Fri Mar 05 20:00:55 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.843921	105.136417	0.000000
-1.933810	92.345954	0.005005
-2.702373	57.761570	0.010010
-4.648755	21.897003	0.015014
-8.738397	8.126645	0.020019
-14.045252	11.171378	0.025024
-19.137382	3.439773	0.030029
-23.472649	-5.954787	0.035034
-27.511646	2.998367	0.040038
-31.357226	-3.670495	0.045043
-34.736130	1.115189	0.050048
-38.133344	4.199131	0.055053
-41.988742	9.174375	0.060058
-46.144649	12.529163	0.065062
-49.757331	8.631699	0.070067
-53.340352	15.383298	0.075072
-57.016078	5.047807	0.080077
-60.954841	11.499776	0.085082
-64.577526	13.512715	0.090086
-68.534127	12.838210	0.095091
-72.358714	14.342479	0.100096
-75.904705	4.093554	0.105101
-79.802762	12.535461	0.110106
-83.631405	7.127104	0.115110
-86.793259	6.530843	0.120115
-90.646680	14.336448	0.125120
-94.812382	11.427711	0.130125
-98.764294	21.019945	0.135130
-102.372446	13.652576	0.140134
-106.216149	13.573549	0.145139
-110.145862	9.747258	0.150144
-113.275454	1.860441	0.155149
-117.433767	10.996778	0.160154
-121.095130	8.673089	0.165158
-125.070861	-1.106648	0.170163
-128.882774	8.283516	0.175168
-132.266125	1.384952	0.180173
-136.172436	8.825329	0.185178
-139.910687	5.585122	0.190182
-143.474037	3.439792	0.195187
-147.276817	2.250447	0.200192
-150.972707	0.550473	0.205197
-155.153445	9.745641	0.210202
-159.213515	1.269353	0.215206
-162.961327	2.419317	0.220211
-167.053523	8.514315	0.225216
-170.367430	6.196760	0.230221
-174.027132	14.646507	0.235226
-177.811377	16.242274	0.240230
-181.284561	18.108527	0.245235
-185.004374	7.318236	0.250240
-188.568217	5.292899	0.255245
-192.846218	8.575954	0.260250
-196.287210	7.797303	0.265254
-200.230748	4.345526	0.270259
-204.359875	17.681457	0.275264
-207.855886	1.039757	0.280269
-211.599342	6.285975	0.285274
-215.401283	10.477104	0.290278
-218.784472	4.218876	0.295283
-222.652463	6.670159	0.300288
-226.219779	5.290399	0.305293
-230.377302	9.968801	0.310298
-234.077631	7.429157	0.315302
-237.272842	3.744474	0.320307
-241.475782	7.636945	0.325312
-245.158045	10.183200	0.330317
-249.309445	12.635604	0.335322
-253.287232	9.340767	0.340326
-256.451291	15.746667	0.345331
-260.679881	18.831146	0.350336
-264.028202	8.241888	0.355341
-267.926155	13.812469	0.360346
-271.816574	19.211547	0.365350
-275.339736	19.357591	0.370355
-279.360030	15.238537	0.375360
-282.932806	12.148759	0.380365
-286.675803	12.536487	0.385370
-290.671370	9.600939	0.390374
-293.911671	14.819008	0.395379
-298.015443	12.604055	0.400384
-301.872725	8.488983	0.405389
-305.961780	11.404611	0.410394
-309.467837	11.607899	0.415398
-312.829088	11.420651	0.420403
-316.830512	13.641074	0.425408
-320.410024	10.000503	0.430413
-324.082878	16.377322	0.435418
-327.908078	22.592390	0.440422
-331.830647	11.760591	0.445427
-335.678119	13.951738	0.450432
-339.346729	9.623684	0.455437
-343.245131	14.323988	0.460442
-347.157788	12.524883	0.465446
-350.673699	12.108492	0.470451
-354.547179	16.432680	0.475456
-358.001162	3.611730	0.480461
-362.002238	8.612301	0.485466
-365.905752	6.095840	0.490470
-369.438699	6.439124	0.495475
-373.227084	8.031125	0.500480
-376.960728	11.650210	0.505485
-380.850266	19.354791	0.510490
-384.565815	18.005241	0.515494
-388.231639	11.522730	0.520499
-392.031356	12.670298	0.525504
-395.628724	10.920279	0.530509
-399.709119	8.809002	0.535514
-403.505410	4.040974	0.540518
-407.099120	5.825868	0.545523
-411.092196	23.082731	0.550528
-414.348621	14.210494	0.555533
-418.194975	15.904860	0.560538
-422.332183	13.706500	0.565542
-425.720633	7.496725	0.570547
-429.645749	11.094425	0.575552
-433.296031	5.084163	0.580557
-437.376994	15.435523	0.585562
-441.299687	9.746311	0.590566
-444.741576	16.458580	0.595571
-448.642341	17.187140	0.600576
-452.021219	15.930589	0.605581
-455.872924	13.894852	0.610586
-459.850995	11.887185	0.615590
-463.326911	11.939230	0.620595
-467.560000	15.931520	0.625600
-471.132066	8.458051	0.630605
-474.949984	15.030141	0.635610
-478.636265	10.213127	0.640614
-481.926955	6.682797	0.645619
-486.137444	11.728051	0.650624
-489.888239	3.217153	0.655629
-493.781446	6.809859	0.660634
-497.352929	15.499866	0.665638
-501.508919	12.393179	0.670643
-505.143188	13.396232	0.675648
-508.486185	5.413161	0.680653
-512.484974	13.892317	0.685658
-516.240816	5.579383	0.690662
-519.780907	4.465372	0.695667
-523.855964	9.943215	0.700672
-527.365697	8.565749	0.705677
-531.287627	10.720213	0.710682
-535.157663	16.669948	0.715686
-538.809119	0.939856	0.720691
-542.919975	13.686780	0.725696
-546.283394	1.288475	0.730701
-549.678033	-0.496841	0.735706
-553.786015	7.184546	0.740710
-557.389590	10.522937	0.745715
-561.442730	11.569328	0.750720
-564.648917	7.117307	0.755725
-568.901805	5.576339	0.760730
-572.731247	6.932364	0.765734
-576.228530	7.088910	0.770739
-580.229235	8.111187	0.775744
-584.150422	4.181833	0.780749
-587.665198	6.766504	0.785754
-591.414864	10.784284	0.790758
-594.972867	5.543273	0.795763
-599.455197	14.508235	0.800768
-602.697670	0.198384	0.805773
-606.297483	8.472026	0.810778
-610.184952	23.346923	0.815782
-613.371716	8.458910	0.820787
-617.840369	8.699735	0.825792
-621.694556	0.656578	0.830797
-625.397549	-0.771866	0.835802
-629.151919	13.244437	0.840806
-632.749920	10.066187	0.845811
-636.964811	10.745893	0.850816
-640.616251	11.591048	0.855821
-644.497796	6.773959	0.860826
-647.963613	3.875808	0.865830
-651.415821	3.799763	0.870835
-655.549671	13.831919	0.875840
-658.986120	6.125774	0.880845
-662.599468	12.736427	0.885850
-666.548048	8.701202	0.890854
-670.106190	4.333948	0.895859
-674.332257	10.293477	0.900864
-678.222150	8.617439	0.905869
-681.935959	14.980826	0.910874
-685.629911	4.906323	0.915878
-688.920563	1.879322	0.920883
-693.005505	10.724183	0.925888
-696.915104	4.199125	0.930893
-700.312623	4.147528	0.935898
-704.140085	3.456597	0.940902
-707.621426	-5.380833	0.945907
-711.775793	9.024347	0.950912
-715.259353	7.537326	0.955917
-719.211363	4.997666	0.960922
-723.357803	9.179975	0.965926
-726.943712	13.700066	0.970931
-731.304375	11.900652	0.975936
-734.689176	1.297445	0.980941
-738.067527	10.472579	0.985946
-741.746493	11.984596	0.990950
-745.380119	8.687638	0.995955
-749.748630	12.367751	1.000960
-753.332876	0.768291	1.005965
-756.802512	9.287845	1.010970
-760.798359	6.468261	1.015974
-764.378047	12.934913	1.020979
-768.374255	20.819567	1.025984
-772.066791	9.888708	1.030989
-775.386042	3.285206	1.035994
-779.567775	4.853981	1.040998
-783.105977	10.509798	1.046003
-787.001944	18.083574	1.051008
-790.708776	12.470845	1.056013
-794.739303	14.780288	1.061018
-798.493071	16.916196	1.066022
-801.939683	13.210973	1.071027
-805.984179	20.067365	1.076032
-809.653855	10.430724	1.081037
-813.322940	23.329822	1.086042
-817.348964	19.885963	1.091046
-820.599944	12.043187	1.096051
-824.582953	13.583431	1.101056
-828.369593	21.522991	1.106061
-832.202455	9.033009	1.111066
-836.276814	16.034569	1.116070
-839.920924	17.955898	1.121075
-843.442761	13.564184	1.126080
-846.882124	14.166025	1.131085
-851.099552	14.546901	1.136090
-855.124631	10.235652	1.141094
-858.317660	6.644517	1.146099
-862.247881	10.781461	1.151104
-865.968210	8.082015	1.156109
-869.629207	9.924088	1.161114
-873.535371	14.864591	1.166118
-877.004733	14.387925	1.171123
-881.028894	17.257881	1.176128
-884.951387	11.960476	1.181133
-888.669815	9.822146	1.186138
-892.706370	13.662333	1.191142
-896.201789	2.036293	1.196147
-899.770152	14.165634	1.201152
-903.354027	12.002662	1.206157
-907.205574	11.628143	1.211162
-911.121888	7.969796	1.216166
-914.853842	6.666286	1.221171
-919.114667	17.428793	1.226176
-922.548031	12.002788	1.231181
-926.281428	15.837139	1.236186
-930.215631	10.793992	1.241190
-933.454994	10.476174	1.246195
-937.587305	11.012327	1.251200
-941.356081	9.151786	1.256205
-944.822689	9.723433	1.261210
-948.921465	21.183889	1.266214
-952.117055	6.649457	1.271219
-956.073530	5.963798	1.276224
-959.859508	10.189798	1.281229
-964.064742	13.613962	1.286234
-968.301937	10.617290	1.291238
-971.510994	3.764652	1.296243
-975.111661	5.611432	1.301248
-978.624843	2.284546	1.306253
-982.366884	13.123468	1.311258
-986.248414	15.284832	1.316262
-989.861217	5.565287	1.321267
-994.164771	7.775227	1.326272
-997.693864	8.554060	1.331277
-1001.521495	8.033950	1.336282
-1005.346428	10.938485	1.341286
-1008.988713	13.684510	1.346291
-1012.737786	16.950657	1.351296
-1016.346701	15.927247	1.356301
-1020.142821	11.311596	1.361306
-1024.391315	17.240627	1.366310
-1027.853674	14.777722	1.371315
-1031.829732	10.621367	1.376320
-1035.450841	12.995047	1.381325
-1038.840322	11.835655	1.386330
-1042.975347	11.848890	1.391334
-1046.534946	13.205097	1.396339
-1050.412895	17.780258	1.401344
-1054.446212	13.417062	1.406349
-1057.920415	6.903416	1.411354
-1061.855489	9.310005	1.416358
-1064.880505	4.675175	1.421363
-1069.039988	11.239735	1.426368
-1073.052684	9.531961	1.431373
-1076.534967	8.694968	1.436378
-1080.646963	11.114118	1.441382
-1084.207611	7.093257	1.446387
-1088.073009	7.828249	1.451392
-1091.795097	15.278500	1.456397
-1095.548807	13.359030	1.461402
-1099.172416	14.922671	1.466406
-1102.798399	6.796531	1.471411
-1106.898004	12.500043	1.476416
-1110.406897	-2.833979	1.481421
-1114.225012	8.119803	1.486426
-1118.327888	14.446741	1.491430
-1121.645007	12.072706	1.496435
-1125.507284	14.686948	1.501440
-1129.085171	4.473204	1.506445
-1133.248450	1.630591	1.511450
-1136.886845	15.004615	1.516454
-1140.676379	15.618750	1.521459
-1144.563902	21.928630	1.526464
-1148.158640	13.625678	1.531469
-1151.753572	9.435369	1.536474
-1155.499079	7.538341	1.541478
-1158.898398	2.908329	1.546483
-1163.454662	10.626179	1.551488
-1167.180043	12.959973	1.556493
-1170.688790	17.031569	1.561498
-1174.907734	11.427291	1.566502
-1177.902794	0.898037	1.571507
-1181.620321	12.737828	1.576512
-1185.607666	10.969425	1.581517
-1189.740352	14.653609	1.586522
-1193.732721	14.776748	1.591526
-1197.103431	6.209383	1.596531
-1200.834459	-3.386813	1.601536
-1204.440304	14.881575	1.606541
-1208.066988	9.925323	1.611546
-1212.293025	5.962246	1.616550
-1215.647249	8.575764	1.621555
-1219.350186	9.748592	1.626560
-1223.312117	0.574146	1.631565
-1227.006813	3.030853	1.636570
-1231.120355	16.378543	1.641574
-1234.602207	9.234052	1.646579
-1238.564147	17.888248	1.651584
-1242.347822	11.779216	1.656589
-1246.001525	0.574881	1.661594
-1249.979028	6.492478	1.666598
-1253.135770	5.589465	1.671603
-1257.291858	18.765816	1.676608
-1260.825589	24.183500	1.681613
-1264.624605	10.591337	1.686618
-1268.539405	21.254915	1.691622
-1272.215619	11.131253	1.696627
-1276.261701	19.682284	1.701632
-1279.472921	15.662576	1.706637
-1283.837450	17.676229	1.711642
-1287.556296	13.023430	1.716646
-1290.729044	9.724541	1.721651
-1294.694609	10.665137	1.726656
-1298.745689	14.453142	1.731661
-1302.247258	5.839077	1.736666
-1306.653328	17.076489	1.741670
-1309.842681	12.819942	1.746675
-1313.832476	22.098447	1.751680
-1317.314296	20.796552	1.756685
-1320.694493	9.633716	1.761690
-1324.613849	16.404705	1.766694
-1328.377508	5.831526	1.771699
-1332.459592	15.534827	1.776704
-1336.316504	7.540651	1.781709
-1340.071883	8.129144	1.786714
-1343.951606	13.092984	1.791718
-1347.444465	9.041188	1.796723
-1351.286542	17.077152	1.801728
-1355.048344	13.435836	1.806733
-1358.888875	12.161462	1.811738
-1362.648093	11.047539	1.816742
-1365.985504	13.737427	1.821747
-1370.180066	12.765741	1.826752
-1373.970311	12.830028	1.831757
-1377.414284	12.797890	1.836762
-1381.540349	15.934161	1.841766
-1385.023217	6.858353	1.846771
-1388.514209	17.555195	1.851776
-1392.579566	19.492773	1.856781
-1396.350919	7.804488	1.861786
-1399.991833	18.124811	1.866790
-1403.622031	13.587321	1.871795
-1407.638556	15.428801	1.876800
-1411.467868	11.777887	1.881805
-1415.174122	5.942180	1.886810
-1419.205419	13.655314	1.891814
-1422.462001	10.737453	1.896819
-1426.294488	13.801569	1.901824
-1430.012638	10.806233	1.906829
-1433.649822	2.321325	1.911834
-1437.808945	8.361349	1.916838
-1441.525463	7.065683	1.921843
-1445.437222	9.235798	1.926848
-1449.148953	9.560443	1.931853
-1452.889772	4.156100	1.936858
-1456.694025	8.500927	1.941862
-1460.165178	9.209683	1.946867
-1464.181398	20.637264	1.951872
-1468.119124	19.348674	1.956877
-1471.656141	10.655403	1.961882
-1475.520167	19.910878	1.966886
-1479.049350	9.413953	1.971891
-1482.697592	22.275979	1.976896
-1486.584368	17.778130	1.981901
-1490.338074	17.751603	1.986906
-1494.449252	17.345520	1.991910
-1497.903943	14.188262	1.996915
-1502.010917	12.083179	2.006912
-1502.774704	13.211297	2.016909
-1500.232193	18.401499	2.026906
-1497.469640	17.207587	2.036902
-1495.307938	15.203586	2.046899
-1493.652140	12.437447	2.056896
-1491.427059	15.761667	2.066893
-1489.509036	8.594114	2.076890
-1487.755562	11.668594	2.086886
-1485.777479	13.625542	2.096883
-1484.070854	12.122312	2.106880
-1482.082120	11.450216	2.116877
-1479.937527	6.490053	2.126874
-1478.185633	10.941621	2.136870
-1476.411462	14.620686	2.146867
-1474.521362	11.063894	2.156864
-1472.514614	7.730002	2.166861
-1470.504383	6.489218	2.176858
-1468.630182	3.973914	2.186854
-1467.086658	2.245762	2.196851
-1465.146887	5.396218	2.206848
-1463.100947	11.240701	2.216845
-1461.091463	12.580018	2.226842
-1459.250484	6.921652	2.236838
-1457.410694	9.207080	2.246835
-1455.919632	12.737281	2.256832
-1453.776688	6.070580	2.266829
-1451.632742	1.601595	2.276826
-1449.640872	-3.043563	2.286822
-1447.967664	5.336373	2.296819
-1446.451595	10.199931	2.306816
-1444.207579	12.952751	2.316813
-1442.207248	7.872035	2.326810
-1440.583725	8.690539	2.336806
-1438.433550	9.770511	2.346803
-1436.877943	4.942580	2.356800
-1435.068103	12.826976	2.366797
-1432.763885	7.667615	2.376794
-1431.141351	10.171004	2.386790
-1429.337778	10.588063	2.396787
-1427.497820	8.400375	2.406784
-1425.278647	12.688755	2.416781
-1423.206019	10.819079	2.426778
-1421.597036	12.069395	2.436774
-1419.963360	16.217836	2.446771
-1417.915875	15.956386	2.456768
-1416.091562	12.092806	2.466765
-1414.082967	7.373945	2.476762
-1412.286698	13.124239	2.486758
-1410.701692	11.852109	2.496755
-1408.322624	12.374418	2.506752
-1406.779652	17.487908	2.516749
-1404.650493	14.661839	2.526746
-1402.807342	16.728882	2.536742
-1401.008309	17.315636	2.546739
-1399.006348	14.467304	2.556736
-1397.396013	21.463158	2.566733
-1395.393402	26.263080	2.576730
-1393.448507	13.561868	2.586726
-1391.623175	11.131815	2.596723
-1389.790875	14.056387	2.606720
-1388.191392	15.696665	2.616717
-1385.833451	13.465562	2.626714
-1383.830438	10.609180	2.636710
-1382.322331	20.163493	2.646707
-1380.603107	13.908888	2.656704
-1378.328451	7.429586	2.666701
-1376.300207	12.926462	2.676698
-1374.762035	11.254489	2.686694
-1372.958133	12.397848	2.696691
-1370.946599	17.700040	2.706688
-1368.978923	22.339788	2.716685
-1367.035679	17.639318	2.726682
-1365.319126	18.188776	2.736678
-1363.660085	17.986396	2.746675
-1361.698037	23.999146	2.756672
-1359.727637	21.065898	2.766669
-1357.698323	16.847444	2.776666
-1355.972644	17.196503	2.786662
-1354.071794	15.968590	2.796659
-1352.056956	14.278752	2.806656
-1350.420492	22.901500	2.816653
-1348.180293	16.936154	2.826650
-1346.418558	19.033644	2.836646
-1344.472354	18.924259	2.846643
-1343.088699	17.450721	2.856640
-1340.972670	17.827310	2.866637
-1339.244355	13.306527	2.876634
-1337.038900	12.647235	2.886630
-1335.124044	8.952380	2.896627
-1333.618737	15.085627	2.906624
-1331.387984	15.331757	2.916621
-1329.464074	12.707553	2.926618
-1327.878645	12.370140	2.936614
-1326.153222	12.504527	2.946611
-1323.801235	19.830149	2.956608
-1321.984103	17.913035	2.966605
-1320.238186	15.213117	2.976602
-1318.292682	20.442244	2.986598
-1316.685663	21.811370	2.996595
-1314.828184	21.223583	3.006592
-1313.021879	10.251441	3.016589
-1310.732107	10.811826	3.026586
-1309.003634	11.566259	3.036582
-1307.049464	17.365582	3.046579
-1305.091748	20.281206	3.056576
-1303.437537	15.156523	3.066573
-1301.464143	10.287072	3.076570
-1299.514640	13.559274	3.086566
-1297.806086	15.401631	3.096563
-1295.924534	14.194222	3.106560
-1293.925137	15.311093	3.116557
-1292.122516	17.703660	3.126554
-1290.168819	19.727841	3.136550
-1288.116199	18.546744	3.146547
-1286.549493	22.925478	3.156544
-1284.608310	19.602234	3.166541
-1282.784212	17.759824	3.176538
-1280.960727	15.664884	3.186534
-1278.937758	21.753222	3.196531
-1277.179273	14.353991	3.206528
-1275.117369	20.199260	3.216525
-1273.238659	12.809213	3.226522
-1271.310846	11.720735	3.236518
-1269.654824	11.853640	3.246515
-1267.846209	13.021591	3.256512
-1266.108112	17.191332	3.266509
-1264.125800	16.799923	3.276506
-1261.839194	14.943514	3.286502
-1259.913947	21.672766	3.296499
-1258.261740	20.478404	3.306496
-1256.532832	15.548639	3.316493
-1254.609538	10.693558	3.326490
-1252.510602	17.211864	3.336486
-1250.799197	10.808600	3.346483
-1249.014754	9.894661	3.356480
-1247.137203	13.401053	3.366477
-1245.037587	15.411396	3.376474
-1243.156354	15.874594	3.386470
-1241.530544	14.668679	3.396467
-1239.698246	16.011283	3.406464
-1237.511995	17.740930	3.416461
-1235.825718	14.264307	3.426458
-1233.990157	9.565386	3.436454
-1232.037145	11.543937	3.446451
-1230.074620	17.490413	3.456448
-1228.139803	12.897191	3.466445
-1226.516825	13.829618	3.476442
-1224.410681	18.690495	3.486438
-1222.854254	14.167298	3.496435
-1220.794006	20.196041	3.506432
-1218.689934	14.893642	3.516429
-1217.096099	23.485424	3.526426
-1215.113117	19.572920	3.536422
-1213.389770	12.956192	3.546419
-1211.479152	19.736775	3.556416
-1209.475597	16.575716	3.566413
-1207.674491	16.972817	3.576410
-1205.700569	23.342228	3.586406
-1203.945092	22.036644	3.596403
-1202.019203	16.900136	3.606400
-1200.189671	13.517457	3.616397
-1198.006865	16.607158	3.626394
-1196.297369	10.538970	3.636390
-1194.706221	23.631169	3.646387
-1192.640086	14.096995	3.656384
-1190.817166	13.598519	3.666381
-1188.860622	16.124434	3.676378
-1187.035218	14.390836	3.686374
-1184.940039	8.733051	3.696371
-1183.321296	14.472469	3.706368
-1181.472373	10.243550	3.716365
-1179.442530	13.218795	3.726362
-1177.520852	17.471340	3.736358
-1175.777854	12.425693	3.746355
-1173.843305	13.159889	3.756352
-1171.941136	14.077687	3.766349
-1170.000705	15.774097	3.776346
-1168.095492	15.835627	3.786342
-1166.315197	8.290880	3.796339
-1164.889764	13.737557	3.806336
-1162.668778	18.610120	3.816333
-1160.791608	9.955674	3.826330
-1158.681356	13.917540	3.836326
-1157.074516	18.627838	3.846323
-1154.850389	17.725732	3.856320
-1153.161355	10.511381	3.866317
-1151.272934	11.931918	3.876314
-1149.562711	6.935745	3.886310
-1147.595641	18.941530	3.896307
-1145.624253	13.440948	3.906304
-1143.807996	9.379914	3.916301
-1141.953022	17.648924	3.926298
-1140.165336	16.586128	3.936294
-1138.232963	12.875993	3.946291
-1136.396241	14.667970	3.956288
-1134.561926	5.466193	3.966285
-1132.467119	11.467383	3.976282
-1130.582240	8.934845	3.986278
-1128.789661	10.487574	3.996275
-1127.071979	15.445423	4.006272
-1125.056852	10.223649	4.016269
-1123.019886	11.112029	4.026266
-1121.229298	10.948778	4.036262
-1119.529416	12.443712	4.046259
-1117.771623	13.100442	4.056256
-1115.647388	10.417522	4.066253
-1113.905174	15.183563	4.076250
-1112.010448	16.500494	4.086246
-1110.078052	17.070879	4.096243
-1108.156222	12.893509	4.106240
-1106.258592	17.282594	4.116237
-1104.349951	12.373131	4.126234
-1102.604450	17.287076	4.136230
-1100.585770	19.504710	4.146227
-1098.923115	16.633535	4.156224
-1096.971620	15.490885	4.166221
-1094.756116	10.886027	4.176218
-1093.268225	12.253838	4.186214
-1091.278689	1.333065	4.196211
-1089.459958	8.156871	4.206208
-1087.636053	5.957802	4.216205
-1085.676225	4.689093	4.226202
-1083.719365	-0.603850	4.236198
-1081.776953	2.576517	4.246195
-1079.920852	3.167024	4.256192
-1078.274251	7.891544	4.266189
-1076.635159	5.666782	4.276186
-1074.255653	12.593537	4.286182
-1072.230004	12.275885	4.296179
-1070.509149	9.911734	4.306176
-1068.886368	9.293787	4.316173
-1066.961800	6.803898	4.326170
-1065.265655	7.712105	4.336166
-1063.365402	7.869250	4.346163
-1061.247355	17.158881	4.356160
-1059.383831	11.850881	4.366157
-1057.419877	7.436290	4.376154
-1055.785709	4.508123	4.386150
-1053.962920	3.504515	4.396147
-1051.776077	9.176853	4.406144
-1049.699596	5.835318	4.416141
-1048.318632	10.858134	4.426138
-1046.638273	15.247283	4.436134
-1044.115973	7.449735	4.446131
-1042.524761	15.994701	4.456128
-1040.513815	14.231540	4.466125
-1038.758406	9.131899	4.476122
-1037.253092	16.921664	4.486118
-1035.306537	16.120906	4.496115
-1032.916163	21.219141	4.506112
-1031.061969	8.633743	4.516109
-1029.262414	11.532270	4.526106
-1027.422543	18.278543	4.536102
-1025.498259	14.715052	4.546099
-1023.788614	13.145354	4.556096
-1021.947599	14.605159	4.566093
-1020.043092	16.640598	4.576090
-1017.935861	12.795225	4.586086
-1016.326718	14.260538	4.596083
-1014.227122	14.728474	4.606080
-1012.690640	10.022282	4.616077
-1010.771964	14.065452	4.626074
-1008.696849	10.127330	4.636070
-1006.636829	13.189483	4.646067
-1005.277164	21.799932	4.656064
-1002.970745	15.339570	4.666061
-1001.245983	12.141163	4.676058
-999.144658	10.363584	4.686054
-997.516630	12.967463	4.696051
-995.760034	13.084479	4.706048
-993.899274	9.734856	4.716045
-991.708069	14.031302	4.726042
-989.988669	3.264325	4.736038
-988.164148	12.079915	4.746035
-986.203914	13.730682	4.756032
-984.420216	13.440744	4.766029
-982.647432	8.900466	4.776026
-980.352065	10.005018	4.786022
-978.626691	7.564421	4.796019
-976.693846	10.512728	4.806016
-974.725487	11.143789	4.816013
-973.141544	13.641052	4.826010
-971.323538	10.642491	4.836006
-969.240485	12.793106	4.846003
-967.609425	12.603376	4.856000
-965.623929	8.305412	4.865997
-963.720156	7.824184	4.875994
-961.712748	14.520038	4.885990
-960.012460	11.265574	4.895987
-958.183338	13.758379	4.905984
-956.537386	13.269435	4.915981
-954.110556	13.141946	4.925978
-952.494666	15.402011	4.935974
-950.693335	17.283480	4.945971
-948.581704	12.172731	4.955968
-946.903630	15.884956	4.965965
-944.847801	13.326807	4.975962
-943.013117	10.170865	4.985958
-941.029491	11.732668	4.995955
-939.242048	14.072680	5.005952
-937.403745	23.932956	5.015949
-935.489382	15.391139	5.025946
-933.953842	15.990387	5.035942
-931.908466	21.006524	5.045939
-930.038624	22.452321	5.055936
-928.314192	18.788228	5.065933
-925.852579	18.235208	5.075930
-924.245915	20.307296	5.085926
-922.110494	15.345922	5.095923
-920.644852	11.802160	5.105920
-918.725529	14.504785	5.115917
-916.622116	9.161696	5.125914
-914.756074	13.025470	5.135910
-912.997596	21.813796	5.145907
-911.213136	20.683793	5.155904
-909.458655	23.346468	5.165901
-907.284129	22.012000	5.175898
-905.702972	21.413451	5.185894
-903.880327	17.735253	5.195891
-901.559819	19.650598	5.205888
-899.823956	21.305734	5.215885
-898.181442	19.805278	5.225882
-896.264510	20.510944	5.235878
-894.347657	20.153996	5.245875
-892.019700	17.171861	5.255872
-890.546275	15.838969	5.265869
-888.560313	13.863614	5.275866
-886.863832	10.488230	5.285862
-885.097682	14.360104	5.295859
-882.794154	19.226069	5.305856
-881.360034	18.766305	5.315853
-879.295664	14.661062	5.325850
-877.367182	22.811190	5.335846
-875.678017	11.128587	5.345843
-873.654580	14.016711	5.355840
-871.617858	12.759569	5.365837
-869.932875	8.754459	5.375834
-868.062078	11.346463	5.385830
-865.703729	18.204201	5.395827
-864.312129	16.252828	5.405824
-862.270378	12.504898	5.415821
-860.207199	11.894061	5.425818
-858.865347	14.297473	5.435814
-856.948988	13.080111	5.445811
-854.969304	20.175235	5.455808
-852.969133	12.216603	5.465805
-850.961059	16.851935	5.475802
-849.352608	12.729598	5.485798
-847.620153	5.903239	5.495795
-845.419916	18.694674	5.505792
-843.332098	17.945703	5.515789
-841.815833	16.309151	5.525786
-839.661763	10.912238	5.535782
-838.003858	11.779357	5.545779
-836.267861	16.983981	5.555776
-834.517380	17.444727	5.565773
-832.320845	14.112605	5.575770
-830.150487	12.482033	5.585766
-828.600874	13.285942	5.595763
-827.057427	14.873993	5.605760
-824.912723	17.910146	5.615757
-822.684773	13.829329	5.625754
-821.113826	13.102995	5.635750
-819.308262	15.040733	5.645747
-817.542315	20.625848	5.655744
-815.539147	16.361493	5.665741
-813.281204	19.820082	5.675738
-811.547062	13.621894	5.685734
-810.196891	9.094024	5.695731
-807.957894	24.228776	5.705728
-805.817321	24.192983	5.715725
-804.180907	21.484095	5.725722
-802.627163	17.727371	5.735718
-800.707861	16.995898	5.745715
-798.595346	13.042500	5.755712
-796.696063	16.975272	5.765709
-794.857125	19.155589	5.775706
-792.823141	22.706837	5.785702
-790.951351	20.582442	5.795699
-789.219988	19.048913	5.805696
-787.487011	23.690378	5.815693
-785.403577	17.510589	5.825690
-783.233391	14.882194	5.835686
-781.794813	16.704932	5.845683
-779.864647	14.703847	5.855680
-778.123730	16.093003	5.865677
-776.062549	14.413613	5.875674
-773.982279	18.213269	5.885670
-772.430309	16.465265	5.895667
-770.489106	16.357157	5.905664
-768.625516	16.105139	5.915661
-766.765586	17.757914	5.925658
-764.618747	12.943272	5.935654
-762.858917	11.754159	5.945651
-761.186587	18.025332	5.955648
-759.245086	15.266138	5.965645
-757.214202	15.775286	5.975642
-755.233440	17.424549	5.985638
-753.650295	19.093149	5.995635
-751.542541	17.381073	6.005632
-749.979871	15.781374	6.015629
-748.194080	17.280223	6.025626
-745.915926	17.669338	6.035622
-744.119339	15.166999	6.045619
-742.519833	16.795096	6.055616
-740.423714	18.260148	6.065613
-738.475059	18.632454	6.075610
-736.588687	23.832076	6.085606
-734.706838	17.517175	6.095603
-732.903210	21.762130	6.105600
-731.014763	19.031962	6.115597
-729.272897	19.980478	6.125594
-727.142231	13.610033	6.135590
-725.146379	21.321639	6.145587
-723.546976	12.413465	6.155584
-721.872201	8.387979	6.165581
-719.888036	11.839883	6.175578
-718.050481	14.088377	6.185574
-716.097386	11.925785	6.195571
-713.893165	12.268325	6.205568
-712.096261	14.867529	6.215565
-710.340533	14.836477	6.225562
-708.445065	17.922040	6.235558
-706.721390	16.205061	6.245555
-704.733591	15.729562	6.255552
-702.787922	17.757109	6.265549
-700.982614	7.856050	6.275546
-699.138562	0.667749	6.285542
-697.322609	5.403389	6.295539
-695.587114	13.008199	6.305536
-693.502054	17.648741	6.315533
-691.649059	13.031113	6.325530
-689.503785	11.242045	6.335526
-687.804471	16.125807	6.345523
-686.270680	11.565503	6.355520
-684.090101	11.667112	6.365517
-682.224681	14.208024	6.375514
-680.661972	16.269938	6.385510
-678.331092	9.780702	6.395507
-676.466811	10.490223	6.405504
-674.607779	9.370588	6.415501
-673.062498	15.876865	6.425498
-670.949080	11.250800	6.435494
-668.974065	10.101585	6.445491
-667.361065	16.017573	6.455488
-665.717387	13.547617	6.465485
-663.488918	14.055277	6.475482
-661.291369	14.809458	6.485478
-659.700849	16.865364	6.495475
-657.894355	15.896240	6.505472
-656.193207	12.487109	6.515469
-654.039444	14.688291	6.525466
-651.950278	12.892431	6.535462
-650.214762	12.790442	6.545459
-648.546117	14.571768	6.555456
-646.626845	11.205163	6.565453
-644.853883	13.421403	6.575450
-643.170646	3.023573	6.585446
-641.189766	12.048168	6.595443
-638.978430	17.045954	6.605440
-637.072058	12.560365	6.615437
-635.263454	8.868818	6.625434
-633.516634	11.627665	6.635430
-631.459312	16.820590	6.645427
-629.697673	16.856547	6.655424
-628.141218	21.982654	6.665421
-625.866571	11.228239	6.675418
-623.899733	12.450366	6.685414
-622.028231	15.685092	6.695411
-620.153355	10.164022	6.705408
-618.433679	11.365638	6.715405
-617.214423	11.704570	6.725402
-614.910204	15.392804	6.735398
-612.662536	18.840602	6.745395
-610.646729	16.188076	6.755392
-609.174119	16.030222	6.765389
-607.231189	14.549867	6.775386
-605.154078	17.415445	6.785382
-603.543140	22.744445	6.795379
-601.579508	19.508155	6.805376
-599.686955	19.589537	6.815373
-597.696025	19.306258	6.825370
-596.032870	19.370605	6.835366
-594.150741	14.483131	6.845363
-592.307778	18.606652	6.855360
-590.293936	20.637614	6.865357
-588.422269	14.526552	6.875354
-586.387606	14.586823	6.885350
-584.607768	16.230433	6.895347
-582.853502	12.424446	6.905344
-581.033138	16.628954	6.915341
-579.033044	17.637385	6.925338
-577.308632	14.944591	6.935334
-575.059138	16.609502	6.945331
-573.638147	20.317285	6.955328
-571.787249	19.003238	6.965325
-569.477587	16.892753	6.975322
-567.523430	12.813268	6.985318
-565.741622	18.006052	6.995315
-564.327683	14.121808	7.005312
-562.436759	16.260849	7.015309
-560.213868	19.298972	7.025306
-558.161710	24.241740	7.035302
-556.557060	19.087561	7.045299
-554.661324	14.107942	7.055296
-552.585583	24.006424	7.065293
-550.941841	21.174953	7.075290
-549.128047	20.032639	7.085286
-547.384853	16.517391	7.095283
-545.059610	19.720760	7.105280
-543.412480	16.814544	7.115277
-541.565941	16.608059	7.125274
-539.589486	19.936617	7.135270
-537.585854	14.088724	7.145267
-535.916354	17.992102	7.155264
-534.413979	21.949017	7.165261
-532.212428	18.711097	7.175258
-530.237600	12.427285	7.185254
-528.391007	22.255020	7.195251
-526.605884	15.859402	7.205248
-524.609626	16.570071	7.215245
-522.748048	14.875408	7.225242
-520.879012	15.443767	7.235238
-518.869468	19.512322	7.245235
-516.958905	18.708262	7.255232
-515.227802	15.723915	7.265229
-513.388852	11.637609	7.275226
-511.327178	15.573106	7.285222
-509.907566	15.046409	7.295219
-507.757146	12.454574	7.305216
-505.999801	12.922362	7.315213
-503.960823	15.768858	7.325210
-502.030618	18.729045	7.335206
-500.348070	10.927197	7.345203
-498.441443	16.496417	7.355200
-496.496434	24.198988	7.365197
-494.489066	14.919474	7.375194
-492.684968	12.441381	7.385190
-490.955364	14.672560	7.395187
-489.208536	16.662568	7.405184
-486.944506	15.816293	7.415181
-485.087776	12.444010	7.425178
-483.272418	6.626229	7.435174
-481.662595	9.781281	7.445171
-479.658759	11.114461	7.455168
-477.741113	20.120892	7.465165
-475.835617	15.607142	7.475162
-474.045740	19.079236	7.485158
-472.033138	17.145757	7.495155
-469.994332	23.514950	7.505152
-468.392870	22.368710	7.515149
-466.459655	22.792653	7.525146
-464.429361	12.675815	7.535142
-462.720172	14.430274	7.545139
-460.997242	11.387271	7.555136
-458.918478	18.964304	7.565133
-456.938146	17.083358	7.575130
-455.296685	10.917575	7.585126
-453.553514	17.938727	7.595123
-451.497147	14.125641	7.605120
-449.307129	13.253325	7.615117
-447.630261	13.852429	7.625114
-445.920016	19.258844	7.635110
-444.018801	18.241596	7.645107
-442.217141	14.360243	7.655104
-440.379075	15.625191	7.665101
-438.280883	17.633342	7.675098
-436.300934	10.654046	7.685094
-434.837845	18.057832	7.695091
-432.625548	20.755139	7.705088
-430.641459	11.321496	7.715085
-429.083492	10.378017	7.725082
-427.155622	14.859167	7.735078
-425.209895	13.239563	7.745075
-423.423095	10.120072	7.755072
-421.182869	10.157134	7.765069
-419.604236	12.518262	7.775066
-417.494325	13.266136	7.785062
-415.910569	7.932225	7.795059
-414.149222	10.354182	7.805056
-411.696091	14.066213	7.815053
-410.228474	16.258757	7.825050
-408.412204	15.547207	7.835046
-406.342823	18.922621	7.845043
-404.389934	17.991892	7.855040
-402.669313	22.065629	7.865037
-400.936817	21.716408	7.875034
-398.978709	10.539038	7.885030
-396.863265	12.018680	7.895027
-395.472861	15.791460	7.905024
-393.182211	11.516278	7.915021
-391.535529	10.948660	7.925018
-389.421190	1.980573	7.935014
-387.768806	6.381002	7.945011
-385.553067	13.677284	7.955008
-383.964194	17.168910	7.965005
-381.960202	16.836356	7.975002
-380.193343	15.287977	7.984998
-378.227592	17.607854	7.994995
-376.494755	17.228596	8.004992
-374.751359	16.885549	8.014989
-372.993760	9.823378	8.024986
-370.459067	14.188748	8.034982
-368.642714	15.414587	8.044979
-367.173693	11.284814	8.054976
-365.181254	15.307287	8.064973
-363.286626	12.502203	8.074970
-361.282272	18.253309	8.084966
-359.585605	18.861946	8.094963
-357.637208	17.174074	8.104960
-355.781344	15.418871	8.114957
-353.869357	11.134703	8.124954
-351.787710	16.919267	8.134950
-350.098142	12.470083	8.144947
-348.080787	19.750709	8.154944
-346.681115	15.186753	8.164941
-344.959463	17.615101	8.174938
-342.639160	14.053654	8.184934
-340.579937	20.849180	8.194931
-338.623020	16.524692	8.204928
-337.123192	14.231076	8.214925
-335.146311	14.202890	8.224922
-333.386682	17.174659	8.234918
-331.361726	17.020380	8.244915
-329.476161	23.759957	8.254912
-327.816042	17.583376	8.264909
-325.695710	17.085455	8.274906
-323.866165	10.340252	8.284902
-321.940076	13.703879	8.294899
-320.102032	17.552091	8.304896
-318.375863	22.278693	8.314893
-316.427688	13.231392	8.324890
-314.355047	12.630567	8.334886
-312.461302	15.963049	8.344883
-310.759470	24.475135	8.354880
-308.683321	15.000040	8.364877
-307.090731	16.729015	8.374874
-305.339657	22.149549	8.384870
-302.952246	15.236362	8.394867
-301.353103	24.380638	8.404864
-299.456813	20.446383	8.414861
-297.482327	11.358581	8.424858
-295.683943	17.939994	8.434854
-293.976590	14.721169	8.444851
-292.168873	19.548459	8.454848
-290.213081	20.477364	8.464845
-288.296937	23.646819	8.474842
-286.131392	17.178009	8.484838
-284.430095	17.165432	8.494835
-282.515003	17.129783	8.504832
-280.708514	21.592541	8.514829
-278.739841	15.578321	8.524826
-277.111372	15.217372	8.534822
-275.278424	17.880640	8.544819
-272.945029	16.044542	8.554816
-271.401317	17.358184	8.564813
-269.520712	16.903312	8.574810
-267.469985	14.903915	8.584807
-265.620877	15.455129	8.594803
-264.063774	16.316637	8.604800
-262.084073	16.136482	8.614797
-259.810185	16.133585	8.624794
-258.204597	10.148913	8.634791
-256.366044	13.338670	8.644787
-254.443729	12.829784	8.654784
-252.686791	17.815210	8.664781
-250.829234	14.499809	8.674778
-248.595539	11.635959	8.684775
-246.638653	15.580526	8.694771
-245.252815	17.590437	8.704768
-243.150495	18.060204	8.714765
-241.292049	16.064674	8.724762
-239.303937	14.744769	8.734759
-237.258905	9.763663	8.744755
-235.897794	12.431212	8.754752
-233.596030	12.758630	8.764749
-231.915394	9.348322	8.774746
-230.072898	8.350087	8.784743
-228.201566	19.140455	8.794739
-226.252040	17.446191	8.804736
-224.353746	9.643239	8.814733
-222.863326	16.175964	8.824730
-220.531368	9.293810	8.834727
-218.658729	14.611324	8.844723
-216.922686	11.318500	8.854720
-215.118577	14.586419	8.864717
-213.115072	5.325102	8.874714
-211.324670	2.333083	8.884711
-209.798175	4.948989	8.894707
-207.494261	3.938715	8.904704
-205.934919	2.444105	8.914701
-203.848439	5.679601	8.924698
-201.560886	2.505620	8.934695
-199.858484	3.697667	8.944691
-198.211642	9.008597	8.954688
-196.653568	9.599992	8.964685
-194.438697	10.762370	8.974682
-192.289391	9.040989	8.984679
-190.699755	6.279970	8.994675
-188.627704	3.396180	9.004672
-186.671439	12.091967	9.014669
-185.286612	14.119444	9.024666
-183.437753	5.695987	9.034663
-181.229958	19.146928	9.044659
-179.169817	12.349237	9.054656
-177.540376	16.068218	9.064653
-175.824184	12.855958	9.074650
-173.783248	8.169242	9.084647
-171.681110	11.864903	9.094643
-169.826622	7.525312	9.104640
-168.259247	11.784731	9.114637
-166.492011	9.064861	9.124634
-164.249517	11.045494	9.134631
-162.481725	12.495557	9.144627
-160.792182	10.511250	9.154624
-158.731492	14.455117	9.164621
-156.919522	8.246521	9.174618
-155.233077	12.297476	9.184615
-153.349774	7.787508	9.194611
-151.154202	13.400920	9.204608
-149.341977	11.892837	9.214605
-147.516003	11.779936	9.224602
-145.606379	13.167907	9.234599
-143.491993	6.378959	9.244595
-142.020096	12.771009	9.254592
-139.971147	13.989912	9.264589
-138.138908	11.974956	9.274586
-136.257007	8.725231	9.284583
-134.407062	7.083245	9.294579
-132.535686	12.462611	9.304576
-130.524753	13.556534	9.314573
-128.852559	16.281882	9.324570
-126.946079	14.209299	9.334567
-124.816092	15.055283	9.344563
-123.144406	13.727537	9.354560
-121.232253	13.048272	9.364557
-119.526069	10.071332	9.374554
-117.573140	10.571359	9.384551
-115.435001	15.322387	9.394547
-114.048427	17.063836	9.404544
-111.997418	21.978771	9.414541
-109.728685	17.656814	9.424538
-108.059141	17.396794	9.434535
-106.235317	18.934277	9.444531
-104.400158	19.364683	9.454528
-102.515450	12.583988	9.464525
-100.727778	13.519344	9.474522
-98.843510	18.582471	9.484519
-96.758762	14.662513	9.494515
-94.805363	16.188805	9.504512
-93.090592	19.213705	9.514509
-91.332980	16.557001	9.524506
-89.394999	14.433632	9.534503
-87.528751	14.977512	9.544499
-85.522978	16.287035	9.554496
-83.702170	15.461318	9.564493
-81.677148	9.892997	9.574490
-80.166119	17.235696	9.584487
-78.038587	16.770000	9.594483
-76.164717	17.105831	9.604480
-74.552657	17.008163	9.614477
-72.563083	18.489229	9.624474
-70.706955	16.221037	9.634471
-68.424532	18.124338	9.644467
-66.526724	9.533674	9.654464
-65.099795	8.876596	9.664461
-63.286692	11.513195	9.674458
-61.092505	10.378457	9.684455
-59.268707	14.162834	9.694451
-57.224930	15.280000	9.704448
-55.927886	14.196802	9.714445
-53.682222	16.668090	9.724442
-51.746385	12.452974	9.734439
-49.937295	17.746031	9.744435
-47.856130	16.711439	9.754432
-46.520222	19.798387	9.764429
-44.529607	20.336674	9.774426
-42.362430	8.777249	9.784423
-40.533916	14.441426	9.794419
-38.762014	15.856189	9.804416
-36.551313	19.921502	9.814413
-35.038066	17.276975	9.824410
-32.864621	13.726608	9.834407
-31.173382	16.600568	9.844403
-29.442761	16.592966	9.854400
-27.447170	16.145203	9.864397
-25.553359	18.192640	9.874394
-23.707085	14.571308	9.884391
-21.702305	11.436278	9.894387
-19.884303	17.416362	9.904384
-18.102193	6.248382	9.914381
-16.185832	11.347509	9.924378
-14.472915	5.140600	9.934375
-12.332672	7.979269	9.944371
-10.446789	10.023245	9.954368
-8.672703	11.202417	9.964365
-6.763207	10.866298	9.974362
-5.230999	19.492523	9.984359
-3.877933	49.060656	9.994355
-2.594342	91.360077	10.004352
-1.388108	149.692206	10.014349
0.000000	196.244853	10.019354
0.269390	230.697904	10.024359
1.068150	264.216619	10.029363
1.395347	304.758754	10.034368
1.831209	324.865019	10.039373
2.251589	345.013206	10.044378
2.408800	371.956011	10.049383
3.130795	377.598415	10.054387
2.948891	390.825179	10.059392
2.898176	398.789147	10.064397
3.015468	403.635439	10.069402
3.436526	419.065295	10.074407
3.624324	421.853425	10.079411
3.763249	435.830165	10.084416
3.708655	438.578110	10.089421
3.894690	439.108283	10.094426
3.410276	450.938833	10.099431
3.661681	439.932393	10.104435
3.446479	444.446947	10.109440
3.553473	443.944186	10.114445
3.953122	451.139323	10.119450
3.962305	458.325777	10.124455
4.341344	452.378446	10.129459
3.984172	464.926742	10.134464
4.123335	458.823699	10.139469
4.316230	451.425267	10.144474
4.027033	469.445907	10.149479
4.170751	452.743207	10.154483
4.020127	465.409950	10.159488
4.398760	468.706981	10.164493
4.634891	485.776509	10.169498
4.299890	477.057165	10.174503
4.452609	475.066317	10.179507
4.794471	493.402659	10.184512
4.639645	486.551691	10.189517
4.642088	473.134293	10.194522
4.657785	482.776669	10.199527
4.805799	471.892355	10.204531
4.530749	473.407570	10.209536
4.675319	492.391980	10.214541
5.221960	503.668605	10.219546
4.995843	500.064989	10.224551
5.296335	483.714150	10.229555
4.906222	483.308022	10.234560
4.702979	486.954914	10.239565
4.932687	482.942701	10.244570
4.816358	501.577642	10.249575
5.020901	503.647163	10.254579
5.388469	515.084826	10.259584
5.219039	516.802402	10.264589
5.467846	519.598167	10.269594
5.533997	523.050710	10.274599
5.398327	515.523297	10.279603
5.366701	525.376681	10.284608
5.540459	527.255568	10.289613
5.898266	518.972914	10.294618
5.558157	524.150829	10.299623
5.561048	507.590379	10.304627
5.277734	503.134847	10.309632
5.521271	516.382180	10.314637
5.572864	534.496782	10.319642
5.652423	537.355816	10.324647
5.940790	527.051487	10.329651
5.768315	538.310368	10.334656
5.641067	538.975671	10.339661
5.884950	531.977508	10.344666
5.761698	542.610360	10.349671
5.786286	542.478717	10.354675
5.834574	545.880496	10.359680
5.793539	550.269530	10.364685
5.814631	546.806250	10.369690
5.914592	558.196741	10.374695
6.092674	559.687002	10.379699
6.105109	576.737121	10.384704
5.971752	575.563040	10.389709
6.115089	576.697712	10.394714
6.004459	584.230566	10.399719
6.044721	582.536769	10.404723
6.183192	586.113414	10.409728
6.423521	596.827092	10.414733
6.520808	608.571297	10.419738
6.405430	624.528493	10.424743
6.726294	619.222753	10.429747
7.051073	621.544359	10.434752
6.496176	629.218272	10.439757
6.845114	618.353842	10.444762
6.805925	628.574367	10.449767
6.878774	630.507211	10.454771
6.921065	633.135658	10.459776
6.911904	628.672632	10.464781
6.879894	632.945129	10.469786
6.729556	640.243852	10.474791
7.066480	629.094316	10.479795
6.992847	632.338937	10.484800
6.823870	640.760307	10.489805
7.213787	630.669950	10.494810
6.783159	634.942946	10.499815
7.035147	646.482730	10.504819
7.201153	655.180274	10.509824
7.366742	665.741915	10.514829
7.451967	668.645804	10.519834
7.157501	674.918821	10.524839
7.679132	666.174700	10.529843
7.633235	666.836495	10.534848
7.464279	673.993119	10.539853
7.462938	670.006667	10.544858
7.422946	666.652454	10.549863
7.731522	670.107368	10.554867
7.592445	677.598286	10.559872
7.564625	671.824573	10.564877
7.928142	686.946914	10.569882
7.925263	697.617452	10.574887
8.208225	694.277957	10.579891
7.996022	696.700992	10.584896
8.049542	698.340449	10.589901
8.226748	709.791282	10.594906
7.948181	699.367512	10.599911
8.184788	703.400060	10.604915
8.332388	710.405284	10.609920
8.415387	706.821702	10.614925
8.445180	707.432001	10.619930
8.081518	707.611449	10.624935
8.060250	706.700188	10.629939
8.042370	708.052979	10.634944
7.864513	706.509080	10.639949
8.593420	704.189749	10.644954
8.542288	714.014832	10.649959
8.464894	709.397077	10.654963
8.690737	718.648110	10.659968
8.744027	724.332651	10.664973
8.748740	718.569501	10.669978
8.702226	718.933340	10.674983
9.076960	728.157478	10.679987
9.000455	735.750413	10.684992
8.948960	735.033214	10.689997
8.810733	737.535924	10.695002
8.791067	746.524922	10.700007
9.144504	742.412476	10.705011
9.218232	745.480647	10.710016
9.469461	748.317074	10.715021
9.465900	741.531749	10.720026
9.100532	747.988000	10.725031
9.532459	739.584586	10.730035
9.439728	747.110727	10.735040
9.280884	747.571335	10.740045
9.664971	742.626065	10.745050
9.346179	753.701861	10.750055
9.473064	748.953737	10.755059
9.968888	748.510379	10.760064
9.681922	743.410355	10.765069
9.673814	732.421431	10.770074
9.304260	735.360021	10.775079
9.603714	740.316150	10.780083
9.454791	755.327899	10.785088
9.344316	749.062692	10.790093
9.780328	752.959367	10.795098
9.801968	759.760768	10.800103
9.765486	757.249680	10.805107
9.851174	760.686546	10.810112
10.020521	769.257465	10.815117
9.932285	762.577103	10.820122
9.914225	769.130940	10.825127
9.929584	771.891446	10.830131
10.290126	790.297728	10.835136
10.194843	793.060114	10.840141
10.598981	779.926887	10.845146
10.347010	789.597965	10.850151
10.365157	794.296192	10.855155
10.215057	796.297735	10.860160
10.344230	795.479174	10.865165
10.519021	789.639981	10.870170
10.902580	803.989661	10.875175
10.801057	787.857149	10.880179
10.936529	786.124488	10.885184
10.639524	790.068697	10.890189
10.923063	790.794653	10.895194
10.674793	794.855675	10.900199
10.742944	802.677898	10.905203
11.068669	794.953741	10.910208
11.086932	806.871568	10.915213
11.183893	803.091761	10.920218
11.308729	806.380463	10.925223
11.076567	787.267710	10.930227
11.289578	775.290965	10.935232
10.933679	784.649018	10.940237
10.800442	780.822351	10.945242
11.009251	802.328041	10.950247
11.368686	796.531939	10.955251
11.246695	811.410134	10.960256
11.401786	803.372551	10.965261
11.293357	806.331011	10.970266
11.123067	805.640640	10.975271
11.078720	803.952428	10.980275
11.150804	805.816028	10.985280
10.909860	813.567701	10.990285
11.286984	821.646597	10.995290
11.166578	834.122752	11.000295
11.662847	829.317264	11.005299
11.562766	831.952684	11.010304
11.728077	842.945027	11.015309
11.859043	843.110243	11.020314
11.592195	835.873258	11.025319
11.597189	846.941638	11.030323
11.983906	831.858781	11.035328
11.646928	832.268951	11.040333
12.346365	845.051191	11.045338
12.380559	863.648396	11.050343
12.401496	844.397424	11.055347
12.282432	838.814825	11.060352
12.127205	842.417875	11.065357
12.592474	827.885493	11.070362
12.192204	837.906700	11.075367
12.186543	834.302533	11.080371
12.209506	840.332595	11.085376
12.332661	858.497691	11.090381
12.675697	861.529243	11.095386
12.473577	868.386885	11.100391
12.913410	855.416639	11.105395
12.864368	860.839998	11.110400
12.402538	863.056857	11.115405
12.838936	861.454396	11.120410
12.528687	873.132922	11.125415
12.887521	875.649421	11.130419
13.117147	870.550541	11.135424
13.084352	872.312600	11.140429
13.176001	856.860443	11.145434
12.807985	853.754055	11.150439
12.711936	856.444033	11.155443
13.480255	868.409445	11.160448
12.776870	870.519745	11.165453
13.380749	867.851307	11.170458
13.105943	868.969111	11.175463
13.260715	871.280025	11.180467
13.370231	869.433216	11.185472
13.256060	860.134343	11.190477
13.392003	870.018007	11.195482
13.321829	876.644863	11.200487
13.427470	864.645744	11.205491
13.543510	861.542580	11.210496
13.261057	870.548335	11.215501
13.382181	874.534692	11.220506
13.202878	883.798407	11.225511
13.645464	872.824231	11.230515
13.343480	873.209896	11.235520
13.401303	873.263770	11.240525
13.480104	882.208760	11.245530
13.496326	889.824836	11.250535
13.948272	899.183433	11.255539
14.113412	903.042923	11.260544
13.900266	901.950931	11.265549
14.319394	892.007131	11.270554
14.057730	892.933597	11.275559
14.013379	901.109724	11.280563
14.062555	895.774673	11.285568
14.129163	902.239369	11.290573
14.347734	896.637591	11.295578
14.552093	896.545085	11.300583
14.527844	893.986288	11.305587
14.520511	901.544622	11.310592
14.145458	901.699078	11.315597
14.338828	898.533107	11.320602
14.316036	896.232710	11.325607
14.372420	891.071562	11.330611
14.373442	895.830903	11.335616
14.324444	899.954793	11.340621
14.698506	901.593615	11.345626
14.523556	917.819268	11.350631
14.984756	923.024068	11.355635
15.165164	921.009819	11.360640
14.489315	917.132456	11.365645
14.923340	914.205657	11.370650
14.899323	923.621259	11.375655
15.072354	921.690193	11.380659
15.381498	931.708710	11.385664
14.924655	931.284822	11.390669
15.182269	923.230821	11.395674
15.086714	936.262948	11.400679
14.991872	918.629461	11.405683
15.387604	925.650410	11.410688
15.059311	932.611789	11.415693
15.468953	928.417784	11.420698
15.136537	931.763673	11.425703
15.494681	930.405510	11.430707
15.233431	938.095829	11.435712
15.316609	939.178620	11.440717
15.610671	930.137884	11.445722
15.369589	936.855108	11.450727
15.445892	929.864559	11.455731
15.870343	931.586816	11.460736
15.568353	938.137126	11.465741
15.660603	932.870890	11.470746
15.654420	941.151344	11.475751
15.754116	954.187041	11.480755
15.921149	951.484178	11.485760
15.683609	956.530760	11.490765
16.152615	956.077483	11.495770
15.945751	962.719871	11.500775
16.197814	965.543592	11.505779
16.503695	952.159362	11.510784
16.180210	956.760733	11.515789
16.469588	951.122409	11.520794
16.368210	959.416480	11.525799
16.303577	952.713341	11.530803
16.378512	960.122959	11.535808
16.509748	954.956158	11.540813
16.732778	950.000236	11.545818
16.660104	959.177602	11.550823
16.400476	949.614849	11.555827
16.674603	954.759606	11.560832
16.620097	958.598947	11.565837
16.523124	962.683195	11.570842
16.501266	960.199703	11.575847
16.637425	956.202281	11.580851
16.594667	955.800663	11.585856
16.480285	961.608239	11.590861
17.045361	954.891402	11.595866
16.677897	962.027786	11.600871
16.864806	958.795020	11.605875
16.708615	955.222716	11.610880
17.023208	953.292724	11.615885
17.023224	949.716009	11.620890
16.740279	955.758637	11.625895
17.071437	969.408749	11.630899
17.436960	981.531545	11.635904
17.705981	983.319602	11.640909
17.640601	969.119310	11.645914
17.418870	957.604437	11.650919
17.390370	962.718611	11.655923
17.412365	961.589111	11.660928
17.345063	951.533609	11.665933
17.278496	958.853825	11.670938
17.584726	974.528107	11.675943
17.411689	986.616949	11.680947
17.925964	985.382123	11.685952
17.634914	995.072185	11.690957
17.945576	988.007958	11.695962
17.661764	990.429845	11.700967
17.686243	994.165129	11.705971
17.841765	986.717191	11.710976
17.932348	992.608791	11.715981
17.847566	984.383849	11.720986
17.798684	988.329539	11.725991
18.117953	990.412375	11.730995
18.263157	988.738066	11.736000
17.921819	990.800100	11.741005
17.971302	994.862575	11.746010
18.130037	996.108372	11.751015
18.101076	989.593503	11.756019
18.353614	999.100671	11.761024
18.001361	996.743988	11.766029
18.437282	1002.055357	11.771034
18.403517	1023.775118	11.776039
18.730184	1015.885105	11.781043
18.812950	1020.060558	11.786048
18.340688	1014.628846	11.791053
18.751003	1013.129883	11.796058
18.719549	1021.486959	11.801063
18.826551	1013.595710	11.806067
18.792716	1029.258053	11.811072
18.729438	1020.499773	11.816077
18.949318	1012.926432	11.821082
18.744458	1022.687927	11.826087
18.740183	1015.751192	11.831091
18.833375	1020.155231	11.836096
18.771202	1026.981164	11.841101
18.973041	1019.622023	11.846106
18.906651	1024.209220	11.851111
18.858966	1022.642946	11.856115
19.039102	1016.116795	11.861120
18.974878	1021.119986	11.866125
18.961848	1022.517767	11.871130
19.227794	1042.530700	11.876135
19.379733	1051.609219	11.881139
19.780694	1048.261864	11.886144
19.469677	1057.382683	11.891149
19.928343	1046.729109	11.896154
19.616149	1044.072698	11.901159
19.659613	1031.370531	11.906163
19.665640	1026.081741	11.911168
19.675293	1037.488589	11.916173
19.738927	1034.904711	11.921178
19.735722	1038.674386	11.926183
19.977467	1041.118121	11.931187
20.048120	1041.458550	11.936192
19.829552	1044.868313	11.941197
20.170070	1043.117113	11.946202
19.982254	1038.146257	11.951207
19.902329	1036.119895	11.956211
19.958230	1036.623535	11.961216
19.968312	1056.008626	11.966221
20.095197	1045.113060	11.971226
19.873523	1047.064547	11.976231
19.962487	1052.945390	11.981235
20.151415	1041.729252	11.986240
19.983573	1050.872966	11.991245
19.965849	1045.822938	11.996250
20.261643	1050.199404	12.001255
20.793431	1063.125281	12.006259
20.724709	1052.752947	12.011264
20.491695	1048.464275	12.016269
20.416440	1040.594195	12.021274
20.486488	1051.713861	12.026279
20.467404	1067.214611	12.031283
20.570975	1071.919805	12.036288
20.670013	1071.165963	12.041293
21.027755	1069.206996	12.046298
20.990775	1066.213355	12.051303
20.891929	1054.639379	12.056307
21.026502	1048.122057	12.061312
20.792785	1049.827868	12.066317
20.877281	1040.289022	12.071322
20.586314	1054.776498	12.076327
20.806811	1047.504258	12.081331
20.722020	1039.290325	12.086336
20.504974	1049.020663	12.091341
20.847499	1040.531983	12.096346
20.726518	1052.634656	12.101351
20.514151	1052.812054	12.106355
20.741814	1042.078624	12.111360
20.602670	1057.046543	12.116365
20.893267	1039.714156	12.121370
20.679723	1028.114338	12.126375
20.554884	1022.641404	12.131379
20.829487	1011.050481	12.136384
20.631954	1022.034596	12.141389
20.418384	1019.103824	12.146394
20.246593	1020.668860	12.151399
20.743294	1038.681560	12.156403
20.526850	1033.940790	12.161408
20.551674	1047.015322	12.166413
20.725675	1042.392060	12.171418
20.997043	1036.937937	12.176423
20.407594	1038.937040	12.181427
20.644461	1020.420996	12.186432
20.495247	1014.899911	12.191437
20.589743	1011.166178	12.196442
20.460390	1018.696723	12.201447
20.512414	1033.703519	12.206451
20.974808	1044.527201	12.211456
20.559780	1028.794527	12.216461
20.748554	1021.511589	12.221466
20.691810	1026.273878	12.226471
20.565799	1023.810140	12.231475
20.874442	1014.883728	12.236480
20.302497	1023.645571	12.241485
20.454421	1019.189852	12.246490
20.454170	1028.344672	12.251495
20.644885	1025.516585	12.256499
20.711307	1022.407107	12.261504
20.439832	1027.085366	12.266509
20.698978	1013.027249	12.271514
20.594687	1019.566566	12.276519
20.515470	1025.095729	12.281523
20.452047	1019.021609	12.286528
20.510623	1043.825571	12.291533
20.636802	1050.023773	12.296538
20.668166	1050.725305	12.301543
20.677389	1041.827707	12.306547
20.664354	1029.672326	12.311552
20.645670	1033.472856	12.316557
20.942278	1030.454404	12.321562
20.677465	1028.735091	12.326567
20.688332	1035.836403	12.331571
20.830483	1026.465000	12.336576
20.744388	1025.157180	12.341581
20.801357	1017.881072	12.346586
20.701163	1024.375581	12.351591
20.548580	1030.121464	12.356595
20.944860	1020.312117	12.361600
20.627266	1027.066818	12.366605
20.904205	1025.497658	12.371610
20.555150	1023.214582	12.376615
20.494168	1027.002931	12.381619
20.690922	1024.886708	12.386624
20.634164	1025.972900	12.391629
20.793359	1021.594872	12.396634
20.771655	1031.202574	12.401639
20.846569	1034.950326	12.406643
20.799013	1036.886658	12.411648
20.453620	1032.754694	12.416653
21.148196	1018.456804	12.421658
20.461051	1010.692216	12.426663
20.529849	1007.680139	12.431667
20.423803	1008.250611	12.436672
20.439378	1009.451429	12.441677
20.731229	1009.941092	12.446682
20.693411	1009.450370	12.451687
20.360339	1012.537745	12.456691
20.992019	1017.106650	12.461696
20.318912	1020.125250	12.466701
20.490276	1015.798902	12.471706
20.646775	1021.668961	12.476711
20.327828	1034.172222	12.481715
20.705674	1032.569620	12.486720
20.847059	1042.848375	12.491725
20.777077	1033.152810	12.496730
20.648485	1023.504449	12.501735
20.546288	1019.475636	12.506739
20.701972	1008.089774	12.511744
20.287761	1018.239491	12.516749
20.661033	1014.937563	12.521754
20.689772	1015.917073	12.526759
20.509468	1019.286031	12.531763
20.689173	1012.184328	12.536768
20.494969	1010.728162	12.541773
20.508332	1014.048884	12.546778
20.772315	1023.480122	12.551783
20.374908	1021.729915	12.556787
20.737975	1022.794882	12.561792
20.570602	1034.925441	12.566797
20.816959	1024.220584	12.571802
20.459651	1022.115453	12.576807
20.456438	1023.431239	12.581811
20.540991	1022.435268	12.586816
20.343788	1037.850848	12.591821
20.648103	1041.645598	12.596826
20.718029	1049.251615	12.601831
20.700647	1048.614120	12.606835
20.865759	1052.528852	12.611840
20.531503	1038.918612	12.616845
20.534132	1030.149814	12.621850
20.572161	1018.285938	12.626855
20.365441	1027.164586	12.631859
20.767450	1034.561503	12.636864
20.734766	1043.549607	12.641869
20.780909	1036.648978	12.646874
20.748869	1032.334565	12.651879
20.380740	1030.600189	12.656883
20.738959	1029.150538	12.661888
20.315855	1026.887156	12.666893
20.453846	1028.749736	12.671898
20.762257	1041.130866	12.676903
20.688719	1045.451112	12.681907
20.712204	1039.598102	12.686912
20.639254	1029.469325	12.691917
21.035913	1031.413660	12.696922
20.910922	1028.635926	12.701927
20.491015	1035.088384	12.706931
20.796148	1026.548902	12.711936
20.800535	1037.305269	12.716941
20.669035	1028.365464	12.721946
20.814329	1036.419952	12.726951
20.719792	1033.110625	12.731955
20.839389	1022.164196	12.736960
20.788776	1029.964480	12.741965
20.894658	1033.633172	12.746970
20.785596	1037.539586	12.751975
20.638499	1025.110682	12.756979
20.695564	1004.128446	12.761984
20.391840	1012.057404	12.766989
20.453657	1015.925519	12.771994
20.695856	1030.009371	12.776999
20.469483	1034.148973	12.782003
20.697525	1031.471060	12.787008
20.663176	1047.912568	12.792013
20.799992	1033.063338	12.797018
20.639188	1021.680631	12.802023
20.407563	1012.821463	12.807027
20.255040	1020.942366	12.812032
20.664874	1031.274497	12.817037
20.733630	1035.723442	12.822042
20.625245	1037.371413	12.827047
20.646743	1043.158927	12.832051
20.707676	1040.969741	12.837056
20.444524	1045.362808	12.842061
20.708098	1034.458066	12.847066
20.889284	1030.043410	12.852071
20.463636	1020.540206	12.857075
20.604371	1008.382397	12.862080
20.701685	1013.940176	12.867085
20.630729	1009.417498	12.872090
20.811411	1003.301297	12.877095
20.614901	1004.105407	12.882099
20.707216	1012.305534	12.887104
20.352425	1013.784632	12.892109
20.499719	1000.318412	12.897114
20.530852	1009.998102	12.902119
20.556089	1008.887006	12.907123
20.633034	1005.857859	12.912128
20.607016	1010.908573	12.917133
20.499719	1008.443430	12.922138
20.519417	1014.491432	12.927143
20.474813	1036.608780	12.932147
20.726234	1026.860382	12.937152
20.637305	1042.173536	12.942157
20.985592	1023.721724	12.947162
20.953569	1013.217402	12.952167
20.502292	1006.796690	12.957171
20.589804	1005.016456	12.962176
20.627631	1010.716193	12.967181
20.288816	1006.480680	12.972186
20.223292	1022.080257	12.977191
20.276331	1018.293206	12.982195
20.689171	1026.535266	12.987200
20.307772	1039.977374	12.992205
20.984356	1041.843947	12.997210
21.070184	1033.986028	13.002215
20.494695	1028.394144	13.007219
20.718529	1013.600446	13.012224
20.676223	1024.838942	13.017229
20.625220	1014.739793	13.022234
20.198219	1015.918153	13.027239
20.288751	1025.585226	13.032243
20.964341	1027.726362	13.037248
20.756901	1033.996690	13.042253
20.520822	1015.860453	13.047258
20.044706	1016.259700	13.052263
20.615397	1038.039204	13.057267
20.437446	1045.241602	13.062272
20.654592	1057.837588	13.067277
20.934310	1054.523762	13.072282
20.839509	1054.079976	13.077287
20.674847	1039.912797	13.082291
20.803260	1021.772039	13.087296
20.592281	1026.008537	13.092301
20.575154	1018.821522	13.097306
20.559785	1012.667195	13.102311
20.368231	1007.197023	13.107315
20.533979	1018.776092	13.112320
20.591670	1025.196531	13.117325
20.511095	1036.482143	13.122330
20.586274	1044.759143	13.127335
20.632446	1055.073593	13.132339
20.793114	1048.463795	13.137344
20.549383	1038.223469	13.142349
20.477471	1035.150245	13.147354
20.504740	1044.519896	13.152359
20.598340	1053.238691	13.157363
20.949929	1055.671218	13.162368
20.486151	1041.072321	13.167373
20.922024	1029.209642	13.172378
20.835697	1031.951721	13.177383
20.402707	1027.411081	13.182387
20.711745	1025.281680	13.187392
20.558437	1021.030769	13.192397
20.726083	1022.339806	13.197402
20.661637	1028.909044	13.202407
20.707692	1022.144062	13.207411
20.609555	1014.427465	13.212416
20.443891	1025.199906	13.217421
20.600830	1029.171132	13.222426
20.623418	1028.375866	13.227431
20.424944	1027.226327	13.232435
20.520556	1032.894777	13.237440
20.368392	1026.912082	13.242445
20.331948	1032.967469	13.247450
20.647832	1042.655386	13.252455
20.640698	1043.747858	13.257459
20.853391	1027.344177	13.262464
20.731938	1024.136922	13.267469
20.878602	1025.185939	13.272474
20.833220	1023.827468	13.277479
20.729234	1028.671414	13.282483
20.784325	1025.472273	13.287488
20.600672	1037.614893	13.292493
20.454762	1028.319396	13.297498
20.682685	1022.121532	13.302503
20.876317	1034.598238	13.307507
20.797868	1030.335385	13.312512
20.425128	1041.751183	13.317517
20.578512	1025.221337	13.322522
20.730047	1034.914959	13.327527
20.275024	1036.637141	13.332531
20.749516	1032.827026	13.337536
20.557601	1036.532175	13.342541
20.470913	1032.425186	13.347546
20.802762	1027.784639	13.352551
20.974366	1021.862279	13.357555
21.042955	1024.098648	13.362560
20.773712	1030.323636	13.367565
20.743752	1026.554552	13.372570
20.255313	1016.039438	13.377575
20.422398	1026.826623	13.382579
20.506543	1031.378774	13.387584
20.958399	1031.049663	13.392589
20.812453	1023.041047	13.397594
20.848308	1025.566507	13.402599
20.734665	1014.223595	13.407603
20.586293	1008.658220	13.412608
20.105545	1012.377888	13.417613
20.866796	1024.024420	13.422618
20.963886	1023.756623	13.427623
20.718468	1008.675050	13.432627
20.556356	1002.973089	13.437632
20.480478	996.046205	13.442637
20.501431	998.961990	13.447642
20.776504	997.752697	13.452647
20.581564	1007.272888	13.457651
20.785325	999.471877	13.462656
20.277954	1002.848839	13.467661
20.322369	1002.266149	13.472666
20.573069	1007.168643	13.477671
20.773006	1016.255255	13.482675
20.660547	1010.515408	13.487680
20.536101	1006.912795	13.492685
20.534268	996.275929	13.497690
20.466253	1004.555242	13.502695
20.815021	1023.588211	13.507699
20.577888	1008.282953	13.512704
20.490707	1003.690321	13.517709
20.702669	1009.349668	13.522714
20.621700	1000.275657	13.527719
20.387095	1011.957999	13.532723
20.912935	1014.171905	13.537728
20.661485	1004.533690	13.542733
20.250543	1008.497705	13.547738
20.424314	1005.456270	13.552743
20.355705	1025.730708	13.557747
20.900504	1030.037491	13.562752
20.728449	1038.166250	13.567757
20.670680	1027.224449	13.572762
20.752971	1019.794482	13.577767
20.371610	1013.455663	13.582771
20.814949	1007.538857	13.587776
20.608960	1015.308718	13.592781
20.765357	1000.377546	13.597786
20.509283	1001.443483	13.602791
20.268301	1007.995133	13.607795
20.922955	1007.340348	13.612800
20.820878	1010.524930	13.617805
20.775992	1003.484284	13.622810
21.024638	1002.870598	13.627815
20.541064	1005.937818	13.632819
20.703439	995.509743	13.637824
20.628852	1005.117977	13.642829
20.521728	1002.389440	13.647834
20.642430	1000.862549	13.652839
20.228751	1005.276458	13.657843
20.619627	1004.886107	13.662848
20.896706	1009.267123	13.667853
20.900502	1006.126633	13.672858
20.612188	1007.964156	13.677863
20.572065	1004.802285	13.682867
20.909790	1003.586153	13.687872
20.568204	1004.779276	13.692877
20.562080	1001.876926	13.697882
20.715987	999.348046	13.702887
20.486887	1001.455262	13.707891
20.460693	1003.075927	13.712896
20.524580	1011.203312	13.717901
20.389046	1002.212124	13.722906
