-6.733055	5.605760
-822.999029	-4.287978	5.615757
-821.191606	-3.523654	5.625754
-819.180085	-7.798779	5.635750
-817.186475	-11.870513	5.645747
-815.566975	-5.890900	5.655744
-814.141166	-5.675045	5.665741
-811.820686	-3.240093	5.675738
-809.566810	-13.894981	5.685734
-808.167359	-4.305463	5.695731
-806.411217	-5.255558	5.705728
-804.455706	-5.274362	5.715725
-802.439594	2.287132	5.725722
-800.671907	-6.223207	5.735718
-798.776924	-6.399700	5.745715
-797.053430	-3.075107	5.755712
-795.063255	-5.107860	5.765709
-792.809288	-4.418042	5.775706
-790.930486	-4.438785	5.785702
-789.220195	-11.619943	5.795699
-787.545205	0.371335	5.805696
-785.639646	-0.817362	5.815693
-783.687562	1.152290	5.825690
-781.728625	-3.535980	5.835686
-779.686834	-6.126442	5.845683
-778.045326	-2.106627	5.855680
-776.096804	-5.607440	5.865677
-774.519175	-2.883200	5.875674
-772.551810	-6.634916	5.885670
-770.414661	-3.804307	5.895667
-768.529705	-8.974951	5.905664
-766.783801	-3.411816	5.915661
-764.941497	-2.773023	5.925658
-763.002478	-2.620209	5.935654
-761.161040	-4.267585	5.945651
-759.540669	0.232463	5.955648
-757.412318	3.222387	5.965645
-755.536244	-0.475254	5.975642
-753.607323	-5.668704	5.985638
-751.580735	1.949584	5.995635
-750.064160	-1.761653	6.005632
-748.297963	-0.798052	6.015629
-746.432574	3.304430	6.025626
-744.163451	-1.733382	6.035622
-742.287281	2.078434	6.045619
-740.604077	8.684245	6.055616
-738.508708	1.984732	6.065613
-736.538873	6.362637	6.075610
-734.934832	1.710590	6.085606
-733.139072	3.602635	6.095603
-731.097181	5.703244	6.105600
-729.176932	4.381191	6.115597
-727.184409	-2.082402	6.125594
-725.562156	-2.243675	6.135590
-723.683998	-2.262682	6.145587
-722.121499	2.262432	6.155584
-719.779469	-2.130167	6.165581
-717.955457	-2.221043	6.175578
-716.130271	-4.050525	6.185574
-714.358412	3.764820	6.195571
-712.151363	1.568005	6.205568
-710.572710	5.151075	6.215565
-708.814502	3.076511	6.225562
-706.731676	5.112179	6.235558
-704.456936	2.435608	6.245555
-702.937339	1.117598	6.255552
-701.027688	1.753575	6.265549
-699.429349	2.720351	6.275546
-697.391868	-4.879348	6.285542
-695.702603	3.250788	6.295539
-693.863179	2.418521	6.305536
-691.723072	2.736629	6.315533
-689.923425	3.330193	6.325530
-687.914768	0.342470	6.335526
-685.982122	3.303731	6.345523
-683.898027	0.288168	6.355520
-682.738425	7.026634	6.365517
-680.715378	-0.406538	6.375514
-678.449664	-3.449537	6.385510
-676.604873	1.463136	6.395507
-674.746352	0.346779	6.405504
-672.647929	1.678933	6.415501
-671.147123	-0.073423	6.425498
-669.388380	-4.604882	6.435494
-667.495416	-11.090413	6.445491
-665.599586	-1.003788	6.455488
-663.417662	-4.399701	6.465485
-661.643786	-7.143047	6.475482
-659.936953	-10.189890	6.485478
-657.978318	-2.996449	6.495475
-655.789443	-6.905043	6.505472
-654.365701	-0.892450	6.515469
-652.404640	-4.614644	6.525466
-650.497933	-5.760785	6.535462
-648.481052	-4.320846	6.545459
-646.492536	-2.840057	6.555456
-644.786189	-4.851024	6.565453
-642.953953	-5.980525	6.575450
-641.301105	-3.006104	6.585446
-639.184782	-3.413621	6.595443
-637.545207	0.095029	6.605440
-635.775722	-4.059176	6.615437
-633.375820	-1.665153	6.625434
-631.461369	-5.523568	6.635430
-629.781907	1.564503	6.645427
-627.941476	-6.748924	6.655424
-626.319907	-1.538444	6.665421
-624.226426	-5.044928	6.675418
-622.039786	-9.622609	6.685414
-620.325275	-1.406448	6.695411
-618.572732	0.809958	6.705408
-616.970771	-0.944314	6.715405
-614.937591	-0.073790	6.725402
-613.103114	-2.733626	6.735398
-610.796306	-3.608917	6.745395
-608.961790	-1.326652	6.755392
-607.326856	1.191183	6.765389
-605.614808	-4.993825	6.775386
-603.647179	4.555600	6.785382
-601.898547	-2.931567	6.795379
-599.419696	-4.956962	6.805376
-598.049621	2.223190	6.815373
-596.061429	0.448285	6.825370
-594.192793	-1.965941	6.835366
-592.248403	-6.086477	6.845363
-590.419966	-4.027437	6.855360
-588.856239	-1.387688	6.865357
-586.500548	2.957131	6.875354
-584.732366	-3.088410	6.885350
-582.720924	-1.693334	6.895347
-581.063716	-6.622197	6.905344
-579.224928	-0.349011	6.915341
-577.274106	5.783124	6.925338
-575.434568	4.857771	6.935334
-573.419222	3.012231	6.945331
-571.841417	-0.623417	6.955328
-569.780113	-3.205769	6.965325
-567.777061	-4.724077	6.975322
-566.141180	0.828373	6.985318
-563.924201	-4.003578	6.995315
-562.503254	-0.831004	7.005312
-560.412704	-4.490126	7.015309
-558.511703	0.132614	7.025306
-556.434414	-1.771754	7.035302
-554.865566	-3.814380	7.045299
-552.966655	5.326070	7.055296
-551.053024	0.807845	7.065293
-549.095354	3.348382	7.075290
-547.382729	-0.097206	7.085286
-545.301823	-2.297405	7.095283
-543.428141	3.491818	7.105280
-541.548213	-0.141542	7.115277
-539.838710	-1.164519	7.125274
-538.122919	4.294664	7.135270
-536.101561	1.587667	7.145267
-534.096145	-1.500466	7.155264
-532.345151	1.131517	7.165261
-530.446486	6.226761	7.175258
-528.566787	-2.923400	7.185254
-526.617903	-1.311441	7.195251
-524.809450	-3.226528	7.205248
-522.926692	-4.596113	7.215245
-520.872248	-6.678380	7.225242
-519.195494	0.530210	7.235238
-517.040188	-3.079218	7.245235
-515.327983	0.893185	7.255232
-513.632495	0.723518	7.265229
-511.606982	2.129040	7.275226
-509.708414	-11.843068	7.285222
-508.056189	2.013663	7.295219
-506.031053	-0.798123	7.305216
-504.091343	-3.217316	7.315213
-502.074196	-2.437293	7.325210
-500.276926	-5.337418	7.335206
-498.607511	-1.361328	7.345203
-496.598213	-4.544787	7.355200
-494.569159	4.189667	7.365197
-492.883836	3.846375	7.375194
-491.074009	-1.904176	7.385190
-489.041158	-7.399813	7.395187
-487.096518	0.306020	7.405184
-485.425522	-0.317610	7.415181
-483.377812	-1.143507	7.425178
-481.752720	-4.691912	7.435174
-479.951530	-10.649494	7.445171
-477.686009	-5.660164	7.455168
-475.658540	-2.687027	7.465165
-474.163809	-12.707246	7.475162
-472.196065	-4.010354	7.485158
-470.501726	-1.591909	7.495155
-468.582285	-9.398369	7.505152
-466.650354	-1.652594	7.515149
-464.469049	-6.451918	7.525146
-462.564317	2.013470	7.535142
-460.735799	-9.286892	7.545139
-459.075711	-1.483489	7.555136
-457.251003	-0.787960	7.565133
-455.465815	3.250203	7.575130
-453.715999	-4.265477	7.585126
-451.638843	-4.677627	7.595123
-449.788648	-1.853001	7.605120
-447.416401	-1.573320	7.615117
-446.000727	-4.481946	7.625114
-443.966041	-9.240471	7.635110
-442.235889	-1.490874	7.645107
-440.543278	-4.478455	7.655104
-438.589254	2.401713	7.665101
-436.421061	-2.734969	7.675098
-434.338890	-6.640542	7.685094
-432.565001	-10.842676	7.695091
-431.195023	-7.008197	7.705088
-429.151859	-5.813844	7.715085
-427.362739	-5.922611	7.725082
-425.371779	0.648512	7.735078
-423.301971	-3.941922	7.745075
-421.523755	-5.863157	7.755072
-419.810125	-5.846180	7.765069
-417.750128	-6.512930	7.775066
-415.697781	-5.381611	7.785062
-414.256903	0.789459	7.795059
-412.070380	-0.754858	7.805056
-410.451268	-3.749631	7.815053
-408.469082	-14.253438	7.825050
-406.507054	-5.241362	7.835046
-404.504984	-3.948847	7.845043
-402.535887	-11.709503	7.855040
-401.004544	-9.504984	7.865037
-399.442599	-1.962181	7.875034
-397.007708	-4.166667	7.885030
-395.297640	-1.960679	7.895027
-393.414089	-4.175028	7.905024
-391.364404	0.334113	7.915021
-389.852040	-2.960972	7.925018
-387.692119	-9.114713	7.935014
-385.727501	-1.094610	7.945011
-384.107989	0.716897	7.955008
-382.109802	-1.433641	7.965005
-380.385193	-3.737869	7.975002
-378.307416	0.357852	7.984998
-376.294611	-0.427644	7.994995
-374.598032	-6.910033	8.004992
-373.004110	4.346117	8.014989
-371.322817	-7.218053	8.024986
-368.809922	-0.059154	8.034982
-367.063191	-1.157427	8.044979
-365.201351	-3.095131	8.054976
-363.431910	2.085622	8.064973
-361.262319	0.397210	8.074970
-359.795024	0.680926	8.084966
-357.921628	-3.840202	8.094963
-355.776902	1.512748	8.104960
-353.770649	-2.363270	8.114957
-351.963781	0.501510	8.124954
-350.182285	-2.467043	8.134950
-348.341177	-5.865112	8.144947
-346.991978	-9.835177	8.154944
-344.657244	-0.374119	8.164941
-342.583182	-4.565691	8.174938
-340.635094	-6.176091	8.184934
-339.152156	1.527793	8.194931
-337.138277	-4.902595	8.204928
-335.489874	-1.641452	8.214925
-333.196776	-3.878503	8.224922
-331.301534	-6.457831	8.234918
-329.568819	-2.801195	8.244915
-327.677191	-1.058351	8.254912
-326.297118	-1.011744	8.264909
-323.667231	-6.072031	8.274906
-322.091893	-10.040288	8.284902
-320.412659	-7.655638	8.294899
-318.506944	-13.514529	8.304896
-316.613774	-2.786111	8.314893
-314.437509	-2.337644	8.324890
-312.504657	-7.319810	8.334886
-310.564187	-11.490029	8.344883
-308.932071	-5.210471	8.354880
-307.252149	-7.308565	8.364877
-305.590684	-7.264232	8.374874
-303.375510	-2.697744	8.384870
-301.416841	2.700748	8.394867
-299.525644	-7.834252	8.404864
-297.805135	-2.290374	8.414861
-295.891608	-9.639450	8.424858
-293.893249	-8.796250	8.434854
-292.190301	-7.316947	8.444851
-290.158491	-5.351712	8.454848
-288.267698	-2.718174	8.464845
-286.409176	0.825256	8.474842
-284.429751	-10.064868	8.484838
-282.656043	-9.703698	8.494835
-280.841420	-6.030099	8.504832
-279.090131	-3.647446	8.514829
-277.334300	1.739232	8.524826
-275.235201	-1.838911	8.534822
-273.062001	-6.797831	8.544819
-271.387164	-9.120880	8.554816
-269.504002	-5.601897	8.564813
-267.652186	-0.120005	8.574810
-265.851700	-10.430501	8.584807
-264.056862	0.168398	8.594803
-262.130507	-0.012676	8.604800
-260.014524	-0.478226	8.614797
-258.362842	-0.724406	8.624794
-256.536485	-5.700586	8.634791
-254.435624	-4.058973	8.644787
-252.880398	1.522373	8.654784
-250.795179	2.317010	8.664781
-248.885068	-2.524112	8.674778
-247.111261	0.873397	8.684775
-244.966419	-4.766240	8.694771
-243.373605	-2.997743	8.704768
-241.392851	2.318329	8.714765
-239.381473	-4.228428	8.724762
-237.301452	-10.018764	8.734759
-235.602850	-0.850802	8.744755
-233.874048	0.783893	8.754752
-232.202319	-1.008107	8.764749
-230.261721	-7.283031	8.774746
-228.348108	-3.429398	8.784743
-226.330824	-6.304440	8.794739
-224.287347	-3.234163	8.804736
-222.603257	-13.713949	8.814733
-220.741990	-9.234587	8.824730
-219.124131	-11.703245	8.834727
-217.079550	-13.832631	8.844723
-215.104955	-8.446084	8.854720
-213.314513	-14.782294	8.864717
-211.431858	-9.240544	8.874714
-209.670783	-6.739400	8.884711
-207.705000	-5.084084	8.894707
-205.925250	-9.855421	8.904704
-203.663649	-9.022576	8.914701
-202.203426	-11.391856	8.924698
-200.057176	-9.438490	8.934695
-198.176222	-14.590708	8.944691
-196.340900	-10.945610	8.954688
-194.711251	-17.271937	8.964685
-192.608102	-10.216405	8.974682
-190.564248	-5.695101	8.984679
-188.936475	-5.375310	8.994675
-187.097403	-1.056587	9.004672
-185.397332	-4.226767	9.014669
-183.369491	-9.784523	9.024666
-181.281333	-3.157639	9.034663
-179.668945	-10.166471	9.044659
-177.685414	-7.612380	9.054656
-175.575179	-3.488499	9.064653
-173.729581	1.084986	9.074650
-172.093358	-2.458684	9.084647
-170.139511	-1.594067	9.094643
-167.977455	-11.711143	9.104640
-166.459830	-3.082671	9.114637
-164.555396	-4.880178	9.124634
-162.527181	-5.590586	9.134631
-160.863960	-4.223270	9.144627
-159.016077	-7.732809	9.154624
-157.065683	-2.579190	9.164621
-155.209847	2.897418	9.174618
-153.502494	-4.526030	9.184615
-151.301224	-2.150344	9.194611
-149.167419	-8.446564	9.204608
-147.726184	-2.095373	9.214605
-145.902627	-5.454179	9.224602
-143.660079	-5.022449	9.234599
-141.975086	-10.395994	9.244595
-140.212176	-10.509839	9.254592
-138.342900	-5.314841	9.264589
-136.199410	-2.547814	9.274586
-134.467085	-4.286257	9.284583
-132.402467	-1.511379	9.294579
-130.556999	-6.927890	9.304576
-129.004785	1.723513	9.314573
-127.277656	-0.631468	9.324570
-125.205480	1.957473	9.334567
-122.686075	6.352441	9.344563
-121.579126	-5.623639	9.354560
-119.892691	-1.662616	9.364557
-117.610141	2.942252	9.374554
-115.613526	-1.825730	9.384551
-113.610156	-4.453724	9.394547
-112.185633	-6.722519	9.404544
-110.237506	-3.254822	9.414541
-108.169035	-2.048440	9.424538
-106.212229	-3.011095	9.434535
-104.177328	-2.639359	9.444531
-102.522732	-0.662727	9.454528
-101.059177	1.003330	9.464525
-98.898238	2.908657	9.474522
-97.045149	3.912567	9.484519
-94.770264	-1.472956	9.494515
-93.271294	-4.007830	9.504512
-91.571311	-0.296843	9.514509
-89.560744	-5.881771	9.524506
-87.371320	-3.685715	9.534503
-85.735937	-8.048673	9.544499
-83.909441	-5.941557	9.554496
-81.985669	-1.947316	9.564493
-80.242893	0.046843	9.574490
-77.981935	-2.303267	9.584487
-76.117816	-7.703768	9.594483
-74.443840	-3.724934	9.604480
-72.876322	-4.931777	9.614477
-70.774130	-2.132839	9.624474
-68.807336	-7.529188	9.634471
-66.882475	-2.387207	9.644467
-65.199178	2.447522	9.654464
-63.182863	2.323308	9.664461
-61.228880	2.938517	9.674458
-59.068540	0.563422	9.684455
-57.659412	5.231892	9.694451
-55.936668	-0.180781	9.704448
-53.787643	2.380175	9.714445
-51.912058	-5.076362	9.724442
-50.151355	-3.741887	9.734439
-47.851099	1.755494	9.744435
-46.515099	-1.029674	9.754432
-44.696911	2.143016	9.764429
-42.655831	1.978552	9.774426
-40.442924	-6.798109	9.784423
-38.720206	2.969329	9.794419
-36.891574	5.282986	9.804416
-35.140341	-0.941066	9.814413
-33.123183	4.516225	9.824410
-31.177245	0.713239	9.834407
-29.336835	6.313993	9.844403
-27.650182	1.846574	9.854400
-25.787190	0.450523	9.864397
-23.886209	6.933730	9.874394
-21.705065	-2.603646	9.884391
-19.895626	-4.172730	9.894387
-18.164398	-3.195111	9.904384
-16.389185	-0.958183	9.914381
-14.551855	5.917293	9.924378
-12.332309	-4.810419	9.934375
-10.609482	-3.296188	9.944371
-9.090387	0.895295	9.954368
-7.136860	4.633800	9.964365
-5.325958	9.786120	9.974362
-4.092178	42.817053	9.984359
-2.382609	80.624338	9.994355
-1.375544	125.227559	10.004352
0.000000	184.428567	10.009357
0.639244	209.651050	10.014362
1.204698	244.378674	10.019367
1.726974	268.112336	10.024371
2.145480	292.540685	10.029376
2.120933	309.117031	10.034381
2.522864	320.451320	10.039386
2.821389	334.389928	10.044391
2.814290	357.809197	10.049395
2.833661	337.425296	10.054400
3.089250	358.489245	10.059405
3.470255	369.487861	10.064410
3.725626	360.068874	10.069415
3.354893	367.462567	10.074419
3.512213	374.720001	10.079424
3.630525	391.776711	10.084429
3.850203	393.299766	10.089434
4.015924	397.690496	10.094439
3.581740	389.053267	10.099443
3.973746	382.152990	10.104448
3.864603	390.088454	10.109453
4.162949	393.210637	10.114458
4.117001	384.281249	10.119463
3.714346	382.106195	10.124467
3.779879	375.595466	10.129472
4.056516	398.051742	10.134477
4.098261	410.326662	10.139482
4.490496	406.779004	10.144487
4.362253	416.535791	10.149491
4.420819	399.627533	10.154496
4.258726	394.111907	10.159501
4.015039	390.198894	10.164506
4.359663	392.228732	10.169511
4.340292	418.218959	10.174515
4.464728	419.836057	10.179520
4.572461	424.573519	10.184525
4.526458	435.449477	10.189530
4.578605	431.963941	10.194535
4.513999	438.977677	10.199539
4.433049	426.381044	10.204544
4.841668	441.152190	10.209549
4.751256	435.497380	10.214554
4.921923	434.859901	10.219559
4.283486	438.639298	10.224563
4.621925	445.110925	10.229568
4.613927	444.008345	10.234573
4.820862	440.189029	10.239578
4.976127	441.935257	10.244583
5.008251	440.438339	10.249587
4.951081	455.906702	10.254592
5.395284	462.370930	10.259597
5.445027	481.017248	10.264602
5.673676	460.323822	10.269607
5.444044	459.762805	10.274611
5.377145	454.227242	10.279616
5.384648	457.987198	10.284621
5.203015	462.354500	10.289626
5.367144	460.532167	10.294631
5.000816	463.708338	10.299635
5.619727	468.007883	10.304640
5.655761	485.238679	10.309645
5.680221	492.889533	10.314650
5.424772	496.932719	10.319655
5.485982	500.669927	10.324659
6.003751	490.584515	10.329664
6.208673	497.213083	10.334669
5.875295	502.230666	10.339674
5.995176	500.891637	10.344679
6.059911	505.451475	10.349683
5.990457	502.553035	10.354688
5.917020	504.457176	10.359693
6.028633	502.086535	10.364698
6.112210	505.216189	10.369703
5.910489	515.366394	10.374707
6.397577	499.998206	10.379712
6.182255	512.266903	10.384717
6.202141	521.918131	10.389722
6.116673	501.374098	10.394727
5.596036	507.851883	10.399731
6.139548	509.299646	10.404736
6.419451	512.022662	10.409741
6.195715	519.784082	10.414746
6.539195	534.649294	10.419751
6.523889	550.781305	10.424755
6.677606	536.387218	10.429760
6.725090	542.433773	10.434765
6.677194	550.012616	10.439770
7.091752	548.399496	10.444775
7.019343	558.606379	10.449779
6.917538	551.721703	10.454784
7.248009	557.950218	10.459789
6.867467	551.840151	10.464794
7.279501	539.260988	10.469799
6.901768	538.755128	10.474803
7.039549	542.342936	10.479808
7.225113	547.489082	10.484813
6.840391	561.271160	10.489818
7.246153	552.032284	10.494823
7.019284	558.373348	10.499827
7.077657	559.015374	10.504832
7.349888	564.739867	10.509837
7.268424	568.942986	10.514842
7.378461	565.263675	10.519847
6.839184	564.231631	10.524851
7.239812	560.304906	10.529856
7.240416	562.193303	10.534861
7.105377	581.009574	10.539866
7.711520	591.111408	10.544871
7.811021	594.766837	10.549875
7.827894	585.563946	10.554880
7.566231	596.550117	10.559885
7.522999	598.294906	10.564890
7.905001	595.475834	10.569895
7.817313	602.945930	10.574899
7.684211	601.569969	10.579904
7.789047	610.703065	10.584909
7.675901	606.207759	10.589914
8.207266	606.350132	10.594919
7.820717	606.872307	10.599923
7.562789	614.664461	10.604928
8.245873	632.686393	10.609933
8.084097	642.707309	10.614938
8.408639	636.970466	10.619943
8.257409	647.037013	10.624947
8.507888	638.881811	10.629952
8.333908	645.206591	10.634957
8.176449	644.988882	10.639962
8.549588	643.275121	10.644967
8.382671	645.060144	10.649971
8.493122	653.080579	10.654976
8.447193	655.213750	10.659981
8.313176	641.664995	10.664986
8.608865	661.155442	10.669991
9.096730	676.674309	10.674995
9.150834	675.158092	10.680000
9.088784	657.339912	10.685005
8.923372	663.008874	10.690010
9.236938	654.181257	10.695015
9.231142	660.835623	10.700019
8.835567	650.375363	10.705024
8.902569	662.597580	10.710029
8.958690	665.419399	10.715034
9.091511	662.968076	10.720039
9.161268	677.178477	10.725043
9.509163	687.832521	10.730048
9.829461	690.995424	10.735053
9.304561	679.257887	10.740058
9.501977	656.590013	10.745063
9.301837	661.871838	10.750067
9.304506	668.026522	10.755072
9.257486	685.371732	10.760077
9.872592	695.465901	10.765082
9.660989	690.997311	10.770087
9.652488	700.517562	10.775091
9.754588	697.773077	10.780096
9.847970	702.074509	10.785101
9.581453	703.151574	10.790106
9.785055	706.859817	10.795111
10.005851	706.703206	10.800115
10.019255	702.756988	10.805120
10.001160	692.299572	10.810125
9.727412	696.937112	10.815130
9.888126	695.366040	10.820135
9.604852	709.506618	10.825139
9.508575	699.173634	10.830144
9.742688	697.329071	10.835149
10.183130	723.076188	10.840154
10.310499	723.954808	10.845159
10.338569	733.533905	10.850163
10.221914	736.818553	10.855168
10.340217	741.573356	10.860173
9.746316	738.233369	10.865178
10.386903	735.609580	10.870183
10.321565	749.892064	10.875187
10.266292	737.830407	10.880192
10.443869	734.130820	10.885197
10.142799	756.742874	10.890202
10.727385	751.454965	10.895207
10.873020	765.336368	10.900211
10.805261	757.400600	10.905216
10.900976	769.263497	10.910221
10.994711	769.332165	10.915226
11.332544	753.328321	10.920231
11.162402	768.624216	10.925235
11.119681	769.593049	10.930240
11.115830	762.206928	10.935245
11.233759	766.296296	10.940250
11.167277	760.123433	10.945255
11.050855	754.425335	10.950259
11.324629	763.987342	10.955264
11.354267	769.957988	10.960269
11.075717	769.540383	10.965274
11.311396	765.326874	10.970279
11.450796	775.097986	10.975283
11.344977	769.358766	10.980288
11.527195	772.188881	10.985293
11.550760	772.569951	10.990298
11.314863	764.227315	10.995303
11.337579	775.754916	11.000307
11.715454	771.810475	11.005312
11.889771	765.657553	11.010317
11.487472	777.699240	11.015322
11.517235	764.990034	11.020327
11.489109	782.057943	11.025331
11.745856	782.904894	11.030336
11.792564	797.525961	11.035341
11.904841	805.249709	11.040346
11.896366	802.402987	11.045351
12.373029	802.864763	11.050355
12.607973	799.769473	11.055360
12.685830	809.107280	11.060365
12.182499	783.161944	11.065370
12.282007	774.485096	11.070375
11.972167	782.028564	11.075379
11.679000	788.965377	11.080384
12.009796	803.348743	11.085389
11.988128	805.700426	11.090394
12.113168	806.412259	11.095399
11.864735	814.598839	11.100403
12.380574	823.499352	11.105408
12.966674	824.560292	11.110413
12.797279	836.255784	11.115418
13.030867	827.819305	11.120423
12.860461	812.694435	11.125427
12.661892	811.890316	11.130432
12.899881	811.577991	11.135437
12.816214	811.719111	11.140442
12.946684	815.300267	11.145447
13.297872	828.376204	11.150451
13.117071	822.838165	11.155456
13.018381	812.458175	11.160461
12.823749	805.689113	11.165466
13.065251	812.381381	11.170471
13.199573	828.615998	11.175475
13.309581	836.081492	11.180480
13.347030	835.148261	11.185485
13.385102	839.434899	11.190490
13.479611	835.869967	11.195495
13.283980	838.008116	11.200499
13.266305	834.309682	11.205504
13.579781	836.729349	11.210509
13.536691	832.091905	11.215514
13.620944	831.739441	11.220519
13.840389	833.639491	11.225523
13.909755	834.888510	11.230528
13.857528	835.466183	11.235533
13.734957	835.383261	11.240538
13.771535	830.838772	11.245543
13.367481	844.298544	11.250547
13.376278	833.773655	11.255552
13.562561	846.473767	11.260557
13.526975	844.025618	11.265562
13.698552	840.795339	11.270567
13.907499	843.810449	11.275571
13.995971	861.719337	11.280576
14.413679	867.695940	11.285581
14.448592	868.139862	11.290586
14.633172	848.906938	11.295591
14.019553	853.224977	11.300595
14.212180	837.824549	11.305600
14.627751	842.109329	11.310605
14.391434	844.257123	11.315610
14.520513	835.156032	11.320615
14.339765	846.791838	11.325619
14.314357	848.645783	11.330624
14.312172	864.621501	11.335629
14.416918	873.898287	11.340634
14.651557	866.338450	11.345639
14.406757	875.175799	11.350643
14.243259	875.468431	11.355648
14.678877	867.868652	11.360653
14.441150	877.083363	11.365658
14.697036	863.219888	11.370663
14.878108	886.283552	11.375667
15.005928	893.881859	11.380672
15.225077	897.467817	11.385677
15.213564	901.689839	11.390682
15.567598	884.576188	11.395687
15.323126	870.726275	11.400691
14.826159	874.568376	11.405696
15.105346	875.940059	11.410701
14.936988	889.758116	11.415706
15.392879	890.891872	11.420711
15.747370	889.111669	11.425715
15.862669	888.563431	11.430720
15.934013	874.489670	11.435725
15.497948	871.108705	11.440730
15.680712	865.723986	11.445735
15.246843	868.877898	11.450739
15.371757	863.623838	11.455744
15.852908	854.838761	11.460749
15.622336	859.373266	11.465754
15.868077	869.512278	11.470759
15.978451	876.425772	11.475763
16.018737	877.359295	11.480768
16.013205	868.820575	11.485773
15.559812	867.039910	11.490778
15.818735	868.299701	11.495783
15.895467	880.577324	11.500787
15.940830	892.309574	11.505792
16.149460	890.879081	11.510797
15.831038	892.921699	11.515802
16.066172	888.313983	11.520807
16.121472	897.316381	11.525811
16.316046	893.762285	11.530816
16.597712	897.548018	11.535821
16.570639	898.225766	11.540826
16.652797	891.188579	11.545831
16.379994	886.977283	11.550835
16.439037	895.239454	11.555840
16.440317	888.707203	11.560845
16.379653	897.135131	11.565850
16.334943	891.253645	11.570855
16.581945	901.949172	11.575859
16.579954	906.535549	11.580864
16.494804	895.360089	11.585869
16.658343	903.082022	11.590874
17.156176	913.404797	11.595879
17.211558	919.819277	11.600883
16.959038	914.459808	11.605888
16.901979	895.236975	11.610893
17.120407	917.178189	11.615898
17.349876	906.365725	11.620903
17.330778	899.890339	11.625907
17.306012	897.073006	11.630912
17.393850	883.895515	11.635917
17.146179	898.308156	11.640922
17.384069	882.132444	11.645927
17.327071	891.170097	11.650931
17.495950	888.336075	11.655936
17.238562	882.955315	11.660941
16.906529	900.685301	11.665946
17.365836	917.609393	11.670951
17.391121	924.014482	11.675955
17.459517	925.501796	11.680960
17.365519	924.034407	11.685965
17.434201	931.252638	11.690970
17.789842	919.107944	11.695975
17.835328	919.559643	11.700979
17.596530	922.993130	11.705984
17.892422	923.717146	11.710989
17.802359	929.845728	11.715994
17.840080	919.874435	11.720999
17.948734	931.863143	11.726003
17.502032	926.097800	11.731008
18.046910	939.109828	11.736013
18.304671	947.067506	11.741018
18.509545	939.007725	11.746023
18.512744	944.359728	11.751027
17.845016	946.809745	11.756032
18.830181	947.297665	11.761037
18.760254	940.174318	11.766042
18.403582	920.035666	11.771047
18.211457	924.247074	11.776051
18.297825	924.392616	11.781056
18.466639	931.520756	11.786061
18.472356	941.687061	11.791066
18.444091	945.403960	11.796071
18.450935	942.767668	11.801075
18.577560	952.182949	11.806080
18.680148	948.709746	11.811085
18.381373	957.956322	11.816090
18.880384	944.317361	11.821095
18.470607	941.769595	11.826099
18.720516	943.136493	11.831104
18.948986	949.867175	11.836109
18.650212	954.180762	11.841114
19.123322	963.759998	11.846119
19.494252	982.699530	11.851123
19.197032	972.329010	11.856128
19.083576	965.822909	11.861133
19.228740	986.597861	11.866138
19.605812	967.878160	11.871143
19.095911	962.939790	11.876147
19.168275	974.442283	11.881152
19.889892	974.853960	11.886157
19.401502	979.235645	11.891162
19.559004	971.454654	11.896167
19.736180	960.984824	11.901171
19.259967	960.475728	11.906176
19.723829	964.347544	11.911181
19.760992	983.575290	11.916186
19.693058	979.594658	11.921191
19.533941	980.635689	11.926195
19.572913	986.027736	11.931200
19.717131	983.580851	11.936205
19.849746	995.016977	11.941210
19.740893	993.864205	11.946215
19.814068	975.785932	11.951219
19.755461	989.725359	11.956224
19.979241	987.538613	11.961229
19.612059	990.715031	11.966234
19.795922	991.070542	11.971239
20.100284	1008.554071	11.976243
20.225313	1011.760807	11.981248
20.575296	1006.969147	11.986253
20.604912	1010.511241	11.991258
20.522568	1004.941658	11.996263
20.473767	985.531297	12.001267
20.191999	983.797364	12.006272
20.565656	988.746503	12.011277
20.489635	1008.113766	12.016282
20.753438	999.528858	12.021287
20.484863	993.829700	12.026291
20.340112	981.731645	12.031296
20.660366	994.863133	12.036301
20.416360	1002.481375	12.041306
20.457636	987.123852	12.046311
20.656409	977.216725	12.051315
20.419887	985.822573	12.056320
20.412504	983.786242	12.061325
20.490177	999.574320	12.066330
20.548944	999.628065	12.071335
20.298545	991.044743	12.076339
20.115704	1002.143235	12.081344
20.701377	1006.367818	12.086349
20.507331	1011.021131	12.091354
20.737816	1007.306729	12.096359
20.553216	1007.508105	12.101363
20.451259	1003.302644	12.106368
20.525288	991.327392	12.111373
20.455854	998.249122	12.116378
20.517525	988.972594	12.121383
20.698014	984.578579	12.126387
20.084707	998.243764	12.131392
20.568894	1002.142313	12.136397
20.568742	1012.572970	12.141402
20.526452	1003.021260	12.146407
20.438356	998.771010	12.151411
20.536803	1004.040031	12.156416
20.733573	993.469275	12.161421
20.529708	992.043057	12.166426
20.700565	992.381718	12.171431
20.657909	989.548295	12.176435
20.158668	990.641996	12.181440
20.511117	987.043773	12.186445
20.418199	993.798925	12.191450
20.163808	983.867870	12.196455
20.499726	996.687760	12.201459
20.486524	1009.631156	12.206464
20.625085	1010.826574	12.211469
20.665167	1003.442785	12.216474
20.801159	988.806635	12.221479
20.844868	987.020791	12.226483
20.548950	998.096311	12.231488
20.956604	989.750256	12.236493
20.560470	1003.505395	12.241498
20.567861	996.342879	12.246503
20.692440	991.602944	12.251507
20.815986	989.660855	12.256512
20.748817	986.987471	12.261517
20.550080	997.514449	12.266522
20.541172	986.694211	12.271527
20.525615	995.810480	12.276531
20.382281	998.823458	12.281536
20.839493	993.052701	12.286541
20.627870	978.725907	12.291546
20.389397	969.330095	12.296551
20.367909	960.312868	12.301555
20.184724	970.698567	12.306560
20.765450	978.721454	12.311565
20.283467	985.718438	12.316570
20.414526	979.788380	12.321575
20.389679	986.955321	12.326579
20.430317	989.822253	12.331584
20.740993	995.276632	12.336589
20.618144	1001.768463	12.341594
20.491208	987.333531	12.346599
20.548335	984.941539	12.351603
20.604444	984.092060	12.356608
20.351419	964.693797	12.361613
20.261062	983.593355	12.366618
20.490706	991.014615	12.371623
20.698508	1001.945140	12.376627
20.242341	1000.644322	12.381632
20.826145	996.607050	12.386637
20.398216	991.969429	12.391642
20.469421	981.806662	12.396647
20.738131	989.209074	12.401651
20.246994	978.024181	12.406656
20.778614	981.554016	12.411661
20.642160	987.704215	12.416666
20.526305	979.900581	12.421671
20.461851	970.647335	12.426675
20.211623	982.762714	12.431680
20.414022	977.223426	12.436685
20.450454	983.997369	12.441690
20.360459	980.159036	12.446695
20.513085	998.258145	12.451699
20.662864	996.016964	12.456704
20.872276	979.853571	12.461709
20.456613	980.052373	12.466714
20.743323	979.905750	12.471719
20.828129	973.790673	12.476723
20.564822	978.601687	12.481728
20.673907	982.544286	12.486733
20.751821	979.475581	12.491738
20.821315	984.233519	12.496743
20.388492	970.984439	12.501747
20.416210	973.703610	12.506752
21.120774	974.075427	12.511757
20.806099	980.285588	12.516762
20.450590	970.701849	12.521767
20.559354	964.037297	12.526771
20.163859	973.127411	12.531776
20.552802	969.707886	12.536781
20.822035	976.318533	12.541786
20.497598	961.571330	12.546791
20.513038	948.376941	12.551795
20.221112	960.800167	12.556800
20.708328	960.110603	12.561805
20.566417	956.036114	12.566810
20.551299	948.460872	12.571815
20.689500	951.435246	12.576819
20.355562	951.083242	12.581824
20.446916	946.142028	12.586829
20.599820	950.260566	12.591834
20.255124	952.648023	12.596839
20.216537	954.745372	12.601843
20.427328	979.636968	12.606848
20.699664	972.914783	12.611853
20.729553	978.508561	12.616858
20.392577	969.199427	12.621863
20.568335	959.647664	12.626867
20.164743	958.816308	12.631872
20.644097	966.339663	12.636877
20.491847	984.096274	12.641882
20.687290	971.838307	12.646887
20.483744	972.392808	12.651891
20.257420	970.479713	12.656896
20.459079	968.526746	12.661901
20.505315	983.868786	12.666906
20.419108	991.548592	12.671911
20.476998	980.604158	12.676915
20.445415	989.347642	12.681920
20.534506	992.765122	12.686925
20.480074	988.050584	12.691930
20.610203	989.695226	12.696935
20.635889	981.933676	12.701939
20.405412	982.612328	12.706944
20.300283	967.188285	12.711949
20.638077	982.095869	12.716954
20.592055	980.664979	12.721959
20.457108	970.970364	12.726963
20.293335	976.599760	12.731968
20.341000	982.379949	12.736973
20.758544	1008.359899	12.741978
20.692691	1006.156262	12.746983
20.776750	1002.406864	12.751987
20.307956	999.280261	12.756992
20.550631	993.122650	12.761997
20.627475	1000.303341	12.767002
20.554489	999.047071	12.772007
20.738559	987.995769	12.777011
20.787063	990.039806	12.782016
21.004452	985.210949	12.787021
20.578771	991.959245	12.792026
20.644002	997.012775	12.797031
21.129906	988.450801	12.802035
20.784411	999.444338	12.807040
20.645601	968.482293	12.812045
20.755895	963.197411	12.817050
20.651739	967.254445	12.822055
20.858062	950.839250	12.827059
20.571367	967.663173	12.832064
20.735841	966.578780	12.837069
20.522709	961.935296	12.842074
20.389931	956.350120	12.847079
20.677104	950.571805	12.852083
20.220914	953.003854	12.857088
20.292483	934.894347	12.862093
20.292338	932.986187	12.867098
19.784047	934.234300	12.872103
19.992097	933.691769	12.877107
20.146861	944.853073	12.882112
20.589917	958.064295	12.887117
20.350121	964.234121	12.892122
20.379128	967.465624	12.897127
20.469143	958.389611	12.902131
20.198071	974.965031	12.907136
20.552536	969.546581	12.912141
20.468206	968.218002	12.917146
20.612225	971.005361	12.922151
20.952997	969.075941	12.927155
20.636423	976.931261	12.932160
20.715347	966.167996	12.937165
20.596793	971.083662	12.942170
20.341309	973.903198	12.947175
20.714215	959.033739	12.952179
20.557199	964.286716	12.957184
20.333872	946.736767	12.962189
20.337718	948.642832	12.967194
20.525146	962.088805	12.972199
20.796190	964.723431	12.977203
20.394675	957.045799	12.982208
20.672380	943.423210	12.987213
20.280118	941.451425	12.992218
20.165236	948.199019	12.997223
20.740663	960.553300	13.002227
20.386361	967.632419	13.007232
20.542417	960.812084	13.012237
20.236772	971.832361	13.017242
20.688208	974.811978	13.022247
20.733180	963.716643	13.027251
20.246817	968.720934	13.032256
20.199150	962.385702	13.037261
20.224183	972.870665	13.042266
20.308689	967.209827	13.047271
20.612997	965.054397	13.052275
20.438235	981.169738	13.057280
20.859121	973.731537	13.062285
20.753790	977.104324	13.067290
20.518377	979.097442	13.072295
20.334506	980.661268	13.077299
20.498654	977.605619	13.082304
20.440713	974.509695	13.087309
20.748267	979.764281	13.092314
20.572686	974.930290	13.097319
20.763564	965.890227	13.102323
20.461204	964.536495	13.107328
20.393151	950.874422	13.112333
20.074882	953.902674	13.117338
20.010591	972.757058	13.122343
20.523610	965.021876	13.127347
20.338098	976.467723	13.132352
20.685872	975.022915	13.137357
20.744569	982.578675	13.142362
20.595527	979.448390	13.147367
20.903016	978.637671	13.152371
20.481820	966.262002	13.157376
20.233440	958.318658	13.162381
20.527746	978.713400	13.167386
20.267372	981.546334	13.172391
20.514835	989.089338	13.177395
20.657834	992.189119	13.182400
20.525121	988.972644	13.187405
20.363249	978.161038	13.192410
20.569063	990.869202	13.197415
21.024699	978.858330	13.202419
20.686355	970.388401	13.207424
20.337345	954.657896	13.212429
20.360139	952.509518	13.217434
20.129907	955.284019	13.222439
20.979965	962.033848	13.227443
20.315061	958.952725	13.232448
20.413590	956.700800	13.237453
20.253642	962.697031	13.242458
20.370315	978.565603	13.247463
20.614350	978.974598	13.252467
20.223993	993.840624	13.257472
20.571284	990.661140	13.262477
20.481463	987.791083	13.267482
20.320893	987.334152	13.272487
20.824611	991.228006	13.277491
20.476147	993.160304	13.282496
20.921621	981.753482	13.287501
20.694198	974.106426	13.292506
20.146184	961.574358	13.297511
20.603252	954.788023	13.302515
20.372323	959.850926	13.307520
20.148669	955.123962	13.312525
20.561254	968.892019	13.317530
20.315915	983.460499	13.322535
20.692933	993.179668	13.327539
20.471027	1000.595676	13.332544
20.668615	990.020062	13.337549
20.688573	967.514056	13.342554
20.236645	965.955506	13.347559
20.692670	960.749533	13.352563
20.335977	961.590248	13.357568
20.663836	959.500453	13.362573
20.716910	960.783623	13.367578
20.520274	959.499766	13.372583
20.464499	956.819839	13.377587
20.247646	962.744717	13.382592
20.311626	958.597963	13.387597
20.467987	966.108174	13.392602
20.472869	970.143087	13.397607
20.558727	967.364871	13.402611
20.389446	975.176196	13.407616
20.509991	975.314711	13.412621
20.560963	979.783848	13.417626
20.637317	976.612884	13.422631
20.203038	968.036825	13.427635
20.276911	994.511558	13.432640
20.634489	990.538756	13.437645
20.854432	992.935518	13.442650
20.591924	984.207467	13.447655
20.594167	973.751335	13.452659
20.368724	976.665433	13.457664
20.365664	963.147533	13.462669
20.437654	960.425149	13.467674
20.201915	969.078173	13.472679
20.668053	974.436782	13.477683
20.619471	974.419333	13.482688
20.299337	971.642786	13.487693
20.652380	981.938238	13.492698
20.445167	979.421240	13.497703
20.571773	971.608904	13.502707
20.577292	969.748724	13.507712
20.581459	962.539427	13.512717
20.461902	964.044106	13.517722
20.213095	966.610248	13.522727
20.547152	967.455920	13.527731
20.401938	977.017081	13.532736
20.686526	977.619893	13.537741
20.601036	970.653563	13.542746
20.456957	971.097649	13.547751
20.650733	968.761140	13.552755
20.672362	977.008824	13.557760
20.431836	970.724849	13.562765
20.499332	969.879863	13.567770
20.172891	972.963042	13.572775
20.529332	971.944231	13.577779
20.415202	971.390002	13.582784
20.381932	966.664212	13.587789
20.551417	975.244724	13.592794
20.180784	984.881269	13.597799
20.532498	992.257828	13.602803
20.846361	999.047459	13.607808
20.800296	985.355037	13.612813
20.276045	984.894605	13.617818
20.268461	980.697754	13.622823
20.341802	970.996728	13.627827
20.424161	989.545453	13.632832
20.504399	995.282603	13.637837
20.474137	989.696835	13.642842
20.571271	1004.351072	13.647847
20.979880	1003.188312	13.652851
20.562907	979.484028	13.657856
20.591269	975.063814	13.662861
20.454652	976.528634	13.667866
20.505654	976.020612	13.672871
20.428223	970.404525	13.677875
20.648757	976.835271	13.682880
20.435751	970.767693	13.687885
20.541498	969.905567	13.692890
20.262275	984.039456	13.697895
20.419274	979.486754	13.702899
20.194113	980.741757	13.707904
20.432974	981.594727	13.712909
20.367598	983.600152	13.717914
20.453200	1007.097152	13.722919
20.927946	1003.113545	13.727923
20.434494	994.201534	13.732928
20.489525	992.519546	13.737933
20.478583	983.549511	13.742938
20.415283	987.339821	13.747943
20.408875	971.499459	13.752947
20.225551	989.492857	13.757952
20.756350	996.732040	13.762957
20.678399	991.902974	13.767962
20.502056	996.853098	13.772967
20.675788	982.974226	13.777971
20.351071	976.047626	13.782976
20.573079	977.780121	13.787981
20.531776	980.294246	13.792986
20.602986	977.521518	13.797991
20.542997	976.294717	13.802995
20.431223	983.265773	13.808000
20.759015	968.950734	13.813005
20.724957	970.348732	13.818010
20.872893	975.830635	13.823015
21.001012	971.891281	13.828019
20.720776	982.628377	13.833024
20.542222	978.600730	13.838029
20.744326	977.207542	13.843034
20.632302	982.090629	13.848039
20.818707	974.897995	13.853043
20.592801	957.556614	13.858048
20.723525	949.669512	13.863053
20.654176	961.393305	13.868058
20.652898	956.271308	13.873063
20.838276	950.633814	13.878067
20.507081	960.918526	13.883072
20.173063	954.524883	13.888077
20.387400	951.853918	13.893082
20.575398	959.505745	13.898087
20.875869	958.232496	13.903091
20.681833	967.801438	13.908096
20.587389	962.074520	13.913101
20.651831	964.623819	13.918106
20.283878	966.500871	13.923111
20.638789	955.474388	13.928115
20.227753	960.991818	13.933120
20.333343	960.367852	13.938125
20.698777	960.517773	13.943130
20.699517	957.268982	13.948135
20.700316	965.024789	13.953139
20.836294	970.133262	13.958144
20.567067	956.793445	13.963149
20.650779	960.965601	13.968154
20.360723	961.926583	13.973159
20.355020	957.344641	13.978163
20.582700	957.879253	13.983168
20.498853	968.148176	13.988173
21.164977	956.496435	13.993178
20.360328	943.256219	13.998183
20.172151	930.387651	14.003187
20.258140	936.040278	14.008192
20.465444	947.224996	14.013210
20.803091	957.326593	14.018227
20.516966	955.909354	14.023245
20.255769	941.317254	14.028263
20.730856	955.894188	14.033280
20.612663	959.480684	14.038298
20.806838	950.881512	14.043315
20.490503	952.203000	14.048333
20.567490	939.180320	14.053351
20.480965	945.198366	14.058368
20.711626	955.092083	14.063386
20.920078	958.060194	14.068403
20.527197	962.237912	14.073421
20.742296	960.051749	14.078439
20.653998	965.068073	14.083456
20.643006	964.846492	14.088474
20.507383	967.790831	14.093491
20.270535	965.489560	14.098509
20.505487	959.045211	14.103527
20.562409	964.128035	14.108544
20.682691	971.579163	14.113562
20.969766	966.084468	14.118579
20.679453	973.472096	14.123597
20.714371	962.711818	14.128615
20.712438	963.519121	14.133632
20.534338	970.572673	14.138650
20.967880	986.619175	14.143667
20.836802	993.743890	14.148685
20.984304	994.381070	14.153703
21.372838	996.241374	14.158720
20.708198	999.026274	14.163738
20.831769	996.574705	14.168755
21.040627	996.469071	14.173773
21.203428	992.370582	14.178791
21.190088	987.099971	14.183808
20.889292	991.926826	14.188826
20.770903	995.810663	14.193843
20.716057	1000.554249	14.198861
20.915448	997.577782	14.203879
21.150813	994.197603	14.208896
20.712200	996.347131	14.213914
21.160597	996.034979	14.218931
20.867498	1018.709730	14.223949
21.422673	1018.921668	14.228967
21.516799	1021.738139	14.233984
21.495730	1030.637005	14.239002
21.611208	1019.546084	14.244019
21.007225	1015.267863	14.249037
21.620896	1015.380810	14.254055
21.535892	1014.175307	14.259072
21.340065	1008.738738	14.264090
21.427855	994.105081	14.269107
21.054122	1004.924211	14.274125
21.183634	1015.606457	14.279143
21.659061	1023.526360	14.284160
21.268586	1020.365541	14.289178
21.699171	1026.140698	14.294195
21.689720	1029.731889	14.299213
21.360060	1030.335062	14.304231
21.568420	1019.919887	14.309248
21.418273	1031.342025	14.314266
21.696510	1029.405332	14.319283
21.596487	1028.821997	14.324301
21.378697	1027.153179	14.329319
21.522814	1021.854297	14.334336
21.476203	1037.483504	14.339354
21.494271	1027.660244	14.344371
21.448260	1025.164932	14.349389
21.345482	1027.528316	14.354407
21.776219	1022.005968	14.359424
21.398277	1029.366702	14.364442
21.752749	1025.044152	14.369459
21.806386	1031.417406	14.374477
21.660501	1030.234196	14.379495
21.937301	1039.082413	14.384512
21.989349	1054.011636	14.389530
22.054106	1044.764512	14.394547
21.873474	1050.733117	14.399565
21.704632	1040.068201	14.404583
21.815693	1039.358390	14.409600
21.766375	1061.549160	14.414618
21.808233	1062.406114	14.419635
22.166197	1056.483225	14.424653
21.795424	1061.587105	14.429671
22.191232	1054.887397	14.434688
22.064060	1059.780964	14.439706
22.281018	1051.093156	14.444723
22.052342	1054.849880	14.449741
22.322205	1055.764851	14.454759
22.386055	1050.352917	14.459776
22.170566	1051.342150	14.464794
22.203422	1049.853578	14.469811
22.054506	1042.196262	14.474829
21.994131	1044.250865	14.479847
22.346432	1049.369979	14.484864
22.194585	1057.220058	14.489882
22.411129	1051.620176	14.494899
22.265258	1055.333805	14.499917
22.241616	1052.145933	14.504935
22.396090	1054.518630	14.509952
22.398673	1055.861621	14.514970
22.699801	1054.902845	14.519987
22.501334	1052.233642	14.525005
22.450767	1051.722642	14.530023
22.350549	1039.138696	14.535040
22.615709	1043.493057	14.540058
22.324085	1033.187503	14.545075
22.246252	1040.789814	14.550093
22.549752	1053.451524	14.555111
22.672795	1048.115094	14.560128
22.790695	1057.948214	14.565146
22.639988	1046.855682	14.570163
22.220864	1029.304643	14.575181
22.438216	1049.532197	14.580199
22.874955	1050.908191	14.585216
22.929088	1044.233093	14.590234
22.553397	1027.274455	14.595251
22.803578	1019.893271	14.600269
22.333879	1027.328413	14.605287
22.709019	1029.813776	14.610304
22.662963	1048.290087	14.615322
22.844665	1052.445403	14.620339
23.037251	1051.176748	14.625357
22.763391	1038.548137	14.630375
22.735508	1027.030190	14.635392
22.643960	1049.263855	14.640410
22.800378	1048.693103	14.645427
22.971376	1060.458874	14.650445
22.654582	1056.318882	14.655463
22.922691	1054.975260	14.660480
22.648925	1054.501432	14.665498
22.973617	1052.269462	14.670515
23.121567	1048.542989	14.675533
22.915890	1054.337837	14.680551
23.042085	1045.455296	14.685568
23.161865	1047.522065	14.690586
23.040163	1049.045327	14.695603
23.081046	1050.149401	14.700621
23.022768	1047.796041	14.705639
23.342049	1050.076385	14.710656
22.822694	1062.655407	14.715674
22.846825	1047.334997	14.720691
22.695734	1046.662278	14.725709
22.870328	1051.749960	14.730727
23.007252	1061.040499	14.735744
22.620040	1063.995095	14.740762
22.999959	1066.619703	14.745779
23.613106	1077.377443	14.750797
23.476029	1082.521137	14.755815
24.056024	1074.653167	14.760832
23.578860	1068.800547	14.765850
23.371355	1054.001567	14.770867
23.472237	1045.354298	14.775885
22.961197	1053.941212	14.780903
23.162594	1039.323997	14.785920
23.237584	1063.758533	14.790938
23.511744	1071.693260	14.795955
23.641162	1076.371303	14.800973
23.169407	1081.999385	14.805991
23.623097	1079.827062	14.811008
23.748824	1082.721877	14.816026
23.451371	1081.245084	14.821043
23.829104	1079.806898	14.826061
23.757711	1072.731807	14.831079
23.585974	1054.151845	14.836096
23.589280	1055.630002	14.841114
23.638259	1069.060632	14.846131
23.580063	1067.813097	14.851149
24.030346	1068.346934	14.856167
24.154922	1058.229813	14.861184
23.625681	1051.355171	14.866202
23.557422	1044.449482	14.871219
23.753413	1052.778912	14.876237
23.595635	1047.479405	14.881255
23.942652	1058.152161	14.886272
23.846925	1053.516013	14.891290
24.240497	1058.822031	14.896307
24.045313	1051.175235	14.901325
23.558748	1052.187253	14.906343
23.649016	1042.407524	14.911360
23.911409	1058.335110	14.916378
23.699279	1073.905812	14.921395
23.990828	1073.939573	14.926413
23.732025	1081.529870	14.931431
23.808940	1079.686628	14.936448
23.881178	1081.240310	14.941466
23.863517	1076.366760	14.946483
24.094493	1074.727037	14.951501
23.960241	1081.735897	14.956519
23.712599	1081.025092	14.961536
24.108914	1071.106870	14.966554
23.789228	1081.181257	14.971571
24.460566	1080.015569	14.976589
24.029509	1095.292447	14.981607
24.364756	1095.517441	14.986624
24.343652	1106.928495	14.991642
24.376623	1105.266866	14.996659
24.581903	1100.752583	15.001677
24.329319	1103.838300	15.006695
24.433809	1076.199189	15.011712
24.194058	1073.366678	15.016730
24.411583	1087.188870	15.021747
24.612403	1089.433057	15.026765
24.278971	1080.985598	15.031783
24.449978	1102.578144	15.036800
24.572922	1102.313178	15.041818
24.702490	1096.928499	15.046835
24.833701	1085.367828	15.051853
24.153256	1094.859536	15.056871
24.347964	1078.082000	15.061888
24.538119	1097.714633	15.066906
24.774221	1116.591198	15.071923
24.686059	1104.181453	15.076941
24.644038	1109.165277	15.081959
24.756159	1100.706520	15.086976
24.759451	1105.893902	15.091994
24.850421	1106.118531	15.097011
24.742076	1097.237184	15.102029
24.669888	1097.513003	15.107047
24.940587	1098.401102	15.112064
25.006122	1106.421032	15.117082
24.677235	1100.923852	15.122099
24.738226	1092.466962	15.127117
24.808378	1102.100087	15.132135
24.882477	1102.063136	15.137152
24.525793	1105.481636	15.142170
24.643373	1110.885175	15.147187
24.978118	1108.184402	15.152205
24.570932	1109.424438	15.157223
24.868374	1107.909391	15.162240
24.771199	1095.630080	15.167258
24.493444	1099.964081	15.172275
24.844631	1112.928125	15.177293
24.947313	1126.148894	15.182311
25.400998	1127.682644	15.187328
25.322322	1136.559301	15.192346
25.245131	1135.808724	15.197363
25.171436	1121.153503	15.202381
24.876656	1130.377657	15.207399
25.365884	1130.933601	15.212416
25.386512	1131.989001	15.217434
25.141549	1133.362043	15.222451
25.350960	1127.508437	15.227469
25.141318	1136.848006	15.232487
25.355150	1132.904935	15.237504
25.514446	1127.976404	15.242522
25.447056	1141.886560	15.247539
25.945397	1123.720315	15.252557
25.595606	1122.838608	15.257575
25.365628	1115.032159	15.262592
25.657973	1096.650261	15.267610
25.195549	1102.884055	15.272627
25.621280	1108.655300	15.277645
25.562573	1119.246518	15.282663
25.356176	1119.979473	15.287680
25.728604	1130.275420	15.292698
25.655149	1133.700665	15.297715
25.826710	1131.093555	15.302733
25.889950	1121.689320	15.307751
25.339071	1120.536089	15.312768
25.464704	1124.804188	15.317786
25.389946	1138.811472	15.322803
25.797957	1128.395839	15.327821
25.668582	1135.391362	15.332839
25.936275	1132.227794	15.337856
25.943543	1136.310280	15.342874
25.660456	1138.881766	15.347891
25.807532	1132.795852	15.352909
25.714477	1137.635240	15.357927
25.778679	1132.921649	15.362944
25.752116	1131.698951	15.367962
25.947987	1135.296748	15.372979
25.804673	1124.064550	15.377997
25.935528	1136.406226	15.383015
25.552228	1132.191873	15.388032
26.135669	1131.414585	15.393050
25.599590	1134.886872	15.398067
26.111875	1157.076308	15.403085
26.202775	1163.555363	15.408103
25.866956	1172.244962	15.413120
26.423565	1158.019293	15.418138
26.107592	1164.918747	15.423155
26.543638	1159.985393	15.428173
26.541512	1159.855205	15.433191
26.366433	1153.712122	15.438208
26.130477	1140.205912	15.443226
25.814921	1150.164856	15.448243
26.544992	1154.707800	15.453261
26.430416	1160.182991	15.458279
26.396925	1173.147092	15.463296
26.545540	1157.352102	15.468314
26.487449	1157.172638	15.473331
26.503541	1170.018716	15.478349
26.419010	1169.321218	15.483367
26.367500	1166.548329	15.488384
26.122838	1158.854311	15.493402
26.211456	1172.481637	15.498419
26.549539	1162.269043	15.503437
26.866287	1163.481713	15.508455
26.441394	1176.785097	15.513472
26.629217	1161.836439	15.518490
26.712512	1167.544346	15.523507
26.802472	1164.382376	15.528525
26.668952	1169.048901	15.533543
26.784812	1164.764367	15.538560
27.037031	1156.767730	15.543578
26.666215	1168.063146	15.548595
26.861713	1159.930835	15.553613
27.123951	1161.348829	15.558631
26.813420	1168.607644	15.563648
26.644788	1164.992981	15.568666
26.612211	1163.044494	15.573683
26.493823	1162.000035	15.578701
26.772503	1164.326199	15.583719
26.649632	1160.237045	15.588736
26.824882	1166.798604	15.593754
26.626395	1177.676428	15.598771
27.072577	1186.898848	15.603789
27.549659	1187.425271	15.608807
27.274054	1177.425375	15.613824
27.287901	1170.309900	15.618842
27.160161	1162.531164	15.623859
26.979255	1159.066326	15.628877
27.087980	1161.904092	15.633895
27.107529	1191.645692	15.638912
27.394897	1194.336995	15.643930
26.973746	1204.427648	15.648947
27.071805	1201.291120	15.653965
27.562140	1194.033572	15.658983
27.586686	1191.611922	15.664000
27.639718	1189.067751	15.669018
27.528673	1187.962343	15.674035
27.390582	1170.042264	15.679053
27.535174	1164.033812	15.684071
27.220094	1163.428141	15.689088
27.421683	1166.973124	15.694106
27.415433	1179.240747	15.699123
27.622199	1194.617352	15.704141
27.873911	1192.310484	15.709159
27.371727	1187.454397	15.714176
27.841224	1183.489414	15.719194
27.586761	1174.656493	15.724211
27.758874	1150.311421	15.729229
27.662747	1163.494718	15.734247
27.173791	1171.798177	15.739264
27.907064	1176.419270	15.744282
27.709958	1185.201586	15.749299
27.796260	1194.961186	15.754317
28.108244	1192.328524	15.759335
27.581358	1190.468308	15.764352
27.861549	1194.197392	15.769370
27.992594	1197.648239	15.774387
27.916088	1188.478611	15.779405
28.036114	1196.327876	15.784423
27.648664	1204.541231	15.789440
28.107371	1193.562180	15.794458
27.908624	1203.601632	15.799475
27.886877	1198.771165	15.804493
27.805169	1186.416950	15.809511
27.675914	1204.294814	15.814528
27.944574	1205.820329	15.819546
27.838040	1202.799802	15.824563
28.033186	1198.892729	15.829581
28.122232	1202.035666	15.834599
27.967456	1195.868878	15.839616
28.033455	1197.041318	15.844634
27.895134	1210.210937	15.849651
27.986198	1223.822190	15.854669
28.710288	1217.770057	15.859687
28.458820	1227.759731	15.864704
28.676230	1215.944533	15.869722
28.794565	1230.045380	15.874739
28.648331	1215.854671	15.879757
28.575159	1193.025739	15.884775
28.124701	1200.788239	15.889792
28.383604	1187.586884	15.894810
28.050772	1196.659844	15.899827
28.363535	1217.441857	15.904845
28.719009	1211.630991	15.909863
28.522390	1228.281640	15.914880
28.495151	1218.245250	15.919898
28.618690	1215.853426	15.924915
28.208803	1221.169669	15.929933
28.696292	1212.081537	15.934951
28.953928	1225.395662	15.939968
28.715435	1215.726453	15.944986
28.895934	1218.027385	15.950003
28.374053	1227.023548	15.955021
28.767974	1220.755081	15.960039
28.268485	1226.566968	15.965056
28.715602	1223.313416	15.970074
28.667270	1221.872382	15.975091
28.676992	1246.830449	15.980109
28.851188	1242.695467	15.985127
28.947270	1245.016159	15.990144
29.413919	1242.915680	15.995162
29.326205	1248.267068	16.000179
29.010391	1235.242275	16.005197
29.227003	1213.568904	16.010215
29.072835	1215.086350	16.015232
29.064180	1218.701057	16.020250
29.060806	1219.233321	16.025267
29.180133	1230.603199	16.030285
29.368154	1243.642149	16.035303
29.448525	1240.256745	16.040320
29.107259	1232.592252	16.045338
29.090886	1223.307617	16.050355
28.761828	1248.794779	16.055373
29.050397	1241.062864	16.060391
28.997803	1247.308435	16.065408
29.460016	1245.781254	16.070426
29.267589	1251.160354	16.075443
29.410952	1251.935062	16.080461
29.576989	1252.786380	16.085479
29.350445	1256.983269	16.090496
29.600008	1253.017165	16.095514
29.897534	1242.784241	16.100531
29.717375	1245.561130	16.105549
29.837202	1241.417515	16.110567
29.785695	1247.246054	16.115584
29.903022	1248.120871	16.120602
29.844741	1245.767479	16.125619
29.780667	1266.947870	16.130637
30.030228	1253.148613	16.135655
29.849981	1251.140293	16.140672
29.904008	1243.400165	16.145690
30.308532	1245.665373	16.150707
29.589914	1251.468173	16.155725
29.875047	1245.257945	16.160743
29.855538	1253.020955	16.165760
30.031320	1245.256689	16.170778
29.955039	1241.893123	16.175795
29.755588	1239.467864	16.180813
30.032269	1232.536959	16.185831
29.746122	1242.190822	16.190848
30.127334	1246.575501	16.195866
30.079745	1244.008042	16.200883
30.040863	1235.625201	16.205901
30.226430	1236.399469	16.210919
30.041485	1236.589452	16.215936
29.836855	1239.552717	16.220954
30.221932	1244.230939	16.225971
29.878579	1249.563322	16.230989
30.326336	1241.659725	16.236007
30.375464	1243.802285	16.241024
30.092534	1242.433272	16.246042
30.321067	1246.969719	16.251059
30.131845	1249.950977	16.256077
30.512281	1257.972680	16.261095
30.518957	1271.559683	16.266112
30.366908	1274.783561	16.271130
30.114123	1270.778018	16.276147
30.372258	1278.421254	16.281165
30.423002	1273.196948	16.286183
30.559162	1267.671153	16.291200
30.645688	1274.635456	16.296218
30.921866	1273.386485	16.301235
30.867808	1273.242556	16.306253
30.815184	1264.776945	16.311271
30.662770	1277.160772	16.316288
30.694216	1271.662687	16.321306
30.772002	1270.964466	16.326323
30.870048	1276.459273	16.331341
30.865168	1269.436400	16.336359
30.720215	1274.203885	16.341376
30.394981	1277.905277	16.346394
30.608317	1273.496624	16.351411
30.181852	1276.868090	16.356429
30.842400	1282.260603	16.361447
31.202514	1289.104199	16.366464
31.079827	1294.566575	16.371482
31.034861	1278.187264	16.376499
30.795204	1294.868449	16.381517
31.095833	1294.694693	16.386535
31.141043	1307.693554	16.391552
30.974198	1303.822163	16.396570
31.434872	1304.635932	16.401587
31.171420	1295.884596	16.406605
31.080372	1297.678279	16.411623
31.398615	1296.641253	16.416640
31.551211	1298.186862	16.421658
31.863355	1294.095933	16.426675
31.615810	1295.673898	16.431693
31.304040	1277.742059	16.436711
31.378716	1281.755632	16.441728
31.643024	1299.725004	16.446746
31.771166	1289.133664	16.451763
31.293069	1279.732292	16.456781
31.593719	1293.055350	16.461799
31.559216	1298.942546	16.466816
31.389986	1293.764328	16.471834
31.461866	1298.325775	16.476851
31.480634	1304.659091	16.481869
31.674451	1291.707128	16.486887
31.818022	1287.251394	16.491904
31.515079	1294.065459	16.496922
31.491819	1293.985832	16.501939
31.598972	1299.210203	16.506957
31.774342	1304.370212	16.511975
31.801137	1294.852126	16.516992
31.655403	1292.194916	16.522010
31.962002	1298.963680	16.527027
31.846319	1309.800082	16.532045
31.672712	1298.956405	16.537063
31.962378	1294.491527	16.542080
31.779907	1315.522555	16.547098
32.116921	1311.871257	16.552115
32.222970	1323.688501	16.557133
32.175066	1321.596142	16.562151
32.603583	1310.884520	16.567168
32.178431	1304.877212	16.572186
32.143132	1292.295277	16.577203
32.193842	1292.041828	16.582221
32.598917	1293.484248	16.587239
32.581609	1288.074158	16.592256
32.229667	1285.506467	16.597274
32.854202	1292.602055	16.602291
32.638280	1289.303222	16.607309
32.164263	1288.472777	16.612327
32.290568	1284.354859	16.617344
32.275008	1293.512561	16.622362
32.572644	1288.041230	16.627379
32.199866	1288.759829	16.632397
32.428398	1285.924951	16.637415
32.551084	1300.817994	16.642432
32.733874	1313.182999	16.647450
32.799992	1316.637937	16.652467
33.140397	1317.689543	16.657485
32.300531	1314.115827	16.662503
32.695643	1309.747387	16.667520
32.749749	1314.187402	16.672538
32.704991	1315.935952	16.677555
32.477359	1321.772160	16.682573
32.843697	1315.503333	16.687591
32.825880	1315.783069	16.692608
32.552981	1320.111640	16.697626
32.955349	1321.968209	16.702643
32.998284	1316.279508	16.707661
32.927997	1319.817552	16.712679
33.097015	1316.158438	16.717696
32.699683	1313.498879	16.722714
32.782237	1317.874582	16.727731
32.883130	1320.287329	16.732749
33.112220	1338.745297	16.737767
33.500760	1343.108387	16.742784
33.632710	1343.966720	16.747802
33.333806	1326.208952	16.752819
33.235296	1319.630433	16.757837
33.124696	1317.845383	16.762855
33.385109	1320.816294	16.767872
33.100360	1319.732287	16.772890
33.558264	1332.133657	16.777907
33.474385	1341.508356	16.782925
33.702367	1341.970692	16.787943
33.998058	1313.625793	16.792960
33.491870	1317.261671	16.797978
33.579872	1306.005024	16.802995
33.521992	1309.190295	16.808013
33.185780	1315.987653	16.813031
33.620218	1314.754338	16.818048
33.672882	1322.609697	16.823066
33.631497	1334.003714	16.828083
33.621642	1334.518139	16.833101
33.394646	1335.699566	16.838119
33.763510	1339.132968	16.843136
34.037611	1337.352629	16.848154
34.041250	1337.095676	16.853171
34.091461	1337.600521	16.858189
34.301864	1341.332909	16.863207
33.893010	1332.760473	16.868224
33.896671	1332.470482	16.873242
34.122585	1344.674476	16.878259
33.778419	1342.616780	16.883277
33.701962	1340.746055	16.888295
33.998007	1337.689609	16.893312
33.673102	1338.421025	16.898330
33.836268	1342.400052	16.903347
33.915370	1334.791160	16.908365
33.635685	1355.548307	16.913383
34.379173	1361.961125	16.918400
34.561162	1370.626462	16.923418
34.515769	1364.728454	16.928435
34.290423	1364.637011	16.933453
34.049642	1367.027178	16.938471
34.598437	1361.002946	16.943488
34.278799	1378.345084	16.948506
34.551658	1369.840086	16.953523
34.521018	1368.644760	16.958541
34.531589	1375.100541	16.963559
34.820865	1363.857368	16.968576
34.693685	1373.663721	16.973594
34.637925	1363.798524	16.978611
35.028824	1357.215869	16.983629
34.646729	1363.432240	16.988647
34.890967	1358.943127	16.993664
35.053201	1364.336492	16.998682
34.880209	1361.162933	17.003699
35.088218	1357.458264	17.008717
34.739905	1359.219051	17.013735
34.734100	1359.745416	17.018752
34.538480	1355.194317	17.023770
34.610357	1352.385984	17.028787
34.598536	1359.567364	17.033805
34.455219	1365.539584	17.038823
35.003209	1353.358512	17.043840
34.724526	1370.134098	17.048858
34.968556	1380.716551	17.053875
35.185643	1384.161586	17.058893
34.841733	1389.089829	17.063911
35.402024	1389.016238	17.068928
35.084665	1399.214743	17.073946
35.328131	1388.516847	17.078963
35.174335	1390.690220	17.083981
35.186368	1404.770437	17.088999
35.783583	1394.253652	17.094016
35.640645	1386.123279	17.099034
35.511331	1394.243659	17.104051
35.627457	1394.484730	17.109069
35.747125	1393.049920	17.114087
35.756340	1384.344709	17.119104
35.575763	1393.892170	17.124122
35.535096	1390.670758	17.129139
35.634157	1390.944439	17.134157
35.465462	1399.705049	17.139175
35.685602	1386.229691	17.144192
35.738497	1392.505692	17.149210