20.655053	1002.412579	13.727911
20.281999	1011.839749	13.732915
20.780943	1009.195909	13.737920
20.325555	1002.842091	13.742925
20.556523	996.962315	13.747930
20.564971	1002.797629	13.752935
20.713328	1008.676867	13.757939
20.748678	1007.035847	13.762944
20.764763	1018.559933	13.767949
20.603867	1004.851109	13.772954
20.866099	1003.375766	13.777959
20.713011	1008.653338	13.782963
20.658561	1009.941023	13.787968
20.585368	1006.342852	13.792973
20.891344	1005.155440	13.797978
20.978381	1004.094415	13.802983
20.433582	1005.009270	13.807987
20.714236	1010.137236	13.812992
20.684845	1006.738672	13.817997
20.885887	1003.057338	13.823002
20.756852	996.545811	13.828007
20.627578	994.095214	13.833011
20.487256	982.496370	13.838016
20.263677	991.032312	13.843021
20.637955	1002.231160	13.848026
20.802488	1011.954234	13.853031
20.518741	1021.665229	13.858035
20.794725	1011.679520	13.863040
20.622036	1009.675841	13.868045
20.721483	1004.603985	13.873050
20.898369	991.912114	13.878055
20.370924	992.420477	13.883059
20.816731	979.065948	13.888064
20.585602	989.178560	13.893069
20.641372	983.717838	13.898074
20.588624	979.960286	13.903079
20.463258	991.312935	13.908083
20.571683	981.265657	13.913088
20.794134	978.429364	13.918093
20.511852	984.687953	13.923098
20.393280	972.186733	13.928103
20.403026	982.219919	13.933107
20.632456	984.832776	13.938112
20.576499	985.937762	13.943117
20.511067	976.744586	13.948122
20.646565	984.849497	13.953127
20.281201	1002.348324	13.958131
20.668765	1003.278488	13.963136
20.821454	1011.222967	13.968141
20.562075	1013.598380	13.973146
20.696163	1002.883057	13.978151
20.516151	1002.112221	13.983155
20.577042	998.754456	13.988160
20.511387	1007.156405	13.993165
20.383631	1014.732427	13.998170
20.809414	1003.366572	14.003175
20.688790	1007.531880	14.008179
20.973022	1002.309121	14.013184
21.158068	989.581255	14.018189
20.616090	988.063243	14.023207
20.530189	978.192097	14.028224
20.497026	984.321170	14.033242
20.449601	978.860930	14.038259
20.493827	980.853201	14.043277
20.555659	983.220188	14.048295
20.751686	980.222222	14.053312
20.226014	991.148912	14.058330
20.903946	1000.650395	14.063347
20.863360	1016.796105	14.068365
20.947587	1014.740901	14.073383
20.874407	1007.727464	14.078400
20.735690	1004.106482	14.083418
20.785752	1004.633340	14.088435
20.800616	1012.997897	14.093453
20.703985	1016.925435	14.098471
21.220402	1009.250100	14.103488
20.724168	1017.375278	14.108506
21.013399	1018.249383	14.113523
20.870751	1021.813028	14.118541
20.813456	1034.996271	14.123559
21.040945	1022.445012	14.128576
20.614837	1020.227383	14.133594
20.746931	1019.419818	14.138611
20.647562	1023.807118	14.143629
20.607646	1026.641799	14.148647
20.958523	1028.789661	14.153664
20.548648	1030.256614	14.158682
20.746677	1029.142804	14.163699
21.309822	1042.886197	14.168717
21.038543	1054.450335	14.173735
21.322788	1051.812665	14.178752
21.149683	1057.257799	14.183770
21.352938	1050.687891	14.188787
21.285835	1057.827574	14.193805
20.959074	1050.171865	14.198823
21.311584	1052.305314	14.203840
20.941064	1058.079236	14.208858
20.983634	1057.661901	14.213875
21.394825	1056.954540	14.218893
21.242340	1058.208984	14.223911
21.447538	1045.005307	14.228928
21.540922	1047.521430	14.233946
21.365971	1050.844842	14.238963
21.370984	1055.692131	14.243981
21.298118	1055.579499	14.248999
21.710022	1051.334283	14.254016
21.318107	1062.472500	14.259034
21.405089	1057.473714	14.264051
21.357373	1051.223832	14.269069
20.979276	1057.411096	14.274087
21.533404	1052.849040	14.279104
21.171146	1055.941205	14.284122
21.208527	1062.156587	14.289139
21.655299	1076.396774	14.294157
21.868915	1083.637989	14.299175
21.885095	1066.646692	14.304192
21.491768	1057.790364	14.309210
21.514177	1059.641406	14.314227
21.762516	1056.078229	14.319245
21.622000	1058.869186	14.324263
21.732849	1050.907728	14.329280
21.397742	1062.043177	14.334298
21.359792	1060.669699	14.339315
21.915283	1066.339979	14.344333
21.872225	1081.312674	14.349351
22.308378	1062.462718	14.354368
21.986991	1061.414444	14.359386
21.671877	1061.930334	14.364403
21.799983	1056.102295	14.369421
21.635256	1062.378227	14.374439
21.896283	1051.886981	14.379456
21.774241	1059.884862	14.384474
21.920248	1060.132152	14.389491
21.943599	1071.622571	14.394509
21.688445	1083.344608	14.399527
22.217342	1078.898254	14.404544
22.017201	1092.107477	14.409562
22.258130	1083.788626	14.414579
22.167810	1063.396122	14.419597
21.593064	1066.287796	14.424615
21.969732	1072.395587	14.429632
21.872233	1078.866871	14.434650
22.018650	1088.328915	14.439667
22.152110	1082.995516	14.444685
21.858338	1092.980802	14.449703
22.312162	1080.553844	14.454720
22.282244	1089.142665	14.459738
22.178858	1087.318722	14.464755
22.209911	1087.139178	14.469773
22.333196	1095.993007	14.474791
22.326323	1083.189636	14.479808
22.270540	1089.163485	14.484826
22.359474	1093.503470	14.489843
22.253354	1084.755475	14.494861
22.010865	1088.352363	14.499879
22.447916	1077.977743	14.504896
22.296448	1088.755160	14.509914
22.352740	1085.993392	14.514931
22.472317	1088.170288	14.519949
22.277121	1095.114913	14.524967
22.636447	1085.696504	14.529984
22.130830	1095.736028	14.535002
22.324490	1093.867855	14.540019
22.541056	1091.723893	14.545037
22.595207	1098.353471	14.550055
22.578060	1085.133310	14.555072
22.569401	1092.251104	14.560090
22.468552	1086.582265	14.565107
22.490549	1097.663932	14.570125
22.552691	1109.399879	14.575143
22.820141	1112.541061	14.580160
22.858485	1117.299684	14.585178
22.737638	1105.043011	14.590195
22.778571	1093.581670	14.595213
22.533878	1088.222064	14.600231
22.759074	1098.823010	14.605248
22.949005	1112.443522	14.610266
22.714669	1106.146302	14.615283
22.826098	1097.306974	14.620301
22.561741	1100.838139	14.625319
23.134819	1108.149452	14.630336
22.783596	1114.187734	14.635354
22.936522	1116.249204	14.640371
23.323897	1111.059343	14.645389
22.675314	1116.385277	14.650407
22.977527	1108.660683	14.655424
23.257662	1115.946361	14.660442
23.071396	1100.752258	14.665459
23.185191	1089.557726	14.670477
22.939667	1089.145440	14.675495
22.809324	1083.898160	14.680512
22.918081	1087.714308	14.685530
22.751311	1097.084735	14.690547
23.022999	1109.789284	14.695565
23.112433	1117.062906	14.700583
23.331934	1112.931730	14.705600
23.570651	1115.344461	14.710618
23.218407	1116.780207	14.715635
23.378812	1114.889020	14.720653
23.473005	1119.868400	14.725671
23.383497	1106.853243	14.730688
23.155223	1091.368547	14.735706
23.198946	1091.665184	14.740723
23.544150	1107.337330	14.745741
23.275813	1105.829131	14.750759
23.080932	1097.540453	14.755776
23.430564	1101.584031	14.760794
23.526235	1114.162500	14.765811
23.527895	1111.793260	14.770829
23.365293	1113.617187	14.775847
23.611091	1121.285873	14.780864
23.692100	1110.584195	14.785882
23.132967	1111.941252	14.790899
23.619199	1100.832031	14.795917
23.290739	1121.563545	14.800935
23.434938	1112.256508	14.805952
23.549418	1108.631297	14.810970
23.531840	1119.426708	14.815987
23.284236	1113.556321	14.821005
23.593664	1110.887883	14.826023
23.523409	1110.505844	14.831040
23.633259	1117.585873	14.836058
23.557825	1112.754545	14.841075
23.549017	1112.721358	14.846093
23.531689	1125.596286	14.851111
23.630885	1119.307214	14.856128
23.872645	1113.421700	14.861146
23.685637	1112.877383	14.866163
23.859862	1109.720846	14.871181
23.484348	1120.590648	14.876199
23.967760	1137.118538	14.881216
24.257410	1139.826746	14.886234
23.766222	1129.224178	14.891251
24.020806	1116.204472	14.896269
23.700870	1125.248558	14.901287
23.898853	1135.278140	14.906304
24.117074	1139.237293	14.911322
24.123762	1141.545461	14.916339
24.380677	1147.128113	14.921357
24.002684	1133.471525	14.926375
23.764022	1125.119028	14.931392
23.858418	1132.251865	14.936410
23.829950	1150.939392	14.941427
24.129573	1145.914526	14.946445
24.445230	1152.253881	14.951463
24.099720	1148.401573	14.956480
24.092288	1138.904770	14.961498
24.036708	1158.095282	14.966515
24.517571	1157.584446	14.971533
24.494146	1152.645708	14.976551
24.339141	1152.794715	14.981568
24.379386	1144.835028	14.986586
24.476747	1145.017719	14.991603
24.566634	1135.620228	14.996621
24.419778	1152.931355	15.001639
24.302580	1151.128483	15.006656
24.337093	1149.395797	15.011674
24.474436	1150.478181	15.016691
24.560779	1146.451604	15.021709
24.258248	1143.877615	15.026727
24.157237	1151.977586	15.031744
24.182436	1142.223890	15.036762
24.124390	1141.787993	15.041779
24.687023	1146.491322	15.046797
24.593469	1154.358868	15.051815
24.450488	1149.815155	15.056832
24.578168	1143.406698	15.061850
24.458924	1149.621930	15.066867
24.479603	1151.635283	15.071885
24.600483	1155.529740	15.076903
24.787296	1170.189010	15.081920
25.135949	1173.263771	15.086938
24.809197	1168.038347	15.091955
24.830818	1141.573247	15.096973
24.913539	1155.330449	15.101991
24.945436	1164.938224	15.107008
25.182082	1164.346787	15.112026
24.997631	1170.990856	15.117043
25.122677	1167.343496	15.122061
25.103355	1168.483901	15.127079
25.198577	1173.137516	15.132096
25.201198	1165.624270	15.137114
25.088809	1171.287853	15.142131
25.474235	1166.601658	15.147149
25.492854	1164.358694	15.152167
24.996853	1169.649300	15.157184
25.531158	1163.177554	15.162202
25.157265	1145.763881	15.167219
24.918413	1111.873167	15.172237
24.919035	1120.913316	15.177255
24.881155	1131.727705	15.182272
25.260505	1131.329015	15.187290
24.951599	1144.558779	15.192307
25.198601	1143.031306	15.197325
25.050937	1139.432166	15.202343
24.798370	1141.078535	15.207360
24.932063	1140.314753	15.212378
25.205027	1146.174846	15.217395
25.327445	1145.280728	15.222413
25.244218	1147.337394	15.227431
25.054874	1134.344427	15.232448
25.334869	1147.996227	15.237466
25.397585	1161.324040	15.242483
25.719982	1158.686559	15.247501
25.546167	1145.525937	15.252519
25.255635	1156.737719	15.257536
25.547934	1160.354726	15.262554
25.463283	1169.487157	15.267571
25.806429	1167.382772	15.272589
25.445737	1175.461251	15.277607
25.445798	1177.974977	15.282624
25.985885	1165.203851	15.287642
25.600245	1176.652616	15.292659
25.722635	1170.882072	15.297677
25.974009	1166.421751	15.302695
25.749534	1161.159568	15.307712
26.280789	1148.246719	15.312730
25.840612	1148.875366	15.317747
25.635909	1139.477666	15.322765
25.569329	1148.281583	15.327783
25.311546	1146.762258	15.332800
25.836913	1153.834236	15.337818
25.699623	1167.716203	15.342835
25.650882	1171.625134	15.347853
25.855478	1166.720811	15.352871
25.756501	1172.967427	15.357888
26.028234	1173.317364	15.362906
25.748927	1171.210006	15.367923
26.110262	1169.827892	15.372941
26.232311	1169.493833	15.377959
26.039422	1179.083985	15.382976
26.344453	1183.087508	15.387994
26.466377	1195.238712	15.393011
25.947054	1195.282227	15.398029
26.497378	1196.515829	15.403047
26.287585	1192.369727	15.408064
26.608898	1190.147697	15.413082
26.498725	1202.290305	15.418099
26.190587	1200.827770	15.423117
26.528062	1192.562673	15.428135
26.138978	1188.322469	15.433152
26.480628	1182.339198	15.438170
26.432799	1197.161761	15.443187
26.151790	1193.940956	15.448205
26.476023	1188.525182	15.453223
26.238545	1196.815258	15.458240
26.338247	1194.682055	15.463258
26.063619	1187.941335	15.468275
26.175888	1192.589091	15.473293
26.300755	1189.215463	15.478311
26.260030	1187.125108	15.483328
26.344430	1177.435879	15.488346
26.202057	1168.278332	15.493363
26.025221	1170.760495	15.498381
26.391249	1180.714543	15.503399
26.354241	1193.896267	15.508416
26.576098	1203.418715	15.513434
26.541987	1196.225920	15.518451
26.952430	1192.989219	15.523469
26.868086	1194.278424	15.528487
26.873334	1198.768643	15.533504
27.004154	1191.294713	15.538522
27.250319	1197.188988	15.543539
26.890601	1186.571703	15.548557
26.804926	1189.876188	15.553575
26.840255	1201.663678	15.558592
27.025795	1192.436514	15.563610
26.871484	1196.447233	15.568627
27.155680	1197.591143	15.573645
27.214008	1191.747437	15.578663
27.064662	1191.923857	15.583680
27.131206	1190.845163	15.588698
27.151880	1186.718935	15.593715
26.812964	1188.849420	15.598733
26.872185	1186.570090	15.603751
26.849018	1188.618756	15.608768
26.784511	1190.590644	15.613786
26.985238	1187.864023	15.618803
26.915186	1185.941941	15.623821
26.999624	1182.343526	15.628839
26.837783	1186.696793	15.633856
27.053738	1185.488876	15.638874
27.605380	1204.406425	15.643891
27.191398	1204.686399	15.648909
27.634908	1204.225565	15.653927
27.437939	1196.630876	15.658944
27.484121	1193.205302	15.663962
27.235622	1189.910098	15.668979
27.281874	1198.672455	15.673997
27.424718	1206.181426	15.679015
27.172878	1223.932529	15.684032
27.721965	1214.751191	15.689050
27.522701	1211.863414	15.694067
27.449935	1223.891534	15.699085
27.634414	1212.583386	15.704103
27.563404	1215.802167	15.709120
27.746365	1208.022607	15.714138
27.853803	1226.141136	15.719155
27.898305	1215.423180	15.724173
28.092477	1217.710897	15.729191
27.658215	1208.138976	15.734208
27.401399	1194.080754	15.739226
27.647244	1205.378489	15.744243
27.857833	1217.222984	15.749261
27.961482	1206.651334	15.754279
27.801786	1216.360487	15.759296
27.792315	1211.181973	15.764314
27.806673	1214.165339	15.769331
27.797164	1225.030329	15.774349
27.966335	1211.094489	15.779367
27.897167	1212.752515	15.784384
27.940107	1211.778259	15.789402
28.041723	1211.664539	15.794419
27.895849	1211.497481	15.799437
28.356022	1206.697103	15.804455
28.141859	1219.005750	15.809472
28.033506	1209.943426	15.814490
28.166556	1217.537336	15.819507
28.351047	1217.278262	15.824525
28.238253	1214.946136	15.829543
27.958883	1222.763129	15.834560
27.987725	1214.868145	15.839578
27.857766	1213.951352	15.844595
27.611348	1224.717271	15.849613
28.265404	1233.562038	15.854631
28.188958	1247.475276	15.859648
28.344885	1246.228164	15.864666
28.341751	1246.205083	15.869683
28.308256	1250.374303	15.874701
28.332654	1241.835062	15.879719
28.206570	1254.721158	15.884736
28.345109	1250.308695	15.889754
28.570567	1245.772259	15.894771
28.259573	1249.859892	15.899789
28.596944	1245.448754	15.904807
28.647488	1252.627971	15.909824
28.508624	1252.906541	15.914842
28.875411	1255.571008	15.919859
28.530276	1248.673187	15.924877
28.800798	1239.800534	15.929895
28.570993	1249.984940	15.934912
28.476227	1262.144017	15.939930
28.931936	1259.192670	15.944947
28.842900	1276.195842	15.949965
28.967758	1269.150694	15.954983
29.057473	1287.069201	15.960000
29.165804	1269.405434	15.965018
29.229732	1244.010940	15.970035
28.720686	1244.452370	15.975053
28.868947	1235.147753	15.980071
28.937928	1247.593740	15.985088
29.083058	1249.181411	15.990106
29.319488	1237.860239	15.995123
29.170802	1239.493197	16.000141
29.239240	1233.086283	16.005159
29.130393	1233.380515	16.010176
29.095534	1232.237765	16.015194
29.225074	1241.461924	16.020211
28.858854	1243.146880	16.025229
29.193785	1232.598099	16.030247
29.264022	1246.830867	16.035264
29.484294	1269.828358	16.040282
29.615943	1252.494379	16.045299
29.392016	1251.310995	16.050317
29.317152	1240.693857	16.055335
29.154761	1239.727178	16.060352
29.381637	1250.260326	16.065370
29.473732	1252.278034	16.070387
29.559745	1265.970321	16.075405
29.796715	1256.291314	16.080423
29.369934	1255.050618	16.085440
29.345505	1254.091823	16.090458
29.298474	1265.244403	16.095475
29.355078	1271.850073	16.100493
29.686959	1267.153509	16.105511
29.770595	1279.529544	16.110528
29.366505	1275.878456	16.115546
29.297916	1272.968253	16.120563
29.437226	1283.375389	16.125581
29.540966	1270.208140	16.130599
29.902336	1277.396000	16.135616
29.522886	1279.449591	16.140634
29.812664	1275.834134	16.145651
29.605349	1294.978240	16.150669
29.705984	1300.041599	16.155687
30.296297	1308.339718	16.160704
30.238611	1297.516874	16.165722
30.356040	1288.202984	16.170739
29.884288	1280.087349	16.175757
29.841297	1270.363319	16.180775
30.068041	1284.786671	16.185792
30.283721	1309.826781	16.190810
30.603795	1293.511931	16.195827
29.997011	1282.177339	16.200845
30.037989	1275.570289	16.205863
30.215542	1280.909243	16.210880
30.229839	1280.296633	16.215898
30.352642	1280.056836	16.220915
30.218492	1285.484830	16.225933
30.264932	1289.046698	16.230951
30.374760	1290.020221	16.235968
30.398291	1301.240228	16.240986
30.375192	1293.347192	16.246003
30.333115	1293.303581	16.251021
30.344789	1301.585441	16.256039
30.480923	1302.049819	16.261056
30.263066	1307.653196	16.266074
30.687159	1302.196286	16.271091
30.323240	1312.685275	16.276109
30.600152	1297.826089	16.281127
30.465491	1285.584051	16.286144
30.429044	1307.751073	16.291162
30.857811	1287.837046	16.296179
30.867591	1289.150575	16.301197
30.745378	1294.936898	16.306215
30.656239	1293.650214	16.311232
30.603763	1295.835706	16.316250
30.937421	1289.682203	16.321267
30.413023	1305.996632	16.326285
30.487102	1288.585275	16.331303
30.694240	1292.137244	16.336320
30.495460	1294.659108	16.341338
30.730059	1311.937901	16.346355
30.658989	1315.244805	16.351373
31.023927	1312.112865	16.356391
30.832303	1318.547356	16.361408
31.120899	1325.334705	16.366426
31.461812	1311.879476	16.371443
31.359217	1321.142282	16.376461
31.392754	1318.431291	16.381479
31.525979	1317.156332	16.386496
31.114888	1304.431391	16.391514
31.244731	1300.902785	16.396531
31.220922	1316.218724	16.401549
31.222913	1314.577724	16.406567
31.216325	1321.017312	16.411584
31.396312	1327.589172	16.416602
31.918241	1309.165675	16.421619
31.185077	1308.546429	16.426637
31.349354	1302.032964	16.431655
31.730273	1310.350322	16.436672
31.674198	1303.233338	16.441690
31.599103	1286.814776	16.446707
31.650604	1288.857839	16.451725
31.365030	1286.389660	16.456743
31.744606	1279.527256	16.461760
31.631544	1293.581661	16.466778
31.697815	1281.853430	16.471795
31.560247	1293.689019	16.476813
31.546477	1301.171106	16.481831
32.106789	1305.752161	16.486848
31.624180	1307.929175	16.491866
32.185142	1297.997117	16.496883
31.824454	1291.288950	16.501901
31.613221	1286.852035	16.506919
32.040495	1286.418957	16.511936
32.113538	1314.848160	16.516954
32.059560	1288.567885	16.521971
31.640239	1287.079026	16.526989
31.837419	1299.573826	16.532007
32.140404	1296.859191	16.537024
31.883583	1302.470354	16.542042
31.878449	1305.477297	16.547059
31.957312	1309.101640	16.552077
32.050684	1307.957310	16.557095
32.328199	1304.485377	16.562112
32.275850	1308.937624	16.567130
32.120036	1301.690253	16.572147
32.335155	1310.370689	16.577165
32.147210	1312.456663	16.582183
32.296036	1304.761149	16.587200
32.209997	1319.679595	16.592218
32.209685	1305.542603	16.597235
32.278035	1315.257923	16.602253
32.261253	1312.548666	16.607271
32.383063	1310.125624	16.612288
32.080486	1316.201849	16.617306
32.186883	1305.160917	16.622323
32.342416	1322.963578	16.627341
32.720862	1333.802956	16.632359
33.072416	1332.513625	16.637376
32.810708	1330.769958	16.642394
32.851065	1307.889713	16.647411
32.791713	1299.588742	16.652429
32.560818	1302.806300	16.657447
32.826499	1293.902924	16.662464
32.410065	1310.170252	16.667482
32.660532	1326.776411	16.672499
32.775035	1334.197157	16.677517
32.646405	1339.866543	16.682535
33.051528	1334.881418	16.687552
32.925737	1339.936857	16.692570
32.838276	1336.106265	16.697587
33.185334	1333.021218	16.702605
32.722477	1331.087830	16.707623
32.864462	1331.299586	16.712640
32.821756	1346.964645	16.717658
32.940958	1336.196933	16.722675
33.188051	1337.013285	16.727693
32.969437	1337.608175	16.732711
33.085987	1340.696395	16.737728
33.100680	1340.714516	16.742746
33.310474	1359.924322	16.747763
33.299629	1365.434929	16.752781
33.336853	1374.354565	16.757799
33.788299	1368.048534	16.762816
33.588848	1354.363261	16.767834
33.683323	1339.253124	16.772851
33.652756	1332.836787	16.777869
33.093802	1340.007860	16.782887
33.576400	1334.458235	16.787904
33.379799	1334.901747	16.792922
33.369679	1338.084101	16.797939
33.443415	1349.477040	16.802957
33.553486	1352.545846	16.807975
33.974553	1355.379432	16.812992
34.044259	1364.271858	16.818010
33.600503	1350.608248	16.823027
33.850620	1335.776893	16.828045
33.638745	1344.605674	16.833063
34.183672	1349.145152	16.838080
33.916167	1338.966087	16.843098
33.788293	1329.961858	16.848115
33.702358	1343.492876	16.853133
33.859089	1353.334129	16.858151
34.040624	1355.107920	16.863168
33.941554	1361.486769	16.868186
33.983036	1361.494326	16.873203
34.388142	1361.461194	16.878221
34.313345	1371.641413	16.883239
34.541090	1356.277190	16.888256
34.173013	1344.767621	16.893274
34.032073	1337.115157	16.898291
33.941177	1329.877869	16.903309
33.945109	1343.742199	16.908327
34.253280	1356.541824	16.913344
34.308305	1361.854731	16.918362
34.105122	1366.120261	16.923379
34.454689	1365.386535	16.928397
34.125345	1365.283343	16.933415
34.311565	1356.269904	16.938432
34.134030	1364.714113	16.943450
33.911924	1364.449097	16.948467
34.352856	1369.157753	16.953485
34.107532	1391.773505	16.958503
34.743182	1391.664278	16.963520
34.793606	1396.570507	16.968538
34.698029	1387.819075	16.973555
34.730140	1393.418799	16.978573
34.575663	1396.436994	16.983591
34.760232	1388.696409	16.988608
34.771732	1389.863377	16.993626
34.729334	1392.764594	16.998643
35.065955	1389.514455	17.003661
34.916143	1392.843373	17.008679
35.177592	1392.817422	17.013696
34.748948	1398.062758	17.018714
35.024232	1390.601867	17.023731
35.280960	1385.432747	17.028749
35.089694	1392.543631	17.033767
35.291440	1377.224432	17.038784
35.428354	1386.351552	17.043802
35.113513	1383.946226	17.048819
35.389464	1377.935600	17.053837
35.361179	1391.424433	17.058855
35.371934	1377.733929	17.063872
35.251856	1375.362038	17.068890
35.117637	1382.117745	17.073907
35.349805	1385.878110	17.078925
35.169749	1385.842346	17.083943
35.146879	1387.437950	17.088960
35.027371	1385.430918	17.093978
35.231322	1380.296960	17.098995
35.498656	1381.193458	17.104013
35.401791	1385.459341	17.109031
35.532576	1381.738652	17.114048
35.505475	1377.448525	17.119066
35.428554	1387.157175	17.124083
35.578848	1374.783096	17.129101
35.369424	1377.434089	17.134119
35.764935	1378.417114	17.139136
35.728909	1387.648895	17.144154
35.735760	1394.630653	17.149171
35.975901	1393.691004	17.154189
35.645664	1407.231154	17.159207
35.734828	1402.629887	17.164224
36.297447	1403.740423	17.169242
35.633815	1405.947895	17.174259
35.859898	1404.172042	17.179277
36.028391	1399.886895	17.184295
36.116084	1399.973601	17.189312
35.884200	1403.450894	17.194330
35.826255	1407.771926	17.199347
35.925367	1399.165619	17.204365
35.810835	1399.456041	17.209383
35.942459	1396.924452	17.214400
36.113715	1400.749592	17.219418
35.907212	1412.500315	17.224435
36.343240	1419.731398	17.229453
36.292017	1433.543261	17.234471
36.249493	1430.485719	17.239488
36.497620	1433.433421	17.244506
36.574376	1431.645199	17.249523
36.716581	1426.610737	17.254541
36.535927	1431.166856	17.259559
36.563134	1430.671735	17.264576
36.823968	1430.353292	17.269594
36.705735	1437.479291	17.274611
36.976984	1428.760569	17.279629
36.413442	1433.023813	17.284647
36.560319	1427.058922	17.289664
36.720436	1425.627077	17.294682
36.892819	1431.435686	17.299699
37.120128	1417.968590	17.304717
36.834619	1428.910785	17.309735
36.801878	1425.787188	17.314752
36.829107	1432.635149	17.319770
36.718162	1431.178893	17.324787
36.992936	1430.645861	17.329805
37.134566	1430.171818	17.334823
36.801558	1438.069841	17.339840
36.872167	1434.528627	17.344858
36.783859	1434.435757	17.349875
36.927630	1441.784249	17.354893
36.797585	1436.064872	17.359911
37.087289	1446.113076	17.364928
37.732848	1454.377302	17.369946
37.401034	1455.543971	17.374963
37.331189	1441.002645	17.379981
37.303883	1449.319121	17.384999
37.373030	1451.683446	17.390016
37.685991	1462.156615	17.395034
37.302113	1454.899134	17.400051
37.649881	1454.445699	17.405069
37.375920	1458.956145	17.410087
37.560510	1465.946558	17.415104
37.632218	1457.051996	17.420122
37.471333	1456.247088	17.425139
37.441912	1462.850047	17.430157
37.466052	1465.770555	17.435175
37.453221	1461.992523	17.440192
37.784011	1458.980833	17.445210
37.642098	1462.633346	17.450227
37.522294	1459.842961	17.455245
37.294467	1468.237047	17.460263
37.606840	1485.750617	17.465280
37.901106	1486.428890	17.470298
37.773914	1492.371820	17.475315
38.122661	1491.666535	17.480333
38.180195	1488.261891	17.485351
38.267495	1484.026636	17.490368
38.250152	1490.774765	17.495386
38.036310	1489.045467	17.500403
38.456269	1473.903731	17.505421
38.343045	1486.966524	17.510439
38.340424	1477.556038	17.515456
38.598970	1469.642371	17.520474
38.370914	1482.070649	17.525491
38.566333	1481.263186	17.530509
38.842012	1469.526576	17.535527
38.510763	1473.521542	17.540544
38.681867	1459.136045	17.545562
37.960607	1455.181552	17.550579
38.556841	1458.253858	17.555597
38.628036	1477.190186	17.560615
38.462389	1477.451007	17.565632
38.955289	1478.458621	17.570650
38.654113	1486.077878	17.575667
38.594706	1486.464120	17.580685
38.630052	1469.947509	17.585703
38.513831	1478.942807	17.590720
38.350091	1481.232590	17.595738
38.393982	1482.512381	17.600755
38.853272	1490.173171	17.605773
38.858078	1510.091504	17.610791
39.074507	1515.573788	17.615808
39.636429	1507.924760	17.620826
39.180982	1493.500722	17.625843
39.147793	1486.134598	17.630861
38.998580	1482.401121	17.635879
39.236077	1481.786728	17.640896
39.270689	1478.679906	17.645914
39.124989	1478.230450	17.650931
39.125652	1476.142103	17.655949
39.381822	1477.978728	17.660967
39.051292	1475.964438	17.665984
39.269972	1491.563583	17.671002
39.442739	1502.944781	17.676019
39.627427	1513.478558	17.681037
39.584678	1507.071953	17.686055
39.745747	1502.972797	17.691072
39.579832	1507.327595	17.696090
39.704791	1507.522407	17.701107
39.658366	1499.304993	17.706125
39.600270	1498.935162	17.711143
39.440095	1506.889031	17.716160
39.482089	1501.206686	17.721178
39.607055	1508.769004	17.726195
39.290509	1505.240752	17.731213
39.660330	1504.584804	17.736231
39.755931	1500.072146	17.741248
39.386697	1508.738140	17.746266
39.595121	1521.432692	17.751283
39.807843	1533.761615	17.756301
40.045505	1535.360517	17.761319
39.944340	1532.608045	17.766336
40.260222	1541.124680	17.771354
40.283502	1534.283587	17.776371
40.311201	1541.651428	17.781389
40.326547	1527.153847	17.786407
40.563953	1531.599278	17.791424
40.412735	1533.360877	17.796442
40.410113	1528.870953	17.801459
40.265968	1530.983008	17.806477
40.362511	1526.272769	17.811495
40.248043	1533.838678	17.816512
40.375437	1525.426781	17.821530
40.269046	1530.593241	17.826547
40.664228	1529.637509	17.831565
40.651370	1528.359088	17.836583
40.172039	1526.751566	17.841600
40.323736	1524.558112	17.846618
40.325663	1539.001055	17.851635
40.830755	1548.599687	17.856653
41.052918	1556.465864	17.861671
40.927838	1555.515236	17.866688
40.986477	1552.896942	17.871706
40.929994	1559.920342	17.876723
40.980248	1557.709239	17.881741
41.138816	1552.483355	17.886759
41.007020	1553.099801	17.891776
41.159908	1554.021642	17.896794
40.993587	1560.218601	17.901811
41.067562	1552.809396	17.906829
41.407609	1551.772004	17.911847
40.451044	1559.985837	17.916864
41.080036	1549.105991	17.921882
41.156925	1554.498854	17.926899
41.114759	1550.896157	17.931917
41.495773	1549.275696	17.936935
41.302809	1551.567792	17.941952
41.280593	1558.319875	17.946970
41.350688	1560.480352	17.951987
41.342107	1551.492355	17.957005
41.464763	1547.800449	17.962023
41.317257	1568.529694	17.967040
42.014078	1576.630866	17.972058
41.837835	1575.723004	17.977075
41.955750	1566.917751	17.982093
41.591648	1557.961279	17.987111
41.341743	1551.836239	17.992128
41.871730	1564.303360	17.997146
42.036295	1572.129966	18.002163
42.180647	1568.769661	18.007181
41.982758	1569.914194	18.012199
42.210242	1577.101534	18.017216
42.563982	1556.550997	18.022234
42.368497	1546.674130	18.027251
42.083951	1545.072508	18.032269
42.118892	1539.009015	18.037287
42.218207	1538.708464	18.042304
42.422287	1526.017356	18.047322
42.122881	1537.091626	18.052339
41.976463	1535.265836	18.057357
42.248281	1530.619669	18.062375
42.337397	1565.449236	18.067392
42.593412	1565.070995	18.072410
42.891920	1566.718402	18.077427
42.418306	1553.977254	18.082445
42.433043	1540.402369	18.087463
42.076263	1568.311499	18.092480
42.537189	1563.673702	18.097498
42.191245	1570.245390	18.102515
41.969373	1575.754337	18.107533
42.529982	1567.654013	18.112551
42.610284	1567.877971	18.117568
42.502405	1577.755285	18.122586
42.951443	1589.902631	18.127603
43.069674	1596.607164	18.132621
43.175111	1591.951331	18.137639
42.760733	1605.055180	18.142656
43.225616	1594.426424	18.147674
43.463822	1598.898491	18.152691
43.043320	1595.454438	18.157709
43.276643	1585.189034	18.162727
42.969939	1585.182119	18.167744
43.052147	1592.357241	18.172762
43.066646	1586.522727	18.177779
42.765564	1603.823591	18.182797
43.147895	1594.066121	18.187815
42.923416	1597.373171	18.192832
43.271604	1593.846640	18.197850
43.108212	1596.830117	18.202867
42.877273	1598.857705	18.207885
43.336727	1606.293581	18.212903
43.435951	1627.039404	18.217920
43.602789	1627.734861	18.222938
43.949696	1615.083034	18.227955
44.227752	1610.829905	18.232973
44.453475	1609.621184	18.237991
44.396795	1589.885631	18.243008
44.201178	1569.136386	18.248026
44.403791	1570.968194	18.253043
44.166098	1572.158401	18.258061
44.421550	1568.948698	18.263079
44.012104	1569.655831	18.268096
44.386866	1572.601457	18.273114
44.357837	1568.769349	18.278131
44.194569	1565.414845	18.283149
44.249489	1545.066928	18.288167
43.750493	1551.100639	18.293184
44.393060	1557.797827	18.298202
44.686847	1562.914635	18.303219
44.160046	1565.572230	18.308237
44.246511	1556.459742	18.313255
44.453062	1574.462222	18.318272
44.179408	1571.108017	18.323290
44.033451	1567.349616	18.328307
44.267992	1571.228419	18.333325
44.360467	1561.617875	18.338343
44.032061	1574.814169	18.343360
44.299208	1574.791243	18.348378
44.498274	1590.606776	18.353395
44.369960	1603.159255	18.358413
44.587016	1601.557072	18.363431
44.506891	1613.652757	18.368448
44.630016	1606.795707	18.373466
44.612780	1606.001702	18.378483
44.298412	1611.453839	18.383501
44.660267	1622.888350	18.388519
44.992094	1633.088849	18.393536
44.996924	1632.066372	18.398554
45.152512	1625.213574	18.403571
44.733033	1632.511200	18.408589
45.543892	1627.727123	18.413607
45.163479	1634.861210	18.418624
45.101368	1644.260129	18.423642
45.203121	1641.499658	18.428659
45.163590	1641.281026	18.433677
45.361937	1634.822542	18.438695
45.220839	1642.147352	18.443712
45.317458	1644.706324	18.448730
45.439547	1656.636869	18.453747
45.492922	1665.687035	18.458765
45.574354	1666.661181	18.463783
45.767768	1675.056635	18.468800
45.623977	1676.622789	18.473818
45.683622	1674.943451	18.478835
45.657619	1671.445116	18.483853
45.712593	1669.462916	18.488871
45.555410	1680.253479	18.493888
46.076632	1674.051813	18.498906
46.047572	1667.806556	18.503923
45.705260	1675.010095	18.508941
46.109648	1665.049277	18.513959
46.124270	1665.177527	18.518976
45.832873	1666.564291	18.523994
46.190108	1667.787834	18.529011
45.990768	1662.513592	18.534029
46.160406	1671.270715	18.539047
46.266588	1669.178884	18.544064
46.255330	1681.463426	18.549082
46.558568	1682.106456	18.554099
46.443944	1691.129945	18.559117
46.146831	1683.960762	18.564135
46.169349	1693.031597	18.569152
46.373103	1695.599448	18.574170
46.627619	1686.436481	18.579187
46.487860	1700.339799	18.584205
46.656314	1696.133227	18.589223
46.860512	1702.949161	18.594240
46.598297	1699.473546	18.599258
46.800171	1698.742911	18.604275
46.737355	1693.219572	18.609293
47.064869	1689.057639	18.614311
46.804988	1684.503297	18.619328
46.876079	1686.389130	18.624346
47.064301	1684.207131	18.629363
46.880332	1696.225060	18.634381
47.222258	1704.660557	18.639399
47.216511	1717.203812	18.644416
47.404646	1723.763542	18.649434
47.731666	1714.202012	18.654451
47.238782	1707.264609	18.659469
47.409496	1692.255997	18.664487
47.546495	1691.437390	18.669504
47.186994	1698.852903	18.674522
47.285280	1705.037612	18.679539
47.449935	1713.967809	18.684557
47.785475	1706.255678	18.689575
47.639942	1711.687219	18.694592
47.666696	1715.570097	18.699610
48.030173	1713.493858	18.704627
47.751313	1714.326469	18.709645
47.945706	1713.864453	18.714663
47.666488	1706.631840	18.719680
47.609012	1705.315686	18.724698
47.814480	1707.750339	18.729715
47.545612	1714.352272	18.734733
47.839062	1707.691391	18.739751
47.764073	1705.854188	18.744768
47.745094	1719.999397	18.749786
48.107526	1723.195570	18.754803
48.011455	1739.771735	18.759821
48.456678	1741.741061	18.764839
48.640348	1732.930727	18.769856
48.421506	1747.360320	18.774874
48.754955	1735.441242	18.779891
48.691840	1731.599583	18.784909
48.468590	1712.124821	18.789927
48.289674	1714.022998	18.794944
48.241390	1718.457418	18.799962
48.799440	1731.492031	18.804979
48.740426	1738.653567	18.809997
48.364449	1750.120900	18.815015
48.705625	1740.022241	18.820032
48.299760	1742.662153	18.825050
48.638990	1736.741182	18.830067
48.772340	1735.304139	18.835085
48.886827	1736.619886	18.840103
48.844009	1740.151267	18.845120
48.789397	1743.103267	18.850138
48.820037	1736.179890	18.855155
49.028962	1754.286827	18.860173
49.396941	1766.300950	18.865191
49.508135	1754.160886	18.870208
49.297671	1763.272854	18.875226
49.644158	1759.888921	18.880243
49.229757	1748.402148	18.885261
49.229892	1750.801911	18.890279
49.321495	1757.276373	18.895296
49.438132	1755.337026	18.900314
49.883924	1751.530612	18.905331
49.885758	1761.197061	18.910349
49.545134	1763.368012	18.915367
49.653298	1760.737850	18.920384
49.632775	1760.003352	18.925402
49.776820	1755.891110	18.930419
49.701963	1760.001788	18.935437
49.901553	1757.818752	18.940455
50.181533	1761.737554	18.945472
49.684151	1766.520476	18.950490
50.046763	1759.613362	18.955507
50.031385	1759.691339	18.960525
49.878105	1760.870459	18.965543
50.172504	1754.011194	18.970560
50.166138	1755.193626	18.975578
50.005214	1764.264658	18.980595
49.820420	1760.308683	18.985613
50.058161	1765.502144	18.990631
49.989651	1762.456542	18.995648
49.925911	1779.237606	19.000666
50.128600	1783.429876	19.005683
50.295179	1779.610564	19.010701
50.051191	1780.483237	19.015719
50.564106	1786.895241	19.020736
50.557536	1803.145729	19.025754
51.131793	1795.327838	19.030771
51.366835	1793.546578	19.035789
51.019269	1785.322755	19.040807
51.208937	1776.039507	19.045824
50.756215	1780.791715	19.050842
50.976127	1773.647790	19.055859
51.325241	1765.059603	19.060877
51.109991	1761.741658	19.065895
51.216266	1773.044794	19.070912
50.775101	1782.424025	19.075930
51.005303	1764.607293	19.080947
51.243460	1779.014375	19.085965
51.101763	1778.628767	19.090983
51.425029	1785.838691	19.096000
51.162737	1803.372718	19.101018
51.380421	1804.523355	19.106035
51.272575	1798.353531	19.111053
51.287920	1796.157399	19.116071
51.417688	1806.300578	19.121088
51.290849	1803.079429	19.126106
51.512454	1804.441024	19.131123
51.551712	1807.827977	19.136141
51.563471	1801.226135	19.141159
51.841505	1816.706048	19.146176
51.498336	1833.794446	19.151194
51.779586	1830.874745	19.156211
51.977814	1831.989947	19.161229
51.671783	1837.082954	19.166247
52.042430	1829.078853	19.171264
51.881818	1829.064368	19.176282
52.121712	1832.232129	19.181299
52.259796	1828.547917	19.186317
52.053677	1832.299642	19.191335
52.386757	1825.872287	19.196352
52.185288	1838.568776	19.201370
52.315423	1848.155830	19.206387
52.689338	1854.881059	19.211405
52.556797	1860.297997	19.216423
52.831163	1859.202629	19.221440
52.922227	1859.118905	19.226458
52.629036	1843.523412	19.231475
52.971267	1840.451617	19.236493
52.509210	1849.499935	19.241511
52.765689	1845.987971	19.246528
52.502466	1862.469803	19.251546
52.886744	1858.412821	19.256563
53.025759	1857.007112	19.261581
52.548817	1860.322234	19.266599
52.886811	1856.289937	19.271616
53.234521	1853.527170	19.276634
52.993642	1854.599136	19.281651
52.914831	1853.629310	19.286669
52.714699	1856.918377	19.291687
53.346888	1867.108110	19.296704
53.415308	1880.425449	19.301722
53.349181	1882.374878	19.306739
53.369648	1884.717148	19.311757
53.187478	1878.006978	19.316775
53.723158	1886.842717	19.321792
53.409728	1879.771212	19.326810
53.691679	1880.715754	19.331827
53.493796	1871.985063	19.336845
53.658819	1884.060754	19.341863
53.880560	1881.531228	19.346880
53.744298	1875.366689	19.351898
53.883991	1877.854336	19.356915
53.739395	1870.788158	19.361933
53.702398	1890.094657	19.366951
53.981646	1891.443922	19.371968
53.857648	1907.283792	19.376986
54.222304	1903.445444	19.382003
54.037951	1906.192426	19.387021
53.859471	1913.568953	19.392039
54.582601	1900.356629	19.397056
54.191581	1903.845259	19.402074
54.165738	1908.711125	19.407091
54.560950	1906.543277	19.412109
54.352744	1907.302492	19.417127
54.503352	1896.943876	19.422144
54.288036	1908.476952	19.427162
54.404064	1920.993882	19.432179
54.679022	1921.468392	19.437197
54.535757	1939.441377	19.442215
54.697865	1927.647003	19.447232
54.901881	1938.447011	19.452250
54.706182	1932.556211	19.457267
54.886088	1927.001154	19.462285
54.688154	1936.794753	19.467303
54.824382	1946.995206	19.472320
55.501047	1943.927474	19.477338
56.026344	1940.220811	19.482355
56.286851	1926.927289	19.487373
55.933303	1928.976834	19.492391
55.721520	1916.705660	19.497408
55.837792	1915.326382	19.502426
55.750448	1911.293472	19.507443
55.912940	1903.839297	19.512461
55.591403	1901.665412	19.517479
55.571961	1893.142219	19.522496
55.772436	1898.241779	19.527514
55.666503	1902.695673	19.532531
55.722879	1905.976093	19.537549
55.695479	1920.579831	19.542567
55.955070	1913.592329	19.547584
56.150301	1915.569299	19.552602
55.806111	1913.280253	19.557619
56.097566	1913.359638	19.562637
55.797956	1912.399064	19.567655
56.112098	1907.621752	19.572672
56.105114	1907.281514	19.577690
55.917159	1911.790966	19.582707
56.060364	1913.880845	19.587725
55.747112	1918.832664	19.592743
56.441979	1930.009019	19.597760
56.505592	1938.313635	19.602778
56.630420	1953.490130	19.607795
56.629721	1941.167182	19.612813
56.776800	1950.917567	19.617831
56.605407	1941.400766	19.622848
56.554227	1950.218443	19.627866
56.433523	1943.844528	19.632883
56.830731	1946.041778	19.637901
56.704940	1953.525548	19.642919
56.809091	1945.914691	19.647936
56.670438	1947.057670	19.652954
56.788256	1954.406629	19.657971
57.144046	1962.784221	19.662989
57.016916	1973.525373	19.668007
57.097266	1973.690338	19.673024
57.229889	1970.906791	19.678042
56.873460	1979.777885	19.683059
57.222378	1967.820757	19.688077
57.321477	1978.935635	19.693095
57.238393	1978.285040	19.698112
57.476353	1981.938453	19.703130
57.292751	2000.759570	19.708147
57.302939	2006.377972	19.713165
57.190446	2006.009723	19.718183
57.316264	2003.699195	19.723200
57.385860	2006.628294	19.728218
57.522364	2021.334204	19.733235
58.202978	2023.373005	19.738253
57.985658	2033.014806	19.743271
57.749476	2044.176123	19.748288
58.077392	2033.296743	19.753306
58.141727	2033.128398	19.758323
58.300782	2025.966526	19.763341
58.308006	2031.155158	19.768359
58.525217	2015.823386	19.773376
58.168918	2026.951146	19.778394
58.176445	2034.141543	19.783411
58.442575	2025.864548	19.788429
58.311739	2026.230731	19.793447
58.526916	2044.727169	19.798464
58.792450	2055.802192	19.803482
59.115293	2052.613101	19.808499
59.129045	2049.141371	19.813517
58.874601	2033.854121	19.818535
58.912938	2026.339454	19.823552
59.091365	2018.115778	19.828570
58.905726	2021.570895	19.833587
59.015218	2007.099509	19.838605
59.018428	2028.210453	19.843623
59.421087	2043.070582	19.848640
59.350124	2042.501428	19.853658
59.413344	2046.484766	19.858675
59.529961	2018.759356	19.863693
59.161990	2018.050365	19.868711
59.318792	2033.982454	19.873728
59.608497	2037.955628	19.878746
59.578719	2046.322393	19.883763
59.503136	2049.064639	19.888781
59.706273	2053.828752	19.893799
59.405162	2051.440785	19.898816
59.470594	2038.542453	19.903834
59.469797	2047.275856	19.908851
60.023128	2052.773836	19.913869
59.532450	2051.033556	19.918887
59.575929	2051.718818	19.923904
60.143516	2062.674885	19.928922
59.928623	2078.474376	19.933939
60.344398	2083.304483	19.938957
60.266169	2070.376332	19.943975
60.023326	2078.095138	19.948992
60.350925	2067.703456	19.954010
59.903084	2074.851654	19.959027
60.472690	2082.753166	19.964045
60.454444	2076.105644	19.969063
60.261658	2078.087097	19.974080
60.439982	2089.700695	19.979098
60.679783	2101.643511	19.984115
61.253883	2083.060489	19.989133
61.336790	2086.733937	19.994151
61.396182	2080.529456	19.999168
61.619074	2059.056770	20.004186
60.925484	2053.573320	20.009203
61.105760	2051.161285	20.014221
61.090722	2051.954199	20.019239
61.223651	2052.402597	20.024256
61.351024	2045.281164	20.029274
61.247520	2048.509242	20.034291
61.382856	2044.081322	20.039309
61.398499	2045.124977	20.044327
61.374655	2053.109315	20.049344
61.503431	2066.001104	20.054362
61.610954	2077.886338	20.059379
61.860166	2078.032241	20.064397
62.158965	2078.075062	20.069415
61.907930	2061.302195	20.074432
62.169162	2055.538264	20.079450
61.826732	2054.247070	20.084467
62.077676	2037.011120	20.089485
61.918041	2046.567433	20.094503
62.058193	2059.443244	20.099520
62.176269	2055.338993	20.104538
62.001705	2076.446108	20.109555
62.115112	2074.496223	20.114573
62.321218	2072.308956	20.119591
62.204732	2084.135531	20.124608
62.449559	2073.707491	20.129626
62.295030	2089.056889	20.134643
62.168589	2076.608363	20.139661
62.386349	2077.672489	20.144679
62.502104	2082.005348	20.149696
62.329242	2073.474267	20.154714
62.168091	2095.166837	20.159731
62.512431	2100.005982	20.164749
62.665166	2104.887483	20.169767
62.628585	2116.179844	20.174784
62.856258	2110.835767	20.179802
62.761395	2112.038634	20.184819
62.870144	2109.768566	20.189837
63.315617	2127.423722	20.194855
62.896754	2144.769178	20.199872
63.410470	2138.975176	20.204890
63.685227	2139.780087	20.209907
63.567183	2140.436052	20.214925
63.333171	2134.766013	20.219943
63.542917	2133.216854	20.224960
63.671381	2136.744613	20.229978
63.518994	2134.086717	20.234995
63.610204	2132.561967	20.240013
63.881306	2135.215906	20.245031
63.509736	2135.021901	20.250048
63.833467	2134.193156	20.255066
63.988313	2134.649074	20.260083
64.060787	2135.682886	20.265101
63.903795	2133.852413	20.270119
63.743573	2133.224337	20.275136
64.529653	2141.561731	20.280154
64.367495	2158.627148	20.285171
64.367438	2153.939192	20.290189
64.263208	2149.654059	20.295207
64.037585	2159.559982	20.300224
64.290036	2152.346972	20.305242
64.253024	2158.142072	20.310259
64.349333	2155.042573	20.315277
64.451575	2161.403825	20.320295
64.552544	2181.992848	20.325312
64.916218	2169.846785	20.330330
64.828658	2180.892476	20.335347
64.625124	2181.929406	20.340365
65.030636	2180.192494	20.345383
65.011045	2176.811788	20.350400
64.977056	2179.257180	20.355418
64.968290	2174.235525	20.360435
65.151045	2169.306036	20.365453
65.272768	2181.819924	20.370471
65.162970	2199.498433	20.375488
65.725859	2196.702075	20.380506
65.645639	2200.315042	20.385523
65.611979	2203.491114	20.390541
65.851229	2201.522717	20.395559
65.782265	2201.610815	20.400576
65.999667	2192.156913	20.405594
65.565973	2203.673132	20.410611
65.891548	2197.597627	20.415629
65.850978	2186.644752	20.420647
65.813107	2202.351648	20.425664
65.957819	2196.024178	20.430682
66.058121	2196.716116	20.435699
65.928147	2210.524756	20.440717
66.160817	2195.157294	20.445735
65.881328	2198.115358	20.450752
66.304426	2214.017764	20.455770
66.102329	2221.483948	20.460787
66.362352	2227.403968	20.465805
66.527411	2223.458145	20.470823
66.248479	2232.951801	20.475840
66.520240	2227.236465	20.480858
66.732241	2223.507331	20.485875
66.466298	2224.389035	20.490893
66.706819	2236.486803	20.495911
66.692818	2254.157180	20.500928
67.118364	2251.595091	20.505946
67.017610	2256.799449	20.510963
67.385026	2253.755018	20.515981
67.413110	2255.629692	20.520999
67.143882	2259.026616	20.526016
67.317005	2246.555343	20.531034
67.250121	2253.330603	20.536051
67.210455	2248.385429	20.541069
67.282402	2246.531017	20.546087
67.533660	2271.884106	20.551104
67.960291	2270.142243	20.556122
68.229917	2277.507273	20.561139
68.197378	2267.913840	20.566157
68.217095	2256.636667	20.571175
68.205014	2259.096669	20.576192
68.258306	2247.377597	20.581210
68.181532	2243.308299	20.586227
67.996126	2247.620802	20.591245
68.139477	2240.898668	20.596263
68.229312	2245.153119	20.601280
68.442350	2259.537154	20.606298
68.153800	2271.296930	20.611315
68.402205	2271.454763	20.616333
68.632887	2271.406193	20.621351
68.266622	2284.064061	20.626368
68.557591	2264.011795	20.631386
68.351455	2270.211469	20.636403
68.510199	2268.459626	20.641421
68.702504	2267.517329	20.646439
68.787171	2291.901209	20.651456
68.794379	2293.426829	20.656474
68.729002	2299.147064	20.661491
68.869275	2304.471892	20.666509
69.068833	2290.080253	20.671527
69.311139	2300.712390	20.676544
69.206559	2293.260492	20.681562
69.506373	2291.789771	20.686579
69.185504	2295.933538	20.691597
69.197640	2296.142422	20.696615
69.483708	2314.268431	20.701632
69.607350	2322.652578	20.706650
70.058565	2325.493354	20.711667
69.932090	2331.534045	20.716685
70.078578	2320.062772	20.721703
69.584937	2336.286126	20.726720
70.006409	2336.220502	20.731738
70.109187	2327.015262	20.736755
69.776560	2328.060989	20.741773
70.212835	2326.478832	20.746791
70.119280	2333.071962	20.751808
70.018224	2337.499253	20.756826
70.176717	2329.979427	20.761843
70.130736	2334.603232	20.766861
70.217000	2327.049304	20.771879
70.093957	2343.879017	20.776896
70.433927	2349.222357	20.781914
70.434243	2345.199731	20.786931
70.510894	2352.210147	20.791949
70.766836	2350.795184	20.796967
71.060188	2367.732357	20.801984
70.775646	2373.409699	20.807002
70.776303	2381.170851	20.812019
70.647621	2383.175157	20.817037
71.032724	2381.637338	20.822055
71.017773	2392.136731	20.827072
71.332306	2383.131303	20.832090
71.469362	2382.263096	20.837107
71.512815	2396.524859	20.842125
71.805718	2404.303919	20.847143
71.410422	2406.812472	20.852160
71.504544	2405.804018	20.857178
71.551327	2405.179888	20.862195
71.713564	2412.901131	20.867213
71.704052	2401.628507	20.872231
71.472973	2413.631726	20.877248
71.664115	2413.228418	20.882266
72.060197	2429.502705	20.887283
72.221874	2442.992895	20.892301
72.177455	2439.098511	20.897319
72.745667	2441.811318	20.902336
72.633623	2435.824380	20.907354
72.823217	2440.228950	20.912371
72.494776	2441.072650	20.917389
72.998305	2432.317865	20.922407
72.627455	2434.684085	20.927424
72.542860	2433.848075	20.932442
72.840037	2429.005655	20.937459
72.540057	2432.237619	20.942477
72.791249	2431.875075	20.947495
72.784038	2436.797927	20.952512
72.722680	2430.275894	20.957530
73.037954	2426.304489	20.962547
72.711261	2446.639584	20.967565
73.166018	2445.360451	20.972583
73.495589	2456.629296	20.977600
73.526211	2462.040887	20.982618
73.466016	2457.447376	20.987635
73.193892	2463.983303	20.992653
73.489078	2452.318310	20.997671
73.649580	2452.832331	21.002688
73.649432	2448.281162	21.007706
73.588286	2448.819516	21.012723
73.672434	2459.234721	21.017741
74.215403	2470.683499	21.022759
74.202053	2473.835939	21.027776
74.071155	2484.111618	21.032794
74.232296	2481.198360	21.037811
74.047929	2482.693196	21.042829
74.375583	2480.879782	21.047847
74.185382	2485.064118	21.052864
74.328247	2484.009343	21.057882
74.383854	2478.628072	21.062899
74.292211	2484.778901	21.067917
74.440669	2482.631445	21.072935
75.264878	2500.949538	21.077952
74.743023	2511.918429	21.082970
75.486698	2491.121123	21.087987
75.382755	2497.456408	21.093005
75.186418	2482.644746	21.098023
75.099232	2473.431950	21.103040
75.218882	2482.951876	21.108058
75.484188	2493.195057	21.113075
75.021218	2504.738203	21.118093
75.334185	2509.189980	21.123111
75.564331	2505.052787	21.128128
75.443878	2516.721452	21.133146
75.457356	2506.288309	21.138163
75.430682	2512.406764	21.143181
75.322229	2502.204661	21.148199
75.690097	2519.421954	21.153216
75.668657	2524.990538	21.158234
75.815546	2526.451431	21.163251
75.803578	2532.431469	21.168269
76.216537	2525.613509	21.173287
76.458278	2533.430688	21.178304
76.352463	2533.991114	21.183322
76.561574	2524.824640	21.188339
76.524105	2526.387300	21.193357
76.535381	2525.440031	21.198375
76.649706	2522.118122	21.203392
76.569128	2536.104042	21.208410
76.589893	2524.470167	21.213427
76.760962	2537.270678	21.218445
76.904902	2540.741005	21.223463
76.989347	2545.790078	21.228480
77.050714	2551.364345	21.233498
77.144699	2544.418684	21.238515
77.379854	2543.766083	21.243533
77.156890	2543.460272	21.248551
77.620025	2540.581436	21.253568
77.231924	2543.233597	21.258586
77.402356	2544.700177	21.263603
77.466426	2541.257276	21.268621
77.577472	2551.515659	21.273639
77.618278	2543.958642	21.278656
77.369266	2542.525862	21.283674
77.621238	2552.067208	21.288691
77.560265	2574.480767	21.293709
77.875211	2575.944757	21.298727
78.384356	2575.932801	21.303744
78.129183	2583.832395	21.308762
78.230962	2576.150009	21.313779
78.240494	2574.155269	21.318797
78.188224	2582.152294	21.323815
78.339308	2572.342170	21.328832
78.201941	2569.042295	21.333850
78.189982	2578.697328	21.338867
78.428894	2600.646995	21.343885
78.501746	2597.431581	21.348903
78.764075	2593.742311	21.353920
78.785479	2610.663352	21.358938
78.908631	2598.890382	21.363955
78.626875	2610.164014	21.368973
78.987976	2620.425832	21.373991
79.270452	2625.577861	21.379008
79.301799	2631.123122	21.384026
79.482902	2627.494779	21.389043
79.396052	2622.689938	21.394061
79.352381	2623.807595	21.399079
79.764638	2621.761214	21.404096
79.392536	2617.384936	21.409114
79.627197	2626.097657	21.414131
79.813196	2632.275067	21.419149
79.954601	2639.591508	21.424167
80.088903	2644.140253	21.429184
80.034913	2655.972268	21.434202
80.023316	2647.857202	21.439219
80.623201	2649.377233	21.444237
80.545905	2641.166457	21.449255
80.602224	2638.398885	21.454272
80.371285	2645.248470	21.459290
80.676275	2637.203275	21.464307
80.664786	2639.995978	21.469325
80.566411	2645.270102	21.474343
80.918786	2638.009457	21.479360
80.594172	2639.173489	21.484378
80.927494	2636.177681	21.489395
80.660901	2645.382525	21.494413
80.510463	2640.970893	21.499431
80.850403	2655.011004	21.504448
81.099764	2673.438290	21.509466
81.138263	2665.688862	21.514483
81.031566	2674.960258	21.519501
81.035933	2669.720024	21.524519
81.116737	2677.830390	21.529536
80.812440	2698.645235	21.534554
81.350198	2704.503070	21.539571
81.428125	2699.751375	21.544589
81.291490	2710.098134	21.549607
81.637470	2723.600098	21.554624
82.055447	2735.040700	21.559642
81.999722	2734.738106	21.564659
82.216562	2724.944925	21.569677
82.215571	2740.124213	21.574695
82.198118	2732.271186	21.579712
82.297203	2732.365526	21.584730
82.613136	2732.349771	21.589747
82.741988	2732.859411	21.594765
82.499413	2732.730562	21.599783
82.727032	2729.978134	21.604800
82.808384	2752.020803	21.609818
82.889545	2755.901575	21.614835
82.998571	2755.696993	21.619853
83.040146	2755.587333	21.624871
83.535540	2744.456539	21.629888
83.216432	2760.643088	21.634906
83.287132	2757.000068	21.639923
83.516281	2754.392914	21.644941
83.232196	2753.187527	21.649959
83.421005	2736.662316	21.654976
83.359152	2748.106291	21.659994
83.328461	2748.007368	21.665011
83.594985	2762.580810	21.670029
83.611180	2777.553665	21.675047
84.048325	2780.874249	21.680064
83.791814	2787.093971	21.685082
83.699016	2774.073913	21.690099
83.972564	2781.696582	21.695117
84.081773	2795.978140	21.700135
84.290191	2807.561556	21.705152
84.117093	2806.722331	21.710170
84.420158	2804.068770	21.715187
84.786876	2810.765704	21.720205
84.662497	2807.459771	21.725223
85.275683	2807.311662	21.730240
84.972153	2817.110100	21.735258
85.076038	2811.164876	21.740275
85.458251	2799.307956	21.745293
85.380323	2796.970799	21.750311
85.290835	2798.615724	21.755328
84.972848	2808.176546	21.760346
85.525712	2804.704408	21.765363
85.704331	2795.011668	21.770381
85.252728	2806.501321	21.775399
85.487730	2802.412827	21.780416
85.569127	2807.168285	21.785434
85.537138	2797.964574	21.790451
85.579140	2805.820044	21.795469
85.477248	2828.719562	21.800487
86.088390	2831.674957	21.805504
85.712456	2840.457643	21.810522
85.756109	2844.582763	21.815539
86.098942	2839.498520	21.820557
86.166000	2843.837013	21.825575
86.301553	2842.809337	21.830592
86.524714	2860.353742	21.835610
86.323631	2862.546645	21.840627
86.687416	2855.243170	21.845645
86.283269	2860.024155	21.850663
86.942720	2858.679312	21.855680
86.791300	2860.666070	21.860698
86.712743	2861.740538	21.865715
87.023925	2872.631132	21.870733
86.930696	2891.014212	21.875751
87.042214	2888.268469	21.880768
87.519805	2889.372246	21.885786
87.299523	2898.510081	21.890803
87.481370	2890.081638	21.895821
87.323909	2890.148454	21.900839
87.482115	2888.014331	21.905856
87.625547	2897.194852	21.910874
87.698332	2916.229550	21.915891
87.800752	2908.817484	21.920909
87.884505	2917.386895	21.925927
88.333359	2912.827698	21.930944
88.398833	2914.646939	21.935962
88.394748	2912.371929	21.940979
88.595232	2911.382665	21.945997
88.061995	2911.224648	21.951015
88.471068	2907.891835	21.956032
88.294067	2917.878616	21.961050
88.705640	2935.363175	21.966067
88.836256	2936.899861	21.971085
88.636939	2951.173347	21.976103
89.058372	2940.188712	21.981120
89.106484	2940.019799	21.986138
88.985547	2929.031199	21.991155
89.292028	2937.210341	21.996173
89.530171	2938.215435	22.001191
89.631709	2927.220464	22.006208
89.612538	2941.650069	22.011226
89.401424	2935.660631	22.016243
89.717183	2924.863553	22.021261
89.220909	2935.124657	22.026279
89.436023	2945.186586	22.031296
89.880210	2955.089282	22.036314
90.024086	2958.680073	22.041331
89.728882	2952.155765	22.046349
89.685568	2962.570416	22.051367
89.856882	2955.343207	22.056384
89.940024	2973.450482	22.061402
90.164729	2986.206650	22.066419
90.502673	2987.316184	22.071437
90.318159	2995.151241	22.076455
90.420088	2990.945470	22.081472
90.477110	2996.961107	22.086490
90.758353	3006.478419	22.091507
90.972320	3009.671816	22.096525
90.745933	3010.827291	22.101543
91.001239	3019.046892	22.106560
91.292411	3018.443550	22.111578
91.087322	3027.925941	22.116595
91.239776	3019.751470	22.121613
91.073621	3020.681808	22.126631
91.370440	3028.745337	22.131648
91.811346	3041.168948	22.136666
91.510905	3043.804070	22.141683
91.734363	3041.229238	22.146701
91.753289	3039.765480	22.151719
92.042008	3036.729508	22.156736
91.974569	3034.486608	22.161754
91.931774	3046.572805	22.166771
92.721133	3058.811861	22.171789
92.397192	3065.063691	22.176807
92.562931	3058.907915	22.181824
92.686062	3065.639091	22.186842
92.728919	3067.283393	22.191859
93.003321	3055.187809	22.196877
92.879272	3064.901940	22.201895
93.109736	3060.327180	22.206912
93.149069	3056.239140	22.211930
92.960059	3057.347754	22.216947
93.293121	3053.562923	22.221965
93.008956	3059.828074	22.226983
92.865797	3055.438753	22.232000
93.204274	3069.284416	22.237018
93.348304	3082.488535	22.242035
93.603432	3081.143645	22.247053
93.501149	3087.404190	22.252071
93.643787	3091.646536	22.257088
94.074686	3081.106303	22.262106
93.585401	3095.515056	22.267123
93.976235	3113.693006	22.272141
93.856068	3118.753666	22.277159
93.868839	3118.003564	22.282176
94.399633	3117.270759	22.287194
94.219168	3120.193547	22.292211
94.250561	3131.825902	22.297229
94.442009	3133.469330	22.302247
94.748306	3140.718038	22.307264
95.188373	3133.514750	22.312282
94.995542	3140.408831	22.317299
95.360902	3131.984026	22.322317
95.233539	3140.565208	22.327335
95.077249	3132.693201	22.332352
95.586854	3135.775766	22.337370
95.510788	3134.298827	22.342387
95.713316	3130.228794	22.347405
96.031783	3135.035445	22.352423
95.697352	3125.182804	22.357440
95.853254	3130.245857	22.362458
95.718757	3136.101728	22.367475
95.953746	3125.909713	22.372493
95.981526	3122.103536	22.377511
96.029486	3117.247143	22.382528
96.107210	3128.807604	22.387546
96.188609	3124.958264	22.392563
96.412023	3140.917128	22.397581
95.951716	3154.467828	22.402599
96.240772	3155.855772	22.407616
96.362950	3150.504544	22.412634
96.320175	3163.789656	22.417651
96.413414	3162.915806	22.422669
96.566590	3180.722690	22.427687
96.557665	3193.159951	22.432704
96.595294	3186.734283	22.437722
96.864010	3206.641168	22.442739
97.087341	3210.424662	22.447757
97.222005	3205.839174	22.452775
97.469653	3213.378884	22.457792
97.711861	3205.786265	22.462810
97.799156	3218.839868	22.467827
97.737186	3223.069255	22.472845
98.421974	3232.634069	22.477863
98.128805	3234.071597	22.482880
98.553192	3234.648979	22.487898
98.484860	3233.753690	22.492915
98.403727	3232.568603	22.497933
98.541683	3225.458283	22.502951
98.484153	3241.414072	22.507968
98.789274	3238.155974	22.512986
98.361956	3249.690868	22.518003
98.512017	3241.463952	22.523021
98.658633	3247.069730	22.528039
98.554864	3243.271911	22.533056
99.110008	3251.195256	22.538074
99.032415	3264.331831	22.543091
99.123634	3259.139681	22.548109
99.121814	3265.733547	22.553127
99.030631	3260.091422	22.558144
99.461578	3256.884839	22.563162
99.311552	3276.422010	22.568179
99.615016	3284.288750	22.573197
99.641285	3296.306716	22.578215
99.855043	3294.917274	22.583232
99.784021	3295.635013	22.588250
99.771543	3299.924180	22.593267
99.845685	3300.922412	22.598285
99.844395	3314.095636	22.603303
99.678880	3327.572741	22.608320
99.904181	3325.917932	22.613338
99.982088	3340.895681	22.618355
100.422210	3353.321258	22.623373
100.392312	3361.858708	22.628391
100.637064	3357.800760	22.633408
100.810655	3353.296336	22.638426
100.884973	3371.252902	22.643443
101.211509	3372.464978	22.648461
101.266109	3369.854084	22.653479
101.226707	3380.487881	22.658496
101.577788	3375.269198	22.663514
101.522092	3383.523651	22.668531
101.704191	3374.741691	22.673549
101.671602	3371.361994	22.678567
101.638646	3379.610459	22.683584
102.062977	3401.206096	22.688602
102.017428	3415.000047	22.693619
102.052081	3409.394437	22.698637
102.276203	3410.762082	22.703655
102.237937	3406.141176	22.708672
102.480332	3403.199048	22.713690
102.328292	3399.946948	22.718707
102.484618	3417.912521	22.723725
102.971210	3425.149928	22.728743
103.241483	3424.261993	22.733760
103.396933	3414.030544	22.738778
103.292816	3431.671088	22.743795
103.310484	3416.120307	22.748813
103.707254	3415.504832	22.753831
103.482630	3423.798831	22.758848
103.544143	3416.867376	22.763866
103.644233	3426.536567	22.768883
103.749941	3421.541855	22.773901
103.795955	3419.639514	22.778919
103.528850	3419.707293	22.783936
103.600133	3413.966831	22.788954
103.365531	3439.839157	22.793971
103.908417	3451.602598	22.798989
103.932285	3452.494795	22.804007
104.085269	3464.454935	22.809024
104.406239	3467.961762	22.814042
104.396697	3476.412648	22.819059
104.349758	3484.931647	22.824077
104.801635	3488.181612	22.829095
104.661856	3486.031988	22.834112
105.149659	3497.598149	22.839130
104.953571	3511.865370	22.844147
105.135072	3515.071136	22.849165
105.430980	3506.108114	22.854183
105.363375	3511.488558	22.859200
105.788920	3504.194583	22.864218
105.643719	3511.490299	22.869235
105.783315	3501.905581	22.874253
106.029628	3496.728735	22.879271
106.115077	3503.977442	22.884288
106.175442	3500.017294	22.889306
105.999956	3501.522613	22.894323
105.991127	3495.359878	22.899341
106.145739	3496.245389	22.904359
105.727415	3521.185873	22.909376
106.533324	3530.623015	22.914394
106.612122	3527.032792	22.919411
106.527957	3529.204002	22.924429
106.716890	3533.454042	22.929447
106.324147	3543.011525	22.934464
106.757946	3555.206222	22.939482
106.818485	3569.438085	22.944499
106.830028	3570.550156	22.949517
107.292606	3574.825012	22.954535
106.813729	3586.925339	22.959552
107.404538	3591.308763	22.964570
107.681112	3594.423081	22.969587
107.660793	3588.444643	22.974605
107.745716	3592.800176	22.979623
107.919960	3611.928160	22.984640
108.102331	3611.360238	22.989658
108.087402	3618.130203	22.994675
108.289168	3623.857129	22.999693
108.530727	3614.817750	23.004711
108.171927	3618.461325	23.009728
108.469950	3627.221183	23.014746
108.756022	3638.095116	23.019763
108.765318	3643.841727	23.024781
108.810191	3649.822597	23.029799
108.965546	3648.355903	23.034816
109.119014	3648.517884	23.039834
109.031309	3651.129416	23.044851
109.372992	3666.333688	23.049869
109.635544	3672.244458	23.054887
109.491363	3677.988022	23.059904
109.328994	3685.450972	23.064922
109.647154	3677.238701	23.069939
109.781189	3676.086920	23.074957
110.086332	3683.907983	23.079975
110.198198	3701.581277	23.084992
110.323888	3698.309212	23.090010
110.541610	3703.243822	23.095027
110.290843	3704.375703	23.100045
110.595911	3702.468203	23.105063
110.291114	3706.716782	23.110080
110.589742	3699.804024	23.115098
110.837951	3706.531285	23.120115
111.005748	3725.591219	23.125133
111.200808	3725.490119	23.130151
111.015251	3739.783415	23.135168
111.375690	3727.808866	23.140186
111.365884	3729.278349	23.145203
111.249581	3727.231932	23.150221
111.614279	3727.261114	23.155239
111.520024	3733.641012	23.160256
111.664308	3737.880924	23.165274
111.660864	3749.396605	23.170291
111.587553	3764.648271	23.175309
111.712770	3760.864152	23.180327
111.853937	3769.826105	23.185344
112.329659	3782.512264	23.190362
112.419216	3797.077199	23.195379
112.418052	3803.907987	23.200397
112.734780	3791.725598	23.205415
112.304223	3793.335337	23.210432
112.426608	3812.299572	23.215450
113.085785	3804.187041	23.220467
112.896677	3811.552839	23.225485
113.049116	3802.208170	23.230503
113.358349	3814.916972	23.235520
113.547095	3833.002176	23.240538
113.971469	3837.365803	23.245555
113.631669	3849.112981	23.250573
113.993267	3842.774608	23.255591
113.796270	3847.326996	23.260608
114.046767	3840.753821	23.265626
114.025616	3844.648051	23.270643
113.545492	3847.527509	23.275661
113.887095	3857.949859	23.280679
114.227529	3870.145548	23.285696
114.250553	3867.398002	23.290714
114.454766	3882.966618	23.295731
114.459702	3905.164808	23.300749
115.016444	3889.852463	23.305767
115.116453	3904.579464	23.310784
115.033657	3903.438640	23.315802
115.101208	3892.287101	23.320819
115.607750	3921.047951	23.325837
115.663032	3917.412610	23.330855
115.808931	3925.364608	23.335872
115.656295	3920.529708	23.340890
116.076829	3915.957419	23.345907
115.997266	3927.143175	23.350925
116.019466	3920.722794	23.355943
115.962452	3934.656728	23.360960
115.720224	3931.447996	23.365978
116.197265	3945.848240	23.370995
116.241877	3952.228116	23.376013
116.408395	3957.239418	23.381031
116.480935	3964.370050	23.386048
116.861008	3984.193371	23.391066
117.190816	3973.124247	23.396083
117.117754	3990.455280	23.401101
117.393458	3969.079156	23.406119
117.448226	3979.758944	23.411136
117.632220	3985.365339	23.416154
117.493464	3979.184571	23.421171
117.364492	3985.250725	23.426189
117.429868	3976.166057	23.431207
117.678158	3995.096293	23.436224
117.745744	4008.504598	23.441242
118.044150	4009.335747	23.446259
117.950931	4011.677606	23.451277
117.984278	4006.825610	23.456295
118.278004	4018.439652	23.461312
118.246142	4034.868933	23.466330
118.573988	4036.623665	23.471347
118.551194	4041.774529	23.476365
118.791820	4039.096882	23.481383
118.706415	4056.671471	23.486400
118.877949	4067.622987	23.491418
119.517825	4059.270314	23.496435
119.305352	4072.492838	23.501453
119.728981	4064.479873	23.506471
119.938076	4056.668681	23.511488
119.922678	4060.456637	23.516506
120.007256	4053.043693	23.521523
119.888529	4060.809037	23.526541
120.114057	4076.089684	23.531559
120.274115	4082.284433	23.536576
119.964686	4089.826103	23.541594
120.422901	4078.632585	23.546611
120.412508	4084.681446	23.551629
120.888150	4091.384421	23.556647
121.039819	4111.520457	23.561664
121.110606	4116.389741	23.566682
121.411462	4113.519968	23.571699
121.018869	4120.321275	23.576717
121.367173	4114.469502	23.581735
121.136769	4117.940109	23.586752
121.397441	4114.428519	23.591770
121.342103	4107.363543	23.596787
121.716710	4135.488975	23.601805
121.740423	4137.851543	23.606823
121.727942	4145.833635	23.611840
121.792924	4143.502581	23.616858
121.843093	4152.540639	23.621875
121.766112	4172.114552	23.626893
121.878232	4178.345307	23.631911
122.226272	4187.660791	23.636928
122.213642	4202.021363	23.641946
122.717736	4205.001201	23.646963
122.605311	4215.521375	23.651981
122.516249	4215.252385	23.656999
123.178197	4227.627606	23.662016
123.414553	4233.894430	23.667034
123.638327	4225.999781	23.672051
123.447311	4232.543219	23.677069
123.635763	4225.255230	23.682087
123.632838	4240.907602	23.687104
123.774211	4250.808333	23.692122
124.007858	4248.875967	23.697139
124.147273	4248.208670	23.702157
124.180826	4251.660822	23.707175
124.548279	4237.725107	23.712192
124.209056	4249.787184	23.717210
124.423845	4253.048381	23.722227
124.646072	4283.187136	23.727245
124.683098	4278.916613	23.732263
124.942940	4287.749038	23.737280
124.665097	4292.946950	23.742298
125.145893	4288.172201	23.747315
124.967330	4310.298777	23.752333
125.083936	4310.966193	23.757351
125.081401	4310.032026	23.762368
125.134631	4330.430291	23.767386
125.353781	4343.083900	23.772403
125.594993	4354.304584	23.777421
125.739498	4361.923484	23.782439
125.925414	4374.480149	23.787456
126.038202	4387.087033	23.792474
126.224674	4376.653298	23.797491
126.282076	4399.344990	23.802509
126.249035	4416.327931	23.807527
126.483975	4413.674725	23.812544
126.847400	4414.466424	23.817562
127.070730	4426.943219	23.822579
126.831836	4451.876330	23.827597
127.227654	4447.889190	23.832615
127.483544	4439.337921	23.837632
127.324671	4459.929098	23.842650
127.835098	4469.340808	23.847667
127.889303	4469.805772	23.852685
127.775432	4476.357472	23.857703
127.973943	4479.680317	23.862720
128.092315	4482.598991	23.867738
128.529874	4481.825144	23.872755
128.353410	4498.303173	23.877773
128.691676	4502.767269	23.882791
128.670690	4503.945959	23.887808
128.377614	4506.369325	23.892826
128.683732	4506.627344	23.897843
129.112902	4530.872697	23.902861
128.832550	4531.245468	23.907879
129.319998	4532.412323	23.912896
129.199116	4542.200872	23.917914
129.257298	4555.099819	23.922931
129.788616	4566.096614	23.927949
129.977051	4558.847798	23.932967
130.468964	4559.409757	23.937984
130.313706	4568.366753	23.943002
130.580221	4551.108071	23.948019
130.699697	4551.127585	23.953037
130.385074	4562.810736	23.958055
130.703313	4545.940311	23.963072
130.804909	4559.513625	23.968090
130.840606	4575.717967	23.973107
131.017913	4586.562746	23.978125
131.057472	4588.301364	23.983143
131.250581	4580.125842	23.988160
130.884070	4595.359034	23.993178
131.165155	4590.483866	23.998195
131.389851	4605.824200	24.003213
131.279981	4612.461859	24.008231
131.188728	4614.273260	24.013248
131.427892	4638.459402	24.018266
131.762868	4647.918870	24.023283
132.032147	4657.243279	24.028301
132.434190	4662.306954	24.033319
132.735686	4674.504803	24.038336
132.783676	4683.159620	24.043354
133.049700	4686.342728	24.048371
133.133521	4675.164402	24.053389
132.961726	4677.176676	24.058407
132.913745	4666.339562	24.063424
132.757534	4690.272573	24.068442
133.063880	4701.275445	24.073459
133.313439	4707.254791	24.078477
133.492851	4711.224264	24.083495
133.678881	4719.932618	24.088512
133.757528	4733.824435	24.093530
133.906675	4725.811612	24.098547
133.893998	4731.628235	24.103565
133.788666	4762.152190	24.108583
134.122132	4759.142568	24.113600
134.345107	4769.715865	24.118618
134.677415	4784.460992	24.123635
134.953710	4789.316614	24.128653
134.975788	4791.699216	24.133671
135.021977	4778.471125	24.138688
135.031704	4794.644447	24.143706
135.418917	4812.348339	24.148723
135.760928	4814.857731	24.153741
135.769419	4819.366638	24.158759
135.882885	4819.885103	24.163776
135.798143	4827.824802	24.168794
135.782800	4833.988832	24.173811
136.021124	4836.078919	24.178829
136.064918	4852.323971	24.183847
136.496469	4853.309381	24.188864
136.737401	4861.293938	24.193882
136.839167	4868.465192	24.198899
137.460994	4866.669895	24.203917
137.586629	4865.981955	24.208935
137.947017	4849.270462	24.213952
138.339953	4841.084964	24.218970
138.460512	4824.706757	24.223987
138.426726	4807.126687	24.229005
138.222144	4807.117626	24.234023
138.172112	4800.614758	24.239040
138.252829	4797.837386	24.244058
138.067984	4810.996373	24.249075
138.178921	4807.965578	24.254093
138.062620	4812.031791	24.259111
138.135912	4813.119950	24.264128
138.244462	4833.396018	24.269146
138.743564	4834.188925	24.274163
138.582064	4831.666513	24.279181
138.489362	4855.356797	24.284199
139.068155	4869.550557	24.289216
138.953221	4871.544350	24.294234
138.980596	4879.439452	24.299251
139.408395	4888.585324	24.304269
139.500397	4904.400278	24.309287
139.647220	4906.071481	24.314304
139.658879	4909.473780	24.319322
139.897218	4931.241368	24.324339
140.232070	4929.847419	24.329357
140.050681	4938.996832	24.334375
140.454327	4937.977407	24.339392
140.480219	4959.197521	24.344410
140.358819	4963.602093	24.349427
140.545318	4967.924532	24.354445
140.610284	4984.090827	24.359463
140.879198	4995.226552	24.364480
140.954202	5004.800081	24.369498
141.236142	5024.505925	24.374515
141.813907	5019.352804	24.379533
141.826213	5023.005205	24.384551
142.233100	5019.545618	24.389568
142.558961	5019.475583	24.394586
142.149422	5027.244531	24.399603
142.716841	5031.621117	24.404621
142.586400	5048.490505	24.409639
142.909622	5046.266041	24.414656
142.925081	5050.065065	24.419674
142.805706	5047.707406	24.424691
143.480904	5045.086169	24.429709
143.317857	5054.744889	24.434727
143.191274	5044.846796	24.439744
143.415828	5066.590033	24.444762
143.604524	5082.358292	24.449779
143.867402	5085.417686	24.454797
143.579648	5085.880548	24.459815
143.959168	5098.049789	24.464832
144.077751	5114.209251	24.469850
143.994942	5117.982264	24.474867
144.242225	5113.902982	24.479885
144.531528	5139.694755	24.484903
144.488616	5140.862045	24.489920
144.729207	5154.309109	24.494938
144.345034	5156.863539	24.499955
145.108224	5161.237273	24.504973
145.349114	5176.693632	24.509991
145.460174	5173.484940	24.515008
145.369526	5180.519451	24.520026
145.430611	5184.109830	24.525043
145.716208	5193.366680	24.530061
145.491008	5208.579543	24.535079
145.982104	5205.545487	24.540096
146.348934	5217.259755	24.545114
146.258856	5236.966192	24.550131
146.539088	5227.280047	24.555149
146.464725	5240.406065	24.560167
146.495867	5237.674278	24.565184
147.055784	5250.984764	24.570202
146.856843	5264.560226	24.575219
147.501213	5258.219442	24.580237
146.983534	5272.278437	24.585255
147.141568	5288.973865	24.590272
147.468409	5288.668439	24.595290
147.676245	5303.754138	24.600307
148.213729	5311.676711	24.605325
147.698503	5328.167977	24.610343
147.864259	5328.242268	24.615360
148.242097	5335.594742	24.620378
148.281750	5354.429395	24.625395
148.659583	5354.404573	24.630413
148.635610	5362.566172	24.635431
148.834641	5381.148865	24.640448
148.946151	5385.878331	24.645466
149.075375	5399.462174	24.650483
149.238246	5398.986989	24.655501
149.701872	5415.440298	24.660519
149.683453	5422.571191	24.665536
149.901599	5417.117302	24.670554
149.799029	5428.671341	24.675571
150.313025	5429.118102	24.680589
150.152052	5449.161052	24.685607
150.178476	5454.810442	24.690624
150.565365	5459.535363	24.695642
150.861096	5476.840811	24.700659
151.015828	5472.701446	24.705677
151.316468	5483.800226	24.710695
151.268604	5482.619877	24.715712
151.661466	5490.608090	24.720730
151.741942	5515.285944	24.725747
151.846019	5505.434948	24.730765
151.705506	5517.859748	24.735783
151.977473	5509.634951	24.740800
152.586926	5508.234934	24.745818
152.355842	5526.193256	24.750835
152.708014	5534.297340	24.755853
152.843728	5541.745168	24.760871
153.025572	5533.454478	24.765888
153.135532	5529.460705	24.770906
152.986290	5537.878400	24.775923
153.352097	5538.865690	24.780941
153.429782	5562.850150	24.785959
153.462130	5573.063400	24.790976
153.723616	5567.185565	24.795994
153.601417	5565.398671	24.801011
153.678910	5563.826980	24.806029
153.914193	5570.573684	24.811047
154.006303	5591.164969	24.816064
154.246693	5600.020956	24.821082
153.976109	5612.588520	24.826099
154.471205	5618.310374	24.831117
154.592435	5628.013833	24.836135
154.683887	5642.217594	24.841152
155.162856	5639.146836	24.846170
154.883344	5655.392390	24.851187
155.243956	5648.258784	24.856205
155.478191	5660.289582	24.861223
155.238059	5678.409242	24.866240
156.147247	5675.836354	24.871258
155.976271	5683.946825	24.876275
156.114198	5686.816203	24.881293
156.564596	5702.425386	24.886311
156.617532	5712.215318	24.891328
157.007672	5703.428708	24.896346
156.799073	5710.693127	24.901363
157.019024	5714.830285	24.906381
157.116850	5729.225871	24.911399
157.262265	5736.753288	24.916416
157.745089	5736.471766	24.921434
157.639614	5737.647503	24.926451
158.112625	5728.850812	24.931469
158.280580	5745.307572	24.936487
158.195135	5761.676508	24.941504
158.707482	5741.284469	24.946522
158.695348	5749.969167	24.951539
158.905372	5749.458917	24.956557
158.981066	5749.386284	24.961575
158.700879	5749.412088	24.966592
159.068830	5755.790761	24.971610
159.400203	5774.511777	24.976627
159.783109	5776.696966	24.981645
159.631961	5787.992315	24.986663
159.342717	5791.891249	24.991680
159.417333	5798.375716	24.996698
159.927825	5818.958836	25.001715
159.953449	5822.130169	25.006733
160.073408	5822.690122	25.011751
160.498585	5844.529976	25.016768
160.564164	5846.246499	25.021786
160.618377	5860.259714	25.026803
160.776025	5852.949876	25.031821
161.010170	5867.594512	25.036839
160.952051	5875.792523	25.041856
161.433183	5874.402706	25.046874
161.258251	5895.882772	25.051891
161.300830	5910.291277	25.056909
161.696892	5909.784406	25.061927
161.441295	5915.624489	25.066944
161.693937	5929.323681	25.071962
162.000837	5942.055156	25.076979
161.945543	5958.281029	25.081997
162.614602	5970.034258	25.087015
162.480898	5973.358484	25.092032
162.952995	5980.741889	25.097050
163.090348	5990.646005	25.102067
163.410198	6005.916766	25.107085
163.328863	6003.746435	25.112103
163.305858	6006.744602	25.117120
163.956752	6018.952379	25.122138
163.911735	6035.607853	25.127155
164.163121	6024.138223	25.132173
164.662303	6022.497680	25.137191
164.405916	6030.756497	25.142208
164.829612	6033.938368	25.147226
165.165043	6056.381357	25.152243
165.181856	6054.439273	25.157261
165.185883	6057.100331	25.162279
165.162331	6060.927865	25.167296
165.365684	6053.307730	25.172314
165.748890	6077.221497	25.177331
165.832229	6086.498568	25.182349
166.113447	6085.226366	25.187367
166.069908	6091.025627	25.192384
166.206905	6083.011649	25.197402
166.310706	6092.058081	25.202419
166.419620	6095.821231	25.207437
166.699761	6099.874944	25.212455
166.538692	6115.112342	25.217472
166.849938	6133.584464	25.222490
167.252664	6139.008109	25.227507
167.182544	6137.074367	25.232525
167.379697	6151.162631	25.237543
167.595345	6176.617839	25.242560
167.595476	6180.259092	25.247578
167.632217	6193.668794	25.252595
167.933342	6202.861648	25.257613
168.239555	6220.349620	25.262631
168.271771	6228.306827	25.267648
168.711097	6234.907221	25.272666
168.416609	6236.873958	25.277683
168.511816	6270.023686	25.282701
169.041558	6263.956467	25.287719
168.904854	6281.663829	25.292736
169.510359	6299.905922	25.297754
169.428572	6305.799486	25.302771
169.529682	6309.080055	25.307789
169.740129	6326.418980	25.312807
169.797029	6352.371090	25.317824
170.240422	6345.431670	25.322842
170.260472	6371.822428	25.327859
170.474216	6387.861893	25.332877
170.599184	6374.691417	25.337895
170.910283	6402.018539	25.342912
170.952133	6406.460454	25.347930
171.160237	6403.964605	25.352947
171.315928	6426.720846	25.357965
171.589023	6434.081131	25.362983
171.678306	6444.205651	25.368000
172.034899	6433.381422	25.373018
172.238228	6452.895564	25.378035
172.223263	6465.868425	25.383053
172.364184	6465.458866	25.388071
172.588421	6468.066007	25.393088
173.041039	6481.631546	25.398106
173.353542	6490.837715	25.403123
173.711928	6487.152635	25.408141
173.870523	6483.354635	25.413159
173.725255	6486.947545	25.418176
173.876106	6481.342702	25.423194
173.923855	6485.463471	25.428211
174.271063	6508.564612	25.433229
174.652190	6499.970953	25.438247
174.561684	6510.453853	25.443264
174.926687	6510.287885	25.448282
174.710194	6502.388261	25.453299
175.097811	6506.122033	25.458317
175.603154	6524.753320	25.463335
175.518219	6540.334652	25.468352
175.640173	6536.662075	25.473370
175.997653	6528.203567	25.478387
175.651228	6541.131773	25.483405
175.701025	6534.764081	25.488423
176.311254	6556.976760	25.493440
176.416565	6558.823936	25.498458
176.641603	6555.304872	25.503475
176.845990	6560.916870	25.508493
177.154784	6568.371456	25.513511
177.276636	6583.320317	25.518528
177.419347	6577.745061	25.523546
177.337036	6579.500197	25.528563
177.484638	6589.903492	25.533581
177.953831	6607.925362	25.538599
177.510771	6618.307182	25.543616
177.600056	6614.894722	25.548634
177.582969	6632.312767	25.553651
177.935405	6645.045458	25.558669
178.559169	6660.308572	25.563687
178.600502	6682.771073	25.568704
178.573814	6690.114761	25.573722
178.804851	6698.438651	25.578739
178.582717	6710.155948	25.583757
179.230853	6720.503142	25.588775
179.190400	6733.931146	25.593792
179.438735	6751.747635	25.598810
180.005603	6758.435727	25.603827
180.268252	6769.340894	25.608845
180.689796	6768.475082	25.613863
180.744299	6785.756790	25.618880
181.210863	6788.083015	25.623898
181.360912	6788.630341	25.628915
181.422389	6781.804326	25.633933
181.548016	6784.885961	25.638951
181.654391	6786.359257	25.643968
181.639515	6783.192329	25.648986
181.842380	6798.509312	25.654003
181.915798	6806.829280	25.659021
182.216728	6821.292688	25.664039
182.161085	6825.727454	25.669056
182.235628	6832.343785	25.674074
182.614845	6845.144766	25.679092
182.605826	6866.342490	25.684109
182.790399	6853.977239	25.689127
183.079468	6869.180625	25.694144
183.204962	6876.158661	25.699162
183.388208	6886.734305	25.704180
183.221652	6912.717510	25.709197
183.690431	6921.548897	25.714215
183.607870	6931.064601	25.719232
184.078637	6945.505775	25.724250
184.034144	6952.741488	25.729268
184.218232	6974.353926	25.734285
184.675469	6989.599867	25.739303
184.641235	7009.606618	25.744320
184.903397	7016.340258	25.749338
185.019285	7032.949953	25.754356
185.300028	7054.620274	25.759373
185.609779	7045.882676	25.764391
185.847993	7061.819043	25.769408
185.936863	7071.353930	25.774426
186.288833	7070.054633	25.779444
186.632210	7089.162523	25.784461
186.869176	7098.374820	25.789479
186.880574	7112.029377	25.794496
186.914821	7119.380085	25.799514
187.692996	7117.431364	25.804532
187.680648	7141.212415	25.809549
187.878611	7134.423492	25.814567
188.027454	7141.734698	25.819584
188.054757	7134.983210	25.824602
188.650787	7151.714777	25.829620
188.008822	7165.478264	25.834637
188.426034	7163.827069	25.839655
188.672884	7180.229570	25.844672
188.754597	7187.068772	25.849690
189.028358	7193.475678	25.854708
188.716638	7220.252093	25.859725
189.191410	7226.190270	25.864743
189.336212	7239.626178	25.869760
189.399995	7256.397078	25.874778
189.955017	7255.244795	25.879796
190.164545	7285.109218	25.884813
190.395090	7299.135810	25.889831
190.603829	7300.649491	25.894848
190.758034	7302.304058	25.899866
190.876235	7320.343409	25.904884
190.947893	7327.645766	25.909901
191.399800	7318.993145	25.914919
191.713574	7322.649199	25.919936
191.329727	7345.431487	25.924954
191.953553	7345.923764	25.929972
191.930015	7357.110257	25.934989
192.130491	7364.991677	25.940007
192.290262	7385.300841	25.945024
192.168548	7388.879195	25.950042
192.849817	7405.762701	25.955060
192.564362	7419.814226	25.960077
193.291560	7422.515252	25.965095
193.482944	7442.944565	25.970112
193.400982	7447.850316	25.975130
193.711041	7459.603747	25.980148
193.785585	7473.617604	25.985165
193.790145	7484.091541	25.990183
194.193666	7488.437566	25.995200
194.677127	7503.402096	26.000218
194.974984	7507.794087	26.005236
195.063889	7514.822320	26.010253
195.123452	7521.987426	26.015271
195.108414	7533.837593	26.020288
195.221298	7552.551625	26.025306
195.635120	7563.458458	26.030324
195.777054	7576.327800	26.035341
196.139872	7570.943703	26.040359
196.200097	7582.030456	26.045376
196.396891	7596.731543	26.050394
196.817392	7607.375317	26.055412
196.920247	7617.894267	26.060429
197.091643	7630.449721	26.065447
197.676275	7632.500745	26.070464
197.313820	7631.464798	26.075482
197.605970	7649.436688	26.080500
197.925200	7664.547166	26.085517
197.872738	7669.076885	26.090535
198.204215	7685.332685	26.095552
198.578398	7692.288770	26.100570
198.875756	7687.599643	26.105588
198.387914	7718.940538	26.110605
198.549202	7724.651127	26.115623
199.139145	7733.440080	26.120640
199.108505	7749.230408	26.125658
199.356867	7755.986257	26.130676
199.964850	7786.698577	26.135693
199.801240	7798.338149	26.140711
199.734732	7805.680078	26.145728
199.770596	7822.899076	26.150746
200.216789	7840.188024	26.155764
200.461781	7864.365918	26.160781
200.637535	7867.861555	26.165799
201.243280	7878.580649	26.170816
200.973424	7905.908726	26.175834
201.620154	7902.550320	26.180852
202.306155	7912.340716	26.185869
203.074748	7899.192193	26.190887
203.330999	7897.700352	26.195904
203.307439	7886.753909	26.200922
203.274115	7869.671380	26.205940
203.415797	7864.465643	26.210957
203.510715	7862.393628	26.215975
203.484871	7869.683467	26.220992
203.612528	7884.495794	26.226010
203.747418	7893.275550	26.231028
204.058106	7895.494611	26.236045
204.066981	7898.200864	26.241063
204.397707	7908.231237	26.246080
204.449226	7922.665447	26.251098
204.599311	7917.041306	26.256116
204.743165	7931.941589	26.261133
204.965773	7958.034540	26.266151
205.266967	7953.711407	26.271168
205.289646	7967.515243	26.276186
205.215365	7981.704384	26.281204
205.683330	7993.122246	26.286221
205.984517	8015.901791	26.291239
206.332096	8020.105025	26.296256
205.953971	8036.619117	26.301274
206.457427	8047.213001	26.306292
206.652769	8051.824906	26.311309
206.422675	8074.301692	26.316327
206.954434	8085.111419	26.321344
206.759565	8101.005021	26.326362
207.126425	8117.863526	26.331380
207.442419	8145.301666	26.336397
207.516901	8158.190920	26.341415
208.180215	8171.618980	26.346432
208.245544	8184.831948	26.351450
208.553994	8195.385811	26.356468
209.019816	8221.150480	26.361485
209.020954	8219.572979	26.366503
209.396033	8235.069763	26.371520
209.432246	8239.452140	26.376538
209.577921	8249.138860	26.381556
209.868360	8272.208121	26.386573
209.814476	8278.886093	26.391591
210.427667	8289.469346	26.396608
210.606321	8310.756846	26.401626
210.706228	8318.371913	26.406644
210.813752	8330.454588	26.411661
210.743969	8348.907585	26.416679
211.278144	8361.008044	26.421696
211.596599	8374.883142	26.426714
211.571576	8380.928609	26.431732
212.089951	8403.429789	26.436749
212.109167	8405.244102	26.441767
212.651043	8413.074803	26.446784
212.906240	8415.670669	26.451802
213.083600	8431.536366	26.456820
213.139823	8436.386181	26.461837
212.958664	8437.650914	26.466855
213.035078	8450.080164	26.471872
213.599077	8471.188821	26.476890
213.359226	8487.498408	26.481908
213.640557	8493.597776	26.486925
213.726665	8517.199283	26.491943
214.055181	8530.617300	26.496960
214.210968	8545.923127	26.501978
214.826052	8552.439104	26.506996
215.372288	8556.143003	26.512013
215.048691	8576.196797	26.517031
216.002005	8588.666579	26.522048
216.088010	8591.494045	26.527066
216.107770	8596.179358	26.532084
216.141484	8600.657063	26.537101
216.156596	8627.161586	26.542119
216.690123	8624.270796	26.547136
216.985948	8647.825701	26.552154
217.077814	8660.245186	26.557172
217.156825	8669.975463	26.562189
217.208849	8691.040925	26.567207
217.643844	8690.909432	26.572224
217.973422	8705.195411	26.577242
217.887965	8717.837581	26.582260
218.565397	8729.657394	26.587277
218.525758	8749.227051	26.592295
218.980399	8761.203591	26.597312
219.008387	8764.506198	26.602330
219.444493	8788.559907	26.607348
219.512684	8792.521064	26.612365
219.597577	8799.498212	26.617383
220.172140	8816.959843	26.622400
220.152646	8834.328116	26.627418
220.224883	8837.085426	26.632436
220.397245	8858.076068	26.637453
220.240136	8868.449656	26.642471
220.662286	8885.332087	26.647488
220.991182	8894.506056	26.652506
221.304171	8913.006146	26.657524
222.006900	8911.154233	26.662541
222.051452	8925.073505	26.667559
222.495662	8931.938745	26.672576
222.726668	8921.959028	26.677594
223.097042	8926.175021	26.682612
223.397094	8917.487463	26.687629
223.636044	8927.491054	26.692647
223.815223	8945.550191	26.697664
224.006943	8956.922334	26.702682
224.022744	8957.757523	26.707700
224.559487	8954.967282	26.712717
224.175444	8963.128049	26.717735
224.222411	8962.306886	26.722752
224.660511	8979.671635	26.727770
224.589839	8984.683898	26.732788
224.938882	8999.059915	26.737805
225.140659	9011.206023	26.742823
225.106899	9025.558884	26.747840
225.552269	9038.072638	26.752858
225.893736	9060.237084	26.757876
225.971554	9060.699220	26.762893
225.767096	9070.147577	26.767911
226.237939	9089.632369	26.772928
226.374601	9101.921136	26.777946
226.581396	9120.014642	26.782964
227.308294	9123.457741	26.787981
227.406011	9138.105315	26.792999
227.618769	9152.092025	26.798016
227.794546	9155.609998	26.803034
227.665692	9183.504985	26.808052
228.364981	9177.063722	26.813069
228.180031	9206.209102	26.818087
228.767482	9207.895552	26.823104
228.939401	9228.344183	26.828122
228.920098	9242.958969	26.833140
229.140514	9260.125019	26.838157
229.391519	9280.206593	26.843175
230.133381	9284.398885	26.848192
230.225729	9297.334275	26.853210
230.040420	9314.703959	26.858228
230.643581	9320.924711	26.863245
230.585428	9348.835490	26.868263
230.888428	9355.412983	26.873280
231.012396	9369.700895	26.878298
231.265728	9392.419735	26.883316
231.362111	9406.631809	26.888333
231.695343	9422.824301	26.893351
231.703108	9430.909879	26.898368
232.166278	9466.981188	26.903386
232.055662	9482.014866	26.908404
232.595252	9498.361449	26.913421
232.767848	9521.488016	26.918439
232.805075	9526.807096	26.923456
233.489763	9556.078951	26.928474
233.676006	9563.456604	26.933492
233.903502	9582.224553	26.938509
234.045550	9587.596987	26.943527
234.722413	9593.019137	26.948544
234.705162	9606.986273	26.953562
234.861015	9616.075734	26.958580
235.558528	9627.164331	26.963597
235.314155	9646.571047	26.968615
235.455491	9664.109025	26.973632
235.493327	9668.506513	26.978650
236.229692	9695.861209	26.983668
236.327271	9699.645575	26.988685
236.434681	9725.482168	26.993703
236.674830	9732.475138	26.998720
236.969668	9739.124142	27.003738
236.875893	9759.426581	27.008756
237.346022	9771.436093	27.013773
237.474754	9783.441403	27.018791
238.254539	9804.142162	27.023808
238.272518	9807.837330	27.028826
238.293015	9822.497881	27.033844
238.876350	9839.110947	27.038861
238.909587	9843.088185	27.043879
239.260882	9861.502283	27.048896
239.849962	9854.639169	27.053914
239.545904	9884.411609	27.058932
240.218876	9871.139299	27.063949
240.136542	9897.503413	27.068967
240.278080	9912.281693	27.073984
240.665668	9916.355142	27.079002
240.562372	9946.151972	27.084020
240.956315	9949.219435	27.089037
241.057100	9966.627687	27.094055
241.222730	9965.840283	27.099072
241.612547	9994.868813	27.104090
241.600534	10014.448697	27.109108
242.114165	10024.616610	27.114125
242.095625	10046.695881	27.119143
241.984948	10072.896009	27.124160
242.803181	10083.417956	27.129178
242.838446	10108.957419	27.134196
243.156755	10110.856871	27.139213
243.406169	10135.855419	27.144231
243.682132	10150.187528	27.149248
244.231076	10168.448513	27.154266
244.486455	10177.021131	27.159284
244.768973	10199.900629	27.164301
245.379489	10195.082116	27.169319
245.419716	10211.874245	27.174336
246.074191	10220.515097	27.179354
245.980346	10231.060153	27.184372
246.210173	10222.928435	27.189389
246.242431	10249.331168	27.194407
246.748109	10256.797547	27.199424
247.027560	10264.625021	27.204442
246.914784	10277.987060	27.209460
247.308669	10287.331359	27.214477
247.919738	10289.083040	27.219495
248.316145	10292.146247	27.224512
248.571631	10304.264381	27.229530
248.583035	10305.607178	27.234548
248.901145	10307.829361	27.239565
248.995954	10302.276497	27.244583
248.851785	10327.482122	27.249600
249.617479	10324.064104	27.254618
249.379909	10341.748658	27.259636
249.687569	10365.965070	27.264653
249.878193	10369.203937	27.269671
250.051227	10363.375328	27.274688
250.473593	10380.080763	27.279706
250.617574	10403.491062	27.284724
250.651344	10398.045088	27.289741
250.876408	10425.471206	27.294759
251.337755	10437.313840	27.299776
251.991794	10435.575373	27.304794
251.722549	10465.525602	27.309812
251.915530	10471.356540	27.314829
252.573098	10483.981905	27.319847
252.184689	10499.866779	27.324864
252.469764	10504.117676	27.329882
252.660405	10531.971315	27.334900
253.226506	10542.771064	27.339917
253.226905	10559.557337	27.344935
253.100902	10572.013524	27.349952
253.805951	10586.612140	27.354970
254.124408	10620.354913	27.359988
254.230200	10619.107163	27.365005
254.624110	10646.922318	27.370023
254.937080	10658.186705	27.375040
255.294191	10666.623367	27.380058
255.318185	10683.381225	27.385076
255.435351	10695.696048	27.390093
255.728117	10719.098862	27.395111
256.151995	10737.236450	27.400128
256.764254	10755.724562	27.405146
256.436162	10778.744767	27.410164
256.731665	10780.759308	27.415181
257.556665	10804.572857	27.420199
257.604447	10821.010689	27.425216
257.776793	10831.021053	27.430234
257.751790	10859.196541	27.435252
258.228264	10867.866929	27.440269
258.416246	10880.054133	27.445287
258.576685	10900.716613	27.450304
259.156795	10913.732662	27.455322
259.227355	10938.774037	27.460340
259.600726	10953.388100	27.465357
259.807139	10968.449461	27.470375
260.004131	10991.625949	27.475392
259.875918	11011.116248	27.480410
260.283567	11031.691887	27.485428
260.673892	11055.115090	27.490445
261.247980	11072.342533	27.495463
261.344052	11096.918108	27.500480
261.887934	11100.789888	27.505498
262.398176	11119.911360	27.510516
262.749277	11126.398934	27.515533
263.015217	11126.417951	27.520551
262.864749	11146.364524	27.525568
263.147868	11164.701756	27.530586
263.067489	11172.071933	27.535604
263.470437	11189.932032	27.540621
263.517852	11200.770856	27.545639
263.743189	11233.979694	27.550656
264.065293	11238.829751	27.555674
264.345389	11253.127621	27.560692
264.750226	11270.594774	27.565709
264.893631	11288.746643	27.570727
264.977201	11305.166704	27.575744
265.253759	11322.364726	27.580762
265.447396	11339.551979	27.585780
265.672601	11356.951055	27.590797
266.055398	11375.790541	27.595815
265.909049	11405.505416	27.600832
266.763207	11423.419804	27.605850
267.003979	11443.106461	27.610868
267.140874	11462.500777	27.615885
267.744942	11470.074865	27.620903
267.966751	11500.017343	27.625920
268.341492	11508.899118	27.630938
268.564713	11523.152789	27.635956
268.903482	11536.032723	27.640973
269.033662	11543.431896	27.645991
269.220427	11566.112482	27.651008
269.732945	11575.670469	27.656026
270.228946	11595.474059	27.661044
269.963035	11600.609213	27.666061
270.790871	11612.863852	27.671079
270.722844	11639.703327	27.676096
270.797666	11644.746015	27.681114
271.159721	11663.006730	27.686132
271.312077	11677.461724	27.691149
271.758309	11690.143831	27.696167
271.279338	11717.503873	27.701184
272.166035	11736.679270	27.706202
272.328657	11762.683510	27.711220
272.158225	11783.298004	27.716237
272.984098	11808.403821	27.721255
273.012016	11831.543609	27.726272
273.254201	11841.715096	27.731290
273.689910	11869.119901	27.736308
274.122015	11881.044290	27.741325
274.658455	11891.345022	27.746343
274.776987	11918.865209	27.751360
275.014739	11928.368632	27.756378
275.196798	11956.961208	27.761396
275.339717	11970.938844	27.766413
276.041439	11985.837860	27.771431
276.231962	12006.536606	27.776448
276.273607	12023.661100	27.781466
276.422835	12047.794874	27.786484
276.572072	12062.058877	27.791501
277.285590	12071.414738	27.796519
277.001287	12100.697229	27.801536
277.590315	12111.417322	27.806554
277.961425	12134.468043	27.811572
277.705759	12158.551807	27.816589
278.374810	12188.475130	27.821607
278.482495	12195.476193	27.826624
278.535210	12205.687372	27.831642
279.254641	12233.204250	27.836660
279.426747	12246.086559	27.841677
279.886861	12256.258617	27.846695
280.009006	12278.313208	27.851712
280.446089	12298.744007	27.856730
280.996676	12306.129677	27.861748
280.984222	12314.058662	27.866765
281.468446	12332.060645	27.871783
281.892932	12348.176018	27.876800
282.255707	12360.466628	27.881818
282.236377	12378.812410	27.886836
282.446248	12388.690313	27.891853
283.042684	12406.704017	27.896871
282.912683	12421.480804	27.901888
283.271078	12421.930010	27.906906
283.499610	12444.193985	27.911924
283.678317	12466.797113	27.916941
283.981146	12478.751238	27.921959
283.970489	12493.811327	27.926976
284.498375	12520.832478	27.931994
284.908712	12553.473575	27.937012
284.655909	12571.967982	27.942029
285.321280	12580.417198	27.947047
285.342119	12616.752693	27.952064
285.980610	12631.438292	27.957082
286.634429	12648.776246	27.962100
286.623914	12666.087668	27.967117
286.999222	12669.263948	27.972135
287.206958	12694.710817	27.977152
287.642102	12708.259226	27.982170
287.828122	12730.880079	27.987188
288.051893	12744.353387	27.992205
288.601419	12757.093329	27.997223
288.974103	12777.807386	28.002240
288.849252	12797.093798	28.007258
289.371963	12811.040801	28.012276
289.591955	12832.708089	28.017293
290.152048	12847.928463	28.022311
289.746213	12860.481106	28.027328
290.250995	12879.420307	28.032346
290.607489	12908.655155	28.037364
290.687349	12925.797400	28.042381
291.333895	12935.710163	28.047399
291.130239	12967.201598	28.052416
291.561425	12988.000386	28.057434
292.195782	13002.835875	28.062452
292.145057	13028.088547	28.067469
292.744661	13038.907092	28.072487
293.177616	13065.658707	28.077504
293.414633	13080.022731	28.082522
293.787409	13094.459688	28.087540
293.742024	13120.245054	28.092557
294.505631	13127.781964	28.097575
294.402009	13143.234065	28.102592
294.761342	13153.399767	28.107610
295.284874	13167.371075	28.112628
295.467764	13186.127095	28.117645
295.771711	13189.037191	28.122663
296.311258	13208.321449	28.127680
296.171235	13218.549759	28.132698
296.710240	13233.728916	28.137716
296.467307	13253.252765	28.142733
297.182908	13257.155307	28.147751
297.156364	13275.340769	28.152768
297.503577	13285.398880	28.157786
298.386857	13291.543107	28.162804
298.560695	13310.467700	28.167821
299.165040	13319.075145	28.172839
298.995122	13333.933267	28.177856
299.328191	13355.571594	28.182874
299.735982	13358.875188	28.187892
299.806809	13382.319949	28.192909
300.085105	13395.768319	28.197927
300.237335	13411.702200	28.202944
300.224410	13432.663296	28.207962
300.367262	13450.485160	28.212980
301.073210	13480.134368	28.217997
300.951191	13498.811058	28.223015
301.380356	13527.651373	28.228032
302.068285	13553.805794	28.233050
302.541734	13563.612149	28.238068
302.136435	13602.401963	28.243085
303.054325	13616.534197	28.248103
303.308665	13640.414443	28.253120
303.300204	13668.167421	28.258138
303.502876	13687.773224	28.263156
303.724534	13710.652377	28.268173
304.388162	13735.447190	28.273191
304.718029	13757.030879	28.278208
305.192975	13775.672889	28.283226
305.724970	13794.138454	28.288244
305.639957	13813.421471	28.293261
306.051406	13842.019996	28.298279
306.274278	13851.975793	28.303296
306.261572	13882.463253	28.308314
307.022947	13902.118737	28.313332
307.720216	13908.007214	28.318349
308.288952	13922.573626	28.323367
308.526699	13938.340434	28.328384
308.520817	13942.469924	28.333402
308.856840	13951.045218	28.338420
308.763003	13976.302490	28.343437
309.110257	13998.670553	28.348455
309.640874	14015.550700	28.353472
309.519602	14041.708676	28.358490
309.890181	14055.849533	28.363508
310.074093	14071.857281	28.368525
310.201019	14102.735518	28.373543
310.845521	14129.449089	28.378560
311.200309	14145.338858	28.383578
312.039426	14147.064325	28.388596
311.911972	14182.587600	28.393613
312.427447	14178.064833	28.398631
312.907228	14193.123025	28.403648
313.141822	14198.891306	28.408666
313.383059	14211.848100	28.413684
313.856362	14228.100274	28.418701
314.029075	14241.368531	28.423719
314.361912	14256.025700	28.428736
314.430491	14269.334980	28.433754
314.452494	14279.274852	28.438772
314.731173	14294.656659	28.443789
314.911357	14320.022463	28.448807
315.412190	14337.700832	28.453824
315.616878	14356.748644	28.458842
315.947796	14387.875097	28.463860
316.286588	14413.235459	28.468877
316.899628	14430.977728	28.473895
317.243768	14449.470485	28.478912
317.359581	14484.875419	28.483930
317.897755	14501.448770	28.488948
317.961284	14519.948151	28.493965
318.048718	14539.199874	28.498983
318.542973	14571.793938	28.504000
318.615334	14594.165155	28.509018
318.912072	14608.079467	28.514036
318.931302	14653.031551	28.519053
319.432280	14682.839459	28.524071
319.660728	14716.425199	28.529088
319.754422	14750.841471	28.534106
320.355946	14778.663386	28.539124
320.853422	14811.321606	28.544141
320.955091	14849.676860	28.549159
321.552243	14873.040516	28.554176
321.655701	14895.129714	28.559194
322.242013	14920.133226	28.564212
322.285047	14952.436202	28.569229
322.876023	14974.075256	28.574247
323.211485	15002.044092	28.579264
323.426704	15034.733205	28.584282
323.835297	15051.726054	28.589300
324.072833	15094.971239	28.594317
324.204387	15128.720243	28.599335
325.121396	15146.890504	28.604352
325.440527	15176.197544	28.609370
325.711801	15199.139605	28.614388
326.076775	15224.307997	28.619405
326.618559	15241.630162	28.624423
326.582262	15256.101787	28.629440
326.874957	15299.585858	28.634458
327.237364	15316.325384	28.639476
327.613507	15340.599921	28.644493
327.807158	15375.169348	28.649511
328.370536	15373.341886	28.654528
328.433273	15410.304882	28.659546
328.998743	15429.961873	28.664564
329.370701	15445.796429	28.669581
329.704335	15465.469549	28.674599
330.178941	15471.212069	28.679616
329.963094	15511.232104	28.684634
330.450397	15522.387692	28.689652
330.566296	15551.521078	28.694669
330.957158	15575.695133	28.699687
331.419597	15594.948939	28.704704
331.704504	15619.441083	28.709722
332.401917	15640.103143	28.714740
332.277013	15674.202729	28.719757
332.363231	15701.475267	28.724775
332.893574	15716.453293	28.729792
333.061271	15753.384542	28.734810
333.623739	15770.226126	28.739828
334.215908	15792.601769	28.744845
334.070831	15822.754282	28.749863
334.731279	15847.678409	28.754880
335.184116	15872.874014	28.759898
335.864257	15898.781367	28.764916
336.123484	15921.524780	28.769933
336.135298	15943.211934	28.774951
336.820191	15963.159985	28.779968
336.836083	15987.296425	28.784986
337.256643	16005.943524	28.790004
337.759928	16024.973082	28.795021
337.894472	16041.891032	28.800039
338.403406	16054.829753	28.805056
338.726326	16082.145746	28.810074
339.267142	16101.017075	28.815092
339.564828	16123.428319	28.820109
339.755660	16143.810611	28.825127
340.354455	16154.958736	28.830144
340.386424	16194.179524	28.835162
340.698354	16212.269843	28.840180
341.191595	16232.979806	28.845197
341.262817	16263.263651	28.850215
341.850688	16278.647776	28.855232
341.675098	16308.181168	28.860250
341.979345	16334.219818	28.865268
342.167789	16368.086375	28.870285
342.660699	16396.702074	28.875303
343.231865	16417.685664	28.880320
343.471444	16464.057372	28.885338
343.956640	16489.577538	28.890356
344.454049	16501.525854	28.895373
344.820330	16540.822581	28.900391
345.222194	16565.650117	28.905408
345.179256	16591.409519	28.910426
345.684567	16609.266751	28.915444
346.086909	16641.386983	28.920461
346.226434	16658.784890	28.925479
346.767262	16675.836018	28.930496
346.973901	16704.950035	28.935514
347.316606	16718.963947	28.940532
347.696733	16744.072966	28.945549
347.814504	16768.548692	28.950567
348.120334	16796.527479	28.955584
348.027919	16832.536888	28.960602
348.120182	16856.833170	28.965620
348.567283	16888.328719	28.970637
349.166984	16929.599328	28.975655
349.846202	16966.265559	28.980672
349.956154	16997.660145	28.985690
350.635515	17024.254907	28.990708
350.730107	17043.792753	28.995725
351.561424	17086.076610	29.000743
351.931049	17099.383076	29.005760
352.269904	17124.796912	29.010778
353.046209	17140.738061	29.015796
353.683279	17156.855737	29.020813
353.893492	17176.873921	29.025831
354.306493	17179.941421	29.030848
354.443615	17208.390137	29.035866
354.863356	17223.436666	29.040884
355.269467	17242.495419	29.045901
354.941978	17267.939692	29.050919
355.717116	17277.660603	29.055936
356.313787	17306.932684	29.060954
356.196368	17329.661422	29.065972
356.561242	17350.187051	29.070989
356.289130	17387.258425	29.076007
357.186667	17402.612835	29.081024
357.701693	17436.023600	29.086042
358.082706	17461.687955	29.091060
358.589375	17483.727727	29.096077
358.704251	17515.072184	29.101095
358.958828	17540.002116	29.106112
359.353872	17572.150443	29.111130
359.642831	17589.368896	29.116148
360.027393	17615.212463	29.121165
360.151529	17649.787918	29.126183
360.690582	17670.235037	29.131200
361.285341	17703.672650	29.136218
361.568519	17723.491334	29.141236
361.946221	17750.492891	29.146253
362.267036	17777.392932	29.151271
362.818271	17796.656011	29.156288
363.107113	17831.937899	29.161306
363.304978	17854.663226	29.166324
363.647521	17872.071878	29.171341
364.181477	17913.825073	29.176359
364.723396	17929.339827	29.181376
364.947489	17961.027227	29.186394
364.679755	17991.440309	29.191412
365.407170	18011.301172	29.196429
365.805184	18043.295278	29.201447
366.144254	18061.043672	29.206464
366.575880	18088.962426	29.211482
366.510227	18118.928198	29.216500
367.064573	18147.067267	29.221517
367.024480	18179.605090	29.226535
367.929136	18197.848170	29.231552
368.072076	18226.753340	29.236570
368.577912	18261.828790	29.241588
369.256124	18277.985179	29.246605
369.752005	18296.096657	29.251623
370.098786	18320.671806	29.256640
370.482656	18348.228943	29.261658
370.864606	18372.533603	29.266676
371.190242	18389.083698	29.271693
371.619496	18420.005467	29.276711
371.651261	18423.803670	29.281728
372.116421	18461.352260	29.286746
372.373694	18496.418632	29.291764
373.097292	18509.182887	29.296781
373.061559	18538.811224	29.301799
373.319581	18559.799197	29.306816
373.660443	18593.973699	29.311834
373.702577	18626.446595	29.316852
374.519276	18651.655684	29.321869
374.850376	18696.311533	29.326887
375.146490	18716.920798	29.331904
375.683904	18746.729475	29.336922
375.883618	18786.411401	29.341940
376.347749	18808.900409	29.346957
376.877447	18843.009539	29.351975
377.008163	18875.658218	29.356992
377.311845	18910.700017	29.362010
377.643120	18938.456748	29.367028
378.208906	18960.433291	29.372045
378.248268	19005.122730	29.377063
379.141426	19026.111709	29.382080
379.165122	19070.495937	29.387098
379.564318	19111.865132	29.392116
380.075630	19137.481570	29.397133
380.169456	19178.560205	29.402151
380.364816	19212.522221	29.407168
381.143717	19249.446689	29.412186
381.527171	19286.934296	29.417204
382.035007	19315.365196	29.422221
382.598362	19342.903369	29.427239
382.933820	19385.305184	29.432256
383.445137	19414.017625	29.437274
383.633216	19448.539631	29.442292
383.989502	19472.951288	29.447309
384.167961	19510.335862	29.452327
384.195692	19536.896234	29.457344
384.880456	19570.379432	29.462362
385.443138	19605.122439	29.467380
385.856542	19641.639490	29.472397
386.031378	19683.901943	29.477415
386.348123	19712.132887	29.482432
386.982886	19733.232113	29.487450
387.022418	19770.890260	29.492468
387.421336	19799.771336	29.497485
387.906287	19833.318829	29.502503
388.338315	19863.826040	29.507520
388.854243	19894.217568	29.512538
389.448716	19927.674969	29.517556
389.830503	19953.548454	29.522573
389.906305	19982.492376	29.527591
390.107349	20017.115945	29.532608
390.754036	20050.386133	29.537626
390.975001	20093.668851	29.542644
391.290503	20121.336483	29.547661
391.782554	20154.013730	29.552679
392.280999	20196.118112	29.557696
392.345510	20229.842516	29.562714
392.864159	20262.918959	29.567732
393.450519	20297.599880	29.572749
393.801049	20336.941975	29.577767
394.248738	20369.646034	29.582784
394.831391	20398.239451	29.587802
395.063503	20437.592003	29.592820
395.829430	20466.569793	29.597837
396.045348	20499.016910	29.602855
396.279426	20531.695098	29.607872
396.521399	20561.044781	29.612890
397.341102	20597.956486	29.617908
397.969144	20620.074292	29.622925
398.313582	20646.468737	29.627943
398.886970	20671.249315	29.632960
399.369313	20696.483883	29.637978
399.607779	20730.539186	29.642996
399.756802	20758.920414	29.648013
399.922774	20792.450300	29.653031
400.591726	20814.258660	29.658048
400.901802	20840.936122	29.663066
401.147764	20878.436843	29.668084
401.492596	20907.331334	29.673101
402.036975	20942.173942	29.678119
402.210414	20984.125096	29.683136
402.747976	21017.586018	29.688154
403.153106	21057.480380	29.693172
403.304847	21094.698933	29.698189
403.696144	21133.357652	29.703207
404.113471	21159.093184	29.708224
404.630601	21195.777285	29.713242
404.740895	21242.769345	29.718260
405.414513	21269.879476	29.723277
405.682032	21308.644980	29.728295
406.270862	21350.775859	29.733312
406.668557	21377.905725	29.738330
407.074422	21425.337954	29.743348
407.618063	21458.870515	29.748365
408.039415	21482.842557	29.753383
408.810852	21510.373048	29.758400
409.534656	21533.003775	29.763418
409.382234	21561.843231	29.768436
410.316011	21580.813768	29.773453
410.537742	21598.328915	29.778471
410.942794	21619.881161	29.783488
411.507758	21635.313637	29.788506
411.327364	21664.600359	29.793524
412.038327	21688.826642	29.798541
412.057944	21723.378911	29.803559
412.507114	21748.389691	29.808576
412.914746	21778.376825	29.813594
413.057336	21822.697109	29.818612
413.785540	21849.180496	29.823629
413.838108	21880.056094	29.828647
413.910811	21922.356583	29.833664
414.582044	21952.538329	29.838682
414.989203	21996.201044	29.843700
415.030164	22030.481223	29.848717
415.668656	22074.513700	29.853735
415.778520	22119.708759	29.858752
416.337061	22164.022010	29.863770
416.406381	22223.166885	29.868788
417.280598	22268.327225	29.873805
417.686104	22306.491933	29.878823
418.041554	22350.819951	29.883840
418.567403	22404.598392	29.888858
419.597751	22421.652456	29.893876
420.081493	22450.440218	29.898893
420.798350	22484.927956	29.903911
421.070582	22522.772591	29.908928
421.510585	22553.705131	29.913946
422.062516	22583.406161	29.918964
422.711190	22610.216188	29.923981
422.745807	22637.463564	29.928999
422.908855	22673.007161	29.934016
423.427568	22704.329937	29.939034
423.893883	22745.976823	29.944052
424.110767	22785.056468	29.949069
424.675425	22812.140933	29.954087
425.040555	22852.317152	29.959104
425.950872	22884.806619	29.964122
425.882711	22923.473609	29.969140
426.304140	22950.507091	29.974157
427.115972	22976.204790	29.979175
426.819136	23029.563495	29.984192
427.180172	23061.152332	29.989210
427.882366	23099.416611	29.994228
428.274952	23140.560366	29.999245
428.940248	23168.752609	30.004263
429.185748	23200.875261	30.009280
429.938291	23234.409029	30.014298
430.146985	23276.663896	30.019316
430.640418	23313.032960	30.024333
430.982374	23347.643747	30.029351
431.094169	23377.603853	30.034368
432.326520	23395.258507	30.039386
432.702183	23432.461847	30.044404
433.033944	23460.943262	30.049421
433.240630	23485.279428	30.054439
433.455868	23517.012128	30.059456
433.929522	23542.046264	30.064474
434.184815	23593.266991	30.069492
434.167424	23629.630731	30.074509
435.062745	23666.439906	30.079527
435.037047	23711.073479	30.084544
435.620145	23755.932349	30.089562
436.011548	23790.887533	30.094580
436.501073	23836.913143	30.099597
436.853601	23876.500827	30.104615
436.856523	23927.728177	30.109632
437.378529	23967.717594	30.114650
438.119412	24018.376315	30.119668
438.679508	24070.972607	30.124685
439.222804	24103.387562	30.129703
440.057198	24128.331280	30.134720
440.615073	24167.036248	30.139738
441.127034	24205.617077	30.144756
441.747303	24231.206334	30.149773
442.385778	24263.138551	30.154791
442.485231	24298.246914	30.159808
443.102374	24324.882118	30.164826
443.436262	24363.137226	30.169844
443.872895	24382.643287	30.174861
444.666757	24417.851605	30.179879
444.936378	24448.017019	30.184896
445.492076	24467.848451	30.189914
446.211708	24505.752565	30.194932
446.626120	24539.204321	30.199949
446.865763	24557.435140	30.204967
446.889099	24600.556463	30.209984
447.487417	24619.972463	30.215002
447.930763	24663.253121	30.220020
448.256511	24703.374907	30.225037
448.949501	24730.476074	30.230055
448.893625	24770.872303	30.235072
449.198955	24806.159309	30.240090
449.413995	24849.955791	30.245108
449.672561	24896.885409	30.250125
450.746335	24937.343929	30.255143
451.079029	24977.438512	30.260160
451.546073	25014.440353	30.265178
452.173077	25053.959661	30.270196
452.223229	25100.865573	30.275213
453.000670	25128.343115	30.280231
453.361889	25173.340579	30.285248
453.860668	25220.870963	30.290266
454.421035	25258.361092	30.295284
454.993687	25301.915139	30.300301
455.207744	25321.926528	30.305319
455.605983	25380.546243	30.310336
456.275345	25403.413336	30.315354
456.418956	25441.955788	30.320372
456.739900	25467.185074	30.325389
457.403126	25499.976074	30.330407
457.579719	25543.448135	30.335424
457.895108	25583.267331	30.340442
458.468168	25628.077920	30.345460
458.544419	25674.923844	30.350477
459.313120	25708.918745	30.355495
459.516589	25762.254912	30.360512
460.051029	25805.140493	30.365530
460.680312	25848.058347	30.370548
460.613395	25907.029814	30.375565
461.369789	25943.034473	30.380583
461.716737	25998.590634	30.385600
462.268618	26042.207511	30.390618
462.770159	26085.608790	30.395636
463.576954	26139.032864	30.400653
464.039244	26179.608488	30.405671
464.792834	26229.146417	30.410688
465.446784	26272.972187	30.415706
465.971400	26307.341274	30.420724
466.144274	26340.427971	30.425741
466.900034	26375.594679	30.430759
467.384498	26415.287375	30.435776
467.697578	26460.494646	30.440794
467.859799	26506.643103	30.445812
468.381329	26548.169790	30.450829
469.133964	26579.455038	30.455847
469.717434	26619.059196	30.460864
470.654308	26659.302809	30.465882
471.335855	26680.484618	30.470900
471.783852	26697.109016	30.475917
472.378117	26719.143035	30.480935
472.887022	26746.514085	30.485952
473.487253	26774.939728	30.490970
473.896665	26801.916259	30.495988
474.114461	26829.885312	30.501005
474.826005	26857.468501	30.506023
474.884124	26884.304171	30.511040
474.918137	26917.434657	30.516058
475.622191	26961.307109	30.521076
475.606123	26998.754469	30.526093
476.638701	27026.698853	30.531111
476.583367	27063.178837	30.536128
476.955393	27114.120410	30.541146
477.378003	27152.582332	30.546164
477.996237	27203.119401	30.551181
478.963927	27231.928517	30.556199
479.445729	27270.174872	30.561216
479.670182	27297.942771	30.566234
480.549416	27328.151212	30.571252
480.322565	27370.936912	30.576269
481.198835	27409.960626	30.581287
482.017838	27442.600783	30.586304
481.753784	27472.651259	30.591322
482.214158	27515.616228	30.596340
482.525336	27564.999474	30.601357
483.068607	27592.805335	30.606375
483.419097	27633.835764	30.611392
483.568656	27691.183807	30.616410
484.707531	27723.518305	30.621428
484.639825	27763.318825	30.626445
485.302290	27812.910021	30.631463
485.794242	27867.897214	30.636480
485.946463	27911.963369	30.641498
486.394151	27955.046559	30.646516
486.519591	28010.692995	30.651533
487.248211	28058.783706	30.656551
487.686620	28113.466677	30.661568
488.068395	28163.878956	30.666586
488.629032	28219.088043	30.671604
488.913650	28284.677090	30.676621
489.427951	28339.143876	30.681639
490.313645	28385.581132	30.686656
491.206882	28440.961761	30.691674
491.898984	28491.978023	30.696692
492.446940	28538.661771	30.701709
492.917991	28579.703756	30.706727
493.516879	28620.181811	30.711744
493.748325	28665.160840	30.716762
494.429058	28702.573628	30.721780
494.337741	28755.313434	30.726797
495.257471	28805.766508	30.731815
495.660278	28858.903852	30.736832
495.954841	28911.919935	30.741850
496.483369	28960.918233	30.746868
496.765580	29010.439713	30.751885
497.431237	29068.252513	30.756903
497.864414	29124.748850	30.761920
498.485908	29172.354062	30.766938
499.344905	29204.422504	30.771956
499.650055	29258.689301	30.776973
500.370250	29307.938626	30.781991
500.988928	29357.978051	30.787008
500.961411	29417.093903	30.792026
501.882970	29452.509602	30.797044
502.173204	29515.193539	30.802061
503.071449	29552.625644	30.807079
503.722965	29597.976873	30.812096
503.658236	29649.300131	30.817114
504.468666	29684.663119	30.822132
504.688219	29740.291019	30.827149
505.456086	29783.999416	30.832167
506.007375	29828.193155	30.837184
506.185350	29884.497956	30.842202
507.047323	29930.032494	30.847220
507.258236	29974.075969	30.852237
507.634686	30012.906618	30.857255
507.823569	30060.710990	30.862272
508.229576	30119.555448	30.867290
509.291574	30165.652934	30.872308
509.524577	30220.664109	30.877325
510.050009	30260.867959	30.882343
510.728715	30299.019163	30.887360
511.297705	30349.137311	30.892378
512.059133	30397.726160	30.897396
512.294887	30444.257062	30.902413
512.409074	30483.679062	30.907431
513.092379	30525.372984	30.912448
513.088832	30579.644481	30.917466
513.925357	30627.399357	30.922484
514.363032	30689.514269	30.927501
515.127327	30736.258110	30.932519
515.587425	30796.495924	30.937536
515.640747	30857.790099	30.942554
516.322332	30913.841700	30.947572
517.001590	30976.511823	30.952589
517.762497	31037.670323	30.957607
518.330046	31068.420816	30.962624
518.464034	31130.924630	30.967642
519.260385	31185.296099	30.972660
519.892420	31225.734363	30.977677
520.701216	31277.927558	30.982695
522.012171	31320.355718	30.987712
522.350443	31351.066032	30.992730
522.977178	31395.855641	30.997748
523.647939	31448.003592	31.002765
524.218812	31470.671943	31.007783
524.594468	31510.168241	31.012800
524.707297	31557.221510	31.017818
525.480053	31594.326809	31.022836
526.059328	31633.285030	31.027853
526.513259	31677.626937	31.032871
527.073682	31709.976407	31.037888
527.097439	31764.234853	31.042906
527.627162	31795.582218	31.047924
528.020360	31852.953345	31.052941
528.517566	31900.862123	31.057959
529.025318	31953.163733	31.062976
529.254965	32001.594578	31.067994
529.840797	32049.161827	31.073012
530.635016	32102.553136	31.078029
531.118705	32151.208756	31.083047
532.691296	32183.754164	31.088064
533.444657	32218.841705	31.093082
533.884507	32243.823788	31.098100
534.313669	32278.212820	31.103117
534.982866	32306.900379	31.108135
535.579701	32338.452455	31.113152
536.140904	32374.002815	31.118170
536.431197	32410.189058	31.123188
536.653564	32447.453301	31.128205
537.314849	32487.530634	31.133223
537.905515	32531.533088	31.138240
537.738478	32572.437674	31.143258
538.232511	32607.315150	31.148276
538.474350	32658.904759	31.153293
538.778575	32694.361183	31.158311
539.425755	32732.988061	31.163328
539.484418	32803.498638	31.168346
539.859954	32853.740353	31.173364
540.406322	32914.884831	31.178381
540.880229	32985.826569	31.183399
541.415342	33033.786194	31.188416
541.807454	33098.426880	31.193434
542.477172	33164.038733	31.198452
542.893227	33231.294339	31.203469
543.343170	33300.292940	31.208487
543.982543	33362.513482	31.213504
544.424293	33422.943515	31.218522
545.026035	33490.957180	31.223540
545.596933	33552.007099	31.228557
545.875776	33635.205517	31.233575
546.856789	33692.148914	31.238592
547.136494	33764.787952	31.243610
547.609917	33830.332818	31.248628
548.375389	33909.553633	31.253645
548.954533	33980.973112	31.258663
549.697227	34049.657064	31.263680
550.167743	34119.004167	31.268698
550.748949	34183.609501	31.273716
551.495969	34243.286101	31.278733
552.020379	34300.124598	31.283751
552.756078	34363.386581	31.288768
553.263325	34427.101361	31.293786
553.918169	34486.333202	31.298804
554.827398	34545.958254	31.303821
555.209129	34619.606291	31.308839
555.997533	34657.981853	31.313856
556.568832	34735.787211	31.318874
556.914791	34793.270623	31.323892
557.639179	34839.761295	31.328909
558.199542	34910.691172	31.333927
558.929624	34958.442432	31.338944
559.107821	35022.569750	31.343962
559.829907	35079.358928	31.348980
560.425212	35130.080144	31.353997
560.666852	35189.452809	31.359015
561.811113	35244.313488	31.364032
562.208882	35310.366512	31.369050
562.649573	35366.331258	31.374068
563.530898	35423.882919	31.379085
563.580890	35482.867798	31.384103
564.342254	35534.511277	31.389120
564.971872	35588.222217	31.394138
565.567356	35641.796880	31.399156
566.137634	35698.995437	31.404173
566.365230	35761.143903	31.409191
567.425376	35804.623059	31.414208
567.611127	35861.030502	31.419226
567.924084	35925.351072	31.424244
569.047904	35965.598040	31.429261
569.111991	36029.160906	31.434279
569.591053	36078.270195	31.439296
570.091569	36144.885591	31.444314
570.508258	36195.279025	31.449332
571.223680	36250.537657	31.454349
571.496232	36326.081991	31.459367
572.493846	36372.998509	31.464384
572.875529	36446.809097	31.469402
573.463613	36510.421190	31.474420
574.150140	36568.118170	31.479437
574.470190	36632.831318	31.484455
575.183923	36688.831095	31.489472
575.594151	36768.181947	31.494490
576.391493	36831.490749	31.499508
577.197769	36886.826874	31.504525
577.335299	36953.347194	31.509543
578.451591	37013.772655	31.514560
578.907567	37071.367757	31.519578
579.583668	37132.560630	31.524596
580.665914	37187.795460	31.529613
581.039012	37243.785113	31.534631
581.886925	37293.502991	31.539648
582.425843	37355.729172	31.544666
582.885694	37412.415077	31.549684
583.520100	37468.896784	31.554701
583.722756	37533.693576	31.559719
584.367554	37578.139046	31.564736
584.799765	37638.434458	31.569754
585.429523	37706.295241	31.574772
586.025275	37767.025468	31.579789
586.190763	37833.808115	31.584807
586.759102	37897.797544	31.589824
587.770931	37975.844184	31.594842
588.077034	38040.136076	31.599860
588.744093	38103.374221	31.604877
589.048355	38176.017408	31.609895
589.991504	38238.362216	31.614912
590.563325	38306.365504	31.619930
590.778016	38375.794583	31.624948
591.911664	38428.013644	31.629965
592.430394	38494.961816	31.634983
593.037671	38560.513302	31.640000
593.227510	38633.025296	31.645018
593.874588	38702.498806	31.650036
594.813896	38774.425316	31.655053
595.008351	38835.625370	31.660071
595.903776	38909.216678	31.665088
596.729671	38968.985814	31.670106
597.155553	39038.320896	31.675124
597.947719	39096.099571	31.680141
598.296140	39159.920643	31.685159
599.203861	39221.710199	31.690176
599.784681	39279.849565	31.695194
600.348972	39326.603629	31.700212
601.141133	39379.480792	31.705229
601.479974	39439.922051	31.710247
601.804706	39493.954168	31.715264
602.852226	39552.078489	31.720282
603.425712	39607.771239	31.725300
603.966894	39651.893313	31.730317
604.254832	39711.044276	31.735335
605.117840	39773.333375	31.740352
605.563329	39843.885989	31.745370
605.510729	39908.907528	31.750388
606.477358	39967.981266	31.755405
607.113344	40037.077225	31.760423
607.691177	40101.652179	31.765440
608.780108	40165.658714	31.770458
608.816226	40238.299789	31.775476
609.696468	40300.465067	31.780493
610.122309	40365.610851	31.785511
610.961652	40429.233917	31.790528
611.554062	40498.308718	31.795546
611.959104	40572.128810	31.800564
612.959298	40634.771376	31.805581
613.156963	40707.833428	31.810599
613.819800	40774.589410	31.815616
614.826361	40849.841449	31.820634
615.188865	40910.312527	31.825652
615.891407	40975.599504	31.830669
616.592722	41034.105720	31.835687
617.365225	41092.840510	31.840704
618.324924	41169.347268	31.845722
618.797150	41229.111257	31.850740
619.673388	41287.568407	31.855757
620.073097	41355.923524	31.860775
620.660742	41413.140182	31.865792
621.173011	41471.539214	31.870810
621.870867	41542.743088	31.875828
622.577658	41599.181245	31.880845
623.259332	41668.356943	31.885863
623.609952	41722.168026	31.890880
624.283146	41783.201462	31.895898
624.566175	41857.898142	31.900916
625.186851	41931.188224	31.905933
626.005571	42000.274042	31.910951
626.372741	42064.845779	31.915968
627.211453	42125.270538	31.920986
627.804240	42198.219231	31.926004
628.622501	42262.467539	31.931021
629.062133	42327.205360	31.936039
629.521689	42395.113474	31.941056
630.425899	42465.042359	31.946074
630.755249	42541.229766	31.951092
632.089659	42598.656351	31.956109
632.808340	42656.935062	31.961127
633.250921	42709.816671	31.966144
633.975133	42759.723194	31.971162
634.844857	42820.183306	31.976180
635.063854	42870.870867	31.981197
635.660382	42920.296639	31.986215
636.374795	42975.807549	31.991232
636.859343	43031.834711	31.996250
637.351355	43098.175833	32.001268
637.833744	43163.657580	32.006285
638.289128	43227.437318	32.011303
639.131719	43287.048529	32.016320
639.602401	43349.277441	32.021338
640.095007	43425.237706	32.026356
640.597098	43493.007717	32.031373
641.108101	43569.514567	32.036391
641.625071	43643.162805	32.041408
642.441151	43711.473569	32.046426
643.152889	43793.952530	32.051444
643.687138	43853.788290	32.056461
644.400468	43938.191966	32.061479
645.060995	44016.121773	32.066496
645.991501	44086.535681	32.071514
646.646210	44170.205332	32.076532
647.161344	44237.405186	32.081549
647.726787	44318.575523	32.086567
648.484552	44390.052891	32.091584
649.111952	44465.699704	32.096602
649.763348	44543.295778	32.101620
650.923925	44612.978000	32.106637
651.657446	44682.299460	32.111655
652.616640	44734.650707	32.116672
653.473791	44797.063028	32.121690
654.250408	44861.652550	32.126708
654.882061	44917.309042	32.131725
655.205794	44976.169506	32.136743
655.593529	45039.995060	32.141760
656.453393	45092.148674	32.146778
656.902081	45172.978781	32.151796
657.626406	45238.988223	32.156813
658.404012	45303.973578	32.161831
658.816992	45379.608021	32.166848
659.345828	45444.043552	32.171866
660.064754	45524.434746	32.176884
660.606748	45593.654663	32.181901
661.102054	45673.690942	32.186919
661.736955	45749.193846	32.191936
662.463009	45816.334649	32.196954
662.655196	45904.635651	32.201972
663.118323	45988.956583	32.206989
663.899034	46067.826058	32.212007
664.513279	46154.878009	32.217024
665.308565	46238.863307	32.222042
666.142101	46321.126594	32.227060
667.018545	46388.431789	32.232077
667.454914	46463.893660	32.237095
667.982047	46539.000658	32.242112
668.855238	46615.579928	32.247130
669.811598	46687.255925	32.252148
670.217321	46754.795227	32.257165