35.340441	1389.699937	17.154227
35.491455	1387.500337	17.159245
35.443480	1387.973652	17.164263
35.603792	1381.523718	17.169280
35.733051	1388.921719	17.174298
35.945733	1397.814991	17.179315
35.963706	1402.894742	17.184333
35.951930	1412.467205	17.189351
36.015204	1411.626569	17.194368
36.462749	1411.452979	17.199386
36.326587	1413.960180	17.204403
36.199461	1397.858111	17.209421
36.118104	1408.328879	17.214439
36.193996	1401.897119	17.219456
35.962333	1415.061360	17.224474
35.929625	1414.538061	17.229491
36.599838	1412.708697	17.234509
36.148209	1414.827324	17.239527
36.334405	1404.822834	17.244544
36.411081	1413.190378	17.249562
36.224221	1412.578403	17.254579
36.684126	1405.978429	17.259597
36.349384	1412.995826	17.264615
36.474179	1401.333678	17.269632
36.628403	1411.488444	17.274650
36.504417	1409.074716	17.279667
36.899100	1402.916165	17.284685
36.699960	1406.153874	17.289703
36.822778	1404.866429	17.294720
36.778284	1404.983675	17.299738
36.339720	1408.210804	17.304755
36.572263	1398.079374	17.309773
36.783096	1409.776155	17.314791
36.834357	1403.771478	17.319808
36.746036	1414.954388	17.324826
36.690284	1433.360373	17.329843
37.396404	1427.551703	17.334861
37.136589	1439.097047	17.339879
37.162416	1442.115622	17.344896
37.049246	1423.312694	17.349914
36.538866	1422.214325	17.354931
37.074159	1428.053173	17.359949
37.146858	1435.068523	17.364967
37.497226	1429.650081	17.369984
37.359479	1432.097760	17.375002
37.151376	1432.926959	17.380019
37.338139	1430.674459	17.385037
36.989502	1447.676016	17.390055
37.136162	1438.548505	17.395072
37.342453	1426.384114	17.400090
36.816571	1431.555331	17.405107
37.330915	1433.474283	17.410125
37.334870	1445.037341	17.415143
37.147069	1445.849932	17.420160
37.547082	1454.984717	17.425178
37.484018	1457.413412	17.430195
37.765328	1458.249504	17.435213
37.828541	1462.420690	17.440231
37.623243	1463.918000	17.445248
38.094110	1455.471825	17.450266
37.875998	1471.466275	17.455283
38.124369	1450.884707	17.460301
37.774567	1463.498380	17.465319
37.865186	1465.498286	17.470336
38.025494	1465.206905	17.475354
38.105642	1468.314353	17.480371
38.100439	1449.482374	17.485389
38.470260	1455.176159	17.490407
38.010903	1459.155398	17.495424
38.096305	1454.301464	17.500442
37.946766	1456.168992	17.505459
38.241190	1450.663506	17.510477
38.089221	1463.591704	17.515495
38.105510	1460.155120	17.520512
38.368525	1461.657182	17.525530
38.190011	1466.844586	17.530547
38.609736	1442.427288	17.535565
38.262512	1460.971032	17.540583
38.397511	1459.676134	17.545600
38.614510	1450.966846	17.550618
38.223872	1460.273350	17.555635
38.316299	1452.155742	17.560653
38.299360	1456.022734	17.565671
38.412853	1454.109902	17.570688
38.636571	1478.261859	17.575706
38.493493	1485.095349	17.580723
39.088901	1483.487913	17.585741
38.818847	1492.095637	17.590759
39.022973	1490.594650	17.595776
39.165582	1485.147971	17.600794
38.904036	1479.635185	17.605811
38.854431	1471.508756	17.610829
38.858191	1475.987525	17.615847
39.257250	1481.656208	17.620864
39.219574	1461.604752	17.625882
38.619962	1461.648505	17.630899
39.004498	1469.643716	17.635917
39.204067	1482.425415	17.640935
39.016979	1491.992068	17.645952
39.148516	1484.875761	17.650970
39.164719	1492.639495	17.655987
39.051089	1481.908816	17.661005
39.179233	1484.852092	17.666023
39.134782	1487.362769	17.671040
39.319958	1486.290322	17.676058
39.211622	1484.755008	17.681075
39.340093	1476.135332	17.686093
39.111536	1487.045711	17.691111
38.996263	1487.413354	17.696128
39.410627	1508.015982	17.701146
39.505190	1515.108898	17.706163
39.929606	1508.184977	17.711181
39.661021	1505.956321	17.716199
39.632699	1523.381950	17.721216
39.557046	1514.138045	17.726234
39.668716	1516.218760	17.731251
39.913557	1509.598767	17.736269
39.935097	1504.356227	17.741287
39.590888	1507.258432	17.746304
39.980426	1503.991194	17.751322
39.963620	1511.345696	17.756339
39.986837	1510.940894	17.761357
39.932559	1509.894049	17.766375
39.936754	1507.565258	17.771392
40.038447	1511.234801	17.776410
39.939974	1513.202734	17.781427
40.157397	1508.773696	17.786445
40.507017	1519.257610	17.791463
40.237508	1515.967270	17.796480
40.261965	1509.992780	17.801498
40.403625	1518.286311	17.806515
40.662956	1520.457526	17.811533
40.793274	1513.961979	17.816551
40.576202	1509.926290	17.821568
40.482450	1508.427974	17.826586
40.591334	1504.893239	17.831603
40.646233	1495.836958	17.836621
40.598572	1494.602649	17.841639
40.236963	1501.730556	17.846656
40.773071	1507.588185	17.851674
40.923741	1518.217089	17.856691
40.964089	1523.830521	17.861709
40.830247	1509.288324	17.866727
40.727351	1509.347243	17.871744
40.948947	1502.285779	17.876762
40.535774	1522.361286	17.881779
40.764199	1523.400879	17.886797
41.472456	1522.995367	17.891815
40.995774	1529.842754	17.896832
41.485990	1522.843837	17.901850
41.031994	1512.534732	17.906867
41.389638	1504.716942	17.911885
41.256978	1499.450230	17.916903
40.873700	1488.985927	17.921920
41.130692	1489.784213	17.926938
40.897369	1520.209417	17.931955
41.305856	1521.441311	17.936973
41.469779	1515.679752	17.941991
41.144677	1524.059525	17.947008
41.255960	1508.281907	17.952026
41.386067	1521.782605	17.957043
41.396562	1516.056526	17.962061
41.392272	1521.666065	17.967079
41.406312	1524.097418	17.972096
41.336316	1513.661001	17.977114
41.455067	1525.920780	17.982131
41.363347	1538.561001	17.987149
41.526904	1545.651580	17.992167
41.583726	1558.279926	17.997184
41.789183	1551.078648	18.002202
41.796851	1552.096820	18.007219
42.206219	1555.685843	18.012237
42.088866	1548.132554	18.017255
42.018746	1557.559468	18.022272
41.988254	1543.839208	18.027290
42.205230	1552.389745	18.032307
42.029972	1551.405452	18.037325
42.272697	1549.227382	18.042343
41.970745	1556.963237	18.047360
42.130983	1546.949420	18.052378
41.941958	1549.606651	18.057395
42.065657	1551.909618	18.062413
42.373369	1547.191666	18.067431
42.047555	1570.176095	18.072448
42.385413	1572.663570	18.077466
42.336776	1575.366846	18.082483
42.550483	1586.412054	18.087501
42.928045	1570.556507	18.092519
42.556994	1579.683777	18.097536
42.702004	1571.834579	18.102554
42.384491	1585.930561	18.107571
42.748929	1578.891113	18.112589
42.781852	1568.699376	18.117607
42.953270	1576.181988	18.122624
42.867026	1579.293187	18.127642
42.421217	1584.858329	18.132659
42.486109	1586.489533	18.137677
42.545091	1572.478899	18.142695
42.621914	1576.938968	18.147712
42.963632	1584.649265	18.152730
43.350683	1591.311738	18.157747
42.898598	1600.235645	18.162765
43.338058	1591.441243	18.167783
42.987354	1596.793013	18.172800
43.267477	1593.295444	18.177818
43.536454	1598.079606	18.182835
43.471210	1597.658234	18.187853
43.188587	1588.400883	18.192871
42.973963	1589.258659	18.197888
43.148015	1591.520567	18.202906
43.284977	1598.326752	18.207923
43.048424	1601.664855	18.212941
43.525293	1601.370966	18.217959
43.371136	1599.157867	18.222976
43.528473	1594.770634	18.227994
43.106051	1600.562510	18.233011
43.299707	1611.244404	18.238029
43.816473	1615.681515	18.243047
43.390286	1625.947086	18.248064
43.462893	1630.646168	18.253082
43.907933	1625.699428	18.258099
43.833116	1627.483484	18.263117
44.120504	1620.360345	18.268135
44.241879	1629.879468	18.273152
44.250899	1625.158788	18.278170
44.199285	1621.302755	18.283187
44.005395	1632.557726	18.288205
44.198256	1623.539140	18.293223
44.233218	1620.097181	18.298240
44.298338	1614.005260	18.303258
44.193177	1621.181992	18.308275
44.087207	1625.895395	18.313293
44.640943	1624.744496	18.318311
44.233947	1631.753856	18.323328
44.525299	1624.774808	18.328346
44.700106	1628.354853	18.333363
44.329242	1629.811727	18.338381
44.332973	1625.726633	18.343399
44.442062	1639.103371	18.348416
44.461690	1649.056389	18.353434
44.815062	1651.413196	18.358451
44.693834	1658.336881	18.363469
44.923422	1651.474641	18.368487
44.834024	1658.133688	18.373504
44.775205	1654.125419	18.378522
44.892737	1655.939366	18.383539
44.634460	1656.523310	18.388557
45.062783	1654.774184	18.393575
45.025575	1656.145600	18.398592
44.900635	1652.705538	18.403610
45.241151	1647.487584	18.408627
45.267187	1652.650298	18.413645
44.809634	1650.170958	18.418663
44.796914	1663.633214	18.423680
44.954683	1669.662938	18.428698
45.614818	1668.414053	18.433715
45.560350	1672.571032	18.438733
45.516929	1677.207618	18.443751
45.504309	1665.921908	18.448768
45.268477	1675.541289	18.453786
45.677623	1672.104926	18.458803
45.633076	1673.527853	18.463821
45.681611	1677.807626	18.468839
45.582423	1680.851694	18.473856
45.594345	1679.114701	18.478874
45.859990	1674.195768	18.483891
45.763607	1684.057982	18.488909
45.790902	1683.624209	18.493927
45.805484	1676.627138	18.498944
45.941510	1686.084970	18.503962
46.025632	1677.030208	18.508979
45.784144	1685.378647	18.513997
45.722770	1676.631820	18.519015
46.003357	1682.280149	18.524032
45.927105	1675.167785	18.529050
46.023108	1681.316694	18.534067
45.844284	1684.498524	18.539085
46.181598	1686.594404	18.544103
46.361759	1696.823888	18.549120
46.442071	1704.610547	18.554138
46.476679	1707.855090	18.559155
46.506792	1711.760266	18.564173
46.637782	1703.025219	18.569191
46.871706	1704.355759	18.574208
46.577314	1706.771048	18.579226
46.844684	1689.403106	18.584243
46.929829	1696.017030	18.589261
47.091195	1675.692852	18.594279
46.772099	1665.113574	18.599296
46.912271	1659.682950	18.604314
46.871536	1656.559808	18.609331
46.820811	1662.423783	18.614349
46.852067	1646.150668	18.619367
47.365348	1659.579374	18.624384
47.319720	1660.179743	18.629402
47.462434	1649.668405	18.634419
47.500117	1663.012507	18.639437
47.182156	1658.093054	18.644455
47.375525	1650.771741	18.649472
47.108280	1658.786844	18.654490
47.082103	1645.905046	18.659507
47.196208	1649.223417	18.664525
46.955551	1647.701323	18.669543
46.935192	1666.588046	18.674560
47.225255	1681.249496	18.679578
47.464550	1678.133603	18.684595
47.643830	1683.551113	18.689613
47.661435	1681.812427	18.694631
48.005642	1682.080840	18.699648
47.529033	1681.403371	18.704666
47.579504	1681.521205	18.709683
47.296641	1692.293313	18.714701
47.530579	1684.996188	18.719719
47.424247	1682.874554	18.724736
47.380471	1697.886578	18.729754
47.735956	1705.663175	18.734771
47.844435	1716.277716	18.739789
47.743844	1718.986159	18.744807
48.100604	1718.683108	18.749824
47.937968	1708.401331	18.754842
48.214887	1711.003947	18.759859
48.196581	1718.170808	18.764877
48.119062	1717.896901	18.769895
48.296341	1712.819794	18.774912
48.101165	1713.714589	18.779930
48.270420	1724.483833	18.784947
48.263919	1734.673110	18.789965
48.127971	1746.675592	18.794983
48.500887	1747.723621	18.800000
48.416248	1755.777299	18.805018
48.820391	1736.568191	18.810035
48.680044	1740.476963	18.815053
48.754813	1736.987728	18.820071
48.860388	1739.704982	18.825088
48.536346	1739.072395	18.830106
48.886153	1729.630719	18.835123
48.801687	1733.731935	18.840141
48.626273	1729.281319	18.845159
48.770871	1739.285259	18.850176
48.738486	1746.875971	18.855194
49.574220	1758.776199	18.860211
49.504002	1765.887651	18.865229
49.356590	1748.523650	18.870247
49.334205	1732.354954	18.875264
49.242529	1743.691242	18.880282
49.341016	1737.469673	18.885299
49.535529	1734.569346	18.890317
49.264754	1749.157491	18.895335
49.648735	1755.582206	18.900352
49.789776	1752.529159	18.905370
49.948628	1747.086872	18.910387
49.932720	1737.091577	18.915405
49.633896	1722.844477	18.920423
49.896977	1719.362968	18.925440
49.488149	1716.825506	18.930458
49.635053	1720.878021	18.935475
49.879279	1731.205071	18.940493
49.877505	1746.530573	18.945511
50.296801	1744.955132	18.950528
50.012603	1750.361635	18.955546
50.046648	1749.540585	18.960563
49.901981	1755.074282	18.965581
49.886234	1762.053557	18.970599
50.545381	1754.960733	18.975616
49.978065	1757.649229	18.980634
50.075844	1746.352928	18.985651
50.547200	1747.070638	18.990669
49.982915	1755.004957	18.995687
50.123842	1747.206656	19.000704
50.057872	1762.638372	19.005722
50.332638	1759.902216	19.010739
50.269127	1762.998816	19.015757
50.341591	1778.989736	19.020775
50.803186	1784.660365	19.025792
50.492293	1778.857229	19.030810
50.752486	1779.754129	19.035827
51.198947	1780.069161	19.040845
50.739478	1791.530212	19.045863
50.735082	1783.771585	19.050880
50.540023	1786.942655	19.055898
50.612289	1782.327461	19.060915
50.590349	1790.080134	19.065933
50.721992	1781.591127	19.070951
50.874808	1785.295847	19.075968
50.946220	1801.652707	19.080986
51.254404	1807.318708	19.086003
51.802236	1799.170753	19.091021
51.461665	1797.744805	19.096039
51.811022	1802.524083	19.101056
51.517866	1795.671206	19.106074
51.624064	1783.919692	19.111091
51.441429	1769.495132	19.116109
51.383407	1788.871750	19.121127
51.865182	1788.569998	19.126144
51.664727	1804.835718	19.131162
51.708768	1803.628446	19.136179
52.025097	1798.186196	19.141197
51.905388	1801.568634	19.146215
52.057288	1795.594939	19.151232
51.608519	1789.610069	19.156250
51.929746	1796.426289	19.161267
52.110162	1801.361504	19.166285
51.679428	1806.177096	19.171303
52.209372	1791.927540	19.176320
51.943458	1785.612259	19.181338
52.047449	1793.194618	19.186355
52.433170	1798.224512	19.191373
51.925578	1790.351064	19.196391
52.043863	1793.493401	19.201408
51.904106	1807.573833	19.206426
52.179424	1808.924525	19.211443
52.352195	1818.065107	19.216461
51.944220	1828.982330	19.221479
52.627845	1818.024364	19.226496
52.434836	1832.844810	19.231514
52.375854	1831.538342	19.236531
52.764422	1827.335973	19.241549
52.619549	1852.856167	19.246567
53.264181	1846.867583	19.251584
53.285931	1849.918355	19.256602
53.167222	1837.024401	19.261619
53.288804	1825.334111	19.266637
52.942186	1830.605085	19.271655
53.205028	1815.196243	19.276672
53.025110	1833.547813	19.281690
52.714674	1825.815160	19.286707
53.253708	1832.235632	19.291725
53.295666	1847.716298	19.296743
53.162775	1852.619694	19.301760
53.452029	1857.459701	19.306778
53.276234	1858.494567	19.311795
53.621846	1855.426966	19.316813
53.480147	1858.917536	19.321831
53.754658	1856.577829	19.326848
53.371945	1856.271576	19.331866
53.400658	1854.922017	19.336883
53.620582	1851.655798	19.341901
53.257811	1861.721073	19.346919
53.452464	1864.765511	19.351936
53.690834	1880.287251	19.356954
53.850126	1876.646854	19.361971
54.012915	1868.936243	19.366989
53.646585	1889.312326	19.372007
54.374021	1878.400815	19.377024
54.193331	1881.932218	19.382042
54.226992	1879.236851	19.387059
54.318078	1874.396030	19.392077
54.381816	1891.312672	19.397095
54.343979	1880.105540	19.402112
54.317002	1885.651193	19.407130
54.218061	1883.390703	19.412147
54.375151	1884.316637	19.417165
54.428825	1894.344623	19.422183
54.788033	1898.969770	19.427200
54.674592	1903.920421	19.432218
54.748255	1907.029784	19.437235
54.729330	1904.064355	19.442253
54.498322	1905.119828	19.447271
54.820720	1901.561959	19.452288
54.717500	1910.705713	19.457306
54.838641	1898.454616	19.462323
54.771822	1900.411260	19.467341
54.773019	1912.465156	19.472359
55.109452	1925.770507	19.477376
55.380374	1930.102983	19.482394
55.055999	1937.331348	19.487411
55.572330	1935.118242	19.492429
55.399338	1934.363236	19.497447
55.546186	1936.050627	19.502464
55.701777	1929.410070	19.507482
55.347273	1934.320519	19.512499
55.607003	1926.094164	19.517517
55.718008	1934.120672	19.522535
55.603537	1925.872977	19.527552
55.711850	1929.370100	19.532570
55.548223	1934.103808	19.537587
56.074124	1932.152675	19.542605
56.173074	1930.157939	19.547623
56.223081	1927.293991	19.552640
56.031990	1929.361698	19.557658
55.505450	1928.038544	19.562675
56.255147	1921.541574	19.567693
55.940162	1923.149235	19.572711
56.096940	1922.091512	19.577728
56.333912	1917.599456	19.582746
56.120237	1926.826906	19.587763
56.279975	1924.974283	19.592781
56.372174	1923.368399	19.597799
56.639257	1928.602888	19.602816
56.294127	1918.076343	19.607834
56.308478	1931.108213	19.612851
56.866426	1944.562310	19.617869
56.783338	1962.558019	19.622887
56.894847	1962.443524	19.627904
57.062815	1961.652232	19.632922
56.634169	1960.820011	19.637939
56.684790	1960.716013	19.642957
56.925579	1959.052607	19.647975
56.599217	1953.296701	19.652992
56.894225	1958.038291	19.658010
56.619955	1954.529943	19.663027
56.919834	1949.432416	19.668045
56.642803	1964.867330	19.673063
56.968267	1977.580621	19.678080
57.041265	1981.700056	19.683098
56.898346	1991.952170	19.688115
57.272222	1989.122296	19.693133
57.153702	1993.155865	19.698151
57.323226	2004.766114	19.703168
57.674297	2020.501281	19.708186
57.719700	2020.925115	19.713203
57.847059	2005.406323	19.718221
57.999514	2001.062223	19.723239
58.353883	2005.654353	19.728256
58.849195	1987.339649	19.733274
58.591355	1981.070189	19.738291
58.509920	1967.040667	19.743309
58.757079	1958.191767	19.748327
58.719964	1950.807167	19.753344
58.786165	1949.236890	19.758362
58.489397	1934.303370	19.763379
58.729184	1918.172885	19.768397
58.529129	1925.208374	19.773415
58.421970	1930.475017	19.778432
58.853501	1921.472459	19.783450
58.652281	1922.892079	19.788467
58.663977	1919.039242	19.793485
58.674371	1919.617316	19.798503
58.401344	1922.831525	19.803520
58.596297	1918.053568	19.808538
58.470274	1923.613458	19.813555
58.719613	1917.610016	19.818573
58.428705	1923.316545	19.823591
58.494742	1950.284372	19.828608
59.092080	1954.498730	19.833626
58.964949	1965.426325	19.838643
59.173287	1950.210090	19.843661
58.867715	1955.993694	19.848679
58.698816	1963.789559	19.853696
58.691173	1953.569413	19.858714
58.797862	1975.521179	19.863731
59.102800	1975.064357	19.868749
59.282300	1983.861815	19.873767
59.264978	1994.456508	19.878784
59.191697	1981.602375	19.883802
59.138080	1988.150467	19.888819
59.239864	2012.614575	19.893837
59.321101	2023.932158	19.898855
59.256174	2018.098351	19.903872
59.786299	2013.460408	19.908890
59.546787	2026.156869	19.913907
59.732820	2023.828100	19.918925
60.015241	2048.880917	19.923943
59.929323	2051.482467	19.928960
60.078480	2047.218322	19.933978
59.980105	2051.474440	19.938995
60.315330	2049.411331	19.944013
60.302016	2053.933903	19.949031
60.104181	2050.220633	19.954048
60.463564	2049.683549	19.959066
60.035894	2052.275887	19.964083
60.368723	2048.923974	19.969101
60.426438	2051.602512	19.974119
60.591827	2068.253807	19.979136
61.055210	2066.349597	19.984154
60.789256	2071.138995	19.989171
60.942726	2076.330304	19.994189
60.856594	2070.646160	19.999207
60.769922	2079.308359	20.004224
61.385539	2064.452589	20.009242
60.702489	2073.919378	20.014259
60.914296	2074.360724	20.019277
60.907905	2074.542690	20.024295
60.913418	2082.517672	20.029312
60.882967	2077.334344	20.034330
60.964705	2089.124626	20.039347
61.078774	2099.896658	20.044365
61.307773	2105.040536	20.049383
61.085984	2110.559922	20.054400
61.564290	2110.646501	20.059418
61.319088	2109.821197	20.064435
61.701624	2119.717450	20.069453
62.151925	2122.881635	20.074471
61.671195	2123.450729	20.079488
62.076263	2122.579930	20.084506
62.136487	2131.297390	20.089523
62.259264	2126.417610	20.094541
61.646556	2114.167737	20.099559
61.939280	2128.536611	20.104576
62.296671	2122.415174	20.109594
62.339575	2136.466792	20.114611
62.146913	2129.832128	20.119629
62.107244	2123.855815	20.124647
62.229176	2126.406140	20.129664
62.815320	2129.156949	20.134682
62.658492	2132.186705	20.139699
62.788749	2130.733618	20.144717
62.803702	2126.866048	20.149735
62.418191	2135.678192	20.154752
62.883605	2128.246398	20.159770
62.502820	2136.048615	20.164787
62.620150	2132.041225	20.169805
62.707289	2131.959719	20.174823
62.748989	2140.456752	20.179840
62.906495	2157.987223	20.184858
63.146327	2154.101089	20.189875
63.129385	2160.428674	20.194893
63.131517	2163.687150	20.199911
63.149088	2171.841957	20.204928
63.489376	2155.970486	20.209946
63.447358	2167.082088	20.214963
63.223586	2173.142192	20.219981
63.542831	2160.863216	20.224999
63.500794	2172.004715	20.230016
63.495985	2163.639502	20.235034
63.341215	2166.008213	20.240051
63.489247	2174.524492	20.245069
63.592189	2176.329821	20.250087
63.533677	2176.763939	20.255104
63.703365	2174.608439	20.260122
63.857271	2180.375490	20.265139
63.906461	2191.054107	20.270157
64.129848	2194.867238	20.275175
64.008045	2211.245146	20.280192
64.204014	2211.090437	20.285210
64.199937	2213.916510	20.290227
64.144491	2202.324942	20.295245
64.438781	2208.179737	20.300263
64.197763	2212.076372	20.305280
64.605831	2206.671256	20.310298
64.309805	2209.042836	20.315315
64.623811	2223.156706	20.320333
64.985381	2220.554500	20.325351
64.967627	2225.652822	20.330368
65.351904	2223.087897	20.335386
65.240946	2224.262684	20.340403
65.014978	2223.804784	20.345421
65.208016	2223.173876	20.350439
65.114812	2239.269592	20.355456
65.361973	2221.824797	20.360474
65.116861	2225.771643	20.365491
65.091588	2243.492614	20.370509
65.256141	2236.820600	20.375527
65.245346	2241.215402	20.380544
65.310768	2237.139176	20.385562
65.676057	2238.746146	20.390579
65.402912	2218.745357	20.395597
65.955690	2224.102721	20.400615
65.472002	2234.053028	20.405632
65.860271	2226.671243	20.410650
65.772972	2251.040052	20.415667
65.826316	2261.574901	20.420685
66.015319	2269.519937	20.425703
65.944394	2266.619362	20.430720
66.177232	2257.347812	20.435738
65.941793	2262.626378	20.440755
65.921238	2263.358065	20.445773
66.264481	2259.010207	20.450791
66.303448	2260.577976	20.455808
66.152846	2259.087861	20.460826
66.236629	2269.014554	20.465843
66.069674	2287.381931	20.470861
66.415833	2273.695308	20.475879
66.244785	2287.192828	20.480896
66.763078	2280.844301	20.485914
66.606877	2295.216499	20.490931
66.714594	2303.320034	20.495949
67.268200	2303.740704	20.500967
67.058972	2317.273444	20.505984
67.297125	2312.253283	20.511002
67.751563	2305.487027	20.516019
67.157680	2312.645286	20.521037
67.763501	2302.835984	20.526055
67.692563	2302.413139	20.531072
67.478671	2289.801400	20.536090
67.469737	2292.607026	20.541107
67.162260	2308.627654	20.546125
67.774160	2310.520164	20.551143
67.961926	2309.272625	20.556160
67.721027	2301.907760	20.561178
67.706096	2299.038364	20.566195
67.581033	2305.592486	20.571213
67.874249	2302.015578	20.576231
68.095410	2294.451965	20.581248
68.001861	2292.616878	20.586266
67.874620	2292.628552	20.591283
67.956550	2306.594666	20.596301
68.339113	2314.021178	20.601319
68.110104	2326.772858	20.606336
68.285862	2333.879183	20.611354
68.567744	2331.487886	20.616371
68.204772	2335.645483	20.621389
68.331322	2326.287797	20.626407
68.453289	2334.943619	20.631424
68.324618	2324.821958	20.636442
68.686585	2347.465098	20.641459
68.644153	2356.742594	20.646477
69.319207	2351.519813	20.651495
69.011407	2360.643771	20.656512
69.041561	2354.656228	20.661530
69.482713	2338.508902	20.666547
69.440273	2356.408156	20.671565
69.722501	2357.186739	20.676583
69.425564	2347.390012	20.681600
69.333540	2356.772954	20.686618
69.662855	2353.860449	20.691635
69.417253	2352.387047	20.696653
69.053546	2347.815243	20.701671
69.463975	2354.846399	20.706688
69.551246	2361.951905	20.711706
69.959696	2358.453358	20.716723
69.896277	2356.477378	20.721741
69.739557	2348.258992	20.726759
69.647964	2350.838688	20.731776
69.785510	2371.564563	20.736794
70.130213	2371.169036	20.741811
69.833477	2378.287806	20.746829
70.012511	2373.054447	20.751847
70.260751	2377.358427	20.756864
69.818684	2372.195799	20.761882
70.076406	2389.193780	20.766899
70.158670	2405.116964	20.771917
70.344542	2410.434586	20.776935
70.385215	2421.720404	20.781952
70.352990	2413.071528	20.786970
70.826493	2421.717751	20.791987
70.667870	2436.062156	20.797005
71.264596	2433.908526	20.802023
71.138595	2429.577242	20.807040
70.969831	2439.605679	20.812058
71.612957	2432.342828	20.817075
71.467178	2444.448133	20.822093
71.263816	2435.552015	20.827111
71.390037	2431.617065	20.832128
71.688555	2447.082624	20.837146
71.690927	2435.215783	20.842163
71.653860	2433.903405	20.847181
71.538589	2434.225447	20.852199
71.692182	2438.020669	20.857216
71.591689	2433.171673	20.862234
71.814300	2432.031050	20.867251
71.845485	2429.401263	20.872269
71.742324	2431.056216	20.877287
71.821513	2433.187867	20.882304
71.861773	2442.640226	20.887322
72.031156	2454.494700	20.892339
72.015415	2468.841523	20.897357
72.251104	2458.957423	20.902375
72.322007	2460.114239	20.907392
72.145107	2461.555990	20.912410
72.624742	2454.770703	20.917427
72.574540	2456.137973	20.922445
72.508671	2460.331604	20.927463
73.153123	2462.142646	20.932480
73.214579	2459.161926	20.937498
73.029761	2450.457916	20.942515
72.665872	2463.367304	20.947533
72.865479	2450.341026	20.952551
73.184480	2460.607904	20.957568
73.302873	2473.455336	20.962586
73.552149	2471.280023	20.967603
73.468056	2482.174397	20.972621
73.519258	2473.818952	20.977639
73.501320	2458.283521	20.982656
73.640800	2469.934329	20.987674
73.811409	2462.712992	20.992691
73.506798	2470.680220	20.997709
73.277721	2471.219419	21.002727
73.874144	2479.382772	21.007744
73.266452	2492.662220	21.012762
73.706193	2478.672590	21.017779
73.380967	2492.042286	21.022797
73.799909	2504.648317	21.027815
73.994037	2512.226116	21.032832
74.001515	2504.923796	21.037850
74.087250	2503.289777	21.042867
74.336247	2510.150105	21.047885
74.545562	2504.559477	21.052903
74.762308	2495.090548	21.057920
74.780827	2495.661844	21.062938
74.979368	2497.785483	21.067955
74.810206	2499.799429	21.072973
74.801988	2495.367536	21.077991
74.904377	2501.714783	21.083008
74.763384	2497.950643	21.088026
75.204394	2499.268688	21.093043
75.118697	2517.510913	21.098061
75.371008	2527.963884	21.103079
75.365538	2525.518482	21.108096
74.886558	2535.664888	21.113114
75.224888	2533.874169	21.118131
75.335033	2523.549888	21.123149
75.392073	2518.650570	21.128167
75.693939	2517.986564	21.133184
75.511688	2520.148907	21.138202
75.657146	2506.754435	21.143219
75.751162	2530.708579	21.148237
76.093001	2538.366668	21.153255
76.365381	2541.787434	21.158272
76.125675	2543.662396	21.163290
76.403670	2533.655083	21.168307
76.346646	2537.975540	21.173325
76.445834	2539.333154	21.178343
76.581715	2528.149737	21.183360
75.975694	2520.426876	21.188378
76.290736	2526.862932	21.193395
76.149761	2541.521624	21.198413
76.516458	2541.039995	21.203431
76.928917	2535.189634	21.208448
76.860837	2553.801941	21.213466
76.660467	2542.820800	21.218483
76.984671	2536.607734	21.223501
76.641823	2549.604300	21.228519
76.718087	2537.720873	21.233536
76.917302	2554.818836	21.238554
77.353117	2562.787603	21.243571
77.451617	2554.118583	21.248589
77.115444	2559.458942	21.253607
77.219716	2551.884732	21.258624
77.280604	2569.449985	21.263642
77.068627	2574.823246	21.268659
77.379129	2563.541161	21.273677
77.527411	2584.003689	21.278695
77.477833	2591.804458	21.283712
77.581419	2601.260194	21.288730
77.680325	2598.127167	21.293747
77.479531	2596.397242	21.298765
77.621264	2608.332550	21.303783
78.129847	2616.762488	21.308800
78.378446	2618.085271	21.313818
78.972033	2617.049089	21.318835
79.034252	2612.916635	21.323853
78.632937	2613.620173	21.328871
78.938657	2613.278841	21.333888
78.599818	2618.963390	21.338906
78.690631	2612.100022	21.343923
78.857280	2617.039285	21.348941
78.732152	2616.293913	21.353959
78.574591	2610.564313	21.358976
78.562309	2617.210713	21.363994
78.554449	2620.847666	21.369011
79.109443	2627.850397	21.374029
79.285966	2639.972114	21.379047
79.568515	2652.597664	21.384064
79.311079	2655.494902	21.389082
79.703109	2640.015824	21.394099
79.692535	2641.614346	21.399117
79.462514	2643.568796	21.404135
79.699787	2632.532743	21.409152
79.922924	2641.687051	21.414170
79.938598	2645.340709	21.419187
80.091883	2636.085539	21.424205
79.507279	2642.632859	21.429223
79.633931	2649.128115	21.434240
79.633425	2666.224235	21.439258
79.904683	2665.204840	21.444275
80.081846	2668.977487	21.449293
79.965000	2670.443504	21.454311
80.369321	2680.631644	21.459328
80.644013	2687.942615	21.464346
80.653448	2689.977663	21.469363
80.840951	2687.925440	21.474381
80.636545	2686.740410	21.479399
80.942365	2687.485360	21.484416
80.810661	2685.629563	21.489434
81.148882	2691.407541	21.494451
80.870703	2691.285177	21.499469
80.743513	2698.582367	21.504487
81.230251	2704.453871	21.509504
81.269559	2719.044662	21.514522
81.268075	2725.322830	21.519539
81.510318	2725.215015	21.524557
81.726562	2718.983691	21.529575
81.746396	2721.254639	21.534592
81.275252	2728.104052	21.539610
81.907104	2710.935571	21.544627
82.115712	2715.044602	21.549645
81.955755	2720.319947	21.554663
82.129402	2718.353310	21.559680
81.937080	2716.077689	21.564698
81.869393	2713.178867	21.569715
82.648918	2730.602971	21.574733
82.396486	2749.283468	21.579751
82.548458	2749.403218	21.584768
82.974993	2750.548184	21.589786
82.836382	2746.852820	21.594803
83.199154	2736.354381	21.599821
82.637848	2732.184454	21.604839
82.903104	2730.427390	21.609856
82.766288	2740.004933	21.614874
82.353957	2745.079830	21.619891
82.910876	2736.889012	21.624909
82.657999	2743.941180	21.629927
83.236963	2749.097130	21.634944
83.148528	2772.712634	21.639962
83.222973	2764.821349	21.644979
83.532191	2761.654750	21.649997
83.135416	2762.840546	21.655015
83.666974	2753.713767	21.660032
83.899688	2747.136844	21.665050
83.548514	2759.190208	21.670067
84.046955	2773.180811	21.675085
84.331697	2784.958949	21.680103
84.192461	2783.438649	21.685120
84.129619	2779.347329	21.690138
84.237890	2781.714309	21.695155
84.783339	2784.762787	21.700173
84.648035	2790.816115	21.705191
84.754901	2791.621902	21.710208
84.852589	2790.340706	21.715226
84.607004	2786.339094	21.720243
84.938124	2785.669627	21.725261
84.918947	2785.538997	21.730279
84.879415	2776.883204	21.735296
85.064151	2780.264515	21.740314
84.852688	2788.531703	21.745331
85.388290	2775.748895	21.750349
84.943360	2783.457849	21.755367
85.121725	2782.959050	21.760384
85.234039	2769.358812	21.765402
85.176949	2779.925805	21.770419
84.870424	2779.682102	21.775437
85.404239	2790.521434	21.780455
85.553424	2793.638610	21.785472
85.929978	2802.865309	21.790490
85.671470	2811.059778	21.795507
86.257229	2799.789468	21.800525
86.233181	2803.348814	21.805543
85.994612	2807.165765	21.810560
86.236422	2799.116409	21.815578
86.300979	2793.906663	21.820595
86.256328	2800.386826	21.825613
86.137613	2800.986311	21.830631
86.528429	2811.982186	21.835648
86.667570	2834.010304	21.840666
86.393679	2838.444880	21.845683
86.790129	2828.602545	21.850701
86.868903	2828.917250	21.855719
86.865399	2829.643099	21.860736
87.107353	2820.147131	21.865754
86.668229	2839.962701	21.870771
86.999149	2846.984753	21.875789
87.054887	2858.829362	21.880807
87.272894	2852.400260	21.885824
87.474177	2845.476690	21.890842
87.125411	2846.485715	21.895859
87.637528	2849.617397	21.900877
87.280204	2864.822210	21.905895
87.577506	2876.035205	21.910912
87.956240	2891.810172	21.915930
87.983365	2880.575393	21.920947
88.199977	2886.104607	21.925965
87.870400	2891.252885	21.930983
87.875463	2882.689032	21.936000
87.899714	2890.571794	21.941018
88.026415	2914.228735	21.946035
88.238275	2909.734090	21.951053
88.437891	2922.561888	21.956071
88.394830	2910.639763	21.961088
88.864199	2903.504293	21.966106
88.692284	2918.274489	21.971123
89.091515	2938.674686	21.976141
88.801929	2934.896369	21.981159
89.250134	2945.067472	21.986176
89.314122	2939.491988	21.991194
89.108653	2948.509530	21.996211
89.442092	2939.421310	22.001229
89.374409	2935.278801	22.006247
89.456030	2941.125331	22.011264
89.681934	2933.808417	22.016282
89.549894	2938.599553	22.021299
89.640845	2940.150453	22.026317
89.879748	2957.428989	22.031335
89.783896	2956.598695	22.036352
90.057188	2961.141133	22.041370
89.820202	2979.772263	22.046387
90.222621	2958.441110	22.051405
89.844095	2976.234245	22.056423
89.705818	2972.021175	22.061440
89.755789	2980.302632	22.066458
89.882818	2986.241053	22.071475
90.315517	2997.766864	22.076493
90.123947	3011.558586	22.081511
90.406996	3029.613642	22.086528
90.958460	3022.358044	22.091546
90.718531	3026.991782	22.096563
90.466180	3023.382134	22.101581
91.080741	3037.399312	22.106599
91.441201	3057.503009	22.111616
91.844178	3057.478116	22.116634
91.893531	3056.855142	22.121651
91.811192	3036.778751	22.126669
91.764918	3048.177245	22.131687
91.987302	3049.892055	22.136704
92.048309	3048.833794	22.141722
92.061810	3045.940051	22.146739
92.347007	3048.445627	22.151757
92.374110	3050.777610	22.156775
92.548917	3045.842818	22.161792
92.555516	3025.111163	22.166810
92.293785	3020.945296	22.171827
91.992480	3033.682372	22.176845
92.417044	3036.629042	22.181863
92.222856	3047.001769	22.186880
92.605969	3037.708124	22.191898
92.344992	3054.544170	22.196915
92.962593	3054.126353	22.201933
93.035697	3063.037400	22.206951
92.785342	3076.081037	22.211968
92.913931	3073.509546	22.216986
92.736393	3074.647032	22.222003
92.962771	3075.233975	22.227021
93.215090	3086.957746	22.232039
93.101107	3108.674233	22.237056
93.260521	3102.458103	22.242074
93.333369	3110.527530	22.247091
93.780896	3113.136238	22.252109
94.009052	3131.946683	22.257127
93.966422	3131.671117	22.262144
94.393998	3130.064328	22.267162
94.288909	3130.922812	22.272179
94.259291	3130.616853	22.277197
94.311249	3129.737807	22.282215
94.398457	3135.735343	22.287232
94.384379	3132.798783	22.292250
94.572451	3129.913372	22.297267
94.381742	3133.779413	22.302285
94.693264	3138.234788	22.307303
95.036201	3156.607689	22.312320
95.470942	3152.761797	22.317338
95.445129	3139.309103	22.322355
95.220186	3122.456122	22.327373
95.249635	3124.925403	22.332391
95.368548	3139.477961	22.337408
95.389133	3146.765968	22.342426
95.753501	3148.665032	22.347443
95.693815	3145.933973	22.352461
95.828961	3143.274108	22.357479
96.239550	3150.190782	22.362496
96.030313	3153.829300	22.367514
95.751851	3156.547489	22.372531
96.091217	3153.269020	22.377549
96.096672	3151.493552	22.382567
95.844720	3154.646452	22.387584
96.070579	3146.184897	22.392602
95.797664	3162.644601	22.397619
96.136561	3174.839201	22.402637
96.329180	3173.682854	22.407655
96.002191	3183.490814	22.412672
96.155237	3201.691888	22.417690
96.472047	3209.213517	22.422707
96.435522	3204.608144	22.427725
96.870074	3226.892601	22.432743
97.327210	3232.186149	22.437760
97.292363	3239.801628	22.442778
97.592494	3243.071823	22.447795
97.267260	3240.374438	22.452813
97.625059	3238.699315	22.457831
97.131692	3236.073578	22.462848
97.929240	3241.094164	22.467866
98.162528	3247.218698	22.472883
98.303938	3241.223278	22.477901
98.679677	3250.511750	22.482919
98.632373	3258.545354	22.487936
98.890462	3243.088575	22.492954
98.326517	3223.130415	22.497971
98.258078	3225.048947	22.502989
98.720164	3236.381472	22.508007
98.675066	3241.074672	22.513024
98.832221	3238.290925	22.518042
99.117479	3253.028675	22.523059
98.923380	3244.795289	22.528077
98.898708	3236.994285	22.533095
99.042516	3259.355833	22.538112
98.771156	3245.153202	22.543130
99.080223	3261.956010	22.548147
99.038000	3269.674157	22.553165
99.493908	3279.299916	22.558183
99.166635	3279.684098	22.563200
99.449396	3271.137881	22.568218
99.833329	3292.623423	22.573235
99.505182	3306.633859	22.578253
99.793501	3304.431748	22.583271
99.472022	3315.720940	22.588288
99.695034	3315.274004	22.593306
99.915757	3318.294142	22.598323
100.104191	3348.093446	22.603341
100.372425	3344.336988	22.608359
100.326079	3339.846415	22.613376
100.306050	3336.081646	22.618394
100.297284	3338.628641	22.623411
100.502714	3354.980032	22.628429
100.811483	3357.477970	22.633447
101.141677	3359.502869	22.638464
101.349296	3357.775377	22.643482
101.159358	3361.687765	22.648499
101.148723	3363.376052	22.653517
101.540055	3363.814776	22.658535
101.665847	3386.410663	22.663552
102.045273	3383.974540	22.668570
102.167359	3381.427632	22.673587
101.930243	3382.999427	22.678605
102.210142	3386.180844	22.683623
102.008823	3386.419868	22.688640
102.089962	3383.165219	22.693658
102.244425	3383.236595	22.698675
101.712285	3387.657448	22.703693
102.080439	3375.232788	22.708711
102.199446	3395.806532	22.713728
101.902966	3407.350613	22.718746
102.106556	3414.190291	22.723763
102.464441	3430.860433	22.728781
102.959967	3438.303338	22.733799
102.965347	3446.485973	22.738816
103.159562	3446.616302	22.743834
103.310965	3442.713253	22.748851
103.231732	3454.829232	22.753869
103.435388	3455.419816	22.758887
103.246537	3462.602926	22.763904
103.720224	3467.460481	22.768922
103.974945	3481.728197	22.773939
103.675179	3485.941324	22.778957
104.118717	3471.271274	22.783975
103.692829	3486.944701	22.788992
103.774544	3485.279750	22.794010
104.490730	3486.908006	22.799027
104.144773	3509.429843	22.804045
104.127862	3498.480086	22.809063
104.304212	3505.995161	22.814080
104.487869	3504.900004	22.819098
104.882203	3519.261919	22.824115
104.945785	3533.998327	22.829133
105.128747	3533.958176	22.834151
105.006452	3533.803076	22.839168
104.924087	3534.669759	22.844186
105.380866	3535.624322	22.849203
105.293731	3538.795074	22.854221
105.446197	3528.363434	22.859239
105.329928	3543.686265	22.864256
105.302439	3537.689337	22.869274
105.829974	3550.788711	22.874291
105.477088	3561.657521	22.879309
105.842015	3562.751023	22.884327
105.701563	3567.960628	22.889344
105.872130	3578.089129	22.894362
106.012167	3587.720622	22.899379
105.705619	3603.433356	22.904397
106.108009	3590.829205	22.909415
106.211127	3609.644469	22.914432
106.634495	3620.626327	22.919450
106.487349	3622.441036	22.924467
106.425521	3634.021822	22.929485
106.922445	3614.762430	22.934503
106.859085	3642.198470	22.939520
106.848853	3653.118908	22.944538
107.451254	3641.383542	22.949555
107.401760	3651.501557	22.954573
107.623101	3648.683900	22.959591
108.034518	3648.250179	22.964608
107.906488	3650.629021	22.969626
108.061831	3644.455792	22.974643
108.177853	3647.413242	22.979661
108.280792	3645.585984	22.984679
108.315814	3653.151203	22.989696
108.316063	3674.029044	22.994714
108.606543	3678.426583	22.999731
108.419916	3680.997278	23.004749
108.720411	3678.834079	23.009767
108.706353	3672.172589	23.014784
108.432390	3670.495106	23.019802
108.338042	3673.518359	23.024819
108.357923	3699.103603	23.029837
108.743809	3705.366050	23.034855
108.920423	3713.721340	23.039872
108.865307	3742.199361	23.044890
109.171043	3738.248026	23.049907
108.983456	3749.656225	23.054925
109.297009	3757.239231	23.059943
109.501546	3772.504852	23.064960
109.372455	3782.642730	23.069978
110.011250	3774.842633	23.074995
109.764248	3775.376078	23.080013
109.896368	3788.397118	23.085031
111.115344	3783.762074	23.090048
110.926412	3789.821216	23.095066
111.539854	3783.532403	23.100083
111.079214	3771.846081	23.105101
110.940213	3753.930048	23.110119
110.950252	3762.437006	23.115136
111.083913	3768.201622	23.120154
111.275240	3775.187385	23.125171
111.204290	3779.669333	23.130189
111.331705	3778.903296	23.135207
111.236816	3781.512874	23.140224
111.196458	3786.398224	23.145242
111.399389	3778.264068	23.150259
111.360273	3775.116614	23.155277
111.618331	3802.807714	23.160295
111.879241	3808.953254	23.165312
111.968752	3823.784939	23.170330
111.927911	3808.485366	23.175347
111.916651	3824.653142	23.180365
111.824011	3822.623409	23.185383
112.437828	3831.768877	23.190400
112.174825	3840.544405	23.195418
112.699011	3829.228855	23.200435
112.683076	3831.563892	23.205453
112.902778	3827.552306	23.210471
113.090972	3841.749169	23.215488
113.473565	3855.483169	23.220506
113.355906	3863.058681	23.225523
113.547435	3858.668472	23.230541
113.667749	3858.821603	23.235559
113.776656	3846.726592	23.240576
113.556029	3854.045545	23.245594
113.567000	3845.144282	23.250611
113.468237	3848.698488	23.255629
113.662785	3870.495918	23.260647
113.890315	3889.079303	23.265664
114.043659	3883.483706	23.270682
114.280021	3880.073610	23.275699
114.457584	3890.693666	23.280717
114.607083	3909.382346	23.285735
114.774319	3911.041547	23.290752
114.613278	3919.130621	23.295770
115.176856	3901.055180	23.300787
115.065467	3897.897983	23.305805
115.210699	3910.747907	23.310823
115.186298	3908.682895	23.315840
115.130375	3918.694346	23.320858
115.503624	3928.137049	23.325875
115.612231	3947.261033	23.330893
115.567038	3939.783889	23.335911
115.783153	3932.600991	23.340928
115.398229	3942.753025	23.345946
115.845485	3958.192540	23.350963
115.737297	3974.794445	23.355981
115.534010	3971.831247	23.360999
116.037806	3979.125219	23.366016
116.506985	3997.035364	23.371034
116.937550	3993.471555	23.376051
116.724993	4002.091240	23.381069
116.761169	3998.067177	23.386087
117.061098	3990.637245	23.391104
116.934728	4011.407526	23.396122
117.089287	4026.124416	23.401139
117.615825	4024.810921	23.406157
117.503588	4030.319060	23.411175
117.839889	4025.616221	23.416192
117.740963	4030.643152	23.421210
117.855193	4031.406143	23.426227
118.142552	4027.028137	23.431245
117.761916	4030.672958	23.436263
118.027750	4018.302621	23.441280
118.190523	4027.960672	23.446298
118.187788	4029.982900	23.451315
118.317625	4040.322751	23.456333
118.301158	4050.844847	23.461351
119.020325	4050.538262	23.466368
118.729614	4053.286099	23.471386
118.836261	4040.929325	23.476403
118.884726	4044.128911	23.481421
118.664657	4060.433295	23.486439
119.114492	4069.520888	23.491456
119.147080	4077.086713	23.496474
118.970270	4081.989199	23.501491
119.202575	4092.121585	23.506509
119.279357	4101.636060	23.511527
119.609662	4107.255387	23.516544
119.902991	4113.526476	23.521562
119.978627	4128.470029	23.526579
120.253498	4140.560791	23.531597
119.930021	4143.728450	23.536615
120.588588	4136.810030	23.541632
120.384855	4144.355358	23.546650
120.491203	4147.221624	23.551667
120.845999	4157.576036	23.556685
121.022799	4168.135841	23.561703
121.563687	4158.639336	23.566720
121.595965	4151.909666	23.571738
121.732503	4154.564223	23.576755
121.802779	4155.480552	23.581773
121.895875	4148.893016	23.586791
122.476203	4141.171281	23.591808
122.305802	4141.279515	23.596826
122.490426	4137.526750	23.601843
122.677507	4121.436869	23.606861
122.355638	4116.007425	23.611879
122.599782	4098.365791	23.616896
122.814776	4102.742456	23.621914
122.809280	4095.411519	23.626931
123.051670	4098.887788	23.631949
122.523351	4107.236129	23.636967
122.995096	4111.450710	23.641984
123.266674	4122.386350	23.647002
123.179375	4133.170750	23.652019
123.284553	4124.276323	23.657037
123.231183	4130.414684	23.662055
123.323914	4126.842564	23.667072
123.239214	4134.921156	23.672090
123.319378	4136.854659	23.677107
123.432529	4152.796061	23.682125
123.313856	4168.048337	23.687143
123.291011	4163.621418	23.692160
123.654207	4184.641143	23.697178
123.633407	4195.574683	23.702195
124.074640	4200.495090	23.707213
124.216368	4214.977424	23.712231
124.352504	4224.399126	23.717248
124.522098	4224.964495	23.722266
124.732640	4233.630921	23.727283
124.571529	4231.962910	23.732301
124.634216	4250.533703	23.737319
124.931188	4247.610259	23.742336
125.112103	4259.327477	23.747354
124.812677	4277.719250	23.752371
125.297840	4286.227849	23.757389
125.247118	4280.969090	23.762407
125.815035	4296.997048	23.767424
125.953140	4310.820022	23.772442
126.109729	4305.251283	23.777459
126.500237	4302.128829	23.782477
126.526453	4309.507772	23.787495
126.499335	4302.940908	23.792512
126.680977	4308.638299	23.797530
126.439720	4313.957069	23.802547
126.932867	4323.912715	23.807565
126.797341	4342.543550	23.812583
127.098231	4348.458737	23.817600
126.656626	4349.687196	23.822618
126.994574	4358.522188	23.827635
127.215903	4365.616733	23.832653
127.100400	4376.060449	23.837671
127.156169	4389.117797	23.842688
127.603156	4402.565128	23.847706
127.701804	4415.875272	23.852723
128.217679	4412.322938	23.857741
128.033232	4415.241130	23.862759
128.266371	4429.058502	23.867776
128.578978	4439.375787	23.872794
128.551801	4439.051316	23.877811
128.708505	4438.235735	23.882829
128.423393	4447.233848	23.887847
128.916903	4461.574584	23.892864
128.977646	4469.556219	23.897882
129.001984	4468.706673	23.902899
129.220140	4473.232418	23.907917
129.188283	4481.228825	23.912935
129.446193	4489.512594	23.917952
129.463796	4503.790007	23.922970
129.455432	4503.263500	23.927987
129.911711	4503.876000	23.933005
130.122966	4523.781295	23.938023
130.299872	4528.046943	23.943040
130.505237	4528.572792	23.948058
130.372252	4527.351829	23.953075
130.437639	4519.685258	23.958093
130.567669	4537.136426	23.963111
130.878660	4546.219707	23.968128
130.746177	4546.697941	23.973146
130.813803	4556.559533	23.978163
131.219784	4552.166395	23.983181
131.313080	4557.591609	23.988199
131.225284	4578.967021	23.993216
131.556483	4588.200514	23.998234
131.412455	4585.248982	24.003251
131.587555	4583.640608	24.008269
131.567526	4600.788509	24.013287
131.754227	4612.368199	24.018304
132.127861	4624.992735	24.023322
132.477801	4624.293448	24.028339
132.971861	4621.825479	24.033357
133.136689	4640.705388	24.038375
133.071687	4641.080821	24.043392
133.180768	4634.897248	24.048410
133.362790	4633.879369	24.053427
133.605287	4634.763548	24.058445
133.646823	4636.161235	24.063463
133.408900	4636.409257	24.068480
133.733664	4635.710837	24.073498
133.412802	4634.866759	24.078515
133.736250	4634.930082	24.083533
133.853944	4651.388167	24.088551
133.814132	4667.744724	24.093568
133.958294	4669.941868	24.098586
134.046567	4675.598433	24.103603
134.197921	4684.129021	24.108621
134.322368	4705.122262	24.113639
134.431542	4703.722639	24.118656
134.778439	4702.721737	24.123674
134.312997	4728.951799	24.128691
134.676792	4718.344803	24.133709
134.947451	4739.325794	24.138727
135.032652	4748.405079	24.143744
135.664091	4744.554959	24.148762
135.139312	4757.308694	24.153779
135.742969	4775.861553	24.158797
135.786507	4784.073463	24.163815
136.106266	4779.891472	24.168832
136.189215	4778.847685	24.173850
136.212450	4800.591991	24.178867
136.818241	4801.151559	24.183885
136.662886	4819.045856	24.188903
136.699649	4819.062845	24.193920
137.083732	4806.032609	24.198938
136.925786	4810.623146	24.203955
137.624879	4816.272847	24.208973
137.804258	4826.651769	24.213991
137.860929	4828.504144	24.219008
137.841290	4824.139453	24.224026
137.831358	4832.141994	24.229043
137.654700	4829.392295	24.234061
137.806956	4836.563380	24.239079
137.992745	4832.309115	24.244096
137.861584	4839.388501	24.249114
137.906625	4852.708374	24.254131
138.032860	4859.922955	24.259149
138.271189	4865.904185	24.264167
138.254746	4889.924637	24.269184
138.485339	4892.860140	24.274202
138.535997	4903.822933	24.279219
138.991514	4913.021862	24.284237
139.024282	4930.168807	24.289255
138.735544	4931.091290	24.294272
139.555130	4933.872313	24.299290
139.523321	4956.561827	24.304307
139.423948	4959.781251	24.309325
139.785963	4962.968020	24.314343
140.218782	4974.565399	24.319360
140.738323	4975.379466	24.324378
140.493764	4988.123335	24.329395
140.899782	4982.487825	24.334413
140.823151	4979.553790	24.339431
140.818676	4985.442398	24.344448
141.252668	4975.576137	24.349466
140.933721	4984.108720	24.354483
140.907845	5001.500329	24.359501
141.303768	5006.239422	24.364519
141.127413	5010.408124	24.369536
141.434274	5029.479876	24.374554
141.450166	5051.276860	24.379571
141.476414	5046.305299	24.384589
141.866435	5048.914096	24.389607
141.849782	5070.791824	24.394624
142.095380	5071.922570	24.399642
142.029925	5087.746343	24.404659
142.374095	5098.290359	24.409677
142.723730	5112.863945	24.414695
142.792922	5117.902203	24.419712
143.320736	5118.502541	24.424730
143.315149	5138.383449	24.429747
143.365423	5149.932604	24.434765
143.384468	5144.797730	24.439783
143.221151	5147.668639	24.444800
143.894171	5157.182354	24.449818
143.807951	5177.390077	24.454835
144.045070	5172.912753	24.459853
144.258043	5169.329078	24.464871
144.068355	5183.847898	24.469888
144.334817	5185.372629	24.474906
144.172460	5202.787022	24.479923
144.753588	5201.386058	24.484941
145.646059	5194.716236	24.489959
145.513992	5206.849944	24.494976
145.731782	5193.509945	24.499994
145.505259	5189.988471	24.505011
145.736118	5190.077577	24.510029
146.008188	5195.419452	24.515047
145.828985	5214.970178	24.520064
146.188589	5213.222177	24.525082
146.201734	5223.182590	24.530099
146.136400	5220.357636	24.535117
146.282256	5215.086869	24.540135
146.235432	5218.679538	24.545152
146.716220	5205.629600	24.550170
146.649422	5229.638178	24.555187
146.546505	5233.294866	24.560205
146.938725	5232.594321	24.565223
147.065624	5232.662239	24.570240
147.488241	5254.832103	24.575258
147.753247	5264.727212	24.580275
148.125223	5266.396411	24.585293
148.334756	5259.418475	24.590311
148.084461	5264.832646	24.595328
148.291217	5264.523570	24.600346
148.030879	5261.769822	24.605363
147.996961	5270.422340	24.610381
148.290391	5274.176341	24.615399
148.533846	5288.418503	24.620416
148.652223	5278.016241	24.625434
148.804432	5290.202249	24.630451
148.787131	5311.830253	24.635469
148.723450	5312.653935	24.640487
148.569278	5326.274278	24.645504
148.644914	5354.784917	24.650522
149.251422	5364.190574	24.655539
149.561279	5377.522198	24.660557
149.692508	5384.572597	24.665575
149.783236	5396.371974	24.670592
150.361016	5414.850307	24.675610
150.763617	5413.207148	24.680627
150.793113	5414.395979	24.685645
151.024082	5410.638653	24.690663
150.874519	5417.273588	24.695680
150.765384	5421.731438	24.700698
150.916542	5437.973430	24.705715
151.200323	5442.819449	24.710733
151.418698	5450.760749	24.715751
151.333175	5456.367435	24.720768
151.705299	5470.135303	24.725786
151.777656	5481.462479	24.730803
151.905897	5488.120028	24.735821
152.432259	5484.823043	24.740839
151.978121	5511.065271	24.745856
152.220278	5517.439534	24.750874
152.202466	5517.687877	24.755891
152.721108	5539.628076	24.760909
152.451048	5551.590525	24.765927
152.580320	5555.455741	24.770944
152.938258	5567.338533	24.775962
153.386993	5573.349446	24.780979
153.273936	5587.439461	24.785997
153.741762	5597.760351	24.791015
153.770129	5610.506872	24.796032
153.908349	5605.739923	24.801050
154.290449	5613.021079	24.806067
154.044595	5605.534957	24.811085
154.670647	5618.600028	24.816103
154.681719	5640.319973	24.821120
154.840421	5636.523760	24.826138
154.668501	5648.714536	24.831155
154.596621	5644.725349	24.836173
154.931663	5653.149324	24.841191
154.984000	5656.657055	24.846208
155.068317	5665.867649	24.851226
155.442711	5678.673927	24.856243
155.472416	5696.778954	24.861261
155.804339	5705.009125	24.866279
155.656286	5705.655097	24.871296
156.214844	5720.065372	24.876314
156.405785	5725.275611	24.881331
156.238349	5733.131449	24.886349
156.618744	5743.006123	24.891367
156.905275	5751.088564	24.896384
156.910466	5757.101034	24.901402
157.090508	5766.518297	24.906419
157.349087	5788.643522	24.911437
158.003376	5774.951746	24.916455
158.003500	5792.334632	24.921472
157.836688	5783.241823	24.926490
158.328220	5768.747534	24.931507
157.993208	5780.634765	24.936525
158.416205	5791.205263	24.941543
158.253451	5801.810150	24.946560
158.450997	5809.327749	24.951578
158.483292	5809.968574	24.956595
158.730002	5826.695358	24.961613
159.159075	5841.603181	24.966631
159.163156	5849.297984	24.971648
159.259226	5855.476175	24.976666
159.706900	5868.052212	24.981683
159.640575	5880.257814	24.986701
159.810197	5882.082085	24.991719
159.779996	5887.560524	24.996736
160.015186	5904.511890	25.001754
160.282559	5907.168724	25.006771
160.366537	5919.359049	25.011789
160.777711	5919.544511	25.016807
160.537886	5929.983965	25.021824
160.795023	5938.303295	25.026842
161.147379	5938.983577	25.031859
161.487567	5961.793922	25.036877
161.858128	5965.666410	25.041895
161.868181	5966.775774	25.046912
161.832229	5966.195391	25.051930
161.948622	5964.969952	25.056947
162.038292	5963.615807	25.061965
162.153891	5969.749234	25.066983
162.380707	5994.472268	25.072000
162.085646	5998.741208	25.077018
162.320136	5999.528404	25.082035
162.378429	6018.633198	25.087053
162.639323	6022.498008	25.092071
162.870159	6028.821584	25.097088
162.908446	6058.545671	25.102106
163.132970	6064.586239	25.107123
163.422963	6074.831963	25.112141
163.577973	6093.877374	25.117159
163.547998	6097.782284	25.122176
163.908316	6099.949116	25.127194
164.525135	6104.920072	25.132211
164.539412	6120.555208	25.137229
164.855638	6120.600816	25.142247
164.936394	6119.214247	25.147264
165.157421	6124.403308	25.152282
165.351810	6130.565153	25.157299
165.335064	6150.121894	25.162317
165.725345	6142.596236	25.167335
165.732460	6146.925618	25.172352
165.604713	6152.484223	25.177370
165.932378	6159.820750	25.182387
165.807769	6175.396261	25.187405
166.445877	6173.974330	25.192423
166.359001	6175.461873	25.197440
166.333520	6191.020023	25.202458
166.649431	6197.703047	25.207475
166.372578	6212.530241	25.212493
167.009113	6223.343170	25.217511
167.109666	6237.509110	25.222528
167.091391	6235.994336	25.227546
167.418441	6247.961282	25.232563
167.434965	6266.346844	25.237581
167.494607	6272.334319	25.242599
167.683375	6289.479999	25.247616
167.951985	6306.288022	25.252634
168.084396	6300.497369	25.257651
168.190853	6324.184261	25.262669
168.756373	6330.589938	25.267687
168.927522	6336.272480	25.272704
168.946999	6363.725543	25.277722
169.405055	6361.854714	25.282739
169.246524	6372.197330	25.287757
169.148287	6381.046434	25.292775
169.689931	6391.629134	25.297792
169.670717	6402.615193	25.302810
169.624655	6408.733662	25.307827
169.660493	6433.554753	25.312845
170.297081	6440.620291	25.317863
170.474399	6460.347923	25.322880
170.181878	6476.744405	25.327898
170.751418	6470.918615	25.332915
170.985843	6490.291775	25.337933
171.246477	6506.886499	25.342951
171.634439	6507.823928	25.347968
171.636359	6506.485298	25.352986
171.500203	6495.232099	25.358003
171.804886	6518.947496	25.363021
172.035231	6519.884876	25.368039
172.250353	6531.579565	25.373056
172.127316	6534.916401	25.378074
172.562873	6547.454823	25.383091
173.024463	6571.023334	25.388109
173.017039	6559.220826	25.393127
173.388179	6557.341013	25.398144
173.417771	6567.007800	25.403162
173.748623	6581.856498	25.408179
173.609487	6584.963802	25.413197
173.930297	6586.712916	25.418215
174.146352	6580.995369	25.423232
174.101927	6593.247633	25.428250
174.546969	6600.042438	25.433267
174.468858	6615.323810	25.438285
174.659168	6616.606696	25.443303
174.537310	6609.536976	25.448320
174.818940	6631.260872	25.453338
175.049206	6636.020614	25.458355
175.267984	6632.333381	25.463373
174.977922	6660.992171	25.468391
175.424784	6661.340338	25.473408
175.483443	6681.133603	25.478426
176.089472	6690.225466	25.483443
175.828891	6696.371958	25.488461
175.852851	6720.729628	25.493479
176.025296	6739.234905	25.498496
176.409860	6734.264665	25.503514
177.061518	6745.630277	25.508531
177.162183	6764.563257	25.513549
177.310394	6758.237231	25.518567
178.045377	6768.927861	25.523584
177.678497	6792.093765	25.528602
177.960999	6796.502177	25.533619
178.227061	6787.659975	25.538637
177.890524	6793.163194	25.543655
178.347978	6800.868827	25.548672
178.215647	6815.816781	25.553690
178.318776	6815.014338	25.558707
178.674118	6837.094231	25.563725
178.744790	6839.919503	25.568743
179.064209	6843.796445	25.573760
179.362018	6873.030722	25.578778
179.727269	6873.945832	25.583795
179.908547	6880.308361	25.588813
179.718347	6878.292970	25.593831
180.458124	6895.283052	25.598848
180.640479	6904.939081	25.603866
180.536753	6898.702730	25.608883
180.574167	6903.907963	25.613901
180.604722	6914.581964	25.618919
180.878272	6915.329938	25.623936
180.989752	6938.809287	25.628954
181.275855	6940.235870	25.633971
181.191325	6943.078823	25.638989
181.198078	6968.886623	25.644007
181.573747	6976.185219	25.649024
181.721699	6987.494412	25.654042
182.207326	6991.930300	25.659059
182.229702	7003.915745	25.664077
182.264853	7011.319789	25.669095
182.814376	7023.590235	25.674112
182.968568	7032.833815	25.679130
182.845374	7036.393461	25.684148
183.480531	7049.418228	25.689165
183.426373	7065.333580	25.694183
183.606435	7062.466003	25.699200
183.739681	7067.745714	25.704218
184.362525	7076.041219	25.709236
184.726242	7095.306431	25.714253
184.488481	7111.173206	25.719271
184.747278	7088.733838	25.724288
184.773799	7094.440516	25.729306
184.537100	7109.927864	25.734324
185.030810	7115.674161	25.739341
184.899997	7124.619386	25.744359
185.141108	7133.904251	25.749376
185.413979	7155.393473	25.754394
185.642267	7159.483311	25.759412
185.972162	7179.523950	25.764429
186.069009	7194.403486	25.769447
186.599901	7183.219675	25.774464
186.372417	7214.288307	25.779482
186.428709	7220.440363	25.784500
186.542683	7221.683541	25.789517
186.523585	7247.264611	25.794535
186.812352	7260.677623	25.799552
186.824663	7280.529433	25.804570
187.103444	7296.762559	25.809588
187.602247	7307.119055	25.814605
187.735494	7318.559102	25.819623
188.126392	7344.672197	25.824640
188.334390	7354.889390	25.829658
188.338290	7365.323251	25.834676
188.818571	7372.971253	25.839693
188.949349	7391.848299	25.844711
189.167358	7399.210795	25.849728
189.478671	7416.640392	25.854746
189.770264	7415.932197	25.859764
189.734875	7413.256272	25.864781
189.746615	7432.743274	25.869799
190.330088	7441.638552	25.874816
190.569983	7446.624423	25.879834
190.647523	7442.747057	25.884852
190.673853	7445.052320	25.889869
190.686655	7460.467206	25.894887
190.941513	7468.637473	25.899904
191.151559	7474.528278	25.904922
191.284558	7478.962303	25.909940
192.160260	7500.641550	25.914957
192.059878	7505.329175	25.919975
192.420692	7503.172348	25.924992
192.250331	7506.773460	25.930010
192.460333	7499.190884	25.935028
193.018192	7503.821571	25.940045
193.328369	7514.368017	25.945063
193.369196	7520.563579	25.950080
193.482458	7524.125775	25.955098
193.637278	7512.738862	25.960116
194.076917	7522.896425	25.965133
193.769626	7522.194783	25.970151
194.183918	7517.814415	25.975168
194.368955	7519.744236	25.980186
194.192692	7548.290590	25.985204
194.813583	7544.846693	25.990221
194.705179	7551.836396	25.995239
194.941917	7554.230096	26.000256
195.152188	7565.946047	26.005274
195.172523	7572.410857	26.010292
195.437107	7564.626765	26.015309
195.466474	7590.650785	26.020327
195.951915	7591.750581	26.025344
196.155043	7595.822520	26.030362
195.999456	7605.351901	26.035380
196.214153	7623.906625	26.040397
196.354231	7639.785330	26.045415
196.371108	7656.415479	26.050432
196.460776	7656.329615	26.055450
196.555435	7685.619910	26.060468
197.077364	7696.696914	26.065485
197.289764	7722.430743	26.070503
197.346035	7737.240177	26.075520
197.509785	7740.648019	26.080538
197.747049	7764.416284	26.085556
197.868738	7774.915850	26.090573
198.156316	7802.482266	26.095591
198.373944	7800.596090	26.100608
198.940544	7824.034969	26.105626
199.633146	7815.398785	26.110644
200.148000	7801.507860	26.115661
200.088358	7810.949683	26.120679
200.373032	7817.067152	26.125696
200.759969	7803.682905	26.130714
200.469660	7819.092189	26.135732
200.532782	7821.061943	26.140749
200.442683	7834.786099	26.145767
200.537125	7838.552025	26.150784
200.842270	7848.131652	26.155802