671.322586	46822.071964	32.262183
672.079378	46888.451598	32.267200
673.383229	46933.529362	32.272218
674.405652	46979.926720	32.277236
675.069971	47024.557550	32.282253
675.581094	47077.012396	32.287271
676.524827	47139.476080	32.292288
677.132635	47187.564905	32.297306
677.467885	47246.371205	32.302324
677.615194	47305.084571	32.307341
678.108315	47372.473499	32.312359
678.552324	47437.040283	32.317376
679.264159	47520.934560	32.322394
679.838077	47596.294193	32.327412
680.483222	47658.898761	32.332429
681.152083	47735.007439	32.337447
681.342452	47819.320616	32.342464
682.138266	47899.584221	32.347482
682.872125	47980.419698	32.352500
683.629210	48061.911309	32.357517
684.425013	48131.709781	32.362535
684.834387	48228.396803	32.367552
685.894658	48302.867935	32.372570
686.392825	48390.473198	32.377588
687.098015	48465.967094	32.382605
687.962592	48544.682847	32.387623
688.305467	48632.768409	32.392640
689.532759	48706.968527	32.397658
689.885772	48793.914163	32.402676
690.166409	48880.524646	32.407693
690.999064	48954.495171	32.412711
691.504888	49058.959081	32.417728
692.374984	49144.808039	32.422746
692.970564	49232.556567	32.427764
693.645615	49327.203513	32.432781
694.526946	49405.324016	32.437799
695.595436	49486.627438	32.442816
696.609451	49570.142503	32.447834
697.333044	49646.891256	32.452852
698.150113	49729.100447	32.457869
698.845813	49802.392602	32.462887
699.111826	49883.386962	32.467904
699.914442	49956.612238	32.472922
700.303369	50049.140636	32.477940
700.825771	50137.201900	32.482957
701.760549	50217.854629	32.487975
702.059690	50309.849578	32.492992
702.923256	50393.966794	32.498010
703.626093	50490.480525	32.503028
704.215298	50574.995715	32.508045
704.964598	50651.801498	32.513063
705.923257	50738.963146	32.518080
706.714649	50814.431182	32.523098
707.629097	50902.468511	32.528116
708.286228	50969.387366	32.533133
709.361933	51031.288314	32.538151
709.849642	51110.170072	32.543168
710.887004	51172.705629	32.548186
711.863317	51240.606653	32.553204
712.530075	51304.716494	32.558221
712.962660	51376.283374	32.563239
713.596535	51443.251882	32.568256
714.213366	51523.686547	32.573274
715.216904	51599.824733	32.578292
715.821765	51661.941679	32.583309
716.195600	51736.627961	32.588327
716.561500	51820.247244	32.593344
717.976249	51893.935289	32.598362
718.640444	51967.541139	32.603380
718.885788	52048.403386	32.608397
719.735983	52135.655361	32.613415
720.052864	52218.773017	32.618432
721.021259	52295.071230	32.623450
721.479066	52384.719209	32.628468
721.836323	52478.369789	32.633485
722.742069	52554.423429	32.638503
723.414236	52659.879173	32.643520
723.965416	52740.964103	32.648538
725.132934	52836.419109	32.653556
725.445283	52931.373209	32.658573
726.149753	53029.942349	32.663591
726.788232	53125.893407	32.668608
728.010215	53216.752622	32.673626
728.682429	53298.076434	32.678644
729.574560	53403.488867	32.683661
730.463298	53484.999988	32.688679
730.998475	53583.583307	32.693696
732.268598	53672.038363	32.698714
732.965963	53758.561827	32.703732
733.629704	53842.875309	32.708749
734.273608	53926.340126	32.713767
734.739880	54019.933969	32.718784
735.319449	54110.012987	32.723802
736.266358	54193.705401	32.728820
737.037497	54287.179490	32.733837
738.263650	54358.893824	32.738855
738.640464	54463.797877	32.743872
739.405083	54541.826690	32.748890
740.619769	54629.714446	32.753908
740.859866	54715.513508	32.758925
742.215812	54785.365475	32.763943
742.542579	54872.767605	32.768960
743.284883	54953.115454	32.773978
744.257508	55044.304435	32.778996
744.611440	55133.215470	32.784013
745.300432	55207.805896	32.789031
745.727125	55303.941038	32.794048
746.377101	55380.779557	32.799066
746.990327	55476.829095	32.804084
747.875482	55564.581256	32.809101
748.478374	55652.808073	32.814119
749.379906	55736.783102	32.819136
750.372402	55810.304912	32.824154
751.370018	55895.247100	32.829172
751.728341	55968.264409	32.834189
752.917146	56058.454924	32.839207
753.459115	56138.249559	32.844224
754.173883	56225.798409	32.849242
754.997102	56304.220006	32.854260
755.394315	56385.105739	32.859277
756.187656	56484.695878	32.864295
756.736273	56574.845622	32.869312
757.869600	56660.751515	32.874330
758.675552	56761.663854	32.879348
759.756157	56848.955399	32.884365
760.529415	56938.212501	32.889383
761.178647	57022.482961	32.894400
761.736496	57111.045948	32.899418
762.884911	57185.909069	32.904436
763.085726	57288.022373	32.909453
764.094408	57391.598747	32.914471
764.841493	57470.469930	32.919488
765.146472	57569.963719	32.924506
766.312068	57641.722648	32.929524
767.011435	57750.868687	32.934541
767.791979	57835.339787	32.939559
768.444853	57925.283794	32.944576
769.194234	58027.923168	32.949594
770.224083	58118.057514	32.954612
770.691802	58213.393094	32.959629
771.618601	58313.751652	32.964647
772.448950	58404.430596	32.969664
772.902077	58511.375595	32.974682
773.803235	58614.126652	32.979700
774.506207	58712.931790	32.984717
775.347716	58807.137482	32.989735
776.260475	58903.469735	32.994752
776.671386	59003.907821	32.999770
777.565923	59103.748525	33.004788
778.414566	59213.150918	33.009805
779.058397	59313.174725	33.014823
779.924833	59414.805427	33.019840
780.662109	59522.910774	33.024858
781.666842	59622.184186	33.029876
782.302339	59716.310444	33.034893
783.336123	59818.586063	33.039911
784.647548	59912.690973	33.044928
785.386679	60011.228858	33.049946
786.223115	60090.974693	33.054964
786.857970	60199.715950	33.059981
787.725173	60275.533001	33.064999
788.961930	60350.495862	33.070016
789.707161	60434.883338	33.075034
790.780215	60490.122912	33.080052
791.222862	60579.045964	33.085069
791.985680	60633.097605	33.090087
792.730808	60710.868236	33.095104
793.366538	60790.506907	33.100122
794.607376	60868.028784	33.105140
795.025874	60953.364180	33.110157
795.893808	61029.395721	33.115175
796.509752	61106.260228	33.120192
796.958528	61195.826211	33.125210
797.787427	61281.546152	33.130228
798.350774	61375.032282	33.135245
798.932156	61464.698426	33.140263
799.770002	61567.188441	33.145280
799.951717	61674.854657	33.150298
800.962891	61767.703077	33.155316
801.434509	61877.114711	33.160333
802.263757	61978.433663	33.165351
803.406659	62093.148880	33.170368
804.013743	62194.630660	33.175386
804.574168	62298.157173	33.180404
805.556643	62421.558530	33.185421
806.356978	62520.339807	33.190439
807.288923	62634.349798	33.195456
807.870894	62759.067597	33.200474
808.902240	62867.224307	33.205492
809.622961	62990.175242	33.210509
810.054625	63085.954991	33.215527
810.937697	63213.441544	33.220544
811.817942	63330.994509	33.225562
813.116439	63440.201454	33.230580
813.713151	63558.713604	33.235597
814.824530	63664.449417	33.240615
815.672125	63793.164490	33.245632
816.464025	63900.499891	33.250650
817.247983	64007.505565	33.255668
818.052205	64124.642874	33.260685
818.887402	64238.775783	33.265703
819.943171	64339.764947	33.270720
820.592550	64459.569135	33.275738
821.860704	64554.269376	33.280756
822.801813	64666.951031	33.285773
823.413503	64768.414223	33.290791
824.575273	64866.600627	33.295808
825.091164	64982.699504	33.300826
825.913186	65085.940561	33.305844
826.735345	65199.497003	33.310861
827.291501	65302.238317	33.315879
828.151400	65409.975625	33.320896
828.944730	65517.746239	33.325914
830.164697	65620.014087	33.330932
830.535870	65743.846901	33.335949
831.265633	65848.354284	33.340967
832.451002	65941.833324	33.345984
832.962268	66054.477831	33.351002
833.647599	66149.616656	33.356020
834.331135	66255.523305	33.361037
835.092624	66366.440054	33.366055
836.186991	66458.656916	33.371072
837.718964	66559.727266	33.376090
839.095788	66646.571729	33.381108
840.085870	66738.465410	33.386125
840.846075	66833.440925	33.391143
841.728132	66916.414034	33.396160
842.099200	67012.008256	33.401178
842.949119	67109.042855	33.406196
843.638127	67193.128103	33.411213
844.567642	67291.464917	33.416231
845.680225	67386.526045	33.421248
846.250281	67489.381026	33.426266
847.291638	67584.107010	33.431284
848.051760	67681.133494	33.436301
848.914021	67778.093670	33.441319
849.914240	67879.498763	33.446336
850.439045	67990.929969	33.451354
851.037653	68085.210829	33.456372
852.015022	68185.995729	33.461389
852.958990	68289.755697	33.466407
853.975069	68390.074316	33.471424
854.869208	68493.868572	33.476442
855.935834	68585.070204	33.481460
856.926809	68677.674183	33.486477
857.603164	68789.717603	33.491495
858.485100	68882.959041	33.496512
859.195214	68990.891734	33.501530
859.785434	69100.423547	33.506548
860.321592	69212.668599	33.511565
861.213857	69319.992882	33.516583
862.167290	69419.423308	33.521600
862.958492	69531.383202	33.526618
863.984932	69647.071800	33.531636
864.737225	69770.973866	33.536653
865.469263	69870.498674	33.541671
866.488661	69980.181918	33.546688
867.212613	70095.687527	33.551706
867.927061	70215.700157	33.556724
869.182930	70318.618849	33.561741
870.056508	70440.123885	33.566759
870.971730	70554.237017	33.571776
872.120292	70675.598656	33.576794
872.700656	70778.507200	33.581812
873.341651	70894.757304	33.586829
874.129121	71008.773347	33.591847
875.135048	71113.606210	33.596864
876.027014	71240.736647	33.601882
876.769615	71357.162856	33.606900
877.730175	71469.498567	33.611917
878.531839	71588.046082	33.616935
879.191203	71688.274034	33.621952
880.053953	71801.543391	33.626970
881.058351	71918.051292	33.631988
881.266538	72022.984320	33.637005
882.254538	72152.594899	33.642023
883.143074	72257.155515	33.647040
883.770188	72380.291382	33.652058
884.565210	72504.633471	33.657076
885.351919	72624.251121	33.662093
886.094147	72760.520660	33.667111
887.059849	72880.035536	33.672128
888.006365	73022.441685	33.677146
888.972497	73145.041767	33.682164
889.991145	73269.163469	33.687181
890.724932	73421.982291	33.692199
891.714531	73541.863839	33.697216
892.951168	73665.011753	33.702234
894.020877	73785.476021	33.707252
895.383110	73900.333479	33.712269
895.813521	74035.650239	33.717287
897.243845	74151.357734	33.722304
897.852277	74276.302962	33.727322
899.060442	74397.500889	33.732340
900.026974	74512.822947	33.737357
900.741005	74637.488199	33.742375
902.012518	74759.310183	33.747392
902.786405	74883.057414	33.752410
903.339990	75008.205503	33.757428
903.852464	75135.604400	33.762445
904.776643	75267.495120	33.767463
905.650188	75388.215079	33.772480
906.265996	75521.243523	33.777498
906.908443	75670.245201	33.782516
908.283015	75808.103251	33.787533
908.560394	75956.236095	33.792551
909.667240	76079.451038	33.797568
910.527248	76226.311313	33.802586
911.848461	76362.746982	33.807604
913.005288	76493.850266	33.812621
914.127175	76630.243608	33.817639
915.369468	76755.697405	33.822656
916.243797	76884.016709	33.827674
917.482726	77003.455706	33.832692
918.738552	77130.123153	33.837709
919.392018	77252.014239	33.842727
920.008075	77379.208492	33.847744
920.813587	77503.510238	33.852762
921.506019	77622.098071	33.857780
922.654649	77754.000834	33.862797
923.528817	77891.933675	33.867815
924.818990	78009.992535	33.872832
925.750790	78144.207725	33.877850
926.403260	78260.858866	33.882868
927.459760	78385.075470	33.887885
928.214196	78509.454661	33.892903
928.715701	78636.314668	33.897920
929.533131	78764.319826	33.902938
930.071114	78888.546126	33.907956
931.389142	79011.561872	33.912973
932.076746	79138.180455	33.917991
933.358934	79252.379326	33.923008
934.195568	79394.677061	33.928026
935.135610	79519.614360	33.933044
936.201442	79640.954669	33.938061
936.794403	79781.612432	33.943079
937.689429	79905.440389	33.948096
938.826226	80034.458258	33.953114
939.864410	80168.638116	33.958132
940.992962	80291.603148	33.963149
941.802083	80426.756674	33.968167
943.306755	80553.234968	33.973184
944.303430	80675.445733	33.978202
945.306093	80797.264336	33.983220
946.185136	80920.639440	33.988237
946.698656	81063.474163	33.993255
947.664765	81188.695532	33.998272
948.803893	81311.848253	34.003290
949.697616	81447.077135	34.008308
950.670754	81574.689286	34.013325
951.542177	81720.196210	34.018343
952.799798	81841.588416	34.023360
953.526220	81970.272683	34.028378
953.919233	82117.407326	34.033396
955.313977	82241.618547	34.038413
956.012870	82377.358590	34.043431
957.123899	82523.389311	34.048448
957.783616	82661.533450	34.053466
958.785235	82807.400218	34.058484
959.883954	82944.256220	34.063501
960.730332	83089.422604	34.068519
962.068632	83216.910805	34.073536
963.142045	83363.667761	34.078554
963.937795	83496.402897	34.083572
965.030744	83633.403391	34.088589
966.010547	83780.216075	34.093607
967.386585	83909.447432	34.098624
968.174401	84046.195677	34.103642
968.524800	84185.524410	34.108660
969.760328	84315.887038	34.113677
970.432382	84474.469095	34.118695
971.298732	84621.078054	34.123712
972.339208	84762.747641	34.128730
972.994483	84915.190066	34.133748
974.019315	85054.575282	34.138765
975.065532	85212.357246	34.143783
976.579410	85350.907873	34.148800
978.027552	85494.945448	34.153818
979.075686	85632.535057	34.158836
980.227055	85759.891280	34.163853
981.510906	85891.545773	34.168871
983.068831	85985.156255	34.173888
984.004202	86092.985498	34.178906
984.921954	86213.894175	34.183924
985.848832	86308.599187	34.188941
986.798852	86421.517845	34.193959
987.487266	86529.451808	34.198976
988.516976	86635.618438	34.203994
989.174851	86761.965231	34.209012
990.025110	86878.038485	34.214029
990.679184	87003.343966	34.219047
991.493886	87136.762753	34.224064
992.564059	87265.298026	34.229082
993.324207	87396.532895	34.234100
994.424108	87526.506738	34.239117
995.345608	87659.203550	34.244135
996.398445	87798.570577	34.249152
997.624815	87919.085648	34.254170
998.080341	88064.057232	34.259188
999.267262	88197.290580	34.264205
999.992198	88347.874549	34.269223
1000.982453	88478.674679	34.274240
1001.998487	88619.987921	34.279258
1002.745058	88776.844608	34.284276
1004.106589	88924.352803	34.289293
1004.411655	89084.854927	34.294311
1005.242084	89235.478869	34.299328
1006.387382	89378.610432	34.304346
1007.313254	89548.193329	34.309364
1008.488850	89709.257223	34.314381
1009.586298	89879.093661	34.319399
1010.484681	90040.185125	34.324416
1011.916104	90193.445810	34.329434
1012.731326	90361.617031	34.334452
1013.956227	90514.969742	34.339469
1014.947725	90668.847630	34.344487
1015.909886	90812.669140	34.349504
1017.112567	90968.760705	34.354522
1018.200201	91120.754436	34.359540
1019.620473	91275.561323	34.364557
1020.865520	91415.844320	34.369575
1022.038792	91569.484573	34.374592
1023.247840	91696.196130	34.379610
1024.118342	91848.267377	34.384628
1025.271706	91993.704297	34.389645
1026.322197	92133.314441	34.394663
1027.527343	92274.058310	34.399680
1028.571440	92409.756155	34.404698
1030.334886	92524.360730	34.409716
1031.669443	92648.774509	34.414733
1032.472738	92781.325173	34.419751
1032.912711	92902.378640	34.424768
1034.645423	93027.705268	34.429786
1035.809420	93160.283049	34.434804
1036.773572	93287.093282	34.439821
1037.718448	93405.324083	34.444839
1038.125864	93531.123687	34.449856
1038.676253	93649.121247	34.454874
1039.595895	93777.725066	34.459892
1040.597122	93900.459436	34.464909
1041.191984	94050.236620	34.469927
1041.550065	94179.545632	34.474944
1043.086658	94313.443618	34.479962
1043.836226	94463.692345	34.484980
1044.711494	94606.919776	34.489997
1045.733711	94763.604445	34.495015
1046.111137	94916.300122	34.500032
1047.696119	95080.456552	34.505050
1048.649034	95248.611326	34.510068
1049.288039	95399.737872	34.515085
1050.864704	95552.392616	34.520103
1052.234158	95717.233206	34.525120
1053.668413	95863.238997	34.530138
1054.229437	96024.111272	34.535156
1054.860368	96180.703573	34.540173
1055.893160	96343.812050	34.545191
1056.954367	96517.177986	34.550208
1058.112757	96679.035329	34.555226
1059.046939	96858.351602	34.560244
1060.120877	97025.488179	34.565261
1061.131101	97203.650049	34.570279
1061.897906	97382.503636	34.575296
1063.499234	97543.904467	34.580314
1064.004887	97727.395197	34.585332
1065.261775	97888.865908	34.590349
1066.940141	98063.145047	34.595367
1068.514739	98231.058588	34.600384
1069.911126	98383.292908	34.605402
1070.873849	98551.742652	34.610420
1072.080323	98704.793813	34.615437
1073.269858	98862.454505	34.620455
1074.068083	99022.962271	34.625472
1075.447969	99179.221968	34.630490
1076.028593	99353.337546	34.635508
1077.270184	99510.905833	34.640525
1078.537166	99670.312286	34.645543
1079.101380	99829.648131	34.650560
1080.131121	100001.425803	34.655578
1081.063471	100167.677765	34.660596
1082.559997	100333.910792	34.665613
1084.025039	100490.849160	34.670631
1084.644127	100664.405387	34.675648
1086.201034	100812.365735	34.680666
1086.854615	100984.507903	34.685684
1088.311421	101149.664812	34.690701
1089.460332	101299.078827	34.695719
1090.461387	101467.967680	34.700736
1091.573041	101619.933287	34.705754
1092.592075	101790.125063	34.710772
1093.880012	101952.125477	34.715789
1094.815965	102103.786819	34.720807
1095.839643	102257.067713	34.725824
1097.183678	102395.498327	34.730842
1098.002671	102544.010979	34.735860
1099.267380	102689.220227	34.740877
1100.219858	102844.427255	34.745895
1101.304677	102997.513435	34.750912
1102.387553	103138.679281	34.755930
1103.312659	103292.621728	34.760948
1103.960574	103454.285025	34.765965
1105.164516	103612.924830	34.770983
1105.670501	103785.680572	34.776000
1106.883023	103948.706577	34.781018
1108.409666	104121.878313	34.786036
1109.552798	104290.264951	34.791053
1110.967352	104447.940303	34.796071
1111.876680	104607.291762	34.801088
1113.402485	104781.208855	34.806106
1114.079582	104935.948171	34.811124
1115.597865	105102.084986	34.816141
1117.363564	105262.291876	34.821159
1118.064506	105426.200439	34.826176
1119.239981	105580.447010	34.831194
1120.149113	105750.735449	34.836212
1121.071658	105912.492051	34.841229
1122.530441	106079.005863	34.846247
1123.383857	106243.224868	34.851264
1124.834043	106404.204733	34.856282
1125.579294	106585.378891	34.861300
1126.601405	106745.163366	34.866317
1128.289172	106918.899392	34.871335
1129.339565	107086.712935	34.876352
1130.905873	107231.224793	34.881370
1131.668524	107401.598865	34.886388
1132.830199	107568.277837	34.891405
1133.911254	107736.204944	34.896423
1134.914773	107908.765785	34.901440
1135.929940	108082.294363	34.906458
1137.289089	108257.415071	34.911476
1137.789577	108428.812755	34.916493
1139.168644	108610.996270	34.921511
1140.228658	108797.251007	34.926528
1141.408435	108968.879932	34.931546
1142.334485	109145.430391	34.936564
1143.335681	109328.445220	34.941581
1144.827722	109511.959354	34.946599
1145.629378	109698.420290	34.951616
1147.004167	109872.341173	34.956634
1147.999643	110066.565835	34.961652
1149.127535	110254.289361	34.966669
1151.288951	110422.215098	34.971687
1152.608966	110595.497854	34.976704
1153.773128	110761.204481	34.981722
1155.328794	110930.382041	34.986740
1156.031835	111097.056761	34.991757
1157.104857	111254.533311	34.996775
1157.977128	111416.625707	35.001792
1159.596288	111564.110939	35.006810
1160.914856	111716.778540	35.011828
1161.714117	111874.169632	35.016845
1163.096558	112023.752532	35.021863
1163.640529	112188.377267	35.026880
1164.845285	112339.262689	35.031898
1165.853782	112496.624453	35.036916
1166.957739	112673.735290	35.041933
1167.747735	112833.444491	35.046951
1168.906934	113022.405789	35.051968
1170.212337	113187.112289	35.056986
1171.186968	113367.945595	35.062004
1172.378755	113539.838605	35.067021
1173.626069	113713.217984	35.072039
1174.396226	113901.196894	35.077056
1175.473419	114076.182154	35.082074
1176.794439	114260.138479	35.087092
1178.255452	114445.397020	35.092109
1179.591960	114633.228037	35.097127
1180.419979	114832.853400	35.102144
1181.740918	115010.193124	35.107162
1182.981803	115191.604961	35.112180
1184.163684	115387.993968	35.117197
1185.655799	115562.866578	35.122215
1186.549640	115755.265016	35.127232
1187.877678	115948.007398	35.132250
1189.151692	116132.674900	35.137268
1190.125884	116328.065873	35.142285
1191.695077	116500.419172	35.147303
1193.445627	116685.261828	35.152320
1194.791094	116857.298553	35.157338
1195.810867	117041.398906	35.162356
1196.886020	117222.256400	35.167373
1198.647822	117390.165713	35.172391
1199.623063	117577.885950	35.177408
1200.472094	117758.928798	35.182426
1201.586482	117938.727719	35.187444
1202.773809	118124.050185	35.192461
1203.707619	118310.072787	35.197479
1204.569202	118508.132246	35.202496
1206.139413	118703.427523	35.207514
1207.274482	118891.062244	35.212532
1208.147210	119095.855197	35.217549
1209.284483	119283.283448	35.222567
1210.228095	119491.145577	35.227584
1211.556614	119689.152470	35.232602
1212.991693	119890.158008	35.237620
1214.231155	120097.186418	35.242637
1215.551909	120300.822142	35.247655
1216.469803	120504.916098	35.252672
1218.239259	120682.141268	35.257690
1219.759158	120868.931160	35.262708
1220.719839	121080.228997	35.267725
1222.306724	121261.755141	35.272743
1223.476430	121447.414316	35.277760
1224.315498	121619.626413	35.282778
1225.749153	121785.171900	35.287796
1226.937800	121976.315785	35.292813
1228.043767	122146.918396	35.297831
1229.684931	122330.748345	35.302848
1230.540936	122506.535159	35.307866
1231.953854	122676.307117	35.312884
1233.026417	122860.978400	35.317901
1234.627803	123035.674958	35.322919
1235.561765	123226.830333	35.327936
1236.512829	123417.528384	35.332954
1237.970950	123600.838906	35.337972
1239.091812	123786.268871	35.342989
1240.345721	123972.451604	35.348007
1241.609290	124168.222454	35.353024
1242.948685	124354.634908	35.358042
1244.282283	124533.095054	35.363060
1245.195558	124730.268324	35.368077
1246.477143	124926.130489	35.373095
1247.549162	125118.658045	35.378112
1248.827185	125326.785057	35.383130
1250.488443	125520.323813	35.388148
1251.612511	125714.734701	35.393165
1252.747600	125906.117798	35.398183
1254.489378	126115.532518	35.403200
1255.823944	126300.793773	35.408218
1257.059491	126480.929085	35.413236
1258.523745	126677.053531	35.418253
1259.983935	126867.568319	35.423271
1261.297103	127054.928235	35.428288
1262.194616	127242.051482	35.433306
1263.717972	127437.487928	35.438324
1264.808879	127632.677811	35.443341
1266.172712	127818.464070	35.448359
1267.559940	128016.624547	35.453376
1268.195422	128203.555294	35.458394
1269.871152	128402.888827	35.463412
1270.999433	128600.511919	35.468429
1272.375108	128796.399529	35.473447
1273.580598	128996.888904	35.478464
1274.413960	129204.381269	35.483482
1275.880883	129404.857367	35.488500
1276.914922	129610.648594	35.493517
1278.367733	129812.688131	35.498535
1279.216081	130027.950262	35.503552
1280.335449	130237.976651	35.508570
1281.906595	130440.825406	35.513588
1282.834750	130666.202410	35.518605
1284.328928	130877.073524	35.523623
1285.626571	131088.991015	35.528640
1287.083590	131304.685629	35.533658
1288.831255	131510.288672	35.538676
1289.888394	131722.236479	35.543693
1291.182380	131913.711805	35.548711
1292.718643	132118.098558	35.553728
1293.914351	132304.549523	35.558746
1295.440375	132489.732882	35.563764
1296.577586	132681.656420	35.568781
1298.003534	132868.264537	35.573799
1299.717414	133038.369364	35.578816
1300.652652	133225.919399	35.583834
1302.063665	133407.287869	35.588852
1303.721276	133608.713806	35.593869
1304.841833	133783.770202	35.598887
1305.643747	133982.141768	35.603904
1306.854234	134176.825906	35.608922
1308.062490	134368.698774	35.613940
1309.097660	134574.462493	35.618957
1310.450542	134786.309983	35.623975
1312.213218	134974.031335	35.628992
1313.086259	135182.701505	35.634010
1314.304590	135386.731265	35.639028
1315.088121	135596.913856	35.644045
1316.774842	135810.401066	35.649063
1317.703980	136037.214088	35.654080
1319.005636	136265.350881	35.659098
1320.533674	136475.294750	35.664116
1322.133458	136695.176173	35.669133
1323.411936	136914.413353	35.674151
1324.964565	137124.446667	35.679168
1326.359006	137346.266417	35.684186
1327.934269	137566.158255	35.689204
1328.928311	137784.826180	35.694221
1330.496636	137995.408117	35.699239
1331.740346	138215.915073	35.704256
1332.762397	138443.124717	35.709274
1334.516587	138651.654149	35.714292
1335.785789	138872.732202	35.719309
1336.694700	139103.728706	35.724327
1338.521234	139320.121219	35.729344
1339.831567	139544.784182	35.734362
1341.555350	139754.821587	35.739380
1343.032081	139968.410234	35.744397
1344.829805	140172.697805	35.749415
1346.564333	140378.986545	35.754432
1347.520620	140586.160796	35.759450
1349.634166	140783.482551	35.764468
1350.789613	140985.228912	35.769485
1352.099056	141171.071850	35.774503
1354.162965	141365.452293	35.779520
1355.436196	141566.461393	35.784538
1356.497063	141753.196557	35.789556
1357.874482	141953.545278	35.794573
1359.183504	142134.552654	35.799591
1360.491897	142325.231687	35.804608
1361.539455	142530.338779	35.809626
1363.253146	142718.864583	35.814644
1364.570722	142918.063085	35.819661
1365.584344	143106.930670	35.824679
1367.130410	143293.572776	35.829696
1367.982465	143487.474875	35.834714
1369.204158	143671.128870	35.839732
1370.252038	143861.579989	35.844749
1371.587553	144048.627693	35.849767
1372.570544	144241.132133	35.854784
1373.622911	144465.213256	35.859802
1374.947559	144661.329129	35.864820
1376.218018	144876.822763	35.869837
1377.378227	145094.743737	35.874855
1378.704450	145312.145503	35.879872
1379.716114	145549.524823	35.884890
1381.114760	145772.799761	35.889908
1382.471918	146003.663004	35.894925
1383.650459	146234.290131	35.899943
1385.208886	146470.905020	35.904960
1386.236399	146714.806063	35.909978
1387.664022	146952.700276	35.914996
1389.151599	147193.603699	35.920013
1390.267525	147442.782295	35.925031
1391.971878	147683.363425	35.930048
1393.389366	147934.234620	35.935066
1394.981257	148178.754415	35.940084
1396.644877	148421.502610	35.945101
1398.361035	148661.734279	35.950119
1399.416990	148890.688756	35.955136
1400.947192	149145.532075	35.960154
1402.391699	149375.518479	35.965172
1404.119405	149615.159597	35.970189
1405.020700	149861.031599	35.975207
1406.525239	150111.994671	35.980224
1408.108553	150368.537949	35.985242
1409.692812	150607.524597	35.990260
1411.410952	150858.091825	35.995277
1412.816310	151085.446906	36.000295
1414.211533	151329.425888	36.005312
1415.570740	151575.174646	36.010330
1417.354669	151814.442643	36.015348
1419.033635	152038.768817	36.020365
1420.512495	152274.221784	36.025383
1422.453608	152494.211469	36.030400
1424.000680	152718.981601	36.035418
1425.327568	152933.696147	36.040436
1427.220565	153160.823220	36.045453
1428.532554	153384.494130	36.050471
1429.905440	153599.205656	36.055488
1431.536884	153824.946107	36.060506
1432.419421	154048.613620	36.065524
1433.863876	154279.268229	36.070541
1435.237210	154508.312794	36.075559
1437.013451	154732.945936	36.080576
1438.033875	154955.988964	36.085594
1439.408839	155188.233058	36.090612
1440.764950	155412.392254	36.095629
1441.898274	155649.660920	36.100647
1443.591450	155862.307235	36.105664
1444.518103	156086.412310	36.110682
1445.615608	156302.795086	36.115700
1447.301826	156518.603857	36.120717
1448.638280	156745.957580	36.125735
1450.275168	156968.193066	36.130752
1451.665478	157183.000588	36.135770
1453.158325	157414.670474	36.140788
1454.655740	157632.608463	36.145805
1455.912861	157864.661184	36.150823
1457.444211	158087.808268	36.155840
1458.731469	158324.601755	36.160858
1460.275786	158554.267557	36.165876
1462.141247	158779.813350	36.170893
1463.094003	159025.528535	36.175911
1464.492420	159261.854208	36.180928
1466.081986	159500.167372	36.185946
1467.112557	159737.455032	36.190964
1468.331416	159997.844725	36.195981
1469.492516	160257.484639	36.200999
1471.139806	160506.054525	36.206016
1472.411572	160767.176983	36.211034
1473.913105	161027.123519	36.216052
1475.728979	161279.007255	36.221069
1476.740833	161551.006810	36.226087
1478.669330	161808.900179	36.231104
1480.099885	162084.489607	36.236122
1481.697406	162339.053307	36.241140
1483.694296	162600.390976	36.246157
1484.968101	162861.122529	36.251175
1486.789450	163119.892001	36.256192
1488.290622	163378.802960	36.261210
1489.856136	163640.990280	36.266228
1491.235733	163897.616041	36.271245
1492.653592	164149.151809	36.276263
1494.330287	164410.870412	36.281280
1495.854848	164673.046262	36.286298
1497.365168	164928.225308	36.291316
1499.018239	165195.368814	36.296333
1500.002037	165455.480026	36.301351
1501.651087	165718.201564	36.306368
1503.428906	165986.726094	36.311386
1504.681696	166245.430309	36.316404
1506.522128	166509.331933	36.321421
1507.759543	166765.886012	36.326439
1509.597087	167026.773070	36.331456
1511.001821	167299.780159	36.336474
1512.878835	167551.938233	36.341492
1514.688960	167800.379571	36.346509
1516.210988	168054.981945	36.351527
1517.839546	168305.560962	36.356544
1519.589563	168557.492213	36.361562
1520.805662	168816.080333	36.366580
1522.759388	169052.380977	36.371597
1524.010236	169301.288782	36.376615
1525.671299	169538.856604	36.381632
1527.079989	169762.627224	36.386650
1528.560468	169985.258813	36.391668
1530.247052	170215.977097	36.396685
1531.221845	170456.564350	36.401703
1532.682017	170688.272757	36.406720
1533.991901	170927.515844	36.411738
1535.317741	171173.087639	36.416756
1536.983819	171416.983248	36.421773
1538.032476	171662.069366	36.426791
1539.057499	171899.435498	36.431808
1540.531061	172176.322458	36.436826
1542.086665	172439.663069	36.441844
1543.830108	172702.721884	36.446861
1545.407526	172969.779375	36.451879
1547.081441	173228.146387	36.456896
1548.880013	173490.529311	36.461914
1550.431199	173760.108015	36.466932
1552.224241	174013.526414	36.471949
1553.614773	174285.823557	36.476967
1555.383930	174545.642799	36.481984
1556.754493	174817.769093	36.487002
1557.887625	175093.169896	36.492020
1559.571818	175367.964896	36.497037
1561.154475	175649.184477	36.502055
1562.401943	175924.382430	36.507072
1564.120780	176200.915560	36.512090
1565.247421	176492.489427	36.517108
1566.976082	176788.422758	36.522125
1568.686800	177074.871341	36.527143
1570.233915	177361.601622	36.532160
1571.711624	177663.924486	36.537178
1573.082213	177951.245083	36.542196
1574.966179	178236.050178	36.547213
1576.664733	178528.663920	36.552231
1578.437124	178821.445588	36.557248
1580.049334	179108.063275	36.562266
1581.590828	179397.942125	36.567284
1583.112348	179687.623121	36.572301
1584.999834	179979.785489	36.577319
1586.549895	180263.629534	36.582336
1588.083603	180558.592588	36.587354
1589.506231	180854.488832	36.592372
1591.149156	181146.456898	36.597389
1592.987382	181441.885135	36.602407
1594.415542	181736.961798	36.607424
1596.148596	182030.634390	36.612442
1597.604600	182324.657474	36.617460
1598.983879	182617.958783	36.622477
1600.828069	182916.986857	36.627495
1602.851140	183207.043086	36.632512
1604.585634	183493.746481	36.637530
1605.973058	183787.904392	36.642548
1607.705616	184073.254128	36.647565
1609.094000	184369.128706	36.652583
1610.488388	184643.483728	36.657600
1612.375582	184911.239971	36.662618
1613.806488	185184.475846	36.667636
1615.335296	185450.693367	36.672653
1617.003002	185730.569458	36.677671
1618.630832	186007.408149	36.682688
1620.625137	186290.471598	36.687706
1621.855335	186575.409300	36.692724
1623.840032	186846.346504	36.697741
1625.316552	187128.494860	36.702759
1627.074080	187392.631601	36.707776
1628.853804	187667.375023	36.712794
1630.345854	187956.594184	36.717812
1632.362001	188219.933151	36.722829
1634.088453	188487.113932	36.727847
1635.575600	188762.075214	36.732864
1637.584537	189025.889378	36.737882
1639.104941	189308.424610	36.742900
1640.652284	189578.812578	36.747917
1642.189556	189858.886473	36.752935
1643.616768	190140.147014	36.757952
1645.539692	190419.934521	36.762970
1647.094032	190707.244288	36.767988
1648.486198	190981.928867	36.773005
1650.169322	191268.422002	36.778023
1652.047897	191558.908795	36.783040
1653.787214	191846.881243	36.788058
1655.288604	192126.174437	36.793076
1657.121826	192409.541130	36.798093
1658.943786	192703.165705	36.803111
1660.619973	192987.322122	36.808128
1662.257758	193271.168982	36.813146
1663.948248	193564.235728	36.818164
1665.277582	193839.783871	36.823181
1667.181037	194135.904171	36.828199
1668.565574	194429.367226	36.833216
1670.331730	194723.126755	36.838234
1671.747307	195027.528576	36.843252
1673.448478	195305.868623	36.848269
1675.105713	195619.678324	36.853287
1676.400925	195920.347773	36.858304
1678.388828	196217.697899	36.863322
1679.723742	196532.376635	36.868340
1681.590669	196836.247892	36.873357
1683.572538	197140.381902	36.878375
1684.802851	197449.231647	36.883392
1686.847859	197753.067265	36.888410
1688.108315	198071.727119	36.893428
1690.091881	198380.932341	36.898445
1691.687085	198693.805739	36.903463
1693.420819	199010.441406	36.908480
1695.343455	199313.696131	36.913498
1696.909969	199627.798046	36.918516
1698.643404	199938.778207	36.923533
1700.111503	200243.861951	36.928551
1701.533994	200548.319991	36.933568
1703.680836	200830.972123	36.938586
1705.277471	201118.295321	36.943604
1706.861219	201410.229724	36.948621
1708.543196	201697.250440	36.953639
1710.682343	201992.374610	36.958656
1712.767292	202284.335579	36.963674
1714.225668	202578.263505	36.968692
1715.739343	202855.085895	36.973709
1717.565537	203151.776395	36.978727
1718.981133	203445.207880	36.983744
1720.979394	203734.181700	36.988762
1722.269297	204033.729195	36.993780
1724.100891	204344.197895	36.998797
1725.764724	204644.133489	37.003815
1727.086124	204952.731585	37.008832
1729.164909	205253.848471	37.013850
1731.475461	205555.844098	37.018868
1733.654960	205850.880242	37.023885
1735.798261	206147.243823	37.028903
1737.335390	206436.926322	37.033920
1739.285106	206728.893205	37.038938
1741.173874	207031.636145	37.043956
1743.096638	207311.575753	37.048973
1745.039265	207600.717123	37.053991
1746.278540	207891.406041	37.059008
1748.150016	208185.004643	37.064026
1749.585850	208481.365124	37.069044
1751.441312	208783.106525	37.074061
1753.406426	209073.901651	37.079079
1755.013900	209379.481131	37.084096
1757.146924	209657.100317	37.089114
1758.515846	209965.907010	37.094132
1760.247128	210274.683090	37.099149
1762.075354	210569.962941	37.104167
1763.220354	210881.018646	37.109184
1765.160732	211176.562817	37.114202
1767.181970	211486.733351	37.119220
1768.592500	211800.607855	37.124237
1770.631930	212105.116296	37.129255
1771.989183	212423.750421	37.134272
1774.177476	212727.146328	37.139290
1775.855865	213049.109577	37.144308
1777.435149	213357.365979	37.149325
1779.479984	213677.598282	37.154343
1780.734939	213994.961282	37.159360
1782.974359	214313.375631	37.164378
1784.690222	214634.845474	37.169396
1786.441452	214952.007259	37.174413
1788.050134	215273.903428	37.179431
1790.235379	215596.077784	37.184448
1792.656139	215884.952035	37.189466
1794.233098	216198.947810	37.194484
1796.288536	216514.773514	37.199501
1798.192070	216800.889702	37.204519
1799.642650	217100.791170	37.209536
1801.561598	217382.958678	37.214554
1803.372706	217662.135339	37.219572
1805.369453	217933.106994	37.224589
1807.315163	218206.030374	37.229607
1809.017145	218492.972590	37.234624
1810.857612	218766.486157	37.239642
1812.645218	219057.797417	37.244660
1814.006102	219344.263881	37.249677
1816.031998	219633.051024	37.254695
1817.355277	219922.319039	37.259712
1818.918699	220225.542204	37.264730
1820.239251	220530.214532	37.269748
1821.928833	220834.981891	37.274765
1824.206563	221137.663673	37.279783
1825.721362	221470.433264	37.284800
1827.504459	221805.079018	37.289818
1829.020612	222150.828005	37.294836
1831.167170	222465.420605	37.299853
1833.270997	222778.103948	37.304871
1834.775864	223114.259740	37.309888
1836.915300	223435.434699	37.314906
1838.494341	223764.026438	37.319924
1840.221056	224084.012469	37.324941
1841.990533	224422.798324	37.329959
1843.691826	224762.053545	37.334976
1846.000813	225089.087306	37.339994
1847.829933	225425.556880	37.345012
1849.426011	225759.741098	37.350029
1851.906034	226091.564223	37.355047
1853.559361	226436.992496	37.360064
1855.575950	226759.609564	37.365082
1857.725767	227082.460683	37.370100
1859.554052	227414.862301	37.375117
1861.702835	227740.636660	37.380135
1863.467953	228081.533303	37.385152
1865.785833	228399.410373	37.390170
1867.601123	228724.250884	37.395188
1869.629352	229057.033409	37.400205
1871.604612	229374.079488	37.405223
1873.306875	229703.792343	37.410240
1875.067540	230031.744736	37.415258
1877.042521	230360.578604	37.420276
1878.751705	230688.033591	37.425293
1880.967316	231012.869634	37.430311
1882.740263	231337.980249	37.435328
1884.727262	231658.156296	37.440346
1886.936168	231983.961896	37.445364
1888.840602	232312.077336	37.450381
1890.830328	232625.779800	37.455399
1892.964102	232942.711362	37.460416
1894.952336	233248.796718	37.465434
1896.975661	233566.636773	37.470452
1899.009309	233876.374208	37.475469
1901.379096	234161.549981	37.480487
1903.197052	234443.258380	37.485504
1905.343313	234721.639083	37.490522
1907.163606	234994.281437	37.495540
1908.406528	235270.902117	37.500557
1910.687927	235540.551931	37.505575
1912.471839	235825.393585	37.510592
1913.898498	236101.326969	37.515610
1915.705893	236389.341275	37.520628
1917.397223	236672.955388	37.525645
1919.262673	236969.165887	37.530663
1921.056711	237258.200625	37.535680
1923.149971	237551.227106	37.540698
1925.703913	237830.110165	37.545716
1927.323955	238136.471649	37.550733
1929.672713	238411.909056	37.555751
1931.132519	238724.037821	37.560768
1933.138641	239013.957898	37.565786
1935.048844	239310.116804	37.570804
1936.789334	239616.996606	37.575821
1938.325197	239924.468487	37.580839
1940.027093	240230.619454	37.585856
1942.302428	240540.921984	37.590874
1944.420753	240852.063036	37.595892
1945.685368	241176.294288	37.600909
1947.442391	241507.661858	37.605927
1949.382729	241836.512045	37.610944
1951.332323	242166.987248	37.615962
1953.296829	242488.647122	37.620980
1955.028414	242832.519149	37.625997
1957.151453	243177.422208	37.631015
1958.721859	243514.717584	37.636032
1960.804359	243868.722248	37.641050
1962.828271	244203.585216	37.646068
1964.571695	244563.436856	37.651085
1966.752933	244914.659996	37.656103
1968.733734	245260.073699	37.661120
1970.513139	245616.721948	37.666138
1972.783030	245961.735933	37.671156
1974.629850	246322.439418	37.676173
1976.921777	246666.638804	37.681191
1979.041279	247017.496028	37.686208
1981.178157	247356.438256	37.691226
1983.430986	247697.648966	37.696244
1985.484256	248055.402870	37.701261
1987.803395	248391.143390	37.706279
1990.100839	248725.491021	37.711296
1991.976379	249072.429163	37.716314
1994.232241	249397.487950	37.721332
1996.063382	249738.135058	37.726349
1998.504370	250069.973425	37.731367
2000.422753	250409.007809	37.736384
2002.610636	250733.673639	37.741402
2004.882447	251063.584920	37.746420
2006.785682	251385.147362	37.751437
2008.492795	251702.372421	37.756455
2010.422536	252015.701668	37.761472
2012.209000	252317.039142	37.766490
2014.577906	252601.875123	37.771508
2016.648473	252886.784284	37.776525
2018.806362	253201.146278	37.781543
2020.964183	253489.446385	37.786560
2022.558142	253781.748295	37.791578
2024.877171	254085.010920	37.796596
2026.433183	254393.678699	37.801613
2028.151944	254698.053585	37.806631
2030.594898	255007.902525	37.811648
2032.809804	255300.565418	37.816666
2034.584811	255621.012361	37.821684
2036.028037	255927.795193	37.826701
2037.918289	256251.044461	37.831719
2040.198301	256578.271357	37.836736
2041.820583	256910.480337	37.841754
2044.056171	257231.440850	37.846772
2046.427285	257555.072976	37.851789
2048.641835	257877.434862	37.856807
2050.890841	258199.486890	37.861824
2052.864294	258535.046421	37.866842
2054.620706	258871.631539	37.871860
2056.340781	259210.229679	37.876877
2058.663632	259541.772315	37.881895
2060.516927	259879.715128	37.886912
2061.960220	260230.602590	37.891930
2063.952924	260574.747823	37.896948
2065.952288	260935.709073	37.901965
2068.411013	261286.512985	37.906983
2070.588576	261645.541634	37.912000
2072.483474	262010.051762	37.917018
2074.786140	262363.904618	37.922036
2076.873621	262727.800757	37.927053
2078.865338	263086.936728	37.932071
2081.115246	263450.325231	37.937088
2082.831563	263815.195914	37.942106
2084.884375	264172.494287	37.947124
2087.004212	264543.855672	37.952141
2089.066250	264904.150831	37.957159
2091.323789	265291.876078	37.962176
2093.207950	265661.294434	37.967194
2095.816089	266030.191823	37.972212
2097.872192	266399.710540	37.977229
2100.324534	266756.795339	37.982247
2102.583318	267126.714323	37.987264
2104.303519	267501.799646	37.992282
2106.256731	267861.250672	37.997300
2108.709996	268226.566980	38.002317
2110.778572	268601.267533	38.007335
2112.781988	268971.660083	38.012352
2114.766841	269353.360257	38.017370
2117.159573	269716.934177	38.022388
2119.142186	270092.766920	38.027405
2121.115734	270452.393935	38.032423
2123.232191	270800.490709	38.037440
2125.100276	271142.555596	38.042458
2127.679104	271480.671963	38.047476
2129.454240	271833.700665	38.052493
2131.450723	272175.085011	38.057511
2133.919596	272523.151824	38.062528
2135.818372	272874.586168	38.067546
2137.877541	273219.263238	38.072564
2139.809085	273586.137779	38.077581
2141.616488	273939.923896	38.082599
2144.028748	274310.964655	38.087616
2145.716149	274679.808684	38.092634
2148.333512	275041.443094	38.097652
2150.805556	275407.723974	38.102669
2152.873175	275773.738736	38.107687
2154.919857	276139.655181	38.112704
2157.004510	276519.969304	38.117722
2159.758759	276880.819791	38.122740
2161.618704	277249.839520	38.127757
2163.967730	277622.287284	38.132775
2166.758533	277985.494281	38.137792
2168.388127	278355.541017	38.142810
2170.757672	278728.975966	38.147828
2172.975787	279095.017022	38.152845
2175.135034	279469.679019	38.157863
2177.589872	279832.227401	38.162880
2179.830874	280215.665677	38.167898
2182.061330	280580.764244	38.172916
2184.161521	280942.631664	38.177933
2186.829827	281306.466474	38.182951
2189.096331	281663.404300	38.187968
2191.283055	282036.257015	38.192986
2193.828878	282393.353343	38.198004
2196.394579	282756.670083	38.203021
2198.518298	283121.403030	38.208039
2200.520604	283478.838848	38.213056
2202.810288	283852.309043	38.218074
2205.094492	284209.140742	38.223092
2207.136247	284571.370661	38.228109
2209.163887	284938.784748	38.233127
2211.660255	285304.472984	38.238144
2213.547056	285676.557501	38.243162
2215.600722	286040.968884	38.248180
2218.013898	286405.348310	38.253197
2219.891016	286770.371230	38.258215
2222.334007	287138.479414	38.263232
2224.312520	287527.567457	38.268250
2226.391676	287899.288899	38.273268
2228.469348	288285.820015	38.278285
2230.459615	288669.138346	38.283303
2232.784200	289052.504791	38.288320
2234.859488	289437.815467	38.293338
2237.089187	289822.491473	38.298356
2239.528287	290213.281195	38.303373
2241.337840	290591.138603	38.308391
2243.793397	290948.367720	38.313408
2245.861489	291319.857823	38.318426
2248.209813	291682.716882	38.323444
2250.072682	292048.167224	38.328461
2251.962194	292412.698296	38.333479
2254.693170	292778.263905	38.338496
2256.406645	293158.190193	38.343514
2258.476942	293536.052484	38.348532
2260.854382	293927.100034	38.353549
2263.106014	294314.305680	38.358567
2265.435394	294706.375518	38.363584
2267.513417	295102.167781	38.368602
2269.849886	295489.256180	38.373620
2271.955326	295888.040004	38.378637
2274.159457	296284.978425	38.383655
2277.234711	296667.019385	38.388672
2279.184197	297082.717759	38.393690
2281.444923	297484.191629	38.398708
2284.018157	297885.183239	38.403725
2285.708180	298294.417123	38.408743
2288.202636	298698.543796	38.413760
2290.397100	299116.840378	38.418778
2293.303944	299527.554940	38.423796
2295.555566	299923.207677	38.428813
2297.769952	300340.304165	38.433831
2300.536649	300741.512375	38.438848
2302.725598	301150.990379	38.443866
2305.122773	301562.263190	38.448884
2307.903239	301964.761545	38.453901
2309.982212	302372.755067	38.458919
2312.098706	302782.773610	38.463936
2314.460674	303193.234715	38.468954
2316.978728	303604.431943	38.473972
2319.229343	304021.055354	38.478989
2321.521166	304447.272475	38.484007
2324.165239	304847.981001	38.489024
2326.129542	305271.199417	38.494042
2328.339363	305687.316252	38.499060
2330.744658	306103.959611	38.504077
2333.210334	306521.811294	38.509095
2335.889110	306937.291030	38.514112
2338.162914	307365.635295	38.519130
2340.918800	307767.714210	38.524148
2343.624630	308171.247565	38.529165
2346.025285	308576.605967	38.534183
2348.563048	308966.447389	38.539200
2350.771934	309373.967104	38.544218
2353.248796	309781.747744	38.549236
2355.623251	310182.024928	38.554253
2358.428292	310567.805576	38.559271
2360.588590	310979.111922	38.564288
2362.944082	311374.536674	38.569306
2365.359449	311759.435268	38.574324
2367.671205	312161.798154	38.579341
2370.121206	312552.581097	38.584359
2372.588146	312915.268716	38.589376
2374.804646	313283.125380	38.594394
2376.625246	313643.017512	38.599412
2379.110206	314005.520781	38.604429
2381.440709	314383.007053	38.609447
2383.383086	314751.994171	38.614464
2385.605913	315134.980838	38.619482
2387.732884	315516.762138	38.624500
2390.178278	315890.719671	38.629517
2392.267591	316299.629259	38.634535
2394.472709	316694.041936	38.639552
2396.869243	317104.042404	38.644570
2398.898437	317510.924634	38.649588
2401.603724	317919.729806	38.654605
2404.056241	318335.913184	38.659623
2406.169346	318746.713458	38.664640
2408.451545	319173.129899	38.669658
2410.833811	319592.645864	38.674676
2413.261882	320012.965356	38.679693
2415.981321	320432.119259	38.684711
2418.526474	320861.813138	38.689728
2421.033421	321282.469753	38.694746
2423.246438	321706.421715	38.699764
2426.137179	322130.645166	38.704781
2428.346129	322570.923520	38.709799
2430.972311	322998.486161	38.714816
2433.169912	323440.437988	38.719834
2435.337474	323875.357570	38.724852
2438.298916	324311.266499	38.729869
2440.370174	324754.450402	38.734887
2442.849310	325187.866161	38.739904
2445.246599	325642.650155	38.744922
2447.515151	326087.116098	38.749940
2450.193543	326546.446978	38.754957
2452.626023	326994.487989	38.759975
2454.966676	327439.544401	38.764992
2457.739823	327904.642354	38.770010
2459.965331	328355.806485	38.775028
2462.990455	328800.746588	38.780045
2465.266416	329258.931632	38.785063
2468.068639	329701.006810	38.790080
2470.597401	330150.309194	38.795098
2472.869607	330603.128457	38.800116
2475.757981	331057.777210	38.805133
2478.664653	331510.490321	38.810151
2480.719990	331951.933885	38.815168
2483.193791	332405.344791	38.820186
2486.084559	332837.940643	38.825204
2489.067354	333276.562763	38.830221
2491.800879	333712.022154	38.835239
2494.023455	334144.157177	38.840256
2496.852605	334571.495792	38.845274
2499.398924	335000.120776	38.850292
2502.494977	335421.774706	38.855309
2504.617641	335840.787123	38.860327
2507.381674	336226.787583	38.865344
2510.223060	336604.089619	38.870362
2512.517090	336978.606993	38.875380
2515.437522	337351.626468	38.880397
2517.419530	337735.304450	38.885415
2519.524094	338117.589638	38.890432
2521.978313	338499.715603	38.895450
2524.269338	338886.638610	38.900468
2526.866156	339277.217849	38.905485
2528.862313	339672.333174	38.910503
2531.042820	340068.965624	38.915520
2533.462244	340492.877450	38.920538
2535.594941	340920.081727	38.925556
2538.289997	341332.036288	38.930573
2540.507751	341774.658134	38.935591
2542.740049	342210.977904	38.940608
2545.184829	342646.346866	38.945626
2547.394587	343095.637705	38.950644
2549.904878	343548.482775	38.955661
2552.280194	344004.697081	38.960679
2555.058510	344460.310865	38.965696
2557.557578	344931.655273	38.970714
2560.048547	345408.455578	38.975732
2562.555322	345859.506226	38.980749
2565.139042	346344.509760	38.985767
2567.618079	346810.789877	38.990784
2570.598736	347286.989249	38.995802
2573.033133	347771.547286	39.000820
2575.788989	348244.981595	39.005837
2578.127046	348737.111769	39.010855
2580.818490	349221.794174	39.015872
2583.527504	349709.414306	39.020890
2586.064908	350193.173234	39.025908
2589.169987	350664.627443	39.030925
2591.778215	351157.886128	39.035943
2594.460082	351648.133157	39.040960
2597.148753	352121.265156	39.045978
2599.442682	352613.798587	39.050996
2601.996972	353105.093090	39.056013
2604.765965	353600.385051	39.061031
2607.449131	354088.476833	39.066048
2610.240681	354578.628292	39.071066
2612.786852	355082.571777	39.076084
2615.869802	355547.817351	39.081101
2618.245476	356043.731815	39.086119
2620.828504	356532.856738	39.091136
2624.301709	356999.169300	39.096154
2626.804593	357494.516199	39.101172
2629.620063	357966.660231	39.106189
2632.188967	358454.347040	39.111207
2634.554035	358944.244077	39.116224
2637.316771	359420.037352	39.121242
2639.703373	359901.926196	39.126260
2642.951764	360380.348828	39.131277
2645.839922	360847.681684	39.136295
2648.081480	361294.909670	39.141312
2650.761127	361728.942564	39.146330
2653.074260	362188.307766	39.151348
2655.205297	362623.155285	39.156365
2657.671700	363086.928780	39.161383
2660.247490	363546.898826	39.166400
2662.872244	363994.243265	39.171418
2665.107202	364463.876665	39.176436
2667.822262	364927.008486	39.181453
2670.687294	365406.429878	39.186471
2673.382382	365873.031953	39.191488
2676.080935	366347.647906	39.196506
2678.471068	366837.280198	39.201524
2681.388719	367304.491860	39.206541
2683.642607	367796.165277	39.211559
2686.045107	368298.036322	39.216576
2688.893289	368785.442793	39.221594
2691.263422	369283.805711	39.226612
2694.268994	369794.597734	39.231629
2697.021137	370304.814817	39.236647
2699.579056	370813.838576	39.241664
2702.571882	371318.524442	39.246682
2705.083422	371843.402287	39.251700
2708.116052	372344.466431	39.256717
2711.488944	372859.147082	39.261735
2714.594159	373347.120273	39.266752
2718.039503	373825.721948	39.271770
2720.834525	374328.271420	39.276788
2723.960685	374808.713659	39.281805
2726.764752	375284.583518	39.286823
2729.495681	375773.449762	39.291840
2732.814565	376257.853086	39.296858
2735.371377	376736.434386	39.301876
2738.257377	377207.194335	39.306893
2740.931846	377681.559475	39.311911
2743.656030	378163.547535	39.316928
2747.094649	378625.298164	39.321946
2749.239790	379112.871587	39.326964
2752.046536	379589.323859	39.331981
2755.131022	380062.529817	39.336999
2757.119005	380547.370301	39.342016
2759.973063	381029.632188	39.347034
2762.679570	381515.818071	39.352052
2765.463871	381994.096067	39.357069
2767.803817	382492.148940	39.362087
2770.519328	382978.771319	39.367104
2773.901072	383465.028260	39.372122
2776.184371	383967.535173	39.377140
2778.795144	384456.158930	39.382157
2781.429382	384953.270099	39.387175
2783.953087	385470.380073	39.392192
2786.616691	385970.263103	39.397210
2789.207503	386481.311338	39.402228
2791.808501	386998.362169	39.407245
2794.644438	387504.284363	39.412263
2797.003598	388004.238411	39.417280
2799.908357	388484.569364	39.422298
2802.115113	388977.584444	39.427316
2805.157143	389463.637921	39.432333
2807.736124	389952.395742	39.437351
2809.901687	390463.454693	39.442368
2813.012049	390969.994463	39.447386
2815.398714	391486.608447	39.452404
2818.134377	391999.583662	39.457421
2820.896048	392527.890261	39.462439
2823.454112	393060.785840	39.467456
2826.399253	393580.754553	39.472474
2828.968175	394135.694653	39.477492
2831.569255	394673.401988	39.482509
2834.740090	395222.320487	39.487527
2837.564984	395789.212969	39.492544
2840.741909	396332.280108	39.497562
2843.202025	396899.896253	39.502580
2846.008457	397459.257690	39.507597
2848.693044	398019.262902	39.512615
2851.608496	398595.196291	39.517632
2854.674027	399162.474993	39.522650
2857.551513	399736.467356	39.527668
2860.304905	400317.644594	39.532685
2863.988213	400877.214653	39.537703
2866.778853	401459.354309	39.542720
2869.904368	402027.435454	39.547738
2872.700687	402611.860438	39.552756
2876.813355	403154.818163	39.557773
2880.437434	403694.903114	39.562791
2883.827205	404250.201423	39.567808
2887.270705	404780.789563	39.572826
2889.925775	405321.557684	39.577844
2892.582609	405852.201452	39.582861
2895.932543	406391.066495	39.587879
2898.536472	406931.054199	39.592896
2901.274004	407462.265956	39.597914
2904.096614	408002.301627	39.602932
2906.730481	408547.477904	39.607949
2909.941323	409092.781218	39.612967
2912.177943	409650.496858	39.617984
2915.246842	410192.355620	39.623002
2918.044687	410747.782310	39.628020
2920.450546	411317.074077	39.633037
2923.613832	411863.323120	39.638055
2926.451376	412434.324681	39.643072
2929.230455	412993.438067	39.648090
2932.073521	413565.075814	39.653108
2934.766491	414142.960586	39.658125
2937.855757	414722.089014	39.663143
2940.645610	415302.368347	39.668160
2943.561053	415879.169710	39.673178
2946.370517	416464.516262	39.678196
2949.287062	417054.319218	39.683213
2952.049272	417619.047751	39.688231
2955.404326	418173.991534	39.693248
2958.083567	418716.893979	39.698266
2960.747249	419263.969327	39.703284
2963.827673	419811.601542	39.708301
2966.566683	420358.542298	39.713319
2969.042912	420912.633665	39.718336
2972.151767	421468.438118	39.723354
2975.377240	422030.648341	39.728372
2978.016848	422604.720875	39.733389
2981.122645	423157.958237	39.738407
2984.261153	423725.265259	39.743424
2987.344495	424281.320911	39.748442
2990.379983	424855.916882	39.753460
2993.334358	425441.583995	39.758477
2996.623337	426004.639604	39.763495
2999.714835	426584.028391	39.768512
3002.789144	427168.194974	39.773530
3005.698569	427746.954068	39.778548
3008.379414	428331.258706	39.783565
3011.595170	428909.006739	39.788583
3015.026980	429504.210315	39.793600
3017.971598	430089.219444	39.798618
3020.916705	430675.481807	39.803636
3023.830837	431269.156799	39.808653
3026.686405	431866.753130	39.813671
3029.337898	432475.486137	39.818688
3032.539972	433075.430961	39.823706
3035.472830	433692.118846	39.828724
3038.422932	434311.726747	39.833741
3041.295759	434928.368914	39.838759
3044.019442	435567.886463	39.843776
3046.852832	436199.191300	39.848794
3050.270979	436827.298503	39.853812
3053.182703	437473.524100	39.858829
3056.526024	438115.233579	39.863847
3059.109633	438764.921171	39.868864
3062.131886	439406.344203	39.873882
3065.449691	440056.261457	39.878900
3068.400601	440711.637582	39.883917
3072.016803	441353.320865	39.888935
3075.224403	442005.127869	39.893952
3077.826129	442657.570168	39.898970
3081.069656	443320.626943	39.903988
3084.105284	443972.205579	39.909005
3087.845412	444623.806932	39.914023
3090.791204	445294.703485	39.919040
3093.708133	445943.361429	39.924058
3096.781306	446603.367152	39.929076
3099.543087	447270.187018	39.934093
3102.884049	447934.415942	39.939111
3106.124138	448586.088459	39.944128
3108.830900	449249.114875	39.949146
3112.576092	449914.337058	39.954164
3115.952016	450588.456110	39.959181
3119.173997	451223.405146	39.964199
3121.889733	451851.887780	39.969216
3125.049207	452460.291799	39.974234
3128.281515	453071.147918	39.979252
3130.994014	453685.966651	39.984269
3134.277998	454301.234965	39.989287
3137.537166	454921.500333	39.994304
3140.517389	455543.361433	39.999322
3143.627346	456162.047416	40.004340
3146.202856	456800.484530	40.009357
3149.410438	457427.620885	40.014375
3152.151305	458071.966033	40.019392
3155.038391	458721.531294	40.024410
3158.146006	459375.191295	40.029428
3161.387637	460031.188511	40.034445
3164.498819	460689.766860	40.039463
3167.563458	461373.020737	40.044480
3170.564431	462038.253585	40.049498
3173.646264	462721.512793	40.054516
3176.249388	463406.647126	40.059533
3179.569732	464108.490584	40.064551
3182.856478	464817.296659	40.069568
3185.817612	465530.885213	40.074586
3189.346865	466234.648779	40.079604
3192.300932	466952.894363	40.084621
3195.338904	467670.090671	40.089639
3198.917812	468385.963135	40.094656
3202.082179	469107.793549	40.099674
3205.347925	469815.979529	40.104692
3208.640376	470556.905428	40.109709
3211.932329	471272.268712	40.114727
3215.121542	472002.337747	40.119744
3218.233161	472744.275366	40.124762
3221.783691	473477.723470	40.129780
3224.816494	474214.614491	40.134797
3228.078782	474951.037975	40.139815
3231.829377	475691.755721	40.144832
3234.990072	476430.567887	40.149850
3238.467454	477160.304497	40.154868
3241.465791	477908.490420	40.159885
3244.976010	478643.576382	40.164903
3248.798785	479385.358854	40.169920
3251.452156	480119.160743	40.174938
3255.364781	480849.248697	40.179956
3258.854384	481583.419601	40.184973
3261.988476	482314.485727	40.189991
3265.647128	483039.831851	40.195008
3269.409497	483764.477483	40.200026
3272.739399	484478.451314	40.205044
3276.002013	485210.701597	40.210061
3279.589811	485912.959189	40.215079
3283.034232	486625.268616	40.220096
3286.624417	487315.398170	40.225114
3290.685173	488003.003092	40.230132
3294.294285	488705.760489	40.235149
3297.845159	489355.101207	40.240167
3300.941342	489992.619572	40.245184
3304.141166	490629.544185	40.250202
3307.293191	491238.166241	40.255220
3310.080690	491881.074113	40.260237
3313.087564	492522.005614	40.265255
3315.943852	493163.645887	40.270272
3318.686098	493819.323133	40.275290
3321.895885	494487.883200	40.280308
3324.464932	495159.701996	40.285325
3327.329685	495830.540328	40.290343
3330.201814	496523.724582	40.295360
3332.939620	497232.659214	40.300378
3336.154171	497942.500669	40.305396
3339.021244	498680.242174	40.310413
3342.015117	499404.401412	40.315431
3345.462946	500145.777872	40.320448
3348.257822	500916.964423	40.325466
3351.577078	501673.090818	40.330484
3354.929973	502437.660996	40.335501
3358.164666	503228.871161	40.340519
3361.252897	504008.812072	40.345536
3364.910334	504793.524660	40.350554
3368.391592	505591.201971	40.355572
3371.744869	506387.449813	40.360589
3375.151051	507175.577580	40.365607
3379.013848	507987.821910	40.370624
3382.323369	508799.106171	40.375642
3385.950703	509591.933332	40.380660
3389.575806	510399.660575	40.385677
3392.911979	511200.028360	40.390695
3396.455460	512010.013296	40.395712
3400.072541	512830.694528	40.400730
3403.455306	513642.291735	40.405748
3406.691916	514462.903252	40.410765
3410.360276	515262.824313	40.415783
3414.019335	516082.684340	40.420800
3417.000395	516897.920156	40.425818
3421.372758	517704.119659	40.430836
3424.687814	518518.920323	40.435853
3428.365584	519320.561007	40.440871
3431.712712	520142.589160	40.445888
3435.138528	520944.593764	40.450906
3438.945784	521767.576920	40.455924
3442.365275	522584.528863	40.460941
3445.849751	523382.672617	40.465959
3449.532287	524195.115014	40.470976
3452.677535	525011.584228	40.475994
3456.124550	525820.250907	40.481012
3459.324238	526643.484620	40.486029
3463.113030	527465.322494	40.491047
3466.576403	528266.704458	40.496064
3469.594480	529088.176803	40.501082
3473.183756	529906.088859	40.506100
3476.540482	530737.602629	40.511117
3479.931966	531552.397633	40.516122
3483.289999	532305.924907	40.521127
3486.202115	533038.217485	40.526132
3489.394243	533690.917055	40.531136
3492.202496	534294.144717	40.536141
3494.907663	534832.808752	40.541146
3498.021021	535325.170967	40.546151
3499.838512	535752.816141	40.551156
3502.813764	536119.200605	40.556160
3504.921376	536453.236584	40.561165
3506.683607	536715.094296	40.566170
3508.738708	536922.151941	40.571175
3510.290011	537104.639383	40.576180
3511.875934	537222.673869	40.581184
3513.028540	537308.048363	40.586189
3514.022753	537350.517876	40.591194
3515.210268	537370.683884	40.596199
3516.397078	537358.072020	40.601204
3517.271296	537304.852630	40.606208
3518.005455	537245.493491	40.611213
3518.491838	537146.677578	40.616218
3519.208311	537029.945388	40.621223
3519.465813	536888.991031	40.626228
3520.033307	536744.501377	40.631232
3520.466012	536574.171608	40.636237
3520.475247	536390.067529	40.641242
3520.873559	536206.657390	40.646247
3521.170253	535992.399615	40.651252
3521.340798	535778.764918	40.656256
3521.234474	535558.351984	40.661261
3521.398426	535330.973030	40.666266
3521.842350	535084.149550	40.671271
3521.295020	534841.721923	40.676276
3521.352439	534593.789866	40.681280
3521.704705	534343.433017	40.686285
3521.375397	534090.300413	40.691290
3521.230401	533818.039127	40.696295
3520.827112	533569.405711	40.701300
3521.154389	533314.186469	40.706304
3521.091470	533053.012881	40.711309
3520.277079	532796.247894	40.716314
3520.462743	532537.552379	40.721319
3520.027368	532274.252171	40.726324
3519.981843	532025.335437	40.731328
3520.177353	531762.482639	40.736333
3519.690430	531506.402506	40.741338
3519.468185	531252.145786	40.746343
3519.416600	530997.857966	40.751348
3519.008804	530739.933847	40.756352
3518.773075	530502.947317	40.761357
3518.377498	530253.097701	40.766362
3518.667511	530011.927866	40.771367
3518.130610	529760.071579	40.776372
3517.983690	529527.452433	40.781376
3517.782667	529301.811767	40.786381
3517.460530	529062.846479	40.791386
3517.112495	528835.908545	40.796391
3516.939802	528608.484839	40.801396
3516.788513	528384.389760	40.806400
3516.844014	528167.535901	40.811405
3516.492192	527948.873622	40.816410
3516.378459	527738.761922	40.821415
3515.798999	527522.302815	40.826420
3515.524639	527311.907631	40.831424
3515.651607	527112.716343	40.836429
3515.253952	526910.977436	40.841434
3514.977079	526702.495086	40.846439
3514.503478	526522.798635	40.851444
3514.782439	526327.161883	40.856448
3514.886818	526137.514243	40.861453
3514.055358	525948.163881	40.866458
3514.049659	525759.489459	40.871463
3514.013036	525582.543775	40.876468
3513.727208	525412.004060	40.881472
3513.599253	525234.209718	40.886477
3513.296476	525062.455897	40.891482
3512.960997	524887.723217	40.896487
3512.818605	524727.060488	40.901492
3512.640042	524562.661421	40.906496
3513.002275	524394.636907	40.911501
3512.187108	524246.763037	40.916506
3512.508859	524089.761116	40.921511
3512.300341	523940.373211	40.926516
3512.093928	523780.519935	40.931520
3511.937950	523641.079119	40.936525
3511.600308	523491.151418	40.941530
3511.830607	523344.873299	40.946535
3511.478257	523205.207005	40.951540
3511.079690	523054.880481	40.956544
3511.474158	522925.658971	40.961549
3510.870026	522796.948119	40.966554
3511.044447	522669.831985	40.971559
3510.839704	522538.781097	40.976564
3510.784782	522397.797013	40.981568
3510.613735	522276.444928	40.986573
3510.311654	522151.118869	40.991578
3510.280593	522033.787180	40.996583
3510.145061	521908.938477	41.001588
3510.370313	521780.745701	41.006592
3510.125240	521665.871837	41.011597
3509.680134	521545.568726	41.016602
3509.742652	521427.257312	41.021607
3509.631609	521317.516561	41.026612
3509.362052	521210.631320	41.031616
3509.224788	521112.774243	41.036621
3509.375187	521010.978175	41.041626
3509.400151	520896.410116	41.046631
3508.861202	520806.602858	41.051636
3508.850449	520707.863870	41.056640
3509.001232	520613.396264	41.061645
3508.795293	520519.287847	41.066650
3508.872170	520419.724323	41.071655
3508.433307	520326.359441	41.076660
3508.676041	520225.150608	41.081664
3508.355352	520142.585864	41.086669
3508.170627	520046.398400	41.091674
3508.398706	519962.330320	41.096679
3508.293743	519880.084085	41.101684
3507.989233	519789.779144	41.106688
3508.152754	519709.866013	41.111693
3508.009561	519614.984061	41.116698
3508.027051	519534.840348	41.121703
3508.159935	519452.301570	41.126708
3507.794372	519379.195261	41.131712
3507.909495	519295.091056	41.136717
3507.714644	519212.350055	41.141722
3508.168803	519134.107343	41.146727
3507.849179	519058.160791	41.151732
3507.798447	518964.625695	41.156736
3507.897944	518895.337162	41.161741
3507.413611	518809.808294	41.166746
3507.730532	518738.259902	41.171751
3507.594962	518661.574527	41.176756
3507.336907	518590.116365	41.181760
3506.978158	518516.499496	41.186765
3507.023665	518460.668054	41.191770
3507.147089	518380.754812	41.196775
3507.296689	518335.221913	41.201780
3507.032099	518257.847130	41.206784
3507.043533	518184.979336	41.211789
3506.843832	518121.297143	41.216794
3506.870466	518051.662620	41.221799
3506.726508	517992.117596	41.226804
3506.776733	517931.985429	41.231808
3506.499039	517878.579758	41.236813
3506.386799	517814.326320	41.241818
3506.782008	517766.224661	41.246823
3506.658965	517711.378113	41.251828
3506.477563	517638.639526	41.256832
3506.567385	517586.540165	41.261837
3506.331946	517530.497146	41.266842
3506.603606	517459.810040	41.271847
3506.319366	517419.804598	41.276852
3506.436412	517353.035265	41.281856
3506.428058	517302.872149	41.286861
3506.113894	517262.011381	41.291866
3506.535978	517202.930321	41.296871
3506.109296	517154.097105	41.301876
3505.850771	517090.319105	41.306880
3506.092294	517048.206882	41.311885
3506.238422	517006.665899	41.316890
3506.137250	516937.350314	41.321895
3505.958310	516901.069172	41.326900
3506.056553	516847.600763	41.331904
3506.420416	516797.630147	41.336909
3506.268220	516754.365711	41.341914
3506.325928	516699.032113	41.346919
3505.955721	516649.429923	41.351924
3505.824667	516589.321542	41.356928
3506.135463	516537.487395	41.361933
3505.690031	516514.851231	41.366938
3505.642458	516452.605159	41.371943
3505.598182	516423.331152	41.376948
3505.528690	516376.259779	41.381952
3505.952337	516331.891796	41.386957
3505.393621	516301.181718	41.391962
3505.634087	516252.442700	41.396967
3505.500050	516214.888657	41.401972
3505.471699	516162.752939	41.406976
3505.757470	516128.267850	41.411981
3505.501718	516082.438828	41.416986
3505.818872	516042.486740	41.421991
3505.524546	516002.580624	41.426996
3505.718760	515960.321410	41.432000
3505.619369	515923.115246	41.437005
3505.451044	515879.294780	41.442010
3505.358311	515842.441398	41.447015
3505.395392	515807.286921	41.452020
3505.265736	515773.220771	41.457024
3505.515055	515733.531533	41.462029
3505.351881	515695.829205	41.467034
3505.570504	515650.126319	41.472039
3505.383280	515627.346990	41.477044
3505.386700	515574.850395	41.482048
3505.561556	515541.039091	41.487053
3505.711168	515510.670775	41.492058
3505.517197	515464.577420	41.497063
3505.586439	515426.888327	41.502068
3505.735652	515386.050867	41.507072
3505.427437	515336.182096	41.512077
3505.097541	515304.928266	41.517082
3505.617107	515260.137679	41.522087
3505.527788	515229.503164	41.527092
3505.034611	515182.394236	41.532096
3505.295907	515151.451287	41.537101
3504.961176	515124.041629	41.542106
3505.143922	515095.993806	41.547111
3505.450249	515057.254895	41.552116
3504.917031	515020.823350	41.557120
3505.174407	514986.643853	41.562125
3505.021152	514963.655946	41.567130
3505.233583	514914.361122	41.572135
3505.387132	514887.834855	41.577140
3504.820101	514854.544029	41.582144
3505.196933	514812.758820	41.587149
3505.056476	514789.364038	41.592154
3505.412468	514751.628107	41.597159
3505.264701	514713.364785	41.602164
3505.094744	514685.624904	41.607168
3505.261489	514653.026939	41.612173
3505.056993	514618.767958	41.617178
3505.129981	514584.262742	41.622183
3505.062984	514552.713070	41.627188
3504.680106	514515.042806	41.632192
3505.003227	514495.468816	41.637197
3504.953193	514470.491394	41.642202
3505.024201	514436.137920	41.647207
3505.039321	514413.375536	41.652212
3505.099012	514382.564190	41.657216
3504.698205	514342.316896	41.662221
3504.601961	514324.073438	41.667226
3505.002404	514286.380015	41.672231
3504.902254	514260.449215	41.677236
3504.858837	514235.571553	41.682240
3505.200047	514193.335230	41.687245
3504.850067	514169.416335	41.692250
3504.969059	514145.575023	41.697255
3504.787826	514119.100454	41.702260
3504.867321	514083.278135	41.707264
3504.717993	514043.900800	41.712269
3504.504524	514032.099076	41.717274
3504.924619	514002.595705	41.722279
3504.611848	513977.355600	41.727284
3504.651637	513955.499122	41.732288
3504.913915	513918.635980	41.737293
3504.667965	513905.423080	41.742298
3504.995518	513866.475754	41.747303
3504.862946	513837.464077	41.752308
3504.822990	513816.833932	41.757312
3504.921961	513785.357749	41.762317
3504.658691	513767.696462	41.767322
3505.000923	513728.341858	41.772327
3504.703852	513708.106276	41.777332
3504.637536	513682.169237	41.782336
3504.576719	513658.659133	41.787341
3504.496858	513638.692619	41.792346
3504.586528	513616.878399	41.797351
3504.461661	513592.012659	41.802356
3504.586397	513563.263325	41.807360
3504.677854	513538.110414	41.812365
3504.546779	513526.447055	41.817370
3504.895984	513483.803047	41.822375
3504.805003	513463.281695	41.827380
3504.549308	513441.420670	41.832384
3504.839602	513414.314081	41.837389
3504.758677	513388.682384	41.842394
3505.185082	513349.617081	41.847399
3504.810152	513327.117199	41.852404
3504.848022	513293.929998	41.857408
3504.976151	513265.736014	41.862413
3504.638132	513248.692972	41.867418
3504.686359	513211.204558	41.872423
3505.008699	513184.901839	41.877428
3504.817374	513168.341346	41.882432
3505.066600	513125.307582	41.887437
3504.743557	513104.873053	41.892442
3504.866400	513065.703325	41.897447
3504.568876	513055.330493	41.902452
3505.083705	513027.833724	41.907456
3504.826875	512991.556422	41.912461
3504.490365	512967.481943	41.917466
3504.861622	512935.404737	41.922471
3504.707517	512910.542614	41.927476
3504.396687	512884.895906	41.932480
3504.667041	512859.207887	41.937485
3504.553425	512845.770909	41.942490
3504.711721	512820.909863	41.947495
3504.622936	512796.745406	41.952500
3504.610048	512775.603884	41.957504
3504.804951	512751.596857	41.962509
3504.434178	512719.636518	41.967514
3504.432333	512697.582660	41.972519
3504.714284	512660.966581	41.977524
3504.382084	512649.030903	41.982528
3504.600269	512609.996801	41.987533
3504.688771	512603.558756	41.992538
3504.774741	512566.467614	41.997543
3504.841460	512551.585567	42.002548
3504.577818	512520.569005	42.007552
3504.820166	512489.219498	42.012557
3504.374730	512460.912489	42.017562
3504.596954	512444.235342	42.022567
3504.847739	512425.732648	42.027572
3504.560362	512407.264404	42.032576
3504.963979	512371.083725	42.037581
3504.872526	512356.024169	42.042586
3504.672812	512317.055441	42.047591
3504.682720	512294.594528	42.052596
3504.585296	512266.434528	42.057600
3504.872311	512231.637755	42.062605
3504.855102	512221.473029	42.067610
3504.853890	512181.056252	42.072615
3504.558407	512155.254258	42.077620
3504.728391	512132.616077	42.082624
3504.475447	512108.173074	42.087629
3504.580481	512086.809716	42.092634
3504.755085	512048.944662	42.097639
3504.337421	512025.387516	42.102644
3504.298039	512011.482879	42.107648
3504.650107	511981.582060	42.112653
3504.188668	511972.145000	42.117658
3504.264592	511940.466686	42.122663
3504.349458	511914.857139	42.127668
3504.497604	511906.638917	42.132672
3504.734746	511885.709695	42.137677
3504.432647	511858.542489	42.142682
3504.604095	511839.697598	42.147687
3504.763012	511820.854666	42.152692
3504.633552	511793.457728	42.157696
3504.589529	511753.046698	42.162701
3504.471933	511745.325671	42.167706
3504.526067	511723.565214	42.172711
3504.568315	511702.413640	42.177716
3504.531079	511686.839062	42.182720
3504.595466	511653.340940	42.187725
3504.706776	511636.073497	42.192730
3504.879320	511602.912286	42.197735
3504.439765	511586.895339	42.202740
3503.991903	511561.318869	42.207744
3504.494131	511535.187510	42.212749
3504.061359	511515.223680	42.217754
3504.161863	511488.700463	42.222759
3504.086656	511484.463091	42.227764
3503.790708	511458.103657	42.232768
3504.082151	511443.488642	42.237773
3504.103531	511441.613570	42.242778
3504.406675	511419.712196	42.247783
3504.581665	511400.562738	42.252788
3504.500563	511384.691295	42.257792
3504.666937	511357.398659	42.262797
3504.238833	511335.106878	42.267802
3504.590159	511308.543738	42.272807
3504.439729	511291.722010	42.277812
3504.616854	511265.540446	42.282816
3504.675659	511245.245670	42.287821
3504.501722	511229.236992	42.292826
3504.686315	511202.497689	42.297831
3504.477598	511180.019269	42.302836
3504.546718	511155.169880	42.307840
3504.882078	511121.476124	42.312845
3504.680731	511104.915197	42.317850
3504.351825	511073.754542	42.322855
3504.435912	511061.347248	42.327860
3504.069395	511040.664159	42.332864
3504.615252	511027.526216	42.337869
3504.336113	511003.541055	42.342874
3504.464873	510984.196084	42.347879
3504.451797	510952.580586	42.352884
3504.437474	510933.612289	42.357888
3504.499209	510907.296647	42.362893
3504.213009	510895.908934	42.367898
3504.342952	510869.076570	42.372903
3504.609768	510853.807294	42.377908
3504.148560	510831.368319	42.382912
3504.489370	510809.662564	42.387917
3503.988228	510798.055814	42.392922
3504.366095	510757.221621	42.397927
3504.689627	510746.192740	42.402932
3504.304937	510736.591094	42.407936
3504.652535	510704.918134	42.412941
3504.306948	510693.337315	42.417946
3504.290424	510665.364234	42.422951
3504.404286	510638.534049	42.427956
3504.100057	510622.191269	42.432960
3504.288326	510597.474004	42.437965
3504.005945	510586.945498	42.442970
3504.026216	510569.033702	42.447975
3504.052403	510536.146495	42.452980
3504.167911	510529.602220	42.457984
3504.295394	510513.140514	42.462989
3504.540874	510495.395406	42.467994
3504.324460	510481.416320	42.472999
3504.161583	510461.307417	42.478004
3504.222855	510447.082056	42.483008
3504.403529	510417.104404	42.488013
3504.221612	510411.922425	42.493018
3504.303793	510377.407190	42.498023
3504.381596	510359.334312	42.503028
3504.088038	510349.920404	42.508032
3504.303687	510334.658752	42.513037
3504.225862	510320.151730	42.518042
3504.158537	510285.305807	42.523047
3504.414263	510280.509931	42.528052
3504.160591	510262.236389	42.533056
3504.387523	510242.217390	42.538061
3504.056733	510231.949266	42.543066
3504.281948	510200.294715	42.548071
3504.437659	510185.042402	42.553076
3504.200644	510167.474393	42.558080
3504.292641	510150.360271	42.563085
3504.353065	510124.448356	42.568090
3504.314458	510105.887703	42.573095
3504.287732	510088.944055	42.578100
3504.150653	510071.511925	42.583104
3504.166796	510051.627199	42.588109
3504.260413	510033.956206	42.593114
3504.424569	510016.982319	42.598119
3504.430454	509996.188514	42.603124
3504.278817	509985.942518	42.608128
3504.197398	509944.926022	42.613133
3504.273669	509940.563143	42.618138
3504.050602	509915.151037	42.623143
3503.988656	509895.885567	42.628148
3503.907310	509891.142856	42.633152
3504.295082	509863.458704	42.638157
3504.284763	509849.497119	42.643162
3504.193643	509845.008897	42.648167
3504.380598	509810.577143	42.653172
3504.063367	509803.493886	42.658176
3504.167825	509781.419451	42.663181
3504.038421	509757.105323	42.668186
3504.005887	509755.289178	42.673191
3503.956642	509725.953756	42.678196
3503.760240	509718.041897	42.683200
3504.173766	509712.715004	42.688205
3504.105107	509701.089744	42.693210
3504.169797	509668.397152	42.698215
3504.299798	509659.826575	42.703220
3504.014162	509652.333525	42.708224
3503.807390	509638.301633	42.713229
3503.876352	509632.675029	42.718234
3504.045524	509605.885077	42.723239
3504.140571	509592.058406	42.728244
3504.011282	509584.338247	42.733248
3503.901965	509550.155164	42.738253
3503.953726	509544.328881	42.743258
3503.780584	509545.469292	42.748263
3504.195973	509518.336735	42.753268
3504.027421	509509.357937	42.758272
3504.111995	509501.907495	42.763277
3504.076697	509480.866612	42.768282
3504.229851	509465.057546	42.773287
3504.081928	509444.439158	42.778292
3504.000899	509437.318417	42.783296
3504.060966	509416.060011	42.788301
3504.257531	509410.413167	42.793306
3504.057980	509383.225809	42.798311
3504.024398	509373.820866	42.803316
3504.094967	509354.685624	42.808321
3504.291718	509335.783382	42.813325
3504.107906	509329.994258	42.818330
3504.132428	509308.488371	42.823335
3504.316931	509284.731077	42.828340
3503.924539	509265.921871	42.833345
3504.270883	509236.776057	42.838349
3504.130712	509234.470936	42.843354
3504.313477	509209.550168	42.848359
3504.195257	509201.828087	42.853364
3504.121347	509179.173949	42.858369
3503.796077	509159.595117	42.863373
3503.983333	509147.170132	42.868378
3503.970518	509134.776758	42.873383
3504.415446	509109.713224	42.878388
3504.278709	509109.481883	42.883393
3504.598572	509078.063272	42.888397
3504.494829	509071.502499	42.893402
3504.313062	509039.201818	42.898407
3504.417233	509009.334986	42.903412
3503.882371	508992.824724	42.908417
3504.311499	508981.575647	42.913421
3504.200787	508969.754161	42.918426
3504.215147	508957.002206	42.923431
3504.164575	508949.927043	42.928436
3504.038545	508921.766047	42.933441
3504.148107	508896.704613	42.938445
3504.057137	508890.091159	42.943450
3503.809909	508873.130567	42.948455
3504.193500	508861.585043	42.953460
3504.232434	508841.341153	42.958465
3504.068082	508826.947732	42.963469
3503.918635	508812.754321	42.968474
3504.063563	508802.764312	42.973479
3504.260138	508781.281169	42.978484
3504.030515	508777.826449	42.983489
3504.357345	508746.608511	42.988493
3504.095650	508736.379162	42.993498
3504.208472	508718.400213	42.998503
3503.960724	508695.266964	43.003508
3503.894390	508689.610841	43.008513
3504.186104	508668.567874	43.013517
3503.802306	508663.316081	43.018522
3503.782938	508638.072268	43.023527
3503.986754	508637.888286	43.028532
3503.958160	508627.571436	43.033537
3503.973000	508604.598944	43.038541
3503.992031	508595.842997	43.043546
3504.062209	508580.147423	43.048551
3504.448322	508562.884046	43.053556
3504.187484	508544.710995	43.058561
3504.220845	508523.101540	43.063565
3504.169625	508500.240541	43.068570
3503.983187	508485.141988	43.073575
3504.391978	508463.574313	43.078580
3503.866074	508452.475834	43.083585
3503.985949	508440.263371	43.088589
3503.851474	508432.492918	43.093594
3503.809689	508420.963735	43.098599
3504.140798	508395.917154	43.103604
3504.060233	508376.703519	43.108609
3504.288385	508357.997626	43.113613
3504.157415	508341.119326	43.118618
3504.079647	508342.345933	43.123623
3504.408716	508310.266723	43.128628
3503.772369	508300.399903	43.133633
3503.966325	508291.110194	43.138637
3504.257331	508274.620501	43.143642
3503.984131	508256.196119	43.148647
3503.951008	508240.718948	43.153652
3504.118463	508220.959980	43.158657
3504.359037	508202.100165	43.163661
3503.857942	508208.149738	43.168666
3503.974528	508179.089046	43.173671
3503.902493	508161.189329	43.178676
3503.761188	508164.399250	43.183681
3503.893884	508122.636217	43.188685
3503.893067	508116.109409	43.193690
3503.872853	508109.231489	43.198695
3503.708807	508103.236440	43.203700
3503.788326	508093.003377	43.208705
3503.902575	508070.014462	43.213709
3503.862901	508074.270867	43.218714
3503.723701	508050.563034	43.223719
3504.152984	508034.961999	43.228724
3503.771665	508019.944436	43.233729
3503.658329	508023.807721	43.238733
3503.740659	507999.508240	43.243738
3503.823477	507987.756687	43.248743
3504.055682	507973.350473	43.253748
3503.571551	507968.569696	43.258753
3503.753270	507966.112337	43.263757
3503.969566	507941.639810	43.268762
3503.933150	507945.389762	43.273767
3504.152783	507930.732515	43.278772
3503.914402	507912.707039	43.283777
3503.959204	507903.187710	43.288781
3504.001401	507898.880297	43.293786
3503.850713	507871.379245	43.298791
3504.214423	507860.848142	43.303796
3503.786325	507849.632620	43.308801
3503.949332	507820.159209	43.313805
3503.720705	507814.882630	43.318810
3503.872542	507809.292931	43.323815
3504.007301	507789.083260	43.328820
3504.066587	507777.234087	43.333825
3503.861813	507759.860908	43.338829
3504.086303	507757.143771	43.343834
3504.066310	507734.428615	43.348839
3504.102291	507728.148833	43.353844
3503.776055	507707.505950	43.358849
3504.269333	507685.114389	43.363853
3504.023939	507677.715310	43.368858
3504.045656	507659.193082	43.373863
3504.156408	507643.085462	43.378868
3504.077385	507637.987576	43.383873
3503.845644	507612.118055	43.388877
3504.071957	507591.134712	43.393882
3503.955017	507583.057517	43.398887
3504.347729	507571.610889	43.403892
3504.113787	507561.730642	43.408897
3504.104825	507551.410047	43.413901
3504.079358	507523.382668	43.418906
3503.856596	507519.977208	43.423911
3504.162639	507508.544236	43.428916
3504.045577	507484.832128	43.433921
3503.976785	507470.877856	43.438925
3503.938496	507469.871954	43.443930
3503.844541	507449.748634	43.448935
3504.320207	507421.135901	43.453940
3504.193826	507409.012230	43.458945
3504.315686	507385.565816	43.463949
3504.126219	507379.169743	43.468954
3503.974808	507358.144621	43.473959
3504.010568	507338.911447	43.478964
3503.996218	507328.844565	43.483969
3503.791428	507309.598778	43.488973
3503.867620	507292.383119	43.493978
3503.927301	507289.742556	43.498983
3504.407517	507275.751956	43.503988
3504.064495	507268.519929	43.508993
3504.320236	507240.599446	43.513997
3504.406393	507219.991999	43.519002
3504.111450	507198.129182	43.524007
3504.252731	507172.149448	43.529012
3503.747390	507163.121457	43.534017
3503.688633	507158.323822	43.539021
3503.645286	507140.620911	43.544026
3504.036725	507120.977086	43.549031
3504.044628	507107.566994	43.554036
3503.686487	507104.891241	43.559041
3504.181760	507079.159017	43.564045
3503.788209	507074.768470	43.569050
3504.007734	507065.018668	43.574055
3504.046132	507039.257394	43.579060
3504.116187	507031.656383	43.584065
3503.943755	507025.712885	43.589069
3504.031842	507005.661476	43.594074
3503.856157	506989.143122	43.599079
3504.029043	506974.441856	43.604084
3503.766383	506965.679004	43.609089
3503.966250	506949.961455	43.614093
3503.900765	506932.261831	43.619098
3503.734298	506926.772756	43.624103
3503.698933	506895.709926	43.629108
3503.731157	506897.020450	43.634113
3504.181024	506885.665539	43.639117
3504.375632	506881.080784	43.644122
3504.215310	506866.280290	43.649127
3504.250988	506850.335600	43.654132
3503.849356	506836.990025	43.659137
3504.101942	506817.013601	43.664141
3503.945604	506801.554617	43.669146
3503.952152	506781.971240	43.674151
3503.955844	506766.082129	43.679156
3503.914742	506774.083514	43.684161
3504.103121	506748.247504	43.689165
3503.993922	506730.655784	43.694170
3503.775530	506727.907284	43.699175
3504.244580	506700.458225	43.704180
3503.667248	506687.241506	43.709185
3503.919887	506680.471696	43.714189
3504.184312	506668.184538	43.719194
3504.008417	506645.340793	43.724199
3504.011685	506635.473127	43.729204
3503.904314	506610.999279	43.734209
3503.957700	506591.003477	43.739213
3503.952985	506591.965656	43.744218
3503.822018	506577.615684	43.749223
3504.003495	506547.681784	43.754228
3503.924420	506560.698779	43.759233
3503.802897	506534.253617	43.764237
3503.957705	506515.304323	43.769242
3504.001269	506501.331513	43.774247
3503.991883	506499.561968	43.779252
3504.034577	506478.049689	43.784257
3503.826538	506457.083025	43.789261
3503.887580	506448.268750	43.794266
3503.897574	506444.978094	43.799271
3504.273616	506418.605922	43.804276
3503.955972	506408.991252	43.809281
3503.842420	506386.289118	43.814285
3504.080490	506375.017951	43.819290
3503.846826	506367.565855	43.824295
3503.861447	506360.428727	43.829300
3503.844147	506343.125700	43.834305
3504.109011	506317.833582	43.839309
3504.140259	506322.838235	43.844314
3503.871330	506296.365407	43.849319
3504.175006	506277.442927	43.854324
3503.835304	506275.624362	43.859329
3503.939871	506251.167112	43.864333
3504.026282	506240.931868	43.869338
3503.929910	506233.964036	43.874343
3503.991438	506201.315989	43.879348
3503.853849	506195.417300	43.884353
3503.913152	506185.439318	43.889357
3503.839625	506171.383546	43.894362
3503.624699	506165.598275	43.899367
3503.872917	506150.024169	43.904372
3504.206681	506154.171422	43.909377
3504.001658	506135.278585	43.914381
3504.022867	506117.210213	43.919386
3503.618984	506111.707800	43.924391
3503.733693	506085.174017	43.929396
3503.362772	506075.921801	43.934401
3503.482146	506064.466783	43.939405
3503.918071	506061.260544	43.944410
3503.629946	506067.985630	43.949415
3503.810148	506048.525790	43.954420
3503.703771	506020.964198	43.959425
3503.600617	506020.474490	43.964429
3503.692562	506026.532290	43.969434
3503.805904	506013.458908	43.974439
3503.804928	505999.897557	43.979444
3503.692716	505989.086325	43.984449
3503.569621	505981.161163	43.989453
3503.871086	505976.660488	43.994458
3503.450414	505975.714935	43.999463
3503.968405	505943.399083	44.004468
3503.866598	505947.514021	44.009473
3503.587022	505933.693034	44.014477
3503.742269	505936.856495	44.019482
3503.870394	505912.142032	44.024487
3504.036896	505891.925138	44.029492
3503.746631	505889.238466	44.034497
3504.062035	505870.263089	44.039501
3504.146775	505860.027885	44.044506
3503.842575	505851.878273	44.049511
3504.057334	505827.200601	44.054516
3503.824596	505811.702208	44.059521
3503.838841	505801.022682	44.064525
3503.997493	505788.903433	44.069530
3503.762484	505776.846394	44.074535
3504.014686	505761.878553	44.079540
3503.869195	505754.665276	44.084545
3503.826008	505741.464619	44.089549
3504.121404	505715.154733	44.094554
3503.664828	505711.026816	44.099559
3503.681955	505702.623934	44.104564
3503.913533	505689.481019	44.109569
3503.812462	505666.219333	44.114573
3504.088292	505667.339638	44.119578
3503.883396	505647.940216	44.124583
3504.057100	505630.100257	44.129588
3503.948548	505624.500408	44.134593
3503.899747	505605.885929	44.139597
3503.942391	505586.346107	44.144602
3503.622298	505591.204084	44.149607
3503.649322	505576.980128	44.154612
3503.758098	505579.999187	44.159617
3503.938631	505547.381711	44.164621
3503.727548	505539.571463	44.169626
3503.611980	505531.948532	44.174631
3504.029785	505526.771502	44.179636
3504.125251	505516.736818	44.184641
3504.150214	505509.749520	44.189645
3504.197623	505500.076651	44.194650
3503.787773	505482.733604	44.199655
3503.903117	505459.032604	44.204660
3503.827339	505460.410912	44.209665
3503.765706	505440.988617	44.214669
3503.898236	505425.735776	44.219674
3503.911812	505416.068208	44.224679
3504.010159	505400.719540	44.229684
3503.784038	505385.320931	44.234689
3503.926551	505374.873894	44.239693
3503.845682	505360.869234	44.244698
3503.963754	505356.447990	44.249703
3503.949251	505334.589109	44.254708
3503.975217	505329.878788	44.259713
3503.886003	505316.179039	44.264717
3503.978602	505300.679377	44.269722
3503.793601	505299.544722	44.274727
3504.134374	505276.617523	44.279732
3503.859601	505258.999880	44.284737
3503.695305	505242.629882	44.289741
3503.857934	505234.608617	44.294746
3503.725859	505227.949655	44.299751
3503.707775	505214.997658	44.304756
3503.831610	505206.274042	44.309761
3503.674366	505196.936981	44.314765
3503.824523	505192.308205	44.319770
3503.826427	505168.371716	44.324775
3504.018902	505155.943053	44.329780
3503.961654	505166.579195	44.334785
3503.998490	505134.641527	44.339789
3504.104237	505116.305732	44.344794
3504.016981	505119.254643	44.349799
3504.168806	505094.383463	44.354804
3503.805369	505077.589336	44.359809
3503.737475	505070.818960	44.364813
3503.983929	505053.169336	44.369818
3503.814337	505039.127834	44.374823
3504.112884	505022.279633	44.379828
3503.824131	505016.353831	44.384833
3503.649534	504992.495603	44.389837
3503.891159	504973.935760	44.394842
3503.959756	504982.780925	44.399847
3503.783271	504961.149601	44.404852
3503.583205	504942.659535	44.409857
3503.501753	504935.233374	44.414861
3503.596987	504934.408645	44.419866
3503.583645	504946.859789	44.424871
3503.689751	504923.868006	44.429876
3503.807502	504904.113128	44.434881
3503.545506	504899.093963	44.439885
3503.714015	504889.755858	44.444890
3503.398139	504887.275501	44.449895
3503.674059	504884.144946	44.454900
3503.582930	504860.374557	44.459905
3503.838641	504847.682651	44.464909
3503.625839	504843.111149	44.469914
3503.425333	504837.626793	44.474919
3503.613851	504839.418831	44.479924
3503.877799	504828.800458	44.484929
3503.951417	504802.827891	44.489933
3504.045639	504794.361781	44.494938
3503.558600	504794.944835	44.499943
3503.715303	504771.540005	44.504948
3503.622608	504766.595256	44.509953
3503.730712	504755.444801	44.514957
3504.094754	504755.792130	44.519962
3503.380750	504749.073140	44.524967
3503.649540	504727.320545	44.529972
3503.758857	504720.977483	44.534977
3503.648109	504715.225870	44.539981
3504.001199	504713.500067	44.544986
3503.806739	504698.854946	44.549991
3503.793800	504680.638666	44.554996
3503.803586	504677.347710	44.560001
3503.787206	504664.344430	44.565005
3503.925698	504636.893773	44.570010
3503.573402	504637.708568	44.575015
3503.779826	504618.698454	44.580020
3503.810063	504626.183481	44.585025
3503.681888	504613.299045	44.590029
3503.834138	504583.670042	44.595034
3503.383556	504589.763480	44.600039
3503.440196	504584.137189	44.605044
3503.483947	504584.433930	44.610049
3503.576965	504571.463897	44.615053
3503.794481	504548.302193	44.620058
3503.601813	504550.559363	44.625063
3503.500261	504536.253669	44.630068
3503.628567	504539.421643	44.635073
3503.387832	504537.941498	44.640077
3503.383347	504519.571894	44.645082
3503.595344	504510.783392	44.650087
3503.505254	504498.095280	44.655092
3503.382872	504503.327163	44.660097
3503.710423	504495.684352	44.665101
3503.508207	504498.803358	44.670106
3503.432914	504502.610801	44.675111
3503.620851	504484.716819	44.680116
3503.714904	504468.912550	44.685121
3503.353159	504459.050737	44.690125
3503.681680	504452.470505	44.695130
3503.571987	504455.878538	44.700135
3503.802688	504448.807692	44.705140
3503.347156	504428.231956	44.710145
3503.527510	504419.296588	44.715149
3503.867208	504414.131578	44.720154
3503.325414	504413.205078	44.725159
3503.803820	504404.475631	44.730164
3503.757045	504403.673322	44.735169
3503.899708	504391.100168	44.740173
3503.970220	504371.099120	44.745178
3503.823517	504356.547379	44.750183
3503.614381	504343.574326	44.755188
3503.519621	504330.684401	44.760193
3503.617561	504324.494817	44.765197
3503.847911	504318.587948	44.770202
3503.574865	504317.973220	44.775207
3503.837949	504293.791827	44.780212
3503.762820	504282.163955	44.785217
3503.749574	504271.690272	44.790221
3503.657286	504253.789736	44.795226
3503.733777	504264.911365	44.800231
3503.681676	504244.018612	44.805236
3503.471973	504234.436289	44.810241
3503.256007	504231.180930	44.815245
3503.721341	504234.346299	44.820250
3503.444720	504232.821192	44.825255
3503.399122	504229.285867	44.830260
3503.547456	504214.130691	44.835265
3503.492300	504199.766782	44.840269
3503.482386	504182.662882	44.845274
3503.605104	504188.918888	44.850279
3503.562009	504171.465965	44.855284
3503.460837	504178.415264	44.860289
3503.652277	504172.615712	44.865293
3503.637836	504159.206887	44.870298
3503.583458	504151.573683	44.875303
3503.343674	504141.692415	44.880308
3503.285386	504133.654956	44.885313
3503.594537	504139.021177	44.890317
3503.873505	504139.179533	44.895322
3503.650126	504122.159920	44.900327
3503.813738	504099.360401	44.905332
3503.409893	504097.602348	44.910337
3503.453452	504093.445606	44.915341
3503.643647	504091.745489	44.920346
3503.732289	504085.405466	44.925351
3503.788461	504076.691983	44.930356
3503.796826	504073.654180	44.935361
3503.340545	504061.175454	44.940365
3503.793015	504062.318556	44.945370
3503.567408	504059.115296	44.950375
3504.041818	504026.701587	44.955380
3503.688285	504021.797853	44.960385
3503.338044	504015.071693	44.965389
3503.748619	504002.810178	44.970394
3503.718936	504004.586181	44.975399
3503.586875	503977.025429	44.980404
3503.905850	503987.754649	44.985409
3503.681209	503964.105364	44.990413
3503.964873	503966.641584	44.995418
3503.638580	503957.482405	45.000423
3503.709024	503927.460356	45.005428
3503.723857	503931.709157	45.010433
3503.480089	503927.547178	45.015437
3503.829593	503920.811605	45.020442
3503.594502	503898.125449	45.025447
3503.404708	503901.090770	45.030452
3503.355373	503878.223403	45.035457
3503.416190	503876.391888	45.040461
3503.803896	503881.695163	45.045466
3503.688722	503878.221372	45.050471
3503.933713	503852.979448	45.055476
3503.716223	503833.681223	45.060481
3503.943183	503838.605045	45.065485
3503.818107	503813.117899	45.070490
3503.784906	503812.313417	45.075495
3503.761960	503795.970335	45.080500
3503.768238	503796.728494	45.085505
3503.730426	503794.052205	45.090509
3503.740892	503762.521081	45.095514
3503.804231	503756.235548	45.100519
3503.537132	503746.611420	45.105524
3503.636057	503743.356810	45.110529
3503.614049	503733.187847	45.115533
3504.027898	503715.965908	45.120538
3503.888974	503708.295264	45.125543
3503.983773	503704.332768	45.130548
3503.796957	503684.118563	45.135553
3503.918947	503682.935282	45.140557
3503.937209	503667.749585	45.145562
3503.887978	503664.973862	45.150567
3503.844245	503624.442573	45.155572
3503.820475	503623.585982	45.160577
3503.473812	503626.626751	45.165581
3503.741040	503606.290086	45.170586
3503.553557	503592.149034	45.175591
3503.758836	503574.555044	45.180596
3503.511678	503568.571566	45.185601
3503.588884	503569.116086	45.190605
3503.806645	503559.820102	45.195610
3503.596766	503542.595354	45.200615
3503.710650	503525.218200	45.205620
3503.846406	503522.160168	45.210625
3503.538720	503522.461862	45.215629
3503.724764	503525.469064	45.220634
3503.579547	503495.379144	45.225639
3503.242164	503489.106239	45.230644
3503.560767	503485.209542	45.235649
3503.506900	503480.916223	45.240653
3503.809933	503476.566496	45.245658
3503.560697	503487.335217	45.250663
3503.750788	503457.951387	45.255668
3503.702065	503444.598046	45.260673
3503.752858	503444.033323	45.265677
3503.975154	503430.080425	45.270682
3503.490329	503411.178260	45.275687
3503.858385	503398.163894	45.280692
3504.121907	503393.567339	45.285697
3503.879092	503388.595318	45.290701
3503.849722	503366.483285	45.295706
3503.677887	503361.854310	45.300711
3503.384870	503369.036690	45.305716
3503.723563	503360.328811	45.310721
3503.442648	503352.022519	45.315725
3503.709190	503325.764227	45.320730
3503.604676	503320.061782	45.325735
3503.826405	503314.560825	45.330740
3503.908439	503312.219793	45.335745
3503.509985	503314.003540	45.340749
3504.044086	503271.507526	45.345754
3503.704222	503277.533304	45.350759
3503.765414	503270.387557	45.355764
3504.096072	503259.302202	45.360769
3503.563566	503241.773877	45.365773
3503.567203	503235.143319	45.370778
3503.851992	503226.798169	45.375783
3503.899334	503218.490544	45.380788
3503.714575	503203.387145	45.385793
3503.465118	503187.281742	45.390797
3503.322712	503183.306009	45.395802
3503.459905	503181.867238	45.400807
3503.541054	503180.234880	45.405812
3503.437869	503182.326248	45.410817
3503.379247	503169.733426	45.415821
3503.771392	503149.325881	45.420826
3503.732704	503152.722943	45.425831
3503.729056	503141.943405	45.430836
3503.759308	503137.383653	45.435841
3503.530074	503118.795054	45.440845
3503.866584	503083.972081	45.445850
3503.846350	503098.956178	45.450855
3503.623859	503095.144916	45.455860
3503.841369	503085.595667	45.460865
3503.448576	503066.779808	45.465869
3503.872573	503046.518944	45.470874
3503.763506	503047.396588	45.475879
3503.501896	503036.101033	45.480884
3503.650449	503035.166567	45.485889
3503.516804	503010.641228	45.490893
3503.548700	502997.578475	45.495898
3503.386566	503008.941057	45.500903
3503.320854	503015.632153	45.505908
3503.675092	503001.405007	45.510913
3503.102445	503006.101162	45.515917
3503.186251	503006.138543	45.520922
3503.402482	502996.943728	45.525927
3503.488225	502988.984205	45.530932
3503.601023	502967.557762	45.535937
3503.544524	502965.036134	45.540941
3503.592082	502944.379146	45.545946
3503.752090	502962.472786	45.550951
3503.497782	502957.198790	45.555956
3503.640961	502933.085094	45.560961
3503.477154	502929.264521	45.565965
3503.617811	502912.135590	45.570970
3503.319565	502919.015309	45.575975
3503.806873	502901.224240	45.580980
3503.868043	502917.207858	45.585985
3503.534140	502889.525471	45.590989
3504.023578	502870.721801	45.595994
3503.710603	502863.533803	45.600999
3503.909337	502874.839437	45.606004
3503.868965	502842.504917	45.611009
3503.863772	502828.688724	45.616013
3503.950234	502826.599988	45.621018
3503.630393	502821.589367	45.626023
3503.613311	502791.933503	45.631028
3503.637431	502788.437480	45.636033
3503.642138	502786.513497	45.641037
3503.988809	502775.526532	45.646042
3503.618637	502761.666748	45.651047
3503.446141	502745.700614	45.656052
3503.664327	502735.442500	45.661057
3503.485225	502731.067568	45.666061
3503.551807	502732.524812	45.671066
3503.640132	502739.950848	45.676071
3503.445440	502711.740058	45.681076
3503.573292	502701.040693	45.686081
3503.242635	502701.346029	45.691085
3503.324986	502687.768951	45.696090
3503.322585	502690.603631	45.701095
3503.271700	502693.496587	45.706100
3503.485269	502701.307742	45.711105
3503.430632	502688.055988	45.716109
3503.770353	502691.393331	45.721114
3503.298672	502678.207483	45.726119
3503.473629	502669.221470	45.731124
3503.212171	502667.187704	45.736129
3503.178194	502667.243702	45.741133
3503.400015	502668.878865	45.746138
3503.423593	502673.480873	45.751143
3503.448580	502656.015689	45.756148
3503.797706	502648.267447	45.761153
3503.590538	502653.513278	45.766157
3503.712884	502628.693888	45.771162
3503.631641	502617.470783	45.776167
3503.768825	502610.667046	45.781172
3503.803027	502601.703246	45.786177
3503.620693	502608.868439	45.791181
3503.700753	502574.084995	45.796186
3503.873447	502571.375250	45.801191
3503.649003	502564.831101	45.806196
3503.777006	502562.128417	45.811201
3503.444777	502552.159641	45.816205
3503.474925	502521.179929	45.821210
3503.239438	502515.548537	45.826215
3503.295401	502509.364951	45.831220
3503.438383	502514.656707	45.836225
3503.330102	502517.508150	45.841229
3503.425770	502517.290594	45.846234
3503.628846	502520.750791	45.851239
3503.732951	502523.568666	45.856244
3504.044752	502498.972214	45.861249
3503.621512	502484.209568	45.866253
3503.785576	502471.479827	45.871258
3503.560748	502469.946378	45.876263
3503.636916	502445.488319	45.881268
3503.756874	502433.777781	45.886273
3503.442773	502428.614303	45.891277
3503.510398	502435.132704	45.896282
3503.529514	502426.879782	45.901287
3503.586906	502424.542528	45.906292
3503.749057	502404.271702	45.911297
3503.472996	502396.520936	45.916301
3503.588794	502382.887724	45.921306
3503.351596	502392.187427	45.926311
3503.289008	502385.921310	45.931316
3503.759359	502386.859248	45.936321
3503.451539	502370.914164	45.941325
3503.797747	502344.489986	45.946330
3503.679125	502344.660590	45.951335
3503.560569	502342.199294	45.956340
3503.518147	502350.304130	45.961345
3503.423507	502353.052217	45.966349
3503.826136	502334.160473	45.971354
3503.822137	502323.279266	45.976359
3503.491320	502311.488052	45.981364
3503.872916	502303.582688	45.986369
3503.184642	502303.134739	45.991373
3503.653981	502296.430224	45.996378
3503.645037	502276.591201	46.001383
3503.542342	502254.843661	46.006388
3503.754297	502249.596986	46.011393
3503.739892	502258.912160	46.016397
3503.678264	502247.078358	46.021402
3503.502143	502227.113861	46.026407
3503.410853	502223.838423	46.031412
3503.833170	502208.334543	46.036417
3503.636586	502214.945398	46.041421
3503.807333	502207.275771	46.046426
3503.850597	502182.367027	46.051431
3503.392458	502171.759959	46.056436
3504.008542	502166.398773	46.061441
3503.666125	502179.460634	46.066445
3503.702613	502146.151034	46.071450
3503.799098	502132.672524	46.076455
3503.554899	502136.760242	46.081460
3503.857755	502120.971484	46.086465
3503.700013	502121.249499	46.091469
3503.564473	502097.381174	46.096474
3503.484926	502078.211069	46.101479
3503.861192	502071.419953	46.106484
3503.895922	502081.587892	46.111489
3503.522053	502072.384637	46.116493
3503.778503	502036.104452	46.121498
3503.680581	502046.040307	46.126503
3503.336718	502043.260281	46.131508
3503.805647	502028.001948	46.136513
3503.674946	502033.185261	46.141517
3503.688439	502011.621515	46.146522
3503.588836	501999.742936	46.151527
3503.721274	501984.942662	46.156532
3503.849579	501991.907165	46.161537
3503.711776	501980.641981	46.166541
3503.538872	501970.040323	46.171546
3503.784173	501964.889524	46.176551
3503.487055	501953.295202	46.181556
3504.109313	501959.776733	46.186561
3503.741890	501931.946302	46.191565
3503.718103	501919.094012	46.196570
3503.675437	501910.799999	46.201575
3503.512090	501904.701480	46.206580
3503.663767	501899.666687	46.211585
3503.103199	501876.573844	46.216589
3503.368588	501865.346091	46.221594
3503.622385	501861.560513	46.226599
3503.653564	501862.871580	46.231604
3503.914461	501857.819513	46.236609
3503.560540	501853.826296	46.241613
3503.663056	501836.904813	46.246618
3503.491431	501827.213932	46.251623
3503.886950	501813.080541	46.256628
3504.042794	501797.618420	46.261633
3503.546716	501803.365696	46.266637
3503.886767	501769.501264	46.271642
3503.792888	501772.046860	46.276647
3503.826088	501769.662729	46.281652
3503.931954	501754.309699	46.286657
3503.667313	501740.331204	46.291661
3503.609577	501723.232481	46.296666
3503.604102	501726.928256	46.301671
3503.388773	501722.710644	46.306676
3503.628811	501718.572906	46.311681
3503.328051	501704.903781	46.316685
3503.756231	501682.413638	46.321690
3503.529750	501686.549273	46.326695
3503.400536	501681.255123	46.331700
3503.926745	501682.032428	46.336705
3503.361657	501657.877095	46.341709
3503.344202	501647.453137	46.346714
3503.585401	501633.647685	46.351719
3503.318373	501635.309593	46.356724
3503.566998	501627.020024	46.361729
3503.535419	501631.985327	46.366733
3503.623375	501628.580218	46.371738
3503.713161	501615.760373	46.376743
3503.416470	501610.796364	46.381748
3503.707647	501601.943290	46.386753
3503.569211	501610.620408	46.391757
3503.469224	501592.364084	46.396762
3503.404030	501587.515327	46.401767
3503.194582	501592.103830	46.406772
3503.605974	501594.417747	46.411777
3503.502929	501578.895123	46.416781
3503.436281	501559.165649	46.421786
3503.487690	501541.847039	46.426791
3503.434175	501549.042915	46.431796
3503.619498	501537.321455	46.436801
3503.417886	501548.387518	46.441805
3503.511205	501534.959671	46.446810
3503.616972	501536.208358	46.451815
3503.501097	501528.735586	46.456820
3503.804436	501501.456468	46.461825
3503.194728	501508.841497	46.466829
3503.296442	501498.196154	46.471834
3503.423375	501494.582396	46.476839
3503.338785	501496.974717	46.481844
3503.547473	501493.196190	46.486849
3503.318838	501506.291177	46.491853
3503.679865	501471.967322	46.496858
3503.559588	501465.153224	46.501863
3503.244586	501455.029259	46.506868
3503.945797	501443.124969	46.511873
3503.443789	501455.959505	46.516877
3503.747279	501443.004528	46.521882
3503.525576	501438.636008	46.526887
3503.374032	501418.767949	46.531892
3504.013996	501407.278243	46.536897
3503.503568	501421.480763	46.541901
3503.759828	501408.583842	46.546906
3503.444759	501396.030291	46.551911
3503.611996	501373.429152	46.556916
3503.540971	501357.800042	46.561921
3503.279482	501374.797752	46.566925
3503.450772	501366.621518	46.571930
3503.613734	501364.419288	46.576935
3503.323073	501354.746963	46.581940
3503.513902	501359.677190	46.586945
3503.474720	501337.564175	46.591949
3503.379845	501320.420318	46.596954
3503.486455	501311.849352	46.601959
3503.579967	501316.794972	46.606964
3503.632923	501311.370688	46.611969
3503.504068	501312.808321	46.616973
3503.377761	501308.171611	46.621978
3503.472491	501286.594146	46.626983
3503.582926	501279.186733	46.631988
3503.609585	501266.781545	46.636993
3503.364268	501268.136357	46.641997
3503.686386	501255.431382	46.647002
3503.464942	501252.884963	46.652007
3503.113137	501257.394819	46.657012
3503.299662	501246.381606	46.662017
3503.225030	501252.669845	46.667021
3503.284868	501241.879118	46.672026
3503.569520	501221.081419	46.677031
3503.471857	501221.451184	46.682036
3503.596360	501221.836453	46.687041
3503.373757	501235.285000	46.692045
3503.558178	501229.991762	46.697050
3503.629520	501233.726115	46.702055
3503.070710	501237.711913	46.707060
3503.560529	501226.549520	46.712065
3503.464193	501210.671199	46.717069
3503.371800	501198.942794	46.722074
3503.811333	501190.572233	46.727079
3503.680474	501196.312597	46.732084
3503.930035	501186.605414	46.737089
3503.741001	501175.449049	46.742093
3503.711409	501159.053967	46.747098
3503.593797	501146.620881	46.752103
3503.687501	501154.755364	46.757108
3503.684874	501143.063351	46.762113
3503.612795	501119.537998	46.767117
3503.631945	501103.641329	46.772122
3503.619987	501101.972881	46.777127
3503.541820	501096.214938	46.782132
3503.797788	501095.465862	46.787137
3503.272666	501086.690933	46.792141
3503.379559	501064.402641	46.797146
3503.664980	501058.890921	46.802151
3503.132559	501066.871320	46.807156
3503.416860	501048.503084	46.812161
3503.598250	501060.774339	46.817165
3503.614375	501048.826216	46.822170
3503.520855	501042.918831	46.827175
3503.611527	501039.513180	46.832180
3504.053281	501020.816329	46.837185
3503.600390	501008.587988	46.842189
3503.583554	501004.186982	46.847194
3503.829256	501011.082698	46.852199
3503.280652	500983.785586	46.857204
3503.570158	500971.136181	46.862209
3503.799170	500972.314812	46.867213
3503.802014	500968.467475	46.872218
3503.865395	500971.292033	46.877223
3503.704588	500944.895296	46.882228
3503.871700	500919.003482	46.887233
3503.556674	500923.153287	46.892237
3503.607032	500920.715714	46.897242
3503.637492	500899.704729	46.902247
3503.276823	500894.548160	46.907252
3503.446984	500878.273101	46.912257
3503.424426	500877.163099	46.917261
3503.409336	500870.433382	46.922266
3503.389183	500875.802029	46.927271
3503.603334	500878.299068	46.932276
3504.009136	500862.189221	46.937281
3503.380508	500849.836694	46.942285
3503.526945	500822.682571	46.947290
3503.868568	500830.727401	46.952295
3503.589887	500821.255361	46.957300
3503.447718	500816.924735	46.962305
3503.606962	500816.241553	46.967309
3503.540990	500794.537039	46.972314
3503.577214	500789.469564	46.977319
3503.542603	500791.752844	46.982324
3503.905259	500785.014010	46.987329
3503.695251	500778.112595	46.992333
3503.644542	500760.809366	46.997338
3503.941198	500734.795575	47.002343
3503.447494	500739.479841	47.007348
3503.475999	500724.593711	47.012353
3503.711577	500741.766552	47.017357
3503.727877	500713.418004	47.022362
3503.826167	500701.001101	47.027367
3503.677089	500704.922256	47.032372
3503.949153	500680.734518	47.037377
3503.448156	500674.638323	47.042381
3503.155651	500659.853493	47.047386
3503.406438	500642.907443	47.052391
3503.346508	500649.699751	47.057396
3503.508667	500637.323327	47.062401
3503.617942	500648.442047	47.067405
3503.622598	500639.633782	47.072410
3503.524334	500648.507490	47.077415
3503.284856	500629.310483	47.082420
3503.754751	500604.990139	47.087425
3503.679776	500608.950221	47.092429
3503.656984	500609.460020	47.097434
3503.608313	500604.254056	47.102439
3503.047475	500601.508093	47.107444
3503.323933	500605.463251	47.112449
3503.501085	500585.238602	47.117453
3503.320674	500563.551894	47.122458
3503.249173	500558.450761	47.127463
3503.402862	500557.009173	47.132468
3503.383712	500564.655579	47.137473
3503.245920	500557.489573	47.142477
3503.501937	500550.969979	47.147482
3503.487039	500552.490899	47.152487
3503.259574	500561.283834	47.157492
3503.749426	500552.601314	47.162497
3503.454791	500548.952758	47.167501
3503.229840	500537.801670	47.172506
3503.757750	500527.139006	47.177511
3503.575885	500537.392679	47.182516
3503.846070	500523.328697	47.187521
3503.669267	500520.218314	47.192525
3503.437875	500502.690300	47.197530
3503.519039	500487.745031	47.202535
3503.578169	500486.571475	47.207540
3503.672156	500477.192208	47.212545
3503.574602	500489.102995	47.217549
3503.333103	500474.866754	47.222554
3503.719549	500477.640330	47.227559
3503.451695	500456.827828	47.232564
3503.597689	500436.354842	47.237569
3503.407096	500434.208378	47.242573
3503.694062	500434.264276	47.247578
3503.405191	500435.170464	47.252583
3503.253725	500440.813089	47.257588
3503.658673	500430.422895	47.262593
3503.500373	500411.617773	47.267597
3503.298995	500395.755328	47.272602
3503.445257	500379.939162	47.277607
3503.179275	500394.255717	47.282612
3503.442918	500385.355775	47.287617
3503.593408	500385.281386	47.292621
3503.631637	500383.503701	47.297626
3503.534342	500385.847559	47.302631
3503.792748	500361.155359	47.307636
3503.870881	500353.651431	47.312641
3503.497741	500351.888141	47.317645
3503.486343	500355.382661	47.322650
3503.884968	500332.743635	47.327655
3503.374851	500326.547523	47.332660
3503.697277	500307.362598	47.337665
3503.560478	500297.108569	47.342669
3503.271750	500296.850504	47.347674
3503.726843	500302.549162	47.352679
3503.766651	500286.041072	47.357684
3503.678777	500257.657647	47.362689
3503.523335	500257.935326	47.367693
3503.591076	500250.989807	47.372698
3503.802921	500255.714543	47.377703
3503.497168	500259.103748	47.382708
3503.621862	500223.448130	47.387713
3503.606304	500219.957875	47.392717
3503.594571	500213.834811	47.397722
3503.987383	500213.924601	47.402727
3503.787926	500200.845739	47.407732
3503.873568	500176.585546	47.412737
3503.372030	500182.384820	47.417741
3503.574895	500165.597750	47.422746
3503.969318	500155.968353	47.427751
3503.574393	500151.778751	47.432756
3503.699329	500116.072262	47.437761
3503.620086	500121.754192	47.442765
3503.631526	500117.854694	47.447770
3503.762794	500111.152179	47.452775
3503.679424	500106.002173	47.457780
3503.717544	500077.497309	47.462785
3503.520652	500081.729876	47.467789
3503.294482	500074.324545	47.472794
3503.389672	500073.246502	47.477799
3503.045754	500080.995065	47.482804
3503.585449	500066.078213	47.487809
3503.521007	500078.439617	47.492813
3503.505140	500052.322371	47.497818
3503.562047	500034.900191	47.502823
3503.669316	500030.074371	47.507828
3504.040777	500023.283241	47.512833
3503.577672	500034.442188	47.517837
3503.807017	500017.397696	47.522842
3503.566821	499983.469727	47.527847
3503.579146	499991.516363	47.532852
3503.677419	499979.757021	47.537857
3503.583423	499988.174802	47.542861
3503.676533	499965.887319	47.547866
3503.318113	499950.049299	47.552871
3503.292147	499942.713512	47.557876
3503.265387	499929.303437	47.562881
3503.284287	499938.462699	47.567885
3503.373805	499933.639659	47.572890
3503.658691	499931.468605	47.577895
3503.335865	499944.275900	47.582900
3503.340739	499931.974468	47.587905
3503.586297	499936.238380	47.592909
3503.793698	499913.527808	47.597914
3503.650593	499899.224936	47.602919
3503.556079	499893.874149	47.607924
3503.721980	499891.013213	47.612929
3503.710541	499880.334170	47.617933
3503.454373	499866.808446	47.622938
3503.642586	499848.808509	47.627943
3503.218693	499851.811499	47.632948
3503.404417	499842.012438	47.637953
3503.171439	499855.362420	47.642957
3503.360771	499836.299267	47.647962
3503.124803	499848.485458	47.652967
3503.166691	499850.655527	47.657972
3503.766195	499836.235235	47.662977
3503.527111	499841.436313	47.667981
3503.110803	499820.292190	47.672986
3503.817130	499790.820714	47.677991
3503.589990	499789.945459	47.682996
3503.392297	499787.800039	47.688001
3503.251206	499794.807981	47.693005
3503.624160	499791.762442	47.698010
3503.788457	499788.800502	47.703015
3503.370746	499769.782602	47.708020
3503.600332	499750.156169	47.713025
3503.335829	499741.035659	47.718029
3503.243688	499747.276573	47.723034
3503.596661	499730.212268	47.728039
3503.398609	499742.848124	47.733044
3503.433438	499735.148299	47.738049
3503.566327	499736.747171	47.743053
3503.438993	499733.983176	47.748058
3503.427912	499703.460668	47.753063
3503.187567	499707.092742	47.758068
3503.458135	499691.813150	47.763073
3503.469015	499689.077924	47.768077
3503.445188	499687.360599	47.773082
3503.495980	499694.388873	47.778087
3503.397591	499694.910646	47.783092
3503.504910	499690.641555	47.788097
3503.444303	499684.222311	47.793101
3503.348787	499670.266080	47.798106
3503.459506	499646.608656	47.803111
3503.085926	499657.854929	47.808116
3503.286668	499644.914893	47.813121
3503.505587	499638.603315	47.818125
3503.119193	499647.118091	47.823130
3503.361785	499644.801824	47.828135
3503.436460	499641.904646	47.833140
3503.672787	499643.385936	47.838145
3503.392187	499651.377780	47.843149
3503.418446	499618.065076	47.848154
3503.439877	499612.948986	47.853159
3503.338848	499603.549463	47.858164
3503.436836	499608.039260	47.863169
3503.706987	499607.945957	47.868173
3502.968643	499609.024467	47.873178
3503.530765	499603.468570	47.878183
3503.380577	499598.632704	47.883188
3503.373039	499600.709373	47.888193
3503.756585	499603.129198	47.893197
3503.347135	499585.830911	47.898202
3503.595024	499565.998901	47.903207
3503.352039	499564.771792	47.908212
3503.286612	499546.356050	47.913217
3503.531234	499550.772065	47.918221
3503.616718	499554.909504	47.923226
3503.728874	499545.526878	47.928231
3503.579738	499538.463498	47.933236
3503.648073	499516.381858	47.938241
3503.242833	499521.811774	47.943245
3503.229272	499520.042189	47.948250
3503.755944	499501.127849	47.953255
3503.142632	499511.450299	47.958260
3503.238340	499508.954745	47.963265
3503.416511	499515.659229	47.968269
3503.067073	499516.271307	47.973274
3503.551877	499512.701831	47.978279
3503.598919	499512.441305	47.983284
3503.328636	499475.378609	47.988289
3503.164289	499478.391260	47.993293
3503.494449	499474.694355	47.998298
3503.931807	499460.754983	48.003303
3503.328678	499462.925801	48.008308
3503.552617	499464.510307	48.013313
3503.970947	499458.521500	48.018317
3503.590575	499435.447629	48.023322
3503.636122	499426.379197	48.028327
3503.752546	499424.133464	48.033332
3503.607261	499428.003677	48.038337
3503.646142	499414.481599	48.043341
3503.049045	499391.695033	48.048346
3503.145313	499385.503995	48.053351
3503.215117	499380.177706	48.058356
3503.345491	499378.942196	48.063361
3503.392842	499377.264213	48.068365
3503.430227	499380.244997	48.073370
3503.238340	499380.376583	48.078375
3503.152723	499379.580184	48.083380
3503.365803	499368.511000	48.088385
3503.536999	499370.913797	48.093389
3503.188187	499379.119029	48.098394
3503.463332	499368.293144	48.103399
3503.421887	499376.500419	48.108404
3503.643229	499362.088896	48.113409
3503.490677	499352.292411	48.118413
3503.379132	499335.098662	48.123418
3503.676956	499336.418394	48.128423
3503.269269	499337.647145	48.133428
3503.542652	499339.932553	48.138433
3503.154562	499338.677740	48.143437
3503.293240	499338.149620	48.148442
3503.562796	499325.350343	48.153447
3503.378895	499314.647599	48.158452
3503.805745	499290.686632	48.163457
3503.627331	499289.702408	48.168461
3503.656622	499283.116946	48.173466
3503.637547	499284.638633	48.178471
3503.413282	499283.206058	48.183476
3503.366675	499275.822638	48.188481
3503.460587	499254.850317	48.193485
3503.233232	499249.874687	48.198490
3503.710159	499245.901429	48.203495
3503.316715	499246.115494	48.208500
3503.149387	499244.471429	48.213505
3503.626865	499241.561145	48.218509
3503.352839	499235.479203	48.223514
3503.522708	499245.273045	48.228519
3503.237681	499237.826048	48.233524
3503.648501	499213.158803	48.238529
3503.500042	499206.652028	48.243533
3503.450904	499209.747759	48.248538
3503.325927	499197.719458	48.253543
3503.332463	499206.627938	48.258548
3503.374392	499205.254528	48.263553
3503.836451	499199.764945	48.268557
3503.720587	499187.532708	48.273562
3503.557794	499167.309567	48.278567
3503.191523	499172.227207	48.283572
3503.437048	499163.886369	48.288577
3503.624567	499161.173767	48.293581
3502.950921	499165.785633	48.298586
3503.319964	499153.476733	48.303591
3503.590682	499156.319431	48.308596
3503.797205	499154.869381	48.313601
3503.754182	499129.716907	48.318605
3503.663929	499128.668117	48.323610
3503.536253	499102.060935	48.328615
3503.514589	499110.670185	48.333620
3503.589406	499105.343022	48.338625
3503.535381	499097.808834	48.343629
3503.275097	499091.471559	48.348634
3503.640174	499075.366548	48.353639
3503.352549	499068.375494	48.358644
3503.664323	499068.174365	48.363649
3503.650695	499070.302680	48.368653
3503.547854	499069.660857	48.373658
3503.725199	499050.092540	48.378663
3503.403201	499036.019744	48.383668
3503.378571	499038.048556	48.388673
3503.624037	499022.519251	48.393677
3503.634826	499026.567373	48.398682
3503.798588	499029.477618	48.403687
3503.463074	499007.408559	48.408692
3503.725957	498982.258152	48.413697
3503.593169	498986.177107	48.418701
3503.549051	498987.044682	48.423706
3503.341753	498973.510558	48.428711
3503.337831	498988.141173	48.433716
3503.198820	498979.658536	48.438721
3503.493461	498976.625239	48.443725
3503.385767	498962.771629	48.448730
3503.575107	498944.011266	48.453735
3503.689309	498948.296175	48.458740
3503.542914	498937.081050	48.463745
3503.556259	498940.420066	48.468749
3503.186372	498937.846153	48.473754
3503.630862	498935.244771	48.478759
3503.565778	498912.829116	48.483764
3503.268156	498905.485218	48.488769
3503.370688	498890.433996	48.493773
3503.506341	498893.854937	48.498778
3503.488010	498885.707542	48.503783
3503.408183	498875.190580	48.508788
3503.555363	498883.925121	48.513793
3503.425240	498873.365484	48.518797
3503.400503	498867.649001	48.523802
3503.356068	498854.443409	48.528807
3503.246620	498846.411644	48.533812
3503.387711	498842.542001	48.538817
3503.067134	498839.605917	48.543821
3503.446560	498842.887092	48.548826
3503.448728	498832.154652	48.553831
3503.457219	498839.999918	48.558836
3503.520474	498839.534327	48.563841
3503.453694	498842.784779	48.568845
3503.324081	498835.566167	48.573850
3503.354057	498820.981964	48.578855
3503.226499	498808.751317	48.583860
3503.201118	498802.427436	48.588865
3503.347589	498794.203330	48.593869
3503.274911	498799.429030	48.598874
3503.411065	498795.762650	48.603879
3503.586872	498805.100185	48.608884
3503.423879	498801.632956	48.613889
3503.373931	498796.781030	48.618893
3503.324877	498799.117470	48.623898
3503.351695	498798.809507	48.628903
3503.498399	498802.886820	48.633908
3503.502923	498784.155502	48.638913
3503.554560	498756.051391	48.643917
3503.644705	498758.821445	48.648922
3503.498026	498749.934924	48.653927
3503.269911	498747.692939	48.658932
3503.339514	498755.326089	48.663937
3503.741545	498755.363810	48.668941
3503.516629	498753.020073	48.673946
3503.289116	498725.820633	48.678951
3503.447616	498714.557180	48.683956
3503.594103	498719.596394	48.688961
3503.654285	498704.804829	48.693965
3503.120866	498707.977187	48.698970
3503.479969	498708.831669	48.703975
3503.080511	498713.096572	48.708980
3503.066457	498713.655667	48.713985
3503.545271	498711.251323	48.718989
3503.285822	498717.569660	48.723994
3503.672491	498704.498316	48.728999
3503.452371	498682.866232	48.734004
3503.449861	498677.956153	48.739009
3503.570963	498664.825506	48.744013
3503.346950	498669.973915	48.749018
3503.486345	498656.334134	48.754023
3503.406200	498667.180281	48.759028
3503.533458	498665.287108	48.764033
3503.493735	498639.880309	48.769037
3503.082182	498639.692252	48.774042
3503.627430	498615.407932	48.779047
3503.592133	498628.221342	48.784052
3503.643210	498617.734163	48.789057
3503.592635	498620.475856	48.794061
3503.698884	498621.623426	48.799066
3503.741425	498582.940110	48.804071
3503.857273	498574.923240	48.809076
3503.896429	498570.158418	48.814081
3503.763257	498568.964507	48.819085
3503.428614	498549.375320	48.824090
3503.582862	498531.581930	48.829095
3503.410613	498537.076564	48.834100
3503.567342	498531.027549	48.839105
3503.475419	498522.385382	48.844109
3503.319367	498528.333074	48.849114
3503.345016	498526.000330	48.854119
3503.360181	498528.478526	48.859124
3503.251293	498510.422961	48.864129
3503.296206	498492.191196	48.869133
3503.230570	498497.820864	48.874138
3503.501939	498481.325141	48.879143
3503.312783	498487.126207	48.884148
3503.103397	498487.513685	48.889153
3503.319466	498482.670255	48.894157
3503.256386	498492.653198	48.899162
3503.357641	498476.690599	48.904167
3503.344614	498488.032487	48.909172
3503.356956	498484.031243	48.914177
3503.222790	498492.253576	48.919181
3503.036167	498485.043833	48.924186
3503.575190	498474.935069	48.929191
3503.226136	498485.722577	48.934196
3503.369658	498476.587558	48.939201
3503.450064	498455.515192	48.944205
3503.341877	498447.786795	48.949210
3503.341180	498435.383971	48.954215
3503.143321	498444.882000	48.959220
3503.161694	498443.765377	48.964225
3503.405764	498433.196964	48.969229
3503.133176	498450.249821	48.974234
3503.383176	498442.717932	48.979239
3503.346677	498445.963669	48.984244
3503.248355	498442.587398	48.989249
3503.502265	498437.991097	48.994253
3503.382926	498441.148679	48.999258
3503.364762	498446.669611	49.004263
3503.607137	498432.659016	49.009268
3503.542455	498405.838351	49.014273
3503.667350	498388.859450	49.019277
3503.084430	498399.329602	49.024282
3503.237491	498394.091112	49.029287
3503.211541	498401.283894	49.034292
3502.959337	498391.249513	49.039297
3503.304288	498387.600673	49.044301
3502.844246	498396.026428	49.049306
3503.243485	498388.268431	49.054311
3503.387031	498399.028760	49.059316
3503.338420	498393.417149	49.064321
3503.760097	498387.731206	49.069325
3503.172950	498397.645158	49.074330
3503.056636	498395.587956	49.079335
3503.217925	498388.323187	49.084340
3503.335225	498391.392753	49.089345
3503.093219	498395.329097	49.094349
3503.141681	498398.612040	49.099354
3503.279832	498382.744775	49.104359
3503.118343	498374.467902	49.109364
3503.201813	498371.214758	49.114369
3503.514806	498364.735995	49.119373
3503.336251	498357.322428	49.124378
3503.253475	498359.816127	49.129383
3503.459044	498364.238609	49.134388
3503.146102	498365.553697	49.139393
3503.296582	498361.378720	49.144397
3503.246809	498361.639724	49.149402
3503.531075	498357.241103	49.154407
3503.472715	498362.920287	49.159412
3503.566660	498359.614861	49.164417
3503.887723	498352.932320	49.169421
3503.481659	498323.229265	49.174426
3503.373498	498315.146435	49.179431
3503.500279	498317.455145	49.184436
3503.471215	498307.537324	49.189441
3503.424943	498290.787883	49.194445
3503.433760	498297.823337	49.199450
3503.469884	498286.578959	49.204455
3503.262837	498270.766155	49.209460
3503.212890	498257.054749	49.214465
3503.461771	498244.257974	49.219469
3503.410044	498250.644893	49.224474
3503.444363	498253.525098	49.229479
3503.612778	498239.576667	49.234484
3503.368223	498253.385288	49.239489