200.903689	7860.070643	26.160820
201.167981	7873.678536	26.165837
201.345691	7890.417076	26.170855
201.411185	7903.569609	26.175872
201.935210	7895.495333	26.180890
201.478135	7913.624004	26.185908
202.003118	7937.342745	26.190925
202.204297	7946.845370	26.195943
202.372888	7954.009070	26.200960
202.540600	7971.123064	26.205978
202.310348	7992.803078	26.210996
202.874770	8003.561145	26.216013
203.240580	8019.736728	26.221031
203.049143	8034.318797	26.226048
203.401909	8046.863036	26.231066
203.588720	8073.213356	26.236084
203.725862	8086.165774	26.241101
204.145312	8093.718012	26.246119
204.569545	8097.720613	26.251136
204.972761	8116.330881	26.256154
205.189427	8135.620886	26.261172
205.230373	8137.949500	26.266189
205.488854	8161.607606	26.271207
205.638117	8168.510487	26.276224
206.276350	8162.267853	26.281242
206.170222	8191.653706	26.286260
206.277031	8192.697451	26.291277
206.376837	8205.581957	26.296295
206.701255	8209.376234	26.301312
207.342062	8220.173431	26.306330
206.878285	8223.802209	26.311348
207.586920	8231.570848	26.316365
207.355807	8253.311967	26.321383
207.548121	8261.482412	26.326400
208.064031	8276.822661	26.331418
208.101416	8280.853537	26.336436
208.102505	8299.243674	26.341453
208.194108	8323.327991	26.346471
208.364908	8320.999502	26.351488
208.588324	8346.078734	26.356506
208.699390	8370.227305	26.361524
209.352010	8380.381801	26.366541
209.477672	8399.655571	26.371559
209.595952	8407.948852	26.376576
210.125441	8421.199026	26.381594
209.844785	8421.950445	26.386612
210.326084	8447.879126	26.391629
210.423732	8454.187201	26.396647
210.939714	8466.972538	26.401664
211.280214	8483.358438	26.406682
211.220020	8493.629791	26.411700
211.610050	8499.002459	26.416717
211.673963	8512.096367	26.421735
211.647183	8533.308383	26.426752
212.144546	8536.139928	26.431770
212.607476	8548.046154	26.436788
212.695313	8549.520243	26.441805
212.957663	8543.942512	26.446823
212.990222	8558.981991	26.451840
213.596495	8574.126758	26.456858
213.265292	8599.734715	26.461876
213.423208	8587.384487	26.466893
213.455721	8596.337604	26.471911
213.610457	8603.582123	26.476928
214.194701	8609.010040	26.481946
213.937454	8632.156587	26.486964
214.003569	8643.148791	26.491981
214.351139	8668.537706	26.496999
214.383379	8680.365539	26.502016
215.067708	8691.776631	26.507034
215.331167	8711.618242	26.512052
215.428903	8711.642437	26.517069
216.036600	8725.878235	26.522087
215.861535	8747.643792	26.527104
215.907568	8760.741161	26.532122
216.181037	8777.732592	26.537140
216.356139	8793.531396	26.542157
216.744571	8805.043255	26.547175
217.058760	8830.533378	26.552192
217.181092	8843.781551	26.557210
217.121019	8853.864661	26.562228
217.375837	8870.795823	26.567245
217.936955	8889.122198	26.572263
218.078405	8910.348457	26.577280
218.599942	8904.912632	26.582298
219.035557	8926.222652	26.587316
219.272286	8944.706255	26.592333
219.093652	8943.551216	26.597351
219.569655	8956.622710	26.602368
219.926315	8967.030179	26.607386
220.143511	8969.547628	26.612404
219.583465	8972.425450	26.617421
220.349541	8985.628972	26.622439
220.673444	8997.645463	26.627456
220.853507	9001.009680	26.632474
220.933206	9036.990443	26.637492
221.184698	9041.731053	26.642509
221.356161	9045.813948	26.647527
221.388568	9067.244709	26.652544
221.537146	9070.288560	26.657562
221.512896	9099.980671	26.662580
221.671804	9112.002308	26.667597
222.081312	9131.014183	26.672615
222.104990	9139.810069	26.677632
222.395597	9164.106394	26.682650
222.632631	9182.136961	26.687668
223.060573	9199.084179	26.692685
223.576090	9213.884036	26.697703
223.893013	9231.561572	26.702720
224.645651	9238.071299	26.707738
224.681753	9244.053491	26.712756
224.595039	9239.078866	26.717773
224.709212	9241.302725	26.722791
224.613765	9256.949588	26.727808
224.711360	9264.586389	26.732826
225.054891	9282.594985	26.737844
225.451759	9293.680529	26.742861
225.337945	9305.136299	26.747879
225.612217	9328.331004	26.752896
226.128889	9325.384948	26.757914
226.146527	9349.492541	26.762932
226.323256	9364.078593	26.767949
226.588478	9373.895359	26.772967
226.618326	9405.363876	26.777984
227.123766	9409.589980	26.783002
227.069005	9432.554777	26.788020
227.169408	9443.330016	26.793037
227.461824	9462.439673	26.798055
227.642088	9480.293531	26.803072
228.081094	9501.439354	26.808090
228.440814	9515.868109	26.813108
228.283598	9545.049125	26.818125
229.031491	9556.324049	26.823143
229.239720	9571.220856	26.828160
229.216402	9582.257909	26.833178
229.308617	9604.209926	26.838196
229.722806	9618.629310	26.843213
230.416241	9627.451718	26.848231
230.391300	9642.179970	26.853248
230.683071	9653.657133	26.858266
231.174125	9658.767405	26.863284
231.219456	9666.779865	26.868301
231.674964	9686.341896	26.873319
231.733721	9701.106837	26.878336
231.756022	9694.750855	26.883354
232.181040	9706.321717	26.888372
232.257855	9720.821736	26.893389
232.819997	9724.148822	26.898407
232.937260	9743.869908	26.903424
233.046904	9741.881874	26.908442
233.104338	9768.504877	26.913460
233.197115	9780.990499	26.918477
233.548384	9786.076665	26.923495
233.630928	9811.603415	26.928512
234.206066	9829.732753	26.933530
234.470708	9841.685000	26.938548
234.703968	9855.616406	26.943565
235.202549	9869.052623	26.948583
235.271296	9883.462401	26.953600
235.779523	9895.834676	26.958618
235.363119	9890.344184	26.963636
235.806917	9916.586347	26.968653
235.928866	9923.053287	26.973671
236.005712	9947.363313	26.978688
236.391293	9957.127828	26.983706
236.838697	9963.130920	26.988724
237.042395	9983.681013	26.993741
237.393365	9981.846507	26.998759
236.968848	9994.799207	27.003776
237.452255	10010.300673	27.008794
237.811681	10015.362795	27.013812
237.788902	10034.202724	27.018829
238.576968	10043.811062	27.023847
238.460381	10047.135840	27.028864
238.749819	10075.723335	27.033882
239.045337	10082.784404	27.038900
239.262616	10104.930885	27.043917
239.528873	10109.526249	27.048935
239.796634	10122.926297	27.053952
239.718025	10133.985160	27.058970
240.149773	10141.556945	27.063988
240.101214	10164.972032	27.069005
240.390281	10178.116106	27.074023
240.929090	10192.216726	27.079040
241.162687	10209.351107	27.084058
241.258052	10210.533759	27.089076
241.444218	10234.256639	27.094093
241.596065	10247.162935	27.099111
241.998666	10268.114564	27.104128
242.431155	10274.576622	27.109146
242.983126	10294.612803	27.114164
242.580923	10302.057888	27.119181
243.040048	10317.432112	27.124199
243.356703	10333.126944	27.129216
243.109770	10341.796675	27.134234
244.045328	10374.319889	27.139252
243.917128	10376.756481	27.144269
244.748229	10382.802468	27.149287
244.696018	10405.590082	27.154304
244.851296	10412.071596	27.159322
245.121659	10425.242872	27.164340
245.190344	10440.988361	27.169357
245.730452	10458.077514	27.174375
245.909535	10466.675868	27.179392
246.110880	10474.801224	27.184410
246.390278	10486.603280	27.189428
246.418528	10506.957361	27.194445
246.893839	10507.680850	27.199463
247.288006	10529.121745	27.204480
247.518208	10532.941871	27.209498
247.862861	10539.490058	27.214516
248.315405	10563.632584	27.219533
248.533352	10558.924948	27.224551
248.712240	10561.665993	27.229568
248.364813	10578.471565	27.234586
248.837318	10587.153864	27.239604
249.155957	10604.791426	27.244621
249.165406	10616.679900	27.249639
249.384849	10626.953388	27.254656
249.553769	10649.725799	27.259674
249.827866	10668.340150	27.264692
250.100883	10668.883789	27.269709
250.383010	10685.187355	27.274727
250.424309	10699.320926	27.279744
250.092825	10719.061298	27.284762
250.557773	10733.044736	27.289780
250.451193	10767.996444	27.294797
250.787686	10789.383940	27.299815
251.083753	10806.740431	27.304832
251.678646	10819.692686	27.309850
252.399653	10841.114591	27.314868
252.551991	10853.297257	27.319885
253.035249	10871.577873	27.324903
253.630697	10880.007783	27.329920
253.777276	10878.746446	27.334938
253.921862	10892.822416	27.339956
253.800268	10913.566901	27.344973
254.270310	10916.156533	27.349991
254.313983	10947.635117	27.355008
254.158875	10957.568715	27.360026
254.579375	10972.401594	27.365044
254.780391	10990.900492	27.370061
254.907145	11012.287499	27.375079
255.432816	11037.764187	27.380096
255.430713	11049.911026	27.385114
256.098632	11061.880244	27.390132
256.494886	11091.287696	27.395149
256.801314	11102.820300	27.400167
257.215971	11111.738401	27.405184
257.060948	11127.698136	27.410202
257.570749	11140.278184	27.415220
257.809064	11147.848257	27.420237
258.056739	11169.568025	27.425255
258.437152	11179.873687	27.430272
258.841008	11192.846484	27.435290
259.036437	11205.038700	27.440308
258.957525	11219.003025	27.445325
259.293955	11230.664351	27.450343
259.573782	11238.166069	27.455360
259.475799	11267.475948	27.460378
260.244887	11274.011112	27.465396
260.002765	11301.211500	27.470413
260.405037	11319.055764	27.475431
260.544324	11333.781526	27.480448
260.469474	11353.908995	27.485466
260.978901	11385.554109	27.490484
261.249591	11400.746184	27.495501
261.796627	11417.296382	27.500519
261.935621	11432.468553	27.505536
262.015963	11467.523127	27.510554
262.252317	11486.700370	27.515572
262.038923	11512.251781	27.520589
262.681115	11537.383319	27.525607
263.326034	11559.620008	27.530624
263.342657	11581.583408	27.535642
263.030983	11608.217522	27.540660
263.554886	11626.568529	27.545677
263.913503	11656.371698	27.550695
264.293346	11662.639684	27.555712
264.585334	11687.456185	27.560730
264.996770	11693.902932	27.565748
265.069282	11706.331591	27.570765
265.316715	11744.456347	27.575783
266.167108	11746.116959	27.580800
266.150557	11770.301555	27.585818
266.929901	11767.516442	27.590836
267.008118	11784.854275	27.595853
267.100794	11799.996220	27.600871
267.307258	11804.111677	27.605888
267.565062	11825.297522	27.610906
267.925055	11830.857611	27.615924
268.463117	11854.890188	27.620941
268.524727	11876.448578	27.625959
269.017189	11879.644016	27.630976
268.950200	11891.549609	27.635994
269.083241	11912.058100	27.641012
269.237704	11934.603149	27.646029
269.772622	11947.390811	27.651047
269.935420	11959.772426	27.656064
269.950295	11985.618827	27.661082
270.473810	12000.905605	27.666100
270.803681	12013.928091	27.671117
270.680407	12045.820454	27.676135
271.089675	12064.205417	27.681152
271.294270	12085.945566	27.686170
271.689053	12105.335258	27.691188
271.694389	12123.460782	27.696205
271.808589	12147.881340	27.701223
272.399555	12169.393948	27.706240
272.518050	12205.787928	27.711258
273.125748	12230.289153	27.716276
273.090603	12246.918099	27.721293
273.482658	12269.219751	27.726311
274.037306	12282.939638	27.731328
274.432288	12292.186062	27.736346
274.960967	12309.532589	27.741364
275.026236	12324.322274	27.746381
275.425153	12330.074893	27.751399
275.818125	12347.300627	27.756416
276.012226	12355.385451	27.761434
276.109539	12367.207179	27.766452
276.675482	12378.615175	27.771469
276.548088	12397.031570	27.776487
277.026513	12405.524679	27.781504
277.076937	12423.095738	27.786522
277.341331	12435.559545	27.791540
277.523717	12457.700671	27.796557
277.433418	12481.511676	27.801575
277.954856	12490.135133	27.806592
278.227212	12518.875393	27.811610
278.335288	12540.264778	27.816628
279.128870	12560.370152	27.821645
278.910853	12574.408465	27.826663
279.428071	12593.131858	27.831680
279.532126	12623.078646	27.836698
279.863110	12627.059758	27.841716
280.277436	12639.055896	27.846733
280.106111	12653.802733	27.851751
280.997814	12663.247089	27.856768
281.080635	12694.568188	27.861786
281.164417	12707.185175	27.866804
281.731683	12719.087339	27.871821
281.797037	12757.162387	27.876839
281.849663	12764.007021	27.881856
282.121656	12793.310462	27.886874
282.849787	12815.287790	27.891892
283.055308	12836.886591	27.896909
282.987289	12839.256127	27.901927
283.943602	12842.008875	27.906944
284.343925	12866.617781	27.911962
284.768065	12877.319470	27.916980
285.541081	12868.275252	27.921997
285.146594	12886.009457	27.927015
285.623062	12904.909951	27.932032
285.938589	12915.083096	27.937050
285.820981	12916.194626	27.942068
286.179528	12935.113754	27.947085
286.063909	12957.853416	27.952103
286.790319	12963.990063	27.957120
287.093585	12985.353392	27.962138
287.194040	13003.517247	27.967156
287.592895	13011.885040	27.972173
287.654752	13033.086288	27.977191
287.797487	13051.258614	27.982208
288.121299	13073.530901	27.987226
288.265356	13094.630283	27.992244
288.585862	13110.822606	27.997261
288.635760	13153.841374	28.002279
288.968826	13167.023939	28.007296
289.614216	13191.212148	28.012314
289.611495	13220.316274	28.017332
290.279441	13232.513234	28.022349
290.918104	13245.958976	28.027367
291.334618	13250.997553	28.032384
291.390790	13275.888182	28.037402
292.070689	13286.006160	28.042420
292.290214	13293.802874	28.047437
292.693132	13319.449578	28.052455
292.818863	13311.645224	28.057472
293.112346	13318.281005	28.062490
293.307626	13340.637068	28.067508
293.709616	13351.677760	28.072525
293.430514	13362.122890	28.077543
293.684050	13376.304828	28.082560
293.963385	13399.450564	28.087578
293.928988	13412.476913	28.092596
294.226786	13437.222240	28.097613
294.397766	13459.434632	28.102631
294.586255	13478.529135	28.107648
294.867915	13515.407473	28.112666
294.708237	13539.587283	28.117684
295.210917	13568.114029	28.122701
295.567235	13595.378202	28.127719
295.527621	13624.933636	28.132736
295.914257	13660.480119	28.137754
296.179330	13694.154362	28.142772
296.732718	13719.790452	28.147789
296.925821	13762.705749	28.152807
297.346619	13788.391820	28.157824
297.490442	13818.489496	28.162842
298.824186	13843.464562	28.167860
299.405659	13854.905836	28.172877
299.630276	13874.723523	28.177895
300.045148	13878.596644	28.182912
300.225935	13895.821249	28.187930
300.074990	13920.314849	28.192948
300.676963	13926.580753	28.197965
300.663750	13942.010432	28.202983
300.991096	13958.977265	28.208000
301.433935	13973.469854	28.213018
301.397983	14006.101115	28.218036
301.455318	14021.843465	28.223053
301.973747	14052.425952	28.228071
302.034890	14071.025579	28.233088
302.392606	14094.969514	28.238106
302.879938	14132.010213	28.243124
303.554144	14136.059732	28.248141
304.580634	14153.474174	28.253159
304.901967	14161.084949	28.258176
305.377839	14168.676436	28.263194
305.499945	14176.241257	28.268212
305.644555	14191.605297	28.273229
305.625108	14202.924253	28.278247
305.937669	14220.132749	28.283264
306.131465	14239.838823	28.288282
306.577202	14253.665335	28.293300
306.841331	14262.926243	28.298317
306.800700	14290.322916	28.303335
307.195088	14309.247585	28.308352
307.469377	14331.460427	28.313370
307.629673	14351.404703	28.318388
307.906297	14377.475385	28.323405
308.359542	14404.580315	28.328423
308.434340	14416.051397	28.333440
308.484948	14454.314279	28.338458
308.638201	14475.073924	28.343476
308.935146	14495.003694	28.348493
309.169694	14528.144504	28.353511
309.688056	14561.340624	28.358528
309.964378	14581.714641	28.363546
310.023722	14610.439258	28.368564
310.509180	14638.041621	28.373581
311.212281	14662.451957	28.378599
311.938439	14680.276997	28.383616
312.223287	14704.991606	28.388634
312.385743	14715.511543	28.393652
312.527417	14734.105340	28.398669
313.162100	14759.909811	28.403687
313.062599	14775.450123	28.408704
313.599982	14783.547363	28.413722
313.639639	14812.529576	28.418740
314.218898	14837.286633	28.423757
314.282768	14859.158654	28.428775
314.429220	14875.445438	28.433792
314.841305	14904.564594	28.438810
314.815424	14934.257932	28.443828
315.487785	14952.287789	28.448845
315.786935	14982.456777	28.453863
315.927721	15007.331617	28.458880
316.700746	15028.129827	28.463898
317.103332	15056.863753	28.468916
317.741483	15071.286602	28.473933
317.850055	15091.980890	28.478951
318.012457	15100.129497	28.483968
318.269790	15124.653338	28.488986
318.311662	15161.373695	28.494004
319.201057	15167.319854	28.499021
319.457517	15195.636267	28.504039
319.826639	15207.303216	28.509056
320.078886	15218.588281	28.514074
320.018942	15244.434007	28.519092
320.386886	15267.747845	28.524109
320.891946	15296.522180	28.529127
320.788087	15312.494755	28.534144
321.038361	15337.864009	28.539162
321.530450	15373.970107	28.544180
321.907183	15386.439584	28.549197
322.490932	15422.937420	28.554215
322.858279	15445.935929	28.559232
323.224520	15453.356882	28.564250
322.970618	15488.381444	28.569268
323.473141	15512.388265	28.574285
323.961777	15542.647920	28.579303
324.183833	15565.181650	28.584320
324.524882	15584.896492	28.589338
325.310219	15606.838626	28.594356
325.656358	15621.310401	28.599373
325.794115	15655.721240	28.604391
325.847696	15671.009254	28.609408
326.449109	15689.398481	28.614426
326.549308	15724.023891	28.619444
326.934737	15740.595902	28.624461
327.462686	15760.611845	28.629479
327.522450	15778.856429	28.634496
328.087487	15795.678577	28.639514
328.260174	15817.842646	28.644532
328.802673	15829.378222	28.649549
328.819132	15845.451547	28.654567
329.144991	15867.249001	28.659584
329.675665	15888.078738	28.664602
329.833825	15915.002686	28.669620
330.050456	15921.121509	28.674637
330.330997	15951.193508	28.679655
330.600140	15976.350895	28.684672
331.363044	15995.362702	28.689690
331.314514	16017.465276	28.694708
332.026112	16035.337620	28.699725
332.098263	16048.376286	28.704743
332.297050	16074.142017	28.709760
333.010026	16086.238737	28.714778
332.957385	16128.126710	28.719796
333.439276	16144.013196	28.724813
333.897445	16150.239074	28.729831
334.302974	16173.366627	28.734848
334.635704	16186.006445	28.739866
334.775346	16212.649252	28.744884
335.186521	16238.318426	28.749901
335.484953	16263.486771	28.754919
335.406509	16286.541045	28.759936
335.953434	16304.973942	28.764954
335.956153	16346.797000	28.769972
336.331828	16375.725455	28.774989
336.818612	16408.868897	28.780007
336.658186	16451.367775	28.785024
337.206774	16475.918509	28.790042
337.601301	16496.009817	28.795060
337.863614	16524.144686	28.800077
338.614164	16547.150108	28.805095
338.809395	16591.878505	28.810112
339.043413	16618.514648	28.815130
339.697665	16644.455381	28.820148
339.948248	16668.182924	28.825165
340.535361	16708.339949	28.830183
340.737219	16735.637270	28.835200
341.267376	16737.603049	28.840218
341.480420	16773.837895	28.845236
341.626279	16794.771715	28.850253
342.141377	16815.860879	28.855271
342.025878	16855.610214	28.860288
343.026841	16881.353192	28.865306
343.211926	16905.104528	28.870324
343.592757	16916.393280	28.875341
344.781788	16943.793679	28.880359
345.064854	16950.985520	28.885376
345.499006	16980.104989	28.890394
345.678162	16991.889882	28.895412
345.883493	16998.529209	28.900429
346.224239	17008.314868	28.905447
346.155230	17027.543197	28.910464
346.345723	17052.967809	28.915482
346.803757	17077.958711	28.920500
347.095300	17091.419371	28.925517
347.533594	17113.657731	28.930535
347.624520	17135.861325	28.935552
348.101748	17152.117095	28.940570
348.191348	17175.096112	28.945588
348.420909	17204.200183	28.950605
348.857792	17226.117292	28.955623
348.956630	17252.976256	28.960640
349.510865	17270.900510	28.965658
349.749415	17290.701384	28.970676
349.882003	17323.744971	28.975693
350.636651	17348.043796	28.980711
350.718741	17383.637971	28.985728
351.190542	17407.517807	28.990746
351.393044	17443.111434	28.995764
351.817060	17472.213367	29.000781
352.114579	17502.524450	29.005799
352.065084	17543.339796	29.010816
352.462522	17575.733859	29.015834
353.440824	17603.268617	29.020852
353.794033	17641.661448	29.025869
353.749902	17667.569131	29.030887
353.877527	17705.674058	29.035904
354.332825	17731.154236	29.040922
354.851164	17763.437301	29.045940
355.388898	17800.239725	29.050957
356.428287	17824.010860	29.055975
356.427544	17847.663922	29.060992
356.952607	17864.226203	29.066010
357.374115	17885.446309	29.071028
357.584358	17923.503566	29.076045
358.304772	17938.104098	29.081063
358.373569	17967.344272	29.086080
358.575295	17989.338911	29.091098
359.013785	18007.643487	29.096116
358.754253	18046.170391	29.101133
359.541375	18068.809658	29.106151
359.759810	18106.173140	29.111168
360.326154	18131.710298	29.116186
360.443309	18171.514113	29.121204
360.557163	18202.141659	29.126221
360.885113	18228.909107	29.131239
361.190190	18282.322053	29.136256
361.517630	18304.317971	29.141274
362.008147	18341.200463	29.146292
362.209048	18376.167334	29.151309
362.495186	18410.817149	29.156327
363.095365	18447.981640	29.161344
363.182370	18479.227413	29.166362
363.793931	18518.261970	29.171380
364.039774	18543.698510	29.176397
365.167545	18563.113635	29.181415
365.566937	18590.761692	29.186432
366.110253	18617.943541	29.191450
366.838611	18637.222397	29.196468
366.736801	18660.519553	29.201485
367.560045	18665.488626	29.206503
367.508286	18684.456004	29.211520
367.439540	18718.681142	29.216538
368.000080	18721.627432	29.221556
368.672307	18745.217537	29.226573
369.315292	18768.734380	29.231591
368.859294	18786.209918	29.236608
369.173919	18817.173235	29.241626
369.959292	18840.093451	29.246644
369.998359	18871.856338	29.251661
370.523729	18889.887860	29.256679
371.002866	18931.121059	29.261696
370.945224	18956.535761	29.266714
371.438475	18980.085446	29.271732
371.594596	19012.032734	29.276749
371.980356	19032.010021	29.281767
372.218198	19076.375959	29.286784
372.397037	19107.192185	29.291802
373.167068	19129.963295	29.296820
373.095122	19173.350055	29.301837
373.518534	19205.329169	29.306855
374.170457	19241.850254	29.311872
374.414926	19279.880563	29.316890
375.071228	19303.607134	29.321908
375.242786	19341.764576	29.326925
375.951392	19370.090793	29.331943
376.140774	19408.366827	29.336960
376.203612	19439.257314	29.341978
377.040458	19479.808134	29.346996
377.289781	19516.041616	29.352013
377.509867	19546.022920	29.357031
377.980500	19581.072750	29.362048
378.094049	19617.122568	29.367066
378.794482	19646.142787	29.372084
378.873023	19689.616064	29.377101
379.590703	19718.403329	29.382119
379.985713	19758.309842	29.387136
380.755409	19784.741039	29.392154
381.474445	19804.708343	29.397172
381.290855	19835.998368	29.402189
381.733783	19864.344192	29.407207
382.190482	19903.267506	29.412224
382.326319	19927.748120	29.417242
382.968630	19965.337915	29.422260
383.238521	19983.990226	29.427277
383.616438	20009.740436	29.432295
383.910691	20048.201349	29.437312
384.422507	20077.608770	29.442330
384.603825	20111.479740	29.447348
385.017260	20148.770573	29.452365
385.108640	20179.579613	29.457383
385.759167	20198.578674	29.462400
386.063602	20237.650326	29.467418
386.732854	20267.741783	29.472436
386.589119	20299.055123	29.477453
387.123944	20318.894147	29.482471
387.957764	20357.359622	29.487488
388.055347	20383.089748	29.492506
388.651331	20403.368809	29.497524
388.467572	20432.435690	29.502541
389.004298	20466.052339	29.507559
389.636679	20489.764052	29.512576
389.938942	20527.207772	29.517594
390.743001	20550.989088	29.522612
390.727960	20579.666307	29.527629
391.179186	20617.685819	29.532647
391.509840	20639.863680	29.537664
391.683887	20685.383899	29.542682
392.276868	20699.759661	29.547700
392.480455	20743.682941	29.552717
392.899936	20784.802160	29.557735
393.336964	20811.668878	29.562752
393.685689	20845.317870	29.567770
394.373912	20870.774337	29.572788
394.480491	20913.094353	29.577805
394.985180	20932.402636	29.582823
395.740922	20966.549347	29.587840
395.900336	21008.973034	29.592858
396.177233	21045.413961	29.597876
396.304704	21083.828773	29.602893
396.516781	21125.382007	29.607911
397.152342	21160.361836	29.612928
397.571884	21192.165271	29.617946
397.941263	21224.751725	29.622964
398.615584	21270.074215	29.627981
399.007101	21295.018686	29.632999
399.421277	21337.427867	29.638016
399.574060	21372.642605	29.643034
400.224906	21401.751557	29.648052
400.430102	21429.694290	29.653069
400.769313	21473.475134	29.658087
401.445516	21507.952300	29.663104
401.624407	21549.241800	29.668122
402.082868	21577.591788	29.673140
402.563948	21615.453801	29.678157
402.514477	21649.436523	29.683175
402.839358	21703.221044	29.688192
403.048093	21741.840307	29.693210
403.795752	21780.293464	29.698228
404.349129	21833.179609	29.703245
404.517664	21876.599693	29.708263
405.038006	21915.416250	29.713280
405.373285	21962.090348	29.718298
406.123184	21999.637155	29.723316
406.413986	22037.245385	29.728333
406.980628	22066.350079	29.733351
407.499074	22103.121988	29.738368
407.781267	22137.130099	29.743386
408.151366	22160.657718	29.748404
409.190315	22197.465846	29.753421
409.213319	22215.979778	29.758439
409.756274	22250.778306	29.763456
409.562272	22287.923283	29.768474
410.251658	22316.066105	29.773492
410.697635	22345.498499	29.778509
411.137590	22377.274293	29.783527
411.847390	22409.030785	29.788544
412.034356	22444.893041	29.793562
412.421474	22472.868494	29.798580
412.557689	22503.612312	29.803597
412.914692	22535.903360	29.808615
413.360162	22568.585220	29.813632
413.651672	22606.996499	29.818650
414.409745	22637.783274	29.823668
414.617335	22680.019463	29.828685
415.901338	22704.512064	29.833703
416.915350	22710.131801	29.838720
416.878513	22739.767089	29.843738
417.314595	22761.411297	29.848756
417.928190	22779.884565	29.853773
418.097774	22797.696088	29.858791
418.647140	22822.839942	29.863808
418.938275	22850.121688	29.868826
419.558102	22864.097399	29.873844
419.886058	22894.178947	29.878861
419.423671	22917.371679	29.883879
420.072230	22952.568442	29.888896
420.239796	22985.776696	29.893914
421.060243	23017.703458	29.898932
421.328107	23046.335348	29.903949
421.395585	23079.489642	29.908967
421.950553	23117.750701	29.913984
422.148772	23154.472104	29.919002
422.496404	23188.053798	29.924020
423.025208	23231.429647	29.929037
422.762677	23270.008782	29.934055
423.545526	23311.441375	29.939072
423.851047	23360.113981	29.944090
424.310618	23404.790749	29.949108
425.059067	23444.706601	29.954125
425.527379	23492.797580	29.959143
426.108331	23520.087865	29.964160
426.448332	23563.397817	29.969178
426.811989	23590.601541	29.974196
428.505515	23609.044719	29.979213
428.777744	23634.172576	29.984231
429.541388	23643.087255	29.989248
429.838696	23684.490267	29.994266
430.150179	23697.018452	29.999284
430.322027	23718.209823	30.004301
430.487104	23747.812456	30.009319
431.120640	23770.086669	30.014336
431.237980	23804.178970	30.019354
431.704584	23833.307581	30.024372
432.223432	23862.843038	30.029389
432.390331	23885.369776	30.034407
432.998403	23914.171947	30.039424
433.298887	23934.742100	30.044442
433.630170	23954.904070	30.049460
434.401568	23978.631974	30.054477
434.565607	24012.281681	30.059495
434.929621	24040.831515	30.064512
435.594107	24076.688332	30.069530
435.695038	24098.642980	30.074548
436.059001	24129.742787	30.079565
436.291111	24166.340606	30.084583
436.845654	24204.730385	30.089600
436.899264	24250.895239	30.094618
437.024321	24288.721898	30.099636
438.044062	24321.685317	30.104653
438.168237	24373.185521	30.109671
438.599134	24402.796647	30.114688
438.833242	24454.263055	30.119706
438.910735	24487.679420	30.124724
439.916144	24536.830974	30.129741
439.839221	24593.891415	30.134759
440.920259	24636.401686	30.139776
441.370748	24680.134263	30.144794
441.778382	24730.824780	30.149812
442.508483	24761.688672	30.154829
442.761118	24805.449961	30.159847
443.365695	24847.023667	30.164864
443.923097	24883.597301	30.169882
444.323869	24931.745133	30.174900
444.821053	24967.043736	30.179917
445.337597	24993.983661	30.184935
446.119793	25028.600491	30.189952
446.246168	25073.082151	30.194970
446.421702	25104.761366	30.199988
447.201459	25139.382765	30.205005
447.425423	25185.890271	30.210023
447.960980	25222.281461	30.215040
448.409258	25265.086431	30.220058
448.718761	25301.654825	30.225076
449.367580	25332.371278	30.230093
449.646117	25376.386026	30.235111
450.235246	25421.061195	30.240128
450.599293	25458.883268	30.245146
450.977901	25499.318525	30.250164
451.339595	25546.262043	30.255181
451.712237	25590.187546	30.260199
452.059824	25626.433139	30.265216
452.484714	25681.257406	30.270234
453.344567	25706.843996	30.275252
454.003432	25734.711779	30.280269
454.134074	25777.060596	30.285287
455.310077	25814.043569	30.290304
455.605539	25844.772396	30.295322
455.719013	25877.976374	30.300340
456.260822	25902.481886	30.305357
457.108745	25937.545561	30.310375
457.580113	25950.351774	30.315392
458.121447	25976.206184	30.320410
458.406012	26001.865201	30.325428
459.504407	26023.251565	30.330445
459.351054	26052.375848	30.335463
460.061898	26070.624750	30.340480
460.322627	26092.924578	30.345498
460.538000	26121.026761	30.350516
461.344950	26139.870981	30.355533
461.262572	26171.259359	30.360551
461.763396	26201.145499	30.365568
462.263263	26239.269989	30.370586
462.566243	26270.971382	30.375604
462.991282	26307.736373	30.380621
463.059299	26352.454613	30.385639
463.399161	26384.414272	30.390656
464.219689	26421.575818	30.395674
463.972816	26480.115682	30.400692
464.675044	26512.692246	30.405709
465.249240	26567.765190	30.410727
465.287023	26608.943733	30.415744
465.957652	26661.646813	30.420762
466.643821	26707.468218	30.425780
467.326660	26750.937017	30.430797
467.983466	26809.179698	30.435815
468.223850	26843.206861	30.440832
468.945229	26885.669327	30.445850
469.022429	26930.052870	30.450868
470.029369	26956.273517	30.455885
470.520484	27004.625891	30.460903
471.111764	27040.642040	30.465920
472.004486	27069.054747	30.470938
472.931319	27084.661034	30.475956
473.473645	27103.560364	30.480973
473.648135	27136.266382	30.485991
474.076993	27153.113363	30.491008
474.716474	27198.792337	30.496026
474.452751	27237.800329	30.501044
475.114186	27255.153991	30.506061
475.616335	27289.903835	30.511079
475.958717	27324.884049	30.516096
476.288275	27369.423202	30.521114
476.384346	27406.817461	30.526132
477.015472	27446.048976	30.531149
477.074094	27489.593207	30.536167
477.525293	27528.751161	30.541184
478.175797	27572.563751	30.546202
478.409104	27623.514919	30.551220
479.257348	27670.039668	30.556237
479.616575	27721.467451	30.561255
480.032674	27761.996176	30.566272
480.448616	27802.764547	30.571290
481.040084	27841.034237	30.576308
481.551551	27886.998705	30.581325
481.954811	27926.012407	30.586343
482.071337	27968.823839	30.591360
482.900566	28007.795095	30.596378
482.796048	28053.587123	30.601396
483.298357	28101.097942	30.606413
483.896735	28154.832225	30.611431
484.226390	28193.090876	30.616448
485.040506	28243.875834	30.621466
484.979325	28300.511166	30.626484
486.020975	28342.818504	30.631501
486.314565	28414.134867	30.636519
486.403701	28455.262649	30.641536
487.454590	28504.568815	30.646554
487.896344	28561.181671	30.651572
488.242532	28612.042320	30.656589
488.868575	28662.768726	30.661607
489.334407	28705.119883	30.666624
490.119159	28749.853488	30.671642
490.620411	28802.097281	30.676660
491.541885	28835.901160	30.681677
492.513363	28867.993620	30.686695
492.977290	28908.315880	30.691712
493.774193	28932.203867	30.696730
494.016649	28971.193694	30.701748
494.183975	29006.162873	30.706765
494.768781	29045.370973	30.711783
495.121604	29086.209355	30.716800
495.471670	29121.970718	30.721818
495.815726	29177.331104	30.726836
496.391909	29211.104093	30.731853
496.744179	29266.980375	30.736871
496.909712	29310.225635	30.741888
497.382177	29365.403886	30.746906
497.866277	29412.828461	30.751924
498.540301	29463.743563	30.756941
499.123341	29501.339285	30.761959
499.376106	29562.983036	30.766976
499.916765	29608.645144	30.771994
500.186265	29677.023848	30.777012
500.282124	29722.794951	30.782029
500.819000	29782.834074	30.787047
501.216933	29843.592129	30.792064
501.972098	29901.180950	30.797082
502.354004	29969.568188	30.802100
502.868603	30035.605259	30.807117
503.496976	30090.319848	30.812135
504.081914	30142.972248	30.817152
505.017963	30203.592342	30.822170
505.556199	30264.688943	30.827188
506.281573	30304.511239	30.832205
506.909433	30346.453153	30.837223
507.232014	30396.142686	30.842240
508.189946	30440.303319	30.847258
508.360388	30481.074951	30.852276
508.770730	30521.220609	30.857293
509.495133	30564.392774	30.862311
509.307972	30606.402134	30.867328
510.244459	30641.734567	30.872346
510.490265	30702.236353	30.877364
510.631998	30737.142389	30.882381
511.428664	30778.837875	30.887399
511.701364	30847.964861	30.892416
512.373481	30891.393660	30.897434
512.678637	30948.993231	30.902452
513.208790	31009.430368	30.907469
514.159702	31051.954643	30.912487
514.499488	31095.971214	30.917504
515.391568	31150.508646	30.922522
515.575375	31201.286589	30.927540
516.120068	31244.030525	30.932557
516.868309	31296.819810	30.937575
517.056979	31350.724448	30.942592
517.299571	31401.925503	30.947610
518.189583	31454.071720	30.952628
518.400798	31503.445053	30.957645
518.945737	31561.265486	30.962663
519.272486	31619.500727	30.967680
519.962044	31684.704857	30.972698
520.581762	31744.027125	30.977716
521.183462	31801.029216	30.982733
521.598021	31849.663501	30.987751
521.973777	31915.123428	30.992768
522.597398	31958.673107	30.997786
523.326469	32020.201360	31.002804
523.589042	32092.990353	31.007821
524.168971	32145.353652	31.012839
524.345975	32214.485854	31.017856
524.640487	32267.276442	31.022874
525.236996	32338.965152	31.027892
526.239700	32397.587252	31.032909
527.004692	32453.481153	31.037927
527.424987	32521.228217	31.042944
528.156741	32563.923719	31.047962
528.985805	32621.508739	31.052980
529.520267	32671.822383	31.057997
530.200462	32708.714863	31.063015
531.092518	32770.866218	31.068032
531.819230	32813.826404	31.073050
532.293060	32860.356230	31.078068
532.719907	32899.688560	31.083085
533.187313	32933.737175	31.088103
533.454602	32988.924027	31.093120
533.895771	33038.657816	31.098138
534.209677	33084.937896	31.103156
534.377446	33139.078684	31.108173
536.348732	33154.228136	31.113191
537.721760	33184.569037	31.118208
538.335971	33204.225353	31.123226
538.351490	33235.985277	31.128244
538.924601	33247.553906	31.133261
539.303443	33273.239304	31.138279
539.531660	33304.319198	31.143296
539.992405	33336.153421	31.148314
540.162142	33373.127113	31.153332
540.337044	33409.067579	31.158349
540.969791	33453.743662	31.163367
540.984973	33506.384077	31.168384
541.588744	33547.439487	31.173402
541.819325	33608.275922	31.178420
542.320462	33658.550585	31.183437
543.118580	33711.316011	31.188455
543.019774	33752.720280	31.193472
543.765159	33824.281369	31.198490
544.441510	33878.843272	31.203508
544.921782	33943.463834	31.208525
545.282883	34002.231649	31.213543
545.372362	34071.932538	31.218560
545.868674	34128.924758	31.223578
546.309400	34208.411629	31.228596
546.702672	34282.639696	31.233613
547.718890	34346.356737	31.238631
548.207936	34421.162895	31.243648
548.886421	34485.492308	31.248666
549.722813	34550.086881	31.253684
550.563801	34607.727352	31.258701
551.363530	34659.368386	31.263719
551.562632	34732.745005	31.268736
552.259583	34783.939322	31.273754
553.071273	34841.549010	31.278772
553.285211	34912.822650	31.283789
553.683014	34961.703627	31.288807
554.682895	35028.654473	31.293824
554.841417	35086.359576	31.298842
555.460865	35145.742934	31.303860
555.925350	35209.041946	31.308877
556.820377	35271.914763	31.313895
557.453906	35334.671816	31.318912
557.799209	35390.889963	31.323930
558.498904	35449.093432	31.328948
559.180542	35504.410233	31.333965
560.504261	35554.275837	31.338983
561.043105	35604.334383	31.344000
561.399615	35662.107683	31.349018
562.003371	35700.250255	31.354036
562.301604	35741.375501	31.359053
563.066924	35792.790621	31.364071
563.903071	35840.615866	31.369088
564.454157	35875.235769	31.374106
565.008990	35915.910676	31.379124
565.387420	35973.211746	31.384141
566.143256	36008.772051	31.389159
566.700536	36064.272896	31.394176
567.164996	36104.215362	31.399194
567.732176	36142.870846	31.404212
568.134200	36199.628168	31.409229
568.739653	36237.718091	31.414247
569.304459	36279.365043	31.419264
569.487080	36319.111689	31.424282
570.236598	36363.665040	31.429300
570.603213	36417.901461	31.434317
571.055040	36463.424797	31.439335
571.314057	36528.809523	31.444352
571.342220	36587.730891	31.449370
572.662625	36639.105928	31.454388
573.240217	36699.687080	31.459405
573.563700	36755.077663	31.464423
574.023317	36815.362694	31.469440
574.285807	36877.348997	31.474458
575.070370	36950.348823	31.479476
575.296484	37005.711591	31.484493
576.222283	37070.331612	31.489511
576.633289	37128.958979	31.494528
577.037075	37195.441091	31.499546
577.967689	37252.168235	31.504564
578.528446	37324.711827	31.509581
579.030958	37396.596490	31.514599
579.840025	37455.978325	31.519616
580.378474	37527.140425	31.524634
581.032958	37586.121628	31.529652
581.139585	37656.448012	31.534669
582.232586	37722.191753	31.539687
582.328796	37785.458210	31.544704
582.676116	37857.872526	31.549722
583.439916	37924.131462	31.554740
583.977035	38008.448953	31.559757
584.903545	38069.621194	31.564775
585.263019	38141.539688	31.569792
586.026918	38224.961232	31.574810
586.842095	38278.862573	31.579828
587.192921	38347.837912	31.584845
588.344057	38411.410162	31.589863
589.063368	38471.648710	31.594880
589.639212	38537.466944	31.599898
590.391404	38588.653025	31.604916
590.752414	38649.625713	31.609933
591.763173	38708.577744	31.614951
592.406272	38757.730279	31.619968
593.522877	38804.532199	31.624986
595.049548	38833.971194	31.630004
595.259584	38877.322532	31.635021
596.085357	38912.169843	31.640039
596.562857	38951.667580	31.645056
597.236804	38988.082946	31.650074
597.642258	39028.060655	31.655092
597.801952	39075.444613	31.660109
598.237713	39107.793640	31.665127
598.473980	39170.692897	31.670144
598.824324	39227.484390	31.675162
599.147147	39268.544933	31.680180
599.342986	39330.330068	31.685197
599.595429	39395.897219	31.690215
600.267406	39451.378317	31.695232
600.429605	39515.350304	31.700250
601.503556	39588.599267	31.705268
601.943462	39644.948974	31.710285
602.715786	39701.562888	31.715303
603.029710	39777.119281	31.720320
603.810453	39840.749568	31.725338
604.586796	39896.232841	31.730356
605.006215	39971.289179	31.735373
605.604848	40035.425425	31.740391
606.077810	40106.558306	31.745408
606.710164	40175.193448	31.750426
607.408044	40245.215612	31.755444
608.445602	40307.617722	31.760461
609.326930	40367.736263	31.765479
610.278394	40428.443096	31.770496
610.587743	40486.259299	31.775514
611.566863	40540.897083	31.780532
612.036341	40591.405649	31.785549
612.481771	40655.502386	31.790567
613.207540	40715.435606	31.795584
613.422098	40776.071782	31.800602
614.283388	40835.725215	31.805620
614.769066	40904.320408	31.810637
615.524841	40970.072077	31.815655
616.069247	41034.305864	31.820672
616.105752	41110.886925	31.825690
616.678667	41172.694369	31.830708
616.899274	41253.205114	31.835725
617.092043	41333.279093	31.840743
618.003747	41405.527140	31.845760
618.773409	41494.120752	31.850778
619.571750	41574.474767	31.855796
620.088269	41654.432451	31.860813
620.855794	41728.373369	31.865831
621.649118	41806.467721	31.870848
621.856393	41886.195003	31.875866
622.626701	41957.171506	31.880884
623.359566	42042.269463	31.885901
624.214858	42116.059285	31.890919
624.925492	42186.677190	31.895936
625.463066	42261.328872	31.900954
626.151371	42325.024112	31.905972
627.482010	42386.475536	31.910989
628.769116	42436.695310	31.916007
630.139893	42471.344824	31.921024
630.772138	42525.511090	31.926042
631.824329	42558.006637	31.931060
632.404751	42594.961895	31.936077
632.933770	42631.357636	31.941095
633.745123	42656.308680	31.946112
633.830673	42699.982867	31.951130
634.457289	42733.057518	31.956148
635.085253	42772.122163	31.961165
635.473976	42802.433748	31.966183
635.963014	42841.978058	31.971200
636.275283	42886.827899	31.976218
637.224925	42927.750082	31.981236
637.208302	42975.513562	31.986253
637.269701	43022.428830	31.991271
637.846683	43081.312028	31.996288
638.297923	43145.401343	32.001306
638.896751	43212.580835	32.006324
639.229582	43284.354832	32.011341
639.380758	43361.416562	32.016359
640.319180	43433.583691	32.021376
640.531760	43525.096556	32.026394
641.052600	43593.088031	32.031412
641.780907	43670.434624	32.036429
642.322821	43750.981561	32.041447
643.604770	43827.776981	32.046464
643.783515	43914.350933	32.051482
644.416378	43992.398702	32.056500
645.197463	44075.678792	32.061517
645.506618	44159.261559	32.066535
646.539316	44243.716920	32.071552
646.992252	44331.851845	32.076570
647.693460	44413.865485	32.081588
648.617607	44505.289134	32.086605
649.007315	44586.684394	32.091623
649.673797	44666.348193	32.096640
650.706070	44755.210084	32.101658
651.210115	44837.594669	32.106676
652.326075	44917.677034	32.111693
653.221495	44995.223743	32.116711
653.809540	45054.761753	32.121728
653.886496	45142.992190	32.126746
655.127998	45209.588076	32.131764
656.170030	45279.408659	32.136781
656.697419	45369.707491	32.141799
657.683368	45431.849271	32.146816
658.036996	45508.648492	32.151834
659.181214	45558.982109	32.156852
660.257685	45609.418151	32.161869
661.260747	45664.207159	32.166887
661.863071	45717.615200	32.171904
662.652029	45774.927863	32.176922
662.918473	45830.620251	32.181940
663.158524	45876.877463	32.186957
663.702617	45955.506573	32.191975
664.153003	46015.479916	32.196992
665.045439	46085.321230	32.202010
665.276238	46151.781913	32.207028
665.739941	46221.244024	32.212045
666.336813	46311.984659	32.217063
667.203212	46373.107666	32.222080
667.411817	46442.926772	32.227098
668.087282	46520.256551	32.232116
668.852899	46583.955082	32.237133
669.511942	46660.846388	32.242151
669.667199	46733.650373	32.247168
670.059156	46815.456330	32.252186
670.938614	46889.581225	32.257204
671.552942	46972.450485	32.262221
672.088134	47055.357976	32.267239
672.894057	47130.937495	32.272256
673.187481	47216.846930	32.277274
674.073180	47315.535649	32.282292
675.203214	47385.729235	32.287309
676.044425	47463.484808	32.292327
676.962948	47538.423416	32.297344
677.688751	47602.592636	32.302362
678.500680	47682.723423	32.307380
679.100817	47753.785346	32.312397
679.388007	47836.190130	32.317415
680.233290	47904.730423	32.322432
680.641625	47991.436239	32.327450
681.449649	48065.154639	32.332468
682.475988	48143.022564	32.337485
683.255690	48231.244942	32.342503
684.053335	48307.121109	32.347520
684.628021	48381.565847	32.352538
685.200334	48456.519294	32.357556
685.892557	48532.094515	32.362573
686.828655	48603.380881	32.367591
687.507236	48673.683019	32.372608
688.449130	48752.892353	32.377626
688.902176	48828.753041	32.382644
689.863434	48889.143914	32.387661
690.426081	48976.309609	32.392679
690.941489	49042.975672	32.397696
691.488744	49127.516030	32.402714
692.386321	49191.108291	32.407732
693.430581	49261.736357	32.412749
694.551534	49320.001686	32.417767
695.285201	49387.246468	32.422784
695.774217	49462.413067	32.427802
696.417279	49529.751701	32.432820
697.092194	49593.330361	32.437837
697.622807	49666.048768	32.442855
698.136525	49735.939570	32.447872
698.802542	49807.453639	32.452890
699.586079	49861.596407	32.457908
700.673042	49938.070920	32.462925
700.887247	50025.461318	32.467943
701.485069	50088.460753	32.472960
702.287273	50159.462265	32.477978
702.518912	50244.547302	32.482996
703.151494	50323.494145	32.488013
703.608171	50410.008397	32.493031
704.136123	50494.220643	32.498048
704.849082	50571.297045	32.503066
705.652375	50663.551327	32.508084
706.665037	50737.727906	32.513101
706.736031	50829.512648	32.518119
707.201615	50909.971895	32.523136
707.968665	50997.212747	32.528154
708.238800	51098.156969	32.533172
709.177722	51179.021757	32.538189
709.511148	51277.403809	32.543207
710.464181	51370.897091	32.548224
711.279320	51468.749051	32.553242
711.887455	51569.973484	32.558260
712.544317	51664.746263	32.563277
713.540998	51762.605636	32.568295
714.618540	51860.960784	32.573312
716.091824	51935.173132	32.578330
716.939854	51999.935217	32.583348
718.096829	52055.246548	32.588365
719.126266	52135.066053	32.593383
719.693682	52205.330346	32.598400
720.675828	52267.196879	32.603418
721.462652	52340.677516	32.608436
722.226356	52402.219496	32.613453
722.832603	52472.393433	32.618471
723.172646	52537.323536	32.623488
724.073947	52590.060799	32.628506
724.611452	52672.299681	32.633524
725.386650	52741.182157	32.638541
725.907520	52809.691927	32.643559
726.673840	52888.328908	32.648576
727.575126	52968.323999	32.653594
727.756310	53047.108475	32.658612
728.403385	53124.698671	32.663629
729.013888	53211.343924	32.668647
729.527653	53289.407388	32.673664
730.291585	53374.169969	32.678682
730.456297	53457.519640	32.683700
731.850240	53554.555357	32.688717
732.585183	53649.262991	32.693735
733.231541	53736.634152	32.698752
733.942623	53821.145260	32.703770
734.333497	53906.784050	32.708788
735.230472	53995.252844	32.713805
736.074905	54099.666999	32.718823
736.622126	54186.434295	32.723840
737.951275	54262.434112	32.728858
738.522916	54355.489054	32.733876
739.319461	54438.528000	32.738893
740.506480	54521.580922	32.743911
741.494256	54602.986698	32.748928
742.385629	54682.094482	32.753946
742.716046	54765.407978	32.758964
743.601833	54833.210738	32.763981
744.150128	54927.058283	32.768999
744.682818	55004.987206	32.774016
745.538560	55084.948361	32.779034
746.210500	55172.615896	32.784052
746.737422	55243.842207	32.789069
747.126406	55319.427912	32.794087
747.772597	55407.791966	32.799104
748.222000	55484.577715	32.804122
748.821671	55582.227327	32.809140
749.697541	55672.541622	32.814157
750.080346	55775.435263	32.819175
750.616788	55870.596392	32.824192
751.710382	55966.767858	32.829210
752.259650	56078.368144	32.834228
753.142862	56161.306416	32.839245
754.143014	56262.450384	32.844263
754.769774	56369.185012	32.849280
755.655644	56459.870932	32.854298
756.498327	56551.081889	32.859316
757.268754	56652.851739	32.864333
757.847610	56746.249141	32.869351
758.545878	56839.268128	32.874368
759.732448	56936.888337	32.879386
760.955411	57037.505471	32.884404
761.743100	57117.492629	32.889421
762.735900	57202.678493	32.894439
763.250817	57297.152744	32.899456
764.460764	57378.589148	32.904474
765.544177	57476.152867	32.909492
766.490317	57543.040515	32.914509
767.279013	57608.570708	32.919527
768.157585	57693.139308	32.924544
769.000315	57765.859418	32.929562
769.492742	57851.784583	32.934580
770.229454	57916.957928	32.939597
771.133730	57992.295787	32.944615
771.697939	58080.161642	32.949632
772.313376	58159.672442	32.954650
772.672278	58245.721713	32.959668
773.429660	58330.312513	32.964685
773.891087	58423.042513	32.969703
774.142288	58528.820169	32.974720
775.474387	58634.353763	32.979738
775.789925	58748.400500	32.984756
776.251638	58839.475011	32.989773
777.112496	58939.850720	32.994791
777.701149	59045.145058	32.999808
778.839660	59155.877653	33.004826
779.524752	59270.904342	33.009844
780.403625	59365.665858	33.014861
781.603714	59464.149701	33.019879
782.306878	59558.621279	33.024896
783.645786	59652.736400	33.029914
784.689745	59742.311318	33.034932
785.536245	59837.323499	33.039949
786.204203	59920.237094	33.044967
786.975088	60016.657783	33.049984
788.013230	60092.825866	33.055002
788.876077	60168.671687	33.060020
789.774548	60230.748907	33.065037
791.522144	60287.115146	33.070055
791.853156	60351.196495	33.075072
792.986649	60396.132964	33.080090
793.636538	60462.573080	33.085108
794.512226	60528.917501	33.090125
794.811841	60589.866129	33.095143
795.442801	60658.406525	33.100160
795.898528	60735.168809	33.105178
796.444405	60815.737666	33.110196
796.977792	60893.587056	33.115213
797.649760	60985.364787	33.120231
798.238188	61076.313192	33.125248
799.273626	61164.759547	33.130266
799.655582	61249.410693	33.135284
800.302639	61346.792578	33.140301
801.193466	61441.606904	33.145319
802.091284	61535.735385	33.150336
802.941937	61634.535714	33.155354
803.561122	61740.775006	33.160372
804.120544	61843.554096	33.165389
805.016309	61944.537153	33.170407
805.418925	62053.581991	33.175424
806.422403	62154.672180	33.180442
807.187339	62275.767454	33.185460
807.652320	62376.309823	33.190477
808.806259	62489.453240	33.195495
809.271948	62613.674007	33.200512
810.175194	62725.649287	33.205530
811.124580	62833.294768	33.210548
811.934827	62952.590332	33.215565
813.205271	63056.904943	33.220583
814.431805	63162.818708	33.225600
815.250743	63252.278777	33.230618
816.310641	63353.372699	33.235636
816.630908	63448.069989	33.240653
817.909314	63555.240874	33.245671
818.556986	63656.793607	33.250688
819.367557	63755.260836	33.255706
819.866965	63871.144131	33.260724
820.364279	63972.264559	33.265741
821.512778	64074.039821	33.270759
822.089588	64195.764672	33.275776
822.803788	64289.345483	33.280794
823.811356	64415.389785	33.285812
824.659943	64523.743025	33.290829
825.838209	64644.197021	33.295847
827.381027	64715.266148	33.300864
828.254965	64805.043726	33.305882
828.871222	64896.748184	33.310900
829.510167	65007.285107	33.315917
830.559890	65095.526440	33.320935
831.105296	65202.418976	33.325952
831.637389	65294.843023	33.330970
832.650339	65398.617669	33.335988
832.931660	65498.574066	33.341005
833.867353	65587.025306	33.346023
834.767049	65697.240454	33.351040
835.759248	65785.475164	33.356058
836.778650	65882.618862	33.361076
837.392119	65984.183064	33.366093
838.577241	66067.214932	33.371111
839.337963	66164.701269	33.376128
839.817091	66260.713709	33.381146
841.207308	66346.711494	33.386164
842.329416	66426.899710	33.391181
843.156806	66516.834826	33.396199
843.967689	66614.463902	33.401216
845.191525	66698.948397	33.406234
846.049474	66793.346058	33.411252
846.545606	66884.674815	33.416269
847.519526	66970.432098	33.421287
847.991577	67069.175506	33.426304
848.990243	67160.766715	33.431322
849.498077	67251.090911	33.436340
849.878639	67359.149249	33.441357
850.969640	67458.743723	33.446375
851.555411	67581.969952	33.451392
852.386388	67680.798333	33.456410
852.892120	67797.841376	33.461428
853.590425	67909.598404	33.466445
854.657827	68022.725076	33.471463
855.504914	68149.154155	33.476480
856.165336	68261.405677	33.481498
857.357415	68380.579398	33.486516
857.910826	68495.957534	33.491533
858.744597	68614.753794	33.496551
859.653077	68743.501843	33.501568
860.378939	68866.783398	33.506586
861.499608	68984.070541	33.511604
862.566426	69111.184792	33.516621
863.646645	69214.915480	33.521639
864.538543	69344.093418	33.526656
865.289040	69457.942216	33.531674
866.071131	69562.297116	33.536692
866.896915	69691.424684	33.541709
867.997559	69811.916868	33.546727
869.028090	69927.884591	33.551744
869.763388	70042.528955	33.556762
870.688957	70149.227107	33.561780
871.203405	70274.231774	33.566797
872.091859	70390.149015	33.571815
872.808132	70511.989249	33.576832
873.799883	70628.605417	33.581850
874.736732	70745.490061	33.586868
875.888489	70866.625040	33.591885
877.167129	70977.479515	33.596903
878.833120	71064.022900	33.601920
879.704612	71167.974030	33.606938
880.845682	71258.955210	33.611956
881.176424	71359.733065	33.616973
881.878354	71435.930138	33.621991
882.811539	71532.468053	33.627008
883.142070	71632.956677	33.632026
884.051116	71740.708634	33.637044
884.194673	71850.939846	33.642061
884.920542	71951.544098	33.647079
885.705875	72073.465107	33.652096
886.691499	72189.004630	33.657114
887.530215	72309.901274	33.662132
888.116750	72439.065921	33.667149
889.072095	72566.472938	33.672167
889.949491	72690.063902	33.677184
890.284530	72817.179454	33.682202
891.622410	72934.442883	33.687220
892.375802	73065.834607	33.692237
893.633912	73193.823043	33.697255
894.432567	73334.024457	33.702272
895.617957	73459.574345	33.707290
896.720056	73578.882258	33.712308
897.584051	73706.772393	33.717325
898.566433	73818.087976	33.722343
899.451299	73958.324281	33.727360
900.207498	74087.396754	33.732378
901.517448	74208.147756	33.737396
902.137109	74342.943704	33.742413
903.041408	74454.395313	33.747431
904.498632	74577.987833	33.752448
905.380334	74702.658542	33.757466
906.374231	74823.861669	33.762484
907.475291	74938.703558	33.767501
908.308407	75047.262746	33.772519
909.282161	75166.215017	33.777536
910.235800	75283.464858	33.782554
911.152041	75391.772525	33.787572
912.563073	75498.213537	33.792589
913.781664	75597.872941	33.797607
914.943982	75696.145099	33.802624
915.526086	75806.239799	33.807642
916.726651	75902.301227	33.812660
917.473009	76019.215444	33.817677
918.037730	76125.333062	33.822695
918.680920	76231.426109	33.827712
919.409193	76346.044593	33.832730
920.483679	76461.088967	33.837748
921.268628	76583.334469	33.842765
921.898368	76695.594228	33.847783
922.790805	76814.720809	33.852800
923.356878	76942.356522	33.857818
924.346959	77060.280795	33.862836
925.052867	77193.982282	33.867853
926.016545	77328.408397	33.872871
927.104971	77462.663861	33.877888
927.736995	77590.703964	33.882906
928.769996	77709.282489	33.887924
929.293750	77834.219019	33.892941
930.182703	77951.279656	33.897959
930.988853	78083.605771	33.902976
931.680359	78210.711160	33.907994
933.353653	78331.258270	33.913012
933.829342	78458.469060	33.918029
934.955429	78598.307187	33.923047
936.108953	78713.926875	33.928064
937.112735	78843.451614	33.933082
938.628420	78945.336676	33.938100
939.920236	79053.945386	33.943117
941.155922	79164.030061	33.948135
942.021804	79268.504244	33.953152
942.941932	79376.864068	33.958170
944.285317	79477.375919	33.963188
945.305492	79589.595744	33.968205
946.004481	79697.442504	33.973223
947.277851	79802.537242	33.978240
948.122957	79897.687918	33.983258
948.791172	80008.840850	33.988276
949.506312	80118.874376	33.993293
950.452616	80244.630643	33.998311
951.510408	80352.569124	34.003328
952.485940	80455.736001	34.008346
953.648071	80559.183451	34.013364
954.690908	80681.153152	34.018381
955.149136	80797.185921	34.023399
956.276709	80906.589082	34.028416
956.933479	81023.388032	34.033434
958.031294	81151.894517	34.038452
958.392167	81279.216792	34.043469
959.549997	81401.652867	34.048487
959.949404	81520.758694	34.053504
960.805247	81650.558442	34.058522
961.951633	81787.273012	34.063540
962.564189	81940.769247	34.068557
963.332776	82087.616502	34.073575
964.420828	82215.524197	34.078592
964.990526	82359.041761	34.083610
966.199303	82506.567909	34.088628
967.294706	82662.394962	34.093645
967.998226	82800.115940	34.098663
969.355194	82938.682177	34.103680
969.995694	83083.344050	34.108698
971.282366	83219.451369	34.113716
972.609009	83369.335645	34.118733
973.650738	83511.199107	34.123751
974.621238	83636.510423	34.128768
975.501750	83786.696246	34.133786
976.296631	83930.378377	34.138804
977.681688	84063.687326	34.143821
978.639296	84201.769035	34.148839
979.563400	84341.696826	34.153856
980.430770	84483.980234	34.158874
981.466202	84602.660915	34.163892
982.190883	84736.945357	34.168909
983.154891	84862.290261	34.173927
983.982799	84987.600652	34.178944
984.639890	85133.266576	34.183962
985.746993	85271.628639	34.188980
986.832746	85402.711101	34.193997
987.707369	85554.529028	34.199015
988.620618	85687.474318	34.204032
989.777886	85827.931222	34.209050
990.587716	85964.599941	34.214068
991.834018	86103.362579	34.219085
992.371096	86257.496527	34.224103
993.576319	86400.921418	34.229120
994.465749	86557.638216	34.234138
995.682909	86694.777950	34.239156
996.827104	86847.713003	34.244173
997.825671	86985.920063	34.249191
998.880979	87132.946363	34.254208
999.539850	87282.863285	34.259226
1000.889776	87428.921529	34.264244
1002.133969	87568.566620	34.269261
1003.246534	87715.006032	34.274279
1004.028411	87852.665045	34.279296
1005.066267	87997.101045	34.284314
1006.587143	88132.038966	34.289332
1008.007681	88249.907144	34.294349
1009.310860	88391.356749	34.299367
1010.413233	88516.789559	34.304384
1011.020504	88657.017292	34.309402
1011.935632	88794.205791	34.314420
1013.255430	88921.073483	34.319437
1013.930471	89054.052184	34.324455
1014.800419	89193.438463	34.329472
1015.863277	89334.831271	34.334490
1016.614716	89471.031923	34.339508
1017.396935	89611.408735	34.344525
1018.358016	89765.784860	34.349543
1019.654362	89908.465992	34.354560
1020.361571	90056.579385	34.359578
1021.607774	90193.483724	34.364596
1022.944616	90336.818935	34.369613
1023.592528	90497.979076	34.374631
1024.346397	90648.542891	34.379648
1025.359416	90806.719048	34.384666
1026.735998	90948.768091	34.389684
1027.923691	91088.919131	34.394701
1029.123304	91240.769549	34.399719
1030.018182	91375.397083	34.404736
1031.105881	91525.211783	34.409754
1032.168144	91672.685101	34.414772
1033.410796	91824.450482	34.419789
1034.287547	91970.481647	34.424807
1035.347949	92108.426795	34.429824
1036.204177	92245.918270	34.434842
1037.480041	92371.592269	34.439860
1038.137980	92506.536364	34.444877
1038.769168	92644.837750	34.449895
1040.260967	92766.842812	34.454912
1041.333455	92908.864310	34.459930
1042.171490	93041.765340	34.464948
1043.286872	93177.070859	34.469965
1043.934001	93317.290401	34.474983
1045.056433	93467.346760	34.480000
1046.081983	93619.203250	34.485018
1046.798078	93762.779640	34.490036
1047.913532	93914.155772	34.495053
1048.295553	94065.061332	34.500071
1049.741124	94215.147232	34.505088
1050.743062	94387.348807	34.510106
1051.856061	94550.558193	34.515124
1052.803106	94703.705964	34.520141
1054.061866	94867.337261	34.525159
1055.489405	95010.144316	34.530176
1056.922615	95157.398307	34.535194
1057.937530	95305.693950	34.540212
1059.527561	95459.566951	34.545229
1060.525687	95609.164040	34.550247
1061.435784	95753.323274	34.555264
1062.463131	95892.758347	34.560282
1062.963335	96059.289689	34.565300
1064.720153	96191.114397	34.570317
1065.686414	96343.194862	34.575335
1067.063626	96478.788649	34.580352
1068.439586	96629.319263	34.585370
1069.683797	96779.916116	34.590388
1070.739049	96913.128165	34.595405
1071.598753	97048.845630	34.600423
1073.052102	97181.369648	34.605440
1073.944147	97323.276970	34.610458
1074.718117	97467.443463	34.615476
1076.129806	97610.459273	34.620493
1076.614008	97761.664309	34.625511
1077.408508	97900.168173	34.630528
1078.403471	98059.746033	34.635546
1079.391429	98220.034691	34.640564
1080.479046	98379.960662	34.645581
1081.373977	98532.459352	34.650599
1082.416603	98680.000799	34.655616
1083.414316	98835.477652	34.660634
1084.331764	99010.302759	34.665652
1085.660124	99177.465402	34.670669
1086.518687	99342.976760	34.675687
1087.540472	99511.006743	34.680704
1088.939248	99684.355860	34.685722
1090.115031	99839.773220	34.690740
1091.260468	100005.851100	34.695757
1092.320968	100172.937026	34.700775
1093.206305	100323.373840	34.705792
1094.626019	100484.318241	34.710810
1095.401059	100643.196071	34.715828
1097.227058	100773.195007	34.720845
1098.398218	100919.003014	34.725863
1099.190193	101071.477919	34.730880
1099.916759	101223.875644	34.735898
1100.983957	101371.012775	34.740916
1102.058363	101522.123299	34.745933
1102.730405	101683.384736	34.750951
1103.800152	101838.478013	34.755968
1104.805413	102002.637272	34.760986
1105.381763	102176.237036	34.766004
1106.816334	102332.250018	34.771021
1107.639915	102516.285198	34.776039
1108.716550	102695.731949	34.781056
1109.778711	102876.663071	34.786074
1110.628910	103055.123479	34.791092
1111.910553	103243.919637	34.796109
1112.345566	103438.901436	34.801127
1113.313721	103624.054988	34.806144
1114.899324	103810.548261	34.811162
1115.643259	104017.388711	34.816180
1117.694628	104206.304299	34.821197
1118.395766	104405.472605	34.826215
1119.303787	104599.350923	34.831232
1120.727997	104791.161658	34.836250
1121.691584	104984.584975	34.841268
1123.243275	105176.745592	34.846285
1124.380049	105373.808663	34.851303
1125.234338	105560.501599	34.856320
1126.708258	105745.933008	34.861338
1128.043055	105947.475240	34.866356
1129.187049	106130.569893	34.871373
1130.738110	106322.594272	34.876391
1131.862288	106517.770167	34.881408
1132.960035	106695.959063	34.886426
1134.504842	106870.249247	34.891444
1135.505210	107050.911844	34.896461
1136.828587	107230.840907	34.901479
1138.331752	107400.704979	34.906496
1139.870171	107572.994983	34.911514
1140.989462	107758.346424	34.916532
1141.926313	107921.221992	34.921549
1143.004224	108096.120592	34.926567
1144.018189	108274.897761	34.931584
1145.343170	108437.037852	34.936602
1146.221327	108607.035093	34.941620
1147.776756	108776.653665	34.946637
1148.912998	108956.903798	34.951655
1150.020607	109121.633755	34.956672
1151.153594	109300.026095	34.961690
1152.790939	109467.807239	34.966708
1154.398187	109621.061682	34.971725
1155.742402	109768.497718	34.976743
1156.967004	109924.764496	34.981760
1158.205266	110075.858763	34.986778
1158.927176	110219.763241	34.991796
1160.333664	110359.755536	34.996813
1161.600118	110495.479312	35.001831
1162.471239	110633.526438	35.006848
1163.581749	110765.522926	35.011866
1164.131863	110927.252044	35.016884
1165.353748	111062.334053	35.021901
1166.318469	111218.637717	35.026919
1167.383965	111377.331744	35.031936
1168.284045	111526.152915	35.036954
1169.050392	111695.246154	35.041972
1170.656166	111859.123988	35.046989
1171.363100	112033.280414	35.052007
1172.245369	112187.425723	35.057024
1173.438548	112366.748579	35.062042
1174.321108	112568.240173	35.067060
1175.215307	112750.246732	35.072077
1176.439900	112938.469174	35.077095
1177.356233	113129.147615	35.082112
1178.715197	113321.624626	35.087130
1179.732655	113520.399328	35.092148
1180.832801	113712.388726	35.097165
1181.844334	113913.345205	35.102183
1182.697154	114110.992251	35.107200
1184.385430	114320.124921	35.112218
1185.437005	114522.497981	35.117236
1186.427558	114727.389380	35.122253
1187.312073	114940.966296	35.127271
1188.650444	115154.276593	35.132288
1190.177628	115359.461313	35.137306
1191.554464	115584.025634	35.142324
1192.770173	115796.518804	35.147341
1194.012827	115993.643736	35.152359
1195.161746	116216.173255	35.157376
1196.721425	116419.405017	35.162394
1197.484678	116628.849417	35.167412
1199.013688	116837.027805	35.172429
1200.420859	117050.532987	35.177447
1201.622856	117246.718005	35.182464
1202.834749	117449.025528	35.187482
1204.022347	117663.343161	35.192500
1205.576561	117870.690158	35.197517
1206.717605	118077.408029	35.202535
1207.779377	118288.224120	35.207552
1209.428824	118482.276937	35.212570
1210.672157	118688.571868	35.217588
1211.734067	118881.859962	35.222605
1213.332152	119079.357292	35.227623
1214.065195	119282.629103	35.232640
1215.702423	119490.362126	35.237658
1216.917904	119679.389282	35.242676
1218.876181	119858.693910	35.247693
1220.000650	120054.114684	35.252711
1221.076855	120245.112052	35.257728
1222.281041	120425.895551	35.262746
1223.624044	120604.872523	35.267764
1224.680369	120778.260520	35.272781
1225.853776	120954.847892	35.277799
1227.208756	121123.808688	35.282816
1228.502532	121299.885312	35.287834
1229.736274	121478.201695	35.292852
1230.654161	121652.909290	35.297869
1232.166508	121827.409548	35.302887
1232.940172	122003.459565	35.307904
1234.076196	122190.889939	35.312922
1235.279971	122371.876832	35.317940
1236.069396	122560.694788	35.322957
1237.251020	122751.693546	35.327975
1238.153388	122952.490653	35.332992
1239.736839	123151.597774	35.338010
1240.598970	123360.637116	35.343028
1241.916645	123569.618339	35.348045
1243.239752	123766.668877	35.353063
1244.178574	123984.301168	35.358080
1245.626832	124189.137287	35.363098
1246.436607	124409.922111	35.368116
1247.406749	124627.934623	35.373133
1248.800707	124849.314169	35.378151
1250.033897	125071.620424	35.383168
1251.802070	125281.569335	35.388186
1252.943902	125510.138447	35.393204
1254.036989	125726.924252	35.398221
1255.466164	125944.722397	35.403239
1256.642228	126170.517528	35.408256
1258.341093	126383.830127	35.413274
1259.916379	126608.754719	35.418292
1260.830093	126824.919072	35.423309
1262.253233	127040.814136	35.428327
1263.542046	127255.414813	35.433344
1265.028442	127477.941146	35.438362
1266.382743	127693.928300	35.443380
1267.195029	127908.660500	35.448397
1268.655562	128122.024514	35.453415
1270.071198	128341.364041	35.458432
1271.499795	128560.335867	35.463450
1272.525653	128781.793110	35.468468
1273.704579	128986.758731	35.473485
1274.950025	129208.906582	35.478503
1276.378586	129424.300017	35.483520
1277.527861	129651.280792	35.488538
1279.015746	129885.481544	35.493556
1280.050706	130113.117690	35.498573
1282.048954	130316.607268	35.503591
1282.777981	130544.675623	35.508608
1284.329956	130758.856148	35.513626
1285.722612	130972.949606	35.518644
1287.313790	131187.393222	35.523661
1288.804006	131390.312519	35.528679
1289.861505	131616.221518	35.533696
1291.135205	131817.556579	35.538714
1292.659164	132013.506608	35.543732
1293.842186	132212.578313	35.548749
1295.591351	132384.637591	35.553767
1297.100090	132569.583623	35.558784
1298.348269	132761.274808	35.563802
1299.562600	132936.589988	35.568820
1300.557648	133129.362844	35.573837
1301.958746	133317.916552	35.578855
1303.183126	133511.593145	35.583872
1305.445206	133676.685926	35.588890
1306.964350	133859.091863	35.593908
1307.752151	134043.072340	35.598925
1309.419917	134218.297952	35.603943
1310.466856	134406.471624	35.608960
1311.443161	134587.422606	35.613978
1312.740351	134778.980102	35.618996
1313.493215	134970.625384	35.624013
1314.781635	135161.844686	35.629031
1315.877132	135367.807343	35.634048
1317.441636	135562.419339	35.639066
1318.951524	135755.976912	35.644084
1320.511116	135967.407504	35.649101
1321.834902	136154.838905	35.654119
1323.035669	136356.660852	35.659136
1324.292657	136555.915539	35.664154
1325.261232	136745.650101	35.669172
1326.400728	136962.730312	35.674189
1327.983051	137173.405680	35.679207
1329.479456	137382.626235	35.684224
1330.801273	137587.478734	35.689242
1332.265944	137795.769513	35.694260
1333.435189	138015.704039	35.699277
1334.957952	138206.208978	35.704295
1336.045211	138419.354359	35.709312
1336.703830	138636.650021	35.714330
1338.625640	138848.677367	35.719348
1339.980550	139084.912927	35.724365
1341.155897	139284.541144	35.729383
1342.381914	139517.974526	35.734400
1343.257994	139730.693932	35.739418
1344.963589	139953.079479	35.744436
1346.138844	140177.768805	35.749453
1347.860903	140397.012016	35.754471
1348.974209	140624.299912	35.759488
1349.979008	140863.203188	35.764506
1351.510681	141089.604302	35.769524
1352.580116	141325.028331	35.774541
1353.724786	141558.287650	35.779559
1355.021572	141806.454653	35.784576
1356.478064	142041.886085	35.789594
1357.920716	142277.194791	35.794612
1359.157990	142524.908143	35.799629
1361.028484	142762.433974	35.804647
1362.270506	142993.065156	35.809664
1363.540601	143228.395910	35.814682
1364.846355	143447.613165	35.819700
1366.034103	143676.673744	35.824717
1367.326485	143893.209218	35.829735
1368.730514	144119.526266	35.834752
1370.024073	144347.370862	35.839770
1371.687058	144564.701363	35.844788
1372.429482	144805.705056	35.849805
1374.457293	145022.017448	35.854823
1375.395474	145267.772227	35.859840
1376.509666	145498.480375	35.864858
1378.171569	145733.121376	35.869876
1379.263533	145973.317967	35.874893
1380.741395	146219.083161	35.879911
1382.056818	146456.877537	35.884928
1383.721584	146697.242136	35.889946
1385.504994	146923.772680	35.894964
1386.916229	147166.221993	35.899981
1388.634401	147401.576323	35.904999
1389.764524	147633.197553	35.910016
1390.633335	147883.597930	35.915034
1392.557174	148115.616270	35.920052
1394.004023	148362.645291	35.925069
1395.576778	148592.301619	35.930087
1397.162326	148823.732327	35.935104
1398.626556	149069.990734	35.940122
1400.335693	149285.115151	35.945140
1401.697968	149528.693037	35.950157
1402.835090	149753.634882	35.955175
1404.371478	149996.313884	35.960192
1405.787123	150243.615809	35.965210
1407.060419	150478.556244	35.970228
1408.551008	150714.896419	35.975245
1410.172193	150951.014708	35.980263
1411.333145	151182.859331	35.985280
1412.743628	151425.061848	35.990298
1414.359994	151657.382607	35.995316
1415.243290	151909.751494	36.000333
1416.867845	152150.847692	36.005351
1418.776467	152388.540761	36.010368
1419.886736	152635.161201	36.015386
1421.454319	152870.693197	36.020404
1423.249064	153112.606129	36.025421
1424.702027	153342.872712	36.030439
1426.169568	153575.940572	36.035456
1427.608542	153811.296788	36.040474
1429.623287	154030.169311	36.045492
1430.732202	154262.842491	36.050509
1432.159634	154500.234013	36.055527
1433.769003	154740.451117	36.060544
1434.704656	154967.806070	36.065562
1436.298071	155198.684337	36.070580
1437.568853	155436.081961	36.075597
1439.010075	155662.651192	36.080615
1440.562031	155897.382696	36.085632
1441.840022	156127.658047	36.090650
1443.467880	156341.306868	36.095668
1444.633820	156575.432334	36.100685
1445.795847	156793.748106	36.105703
1447.357604	157010.657670	36.110720
1448.296596	157244.316548	36.115738
1449.799416	157467.274089	36.120756
1450.897857	157709.901049	36.125773
1452.082426	157946.378718	36.130791
1453.257421	158190.543883	36.135808
1454.272909	158451.360322	36.140826
1455.693155	158698.837752	36.145844
1456.955648	158967.772465	36.150861
1458.184856	159233.075127	36.155879
1459.797872	159500.018059	36.160896
1461.050552	159772.080003	36.165914
1462.645513	160052.763565	36.170932
1463.921909	160331.217344	36.175949
1465.654968	160603.539075	36.180967
1467.068809	160886.426523	36.185984
1468.236774	161163.242778	36.191002
1469.623452	161430.134755	36.196020
1471.736762	161720.222302	36.201037
1473.433758	161997.620410	36.206055
1475.270181	162270.230101	36.211072
1476.585672	162545.625888	36.216090
1477.956126	162825.441101	36.221108
1479.479874	163103.699571	36.226125
1480.967444	163391.414248	36.231143
1482.819522	163674.685170	36.236160
1484.173453	163957.885241	36.241178
1486.067126	164220.493971	36.246196
1488.173166	164486.596633	36.251213
1489.518204	164755.384044	36.256231
1491.477824	165016.453365	36.261248
1493.181574	165270.995401	36.266266
1495.166302	165520.852552	36.271284
1496.085239	165786.138521	36.276301
1498.241922	166034.855694	36.281319
1500.108769	166266.929334	36.286336
1501.515036	166519.028557	36.291354
1503.013786	166762.870524	36.296372
1504.970461	166991.421061	36.301389
1506.051334	167244.693001	36.306407
1507.330386	167481.306799	36.311424
1509.117511	167731.146671	36.316442
1510.341590	167979.580937	36.321460
1512.029199	168226.027914	36.326477
1513.189352	168464.391749	36.331495
1514.745521	168714.135245	36.336512
1515.641864	168984.673143	36.341530
1517.548146	169225.827881	36.346548
1519.166005	169481.084242	36.351565
1520.560774	169745.979875	36.356583
1521.925968	169997.867670	36.361600
1523.265834	170256.433245	36.366618
1524.525204	170501.389942	36.371636
1525.801780	170746.421556	36.376653
1527.180105	170983.485130	36.381671
1528.629296	171230.762955	36.386688
1529.751945	171488.889175	36.391706
1531.586044	171745.204270	36.396724
1533.294923	172003.431021	36.401741
1534.574255	172263.719283	36.406759
1536.291167	172516.683718	36.411776
1537.431595	172779.090514	36.416794
1538.643089	173045.191926	36.421812
1540.333922	173317.231954	36.426829
1541.590875	173587.287668	36.431847
1543.402567	173861.659052	36.436864
1544.459086	174143.687675	36.441882
1546.231466	174419.210832	36.446900
1547.902834	174704.114220	36.451917
1549.121092	174994.977953	36.456935
1550.873340	175281.204586	36.461952
1552.353867	175582.864903	36.466970
1554.016799	175860.774867	36.471988
1555.456930	176153.400387	36.477005
1556.951900	176449.444658	36.482023
1558.573588	176732.086471	36.487040
1560.349590	177035.423202	36.492058
1561.976872	177319.615919	36.497076
1563.706150	177613.563326	36.502093
1565.325529	177909.179572	36.507111
1566.820585	178202.178728	36.512128
1568.804912	178491.219925	36.517146
1570.159162	178785.450791	36.522164
1571.760925	179084.249913	36.527181
1573.243197	179382.435745	36.532199
1575.076423	179661.638072	36.537216
1576.549137	179958.814450	36.542234
1578.543494	180245.975538	36.547252
1580.332629	180536.102029	36.552269
1581.827556	180836.440221	36.557287
1583.508569	181116.221764	36.562304
1585.157179	181392.863618	36.567322
1587.254255	181675.830836	36.572340
1589.033194	181961.692586	36.577357
1590.586859	182234.193117	36.582375
1592.749383	182504.644627	36.587392
1594.128753	182778.051714	36.592410
1595.835495	183056.458546	36.597428
1597.252717	183313.646964	36.602445
1598.558177	183600.787281	36.607463
1599.926956	183871.677742	36.612480
1601.494161	184161.850787	36.617498
1602.818339	184436.266567	36.622516
1604.513235	184722.235604	36.627533
1606.171843	185009.696844	36.632551
1608.251019	185287.982282	36.637568
1609.777234	185559.517735	36.642586
1611.270790	185827.037475	36.647604
1613.012128	186088.263554	36.652621
1614.031914	186361.609967	36.657639
1615.616008	186623.371646	36.662656
1617.241015	186896.003329	36.667674
1618.751961	187162.221055	36.672692
1620.341142	187440.026344	36.677709
1621.501658	187709.399167	36.682727
1623.467165	187971.704315	36.687744
1625.297016	188255.338987	36.692762
1626.677023	188537.092542	36.697780
1628.411787	188810.492085	36.702797
1629.802432	189096.105096	36.707815
1631.063999	189379.354549	36.712832
1633.014423	189667.242496	36.717850
1634.347430	189959.341939	36.722868
1636.236426	190235.174442	36.727885
1637.871727	190537.470659	36.732903
1639.690573	190823.178279	36.737920
1641.671608	191119.065203	36.742938
1642.703719	191416.475234	36.747956
1644.633310	191693.261423	36.752973
1645.954066	192005.997904	36.757991
1647.369238	192304.583531	36.763008
1649.450563	192598.762886	36.768026
1651.041604	192909.253924	36.773044
1652.649350	193210.035406	36.778061
1654.281592	193522.922391	36.783079
1656.246560	193809.906003	36.788096
1658.065760	194122.284772	36.793114
1659.366555	194429.391941	36.798132
1661.307206	194720.344388	36.803149
1663.012015	195036.795623	36.808167
1664.370007	195338.276760	36.813184
1666.392646	195656.445535	36.818202
1667.599223	195973.819350	36.823220
1669.552935	196268.852671	36.828237
1670.731707	196589.801157	36.833255
1672.849934	196892.833343	36.838272
1674.552735	197210.719777	36.843290
1676.484178	197517.250243	36.848308
1678.303845	197824.422175	36.853325
1679.836440	198141.249715	36.858343
1681.517795	198448.815321	36.863360
1683.586245	198755.318519	36.868378
1685.196335	199064.447498	36.873396
1687.625160	199362.494363	36.878413
1689.027153	199667.509307	36.883431
1691.408069	199953.559585	36.888448
1693.548003	200238.583424	36.893466
1695.088085	200530.050541	36.898484
1697.202338	200801.766361	36.903501
1699.177932	201069.989526	36.908519
1700.800170	201346.711127	36.913536
1702.349149	201606.779401	36.918554
1704.267188	201863.921592	36.923572
1705.985116	202107.260889	36.928589
1706.958027	202370.089819	36.933607
1708.892569	202612.927264	36.938624
1710.689533	202877.392133	36.943642
1711.770620	203133.352899	36.948660
1713.501391	203386.050929	36.953677
1715.330559	203648.546759	36.958695
1716.806090	203911.798105	36.963712
1718.254182	204183.014097	36.968730
1719.795422	204463.254684	36.973748
1721.525224	204733.793843	36.978765
1722.704666	205011.581110	36.983783
1724.505368	205303.717011	36.988800
1726.385951	205583.883740	36.993818
1727.863607	205880.884916	36.998836
1729.712590	206165.400877	37.003853
1730.918234	206470.902636	37.008871
1732.487206	206768.566572	37.013888
1734.021395	207074.730155	37.018906
1735.675195	207385.979539	37.023924
1737.630441	207694.719908	37.028941
1739.470125	208004.775062	37.033959
1740.781058	208319.130413	37.038976
1742.718471	208639.443369	37.043994
1744.443572	208964.971232	37.049012
1746.387772	209283.191799	37.054029
1748.217239	209600.213489	37.059047
1750.277538	209932.040745	37.064064
1752.102359	210245.600682	37.069082
1753.884302	210555.004949	37.074100
1756.053585	210866.418574	37.079117
1757.688485	211187.465483	37.084135
1759.585899	211507.113920	37.089152
1761.704068	211810.135888	37.094170
1763.020349	212136.100501	37.099188
1764.885215	212447.240046	37.104205
1766.728197	212762.294822	37.109223
1768.456607	213090.204702	37.114240
1769.853592	213398.084061	37.119258
1771.582737	213733.677984	37.124276
1773.527004	214046.869220	37.129293
1775.130312	214378.144357	37.134311
1776.626258	214710.707774	37.139328
1778.715833	215025.734130	37.144346
1780.289376	215366.693276	37.149364
1782.208472	215681.470412	37.154381
1784.642252	216004.267525	37.159399
1786.315694	216339.832415	37.164416
1788.441216	216660.485053	37.169434
1789.954013	216972.145754	37.174452
1791.973598	217294.468654	37.179469
1793.800731	217604.888785	37.184487
1795.739332	217930.960236	37.189504
1798.076339	218226.891458	37.194522
1799.696386	218533.945790	37.199540
1801.385759	218805.185450	37.204557
1803.454012	219091.462532	37.209575
1804.841009	219376.477614	37.214592
1806.504635	219663.151285	37.219610
1808.036892	219963.762832	37.224628
1809.720365	220257.838012	37.229645
1811.812090	220559.264657	37.234663
1813.257532	220858.116003	37.239680
1815.472809	221155.094126	37.244698
1817.313378	221465.033299	37.249716
1818.825139	221739.562370	37.254733
1820.624027	222110.241969	37.259751
1822.195420	222426.652623	37.264768
1823.980022	222733.647304	37.269786
1825.567114	223062.501565	37.274804
1827.472958	223370.419118	37.279821
1829.201733	223694.161808	37.284839
1831.118609	224019.120333	37.289856
1833.379145	224335.315001	37.294874
1835.349796	224652.471163	37.299892
1837.040095	224967.349366	37.304909
1839.408344	225279.505423	37.309927
1841.312731	225598.072552	37.314944
1843.486189	225901.830479	37.319962
1845.364120	226214.436142	37.324980
1847.480184	226516.719757	37.329997
1849.614684	226827.915600	37.335015
1851.166593	227133.287719	37.340032
1853.444856	227436.285373	37.345050
1854.863561	227742.137945	37.350068
1856.864979	228050.007033	37.355085
1858.938113	228358.399161	37.360103
1860.183855	228669.488765	37.365120
1862.432370	228972.293334	37.370138
1864.167972	229290.215318	37.375156
1866.854612	229581.015881	37.380173
1869.053591	229874.866244	37.385191
1871.055903	230176.748884	37.390208
1873.130331	230455.484189	37.395226
1875.081629	230753.059304	37.400244
1876.707521	231046.013901	37.405261
1878.686837	231326.798734	37.410279
1880.263148	231625.096496	37.415296
1882.437893	231916.112701	37.420314
1884.052494	232211.358525	37.425332
1886.193902	232494.356116	37.430349
1887.876244	232790.583494	37.435367
1889.528500	233084.403752	37.440384
1891.763491	233377.954633	37.445402
1893.131887	233675.910802	37.450420
1895.288260	233970.161680	37.455437
1897.115709	234253.823761	37.460455
1898.917161	234567.562393	37.465472
1901.112424	234851.701160	37.470490
1902.770967	235138.770527	37.475508
1904.739671	235406.336197	37.480525
1906.736493	235665.033989	37.485543
1908.149070	235951.839875	37.490560
1910.038106	236213.603979	37.495578
1911.674188	236494.965954	37.500596
1913.390999	236782.563990	37.505613
1915.324266	237071.017416	37.510631
1916.973310	237361.548641	37.515648
1918.900427	237642.562664	37.520666
1920.724797	237943.913030	37.525684
1922.355948	238249.815944	37.530701
1924.458020	238537.281293	37.535719
1926.127803	238854.609416	37.540736
1928.105012	239172.880227	37.545754
1930.123348	239468.819250	37.550772
1931.987741	239787.160475	37.555789
1933.994116	240098.825344	37.560807
1935.599726	240413.755000	37.565824
1937.750303	240727.913230	37.570842
1939.746520	241050.123131	37.575860
1941.931215	241369.484603	37.580877
1943.929029	241681.891580	37.585895
1945.646913	242017.864202	37.590912
1947.807729	242336.749390	37.595930
1949.612404	242658.003318	37.600948
1951.623802	242983.721105	37.605965
1953.414827	243320.752424	37.610983
1955.120302	243654.521553	37.616000
1956.898148	243991.632913	37.621018
1958.850562	244332.019503	37.626036
1960.763217	244672.159268	37.631053
1962.784286	245020.334689	37.636071
1964.742151	245365.091939	37.641088
1967.030227	245702.634650	37.646106
1969.061625	246047.178728	37.651124
1970.918788	246397.999910	37.656141
1972.941247	246737.466914	37.661159
1975.263739	247088.012749	37.666176
1977.538140	247422.234180	37.671194
1979.746199	247768.405416	37.676212
1981.725476	248107.984047	37.681229
1983.982654	248435.402966	37.686247
1985.834205	248778.229312	37.691264
1987.687099	249105.332777	37.696282
1989.834030	249450.145839	37.701300
1991.411447	249784.610013	37.706317
1993.648198	250118.284433	37.711335
1995.457691	250472.627971	37.716352
1997.403632	250799.440689	37.721370
1999.444683	251151.996220	37.726388
2001.259534	251492.116133	37.731405
2004.247026	251828.545233	37.736423
2006.160735	252170.073282	37.741440
2008.046838	252487.296804	37.746458
2010.489706	252791.960228	37.751476
2012.185941	253102.280231	37.756493
2014.049035	253403.937612	37.761511
2016.220090	253704.174911	37.766528
2018.280796	254001.839181	37.771546
2020.176916	254305.423302	37.776564
2021.570708	254628.393198	37.781581
2023.624004	254934.925397	37.786599
2025.496589	255269.302142	37.791616
2027.649367	255581.306405	37.796634
2029.891636	255896.396016	37.801652
2031.512258	256218.671958	37.806669
2033.738095	256545.653414	37.811687
2035.596417	256882.524384	37.816704
2037.887754	257204.669964	37.821722
2039.685959	257537.182226	37.826740
2041.527264	257878.121758	37.831757
2043.745138	258211.203461	37.836775
2045.120157	258556.180721	37.841792
2046.964339	258904.132349	37.846810
2049.081348	259257.172511	37.851828
2050.819330	259623.736701	37.856845
2052.851246	259988.400375	37.861863
2054.733129	260361.852287	37.866880
2057.134878	260726.483678	37.871898
2059.065061	261095.559624	37.876916
2060.947690	261479.275619	37.881933
2063.420361	261843.439902	37.886951
2065.303024	262225.962897	37.891968
2067.255740	262599.203166	37.896986
2069.584084	262971.749203	37.902004
2071.592625	263360.451877	37.907021
2073.886340	263734.375997	37.912039
2075.929288	264117.282154	37.917056
2078.321453	264492.080538	37.922074
2080.765797	264857.852910	37.927092
2082.871943	265238.260652	37.932109
2085.184171	265606.950609	37.937127
2087.841872	265961.385716	37.942144
2090.221059	266322.470107	37.947162
2092.469190	266670.416708	37.952180
2095.013795	267026.521774	37.957197
2097.021921	267377.148873	37.962215
2099.181080	267735.144594	37.967232
2101.239085	268083.401735	37.972250
2103.847954	268413.636995	37.977268
2106.122805	268771.462583	37.982285
2108.177282	269105.876068	37.987303
2110.007245	269444.999537	37.992320
2112.039457	269788.257232	37.997338
2114.186675	270121.640342	38.002356
2116.114140	270470.630696	38.007373
2118.526381	270806.842619	38.012391
2120.481675	271162.509904	38.017408
2122.334568	271484.051412	38.022426
2124.964551	271792.971298	38.027444
2126.830586	272118.448417	38.032461
2128.929483	272431.085369	38.037479
2130.845114	272732.751778	38.042496
2132.795597	273055.395924	38.047514
2134.731049	273363.994421	38.052532
2136.807116	273692.055072	38.057549
2138.533134	274022.482986	38.062567
2140.434105	274362.841320	38.067584
2142.253775	274700.189560	38.072602
2144.595092	275037.150241	38.077620
2146.295066	275391.588570	38.082637
2148.435772	275741.384378	38.087655
2150.845674	276093.982657	38.092672
2152.816237	276451.070772	38.097690
2154.832903	276805.230140	38.102708
2157.007198	277176.867401	38.107725
2158.970844	277543.965384	38.112743
2161.089920	277915.001565	38.117760
2163.309058	278281.372963	38.122778
2165.364296	278658.617488	38.127796
2167.282522	279044.114305	38.132813
2169.619580	279418.265468	38.137831
2171.820317	279793.378023	38.142848
2173.956834	280196.469668	38.147866
2176.369049	280581.963695	38.152884
2178.569862	280963.401113	38.157901
2180.506938	281350.672094	38.162919
2183.313231	281741.285254	38.167936
2185.854876	282118.501809	38.172954
2188.321266	282491.665533	38.177972
2190.716329	282877.948378	38.182989
2192.952871	283256.914548	38.188007
2195.464694	283628.977919	38.193024
2197.464403	284007.422190	38.198042
2199.908378	284379.267093	38.203060
2202.189599	284751.442325	38.208077
2204.640307	285115.105719	38.213095
2206.973616	285497.280841	38.218112
2208.969572	285866.070869	38.223130
2211.521653	286224.534937	38.228148
2212.938829	286598.115572	38.233165
2215.069053	286967.467467	38.238183
2217.701733	287340.321109	38.243200
2219.765492	287727.337756	38.248218
2222.370419	288095.495400	38.253236
2224.791180	288479.507789	38.258253
2226.741596	288845.837701	38.263271
2229.079810	289214.976185	38.268288
2231.016215	289587.632682	38.273306
2233.793035	289960.866707	38.278324
2235.967530	290332.493747	38.283341
2237.604790	290712.664532	38.288359
2240.205797	291081.708029	38.293376
2242.045243	291455.825241	38.298394
2244.580208	291798.738909	38.303412
2246.800062	292150.719945	38.308429
2249.133162	292490.667142	38.313447
2251.224652	292839.619209	38.318464
2253.048768	293185.310827	38.323482
2255.762841	293526.771037	38.328500
2257.651430	293884.339648	38.333517
2259.873853	294239.670147	38.338535
2261.932023	294591.850816	38.343552
2263.963538	294947.566021	38.348570
2266.313586	295315.499339	38.353588
2268.699689	295684.543961	38.358605
2270.948614	296044.439507	38.363623
2273.334713	296414.879868	38.368640
2275.184700	296796.327340	38.373658
2277.403036	297165.217910	38.378676
2279.661729	297556.226345	38.383693
2281.958387	297944.205106	38.388711
2284.294424	298316.376907	38.393728
2286.362810	298702.510467	38.398746
2288.845661	299086.977154	38.403764
2291.341679	299481.601506	38.408781
2293.361165	299870.686741	38.413799
2296.014963	300266.020856	38.418816
2298.087821	300666.958199	38.423834
2300.345880	301060.143176	38.428852
2302.683222	301454.025835	38.433869
2304.977219	301869.225947	38.438887
2307.372990	302267.948877	38.443904
2309.542558	302676.587609	38.448922
2311.880759	303080.702507	38.453940
2314.173669	303490.310057	38.458957
2316.582230	303901.218947	38.463975
2319.220806	304304.114347	38.468992
2321.759189	304713.095228	38.474010
2324.082510	305110.704117	38.479028
2326.503749	305519.599551	38.484045
2328.814086	305921.373793	38.489063
2331.672407	306314.652429	38.494080
2333.925249	306724.205842	38.499098
2336.283054	307124.368639	38.504116
2338.685347	307529.171348	38.509133
2341.087850	307932.474118	38.514151
2343.342475	308335.214819	38.519168
2345.416977	308738.668544	38.524186
2348.440701	309131.658150	38.529204
2350.706456	309530.887941	38.534221
2353.240036	309931.242316	38.539239
2355.888249	310324.490680	38.544256
2358.419623	310712.701737	38.549274
2360.323462	311107.843373	38.554292
2362.670272	311499.154324	38.559309
2365.253989	311900.916221	38.564327
2367.624261	312298.138655	38.569344
2369.638417	312684.113538	38.574362
2371.644509	313052.309087	38.579380
2374.277649	313423.299454	38.584397
2376.507184	313787.367844	38.589415
2378.742090	314157.758389	38.594432
2380.672150	314536.831445	38.599450
2382.533751	314925.768563	38.604468
2384.771502	315312.053953	38.609485
2386.689047	315695.213838	38.614503
2389.968261	316083.921831	38.619520
2391.829748	316490.784036	38.624538
2394.139966	316891.503329	38.629556
2396.913956	317288.998138	38.634573
2399.036392	317698.252142	38.639591
2401.674252	318103.054314	38.644608
2403.920479	318509.593062	38.649626
2406.447034	318912.250611	38.654644
2409.315250	319329.582708	38.659661
2411.577605	319749.472462	38.664679
2414.264197	320150.981759	38.669696
2416.281335	320570.576419	38.674714
2418.460372	320970.994237	38.679732
2421.797476	321396.623448	38.684749
2423.863605	321801.677602	38.689767
2426.185468	322223.882767	38.694784
2428.425033	322654.987639	38.699802
2430.934480	323076.193835	38.704820
2433.769805	323501.638242	38.709837
2435.820403	323923.649420	38.714855
2438.591507	324340.719074	38.719872
2441.021594	324778.512779	38.724890
2443.549930	325203.438417	38.729908
2446.349438	325628.471235	38.734925
2448.878490	326050.598815	38.739943
2451.688543	326467.981530	38.744960
2453.723559	326889.014778	38.749978
2456.549197	327311.139442	38.754996
2459.102477	327733.838273	38.760013
2461.577300	328165.867057	38.765031
2464.467231	328578.553216	38.770048
2466.650067	328993.329947	38.775066
2468.871139	329422.903167	38.780084
2471.563354	329837.213621	38.785101
2473.537214	330264.967406	38.790119
2476.126990	330687.415395	38.795136
2478.558796	331119.992644	38.800154
2481.147845	331547.463710	38.805172
2483.723880	331984.710734	38.810189
2485.796875	332420.460422	38.815207
2488.914420	332851.293436	38.820224
2491.179626	333279.160944	38.825242
2493.547107	333711.910423	38.830260
2496.440904	334138.047933	38.835277
2498.824885	334569.138927	38.840295
2501.435208	334986.961998	38.845312
2504.134953	335407.866167	38.850330
2506.760986	335807.069306	38.855348
2509.140871	336203.312844	38.860365
2511.265752	336593.703575	38.865383
2513.763844	336977.050219	38.870400
2516.090951	337373.879123	38.875418
2518.066908	337770.126476	38.880436
2521.026553	338175.077021	38.885453
2523.029804	338600.286102	38.890471
2525.508340	338992.942390	38.895488
2527.808634	339426.350887	38.900506
2530.118252	339854.473752	38.905524
2532.348218	340264.833207	38.910541
2534.696047	340707.898999	38.915559
2537.414703	341148.897084	38.920576
2539.695847	341595.369322	38.925594
2542.010075	342041.299886	38.930612
2545.011276	342490.088889	38.935629
2547.488242	342942.842139	38.940647
2550.085681	343391.789949	38.945664
2552.482412	343853.435125	38.950682
2554.991111	344307.239315	38.955700
2557.852875	344772.815011	38.960717
2560.250625	345243.182690	38.965735
2562.916512	345704.186734	38.970752
2565.890343	346168.260993	38.975770
2568.594871	346621.686036	38.980788
2571.428795	347076.635593	38.985805
2574.124906	347544.880752	38.990823
2576.666080	348001.570158	38.995840
2579.921440	348465.936389	39.000858
2582.206474	348912.758113	39.005876
2584.973783	349373.182991	39.010893
2587.440206	349839.388901	39.015911
2590.255878	350298.199009	39.020928
2592.814579	350758.315214	39.025946
2594.972281	351214.708591	39.030964
2598.335126	351679.360421	39.035981
2601.007623	352136.628998	39.040999
2603.540673	352589.549542	39.046016
2606.045024	353039.627668	39.051034
2608.623558	353510.962166	39.056052
2611.260990	353964.006565	39.061069
2613.592200	354434.584929	39.066087
2616.079228	354900.565257	39.071104
2618.648555	355371.122675	39.076122
2620.915557	355852.029149	39.081140
2624.147641	356335.240306	39.086157
2626.492323	356807.114432	39.091175
2628.863079	357286.594667	39.096192
2631.328863	357767.679664	39.101210
2633.950772	358255.029934	39.106228
2636.804001	358735.714116	39.111245
2639.274633	359218.484659	39.116263
2642.035408	359697.676458	39.121280
2644.654394	360170.363066	39.126298
2647.303335	360634.131669	39.131316
2649.853333	361083.546141	39.136333
2652.045736	361538.495090	39.141351
2654.610727	361997.339894	39.146368
2657.419321	362452.283917	39.151386
2659.731337	362921.946047	39.156404
2662.567011	363376.191494	39.161421
2665.027339	363852.165463	39.166439
2667.564205	364320.787957	39.171456
2670.242366	364795.626329	39.176474
2672.541396	365285.340566	39.181492
2675.055240	365758.342263	39.186509
2677.955714	366251.097585	39.191527
2680.504794	366747.430556	39.196544
2683.251764	367242.686186	39.201562
2686.049240	367734.299401	39.206580
2689.031371	368243.032298	39.211597
2691.880982	368736.173973	39.216615
2694.910146	369224.688598	39.221632
2698.394387	369707.187766	39.226650
2700.943696	370198.178029	39.231668
2703.999008	370688.828776	39.236685
2706.707352	371171.865675	39.241703
2709.351167	371655.490894	39.246720
2712.254955	372135.669269	39.251738
2714.896635	372625.221198	39.256756
2717.944730	373105.365588	39.261773
2720.814837	373605.501296	39.266791
2723.312850	374083.919954	39.271808
2726.151609	374571.489328	39.276826
2728.822842	375061.286805	39.281844
2731.716474	375541.858520	39.286861
2734.472975	376033.838123	39.291879
2737.433693	376518.421692	39.296896
2740.416883	376994.801000	39.301914
2742.986035	377494.733488	39.306932
2745.770620	377974.050164	39.311949
2748.243871	378467.541480	39.316967
2750.785910	378956.702851	39.321984
2753.648316	379447.075858	39.327002
2756.622623	379953.204585	39.332020
2759.214256	380445.967200	39.337037
2761.781800	380948.316629	39.342055
2764.536627	381452.025085	39.347072
2767.206142	381951.985977	39.352090
2769.706192	382453.260876	39.357108
2772.160694	382969.629805	39.362125
2775.001296	383489.405780	39.367143
2777.718633	384013.328799	39.372160
2780.486363	384530.692040	39.377178
2782.896835	385058.225567	39.382196
2786.032137	385565.775725	39.387213
2789.196279	386082.496454	39.392231
2792.250933	386606.354698	39.397248
2795.352115	387098.137575	39.402266
2797.987341	387592.676142	39.407284
2800.572543	388068.269237	39.412301
2803.103856	388547.719799	39.417319
2805.605978	389024.378643	39.422336
2808.692476	389500.608886	39.427354
2811.004465	390004.879218	39.432372
2813.630931	390500.647065	39.437389
2816.345315	390993.933946	39.442407
2819.159123	391493.690610	39.447424
2821.553981	391996.448303	39.452442
2824.492480	392515.368703	39.457460
2827.222567	393027.314942	39.462477
2829.703714	393542.792623	39.467495
2832.249095	394078.489105	39.472512
2835.125358	394606.669291	39.477530
2837.655580	395157.972277	39.482548
2840.714368	395682.429841	39.487565
2843.844445	396225.886217	39.492583
2846.566443	396772.111617	39.497600
2849.697178	397318.567660	39.502618
2852.149728	397875.568927	39.507636
2855.339775	398435.410722	39.512653
2858.288458	398989.145165	39.517671
2861.136404	399541.060636	39.522688
2864.697350	400092.194686	39.527706
2867.208398	400661.563178	39.532724
2870.104190	401209.791722	39.537741
2873.129944	401766.052742	39.542759
2876.203069	402326.682674	39.547776
2879.213390	402892.104326	39.552794
2882.119587	403453.907057	39.557812
2884.883212	404026.978490	39.562829
2888.053379	404574.877520	39.567847
2890.647549	405142.226085	39.572864
2893.598794	405710.978137	39.577882
2896.906411	406280.347819	39.582900
2899.264245	406850.364350	39.587917
2902.435807	407414.943636	39.592935
2904.967164	407992.465484	39.597952
2907.959403	408570.030207	39.602970
2910.628366	409156.075811	39.607988
2913.533299	409737.915837	39.613005
2916.622591	410324.632658	39.618023
2919.080470	410921.550964	39.623040
2922.289569	411506.730261	39.628058
2925.396485	412106.056672	39.633076
2928.173157	412697.338373	39.638093
2931.580511	413291.144166	39.643111
2934.562631	413873.727458	39.648128
2937.583290	414459.638304	39.653146
2940.216285	415054.671274	39.658164
2943.309759	415646.147327	39.663181
2946.402214	416236.141629	39.668199
2948.875123	416836.383527	39.673216
2952.158897	417420.266754	39.678234
2955.120919	417978.747839	39.683252
2957.905198	418520.572834	39.688269
2960.873948	419075.990520	39.693287
2963.985495	419621.391377	39.698304
2966.728530	420176.341624	39.703322
2969.283207	420731.310667	39.708340
2971.740686	421297.812265	39.713357
2974.881342	421854.237036	39.718375
2977.447768	422448.263685	39.723392
2980.437392	423034.407314	39.728410
2983.084221	423620.617994	39.733428
2986.066704	424212.133796	39.738445
2988.624376	424809.733337	39.743463
2991.397472	425421.877385	39.748480
2994.681431	426035.522639	39.753498
2997.491269	426658.247017	39.758516
3000.199521	427289.078956	39.763533
3003.852247	427895.935746	39.768551
3006.075849	428537.377618	39.773568
3009.621904	429159.572290	39.778586
3012.491265	429797.689816	39.783604
3015.605490	430441.679846	39.788621
3018.718680	431077.296060	39.793639
3021.543751	431734.419531	39.798656
3024.584887	432369.990132	39.803674
3027.630066	433024.715924	39.808692
3030.607464	433688.527402	39.813709
3033.955611	434343.678029	39.818727
3036.861229	435005.136752	39.823744
3039.962373	435673.688357	39.828762
3043.347926	436340.505973	39.833780
3046.583881	436991.908674	39.838797
3050.036786	437650.704463	39.843815
3053.122426	438313.693478	39.848832
3056.368408	438962.257850	39.853850
3059.637317	439622.777457	39.858868
3062.646973	440267.876192	39.863885
3066.712446	440916.031565	39.868903
3069.814192	441565.334886	39.873920
3072.534871	442213.212822	39.878938
3075.661176	442855.743612	39.883956
3078.897415	443502.999112	39.888973
3082.048860	444142.301922	39.893991
3085.373729	444787.686117	39.899008
3088.826010	445416.376799	39.904026
3091.879747	446058.731886	39.909044
3094.943541	446706.737739	39.914061
3098.366156	447328.548217	39.919079
3101.421618	447970.547234	39.924096
3104.431234	448594.009349	39.929114
3107.435914	449233.248281	39.934132
3110.536443	449866.481750	39.939149
3113.533067	450492.982561	39.944167
3116.538726	451141.785464	39.949184
3119.525709	451760.458840	39.954202
3122.405862	452357.926505	39.959220
3125.461758	452971.242081	39.964237
3128.302234	453557.904748	39.969255
3131.202693	454170.250966	39.974272
3133.993768	454775.310716	39.979290
3137.547312	455396.831691	39.984308
3140.278766	456006.826894	39.989325
3143.233857	456627.497526	39.994343
3145.961979	457257.851320	39.999360
3148.630617	457898.468076	40.004378
3151.866988	458527.086219	40.009396
3154.747111	459191.260720	40.014413
3158.253115	459840.390962	40.019431
3161.006033	460506.114153	40.024448
3164.017848	461168.184122	40.029466
3167.121638	461832.698234	40.034484
3169.971747	462506.388428	40.039501
3173.407100	463197.113661	40.044519
3176.588213	463890.942544	40.049536
3179.632153	464596.252901	40.054554
3183.170708	465285.326348	40.059572
3185.890149	465990.692399	40.064589
3189.470960	466677.741310	40.069607
3192.885820	467383.355485	40.074624
3195.920683	468086.679640	40.079642
3199.323990	468803.778780	40.084660
3202.677550	469508.218405	40.089677
3206.002725	470214.863671	40.094695
3208.855184	470938.701922	40.099712
3211.655637	471649.477058	40.104730
3215.200935	472371.334978	40.109748
3217.927134	473110.437515	40.114765
3221.308779	473829.185509	40.119783
3224.892199	474577.503388	40.124800
3228.000312	475317.880829	40.129818
3231.422909	476047.463747	40.134836
3234.505685	476794.362969	40.139853
3237.588085	477529.354896	40.144871
3241.250473	478275.955382	40.149888
3244.434669	479024.574756	40.154906
3248.219510	479752.296708	40.159924
3251.599391	480509.674249	40.164941
3255.156077	481233.081313	40.169959
3258.817973	481971.152007	40.174976
3261.736036	482709.716682	40.179994
3265.325066	483435.614306	40.185012
3268.386375	484169.754634	40.190029
3272.009755	484913.227596	40.195047
3275.139762	485646.896465	40.200064
3278.038612	486383.049645	40.205082
3281.564578	487106.292156	40.210100
3284.803194	487849.105429	40.215117
3288.454683	488572.171165	40.220135
3292.086896	489295.616407	40.225152
3295.406965	490011.252841	40.230170
3298.485319	490700.581116	40.235188
3301.881557	491373.567986	40.240205
3305.422620	492040.951225	40.245223
3308.453566	492712.987628	40.250240
3311.395535	493395.772145	40.255258
3314.708011	494071.401790	40.260276
3317.576451	494754.248586	40.265293
3320.709095	495436.573639	40.270311
3324.116893	496142.161445	40.275328
3326.874586	496846.259214	40.280346
3329.893085	497551.853866	40.285364
3332.471454	498283.243369	40.290381
3335.679792	499006.576120	40.295399
3339.468680	499730.595834	40.300416
3342.633791	500485.029064	40.305434
3345.757878	501230.500648	40.310452
3348.605966	501997.036942	40.315469
3351.614970	502767.048464	40.320487
3354.709343	503552.863873	40.325504
3357.422074	504336.281584	40.330522
3360.746930	505124.362776	40.335540
3363.570560	505954.380957	40.340557
3366.736456	506770.425852	40.345575
3370.076780	507594.126558	40.350592
3373.686240	508422.640735	40.355610
3377.474841	509257.394759	40.360628
3380.875962	510090.352819	40.365645
3384.404783	510941.264050	40.370663
3388.148345	511775.397680	40.375680
3391.844157	512626.551381	40.380698
3395.603644	513442.588274	40.385716
3399.285376	514277.264159	40.390733
3402.789356	515124.386984	40.395751
3405.945454	515949.326490	40.400768
3409.060301	516799.048986	40.405786
3412.972048	517642.599806	40.410804
3416.189628	518487.730454	40.415821
3419.933184	519336.012856	40.420839
3423.461371	520176.418233	40.425856
3427.164439	521029.612142	40.430874
3430.811700	521861.540894	40.435892
3434.490083	522711.473755	40.440909
3438.303967	523543.037853	40.445927
3441.661812	524373.572418	40.450944
3445.079363	525209.701225	40.455962
3449.317537	526032.448511	40.460980
3452.726061	526859.871909	40.465997
3456.558632	527677.254953	40.471015
3460.328668	528483.869463	40.476032
3463.999169	529284.964677	40.481050
3468.056997	530084.395561	40.486068
3471.768420	530880.010304	40.491085
3475.166790	531666.361426	40.496103
3478.615813	532449.641391	40.501120
3481.958782	533225.028453	40.506125
3485.703140	533933.705687	40.511130
3488.734111	534615.084449	40.516135
3491.456311	535239.807218	40.521140
3494.670110	535791.843529	40.526144
3497.272953	536285.618916	40.531149
3499.691286	536716.980477	40.536154
3501.913724	537112.653034	40.541159
3504.107316	537461.905889	40.546164
3505.900736	537722.630018	40.551168
3507.464614	537963.790684	40.556173
3509.670122	538141.970356	40.561178
3510.812471	538286.125973	40.566183
3512.018798	538395.070335	40.571188
3513.265345	538471.888554	40.576192
3514.213843	538511.382420	40.581197
3514.988191	538519.491822	40.586202
3516.220577	538510.206825	40.591207
3516.504886	538447.186422	40.596212
3517.475580	538366.684612	40.601216
3517.899923	538294.349079	40.606221
3518.531725	538171.932397	40.611226
3518.938824	538050.408796	40.616231
3519.124476	537910.283446	40.621236
3519.806578	537725.584301	40.626240
3519.786572	537559.074558	40.631245
3519.853415	537382.498735	40.636250
3520.378274	537186.353229	40.641255
3520.367546	536979.834994	40.646260
3520.607272	536768.223667	40.651264
3520.638445	536547.904495	40.656269
3521.072831	536317.315670	40.661274
3520.319077	536085.597904	40.666279
3520.395668	535848.997447	40.671284
3520.607863	535611.058631	40.676288
3520.786304	535362.867560	40.681293
3520.340257	535108.305556	40.686298
3519.908939	534887.126444	40.691303
3520.280302	534623.536888	40.696308
3520.382320	534361.702917	40.701312
3520.068149	534141.201821	40.706317
3520.066709	533859.219846	40.711322
3519.785604	533637.039288	40.716327
3519.247084	533374.178463	40.721332
3519.710562	533125.451770	40.726336
3519.095763	532873.102506	40.731341
3519.053736	532626.670604	40.736346
3518.879371	532387.076132	40.741351
3519.020825	532134.797468	40.746356
3518.662707	531896.083373	40.751360
3518.442369	531654.312416	40.756365
3518.039797	531419.033684	40.761370
3518.233692	531172.743640	40.766375
3517.899866	530950.078368	40.771380
3517.752174	530708.685533	40.776384
3517.593016	530475.173129	40.781389
3517.655581	530232.931305	40.786394
3517.465427	530009.674172	40.791399
3517.039694	529781.650755	40.796404
3516.761680	529550.063538	40.801408
3516.654524	529330.169214	40.806413
3516.664092	529103.987392	40.811418
3516.107781	528901.035808	40.816423
3515.601508	528687.461678	40.821428
3515.967610	528459.041340	40.826432
3515.479206	528264.914348	40.831437
3515.501968	528050.388922	40.836442
3515.070405	527853.367380	40.841447
3514.657956	527657.452180	40.846452
3514.751065	527456.906297	40.851456
3514.292065	527279.945319	40.856461
3514.222072	527086.344242	40.861466
3514.245380	526898.841310	40.866471
3513.776881	526716.973273	40.871476
3513.703539	526533.827741	40.876480
3513.520702	526359.946399	40.881485
3513.362661	526191.214472	40.886490
3513.227858	526015.755008	40.891495
3512.588537	525845.579235	40.896500
3512.782747	525673.804169	40.901504
3512.538252	525522.465656	40.906509
3512.116696	525364.734605	40.911514
3512.210011	525203.433056	40.916519
3511.876132	525058.422356	40.921524
3511.755272	524909.939588	40.926528
3511.502294	524763.548712	40.931533
3511.613529	524620.030631	40.936538
3511.357143	524488.296231	40.941543
3511.632923	524341.969593	40.946548
3511.333241	524191.031635	40.951552
3511.291634	524058.855396	40.956557
3511.231409	523915.964718	40.961562
3511.294397	523768.655536	40.966567
3510.679494	523638.082926	40.971572
3510.702177	523511.654683	40.976576
3510.041639	523398.021536	40.981581
3510.315775	523257.346948	40.986586
3510.161701	523131.348071	40.991591
3510.094785	523014.737003	40.996596
3510.124588	522886.381794	41.001600
3509.809646	522790.534539	41.006605
3509.555577	522669.855846	41.011610
3509.683377	522546.487154	41.016615
3509.612218	522435.989489	41.021620
3509.545876	522329.585148	41.026624
3508.903918	522226.102100	41.031629
3509.375550	522110.208277	41.036634
3509.325030	522017.802909	41.041639
3509.158585	521910.552219	41.046644
3508.978307	521804.010780	41.051648
3508.729783	521699.299428	41.056653
3508.640171	521603.156775	41.061658
3509.106930	521509.200649	41.066663
3508.742614	521404.000137	41.071668
3508.624512	521314.634844	41.076672
3508.065043	521222.558183	41.081677
3508.428219	521125.431128	41.086682
3508.443635	521040.391156	41.091687
3508.181167	520955.546334	41.096692
3508.307860	520855.371021	41.101696
3508.260282	520767.053305	41.106701
3507.723415	520692.311599	41.111706
3507.791638	520613.328093	41.116711
3507.701049	520529.111157	41.121716
3507.621265	520449.088508	41.126720
3507.784143	520367.813686	41.131725
3507.842901	520287.667233	41.136730
3507.788453	520202.482268	41.141735
3507.596004	520122.930873	41.146740
3507.719024	520041.610172	41.151744
3507.461748	519983.708283	41.156749
3507.083981	519900.797524	41.161754
3507.198995	519835.403794	41.166759
3506.922739	519767.341323	41.171764
3506.942044	519680.524022	41.176768
3506.467483	519632.261962	41.181773
3507.123602	519561.472622	41.186778
3506.997921	519496.570644	41.191783
3506.836129	519438.601178	41.196788
3506.867722	519359.111797	41.201792
3506.489741	519304.058099	41.206797
3506.386079	519244.713564	41.211802
3506.322342	519195.121212	41.216807
3506.426991	519141.001956	41.221812
3506.737442	519069.961756	41.226816
3506.355995	519014.149181	41.231821
3506.585552	518954.295861	41.236826
3506.509757	518890.698271	41.241831
3506.089578	518841.363444	41.246836
3506.646919	518775.946160	41.251840
3506.411872	518718.541945	41.256845
3506.252710	518674.626353	41.261850
3506.005235	518619.600305	41.266855
3506.176931	518569.260950	41.271860
3506.250560	518503.919037	41.276864
3506.060715	518461.878646	41.281869
3506.570900	518411.586445	41.286874
3506.227949	518350.607843	41.291879
3506.217675	518293.419453	41.296884
3506.193048	518245.638441	41.301888
3506.055041	518191.503855	41.306893
3505.806955	518133.290603	41.311898
3505.905278	518085.590829	41.316903
3505.768294	518046.676157	41.321908
3506.002777	517981.256189	41.326912
3505.523627	517937.743178	41.331917
3505.534683	517902.344466	41.336922
3505.745601	517862.818138	41.341927
3505.365051	517822.424414	41.346932
3505.807113	517770.927415	41.351936
3505.787996	517728.403066	41.356941
3505.669177	517680.635308	41.361946
3505.844749	517640.557790	41.366951
3505.669484	517608.070271	41.371956
3506.043353	517547.885643	41.376960
3505.833595	517505.643694	41.381965
3505.626951	517461.530109	41.386970
3505.886369	517402.627256	41.391975
3505.498013	517358.238703	41.396980
3505.647270	517318.164565	41.401984
3505.730721	517278.758129	41.406989
3505.768887	517220.951550	41.411994
3505.934827	517179.964195	41.416999
3505.659274	517141.221005	41.422004
3505.719593	517090.035075	41.427008
3505.570218	517044.899937	41.432013
3505.265479	516996.906744	41.437018
3505.783131	516959.656005	41.442023
3505.358651	516922.857504	41.447028
3505.754830	516879.810213	41.452032
3505.424243	516831.112642	41.457037
3505.709756	516790.257139	41.462042
3505.543706	516756.148236	41.467047
3505.206095	516719.992976	41.472052
3505.356618	516652.052497	41.477056
3505.372608	516632.276729	41.482061
3505.552194	516585.166651	41.487066
3505.786385	516552.460639	41.492071
3505.750296	516510.340424	41.497076
3505.171255	516469.469060	41.502080
3505.464153	516428.813789	41.507085
3505.382942	516396.207891	41.512090
3505.178516	516352.849587	41.517095
3505.109616	516316.145260	41.522100
3505.464479	516267.034271	41.527104
3504.967600	516245.012781	41.532109
3505.118559	516202.356501	41.537114
3505.376321	516163.678461	41.542119
3505.431362	516136.310057	41.547124
3505.088253	516096.462512	41.552128
3505.138968	516049.067850	41.557133
3505.098846	516020.652267	41.562138
3505.355143	515976.916732	41.567143
3504.932227	515948.510953	41.572148
3505.050202	515913.748557	41.577152
3504.673592	515881.946938	41.582157
3504.859573	515852.989601	41.587162
3505.032504	515821.657322	41.592167
3504.879401	515792.298309	41.597172
3505.260795	515753.296337	41.602176
3504.823016	515721.150062	41.607181
3504.941611	515676.272305	41.612186
3504.743302	515655.922361	41.617191
3504.621622	515631.160335	41.622196
3504.913992	515601.427137	41.627200
3504.734625	515572.628205	41.632205
3504.654643	515526.769946	41.637210
3504.712848	515495.556336	41.642215
3504.409497	515490.395139	41.647220
3504.829972	515453.560996	41.652224
3504.505537	515437.630713	41.657229
3504.773906	515396.167612	41.662234
3504.923472	515367.012890	41.667239
3504.513932	515347.454578	41.672244
3505.191682	515314.423165	41.677248
3505.057023	515282.430438	41.682253
3504.870986	515247.917007	41.687258
3505.104104	515222.845425	41.692263
3504.755599	515191.493226	41.697268
3504.980364	515155.346839	41.702272
3504.950696	515142.100766	41.707277
3504.972295	515100.220754	41.712282
3505.000585	515070.983533	41.717287
3504.741722	515043.662952	41.722292
3505.175913	515003.133612	41.727296
3504.785467	514979.323467	41.732301
3504.585122	514959.529333	41.737306
3504.797444	514917.871602	41.742311
3504.405106	514898.512351	41.747316
3504.475934	514854.499738	41.752320
3504.421090	514845.859866	41.757325
3504.684704	514813.499838	41.762330
3504.672597	514789.781357	41.767335
3504.607873	514771.432289	41.772340
3505.029376	514735.253904	41.777344
3504.887661	514706.042915	41.782349
3504.811122	514671.106375	41.787354
3504.808602	514640.457116	41.792359
3504.561029	514615.966371	41.797364
3504.494180	514581.533883	41.802368
3504.740593	514562.579063	41.807373
3504.585736	514530.183473	41.812378
3504.835256	514496.712359	41.817383
3504.743112	514474.978606	41.822388
3504.758422	514448.321809	41.827392
3504.709416	514423.243044	41.832397
3504.808920	514400.012150	41.837402
3504.964144	514372.726185	41.842407
3504.882545	514342.291193	41.847412
3505.004795	514301.050792	41.852416
3504.728943	514289.663766	41.857421
3504.939605	514249.572563	41.862426
3505.019786	514212.587168	41.867431
3504.528179	514193.343947	41.872436
3504.789326	514142.572455	41.877440
3504.698883	514130.599653	41.882445
3504.866387	514089.452738	41.887450
3504.980172	514070.214853	41.892455
3504.299723	514038.407170	41.897460
3504.729260	514013.151004	41.902464
3504.712841	513984.576484	41.907469
3504.646852	513959.600870	41.912474
3504.596788	513924.102221	41.917479
3504.472810	513907.885903	41.922484
3504.778310	513874.708181	41.927488
3505.011851	513843.615526	41.932493
3504.575615	513824.009073	41.937498
3504.654506	513793.092506	41.942503
3504.475942	513774.153385	41.947508
3504.713494	513732.235831	41.952512
3504.518127	513723.567011	41.957517
3504.424677	513694.953595	41.962522
3504.486197	513673.902639	41.967527
3504.193715	513649.114101	41.972532
3504.742244	513634.359214	41.977536
3504.473859	513603.750085	41.982541
3504.601205	513575.354471	41.987546
3504.443212	513547.712031	41.992551
3504.212792	513522.862917	41.997556
3504.312131	513501.148223	42.002560
3504.555856	513473.290429	42.007565
3504.829307	513449.120280	42.012570
3504.621532	513420.018659	42.017575
3504.243364	513395.647936	42.022580
3504.402282	513372.254492	42.027584
3504.656072	513354.460509	42.032589
3504.867332	513322.004729	42.037594
3504.591626	513299.640915	42.042599
3504.502911	513268.598132	42.047604
3504.444811	513246.857413	42.052608
3504.316468	513205.299867	42.057613
3504.422517	513203.158722	42.062618
3504.367707	513164.725501	42.067623
3504.648386	513142.577034	42.072628
3504.437029	513130.926121	42.077632
3504.453847	513108.313494	42.082637
3504.388667	513078.632349	42.087642
3504.547310	513056.604219	42.092647
3504.317005	513040.757944	42.097652
3504.690649	513009.692193	42.102656
3504.831735	512990.853418	42.107661
3504.184692	512960.960535	42.112666
3504.168864	512939.718561	42.117671
3504.663006	512909.594643	42.122676
3504.561082	512889.074364	42.127680
3504.334290	512865.690597	42.132685
3504.225457	512845.828929	42.137690
3504.689562	512820.717266	42.142695
3504.286718	512796.400159	42.147700
3504.354202	512773.273251	42.152704
3504.321984	512753.449948	42.157709
3504.478703	512740.981851	42.162714
3504.761322	512707.350208	42.167719
3504.644620	512688.653006	42.172724
3504.593376	512660.638161	42.177728
3504.482651	512632.885586	42.182733
3504.587076	512607.577539	42.187738
3504.677809	512583.080950	42.192743
3504.426418	512550.140394	42.197748
3504.996121	512532.093284	42.202752
3504.749989	512493.081774	42.207757
3504.343096	512473.317360	42.212762
3504.735587	512441.539418	42.217767
3504.475486	512413.253672	42.222772
3504.470550	512390.694108	42.227776
3504.413554	512369.812011	42.232781
3504.374043	512349.331797	42.237786
3504.622041	512327.339181	42.242791
3504.271005	512310.904295	42.247796
3504.483937	512282.240063	42.252800
3504.367552	512259.900276	42.257805
3504.157879	512237.474035	42.262810
3504.469344	512204.747355	42.267815
3504.019073	512188.378617	42.272820
3504.445940	512174.754550	42.277824
3504.348978	512152.411552	42.282829
3504.260811	512124.654579	42.287834
3504.382315	512106.374347	42.292839
3504.487235	512086.326251	42.297844
3504.473150	512057.697519	42.302848
3504.480508	512027.901897	42.307853
3504.062898	512023.111781	42.312858
3504.377683	511980.924758	42.317863
3504.552476	511976.192756	42.322868
3504.292620	511936.777454	42.327872
3504.144447	511925.267479	42.332877
3504.349601	511894.782754	42.337882
3504.858879	511879.374940	42.342887
3504.660303	511862.915522	42.347892
3504.068823	511824.462908	42.352896
3504.533104	511804.458854	42.357901
3504.327277	511786.331183	42.362906
3504.645880	511761.139780	42.367911
3504.778148	511733.195571	42.372916
3504.537880	511705.866639	42.377920
3504.537653	511674.908121	42.382925
3504.410005	511662.990036	42.387930
3504.196343	511629.839384	42.392935
3504.047577	511603.406376	42.397940
3504.319662	511587.631096	42.402944
3504.639646	511568.256606	42.407949
3504.622619	511553.892819	42.412954
3504.406533	511517.454219	42.417959
3504.313308	511499.257858	42.422964
3503.944717	511469.874781	42.427968
3504.195291	511457.896775	42.432973
3503.955721	511434.260119	42.437978
3504.298894	511412.655972	42.442983
3503.732336	511407.636287	42.447988
3504.459414	511372.616501	42.452992
3504.659242	511365.705138	42.457997
3504.301539	511343.554046	42.463002
3504.135412	511311.154064	42.468007
3504.169760	511292.987908	42.473012
3504.232978	511272.844269	42.478016
3504.422542	511256.171157	42.483021
3504.134246	511237.701824	42.488026
3504.068241	511208.321058	42.493031
3503.852864	511202.132887	42.498036
3504.328431	511183.694530	42.503040
3504.262070	511160.232467	42.508045
3503.979968	511149.147833	42.513050
3503.984439	511123.094559	42.518055
3504.049961	511115.597270	42.523060
3504.238997	511096.242940	42.528064
3504.239992	511069.127791	42.533069
3504.095616	511065.154210	42.538074
3504.352542	511023.935129	42.543079
3504.223004	511005.389865	42.548084
3504.274926	510980.846513	42.553088
3504.297759	510974.114729	42.558093
3504.316468	510953.067163	42.563098
3504.450009	510932.052009	42.568103
3504.296737	510913.712748	42.573108
3504.276069	510883.666611	42.578112
3504.135571	510866.539400	42.583117
3504.102680	510849.951638	42.588122
3504.361081	510836.555484	42.593127
3504.032224	510808.986169	42.598132
3503.912399	510802.934516	42.603136
3504.097804	510771.995607	42.608141
3504.186313	510760.042726	42.613146
3504.194844	510733.532917	42.618151
3503.878703	510726.247544	42.623156
3504.033028	510705.380593	42.628160
3504.020379	510690.711853	42.633165
3504.022950	510672.600647	42.638170
3504.093821	510654.782161	42.643175
3504.038669	510641.233054	42.648180
3503.949742	510629.814016	42.653184
3504.272203	510601.939071	42.658189
3504.205785	510597.548346	42.663194
3504.451308	510591.641232	42.668199
3503.839420	510578.736547	42.673204
3504.014064	510561.255687	42.678208
3504.292186	510542.341953	42.683213
3504.066526	510536.863415	42.688218
3504.367861	510511.571718	42.693223
3504.583171	510493.224341	42.698228
3504.447454	510462.841520	42.703232
3504.273830	510438.636573	42.708237
3504.070253	510422.480090	42.713242
3503.984850	510405.090760	42.718247
3504.036524	510385.352616	42.723252
3504.171183	510363.274201	42.728256
3504.388785	510350.946502	42.733261
3503.686915	510329.152024	42.738266
3503.957880	510315.702887	42.743271
3504.048859	510296.211379	42.748276
3503.950458	510280.796989	42.753280
3503.750887	510273.442408	42.758285
3503.698852	510263.079687	42.763290
3503.882577	510229.307012	42.768295
3504.011230	510226.453658	42.773300
3504.269259	510219.633815	42.778304
3504.371180	510178.184242	42.783309
3504.217541	510177.803836	42.788314
3504.320277	510146.826271	42.793319
3504.102802	510135.275448	42.798324
3503.974902	510116.779549	42.803329
3503.748436	510098.602752	42.808333
3503.985318	510088.700169	42.813338
3504.186387	510056.492723	42.818343
3503.429444	510056.764164	42.823348
3503.892513	510044.599813	42.828353
3504.014770	510027.076096	42.833357
3503.866892	510017.335464	42.838362
3504.335239	509998.441656	42.843367
3503.861653	509969.629087	42.848372