3503.728487	498245.835890	49.244493
3503.383110	498238.398016	49.249498
3503.484123	498207.298380	49.254503
3503.487585	498217.068458	49.259508
3503.496420	498204.461470	49.264513
3503.737116	498195.209700	49.269517
3503.290295	498202.266580	49.274522
3503.381442	498204.783437	49.279527
3503.615672	498197.102064	49.284532
3503.507536	498184.867924	49.289537
3503.406726	498166.911987	49.294541
3503.336838	498167.277423	49.299546
3503.267394	498154.632147	49.304551
3503.331643	498157.406387	49.309556
3503.311516	498158.624585	49.314561
3503.549513	498149.980720	49.319565
3503.201780	498165.729469	49.324570
3503.371572	498163.930771	49.329575
3503.397788	498168.331023	49.334580
3503.460551	498170.194245	49.339585
3503.855799	498143.806749	49.344589
3503.476925	498133.336618	49.349594
3503.659657	498140.091521	49.354599
3503.400143	498123.730004	49.359604
3503.329303	498140.093139	49.364609
3503.391205	498129.654591	49.369613
3503.574997	498134.485572	49.374618
3503.540855	498101.888362	49.379623
3503.573087	498097.175135	49.384628
3503.582564	498088.972360	49.389633
3503.743728	498087.276270	49.394637
3503.701014	498089.814299	49.399642
3503.770109	498070.059528	49.404647
3503.801247	498047.070711	49.409652
3503.424996	498039.587008	49.414657
3503.659309	498041.271254	49.419661
3503.834347	498047.976782	49.424666
3503.436939	498022.878773	49.429671
3503.561166	498003.115216	49.434676
3503.285036	498012.878969	49.439681
3503.593844	498002.300073	49.444685
3503.213391	498000.233948	49.449690
3503.538813	498002.764431	49.454695
3503.637027	497995.205720	49.459700
3503.342722	497988.215300	49.464705
3503.527285	497950.115689	49.469709
3503.376471	497957.935890	49.474714
3503.502493	497946.525215	49.479719
3503.649414	497955.969007	49.484724
3503.524846	497949.964258	49.489729
3503.816171	497945.311294	49.494733
3503.267351	497933.855393	49.499738
3503.449984	497902.792959	49.504743
3503.746344	497906.644319	49.509748
3503.322480	497908.027597	49.514753
3503.740547	497909.075303	49.519757
3503.583401	497915.732131	49.524762
3503.556159	497897.359293	49.529767
3503.744632	497859.663880	49.534772
3503.481777	497849.630880	49.539777
3503.457858	497844.572081	49.544781
3503.580294	497859.791151	49.549786
3503.417044	497850.704302	49.554791
3503.690775	497853.091098	49.559796
3503.463097	497827.409107	49.564801
3503.479349	497816.218203	49.569805
3503.672773	497816.896412	49.574810
3503.632715	497814.776465	49.579815
3503.662574	497811.126685	49.584820
3503.364693	497812.085050	49.589825
3503.639873	497778.425847	49.594829
3503.227018	497775.149788	49.599834
3503.248992	497770.792481	49.604839
3503.640153	497770.528168	49.609844
3503.253678	497772.209303	49.614849
3503.325821	497770.932262	49.619853
3503.727215	497769.400678	49.624858
3503.278801	497777.926133	49.629863
3503.546293	497766.037350	49.634868
3503.479489	497753.188871	49.639873
3503.733425	497729.253164	49.644877
3503.418922	497728.189108	49.649882
3503.324485	497721.774510	49.654887
3503.925865	497716.211836	49.659892
3503.772937	497723.121199	49.664897
3503.416685	497704.952045	49.669901
3503.269991	497695.457489	49.674906
3503.497831	497680.689214	49.679911
3503.213666	497686.809310	49.684916
3503.005810	497680.767009	49.689921
3503.339183	497673.778514	49.694925
3503.233008	497689.894509	49.699930
3503.634962	497684.667102	49.704935
3503.759037	497680.951780	49.709940
3503.572121	497678.298137	49.714945
3503.679884	497655.954855	49.719949
3503.498265	497648.440228	49.724954
3503.678766	497650.031763	49.729959
3503.852910	497647.017290	49.734964
3503.342481	497648.262389	49.739969
3503.330551	497623.457286	49.744973
3503.132176	497611.591405	49.749978
3503.415221	497604.610838	49.754983
3503.437413	497591.697552	49.759988
3503.316678	497611.207904	49.764993
3503.485460	497596.702027	49.769997
3503.438226	497612.100003	49.775002
3503.389406	497602.691183	49.780007
3503.718044	497594.336487	49.785012
3503.514823	497593.609221	49.790017
3503.733249	497576.969163	49.795021
3503.512252	497565.208081	49.800026
3503.561751	497549.202217	49.805031
3503.344245	497551.767948	49.810036
3503.352494	497553.336090	49.815041
3503.373800	497547.460031	49.820045
3503.457293	497559.040380	49.825050
3503.482860	497544.810231	49.830055
3503.090575	497511.002891	49.835060
3502.962582	497515.883316	49.840065
3503.252762	497501.256922	49.845069
3503.360890	497504.935612	49.850074
3503.121432	497506.593535	49.855079
3503.406457	497503.257753	49.860084
3503.308778	497506.817090	49.865089
3503.548621	497499.488922	49.870093
3503.140963	497502.894745	49.875098
3503.393861	497504.576104	49.880103
3503.730200	497499.105881	49.885108
3503.495653	497509.774617	49.890113
3503.536422	497497.820238	49.895117
3503.278162	497485.254963	49.900122
3502.860700	497468.715308	49.905127
3503.240508	497468.250278	49.910132
3503.093436	497481.790944	49.915137
3503.285591	497456.548340	49.920141
3502.895809	497468.304804	49.925146
3503.302872	497479.378420	49.930151
3503.324187	497468.743398	49.935156
3503.275574	497482.116622	49.940161
3503.448241	497458.244028	49.945165
3503.595755	497462.675908	49.950170
3503.477611	497463.707136	49.955175
3503.627448	497457.658853	49.960180
3503.333193	497462.616197	49.965185
3503.340298	497455.476678	49.970189
3503.299054	497458.318326	49.975194
3503.520027	497443.196553	49.980199
3503.277781	497423.135895	49.985204
3503.234282	497419.902648	49.990209
3503.703621	497413.500090	49.995213
3503.464356	497412.019106	50.000218
3503.174846	497416.115052	50.005223
3503.727808	497416.837705	50.010228
3503.383743	497419.119694	50.015233
3503.414271	497406.863111	50.020237
3503.476157	497393.285256	50.025242
3503.596825	497378.280537	50.030247
3503.421278	497376.435089	50.035252
3503.080146	497377.754703	50.040257
3503.430135	497356.030921	50.045261
3503.553866	497366.440606	50.050266
3503.553503	497366.187542	50.055271
3503.556573	497365.478290	50.060276
3503.664159	497354.475174	50.065281
3503.719097	497331.177922	50.070285
3503.552814	497324.470774	50.075290
3503.558265	497316.673305	50.080295
3503.685732	497313.514273	50.085300
3503.479051	497321.191696	50.090305
3503.520498	497299.668495	50.095309
3503.369795	497281.061407	50.100314
3503.070161	497285.310865	50.105319
3503.353223	497275.140635	50.110324
3502.913748	497280.880394	50.115329
3503.112684	497282.064028	50.120333
3503.251386	497272.321633	50.125338
3503.241274	497279.562986	50.130343
3503.750249	497271.635287	50.135348
3503.096704	497284.395481	50.140353
3503.715014	497279.437528	50.145357
3503.776349	497269.859243	50.150362
3503.410617	497252.450545	50.155367
3503.225716	497243.265557	50.160372
3503.395233	497226.379769	50.165377
3503.463926	497224.951352	50.170381
3503.394916	497230.632575	50.175386
3503.380804	497224.002594	50.180391
3503.586297	497220.628703	50.185396
3503.708049	497227.393586	50.190401
3503.579048	497215.769619	50.195405
3503.531072	497200.335758	50.200410
3503.481460	497189.914294	50.205415
3503.726289	497182.939606	50.210420
3503.625212	497178.044699	50.215425
3503.960357	497164.575367	50.220429
3503.863274	497142.871364	50.225434
3503.658333	497128.930460	50.230439
3503.923661	497125.698978	50.235444
3503.686892	497136.570796	50.240449
3503.888529	497113.098194	50.245453
3503.629001	497091.065407	50.250458
3503.663771	497097.692201	50.255463
3503.585982	497091.679773	50.260468
3503.272047	497094.817718	50.265473
3503.418144	497059.000575	50.270477
3503.504530	497055.442966	50.275482
3503.226615	497047.032001	50.280487
3503.414667	497043.508950	50.285492
3503.100240	497046.444467	50.290497
3503.554525	497045.765144	50.295501
3503.569690	497046.977839	50.300506
3503.620040	497039.173154	50.305511
3503.607999	497036.998060	50.310516
3503.713147	497025.893874	50.315521
3503.773639	497005.886162	50.320525
3503.696083	497008.379222	50.325530
3503.735006	496998.905592	50.330535
3504.026472	496993.087912	50.335540
3503.694680	496975.825469	50.340545
3503.877530	496953.925110	50.345549
3503.704697	496959.673455	50.350554
3503.457390	496937.790435	50.355559
3503.600394	496927.540891	50.360564
3503.338843	496921.861221	50.365569
3503.522502	496916.769355	50.370573
3503.482418	496923.863701	50.375578
3503.419999	496921.139641	50.380583
3503.621742	496921.867198	50.385588
3503.410209	496922.660074	50.390593
3503.315500	496891.032200	50.395597
3503.578991	496874.131232	50.400602
3503.406912	496870.513180	50.405607
3503.322657	496872.399773	50.410612
3503.107440	496882.255763	50.415617
3503.480091	496865.742564	50.420621
3503.338616	496872.701068	50.425626
3503.176727	496872.625413	50.430631
3503.271891	496876.964452	50.435636
3503.307238	496872.908588	50.440641
3503.402937	496870.108901	50.445645
3503.475613	496875.615954	50.450650
3503.122230	496850.256217	50.455655
3503.644411	496835.288847	50.460660
3503.517298	496823.968104	50.465665
3503.587770	496821.425540	50.470669
3503.660572	496823.894861	50.475674
3503.074900	496830.316042	50.480679
3503.820988	496821.895014	50.485684
3503.339221	496816.098230	50.490689
3503.338962	496786.581656	50.495693
3503.309004	496782.131061	50.500698
3503.168548	496788.178117	50.505703
3503.382538	496772.246827	50.510708
3503.482613	496778.002725	50.515713
3503.800256	496781.243416	50.520717
3503.745130	496777.910635	50.525722
3503.236434	496766.093247	50.530727
3503.534617	496738.706472	50.535732
3503.539393	496721.491850	50.540737
3503.793115	496669.404984	50.545741
3503.719976	496624.710890	50.550746
3503.145429	496569.666256	50.555751
3503.243610	496483.377859	50.560756
3502.728509	496416.729150	50.565761
3502.984389	496337.958998	50.570765
3502.672066	496235.836432	50.575770
3502.246017	496135.503343	50.580775
3502.474762	496024.129911	50.585780
3502.317737	495909.120683	50.590785
3502.055783	495777.823910	50.595789
3501.573552	495649.041979	50.600794
3501.588008	495496.940339	50.605799
3501.315922	495344.933355	50.610804
3500.734083	495193.075332	50.615809
3500.652779	495017.440325	50.620813
3500.588433	494844.585842	50.625818
3500.377108	494676.765802	50.630823
3500.036979	494483.596322	50.635828
3499.689914	494282.273537	50.640833
3499.020138	494081.759098	50.645837
3498.952992	493879.931939	50.650842
3498.357117	493666.792694	50.655847
3498.321903	493452.650883	50.660852
3497.184986	493234.528341	50.665857
3497.256830	493007.502207	50.670861
3497.390235	492777.678358	50.675866
3496.737654	492544.177842	50.680871
3496.571082	492297.177630	50.685876
3496.081969	492045.363481	50.690881
3495.546948	491789.400477	50.695885
3495.302777	491532.172538	50.700890
3494.573990	491267.370387	50.705895
3494.475094	490992.184017	50.710900
3493.801179	490723.972275	50.715905
3493.093548	490444.214656	50.720909
3492.709431	490162.730368	50.725914
3492.088337	489883.153278	50.730919
3491.884343	489594.490647	50.735924
3491.149734	489300.589263	50.740929
3490.711827	489012.359865	50.745933
3490.551391	488716.231303	50.750938
3489.998282	488415.601501	50.755943
3489.420378	488106.359895	50.760948
3488.697068	487804.227699	50.765953
3488.266287	487488.773038	50.770957
3488.042525	487175.357275	50.775962
3487.378119	486856.433841	50.780967
3486.664920	486522.872960	50.785972
3486.162325	486203.001193	50.790977
3485.830905	485873.674526	50.795981
3485.176156	485547.736819	50.800986
3484.447724	485226.212658	50.805991
3483.973556	484875.310116	50.810996
3483.118157	484549.741806	50.816001
3482.805725	484213.493619	50.821005
3482.175901	483869.436848	50.826010
3481.424879	483525.241113	50.831015
3480.913736	483186.422562	50.836020
3480.127961	482836.697532	50.841025
3480.086406	482493.029997	50.846029
3479.197363	482136.569924	50.851034
3478.606062	481795.865077	50.856039
3478.125838	481439.327641	50.861044
3477.414240	481083.529673	50.866049
3476.891760	480724.604357	50.871053
3476.597764	480360.467722	50.876058
3475.591478	480007.737206	50.881063
3475.034737	479644.439634	50.886068
3474.525788	479282.749442	50.891073
3473.676916	478915.481255	50.896077
3473.089918	478555.665145	50.901082
3472.324011	478186.697978	50.906087
3471.812666	477817.278289	50.911092
3470.640301	477460.068844	50.916097
3470.136519	477095.651939	50.921101
3469.865842	476736.715905	50.926106
3468.974384	476374.577161	50.931111
3468.336765	475995.361912	50.936116
3467.523457	475635.022101	50.941121
3466.940709	475266.935139	50.946125
3466.364125	474905.328400	50.951130
3465.568954	474542.837365	50.956135
3465.324807	474160.180031	50.961140
3464.575842	473803.599044	50.966145
3463.854975	473419.634493	50.971149
3463.273015	473051.659247	50.976154
3462.781399	472681.534005	50.981159
3461.934237	472300.457820	50.986164
3460.841128	471933.405029	50.991169
3460.496652	471549.092375	50.996173
3459.720744	471186.589356	51.001178
3458.972452	470824.633259	51.006183
3458.235476	470449.335491	51.011188
3457.599816	470083.089977	51.016193
3456.744452	469713.881438	51.021197
3456.293231	469342.067420	51.026202
3455.651853	468976.918708	51.031207
3455.481300	468602.359939	51.036212
3454.210796	468236.030148	51.041217
3453.548123	467857.631676	51.046221
3453.057917	467486.095002	51.051226
3452.192871	467120.239372	51.056231
3451.472861	466745.886411	51.061236
3450.748785	466372.643018	51.066241
3449.889558	466001.797702	51.071245
3449.492068	465634.016890	51.076250
3448.207922	465273.925712	51.081255
3447.993150	464903.162157	51.086260
3447.135905	464541.368333	51.091265
3446.310541	464174.289184	51.096269
3445.846435	463815.767980	51.101274
3445.205835	463449.560043	51.106279
3444.837503	463071.790379	51.111284
3443.959569	462711.033941	51.116289
3443.306355	462345.620664	51.121293
3442.499377	461972.871375	51.126298
3441.612908	461614.329562	51.131303
3440.793015	461240.301730	51.136308
3440.228263	460888.239928	51.141313
3439.652134	460534.449697	51.146317
3438.880627	460169.982193	51.151322
3437.961767	459813.140386	51.156327
3437.431333	459448.318407	51.161332
3436.779894	459090.408077	51.166337
3435.831186	458738.981077	51.171341
3435.485703	458377.257079	51.176346
3434.506951	458022.678365	51.181351
3433.764120	457665.418804	51.186356
3433.375368	457311.090518	51.191361
3432.672300	456957.465753	51.196365
3432.013157	456592.312578	51.201370
3431.021147	456250.288835	51.206375
3430.366312	455895.066917	51.211380
3429.770487	455532.017148	51.216385
3429.108814	455182.111971	51.221389
3428.323908	454834.605352	51.226394
3427.726592	454487.114448	51.231399
3427.327710	454121.626216	51.236404
3426.387382	453777.882365	51.241409
3425.593988	453423.353666	51.246413
3425.037962	453066.447929	51.251418
3423.998572	452728.031381	51.256423
3423.539390	452364.148037	51.261428
3422.848836	452020.135164	51.266433
3421.881442	451669.412243	51.271437
3421.119211	451330.322278	51.276442
3420.129272	450986.594934	51.281447
3419.904839	450636.956627	51.286452
3418.837345	450299.472792	51.291457
3418.287181	449953.985955	51.296461
3417.956208	449619.724962	51.301466
3416.912787	449281.207552	51.306471
3416.288021	448937.493511	51.311476
3415.651856	448603.469143	51.316481
3415.063151	448257.607945	51.321485
3414.212522	447916.604278	51.326490
3413.126731	447589.233985	51.331495
3412.633912	447247.961024	51.336500
3412.167579	446919.671448	51.341505
3411.144302	446584.867493	51.346509
3410.732898	446244.176159	51.351514
3409.768409	445913.261413	51.356519
3409.320723	445589.619800	51.361524
3408.607747	445258.250117	51.366529
3407.692448	444926.806294	51.371533
3406.929361	444596.145911	51.376538
3406.056007	444268.188542	51.381543
3406.023108	443931.261845	51.386548
3405.144460	443603.753047	51.391553
3404.491441	443287.168225	51.396557
3403.731197	442943.388588	51.401562
3403.083052	442626.388234	51.406567
3402.340606	442288.535517	51.411572
3401.545026	441969.874733	51.416577
3400.831534	441634.952559	51.421581
3400.237540	441315.591402	51.426586
3399.841339	440993.047386	51.431591
3399.016046	440668.231750	51.436596
3398.085720	440345.154449	51.441601
3397.157167	440011.817758	51.446605
3396.941813	439686.486551	51.451610
3395.962379	439369.572404	51.456615
3395.319160	439052.778718	51.461620
3394.883604	438733.638140	51.466625
3394.092646	438412.493459	51.471629
3393.339583	438085.779255	51.476634
3392.401914	437772.645857	51.481639
3391.854790	437454.420362	51.486644
3391.092218	437129.497519	51.491649
3390.101917	436817.756705	51.496653
3389.717024	436506.601738	51.501658
3388.815805	436198.977209	51.506663
3388.368619	435875.384552	51.511668
3387.317795	435567.522087	51.516673
3386.677312	435254.259481	51.521677
3385.975334	434947.578329	51.526682
3385.411155	434633.762829	51.531687
3384.925910	434318.559963	51.536692
3384.299239	434017.898283	51.541697
3383.549420	433712.936284	51.546701
3382.894451	433390.690456	51.551706
3381.862772	433091.199069	51.556711
3381.757861	432772.438532	51.561716
3380.781869	432468.233813	51.566721
3380.025342	432153.250316	51.571725
3379.404149	431839.282631	51.576730
3378.467635	431542.297340	51.581735
3377.828102	431233.378179	51.586740
3377.087853	430933.587145	51.591745
3376.215635	430635.921118	51.596749
3375.785956	430328.887883	51.601754
3375.065317	430019.002207	51.606759
3374.672238	429708.984890	51.611764
3374.039683	429419.240708	51.616769
3373.297855	429109.246057	51.621773
3372.652712	428803.194008	51.626778
3371.761542	428505.862321	51.631783
3371.364300	428196.488120	51.636788
3370.585894	427902.128436	51.641793
3369.522596	427595.747607	51.646797
3369.193960	427291.151782	51.651802
3368.262144	426989.720790	51.656807
3367.458232	426692.329610	51.661812
3366.768838	426388.288458	51.666817
3366.237364	426099.050774	51.671821
3365.598705	425797.153652	51.676826
3364.572425	425504.914735	51.681831
3364.023375	425212.622590	51.686836
3363.159248	424918.040471	51.691841
3362.526496	424619.862779	51.696845
3362.247035	424326.756492	51.701850
3361.315882	424038.321908	51.706855
3360.454504	423738.976951	51.711860
3359.736609	423447.860876	51.716865
3358.999879	423158.116269	51.721869
3358.793941	422865.490662	51.726874
3357.676380	422594.113766	51.731879
3357.035419	422292.000311	51.736884
3356.542753	421993.975041	51.741889
3355.569324	421725.437100	51.746893
3354.816860	421422.925351	51.751898
3354.168897	421143.458500	51.756903
3353.730315	420865.886275	51.761908
3352.931964	420570.993080	51.766913
3352.218900	420290.969116	51.771917
3351.697213	420002.198959	51.776922
3350.787185	419721.082715	51.781927
3350.227443	419429.950205	51.786932
3349.236703	419161.822170	51.791937
3348.416427	418876.821965	51.796941
3347.939311	418590.062553	51.801946
3347.280445	418317.707767	51.806951
3346.629924	418035.873177	51.811956
3346.077844	417759.710881	51.816961
3345.333251	417494.043191	51.821965
3344.804683	417194.905608	51.826970
3343.899599	416931.036418	51.831975
3343.134437	416651.060861	51.836980
3342.854649	416369.303620	51.841985
3342.128580	416092.034866	51.846989
3341.506802	415821.047748	51.851994
3340.752298	415544.540415	51.856999
3340.108924	415255.106142	51.862004
3339.473007	414977.126438	51.867009
3338.738275	414701.014439	51.872013
3338.097753	414417.389660	51.877018
3337.193810	414144.297241	51.882023
3336.488674	413860.016653	51.887028
3335.976794	413581.800758	51.892033
3335.162466	413311.964082	51.897037
3334.343672	413038.161849	51.902042
3333.756543	412767.826892	51.907047
3333.371762	412496.720589	51.912052
3332.622988	412217.944848	51.917057
3331.689339	411941.914566	51.922061
3331.325765	411664.597297	51.927066
3330.089745	411405.075545	51.932071
3329.705553	411125.520409	51.937076
3328.929382	410853.546220	51.942081
3328.060472	410594.467581	51.947085
3327.481442	410318.239135	51.952090
3326.672808	410056.935547	51.957095
3326.179154	409778.986080	51.962100
3325.712380	409519.072231	51.967105
3324.682034	409254.442381	51.972109
3324.491474	408981.647127	51.977114
3323.616867	408719.884984	51.982119
3322.923834	408450.900062	51.987124
3322.423630	408179.747581	51.992129
3321.706309	407914.090865	51.997133
3321.220217	407636.730510	52.002138
3320.191211	407372.033261	52.007143
3319.592795	407096.820533	52.012148
3318.636413	406842.145718	52.017153
3317.774482	406578.940069	52.022157
3317.373210	406304.502350	52.027162
3316.479740	406048.667389	52.032167
3315.899705	405786.071202	52.037172
3315.277360	405531.993571	52.042177
3314.534134	405262.073783	52.047181
3313.738870	404997.725908	52.052186
3313.008949	404746.200450	52.057191
3312.634015	404488.745736	52.062196
3312.105779	404223.510372	52.067201
3311.070222	403968.239996	52.072205
3310.690608	403712.202987	52.077210
3309.898050	403452.645431	52.082215
3309.343441	403189.489728	52.087220
3308.536811	402940.529115	52.092225
3307.670448	402669.005283	52.097229
3307.210416	402404.074314	52.102234
3306.226358	402168.759603	52.107239
3305.985096	401894.537703	52.112244
3305.334435	401643.661365	52.117249
3304.289841	401390.811886	52.122253
3304.026324	401125.051291	52.127258
3303.125365	400863.049636	52.132263
3302.236172	400609.762750	52.137268
3301.669821	400357.515857	52.142273
3300.971985	400105.516572	52.147277
3300.454453	399842.480087	52.152282
3299.601516	399592.407833	52.157287
3299.037152	399336.543085	52.162292
3298.538830	399094.952097	52.167297
3297.791492	398842.188276	52.172301
3297.222280	398572.209954	52.177306
3296.065092	398331.531008	52.182311
3295.899865	398070.381992	52.187316
3295.078059	397812.359881	52.192321
3294.820012	397555.415990	52.197325
3294.019364	397297.564476	52.202330
3292.976216	397041.427157	52.207335
3292.536834	396788.904005	52.212340
3291.941159	396532.539479	52.217345
3291.065455	396288.013291	52.222349
3290.579398	396021.585652	52.227354
3289.562344	395760.070219	52.232359
3288.483740	395512.875657	52.237364
3288.145259	395260.986054	52.242369
3287.215622	395021.798074	52.247373
3286.795413	394759.214412	52.252378
3285.548150	394523.174828	52.257383
3285.238683	394279.764890	52.262388
3284.833911	394033.597058	52.267393
3283.932027	393789.667138	52.272397
3283.609438	393540.253870	52.277402
3282.833916	393296.885223	52.282407
3282.122871	393044.885627	52.287412
3281.593948	392796.109791	52.292417
3280.781565	392551.139929	52.297421
3280.322098	392303.875080	52.302426
3279.551993	392052.335247	52.307431
3279.082672	391802.958066	52.312436
3278.364803	391548.075548	52.317441
3277.267376	391311.252907	52.322445
3276.735745	391056.515333	52.327450
3275.851754	390808.315393	52.332455
3275.268749	390567.643247	52.337460
3274.688351	390334.393682	52.342465
3274.159607	390083.513482	52.347469
3273.715154	389833.126716	52.352474
3272.884602	389600.623835	52.357479
3272.374485	389352.481670	52.362484
3271.367963	389089.795338	52.367489
3270.418428	388857.611553	52.372493
3269.931550	388606.485456	52.377498
3269.143756	388368.602454	52.382503
3268.364033	388136.183708	52.387508
3267.949887	387884.125631	52.392513
3267.178740	387645.040067	52.397517
3266.651964	387395.030688	52.402522
3265.552814	387163.520781	52.407527
3264.953134	386929.260327	52.412532
3264.400624	386684.157966	52.417537
3263.423165	386459.642851	52.422541
3262.915770	386221.345375	52.427546
3262.297960	385989.319569	52.432551
3261.637295	385748.347686	52.437556
3261.149822	385505.770154	52.442561
3260.351171	385286.331053	52.447565
3259.966107	385040.784338	52.452570
3259.163532	384802.676942	52.457575
3258.081714	384565.858295	52.462580
3257.823547	384329.492781	52.467585
3257.033117	384101.424234	52.472589
3256.525915	383855.939868	52.477594
3255.802476	383626.153920	52.482599
3255.126038	383393.358189	52.487604
3254.290998	383151.456065	52.492609
3253.482909	382923.662892	52.497613
3252.789908	382681.887878	52.502618
3252.302111	382457.550873	52.507623
3251.529981	382234.020486	52.512628
3250.722264	381999.380352	52.517633
3250.028028	381766.450252	52.522637
3249.768873	381528.465056	52.527642
3249.036378	381308.051216	52.532647
3248.264122	381074.646010	52.537652
3247.711888	380835.583800	52.542657
3246.842603	380609.032697	52.547661
3246.447402	380366.305738	52.552666
3245.528920	380139.174682	52.557671
3244.996979	379910.429679	52.562676
3244.263147	379677.569492	52.567681
3243.318950	379442.706438	52.572685
3242.756537	379209.638299	52.577690
3241.723255	378988.546649	52.582695
3241.405437	378762.457110	52.587700
3240.773107	378540.002337	52.592705
3239.941903	378315.186867	52.597709
3239.382612	378082.467629	52.602714
3238.627817	377854.279999	52.607719
3237.760295	377625.167771	52.612724
3237.379875	377397.986589	52.617729
3236.606799	377179.209154	52.622733
3236.066234	376946.556598	52.627738
3235.575169	376723.509692	52.632743
3234.786212	376496.616922	52.637748
3234.134912	376266.979404	52.642753
3233.263998	376044.955389	52.647757
3232.755605	375820.405456	52.652762
3232.000284	375602.557768	52.657767
3231.599533	375363.285808	52.662772
3230.594783	375136.368645	52.667777
3229.975117	374917.554650	52.672781
3229.379886	374699.600484	52.677786
3228.854299	374482.193764	52.682791
3227.849445	374244.740540	52.687796
3227.037422	374023.840865	52.692801
3226.289704	373811.578717	52.697805
3225.926039	373582.440188	52.702810
3225.318296	373365.803701	52.707815
3224.142259	373150.400696	52.712820
3223.687922	372933.661370	52.717825
3223.263497	372718.951268	52.722829
3222.432487	372489.626242	52.727834
3221.995513	372269.319296	52.732839
3220.913090	372063.002964	52.737844
3220.490497	371844.904702	52.742849
3219.408712	371623.755115	52.747853
3219.258437	371402.126310	52.752858
3218.308526	371193.291696	52.757863
3217.576763	370973.991302	52.762868
3217.481986	370754.131100	52.767873
3216.609308	370535.613926	52.772877
3215.917559	370316.303811	52.777882
3214.996154	370095.884091	52.782887
3214.675760	369874.477758	52.787892
3214.122955	369649.189224	52.792897
3213.052623	369434.768162	52.797901
3212.456166	369218.820958	52.802906
3211.708528	368993.966870	52.807911
3211.173955	368782.739688	52.812916
3210.648499	368565.276981	52.817921
3209.755087	368356.165214	52.822925
3209.246442	368121.448518	52.827930
3208.310225	367912.824784	52.832935
3207.820798	367699.499019	52.837940
3206.909940	367481.506732	52.842945
3206.120144	367267.564904	52.847949
3205.609699	367053.908594	52.852954
3204.938668	366837.401703	52.857959
3204.052708	366624.642312	52.862964
3203.792954	366414.301631	52.867969
3203.216545	366200.880632	52.872973
3202.570679	365987.927566	52.877978
3201.607403	365774.311302	52.882983
3200.803555	365556.470745	52.887988
3200.646280	365344.251504	52.892993
3199.487422	365138.550456	52.897997
3198.723346	364925.483844	52.903002
3198.160844	364713.758278	52.908007
3197.676786	364504.996190	52.913012
3196.940780	364296.756426	52.918017
3196.232416	364083.880603	52.923021
3195.783343	363866.306572	52.928026
3195.099139	363665.434417	52.933031
3194.119091	363441.352412	52.938036
3193.977960	363227.416016	52.943041
3193.036256	363024.775272	52.948045
3192.277395	362799.459284	52.953050
3191.684930	362589.636983	52.958055
3190.836496	362387.080476	52.963060
3190.377277	362177.973133	52.968065
3189.426693	361968.637247	52.973069
3189.131683	361759.400277	52.978074
3188.369035	361547.437404	52.983079
3187.432570	361340.717319	52.988084
3186.696034	361130.860384	52.993089
3186.085438	360922.051299	52.998093
3185.458206	360711.946209	53.003098
3184.967671	360503.625200	53.008103
3184.021565	360301.456862	53.013108
3183.537864	360090.995534	53.018113
3182.953626	359883.297341	53.023117
3182.492826	359666.545394	53.028122
3181.485459	359477.080821	53.033127
3180.803354	359267.486995	53.038132
3180.462970	359053.206970	53.043137
3179.398105	358854.333913	53.048141
3179.144740	358639.478475	53.053146
3178.457096	358434.513197	53.058151
3177.617704	358222.827675	53.063156
3176.759029	358019.541753	53.068161
3175.846843	357813.413394	53.073165
3175.443516	357608.705047	53.078170
3174.692712	357423.746934	53.083175
3173.959705	357204.889547	53.088180
3173.571129	356991.727815	53.093185
3173.000741	356795.312935	53.098189
3171.999495	356590.389604	53.103194
3171.416571	356387.740442	53.108199
3170.628265	356180.135181	53.113204
3170.236863	355975.061958	53.118209
3169.265559	355777.815835	53.123213
3168.523774	355575.468457	53.128218
3167.895902	355373.433075	53.133223
3167.053670	355179.421569	53.138228
3166.609318	354971.935066	53.143233
3166.080667	354779.857403	53.148237
3165.167598	354575.828092	53.153242
3164.726408	354386.279976	53.158247
3163.758534	354183.275721	53.163252
3163.446361	353979.352566	53.168257
3162.547431	353789.900118	53.173261
3161.885202	353580.661031	53.178266
3161.427655	353384.367809	53.183271
3160.396061	353186.459561	53.188276
3160.052177	352986.431260	53.193281
3159.162192	352790.407811	53.198285
3158.507696	352590.936128	53.203290
3158.149461	352400.044258	53.208295
3157.328826	352201.182724	53.213300
3156.758774	352001.237352	53.218305
3156.106428	351801.685993	53.223309
3155.514297	351604.287613	53.228314
3154.669383	351398.708093	53.233319
3153.886435	351207.141064	53.238324
3153.460940	351003.351534	53.243329
3152.461136	350803.444206	53.248333
3152.395956	350602.650204	53.253338
3151.428239	350407.139269	53.258343
3150.845834	350206.400172	53.263348
3150.149680	349992.520255	53.268353
3149.056948	349806.011068	53.273357
3148.919004	349600.643702	53.278362
3148.112803	349414.087844	53.283367
3147.113578	349208.957075	53.288372
3146.423003	349003.064073	53.293377
3145.707423	348816.135527	53.298381
3145.287632	348621.422310	53.303386
3144.353568	348433.687140	53.308391
3143.780371	348235.459074	53.313396
3143.337984	348032.093808	53.318401
3142.483358	347844.522245	53.323405
3142.055717	347653.522848	53.328410
3141.258055	347465.457416	53.333415
3140.502290	347259.975510	53.338420
3140.241137	347061.515756	53.343425
3139.570948	346876.533357	53.348429
3139.052833	346678.163819	53.353434
3138.485836	346476.263435	53.358439
3137.562789	346274.444121	53.363444
3136.953139	346073.465353	53.368449
3136.016990	345884.576660	53.373453
3135.383452	345676.906225	53.378458
3134.637626	345477.245009	53.383463
3133.693632	345280.083394	53.388468
3133.265139	345094.217058	53.393473
3132.291570	344895.200743	53.398477
3132.090273	344708.915434	53.403482
3131.071716	344506.163290	53.408487
3130.767490	344316.864077	53.413492
3130.248461	344118.053192	53.418497
3129.358614	343936.685078	53.423501
3128.662078	343720.439808	53.428506
3127.995687	343528.548191	53.433511
3126.979067	343346.256541	53.438516
3126.471563	343148.306011	53.443521
3125.824729	342964.020193	53.448525
3125.187850	342769.703342	53.453530
3124.703973	342577.601619	53.458535
3123.731302	342386.798423	53.463540
3123.396014	342190.981101	53.468545
3122.691960	342006.370504	53.473549
3121.913770	341803.520243	53.478554
3121.395072	341613.737331	53.483559
3120.518366	341427.701393	53.488564
3120.098448	341235.865314	53.493569
3119.196332	341042.297643	53.498573
3118.692618	340844.339006	53.503578
3117.954068	340663.471689	53.508583
3117.233423	340474.404504	53.513588
3116.882450	340271.481605	53.518593
3116.207041	340088.948048	53.523597
3115.138890	339877.660780	53.528602
3114.626523	339685.274529	53.533607
3114.061203	339503.740066	53.538612
3113.685030	339315.047624	53.543617
3112.779292	339123.892857	53.548621
3112.524577	338929.681656	53.553626
3111.419002	338734.153516	53.558631
3110.686093	338542.918750	53.563636
3110.158742	338334.162720	53.568641
3109.381270	338147.388602	53.573645
3108.725786	337954.917953	53.578650
3108.041362	337762.782240	53.583655
3106.917626	337567.711644	53.588660
3106.409335	337372.364890	53.593665
3105.619413	337191.877683	53.598669
3105.259528	336994.953485	53.603674
3104.518109	336814.152089	53.608679
3103.584751	336626.481850	53.613684
3103.370930	336438.468118	53.618689
3102.677737	336259.668645	53.623693
3101.542678	336065.435459	53.628698
3101.219090	335877.870276	53.633703
3100.479693	335703.506109	53.638708
3099.771911	335511.520282	53.643713
3099.132495	335326.956540	53.648717
3098.661170	335133.048403	53.653722
3097.860757	334945.836102	53.658727
3097.036909	334768.911713	53.663732
3096.843719	334572.997763	53.668737
3096.126730	334388.061888	53.673741
3095.133664	334200.776199	53.678746
3094.829401	334004.776374	53.683751
3094.109994	333825.414564	53.688756
3093.652819	333636.591469	53.693761
3092.518866	333442.707034	53.698765
3092.115068	333258.787807	53.703770
3091.286641	333075.622649	53.708775
3090.731248	332893.737621	53.713780
3090.120591	332701.626760	53.718785
3089.406738	332515.157935	53.723789
3088.442193	332324.476782	53.728794
3087.965837	332140.158790	53.733799
3087.224142	331945.444425	53.738804
3086.676964	331758.081664	53.743809
3086.008679	331573.232499	53.748813
3085.309027	331386.096563	53.753818
3084.944753	331205.398995	53.758823
3083.751529	331017.576452	53.763828
3083.595029	330812.786668	53.768833
3082.629386	330633.303019	53.773837
3081.838903	330445.720781	53.778842
3081.263058	330262.737610	53.783847
3080.507971	330077.032787	53.788852
3079.878204	329891.893223	53.793857
3078.983691	329711.250421	53.798861
3078.381455	329526.029213	53.803866
3077.799359	329353.177509	53.808871
3077.193050	329165.308301	53.813876
3076.678521	328987.200465	53.818881
3075.870501	328802.290088	53.823885
3075.230055	328617.607337	53.828890
3074.576217	328429.260094	53.833895
3074.037159	328246.087966	53.838900
3073.561388	328057.202438	53.843905
3072.779882	327880.076265	53.848909
3071.978700	327689.891967	53.853914
3071.765700	327503.280335	53.858919
3070.663494	327313.320967	53.863924
3070.201717	327122.801514	53.868929
3069.185737	326939.676304	53.873933
3068.527493	326759.320118	53.878938
3068.047643	326572.239291	53.883943
3067.258044	326399.235569	53.888948
3066.877029	326210.585179	53.893953
3066.126555	326033.169856	53.898957
3065.307724	325848.992515	53.903962
3064.802458	325655.675781	53.908967
3064.108835	325469.695532	53.913972
3063.519164	325280.694067	53.918977
3062.852125	325101.735858	53.923981
3062.046070	324907.064605	53.928986
3061.531306	324731.314983	53.933991
3060.569350	324544.000205	53.938996
3060.150032	324357.312031	53.944001
3059.347894	324178.169499	53.949005
3058.986888	323995.188561	53.954010
3058.013095	323803.774779	53.959015
3057.317128	323624.563332	53.964020
3056.815029	323437.224208	53.969025
3056.110941	323258.980786	53.974029
3055.588450	323072.917135	53.979034
3054.947678	322888.908692	53.984039
3053.857717	322707.746213	53.989044
3053.273267	322515.962363	53.994049
3052.702864	322335.684408	53.999053
3051.946596	322155.842871	54.004058
3051.357264	321961.385109	54.009063
3050.651687	321787.340005	54.014068
3050.043426	321605.182366	54.019073
3049.462246	321421.084977	54.024077
3048.448195	321236.571932	54.029082
3048.138245	321067.707901	54.034087
3047.167992	320886.828225	54.039092
3046.562470	320701.180017	54.044097
3045.635737	320526.250795	54.049101
3045.218169	320347.090356	54.054106
3044.742449	320172.827467	54.059111
3043.828341	320001.485369	54.064116
3043.334080	319814.977476	54.069121
3042.645224	319632.064698	54.074125
3042.083044	319450.761088	54.079130
3041.213921	319273.070411	54.084135
3040.772624	319101.524489	54.089140
3040.178601	318911.745909	54.094145
3039.510491	318728.318806	54.099149
3038.913762	318543.912472	54.104154
3038.378610	318358.248367	54.109159
3037.178878	318189.825369	54.114164
3037.092302	317999.022518	54.119169
3036.072408	317816.591424	54.124173
3035.295552	317631.549786	54.129178
3035.085678	317462.408667	54.134183
3034.242409	317282.189323	54.139188
3033.375918	317090.515037	54.144193
3032.986796	316914.348116	54.149197
3031.877944	316727.447566	54.154202
3031.777842	316542.653222	54.159207
3030.790061	316366.478204	54.164212
3030.280716	316183.377584	54.169217
3029.618217	315999.104098	54.174221
3028.919017	315816.236553	54.179226
3028.154623	315626.885868	54.184231
3027.117859	315463.830562	54.189236
3026.931283	315270.135394	54.194241
3026.301092	315096.193241	54.199245
3025.534234	314912.494472	54.204250
3025.201110	314726.536873	54.209255
3024.274749	314552.564276	54.214260
3023.799276	314363.572929	54.219265
3023.011811	314180.869193	54.224269
3022.236138	313994.802071	54.229274
3021.740307	313815.871085	54.234279
3021.008540	313635.780339	54.239284
3020.137725	313436.944499	54.244289
3019.689351	313268.063260	54.249293
3018.988816	313085.420256	54.254298
3018.264131	312899.037570	54.259303
3017.493050	312731.276041	54.264308
3016.877866	312548.542225	54.269313
3016.213902	312367.241807	54.274317
3015.602744	312175.899889	54.279322
3015.035116	311990.458421	54.284327
3014.224451	311817.787180	54.289332
3013.905091	311635.616163	54.294337
3013.037545	311457.122063	54.299341
3012.030220	311274.244482	54.304346
3011.588151	311085.776851	54.309351
3010.502717	310917.272924	54.314356
3009.831843	310737.677055	54.319361
3008.853590	310566.252704	54.324365
3008.507608	310381.588363	54.329370
3008.173813	310213.753837	54.334375
3007.306160	310050.612643	54.339380
3006.973500	309880.434717	54.344385
3006.056735	309704.746774	54.349389
3005.307077	309521.036218	54.354394
3004.977950	309338.582982	54.359399
3003.869509	309176.038906	54.364404
3003.451526	308999.659820	54.369409
3002.777977	308818.508075	54.374413
3002.037678	308642.077618	54.379418
3001.515732	308461.894472	54.384423
3000.548270	308297.544357	54.389428
2999.996599	308129.639515	54.394433
2999.447028	307959.187612	54.399437
2998.891305	307776.003937	54.404442
2998.437651	307587.532569	54.409447
2997.685503	307410.822107	54.414452
2997.058908	307222.861400	54.419457
2996.228177	307052.427296	54.424461
2995.471049	306873.832449	54.429466
2995.137005	306693.209565	54.434471
2993.981514	306514.499012	54.439476
2993.814644	306335.809994	54.444481
2993.055565	306165.236047	54.449485
2992.218118	305986.117914	54.454490
2991.752128	305808.188550	54.459495
2990.892766	305638.342824	54.464500
2990.479432	305449.327173	54.469505
2989.518531	305275.804561	54.474509
2988.973127	305092.819174	54.479514
2988.221977	304913.431287	54.484519
2987.436386	304735.194567	54.489524
2986.938299	304556.148140	54.494529
2986.517726	304377.496663	54.499533
2985.709464	304200.230536	54.504538
2985.283725	304018.701790	54.509543
2984.493297	303845.303185	54.514548
2983.813904	303663.101087	54.519553
2983.079279	303490.864643	54.524557
2982.240219	303305.478663	54.529562
2982.116090	303128.230240	54.534567
2981.018768	302957.985975	54.539572
2980.625622	302769.320021	54.544577
2980.129369	302587.545965	54.549581
2979.320913	302413.791970	54.554586
2978.539038	302229.388750	54.559591
2978.043214	302049.498457	54.564596
2977.583927	301864.661738	54.569601
2976.817062	301678.956696	54.574605
2976.167926	301504.539781	54.579610
2975.662396	301310.389085	54.584615
2974.820785	301122.021248	54.589620
2974.050336	300935.475493	54.594625
2973.603484	300754.506349	54.599629
2972.826736	300575.626523	54.604634
2972.169040	300389.011343	54.609639
2971.533344	300201.832203	54.614644
2970.968444	300015.762163	54.619649
2969.929094	299829.665142	54.624653
2969.091990	299650.284517	54.629658
2968.653132	299461.647249	54.634663
2967.975921	299283.845308	54.639668
2967.442365	299100.086731	54.644673
2966.779347	298913.394320	54.649677
2966.144709	298741.671586	54.654682
2965.578992	298550.583119	54.659687
2964.861893	298365.834139	54.664692
2964.334752	298178.049823	54.669697
2963.856630	297993.491823	54.674701
2962.911729	297792.912525	54.679706
2962.247117	297609.937118	54.684711
2961.324188	297440.347021	54.689716
2960.653460	297245.861216	54.694721
2960.077433	297063.507907	54.699725
2959.234579	296879.719574	54.704730
2958.735648	296705.936050	54.709735
2958.055615	296529.354203	54.714740
2957.443720	296340.257127	54.719745
2956.828123	296155.515305	54.724749
2956.081177	295980.165956	54.729754
2955.638474	295795.549224	54.734759
2954.723384	295611.643769	54.739764
2954.136689	295422.821949	54.744769
2953.823620	295240.247011	54.749773
2952.952254	295063.821457	54.754778
2952.459701	294876.639585	54.759783
2951.497959	294693.530157	54.764788
2951.100421	294508.548553	54.769793
2950.332461	294315.959789	54.774797
2949.437324	294139.053332	54.779802
2948.738528	293951.928744	54.784807
2948.198530	293764.218576	54.789812
2947.625735	293581.479561	54.794817
2946.903046	293402.227678	54.799821
2946.118342	293215.523534	54.804826
2945.589307	293029.491848	54.809831
2944.940375	292860.083726	54.814836
2944.476108	292669.788439	54.819841
2943.598385	292482.945612	54.824845
2942.863470	292295.799887	54.829850
2942.565523	292111.157056	54.834855
2941.810926	291923.606672	54.839860
2940.824662	291745.031910	54.844865
2940.058012	291563.162408	54.849869
2939.451840	291379.408238	54.854874
2939.108342	291203.329023	54.859879
2938.063004	291018.549001	54.864884
2937.383024	290833.889282	54.869889
2936.710715	290647.063468	54.874893
2936.245251	290466.826363	54.879898
2936.055541	290289.550665	54.884903
2934.898913	290098.955513	54.889908
2934.240058	289911.923309	54.894913
2933.626862	289733.822914	54.899917
2933.115210	289549.262996	54.904922
2932.460055	289360.421624	54.909927
2931.767466	289186.102673	54.914932
2931.486163	288988.262691	54.919937
2931.061519	288807.941636	54.924941
2929.957599	288618.814270	54.929946
2929.181813	288418.148853	54.934951
2928.786712	288240.318625	54.939956
2927.956240	288041.902786	54.944961
2927.458788	287861.694565	54.949965
2926.678954	287664.671204	54.954970
2926.242814	287478.493575	54.959975
2925.008977	287292.289310	54.964980
2924.644071	287103.375125	54.969985
2923.953698	286914.435952	54.974989
2922.987768	286732.365709	54.979994
2922.876943	286527.569913	54.984999
2921.978257	286345.030399	54.990004
2921.349709	286156.284772	54.995009
2920.546281	285967.362988	55.000013
2919.864757	285786.469705	55.005018
2919.575273	285594.155528	55.010023
2918.445216	285417.713576	55.015028
2917.790892	285225.227760	55.020033
2917.232242	285029.492260	55.025037
2916.529305	284850.843122	55.030042
2915.935223	284660.308542	55.035047
2915.109460	284495.838956	55.040052
2914.453863	284295.865284	55.045057
2913.945233	284113.797816	55.050061
2913.216004	283924.634117	55.055066
2912.845280	283732.637557	55.060071
2911.926413	283551.195106	55.065076
2910.914241	283371.957619	55.070081
2910.641163	283177.500431	55.075085
2909.789202	282996.734822	55.080090
2909.383592	282809.123946	55.085095
2908.508416	282623.242773	55.090100
2907.893987	282442.821389	55.095105
2907.321033	282250.576125	55.100109
2906.549298	282075.502383	55.105114
2906.112262	281887.666950	55.110119
2905.408886	281706.011468	55.115124
2904.771055	281513.215929	55.120129
2904.253834	281320.936068	55.125133
2903.469393	281135.549419	55.130138
2902.990440	280938.195201	55.135143
2902.496970	280755.283741	55.140148
2901.717353	280557.569520	55.145153
2900.764636	280363.320871	55.150157
2900.079098	280172.951991	55.155162
2899.677942	279984.320825	55.160167
2898.966982	279804.143206	55.165172
2897.948771	279615.966201	55.170177
2897.699671	279415.468064	55.175181
2896.913772	279238.027303	55.180186
2896.066501	279037.088950	55.185191
2895.389327	278839.128891	55.190196
2894.550861	278647.535948	55.195201
2894.175890	278455.156479	55.200205
2893.382310	278262.945125	55.205210
2893.023950	278080.037193	55.210215
2892.222583	277892.080231	55.215220
2891.500666	277702.760841	55.220225
2890.634201	277517.742997	55.225229
2889.892083	277330.082204	55.230234
2889.435479	277138.632335	55.235239
2888.789963	276955.107553	55.240244
2888.276874	276774.949082	55.245249
2887.492182	276575.630437	55.250253
2886.744932	276397.037113	55.255258
2886.130304	276201.995671	55.260263
2885.289863	276021.685228	55.265268
2884.576304	275843.697780	55.270273
2883.892861	275649.049231	55.275277
2883.426739	275473.951459	55.280282
2883.045578	275281.572664	55.285287
2882.243748	275096.315211	55.290292
2881.579708	274910.068142	55.295297
2880.980678	274722.919387	55.300301
2880.317024	274526.026472	55.305306
2880.056996	274335.869718	55.310311
2879.209123	274146.111658	55.315316
2878.429139	273952.981030	55.320321
2878.024086	273761.573838	55.325325
2877.314945	273572.557891	55.330330
2876.668335	273371.281764	55.335335
2875.747658	273179.803434	55.340340
2875.138744	272996.349236	55.345345
2874.256759	272802.929216	55.350349
2873.526177	272605.512177	55.355354
2872.861658	272408.110170	55.360359
2872.023360	272234.777841	55.365364
2871.560650	272048.295326	55.370369
2871.121963	271859.415005	55.375373
2870.047476	271669.998667	55.380378
2869.140288	271480.199313	55.385383
2868.709247	271306.191384	55.390388
2868.184583	271126.722611	55.395393
2867.846151	270932.019781	55.400397
2867.036802	270748.877768	55.405402
2866.264578	270542.859349	55.410407
2865.766360	270364.889157	55.415412
2864.869440	270180.360362	55.420417
2864.620525	269990.431599	55.425421
2863.960933	269810.831631	55.430426
2863.468025	269615.389495	55.435431
2862.492966	269424.633510	55.440436
2861.842434	269221.881563	55.445441
2861.253613	269035.801628	55.450445
2860.276988	268852.482782	55.455450
2859.733495	268658.169520	55.460455
2858.985648	268468.804046	55.465460
2858.124202	268292.929322	55.470465
2857.559502	268095.512463	55.475469
2857.094911	267918.276131	55.480474
2856.530222	267720.222690	55.485479
2855.662546	267533.041285	55.490484
2855.236727	267337.360004	55.495489
2854.894970	267144.619795	55.500493
2854.131938	266949.985309	55.505498
2853.242806	266747.501193	55.510503
2852.781765	266569.322421	55.515508
2851.999548	266386.151870	55.520513
2851.337022	266197.894275	55.525517
2850.507751	266005.460913	55.530522
2850.229602	265798.831025	55.535527
2849.241406	265617.450693	55.540532
2848.736319	265431.129534	55.545537
2848.448466	265227.252006	55.550541
2847.344114	265046.272330	55.555546
2847.032895	264840.666860	55.560551
2846.387289	264640.666478	55.565556
2845.629765	264435.259224	55.570561
2845.071666	264248.717784	55.575565
2844.138102	264057.014941	55.580570
2843.892660	263853.105933	55.585575
2843.387008	263656.980511	55.590580
2842.138080	263461.609584	55.595585
2841.816888	263249.741431	55.600589
2840.580450	263066.313223	55.605594
2840.056822	262862.830849	55.610599
2839.270131	262667.692794	55.615604
2838.391006	262480.439073	55.620609
2837.997354	262290.892882	55.625613
2837.298840	262106.310376	55.630618
2837.230442	261901.050167	55.635623
2836.397023	261706.251173	55.640628
2835.415887	261516.874873	55.645633
2835.051453	261315.176489	55.650637
2834.163478	261118.094407	55.655642
2833.550164	260919.007947	55.660647
2833.084701	260726.265152	55.665652
2832.469774	260539.072654	55.670657
2831.803741	260338.059394	55.675661
2831.179336	260135.027737	55.680666
2830.182327	259938.931507	55.685671
2829.377529	259734.833600	55.690676
2828.886861	259550.729152	55.695681
2828.575359	259346.909977	55.700685
2827.416127	259163.777563	55.705690
2826.902674	258963.861744	55.710695
2825.957524	258774.838159	55.715700
2825.191665	258584.793092	55.720705
2824.609291	258383.589799	55.725709
2823.812895	258191.996347	55.730714
2823.484549	258009.318959	55.735719
2822.899744	257818.736464	55.740724
2822.212491	257634.231599	55.745729
2821.480003	257440.234686	55.750733
2820.766512	257252.703651	55.755738
2820.171093	257054.941644	55.760743
2819.414075	256865.405892	55.765748
2818.618872	256672.692926	55.770753
2818.105212	256490.147946	55.775757
2817.392565	256295.079239	55.780762
2817.082986	256094.700619	55.785767
2816.288072	255900.944123	55.790772
2815.621617	255720.232158	55.795777
2815.240928	255513.702266	55.800781
2814.486556	255325.873737	55.805786
2813.737946	255130.582583	55.810791
2813.181394	254935.031997	55.815796
2812.553246	254735.953005	55.820801
2811.943472	254535.470609	55.825805
2811.169901	254340.897245	55.830810
2810.685499	254132.959015	55.835815
2809.900708	253935.892056	55.840820
2809.048374	253751.187486	55.845825
2808.776238	253546.348709	55.850829
2807.699464	253362.545931	55.855834
2806.987736	253151.716057	55.860839
2806.471955	252954.225508	55.865844
2806.081475	252759.440281	55.870849
2804.968834	252572.129534	55.875853
2804.461810	252382.150928	55.880858
2803.827775	252168.788660	55.885863
2803.213035	251976.535529	55.890868
2802.467482	251782.393315	55.895873
2802.051290	251582.545552	55.900877
2801.090746	251386.960752	55.905882
2800.573156	251192.884959	55.910887
2799.743483	250993.459885	55.915892
2798.944838	250801.771970	55.920897
2798.683601	250598.717487	55.925901
2797.847181	250412.052908	55.930906
2797.213080	250205.772767	55.935911
2796.428475	250016.120848	55.940916
2795.813141	249822.316782	55.945921
2795.200236	249624.208740	55.950925
2794.666538	249433.193514	55.955930
2794.008566	249229.133965	55.960935
2793.315575	249027.805118	55.965940
2792.660648	248834.874370	55.970945
2792.357481	248640.640308	55.975949
2791.364899	248444.019977	55.980954
2791.060385	248235.474628	55.985959
2790.104421	248033.093668	55.990964
2789.267455	247843.579985	55.995969
2788.799395	247645.018594	56.000973
2788.042772	247442.632326	56.005978
2787.373910	247240.665356	56.010983
2786.810724	247042.170767	56.015988
2785.525267	246845.191454	56.020993
2785.387988	246655.084634	56.025997
2784.389283	246460.912614	56.031002
2784.165690	246260.659101	56.036007
2783.527816	246062.737933	56.041012
2782.382156	245870.423528	56.046017
2782.005376	245668.870891	56.051021
2781.218077	245474.030103	56.056026
2780.724227	245274.966748	56.061031
2780.228846	245080.742391	56.066036
2779.090917	244887.460432	56.071041
2778.619352	244686.102502	56.076045
2778.175394	244485.071551	56.081050
2777.498580	244290.214957	56.086055
2776.864744	244096.930697	56.091060
2775.864517	243900.776224	56.096065
2775.431480	243700.203107	56.101069
2774.720755	243500.132650	56.106074
2774.199289	243302.069751	56.111079
2773.480518	243099.734777	56.116084
2772.704230	242908.435663	56.121089
2772.550704	242710.901104	56.126093
2771.547383	242520.122367	56.131098
2770.950748	242312.676277	56.136103
2770.433386	242104.021119	56.141108
2769.711742	241911.110568	56.146113
2769.253063	241709.169540	56.151117
2768.469617	241502.340084	56.156122
2767.414883	241293.898725	56.161127
2766.932424	241099.067171	56.166132
2766.139337	240903.724900	56.171137
2765.833066	240692.313988	56.176141
2764.639173	240511.703528	56.181146
2764.246022	240301.096475	56.186151
2763.793730	240105.243179	56.191156
2762.705263	239906.460677	56.196161
2762.408397	239702.205594	56.201165
2761.633090	239507.652220	56.206170
2760.833003	239292.782472	56.211175
2760.065936	239097.082588	56.216180
2759.431051	238904.290506	56.221185
2758.875845	238703.999625	56.226189
2758.354819	238516.715926	56.231194
2757.773875	238308.255797	56.236199
2757.316966	238101.202406	56.241204
2756.354764	237906.197568	56.246209
2755.793167	237705.552994	56.251213
2755.319413	237500.133099	56.256218
2754.451572	237296.787661	56.261223
2753.715549	237097.521421	56.266228
2752.981518	236905.308731	56.271233
2752.590497	236699.724468	56.276237
2751.598699	236503.708284	56.281242
2750.846621	236304.267815	56.286247
2750.120761	236095.300146	56.291252
2749.529940	235908.795910	56.296257
2749.268707	235718.547582	56.301261
2748.519379	235515.594198	56.306266
2747.859950	235307.890762	56.311271
2747.036922	235108.438351	56.316276
2746.210611	234908.935921	56.321281
2745.956074	234692.206485	56.326285
2744.839710	234497.588838	56.331290
2744.376560	234301.340314	56.336295
2743.585741	234095.264346	56.341300
2742.793589	233905.052558	56.346305
2742.343927	233707.249810	56.351309
2741.339852	233512.361665	56.356314
2740.991055	233317.090028	56.361319
2740.270175	233122.692525	56.366324
2739.358165	232922.927545	56.371329
2738.820983	232720.022605	56.376333
2738.311577	232536.669118	56.381338
2737.362279	232344.371840	56.386343
2736.965946	232141.904138	56.391348
2736.621985	231950.021029	56.396353
2735.923277	231745.972451	56.401357
2734.875898	231562.069479	56.406362
2734.285944	231358.029977	56.411367
2733.906496	231148.865092	56.416372
2733.163557	230959.033264	56.421377
2732.386637	230752.147451	56.426381
2731.638656	230564.939847	56.431386
2731.011598	230364.320348	56.436391
2730.412453	230166.064847	56.441396
2729.603485	229976.321890	56.446401
2728.946866	229769.572014	56.451405
2728.522719	229579.743474	56.456410
2727.859648	229377.120361	56.461415
2727.010631	229187.716411	56.466420
2726.263008	228984.929346	56.471425
2726.177002	228790.898644	56.476429
2725.717981	228586.640918	56.481434
2724.735396	228383.943367	56.486439
2724.419412	228182.439244	56.491444
2723.540388	227963.710925	56.496449
2722.678022	227763.771079	56.501453
2721.906854	227577.209953	56.506458
2721.171639	227367.626471	56.511463
2720.714694	227165.917886	56.516468
2719.725844	226967.120223	56.521473
2719.549365	226764.298792	56.526477
2718.572334	226575.277265	56.531482
2717.973369	226364.910836	56.536487
2717.477913	226163.096161	56.541492
2716.554746	225962.915565	56.546497
2715.963016	225755.439337	56.551501
2715.157879	225551.880201	56.556506
2714.520465	225342.579064	56.561511
2714.334180	225138.286407	56.566516
2713.037327	224945.971161	56.571521
2712.770115	224742.316095	56.576525
2711.949006	224536.585132	56.581530
2711.418215	224339.936268	56.586535
2710.918275	224139.934959	56.591540
2710.064252	223946.368037	56.596545
2709.636316	223734.109930	56.601549
2708.633085	223537.130502	56.606554
2708.068158	223319.293962	56.611559
2707.573214	223118.034147	56.616564
2706.390368	222926.634979	56.621569
2706.295908	222721.570127	56.626573
2705.713697	222526.168701	56.631578
2704.701552	222318.857041	56.636583
2704.145187	222113.230460	56.641588
2703.334609	221914.276929	56.646593
2702.829984	221715.148151	56.651597
2702.217422	221509.175650	56.656602
2701.364754	221306.742409	56.661607
2701.241588	221103.061211	56.666612
2700.190380	220904.072047	56.671617
2699.313997	220692.326097	56.676621
2698.931253	220495.918075	56.681626
2698.273098	220291.789166	56.686631
2697.448325	220089.889414	56.691636
2696.567439	219890.659559	56.696641
2696.323589	219687.523227	56.701645
2695.706583	219483.313644	56.706650
2695.134231	219276.207985	56.711655
2694.706427	219074.540901	56.716660
2693.533358	218877.333118	56.721665
2693.270092	218673.451638	56.726669
2692.297016	218465.584354	56.731674
2691.869781	218260.558919	56.736679
2690.938990	218055.282874	56.741684
2690.396475	217843.874120	56.746689
2690.006786	217639.811923	56.751693
2689.071671	217432.310762	56.756698
2687.929359	217221.278905	56.761703
2687.705030	217025.695259	56.766708
2686.815947	216835.232660	56.771713
2686.250889	216626.580557	56.776717
2685.644907	216422.734342	56.781722
2684.654899	216216.734738	56.786727
2684.137989	216020.016466	56.791732
2683.381235	215817.061467	56.796737
2682.914690	215606.907553	56.801741
2682.134231	215416.622565	56.806746
2681.547759	215210.282009	56.811751
2681.059952	215013.498359	56.816756
2679.962904	214823.901601	56.821761
2679.257717	214615.150496	56.826765
2678.487112	214413.118314	56.831770
2678.011715	214219.555312	56.836775
2677.629460	214023.165131	56.841780
2676.825432	213830.304459	56.846785
2676.207779	213624.737386	56.851789
2675.489362	213435.440959	56.856794
2674.934950	213230.870622	56.861799
2674.586132	213022.182587	56.866804
2673.736613	212829.764788	56.871809
2673.339143	212619.367430	56.876813
2672.415762	212421.960364	56.881818
2671.860022	212209.998380	56.886823
2671.346978	211996.210214	56.891828
2670.815552	211797.075581	56.896833
2670.139020	211590.887807	56.901837
2669.434086	211388.141728	56.906842
2668.580466	211174.970261	56.911847
2668.048510	210964.090468	56.916852
2667.229409	210763.375450	56.921857
2666.573891	210556.182183	56.926861
2665.856359	210351.188583	56.931866
2665.145548	210146.703689	56.936871
2664.218701	209946.479253	56.941876
2663.759585	209750.979658	56.946881
2663.054745	209536.211920	56.951885
2662.204692	209335.939089	56.956890
2661.580093	209144.171312	56.961895
2661.084491	208932.948924	56.966900
2660.082398	208742.451297	56.971905
2659.358601	208538.215558	56.976909
2658.934098	208342.473097	56.981914
2658.710180	208136.963136	56.986919
2658.106837	207945.704814	56.991924
2657.388442	207743.990856	56.996929
2656.592578	207536.473545	57.001933
2655.819905	207318.338886	57.006938
2655.083448	207126.416972	57.011943
2654.683699	206915.822733	57.016948
2653.870061	206718.925366	57.021953
2653.261247	206507.716607	57.026957
2652.576087	206316.030974	57.031962
2651.626493	206113.353694	57.036967
2651.523021	205904.497842	57.041972
2650.637725	205708.111518	57.046977
2650.086246	205492.392027	57.051981
2649.436134	205295.397121	57.056986
2648.603590	205089.497703	57.061991
2648.245895	204866.762910	57.066996
2647.245800	204678.441408	57.072001
2646.760947	204476.179763	57.077005
2646.114700	204266.448531	57.082010
2644.952718	204062.004853	57.087015
2644.705721	203861.985699	57.092020
2643.558753	203662.466155	57.097025
2643.242035	203458.743376	57.102029
2642.695880	203252.614242	57.107034
2641.746579	203057.163334	57.112039
2641.112715	202845.055556	57.117044
2640.494861	202653.944035	57.122049
2639.779961	202455.912856	57.127053
2639.188821	202261.413313	57.132058
2638.709907	202053.356275	57.137063
2638.250618	201846.989444	57.142068
2637.168091	201656.133099	57.147073
2636.485353	201446.481707	57.152077
2636.129826	201241.271453	57.157082
2635.161070	201035.166509	57.162087
2634.586975	200833.733749	57.167092
2633.825733	200644.395247	57.172097
2633.196763	200435.629966	57.177101
2632.743896	200232.767667	57.182106
2631.970157	200042.275205	57.187111
2631.551896	199832.231751	57.192116
2630.669720	199632.621056	57.197121
2629.989636	199426.552792	57.202125
2629.499252	199230.915434	57.207130
2628.486606	199024.163329	57.212135
2628.292255	198824.255772	57.217140
2627.278766	198619.426862	57.222145
2626.486911	198414.970826	57.227149
2626.146076	198219.606140	57.232154
2625.298036	198015.465940	57.237159
2624.756793	197803.299385	57.242164
2624.131001	197612.423084	57.247169
2623.503438	197397.217862	57.252173
2623.035344	197198.644999	57.257178
2622.263415	197000.490043	57.262183
2621.865965	196792.911134	57.267188
2620.911268	196587.686324	57.272193
2620.394179	196381.056908	57.277197
2619.762948	196174.586368	57.282202
2618.950092	195959.938133	57.287207
2618.690175	195755.739015	57.292212
2617.819534	195555.772893	57.297217
2617.113606	195334.328226	57.302221
2616.597352	195118.923944	57.307226
2615.674763	194919.782888	57.312231
2615.283254	194712.669477	57.317236
2614.268473	194503.696144	57.322241
2613.889600	194300.692302	57.327245
2613.212194	194094.504673	57.332250
2612.208691	193879.780874	57.337255
2611.642765	193661.769512	57.342260
2610.826246	193469.730027	57.347265
2610.385286	193259.665753	57.352269
2610.081961	193056.565898	57.357274
2609.048787	192843.492610	57.362279
2608.765639	192645.009941	57.367284
2607.735330	192433.897400	57.372289
2607.281061	192208.838556	57.377293
2606.341809	192017.473031	57.382298
2605.774728	191803.147095	57.387303
2605.221525	191597.955283	57.392308
2604.560933	191398.417781	57.397313
2603.777589	191183.836184	57.402317
2603.025728	190976.846307	57.407322
2602.656200	190763.524213	57.412327
2601.506491	190554.359898	57.417332
2601.021344	190351.630844	57.422337
2600.568133	190141.352841	57.427341
2599.746882	189942.788290	57.432346
2599.028277	189747.020057	57.437351
2598.772180	189527.705701	57.442356
2597.825809	189321.478959	57.447361
2597.145190	189114.663926	57.452365
2596.788913	188900.775487	57.457370
2596.005528	188698.278814	57.462375
2595.164105	188488.871130	57.467380
2594.482042	188288.039540	57.472385
2594.208977	188069.955973	57.477389
2593.411293	187862.770573	57.482394
2592.444670	187652.750333	57.487399
2591.958524	187445.949977	57.492404
2591.310002	187242.700321	57.497409
2590.700271	187024.026145	57.502413
2590.151188	186808.320361	57.507418
2589.268461	186595.607241	57.512423
2588.618666	186390.542272	57.517428
2587.857664	186189.401470	57.522433
2587.193294	185973.768745	57.527437
2586.606493	185770.643008	57.532442
2585.896085	185570.756364	57.537447
2585.589614	185353.708624	57.542452
2584.718457	185141.738277	57.547457
2583.877078	184927.372543	57.552461
2583.508238	184721.290989	57.557466
2582.674191	184517.815658	57.562471
2582.044470	184306.268941	57.567476
2581.231459	184106.112424	57.572481
2580.688938	183892.480258	57.577485
2579.990824	183679.051862	57.582490
2579.093641	183479.572987	57.587495
2578.791622	183265.867544	57.592500
2577.972877	183061.874839	57.597505
2577.088902	182851.202166	57.602509
2576.575087	182641.845703	57.607514
2575.733296	182436.994507	57.612519
2575.451009	182228.582824	57.617524
2574.635824	182033.053646	57.622529
2573.913153	181820.464949	57.627533
2573.528876	181603.918429	57.632538
2572.663271	181398.757838	57.637543
2572.241346	181190.271458	57.642548
2571.333276	180976.609565	57.647553
2570.252639	180767.542687	57.652557
2569.989375	180557.342395	57.657562