3503.711289	509968.084564	42.853377
3504.148563	509957.037231	42.858381
3504.198705	509931.076103	42.863386
3504.246474	509921.051539	42.868391
3503.987307	509893.570914	42.873396
3503.706242	509879.652179	42.878401
3504.554123	509866.617422	42.883405
3503.861261	509845.731546	42.888410
3504.069051	509826.119858	42.893415
3504.327216	509806.753144	42.898420
3504.355974	509784.083622	42.903425
3504.284674	509770.637560	42.908429
3504.367576	509753.575109	42.913434
3504.238028	509728.400949	42.918439
3504.284087	509705.779181	42.923444
3504.126880	509681.064649	42.928449
3504.617872	509656.652371	42.933453
3503.910298	509633.694290	42.938458
3504.099343	509614.641836	42.943463
3504.271400	509604.243298	42.948468
3504.342541	509591.078136	42.953473
3504.215601	509569.545965	42.958477
3504.089250	509556.614359	42.963482
3504.219390	509533.473152	42.968487
3503.973423	509507.507590	42.973492
3504.093692	509489.831862	42.978497
3504.329720	509474.262705	42.983501
3504.070537	509446.174255	42.988506
3504.623947	509438.244973	42.993511
3504.434903	509411.460788	42.998516
3504.108189	509388.239813	43.003521
3503.829705	509370.728170	43.008525
3503.891495	509349.267079	43.013530
3503.955227	509337.519494	43.018535
3503.845481	509319.677573	43.023540
3503.933664	509304.738745	43.028545
3504.166940	509280.366664	43.033549
3504.122653	509278.198197	43.038554
3504.168980	509257.700704	43.043559
3503.892932	509231.435920	43.048564
3503.948204	509224.597135	43.053569
3504.068891	509189.516953	43.058573
3504.143427	509183.231634	43.063578
3504.248471	509156.349977	43.068583
3503.989951	509155.733156	43.073588
3503.812113	509135.068573	43.078593
3504.078113	509115.851623	43.083597
3503.811235	509103.852569	43.088602
3503.881478	509079.708346	43.093607
3504.049669	509075.482525	43.098612
3503.837853	509047.132966	43.103617
3504.001122	509039.922883	43.108621
3504.288534	509023.383916	43.113626
3503.882935	508994.710741	43.118631
3504.260888	508984.633445	43.123636
3504.188439	508958.690223	43.128641
3504.330431	508951.129307	43.133645
3504.299440	508917.742146	43.138650
3504.305456	508907.065866	43.143655
3504.215342	508887.955539	43.148660
3503.839430	508875.366428	43.153665
3503.991034	508860.518378	43.158669
3503.408063	508838.298451	43.163674
3503.807650	508825.181981	43.168679
3503.731104	508832.024357	43.173684
3503.654940	508810.129048	43.178689
3504.106833	508782.939017	43.183693
3503.798408	508782.633636	43.188698
3503.466494	508761.284631	43.193703
3503.826575	508748.224941	43.198708
3503.662221	508726.748222	43.203713
3503.991827	508732.969904	43.208717
3503.253481	508723.423048	43.213722
3503.970873	508694.521290	43.218727
3503.941690	508693.514042	43.223732
3503.631720	508693.967826	43.228737
3503.833776	508663.427242	43.233741
3503.452046	508660.603701	43.238746
3503.523315	508654.521084	43.243751
3503.714597	508653.276610	43.248756
3503.390552	508632.027390	43.253761
3503.860960	508613.485904	43.258765
3503.611931	508613.677083	43.263770
3504.027910	508604.200696	43.268775
3503.746246	508589.926842	43.273780
3503.607303	508567.282219	43.278785
3503.705054	508560.942409	43.283789
3503.512522	508562.541324	43.288794
3504.074786	508536.446555	43.293799
3504.055323	508527.038946	43.298804
3503.958402	508509.700110	43.303809
3504.088781	508476.387780	43.308813
3503.771335	508475.830842	43.313818
3503.878520	508455.828731	43.318823
3503.888468	508436.347920	43.323828
3504.021272	508432.582895	43.328833
3503.842147	508408.173569	43.333837
3503.898448	508383.322235	43.338842
3504.283921	508379.567860	43.343847
3503.866122	508358.940269	43.348852
3503.640034	508340.508571	43.353857
3503.903758	508334.547212	43.358861
3503.725536	508335.030778	43.363866
3503.902380	508305.353674	43.368871
3504.213525	508289.872767	43.373876
3503.833499	508285.733399	43.378881
3504.177309	508250.818425	43.383885
3504.231135	508244.586633	43.388890
3503.879939	508219.546486	43.393895
3503.945193	508209.922931	43.398900
3503.672477	508196.962838	43.403905
3503.828098	508177.610500	43.408909
3503.524975	508190.155726	43.413914
3503.549442	508172.089018	43.418919
3503.475966	508164.157042	43.423924
3503.531655	508156.052859	43.428929
3504.088449	508138.559734	43.433933
3503.704346	508131.739362	43.438938
3503.842857	508109.202076	43.443943
3503.764321	508085.838922	43.448948
3503.739255	508080.176102	43.453953
3503.914919	508068.106381	43.458957
3503.601877	508046.955894	43.463962
3503.511553	508045.249917	43.468967
3503.575420	508037.093789	43.473972
3503.571358	508038.207594	43.478977
3503.697620	508030.749955	43.483981
3503.511161	508006.695398	43.488986
3504.075476	507995.525540	43.493991
3503.607271	507998.432997	43.498996
3503.668680	507983.244271	43.504001
3503.800791	507955.850496	43.509005
3503.762268	507953.174981	43.514010
3503.675719	507949.545713	43.519015
3503.858050	507938.132609	43.524020
3503.693912	507913.163647	43.529025
3503.691250	507903.297670	43.534029
3503.719390	507902.129524	43.539034
3503.534597	507884.095588	43.544039
3503.738845	507864.785812	43.549044
3503.814737	507867.202519	43.554049
3503.953060	507856.656468	43.559053
3504.152396	507835.930714	43.564058
3503.722095	507821.274935	43.569063
3503.949737	507812.080870	43.574068
3503.473254	507790.196938	43.579073
3503.537217	507769.239512	43.584077
3503.541876	507768.530446	43.589082
3503.530043	507765.597696	43.594087
3503.471033	507749.668834	43.599092
3503.480115	507737.827602	43.604097
3503.873718	507721.118812	43.609101
3503.972859	507724.695611	43.614106
3503.770831	507706.512420	43.619111
3503.802061	507700.031014	43.624116
3503.673883	507688.919810	43.629121
3504.088514	507674.838735	43.634125
3503.907140	507665.861030	43.639130
3503.927204	507643.392455	43.644135
3503.934791	507634.131879	43.649140
3503.687861	507610.895894	43.654145
3503.679911	507601.131776	43.659149
3503.683801	507601.586578	43.664154
3503.645203	507574.978150	43.669159
3503.939224	507565.824061	43.674164
3503.941834	507560.308491	43.679169
3503.973084	507538.293395	43.684173
3503.753506	507522.339103	43.689178
3503.900039	507505.365566	43.694183
3503.812604	507497.384892	43.699188
3503.744432	507489.957751	43.704193
3503.998686	507471.449206	43.709197
3503.639592	507477.678996	43.714202
3503.852308	507449.968091	43.719207
3504.059781	507430.201935	43.724212
3503.799212	507415.923774	43.729217
3503.880193	507398.606303	43.734221
3503.642415	507389.030186	43.739226
3503.664113	507381.487597	43.744231
3503.772323	507379.547781	43.749236
3503.685643	507354.919961	43.754241
3503.971616	507336.760451	43.759245
3503.948659	507341.823990	43.764250
3503.752252	507316.707471	43.769255
3503.819500	507301.213631	43.774260
3503.868074	507300.092814	43.779265
3503.875118	507263.812307	43.784269
3503.795063	507265.848954	43.789274
3503.577272	507246.554593	43.794279
3503.454494	507243.082700	43.799284
3503.567258	507218.423164	43.804289
3503.750458	507208.223821	43.809293
3503.382667	507212.127519	43.814298
3503.521642	507199.961795	43.819303
3503.334136	507214.513419	43.824308
3503.685131	507187.691024	43.829313
3503.458853	507166.070352	43.834317
3503.460172	507172.951677	43.839322
3503.504658	507162.521234	43.844327
3503.946709	507161.945411	43.849332
3503.592938	507145.556587	43.854337
3503.712880	507126.158114	43.859341
3503.777013	507111.271790	43.864346
3503.643159	507112.557966	43.869351
3503.515395	507088.796451	43.874356
3503.532314	507077.105327	43.879361
3504.069679	507071.960479	43.884365
3503.988218	507068.532620	43.889370
3503.747462	507045.750296	43.894375
3503.822931	507032.987296	43.899380
3503.570062	507035.203082	43.904385
3504.058652	507007.144271	43.909389
3503.803497	506992.257707	43.914394
3503.833398	506984.308851	43.919399
3503.633861	506966.782286	43.924404
3503.677703	506953.214629	43.929409
3503.912845	506939.616726	43.934413
3503.779243	506946.215866	43.939418
3503.940086	506926.861306	43.944423
3503.978327	506903.427500	43.949428
3503.853594	506899.753447	43.954433
3503.872820	506865.898985	43.959437
3503.743431	506855.040437	43.964442
3503.534195	506861.702162	43.969447
3503.351912	506851.256773	43.974452
3503.511328	506839.441767	43.979457
3503.504942	506810.853666	43.984461
3503.641479	506803.646878	43.989466
3503.818961	506809.387298	43.994471
3503.610916	506803.803580	43.999476
3503.276677	506787.563131	44.004481
3503.998669	506764.021071	44.009485
3503.512098	506771.030266	44.014490
3503.912103	506764.237225	44.019495
3503.607776	506742.223556	44.024500
3503.958537	506740.751339	44.029505
3503.823174	506724.074595	44.034509
3503.211961	506709.851270	44.039514
3503.514739	506687.741579	44.044519
3503.820555	506682.228409	44.049524
3503.900230	506681.760445	44.054529
3503.681984	506672.332646	44.059533
3503.909555	506651.854018	44.064538
3503.790679	506649.747610	44.069543
3503.970443	506632.413762	44.074548
3503.683925	506604.932215	44.079553
3503.857962	506599.439846	44.084557
3503.720365	506598.803816	44.089562
3503.571092	506575.044998	44.094567
3503.695397	506562.324535	44.099572
3503.882696	506548.126676	44.104577
3504.035589	506538.285937	44.109581
3503.571759	506523.178947	44.114586
3503.847032	506508.258735	44.119591
3503.880753	506510.024482	44.124596
3503.869801	506489.937570	44.129601
3503.776784	506473.962310	44.134605
3503.557249	506455.729972	44.139610
3503.829978	506455.737503	44.144615
3503.985245	506424.896761	44.149620
3503.805008	506411.667705	44.154625
3503.719271	506412.187305	44.159629
3503.606724	506401.123406	44.164634
3503.766696	506375.493784	44.169639
3503.755331	506373.117342	44.174644
3503.821546	506365.516675	44.179649
3504.019000	506335.934146	44.184653
3504.014487	506337.098733	44.189658
3503.698025	506320.500826	44.194663
3503.952752	506293.995879	44.199668
3503.805159	506275.600176	44.204673
3503.994777	506274.659409	44.209677
3504.185551	506256.463216	44.214682
3503.673815	506248.447823	44.219687
3503.741940	506229.410753	44.224692
3503.628416	506216.980637	44.229697
3503.899360	506197.860876	44.234701
3503.506949	506190.029005	44.239706
3504.038876	506190.906409	44.244711
3504.089631	506163.067244	44.249716
3503.941908	506156.259331	44.254721
3503.933956	506137.639003	44.259725
3503.692491	506113.084488	44.264730
3503.483508	506093.736850	44.269735
3503.794849	506104.212971	44.274740
3503.836561	506090.391966	44.279745
3504.076003	506068.696319	44.284749
3503.701704	506066.326594	44.289754
3503.507424	506050.012732	44.294759
3503.899425	506015.794083	44.299764
3503.621532	506028.083867	44.304769
3503.679141	506012.641005	44.309773
3503.846069	506011.906220	44.314778
3503.687782	505985.668493	44.319783
3503.692188	505977.115974	44.324788
3503.841918	505979.976699	44.329793
3504.124436	505945.218586	44.334797
3504.024195	505937.340423	44.339802
3503.854201	505930.738353	44.344807
3504.087107	505896.797631	44.349812
3503.779906	505896.542601	44.354817
3503.705487	505858.399727	44.359821
3503.606356	505844.094756	44.364826
3503.476696	505842.192366	44.369831
3503.657363	505832.346840	44.374836
3503.588596	505843.541035	44.379841
3503.658531	505813.218728	44.384845
3503.696368	505805.268079	44.389850
3503.470482	505803.937528	44.394855
3503.713086	505800.863026	44.399860
3503.680966	505780.576229	44.404865
3503.556322	505760.000412	44.409869
3503.698648	505755.727271	44.414874
3503.969236	505752.648338	44.419879
3503.941053	505737.471809	44.424884
3504.035808	505713.521435	44.429889
3503.877183	505701.401700	44.434893
3503.752135	505672.577467	44.439898
3503.721331	505667.066577	44.444903
3503.838537	505661.937121	44.449908
3503.814959	505655.919049	44.454913
3503.778828	505627.789141	44.459917
3503.974373	505617.232690	44.464922
3503.710561	505612.618874	44.469927
3503.993780	505578.062334	44.474932
3503.671990	505595.166727	44.479937
3503.659278	505580.594863	44.484941
3503.533571	505551.821139	44.489946
3503.614413	505544.521426	44.494951
3503.636128	505538.850382	44.499956
3503.824385	505542.818379	44.504961
3503.864522	505513.664153	44.509965
3503.893127	505495.340985	44.514970
3503.840134	505486.746694	44.519975
3504.104364	505475.268427	44.524980
3503.869627	505456.025360	44.529985
3503.761416	505445.668627	44.534989
3503.676016	505420.683636	44.539994
3503.472314	505404.724889	44.544999
3503.719279	505403.268969	44.550004
3503.430972	505390.208030	44.555009
3503.556385	505399.853686	44.560013
3503.371053	505386.118612	44.565018
3503.601224	505376.568632	44.570023
3503.707879	505368.758721	44.575028
3503.552850	505369.542326	44.580033
3503.515670	505358.820084	44.585037
3503.694959	505346.950322	44.590042
3503.624947	505322.063967	44.595047
3504.007675	505319.928722	44.600052
3503.518939	505307.759678	44.605057
3503.557734	505286.651425	44.610061
3503.177755	505275.173635	44.615066
3503.623845	505277.329775	44.620071
3503.601346	505277.586390	44.625076
3503.502177	505274.413999	44.630081
3504.021752	505261.731326	44.635085
3503.754750	505231.258842	44.640090
3503.656399	505228.744178	44.645095
3503.597592	505216.304700	44.650100
3503.541301	505209.228940	44.655105
3503.653399	505186.843857	44.660109
3503.681904	505169.937305	44.665114
3503.488009	505154.938276	44.670119
3503.912732	505124.609305	44.675124
3503.432061	505124.584100	44.680129
3503.779673	505100.036265	44.685133
3503.717803	505098.882157	44.690138
3503.997283	505078.848929	44.695143
3503.858631	505062.727772	44.700148
3503.681647	505056.278291	44.705153
3503.629138	505042.521954	44.710157
3503.472610	505025.644507	44.715162
3503.291424	505018.284777	44.720167
3503.772409	504994.778430	44.725172
3503.507994	505017.339719	44.730177
3503.617160	504997.181499	44.735181
3503.847716	504987.681853	44.740186
3503.723066	504974.392314	44.745191
3503.785528	504960.769559	44.750196
3503.654815	504953.503036	44.755201
3503.920151	504928.006456	44.760205
3503.729808	504916.802092	44.765210
3503.633155	504918.993452	44.770215
3503.697511	504892.061017	44.775220
3503.536539	504879.384417	44.780225
3503.714426	504874.700594	44.785229
3503.698593	504875.614038	44.790234
3503.799490	504858.493320	44.795239
3503.514475	504841.079336	44.800244
3503.602000	504836.308572	44.805249
3504.086925	504828.033787	44.810253
3503.518970	504807.122065	44.815258
3503.783031	504792.100950	44.820263
3504.036633	504779.004511	44.825268
3503.852241	504779.033690	44.830273
3503.846782	504737.335037	44.835277
3503.527999	504748.620053	44.840282
3503.537139	504728.780971	44.845287
3503.660611	504724.915410	44.850292
3503.312536	504715.405856	44.855297
3503.671024	504693.993329	44.860301
3503.521967	504691.739633	44.865306
3503.248018	504701.853645	44.870311
3503.461681	504688.206780	44.875316
3503.134146	504668.775087	44.880321
3503.538156	504660.968471	44.885325
3503.600085	504653.215917	44.890330
3503.541463	504641.130247	44.895335
3503.782413	504644.988907	44.900340
3503.385557	504656.235715	44.905345
3503.794633	504623.985304	44.910349
3503.675596	504611.048849	44.915354
3503.595524	504611.213359	44.920359
3503.859534	504595.635411	44.925364
3503.609047	504590.766184	44.930369
3503.580062	504574.272997	44.935373
3503.949874	504570.823929	44.940378
3503.871469	504555.806132	44.945383
3504.002405	504529.874754	44.950388
3503.651013	504522.541717	44.955393
3503.582634	504515.113339	44.960397
3503.533340	504487.945210	44.965402
3503.418164	504479.916929	44.970407
3503.876514	504467.293969	44.975412
3503.606129	504467.893416	44.980417
3503.880626	504465.218498	44.985421
3503.701743	504441.714490	44.990426
3503.700451	504428.506255	44.995431
3503.505450	504430.055326	45.000436
3503.397575	504417.926679	45.005441
3503.412227	504392.266513	45.010445
3503.851739	504379.393430	45.015450
3503.502339	504382.333306	45.020455
3503.431840	504382.546913	45.025460
3503.657826	504377.754141	45.030465
3503.220641	504354.240233	45.035469
3503.572114	504343.455943	45.040474
3503.318104	504343.293695	45.045479
3503.496933	504334.965842	45.050484
3503.455823	504339.375224	45.055489
3503.477178	504328.238240	45.060493
3503.550123	504302.214477	45.065498
3503.448207	504305.418896	45.070503
3503.547910	504290.423330	45.075508
3503.162431	504293.925607	45.080513
3503.434713	504289.226709	45.085517
3503.843227	504291.996204	45.090522
3503.532007	504272.207239	45.095527
3503.781229	504245.497631	45.100532
3503.490907	504258.903987	45.105537
3503.673545	504247.336599	45.110541
3503.925551	504225.586078	45.115546
3503.399026	504216.256279	45.120551
3503.428552	504207.294063	45.125556
3503.223093	504209.502708	45.130561
3503.379777	504199.609449	45.135565
3503.465446	504186.893366	45.140570
3503.307917	504172.798690	45.145575
3503.804357	504156.879970	45.150580
3503.558283	504159.246865	45.155585
3503.350969	504162.366752	45.160589
3503.634479	504158.374557	45.165594
3503.659481	504130.637445	45.170599
3503.629712	504117.231044	45.175604
3503.506299	504103.333352	45.180609
3503.493073	504105.359803	45.185613
3503.633101	504101.086623	45.190618
3503.416863	504087.355414	45.195623
3503.588932	504064.908814	45.200628
3503.506364	504075.499020	45.205633
3503.598615	504057.872805	45.210637
3503.628836	504058.930838	45.215642
3503.187745	504050.194747	45.220647
3503.821684	504024.638599	45.225652
3503.573094	504024.171840	45.230657
3503.625567	504013.029738	45.235661
3503.505497	504007.987909	45.240666
3503.418799	503997.626919	45.245671
3503.653294	503973.297823	45.250676
3503.684635	503980.884180	45.255681
3503.815282	503978.484967	45.260685
3503.963528	503961.760760	45.265690
3503.892122	503936.771441	45.270695
3503.884189	503920.021270	45.275700
3503.790134	503923.022082	45.280705
3503.751167	503909.313324	45.285709
3503.784553	503903.994168	45.290714
3503.633815	503886.254361	45.295719
3503.935908	503863.280865	45.300724
3504.041309	503855.470480	45.305729
3503.750433	503848.836119	45.310733
3503.849147	503818.252768	45.315738
3503.540754	503811.266898	45.320743
3503.807579	503799.331647	45.325748
3503.942387	503797.589669	45.330753
3503.712111	503760.833305	45.335757
3503.855789	503755.142409	45.340762
3503.447235	503742.352290	45.345767
3503.763483	503745.389502	45.350772
3503.413587	503730.413908	45.355777
3503.531527	503719.109446	45.360781
3503.569247	503708.171919	45.365786
3503.310859	503703.253083	45.370791
3503.606921	503688.782672	45.375796
3503.574130	503683.119644	45.380801
3503.416100	503671.049017	45.385805
3503.749331	503675.247573	45.390810
3503.385252	503664.677180	45.395815
3503.654583	503645.150018	45.400820
3503.224995	503633.223504	45.405825
3503.817552	503621.641527	45.410829
3503.611088	503608.920589	45.415834
3503.189690	503614.959154	45.420839
3503.606279	503608.972029	45.425844
3503.470527	503589.407609	45.430849
3503.509233	503576.344241	45.435853
3503.678614	503567.460814	45.440858
3503.377650	503572.316336	45.445863
3503.461467	503573.163488	45.450868
3503.690818	503562.954729	45.455873
3503.641935	503540.542382	45.460877
3503.783632	503527.412090	45.465882
3503.731995	503519.930035	45.470887
3503.697715	503509.560473	45.475892
3503.296120	503492.872113	45.480897
3503.258574	503477.644498	45.485901
3503.421475	503483.641368	45.490906
3503.266229	503480.325685	45.495911
3503.712265	503475.599110	45.500916
3503.781520	503465.921698	45.505921
3503.886084	503440.397763	45.510925
3503.696647	503445.539352	45.515930
3503.625555	503439.376199	45.520935
3503.672920	503408.445982	45.525940
3503.719914	503403.073914	45.530945
3503.665519	503390.278174	45.535949
3503.823893	503399.970331	45.540954
3503.492040	503370.314627	45.545959
3503.584693	503359.671863	45.550964
3503.459554	503356.300788	45.555969
3503.287852	503355.771248	45.560973
3503.656934	503351.208633	45.565978
3503.503039	503333.823040	45.570983
3503.531592	503299.757763	45.575988
3503.722536	503302.814857	45.580993
3503.623944	503304.146346	45.585997
3503.585104	503294.992029	45.591002
3503.377645	503271.440362	45.596007
3503.748789	503255.844298	45.601012
3503.390419	503257.824176	45.606017
3503.181736	503259.223679	45.611021
3503.569914	503255.467791	45.616026
3503.374137	503251.551143	45.621031
3503.444952	503227.803605	45.626036
3503.316830	503222.307328	45.631041
3503.481860	503223.495936	45.636045
3503.614821	503221.703583	45.641050
3503.368863	503213.138676	45.646055
3503.871461	503212.249504	45.651060
3503.542199	503189.425529	45.656065
3503.499050	503186.800624	45.661069
3503.889650	503173.681341	45.666074
3503.554727	503172.722094	45.671079
3503.449438	503134.527565	45.676084
3503.288687	503124.683875	45.681089
3503.218081	503134.867867	45.686093
3503.488481	503118.781497	45.691098
3503.406741	503132.864294	45.696103
3503.698410	503126.947363	45.701108
3503.717649	503093.389270	45.706113
3503.473372	503095.249910	45.711117
3503.431684	503087.563655	45.716122
3503.709011	503091.669965	45.721127
3503.418004	503092.829437	45.726132
3503.396678	503061.251525	45.731137
3503.207783	503048.173127	45.736141
3503.408631	503029.263442	45.741146
3503.447423	503034.419690	45.746151
3503.893125	503033.995003	45.751156
3504.062214	503029.666361	45.756161
3503.777227	503011.896279	45.761165
3504.032391	503004.972851	45.766170
3503.841681	502979.140638	45.771175
3504.106117	502965.130136	45.776180
3503.654161	502962.417976	45.781185
3503.535159	502945.633822	45.786189
3503.979514	502927.950829	45.791194
3503.654764	502913.476680	45.796199
3503.620193	502908.927139	45.801204
3503.637806	502892.070730	45.806209
3503.817704	502880.857162	45.811213
3503.860686	502862.579589	45.816218
3504.050459	502857.286013	45.821223
3503.919068	502835.543763	45.826228
3503.554757	502825.327184	45.831233
3503.552597	502810.903189	45.836237
3504.056514	502803.586085	45.841242
3503.797549	502791.632032	45.846247
3503.552159	502778.410528	45.851252
3503.471644	502776.398810	45.856257
3503.294602	502760.230996	45.861261
3503.694163	502732.584323	45.866266
3503.467352	502726.647980	45.871271
3503.605149	502722.273596	45.876276
3503.398488	502725.039347	45.881281
3503.641148	502724.090012	45.886285
3503.499900	502703.361400	45.891290
3503.424872	502683.229644	45.896295
3503.265209	502690.087561	45.901300
3503.322326	502675.704700	45.906305
3503.335921	502664.618503	45.911309
3503.292349	502684.465423	45.916314
3503.080959	502677.311933	45.921319
3503.591214	502663.869688	45.926324
3503.334222	502657.786255	45.931329
3503.192549	502638.019267	45.936333
3503.295720	502635.168704	45.941338
3503.310169	502631.016242	45.946343
3503.477154	502634.937649	45.951348
3503.350577	502627.416448	45.956353
3503.058879	502636.269137	45.961357
3503.372049	502626.249040	45.966362
3503.453586	502636.561110	45.971367
3503.426439	502609.690259	45.976372
3503.394775	502591.879717	45.981377
3503.329403	502576.098984	45.986381
3503.557586	502575.253155	45.991386
3503.177556	502575.566317	45.996391
3503.577831	502583.854153	46.001396
3503.394382	502571.381890	46.006401
3503.653021	502559.194035	46.011405
3503.542163	502536.081632	46.016410
3503.143623	502540.396118	46.021415
3503.508843	502529.659163	46.026420
3503.335538	502526.497992	46.031425
3503.161541	502539.887265	46.036429
3503.527220	502521.811402	46.041434
3503.485173	502509.924100	46.046439
3503.320587	502496.082260	46.051444
3503.374907	502490.050792	46.056449
3503.382538	502483.571185	46.061453
3503.637578	502491.072215	46.066458
3503.088732	502491.209608	46.071463
3503.505385	502481.324912	46.076468
3503.322213	502472.547270	46.081473
3503.183557	502454.854725	46.086477
3503.690305	502458.115118	46.091482
3503.619480	502452.811996	46.096487
3503.773300	502457.697168	46.101492
3503.591122	502442.036003	46.106497
3503.595644	502422.549345	46.111501
3503.596709	502411.464970	46.116506
3503.444305	502410.173155	46.121511
3503.573714	502402.054656	46.126516
3503.456067	502393.975201	46.131521
3503.154098	502367.451096	46.136525
3503.463870	502370.489571	46.141530
3503.180071	502356.615851	46.146535
3503.397376	502352.633715	46.151540
3503.240461	502349.318082	46.156545
3503.476396	502354.443370	46.161549
3503.627073	502343.841438	46.166554
3503.313510	502331.085892	46.171559
3503.414675	502317.353750	46.176564
3503.300521	502310.943942	46.181569
3503.097478	502313.607959	46.186573
3503.258498	502315.809528	46.191578
3503.320595	502311.598848	46.196583
3503.478950	502314.357585	46.201588
3503.689633	502320.094233	46.206593
3503.050374	502299.342631	46.211597
3503.342325	502283.505163	46.216602
3503.094106	502285.012217	46.221607
3503.217826	502276.337813	46.226612
3503.384258	502266.543159	46.231617
3503.253984	502282.658839	46.236621
3503.481721	502264.452675	46.241626
3503.420990	502274.230695	46.246631
3503.770900	502272.454572	46.251636
3503.479063	502246.080524	46.256641
3503.653881	502229.907226	46.261645
3503.811241	502219.304164	46.266650
3503.548806	502236.655500	46.271655
3503.486608	502211.004307	46.276660
3503.521530	502194.498793	46.281665
3503.328536	502196.806944	46.286669
3503.539859	502184.170787	46.291674
3503.415582	502189.302442	46.296679
3503.328008	502182.483477	46.301684
3503.613477	502167.608590	46.306689
3503.271629	502145.190163	46.311693
3503.617645	502137.290377	46.316698
3503.358583	502140.671865	46.321703
3503.401425	502131.149739	46.326708
3503.516718	502136.192931	46.331713
3503.125870	502130.434154	46.336717
3503.335113	502115.571271	46.341722
3503.408704	502107.866370	46.346727
3503.603028	502092.196004	46.351732
3503.695340	502095.673808	46.356737
3503.385262	502090.610847	46.361741
3503.846190	502079.453583	46.366746
3503.335392	502067.184545	46.371751
3503.575368	502048.470086	46.376756
3503.435853	502051.377170	46.381761
3503.434529	502039.483116	46.386765
3503.471132	502039.730437	46.391770
3503.447980	502030.218687	46.396775
3503.478584	502018.673871	46.401780
3503.454505	502005.821723	46.406785
3503.713762	502004.717885	46.411789
3504.150322	501984.605707	46.416794
3503.573431	501972.498891	46.421799
3503.450788	501957.435259	46.426804
3503.688233	501942.871459	46.431809
3503.722322	501952.938355	46.436813
3503.633269	501934.123936	46.441818
3503.366145	501922.828572	46.446823
3503.727414	501908.903161	46.451828
3503.485634	501902.867677	46.456833
3503.285532	501904.873302	46.461837
3503.548755	501887.319131	46.466842
3503.444774	501871.189572	46.471847
3503.535498	501861.254817	46.476852
3503.509290	501854.476642	46.481857
3503.477519	501859.290083	46.486861
3503.622458	501856.432794	46.491866
3503.532696	501845.969796	46.496871
3503.411764	501814.709092	46.501876
3503.374580	501813.803939	46.506881
3503.283566	501817.260158	46.511885
3503.485267	501814.140818	46.516890
3503.369602	501822.358713	46.521895
3503.457668	501791.773542	46.526900
3503.290787	501789.319829	46.531905
3503.412476	501770.117624	46.536909
3503.583895	501761.941579	46.541914
3503.328568	501766.942223	46.546919
3503.289094	501758.748892	46.551924
3503.694923	501772.856939	46.556929
3502.959467	501751.056986	46.561933
3503.487764	501741.913459	46.566938
3503.318761	501739.510690	46.571943
3503.247427	501727.070727	46.576948
3503.370731	501731.049854	46.581953
3503.350061	501726.953347	46.586957
3503.526234	501723.281261	46.591962
3503.186461	501728.092803	46.596967
3503.191370	501728.901901	46.601972
3503.472956	501730.983259	46.606977
3503.297678	501711.827927	46.611981
3503.438397	501698.595205	46.616986
3503.211948	501698.124881	46.621991
3503.488612	501680.770842	46.626996
3503.590647	501682.171972	46.632001
3503.161558	501680.569528	46.637005
3503.531808	501686.888543	46.642010
3503.146063	501652.834964	46.647015
3503.219070	501654.240684	46.652020
3503.645696	501638.735663	46.657025
3503.383085	501647.179325	46.662029
3503.958321	501637.471559	46.667034
3503.659354	501632.659786	46.672039
3503.727271	501608.556229	46.677044
3503.580120	501598.355232	46.682049
3503.415946	501596.862756	46.687053
3503.589462	501588.989991	46.692058
3503.559920	501581.250547	46.697063
3503.279898	501564.186841	46.702068
3503.693402	501553.694745	46.707073
3503.605612	501554.164194	46.712077
3503.766046	501546.495940	46.717082
3503.589332	501533.313266	46.722087
3503.594915	501504.309716	46.727092
3503.675841	501501.310642	46.732097
3503.595210	501496.312477	46.737101
3503.647156	501479.955456	46.742106
3503.457145	501478.062128	46.747111
3503.495893	501469.046450	46.752116
3503.859885	501450.362377	46.757121
3503.664661	501455.100530	46.762125
3503.741817	501422.694282	46.767130
3503.728882	501413.838592	46.772135
3503.338479	501419.113761	46.777140
3503.583033	501413.709867	46.782145
3503.497381	501407.143380	46.787149
3503.804602	501382.090609	46.792154
3503.363425	501371.277945	46.797159
3503.289919	501367.189705	46.802164
3503.620264	501371.642350	46.807169
3503.124674	501375.567525	46.812173
3503.488047	501358.452548	46.817178
3503.652557	501342.077609	46.822183
3503.445043	501322.724488	46.827188
3503.475990	501321.099917	46.832193
3503.345999	501322.234052	46.837197
3503.638736	501317.227442	46.842202
3503.449409	501309.867447	46.847207
3503.623107	501287.163988	46.852212
3503.671779	501273.236871	46.857217
3503.408541	501280.415399	46.862221
3503.395039	501272.420205	46.867226
3503.349994	501274.249544	46.872231
3503.337100	501252.992787	46.877236
3503.618418	501242.825098	46.882241
3503.247636	501235.139437	46.887245
3503.388305	501223.880407	46.892250
3503.648297	501230.520711	46.897255
3503.618172	501225.565104	46.902260
3503.670269	501210.878152	46.907265
3503.249341	501197.227662	46.912269
3503.542044	501192.271639	46.917274
3503.214810	501183.465510	46.922279
3503.241705	501180.069989	46.927284
3503.323266	501191.293993	46.932289
3503.345425	501185.267165	46.937293
3503.226383	501155.574114	46.942298
3503.306115	501162.293550	46.947303
3503.086565	501141.879187	46.952308
3503.336113	501133.336189	46.957313
3503.061925	501144.768298	46.962317
3503.157594	501131.137342	46.967322
3503.302976	501141.845124	46.972327
3503.143956	501141.718443	46.977332
3503.211667	501140.391744	46.982337
3503.335262	501138.550047	46.987341
3503.493682	501128.553567	46.992346
3503.083207	501140.513386	46.997351
3503.133934	501120.309364	47.002356
3503.214232	501109.717821	47.007361
3503.145580	501094.796774	47.012365
3503.352902	501093.599857	47.017370
3503.409662	501102.853783	47.022375
3503.100462	501090.450970	47.027380
3503.700165	501094.608029	47.032385
3502.842052	501100.463381	47.037389
3503.692581	501073.552721	47.042394
3503.343997	501089.501519	47.047399
3503.324772	501079.735556	47.052404
3503.345885	501040.807904	47.057409
3503.500255	501051.818021	47.062413
3503.412590	501044.188763	47.067418
3503.287544	501036.565411	47.072423
3503.547978	501047.913085	47.077428
3503.522405	501042.703623	47.082433
3503.205563	501037.135260	47.087437
3503.486687	501014.920645	47.092442
3503.206726	501013.901971	47.097447
3503.251256	501020.171472	47.102452
3503.466171	501009.052423	47.107457
3503.379785	501014.988298	47.112461
3503.469699	501012.291423	47.117466
3503.241095	501016.984350	47.122471
3503.447565	501007.587612	47.127476
3503.220747	500984.896453	47.132481
3502.918808	500980.793611	47.137485
3503.289866	500971.016521	47.142490
3503.319317	500970.708199	47.147495
3503.318445	500957.497306	47.152500
3503.541974	500963.384216	47.157505
3503.439724	500963.299177	47.162509
3503.360364	500967.766061	47.167514
3503.140464	500964.966294	47.172519
3503.232315	500951.740741	47.177524
3503.457387	500930.294137	47.182529
3503.320647	500932.796027	47.187533
3503.409324	500924.379589	47.192538
3503.270253	500929.463326	47.197543
3503.375663	500929.547936	47.202548
3503.544700	500917.069416	47.207553
3503.299206	500921.410718	47.212557
3503.701656	500898.873079	47.217562
3503.326414	500880.862037	47.222567
3503.195846	500883.818515	47.227572
3503.474431	500875.574508	47.232577
3503.366360	500886.524971	47.237581
3503.570023	500863.664386	47.242586
3503.720115	500862.172794	47.247591
3503.411467	500848.301820	47.252596
3503.683570	500830.897059	47.257601
3503.253831	500825.852647	47.262605
3503.712376	500830.639489	47.267610
3503.435480	500827.190680	47.272615
3503.149946	500808.355506	47.277620
3503.461443	500778.087603	47.282625
3503.312339	500780.338380	47.287629
3503.223413	500771.140059	47.292634
3503.688558	500784.277782	47.297639
3503.234527	500785.665635	47.302644
3503.739275	500783.409337	47.307649
3503.503327	500764.110720	47.312653
3503.380811	500739.681763	47.317658
3503.455171	500748.528150	47.322663
3503.349121	500744.394292	47.327668
3503.752674	500732.840316	47.332673
3503.460424	500727.976617	47.337677
3503.729152	500705.561105	47.342682
3503.557744	500705.537614	47.347687
3503.385409	500697.111704	47.352692
3503.674679	500695.142541	47.357697
3503.874407	500682.355300	47.362701
3503.500694	500662.977112	47.367706
3503.553351	500662.310791	47.372711
3503.444770	500656.000740	47.377716
3503.897484	500648.741468	47.382721
3503.739549	500624.824132	47.387725
3503.658241	500612.941766	47.392730
3503.736493	500601.337883	47.397735
3503.717736	500584.535651	47.402740
3503.722293	500561.199966	47.407745
3503.851970	500560.268377	47.412749
3503.714769	500547.331818	47.417754
3503.416797	500534.370041	47.422759
3503.261929	500530.800652	47.427764
3503.504034	500506.010036	47.432769
3503.406037	500512.454096	47.437773
3503.566555	500511.618867	47.442778
3503.774228	500513.054013	47.447783
3503.180743	500484.649672	47.452788
3503.342029	500478.853709	47.457793
3503.598252	500477.598404	47.462797
3503.445180	500469.726146	47.467802
3503.315715	500471.012106	47.472807
3503.256136	500469.553621	47.477812
3503.549757	500463.837974	47.482817
3503.393051	500435.212665	47.487821
3503.277853	500430.067808	47.492826
3503.519583	500420.715808	47.497831
3503.416173	500423.971781	47.502836
3503.323454	500412.293560	47.507841
3503.569779	500423.188294	47.512845
3503.461841	500417.485481	47.517850
3503.556256	500387.403083	47.522855
3503.235773	500392.414407	47.527860
3503.362893	500370.678901	47.532865
3503.270894	500391.447171	47.537869
3503.226919	500386.594757	47.542874
3503.280487	500389.927163	47.547879
3503.428624	500373.047736	47.552884
3503.529296	500359.111688	47.557889
3503.620237	500345.683355	47.562893
3503.730717	500325.114658	47.567898
3503.415747	500330.631317	47.572903
3503.254564	500330.302495	47.577908
3503.291425	500324.779243	47.582913
3503.037536	500327.603446	47.587917
3503.247037	500299.375610	47.592922
3503.288133	500283.322921	47.597927
3503.384286	500278.448330	47.602932
3503.217541	500282.119291	47.607937
3502.823013	500281.624872	47.612941
3503.288514	500272.389285	47.617946
3503.490088	500268.510411	47.622951
3503.015125	500266.813846	47.627956
3503.497977	500268.306758	47.632961
3503.266859	500273.962039	47.637965
3503.226217	500266.274398	47.642970
3503.291020	500266.821001	47.647975
3503.216930	500242.738043	47.652980
3503.218782	500234.891815	47.657985
3503.176987	500233.379880	47.662989
3503.164370	500228.471848	47.667994
3503.270890	500229.720528	47.672999
3503.033508	500231.580372	47.678004
3502.966904	500234.121894	47.683009
3503.295132	500218.681814	47.688013
3503.177496	500217.232484	47.693018
3503.134774	500222.503671	47.698023
3503.157217	500226.802792	47.703028
3503.326338	500223.688325	47.708033
3503.210573	500221.934985	47.713037
3503.325288	500212.349855	47.718042
3503.188565	500224.317637	47.723047
3502.893502	500227.198982	47.728052
3503.491364	500220.220312	47.733057
3503.475739	500195.824336	47.738061
3503.277283	500182.998433	47.743066
3503.210277	500168.430687	47.748071
3503.136180	500184.539385	47.753076
3503.276264	500173.532883	47.758081
3503.346923	500174.382280	47.763085
3503.502161	500177.749275	47.768090
3503.511205	500170.711791	47.773095
3503.435236	500165.611277	47.778100
3503.524514	500136.035462	47.783105
3503.153869	500126.881335	47.788109
3503.584887	500124.332892	47.793114
3503.743525	500126.028917	47.798119
3503.556330	500132.841549	47.803124
3503.710773	500095.966163	47.808129
3503.398944	500100.520624	47.813133
3503.568474	500083.181968	47.818138
3503.816110	500081.016840	47.823143
3504.042962	500066.048229	47.828148
3503.806138	500043.964890	47.833153
3503.531181	500056.562069	47.838157
3503.730759	500025.652527	47.843162
3503.514401	500009.893382	47.848167
3503.454579	499995.830558	47.853172
3503.447142	499995.730529	47.858177
3503.261041	499999.303367	47.863181
3503.408886	499993.306892	47.868186
3503.484490	499992.991259	47.873191
3503.311763	499975.352253	47.878196
3503.555446	499952.281698	47.883201
3503.050211	499949.628107	47.888205
3503.308638	499948.827998	47.893210
3503.418166	499945.520423	47.898215
3503.309518	499941.842369	47.903220
3503.986370	499924.018416	47.908225
3503.319787	499926.958528	47.913229
3503.595606	499905.502676	47.918234
3503.461723	499903.043486	47.923239
3502.896736	499899.488169	47.928244
3503.301883	499894.058436	47.933249
3503.363887	499899.161305	47.938253
3503.332760	499905.848116	47.943258
3503.760913	499897.833122	47.948263
3503.586097	499880.194352	47.953268
3503.716909	499852.231350	47.958273
3503.349238	499865.147038	47.963277
3503.347882	499859.629682	47.968282
3503.458120	499859.359193	47.973287
3503.277808	499839.291479	47.978292
3503.478771	499814.506409	47.983297
3503.400330	499810.621073	47.988301
3503.339990	499803.037587	47.993306
3503.413598	499811.125251	47.998311
3503.377768	499813.864449	48.003316
3503.575449	499801.330005	48.008321
3503.285849	499795.301362	48.013325
3503.338681	499774.437421	48.018330
3503.354533	499761.830446	48.023335
3503.340222	499778.790609	48.028340
3503.631144	499768.620567	48.033345
3503.362286	499766.283932	48.038349
3503.536895	499765.294580	48.043354
3503.264227	499748.481074	48.048359
3503.380137	499734.238408	48.053364
3503.714480	499728.516093	48.058369
3503.525966	499727.837234	48.063373
3503.292685	499711.776778	48.068378
3503.499613	499712.756521	48.073383
3503.115186	499711.197454	48.078388
3503.259095	499689.964675	48.083393
3503.242812	499679.539413	48.088397
3503.497689	499673.677777	48.093402
3503.353021	499667.626185	48.098407
3502.563697	499681.266717	48.103412
3503.239927	499672.604966	48.108417
3503.127037	499670.294288	48.113421
3503.210401	499666.130243	48.118426
3503.394541	499664.936897	48.123431
3503.241170	499671.440633	48.128436
3503.610539	499663.586688	48.133441
3503.336627	499672.387410	48.138445
3503.240760	499643.649978	48.143450
3503.583749	499628.308300	48.148455
3503.121434	499627.065261	48.153460
3503.402817	499619.326445	48.158465
3503.451631	499621.951053	48.163469
3503.327012	499614.630751	48.168474
3503.298341	499622.025972	48.173479
3503.588728	499618.993477	48.178484
3503.469254	499596.283588	48.183489
3503.285059	499589.377660	48.188493
3503.154266	499585.399307	48.193498
3503.239677	499580.981814	48.198503
3503.222625	499590.703779	48.203508
3503.083613	499577.665562	48.208513
3503.017134	499584.763048	48.213517
3502.868157	499589.038795	48.218522
3503.218429	499577.846844	48.223527
3503.059035	499576.707788	48.228532
3503.391106	499583.286694	48.233537
3503.067809	499585.919499	48.238541
3502.914973	499582.754566	48.243546
3503.167644	499576.437658	48.248551
3502.872223	499602.959169	48.253556
3503.143163	499580.035691	48.258561
3503.169891	499585.751678	48.263565
3503.073615	499588.956053	48.268570
3503.466240	499577.504304	48.273575
3503.225241	499564.279712	48.278580
3503.168853	499548.494878	48.283585
3503.048009	499556.967737	48.288589
3503.024709	499545.784190	48.293594
3503.721766	499537.524051	48.298599
3503.361188	499550.135117	48.303604
3503.545194	499533.957927	48.308609
3503.673751	499537.886094	48.313613
3503.547252	499525.503936	48.318618
3503.586226	499504.439387	48.323623
3503.458366	499495.702154	48.328628
3503.473241	499499.445811	48.333633
3503.307681	499503.217986	48.338637
3503.293687	499502.612778	48.343642
3503.738454	499486.191847	48.348647
3503.303137	499478.211897	48.353652
3503.372660	499455.471958	48.358657
3503.729299	499451.720265	48.363661
3503.473322	499450.748330	48.368666
3503.513599	499446.692287	48.373671
3503.294470	499427.541433	48.378676
3503.773361	499414.152330	48.383681
3503.197372	499405.435258	48.388685
3503.518066	499405.840201	48.393690
3503.569169	499403.098597	48.398695
3503.419390	499411.120505	48.403700
3503.320274	499388.255270	48.408705
3503.668300	499376.354848	48.413709
3503.779456	499365.200558	48.418714
3503.565698	499365.436865	48.423719
3503.556172	499367.868244	48.428724
3503.846643	499332.437817	48.433729
3503.535701	499333.752540	48.438733
3503.538396	499313.554070	48.443738
3503.658766	499310.902748	48.448743
3503.535133	499293.862773	48.453748
3503.594974	499279.780474	48.458753
3503.742142	499274.492573	48.463757
3503.532669	499274.880069	48.468762
3503.587248	499258.014381	48.473767
3503.644023	499250.159041	48.478772
3503.431677	499225.792837	48.483777
3503.333513	499240.083793	48.488781
3503.139511	499222.093054	48.493786
3503.503032	499224.364248	48.498791
3503.126106	499236.117542	48.503796
3503.043530	499229.954744	48.508801
3503.386970	499231.014182	48.513805
3503.323690	499211.433489	48.518810
3503.490973	499195.916725	48.523815
3503.051589	499189.354708	48.528820
3503.244408	499183.553344	48.533825
3503.175707	499192.119378	48.538829
3503.239291	499174.897834	48.543834
3503.397117	499182.567493	48.548839
3503.136864	499191.872512	48.553844
3503.689883	499179.433340	48.558849
3503.451415	499181.040352	48.563853
3503.399872	499159.179750	48.568858
3503.267969	499138.850490	48.573863
3503.185426	499137.699259	48.578868
3503.555621	499133.337890	48.583873
3503.217815	499144.983817	48.588877
3503.219542	499127.518892	48.593882
3503.749254	499129.510720	48.598887
3503.048751	499131.646362	48.603892
3503.131381	499096.957033	48.608897
3503.149112	499108.394923	48.613901
3503.476914	499093.915771	48.618906
3503.621191	499089.843210	48.623911
3503.247139	499102.304851	48.628916
3503.376013	499082.339290	48.633921
3503.656276	499094.646899	48.638925
3503.607197	499071.267128	48.643930
3503.823256	499058.729263	48.648935
3503.402876	499052.164191	48.653940
3503.612820	499046.360076	48.658945
3503.591424	499050.008315	48.663949
3503.634383	499028.284485	48.668954
3503.512020	499011.851513	48.673959
3503.393716	499013.945774	48.678964
3503.468318	499003.758868	48.683969
3503.471071	499002.138543	48.688973
3503.247398	498992.403754	48.693978
3503.552897	498961.728754	48.698983
3503.464173	498954.756869	48.703988
3503.614164	498953.417005	48.708993
3503.823932	498955.155684	48.713997
3503.459437	498940.482090	48.719002
3503.675713	498910.529824	48.724007
3503.533326	498911.463576	48.729012
3503.777486	498904.439059	48.734017
3503.464806	498908.386479	48.739021
3503.219631	498887.568608	48.744026
3503.565285	498861.544405	48.749031
3503.262321	498859.314286	48.754036
3503.282433	498862.399149	48.759041
3503.272640	498857.642165	48.764045
3503.475675	498860.090640	48.769050
3503.324944	498857.532722	48.774055
3503.027961	498857.630319	48.779060
3503.956289	498860.267899	48.784065
3503.537230	498832.086480	48.789069
3503.257614	498832.130709	48.794074
3503.595289	498822.307106	48.799079
3503.502263	498831.029026	48.804084
3503.764399	498810.687740	48.809089
3503.516642	498795.995577	48.814093
3503.262354	498782.975003	48.819098
3503.519879	498768.354827	48.824103
3503.296932	498779.982835	48.829108
3503.356122	498772.582515	48.834113
3503.376526	498774.907997	48.839117
3503.228468	498763.237447	48.844122
3503.252633	498740.250657	48.849127
3503.316367	498727.230402	48.854132
3503.175166	498732.061979	48.859137
3503.202229	498725.881679	48.864141
3503.399449	498742.201906	48.869146
3503.505702	498733.731039	48.874151
3503.262774	498738.933057	48.879156
3503.130888	498730.601074	48.884161
3503.843765	498730.640309	48.889165
3503.341982	498709.154061	48.894170
3503.563153	498677.479436	48.899175
3503.290871	498688.558441	48.904180
3503.439225	498685.902604	48.909185
3503.500010	498678.299499	48.914189
3503.306158	498686.024953	48.919194
3503.594098	498664.869448	48.924199
3503.057014	498649.412916	48.929204
3503.502289	498643.925844	48.934209
3503.601675	498632.570466	48.939213
3503.312077	498639.197352	48.944218
3503.752524	498639.127774	48.949223
3503.729006	498632.702318	48.954228
3503.256160	498607.870212	48.959233
3503.552219	498599.723650	48.964237
3503.521927	498596.286055	48.969242
3503.622541	498585.284820	48.974247
3503.401191	498575.195072	48.979252
3503.471382	498560.300593	48.984257
3503.885149	498545.604918	48.989261
3503.353995	498553.434365	48.994266
3503.551124	498553.757611	48.999271
3503.415086	498545.071831	49.004276
3503.379432	498517.487431	49.009281
3503.249903	498499.890771	49.014285
3503.199112	498497.772623	49.019290
3503.416130	498499.915194	49.024295
3503.159043	498501.575832	49.029300
3503.288777	498487.583115	49.034305
3503.575864	498494.928894	49.039309
3503.252660	498494.575019	49.044314
3503.518864	498470.284028	49.049319
3503.371458	498463.321226	49.054324
3503.325102	498455.431215	49.059329
3503.433142	498448.681156	49.064333
3503.459377	498455.460688	49.069338
3503.639048	498456.292937	49.074343
3502.963073	498461.765974	49.079348
3503.250201	498440.255965	49.084353
3503.409891	498429.599668	49.089357
3503.055012	498408.899831	49.094362
3503.389479	498402.670835	49.099367
3503.233234	498410.997955	49.104372
3503.222823	498404.013478	49.109377
3503.388352	498396.849318	49.114381
3503.471799	498405.847298	49.119386
3503.415528	498404.438746	49.124391
3503.208420	498403.459028	49.129396
3503.476954	498393.038628	49.134401
3503.666098	498366.228458	49.139405
3503.426295	498361.001451	49.144410
3503.490872	498364.737490	49.149415
3503.161922	498359.170201	49.154420
3502.996339	498355.703319	49.159425
3503.151892	498355.425646	49.164429
3503.164829	498357.043620	49.169434
3503.213660	498357.744680	49.174439
3503.229003	498346.858026	49.179444
3503.121451	498338.673889	49.184449
3503.658162	498323.097986	49.189453
3503.621363	498314.649533	49.194458
3503.712696	498316.761366	49.199463
3503.397704	498317.570554	49.204468
3503.687146	498306.792429	49.209473
3503.391009	498286.943786	49.214477
3503.043380	498286.897515	49.219482
3503.291273	498266.304743	49.224487
3503.079320	498280.260072	49.229492
3503.024244	498266.600142	49.234497
3503.312073	498275.667133	49.239501
3503.046767	498273.329740	49.244506
3503.161281	498260.250497	49.249511
3502.932680	498270.006611	49.254516
3503.252135	498273.550510	49.259521
3503.199598	498269.964494	49.264525
3502.956420	498277.444796	49.269530
3503.291714	498269.646258	49.274535
3503.386012	498266.948279	49.279540
3503.098620	498263.905628	49.284545
3503.377946	498270.037732	49.289549
3503.191012	498250.829911	49.294554
3503.222327	498224.601347	49.299559
3503.386084	498227.714240	49.304564
3503.037705	498218.049367	49.309569
3503.306906	498221.803719	49.314573
3503.086215	498220.522388	49.319578
3503.155529	498224.358957	49.324583
3502.976713	498235.879090	49.329588
3503.125410	498217.833182	49.334593
3503.478730	498209.930519	49.339597
3503.213708	498221.717410	49.344602
3503.332298	498221.445578	49.349607
3503.070075	498219.816438	49.354612
3503.223657	498217.463456	49.359617
3503.438369	498215.505810	49.364621
3503.302976	498196.036660	49.369626
3503.256204	498178.021607	49.374631
3503.358212	498186.105513	49.379636
3503.277708	498183.131400	49.384641
3503.608617	498167.739766	49.389645
3503.520302	498176.916882	49.394650
3503.666375	498164.743832	49.399655
3503.184952	498141.836188	49.404660
3503.197012	498134.341805	49.409665
3503.409110	498132.232689	49.414669
3503.157102	498132.525680	49.419674
3503.449125	498128.277676	49.424679
3503.152878	498134.855172	49.429684
3503.141357	498125.440758	49.434689
3503.244017	498124.310815	49.439693
3503.184622	498128.268997	49.444698
3503.511035	498131.710575	49.449703
3503.297254	498108.254336	49.454708
3503.162170	498098.758187	49.459713
3503.257605	498088.010594	49.464717
3503.172514	498099.262875	49.469722
3503.613778	498099.851295	49.474727
3503.227633	498091.407327	49.479732
3503.598370	498091.601893	49.484737
3503.132006	498103.775060	49.489741
3503.207560	498099.105636	49.494746
3503.349181	498074.378177	49.499751
3503.107374	498060.798229	49.504756
3503.450603	498055.529610	49.509761
3503.605857	498050.645076	49.514765
3503.177051	498045.144097	49.519770
3503.046661	498045.620369	49.524775
3503.223290	498042.200589	49.529780
3503.164997	498045.753612	49.534785
3503.312248	498039.705957	49.539789
3503.532080	498053.086963	49.544794
3503.594637	498031.409460	49.549799
3503.282520	498015.208071	49.554804
3503.030505	498011.400405	49.559809
3503.435307	498001.110119	49.564813
3503.047148	498001.728383	49.569818
3503.584710	498000.681572	49.574823
3503.433594	498005.666786	49.579828
3503.566510	498003.620796	49.584833
3503.349864	497977.228562	49.589837
3502.925211	497973.346923	49.594842
3503.415726	497966.384355	49.599847
3503.480972	497958.982744	49.604852
3503.492806	497957.209014	49.609857
3503.640291	497952.072553	49.614861
3503.288068	497952.027007	49.619866
3503.478932	497943.491772	49.624871
3503.559081	497929.962091	49.629876
3503.390767	497918.294196	49.634881
3503.168992	497900.306525	49.639885
3503.078697	497907.104681	49.644890
3503.671074	497898.303462	49.649895
3503.155810	497911.800756	49.654900
3503.051073	497909.792316	49.659905
3503.452349	497901.679437	49.664909
3503.338106	497900.786265	49.669914
3503.148391	497881.679742	49.674919
3503.194475	497868.509780	49.679924
3503.402838	497864.781196	49.684929
3503.462119	497868.315671	49.689933
3503.206654	497871.950517	49.694938
3503.726290	497859.465091	49.699943
3503.409978	497862.907052	49.704948
3503.210081	497836.765095	49.709953
3503.414954	497817.444261	49.714957
3503.160232	497824.065932	49.719962
3503.425090	497812.886391	49.724967
3503.422732	497812.684295	49.729972
3503.467921	497816.372885	49.734977
3503.596919	497822.478275	49.739981
3503.093661	497797.852362	49.744986
3503.424385	497785.903003	49.749991
3503.396909	497775.984668	49.754996
3502.951380	497780.003955	49.760001
3503.284677	497765.421620	49.765005
3503.148639	497769.391993	49.770010
3503.480875	497770.655797	49.775015
3503.443491	497762.460309	49.780020
3503.346246	497768.398970	49.785025
3503.521782	497754.297195	49.790029
3503.325660	497750.278135	49.795034
3503.391951	497717.563157	49.800039
3503.537489	497725.184754	49.805044
3503.300894	497729.019151	49.810049
3503.361988	497725.060684	49.815053
3503.233243	497725.891087	49.820058
3503.254365	497732.823577	49.825063
3503.384809	497733.258632	49.830068
3503.534207	497709.086332	49.835073
3503.388916	497686.580620	49.840077
3503.215807	497682.811039	49.845082
3503.679215	497691.293684	49.850087
3503.401163	497683.591835	49.855092
3503.584324	497682.297263	49.860097
3503.579638	497647.973334	49.865101
3503.131169	497642.525966	49.870106
3503.203765	497641.704503	49.875111
3503.016882	497630.646875	49.880116
3503.029760	497633.935597	49.885121
3503.360684	497625.479329	49.890125
3503.070535	497642.434472	49.895130
3503.403907	497631.851508	49.900135
3503.388867	497643.903024	49.905140
3502.923960	497634.256254	49.910145
3503.209775	497637.198079	49.915149
3503.286005	497634.350982	49.920154
3502.887064	497628.845155	49.925159
3503.244207	497643.622305	49.930164
3503.100980	497620.204907	49.935169
3503.228433	497604.288059	49.940173
3503.303269	497598.808596	49.945178
3503.263848	497578.513586	49.950183
3503.046382	497588.167053	49.955188
3503.065157	497598.340069	49.960193
3503.348459	497583.259223	49.965197
3503.296782	497589.443875	49.970202
3503.481230	497586.832800	49.975207
3503.250106	497593.450825	49.980212
3503.182542	497581.311148	49.985217
3503.598728	497593.952688	49.990221
3503.442393	497573.625524	49.995226
3503.700252	497557.232385	50.000231
3503.234366	497551.281474	50.005236
3503.166200	497550.178495	50.010241
3503.214731	497542.475596	50.015245
3502.861165	497544.151569	50.020250
3502.919635	497553.660188	50.025255
3503.232599	497550.269395	50.030260
3503.000966	497553.546151	50.035265
3503.320496	497545.901674	50.040269
3503.015387	497549.139417	50.045274
3503.148211	497550.080367	50.050279
3503.308234	497537.651557	50.055284
3503.201658	497553.615861	50.060289
3503.242319	497552.141294	50.065293
3503.392604	497528.525508	50.070298
3502.996587	497506.565467	50.075303
3503.186840	497510.028685	50.080308
3503.275099	497500.345041	50.085313
3503.328392	497488.591216	50.090317
3503.117951	497504.369472	50.095322
3503.458682	497493.076488	50.100327
3503.508891	497494.536767	50.105332
3503.119213	497494.294630	50.110337
3503.212910	497492.507915	50.115341
3503.342242	497485.450370	50.120346
3503.236019	497479.999487	50.125351
3502.979913	497453.916488	50.130356
3502.898207	497451.499341	50.135361
3503.422135	497444.531294	50.140365
3503.211793	497465.220389	50.145370
3503.045192	497453.805057	50.150375
3503.499595	497456.315250	50.155380
3502.962831	497456.197614	50.160385
3503.037433	497448.541181	50.165389
3503.128607	497448.678687	50.170394
3503.330580	497441.660270	50.175399
3503.258671	497443.696752	50.180404
3503.354923	497453.857604	50.185409
3503.640030	497437.308169	50.190413
3503.133281	497432.528099	50.195418
3503.435637	497409.141258	50.200423
3503.028068	497398.675265	50.205428
3503.141002	497401.593826	50.210433
3503.002818	497407.235313	50.215437
3502.920778	497401.527449	50.220442
3502.985547	497400.859094	50.225447
3503.302720	497403.745374	50.230452
3503.125443	497400.280155	50.235457
3503.468078	497391.163774	50.240461
3503.281737	497401.116184	50.245466
3503.193038	497400.117696	50.250471
3503.424598	497404.586948	50.255476
3503.389904	497404.339331	50.260481
3503.421428	497390.766306	50.265485
3503.296902	497382.989436	50.270490
3503.260205	497366.794561	50.275495
3503.286265	497359.601408	50.280500
3503.045602	497364.854087	50.285505
3503.459976	497359.675278	50.290509
3503.284110	497363.247017	50.295514
3503.173434	497362.960781	50.300519
3503.165388	497353.342907	50.305524
3503.392595	497359.027914	50.310529
3503.273942	497358.489802	50.315533
3503.264409	497351.757917	50.320538
3503.023715	497327.950528	50.325543
3503.189659	497328.379981	50.330548
3503.013578	497315.194103	50.335553
3503.345269	497318.229984	50.340557
3503.354899	497305.875413	50.345562
3503.282806	497318.948711	50.350567
3503.160394	497308.285714	50.355572
3502.994886	497318.943660	50.360577
3503.308611	497302.693343	50.365581
3503.097685	497317.307407	50.370586
3503.447421	497300.595750	50.375591
3503.603366	497312.063560	50.380596
3503.353549	497300.813166	50.385601
3503.592321	497275.056713	50.390605
3503.219225	497274.052539	50.395610
3503.309647	497275.962128	50.400615
3503.438336	497264.500006	50.405620
3503.182269	497284.234610	50.410625
3503.358898	497274.486252	50.415629
3503.440366	497272.245801	50.420634
3503.343208	497244.517297	50.425639
3503.411712	497225.217386	50.430644
3503.216525	497233.703084	50.435649
3503.239520	497218.814960	50.440653
3503.363481	497217.681595	50.445658
3503.065707	497216.766768	50.450663
3503.277545	497222.960523	50.455668
3503.044593	497214.947580	50.460673
3503.573583	497208.535548	50.465677
3503.074750	497229.726156	50.470682
3503.220289	497215.831214	50.475687
3503.031436	497198.900823	50.480692
3502.875202	497191.078254	50.485697
3503.335976	497198.802133	50.490701
3503.262256	497183.017967	50.495706
3503.033949	497186.952423	50.500711
3503.470667	497176.707255	50.505716
3503.388417	497187.453374	50.510721
3503.679955	497178.243708	50.515725
3502.891423	497173.609361	50.520730
3503.335610	497160.274708	50.525735
3503.518238	497133.210603	50.530740
3503.191690	497095.848198	50.535745
3503.184876	497049.879029	50.540749
3502.912752	497001.875919	50.545754
3502.640105	496924.609528	50.550759
3502.653926	496854.334918	50.555764
3502.405947	496777.975320	50.560769
3502.433345	496688.712083	50.565773
3501.738779	496600.878879	50.570778
3502.005860	496486.667096	50.575783
3502.304685	496364.855076	50.580788
3501.408763	496251.180041	50.585793
3501.520753	496115.371270	50.590797
3501.273180	495986.200360	50.595802
3500.886859	495823.329891	50.600807
3500.943681	495668.286516	50.605812
3500.511739	495503.040697	50.610817
3500.527019	495329.317639	50.615821
3500.166518	495155.804225	50.620826
3499.338618	494970.413443	50.625831
3499.351837	494765.646756	50.630836
3499.101298	494577.072039	50.635841
3498.703242	494375.049651	50.640845
3498.349329	494164.359289	50.645850
3497.984735	493953.718839	50.650855
3497.898267	493730.423333	50.655860
3497.371051	493507.397335	50.660865
3496.867719	493257.678336	50.665869
3496.652492	493029.533391	50.670874
3496.249133	492790.325234	50.675879
3495.626340	492528.005924	50.680884
3494.779326	492291.596040	50.685889
3494.792719	492034.689094	50.690893
3494.276752	491786.420871	50.695898
3493.888577	491517.264082	50.700903
3493.627166	491244.588924	50.705908
3492.837355	490982.274197	50.710913
3492.895400	490700.424527	50.715917
3491.998871	490420.443461	50.720922
3491.728481	490131.647938	50.725927
3491.560920	489829.410016	50.730932
3490.633184	489547.698816	50.735937
3490.161760	489237.041058	50.740941
3489.770363	488951.285488	50.745946
3488.913441	488625.888689	50.750951
3488.671232	488330.476411	50.755956
3487.683944	488018.512521	50.760961
3487.964815	487711.914943	50.765965
3487.382218	487386.250851	50.770970
3486.689964	487065.410766	50.775975
3486.219783	486729.181334	50.780980
3485.706913	486407.339336	50.785985
3485.363347	486068.444073	50.790989
3484.693515	485748.135516	50.795994
3483.975872	485408.223849	50.800999
3483.159637	485056.061863	50.806004
3482.571693	484728.428192	50.811009
3481.996736	484386.500090	50.816013
3481.935742	484035.770589	50.821018
3480.901006	483705.656985	50.826023
3480.485641	483338.302305	50.831028
3479.870437	482994.430654	50.836033
3479.220745	482646.200999	50.841037
3478.587455	482288.943627	50.846042
3477.933826	481935.939098	50.851047
3477.549053	481564.644566	50.856052
3476.514359	481224.101493	50.861057
3475.960720	480854.999020	50.866061
3475.531866	480496.105735	50.871066
3474.721004	480152.366969	50.876071
3474.211655	479780.703640	50.881076
3473.365665	479426.316129	50.886081
3472.780938	479056.272681	50.891085
3472.081947	478701.848946	50.896090
3471.531931	478347.547361	50.901095
3470.830379	477983.735758	50.906100
3469.892315	477628.469112	50.911105
3469.215331	477252.122320	50.916109
3468.510678	476897.464610	50.921114
3467.891159	476546.030845	50.926119
3467.492748	476171.444262	50.931124
3466.519340	475809.055182	50.936129
3466.094005	475436.689280	50.941133
3465.531289	475084.612754	50.946138
3464.809006	474713.699661	50.951143
3464.255454	474350.913892	50.956148
3463.117235	473985.274081	50.961153
3462.913329	473610.153034	50.966157
3462.551815	473258.773335	50.971162
3461.339227	472880.604767	50.976167
3461.019680	472501.071402	50.981172
3460.373730	472149.920355	50.986177
3459.575097	471772.679742	50.991181
3458.966291	471407.011457	50.996186
3457.867350	471026.864288	51.001191
3457.568674	470654.948666	51.006196
3456.471817	470297.601511	51.011201
3456.395726	469916.714544	51.016205
3455.626299	469562.953293	51.021210
3454.704834	469171.387182	51.026215
3454.356180	468811.969539	51.031220
3453.646496	468437.290555	51.036225
3452.913498	468071.380266	51.041229
3451.699972	467707.466313	51.046234
3450.959599	467329.983617	51.051239
3450.627329	466972.965678	51.056244
3449.685540	466604.679641	51.061249
3449.113132	466242.160207	51.066253
3448.649199	465872.771709	51.071258
3447.839281	465502.670817	51.076263
3447.121224	465138.228545	51.081268
3446.448723	464778.134017	51.086273
3445.877175	464405.491486	51.091277
3445.186015	464040.164072	51.096282
3444.106891	463682.093155	51.101287
3443.775123	463307.922892	51.106292
3443.085743	462944.351547	51.111297
3442.443112	462578.890150	51.116301
3441.650612	462223.589764	51.121306
3440.892805	461857.475032	51.126311
3440.068267	461491.922568	51.131316
3439.108499	461122.581312	51.136321
3438.592897	460758.844314	51.141325
3437.993928	460408.860031	51.146330
3437.042055	460050.353801	51.151335
3436.518417	459695.020295	51.156340
3435.167679	459356.550780	51.161345
3434.739250	458999.263428	51.166349
3434.377407	458646.068542	51.171354
3433.544898	458299.638321	51.176359
3432.945233	457943.172542	51.181364
3432.248271	457595.644580	51.186369
3431.574722	457231.620512	51.191373
3430.743008	456883.392487	51.196378
3430.173709	456539.125253	51.201383
3429.716072	456181.239012	51.206388
3428.882501	455840.909111	51.211393
3428.203467	455479.546113	51.216397
3427.479225	455129.142961	51.221402
3426.479339	454779.995554	51.226407
3426.152485	454430.127507	51.231412
3425.139999	454085.233106	51.236417
3424.398019	453741.508366	51.241421
3423.747905	453397.713149	51.246426
3422.944636	453064.033903	51.251431
3422.723887	452710.875262	51.256436
3421.712360	452371.535985	51.261441
3421.364265	452022.902689	51.266445
3420.465601	451682.672744	51.271450
3419.815146	451334.381216	51.276455
3419.224863	450995.462369	51.281460
3418.101164	450650.990291	51.286465
3417.605929	450301.491481	51.291469
3416.679884	449971.186499	51.296474
3416.004298	449631.296942	51.301479
3415.761754	449287.172701	51.306484
3414.543390	448958.472661	51.311489
3413.895256	448619.375923	51.316493
3413.313626	448285.744640	51.321498
3412.779407	447946.670874	51.326503
3411.945968	447606.370743	51.331508
3411.140687	447272.100623	51.336513
3410.481605	446942.674823	51.341517
3409.767770	446616.551995	51.346522
3408.772907	446279.354107	51.351527
3408.320000	445953.688413	51.356532
3407.485112	445622.597119	51.361537
3406.761262	445296.508445	51.366541
3406.280254	444968.549687	51.371546
3405.614790	444644.422345	51.376551
3405.242850	444308.011627	51.381556
3404.095004	443984.560693	51.386561
3403.584501	443653.898379	51.391565
3403.202170	443329.454687	51.396570
3402.340087	443008.026570	51.401575
3401.658160	442670.322165	51.406580
3400.891959	442341.458905	51.411585
3399.920208	442019.324313	51.416589
3399.416050	441691.730631	51.421594
3398.426547	441368.067315	51.426599
3398.208499	441046.359071	51.431604
3397.092393	440722.351849	51.436609
3396.677729	440401.427676	51.441613
3395.907044	440081.317086	51.446618
3395.522177	439763.933513	51.451623
3394.513076	439437.150972	51.456628
3393.746794	439115.453318	51.461633
3393.017329	438798.035640	51.466637
3392.565121	438481.560064	51.471642
3391.610882	438157.671194	51.476647
3390.979176	437842.612037	51.481652
3390.343072	437533.591415	51.486657
3389.831664	437207.589306	51.491661
3388.509552	436892.424215	51.496666
3388.036782	436585.016162	51.501671
3387.684241	436262.962364	51.506676
3386.668770	435956.063999	51.511681
3386.124655	435647.411780	51.516685
3385.378454	435330.790505	51.521690
3384.663755	435020.177327	51.526695
3384.227086	434713.096185	51.531700
3383.210767	434404.376527	51.536705
3382.535434	434091.663871	51.541709
3381.831483	433774.280217	51.546714
3380.909057	433476.934408	51.551719
3380.528218	433167.464561	51.556724
3379.543549	432867.734843	51.561729
3378.837858	432563.133266	51.566733
3378.243372	432265.137578	51.571738
3377.575505	431963.290560	51.576743
3377.021494	431667.820717	51.581748
3376.219337	431369.720581	51.586753
3375.747351	431060.595355	51.591757
3375.053566	430751.272990	51.596762
3373.994009	430455.742326	51.601767
3373.730769	430150.179077	51.606772
3372.889395	429859.711197	51.611777
3372.083684	429555.039362	51.616781
3371.545090	429255.222803	51.621786
3370.615324	428960.924454	51.626791
3370.011334	428664.768292	51.631796
3368.815094	428379.215930	51.636801
3368.260248	428076.874455	51.641805
3367.931545	427789.629459	51.646810
3367.104762	427496.720680	51.651815
3366.630226	427202.280013	51.656820
3365.763859	426904.266381	51.661825
3365.278541	426609.109780	51.666829
3364.568066	426320.766479	51.671834
3363.699377	426026.298995	51.676839
3363.106347	425736.356227	51.681844
3362.277765	425444.339575	51.686849
3361.771420	425143.150951	51.691853
3361.188010	424851.292304	51.696858
3360.169593	424580.859416	51.701863
3359.825475	424289.845835	51.706868
3359.012038	423995.779268	51.711873
3358.147027	423709.083475	51.716877
3357.669541	423421.713806	51.721882
3357.050246	423140.027698	51.726887
3356.580945	422842.795530	51.731892
3355.608745	422559.914662	51.736897
3354.631722	422275.507611	51.741901
3354.270366	421971.466996	51.746906
3353.438776	421701.814349	51.751911
3352.738447	421409.607280	51.756916
3352.141085	421128.862405	51.761921
3351.528486	420840.877554	51.766925
3351.045268	420563.512781	51.771930
3350.054159	420272.076401	51.776935
3349.812018	419978.918182	51.781940
3348.756102	419698.485445	51.786945
3348.438058	419409.118311	51.791949
3347.286004	419129.660418	51.796954
3346.837843	418851.663481	51.801959
3346.404914	418560.070265	51.806964
3345.469903	418284.812153	51.811969
3344.695278	417997.204828	51.816973
3344.144453	417712.379128	51.821978
3343.475063	417441.643694	51.826983
3343.010941	417146.153930	51.831988
3341.789377	416870.368528	51.836993
3341.106462	416584.129748	51.841997
3340.795237	416306.594407	51.847002
3339.804838	416025.606910	51.852007
3339.202820	415745.723954	51.857012
3338.682716	415468.111938	51.862017
3337.699493	415188.919035	51.867021
3337.299984	414911.841567	51.872026
3336.420916	414632.194911	51.877031
3335.825041	414369.574763	51.882036
3335.099099	414086.671876	51.887041
3334.436107	413808.863339	51.892045
3333.799228	413536.358397	51.897050
3333.079116	413261.704347	51.902055
3332.138375	412980.145989	51.907060
3331.653143	412721.787675	51.912065
3330.801207	412443.437103	51.917069
3330.028846	412172.160606	51.922074
3329.494678	411910.880838	51.927079
3328.786063	411632.754081	51.932084
3328.347920	411368.786304	51.937089
3327.601769	411094.471995	51.942093
3327.054820	410816.566159	51.947098
3326.060441	410560.759815	51.952103
3325.318745	410292.358201	51.957108
3324.387625	410027.287627	51.962113
3323.883109	409757.141161	51.967117
3323.393728	409496.290628	51.972122
3322.452022	409230.858959	51.977127
3321.812436	408956.889471	51.982132
3320.847387	408697.784490	51.987137
3319.944259	408440.903831	51.992141
3319.771250	408186.573906	51.997146
3318.995512	407915.488235	52.002151
3318.578541	407659.947260	52.007156
3317.796156	407407.791122	52.012161
3317.205443	407140.684685	52.017165
3316.393607	406885.784225	52.022170
3315.593316	406636.775937	52.027175
3315.265936	406364.919496	52.032180
3314.751614	406109.076069	52.037185
3313.917527	405847.486502	52.042189
3313.155872	405586.086598	52.047194
3312.694311	405324.865780	52.052199
3312.285052	405062.109571	52.057204
3311.138867	404799.620184	52.062209
3310.330327	404531.585353	52.067213
3309.972312	404280.277079	52.072218
3309.303992	404020.908044	52.077223
3308.763485	403746.037955	52.082228
3307.775745	403484.224193	52.087233
3307.205154	403232.839523	52.092237
3306.668219	402965.841364	52.097242
3305.944423	402705.911141	52.102247
3305.222494	402448.215253	52.107252
3304.728526	402197.623647	52.112257
3304.102634	401929.614158	52.117261
3303.344689	401660.809926	52.122266
3302.356851	401397.326843	52.127271
3301.873312	401137.905092	52.132276
3300.878220	400882.273311	52.137281
3299.816038	400636.080593	52.142285
3299.635949	400374.876227	52.147290
3298.900249	400121.688504	52.152295
3298.561121	399865.207793	52.157300
3297.743876	399612.410297	52.162305
3296.724585	399355.601003	52.167309
3296.477116	399090.380619	52.172314
3295.463877	398846.530714	52.177319
3295.231355	398590.251927	52.182324
3294.443545	398333.321757	52.187329
3293.618931	398077.208879	52.192333
3293.039289	397823.241502	52.197338
3292.075570	397570.731097	52.202343
3291.440980	397314.760219	52.207348
3290.836271	397065.316056	52.212353
3290.003340	396816.795891	52.217357
3289.598411	396559.638898	52.222362
3288.964614	396318.913580	52.227367
3288.243156	396056.896261	52.232372
3287.413758	395803.054688	52.237377
3286.633001	395551.949190	52.242381
3286.008601	395302.698410	52.247386
3285.277311	395057.505011	52.252391
3284.617187	394803.654577	52.257396
3284.216072	394572.337554	52.262401
3283.426312	394312.173443	52.267405
3282.846334	394053.753857	52.272410
3281.958974	393815.796636	52.277415
3281.267676	393566.264045	52.282420
3280.579193	393315.000317	52.287425
3279.879241	393072.279312	52.292429
3279.912594	392826.923546	52.297434
3278.847923	392576.603803	52.302439
3278.141399	392322.386373	52.307444
3277.058521	392068.099474	52.312449
3276.589167	391832.859271	52.317453
3276.039545	391585.349454	52.322458
3275.148880	391340.485283	52.327463
3274.513952	391090.875087	52.332468
3273.880063	390852.959121	52.337473
3272.853837	390604.475261	52.342477
3272.296299	390365.831977	52.347482
3271.682708	390126.865392	52.352487
3271.379798	389876.304125	52.357492
3270.683359	389641.619127	52.362497
3269.633037	389398.114350	52.367501
3269.234807	389144.842252	52.372506
3268.474962	388905.204024	52.377511
3267.805952	388671.932256	52.382516
3267.043170	388424.128872	52.387521
3266.119760	388195.522169	52.392525
3265.800578	387943.754772	52.397530
3264.905378	387710.944819	52.402535
3264.406236	387472.934093	52.407540
3263.584518	387231.107606	52.412545
3262.629161	387006.745074	52.417549
3262.677083	386757.021980	52.422554
3261.328635	386521.402554	52.427559
3260.827751	386290.479195	52.432564
3260.171791	386049.508682	52.437569
3259.362764	385827.022989	52.442573
3259.217155	385588.893183	52.447578
3258.276463	385357.524908	52.452583
3257.798244	385107.441474	52.457588
3257.087361	384872.676984	52.462593
3256.132304	384633.422938	52.467597
3255.621978	384396.640108	52.472602
3254.661069	384164.377490	52.477607
3254.268725	383935.126118	52.482612
3253.827859	383696.674821	52.487617
3252.878939	383457.005348	52.492621
3251.976557	383228.923883	52.497626
3251.338495	382997.543938	52.502631
3250.783067	382765.361107	52.507636
3250.247590	382535.157410	52.512641
3249.117481	382304.232526	52.517645
3248.877426	382057.066637	52.522650
3248.088415	381839.742272	52.527655
3247.150780	381605.781638	52.532660
3246.408187	381383.182721	52.537665
3245.691944	381156.025802	52.542669
3245.396199	380925.062326	52.547674
3244.192466	380711.052611	52.552679
3243.972913	380480.201580	52.557684
3243.286932	380256.468101	52.562689
3242.348646	380029.237918	52.567693
3242.006962	379797.181300	52.572698
3241.219207	379580.556123	52.577703
3240.584138	379350.425375	52.582708
3239.705603	379128.038438	52.587713
3238.957819	378902.017833	52.592717
3238.386908	378680.139255	52.597722
3237.790049	378464.749439	52.602727
3237.205121	378226.236059	52.607732
3236.710611	378002.891777	52.612737
3236.104389	377785.286864	52.617741
3235.193617	377553.713953	52.622746
3234.192440	377328.436601	52.627751
3233.725887	377105.057405	52.632756
3233.170361	376890.847974	52.637761
3232.538384	376661.158905	52.642765
3231.902875	376428.620218	52.647770
3231.327719	376219.548423	52.652775
3230.553049	375987.003755	52.657780
3230.033655	375764.795529	52.662785
3229.179476	375544.775727	52.667789
3228.427200	375318.099568	52.672794
3227.740409	375093.853745	52.677799
3226.971047	374858.986983	52.682804
3226.447190	374644.200999	52.687809
3225.393163	374422.731370	52.692813
3225.003666	374207.031524	52.697818
3224.208826	373996.278713	52.702823
3223.507635	373768.008730	52.707828
3223.090064	373558.872907	52.712833
3222.173672	373346.711471	52.717837
3221.791372	373121.389176	52.722842
3221.135011	372898.449347	52.727847
3220.424316	372679.561651	52.732852
3219.571861	372469.039125	52.737857
3219.153495	372252.926647	52.742861
3218.462056	372025.713978	52.747866
3217.760155	371812.467804	52.752871
3217.234289	371587.541533	52.757876
3216.745740	371373.623408	52.762881
3215.554669	371161.087301	52.767885
3214.796927	370929.579936	52.772890
3214.194681	370714.353604	52.777895
3213.506407	370501.963619	52.782900
3212.798618	370297.055029	52.787905
3212.222456	370077.674634	52.792909
3211.515146	369848.697436	52.797914
3210.788240	369643.737863	52.802919
3210.369930	369429.493588	52.807924
3209.949153	369215.833773	52.812929
3208.968134	368993.815185	52.817933
3208.291546	368771.976270	52.822938
3207.788069	368561.175691	52.827943
3207.032184	368341.458729	52.832948
3206.588871	368135.454954	52.837953
3205.402279	367927.023644	52.842957
3204.917131	367703.622529	52.847962
3204.255701	367496.098318	52.852967
3203.622899	367273.608833	52.857972
3203.104387	367049.013910	52.862977
3202.098711	366845.510033	52.867981
3201.683387	366626.799197	52.872986
3200.864958	366416.699658	52.877991
3200.544424	366202.704006	52.882996
3199.256905	365992.015168	52.888001
3198.548106	365777.417394	52.893005
3198.235571	365555.733706	52.898010
3197.213058	365359.502349	52.903015
3196.711368	365151.127771	52.908020
3196.374988	364934.024537	52.913025
3195.712689	364726.004168	52.918029
3194.727683	364519.051629	52.923034
3194.163455	364303.202702	52.928039
3193.493067	364089.786687	52.933044
3192.707142	363881.654801	52.938049
3192.137976	363675.828511	52.943053
3191.682995	363460.467204	52.948058
3190.797942	363263.696193	52.953063
3189.951906	363044.425532	52.958068
3189.410982	362836.224718	52.963073
3188.691827	362624.794281	52.968077
3187.856082	362426.561582	52.973082
3187.150024	362214.236649	52.978087
3186.643387	362000.810526	52.983092
3185.896770	361796.937767	52.988097
3185.437659	361603.654632	52.993101
3185.010850	361380.365861	52.998106
3184.139342	361189.029199	53.003111
3183.261196	360964.842945	53.008116
3182.902114	360770.853553	53.013121
3182.000119	360565.778678	53.018125
3181.276955	360351.030737	53.023130
3180.759812	360149.150227	53.028135
3180.060393	359939.460381	53.033140
3179.476758	359737.359642	53.038145
3178.430900	359538.257471	53.043149
3178.088011	359329.857205	53.048154
3177.459476	359123.231575	53.053159
3176.891597	358919.369123	53.058164
3175.956782	358707.929917	53.063169
3174.981355	358505.656993	53.068173
3174.417710	358297.923385	53.073178
3173.849573	358108.358627	53.078183
3173.357769	357912.317547	53.083188
3172.951412	357693.461642	53.088193
3172.104263	357496.279109	53.093197
3171.743722	357276.167196	53.098202
3170.444414	357081.930079	53.103207
3169.853041	356883.432275	53.108212
3169.137826	356682.637544	53.113217
3168.337867	356474.577386	53.118221
3168.057741	356274.628298	53.123226
3167.373293	356083.394644	53.128231
3166.609992	355883.545886	53.133236
3165.840698	355671.329530	53.138241
3165.174822	355474.695641	53.143245
3164.894387	355260.084439	53.148250
3164.053207	355068.464566	53.153255
3163.377999	354868.317930	53.158260
3162.782840	354660.472381	53.163265
3162.104172	354461.164500	53.168269
3161.400942	354260.587292	53.173274
3160.422121	354061.121753	53.178279
3160.276172	353861.091045	53.183284
3159.355040	353643.011575	53.188289
3158.442705	353450.735244	53.193293
3158.164752	353244.386199	53.198298
3157.177310	353049.193601	53.203303
3156.451931	352841.208639	53.208308
3156.163992	352643.689758	53.213313
3155.383577	352448.436717	53.218317
3154.836701	352240.064837	53.223322
3153.917350	352046.486520	53.228327
3153.239466	351842.918368	53.233332
3152.527865	351646.277178	53.238337
3151.594430	351457.661693	53.243341
3151.565271	351247.906051	53.248346
3150.677098	351048.771019	53.253351
3150.045862	350842.697536	53.258356
3149.371090	350650.856983	53.263361
3148.456515	350457.679354	53.268365
3148.243055	350253.980779	53.273370
3147.188518	350059.627689	53.278375
3146.272081	349857.311381	53.283380
3145.910634	349660.174866	53.288385
3144.847908	349465.642793	53.293389
3144.308919	349261.177571	53.298394
3143.726814	349070.309374	53.303399
3143.079608	348886.602637	53.308404
3142.558109	348687.197328	53.313409
3141.900125	348499.011558	53.318413
3141.608981	348286.231771	53.323418
3140.593652	348098.177532	53.328423
3139.713519	347898.978844	53.333428
3139.343509	347698.451595	53.338433
3138.573232	347500.633961	53.343437
3137.761022	347305.163853	53.348442
3136.976741	347120.378544	53.353447
3136.430533	346931.329897	53.358452
3136.015293	346731.849905	53.363457
3134.789017	346545.529157	53.368461
3134.836316	346341.087755	53.373466
3133.950999	346151.072067	53.378471
3133.093003	345949.954071	53.383476
3132.573511	345753.261495	53.388481
3131.336764	345569.611765	53.393485
3131.008209	345373.193118	53.398490
3130.505679	345198.130936	53.403495
3129.794583	344994.008367	53.408500
3129.336609	344805.066025	53.413505
3128.566610	344615.765187	53.418509
3128.017181	344415.891163	53.423514
3127.554526	344220.177088	53.428519
3126.586048	344026.298685	53.433524
3126.391075	343826.850196	53.438529
3125.061140	343638.143878	53.443533
3124.675026	343434.346281	53.448538
3123.860137	343243.088205	53.453543
3123.043870	343046.357144	53.458548
3122.835772	342854.823642	53.463553
3121.986985	342667.005379	53.468557
3121.367468	342457.310586	53.473562
3120.401257	342281.524066	53.478567
3119.769466	342087.917010	53.483572
3119.145502	341883.719068	53.488577
3118.480886	341705.795901	53.493581
3117.824197	341511.452773	53.498586
3117.194574	341314.584736	53.503591
3116.586816	341118.654435	53.508596
3115.554541	340923.808871	53.513601
3114.874515	340742.143495	53.518605
3114.316816	340549.232598	53.523610
3113.756686	340368.208987	53.528615
3113.117090	340183.964625	53.533620
3112.742136	339992.346756	53.538625
3111.849253	339812.163295	53.543629
3111.156820	339612.117898	53.548634
3110.601271	339425.439755	53.553639
3109.933364	339230.505806	53.558644
3109.284998	339040.659280	53.563649
3108.408475	338850.237352	53.568653
3107.866677	338652.837938	53.573658
3107.023210	338461.544127	53.578663
3106.254728	338280.267495	53.583668
3106.145307	338079.310450	53.588673
3105.371029	337896.735403	53.593677
3104.780558	337707.512175	53.598682
3103.704807	337511.211997	53.603687
3103.200824	337318.995583	53.608692
3102.692602	337134.467082	53.613697
3101.322672	336944.321266	53.618701
3100.656914	336759.460249	53.623706
3100.159163	336574.852152	53.628711
3099.448357	336386.356935	53.633716
3099.070567	336208.576664	53.638721
3098.240222	336029.034641	53.643725
3097.638512	335841.131579	53.648730
3097.196219	335655.137490	53.653735
3096.486446	335470.152573	53.658740
3095.988553	335290.835996	53.663745
3095.017932	335101.869135	53.668749
3094.333713	334914.765717	53.673754
3093.846419	334721.928204	53.678759
3093.013605	334544.291914	53.683764
3092.637324	334361.109590	53.688769
3091.676119	334173.055132	53.693773
3091.186771	333989.024155	53.698778
3090.354789	333803.850399	53.703783
3089.425122	333615.967637	53.708788
3089.031671	333432.963772	53.713793
3088.180040	333253.621475	53.718797
3087.792204	333057.072200	53.723802
3087.195425	332887.642656	53.728807
3086.276284	332698.355579	53.733812
3085.528672	332505.222146	53.738817
3084.999049	332340.006698	53.743821
3084.511713	332151.082619	53.748826
3083.709198	331966.739480	53.753831
3083.271592	331776.890046	53.758836
3082.677810	331587.192114	53.763841
3081.650050	331420.016696	53.768845
3081.128088	331219.257472	53.773850
3080.568221	331039.990723	53.778855
3079.596020	330870.641268	53.783860
3078.801302	330675.168178	53.788865
3078.120663	330502.971278	53.793869
3077.459547	330324.533476	53.798874
3076.597935	330142.155382	53.803879
3076.300647	329957.930873	53.808884
3075.688817	329780.502316	53.813889
3074.752795	329606.841658	53.818893
3074.563557	329434.844563	53.823898
3073.920731	329239.445484	53.828903
3073.159970	329065.730379	53.833908
3072.382040	328874.527047	53.838913
3071.567098	328700.946973	53.843917
3071.275082	328515.063228	53.848922
3070.130362	328338.606677	53.853927
3069.572955	328164.526356	53.858932
3069.453772	327975.940697	53.863937
3068.366509	327804.514827	53.868941
3067.884331	327621.765087	53.873946
3066.832230	327436.177227	53.878951
3065.786255	327249.518641	53.883956
3065.561199	327080.118818	53.888961
3065.130115	326910.140192	53.893965
3064.486099	326722.933003	53.898970
3063.672482	326549.322428	53.903975
3062.935216	326362.180060	53.908980
3062.598301	326186.991107	53.913985
3061.741323	326014.786535	53.918989
3060.935570	325829.919715	53.923994
3060.432359	325643.782495	53.928999
3060.003486	325467.333501	53.934004
3059.314340	325288.022815	53.939009
3058.728759	325106.276593	53.944013
3058.155758	324914.929330	53.949018
3057.377423	324737.108258	53.954023
3056.303583	324561.905095	53.959028
3055.792000	324373.984044	53.964033
3054.772762	324208.752106	53.969037
3054.426578	324016.755801	53.974042
3053.722965	323843.656701	53.979047
3052.815401	323655.516617	53.984052
3052.761913	323468.946843	53.989057
3052.272215	323300.854054	53.994061
3051.362580	323113.349612	53.999066
3050.467899	322923.372653	54.004071
3049.685887	322748.679653	54.009076
3049.341197	322563.274263	54.014081
3048.211298	322394.313465	54.019085
3047.612512	322223.205910	54.024090
3047.384725	322044.146253	54.029095
3046.473344	321859.974795	54.034100
3045.891779	321676.030830	54.039105
3044.952000	321507.165522	54.044109
3044.537938	321329.177800	54.049114
3043.972202	321149.635094	54.054119
3043.099207	320974.800152	54.059124
3042.550719	320790.569022	54.064129
3041.487316	320611.103983	54.069133
3040.976547	320440.972040	54.074138
3040.849679	320256.545774	54.079143
3040.003936	320077.019759	54.084148
3039.384761	319895.267793	54.089153
3038.416917	319719.834325	54.094157
3037.949436	319537.090076	54.099162
3037.423347	319360.567520	54.104167
3036.327769	319188.947122	54.109172
3035.866572	318998.587586	54.114177
3035.202511	318830.666656	54.119181
3034.441248	318645.497282	54.124186
3034.287335	318473.701072	54.129191
3033.120162	318305.960670	54.134196
3032.820529	318119.826013	54.139201
3031.626378	317943.813901	54.144205
3030.932970	317759.879715	54.149210
3030.649087	317587.083956	54.154215
3029.932304	317410.842535	54.159220
3029.433540	317223.235339	54.164225
3028.813395	317044.304358	54.169229
3027.882660	316868.248584	54.174234
3027.218088	316686.675834	54.179239
3026.744561	316515.690580	54.184244
3026.413106	316325.483412	54.189249
3025.339140	316158.462946	54.194253
3024.750794	315968.575841	54.199258
3023.908840	315783.490125	54.204263
3023.205681	315622.597626	54.209268
3022.749301	315428.181619	54.214273
3021.959004	315255.614682	54.219277
3021.197799	315081.209485	54.224282
3020.877919	314900.597463	54.229287
3020.131829	314716.538620	54.234292
3019.554715	314539.302384	54.239297
3018.503463	314364.432599	54.244301
3017.887414	314195.146557	54.249306
3017.340262	314021.062174	54.254311
3016.198746	313839.279688	54.259316
3015.938126	313664.079889	54.264321
3015.312654	313495.227089	54.269325
3014.605036	313302.094564	54.274330
3014.150043	313130.846070	54.279335
3013.349155	312956.138030	54.284340
3012.836911	312773.948560	54.289345
3011.910138	312605.320286	54.294349
3011.259723	312419.459812	54.299354
3010.868976	312243.539828	54.304359
3010.045181	312073.952264	54.309364
3009.621087	311888.691671	54.314369
3009.025672	311712.166626	54.319373
3008.023464	311521.114692	54.324378
3007.538830	311342.508927	54.329383
3006.827743	311168.573219	54.334388
3006.531293	310983.418241	54.339393
3005.827130	310807.825699	54.344397
3004.815538	310623.470857	54.349402
3004.024766	310436.687111	54.354407
3002.840392	310266.466348	54.359412
3002.793451	310101.591114	54.364417
3002.341021	309923.385461	54.369421
3001.475376	309743.564273	54.374426
3000.633667	309563.407980	54.379431
2999.944686	309397.640250	54.384436
2999.330057	309208.713090	54.389441
2998.488994	309041.466514	54.394445
2998.150193	308863.801503	54.399450
2997.844100	308676.912784	54.404455
2996.663197	308504.677212	54.409460
2996.156963	308327.368957	54.414465
2995.399140	308151.882811	54.419469
2994.921043	307972.914368	54.424474
2994.118943	307788.903944	54.429479
2993.115337	307622.852539	54.434484
2992.498584	307439.092378	54.439489
2991.972147	307277.930684	54.444493
2991.192663	307108.838242	54.449498
2990.694369	306920.169266	54.454503
2989.644129	306760.541336	54.459508
2989.200314	306584.493994	54.464513
2988.677772	306413.042625	54.469517
2987.994300	306235.886801	54.474522
2987.562883	306060.600745	54.479527
2986.666840	305898.018831	54.484532
2985.981525	305707.289529	54.489537
2985.340031	305547.213438	54.494541
2984.866431	305372.213265	54.499546
2984.293990	305182.509433	54.504551
2983.629152	305014.338360	54.509556
2982.980731	304837.684438	54.514561
2982.059848	304670.572092	54.519565
2981.383523	304490.840797	54.524570
2980.712142	304318.748194	54.529575
2980.024093	304149.230055	54.534580
2979.496138	303970.926149	54.539585
2978.742601	303801.086899	54.544589
2978.026489	303633.151457	54.549594
2977.552164	303449.847106	54.554599
2976.928360	303271.863084	54.559604
2976.353445	303092.903398	54.564609
2975.365200	302931.529483	54.569613
2974.840455	302747.137185	54.574618
2974.207297	302579.569378	54.579623
2973.313860	302408.782926	54.584628
2972.914773	302224.930340	54.589633
2971.918147	302064.957437	54.594637
2971.559575	301883.364501	54.599642
2970.813348	301710.720393	54.604647
2970.065500	301537.388759	54.609652
2969.249899	301371.580184	54.614657
2968.744986	301196.248815	54.619661
2968.346574	301028.412938	54.624666
2967.805398	300858.256580	54.629671
2966.668936	300690.333434	54.634676
2966.339550	300508.021208	54.639681
2965.454141	300332.723639	54.644685
2965.156773	300156.721605	54.649690
2964.270135	299977.629350	54.654695
2963.639797	299803.360423	54.659700
2963.171299	299624.558125	54.664705
2961.989785	299451.878593	54.669709
2961.147847	299280.698590	54.674714
2961.024738	299109.710228	54.679719
2960.121543	298950.712601	54.684724
2959.523300	298761.870619	54.689729
2958.909123	298587.725202	54.694733
2958.242930	298416.796644	54.699738
2957.782629	298244.511058	54.704743
2957.166119	298084.626853	54.709748
2956.482670	297897.019820	54.714753
2955.744564	297721.670755	54.719757
2954.687453	297535.752362	54.724762
2954.439211	297359.077530	54.729767
2953.479879	297202.684824	54.734772
2953.300109	297018.027702	54.739777
2952.731281	296848.304644	54.744781
2952.041144	296672.132038	54.749786
2951.296601	296482.011997	54.754791
2950.574098	296313.942666	54.759796
2949.638048	296129.251582	54.764801
2949.457987	295951.978887	54.769805
2948.560303	295779.098087	54.774810
2948.082867	295599.452777	54.779815
2947.372045	295431.355365	54.784820
2946.982715	295256.814679	54.789825
2946.376538	295059.948035	54.794829
2945.556814	294880.483597	54.799834
2945.058452	294696.027500	54.804839
2944.212171	294522.169730	54.809844
2943.560633	294320.980136	54.814849
2942.832060	294138.877504	54.819853
2941.964430	293964.003963	54.824858
2941.307846	293782.449911	54.829863
2940.415659	293605.746323	54.834868
2940.080594	293433.436648	54.839873
2939.361598	293252.605121	54.844877
2938.572935	293079.068140	54.849882
2938.189509	292890.593927	54.854887
2937.476374	292715.389331	54.859892
2936.734260	292539.374231	54.864897
2935.851254	292348.813926	54.869901
2935.497065	292180.937663	54.874906
2934.902336	291992.648973	54.879911
2934.024868	291808.836237	54.884916
2933.680273	291625.804904	54.889921
2932.571838	291445.517506	54.894925
2931.812140	291277.297327	54.899930
2931.482417	291090.010160	54.904935
2930.537793	290917.285786	54.909940
2930.075677	290732.820749	54.914945
2929.302490	290564.907845	54.919949
2928.397530	290387.541730	54.924954
2927.898591	290207.233376	54.929959
2927.222413	290045.417023	54.934964
2926.902788	289852.931963	54.939969
2926.466923	289676.586230	54.944973
2925.531539	289501.261766	54.949978
2924.622654	289314.141433	54.954983
2923.988002	289129.116857	54.959988
2923.701671	288949.818205	54.964993
2922.901675	288779.132468	54.969997
2922.147524	288593.158691	54.975002
2921.491473	288402.788804	54.980007
2920.435497	288235.148482	54.985012
2920.218233	288042.544141	54.990017
2919.298341	287868.387775	54.995021
2918.653356	287700.325552	55.000026
2918.092409	287526.494193	55.005031
2917.415059	287343.869273	55.010036
2916.990991	287162.935973	55.015041
2916.252005	286987.426163	55.020045
2915.560566	286804.752242	55.025050
2915.119943	286626.240730	55.030055
2914.000969	286447.072477	55.035060
2913.863864	286260.261107	55.040065
2912.993897	286076.036054	55.045069
2912.201909	285898.369311	55.050074
2911.606748	285712.190472	55.055079
2910.753269	285538.277093	55.060084
2910.158275	285360.044082	55.065089
2909.271150	285181.704429	55.070093
2908.616291	285005.390840	55.075098
2908.342397	284823.694034	55.080103
2907.382678	284649.567873	55.085108
2907.112080	284460.994001	55.090113
2906.182603	284286.404477	55.095117
2905.574395	284115.635178	55.100122
2904.826082	283943.665523	55.105127
2904.355733	283757.364167	55.110132
2903.964140	283570.133415	55.115137
2903.005970	283393.714383	55.120141
2902.622814	283217.637213	55.125146
2901.830819	283021.199220	55.130151
2901.230732	282843.831915	55.135156
2900.400250	282659.751950	55.140161
2900.002748	282473.311235	55.145165
2899.094943	282291.790206	55.150170
2898.557285	282116.832256	55.155175
2897.856026	281932.833461	55.160180
2897.163106	281741.243751	55.165185
2896.815702	281553.852477	55.170189
2895.901383	281377.833337	55.175194
2895.218573	281185.426869	55.180199
2894.367231	281016.019409	55.185204
2893.709768	280823.634290	55.190209
2893.138346	280647.611606	55.195213
2892.374868	280462.221483	55.200218
2891.728493	280283.281722	55.205223
2890.898934	280116.799454	55.210228
2890.872369	279923.142675	55.215233
2890.113969	279741.419012	55.220237
2889.170760	279565.174791	55.225242
2888.881392	279361.677780	55.230247
2887.921651	279180.902738	55.235252
2886.997573	278989.552655	55.240257
2886.636294	278808.759201	55.245261
2885.726598	278632.152944	55.250266
2885.108254	278437.876434	55.255271
2884.053367	278259.637663	55.260276
2883.806680	278075.871620	55.265281
2883.106509	277899.181146	55.270285
2882.424003	277728.472918	55.275290
2882.024280	277539.841105	55.280295
2881.393709	277365.380763	55.285300
2880.287355	277182.693040	55.290305
2879.685433	276990.654947	55.295309
2879.459843	276815.239041	55.300314
2878.491648	276632.911419	55.305319
2877.410224	276459.082682	55.310324
2876.987125	276282.602866	55.315329
2876.580423	276096.391520	55.320333
2875.836258	275920.319074	55.325338
2875.196181	275741.428618	55.330343
2874.571152	275558.002399	55.335348
2874.003588	275377.546879	55.340353
2873.530574	275191.091313	55.345357
2872.643629	275011.654152	55.350362
2872.078404	274826.410197	55.355367
2871.060069	274646.484471	55.360372
2870.668320	274464.727690	55.365377
2870.068811	274279.820259	55.370381
2869.304295	274105.686618	55.375386
2868.860728	273914.311006	55.380391
2868.031998	273734.864653	55.385396
2867.412287	273545.961914	55.390401
2866.605546	273365.951796	55.395405
2865.971150	273183.571311	55.400410
2865.796265	272987.416099	55.405415
2864.636903	272813.497859	55.410420
2864.079846	272619.720814	55.415425
2864.007116	272442.548889	55.420429
2862.623057	272264.744150	55.425434
2862.632455	272067.642999	55.430439
2861.461327	271877.605246	55.435444
2861.027339	271681.211060	55.440449
2860.148988	271505.898654	55.445453
2859.598969	271321.009124	55.450458
2858.997980	271133.402582	55.455463
2858.066674	270953.361533	55.460468
2857.641728	270767.841055	55.465473
2856.971503	270576.247047	55.470477
2856.375391	270396.382243	55.475482
2855.601216	270206.180060	55.480487
2855.242243	270017.032785	55.485492
2854.373518	269831.608232	55.490497
2853.705886	269649.335419	55.495501
2852.842344	269454.817949	55.500506
2852.274853	269259.948035	55.505511
2851.607007	269088.091925	55.510516
2850.810422	268889.718294	55.515521
2850.041726	268712.046010	55.520525
2849.657686	268530.696375	55.525530
2849.343064	268345.515561	55.530535
2848.569883	268160.178195	55.535540
2847.560528	267965.073008	55.540545
2847.369669	267774.931933	55.545549
2846.392489	267594.669756	55.550554
2846.043611	267400.351571	55.555559
2845.490779	267210.395343	55.560564
2844.647847	267021.885869	55.565569
2843.820677	266822.091559	55.570573
2843.013968	266649.213954	55.575578
2842.529445	266456.496627	55.580583
2841.391144	266266.124094	55.585588
2841.083291	266075.136249	55.590593
2840.435680	265895.382794	55.595597
2839.765626	265706.209755	55.600602
2839.264275	265514.463273	55.605607
2838.244217	265336.959276	55.610612
2837.809982	265149.277226	55.615617
2837.530078	264949.320675	55.620621
2836.646367	264770.445520	55.625626
2836.049560	264578.587241	55.630631
2835.348959	264386.643618	55.635636
2834.993570	264192.811729	55.640641
2834.275744	263998.655308	55.645645
2833.366159	263809.928569	55.650650
2832.657715	263613.529679	55.655655
2831.611127	263422.812862	55.660660
2830.942810	263237.384524	55.665665
2830.557371	263046.308543	55.670669
2829.657315	262867.105810	55.675674
2829.141818	262673.580240	55.680679
2828.443192	262490.041734	55.685684
2827.682276	262297.039135	55.690689
2827.293601	262111.516202	55.695693
2826.503008	261932.653196	55.700698
2826.112888	261736.739820	55.705703
2825.610405	261543.034595	55.710708
2824.502576	261355.206541	55.715713
2824.002224	261153.249653	55.720717
2823.362040	260973.726697	55.725722
2822.934329	260780.035592	55.730727
2821.862016	260592.558950	55.735732
2821.180522	260408.305883	55.740737
2820.424750	260211.993000	55.745741
2819.211454	260026.703815	55.750746
2819.090377	259841.700223	55.755751
2818.620044	259663.526460	55.760756
2817.917364	259475.533627	55.765761
2817.227244	259286.138219	55.770765
2816.545507	259104.814854	55.775770
2815.951350	258924.216309	55.780775
2815.310265	258736.061451	55.785780
2814.804777	258544.472608	55.790785
2813.977630	258353.164056	55.795789
2813.114627	258168.992235	55.800794
2813.028834	257977.744853	55.805799
2811.956845	257788.029032	55.810804
2811.613800	257603.316892	55.815809
2810.986097	257402.478148	55.820813
2810.032351	257211.725370	55.825818
2809.347298	257017.874113	55.830823
2808.554701	256837.206684	55.835828
2807.824103	256649.449657	55.840833
2807.490052	256463.718314	55.845837
2806.454961	256276.697437	55.850842
2806.037607	256086.930300	55.855847
2805.717049	255899.643793	55.860852
2804.808207	255710.769768	55.865857
2804.229577	255519.959046	55.870861
2803.345389	255337.168117	55.875866
2802.831218	255134.912765	55.880871
2801.888897	254947.088885	55.885876
2801.132025	254750.755256	55.890881
2801.183446	254561.806614	55.895885
2800.083125	254376.172988	55.900890
2799.755267	254183.617505	55.905895
2798.751534	254000.159102	55.910900
2797.939574	253808.673863	55.915905
2797.964535	253627.726945	55.920909
2796.757804	253429.071975	55.925914
2796.360806	253237.470659	55.930919
2795.633249	253042.713055	55.935924
2794.935535	252854.343114	55.940929
2794.327860	252660.432799	55.945933
2793.302699	252476.164328	55.950938
2793.292943	252277.983173	55.955943
2792.422482	252094.658330	55.960948
2791.646607	251895.758515	55.965953
2790.984592	251710.592919	55.970957
2790.467868	251504.751024	55.975962
2789.764366	251321.426010	55.980967
2788.959885	251131.292124	55.985972
2788.101867	250939.231464	55.990977
2787.938780	250737.434605	55.995981
2786.886933	250557.196098	56.000986
2786.767185	250360.206004	56.005991
2785.971959	250166.149894	56.010996
2785.336074	249974.793689	56.016001
2784.698335	249783.106938	56.021005
2784.163480	249586.540038	56.026010
2783.366927	249388.232175	56.031015
2782.442111	249189.231813	56.036020
2781.903658	248986.808962	56.041025
2781.208238	248790.064741	56.046029
2780.401149	248597.056523	56.051034
2779.916176	248405.474572	56.056039
2779.505902	248212.072932	56.061044
2778.789876	248018.261565	56.066049
2777.934036	247816.730891	56.071053
2777.186316	247630.692204	56.076058
2776.603548	247414.297568	56.081063
2776.094350	247227.992414	56.086068
2775.290003	247035.291346	56.091073
2774.513662	246830.362444	56.096077
2773.289579	246647.048896	56.101082
2773.171088	246449.452395	56.106087
2772.648893	246257.700845	56.111092
2771.758747	246069.216516	56.116097
2771.242490	245866.590655	56.121101
2770.489585	245669.605025	56.126106
2769.986262	245483.250274	56.131111
2769.476968	245287.703613	56.136116
2768.717393	245097.697442	56.141121
2768.283570	244894.754357	56.146125
2767.416418	244699.163348	56.151130
2766.883302	244495.065170	56.156135
2766.181180	244298.557314	56.161140
2765.480067	244101.158297	56.166145
2764.915871	243905.163953	56.171149
2764.009254	243710.904844	56.176154
2763.599541	243509.207848	56.181159
2762.737387	243316.164621	56.186164
2761.970714	243119.999800	56.191169
2761.316585	242911.212177	56.196173
2760.488768	242721.525812	56.201178
2760.121200	242530.850095	56.206183
2759.538171	242331.983565	56.211188
2758.787582	242139.790266	56.216193
2757.804045	241935.716532	56.221197
2757.103550	241744.381721	56.226202
2756.616832	241541.146693	56.231207
2755.977056	241359.097565	56.236212
2755.220114	241164.614954	56.241217
2754.941145	240970.566251	56.246221
2753.951224	240779.991809	56.251226
2753.187785	240589.712842	56.256231
2752.365543	240389.155760	56.261236
2751.669255	240203.450421	56.266241
2751.014078	240015.217867	56.271245
2750.562147	239820.332641	56.276250
2749.757700	239623.033514	56.281255
2749.385473	239442.625609	56.286260
2748.615804	239252.400732	56.291265
2747.975151	239054.771064	56.296269
2747.579670	238863.061565	56.301274
2746.525875	238659.921325	56.306279
2745.962811	238471.804034	56.311284
2745.183892	238276.132910	56.316289
2744.797744	238075.332552	56.321293
2744.073333	237900.865110	56.326298
2743.281376	237692.261303	56.331303
2742.932426	237504.926591	56.336308
2741.726899	237317.906114	56.341313
2741.087475	237120.992679	56.346317
2740.578594	236940.763247	56.351322
2739.948770	236744.409184	56.356327
2739.477927	236546.808039	56.361332
2738.595917	236363.379309	56.366337
2737.938088	236173.625850	56.371341
2737.490652	235982.082416	56.376346
2737.259265	235772.629647	56.381351
2736.298407	235575.362569	56.386356
2735.519963	235399.201705	56.391361
2735.316512	235195.856921	56.396365
2734.346481	235005.594843	56.401370
2733.363396	234799.904373	56.406375
2732.622664	234604.997851	56.411380
2732.047402	234422.898993	56.416385
2731.429465	234222.448226	56.421389
2730.587682	234041.054316	56.426394
2730.062528	233844.052605	56.431399
2729.482429	233651.694269	56.436404
2728.609215	233465.748494	56.441409
2728.340186	233267.459673	56.446413
2727.723103	233070.779620	56.451418
2727.218555	232867.105306	56.456423
2726.497619	232676.859146	56.461428
2725.627690	232481.569864	56.466433
2725.385141	232284.679306	56.471437
2724.612198	232085.836147	56.476442
2723.929896	231885.502213	56.481447
2723.240370	231675.366755	56.486452
2722.314835	231483.245685	56.491457
2721.711322	231288.069430	56.496461
2721.149356	231088.431079	56.501466
2720.225293	230886.558896	56.506471
2719.875359	230697.072746	56.511476
2718.928235	230506.892244	56.516481
2718.302383	230300.314516	56.521485
2717.304490	230107.214731	56.526490
2716.644927	229908.969349	56.531495
2716.266589	229718.522163	56.536500
2715.550000	229541.292799	56.541505
2715.386226	229343.937682	56.546509
2714.099843	229142.152214	56.551514
2713.329362	228945.988934	56.556519
2713.204957	228756.903968	56.561524
2712.471770	228554.548439	56.566529
2711.882028	228358.714296	56.571533
2711.242921	228170.399579	56.576538
2710.232155	227964.830294	56.581543
2709.876495	227768.985857	56.586548
2708.950255	227580.616052	56.591553
2708.223892	227383.685442	56.596557
2707.710719	227194.487212	56.601562
2707.105013	226986.411813	56.606567
2706.483126	226809.147519	56.611572
2705.636596	226608.825931	56.616577
2705.077505	226410.623479	56.621581
2704.334663	226221.094612	56.626586
2703.733391	226024.567447	56.631591
2703.208504	225826.742871	56.636596
2702.339636	225632.639611	56.641601
2701.927165	225442.436393	56.646605
2701.484598	225239.991777	56.651610
2700.814598	225035.075811	56.656615
2699.911601	224843.042131	56.661620
2699.199864	224647.936074	56.666625
2698.772503	224437.560082	56.671629
2697.752026	224252.535305	56.676634
2697.313013	224044.733683	56.681639
2696.939843	223841.543208	56.686644
2696.020936	223647.885433	56.691649
2695.481958	223445.065945	56.696653
2694.548041	223243.989900	56.701658
2694.038956	223045.558564	56.706663
2693.316584	222847.136053	56.711668
2692.528694	222646.140244	56.716673
2692.215527	222441.339890	56.721677
2691.285474	222250.169653	56.726682
2690.349583	222054.023442	56.731687
2690.400948	221850.796324	56.736692
2689.254542	221664.308191	56.741697
2688.916154	221463.791630	56.746701
2687.976138	221267.011594	56.751706
2687.414219	221065.067572	56.756711
2686.597892	220860.071083	56.761716
2685.461261	220667.002619	56.766721
2685.573304	220471.801956	56.771725
2684.710940	220285.030361	56.776730
2684.033418	220080.357709	56.781735
2683.440350	219879.121932	56.786740
2682.550074	219674.942359	56.791745
2682.041096	219483.355987	56.796749
2681.214572	219291.985897	56.801754
2680.507826	219088.249866	56.806759
2680.066641	218890.773344	56.811764
2679.304264	218701.558620	56.816769
2678.881694	218501.661642	56.821773
2677.953370	218308.668188	56.826778
2677.399806	218099.806252	56.831783
2676.899504	217907.688028	56.836788
2676.109573	217713.108567	56.841793
2675.687147	217514.270827	56.846797
2674.779534	217322.626031	56.851802
2674.161607	217109.474774	56.856807
2673.652109	216913.083751	56.861812
2672.590040	216714.731453	56.866817
2672.241681	216511.187830	56.871821
2671.302336	216315.490289	56.876826
2670.639625	216110.508355	56.881831
2670.152034	215924.325149	56.886836
2669.147550	215724.260893	56.891841
2668.646941	215526.383107	56.896845
2667.966040	215339.557480	56.901850
2667.552767	215142.621615	56.906855
2667.056632	214947.405077	56.911860
2665.846932	214747.172527	56.916865
2665.311764	214550.766826	56.921869
2664.513263	214360.500358	56.926874
2663.744987	214165.303727	56.931879
2663.251828	213972.520665	56.936884
2662.436072	213773.221419	56.941889
2661.835102	213577.859984	56.946893
2661.073648	213393.725453	56.951898
2660.416492	213208.709389	56.956903
2660.333556	213007.234369	56.961908
2659.488786	212824.272891	56.966913
2659.147615	212609.284470	56.971917
2658.336810	212423.900379	56.976922
2657.354741	212221.462863	56.981927
2656.942773	212027.017966	56.986932
2656.118808	211836.457321	56.991937
2655.600176	211621.360266	56.996941
2655.119423	211441.896106	57.001946
2653.974147	211241.663987	57.006951
2653.493882	211038.845212	57.011956
2652.808584	210845.630872	57.016961
2652.423771	210637.096195	57.021965
2651.593303	210450.155387	57.026970
2650.978413	210253.355203	57.031975
2650.421458	210046.084329	57.036980
2649.596624	209853.773329	57.041985
2648.947289	209642.560135	57.046989
2648.110398	209456.590592	57.051994
2647.480949	209261.768592	57.056999
2647.225598	209063.884258	57.062004
2646.394416	208869.286360	57.067009
2645.774302	208670.391970	57.072013
2645.303332	208465.492751	57.077018
2644.245834	208267.534413	57.082023
2643.724729	208076.389902	57.087028
2643.166903	207875.528226	57.092033
2642.515874	207668.827485	57.097037
2641.878999	207472.739619	57.102042
2641.094917	207268.428567	57.107047
2640.636669	207064.397488	57.112052
2640.052375	206866.585113	57.117057
2639.150205	206664.623858	57.122061
2638.779677	206462.184526	57.127066
2637.917090	206263.107365	57.132071
2637.364257	206059.756495	57.137076
2636.536603	205861.184221	57.142081
2635.908599	205645.425355	57.147085
2635.725632	205447.897740	57.152090
2634.633188	205241.440781	57.157095
2634.156185	205041.364884	57.162100
2633.017247	204843.163533	57.167105
2632.289177	204632.005811	57.172109
2632.038441	204440.397438	57.177114
2631.159745	204240.044323	57.182119
2630.636180	204034.506910	57.187124
2629.833347	203840.506353	57.192129
2629.310278	203629.828871	57.197133
2628.405935	203430.666185	57.202138
2627.833101	203233.818745	57.207143
2627.507289	203028.419054	57.212148
2626.632510	202836.011351	57.217153
2625.975500	202628.476691	57.222157
2625.233812	202432.371445	57.227162
2624.439165	202227.914310	57.232167
2623.915459	202027.041882	57.237172
2623.394043	201831.501955	57.242177
2622.854724	201627.273804	57.247181
2621.720778	201424.196852	57.252186
2621.046704	201228.110570	57.257191
2620.673642	201023.336543	57.262196
2619.687348	200831.576968	57.267201
2619.449124	200633.005871	57.272205
2618.588222	200429.723884	57.277210
2618.032313	200229.308473	57.282215
2617.488302	200027.835697	57.287220
2616.686440	199832.512721	57.292225
2616.051655	199620.302858	57.297229
2615.649209	199417.982766	57.302234
2614.742282	199214.738062	57.307239
2614.061818	199015.835723	57.312244
2613.369905	198814.810828	57.317249
2612.875062	198616.160514	57.322253
2611.991656	198415.638288	57.327258
2611.333412	198215.768294	57.332263
2610.959998	198015.357648	57.337268
2609.955216	197807.132881	57.342273
2609.633819	197595.772134	57.347277
2608.943820	197400.058561	57.352282
2607.816831	197199.846753	57.357287
2607.134724	196997.847382	57.362292
2606.467100	196797.157139	57.367297
2605.770425	196611.589150	57.372301
2605.660314	196407.452765	57.377306
2604.580853	196207.529899	57.382311
2603.817994	196001.004523	57.387316
2603.225407	195817.331558	57.392321
2602.706642	195607.257133	57.397325
2602.252085	195406.703931	57.402330
2601.166429	195207.422143	57.407335
2600.956693	195007.862380	57.412340
2600.031561	194811.025209	57.417345
2599.523917	194606.742641	57.422349
2598.627574	194410.907666	57.427354
2598.336568	194210.104222	57.432359
2597.546851	194007.904610	57.437364
2596.781273	193803.691599	57.442369
2596.651508	193600.460208	57.447373
2596.026338	193388.948566	57.452378
2594.971309	193187.328696	57.457383
2594.549362	192986.423652	57.462388
2593.380413	192790.956282	57.467393
2593.006781	192577.792317	57.472397
2592.300056	192370.522173	57.477402
2591.504518	192165.900741	57.482407
2591.134946	191966.073035	57.487412
2590.081343	191768.644742	57.492417
2589.574871	191560.150277	57.497421
2588.732040	191360.629045	57.502426
2587.905415	191165.457420	57.507431
2587.753819	190953.245014	57.512436
2586.764829	190766.014562	57.517441
2586.243113	190557.399573	57.522445
2585.742333	190351.619408	57.527450
2584.693858	190153.408032	57.532455
2584.483796	189953.156183	57.537460
2583.532783	189757.424696	57.542465
2582.937803	189555.568797	57.547469
2582.341961	189346.856301	57.552474
2581.403940	189141.519573	57.557479
2581.085499	188948.452008	57.562484
2580.263380	188750.312370	57.567489
2579.466430	188543.569110	57.572493
2579.122587	188345.660726	57.577498
2578.400251	188152.762188	57.582503
2577.693825	187940.791017	57.587508
2576.530756	187748.612820	57.592513
2575.988201	187539.619976	57.597517
2575.315540	187344.350548	57.602522
2574.809500	187155.416638	57.607527
2574.533950	186947.020254	57.612532
2573.813220	186754.877846	57.617537
2573.277806	186545.137739	57.622541
2572.450441	186344.986330	57.627546
2571.761397	186140.030431	57.632551
2571.375561	185929.162621	57.637556
2570.339202	185746.717608	57.642561
2570.041117	185535.430609	57.647565
2569.423258	185333.812860	57.652570
2568.600145	185124.124844	57.657575
2567.957544	184915.414198	57.662580
2567.149518	184719.312313	57.667585
2566.593371	184507.752947	57.672589
2565.727055	184313.939203	57.677594
2565.137338	184099.868232	57.682599
2564.807401	183889.764324	57.687604
2563.767031	183690.879613	57.692609
2563.206489	183482.238938	57.697613
2562.498774	183275.518007	57.702618
2561.877116	183077.841794	57.707623
2561.410225	182879.938399	57.712628
2560.744928	182679.306883	57.717633
2559.988100	182467.890750	57.722637
2559.481494	182262.974483	57.727642
2558.427667	182055.665335	57.732647
2558.069384	181842.700722	57.737652
2557.022793	181642.032591	57.742657
2556.412976	181441.537861	57.747661
2555.749040	181242.032110	57.752666
2555.091101	181034.703233	57.757671
2554.590122	180832.604003	57.762676
2553.784048	180638.720527	57.767681
2553.140309	180433.758262	57.772685
2552.480386	180229.460987	57.777690
2551.834078	180030.288753	57.782695
2551.385759	179826.926590	57.787700
2550.516312	179631.760241	57.792705
2549.970458	179424.841109	57.797709
2549.234847	179222.214227	57.802714
2548.600788	179014.560587	57.807719
2548.223389	178801.105216	57.812724
2546.947393	178608.424745	57.817729
2546.282731	178398.807409	57.822733
2545.740556	178213.351712	57.827738
2545.250379	178011.912809	57.832743
2544.883228	177805.558364	57.837748
2543.939970	177605.503318	57.842753
2543.033649	177399.732371	57.847757
2542.706808	177192.598675	57.852762
2541.963932	176996.661288	57.857767
2541.619495	176795.472249	57.862772
2540.905973	176595.258451	57.867777
2540.283459	176380.238915	57.872781
2539.331914	176175.218902	57.877786
2538.285703	175979.894028	57.882791
2538.268731	175764.819894	57.887796
2537.512366	175569.272973	57.892801
2536.377064	175363.281340	57.897805
2536.132024	175162.224422	57.902810
2535.188151	174969.495477	57.907815
2534.825532	174753.196847	57.912820
2533.987991	174556.980834	57.917825
2533.452516	174358.962755	57.922829
2532.767218	174150.603906	57.927834
2532.033080	173949.694084	57.932839
2531.909950	173729.712806	57.937844
2531.023168	173533.420536	57.942849
2530.423383	173327.379817	57.947853
2529.693907	173120.686653	57.952858
2528.874979	172918.307412	57.957863
2528.188584	172698.471922	57.962868
2527.520282	172507.110052	57.967873
2526.886612	172297.188352	57.972877
2526.510563	172089.986681	57.977882
2525.632739	171894.629448	57.982887
2524.987609	171679.485878	57.987892
2524.157014	171468.467915	57.992897
2523.462708	171270.083355	57.997901
2522.974666	171059.928953	58.002906
2522.489672	170850.182148	58.007911
2521.743997	170643.631658	58.012916
2520.903306	170447.321941	58.017921
2520.217393	170240.649658	58.022925
2519.531684	170021.744632	58.027930
2518.544348	169822.256611	58.032935
2518.173831	169611.748028	58.037940
2517.309563	169412.903893	58.042945
2516.629301	169217.795790	58.047949
2516.200856	169017.218725	58.052954
2515.454215	168814.709335	58.057959
2514.946666	168604.037222	58.062964
2513.763821	168406.393273	58.067969
2513.339401	168207.269488	58.072973
2512.749768	168006.723257	58.077978
2511.919917	167811.671454	58.082983
2511.620922	167605.842148	58.087988
2510.643397	167406.034520	58.092993
2510.139944	167212.421862	58.097997
2509.565439	167005.304288	58.103002
2508.721607	166801.969034	58.108007
2508.186051	166594.860258	58.113012
2507.530158	166399.330398	58.118017
2507.278484	166204.691178	58.123021
2506.579729	165990.617919	58.128026
2505.366552	165792.610975	58.133031
2505.099066	165585.528870	58.138036
2504.689460	165383.480347	58.143041
2503.702619	165181.562553	58.148045
2502.934152	164968.943058	58.153050
2502.377723	164766.514272	58.158055
2502.029934	164554.313668	58.163060
2501.420674	164348.449721	58.168065
2500.593443	164081.767162	58.173069
2500.119768	163870.734802	58.178074
2499.328863	163663.275964	58.183079
2498.837501	163438.249783	58.188084
2498.255144	163241.873048	58.193089
2497.279839	163031.980356	58.198093
2496.625388	162807.378071	58.203098
2495.880062	162609.364964	58.208103
2495.299542	162392.026251	58.213108
2494.307052	162200.678790	58.218113
2493.727690	161988.504366	58.223117
2493.319760	161782.737432	58.228122
2492.498749	161579.541836	58.233127
2491.724946	161370.109995	58.238132
2491.516810	161169.209839	58.243137
2490.804534	160959.465510	58.248141
2490.124756	160749.450270	58.253146
2489.175289	160540.063846	58.258151
2488.334429	160330.585158	58.263156
2487.741970	160133.286167	58.268161
2487.329751	159918.364094	58.273165
2486.787648	159707.544949	58.278170
2485.914840	159512.607709	58.283175
2485.328705	159306.374778	58.288180
2484.476056	159097.858762	58.293185
2483.640897	158889.214079	58.298189
2482.889652	158678.968195	58.303194
2482.105958	158483.374171	58.308199
2481.792179	158271.230717	58.313204
2480.996596	158077.344392	58.318209
2480.155307	157879.283862	58.323213
2479.546681	157670.775820	58.328218
2478.682888	157479.840289	58.333223
2478.123135	157277.632365	58.338228
2477.699950	157080.018636	58.343233
2476.882059	156871.650273	58.348237
2476.307082	156681.855633	58.353242
2475.479899	156480.050717	58.358247
2474.835461	156277.518847	58.363252
2474.387362	156081.275010	58.368257
2473.759007	155883.255747	58.373261
2472.931452	155686.438711	58.378266
2472.436904	155487.154755	58.383271
2471.864525	155287.185146	58.388276
2471.318790	155087.644692	58.393281
2470.671831	154883.952001	58.398285
2469.851875	154681.304887	58.403290
2469.252058	154486.530705	58.408295
2468.830703	154275.534886	58.413300
2468.303373	154071.980661	58.418305
2467.343945	153869.818137	58.423309
2466.971019	153665.161435	58.428314
2466.011830	153458.260042	58.433319
2465.283567	153241.624736	58.438324
2464.657366	153041.054127	58.443329
2463.864066	152830.723763	58.448333
2463.213105	152625.634472	58.453338
2462.533921	152440.722981	58.458343
2462.011747	152225.014927	58.463348
2461.303449	152027.119986	58.468353
2460.062102	151825.472122	58.473357
2459.769124	151620.840726	58.478362
2459.250449	151428.092489	58.483367
2458.801705	151229.169774	58.488372
2458.215910	151015.132050	58.493377
2457.205825	150823.965057	58.498381
2456.551465	150608.402920	58.503386
2455.518092	150411.128466	58.508391
2455.507868	150207.325337	58.513396
2454.435602	150003.107167	58.518401
2453.656888	149806.558597	58.523405
2453.269082	149601.942127	58.528410
2452.766048	149403.115388	58.533415
2451.991948	149210.890971	58.538420
2451.343587	149006.370399	58.543425
2450.348899	148798.245709	58.548429
2450.018925	148598.265349	58.553434
2449.294644	148410.905471	58.558439
2448.607323	148195.161245	58.563444
2448.164154	148001.671504	58.568449
2447.170418	147799.678910	58.573453
2446.582544	147593.912250	58.578458
2445.926717	147408.911239	58.583463
2445.050273	147203.040335	58.588468
2444.650726	146996.815576	58.593473
2444.049934	146801.858465	58.598477
2443.895089	146584.414016	58.603482
2442.533674	146403.724513	58.608487
2442.274727	146190.289724	58.613492
2441.669001	145988.399634	58.618497
2441.113171	145778.051972	58.623501
2440.132858	145567.112179	58.628506
2439.563327	145365.614295	58.633511
2439.175782	145171.357807	58.638516
2437.976991	144965.209467	58.643521
2437.541816	144760.936564	58.648525
2436.872995	144554.300277	58.653530
2435.985458	144352.173110	58.658535
2435.539818	144156.242027	58.663540
2434.723171	143943.342992	58.668545
2433.940652	143747.760156	58.673549
2433.441205	143538.003172	58.678554
2432.521447	143347.095490	58.683559
2431.805466	143150.476597	58.688564
2431.434772	142961.479281	58.693569
2430.817966	142749.497107	58.698573
2430.376961	142545.951307	58.703578
2429.279486	142352.066432	58.708583
2428.569810	142150.319384	58.713588
2428.271846	141949.016666	58.718593
2427.269502	141755.946418	58.723597
2426.796375	141548.397068	58.728602
2426.004418	141342.106778	58.733607
2425.582860	141135.479632	58.738612
2424.798640	140946.966908	58.743617
2424.443788	140753.457310	58.748621
2423.763202	140546.582993	58.753626
2422.681768	140348.566160	58.758631
2422.294543	140132.601525	58.763636
2421.650232	139937.910562	58.768641
2420.767617	139732.280902	58.773645
2420.261151	139526.986894	58.778650
2419.611983	139322.110783	58.783655
2419.076091	139117.497634	58.788660
2418.212297	138920.395910	58.793665
2417.460710	138720.787465	58.798669
2417.175517	138517.129695	58.803674
2416.144032	138312.537098	58.808679
2415.475473	138109.476503	58.813684
2415.090446	137909.675630	58.818689
2414.213976	137717.399049	58.823693
2413.914273	137510.650492	58.828698
2413.113342	137305.558215	58.833703
2412.314625	137092.729922	58.838708
2411.699759	136897.431629	58.843713
2410.988731	136701.679811	58.848717
2410.526255	136488.777171	58.853722
2409.329638	136291.720294	58.858727
2409.011213	136085.137159	58.863732
2408.498373	135878.929311	58.868737
2407.782015	135685.014511	58.873741
2407.114726	135480.739554	58.878746
2406.462707	135284.073182	58.883751
2405.978922	135078.399946	58.888756
2405.027738	134872.103562	58.893761
2404.340344	134677.619220	58.898765
2404.107000	134462.586255	58.903770
2403.443283	134262.346292	58.908775
2402.401340	134049.959845	58.913780
2401.897015	133851.602951	58.918785
2401.099934	133654.614954	58.923789
2400.484897	133442.114501	58.928794
2399.574765	133237.042783	58.933799
2399.178427	133032.526220	58.938804
2398.548793	132828.988102	58.943809
2397.590213	132637.761619	58.948813
2397.536825	132431.721477	58.953818
2396.415867	132236.903199	58.958823
2395.951085	132019.448241	58.963828
2395.416155	131817.337697	58.968833
2394.319577	131613.209071	58.973837
2393.779327	131412.270855	58.978842
2393.275942	131216.320106	58.983847
2392.709705	131006.472092	58.988852
2392.240026	130793.955652	58.993857
2391.517984	130588.123818	58.998861
2390.983605	130378.313533	59.003866
2389.942257	130180.257891	59.008871
2389.494486	129965.927914	59.013876
2388.985168	129753.285910	59.018881