2569.093073	180363.563535	57.662567
2568.659755	180151.636768	57.667572
2567.739941	179952.673640	57.672577
2567.170445	179751.760631	57.677581
2566.499369	179542.723844	57.682586
2565.517320	179341.992613	57.687591
2565.606860	179132.989945	57.692596
2564.689777	178932.441147	57.697601
2563.982095	178724.253687	57.702605
2563.383090	178511.559970	57.707610
2562.716575	178317.003527	57.712615
2562.424614	178105.102698	57.717620
2561.689088	177898.933414	57.722625
2560.991685	177673.947012	57.727629
2560.465796	177471.079110	57.732634
2559.452896	177271.329288	57.737639
2558.992801	177057.336267	57.742644
2558.373380	176844.221781	57.747649
2557.123685	176636.524865	57.752653
2556.415329	176426.924379	57.757658
2555.703349	176227.844159	57.762663
2555.543769	176018.247817	57.767668
2554.542485	175824.201220	57.772673
2554.037968	175619.774563	57.777677
2553.584084	175412.110333	57.782682
2552.592130	175214.631074	57.787687
2551.695874	174998.390326	57.792692
2551.198733	174794.742459	57.797697
2550.632153	174591.437297	57.802701
2550.123001	174389.039780	57.807706
2549.406276	174187.795384	57.812711
2548.943857	173976.769457	57.817716
2547.998738	173778.094241	57.822721
2547.235387	173567.766774	57.827725
2546.736355	173371.413896	57.832730
2545.560519	173166.292021	57.837735
2545.261221	172965.598056	57.842740
2544.603717	172763.842684	57.847745
2543.873532	172564.211018	57.852749
2543.508704	172361.088646	57.857754
2542.620018	172156.727684	57.862759
2542.139581	171952.328515	57.867764
2541.617788	171752.197355	57.872769
2540.934731	171543.355811	57.877773
2540.554365	171328.630084	57.882778
2539.588334	171128.470750	57.887783
2538.742234	170907.983837	57.892788
2537.902369	170715.106374	57.897793
2537.671721	170507.762870	57.902797
2536.809045	170313.670153	57.907802
2536.217595	170108.611450	57.912807
2535.895369	169893.731783	57.917812
2534.865900	169696.196839	57.922817
2534.323552	169486.453808	57.927821
2534.019598	169279.688019	57.932826
2532.855558	169075.107035	57.937831
2532.243331	168863.890606	57.942836
2531.521529	168658.593205	57.947841
2531.032485	168447.855492	57.952845
2530.491049	168251.204367	57.957850
2529.458298	168043.022044	57.962855
2529.354863	167828.818642	57.967860
2528.432991	167628.454272	57.972865
2527.668205	167414.866662	57.977869
2527.038718	167199.084359	57.982874
2526.602722	166995.276568	57.987879
2526.065572	166787.772842	57.992884
2525.131543	166580.129702	57.997889
2524.645095	166361.112402	58.002893
2523.863198	166152.773576	58.007898
2522.984100	165943.548501	58.012903
2522.451864	165738.046165	58.017908
2521.746834	165540.087236	58.022913
2520.983309	165320.268004	58.027917
2520.492165	165110.909828	58.032922
2519.580896	164907.150586	58.037927
2519.097984	164699.141257	58.042932
2518.467499	164493.114626	58.047937
2518.132623	164300.011724	58.052941
2517.297882	164007.328553	58.057946
2516.610309	163802.433758	58.062951
2516.155101	163585.118990	58.067956
2515.309591	163379.717566	58.072961
2514.487239	163163.722255	58.077965
2513.928940	162961.367350	58.082970
2512.909564	162748.851400	58.087975
2512.224347	162546.709638	58.092980
2511.561883	162346.510708	58.097985
2511.406707	162132.284821	58.102989
2510.757300	161926.123111	58.107994
2510.125075	161724.066552	58.112999
2509.393319	161508.346474	58.118004
2508.609647	161299.730374	58.123009
2507.775752	161086.864258	58.128013
2507.617602	160874.019452	58.133018
2506.662189	160661.353125	58.138023
2506.078817	160448.718100	58.143028
2505.504598	160247.957491	58.148033
2504.532832	160025.571578	58.153037
2504.099080	159812.242830	58.158042
2503.180015	159614.858698	58.163047
2502.551808	159392.346036	58.168052
2501.902841	159195.646106	58.173057
2501.296897	158986.494186	58.178061
2500.686233	158776.339919	58.183066
2500.166103	158575.275141	58.188071
2499.585539	158363.465878	58.193076
2498.658261	158155.984399	58.198081
2497.984560	157943.442383	58.203085
2497.518774	157726.597215	58.208090
2496.511638	157517.110870	58.213095
2496.315554	157309.683821	58.218100
2495.455271	157101.168303	58.223105
2494.693124	156888.341671	58.228109
2493.999723	156668.653472	58.233114
2493.444132	156470.530359	58.238119
2492.904985	156250.006797	58.243124
2492.080154	156044.937078	58.248129
2491.021114	155827.549555	58.253133
2490.558010	155624.268281	58.258138
2489.588261	155418.487994	58.263143
2489.044722	155219.086313	58.268148
2488.704244	155013.297724	58.273153
2487.756711	154809.030308	58.278157
2487.610812	154593.387277	58.283162
2486.448910	154391.952913	58.288167
2485.808547	154181.742441	58.293172
2485.352408	153983.007896	58.298177
2484.557089	153769.087409	58.303181
2483.948395	153569.909166	58.308186
2482.919062	153368.510766	58.313191
2482.749880	153168.705955	58.318196
2481.946736	152964.159922	58.323201
2481.375860	152756.031980	58.328205
2481.000834	152549.285200	58.333210
2480.069254	152338.522339	58.338215
2479.584513	152130.448213	58.343220
2478.789448	151928.131645	58.348225
2477.941102	151719.316965	58.353229
2477.379923	151505.945879	58.358234
2476.597187	151296.271877	58.363239
2476.272268	151091.458240	58.368244
2475.766511	150884.501096	58.373249
2474.803394	150673.893680	58.378253
2474.225750	150468.552033	58.383258
2473.220165	150253.276758	58.388263
2472.629770	150047.812678	58.393268
2471.882932	149844.675165	58.398273
2471.131159	149637.726784	58.403277
2470.755326	149431.012457	58.408282
2469.908247	149234.808697	58.413287
2469.277344	149026.739326	58.418292
2468.705374	148828.537164	58.423297
2467.840882	148626.735007	58.428301
2467.482016	148410.022279	58.433306
2466.385881	148208.411973	58.438311
2465.913526	147994.223742	58.443316
2465.298549	147794.064866	58.448321
2464.594174	147592.561557	58.453325
2464.171344	147388.066442	58.458330
2463.419181	147188.695633	58.463335
2462.875505	146987.208803	58.468340
2461.945537	146774.867794	58.473345
2461.454620	146574.404616	58.478349
2460.970271	146365.249096	58.483354
2460.147046	146159.376593	58.488359
2459.612612	145947.677396	58.493364
2459.017938	145751.327943	58.498369
2457.893878	145544.465068	58.503373
2457.760325	145337.205101	58.508378
2456.575232	145129.337994	58.513383
2456.523318	144918.865450	58.518388
2455.584508	144715.613126	58.523393
2455.051070	144504.952831	58.528397
2454.645784	144305.316545	58.533402
2453.546607	144084.036267	58.538407
2453.296620	143878.138721	58.543412
2452.504188	143672.760572	58.548417
2451.754397	143464.276456	58.553421
2450.954556	143246.296718	58.558426
2450.296070	143041.295453	58.563431
2449.549301	142834.530565	58.568436
2448.824976	142635.806983	58.573441
2448.814806	142434.887564	58.578445
2447.666441	142216.068182	58.583450
2447.001659	142013.107851	58.588455
2446.617428	141805.466497	58.593460
2446.029769	141586.054481	58.598465
2445.045984	141375.791901	58.603469
2444.578268	141159.756548	58.608474
2443.835782	140952.838519	58.613479
2443.017267	140744.421924	58.618484
2442.451560	140533.819368	58.623489
2442.109826	140328.951277	58.628493
2441.328111	140111.855044	58.633498
2440.472686	139906.690070	58.638503
2440.205509	139686.745478	58.643508
2439.558197	139469.937504	58.648513
2438.563461	139266.946225	58.653517
2437.880828	139049.714901	58.658522
2436.924850	138842.603804	58.663527
2436.495358	138623.925156	58.668532
2435.942079	138417.134333	58.673537
2435.278398	138206.347651	58.678541
2434.683357	138002.615541	58.683546
2433.554377	137791.664165	58.688551
2433.120788	137582.979853	58.693556
2432.589474	137379.953389	58.698561
2431.576497	137175.835848	58.703565
2431.126236	136962.940627	58.708570
2430.445390	136750.604378	58.713575
2429.571840	136538.528886	58.718580
2428.779892	136343.351344	58.723585
2428.151805	136143.321543	58.728589
2427.902185	135936.360209	58.733594
2426.645560	135734.476412	58.738599
2426.047032	135527.319204	58.743604
2425.602528	135327.697817	58.748609
2424.931559	135122.409727	58.753613
2424.280755	134923.586039	58.758618
2423.824609	134720.286615	58.763623
2423.149526	134503.684698	58.768628
2422.656188	134302.795051	58.773633
2422.153050	134100.447477	58.778637
2421.377843	133885.009363	58.783642
2420.464911	133681.903982	58.788647
2419.660714	133473.396729	58.793652
2419.171007	133261.385945	58.798657
2418.275571	133057.520033	58.803661
2418.214232	132847.616582	58.808666
2417.025956	132649.605141	58.813671
2416.590603	132436.181861	58.818676
2416.101524	132225.753767	58.823681
2415.133396	132023.545377	58.828685
2414.622004	131814.317884	58.833690
2413.854528	131614.849687	58.838695
2413.532350	131408.745327	58.843700
2412.722609	131188.645965	58.848705
2411.982925	130977.199893	58.853709
2411.283897	130775.669059	58.858714
2410.708874	130569.420378	58.863719
2410.424787	130348.901292	58.868724
2409.650311	130145.659512	58.873729
2408.817610	129933.423133	58.878733
2408.577576	129721.437343	58.883738
2407.336342	129511.618670	58.888743
2406.651036	129295.616905	58.893748
2406.018582	129082.339153	58.898753
2405.228929	128880.188569	58.903757
2404.642551	128669.243650	58.908762
2404.099286	128465.113797	58.913767
2403.476421	128254.266721	58.918772
2402.735187	128042.131860	58.923777
2401.996171	127823.508345	58.928781
2401.269429	127621.420473	58.933786
2400.750026	127428.204097	58.938791
2400.181454	127211.018948	58.943796
2399.637996	127002.200878	58.948801
2398.857779	126795.860324	58.953805
2398.549283	126579.146940	58.958810
2397.826559	126367.872945	58.963815
2397.005165	126154.952568	58.968820
2396.488852	125942.036284	58.973825
2395.522187	125736.622255	58.978829
2394.972662	125522.609660	58.983834
2394.203126	125317.700919	58.988839
2393.531415	125098.796410	58.993844
2392.966283	124879.597393	58.998849
2391.995065	124677.366877	59.003853
2391.920909	124460.607817	59.008858
2390.712820	124249.770117	59.013863
2390.348610	124035.358938	59.018868
2389.631984	123829.983238	59.023873
2389.058484	123619.735594	59.028877
2388.355498	123396.214916	59.033882
2387.520643	123203.802408	59.038887
2387.162969	122982.643112	59.043892
2386.589985	122760.973763	59.048897
2385.695590	122557.197874	59.053901
2385.173944	122348.691626	59.058906
2384.314764	122134.221775	59.063911
2383.779378	121917.696088	59.068916
2383.232583	121712.817655	59.073921
2382.464037	121503.404869	59.078925
2381.696750	121285.194259	59.083930
2380.738321	121078.163962	59.088935
2380.557624	120861.692260	59.093940
2379.920359	120635.886196	59.098945
2378.835577	120425.922642	59.103949
2378.440541	120215.648263	59.108954
2377.735604	120017.143812	59.113959
2377.308972	119800.821412	59.118964
2376.682510	119582.507382	59.123969
2375.958977	119367.048222	59.128973
2375.521762	119147.958730	59.133978
2374.743816	118937.825164	59.138983
2373.672635	118713.602641	59.143988
2373.257826	118496.952736	59.148993
2372.516924	118289.034000	59.153997
2371.787790	118070.190317	59.159002
2371.082017	117864.243624	59.164007
2370.730927	117647.006723	59.169012
2370.005698	117422.892879	59.174017
2368.923268	117222.057491	59.179021
2368.590683	117005.013499	59.184026
2367.842498	116794.384824	59.189031
2367.011687	116579.784723	59.194036
2366.930984	116362.979168	59.199041
2366.299041	116148.681219	59.204045
2365.590620	115924.857081	59.209050
2364.676647	115717.780001	59.214055
2364.039646	115492.355157	59.219060
2363.498086	115270.306591	59.224065
2362.481304	115059.766547	59.229069
2362.192894	114840.410881	59.234074
2361.337709	114627.697135	59.239079
2360.648784	114423.920783	59.244084
2360.290202	114193.645963	59.249089
2359.469736	113981.021012	59.254093
2358.818583	113760.786540	59.259098
2358.246694	113543.981383	59.264103
2357.730852	113319.381777	59.269108
2356.784921	113093.113384	59.274113
2355.832465	112895.553805	59.279117
2355.766500	112667.734438	59.284122
2355.171591	112455.740341	59.289127
2354.257993	112228.795565	59.294132
2353.797697	112011.605198	59.299137
2352.917132	111793.563141	59.304141
2352.335427	111572.873635	59.309146
2351.648495	111356.765712	59.314151
2351.385333	111129.308992	59.319156
2350.403029	110912.471198	59.324161
2349.356858	110694.611025	59.329165
2348.644196	110468.615093	59.334170
2348.466580	110249.485202	59.339175
2347.780088	110030.869466	59.344180
2346.865877	109808.712732	59.349185
2346.306341	109598.374712	59.354189
2346.047011	109367.646528	59.359194
2345.062195	109160.958675	59.364199
2344.673321	108930.915095	59.369204
2344.001804	108699.681116	59.374209
2342.722397	108489.872883	59.379213
2342.326962	108266.023462	59.384218
2341.891082	108047.036721	59.389223
2340.943424	107826.737131	59.394228
2340.638738	107604.573611	59.399233
2339.598883	107384.184792	59.404237
2338.966176	107157.515189	59.409242
2338.356185	106945.958090	59.414247
2337.497753	106719.651987	59.419252
2337.064679	106503.343677	59.424257
2336.175857	106280.472801	59.429261
2335.751824	106073.043453	59.434266
2335.108142	105842.352639	59.439271
2334.599145	105631.393843	59.444276
2333.649123	105397.849995	59.449281
2333.057812	105191.888694	59.454285
2332.632791	104966.545545	59.459290
2332.159637	104749.567863	59.464295
2331.542159	104509.927322	59.469300
2330.905412	104295.098765	59.474305
2330.016755	104068.924037	59.479309
2329.230427	103834.398886	59.484314
2328.828049	103613.639179	59.489319
2327.865192	103385.205180	59.494324
2327.116329	103171.667072	59.499329
2326.361854	102954.103333	59.504333
2325.981754	102730.950305	59.509338
2325.370050	102508.946299	59.514343
2324.693701	102282.723299	59.519348
2324.239162	102055.154146	59.524353
2323.103179	101846.517071	59.529357
2322.478016	101616.727211	59.534362
2321.936634	101390.377242	59.539367
2321.313922	101168.793671	59.544372
2321.043559	100943.001357	59.549377
2319.996681	100718.501551	59.554381
2319.713655	100487.456973	59.559386
2318.907438	100272.533494	59.564391
2317.984364	100046.637714	59.569396
2317.736779	99822.076924	59.574401
2316.786351	99588.127788	59.579405
2316.275309	99354.092319	59.584410
2315.605391	99132.009217	59.589415
2314.783895	98905.810364	59.594420
2314.450031	98675.356469	59.599425
2313.453158	98457.296009	59.604429
2312.885751	98208.407277	59.609434
2312.150319	98001.009880	59.614439
2311.323553	97765.290075	59.619444
2311.137649	97538.185726	59.624449
2310.150725	97315.751869	59.629453
2309.617906	97090.324320	59.634458
2309.058425	96860.799727	59.639463
2308.291314	96635.635816	59.644468
2307.710703	96404.920484	59.649473
2306.772089	96182.039758	59.654477
2306.729953	95958.359488	59.659482
2305.643367	95719.030016	59.664487
2304.920610	95503.161406	59.669492
2304.599243	95260.728378	59.674497
2303.521129	95033.663736	59.679501
2303.137093	94802.838459	59.684506
2302.330704	94572.704014	59.689511
2301.612163	94350.485056	59.694516
2300.861232	94122.826016	59.699521
2299.995760	93886.353720	59.704525
2299.664172	93654.422180	59.709530
2298.784513	93446.353823	59.714535
2298.213615	93223.570947	59.719540
2297.814711	92985.226931	59.724545
2296.977858	92756.194036	59.729549
2296.164531	92539.778623	59.734554
2295.421467	92315.928784	59.739559
2295.172829	92079.289088	59.744564
2294.537271	91858.001274	59.749569
2293.522344	91634.994050	59.754573
2292.769594	91397.648981	59.759578
2292.007449	91183.946238	59.764583
2291.355505	90960.571236	59.769588
2290.885291	90735.070938	59.774593
2290.231071	90513.901026	59.779597
2289.786747	90295.553277	59.784602
2288.906243	90059.441265	59.789607
2288.546123	89840.101936	59.794612
2287.712450	89606.365020	59.799617
2286.743222	89382.517490	59.804621
2286.317469	89157.990096	59.809626
2285.472815	88937.157980	59.814631
2284.603490	88711.107835	59.819636
2283.948939	88489.876053	59.824641
2283.575933	88269.413385	59.829645
2283.042951	88045.085669	59.834650
2282.512834	87823.314749	59.839655
2281.715666	87602.640845	59.844660
2281.051925	87368.419250	59.849665
2279.879471	87146.807860	59.854669
2279.724905	86917.467959	59.859674
2279.228625	86688.945424	59.864679
2278.313777	86473.677588	59.869684
2277.824841	86240.302703	59.874689
2276.848639	86020.269314	59.879693
2276.259233	85791.263970	59.884698
2275.659161	85572.158110	59.889703
2274.871690	85351.283929	59.894708
2274.535508	85109.548640	59.899713
2273.385696	84904.488892	59.904718
2273.215073	84671.308863	59.909722
2272.352023	84451.571634	59.914727
2271.704335	84228.836011	59.919732
2271.313792	84000.566347	59.924737
2270.432521	83770.240869	59.929742
2269.829820	83550.788619	59.934746
2269.176524	83324.672299	59.939751
2268.385891	83104.905872	59.944756
2267.950368	82865.240203	59.949761
2267.467963	82655.260284	59.954766
2266.662521	82424.119847	59.959770
2265.978736	82189.723894	59.964775
2265.330046	81959.799638	59.969780
2264.520473	81728.052737	59.974785
2263.853869	81515.261360	59.979790
2263.664759	81278.179607	59.984794
2262.632021	81046.272848	59.989799
2262.028884	80832.565727	59.994804
2261.418175	80590.241341	59.999809
2260.806431	80363.275793	60.004814
2260.147572	80127.511114	60.009818
2259.371009	79903.447604	60.014823
2258.167898	79677.901519	60.019828
2258.135843	79444.700538	60.024833
2257.487624	79227.924506	60.029838
2256.883223	78985.484795	60.034842
2256.144409	78751.250374	60.039847
2255.173322	78527.530475	60.044852
2254.914830	78292.870218	60.049857
2253.780075	78070.328230	60.054862
2253.527937	77844.841485	60.059866
2252.675790	77620.111396	60.064871
2252.138200	77382.983801	60.069876
2251.296109	77154.936833	60.074881
2250.171928	76942.113032	60.079886
2249.467861	76706.673511	60.084890
2249.013422	76483.280523	60.089895
2248.528707	76260.661476	60.094900
2247.987507	76039.688564	60.099905
2247.109669	75820.127380	60.104910
2246.079009	75598.470227	60.109914
2245.999983	75373.198776	60.114919
2245.217186	75151.855678	60.119924
2244.825956	74923.553149	60.124929
2243.917547	74705.250732	60.129934
2243.732426	74477.243683	60.134938
2242.305085	74249.068766	60.139943
2241.910906	74023.374508	60.144948
2241.303243	73804.191527	60.149953
2240.443942	73584.189230	60.154958
2239.662181	73357.581931	60.159962
2239.330908	73136.189380	60.164967
2238.405552	72908.558278	60.169972
2238.080485	72688.417735	60.174977
2237.150268	72470.048060	60.179982
2236.735820	72240.024904	60.184986
2236.136986	72027.556091	60.189991
2235.228059	71805.142298	60.194996
2234.733238	71573.517863	60.200001
2234.001811	71342.744500	60.205006
2233.600749	71121.898501	60.210010
2233.213514	70892.006986	60.215015
2232.112227	70664.201426	60.220020
2231.334775	70429.284237	60.225025
2230.725395	70209.672335	60.230030
2230.161774	69972.718671	60.235034
2229.510796	69753.511173	60.240039
2228.548258	69530.365023	60.245044
2227.877915	69307.320746	60.250049
2227.334084	69092.391792	60.255054
2226.636996	68867.918931	60.260058
2225.850084	68632.993026	60.265063
2225.621565	68421.340360	60.270068
2224.748016	68184.919802	60.275073
2224.067600	67966.528668	60.280078
2223.662883	67746.278516	60.285082
2222.837260	67518.060411	60.290087
2221.901546	67289.438105	60.295092
2221.597785	67064.043257	60.300097
2220.767024	66848.019191	60.305102
2220.112966	66622.925691	60.310106
2219.401420	66396.010484	60.315111
2218.771262	66177.305332	60.320116
2218.299503	65948.447924	60.325121
2217.440108	65727.000884	60.330126
2216.866980	65500.188233	60.335130
2216.177718	65274.615728	60.340135
2215.306198	65062.797708	60.345140
2214.985231	64832.824573	60.350145
2214.242656	64608.515863	60.355150
2213.607120	64379.848726	60.360154
2212.720723	64156.787112	60.365159
2211.913444	63938.483784	60.370164
2211.404852	63711.004474	60.375169
2210.518268	63491.385895	60.380174
2210.240954	63267.316719	60.385178
2209.374241	63050.169586	60.390183
2208.519630	62829.100368	60.395188
2207.928580	62616.372153	60.400193
2207.225436	62398.775944	60.405198
2206.610658	62181.307512	60.410202
2206.022542	61959.769251	60.415207
2205.382079	61747.413190	60.420212
2204.741605	61521.931115	60.425217
2203.991966	61299.672753	60.430222
2203.187006	61078.584423	60.435226
2202.743617	60859.464179	60.440231
2201.816037	60652.604554	60.445236
2201.463989	60434.737840	60.450241
2200.786700	60209.343779	60.455246
2200.704894	59994.050873	60.460250
2199.723784	59778.156036	60.465255
2198.600371	59541.821783	60.470260
2198.337310	59316.882374	60.475265
2197.345544	59107.774052	60.480270
2197.031859	58881.901465	60.485274
2196.259413	58662.352633	60.490279
2195.466449	58443.217957	60.495284
2195.043334	58212.847706	60.500289
2194.181445	57994.219855	60.505294
2193.481982	57773.071527	60.510298
2192.925585	57556.815354	60.515303
2192.225981	57335.267135	60.520308
2191.549102	57104.966707	60.525313
2190.875316	56895.032084	60.530318
2189.961628	56674.794885	60.535322
2189.701400	56451.870934	60.540327
2188.605212	56232.674398	60.545332
2188.435195	56015.200798	60.550337
2187.545173	55800.464421	60.555342
2186.895702	55573.764457	60.560346
2186.330851	55350.965446	60.565351
2185.396234	55136.205931	60.570356
2184.732076	54915.500821	60.575361
2183.980078	54703.302916	60.580366
2183.567603	54486.319432	60.585370
2182.800012	54258.315865	60.590375
2181.611316	54046.036639	60.595380
2181.269273	53827.534019	60.600385
2180.784788	53626.391246	60.605390
2179.971989	53411.822541	60.610394
2179.681141	53202.787101	60.615399
2178.662831	52991.588003	60.620404
2178.234465	52763.033566	60.625409
2177.453057	52542.878900	60.630414
2176.746035	52322.718273	60.635418
2176.290757	52104.276489	60.640423
2175.440099	51901.423179	60.645428
2174.873924	51681.985248	60.650433
2174.482526	51471.318271	60.655438
2173.590608	51245.862374	60.660442
2173.066457	51029.127773	60.665447
2172.388566	50819.339661	60.670452
2171.956828	50593.436104	60.675457
2171.110383	50376.115072	60.680462
2170.576634	50148.278045	60.685466
2169.947030	49919.816877	60.690471
2169.043546	49706.309531	60.695476
2168.337857	49478.584232	60.700481
2167.751329	49268.138577	60.705486
2167.059137	49037.506208	60.710490
2166.176422	48830.127622	60.715495
2165.188649	48609.164939	60.720500
2165.144511	48396.992163	60.725505
2164.178541	48183.699612	60.730510
2163.693437	47961.716197	60.735514
2162.948601	47747.039872	60.740519
2162.106314	47542.934503	60.745524
2161.528344	47322.707332	60.750529
2160.742609	47112.432687	60.755534
2160.054845	46897.074353	60.760538
2159.715402	46684.779126	60.765543
2158.812158	46477.301638	60.770548
2158.393541	46256.028139	60.775553
2157.331244	46042.931691	60.780558
2156.683524	45835.161863	60.785562
2156.331090	45619.411692	60.790567
2155.387980	45409.160207	60.795572
2154.596600	45195.616715	60.800577
2153.916475	44988.149883	60.805582
2153.521484	44777.433152	60.810586
2152.480013	44567.280127	60.815591
2151.555481	44373.997096	60.820596
2151.430353	44148.117621	60.825601
2150.392493	43956.935103	60.830606
2149.707522	43750.593847	60.835610
2148.965175	43538.558776	60.840615
2148.355518	43335.790574	60.845620
2147.885003	43129.381551	60.850625
2146.833871	42930.192222	60.855630
2146.558187	42733.408973	60.860634
2145.900433	42529.680616	60.865639
2144.813450	42336.648411	60.870644
2144.712681	42133.968486	60.875649
2144.035126	41916.449951	60.880654
2143.116752	41723.960734	60.885658
2142.459051	41513.929258	60.890663
2141.815258	41310.994134	60.895668
2141.239021	41110.855532	60.900673
2140.379694	40907.171982	60.905678
2139.921811	40710.472316	60.910682
2139.119891	40506.193100	60.915687
2138.113151	40318.103607	60.920692
2137.774280	40113.834651	60.925697
2137.200566	39914.289822	60.930702
2136.149620	39709.967911	60.935706
2135.868154	39511.984500	60.940711
2134.883071	39321.167505	60.945716
2134.357323	39123.445521	60.950721
2133.477546	38929.552409	60.955726
2132.984274	38735.830990	60.960730
2132.164921	38533.011971	60.965735
2131.058751	38354.860743	60.970740
2130.756139	38156.400050	60.975745
2130.105046	37969.644269	60.980750
2129.044598	37781.700351	60.985754
2128.717201	37587.009340	60.990759
2128.001732	37406.446011	60.995764
2127.365181	37208.321281	61.000769
2126.414370	37030.775806	61.005774
2125.902448	36847.841956	61.010778
2125.418348	36652.797707	61.015783
2124.007510	36478.291634	61.020788
2123.898192	36287.372988	61.025793
2123.184748	36104.415948	61.030798
2122.395549	35929.238430	61.035802
2121.379010	35742.459351	61.040807
2120.848422	35569.073297	61.045812
2119.869816	35382.412329	61.050817
2119.272335	35208.392587	61.055822
2118.621868	35035.189124	61.060826
2118.383623	34870.676469	61.065831
2117.076694	34702.181460	61.070836
2116.894604	34520.799512	61.075841
2116.314291	34354.583976	61.080846
2115.302931	34181.942872	61.085850
2114.565544	34006.563880	61.090855
2113.814239	33844.772553	61.095860
2113.271546	33674.143745	61.100865
2112.465345	33509.816788	61.105870
2111.524523	33351.116777	61.110874
2111.138674	33178.759791	61.115879
2110.114684	33024.072795	61.120884
2109.202947	32860.751967	61.125889
2108.308051	32715.725220	61.130894
2107.589594	32562.417905	61.135898
2107.143779	32418.370237	61.140903
2106.146102	32270.169967	61.145908
2105.503870	32116.518090	61.150913
2104.396557	31984.912968	61.155918
2103.490647	31849.120962	61.160922
2103.190286	31708.709862	61.165927
2102.063020	31578.587058	61.170932
2101.371337	31437.328585	61.175937
2100.841797	31316.941729	61.180942
2100.047985	31187.783570	61.185946
2099.211650	31058.618951	61.190951
2098.071333	30934.561579	61.195956
2097.533094	30806.105367	61.200961
2096.973114	30698.081244	61.205966
2096.324133	30585.390121	61.210970
2095.740041	30462.603781	61.215975
2094.586079	30343.004147	61.220980
2094.066944	30236.303844	61.225985
2093.502957	30115.605755	61.230990
2092.734279	30005.998167	61.235994
2092.047373	29894.498100	61.240999
2091.707015	29794.719705	61.246004
2090.966566	29670.510486	61.251009
2090.079962	29567.557429	61.256014
2089.175500	29457.262482	61.261018
2088.847272	29344.748615	61.266023
2088.259629	29240.538338	61.271028
2087.733824	29128.348026	61.276033
2087.147836	29022.263469	61.281038
2086.264974	28911.806045	61.286042
2085.797683	28803.558523	61.291047
2084.606166	28703.465249	61.296052
2084.314393	28592.666571	61.301057
2083.558184	28486.776820	61.306062
2082.479426	28390.405614	61.311066
2082.131077	28282.760416	61.316071
2081.336999	28173.586252	61.321076
2081.070326	28082.950891	61.326081
2080.406589	27975.858583	61.331086
2079.822554	27865.619940	61.336090
2079.092229	27753.708526	61.341095
2078.067401	27655.130853	61.346100
2077.602913	27545.189801	61.351105
2077.035571	27459.098595	61.356110
2076.213047	27353.040344	61.361114
2075.758412	27250.076063	61.366119
2074.930366	27146.141681	61.371124
2073.988060	27049.567222	61.376129
2073.339717	26944.232816	61.381134
2072.789015	26854.227578	61.386138
2072.328846	26745.905757	61.391143
2071.532518	26659.005252	61.396148
2071.069293	26555.322455	61.401153
2070.262694	26453.969575	61.406158
2069.157057	26360.340489	61.411162
2068.477196	26258.387403	61.416167
2068.052133	26180.096683	61.421172
2067.664441	26079.586415	61.426177
2066.830171	25987.666699	61.431182
2066.256280	25890.932510	61.436186
2065.724458	25793.012240	61.441191
2064.830464	25699.655123	61.446196
2064.357299	25596.061424	61.451201
2063.933918	25503.359760	61.456206
2062.859996	25413.677004	61.461210
2062.347656	25306.278246	61.466215
2061.562793	25220.865336	61.471220
2060.747009	25109.755861	61.476225
2060.403039	25038.738049	61.481230
2059.686823	24945.030931	61.486234
2059.250958	24833.741455	61.491239
2058.167431	24754.920083	61.496244
2057.965791	24658.403555	61.501249
2057.104744	24559.619030	61.506254
2056.088515	24470.175646	61.511258
2055.787416	24372.375114	61.516263
2055.382832	24281.887237	61.521268
2054.546608	24185.547706	61.526273
2054.063505	24092.696250	61.531278
2053.002609	23994.036963	61.536282
2052.386772	23911.548325	61.541287
2051.630704	23827.634810	61.546292
2051.071010	23727.011789	61.551297
2050.130093	23636.736662	61.556302
2049.266881	23553.821621	61.561306
2048.849539	23465.185940	61.566311
2047.929950	23380.770048	61.571316
2047.586037	23297.214040	61.576321
2046.912156	23205.771298	61.581326
2045.887341	23115.701175	61.586330
2045.705825	23025.629616	61.591335
2044.516153	22955.833970	61.596340
2043.810300	22871.581913	61.601345
2043.464655	22784.414542	61.606350
2042.601112	22703.321015	61.611354
2041.833870	22622.667465	61.616359
2041.384170	22544.325005	61.621364
2040.691806	22467.179070	61.626369
2039.710080	22385.694513	61.631374
2039.223159	22309.976011	61.636378
2038.599561	22229.967333	61.641383
2037.822867	22152.416225	61.646388
2037.242586	22071.200437	61.651393
2036.812363	21982.759051	61.656398
2035.934475	21914.087959	61.661402
2035.265182	21833.299701	61.666407
2034.213305	21759.985494	61.671412
2033.714200	21674.619687	61.676417
2033.292648	21602.450611	61.681422
2032.326524	21525.552481	61.686426
2032.128007	21459.400990	61.691431
2031.440931	21390.579504	61.696436
2030.497691	21313.422947	61.701441
2030.035634	21241.359858	61.706446
2029.242607	21160.493609	61.711450
2028.874270	21078.382320	61.716455
2028.165568	21013.588837	61.721460
2027.676451	20933.762773	61.726465
2026.781141	20847.809753	61.731470
2026.126322	20773.930214	61.736474
2025.745737	20697.885152	61.741479
2024.726203	20621.956070	61.746484
2024.647632	20532.919039	61.751489
2023.944967	20457.763180	61.756494
2022.841159	20382.607388	61.761498
2022.153176	20297.727469	61.766503
2021.582061	20226.497190	61.771508
2020.855980	20151.203606	61.776513
2020.229770	20070.290035	61.781518
2019.459944	19995.008485	61.786522
2019.296466	19918.322035	61.791527
2017.990518	19849.987238	61.796532
2017.261199	19769.626481	61.801537
2016.975610	19693.505275	61.806542
2016.052588	19619.640963	61.811546
2015.545264	19536.211690	61.816551
2014.562462	19463.526070	61.821556
2014.037538	19400.519614	61.826561
2013.456505	19321.862280	61.831566
2012.603241	19261.141976	61.836570
2012.019227	19185.135733	61.841575
2011.661939	19119.504414	61.846580
2010.765323	19043.828340	61.851585
2010.292331	18972.814372	61.856590
2009.396581	18907.095321	61.861594
2008.856180	18820.053796	61.866599
2008.151017	18755.066977	61.871604
2007.709881	18685.195564	61.876609
2006.893478	18609.947015	61.881614
2006.090690	18534.710878	61.886618
2005.762671	18459.146342	61.891623
2004.997946	18389.396685	61.896628
2004.340601	18318.889800	61.901633
2003.679472	18250.369674	61.906638
2003.069153	18183.647622	61.911642
2002.379686	18102.431388	61.916647
2001.748985	18034.088558	61.921652
2001.284241	17953.755539	61.926657
2000.338507	17880.088578	61.931662
1999.355513	17815.995241	61.936666
1998.941676	17730.441183	61.941671
1998.272062	17672.944782	61.946676
1997.531084	17605.420223	61.951681
1996.881631	17515.511291	61.956686
1996.226236	17460.869481	61.961690
1995.563187	17391.571145	61.966695
1994.826801	17325.239854	61.971700
1994.199667	17249.673794	61.976705
1993.566839	17183.990548	61.981710
1992.901724	17122.845346	61.986714
1992.530234	17050.684947	61.991719
1991.893515	16983.408225	61.996724
1990.680804	16914.878121	62.001729
1990.183622	16834.369350	62.006734
1989.169210	16775.485270	62.011738
1988.663549	16709.083686	62.016743
1987.771048	16644.293493	62.021748
1987.609584	16583.386030	62.026753
1987.192469	16513.487998	62.031758
1986.337890	16458.147635	62.036762
1985.548093	16383.427014	62.041767
1985.096136	16319.445817	62.046772
1984.700683	16247.996066	62.051777
1983.468872	16172.873607	62.056782
1983.505995	16109.270508	62.061786
1982.723511	16033.498042	62.066791
1981.695010	15981.669902	62.071796
1981.142123	15906.854786	62.076801
1980.620970	15827.092483	62.081806
1979.823702	15769.996166	62.086810
1979.023274	15696.442033	62.091815
1978.360862	15623.814305	62.096820
1977.487894	15559.540391	62.101825
1977.211359	15496.103652	62.106830
1976.175808	15435.020370	62.111834
1976.129198	15362.640267	62.116839
1974.877671	15297.510371	62.121844
1974.355673	15229.069729	62.126849
1973.788599	15165.797279	62.131854
1972.922832	15101.912264	62.136858
1972.684922	15038.725129	62.141863
1971.585199	14972.413464	62.146868
1971.018530	14902.295970	62.151873
1970.242730	14846.514498	62.156878
1969.805278	14784.391949	62.161882
1969.183430	14712.256261	62.166887
1968.277674	14652.127368	62.171892
1967.489304	14588.538239	62.176897
1967.110855	14515.787896	62.181902
1966.482163	14462.794105	62.186906
1965.941627	14386.865950	62.191911
1965.081168	14326.268846	62.196916
1964.356297	14264.629679	62.201921
1963.996573	14197.274781	62.206926
1962.954684	14144.076673	62.211930
1962.559849	14073.674255	62.216935
1961.545913	14018.767217	62.221940
1960.952280	13944.569204	62.226945
1960.433696	13886.669150	62.231950
1959.522603	13830.967898	62.236954
1959.444524	13765.659344	62.241959
1958.785710	13707.109990	62.246964
1957.818464	13624.628820	62.251969
1957.069500	13562.057056	62.256974
1955.879151	13501.380529	62.261978
1956.063410	13432.970256	62.266983
1955.048694	13386.195214	62.271988
1954.278035	13324.018124	62.276993
1953.916207	13264.896442	62.281998
1952.961181	13208.329722	62.287002
1952.437433	13137.053194	62.292007
1951.519845	13080.026020	62.297012
1950.935588	13023.567749	62.302017
1950.373974	12957.804334	62.307022
1949.801991	12901.506050	62.312026
1949.611692	12830.625680	62.317031
1948.670956	12781.203073	62.322036
1947.804924	12721.096387	62.327041
1947.346198	12651.327879	62.332046
1946.486599	12595.861784	62.337050
1945.631256	12528.956111	62.342055
1945.297261	12468.323359	62.347060
1944.469851	12409.101634	62.352065
1944.031560	12340.888282	62.357070
1943.027505	12289.347540	62.362074
1942.759924	12226.839097	62.367079
1941.831218	12152.388612	62.372084
1941.204325	12089.354011	62.377089
1940.725162	12026.841505	62.382094
1939.935680	11968.940215	62.387098
1939.315369	11909.070474	62.392103
1938.625373	11847.303364	62.397108
1938.063965	11790.058803	62.402113
1937.275881	11729.439326	62.407118
1936.261817	11676.893974	62.412122
1935.974110	11610.532146	62.417127
1935.336333	11555.908569	62.422132
1934.417217	11495.128745	62.427137
1933.811991	11421.191546	62.432142
1933.131992	11369.317238	62.437146
1932.717687	11306.688902	62.442151
1932.466777	11245.826499	62.447156
1931.563962	11190.998932	62.452161
1930.925846	11115.049983	62.457166
1930.211818	11061.018095	62.462170
1929.249942	10993.218415	62.467175
1928.657759	10932.050840	62.472180
1927.963340	10883.319587	62.477185
1927.794905	10816.236681	62.482190
1927.155874	10762.323953	62.487194
1926.266417	10697.934269	62.492199
1925.817011	10633.535368	62.497204
1925.143606	10572.358864	62.502209
1924.623113	10494.451529	62.507214
1923.421957	10443.718273	62.512218
1923.131729	10364.977334	62.517223
1922.016808	10304.825551	62.522228
1921.146579	10248.219728	62.527233
1920.603146	10178.229073	62.532238
1919.783730	10118.379481	62.537242
1919.214190	10070.457927	62.542247
1918.727584	10011.849526	62.547252
1917.977909	9950.071825	62.552257
1917.425908	9893.082673	62.557262
1916.718014	9839.865485	62.562266
1915.998597	9770.372345	62.567271
1915.532498	9708.204247	62.572276
1914.654401	9656.713840	62.577281
1914.290614	9589.488288	62.582286
1913.376887	9527.015646	62.587290
1912.853628	9472.119088	62.592295
1912.132545	9422.052751	62.597300
1911.361149	9358.877712	62.602305
1910.952908	9295.918672	62.607310
1910.062957	9247.439932	62.612314
1909.613018	9178.939517	62.617319
1909.126645	9111.288213	62.622324
1908.148390	9056.670139	62.627329
1907.448328	8992.286878	62.632334
1906.858332	8936.704637	62.637338
1906.329541	8873.360977	62.642343
1905.563556	8823.283253	62.647348
1904.912666	8768.761795	62.652353
1904.549292	8697.831693	62.657358
1903.551822	8636.142517	62.662362
1903.114460	8586.106907	62.667367
1902.664146	8520.712467	62.672372
1901.689093	8466.312602	62.677377
1901.216015	8397.307407	62.682382
1900.213034	8340.258070	62.687386
1899.780208	8281.492854	62.692391
1899.071259	8220.647922	62.697396
1898.220413	8153.648122	62.702401
1897.558942	8085.851338	62.707406
1896.701087	8047.603641	62.712410
1895.765525	7982.163937	62.717415
1895.532322	7927.077489	62.722420
1894.873450	7877.229700	62.727425
1894.458627	7815.579613	62.732430
1894.063995	7760.821553	62.737434
1893.256159	7694.299003	62.742439
1892.132158	7643.912466	62.747444
1891.699518	7581.160146	62.752449
1890.978037	7520.003316	62.757454
1890.321219	7468.327533	62.762458
1889.559122	7413.124988	62.767463
1888.945523	7347.825890	62.772468
1888.335726	7301.759241	62.777473
1887.794054	7237.434513	62.782478
1887.067446	7182.829885	62.787482
1886.488032	7115.104551	62.792487
1885.576136	7057.021716	62.797492
1884.919851	7002.705563	62.802497
1884.534046	6941.489929	62.807502
1883.936755	6892.747153	62.812506
1883.084601	6834.749575	62.817511
1882.733802	6770.476234	62.822516
1881.735914	6719.040999	62.827521
1881.039401	6648.872815	62.832526
1880.462991	6614.742101	62.837530
1879.659506	6543.628224	62.842535
1878.856528	6492.992684	62.847540
1878.228893	6425.925773	62.852545
1877.791079	6369.211552	62.857550
1877.315553	6324.040075	62.862554
1876.439403	6262.488580	62.867559
1875.964708	6212.941723	62.872564
1875.149925	6150.869007	62.877569
1874.611334	6090.705798	62.882574
1873.787812	6036.265910	62.887578
1873.389125	5970.261152	62.892583
1872.711959	5907.700633	62.897588
1871.559839	5860.205320	62.902593
1871.102217	5795.436490	62.907598
1870.109076	5743.187485	62.912602
1869.613069	5692.863266	62.917607
1869.040230	5639.030270	62.922612
1868.213730	5586.030469	62.927617
1868.003220	5521.627460	62.932622
1867.158083	5475.016199	62.937626
1866.550469	5413.927260	62.942631
1865.899676	5358.306886	62.947636
1865.044356	5302.784661	62.952641
1864.513587	5241.452336	62.957646
1863.622951	5190.737358	62.962650
1863.187536	5137.333964	62.967655
1862.655786	5083.746501	62.972660
1861.778012	5029.800072	62.977665
1861.398220	4968.327385	62.982670
1860.830403	4923.179563	62.987674
1859.896409	4868.244095	62.992679
1859.331829	4813.205222	62.997684
1858.363975	4767.118899	63.002689
1858.266459	4702.666807	63.007694
1857.489870	4652.217154	63.012698
1856.765020	4589.583808	63.017703
1856.069337	4533.352148	63.022708
1855.374021	4480.317348	63.027713
1854.706381	4412.832895	63.032718
1853.686548	4361.866807	63.037722
1853.294265	4307.491018	63.042727
1852.794344	4248.832454	63.047732
1851.802279	4195.785062	63.052737
1851.332163	4128.821858	63.057742
1850.576154	4077.852724	63.062746
1849.860371	4027.144751	63.067751
1849.252344	3966.181751	63.072756
1848.478215	3922.701568	63.077761
1848.084208	3866.591760	63.082766
1847.598483	3817.055473	63.087770
1846.691308	3759.720689	63.092775
1846.042994	3705.490301	63.097780
1845.371299	3652.967377	63.102785
1844.434359	3588.922367	63.107790
1843.832370	3544.453786	63.112794
1842.874178	3496.389550	63.117799
1842.520523	3437.243315	63.122804
1841.818678	3384.842071	63.127809
1841.221381	3332.033239	63.132814
1840.114848	3291.439796	63.137818
1840.070017	3235.240679	63.142823
1839.526586	3178.889076	63.147828
1838.582979	3126.881246	63.152833
1838.193866	3066.526030	63.157838
1837.408846	3025.906725	63.162842
1836.544346	2968.962581	63.167847
1836.165592	2922.894192	63.172852
1835.458174	2867.749630	63.177857
1834.913504	2804.562162	63.182862
1833.935729	2753.794510	63.187866
1833.282173	2705.727876	63.192871
1832.706908	2654.566224	63.197876
1831.867016	2596.601503	63.202881
1831.375847	2542.292897	63.207886
1830.765126	2494.285612	63.212890
1829.995542	2443.459169	63.217895
1829.060186	2394.038510	63.222900
1828.369451	2346.769151	63.227905
1828.322154	2290.570886	63.232910
1827.536643	2237.672072	63.237914
1827.169046	2189.100398	63.242919
1826.177865	2142.496880	63.247924
1825.492761	2088.592181	63.252929
1824.746455	2031.888426	63.257934
1824.051548	1985.978857	63.262938
1823.406202	1928.045043	63.267943
1822.919767	1882.223353	63.272948
1821.993399	1834.246276	63.277953
1821.289582	1773.760252	63.282958
1820.557102	1737.354307	63.287962
1819.865630	1677.532282	63.292967
1819.361442	1622.414563	63.297972
1818.201549	1583.646489	63.302977
1817.823807	1530.508065	63.307982
1817.226745	1488.125195	63.312986
1816.736987	1438.006962	63.317991
1815.973089	1393.047815	63.322996
1815.101497	1348.311722	63.328001
1814.561861	1297.607319	63.333006
1813.845168	1254.194560	63.338010
1813.126968	1209.947883	63.343015
1812.744535	1158.321634	63.348020
1811.752696	1127.860675	63.353025
1811.169572	1074.390641	63.358030
1810.398028	1027.330009	63.363034
1809.682711	984.364151	63.368039
1809.454890	936.362704	63.373044
1808.571130	890.148296	63.378049
1808.169117	848.230730	63.383054
1807.010428	812.154996	63.388058
1806.557708	762.789405	63.393063
1806.238151	718.313760	63.398068
1805.329672	682.115036	63.403073
1804.610730	629.075084	63.408078
1804.011119	595.014884	63.413082
1802.988317	547.885312	63.418087
1802.208836	515.419850	63.423092
1801.499804	470.487967	63.428097
1801.320821	427.799732	63.433102
1800.150686	392.922240	63.438106
1799.350006	353.895410	63.443111
1798.717931	311.623250	63.448116
1797.658752	285.960963	63.453121
1797.198050	248.115225	63.458126
1796.640693	219.377869	63.463130
1796.020406	188.606785	63.468135
1795.161097	150.425619	63.473140
1794.618164	120.448236	63.478145
1794.006194	97.688672	63.483150
1792.799913	73.974826	63.488154
1791.516164	59.031838	63.493159
1791.289334	49.533484	63.498164
1789.339961	51.831611	63.503169
1787.693895	77.148000	63.508174
1786.660556	92.361202	63.513178
1786.446191	90.829318	63.518183
1786.337049	89.047332	63.523188
1786.051297	97.674641	63.528193
1786.014430	91.880383	63.533198
1785.429828	88.887083	63.538202
1784.789274	96.389576	63.543207
1783.773315	90.917953	63.548212
1782.444983	101.825550	63.553217
1781.679964	105.050544	63.558222
1781.403007	100.989661	63.563226
1780.896061	104.580534	63.568231
1780.091234	99.469628	63.573236
1779.889126	111.840028	63.578241
1779.586698	92.071744	63.583246
1779.140441	97.972714	63.588250
1778.253190	99.165468	63.593255
1777.662323	91.978400	63.598260
1776.267693	105.424427	63.603265
1775.947840	107.075869	63.608270
1775.138274	103.571081	63.613274
1773.907105	106.572052	63.618279
1773.718837	106.723392	63.623284
1773.382596	103.253830	63.628289
1773.105413	97.062486	63.633294
1772.306406	101.302145	63.638298
1771.622845	107.267612	63.643303
1771.072464	99.325048	63.648308
1769.706070	103.165947	63.653313
1769.130647	98.846529	63.658318
1768.500304	105.342872	63.663322
1767.467762	99.582145	63.668327
1767.225940	94.755583	63.673332
1766.971298	108.107317	63.678337
1766.357232	96.820634	63.683342
1765.946767	102.228637	63.688346
1765.078149	105.271387	63.693351
1764.197721	101.249568	63.698356
1762.889329	102.811986	63.703361
1762.371453	98.721555	63.708366
1762.202220	98.764215	63.713370
1761.039675	106.554618	63.718375
1760.581330	104.020674	63.723380
1760.494823	112.909669	63.728385
1760.217785	99.672357	63.733390
1758.627179	115.724729	63.738394
1758.494150	102.735786	63.743399
1757.611022	96.624902	63.748404
1757.026373	109.480256	63.753409
1756.466445	108.597772	63.758414
1755.951524	105.057238	63.763418
1754.542009	115.783780	63.768423
1754.428934	110.637142	63.773428
1753.763789	110.047339	63.778433
1753.582070	98.444413	63.783438
1752.697932	107.639850	63.788442
1750.975600	110.591097	63.793447
1750.729390	113.080840	63.798452
1749.853984	112.193263	63.803457
1749.732641	106.473919	63.808462
1749.182815	110.298693	63.813466
1748.331623	113.300835	63.818471
1748.234297	105.518142	63.823476
1746.928044	109.675936	63.828481
1746.474983	102.947967	63.833486
1745.776763	105.099478	63.838490
1745.186404	109.203507	63.843495
1744.876242	101.268533	63.848500
1744.147886	109.152419	63.853505
1743.444232	113.313866	63.858510
1743.236613	109.770264	63.863514
1742.157148	105.488320	63.868519
1741.116216	103.365451	63.873524
1740.568085	108.415270	63.878529
1740.069600	98.155777	63.883534
1738.944980	103.043254	63.888538
1738.405349	112.699658	63.893543
1738.537200	104.022693	63.898548
1736.932737	105.862382	63.903553
1736.589699	106.580785	63.908558
1736.186523	102.320754	63.913562
1735.075599	96.487335	63.918567
1734.220948	96.120025	63.923572
1733.792001	99.092957	63.928577
1733.393856	97.207059	63.933582
1733.022046	94.733496	63.938586
1732.312842	96.776365	63.943591
1731.468385	95.341400	63.948596
1730.348906	110.636124	63.953601
1729.745124	102.727284	63.958606
1729.858780	106.631196	63.963610
1728.314875	107.962947	63.968615
1728.243397	105.965243	63.973620
1727.264472	108.632856	63.978625
1726.722608	103.642633	63.983630
1726.029561	102.469056	63.988634
1725.129724	97.642923	63.993639
1725.329443	92.815630	63.998644
1724.224144	98.553187	64.003649
1723.770127	107.735515	64.008654
1722.944234	105.701505	64.013658
1722.223617	108.891077	64.018663
1721.707911	101.734664	64.023668
1720.933077	102.846503	64.028673
1720.483932	100.293760	64.033678
1720.127921	98.890035	64.038682
1718.412146	109.343524	64.043687
1718.050709	95.578727	64.048692
1717.820831	106.475901	64.053697
1716.818453	100.486476	64.058702
1715.660501	103.117869	64.063706
1715.706436	106.040615	64.068711
1714.819359	108.184281	64.073716
1713.817202	110.626927	64.078721
1713.952340	98.185196	64.083726
1713.011553	99.990456	64.088730
1712.108927	101.385950	64.093735
1711.653393	99.196928	64.098740
1711.135192	99.623027	64.103745
1710.085973	102.286039	64.108750
1709.765406	98.377176	64.113754
1709.126492	110.140422	64.118759
1708.552640	98.818986	64.123764
1707.911624	103.792096	64.128769
1707.592171	95.707218	64.133774
1706.828484	96.266926	64.138778
1705.292625	102.626395	64.143783
1704.765137	102.807962	64.148788
1704.135718	108.328020	64.153793
1703.397940	106.467683	64.158798
1703.337725	104.890821	64.163802
1702.391499	105.061623	64.168807
1701.924559	90.878346	64.173812
1701.652797	101.640240	64.178817
1700.854297	95.104348	64.183822
1700.372391	97.989500	64.188826
1699.331208	107.935303	64.193831
1697.770179	92.039732	64.198836
1697.502640	97.663162	64.203841
1697.334940	96.122298	64.208846
1696.539666	87.229894	64.213850
1695.505151	95.848394	64.218855
1695.376753	92.779504	64.223860
1694.419688	95.727510	64.228865
1693.982865	95.841061	64.233870
1693.264219	95.015341	64.238874
1692.687454	97.562318	64.243879
1692.633459	91.559472	64.248884
1691.721449	102.377326	64.253889
1690.422505	96.859225	64.258894
1689.841998	92.617910	64.263898
1688.925826	104.776857	64.268903
1688.287484	92.729226	64.273908
1687.618156	103.306683	64.278913
1687.076540	96.922385	64.283918
1686.701657	94.296352	64.288922
1686.346079	110.453789	64.293927
1686.074102	98.504085	64.298932
1685.027755	100.833908	64.303937
1683.879492	96.657540	64.308942
1683.188972	96.958048	64.313946
1682.275113	105.052759	64.318951
1682.075070	96.404864	64.323956
1681.483657	96.262269	64.328961
1680.804495	97.459850	64.333966
1680.266868	93.180187	64.338970
1679.733458	99.978119	64.343975
1678.727899	95.470000	64.348980
1677.743908	93.224572	64.353985
1676.937883	98.916189	64.358990
1676.611450	91.534184	64.363994
1675.809054	104.834140	64.368999
1676.006044	97.178180	64.374004
1674.859933	97.336586	64.379009
1674.042661	97.013822	64.384014
1674.135428	100.064746	64.389018
1673.227743	106.999402	64.394023
1672.297578	91.867830	64.399028
1671.270852	103.916605	64.404033
1670.501566	97.658362	64.409038
1670.214108	97.984739	64.414042
1669.397078	101.702154	64.419047
1669.273431	98.955791	64.424052
1668.581157	104.514224	64.429057
1667.775094	97.243097	64.434062
1666.925016	95.542537	64.439066
1665.998050	103.692952	64.444071
1665.621178	101.046736	64.449076
1664.834951	108.028336	64.454081
1664.404690	103.324759	64.459086
1664.228801	94.292979	64.464090
1662.780526	100.860911	64.469095
1661.882832	90.272192	64.474100
1660.881007	101.501716	64.479105
1660.859212	97.873415	64.484110
1660.487813	95.060749	64.489114
1659.310517	96.504620	64.494119
1659.085634	88.120880	64.499124
1658.611314	94.068897	64.504129
1658.188020	83.829036	64.509134
1657.566189	86.889385	64.514138
1656.375328	103.308804	64.519143
1655.343868	92.142083	64.524148
1654.829220	92.480894	64.529153
1654.209925	97.333866	64.534158
1653.907044	93.636673	64.539162
1653.224112	90.766261	64.544167
1652.649380	89.853036	64.549172
1651.421065	94.481044	64.554177
1650.777084	98.716609	64.559182
1650.280612	90.874335	64.564186
1649.392172	99.434953	64.569191
1649.077084	89.304060	64.574196
1648.685630	91.356400	64.579201
1648.180627	94.577971	64.584206
1647.545776	99.971164	64.589210
1646.351261	103.966172	64.594215
1645.429110	94.420569	64.599220
1644.480144	92.459756	64.604225
1644.252796	102.814043	64.609230
1644.285870	97.748286	64.614234
1643.139047	108.723305	64.619239
1642.966970	95.202844	64.624244
1642.724900	95.440011	64.629249
1641.095957	99.196518	64.634254
1640.154164	91.401331	64.639258
1639.367952	98.569012	64.644263
1639.222837	89.727896	64.649268
1638.623890	100.644266	64.654273
1638.114551	99.266487	64.659278
1637.667947	98.869084	64.664282
1636.019418	103.079721	64.669287
1635.433386	91.954218	64.674292
1635.012517	95.603979	64.679297
1634.488046	100.336235	64.684302
1633.991803	94.726926	64.689306
1633.435018	102.279218	64.694311
1632.943103	97.601214	64.699316
1632.342083	92.368101	64.704321
1631.121409	90.669654	64.709326
1630.418493	88.934692	64.714330
1629.680081	98.586404	64.719335
1629.301097	88.060383	64.724340
1628.861799	97.836470	64.729345
1628.277960	102.138181	64.734350
1627.757482	95.245910	64.739354
1626.162494	93.330956	64.744359
1625.913226	88.928229	64.749364
1625.423840	95.421123	64.754369
1624.746297	96.438686	64.759374
1624.286119	93.600706	64.764378
1623.621468	103.775300	64.769383
1622.510242	98.475001	64.774388
1621.832623	90.898058	64.779393
1621.030358	98.847319	64.784398
1620.618929	95.116912	64.789402
1619.819285	99.105972	64.794407
1619.501919	94.397089	64.799412
1619.122137	97.590888	64.804417
1618.456083	101.822082	64.809422
1617.645025	96.934579	64.814426
1616.463389	104.862109	64.819431
1616.110157	93.404735	64.824436
1615.564678	103.260772	64.829441
1615.110438	100.823978	64.834446
1614.592265	97.992058	64.839450
1613.175261	99.087671	64.844455
1612.764200	82.364508	64.849460
1611.760407	95.221791	64.854465
1611.286093	95.161537	64.859470
1611.122924	87.532835	64.864474
1610.540005	93.668423	64.869479
1609.598944	93.797436	64.874484
1608.580372	97.283529	64.879489
1607.936455	99.219862	64.884494
1607.651681	91.306121	64.889498
1606.790703	100.426945	64.894503
1606.586819	85.916482	64.899508
1606.012786	91.085550	64.904513
1604.589286	97.786770	64.909518
1604.111160	85.458254	64.914522
1603.112481	95.022004	64.919527
1602.989675	92.959921	64.924532
1602.624270	93.763896	64.929537
1601.967828	96.638943	64.934542
1600.704768	92.223807	64.939546
1599.691021	95.977223	64.944551
1599.247156	91.611721	64.949556
1598.707857	99.057158	64.954561
1598.331025	97.864920	64.959566
1598.273247	83.313904	64.964570
1597.551565	97.165600	64.969575
1596.803155	93.542350	64.974580
1595.883804	91.461731	64.979585
1595.021606	91.316443	64.984590
1594.810780	102.935992	64.989594
1593.415972	101.867632	64.994599
1592.810290	86.495319	64.999604
1592.453379	93.793506	65.004609
1591.590586	97.075081	65.009614
1591.533990	86.348041	65.014618
1590.522262	92.125973	65.019623
1589.610836	91.188982	65.024628
1588.752464	92.162741	65.029633
1588.178029	90.566653	65.034638
1588.084683	95.627819	65.039642
1587.210274	102.211852	65.044647
1586.594074	90.349982	65.049652
1585.898624	80.751053	65.054657
1584.644958	91.616895	65.059662
1584.350911	79.746431	65.064666
1583.853946	91.703171	65.069671
1583.447422	93.792607	65.074676
1582.654439	92.366862	65.079681
1581.552741	88.695666	65.084686
1580.730610	93.424754	65.089690
1579.917987	93.104436	65.094695
1579.364938	86.587946	65.099700
1578.942403	88.646810	65.104705
1578.455243	99.488655	65.109710
1578.508000	92.005425	65.114714
1577.678764	99.422811	65.119719
1576.815618	85.297797	65.124724
1575.800930	90.730846	65.129729
1574.828411	97.731020	65.134734
1574.682835	92.808769	65.139738
1573.983871	94.233453	65.144743
1573.509398	95.226650	65.149748
1572.567779	96.570037	65.154753
1571.804282	90.449687	65.159758
1571.354277	85.547421	65.164762
1570.692314	98.249481	65.169767
1570.236503	92.176442	65.174772
1569.080907	96.143219	65.179777
1568.330539	100.700060	65.184782
1567.715919	94.048271	65.189786
1566.804191	97.528442	65.194791
1566.677492	97.050263	65.199796
1566.483572	101.190686	65.204801
1565.507468	98.136639	65.209806
1564.833844	88.035921	65.214810
1563.929640	96.972807	65.219815
1563.648446	93.740544	65.224820
1563.154169	91.136656	65.229825
1561.743390	97.282357	65.234830
1561.186025	87.439141	65.239834
1560.430253	91.520593	65.244839
1560.190971	88.991312	65.249844
1559.894429	95.936129	65.254849
1558.921279	104.056062	65.259854
1557.846354	92.506784	65.264858
1557.054486	103.316620	65.269863
1556.768302	97.694455	65.274868
1556.531515	88.278129	65.279873
1555.326426	96.977390	65.284878
1554.421039	90.969478	65.289882
1553.483162	94.313457	65.294887
1552.823870	94.990665	65.299892
1553.014236	90.890263	65.304897
1552.153819	102.772294	65.309902
1552.144491	93.368712	65.314906
1551.326253	97.441170	65.319911
1550.122094	91.709391	65.324916
1549.516604	95.025791	65.329921
1549.111474	94.528773	65.334926
1548.492101	92.088269	65.339930
1547.154221	102.043405	65.344935
1546.342091	93.787681	65.349940
1546.033994	94.603058	65.354945
1545.235296	100.279351	65.359950
1544.994233	92.385485	65.364954
1544.296657	98.782157	65.369959
1543.812765	96.747487	65.374964
1542.986944	91.192145	65.379969
1541.990599	107.210106	65.384974
1541.550796	95.716041	65.389978
1540.937070	95.364133	65.394983
1540.451654	90.669351	65.399988
1539.877262	92.419607	65.404993
1538.313129	91.975855	65.409998
1538.497105	90.051115	65.415002
1537.452358	93.456235	65.420007
1537.116702	94.305955	65.425012
1536.758706	89.747049	65.430017
1535.649632	94.673131	65.435022
1534.821957	93.869511	65.440026
1533.993452	98.691091	65.445031
1533.526784	91.798182	65.450036
1533.390906	90.939836	65.455041
1532.567571	92.303866	65.460046
1531.320190	91.235770	65.465050
1530.662996	92.628596	65.470055
1530.441989	99.872078	65.475060
1530.195254	95.002176	65.480065
1529.142813	95.827015	65.485070
1528.316039	89.352455	65.490074
1527.359258	92.934415	65.495079
1526.868420	94.657205	65.500084
1526.454185	89.982656	65.505089
1526.038141	95.527186	65.510094
1525.073733	88.880529	65.515098
1524.162176	86.905934	65.520103
1523.496588	86.112833	65.525108
1523.270143	82.919188	65.530113
1522.514160	88.246492	65.535118
1522.050872	80.029974	65.540122
1520.897447	83.165357	65.545127
1520.337238	87.844956	65.550132
1519.805803	91.299407	65.555137
1519.266721	91.389812	65.560142
1518.580498	86.381587	65.565146
1517.297843	93.461018	65.570151
1516.764078	91.740212	65.575156
1516.434445	86.028768	65.580161
1515.749847	93.533570	65.585166
1515.502555	85.184958	65.590170
1514.942736	94.289485	65.595175
1513.671542	90.907030	65.600180
1513.040754	91.664875	65.605185
1512.652204	91.124227	65.610190
1512.305112	90.698418	65.615194
1511.092881	92.091133	65.620199
1509.989523	91.772880	65.625204
1509.516988	90.775639	65.630209
1508.531774	90.277762	65.635214
1508.496433	82.291294	65.640218
1508.166263	88.639049	65.645223
1507.877906	93.311725	65.650228
1507.531097	86.243660	65.655233
1506.048092	96.742271	65.660238
1505.621692	85.670302	65.665242
1504.556169	94.754262	65.670247
1503.605118	88.025066	65.675252
1503.064683	84.028175	65.680257
1502.352902	96.058482	65.685262
1502.282249	84.884253	65.690266
1501.543202	90.885392	65.695271
1500.529307	89.695053	65.700276
1499.716365	89.926751	65.705281
1499.035239	94.781691	65.710286
1498.519792	86.592388	65.715290
1498.014266	90.783903	65.720295
1497.732444	86.209747	65.725300
1496.704812	89.053913	65.730305
1495.621451	92.870466	65.735310
1495.563726	89.525432	65.740314
1494.926847	88.420266	65.745319
1494.345612	92.093950	65.750324
1493.425941	87.759926	65.755329
1492.584103	88.228034	65.760334
1491.959710	83.799781	65.765338
1491.180675	100.633201	65.770343
1491.037112	95.906184	65.775348
1490.099034	87.724117	65.780353
1489.263720	92.665062	65.785358
1488.911800	85.935285	65.790362
1488.199244	89.901076	65.795367
1487.538146	86.920010	65.800372
1486.939854	86.583009	65.805377
1485.721793	94.019623	65.810382
1485.325879	84.817837	65.815386
1485.001232	88.482286	65.820391
1484.370109	96.169412	65.825396
1483.269380	85.330765	65.830401
1482.342330	92.285890	65.835406
1482.151132	78.145615	65.840410
1481.267714	87.522341	65.845415
1480.975244	83.560169	65.850420
1481.109494	77.757672	65.855425
1480.071090	84.024006	65.860430
1479.166767	82.114512	65.865434
1477.962806	94.450118	65.870439
1477.005912	96.221748	65.875444
1476.827277	82.990964	65.880449
1475.848167	96.011517	65.885454
1475.880013	87.769941	65.890458
1475.205669	85.636241	65.895463
1474.028310	89.481931	65.900468
1473.147623	89.191387	65.905473
1472.522435	91.701946	65.910478
1472.100370	83.560891	65.915482
1471.453444	91.608500	65.920487
1471.320631	99.276366	65.925492
1471.076496	90.003151	65.930497
1469.921038	94.974476	65.935502
1469.302450	88.129384	65.940506
1468.420423	89.912773	65.945511
1467.062771	86.736474	65.950516
1466.525098	81.256800	65.955521
1465.622159	91.705822	65.960526
1465.265852	83.615822	65.965530
1464.828660	94.068102	65.970535
1464.685851	84.502819	65.975540
1464.327319	86.639837	65.980545
1463.211201	102.467105	65.985550
1462.592405	89.131224	65.990554
1461.999086	96.987390	65.995559
1461.153830	90.460598	66.000564
1460.053051	92.426990	66.005569
1459.303831	97.977167	66.010574
1459.064975	87.586619	66.015578
1458.773556	85.215449	66.020583
1457.816806	95.061161	66.025588
1457.218315	87.741364	66.030593
1456.165301	91.494761	66.035598
1455.747170	79.957866	66.040602
1455.273184	83.923596	66.045607
1454.836227	87.836134	66.050612
1453.661301	87.005724	66.055617
1452.746930	88.119314	66.060622
1452.302385	83.613605	66.065626
1452.182254	87.661876	66.070631
1451.311414	84.487069	66.075636
1450.493307	79.269590	66.080641
1449.394007	88.461435	66.085646
1448.920065	83.050485	66.090650
1448.856713	85.146902	66.095655
1447.951183	87.235235	66.100660
1446.930626	94.850213	66.105665
1446.065448	94.978265	66.110670
1445.869374	85.812539	66.115674
1445.230293	88.382082	66.120679
1444.812678	90.437029	66.125684
1444.285190	87.090961	66.130689
1443.275220	91.780551	66.135694
1442.767139	84.570972	66.140698
1441.984529	88.540022	66.145703
1440.861192	85.055260	66.150708
1440.311414	80.009608	66.155713
1439.415525	87.499115	66.160718
1439.276676	83.805852	66.165722
1438.436537	77.204145	66.170727
1438.183296	83.681603	66.175732
1437.663915	84.902737	66.180737
1436.333183	90.578451	66.185742
1435.813482	86.690246	66.190746
1435.440138	89.583415	66.195751
1434.844189	89.141974	66.200756
1433.968425	84.250634	66.205761
1432.883219	85.356689	66.210766
1432.676321	82.033791	66.215770
1432.100722	93.118357	66.220775
1431.367497	88.355752	66.225780
1430.620811	80.332536	66.230785
1429.596773	89.671700	66.235790
1429.278804	83.409633	66.240794
1428.868646	80.464397	66.245799
1428.468490	86.026909	66.250804
1427.691703	77.555888	66.255809
1426.226265	91.956320	66.260814
1425.812005	80.917141	66.265818
1425.477234	91.408337	66.270823
1425.059429	82.008195	66.275828
1424.466750	81.659278	66.280833
1423.308673	96.774120	66.285838
1423.337285	79.720947	66.290842
1422.059829	85.820289	66.295847
1420.865415	83.796070	66.300852
1420.644004	83.810775	66.305857
1419.798018	84.989202	66.310862
1419.554617	82.211431	66.315866
1418.969385	81.820331	66.320871
1418.003550	88.401587	66.325876
1417.046757	78.800105	66.330881
1416.472561	85.986173	66.335886
1416.384605	86.780769	66.340890
1415.981102	78.165267	66.345895
1414.849251	79.176239	66.350900
1414.211295	77.137700	66.355905
1413.070801	88.775677	66.360910
1413.320870	79.856023	66.365914
1412.437041	79.291606	66.370919
1411.120931	83.714468	66.375924
1410.731264	72.836972	66.380929
1410.070113	87.294080	66.385934
1409.476545	82.782103	66.390938
1409.182772	80.397122	66.395943
1407.982005	80.069163	66.400948
1407.164224	76.605241	66.405953
1406.408808	85.116383	66.410958
1406.242846	88.933816	66.415962
1405.589992	79.643580	66.420967
1404.967160	80.901662	66.425972
1404.548276	83.190207	66.430977
1403.539709	87.425418	66.435982
1402.667316	80.832004	66.440986
1402.637965	75.645299	66.445991
1401.778375	80.165916	66.450996
1400.980871	73.426561	66.456001
1400.089744	79.677396	66.461006
1399.903781	83.928519	66.466010
1399.440114	89.348164	66.471015
1398.216873	83.975897	66.476020
1397.658488	80.393476	66.481025
1397.049307	85.300078	66.486030
1396.494795	80.837092	66.491034
1395.325613	88.220237	66.496039
1394.581800	81.112798	66.501044
1394.127755	77.581604	66.506049
1393.531375	89.260838	66.511054
1392.990594	83.934643	66.516058
1392.659206	84.435191	66.521063
1392.232614	81.027368	66.526068
1391.233394	78.704055	66.531073
1390.525673	92.268121	66.536078