2388.063800	129544.063973	59.023885
2387.343725	129335.294335	59.028890
2386.497514	129128.870549	59.033895
2386.096121	128921.437901	59.038900
2385.448907	128730.861718	59.043905
2384.688707	128523.336514	59.048909
2384.267103	128306.398781	59.053914
2383.343772	128103.347820	59.058919
2382.718538	127901.444936	59.063924
2382.198888	127693.849711	59.068929
2381.445729	127485.099241	59.073933
2380.975535	127268.431366	59.078938
2380.261029	127065.723243	59.083943
2379.683434	126846.230899	59.088948
2378.975726	126643.270818	59.093953
2378.228172	126446.757366	59.098957
2377.715490	126230.523517	59.103962
2377.110076	126020.592394	59.108967
2376.413335	125800.416153	59.113972
2375.723292	125587.657089	59.118977
2374.954654	125377.972687	59.123981
2374.540890	125168.665416	59.128986
2373.634228	124967.451054	59.133991
2372.993693	124761.230674	59.138996
2372.538531	124535.019756	59.144001
2371.558007	124328.475613	59.149005
2371.188195	124114.051907	59.154010
2370.138258	123911.737943	59.159015
2369.722831	123699.966083	59.164020
2369.270786	123481.598515	59.169025
2368.213642	123277.690471	59.174029
2367.885454	123072.335093	59.179034
2366.808196	122859.417682	59.184039
2366.093638	122645.022285	59.189044
2365.876693	122437.927215	59.194049
2364.641256	122221.408371	59.199053
2364.340662	122022.545293	59.204058
2363.832808	121815.412309	59.209063
2363.042358	121596.897966	59.214068
2362.605249	121401.095902	59.219073
2361.669840	121188.410646	59.224077
2361.024669	120983.058181	59.229082
2360.039531	120777.393000	59.234087
2359.607126	120566.334428	59.239092
2359.391937	120347.828101	59.244097
2358.115131	120150.835282	59.249101
2357.623402	119929.976577	59.254106
2357.074226	119725.939175	59.259111
2356.343255	119523.347851	59.264116
2355.643234	119305.847584	59.269121
2354.993908	119105.595397	59.274125
2354.325226	118896.428718	59.279130
2353.874963	118689.895276	59.284135
2353.097130	118476.832525	59.289140
2352.425649	118261.894710	59.294145
2351.506523	118054.767780	59.299149
2351.154317	117843.889909	59.304154
2350.226406	117646.327518	59.309159
2349.821359	117439.028798	59.314164
2349.149204	117223.890249	59.319169
2348.630320	117021.049988	59.324173
2348.083586	116798.341406	59.329178
2347.139048	116594.664296	59.334183
2346.297400	116382.441457	59.339188
2345.942486	116167.547099	59.344193
2345.081383	115960.992761	59.349197
2344.551852	115746.104245	59.354202
2344.102780	115545.987610	59.359207
2343.198639	115338.207422	59.364212
2342.593175	115118.010917	59.369217
2341.696208	114911.293062	59.374221
2341.229181	114698.904255	59.379226
2340.471186	114492.288379	59.384231
2339.986887	114286.017959	59.389236
2339.390518	114072.759995	59.394241
2338.531788	113860.808459	59.399245
2338.135023	113645.427995	59.404250
2337.632461	113444.276542	59.409255
2336.679160	113224.551543	59.414260
2335.896711	113008.647449	59.419265
2335.299845	112801.194842	59.424269
2334.566913	112574.224526	59.429274
2334.128771	112366.394952	59.434279
2333.237410	112160.695217	59.439284
2332.893448	111945.587549	59.444289
2331.807194	111732.408143	59.449293
2331.432688	111515.944574	59.454298
2330.675889	111315.148856	59.459303
2329.704992	111105.878504	59.464308
2329.521143	110901.454131	59.469313
2328.424027	110690.366936	59.474317
2328.096750	110476.335505	59.479322
2327.222020	110265.572058	59.484327
2326.654014	110057.725313	59.489332
2325.883623	109846.231827	59.494337
2325.571094	109634.318543	59.499341
2324.780387	109414.753810	59.504346
2323.895263	109211.006748	59.509351
2323.429652	109003.501709	59.514356
2322.957633	108782.515116	59.519361
2322.040529	108572.083881	59.524365
2321.598749	108359.199546	59.529370
2320.894318	108148.744592	59.534375
2320.278646	107941.088373	59.539380
2319.717232	107715.791765	59.544385
2319.221919	107508.818142	59.549389
2318.383402	107291.564413	59.554394
2317.607849	107074.822952	59.559399
2316.685000	106856.241344	59.564404
2316.539426	106628.350900	59.569409
2315.780248	106438.845323	59.574413
2314.885876	106204.719983	59.579418
2314.353629	105996.705592	59.584423
2313.447493	105790.452692	59.589428
2313.167455	105561.971891	59.594433
2312.577331	105356.421296	59.599437
2311.725159	105134.240387	59.604442
2311.091871	104920.141517	59.609447
2310.257335	104703.849564	59.614452
2310.057464	104492.439318	59.619457
2308.935273	104274.515606	59.624461
2308.430092	104048.730608	59.629466
2307.857085	103839.225196	59.634471
2306.943007	103620.018334	59.639476
2306.697054	103396.964512	59.644481
2305.583283	103188.273848	59.649485
2304.950501	102960.305383	59.654490
2304.279671	102759.281646	59.659495
2303.651671	102543.509574	59.664500
2303.077699	102319.839159	59.669505
2302.519245	102113.398163	59.674509
2302.305828	101884.314214	59.679514
2301.146685	101668.602695	59.684519
2300.297024	101459.054495	59.689524
2300.021299	101241.030971	59.694529
2299.169735	101015.577407	59.699533
2298.654459	100795.769105	59.704538
2297.632121	100590.303212	59.709543
2297.175449	100382.611732	59.714548
2296.751784	100162.515785	59.719553
2295.588953	99934.933638	59.724557
2295.182494	99712.593742	59.729562
2294.472905	99508.978097	59.734567
2293.756511	99297.506310	59.739572
2293.175453	99073.379804	59.744577
2292.364420	98863.056060	59.749581
2291.776420	98645.074763	59.754586
2291.271074	98432.213743	59.759591
2290.587615	98209.101374	59.764596
2290.105089	97987.367386	59.769601
2289.305357	97779.385883	59.774605
2288.503148	97551.351520	59.779610
2288.025923	97329.749918	59.784615
2287.231336	97125.274610	59.789620
2286.955465	96899.395832	59.794625
2285.953889	96684.574856	59.799629
2285.626222	96466.370100	59.804634
2284.601572	96248.303340	59.809639
2283.992766	96033.717980	59.814644
2283.569490	95811.247415	59.819649
2282.990040	95594.803338	59.824653
2281.989920	95359.034399	59.829658
2281.342343	95152.460739	59.834663
2280.507807	94932.772034	59.839668
2279.890523	94712.270986	59.844673
2279.547701	94484.480023	59.849677
2278.648057	94275.734801	59.854682
2278.189753	94058.125776	59.859687
2277.501192	93840.999286	59.864692
2276.929749	93619.372930	59.869697
2276.095970	93409.242914	59.874701
2275.603181	93174.976462	59.879706
2274.953911	92957.871357	59.884711
2274.161712	92741.158826	59.889716
2273.536521	92514.529759	59.894721
2272.895966	92294.265531	59.899725
2272.342110	92073.602942	59.904730
2271.501407	91859.607985	59.909735
2270.917206	91634.807607	59.914740
2270.550734	91407.191371	59.919745
2269.776248	91193.141644	59.924750
2269.104553	90966.840168	59.929754
2268.260386	90735.578305	59.934759
2267.099911	90520.556476	59.939764
2266.514655	90298.648520	59.944769
2266.035809	90082.178704	59.949774
2265.405504	89862.748735	59.954778
2264.756387	89660.550561	59.959783
2264.444753	89445.119362	59.964788
2263.512982	89216.956111	59.969793
2262.376089	89004.500546	59.974798
2262.008348	88783.245538	59.979802
2261.615028	88567.544329	59.984807
2260.720395	88346.428051	59.989812
2260.122528	88126.769509	59.994817
2259.401140	87906.314950	59.999822
2258.956479	87694.491506	60.004826
2258.473443	87480.045259	60.009831
2257.855124	87253.805569	60.014836
2257.268847	87026.637598	60.019841
2256.622785	86803.602163	60.024846
2255.745746	86584.086007	60.029850
2254.969243	86366.996798	60.034855
2254.283948	86143.911041	60.039860
2254.326493	85922.537866	60.044865
2253.349655	85699.521992	60.049870
2252.164388	85477.828336	60.054874
2251.714278	85248.629098	60.059879
2250.690622	85036.441937	60.064884
2250.198672	84807.374519	60.069889
2249.544488	84591.703859	60.074894
2248.844365	84379.237405	60.079898
2248.389618	84158.969266	60.084903
2247.548719	83937.420871	60.089908
2247.100743	83719.431792	60.094913
2246.128947	83500.152584	60.099918
2246.029355	83274.893293	60.104922
2245.028838	83067.197102	60.109927
2244.137265	82844.166017	60.114932
2243.944618	82621.463782	60.119937
2242.796564	82406.812783	60.124942
2242.045025	82180.863646	60.129946
2241.592534	81964.744160	60.134951
2240.900523	81751.973307	60.139956
2240.357001	81530.339698	60.144961
2239.540591	81315.634603	60.149966
2238.928280	81093.002489	60.154970
2238.534653	80875.414562	60.159975
2237.540196	80668.039065	60.164980
2237.033653	80441.144587	60.169985
2236.446150	80222.288698	60.174990
2235.489847	80002.859866	60.179994
2234.991522	79782.321390	60.184999
2234.147703	79569.749008	60.190004
2233.750323	79352.868393	60.195009
2232.898886	79131.809829	60.200014
2232.212981	78925.537183	60.205018
2231.672419	78712.646691	60.210023
2230.917926	78493.803891	60.215028
2230.676655	78269.039393	60.220033
2229.499858	78048.044066	60.225038
2229.065764	77834.835267	60.230042
2228.221886	77615.534407	60.235047
2227.516385	77403.925629	60.240052
2227.100847	77181.405837	60.245057
2226.322139	76966.733624	60.250062
2225.804103	76747.947998	60.255066
2225.276811	76533.170769	60.260071
2224.296518	76317.675617	60.265076
2224.115535	76091.163993	60.270081
2223.127603	75872.227868	60.275086
2222.533359	75656.196951	60.280090
2221.769253	75442.628311	60.285095
2221.002785	75222.624966	60.290100
2220.506212	75000.173567	60.295105
2219.435144	74789.505323	60.300110
2218.920548	74573.707756	60.305114
2218.487565	74357.012557	60.310119
2217.673854	74147.875111	60.315124
2217.257227	73930.833444	60.320129
2216.320275	73719.927036	60.325134
2215.412014	73497.500510	60.330138
2215.331792	73273.050845	60.335143
2214.308832	73060.340439	60.340148
2213.913779	72843.826603	60.345153
2213.098898	72635.889795	60.350158
2212.254495	72413.199117	60.355162
2211.959800	72202.460235	60.360167
2211.052944	71998.630736	60.365172
2210.671983	71768.303507	60.370177
2209.949124	71554.997754	60.375182
2209.047821	71343.407635	60.380186
2208.625722	71127.201811	60.385191
2207.576917	70907.404685	60.390196
2207.562883	70678.507862	60.395201
2206.606830	70475.379615	60.400206
2205.691868	70247.580854	60.405210
2205.215972	70037.761524	60.410215
2204.284768	69828.327025	60.415220
2203.743988	69609.116202	60.420225
2203.223301	69389.524589	60.425230
2202.738723	69169.708010	60.430234
2202.212425	68962.384751	60.435239
2201.347933	68741.461451	60.440244
2200.853618	68513.242367	60.445249
2199.823749	68295.555247	60.450254
2199.408688	68076.892649	60.455258
2198.834651	67863.653951	60.460263
2197.823365	67652.906355	60.465268
2197.194593	67426.805036	60.470273
2196.743480	67205.801880	60.475278
2195.769499	66987.404838	60.480282
2195.388948	66779.099994	60.485287
2194.484133	66571.767195	60.490292
2193.901559	66343.954864	60.495297
2193.126102	66137.888648	60.500302
2192.670318	65918.357509	60.505306
2192.313491	65704.183470	60.510311
2191.393819	65488.093582	60.515316
2190.530011	65277.541590	60.520321
2190.078588	65059.561564	60.525326
2189.401528	64840.327945	60.530330
2188.494823	64620.908450	60.535335
2187.690414	64416.818834	60.540340
2187.267295	64196.048329	60.545345
2186.527758	63983.220653	60.550350
2185.823258	63767.404123	60.555354
2185.501800	63561.043393	60.560359
2184.124847	63346.025340	60.565364
2183.817678	63129.921866	60.570369
2183.200397	62925.365753	60.575374
2182.398922	62711.257701	60.580378
2182.118628	62491.383390	60.585383
2181.158927	62292.878324	60.590388
2180.815709	62066.294573	60.595393
2179.694818	61857.210878	60.600398
2178.910329	61647.458803	60.605402
2178.596638	61424.987224	60.610407
2177.666153	61228.593904	60.615412
2177.229845	61011.597997	60.620417
2176.379089	60805.864028	60.625422
2175.411308	60604.025571	60.630426
2174.825217	60382.967538	60.635431
2173.914913	60199.244028	60.640436
2173.648788	59983.616315	60.645441
2172.850371	59773.124434	60.650446
2172.258827	59573.500677	60.655450
2172.058744	59354.856226	60.660455
2170.967799	59161.263866	60.665460
2170.572967	58947.836764	60.670465
2170.022103	58751.706681	60.675470
2169.117569	58538.016940	60.680474
2168.730811	58328.020454	60.685479
2167.684100	58117.539140	60.690484
2167.268312	57910.217060	60.695489
2166.571669	57705.863247	60.700494
2165.756464	57497.729232	60.705498
2165.460019	57283.634608	60.710503
2164.567648	57077.869177	60.715508
2163.636294	56871.080437	60.720513
2163.195710	56667.551999	60.725518
2162.303040	56455.381383	60.730522
2161.835823	56253.403043	60.735527
2160.900461	56053.976079	60.740532
2160.718367	55834.417608	60.745537
2159.647388	55632.655788	60.750542
2158.915914	55434.829878	60.755546
2158.274758	55222.234822	60.760551
2157.692281	55022.775725	60.765556
2156.996437	54817.934778	60.770561
2156.051520	54625.537644	60.775566
2155.487168	54427.430270	60.780570
2155.291040	54214.133912	60.785575
2154.288611	54022.514899	60.790580
2153.494840	53814.599541	60.795585
2153.093599	53612.250604	60.800590
2152.044264	53418.493586	60.805594
2151.586815	53210.553921	60.810599
2150.974207	53014.241593	60.815604
2150.291017	52815.335224	60.820609
2149.518450	52611.018550	60.825614
2148.551470	52422.103550	60.830618
2148.324993	52231.032155	60.835623
2147.297191	52041.023323	60.840628
2146.893012	51830.648322	60.845633
2146.281145	51633.882553	60.850638
2145.394091	51436.577242	60.855642
2144.958361	51248.982404	60.860647
2144.047052	51049.638073	60.865652
2143.117860	50854.241042	60.870657
2142.409708	50660.687258	60.875662
2141.694257	50478.824021	60.880666
2141.145724	50285.663423	60.885671
2140.201120	50099.259167	60.890676
2139.759948	49911.182446	60.895681
2138.691784	49740.512778	60.900686
2137.919392	49552.957440	60.905690
2137.356492	49366.573028	60.910695
2136.807431	49193.023227	60.915700
2136.172441	49010.102337	60.920705
2135.089610	48832.290778	60.925710
2134.574734	48655.782847	60.930714
2134.090588	48475.902655	60.935719
2132.804193	48309.890540	60.940724
2132.866158	48128.721933	60.945729
2131.891533	47963.501908	60.950734
2130.924412	47791.306966	60.955738
2130.156746	47617.326391	60.960743
2129.449745	47452.824712	60.965748
2128.719988	47287.135609	60.970753
2127.727718	47125.548179	60.975758
2127.135963	46962.940222	60.980762
2126.416892	46802.362601	60.985767
2125.453350	46661.111147	60.990772
2124.715983	46506.365708	60.995777
2124.010494	46348.387018	61.000782
2122.975836	46204.148706	61.005786
2122.436037	46053.601806	61.010791
2121.746300	45921.216908	61.015796
2120.786216	45774.158341	61.020801
2120.020514	45635.480580	61.025806
2119.230942	45509.197078	61.030810
2118.360002	45375.415381	61.035815
2117.662636	45255.878305	61.040820
2117.012054	45122.408339	61.045825
2116.346133	44994.037228	61.050830
2115.225492	44873.791850	61.055834
2114.989803	44746.881956	61.060839
2114.004559	44630.516551	61.065844
2113.535317	44507.671717	61.070849
2112.675843	44396.003650	61.075854
2111.958270	44265.833817	61.080858
2111.663927	44154.589997	61.085863
2110.932252	44042.666713	61.090868
2110.214573	43922.060343	61.095873
2109.508006	43807.775219	61.100878
2108.665717	43688.259223	61.105882
2108.455221	43565.126967	61.110887
2107.302991	43454.058528	61.115892
2106.841984	43327.539440	61.120897
2106.194420	43218.998400	61.125902
2105.451104	43110.998214	61.130906
2105.178634	42986.039297	61.135911
2104.390779	42878.578928	61.140916
2103.514774	42766.402144	61.145921
2103.167483	42652.197286	61.150926
2102.580536	42539.444816	61.155930
2102.094146	42421.380078	61.160935
2101.467850	42299.426462	61.165940
2100.744127	42174.924482	61.170945
2100.041316	42057.538528	61.175950
2098.991089	41946.586914	61.180954
2098.671585	41822.839218	61.185959
2097.891002	41715.062376	61.190964
2097.416168	41597.665517	61.195969
2096.817415	41479.068492	61.200974
2095.872438	41363.234081	61.205978
2095.325495	41243.732386	61.210983
2094.472073	41129.349123	61.215988
2094.039317	41020.171193	61.220993
2093.721261	40893.002166	61.225998
2092.795854	40781.339431	61.231002
2092.548200	40658.875681	61.236007
2091.392694	40542.985344	61.241012
2090.792383	40426.795841	61.246017
2090.631125	40307.328001	61.251022
2089.682971	40190.749445	61.256026
2089.113348	40066.867515	61.261031
2088.017131	39957.543919	61.266036
2087.574973	39840.127013	61.271041
2087.347750	39724.265674	61.276046
2086.038671	39606.521546	61.281050
2085.540722	39477.298393	61.286055
2084.823812	39363.268881	61.291060
2084.312040	39244.363654	61.296065
2083.744412	39126.256991	61.301070
2083.216284	39023.381541	61.306074
2082.380936	38896.132372	61.311079
2081.724503	38780.589000	61.316084
2081.077965	38665.697739	61.321089
2080.282034	38538.180989	61.326094
2079.851432	38435.208254	61.331098
2079.345440	38312.584158	61.336103
2078.787634	38201.529693	61.341108
2078.075344	38076.181509	61.346113
2077.669813	37954.628490	61.351118
2076.669295	37838.093317	61.356122
2075.912156	37706.272185	61.361127
2075.039075	37599.988715	61.366132
2074.138767	37468.029338	61.371137
2073.862308	37354.246925	61.376142
2073.236932	37253.651768	61.381146
2072.756346	37122.606958	61.386151
2071.798404	37011.687018	61.391156
2070.963590	36903.143027	61.396161
2070.504607	36786.922766	61.401166
2069.958979	36666.864946	61.406170
2069.582240	36541.142952	61.411175
2068.836822	36427.915393	61.416180
2067.996044	36298.412049	61.421185
2067.549941	36184.590149	61.426190
2066.781980	36068.005007	61.431194
2066.367404	35955.214961	61.436199
2065.631264	35830.462573	61.441204
2064.303603	35718.702559	61.446209
2063.873482	35591.946617	61.451214
2063.468697	35469.968815	61.456218
2062.732273	35350.051826	61.461223
2062.005838	35237.526301	61.466228
2061.228223	35114.355298	61.471233
2060.841740	35004.695051	61.476238
2060.233237	34899.905532	61.481242
2059.276880	34769.220080	61.486247
2058.633104	34650.331788	61.491252
2057.616324	34534.904714	61.496257
2057.402706	34419.175558	61.501262
2056.971907	34299.743894	61.506266
2056.287124	34184.837102	61.511271
2055.491585	34071.992174	61.516276
2055.043619	33947.307662	61.521281
2054.621470	33827.919094	61.526286
2053.704909	33710.811331	61.531290
2052.808912	33588.827219	61.536295
2052.421729	33477.144740	61.541300
2051.546176	33358.601130	61.546305
2050.552979	33232.549817	61.551310
2049.728615	33112.147671	61.556314
2049.626686	32991.092865	61.561319
2048.696880	32885.979817	61.566324
2048.206230	32781.602124	61.571329
2047.857322	32659.485872	61.576334
2046.726014	32546.973234	61.581338
2046.266645	32431.489692	61.586343
2045.722235	32316.641494	61.591348
2044.900237	32195.207400	61.596353
2044.173289	32075.494220	61.601358
2043.271371	31971.970696	61.606362
2043.008670	31843.723384	61.611367
2042.440343	31735.741171	61.616372
2041.402735	31618.303958	61.621377
2041.372996	31499.838540	61.626382
2040.100605	31398.542260	61.631386
2039.402480	31280.231891	61.636391
2038.552932	31158.703926	61.641396
2038.173738	31043.122560	61.646401
2037.882913	30931.241291	61.651406
2036.979373	30819.612867	61.656410
2036.507981	30688.008821	61.661415
2035.661535	30581.200190	61.666420
2034.994925	30468.964554	61.671425
2034.684153	30347.293883	61.676430
2033.827043	30228.518588	61.681434
2033.059132	30109.685757	61.686439
2032.620467	29986.680790	61.691444
2031.711226	29868.117045	61.696449
2031.194747	29756.080508	61.701454
2030.254203	29646.813850	61.706458
2029.975907	29517.233084	61.711463
2028.872735	29406.740902	61.716468
2028.129847	29295.068930	61.721473
2027.504923	29177.896528	61.726478
2026.715015	29068.690409	61.731482
2026.317527	28960.877872	61.736487
2025.721781	28844.535863	61.741492
2024.968508	28735.496794	61.746497
2024.401594	28623.005215	61.751502
2023.555187	28509.386484	61.756506
2022.874000	28392.451421	61.761511
2022.196829	28287.571018	61.766516
2021.205255	28172.558948	61.771521
2020.802518	28058.346862	61.776526
2019.880407	27952.537462	61.781530
2019.364817	27841.736734	61.786535
2018.630227	27731.963647	61.791540
2018.023917	27627.310075	61.796545
2017.733618	27507.837458	61.801550
2016.693999	27407.521115	61.806554
2016.184999	27298.012165	61.811559
2015.643008	27185.343331	61.816564
2014.761416	27080.105073	61.821569
2014.720221	26969.026493	61.826574
2013.921471	26862.714910	61.831578
2013.241514	26743.374539	61.836583
2012.634507	26629.189931	61.841588
2011.605222	26515.156871	61.846593
2011.207174	26394.519263	61.851598
2010.138212	26292.475257	61.856602
2009.623386	26186.209952	61.861607
2009.107525	26069.011096	61.866612
2008.130044	25962.193567	61.871617
2007.591293	25845.922482	61.876622
2006.973598	25745.474475	61.881626
2006.202767	25631.953201	61.886631
2005.525250	25524.614717	61.891636
2005.004111	25418.567146	61.896641
2004.470632	25299.958207	61.901646
2003.362146	25200.989426	61.906650
2003.080504	25098.475010	61.911655
2002.480987	24985.524242	61.916660
2001.731276	24876.310822	61.921665
2000.986004	24759.129490	61.926670
2000.336928	24651.883941	61.931674
1999.605190	24546.095113	61.936679
1998.982516	24450.752291	61.941684
1998.072755	24333.358517	61.946689
1997.943195	24238.647098	61.951694
1996.823535	24133.563834	61.956698
1996.491753	24022.016266	61.961703
1995.742612	23911.370454	61.966708
1994.698880	23807.562167	61.971713
1994.459385	23700.618894	61.976718
1993.644757	23588.557910	61.981722
1993.224558	23487.825791	61.986727
1992.674228	23389.830734	61.991732
1991.803768	23268.603777	61.996737
1991.352418	23160.689310	62.001742
1990.199116	23060.406334	62.006746
1989.614188	22961.085634	62.011751
1988.708805	22850.919729	62.016756
1988.066561	22749.053282	62.021761
1987.434186	22638.492538	62.026766
1986.588186	22552.779842	62.031770
1985.755519	22448.125683	62.036775
1985.178688	22349.074426	62.041780
1984.458374	22249.870469	62.046785
1984.126179	22147.133499	62.051790
1983.202069	22069.152938	62.056794
1982.512813	21959.793560	62.061799
1981.907417	21867.162413	62.066804
1981.258306	21782.009327	62.071809
1980.886770	21683.881133	62.076814
1979.707612	21580.409742	62.081818
1978.922360	21485.251835	62.086823
1978.273240	21388.882180	62.091828
1977.481883	21305.488197	62.096833
1976.905399	21221.599430	62.101838
1976.067390	21137.015933	62.106842
1975.466573	21045.621418	62.111847
1974.970530	20953.637570	62.116852
1973.977597	20871.890980	62.121857
1973.785517	20777.568573	62.126862
1972.720077	20695.052737	62.131866
1972.388966	20603.227934	62.136871
1971.389225	20519.324810	62.141876
1970.661013	20435.337191	62.146881
1970.293146	20347.330878	62.151886
1969.498137	20270.171693	62.156890
1968.875349	20172.735462	62.161895
1968.359583	20084.422884	62.166900
1967.514435	19998.239939	62.171905
1966.860827	19918.763295	62.176910
1966.212009	19840.161083	62.181914
1965.764536	19752.777876	62.186919
1965.004351	19676.653901	62.191924
1964.206624	19591.788096	62.196929
1963.738637	19497.369122	62.201934
1963.072579	19424.284446	62.206938
1962.594861	19330.241456	62.211943
1961.728040	19233.826394	62.216948
1961.029021	19148.195730	62.221953
1960.295197	19072.176695	62.226958
1959.202479	18988.034020	62.231962
1958.893301	18898.665059	62.236967
1958.048797	18820.353630	62.241972
1956.933830	18741.198559	62.246977
1957.089224	18652.347786	62.251982
1956.264894	18583.488939	62.256986
1955.585183	18507.400511	62.261991
1954.975163	18429.478551	62.266996
1953.904379	18351.547224	62.272001
1953.629532	18275.184489	62.277006
1953.122091	18198.731947	62.282010
1952.760359	18105.264073	62.287015
1951.772462	18024.275985	62.292020
1950.920381	17952.515282	62.297025
1950.283584	17857.074784	62.302030
1949.493635	17783.691026	62.307034
1948.994670	17702.546090	62.312039
1948.018394	17627.742491	62.317044
1947.336409	17547.043041	62.322049
1946.943401	17476.616414	62.327054
1946.156416	17399.397506	62.332058
1945.454723	17311.698866	62.337063
1945.031018	17236.544599	62.342068
1944.374455	17164.849253	62.347073
1943.595376	17070.676292	62.352078
1942.660901	16996.345888	62.357082
1942.013694	16928.617562	62.362087
1941.566244	16852.586009	62.367092
1940.713380	16779.616011	62.372097
1940.356382	16703.406050	62.377102
1939.439800	16632.625107	62.382106
1938.845400	16552.403962	62.387111
1938.184210	16484.017530	62.392116
1937.469885	16417.403240	62.397121
1936.918166	16340.646394	62.402126
1936.348832	16259.961216	62.407130
1935.615381	16193.593846	62.412135
1935.087709	16098.538153	62.417140
1934.182234	16034.731344	62.422145
1933.769091	15957.380955	62.427150
1932.636398	15884.779474	62.432154
1932.378293	15809.999317	62.437159
1931.682322	15730.623001	62.442164
1930.742243	15668.663681	62.447169
1930.151185	15592.816410	62.452174
1929.465288	15523.815389	62.457178
1928.703323	15437.596950	62.462183
1928.181180	15378.575736	62.467188
1927.396856	15304.375461	62.472193
1926.907017	15231.410602	62.477198
1926.385791	15166.638317	62.482202
1925.702923	15084.330761	62.487207
1925.170505	15021.527060	62.492212
1924.184806	14950.650954	62.497217
1923.522265	14865.057276	62.502222
1922.757810	14794.537261	62.507226
1922.176845	14725.324564	62.512231
1921.917932	14664.926898	62.517236
1920.796616	14590.865643	62.522241
1920.316266	14517.936205	62.527246
1919.357653	14445.444409	62.532250
1918.911211	14373.635345	62.537255
1918.306888	14308.597613	62.542260
1917.525093	14250.651018	62.547265
1916.949762	14171.689586	62.552270
1916.119694	14106.292550	62.557274
1915.482125	14037.287374	62.562279
1914.969191	13966.271515	62.567284
1914.289250	13894.618984	62.572289
1913.735266	13825.199290	62.577294
1912.999977	13758.064358	62.582298
1912.334171	13686.879422	62.587303
1911.786255	13620.149613	62.592308
1910.666632	13553.653302	62.597313
1910.241997	13483.840934	62.602318
1909.611747	13418.161393	62.607322
1908.647076	13348.720173	62.612327
1908.114821	13281.403579	62.617332
1907.525466	13223.756063	62.622337
1906.835541	13154.794452	62.627342
1906.013086	13094.829806	62.632346
1905.584725	13021.316112	62.637351
1904.890718	12956.056189	62.642356
1904.091364	12896.096747	62.647361
1903.613989	12828.129676	62.652366
1903.126311	12760.156258	62.657370
1902.460413	12685.441452	62.662375
1901.864872	12620.336214	62.667380
1900.961027	12557.534209	62.672385
1900.227301	12488.141924	62.677390
1899.533491	12422.003372	62.682394
1898.688363	12358.351641	62.687399
1898.421412	12290.842828	62.692404
1897.370508	12230.355792	62.697409
1896.950863	12163.048749	62.702414
1896.077403	12107.364495	62.707418
1895.561777	12042.421468	62.712423
1894.969971	11972.957316	62.717428
1894.464418	11920.247932	62.722433
1893.960572	11843.715897	62.727438
1893.138986	11783.182993	62.732442
1892.771542	11723.018557	62.737447
1891.961338	11640.253114	62.742452
1890.975847	11572.569197	62.747457
1890.604987	11516.340571	62.752462
1889.914588	11444.486364	62.757466
1889.252780	11368.677385	62.762471
1888.537215	11301.855726	62.767476
1887.679863	11238.092666	62.772481
1887.344403	11170.098245	62.777486
1886.007073	11110.182140	62.782490
1885.573323	11045.562187	62.787495
1885.008688	10964.985446	62.792500
1884.191272	10907.592319	62.797505
1883.753303	10841.254338	62.802510
1883.236591	10783.656920	62.807514
1882.531260	10718.246063	62.812519
1881.712643	10659.571460	62.817524
1880.775464	10593.765944	62.822529
1880.195771	10526.667528	62.827534
1879.608302	10450.740089	62.832538
1878.833038	10410.737761	62.837543
1878.391663	10337.096034	62.842548
1877.718165	10289.082977	62.847553
1877.219251	10217.050338	62.852558
1876.395577	10162.339989	62.857562
1875.765055	10101.074152	62.862567
1875.051075	10036.337898	62.867572
1874.057752	9979.464237	62.872577
1874.018173	9919.213100	62.877582
1873.545346	9856.398454	62.882586
1872.484084	9788.795511	62.887591
1872.212105	9722.125223	62.892596
1871.264219	9656.405189	62.897601
1870.667245	9592.444028	62.902606
1869.904717	9528.851845	62.907610
1869.332230	9458.405396	62.912615
1868.959675	9389.851872	62.917620
1867.888882	9336.747725	62.922625
1867.566790	9263.571609	62.927630
1866.772249	9202.290498	62.932634
1865.616315	9138.300875	62.937639
1865.742865	9063.074186	62.942644
1864.635286	9003.909103	62.947649
1863.663873	8938.941515	62.952654
1863.170981	8884.101842	62.957658
1862.665712	8828.655654	62.962663
1862.495869	8759.669663	62.967668
1861.309878	8700.055508	62.972673
1860.823375	8624.307441	62.977678
1860.187915	8562.520458	62.982682
1859.306495	8504.278429	62.987687
1858.933831	8428.443063	62.992692
1858.397398	8363.403782	62.997697
1857.304937	8302.661996	63.002702
1856.663111	8234.933983	63.007706
1855.899951	8171.174092	63.012711
1855.466124	8110.579394	63.017716
1854.306139	8053.503218	63.022721
1853.681706	7988.798654	63.027726
1853.117026	7930.992173	63.032730
1852.582620	7882.905956	63.037735
1851.914762	7820.305535	63.042740
1851.467751	7764.717950	63.047745
1851.204172	7691.639217	63.052750
1850.169203	7624.443808	63.057754
1849.728797	7567.603146	63.062759
1849.118399	7496.031202	63.067764
1848.005170	7444.389305	63.072769
1847.594570	7375.498398	63.077774
1846.866884	7313.029906	63.082778
1845.989508	7250.669851	63.087783
1845.158828	7183.767432	63.092788
1844.601408	7129.383047	63.097793
1844.393923	7066.886637	63.102798
1843.424555	7002.797260	63.107802
1842.627338	6947.667484	63.112807
1842.311790	6883.416043	63.117812
1841.446798	6825.447353	63.122817
1840.966662	6762.026801	63.127822
1840.295567	6698.177731	63.132826
1839.588389	6632.801157	63.137831
1838.790683	6560.338925	63.142836
1838.395542	6504.915822	63.147841
1837.518039	6434.093450	63.152846
1836.911847	6371.849422	63.157850
1836.337610	6315.523068	63.162855
1835.720030	6248.061721	63.167860
1834.808383	6194.028860	63.172865
1834.325141	6126.611418	63.177870
1833.549166	6066.233564	63.182874
1832.709945	6009.895226	63.187879
1832.410511	5946.245950	63.192884
1831.610828	5889.335430	63.197889
1831.202418	5828.449778	63.202894
1830.481446	5766.564907	63.207898
1829.529375	5704.523733	63.212903
1829.345517	5636.868515	63.217908
1828.182277	5575.705412	63.222913
1827.593596	5503.857220	63.227918
1826.994182	5440.156780	63.232922
1826.181557	5386.046466	63.237927
1825.494024	5327.863781	63.242932
1824.741764	5275.967831	63.247937
1824.603978	5212.825298	63.252942
1823.662174	5155.273661	63.257946
1822.644626	5093.234406	63.262951
1822.368477	5023.066305	63.267956
1821.658952	4980.127234	63.272961
1821.108748	4924.330028	63.277966
1820.428643	4856.182958	63.282970
1819.585107	4800.265582	63.287975
1819.197493	4736.652854	63.292980
1818.246702	4672.796186	63.297985
1817.786545	4606.713382	63.302990
1817.127884	4551.680946	63.307994
1816.255749	4490.426430	63.312999
1815.815432	4419.892895	63.318004
1814.649506	4361.732400	63.323009
1814.520885	4315.317843	63.328014
1813.967182	4244.889907	63.333018
1813.063474	4184.676468	63.338023
1812.461970	4121.126381	63.343028
1811.868022	4071.728661	63.348033
1810.928444	4012.817462	63.353038
1810.419057	3945.818712	63.358042
1809.952459	3895.157587	63.363047
1809.375606	3826.120277	63.368052
1808.603675	3768.583363	63.373057
1807.966528	3707.246683	63.378062
1807.448880	3642.171075	63.383066
1806.584469	3576.803008	63.388071
1805.972188	3512.769856	63.393076
1804.992075	3447.910502	63.398081
1804.666205	3397.576549	63.403086
1803.896943	3330.418390	63.408090
1803.110447	3271.273707	63.413095
1802.601841	3208.134747	63.418100
1801.827438	3148.784375	63.423105
1801.009597	3101.565089	63.428110
1800.428751	3044.257772	63.433114
1799.455309	2979.968045	63.438119
1798.859851	2921.712421	63.443124
1798.032753	2868.567918	63.448129
1797.658224	2815.199538	63.453134
1796.898877	2759.925605	63.458138
1796.577931	2700.912765	63.463143
1796.175309	2634.554450	63.468148
1795.172785	2585.033397	63.473153
1794.084301	2521.558884	63.478158
1793.620327	2457.024944	63.483162
1792.952030	2399.299509	63.488167
1792.323798	2349.545535	63.493172
1791.530113	2304.519693	63.498177
1790.953113	2243.948477	63.503182
1790.224984	2196.992301	63.508186
1789.384297	2147.042482	63.513191
1789.053997	2090.997148	63.518196
1788.235299	2042.699462	63.523201
1787.778085	1983.561319	63.528206
1787.486952	1924.359979	63.533210
1786.411814	1876.342507	63.538215
1786.174768	1814.476275	63.543220
1784.782996	1766.806740	63.548225
1784.430689	1714.785740	63.553230
1783.611362	1653.751551	63.558234
1783.086683	1602.599731	63.563239
1782.550553	1541.960273	63.568244
1781.528622	1496.407768	63.573249
1781.132900	1433.399693	63.578254
1780.330796	1381.257322	63.583258
1779.667457	1324.239534	63.588263
1778.938250	1278.388891	63.593268
1778.181866	1224.408010	63.598273
1777.347295	1176.543111	63.603278
1777.385581	1125.738058	63.608282
1776.448739	1086.773457	63.613287
1775.748239	1024.917930	63.618292
1775.017382	979.103189	63.623297
1774.421001	920.545009	63.628302
1773.356452	870.374114	63.633306
1772.965645	830.544422	63.638311
1772.446917	771.066126	63.643316
1771.326205	726.121544	63.648321
1770.893864	672.457130	63.653326
1770.229051	626.484771	63.658330
1769.493218	580.765122	63.663335
1768.911209	531.677890	63.668340
1768.079310	491.086504	63.673345
1767.674605	439.258949	63.678350
1766.787984	394.834908	63.683354
1766.217003	359.015502	63.688359
1765.419943	303.737162	63.693364
1764.710981	266.652274	63.698369
1764.015182	211.501712	63.703374
1763.168160	172.025403	63.708378
1762.324272	138.419818	63.713383
1761.744645	100.751044	63.718388
1760.754879	71.614291	63.723393
1760.161505	32.315706	63.728398
1759.382867	9.095473	63.733402
1758.163349	-22.037319	63.738407
1757.097884	-31.306229	63.743412
1754.913044	-14.022595	63.748417
1751.193406	65.809449	63.753422
1751.590985	64.128367	63.758426
1752.100958	78.132978	63.763431
1752.559448	71.539397	63.768436
1752.807083	74.248778	63.773441
1752.344691	70.578500	63.778446
1752.198280	64.333303	63.783450
1751.031970	65.635058	63.788455
1750.203229	64.733785	63.793460
1748.981586	73.135995	63.798465
1747.656239	81.415906	63.803470
1746.779661	76.887295	63.808474
1746.521941	77.043379	63.813479
1746.651189	75.636725	63.818484
1746.488291	80.026129	63.823489
1745.743665	80.899791	63.828494
1745.261606	75.859089	63.833498
1744.000408	83.099048	63.838503
1743.162334	68.941605	63.843508
1741.994838	75.895441	63.848513
1741.437849	84.557964	63.853518
1741.513779	79.682539	63.858522
1740.475292	85.888904	63.863527
1740.336665	77.852595	63.868532
1739.515277	81.504470	63.873537
1738.089746	87.573606	63.878542
1738.193143	79.768523	63.883546
1737.690566	87.134015	63.888551
1737.323868	78.952574	63.893556
1736.408059	85.287694	63.898561
1735.692306	77.437661	63.903566
1735.186007	77.350944	63.908570
1734.365180	87.061483	63.913575
1733.769109	80.726842	63.918580
1732.651236	84.993518	63.923585
1731.519199	87.021559	63.928590
1731.185489	76.931468	63.933594
1730.965314	88.259213	63.938599
1730.459078	77.494766	63.943604
1729.919897	74.842800	63.948609
1729.171798	77.363383	63.953614
1728.488758	76.785911	63.958618
1727.078415	79.974653	63.963623
1726.816172	75.181323	63.968628
1726.238216	81.380784	63.973633
1725.593423	75.288855	63.978638
1725.562705	75.993947	63.983642
1724.725387	83.319561	63.988647
1723.694864	73.896815	63.993652
1723.172858	73.962408	63.998657
1722.846046	78.409384	64.003662
1722.214730	77.503573	64.008666
1720.654171	78.145701	64.013671
1720.564212	75.018684	64.018676
1720.402378	79.713853	64.023681
1719.362840	84.622539	64.028686
1718.376260	75.440401	64.033690
1717.568134	77.905865	64.038695
1717.389527	72.454271	64.043700
1716.513408	76.247309	64.048705
1716.042741	78.428939	64.053710
1715.582280	69.518067	64.058714
1714.569249	80.487597	64.063719
1714.147274	75.664444	64.068724
1713.275066	73.560544	64.073729
1712.125923	73.661088	64.078734
1711.788022	71.861842	64.083738
1710.964663	77.499451	64.088743
1710.552277	71.264959	64.093748
1710.006077	63.138852	64.098753
1709.269388	79.722683	64.103758
1708.766754	74.224781	64.108762
1707.802966	71.175050	64.113767
1707.532529	68.868342	64.118772
1707.133113	69.825961	64.123777
1705.969765	76.550489	64.128782
1705.543652	69.923935	64.133786
1704.408582	75.623669	64.138791
1703.818798	70.557509	64.143796
1703.929391	73.649778	64.148801
1703.028024	79.635676	64.153806
1702.440390	65.704988	64.158810
1701.539042	81.034470	64.163815
1701.138769	72.085655	64.168820
1700.250643	77.374003	64.173825
1699.411843	78.432949	64.178830
1698.717303	74.282305	64.183834
1697.935386	78.378937	64.188839
1697.241020	72.104078	64.193844
1696.642708	70.022915	64.198849
1695.995611	73.861587	64.203854
1695.834091	61.902257	64.208858
1695.154052	71.366502	64.213863
1694.452615	67.090799	64.218868
1693.720462	79.417654	64.223873
1693.030813	76.631896	64.228878
1692.777430	63.501270	64.233882
1691.870299	72.086939	64.238887
1691.477306	76.478196	64.243892
1690.864821	68.458815	64.248897
1689.105892	77.607141	64.253902
1688.600094	70.147988	64.258906
1688.482327	73.628192	64.263911
1687.955329	64.608049	64.268916
1686.813335	79.759709	64.273921
1686.116581	84.047826	64.278926
1685.875749	73.127699	64.283930
1684.814260	81.105525	64.288935
1684.809173	69.189154	64.293940
1683.688498	77.654204	64.298945
1682.772383	74.361940	64.303950
1682.492669	69.341156	64.308954
1681.451196	83.833449	64.313959
1680.892141	71.650247	64.318964
1680.620704	82.164523	64.323969
1680.137252	77.696499	64.328974
1679.554458	75.291172	64.333978
1678.839810	80.545665	64.338983
1678.470663	74.435200	64.343988
1677.093741	72.015660	64.348993
1676.524243	79.423325	64.353998
1675.519727	66.678517	64.359002
1674.879270	77.442218	64.364007
1674.949851	70.639005	64.369012
1673.862255	77.752065	64.374017
1672.715481	83.474174	64.379022
1672.294883	71.760999	64.384026
1672.286647	77.092523	64.389031
1671.389859	65.836620	64.394036
1670.594272	68.415223	64.399041
1669.944884	75.278904	64.404046
1669.466835	75.777502	64.409050
1668.747713	82.896695	64.414055
1668.299966	79.903784	64.419060
1667.628054	74.130000	64.424065
1666.722781	75.775111	64.429070
1665.733086	69.368976	64.434074
1664.920035	70.389149	64.439079
1664.643251	74.703601	64.444084
1664.246277	70.269157	64.449089
1662.980879	78.708315	64.454094
1662.698040	69.750320	64.459098
1661.792321	83.967161	64.464103
1661.427336	75.359684	64.469108
1660.790710	72.928219	64.474113
1660.110639	78.323881	64.479118
1659.826499	76.334751	64.484122
1659.145609	72.998825	64.489127
1658.662188	66.100685	64.494132
1657.673781	61.569376	64.499137
1656.197883	72.208734	64.504142
1655.858145	62.789844	64.509146
1654.867557	70.324320	64.514151
1654.829951	72.134389	64.519156
1654.369364	68.705124	64.524161
1653.563069	72.058151	64.529166
1653.330543	68.597391	64.534170
1652.743999	70.791128	64.539175
1651.769858	74.019428	64.544180
1650.944262	78.575603	64.549185
1649.594374	78.003153	64.554190
1649.142740	69.764266	64.559194
1648.551961	84.637568	64.564199
1647.652772	78.493031	64.569204
1648.029545	72.355551	64.574209
1647.014938	90.171010	64.579214
1646.633220	78.287656	64.584218
1645.698648	85.858977	64.589223
1645.438846	86.326066	64.594228
1644.616124	74.110640	64.599233
1643.148446	83.097612	64.604238
1642.867236	78.591163	64.609242
1641.540709	82.649741	64.614247
1641.610717	81.681430	64.619252
1641.042466	78.682436	64.624257
1640.280247	81.470218	64.629262
1640.082414	75.986993	64.634266
1639.317362	91.181303	64.639271
1638.577021	87.649817	64.644276
1638.196319	79.874329	64.649281
1636.502202	80.968238	64.654286
1636.280178	78.474072	64.659290
1635.633126	86.397121	64.664295
1634.603147	75.878333	64.669300
1634.264429	81.207160	64.674305
1633.609342	77.621134	64.679310
1633.397544	77.722624	64.684314
1632.705092	76.507998	64.689319
1632.345112	72.278998	64.694324
1631.295297	71.272531	64.699329
1630.068658	76.297701	64.704334
1629.364404	78.021280	64.709338
1628.770053	80.345576	64.714343
1628.216963	78.769763	64.719348
1627.929646	78.572586	64.724353
1627.291214	84.715437	64.729358
1626.938733	76.627960	64.734362
1626.287807	76.143187	64.739367
1625.143146	75.495570	64.744372
1625.046415	86.463073	64.749377
1623.819815	78.415106	64.754382
1623.324554	72.179607	64.759386
1622.929582	81.098683	64.764391
1621.839713	83.520622	64.769396
1620.723433	81.701535	64.774401
1619.808808	79.881954	64.779406
1620.320261	79.076909	64.784410
1619.436225	84.534946	64.789415
1618.605496	79.067107	64.794420
1618.239395	79.178918	64.799425
1617.832024	84.458729	64.804430
1616.776171	70.939924	64.809434
1615.428551	80.513393	64.814439
1614.981973	75.378775	64.819444
1614.629532	85.981616	64.824449
1613.954004	86.070043	64.829454
1613.363528	76.383476	64.834458
1612.980334	84.332420	64.839463
1612.322794	82.118758	64.844468
1611.169952	79.696772	64.849473
1610.070094	82.424658	64.854478
1609.685898	81.306150	64.859482
1609.019177	76.815218	64.864487
1608.703570	75.274223	64.869492
1608.221688	76.279650	64.874497
1607.828051	78.873266	64.879502
1607.078906	79.575795	64.884506
1606.556942	85.208131	64.889511
1605.168783	85.898634	64.894516
1604.662170	86.985264	64.899521
1604.187648	90.574188	64.904526
1603.774130	79.667315	64.909530
1603.137798	79.049341	64.914535
1601.974651	81.754168	64.919540
1601.015364	82.948982	64.924545
1600.148295	77.841744	64.929550
1599.749805	74.730635	64.934554
1599.188717	74.222135	64.939559
1599.008564	80.068253	64.944564
1598.699383	76.305857	64.949569
1597.840961	83.679010	64.954574
1597.016260	65.528190	64.959578
1596.056424	81.319574	64.964583
1595.370274	78.309359	64.969588
1594.905732	73.682232	64.974593
1594.115504	82.496945	64.979598
1593.754725	76.509749	64.984602
1593.472350	88.878713	64.989607
1592.222942	75.903184	64.994612
1591.671870	72.731160	64.999617
1590.527184	79.397574	65.004622
1590.124362	80.398329	65.009626
1590.011794	77.990860	65.014631
1589.219363	85.198988	65.019636
1588.028952	78.266522	65.024641
1587.033841	82.764489	65.029646
1586.709961	75.752707	65.034650
1586.208804	79.270168	65.039655
1585.340389	82.573161	65.044660
1585.169037	69.500487	65.049665
1584.611800	71.970283	65.054670
1583.910899	75.186736	65.059674
1582.791121	80.986591	65.064679
1581.908137	79.590935	65.069684
1581.263426	69.998156	65.074689
1580.519228	83.987499	65.079694
1580.234945	74.974552	65.084698
1579.709942	81.618214	65.089703
1579.193769	73.638759	65.094708
1579.082239	77.777150	65.099713
1577.759720	84.135928	65.104718
1577.001076	78.276602	65.109722
1576.312118	82.776395	65.114727
1575.708060	77.077016	65.119732
1575.848966	70.865039	65.124737
1574.806788	72.629704	65.129742
1573.434410	70.444469	65.134746
1572.751563	81.295346	65.139751
1572.269895	80.288525	65.144756
1571.761921	82.367294	65.149761
1571.135383	81.462339	65.154766
1570.814493	83.689583	65.159770
1569.767497	82.835660	65.164775
1568.789612	78.876731	65.169780
1568.504629	71.584381	65.174785
1567.417927	87.911605	65.179790
1567.326767	76.157155	65.184794
1567.001515	75.034020	65.189799
1566.034499	75.203464	65.194804
1565.270653	69.218815	65.199809
1564.400645	81.982337	65.204814
1564.020639	72.831637	65.209818
1563.402089	71.094350	65.214823
1562.434385	77.953431	65.219828
1561.532520	79.180138	65.224833
1560.568606	77.822579	65.229838
1560.279513	81.145500	65.234842
1559.635678	81.594764	65.239847
1559.175594	85.346982	65.244852
1558.756438	78.820281	65.249857
1558.496232	75.775518	65.254862
1557.788912	74.575892	65.259866
1556.773888	82.139517	65.264871
1556.209487	80.051424	65.269876
1555.646939	73.910212	65.274881
1554.295678	80.519573	65.279886
1553.518247	79.632289	65.284890
1552.763326	81.415979	65.289895
1552.349388	76.982673	65.294900
1552.002319	77.805839	65.299905
1551.379974	88.129864	65.304910
1551.397938	82.438895	65.309914
1550.696283	89.536415	65.314919
1549.121151	85.170908	65.319924
1548.515805	77.858496	65.324929
1547.871427	86.066566	65.329934
1547.509885	75.181416	65.334938
1547.038812	74.455196	65.339943
1545.881679	75.593155	65.344948
1545.276661	75.906942	65.349953
1544.307642	79.957647	65.354958
1543.934304	73.873109	65.359962
1543.476004	75.622287	65.364967
1543.276484	74.149590	65.369972
1542.388901	66.382129	65.374977
1541.325540	78.799477	65.379982
1540.569191	74.742283	65.384986
1540.305476	62.731411	65.389991
1539.769973	76.157729	65.394996
1538.586515	73.649178	65.400001
1537.831180	76.178846	65.405006
1537.129783	76.755534	65.410010
1536.690102	75.876092	65.415015
1536.105094	76.464250	65.420020
1535.820832	70.673071	65.425025
1535.023524	76.998877	65.430030
1534.054893	68.727048	65.435034
1533.349221	75.807857	65.440039
1532.269159	71.258046	65.445044
1532.100752	70.649320	65.450049
1531.302976	75.221605	65.455054
1530.890574	76.657559	65.460058
1530.797593	84.525702	65.465063
1529.725237	77.675437	65.470068
1529.053194	72.469430	65.475073
1528.104257	82.400640	65.480078
1527.561135	85.629886	65.485082
1527.176955	75.476901	65.490087
1525.581200	84.058496	65.495092
1525.077342	73.298470	65.500097
1524.510923	78.195124	65.505102
1524.426209	66.065923	65.510106
1523.597873	74.635962	65.515111
1522.832748	76.541130	65.520116
1523.231104	75.842348	65.525121
1521.649044	78.072870	65.530126
1521.168776	73.337871	65.535130
1520.452285	80.082930	65.540135
1519.438724	75.861607	65.545140
1519.537701	69.542751	65.550145
1518.035175	71.580861	65.555150
1517.424874	66.371358	65.560154
1516.754311	72.095123	65.565159
1515.877825	80.787938	65.570164
1515.706881	65.983699	65.575169
1515.483793	76.602251	65.580174
1514.544302	71.110736	65.585178
1513.422741	69.841326	65.590183
1512.739172	72.870535	65.595188
1512.467072	69.283615	65.600193
1511.657258	80.422760	65.605198
1511.009866	71.640996	65.610202
1510.895925	70.787071	65.615207
1509.543006	74.941366	65.620212
1508.936345	63.024420	65.625217
1508.243547	73.839035	65.630222
1508.036547	67.575109	65.635226
1507.509817	71.003603	65.640231
1506.516858	82.433631	65.645236
1505.777077	69.129596	65.650241
1505.027821	78.909230	65.655246
1504.799774	65.914972	65.660250
1503.881913	78.222477	65.665255
1502.233907	77.899329	65.670260
1502.024400	73.578632	65.675265
1501.686457	68.858870	65.680270
1500.961256	65.276143	65.685274
1500.809647	72.290990	65.690279
1499.898068	75.118312	65.695284
1499.733921	68.112707	65.700289
1498.317585	75.688078	65.705294
1497.922546	71.518291	65.710298
1497.150676	68.277298	65.715303
1496.749930	74.007079	65.720308
1496.587529	66.230059	65.725313
1494.740870	79.211867	65.730318
1494.187304	69.800180	65.735322
1493.924374	65.456436	65.740327
1493.446588	76.415086	65.745332
1493.120407	64.494576	65.750337
1491.788832	70.205112	65.755342
1491.091199	65.419507	65.760346
1490.918327	66.666013	65.765351
1490.202347	67.260801	65.770356
1489.674190	59.245436	65.775361
1488.463398	67.013652	65.780366
1487.841526	68.315739	65.785370
1487.095604	71.939919	65.790375
1486.592946	75.765143	65.795380
1486.424760	66.806313	65.800385
1485.082790	77.769827	65.805390
1484.475738	68.475455	65.810394
1483.952553	76.008250	65.815399
1483.254107	69.398218	65.820404
1483.007488	65.288429	65.825409
1481.999815	70.614758	65.830414
1481.134282	71.130810	65.835418
1480.444526	62.589186	65.840423
1480.088105	69.748544	65.845428
1480.117242	64.560442	65.850433
1478.772242	75.221658	65.855438
1477.784049	64.158571	65.860442
1477.353868	70.340890	65.865447
1476.139321	74.613562	65.870452
1476.305624	65.904359	65.875457
1475.854467	73.354744	65.880462
1474.955584	65.907656	65.885466
1474.157825	58.479196	65.890471
1472.992857	69.892402	65.895476
1472.560955	61.264073	65.900481
1472.330743	66.581971	65.905486
1471.679851	72.096036	65.910490
1470.797026	64.028226	65.915495
1469.661300	71.038614	65.920500
1469.527509	66.677505	65.925505
1468.729299	73.058662	65.930510
1468.353787	67.457041	65.935514
1468.124310	67.933520	65.940519
1466.778823	74.521500	65.945524
1466.240021	68.442775	65.950529
1465.715042	66.337402	65.955534
1464.784657	66.234554	65.960538
1463.918279	62.584387	65.965543
1462.919176	71.323503	65.970548
1462.584180	69.131168	65.975553
1462.534078	67.527500	65.980558
1461.900859	69.375451	65.985562
1461.220435	63.653554	65.990567
1459.905050	71.441558	65.995572
1459.283781	61.430360	66.000577
1458.535603	63.093151	66.005582
1457.937764	78.626755	66.010586
1458.018610	74.803976	66.015591
1457.360675	82.367654	66.020596
1456.294903	65.138325	66.025601
1455.740630	72.597214	66.030606
1455.102200	69.308219	66.035610
1454.619861	68.052368	66.040615
1453.309262	81.759574	66.045620
1452.282526	63.972104	66.050625
1451.833303	68.605710	66.055630
1451.391126	75.021755	66.060634
1451.212379	72.787242	66.065639
1450.556555	80.314315	66.070644
1450.380841	75.977214	66.075649
1449.400514	71.357974	66.080654
1448.820300	73.943413	66.085658
1448.106795	57.407176	66.090663
1446.772488	71.629081	66.095668
1445.790261	65.567218	66.100673
1445.309361	60.933267	66.105678
1444.834941	68.904597	66.110682
1444.685744	59.897028	66.115687
1444.082765	65.244207	66.120692
1442.891101	61.429700	66.125697
1442.147285	69.693006	66.130702
1441.639874	68.504220	66.135706
1441.329482	59.001870	66.140711
1440.623461	71.039170	66.145716
1440.020786	59.761869	66.150721
1439.233745	65.037375	66.155726
1438.751562	63.628537	66.160730
1438.086835	67.295018	66.165735
1437.190933	62.544096	66.170740
1436.532503	59.794458	66.175745
1435.625004	60.176844	66.180750
1435.214780	70.561777	66.185754
1434.831353	69.616643	66.190759
1433.396970	66.902016	66.195764
1432.830859	66.277656	66.200769
1432.032930	65.071966	66.205774
1432.053012	65.494592	66.210778
1431.747950	70.365491	66.215783
1430.661947	74.742334	66.220788
1429.927081	67.671325	66.225793
1428.962644	72.814179	66.230798
1428.241322	62.049330	66.235802
1427.789855	58.989255	66.240807
1427.536248	67.482161	66.245812
1426.673372	65.720662	66.250817
1425.703173	64.061378	66.255822
1425.050110	68.828312	66.260826
1424.800651	62.325141	66.265831
1423.877976	68.380732	66.270836
1423.514185	65.125370	66.275841
1422.334143	71.983544	66.280846
1421.702892	64.894495	66.285850
1421.469705	69.861204	66.290855
1420.708420	67.400732	66.295860
1420.261558	70.475921	66.300865
1418.915692	66.490388	66.305870
1418.291959	68.581272	66.310874
1417.843078	67.878358	66.315879
1417.187555	70.822706	66.320884
1417.114925	66.641118	66.325889
1416.125367	74.487744	66.330894
1414.981811	69.117016	66.335898
1414.496685	61.083795	66.340903
1413.707659	77.675972	66.345908
1413.936877	67.550111	66.350913
1413.119835	72.426690	66.355918
1412.058439	65.262506	66.360922
1411.748121	61.973416	66.365927
1410.941455	75.430223	66.370932
1409.791881	67.411142	66.375937
1408.798606	60.422218	66.380942
1408.247542	72.012265	66.385946
1407.939600	67.626802	66.390951
1407.242211	75.549998	66.395956
1407.006426	68.923227	66.400961
1406.762405	71.663399	66.405966
1405.458957	69.596614	66.410970
1404.689703	64.399792	66.415975
1404.177509	73.153002	66.420980
1403.598960	69.759886	66.425985
1402.716280	61.493385	66.430990
1401.583407	74.964195	66.435994
1401.288807	67.816911	66.440999
1400.484764	70.540438	66.446004
1400.416189	68.944440	66.451009
1400.064343	69.471913	66.456014
1399.278255	66.168557	66.461018
1398.317854	59.286378	66.466023
1397.439756	69.652636	66.471028
1396.937741	68.623854	66.476033
1395.990587	68.463771	66.481038
1395.050337	70.925095	66.486042
1394.878042	67.115745	66.491047
1394.041241	72.214668	66.496052
1393.773603	61.592190	66.501057
1393.314513	62.155634	66.506062
1391.941181	69.670599	66.511066
1391.382787	60.717040	66.516071
1390.761297	63.326396	66.521076
1390.361186	62.317688	66.526081
1390.379978	64.686500	66.531086
1389.270589	65.134109	66.536090
1388.551566	53.060032	66.541095
1387.394074	69.143061	66.546100
1386.460251	57.595138	66.551105
1385.917984	63.456230	66.556110
1385.290327	74.202161	66.561114
1385.000192	60.963912	66.566119
1384.469595	64.714741	66.571124
1384.090496	69.245746	66.576129
1383.285684	65.190003	66.581134
1382.646889	64.194004	66.586138
1382.065759	66.713368	66.591143
1380.921479	69.080968	66.596148
1380.084722	68.012356	66.601153
1379.238568	70.608540	66.606158
1378.734220	66.989169	66.611162
1378.702355	67.677098	66.616167
1378.161499	68.955293	66.621172
1377.260084	68.154005	66.626177
1376.316311	63.068514	66.631182
1375.584543	66.673124	66.636186
1375.222739	63.707618	66.641191
1374.363241	71.005296	66.646196
1373.395463	62.484249	66.651201
1372.860945	69.752348	66.656206
1372.245846	69.025401	66.661210
1371.742309	69.193786	66.666215
1370.874103	72.288647	66.671220
1370.525645	70.905874	66.676225
1370.221949	67.681970	66.681230
1369.066324	68.710954	66.686234
1368.550112	71.295697	66.691239
1368.033846	68.985531	66.696244
1367.338137	67.189596	66.701249
1366.450259	60.297480	66.706254
1365.473231	69.608709	66.711258
1365.285928	70.545275	66.716263
1364.435586	68.415949	66.721268
1363.692808	68.877834	66.726273
1362.903487	67.044741	66.731278
1361.927915	79.165907	66.736282
1361.582614	74.278603	66.741287
1361.480241	72.262196	66.746292
1361.358200	69.550318	66.751297
1360.284879	66.727877	66.756302
1359.254681	72.021557	66.761306
1358.822310	68.368671	66.766311
1357.993492	66.672747	66.771316
1357.006780	63.360296	66.776321
1356.422838	67.187420	66.781326
1355.984967	72.505217	66.786330
1355.845346	57.849011	66.791335
1354.322076	67.174532	66.796340
1353.508790	71.858139	66.801345
1353.486495	74.236636	66.806350
1352.793685	73.757015	66.811354
1352.525369	64.282687	66.816359
1351.187980	68.344700	66.821364
1350.540424	67.772729	66.826369
1350.274780	63.591867	66.831374
1349.267015	68.612321	66.836378
1348.297461	60.555199	66.841383
1347.659886	62.306096	66.846388
1346.995622	62.181488	66.851393
1346.583257	66.235231	66.856398
1345.593366	71.595048	66.861402
1345.920138	70.945467	66.866407
1345.043510	70.859348	66.871412
1343.781733	64.389379	66.876417
1343.582599	65.247402	66.881422
1342.834673	66.206857	66.886426
1342.470668	60.482009	66.891431
1341.035621	70.769659	66.896436
1340.377271	70.443837	66.901441
1340.456280	68.062703	66.906446
1339.579607	68.717770	66.911450
1339.054912	59.426131	66.916455
1337.809098	69.300495	66.921460
1337.070795	57.592203	66.926465
1337.152294	65.125081	66.931470
1335.955501	66.712563	66.936474
1335.387827	56.599850	66.941479
1334.163374	67.137877	66.946484
1334.034129	64.174831	66.951489
1333.130501	67.773656	66.956494
1332.837086	65.273530	66.961498
1332.725063	68.576202	66.966503
1331.838042	73.161148	66.971508
1331.347007	67.049636	66.976513
1330.564461	67.047916	66.981518
1329.122102	67.439672	66.986522
1328.676878	72.201971	66.991527
1328.197417	72.216725	66.996532
1327.744202	71.667482	67.001537
1327.087516	73.891360	67.006542
1325.571768	77.887124	67.011546
1325.268297	65.135137	67.016551
1324.516721	71.772269	67.021556
1324.029291	61.481218	67.026561
1323.853730	69.597439	67.031566
1323.443651	77.757254	67.036570
1322.624423	75.534685	67.041575
1321.394723	73.654917	67.046580
1321.081941	74.401698	67.051585
1320.449487	69.202081	67.056590
1319.136046	76.013694	67.061594
1318.622531	66.698202	67.066599
1318.144125	85.076611	67.071604
1317.676089	77.789752	67.076609
1317.632107	68.858512	67.081614
1316.196025	74.872753	67.086618
1315.764924	70.740275	67.091623
1314.971713	78.317596	67.096628
1314.433445	81.020975	67.101633
1313.567163	72.398659	67.106638
1312.725911	71.278743	67.111642
1312.268248	61.990647	67.116647
1311.765633	70.417485	67.121652
1311.044212	70.669407	67.126657
1310.996246	59.067421	67.131662
1309.513908	76.164073	67.136666
1308.970306	67.070989	67.141671
1308.812569	71.229338	67.146676
1307.600341	64.212189	67.151681
1306.658051	58.208697	67.156686
1305.518901	74.878625	67.161690
1305.527925	60.921047	67.166695
1305.248864	70.977624	67.171700
1304.582665	74.709026	67.176705
1304.405490	60.419925	67.181710
1303.244223	65.835385	67.186714
1302.624170	65.607565	67.191719
1302.079715	65.314109	67.196724
1300.774713	65.818086	67.201729
1300.171316	64.633552	67.206734
1299.413470	69.150662	67.211738
1299.367512	61.979641	67.216743
1298.998227	62.558786	67.221748
1297.314646	72.460187	67.226753
1296.811426	56.999198	67.231758
1295.924155	77.855361	67.236762
1295.941627	64.162947	67.241767
1295.522858	63.213992	67.246772
1295.051205	65.876819	67.251777
1294.319056	64.469902	67.256782
1293.001303	71.961884	67.261786
1292.898982	61.855623	67.266791
1291.700789	66.751828	67.271796
1290.413120	64.778791	67.276801
1290.117406	60.296787	67.281806
1289.612233	65.253125	67.286810
1289.409102	66.061324	67.291815
1288.840433	66.452971	67.296820
1288.100868	71.978015	67.301825
1287.441101	71.683972	67.306830
1286.978911	61.294301	67.311834
1286.717526	62.039221	67.316839
1284.984957	68.007571	67.321844
1284.339479	69.102144	67.326849
1283.825650	69.164948	67.331854
1283.156787	73.973848	67.336858
1282.924680	72.668785	67.341863
1282.096273	71.646186	67.346868
1281.262058	65.746947	67.351873
1281.031507	60.223247	67.356878
1279.866665	62.013834	67.361882
1279.039432	61.729072	67.366887
1278.163119	63.659869	67.371892
1277.494967	71.786598	67.376897
1277.509070	70.038686	67.381902
1276.869589	75.782790	67.386906
1276.429238	68.433197	67.391911
1275.374587	72.511797	67.396916
1274.706326	64.651233	67.401921
1274.462871	66.877232	67.406926
1272.927851	74.802741	67.411930
1272.237394	61.404239	67.416935
1271.733249	66.765697	67.421940
1271.453944	61.740187	67.426945
1271.475646	64.026530	67.431950
1270.106002	73.958458	67.436954
1269.389009	68.444289	67.441959
1268.446516	63.759190	67.446964
1267.973846	70.586957	67.451969
1267.825486	71.801192	67.456974
1266.708227	72.565499	67.461978
1266.030544	72.201769	67.466983
1265.445842	70.284134	67.471988
1264.683101	69.437184	67.476993
1264.253592	69.352543	67.481998
1263.123898	75.318096	67.487002
1262.499754	71.605833	67.492007
1262.017863	64.447356	67.497012
1261.690899	66.978372	67.502017
1261.489341	55.514359	67.507022
1260.624143	68.756563	67.512026
1259.680913	65.897714	67.517031
1259.216028	68.438044	67.522036
1257.790478	70.587064	67.527041
1257.250952	59.354983	67.532046
1256.693974	62.752056	67.537050
1256.533420	63.801071	67.542055
1255.925098	69.743651	67.547060
1255.296131	68.411805	67.552065
1254.984116	59.512157	67.557070
1253.813787	77.404477	67.562074
1252.938650	66.596342	67.567079
1252.542756	66.009614	67.572084
1251.437623	69.107489	67.577089
1250.522352	59.428543	67.582094
1249.756845	62.895044	67.587098
1249.417393	66.978206	67.592103
1248.990407	65.007114	67.597108
1248.695200	66.109079	67.602113
1248.305445	56.860670	67.607118
1247.100514	68.185685	67.612122
1246.489410	65.966321	67.617127
1245.946743	67.645380	67.622132
1244.724047	69.847310	67.627137
1244.328851	64.505913	67.632142
1243.505167	67.243646	67.637146
1243.391313	69.695046	67.642151
1242.051229	68.829515	67.647156
1241.184233	61.967246	67.652161
1240.839349	65.604991	67.657166
1240.194483	74.783017	67.662170
1239.966672	68.320588	67.667175
1239.624964	72.124988	67.672180
1238.134467	66.021032	67.677185
1237.757333	61.324900	67.682190
1237.300782	74.976803	67.687194
1236.591894	63.654959	67.692199
1235.721193	61.211947	67.697204
1234.892650	67.035003	67.702209
1234.806309	52.062848	67.707214
1233.937360	61.284382	67.712218
1232.887741	62.572540	67.717223
1232.063873	63.201899	67.722228
1231.400061	65.702900	67.727233
1231.380204	65.658784	67.732238
1230.774863	62.894455	67.737242
1230.056949	64.055752	67.742247
1228.988586	53.369827	67.747252
1228.166634	67.297447	67.752257
1227.891672	64.529471	67.757262
1227.379321	61.420770	67.762266
1226.476525	50.489323	67.767271
1225.886497	53.781267	67.772276
1225.256757	66.259053	67.777281
1224.630674	53.302932	67.782286
1223.308973	69.002106	67.787290
1222.870166	70.760850	67.792295
1222.142044	60.091784	67.797300
1221.964240	79.255023	67.802305
1221.679730	66.722399	67.807310
1220.747573	67.999769	67.812314
1220.018155	68.016442	67.817319
1219.475279	67.055696	67.822324
1218.874456	68.094297	67.827329
1217.692422	50.079364	67.832334
1216.719885	51.027261	67.837338
1216.239033	64.916411	67.842343
1215.883872	67.429837	67.847348
1215.089384	69.704039	67.852353
1215.283790	65.219804	67.857358
1214.140740	64.035948	67.862362
1213.354988	61.172578	67.867367
1212.912707	63.267769	67.872372
1211.764160	67.955838	67.877377
1210.764984	59.588098	67.882382
1210.194987	70.553539	67.887386
1209.759311	65.765794	67.892391
1209.590291	59.828617	67.897396
1209.041342	71.861474	67.902401
1208.257512	64.263742	67.907406
1207.336901	59.373339	67.912410
1206.787409	71.620749	67.917415
1206.354849	55.287534	67.922420
1204.987834	74.002777	67.927425
1204.574367	67.916810	67.932430
1203.708949	68.339895	67.937434
1203.031752	68.319883	67.942439
1203.480375	68.434661	67.947444
1201.931614	69.748588	67.952449
1201.148554	63.530583	67.957454
1200.566545	71.618396	67.962458
1200.282984	61.444775	67.967463
1199.610404	63.158694	67.972468
1198.542134	70.713546	67.977473
1198.231602	65.355541	67.982478
1197.595293	68.077683	67.987482
1196.803051	62.132380	67.992487
1195.994083	61.642888	67.997492
1195.132978	65.556695	68.002497
1194.735431	60.882741	68.007502
1194.063591	70.218026	68.012506
1193.901716	60.323104	68.017511
1192.486440	58.472914	68.022516
1191.711621	72.173851	68.027521
1191.383609	53.538992	68.032526
1190.815416	68.105937	68.037530
1190.614488	59.574995	68.042535
1189.839593	62.839576	68.047540
1188.493752	72.712559	68.052545
1188.056468	64.868912	68.057550
1187.670515	69.386833	68.062554
1187.318711	72.517901	68.067559
1186.768020	67.428327	68.072564
1185.908798	69.197162	68.077569
1185.087980	58.784130	68.082574
1183.875869	66.883835	68.087578
1183.253740	67.489013	68.092583
1182.958646	59.304210	68.097588
1182.320319	68.919598	68.102593
1181.233394	66.397449	68.107598
1180.476665	60.241499	68.112602
1179.956158	59.185740	68.117607
1179.814799	69.201494	68.122612
1179.240384	60.319937	68.127617
1178.583743	58.549385	68.132622
1177.471093	72.050158	68.137626
1176.986489	57.015188	68.142631
1176.320733	67.827124	68.147636
1175.857519	63.278735	68.152641
1175.064994	56.704277	68.157646
1174.279560	66.743608	68.162650
1173.892380	63.854713	68.167655
1172.953411	67.853450	68.172660
1171.805937	62.084498	68.177665
1171.483928	54.317147	68.182670
1170.958552	60.068349	68.187674
1170.328155	67.072597	68.192679
1170.103969	55.292078	68.197684
1169.060350	66.854818	68.202689
1168.380939	56.148068	68.207694
1167.864372	63.485876	68.212698
1167.241961	70.220772	68.217703
1166.343665	65.490840	68.222708
1165.622665	74.931723	68.227713
1165.331470	60.897331	68.232718
1164.645368	69.678220	68.237722
1163.364163	66.508880	68.242727
1162.785862	64.861492	68.247732
1161.973072	67.972834	68.252737
1161.869432	62.506239	68.257742
1161.294144	66.868192	68.262746
1160.982275	66.148266	68.267751
1160.227152	63.319466	68.272756
1159.047727	81.258994	68.277761
1158.659673	66.706988	68.282766
1157.407929	68.700686	68.287770
1156.609090	58.180091	68.292775
1156.148779	60.517856	68.297780
1155.698096	69.401656	68.302785
1155.619085	58.320300	68.307790
1154.934542	59.217687	68.312794
1153.768507	60.043415	68.317799
1153.188993	61.537539	68.322804
1152.145249	56.078535	68.327809
1152.100021	57.203832	68.332814
1151.042816	63.451209	68.337818
1150.242595	64.401688	68.342823
1150.010420	62.289244	68.347828
1149.306210	65.682944	68.352833
1148.895981	64.264298	68.357838
1148.347373	71.162503	68.362842
1147.540717	61.999344	68.367847
1146.757304	56.156737	68.372852
1145.054255	69.092243	68.377857
1144.742056	65.819263	68.382862
1144.046513	67.927936	68.387866
1143.649448	68.957803	68.392871
1143.538016	60.404750	68.397876
1142.829336	68.134242	68.402881
1142.614102	59.637123	68.407886
1141.399645	65.628814	68.412890
1140.728239	52.940135	68.417895
1140.521514	60.761680	68.422900
1139.112913	65.148936	68.427905
1138.684712	63.663763	68.432910
1137.853747	62.211109	68.437914
1137.757941	67.272673	68.442919
1136.810892	63.995009	68.447924
1135.927013	67.543445	68.452929
1135.511938	64.826152	68.457934
1134.818025	63.913101	68.462938
1134.099048	60.591279	68.467943
1132.915615	63.805733	68.472948
1132.425619	67.742537	68.477953
1132.385648	62.776756	68.482958
1131.632013	59.168709	68.487962
1130.561721	57.516001	68.492967
1129.967614	53.303837	68.497972
1129.350104	62.807107	68.502977
1129.125560	53.535608	68.507982
1127.932350	59.200645	68.512986
1127.123393	61.779948	68.517991
1126.872060	55.822760	68.522996
1126.199573	65.383662	68.528001
1125.969776	58.486329	68.533006
1124.929468	58.069926	68.538010
1124.148776	60.723583	68.543015
1123.609196	53.467090	68.548020
1121.950583	58.526481	68.553025
1121.470108	61.763175	68.558030
1121.230271	61.392923	68.563034
1120.777366	59.519019	68.568039
1120.794345	62.091538	68.573044
1119.928208	66.249020	68.578049
1118.996336	63.766893	68.583054
1118.077227	70.537950	68.588058
1117.756449	67.307340	68.593063
1116.882906	62.212366	68.598068
1115.826811	69.043058	68.603073
1115.530546	56.017172	68.608078
1114.562888	60.581889	68.613082
1114.190363	68.048184	68.618087
1113.919845	61.993120	68.623092
1112.851142	66.214363	68.628097
1112.179615	58.269223	68.633102
1111.449196	54.441447	68.638106
1110.848450	55.442213	68.643111
1110.460609	58.170584	68.648116
1109.449012	64.751346	68.653121
1109.032356	58.336326	68.658126
1108.376190	61.935284	68.663130
1107.812235	64.988138	68.668135
1106.695184	58.044275	68.673140
1105.592312	72.496000	68.678145
1105.320941	60.924847	68.683150
1105.272810	67.713489	68.688154
1104.830585	62.161982	68.693159
1104.294334	58.673910	68.698164
1103.230335	65.198354	68.703169
1102.306822	63.266842	68.708174
1101.583978	66.677711	68.713178
1100.532054	68.604959	68.718183
1100.170103	60.725699	68.723188
1099.474919	73.185529	68.728193
1099.159298	68.419713	68.733198
1098.845354	66.705060	68.738202
1097.366966	68.749029	68.743207
1097.118464	63.553066	68.748212
1096.273944	71.830883	68.753217
1095.920245	63.888809	68.758222
1095.157262	63.560771	68.763226
1094.323060	70.510718	68.768231
1094.019363	68.816513	68.773236
1093.101465	70.273011	68.778241
1092.477851	65.040520	68.783246
1091.570835	69.280208	68.788250
1091.412877	77.242239	68.793255
1090.898738	73.252329	68.798260
1089.667885	71.218319	68.803265
1088.903223	64.789270	68.808270
1088.547208	68.461916	68.813274
1088.091721	77.494725	68.818279
1086.990379	65.000602	68.823284
1086.100204	71.730796	68.828289
1085.939198	65.685124	68.833294
1085.317990	64.311087	68.838298
1084.388704	70.683223	68.843303
1083.884131	60.312971	68.848308
1082.714291	63.451167	68.853313
1082.183796	58.823617	68.858318
1082.126870	69.012016	68.863322
1081.622501	68.283297	68.868327
1080.818373	65.192657	68.873332
1079.871050	63.534603	68.878337
1079.480329	60.818178	68.883342
1078.575674	61.608671	68.888346
1077.368731	75.687451	68.893351
1076.985490	59.784828	68.898356
1076.333859	69.782397	68.903361
1076.021954	68.783365	68.908366
1075.582181	63.384440	68.913370
1074.827916	63.679499	68.918375
1074.308424	58.575534	68.923380
1073.472931	53.383065	68.928385
1072.325305	56.535077	68.933390
1071.585660	58.307004	68.938394
1070.966273	59.239781	68.943399
1070.892787	56.015575	68.948404
1070.008141	63.217979	68.953409
1069.738380	55.525917	68.958414
1068.824814	55.005796	68.963418
1068.140488	60.564677	68.968423
1067.544194	48.889110	68.973428
1066.006568	62.930597	68.978433
1065.429865	57.608652	68.983438
1065.259633	48.809503	68.988442
1064.444662	57.943641	68.993447
1064.458746	49.984077	68.998452
1063.635380	55.076216	69.003457
1062.787991	58.689832	69.008462
1062.132491	50.426773	69.013466
1061.435422	57.952577	69.018471
1060.986989	53.323018	69.023476
1059.699377	54.466175	69.028481
1059.185764	51.718842	69.033486
1058.679363	48.606084	69.038490
1058.014293	63.568491	69.043495
1057.567881	54.652423	69.048500
1056.237547	57.847699	69.053505
1056.079732	52.608935	69.058510
1055.695248	51.722379	69.063514
1055.179725	63.070252	69.068519
1054.102949	48.530085	69.073524
1053.178678	61.280244	69.078529
1052.671027	58.230763	69.083534
1052.678395	57.340219	69.088538
1051.511143	62.540685	69.093543
1050.726785	50.253215	69.098548
1050.017681	57.468698	69.103553
1049.616637	51.268833	69.108558
1049.236545	58.037736	69.113562
1047.769822	58.725264	69.118567
1047.071969	53.883072	69.123572
1046.803780	62.507608	69.128577
1046.354532	57.323089	69.133582
1045.866027	50.142075	69.138586
1045.150673	61.274154	69.143591
1044.974643	51.983915	69.148596
1043.685108	61.231401	69.153601
1042.346199	47.813164	69.158606
1042.169799	50.265053	69.163610
1041.257098	53.054851	69.168615
1041.008924	45.032934	69.173620
1040.444617	56.481604	69.178625
1039.372243	62.144802	69.183630
1039.104775	52.933765	69.188634
1038.379427	61.252556	69.193639
1037.730068	50.690891	69.198644
1036.791214	53.409157	69.203649
1036.392749	52.674639	69.208654
1035.724355	49.234417	69.213658
1034.973965	57.645500	69.218663
1034.147144	53.952936	69.223668
1033.134796	51.325951	69.228673
1032.818234	50.698254	69.233678
1032.478703	57.552169	69.238682
1032.007159	60.139323	69.243687
1031.371832	46.990789	69.248692
1030.263679	55.433556	69.253697
1029.637856	49.009257	69.258702
1029.403901	47.415933	69.263706
1028.190423	58.994690	69.268711
1027.732050	47.857019	69.273716
1027.062637	51.612641	69.278721
1026.479997	50.563647	69.283726
1025.859029	44.881329	69.288730
1024.769631	57.260367	69.293735
1024.730463	49.886447	69.298740
1023.809452	56.126390	69.303745
1022.601004	64.503119	69.308750
1022.023660	44.903469	69.313754
1021.330683	47.150534	69.318759
1021.170176	47.914123	69.323764
1020.700663	51.828757	69.328769
1020.079840	51.552244	69.333774
1019.293020	46.990724	69.338778
1018.447089	59.354686	69.343783
1018.141627	50.031428	69.348788
1017.052747	52.402982	69.353793
1015.983947	57.890575	69.358798
1015.669604	60.788616	69.363802
1015.069395	63.459322	69.368807
1014.746441	60.161267	69.373812
1013.931430	58.624116	69.378817
1013.186305	59.233132	69.383822
1012.485874	52.352349	69.388826
1011.885223	54.472765	69.393831
1011.580254	58.082101	69.398836
1010.501885	55.161276	69.403841
1009.510607	59.982099	69.408846
1009.223566	51.956906	69.413850
1008.473098	68.770071	69.418855
1007.997178	57.624151	69.423860
1007.144932	61.035128	69.428865
1006.401161	63.993607	69.433870
1006.432604	52.697584	69.438874
1004.932370	58.279053	69.443879
1004.369659	53.249793	69.448884
1003.465313	63.618736	69.453889
1003.120477	63.098043	69.458894
1002.935227	55.443010	69.463898
1002.119918	63.153222	69.468903
1001.359222	52.686554	69.473908
1000.495567	52.958038	69.478913
999.957804	57.955870	69.483918
999.534430	56.011060	69.488922
998.780132	60.082973	69.493927
998.280592	58.702218	69.498932
997.599426	55.025916	69.503937
996.912645	52.414959	69.508942
996.185897	58.838471	69.513946
995.304086	58.734375	69.518951
994.779789	52.670826	69.523956
993.645502	49.626442	69.528961
992.878079	58.112784	69.533966
992.433897	46.137076	69.538970
991.670045	61.638756	69.543975
991.647980	61.265408	69.548980
991.118587	56.737055	69.553985
990.050809	66.562723	69.558990
989.475251	53.776852	69.563994
988.774398	58.269198	69.568999
988.260986	54.373820	69.574004
987.008400	69.259404	69.579009
986.336029	67.860417	69.584014
986.110178	59.063815	69.589018
985.659039	69.456854	69.594023
985.105526	52.471179	69.599028
984.059549	59.128412	69.604033
983.574055	57.649231	69.609038
983.138101	59.323977	69.614042
981.824355	64.528857	69.619047
981.237446	59.681648	69.624052
980.685154	61.977305	69.629057
980.039425	61.223790	69.634062
979.927865	55.555049	69.639066
978.734335	61.764250	69.644071
978.218981	57.142203	69.649076
977.458526	57.061382	69.654081
977.129684	55.369619	69.659086
975.887092	55.263008	69.664090
975.211481	61.957512	69.669095
974.864331	56.979117	69.674100
974.404886	71.322194	69.679105
973.656291	57.026319	69.684110
972.801094	57.156117	69.689114
971.956579	59.730084	69.694119
971.716120	55.725048	69.699124
971.199482	58.052880	69.704129
970.270431	63.973998	69.709134
969.453950	59.472406	69.714138
968.795555	61.851180	69.719143
968.216280	61.659531	69.724148
967.558991	62.372857	69.729153
966.924814	72.137429	69.734158
966.172656	63.301568	69.739162
965.208944	62.209142	69.744167
965.258286	60.400435	69.749172
964.972120	62.360436	69.754177
963.774683	67.857481	69.759182
963.082855	65.696769	69.764186
962.370095	59.261088	69.769191
961.472285	56.415635	69.774196
960.465235	56.490751	69.779201
959.897756	57.096748	69.784206
960.024055	51.014846	69.789210
959.061375	61.456159	69.794215
958.780537	62.809759	69.799220
958.029853	48.705044	69.804225
956.800339	58.211097	69.809230
956.786611	49.558951	69.814234
955.125486	66.381402	69.819239
954.519663	51.887780	69.824244
954.002467	61.364072	69.829249
953.740820	51.653808	69.834254
953.458690	50.017695	69.839258
952.800584	54.555285	69.844263
951.849597	56.043904	69.849268
951.071650	58.481128	69.854273
950.570081	60.434404	69.859278
950.129178	57.350671	69.864282
948.840343	64.377725	69.869287
948.296695	60.595976	69.874292
948.133529	56.208058	69.879297
946.772324	57.490715	69.884302
946.104682	60.391363	69.889306
945.190160	53.858485	69.894311
945.096286	53.704723	69.899316
944.360585	63.553256	69.904321
944.049895	58.056553	69.909326
943.494521	48.490803	69.914330
942.348558	57.564094	69.919335
942.090569	49.171592	69.924340
941.474063	59.639827	69.929345
940.407369	60.328418	69.934350
939.897145	47.529021	69.939354
939.212753	57.243230	69.944359
938.897645	57.217713	69.949364
937.929957	52.506804	69.954369
936.971787	55.103598	69.959374
936.506311	49.604721	69.964378
935.849735	55.048825	69.969383
935.339547	52.149587	69.974388
934.375066	56.269153	69.979393
933.733441	51.484285	69.984398
933.474395	55.266093	69.989402
932.937758	56.464856	69.994407
931.819858	53.555089	69.999412
931.492649	52.654707	70.004417
930.488570	57.244203	70.009422
930.325088	49.024323	70.014426
929.106139	58.402548	70.019431
928.307607	55.613850	70.024436
927.854591	56.720460	70.029441
927.186496	64.787312	70.034446
926.927584	57.836298	70.039450
925.688648	66.520694	70.044455
925.023860	54.701531	70.049460
924.637367	59.888193	70.054465
924.180900	56.934677	70.059470
923.946634	51.118311	70.064474
922.641527	58.967982	70.069479
922.447650	52.763564	70.074484
921.531686	49.894208	70.079489
920.172177	48.382235	70.084494
919.834721	58.085394	70.089498
919.114692	64.242926	70.094503
918.817922	56.976239	70.099508
918.583245	58.620543	70.104513
917.532085	51.549600	70.109518
916.657806	55.676895	70.114522
915.982754	61.958158	70.119527
915.623742	57.185090	70.124532
914.654025	60.758292	70.129537
913.729259	59.516186	70.134542
913.667766	53.760637	70.139546
913.020692	55.516299	70.144551
911.926841	47.430283	70.149556
911.355880	54.232722	70.154561
910.468247	56.938150	70.159566
910.298987	45.101646	70.164570
909.540093	56.245402	70.169575
909.000198	51.974211	70.174580
908.220118	54.284053	70.179585
907.433708	57.506386	70.184590
907.109510	50.890622	70.189594
906.481584	55.939086	70.194599
905.363743	51.401899	70.199604
905.125410	49.933865	70.204609
904.371425	54.303796	70.209614
903.139223	54.947778	70.214618
902.517583	53.602244	70.219623
901.919385	53.342659	70.224628
901.832389	49.634912	70.229633
901.123231	52.488559	70.234638
900.436829	54.367178	70.239642
899.587883	50.671876	70.244647
898.966701	46.793673	70.249652
898.571448	60.401124	70.254657
897.262835	54.071331	70.259662
896.543056	50.100008	70.264666
896.125144	59.588890	70.269671
895.752303	52.275968	70.274676
895.217324	53.045542	70.279681
894.269157	56.438700	70.284686
893.919303	55.245459	70.289690
893.240117	53.688311	70.294695
892.002766	54.219576	70.299700
891.104807	56.010439	70.304705
890.451840	54.447542	70.309710
890.168114	47.981462	70.314714
890.043488	51.677224	70.319719
889.455856	54.719693	70.324724
888.674034	58.594163	70.329729
887.866339	65.699215	70.334734
886.876185	59.591560	70.339738
885.880562	64.261730	70.344743
885.292431	47.617503	70.349748
884.933124	57.680533	70.354753
884.445941	64.868619	70.359758
884.039122	53.882056	70.364762
883.105395	61.563831	70.369767
882.337702	54.629142	70.374772
881.832588	54.264862	70.379777
881.362772	57.485703	70.384782
880.784657	59.809143	70.389786
879.628316	63.057242	70.394791
878.952518	58.954343	70.399796
878.353152	49.453962	70.404801
877.694367	51.835972	70.409806
876.825751	52.724879	70.414810
875.922289	59.900366	70.419815
875.333806	61.840679	70.424820
875.152311	52.483530	70.429825
874.591171	64.480500	70.434830
874.092698	50.994852	70.439834
873.184133	59.107866	70.444839
872.830120	51.271556	70.449844
872.327142	57.027120	70.454849
870.632762	63.112648	70.459854
870.523154	62.685424	70.464858
869.690685	60.351581	70.469863
869.391614	59.834662	70.474868
869.006557	53.775796	70.479873
867.816234	58.423340	70.484878
867.277142	56.905405	70.489882
866.582043	52.988510	70.494887
865.853961	50.056158	70.499892
865.081191	50.338455	70.504897
864.137992	65.121219	70.509902
863.677861	51.277810	70.514906
863.288555	57.262867	70.519911
863.015535	52.646437	70.524916
861.904504	45.763250	70.529921
861.040514	52.815760	70.534926
860.915779	58.575783	70.539930
860.393388	52.877823	70.544935
859.447590	49.320955	70.549940
859.127317	49.953862	70.554945
857.625844	51.131156	70.559950
856.910664	42.984904	70.564954
856.179975	45.939759	70.569959
855.860210	45.815645	70.574964
855.761257	52.207076	70.579969
854.975147	44.881093	70.584974
854.211261	44.198458	70.589978
853.353661	47.842143	70.594983
852.840700	50.845926	70.599988
851.696339	48.697350	70.604993
850.939796	51.180080	70.609998
850.629624	50.800549	70.615002
849.957462	49.464647	70.620007
849.529614	55.613535	70.625012
849.134393	45.815746	70.630017
847.880891	55.290963	70.635022
847.366320	47.122246	70.640026
846.627874	44.543213	70.645031
846.369160	49.305840	70.650036
845.414793	47.715233	70.655041
844.131140	57.039133	70.660046
844.049825	49.121581	70.665050
843.739412	59.671997	70.670055
843.068330	49.929152	70.675060
842.095625	51.974779	70.680065
841.195986	56.799996	70.685070
841.344046	56.033718	70.690074
840.266008	54.612607	70.695079
839.258326	58.217109	70.700084
839.042540	55.004529	70.705089
838.181594	52.700462	70.710094
837.313166	49.957615	70.715098
836.514135	59.267463	70.720103
835.881421	54.071196	70.725108
835.690818	54.875856	70.730113
835.247003	57.999525	70.735118
834.317767	51.311343	70.740122
833.184750	56.388174	70.745127
832.519619	56.929316	70.750132
832.503848	53.260700	70.755137
831.534956	57.701126	70.760142
830.773466	56.064055	70.765146
829.750923	58.108158	70.770151
829.605066	63.051525	70.775156
829.417038	56.246944	70.780161
828.134236	60.783068	70.785166
827.439078	51.055099	70.790170
826.726447	60.985136	70.795175
826.245760	53.678356	70.800180
825.969170	54.581859	70.805185
824.670384	54.864314	70.810190
824.174409	54.612132	70.815194
823.547993	50.499815	70.820199
823.111052	52.567406	70.825204
822.557556	54.536853	70.830209
821.526194	57.635772	70.835214
821.272922	53.602834	70.840218
820.730437	57.500728	70.845223
819.348869	61.768725	70.850228
818.814228	50.692141	70.855233
817.845747	58.994479	70.860238
818.211672	59.779943	70.865242
817.396439	54.746775	70.870247
816.159176	54.929555	70.875252
815.866636	49.652342	70.880257
815.140485	58.458582	70.885262
814.399811	53.937098	70.890266
813.642875	52.362387	70.895271
813.101516	51.497686	70.900276
812.922304	52.448768	70.905281
811.525595	48.157867	70.910286
811.056673	46.665046	70.915290
810.302494	51.479733	70.920295
809.781571	46.328761	70.925300
809.113128	45.858029	70.930305
808.139097	58.333886	70.935310
807.779980	49.807695	70.940314
807.336524	55.003435	70.945319
806.732138	51.723404	70.950324
805.817013	46.263019	70.955329
804.887820	51.588114	70.960334
804.326291	54.680062	70.965338
804.009348	49.841975	70.970343
802.905709	55.415615	70.975348
802.059137	52.748149	70.980353
801.170067	53.110480	70.985358
801.671964	52.999085	70.990362
800.892442	49.177653	70.995367
799.911439	49.366959	71.000372
799.019962	50.297378	71.005377
798.195850	61.367960	71.010382
798.291038	48.898021	71.015386
797.344662	60.498999	71.020391
796.104900	59.780166	71.025396
795.858174	46.520982	71.030401
795.049064	65.883982	71.035406
795.034066	54.232674	71.040410
793.646217	58.487490	71.045415
793.060954	55.458309	71.050420
792.767041	46.137997	71.055425
792.064466	51.018591	71.060430
791.529155	52.895263	71.065434
790.496954	41.498928	71.070439
789.792977	49.140998	71.075444
789.532445	49.999370	71.080449
788.324472	45.851905	71.085454
787.724988	44.569108	71.090458
787.057568	48.907940	71.095463
786.151887	44.832206	71.100468
786.251783	50.010839	71.105473
785.759049	51.254682	71.110478
785.259723	50.093137	71.115482
784.111979	52.679160	71.120487
783.084038	49.168515	71.125492
782.407626	42.992049	71.130497
781.591317	66.561943	71.135502
781.400927	52.281382	71.140506
781.101401	54.601494	71.145511
780.319371	55.995470	71.150516
779.177667	41.434269	71.155521
778.784241	52.778489	71.160526
778.209927	52.469401	71.165530
777.451101	47.860934	71.170535
776.143997	53.999984	71.175540
775.798072	54.744218	71.180545
774.923506	60.656721	71.185550
774.984504	54.104244	71.190554
774.709797	44.252598	71.195559
773.544512	54.954867	71.200564
772.787458	45.840751	71.205569
772.422639	51.055514	71.210574
771.563409	46.158680	71.215578
770.903183	45.913733	71.220583
769.884222	48.159138	71.225588
769.697408	44.599757	71.230593
768.701180	57.036578	71.235598
767.951198	51.502608	71.240602
767.503668	51.286880	71.245607
766.915713	54.364118	71.250612
766.147815	52.441082	71.255617
765.014984	51.262117	71.260622
764.834809	50.048192	71.265626
764.213207	48.346297	71.270631
763.885267	51.634455	71.275636
763.091415	43.199564	71.280641
762.028893	53.279925	71.285646
761.810163	41.697334	71.290650
761.005476	50.318964	71.295655
759.926390	46.477426	71.300660
759.580306	44.425741	71.305665
758.732578	54.448255	71.310670
758.131613	38.252415	71.315674
757.856497	45.805717	71.320679
756.450562	58.197378	71.325684
756.186434	44.149343	71.330689
755.527774	45.361259	71.335694
755.305814	50.464971	71.340698
754.121818	42.666206	71.345703
753.160040	58.847552	71.350708
752.693050	47.910033	71.355713
752.408547	46.774220	71.360718
751.808571	35.938306	71.365722
750.910606	39.113783	71.370727
749.949393	49.513908	71.375732
749.996690	47.593564	71.380737
749.118195	41.734711	71.385742
748.539966	41.347405	71.390746
747.657292	43.074380	71.395751
746.929655	55.909994	71.400756
746.777638	49.247929	71.405761
745.665494	48.570307	71.410766
744.958062	47.538095	71.415770
744.251742	49.784200	71.420775
743.770274	53.393271	71.425780
743.144198	48.700604	71.430785
742.060668	49.945470	71.435790
741.298130	50.024325	71.440794
741.027244	46.880455	71.445799
740.411999	53.678931	71.450804
740.181761	44.097759	71.455809
738.664875	55.090982	71.460814
738.063903	55.770168	71.465818
737.817064	44.704567	71.470823
737.523241	47.821715	71.475828
736.800816	41.067540	71.480833
735.692477	42.182316	71.485838
735.185531	43.545125	71.490842
734.682165	43.825573	71.495847
733.490230	43.988561	71.500852
732.832886	39.652540	71.505857
732.248563	47.363880	71.510862
732.167483	44.153524	71.515866
730.969590	48.419128	71.520871
729.630336	51.270630	71.525876
729.635978	45.537529	71.530881
729.411825	49.689109	71.535886
729.033880	42.744473	71.540890
728.332675	36.743863	71.545895
727.206171	57.429994	71.550900
726.580257	48.887952	71.555905
725.968065	43.723149	71.560910
724.976698	45.552592	71.565914
724.494673	36.476716	71.570919
723.776986	40.615405	71.575924
723.839797	39.337568	71.580929
722.861145	47.945900	71.585934
721.868915	50.496152	71.590938
721.354285	47.471516	71.595943
720.700707	46.192617	71.600948
719.829317	47.820034	71.605953
719.211467	54.989513	71.610958
718.531398	51.735750	71.615962
718.266660	31.909864	71.620967
716.779782	51.081139	71.625972
716.277164	42.275047	71.630977
715.825502	39.902711	71.635982
715.261013	41.211607	71.640986
715.109064	41.934426	71.645991
713.945266	46.185146	71.650996
713.179862	42.169110	71.656001
712.345591	48.338562	71.661006
711.831410	46.545460	71.666010
711.784481	49.842499	71.671015
710.562922	48.728150	71.676020
710.216518	44.872485	71.681025
709.446333	54.325999	71.686030
708.544434	47.772294	71.691034
707.489085	43.280451	71.696039
706.518368	55.527144	71.701044
706.290583	44.174664	71.706049
706.222008	56.112142	71.711054
705.950198	51.995441	71.716058
705.789155	45.451516	71.721063
704.247147	63.486719	71.726068
703.497112	41.841011	71.731073
702.388689	49.063367	71.736078
701.756881	46.527327	71.741082
701.437862	39.619049	71.746087
700.787020	47.345715	71.751092
700.554522	49.962670	71.756097
699.258238	53.196854	71.761102
698.766692	48.774519	71.766106
698.392926	52.971999	71.771111
697.754883	58.052077	71.776116
696.818564	45.539806	71.781121
695.924578	48.801402	71.786126
695.396599	50.044565	71.791130
695.165445	53.117047	71.796135
694.045285	50.349679	71.801140
693.230166	49.355129	71.806145
692.618810	51.202927	71.811150
692.217343	46.603824	71.816154
691.882698	42.345745	71.821159
690.460325	48.447991	71.826164
689.800565	43.129923	71.831169
689.502968	50.880774	71.836174
689.069171	43.251180	71.841178
688.487767	47.437566	71.846183
687.571153	52.858467	71.851188
686.918497	41.133672	71.856193
686.484274	52.124844	71.861198
685.359787	49.206782	71.866202
684.731257	45.539547	71.871207
683.950029	50.260800	71.876212
683.419341	44.529520	71.881217
683.321969	47.467159	71.886222
682.357328	45.190701	71.891226
681.561044	46.732054	71.896231
680.414796	47.736196	71.901236
680.357490	45.094493	71.906241
680.130111	48.678885	71.911246
679.270377	44.182716	71.916250
678.562205	45.407265	71.921255
677.867157	47.192698	71.926260
677.091392	56.082557	71.931265
676.241924	51.543752	71.936270
675.532413	43.674210	71.941274
675.353007	45.188304	71.946279
674.103310	52.515169	71.951284
673.297234	42.333417	71.956289
672.882994	49.741717	71.961294
672.484398	45.216279	71.966298
672.201503	44.991700	71.971303
670.854305	44.641700	71.976308
670.451869	44.086071	71.981313
669.903650	50.132716	71.986318
668.905877	47.415260	71.991322
668.123547	38.459757	71.996327
666.948333	48.222197	72.001332
666.863699	44.883101	72.006337
666.692681	42.994367	72.011342
666.152775	46.377786	72.016346
665.320919	49.317261	72.021351
664.288906	51.463861	72.026356
664.127006	44.434375	72.031361
663.431814	43.452278	72.036366
662.152163	48.642410	72.041370
661.561580	42.136927	72.046375
660.785971	47.213683	72.051380
660.838124	45.320952	72.056385
659.909854	53.199038	72.061390
658.989646	57.540306	72.066394
658.523069	41.513917	72.071399
657.831964	59.771611	72.076404
657.340096	47.393591	72.081409
656.312582	53.959684	72.086414
655.445060	47.247564	72.091418
655.174590	44.969389	72.096423
654.627366	60.747277	72.101428
654.356403	46.214653	72.106433
652.985118	46.089271	72.111438
652.167558	39.873825	72.116442
652.159748	49.568648	72.121447
651.283120	54.834960	72.126452
650.402916	50.666914	72.131457
649.914772	48.167934	72.136462
649.093110	44.479424	72.141466
648.953763	41.699400	72.146471
647.811816	50.221795	72.151476
647.209188	41.007448	72.156481
646.504529	44.590571	72.161486
646.152000	58.311066	72.166490
645.631956	50.915987	72.171495
644.436161	46.331419	72.176500
643.632427	40.296702	72.181505
643.598768	39.001110	72.186510
642.725184	42.835060	72.191514
641.969623	43.083146	72.196519
640.895504	53.564361	72.201524
640.695992	41.649153	72.206529
640.416351	47.738188	72.211534
639.403014	46.638025	72.216538
638.782937	42.245635	72.221543
637.989232	45.833479	72.226548
637.293201	38.892210	72.231553
636.911184	49.031399	72.236558
635.350027	50.185211	72.241562
635.300774	45.897464	72.246567
634.663111	44.032580	72.251572
634.085382	48.570053	72.256577
633.527313	41.278808	72.261582
632.414389	43.786810	72.266586
632.062354	36.380757	72.271591
631.522424	35.052247	72.276596
631.206629	38.368443	72.281601
630.464691	44.695099	72.286606
629.632942	42.846932	72.291610
629.111528	40.719111	72.296615
627.851885	46.413851	72.301620
627.249691	38.533548	72.306625
626.603891	39.767101	72.311630
625.971504	44.209199	72.316634
625.719472	33.896665	72.321639
624.683002	40.768542	72.326644
624.124112	37.875560	72.331649
623.556798	44.652226	72.336654
623.105703	44.359821	72.341658
622.176919	34.826843	72.346663
621.146433	41.341377	72.351668
620.883966	33.231935	72.356673
620.761408	37.250643	72.361678
619.297643	38.461494	72.366682
618.695284	40.173834	72.371687
617.983243	40.304609	72.376692
617.714572	32.319159	72.381697
616.941770	37.849638	72.386702
615.942438	41.791932	72.391706
615.623746	34.694387	72.396711
615.173408	50.627148	72.401716
614.073154	47.165943	72.406721
613.242186	43.046842	72.411726
612.632496	43.525596	72.416730
612.361870	45.946777	72.421735
611.813014	46.497844	72.426740
611.286363	46.217474	72.431745
610.297711	40.231142	72.436750
609.509756	42.165429	72.441754
609.329028	40.860143	72.446759
608.016199	45.702345	72.451764
607.280787	39.853880	72.456769
606.869260	40.974436	72.461774
606.288913	50.273156	72.466778
606.145070	46.943493	72.471783
605.217177	54.807343	72.476788
604.297917	53.313742	72.481793
603.697643	44.539004	72.486798
603.082205	47.601727	72.491802
602.174814	43.002792	72.496807
601.256866	48.218926	72.501812
600.926661	37.571915	72.506817
600.593639	38.621622	72.511822
599.877221	52.955151	72.516826
599.340472	39.570323	72.521831
598.143879	43.615002	72.526836
598.048746	45.725960	72.531841
597.324590	39.617087	72.536846
596.276957	50.109864	72.541850
595.883597	52.845485	72.546855
594.938182	63.840812	72.551860
594.655186	55.346702	72.556865
593.480609	45.901760	72.561870
592.848399	47.830172	72.566874
592.765316	43.450045	72.571879
592.027114	52.475864	72.576884
590.668201	49.402794	72.581889
590.215508	49.219460	72.586894
589.275560	50.752183	72.591898
589.312674	40.040365	72.596903
588.735036	42.251823	72.601908
588.176324	39.311512	72.606913
587.281812	45.058505	72.611918
586.328523	35.269248	72.616922
585.845251	41.207787	72.621927
584.944148	48.917562	72.626932
584.273454	46.084972	72.631937
583.864310	48.031477	72.636942
583.081115	53.505278	72.641946
583.041266	51.089457	72.646951
582.038288	54.122444	72.651956
581.248693	42.695467	72.656961
580.710849	50.268541	72.661966
579.717963	46.082200	72.666970
578.985304	44.338118	72.671975
578.123840	48.376740	72.676980
577.758312	42.442567	72.681985
577.868961	47.182650	72.686990
576.638836	54.044391	72.691994
575.872090	45.797647	72.696999
575.207356	46.997960	72.702004
574.823500	44.089727	72.707009
574.053599	41.876915	72.712014
573.154183	39.101258	72.717018
572.526791	40.680400	72.722023
571.950341	41.198024	72.727028
571.617794	42.872132	72.732033
570.683732	39.393943	72.737038
569.544174	53.323361	72.742042
569.348340	44.044249	72.747047
568.904281	45.119529	72.752052
568.121298	39.261310	72.757057
567.003187	48.576298	72.762062
566.398655	51.452788	72.767066
566.442227	38.374514	72.772071
565.561504	43.865427	72.777076
564.633326	48.860852	72.782081
564.035311	44.354583	72.787086
563.410311	54.748521	72.792090
562.995914	46.183888	72.797095
561.983795	51.530152	72.802100
561.308854	51.590379	72.807105
560.772657	49.979014	72.812110
560.261982	52.399010	72.817114
559.318478	45.397834	72.822119
558.603793	48.146791	72.827124
558.113280	46.638537	72.832129
557.657092	48.201454	72.837134
556.480455	47.931582	72.842138
556.158564	39.085715	72.847143
555.216108	49.104436	72.852148
554.895112	43.858611	72.857153
554.727831	42.708883	72.862158
553.308769	49.654342	72.867162
552.783748	44.770597	72.872167
552.040755	47.145595	72.877172
551.605439	48.053906	72.882177
550.702203	46.958321	72.887182
549.878546	45.960448	72.892186
549.714754	48.195884	72.897191
548.874918	45.732445	72.902196
548.122626	54.184929	72.907201
547.204432	51.038533	72.912206
546.464366	49.025982	72.917210
546.033072	34.585168	72.922215
545.776580	49.201835	72.927220
545.456593	43.697230	72.932225
544.382988	39.689344	72.937230
543.598629	39.842698	72.942234
543.364353	36.273559	72.947239
542.225625	45.574491	72.952244
541.289537	46.089481	72.957249
541.050239	40.854301	72.962254
540.436670	35.322346	72.967258
539.808944	33.921109	72.972263
538.699292	36.337165	72.977268
538.461455	41.269944	72.982273
538.101947	30.088304	72.987278
536.789984	43.931644	72.992282
536.105368	46.464505	72.997287
535.118896	46.042928	73.002292
534.954184	42.894793	73.007297
534.366974	36.445585	73.012302
533.332638	49.169228	73.017306
532.908194	39.880808	73.022311
532.417397	45.749591	73.027316
532.140285	41.532840	73.032321
531.431197	49.007040	73.037326
530.168274	50.510805	73.042330
529.773258	43.668282	73.047335
529.133367	44.069865	73.052340
528.188685	42.892581	73.057345
527.510992	41.806811	73.062350
527.002056	46.729160	73.067354
527.086740	36.304664	73.072359
525.479350	46.918163	73.077364
524.614618	49.612181	73.082369
524.446124	54.688462	73.087374
523.784442	52.261308	73.092378
523.538568	40.951176	73.097383
522.541864	49.985067	73.102388
521.623122	47.930022	73.107393
521.512187	43.131714	73.112398
520.225487	51.104779	73.117402
519.946807	36.308502	73.122407
518.877584	40.812319	73.127412
518.680960	42.740749	73.132417
518.099454	42.603178	73.137422
517.103439	50.033201	73.142426
516.342676	40.654855	73.147431
515.967187	46.972051	73.152436
515.335797	52.530498	73.157441
514.245491	40.779292	73.162446
513.381428	37.617982	73.167450
513.345536	45.942159	73.172455
512.673143	46.216460	73.177460
512.113412	44.055345	73.182465
510.998147	47.273400	73.187470
510.366193	45.678878	73.192474
510.083455	46.960283	73.197479
509.458882	53.984212	73.202484
508.238579	54.314253	73.207489
507.776957	39.618081	73.212494
507.005219	39.523431	73.217498
506.777389	42.366734	73.222503
506.125931	48.084496	73.227508
504.994583	46.053863	73.232513
504.445361	41.006830	73.237518
503.961232	47.442258	73.242522
503.439908	42.193662	73.247527
502.921266	46.493087	73.252532
502.138494	39.653994	73.257537
501.579262	37.420263	73.262542
500.483579	52.541196	73.267546
499.799318	43.677370	73.272551
499.304955	47.086681	73.277556
498.796787	48.530154	73.282561
498.252355	43.685786	73.287566
496.901293	45.594692	73.292570
496.448030	39.322853	73.297575
495.622892	45.393135	73.302580
495.314472	44.191778	73.307585
495.210237	37.315561	73.312590
493.725838	48.319492	73.317594
493.695034	43.374381	73.322599
493.256635	44.904511	73.327604
491.761676	40.396070	73.332609
491.057209	43.039336	73.337614
490.468314	52.419858	73.342618
490.084593	44.722414	73.347623
489.582448	46.986521	73.352628
488.661709	42.727228	73.357633
488.571823	40.095457	73.362638
487.514419	49.328262	73.367642
486.761616	35.561582	73.372647
485.801080	36.585111	73.377652
485.069610	44.936516	73.382657
484.835453	32.681515	73.387662
483.940265	47.275344	73.392666
483.986484	43.142710	73.397671
482.979580	47.037373	73.402676
482.114265	49.783537	73.407681
481.692787	39.338753	73.412686
480.415432	47.944280	73.417690
479.731894	48.652449	73.422695
479.355729	41.302311	73.427700
478.921412	42.901180	73.432705
478.779912	41.174918	73.437710
477.389802	48.117378	73.442714
476.711247	45.626694	73.447719
475.884238	41.724636	73.452724
475.281376	44.536223	73.457729
475.244307	37.958390	73.462734
473.850094	49.935137	73.467738
473.466694	47.387972	73.472743
473.017284	42.817055	73.477748
472.346858	54.017756	73.482753
471.764162	37.429620	73.487758
470.710594	43.518953	73.492762
470.206859	40.262409	73.497767
469.814550	46.900833	73.502772
468.984966	50.056048	73.507777
468.178460	39.276791	73.512782
467.423238	47.272439	73.517786
466.767293	47.085238	73.522791
466.797275	41.573781	73.527796
465.902461	42.791852	73.532801
465.269712	35.916259	73.537806
464.285987	48.187157	73.542810
463.237281	40.814858	73.547815
462.366932	43.957644	73.552820
461.646869	48.200856	73.557825
461.452844	45.697640	73.562830
460.956866	39.396346	73.567834
460.766373	34.016210	73.572839
460.364781	44.248407	73.577844
459.030662	51.353845	73.582849
458.782836	37.000524	73.587854
457.558433	42.994075	73.592858
456.519445	40.144506	73.597863
456.334625	47.202460	73.602868
455.384559	44.434918	73.607873
455.195403	41.369534	73.612878
454.516261	50.449047	73.617882
453.351179	47.002979	73.622887
452.925028	33.263122	73.627892
452.173129	48.099058	73.632897
452.190480	38.224612	73.637902
451.666086	45.967446	73.642906
450.580999	42.544905	73.647911
450.120533	40.620304	73.652916
449.341907	43.417322	73.657921
448.764096	45.548412	73.662926
448.008691	45.328176	73.667930
447.168894	35.096707	73.672935
446.046019	33.954155	73.677940
445.333475	40.537942	73.682945
444.799173	34.890886	73.687950
444.446511	52.053878	73.692954
444.264471	36.993066	73.697959
443.240573	39.874893	73.702964
442.220474	40.103684	73.707969
441.951042	34.422315	73.712974
441.336041	37.305228	73.717978
440.801435	44.508796	73.722983
439.728010	41.477063	73.727988
439.044410	47.534273	73.732993
438.678112	39.007745	73.737998
437.952695	57.116377	73.743002
436.883566	50.701396	73.748007
436.532289	48.483433	73.753012
435.762093	39.245396	73.758017
435.667516	43.773734	73.763022
434.687768	48.485681	73.768026
434.001248	39.838285	73.773031
433.537761	43.813542	73.778036
432.445603	45.140337	73.783041
431.709004	38.200876	73.788046
430.642443	45.897630	73.793050
430.388893	42.153379	73.798055
430.472843	32.758761	73.803060
429.594866	44.684811	73.808065
428.886096	46.297453	73.813070
427.908046	51.600489	73.818074
427.270621	36.623276	73.823079
426.731699	43.031172	73.828084
425.623892	53.314395	73.833089
425.436514	47.619950	73.838094
424.587459	52.246423	73.843098
424.135166	51.673548	73.848103
423.497790	41.594338	73.853108
422.475658	49.455905	73.858113
422.023454	43.193376	73.863118
421.481983	46.693783	73.868122
420.783281	35.589869	73.873127
419.589838	46.497014	73.878132
419.283751	50.677431	73.883137
419.062965	41.214667	73.888142
418.247850	43.314188	73.893146
417.230145	40.817636	73.898151
416.280851	46.567100	73.903156
415.827664	47.389972	73.908161
415.335540	37.975174	73.913166
415.081280	45.859475	73.918170
414.297396	48.272565	73.923175
413.632952	48.370584	73.928180
412.802901	44.713460	73.933185
412.434887	40.750908	73.938190
411.409589	49.825658	73.943194
410.826241	45.135748	73.948199
410.415991	40.888189	73.953204
409.103188	44.871043	73.958209
408.604718	38.928128	73.963214
407.730764	41.260953	73.968218
407.325657	41.598349	73.973223
406.993153	32.687980	73.978228
406.362017	41.710961	73.983233
406.048827	35.683333	73.988238
404.893411	44.799315	73.993242
404.431443	53.420036	73.998247
403.453168	38.932379	74.003252
402.354295	52.655092	74.008257
402.101733	45.640090	74.013262
401.913540	46.792901	74.018266
401.128176	43.527630	74.023271
400.097228	44.601836	74.028276
399.109352	52.744959	74.033281
398.814654	44.063527	74.038286
398.700856	48.703738	74.043290
397.729153	45.953860	74.048295
397.048811	38.122355	74.053300
396.349114	43.549780	74.058305
395.798706	41.585905	74.063310
394.340999	50.245437	74.068314
394.050255	48.569770	74.073319
393.602525	43.708444	74.078324
392.912750	40.929416	74.083329
392.645775	39.710432	74.088334
392.009186	53.387873	74.093338
391.155165	49.166873	74.098343
390.670842	44.757656	74.103348
389.569164	54.232517	74.108353
389.019462	46.295038	74.113358
388.343855	41.244522	74.118362
387.713398	46.279295	74.123367
387.087095	40.697375	74.128372
385.606649	53.050601	74.133377
385.468839	45.881699	74.138382
384.693823	46.241771	74.143386
384.425222	42.566158	74.148391
384.367673	47.902302	74.153396
383.243576	46.307387	74.158401
382.580995	47.520022	74.163406
381.957458	51.998608	74.168410
380.880403	45.283723	74.173415
380.261808	45.376022	74.178420
379.291346	50.833983	74.183425
379.247371	45.495162	74.188430
379.020851	49.147241	74.193434
377.709408	44.727901	74.198439
376.912490	37.552068	74.203444
376.403243	49.354722	74.208449
375.998651	41.638555	74.213454
374.618520	42.460907	74.218458
373.849913	45.562279	74.223463
373.664730	42.213995	74.228468
373.326076	40.276307	74.233473
372.746272	46.533033	74.238478
372.457788	47.682903	74.243482
371.373821	51.555195	74.248487
370.788676	35.637699	74.253492
369.616650	41.946216	74.258497
368.950184	49.763741	74.263502
368.186397	46.230115	74.268506
367.623838	47.401583	74.273511
367.537934	45.038843	74.278516
366.477759	54.324172	74.283521
365.865996	37.366975	74.288526
365.214374	44.347926	74.293530
364.680753	46.801575	74.298535
364.468722	43.367685	74.303540
362.917728	45.576602	74.308545
362.263650	37.144838	74.313550
361.969157	39.401108	74.318554
361.563925	43.223590	74.323559
360.577721	44.929346	74.328564
359.559874	38.359582	74.333569
359.169080	37.002638	74.338574
358.912774	37.638027	74.343578
358.113737	38.784102	74.348583
357.522565	38.264911	74.353588
356.768060	45.481455	74.358593
356.321627	43.166707	74.363598
355.226551	44.911892	74.368602
354.256371	48.977369	74.373607
353.905460	42.205131	74.378612
353.386801	45.534758	74.383617
353.071701	43.205390	74.388622
351.849309	47.588602	74.393626
350.729294	42.687765	74.398631
350.799399	35.045771	74.403636
350.334040	47.845949	74.408641
349.631668	39.771967	74.413646
348.611337	50.066505	74.418650
347.740156	48.164797	74.423655
347.419537	48.037731	74.428660
346.898857	51.996886	74.433665
345.875931	45.864750	74.438670
345.334689	41.444115	74.443674
344.512243	50.377751	74.448679
344.421896	47.354978	74.453684
343.446011	45.971429	74.458689
342.553957	46.089969	74.463694
341.959084	48.192262	74.468698
341.545922	43.114129	74.473703
341.386395	38.028694	74.478708
339.922880	44.632835	74.483713
339.445926	36.750016	74.488718
338.993588	39.763147	74.493722
338.315046	48.804737	74.498727
337.338708	37.670984	74.503732
336.282493	38.222540	74.508737
336.262950	39.752177	74.513742
335.824317	34.990344	74.518746
335.096928	41.459827	74.523751
334.285860	43.749539	74.528756
333.541914	44.427950	74.533761
333.255484	42.592332	74.538766
332.239941	44.581895	74.543770
331.122381	51.651303	74.548775
330.791422	40.687511	74.553780
330.279557	45.594586	74.558785
329.419852	49.959433	74.563790
328.519049	36.292104	74.568794
327.713947	41.957114	74.573799
327.770763	42.697146	74.578804
327.139908	49.994918	74.583809
326.413494	43.936962	74.588814
325.528147	47.653039	74.593818
324.565768	43.308987	74.598823
324.560432	35.669555	74.603828
324.012540	48.251077	74.608833
323.080651	53.322865	74.613838
322.765666	46.601676	74.618842
321.744139	40.480369	74.623847
320.670072	41.085240	74.628852
320.109635	41.810103	74.633857
319.598373	31.039059	74.638862
319.239100	44.486223	74.643866
318.401915	34.602903	74.648871
317.532555	35.178305	74.653876
316.728105	46.130724	74.658881
316.256510	43.225485	74.663886
315.924916	46.870658	74.668890
315.027779	43.845581	74.673895
314.480812	39.022169	74.678900
313.877399	41.895379	74.683905
313.203215	35.874839	74.688910
311.754340	47.316318	74.693914
311.425869	42.538507	74.698919
311.171259	44.447806	74.703924
310.645850	39.103720	74.708929
310.152252	37.449356	74.713934
309.235814	43.961591	74.718938
308.237126	42.922312	74.723943
308.035587	32.373143	74.728948
306.935957	47.168324	74.733953
306.379456	44.486353	74.738958
305.615787	41.927286	74.743962
304.958350	43.948095	74.748967
304.923618	32.673753	74.753972
303.584552	40.931219	74.758977
303.047568	39.581814	74.763982
302.543818	40.999389	74.768986
302.078323	52.397687	74.773991
301.236971	40.341998	74.778996
299.984451	44.756842	74.784001
299.913419	37.839086	74.789006
299.737354	39.358976	74.794010
298.423069	38.557657	74.799015
297.675181	43.037154	74.804020
297.089070	43.278837	74.809025
296.661143	42.252673	74.814030
296.189751	41.616635	74.819034
295.115562	41.477217	74.824039
294.799905	44.522188	74.829044
293.842861	42.307758	74.834049
293.089369	46.669879	74.839054
292.190892	36.023633	74.844058
291.611344	46.120200	74.849063
291.214833	48.164080	74.854068
290.798086	45.048255	74.859073
290.203474	48.333229	74.864078
289.139472	48.889201	74.869082
288.655752	41.034281	74.874087
288.310607	35.667779	74.879092
287.195654	45.510636	74.884097
286.404684	43.720747	74.889102
285.668984	39.714322	74.894106
285.435662	44.025076	74.899111
285.348407	25.880465	74.904116
283.710566	43.710322	74.909121
282.989935	35.421659	74.914126
282.838097	45.965718	74.919130
282.290715	45.674530	74.924135
281.324325	37.994316	74.929140
280.703893	40.939631	74.934145
280.020218	37.200882	74.939150
279.743241	45.916703	74.944154
278.269789	44.497369	74.949159
277.667459	33.624158	74.954164
277.142800	50.808246	74.959169
276.842781	37.631810	74.964174
276.405310	43.753901	74.969178
275.316360	51.397510	74.974183
274.641317	30.914926	74.979188
274.015532	43.253397	74.984193
273.598104	38.781509	74.989198
272.784720	38.961652	74.994202
272.027133	49.706342	74.999207
271.587617	39.188799	75.004212
271.074526	33.940534	75.009217
270.315517	36.972593	75.014222
269.708585	29.421174	75.019226
268.718299	44.498554	75.024231
267.942768	44.180658	75.029236
267.067248	43.465538	75.034241
266.619522	40.472927	75.039246
266.358406	41.251017	75.044250
265.813430	34.946549	75.049255
265.200376	41.640673	75.054260
263.787605	47.315829	75.059265
263.372934	48.594634	75.064270
263.094077	37.980524	75.069274
262.003205	53.636919	75.074279
261.088229	44.841496	75.079284
260.544233	53.137837	75.084289
260.021828	37.368079	75.089294
259.842635	43.704469	75.094298
259.321364	45.979551	75.099303
258.414456	38.570562	75.104308
257.634793	49.542700	75.109313
257.138853	43.086912	75.114318
256.259136	38.956796	75.119322
255.451143	52.120678	75.124327
255.168915	40.464742	75.129332
254.430717	50.381602	75.134337
253.082316	48.839848	75.139342
252.811310	38.711766	75.144346
252.140624	45.143846	75.149351
251.867613	45.464942	75.154356
251.201907	55.471174	75.159361
250.262891	43.697579	75.164366
249.786298	37.604563	75.169370
249.285324	44.993607	75.174375
248.677367	40.373899	75.179380
247.520741	43.467769	75.184385
247.012075	46.470971	75.189390
246.630771	38.019422	75.194394
245.246074	44.669395	75.199399
244.510912	42.657737	75.204404
243.840412	40.225765	75.209409
243.611251	44.515358	75.214414
243.464693	37.245372	75.219418
242.520733	40.453578	75.224423
241.624209	38.473950	75.229428
240.909669	47.229559	75.234433
240.295382	51.022304	75.239438
240.087322	39.400282	75.244442
238.963484	46.019716	75.249447
238.533577	40.863852	75.254452
237.821709	44.359915	75.259457
237.144816	50.430291	75.264462
236.283288	46.103317	75.269466
235.558239	46.129043	75.274471
235.359836	42.111103	75.279476
234.361481	42.628249	75.284481
233.680513	38.849659	75.289486
233.130598	37.759375	75.294490
232.405292	41.904129	75.299495
232.131622	46.987714	75.304500
231.644421	45.953664	75.309505
230.432259	44.519517	75.314510
229.945697	41.291831	75.319514
229.308129	43.396223	75.324519
228.300676	34.309636	75.329524
227.427463	42.835074	75.334529
226.587437	35.653559	75.339534
226.373369	36.872006	75.344538
225.736082	45.984308	75.349543
225.793523	40.772837	75.354548
224.673774	40.140819	75.359553
224.005842	35.202676	75.364558
223.457116	31.136507	75.369562
222.456447	43.935289	75.374567
221.872307	46.622522	75.379572
221.196788	39.621363	75.384577
220.167104	44.557384	75.389582
220.483397	38.492522	75.394586
219.035760	42.148456	75.399591
218.347980	35.228103	75.404596
217.837981	44.121418	75.409601
217.330603	49.046720	75.414606
217.048545	38.491478	75.419610
215.704737	51.545241	75.424615
215.384754	44.138899	75.429620
214.689588	37.326956	75.434625
214.111039	48.877319	75.439630
213.273467	40.574206	75.444634
212.547243	49.975080	75.449639
212.228221	38.656180	75.454644
211.376411	47.004748	75.459649
210.327070	48.507740	75.464654
209.841173	38.210498	75.469658
209.070827	47.829715	75.474663
208.770381	51.583474	75.479668
208.346881	43.040888	75.484673
207.588330	47.146795	75.489678
206.858249	46.389588	75.494682
205.830563	55.870064	75.499687
205.410805	41.670369	75.504692
204.449765	40.300280	75.509697
203.673594	45.213240	75.514702
203.304816	45.126986	75.519706
203.014167	55.041896	75.524711
202.510568	43.214682	75.529716
201.322026	39.717291	75.534721
200.859198	45.125922	75.539726
200.486471	33.754090	75.544730
199.004862	42.302409	75.549735
198.432639	44.368006	75.554740
197.978963	34.691682	75.559745
197.506664	44.592966	75.564750
197.640642	44.363486	75.569754
196.175186	47.000413	75.574759
195.582361	42.034534	75.579764
195.069604	41.658999	75.584769
193.545485	41.883089	75.589774
192.931255	40.978108	75.594778
192.126333	41.417125	75.599783
191.967844	42.439058	75.604788
191.931219	42.725629	75.609793
191.289334	44.237786	75.614798
190.686854	40.356811	75.619802
189.331097	44.756626	75.624807
188.806451	31.573453	75.629812
188.371138	41.024140	75.634817
187.687222	47.001028	75.639822
186.884955	43.465717	75.644826
186.488839	47.843431	75.649831
185.852752	39.374168	75.654836
184.699398	46.964997	75.659841
183.707113	46.259061	75.664846
183.720671	32.225266	75.669850
183.071394	37.591082	75.674855
182.541350	28.921994	75.679860
181.718532	45.461334	75.684865
181.045268	40.287511	75.689870
180.463984	37.683641	75.694874
179.173909	46.390669	75.699879
178.659718	39.642925	75.704884
178.373784	37.554938	75.709889
177.756534	37.629727	75.714894
177.439109	35.125716	75.719898
176.338357	44.578419	75.724903
175.923550	34.126355	75.729908
175.253723	50.939353	75.734913
173.888157	37.114389	75.739918
173.392800	40.118635	75.744922
172.878721	40.639021	75.749927
172.480488	44.584990	75.754932
171.990204	46.080867	75.759937
170.797251	45.973053	75.764942
170.441506	39.851329	75.769946
169.559583	42.392083	75.774951
169.317921	42.362839	75.779956
168.761806	47.363726	75.784961
167.849131	49.620804	75.789966
167.278221	41.259426	75.794970
166.339256	48.811351	75.799975
165.314912	48.757083	75.804980
164.970238	45.628215	75.809985
164.322691	49.743245	75.814990
164.000357	42.386175	75.819994
163.109160	50.403570	75.824999
162.179179	33.282738	75.830004
161.988002	49.331874	75.835009
161.112461	44.754853	75.840014
160.936797	45.940374	75.845018
159.657632	43.334236	75.850023
158.977054	50.643119	75.855028
158.457862	40.485241	75.860033
158.016197	46.133353	75.865038
157.353797	40.719687	75.870042
156.257208	50.282123	75.875047
156.210251	47.728683	75.880052
155.674732	40.113871	75.885057
154.204620	45.558528	75.890062
153.895778	40.008069	75.895066
153.085741	44.847594	75.900071
152.803536	35.959225	75.905076
151.916856	33.544403	75.910081
150.630212	47.334969	75.915086
150.551029	33.151963	75.920090
149.826827	46.166882	75.925095
149.395987	36.690356	75.930100
148.764725	42.155810	75.935105
147.459331	48.619724	75.940110
147.063295	40.711440	75.945114
147.154235	43.921831	75.950119
145.767952	44.647520	75.955124
144.726676	38.404870	75.960129
144.164723	40.065142	75.965134
144.053980	41.626665	75.970138
143.673560	42.154132	75.975143
142.831509	35.135401	75.980148
141.720050	48.898040	75.985153
141.054463	50.902843	75.990158
140.874592	39.995435	75.995162
140.372384	48.627323	76.000167
139.197992	46.731462	76.005172
138.843830	40.806610	76.010177
137.831506	40.130697	76.015182
137.516630	42.546357	76.020186
136.703977	44.096794	76.025191
135.943141	36.235642	76.030196
135.777694	34.327146	76.035201
134.788735	42.700753	76.040206
133.950415	43.684429	76.045210
133.460319	40.173480	76.050215
132.953719	40.697413	76.055220
132.389096	35.373822	76.060225
131.538017	43.375364	76.065230
130.818246	33.791951	76.070234
130.412556	41.820246	76.075239
129.267240	33.012735	76.080244
128.625747	35.616090	76.085249
127.919063	44.471392	76.090254
127.861363	42.173556	76.095258
126.366855	40.629940	76.100263
125.503644	37.463914	76.105268
124.812252	36.744719	76.110273
124.242542	33.011503	76.115278
124.092683	32.180730	76.120282
123.604723	46.460541	76.125287
123.403231	37.507268	76.130292
122.791624	35.581604	76.135297
121.593531	50.091344	76.140302
121.325931	43.848342	76.145306
120.054672	43.406111	76.150311
119.509740	42.871720	76.155316
118.928469	38.186296	76.160321
118.164999	46.804652	76.165326
117.380014	37.450836	76.170330
116.417481	47.930190	76.175335
115.962255	42.261153	76.180340
115.893236	43.551097	76.185345
115.007922	39.436123	76.190350
114.544957	38.097038	76.195354
113.607379	44.103349	76.200359
113.253908	42.169642	76.205364
112.141088	41.091874	76.210369
111.044370	40.301696	76.215374
110.423007	35.974327	76.220378
110.295178	38.795400	76.225383
109.869579	45.008656	76.230388
109.505068	35.147830	76.235393
108.186468	44.927028	76.240398
107.977075	28.244838	76.245402
106.989070	39.180833	76.250407
105.844137	36.264740	76.255412
105.375079	33.105258	76.260417
104.958459	41.773961	76.265422
104.649974	32.154938	76.270426
103.992827	45.086631	76.275431
103.046956	29.231505	76.280436
102.419661	26.546686	76.285441
101.794013	32.473294	76.290446
101.107632	28.047489	76.295450
100.069010	35.579049	76.300455
99.572236	30.039648	76.305460
99.215841	26.425390	76.310465
98.179968	43.380333	76.315470
98.131358	44.597637	76.320474
97.416890	34.653848	76.325479
96.522693	33.080758	76.330484
96.052354	31.911586	76.335489
94.640639	33.734181	76.340494
94.129876	33.386735	76.345498
93.599886	32.574003	76.350503
93.259678	27.891150	76.355508
92.816464	30.041850	76.360513
91.303035	39.257612	76.365518
91.260375	35.164394	76.370522
90.847851	35.225482	76.375527
89.812687	40.104076	76.380532
89.245157	35.761821	76.385537
88.340356	41.704566	76.390542
87.814784	34.233271	76.395546
86.849664	41.551268	76.400551
86.218597	36.064823	76.405556
85.736382	30.743875	76.410561
85.339829	39.931347	76.415566
85.306045	33.491798	76.420570
84.157561	32.538002	76.425575
83.041798	39.985678	76.430580
82.558064	30.817229	76.435585
81.393095	40.076776	76.440590
80.768115	27.873159	76.445594
80.240468	42.088333	76.450599
79.486944	29.802712	76.455604
79.403404	35.857342	76.460609
78.699710	45.503802	76.465614
78.719580	39.167658	76.470618
77.353127	38.048352	76.475623
76.754307	36.798747	76.480628
76.074182	45.287126	76.485633
74.892126	45.991326	76.490638
74.770874	27.796991	76.495642
74.221844	39.916663	76.500647
73.187996	34.361990	76.505652
72.255849	36.275277	76.510657
71.448554	38.938203	76.515662
71.169838	44.759034	76.520666
71.155502	35.988813	76.525671
70.342156	36.730409	76.530676
69.553151	37.594279	76.535681
68.357653	46.420313	76.540686
68.140893	36.066005	76.545690
67.307894	32.086212	76.550695
66.515987	38.607044	76.555700
66.037064	35.805532	76.560705
65.257063	37.863291	76.565710
65.104597	27.517660	76.570714
63.829033	31.939439	76.575719
63.127348	38.665078	76.580724
62.843205	35.471384	76.585729
62.412144	37.856694	76.590734
61.258739	31.092656	76.595738
60.483123	30.246563	76.600743
59.624088	39.892565	76.605748
59.604555	34.065754	76.610753
59.041286	45.657850	76.615758
58.087509	34.869151	76.620762
57.297388	41.232007	76.625767
57.225553	32.038877	76.630772
56.620294	34.516622	76.635777
55.213932	41.187489	76.640782
54.941989	36.796527	76.645786
54.129306	42.847593	76.650791
53.104995	41.574389	76.655796
52.420039	37.834340	76.660801
51.845357	29.773228	76.665806
51.383550	33.177416	76.670810
51.355519	41.462454	76.675815
50.332889	45.071203	76.680820
49.314234	43.904330	76.685825
48.524331	46.315333	76.690830
48.318918	37.313814	76.695834
47.736812	31.898421	76.700839
46.804069	42.379347	76.705844
46.162101	36.435762	76.710849
45.357114	46.935741	76.715854
45.247040	35.276060	76.720858
44.496179	40.216562	76.725863
43.607527	32.011560	76.730868
43.426609	35.224297	76.735873
42.092583	45.931651	76.740878
40.998261	38.681960	76.745882
40.555880	43.529111	76.750887
39.901077	45.981648	76.755892
39.731418	34.609014	76.760897
39.451429	38.760065	76.765902
38.519416	40.824729	76.770906
37.382667	41.190562	76.775911
36.887559	50.742266	76.780916
36.764885	37.225376	76.785921
35.304949	44.016762	76.790926
34.634410	35.830591	76.795930
34.008177	40.653449	76.800935
33.742925	37.286437	76.805940
33.532237	33.847645	76.810945
32.468279	42.338900	76.815950
31.842706	38.780197	76.820954
31.175966	33.495000	76.825959
30.122602	38.291364	76.830964
29.519283	34.315954	76.835969
28.931630	41.127493	76.840974
28.604948	32.228900	76.845978
27.838952	42.982857	76.850983
26.730424	37.711351	76.855988
26.307289	31.961529	76.860993
25.546229	41.420028	76.865998
25.347584	35.779480	76.871002
24.528034	40.179012	76.876007
23.701153	38.434365	76.881012
23.373913	39.030638	76.886017
22.603726	31.525838	76.891022
21.868160	41.834974	76.896026
20.764552	32.882102	76.901031
20.220605	41.328269	76.906036
20.034438	36.516781	76.911041
19.190427	37.348439	76.916046
18.109071	36.625240	76.921050
17.531669	36.608558	76.926055
17.033233	43.916801	76.931060
17.116069	34.617004	76.936065
16.058486	42.274622	76.941070
14.888148	42.051315	76.946074
14.397725	40.929517	76.951079
13.952611	35.260472	76.956084
13.464130	29.968928	76.961089
12.370919	33.719832	76.966094
11.831738	32.530118	76.971098
11.612103	30.373235	76.976103
10.108556	30.931623	76.981108
9.444718	36.205180	76.986113
8.720107	37.421495	76.991118
8.685451	33.568279	76.996122
8.160936	34.833104	77.001127
7.478915	36.857906	77.006132
6.884817	40.021430	77.011137
6.110450	36.529045	77.016142
5.728971	35.555452	77.021147
4.396114	35.197223	77.026151
3.752632	38.020120	77.031156
3.398721	42.123041	77.036161