1389.941063	81.778006	66.541082
1388.763209	77.481911	66.546087
1387.753682	80.230196	66.551092
1387.652171	87.894654	66.556097
1387.017827	86.170941	66.561102
1386.807347	74.683067	66.566106
1386.225077	81.837305	66.571111
1385.093105	92.105129	66.576116
1384.539220	73.690589	66.581121
1383.837381	83.995695	66.586126
1382.696727	77.567934	66.591130
1381.869895	83.680822	66.596135
1381.078261	86.891222	66.601140
1381.144136	74.993566	66.606145
1380.349385	82.932216	66.611150
1380.139995	89.104661	66.616154
1379.892704	84.856200	66.621159
1378.903333	82.058234	66.626164
1378.134494	76.274704	66.631169
1377.173456	73.516393	66.636174
1376.291989	80.295561	66.641178
1375.419516	73.456167	66.646183
1374.744884	81.818854	66.651188
1374.465331	78.539052	66.656193
1373.958209	84.568007	66.661198
1373.805735	84.811457	66.666202
1373.101412	81.531364	66.671207
1372.368813	87.487350	66.676212
1371.625785	79.373687	66.681217
1370.580182	80.326813	66.686222
1369.759371	82.403281	66.691226
1369.065617	86.791893	66.696231
1368.583850	98.624808	66.701236
1367.930222	89.527093	66.706241
1366.763988	86.574316	66.711246
1366.351374	85.135489	66.716250
1366.020731	82.111393	66.721255
1365.546967	79.966342	66.726260
1365.121534	81.773381	66.731265
1363.761602	83.549190	66.736270
1363.189682	83.253758	66.741274
1362.726103	80.006364	66.746279
1362.163880	89.298947	66.751284
1361.288681	81.119563	66.756289
1360.363543	82.643332	66.761294
1359.785899	86.685479	66.766298
1359.517082	82.120318	66.771303
1358.969656	82.081194	66.776308
1358.122107	76.849507	66.781313
1357.143280	85.068162	66.786318
1356.335088	85.568813	66.791322
1355.954652	87.698287	66.796327
1355.636081	88.824436	66.801332
1355.090553	80.953777	66.806337
1353.708585	82.034497	66.811342
1353.248421	82.372591	66.816346
1352.960618	84.189293	66.821351
1352.513864	81.016498	66.826356
1351.637353	78.651617	66.831361
1350.876197	83.856777	66.836366
1350.268665	79.720780	66.841370
1349.173015	74.594769	66.846375
1348.276016	76.543003	66.851380
1347.716039	76.917466	66.856385
1347.495711	89.155098	66.861390
1346.955838	83.965968	66.866394
1346.392757	79.715672	66.871399
1345.592008	83.343850	66.876404
1344.963313	73.970950	66.881409
1343.906059	74.828167	66.886414
1343.736276	82.676939	66.891418
1343.374854	84.052755	66.896423
1341.864162	92.409583	66.901428
1341.211094	80.785487	66.906433
1340.852578	79.634536	66.911438
1340.294131	80.846127	66.916442
1339.537950	74.871364	66.921447
1338.508204	80.783127	66.926452
1338.141728	78.012317	66.931457
1337.771361	84.249775	66.936462
1337.210520	79.773619	66.941466
1336.494800	79.102079	66.946471
1335.205056	75.132885	66.951476
1334.840058	71.380968	66.956481
1334.303038	84.343881	66.961486
1333.616531	74.902904	66.966490
1332.660709	75.898543	66.971495
1331.864895	80.257653	66.976500
1331.358114	79.776830	66.981505
1331.003433	80.941838	66.986510
1330.689417	74.008954	66.991514
1330.079216	75.914756	66.996519
1328.663655	75.373397	67.001524
1328.585572	74.357642	67.006529
1327.927056	71.704224	67.011534
1326.651791	72.671799	67.016538
1325.972361	70.608339	67.021543
1325.335530	81.161741	67.026548
1325.145310	76.454781	67.031553
1324.690054	72.608402	67.036558
1323.746481	72.559722	67.041562
1323.009033	68.203113	67.046567
1322.170406	75.290877	67.051572
1322.099650	68.779800	67.056577
1321.230076	78.588024	67.061582
1320.065712	74.009120	67.066586
1319.700288	73.450634	67.071591
1318.919480	80.691637	67.076596
1318.592060	74.820609	67.081601
1318.054449	80.059625	67.086606
1316.734299	80.729986	67.091610
1316.754670	71.164025	67.096615
1315.797918	73.743095	67.101620
1315.348725	65.734138	67.106625
1314.164247	75.526191	67.111630
1313.426642	81.438828	67.116634
1313.143198	84.238870	67.121639
1312.245283	87.297449	67.126644
1311.947736	79.117719	67.131649
1310.807763	88.713471	67.136654
1310.103672	83.069482	67.141658
1309.755340	77.184433	67.146663
1308.862151	84.936898	67.151668
1308.856609	76.680785	67.156673
1308.140558	83.574026	67.161678
1306.955123	84.330209	67.166682
1306.632493	76.220702	67.171687
1305.715667	80.622712	67.176692
1305.586937	75.486505	67.181697
1304.508272	85.589756	67.186702
1303.700960	86.456140	67.191706
1303.553531	84.770158	67.196711
1302.671347	90.215349	67.201716
1301.830204	82.011653	67.206721
1300.815735	80.119736	67.211726
1300.491384	80.239127	67.216730
1300.108087	77.598733	67.221735
1299.374659	84.135189	67.226740
1299.007881	80.110743	67.231745
1297.956096	88.131280	67.236750
1297.248782	82.490962	67.241754
1296.776735	74.983960	67.246759
1295.896673	82.877845	67.251764
1295.378334	76.466311	67.256769
1294.673891	80.803019	67.261774
1293.971974	77.585648	67.266778
1293.648967	73.825484	67.271783
1292.089252	82.612753	67.276788
1291.628585	75.930275	67.281793
1291.167370	75.678761	67.286798
1290.579842	80.813752	67.291802
1290.589122	81.829437	67.296807
1289.276448	80.268790	67.301812
1288.716781	76.172510	67.306817
1288.054544	71.974267	67.311822
1287.685571	70.075927	67.316826
1286.552647	76.751592	67.321831
1285.775795	86.983486	67.326836
1285.205190	72.111945	67.331841
1285.004612	78.204137	67.336846
1284.368073	73.662760	67.341850
1283.500639	70.626251	67.346855
1282.412945	77.867167	67.351860
1282.209050	82.149529	67.356865
1281.544079	83.384376	67.361870
1280.760379	84.751643	67.366874
1279.873125	74.457923	67.371879
1278.906074	78.711806	67.376884
1278.896230	81.954056	67.381889
1278.468146	78.218485	67.386894
1278.026061	79.525130	67.391898
1276.808244	76.236822	67.396903
1276.240567	83.108056	67.401908
1275.854149	75.965917	67.406913
1274.661963	79.276299	67.411918
1273.846839	83.529685	67.416922
1273.608459	72.284395	67.421927
1272.961702	84.545663	67.426932
1272.344345	75.902698	67.431937
1271.764249	72.383689	67.436942
1270.522334	77.078671	67.441946
1270.407299	79.232191	67.446951
1269.340687	81.428195	67.451956
1268.476286	82.021388	67.456961
1267.851211	81.370150	67.461966
1267.514725	81.330623	67.466970
1267.405888	74.718370	67.471975
1266.571736	76.767026	67.476980
1265.690361	75.117318	67.481985
1264.872787	84.404777	67.486990
1264.003470	76.938869	67.491994
1263.979089	71.732460	67.496999
1262.539248	76.641844	67.502004
1261.758553	77.346311	67.507009
1261.444184	79.891073	67.512014
1260.735713	82.501650	67.517018
1260.747434	73.594665	67.522023
1259.874206	78.313035	67.527028
1258.998405	68.280862	67.532033
1258.260105	67.595589	67.537038
1257.420578	75.382108	67.542042
1257.372663	75.982682	67.547047
1256.009426	80.602343	67.552052
1255.291227	73.117145	67.557057
1255.045634	75.958480	67.562062
1254.283751	73.099166	67.567066
1254.176461	71.622853	67.572071
1252.928328	81.619020	67.577076
1252.299934	79.260457	67.582081
1251.935966	79.870282	67.587086
1251.210681	76.312860	67.592090
1250.186009	71.774860	67.597095
1249.106377	67.811732	67.602100
1249.014294	65.065121	67.607105
1248.522420	71.055392	67.612110
1248.198121	75.008388	67.617114
1247.398569	70.201204	67.622119
1246.388169	80.773013	67.627124
1245.804181	67.144693	67.632129
1245.426737	73.895793	67.637134
1243.892506	70.993707	67.642138
1243.451429	75.290126	67.647143
1242.918465	73.919344	67.652148
1242.320781	64.897950	67.657153
1241.745759	77.508935	67.662158
1241.261710	73.547303	67.667162
1240.567454	69.696368	67.672167
1239.437287	74.632217	67.677172
1239.371437	70.703440	67.682177
1238.884944	74.187059	67.687182
1237.953302	79.315273	67.692186
1237.387538	66.734320	67.697191
1236.567787	73.347589	67.702196
1236.317699	75.587239	67.707201
1235.184563	75.743776	67.712206
1234.313105	73.666721	67.717210
1233.989131	72.202785	67.722215
1233.087676	80.142664	67.727220
1232.456518	71.535026	67.732225
1231.734540	75.555989	67.737230
1230.681691	76.617556	67.742234
1230.816941	67.706705	67.747239
1230.106603	78.975133	67.752244
1229.326436	72.311936	67.757249
1228.486891	75.411721	67.762254
1227.710076	82.958042	67.767258
1227.607899	73.764816	67.772263
1226.864386	78.740116	67.777268
1226.080736	70.543086	67.782273
1225.622614	74.012733	67.787278
1224.599397	71.283294	67.792282
1223.753974	72.761317	67.797287
1222.897990	78.434174	67.802292
1222.538173	71.005543	67.807297
1222.053132	77.974030	67.812302
1221.581257	77.430908	67.817306
1220.996055	65.177909	67.822311
1219.626085	70.583984	67.827316
1219.450270	69.140647	67.832321
1218.953259	74.986660	67.837326
1218.129580	82.739133	67.842330
1217.416577	75.136426	67.847335
1216.901631	77.702047	67.852340
1216.318828	76.766554	67.857345
1215.081132	70.210810	67.862350
1213.924250	78.628129	67.867354
1213.601198	73.350944	67.872359
1213.199869	82.226868	67.877364
1212.915238	76.557216	67.882369
1212.658015	73.505702	67.887374
1211.453243	81.151617	67.892378
1210.865317	72.469302	67.897383
1209.941815	81.086058	67.902388
1209.563407	72.655858	67.907393
1209.024778	73.224076	67.912398
1207.425188	84.157674	67.917402
1207.214387	77.306172	67.922407
1206.637223	79.077436	67.927412
1206.416680	80.150166	67.932417
1206.011274	74.717342	67.937422
1204.860445	86.509992	67.942426
1204.627531	77.731798	67.947431
1203.562532	76.373088	67.952436
1202.340262	68.994876	67.957441
1201.711339	72.132139	67.962446
1200.947320	69.217989	67.967450
1200.995116	63.463942	67.972455
1200.656791	70.804916	67.977460
1199.910729	68.666932	67.982465
1198.909475	71.486509	67.987470
1197.953509	75.325490	67.992474
1197.607132	64.415944	67.997479
1197.058352	66.758287	68.002484
1196.354554	70.237043	68.007489
1195.550415	69.097054	68.012494
1194.742983	68.604145	68.017498
1194.814257	64.573141	68.022503
1193.295972	74.400973	68.027508
1192.709778	66.319216	68.032513
1192.047144	73.355370	68.037518
1191.536798	72.198624	68.042522
1191.038276	70.536946	68.047527
1190.309958	73.915524	68.052532
1189.792666	65.887467	68.057537
1189.187628	69.596526	68.062542
1188.676709	76.783599	68.067546
1187.446208	67.776122	68.072551
1186.676719	73.268074	68.077556
1186.260080	67.535843	68.082561
1185.950367	80.684967	68.087566
1184.950214	76.393834	68.092570
1184.367542	72.351705	68.097575
1183.489654	78.630457	68.102580
1183.034361	79.887178	68.107585
1182.599177	74.299821	68.112590
1181.282603	78.308120	68.117594
1180.854119	79.358726	68.122599
1180.224649	81.605096	68.127604
1179.685384	78.956410	68.132609
1179.612424	77.763226	68.137614
1178.663095	73.609094	68.142618
1178.135172	76.161016	68.147623
1177.277091	79.836204	68.152628
1176.281969	75.473311	68.157633
1175.274360	75.745531	68.162638
1174.699061	77.376155	68.167642
1174.272884	64.396133	68.172647
1174.159377	80.513442	68.177652
1173.556184	79.040302	68.182657
1172.254481	76.183283	68.187662
1171.621659	71.136721	68.192666
1171.405702	72.180338	68.197671
1170.677713	70.862665	68.202676
1169.535183	69.894772	68.207681
1168.956643	68.390905	68.212686
1168.410544	67.460626	68.217690
1168.347961	64.849678	68.222695
1167.052695	74.687787	68.227700
1166.268350	69.294738	68.232705
1165.746611	70.626684	68.237710
1164.939972	80.998952	68.242714
1165.184121	71.698619	68.247719
1163.948202	78.051662	68.252724
1163.064304	77.468420	68.257729
1162.775484	64.628985	68.262734
1161.905064	68.496950	68.267738
1161.239832	70.985555	68.272743
1160.167710	73.458445	68.277748
1159.823664	75.941703	68.282753
1159.649413	71.620160	68.287758
1158.525903	75.529955	68.292762
1157.740779	69.525169	68.297767
1157.277121	76.745731	68.302772
1156.789615	72.871402	68.307777
1156.006860	73.856928	68.312782
1155.133415	82.369543	68.317786
1154.892417	76.025905	68.322791
1153.817805	76.130592	68.327796
1153.512405	83.471069	68.332801
1152.540906	78.374293	68.337806
1151.127940	76.601010	68.342810
1150.895749	66.244176	68.347815
1150.607876	72.517408	68.352820
1150.183187	72.931899	68.357825
1150.119191	65.639168	68.362830
1148.927830	72.415639	68.367834
1148.114180	70.562813	68.372839
1147.526644	73.502693	68.377844
1146.518123	66.768614	68.382849
1145.744972	70.067599	68.387854
1144.992995	71.119197	68.392858
1144.484522	69.870699	68.397863
1143.938778	74.139622	68.402868
1143.799760	71.772645	68.407873
1142.921998	70.163408	68.412878
1141.786959	75.585775	68.417882
1141.531500	66.331789	68.422887
1141.148441	75.794592	68.427892
1140.136590	75.419367	68.432897
1139.547598	68.809380	68.437902
1138.380031	78.196682	68.442906
1138.622268	64.269841	68.447911
1137.158571	76.192690	68.452916
1135.939396	75.566587	68.457921
1135.860254	79.425408	68.462926
1135.176209	80.158696	68.467930
1134.903436	73.544147	68.472935
1134.526380	78.909043	68.477940
1133.704172	70.265594	68.482945
1132.853555	72.983965	68.487950
1131.788941	73.107572	68.492954
1131.858256	64.543108	68.497959
1131.285791	73.954032	68.502964
1129.951305	69.790217	68.507969
1129.665304	68.941581	68.512974
1129.123130	78.451771	68.517978
1128.249847	73.301539	68.522983
1127.410641	72.449426	68.527988
1126.949100	69.778931	68.532993
1126.513244	81.008451	68.537998
1125.294243	78.395349	68.543002
1124.724062	67.611302	68.548007
1123.983979	72.559270	68.553012
1123.438786	75.490843	68.558017
1123.365077	72.993631	68.563022
1122.178763	65.010501	68.568026
1121.685865	62.655657	68.573031
1120.788950	70.394564	68.578036
1120.554209	80.134980	68.583041
1119.902354	67.621379	68.588046
1118.670267	74.361763	68.593050
1118.226018	64.795608	68.598055
1117.987502	80.882329	68.603060
1117.124957	67.645296	68.608065
1115.942570	69.946506	68.613070
1114.968456	74.177911	68.618074
1114.957588	70.909030	68.623079
1114.600781	71.148725	68.628084
1113.909414	63.250882	68.633089
1113.025878	66.945904	68.638094
1111.981243	73.060382	68.643098
1111.897932	64.617967	68.648103
1111.390684	69.771755	68.653108
1110.367046	67.700028	68.658113
1109.725497	68.224712	68.663118
1108.602820	72.096546	68.668122
1108.726712	63.450862	68.673127
1107.946840	69.792890	68.678132
1106.895313	64.664713	68.683137
1106.468792	66.812584	68.688142
1105.857121	69.929776	68.693146
1105.185521	60.103321	68.698151
1104.149308	74.047664	68.703156
1103.538604	78.200770	68.708161
1103.053674	64.493673	68.713166
1102.431666	77.705081	68.718170
1102.027303	62.452362	68.723175
1100.871781	72.077455	68.728180
1100.085205	69.384548	68.733185
1099.558139	67.978168	68.738190
1099.400171	71.403244	68.743194
1098.893830	70.903475	68.748199
1098.115353	73.350183	68.753204
1097.192389	69.221856	68.758209
1096.766445	65.571142	68.763214
1095.701380	75.490936	68.768218
1095.199682	63.005504	68.773223
1094.336311	65.522486	68.778228
1093.838619	77.414703	68.783233
1093.770561	66.377333	68.788238
1092.346704	73.928828	68.793242
1091.557017	74.779857	68.798247
1091.328634	74.336802	68.803252
1090.662789	69.563602	68.808257
1090.013363	67.872333	68.813262
1088.933175	72.208928	68.818266
1088.351308	75.009145	68.823271
1087.973198	77.190322	68.828276
1087.508093	63.967359	68.833281
1086.690124	59.880685	68.838286
1085.784299	70.275047	68.843290
1085.494718	72.503643	68.848295
1085.111880	68.816111	68.853300
1084.160444	70.689512	68.858305
1083.595151	67.661789	68.863310
1082.619777	80.975143	68.868314
1081.682589	68.738756	68.873319
1080.698819	61.251716	68.878324
1080.299946	75.047377	68.883329
1080.107452	68.082600	68.888334
1079.251499	78.756044	68.893338
1079.232365	60.687099	68.898343
1077.994371	65.115031	68.903348
1076.844664	73.679490	68.908353
1076.799083	71.458506	68.913358
1076.321067	76.612383	68.918362
1075.614867	75.948866	68.923367
1074.460099	76.063184	68.928372
1073.360613	73.175630	68.933377
1073.635078	69.258963	68.938382
1072.703451	74.155410	68.943386
1072.364862	73.662079	68.948391
1071.392885	78.839338	68.953396
1070.777178	72.154772	68.958401
1070.532732	65.668197	68.963406
1069.169719	75.171767	68.968410
1068.537696	67.758087	68.973415
1068.054181	72.591138	68.978420
1067.708437	70.534598	68.983425
1067.050817	67.754956	68.988430
1065.935062	72.215490	68.993434
1065.275724	66.461970	68.998439
1064.739340	75.646389	69.003444
1064.158239	78.058556	69.008449
1063.509980	68.573753	69.013454
1062.338597	80.972114	69.018458
1062.069355	77.298053	69.023463
1061.998437	83.043193	69.028468
1061.169027	77.264683	69.033473
1060.214532	76.566551	69.038478
1059.274013	75.195987	69.043482
1058.937681	81.270354	69.048487
1058.228615	76.387342	69.053492
1056.874985	84.276196	69.058497
1056.637413	73.000862	69.063502
1056.128534	80.305900	69.068506
1055.696823	70.679417	69.073511
1055.391182	71.871351	69.078516
1053.935610	69.067261	69.083521
1053.547119	63.519820	69.088526
1052.940930	81.036982	69.093530
1052.685244	66.788804	69.098535
1051.504494	74.883545	69.103540
1050.493791	74.992302	69.108545
1050.202083	73.100633	69.113550
1049.764939	79.806053	69.118554
1049.207212	72.979805	69.123559
1048.155595	77.351296	69.128564
1047.361135	83.947979	69.133569
1047.098850	77.852174	69.138574
1046.432674	82.594439	69.143578
1045.759261	83.403331	69.148583
1044.856118	72.744816	69.153588
1044.145795	78.569593	69.158593
1043.950177	73.311591	69.163598
1043.147842	73.868177	69.168602
1042.195568	82.410708	69.173607
1041.942302	72.598143	69.178612
1041.198918	86.313002	69.183617
1040.674668	72.282588	69.188622
1039.389212	82.075038	69.193626
1039.150742	71.586757	69.198631
1038.495781	75.538756	69.203636
1037.727099	86.627265	69.208641
1037.389415	73.713625	69.213646
1036.492616	80.227241	69.218650
1035.980120	76.978238	69.223655
1035.069922	81.451818	69.228660
1033.923347	81.457617	69.233665
1033.550668	76.874339	69.238670
1033.227933	83.550522	69.243674
1032.698963	79.201843	69.248679
1031.835189	72.976225	69.253684
1030.608990	82.521130	69.258689
1030.562999	76.597501	69.263694
1029.752034	81.654542	69.268698
1029.197913	75.073731	69.273703
1028.112776	83.892871	69.278708
1027.244250	85.532328	69.283713
1027.106389	74.137058	69.288718
1026.515848	78.671750	69.293722
1026.533949	74.363776	69.298727
1025.365235	70.766586	69.303732
1024.501467	74.535763	69.308737
1024.539515	72.913338	69.313742
1022.964541	78.902485	69.318746
1022.295585	76.235046	69.323751
1021.764734	71.072958	69.328756
1021.172098	80.677922	69.333761
1021.121693	73.376730	69.338766
1019.552321	70.936120	69.343770
1018.965670	71.486785	69.348775
1018.677265	80.212289	69.353780
1017.808617	82.126160	69.358785
1017.423422	73.600891	69.363790
1016.178365	79.622711	69.368794
1015.654281	72.316455	69.373799
1015.516151	71.280303	69.378804
1014.744297	74.328381	69.383809
1014.460237	70.896386	69.388814
1013.137508	81.650414	69.393818
1012.759408	78.536155	69.398823
1012.250220	67.925371	69.403828
1010.829832	83.889454	69.408833
1010.420453	72.923741	69.413838
1009.373339	73.396277	69.418842
1009.090539	68.693050	69.423847
1009.044633	78.794508	69.428852
1008.440741	78.218814	69.433857
1007.801992	70.240093	69.438862
1006.967221	78.041688	69.443866
1006.086014	71.158107	69.448871
1004.949171	67.331929	69.453876
1004.237162	65.462982	69.458881
1004.020295	73.241962	69.463886
1003.309360	72.237019	69.468890
1002.828494	76.500375	69.473895
1002.013843	81.176385	69.478900
1001.188454	78.538570	69.483905
1000.844023	72.881624	69.488910
1000.601127	87.204418	69.493914
999.208789	77.607778	69.498919
998.628339	75.099730	69.503924
997.675253	77.258855	69.508929
997.482405	66.042656	69.513934
997.005827	72.528846	69.518938
996.251730	71.174379	69.523943
995.399696	77.922158	69.528948
994.705445	80.259301	69.533953
994.535421	74.815882	69.538958
993.203528	73.668462	69.543962
992.485123	77.236325	69.548967
992.041531	68.532698	69.553972
991.400781	79.840554	69.558977
991.358477	73.938420	69.563982
990.365139	84.398778	69.568986
989.541329	81.336512	69.573991
989.574509	78.385481	69.578996
988.062552	79.496538	69.584001
987.213449	73.809502	69.589006
986.319638	85.591291	69.594010
986.132035	84.452624	69.599015
986.086790	80.528469	69.604020
984.768459	80.058565	69.609025
984.145008	74.516979	69.614030
983.306271	76.126479	69.619034
983.145651	76.319208	69.624039
982.456868	76.050341	69.629044
981.374203	82.912092	69.634049
981.020828	78.467679	69.639054
980.386892	80.148674	69.644058
979.761527	76.916067	69.649063
978.776315	79.532898	69.654068
978.220721	79.216033	69.659073
977.642194	83.859212	69.664078
977.155001	79.220047	69.669082
976.524873	73.916070	69.674087
975.668620	73.583964	69.679092
974.775662	76.116732	69.684097
974.718688	76.313471	69.689102
973.289129	76.334360	69.694106
972.819197	69.773289	69.699111
972.525522	74.833193	69.704116
971.721696	73.926618	69.709121
971.447872	72.497319	69.714126
970.091889	74.668518	69.719130
969.734877	70.814472	69.724135
969.307125	74.217822	69.729140
967.837478	71.758223	69.734145
967.497704	75.306849	69.739150
966.618815	82.047871	69.744154
966.395247	82.689013	69.749159
966.017371	71.360330	69.754164
965.349503	71.181181	69.759169
964.440459	70.258234	69.764174
963.847284	77.321226	69.769178
963.051934	83.508060	69.774183
962.129737	65.920293	69.779188
961.253393	78.164506	69.784193
960.979097	80.584648	69.789198
960.233749	79.301340	69.794202
960.203252	71.662672	69.799207
959.715628	78.942261	69.804212
958.560929	77.299884	69.809217
958.165573	75.732227	69.814222
957.305873	78.311749	69.819226
956.128364	82.093022	69.824231
955.582258	74.985830	69.829236
955.027191	75.873685	69.834241
954.648165	76.884918	69.839246
954.060345	79.000131	69.844250
952.884302	79.360741	69.849255
952.475327	69.285966	69.854260
951.934289	78.103708	69.859265
951.466483	68.429381	69.864270
950.501614	74.037635	69.869274
949.680189	72.063110	69.874279
949.365523	74.249978	69.879284
948.640134	73.848173	69.884289
948.205116	69.121868	69.889294
947.003379	67.531137	69.894298
946.137034	69.733247	69.899303
946.014255	70.366237	69.904308
945.415637	78.967637	69.909313
944.521168	70.430383	69.914318
944.038117	83.274346	69.919322
943.356187	71.052604	69.924327
943.137419	70.062405	69.929332
941.918729	73.747733	69.934337
941.097188	76.989819	69.939342
940.284636	81.512547	69.944346
939.688757	76.693565	69.949351
939.759722	79.768403	69.954356
938.439033	83.534621	69.959361
937.727733	74.282242	69.964366
937.330923	75.009300	69.969370
937.022165	72.008603	69.974375
936.379543	69.158803	69.979380
935.009297	81.047951	69.984385
934.987809	67.834870	69.989390
934.187315	76.479432	69.994394
932.930440	77.332310	69.999399
932.529387	79.543965	70.004404
931.659135	89.663057	70.009409
931.341897	77.813793	70.014414
931.183827	76.094842	70.019418
930.138884	77.283006	70.024423
929.253597	77.321392	70.029428
928.711221	76.511999	70.034433
928.424741	77.014920	70.039438
927.332070	71.749869	70.044442
926.211391	75.432224	70.049447
926.113653	72.896268	70.054452
925.286653	75.864836	70.059457
925.270405	73.328529	70.064462
924.132113	80.765280	70.069466
923.298954	76.952316	70.074471
923.158024	67.270139	70.079476
922.199428	71.112783	70.084481
921.480826	64.985539	70.089486
920.606001	77.174324	70.094490
920.007221	74.397976	70.099495
919.696900	68.240455	70.104500
918.821155	75.635426	70.109505
917.744195	73.980698	70.114510
917.139607	80.022067	70.119514
916.776290	76.000298	70.124519
916.876938	67.585402	70.129524
915.632851	75.975704	70.134529
914.705564	77.129382	70.139534
914.106972	74.726746	70.144538
913.658851	80.091932	70.149543
913.256296	66.051667	70.154548
912.139312	82.297089	70.159553
911.214459	74.833863	70.164558
910.968463	76.090439	70.169562
910.355038	78.195543	70.174567
909.888348	73.870102	70.179572
908.773448	81.415101	70.184577
908.335803	76.517332	70.189582
907.814946	81.690666	70.194586
906.724422	81.484174	70.199591
906.048150	73.998739	70.204596
905.388843	85.479875	70.209601
905.222534	79.539132	70.214606
904.723699	73.695464	70.219610
903.411064	80.652185	70.224615
903.145951	73.673758	70.229620
902.237548	84.801871	70.234625
902.076396	69.813283	70.239630
900.726484	76.216114	70.244634
899.899825	78.276306	70.249639
899.940214	73.056461	70.254644
899.217440	82.111291	70.259649
898.701700	74.619235	70.264654
897.630637	71.090148	70.269658
897.285155	78.583668	70.274663
896.589887	79.478078	70.279668
895.149368	73.749578	70.284673
894.447595	73.351915	70.289678
893.897264	81.079887	70.294682
893.378235	74.881465	70.299687
893.478245	73.610303	70.304692
893.090684	75.401922	70.309697
892.181573	73.435063	70.314702
891.183214	72.717169	70.319706
890.355013	80.301704	70.324711
889.834928	75.721412	70.329716
889.027534	82.186149	70.334721
888.694239	69.385397	70.339726
888.161994	68.973372	70.344730
886.977514	81.101060	70.349735
886.335459	69.678824	70.354740
885.711975	75.404659	70.359745
885.506816	75.640752	70.364750
884.466911	84.602552	70.369754
883.548168	77.466373	70.374759
883.142928	76.933212	70.379764
882.397576	86.833738	70.384769
882.250068	82.842284	70.389774
881.219631	76.253741	70.394778
880.423526	79.334101	70.399783
880.058985	78.553188	70.404788
878.937580	79.569037	70.409793
878.046915	82.667601	70.414798
877.484866	83.438313	70.419802
876.720746	76.544035	70.424807
876.685178	73.518793	70.429812
876.351409	85.050626	70.434817
875.691293	76.261636	70.439822
874.909054	81.948085	70.444826
874.448392	79.216000	70.449831
873.432268	77.698266	70.454836
871.991299	77.358328	70.459841
871.353133	66.973121	70.464846
871.053501	80.139556	70.469850
870.431960	78.682029	70.474855
870.281665	78.311724	70.479860
869.463543	83.216982	70.484865
868.831499	80.937952	70.489870
868.364991	80.892364	70.494874
867.420002	86.396559	70.499879
866.210524	78.989688	70.504884
865.426397	82.036607	70.509889
865.346045	74.929433	70.514894
864.892368	75.306005	70.519898
864.060610	85.414252	70.524903
863.424379	75.254240	70.529908
862.703451	87.997297	70.534913
862.206064	88.256247	70.539918
861.715805	75.236050	70.544922
860.426302	81.246086	70.549927
859.795653	70.716182	70.554932
859.228803	83.833685	70.559937
859.185543	83.168800	70.564942
858.147794	83.578407	70.569946
857.307478	81.288373	70.574951
856.826191	65.243725	70.579956
856.326005	77.216779	70.584961
855.708942	64.114273	70.589966
854.927119	76.783435	70.594970
854.118588	75.354096	70.599975
853.850195	69.148912	70.604980
852.455307	73.712304	70.609985
851.954254	78.961342	70.614990
851.289858	72.492753	70.619994
850.760624	83.858576	70.624999
850.510488	67.985296	70.630004
849.163635	76.092358	70.635009
848.487926	75.003005	70.640014
848.186690	78.269541	70.645018
847.555423	78.062520	70.650023
847.103637	73.181210	70.655028
845.852703	77.387379	70.660033
845.337799	78.853917	70.665038
845.021914	74.562837	70.670042
844.198463	74.744376	70.675047
843.150530	68.431453	70.680052
842.571631	75.104259	70.685057
842.447629	73.387778	70.690062
842.185049	73.292390	70.695066
841.182057	76.419882	70.700071
840.162558	70.463558	70.705076
839.627877	80.226478	70.710081
838.946693	67.660886	70.715086
837.858552	69.004196	70.720090
837.205138	80.102775	70.725095
836.894936	69.709535	70.730100
836.288435	76.079228	70.735105
835.992214	69.927363	70.740110
835.003038	77.611648	70.745114
834.067322	76.229367	70.750119
833.761781	69.946521	70.755124
833.323966	81.166905	70.760129
832.729652	70.956080	70.765134
831.887914	78.493897	70.770138
831.033688	80.780850	70.775143
830.653923	71.642903	70.780148
828.985676	75.947040	70.785153
828.759945	71.520189	70.790158
828.302864	70.413390	70.795162
827.887816	70.105728	70.800167
827.185989	70.925506	70.805172
825.987010	72.945632	70.810177
825.448612	79.119985	70.815182
824.625027	68.521455	70.820186
824.179218	74.537566	70.825191
824.156713	77.162071	70.830196
823.335182	72.762243	70.835201
822.474785	71.459442	70.840206
821.989636	80.053838	70.845210
820.908349	76.174751	70.850215
820.389036	71.441390	70.855220
819.596950	78.260099	70.860225
818.907080	74.667219	70.865230
818.588149	80.663138	70.870234
818.031793	89.292528	70.875239
817.057379	77.281391	70.880244
816.146230	73.580231	70.885249
815.890690	80.252036	70.890254
815.655939	78.363949	70.895258
814.250662	80.650309	70.900263
813.451952	70.281214	70.905268
812.992937	75.902034	70.910273
812.842935	75.802923	70.915278
811.837733	71.441797	70.920282
810.738319	77.789029	70.925287
810.628089	76.947147	70.930292
809.787959	83.492808	70.935297
809.653621	69.584923	70.940302
808.399707	73.857814	70.945306
807.441922	78.909898	70.950311
807.348066	75.580121	70.955316
806.794936	78.150315	70.960321
806.269872	72.293502	70.965326
805.805539	73.610071	70.970330
804.903513	76.035527	70.975335
803.951602	70.364931	70.980340
802.923708	70.107515	70.985345
802.493789	75.709513	70.990350
802.425311	68.647767	70.995354
801.233179	75.493886	71.000359
800.513637	68.646163	71.005364
799.780774	73.927374	71.010369
799.350476	76.399169	71.015374
798.334796	70.085865	71.020378
797.311771	73.052556	71.025383
797.203930	67.367455	71.030388
796.561508	70.776613	71.035393
795.823113	73.314797	71.040398
795.672109	69.803307	71.045402
794.971475	77.121552	71.050407
794.122214	75.328132	71.055412
793.691237	73.897062	71.060417
792.583870	74.536975	71.065422
791.906429	65.332885	71.070426
791.101486	75.141981	71.075431
790.905379	69.932979	71.080436
790.285495	76.427813	71.085441
789.346494	73.044912	71.090446
788.427311	71.254740	71.095450
787.909442	71.340345	71.100455
787.920136	62.720581	71.105460
786.250608	73.463668	71.110465
785.729294	69.481268	71.115470
785.046658	65.101925	71.120474
784.758170	76.533504	71.125479
784.707468	69.825322	71.130484
783.729249	73.855642	71.135489
782.574485	68.953786	71.140494
782.128142	75.362650	71.145498
781.457072	75.797497	71.150503
781.352113	65.765840	71.155508
780.142875	78.351667	71.160513
779.182052	62.891166	71.165518
778.800114	68.420870	71.170522
778.009046	79.014665	71.175527
777.227400	66.662211	71.180532
776.686513	71.936522	71.185537
776.179745	70.142204	71.190542
776.012729	74.190051	71.195546
775.019660	67.966199	71.200551
774.328472	65.467955	71.205556
773.531030	69.642965	71.210561
772.725395	68.265233	71.215566
772.083381	71.847797	71.220570
771.005722	64.303308	71.225575
770.647073	75.484280	71.230580
770.246623	79.969835	71.235585
770.065363	75.862342	71.240590
769.300979	70.270719	71.245594
768.142493	74.290316	71.250599
767.673406	65.650735	71.255604
767.149797	78.267769	71.260609
766.148931	67.840991	71.265614
765.505128	71.701386	71.270618
764.920639	68.120134	71.275623
764.695492	73.503456	71.280628
763.429700	69.742080	71.285633
762.462954	63.435198	71.290638
762.385069	66.319252	71.295642
761.590945	77.966943	71.300647
761.339284	68.996281	71.305652
760.377178	65.594994	71.310657
759.594590	71.554337	71.315662
759.287832	78.521303	71.320666
758.367186	73.055484	71.325671
757.499899	67.311513	71.330676
756.807179	67.888586	71.335681
756.576964	70.435767	71.340686
756.064892	68.733762	71.345690
754.424191	74.799753	71.350695
754.169277	69.538616	71.355700
753.459996	71.684245	71.360705
753.226841	74.358052	71.365710
753.027828	73.014642	71.370714
751.649439	77.663769	71.375719
750.814026	70.165878	71.380724
750.619156	68.747692	71.385729
749.957081	69.419236	71.390734
749.444404	61.855779	71.395738
748.158599	75.616020	71.400743
747.798467	74.880158	71.405748
747.152705	70.684190	71.410753
746.300329	73.437653	71.415758
745.503013	74.569123	71.420762
744.698344	79.410770	71.425767
744.822657	69.659585	71.430772
743.925067	77.739327	71.435777
742.977222	76.461516	71.440782
742.299470	66.860099	71.445786
741.623333	77.124942	71.450791
741.330727	69.526448	71.455796
740.894186	76.774274	71.460801
739.585451	77.685966	71.465806
739.150179	66.290793	71.470810
738.275146	67.510332	71.475815
737.905967	65.031797	71.480820
737.550596	78.809498	71.485825
736.465058	74.939013	71.490830
736.086515	73.643110	71.495834
735.128515	81.018111	71.500839
734.346944	75.118574	71.505844
733.354232	74.385652	71.510849
733.043935	71.932436	71.515854
732.953241	68.846591	71.520858
732.252144	77.964231	71.525863
731.354559	68.810980	71.530868
730.408208	75.313645	71.535873
730.054274	80.745860	71.540878
729.547624	69.740521	71.545882
728.284718	72.007413	71.550887
727.980878	70.321148	71.555892
727.209599	75.531222	71.560897
726.868144	73.221740	71.565902
726.086790	76.977886	71.570906
725.142634	81.449084	71.575911
724.569407	64.162288	71.580916
724.210788	69.281430	71.585921
723.364981	74.068130	71.590926
722.589909	60.282781	71.595930
721.893558	72.200339	71.600935
721.435029	76.304060	71.605940
721.145249	68.824969	71.610945
719.797226	73.171231	71.615950
719.118380	67.261656	71.620954
718.408018	73.796138	71.625959
718.017771	68.625940	71.630964
717.773684	78.659575	71.635969
716.612138	76.818129	71.640974
716.061638	66.658721	71.645978
715.517092	80.934899	71.650983
714.812177	64.375550	71.655988
713.821761	77.722922	71.660993
713.455952	82.627172	71.665998
713.318705	71.421098	71.671002
712.253295	80.707133	71.676007
711.261256	71.141572	71.681012
710.759265	77.343260	71.686017
710.092687	78.931744	71.691022
710.037568	69.668024	71.696026
708.430899	82.608892	71.701031
707.835684	84.496676	71.706036
707.794185	74.421805	71.711041
707.061470	78.983924	71.716046
706.120484	67.077919	71.721050
705.052605	77.091324	71.726055
704.706306	66.098313	71.731060
704.521771	76.377931	71.736065
703.406490	73.366909	71.741070
702.702693	67.598507	71.746074
702.046937	81.343612	71.751079
701.724955	70.066029	71.756084
701.326918	65.620899	71.761089
700.090108	70.862521	71.766094
699.472373	67.901594	71.771098
698.931100	78.554980	71.776103
698.488707	64.519551	71.781108
697.545377	69.881604	71.786113
696.632964	74.248406	71.791118
696.656493	68.476167	71.796122
695.764840	76.085042	71.801127
694.790061	64.086654	71.806132
694.032948	67.315398	71.811137
693.518814	66.611949	71.816142
693.031171	66.656491	71.821146
692.128625	80.893478	71.826151
691.593028	69.982647	71.831156
690.868760	63.733385	71.836161
690.334553	67.448611	71.841166
689.980214	69.313813	71.846170
688.850186	78.296329	71.851175
688.188477	68.331255	71.856180
687.754841	63.379286	71.861185
687.129150	70.698232	71.866190
686.441458	65.430321	71.871194
685.369696	79.079237	71.876199
685.003122	74.108703	71.881204
684.475735	68.763228	71.886209
683.625810	77.059324	71.891214
683.038753	68.607283	71.896218
681.925794	74.729636	71.901223
681.985974	74.119249	71.906228
681.356159	73.481530	71.911233
680.555905	72.200744	71.916238
679.717404	73.753531	71.921242
678.971066	76.264626	71.926247
678.494514	75.066340	71.931252
678.055377	73.538820	71.936257
676.766323	70.929219	71.941262
676.455471	68.890839	71.946266
675.658705	66.702750	71.951271
675.303596	61.741434	71.956276
674.401530	67.994211	71.961281
673.416410	74.991923	71.966286
673.274301	63.163738	71.971290
672.680613	67.922922	71.976295
671.900888	67.197112	71.981300
671.198575	70.573256	71.986305
670.341083	74.357310	71.991310
670.119262	71.216654	71.996314
669.184708	72.245420	72.001319
668.641095	69.282161	72.006324
668.196324	68.908296	72.011329
667.304762	74.180115	72.016334
666.326190	67.618114	72.021338
665.660065	73.180466	72.026343
665.077110	73.492503	72.031348
664.604244	69.877735	72.036353
664.002657	74.895224	72.041358
663.155852	68.747483	72.046362
662.538659	73.885728	72.051367
662.148249	63.013296	72.056372
661.160057	64.889545	72.061377
660.038254	66.720839	72.066382
659.849267	60.919365	72.071386
659.339242	71.523620	72.076391
658.796519	69.749247	72.081396
658.244421	71.034085	72.086401
657.135080	70.119492	72.091406
656.580796	64.819310	72.096410
655.844773	73.565630	72.101415
655.530230	74.096703	72.106420
654.712246	72.659475	72.111425
653.830647	71.016335	72.116430
653.615330	64.253957	72.121434
652.797701	74.061948	72.126439
651.753695	72.678059	72.131444
651.172241	70.805775	72.136449
650.012037	78.928938	72.141454
650.285225	70.738894	72.146458
649.645945	70.421236	72.151463
648.932725	65.725107	72.156468
648.069920	70.337915	72.161473
647.556111	66.926791	72.166478
646.914155	66.967529	72.171482
645.496092	72.033033	72.176487
645.025973	65.596659	72.181492
644.694820	71.517260	72.186497
644.181475	71.136972	72.191502
643.762713	67.389014	72.196506
642.623872	77.293891	72.201511
642.072260	77.321821	72.206516
641.843605	66.029395	72.211521
640.262699	68.998250	72.216526
639.806803	62.711001	72.221530
638.941918	68.705555	72.226535
638.753023	76.431196	72.231540
638.593866	68.201191	72.236545
637.521377	71.130087	72.241550
636.969894	71.612161	72.246554
635.755278	68.867727	72.251559
635.697555	71.649222	72.256564
635.188830	71.749172	72.261569
634.074763	68.990304	72.266574
633.235468	73.413292	72.271578
632.680497	78.588945	72.276583
632.521636	69.922075	72.281588
631.490414	67.974763	72.286593
630.440064	74.590214	72.291598
630.418141	73.281693	72.296602
629.857504	67.247668	72.301607
629.056212	67.993452	72.306612
628.319969	66.150556	72.311617
627.439882	70.521693	72.316622
627.118860	66.728213	72.321626
625.665650	70.873651	72.326631
625.115368	72.085666	72.331636
624.667715	65.767146	72.336641
624.295692	65.585131	72.341646
624.175167	58.280961	72.346650
623.386253	69.420063	72.351655
622.825352	66.305027	72.356660
622.111262	71.187474	72.361665
620.819892	80.930570	72.366670
619.987507	65.101194	72.371674
619.546641	69.574276	72.376679
619.422584	65.771508	72.381684
618.274309	70.462901	72.386689
617.702336	72.394311	72.391694
617.295409	58.884700	72.396698
616.307119	60.778328	72.401703
615.501869	62.070373	72.406708
614.532340	57.844008	72.411713
613.864011	68.363088	72.416718
613.729038	61.297763	72.421722
613.431704	66.233689	72.426727
612.760494	73.077349	72.431732
611.973328	63.714183	72.436737
610.877280	64.890113	72.441742
610.697554	63.114714	72.446746
609.372315	68.004604	72.451751
608.634638	63.541043	72.456756
608.290373	63.460266	72.461761
607.873853	73.814669	72.466766
607.507736	63.515549	72.471770
606.690147	69.961473	72.476775
605.697663	69.659076	72.481780
605.342639	59.892779	72.486785
604.182068	67.918241	72.491790
603.641887	60.766061	72.496794
602.989690	74.157365	72.501799
602.616185	63.310642	72.506804
602.231121	74.929486	72.511809
600.609231	68.883130	72.516814
600.189585	59.868296	72.521818
599.603790	68.619084	72.526823
599.474710	63.788943	72.531828
598.768447	68.756880	72.536833
597.516810	68.765417	72.541838
597.088688	59.608431	72.546842
596.190786	65.896836	72.551847
596.130101	70.714652	72.556852
595.539759	62.241089	72.561857
594.298188	61.279775	72.566862
593.912989	62.615316	72.571866
593.367139	62.875728	72.576871
592.256271	54.548149	72.581876
591.535808	52.614443	72.586881
590.626997	69.298291	72.591886
590.478429	63.061458	72.596890
590.139200	72.749116	72.601895
589.619490	56.945661	72.606900
588.740328	56.577915	72.611905
588.086425	63.376241	72.616910
587.889781	63.759235	72.621914
586.485352	63.943500	72.626919
585.565604	55.779450	72.631924
584.973906	58.713795	72.636929
584.814233	61.885263	72.641934
584.460486	57.075138	72.646938
583.265143	65.443612	72.651943
582.570361	67.377240	72.656948
582.389532	61.758982	72.661953
581.237256	62.459755	72.666958
580.401084	50.262745	72.671962
579.807129	59.743382	72.676967
579.372408	63.146314	72.681972
578.958699	63.183834	72.686977
578.051516	72.574018	72.691982
577.259368	59.303968	72.696986
576.670440	67.378745	72.701991
576.272917	62.088312	72.706996
575.336643	61.740705	72.712001
574.343331	68.607286	72.717006
573.890658	63.959573	72.722010
573.510889	67.677031	72.727015
572.604002	69.865217	72.732020
572.006391	64.513613	72.737025
571.141788	71.963670	72.742030
570.804411	68.396731	72.747034
570.028857	74.605737	72.752039
569.542376	67.364587	72.757044
569.104023	69.511268	72.762049
568.233472	71.148043	72.767054
567.882048	70.928062	72.772058
566.790269	79.166515	72.777063
565.616711	77.656639	72.782068
565.346282	72.306540	72.787073
564.849247	78.606807	72.792078
564.481889	70.982406	72.797082
563.157865	79.656820	72.802087
562.246304	78.510495	72.807092
561.985942	69.675299	72.812097
561.619314	79.521869	72.817102
561.359916	66.132274	72.822106
560.393960	73.782982	72.827111
559.453424	65.205934	72.832116
559.110600	63.748254	72.837121
558.335352	75.780906	72.842126
557.412634	58.172960	72.847130
556.837544	60.879161	72.852135
556.098939	59.490827	72.857140
555.857429	59.235995	72.862145
554.693026	66.893078	72.867150
554.444077	69.870610	72.872154
553.707389	70.546204	72.877159
553.036424	70.653088	72.882164
551.930208	61.962085	72.887169
551.118947	74.788951	72.892174
550.754207	69.442838	72.897178
550.142261	71.725981	72.902183
549.732842	75.914944	72.907188
549.546917	69.422289	72.912193
548.050476	74.106089	72.917198
547.812719	61.999850	72.922202
547.271478	70.406082	72.927207
546.338371	65.558931	72.932212
545.667459	57.596538	72.937217
544.936981	66.879734	72.942222
544.581659	65.231658	72.947226
543.318399	73.082689	72.952231
542.411770	70.234054	72.957236
542.339564	64.697846	72.962241
541.816416	71.708747	72.967246
541.308829	78.037506	72.972250
540.304675	74.480582	72.977255
539.774094	76.678228	72.982260
539.265633	66.400219	72.987265
538.494636	79.586531	72.992270
537.920814	68.735458	72.997274
537.047715	60.302223	73.002279
536.337567	71.023520	73.007284
535.902593	67.591981	73.012289
534.601557	73.406879	73.017294
534.091623	67.246534	73.022298
533.714306	66.795717	73.027303
533.059121	71.600993	73.032308
533.115390	65.063456	73.037313
531.778096	72.028998	73.042318
531.181271	64.521584	73.047322
530.839482	69.645948	73.052327
529.952700	75.826949	73.057332
529.176157	72.747862	73.062337
528.190979	69.651546	73.067342
527.936754	68.321683	73.072346
527.299716	71.039337	73.077351
525.826701	69.673376	73.082356
525.843618	59.653889	73.087361
524.999881	79.232141	73.092366
524.757655	69.629241	73.097370
524.269889	71.386408	73.102375
523.303801	72.825527	73.107380
522.498234	67.382481	73.112385
521.846208	73.669593	73.117390
521.413610	69.802439	73.122394
520.482505	75.181526	73.127399
519.728898	76.405451	73.132404
519.490696	69.381809	73.137409
518.611173	75.810817	73.142414
517.429379	71.321834	73.147418
516.805205	60.808379	73.152423
516.391884	69.823442	73.157428
515.996967	73.224775	73.162433
515.871416	73.686337	73.167438
514.713013	71.529099	73.172442
513.977898	76.951086	73.177447
513.307029	71.639551	73.182452
513.187119	67.270005	73.187457
511.664213	83.580195	73.192462
511.399141	75.225150	73.197466
510.851227	71.068861	73.202471
510.092477	66.558228	73.207476
509.257787	65.150521	73.212481
508.288183	70.223506	73.217486
508.072680	70.281504	73.222490
507.943262	73.520697	73.227495
506.314456	83.978338	73.232500
505.966617	73.001388	73.237505
505.384221	69.784151	73.242510
504.811853	69.933689	73.247514
503.503781	69.534948	73.252519
502.839269	65.185924	73.257524
502.729664	65.629177	73.262529
502.184756	76.145965	73.267534
502.014256	67.413163	73.272538
500.805289	80.809598	73.277543
500.199444	74.804886	73.282548
499.675802	64.250189	73.287553
498.902798	82.667583	73.292558
498.076325	70.152082	73.297562
497.200163	76.025473	73.302567
496.707255	73.350646	73.307572
496.742884	66.521508	73.312577
495.135029	62.136682	73.317582
494.628255	69.969726	73.322586
494.204831	72.743245	73.327591
493.477027	75.295593	73.332596
492.624986	68.787634	73.337601
491.911313	70.352134	73.342606
491.605593	66.743897	73.347610
491.140229	66.280304	73.352615
490.297388	69.358756	73.357620
489.873367	58.214186	73.362625
488.806157	72.221970	73.367630
488.235653	73.363119	73.372634
487.496227	73.780548	73.377639
486.421205	73.059261	73.382644
486.591042	62.029820	73.387649
485.872085	75.357657	73.392654
484.949497	66.344122	73.397658
484.228992	63.476899	73.402663
483.520413	62.955859	73.407668
483.188554	68.056567	73.412673
482.157176	64.341581	73.417678
481.137608	65.008644	73.422682
480.636397	67.581667	73.427687
479.931626	73.687955	73.432692
480.142055	62.987938	73.437697
478.829586	63.425695	73.442702
478.003798	63.662919	73.447706
477.817773	62.421546	73.452711
477.101902	61.248812	73.457716
476.665412	63.494557	73.462721
475.234800	73.539010	73.467726
475.011587	59.385165	73.472730
474.784341	60.618289	73.477735
473.517913	68.676433	73.482740
472.791074	53.855351	73.487745
471.789103	68.779990	73.492750
471.837157	65.378748	73.497754
471.229401	74.833223	73.502759
470.287307	75.735530	73.507764
469.708492	66.086917	73.512769
468.791681	71.985713	73.517774
468.529896	67.436924	73.522778
468.348042	66.078192	73.527783
466.995985	71.633166	73.532788
466.396257	74.523086	73.537793
465.367432	70.842392	73.542798
465.220795	70.548801	73.547802
464.360139	73.035589	73.552807
463.828256	68.993454	73.557812
463.432730	64.272008	73.562817
462.656766	68.311216	73.567822
461.414146	61.491759	73.572826
460.763701	64.585300	73.577831
460.207688	76.102073	73.582836
459.991676	58.496712	73.587841
459.410849	71.132338	73.592846
458.496272	73.130978	73.597850
458.019199	67.082113	73.602855
457.163613	71.230203	73.607860
456.399947	70.293747	73.612865
455.466415	67.652859	73.617870
455.119913	67.217645	73.622874
454.726920	64.880149	73.627879
454.095211	81.680738	73.632884
453.347184	71.295840	73.637889
452.282889	67.712268	73.642894
451.776308	68.072110	73.647898
451.476374	71.909327	73.652903
450.340572	69.724866	73.657908
449.937586	65.236423	73.662913
449.044883	72.523833	73.667918
448.639255	65.243028	73.672922
448.023544	60.938288	73.677927
446.748900	75.018558	73.682932
446.182363	71.033988	73.687937
445.834704	74.861463	73.692942
445.641994	72.684446	73.697946
444.958603	74.493295	73.702951
443.509146	70.930089	73.707956
443.529154	66.110904	73.712961
442.960471	69.726010	73.717966
442.340048	73.216897	73.722970
441.533970	62.473829	73.727975
440.919492	69.950302	73.732980
439.795447	71.107112	73.737985
438.651536	80.120314	73.742990
438.078726	74.562945	73.747994
438.201938	75.355460	73.752999
437.797696	73.442382	73.758004
437.036998	67.555405	73.763009
435.965036	83.202424	73.768014
435.192445	68.147359	73.773018
434.978603	67.099656	73.778023
433.673892	75.607043	73.783028
432.879765	73.418616	73.788033
432.317774	74.998390	73.793038
432.020566	67.351808	73.798042
431.773491	62.879529	73.803047
430.958759	73.380965	73.808052
430.191799	68.384390	73.813057
429.666097	73.109133	73.818062
428.686284	75.957116	73.823066
427.620379	68.925017	73.828071
426.792976	72.698042	73.833076
426.624038	72.873207	73.838081
425.790039	71.812349	73.843086
425.609646	70.182152	73.848090
425.550130	72.719504	73.853095
424.328121	77.222454	73.858100
423.932514	64.143181	73.863105
422.984070	74.544498	73.868110
421.589075	76.600772	73.873114
421.002904	74.705644	73.878119
420.431719	76.070844	73.883124
420.168280	69.844447	73.888129
419.589543	65.347743	73.893134
419.424257	64.949893	73.898138
418.432659	64.130190	73.903143
417.681312	73.910325	73.908148
417.334065	66.713265	73.913153
415.960212	67.113527	73.918158
415.638988	76.747862	73.923162
414.979571	69.657310	73.928167
413.896108	75.792412	73.933172
413.301559	67.478850	73.938177
412.482022	65.646139	73.943182
412.082766	66.802596	73.948186
411.682098	65.157036	73.953191
411.321960	68.860345	73.958196
410.383811	64.413025	73.963201
409.509551	60.218878	73.968206
409.035035	65.394360	73.973210
408.524401	65.338542	73.978215
407.314857	69.729124	73.983220
406.802695	61.490750	73.988225
406.157614	66.122552	73.993230
405.984298	69.261508	73.998234
404.980704	63.277629	74.003239
403.938390	69.614334	74.008244
403.901207	67.996013	74.013249
403.124216	64.831888	74.018254
402.409972	64.261312	74.023258
401.677544	56.635202	74.028263
400.685895	58.560985	74.033268
400.411940	62.144906	74.038273
400.041983	65.319925	74.043278
398.855596	55.753960	74.048282
398.414703	57.014823	74.053287
397.689205	64.262986	74.058292
397.200735	65.301197	74.063297
396.261570	65.630630	74.068302
395.336713	70.868411	74.073306
395.167975	67.091706	74.078311
394.655913	64.951389	74.083316
393.858080	60.071712	74.088321
392.949584	64.031131	74.093326
392.497762	67.663896	74.098330
391.948875	63.238137	74.103335
390.965442	61.475705	74.108340
390.334324	55.571257	74.113345
389.574209	61.564953	74.118350
388.930560	62.296732	74.123354
389.074239	59.203531	74.128359
387.963456	66.254469	74.133364
387.284035	61.248694	74.138369
386.529183	65.475369	74.143374
385.351547	68.168808	74.148378
384.728643	58.509908	74.153383
384.093425	68.750935	74.158388
383.716685	66.819292	74.163393
383.503600	65.366197	74.168398
382.790514	73.087051	74.173402
381.898437	68.966715	74.178407
381.048939	72.647080	74.183412
381.055379	68.596458	74.188417
379.573090	75.643524	74.193422
378.589301	66.521520	74.198426
378.367082	67.798005	74.203431
377.642761	64.153988	74.208436
377.559056	59.494837	74.213441
376.982180	67.905190	74.218446
376.138310	65.576477	74.223450
375.426042	59.755925	74.228455
374.789653	69.981371	74.233460
373.725065	61.597646	74.238465
372.972540	66.735431	74.243470
372.196769	72.496665	74.248474
372.252325	62.004258	74.253479
371.658458	71.473878	74.258484
370.372558	69.081562	74.263489
369.760302	62.551217	74.268494
369.043700	68.910147	74.273498
369.163332	61.436854	74.278503
367.929162	64.740127	74.283508
367.328242	62.062043	74.288513
366.542403	65.823731	74.293518
365.782671	65.877002	74.298522
365.573923	65.311040	74.303527
364.201470	70.561808	74.308532
363.781184	59.924457	74.313537
363.217307	62.939570	74.318542
362.647313	62.251402	74.323546
362.441586	60.204203	74.328551
361.608098	66.381488	74.333556
361.021762	65.746386	74.338561
360.384254	59.849272	74.343566
359.241279	58.564862	74.348570
358.885519	57.699053	74.353575
357.913890	60.041132	74.358580
357.490658	59.458888	74.363585
356.641959	57.216107	74.368590
355.796396	61.969753	74.373594
355.599977	59.430641	74.378599
354.838930	67.129179	74.383604
354.131828	56.740965	74.388609
353.035434	65.899582	74.393614
352.198649	64.801346	74.398618
352.120312	55.741653	74.403623
351.447494	66.337180	74.408628
351.278945	63.593353	74.413633
350.450988	63.346842	74.418638
349.830881	70.086214	74.423642
349.425905	62.888909	74.428647
348.175598	66.817659	74.433652
347.364734	61.706687	74.438657
346.915779	63.079231	74.443662
346.027478	68.423164	74.448666
345.186361	60.979974	74.453671
344.361569	64.643796	74.458676
344.075890	68.863525	74.463681
343.492984	64.999864	74.468686
343.165069	54.133337	74.473690
342.651031	53.431527	74.478695
341.362900	57.926122	74.483700
341.194131	65.419889	74.488705
340.726864	67.383555	74.493710
339.397649	65.576900	74.498714
338.537813	64.934928	74.503719
337.831161	60.789793	74.508724
337.802531	70.953083	74.513729
337.385364	65.601178	74.518734
336.248467	65.905375	74.523738
335.718612	60.789049	74.528743
334.852912	72.774653	74.533748
334.230907	65.198776	74.538753
333.652667	65.450214	74.543758
332.468265	66.115220	74.548762
332.371437	67.174607	74.553767
332.003709	67.252149	74.558772
331.235305	60.350887	74.563777
330.442645	66.732984	74.568782
329.699484	67.311904	74.573786
329.179104	56.528090	74.578791
327.958177	58.231821	74.583796
327.321495	64.294171	74.588801
326.857630	64.264033	74.593806
326.455665	68.052864	74.598810
326.031393	63.635649	74.603815
324.786811	66.629943	74.608820
324.028621	59.140431	74.613825
323.778928	63.261384	74.618830
323.200768	62.222867	74.623834
322.728193	59.350878	74.628839
321.513957	68.301206	74.633844
320.910352	62.589512	74.638849
320.797321	62.268497	74.643854
319.805461	62.935939	74.648858
318.895398	58.280758	74.653863
318.249510	66.001951	74.658868
318.133731	66.140267	74.663873
317.827076	58.984072	74.668878
316.202467	63.426649	74.673882
315.804209	55.469773	74.678887
314.934987	64.335154	74.683892
314.783214	67.128482	74.688897
313.551008	66.350321	74.693902
312.628413	65.923364	74.698906
312.531074	69.013944	74.703911
312.054374	71.212508	74.708916
311.548226	63.676522	74.713921
310.409990	63.865827	74.718926
309.637181	62.590253	74.723930
309.440355	58.299221	74.728935
308.668042	68.633070	74.733940
307.612994	63.877996	74.738945
307.065420	62.309485	74.743950
306.410832	63.531882	74.748954
306.181322	61.825947	74.753959
305.383505	71.301272	74.758964
304.882043	65.350953	74.763969
304.263991	63.112432	74.768974
303.061353	75.738369	74.773978
302.549889	68.897089	74.778983
301.391442	72.647218	74.783988
301.076381	64.699158	74.788993
300.747586	68.913146	74.793998
299.880822	65.552053	74.799002
299.197039	55.475536	74.804007
298.709119	71.038956	74.809012
298.435713	66.689164	74.814017
297.367981	66.450924	74.819022
296.387957	70.445430	74.824026
295.975484	63.116869	74.829031
295.771285	62.614844	74.834036
294.378101	63.906076	74.839041
293.885627	72.809192	74.844046
293.159974	75.574139	74.849050
292.911701	71.452153	74.854055
292.165586	69.409087	74.859060
291.374389	61.566880	74.864065
290.790867	58.982239	74.869070
289.828760	68.013820	74.874074
289.570110	62.332311	74.879079
288.563524	75.776982	74.884084
287.796476	64.726562	74.889089
287.251937	66.092274	74.894094
286.908454	65.438984	74.899098
286.690509	61.081934	74.904103
285.366177	69.354390	74.909108
284.811782	62.201416	74.914113
284.306661	70.556193	74.919118
283.222070	67.624062	74.924122
282.807364	68.680499	74.929127
281.843750	72.672396	74.934132
281.525683	60.702022	74.939137
281.186752	63.053673	74.944142
280.012062	64.519823	74.949146
279.187865	64.794706	74.954151
278.733596	66.530807	74.959156
278.042270	71.751904	74.964161
277.008265	68.822751	74.969166
275.916250	71.051585	74.974170
276.353058	60.231917	74.979175
275.576057	66.838614	74.984180
275.309515	65.744132	74.989185
274.677679	59.896604	74.994190
273.585260	64.002072	74.999194
273.004362	57.558224	75.004199
272.351104	70.598073	75.009204
271.678672	64.529934	75.014209
270.798121	57.641841	75.019214
270.254122	64.468442	75.024218
269.738538	65.293379	75.029223
268.634373	74.905853	75.034228
268.073407	67.933701	75.039233
267.575182	58.524629	75.044238
267.041211	64.994819	75.049242
266.595515	59.978639	75.054247
265.293675	60.402199	75.059252
264.597752	61.577579	75.064257
264.482324	55.078466	75.069262
263.714371	61.663221	75.074266
262.998201	55.244093	75.079271
261.866783	61.776395	75.084276
261.412523	68.527194	75.089281
261.242790	62.809440	75.094286
260.599029	61.544852	75.099290
260.177725	57.885693	75.104295
259.178097	62.351688	75.109300
258.441148	62.756174	75.114305
257.364355	63.142290	75.119310
256.480106	70.642871	75.124314
256.248703	62.055438	75.129319
255.935953	65.585630	75.134324
255.484380	62.120529	75.139329
254.715264	63.134114	75.144334
253.638766	68.057066	75.149338
253.268429	61.297386	75.154343
252.095513	66.617328	75.159348
251.427007	60.928616	75.164353
250.896002	67.940807	75.169358
250.343704	72.643011	75.174362
250.061442	62.103538	75.179367
249.124955	67.329025	75.184372
248.308047	66.722820	75.189377
248.050742	65.298864	75.194382
247.038339	69.500398	75.199386
246.372764	49.530383	75.204391
245.259023	66.530806	75.209396
244.855501	55.758357	75.214401
244.875545	51.464304	75.219406
244.049922	67.805370	75.224410
243.409907	59.756159	75.229415
242.526256	70.192925	75.234420
242.195942	62.105385	75.239425
241.056493	61.312477	75.244430
240.087545	62.722195	75.249434
239.926137	55.546019	75.254439
239.490953	61.902694	75.259444
238.503462	63.026787	75.264449
237.630852	65.425666	75.269454
236.874751	61.688992	75.274458
236.951497	59.144195	75.279463
236.473854	66.878008	75.284468
235.241579	74.694270	75.289473
234.634317	62.765276	75.294478
233.772835	64.391254	75.299482
233.567991	62.541047	75.304487
232.737340	64.379730	75.309492
232.015551	67.960935	75.314497
231.828653	58.677288	75.319502
230.346550	63.587632	75.324506
229.947222	53.935730	75.329511
229.361727	62.150356	75.334516
228.456848	70.319705	75.339521
227.861999	69.260217	75.344526
226.741008	70.314133	75.349530
226.679828	69.328846	75.354535
226.138166	69.175511	75.359540
225.705247	59.822273	75.364545
224.889838	59.627420	75.369550
223.765269	62.437050	75.374554
223.395456	61.182419	75.379559
222.385008	62.701261	75.384564
221.178975	61.814898	75.389569
220.652671	56.944043	75.394574
220.254796	63.652740	75.399578
220.059543	59.646895	75.404583
219.638740	62.828462	75.409588
219.373161	65.381314	75.414593
218.319684	59.306130	75.419598
217.370671	70.262676	75.424602
216.729835	59.945953	75.429607
216.072898	60.451236	75.434612
215.389895	63.419137	75.439617
214.647531	66.218305	75.444622
214.050437	61.245195	75.449626
213.850020	56.435932	75.454631
212.794503	63.391391	75.459636
211.796188	63.929019	75.464641
211.732920	63.648962	75.469646
210.675686	60.887547	75.474650
209.668661	57.364348	75.479655
208.832918	65.905877	75.484660
208.126613	72.141778	75.489665
207.728853	61.450417	75.494670
207.597343	69.520139	75.499674
207.372863	55.511646	75.504679
206.965665	65.295300	75.509684
205.539448	66.178688	75.514689
205.128822	62.648723	75.519694
203.956263	71.762766	75.524698
202.912641	64.515920	75.529703
202.262947	67.726095	75.534708
202.074860	62.777671	75.539713
201.787867	63.266561	75.544718
201.227191	71.090887	75.549722
200.736214	67.124301	75.554727
199.708387	69.311396	75.559732
198.960607	64.400158	75.564737
198.463100	54.293985	75.569742
196.901786	71.156044	75.574746
196.559905	64.719844	75.579751
195.880657	73.256932	75.584756
195.492724	76.121030	75.589761
195.455446	64.862848	75.594766
194.233103	65.601777	75.599770
193.623227	56.682036	75.604775
192.947932	70.360916	75.609780
192.410148	68.240516	75.614785
191.789308	71.009279	75.619790
190.984506	68.631828	75.624794
190.586925	62.683902	75.629799
189.875412	68.315088	75.634804
188.756675	71.368232	75.639809
188.259425	63.398780	75.644814
187.695759	75.839312	75.649818
187.241885	71.270727	75.654823
186.230383	69.859783	75.659828
185.552209	68.209619	75.664833
185.134199	67.320645	75.669838
184.705980	73.263060	75.674842
183.530773	64.441330	75.679847
182.627123	69.976994	75.684852
182.192416	64.780885	75.689857
182.145019	61.456368	75.694862
181.205571	73.113142	75.699866
180.245592	64.052098	75.704871
179.300313	59.881982	75.709876
178.776712	68.443141	75.714881
178.908376	62.858695	75.719886
178.303654	67.216031	75.724890
177.056545	64.989525	75.729895
176.578459	67.541568	75.734900
175.770224	71.738964	75.739905
174.958438	65.278337	75.744910
174.047175	62.690785	75.749914
173.579769	63.888105	75.754919
173.496516	65.530380	75.759924
172.505145	60.924492	75.764929
171.938181	48.840875	75.769934
170.673488	57.302563	75.774938
170.575320	56.865646	75.779943
170.429737	64.097095	75.784948
169.353126	55.398431	75.789953
168.797496	52.077674	75.794958
168.150541	60.024564	75.799962
167.181859	61.825350	75.804967
166.328597	61.521435	75.809972
165.700171	69.794958	75.814977
165.611181	60.391634	75.819982
164.048976	66.836540	75.824986
163.511358	63.405678	75.829991
162.971659	69.302790	75.834996
162.473694	63.796651	75.840001
162.282790	58.265212	75.845006
161.400757	63.348004	75.850010
160.487815	52.338257	75.855015
159.983531	57.654133	75.860020
159.571173	53.258713	75.865025
158.701316	58.429448	75.870030
157.587447	64.370793	75.875034
157.244311	63.690659	75.880039
156.746659	63.913521	75.885044
155.984718	67.247258	75.890049
155.008265	62.445035	75.895054
154.341507	62.245429	75.900058
154.103395	55.458385	75.905063
153.772958	57.761386	75.910068
152.686504	59.245065	75.915073
151.983276	51.390472	75.920078
151.394413	55.344737	75.925082
150.773818	54.325645	75.930087
149.738438	54.960670	75.935092
149.138150	58.967220	75.940097
148.957700	49.964839	75.945102
148.384786	60.621735	75.950106
147.649720	50.452533	75.955111
146.839545	54.148773	75.960116
146.096566	48.579208	75.965121
145.623445	48.711428	75.970126
144.387706	56.861006	75.975130
143.731054	53.766096	75.980135
143.289698	53.901137	75.985140
142.607474	59.948705	75.990145
142.478277	60.904448	75.995150
141.445819	53.507626	76.000154
140.809571	54.066401	76.005159
140.315714	52.331671	76.010164
139.166394	61.631260	76.015169
138.466114	51.885444	76.020174
137.656396	57.440833	76.025178
137.510477	52.895703	76.030183
137.324366	47.560626	76.035188
136.382368	47.512143	76.040193
135.558339	51.328865	76.045198
134.796023	61.580726	76.050202
134.391872	53.504988	76.055207
133.488691	60.062449	76.060212
132.382830	62.821827	76.065217
131.953052	56.573123	76.070222
131.368161	58.344268	76.075226
131.443371	59.270574	76.080231
130.407502	60.870775	76.085236
129.366402	66.709067	76.090241
129.039458	56.410139	76.095246
128.492819	63.161488	76.100250
127.341146	57.672861	76.105255
126.514665	66.522015	76.110260
126.000488	63.579432	76.115265
125.821051	61.726761	76.120270
124.972123	67.589606	76.125274
124.175151	53.956269	76.130279
123.487818	58.020858	76.135284
123.090579	62.963283	76.140289
122.809809	62.915028	76.145294
121.768819	63.740192	76.150298
121.027342	64.739949	76.155303
120.590578	58.030317	76.160308
119.525670	61.814493	76.165313
118.578993	60.409012	76.170318
117.963472	72.903548	76.175322
118.024278	58.635120	76.180327
117.079981	64.741830	76.185332
115.752190	65.964387	76.190337
115.434099	57.106957	76.195342
114.677158	63.087598	76.200346
114.764738	61.293277	76.205351
114.072497	61.766370	76.210356
113.035560	65.188122	76.215361
112.428040	56.961890	76.220366
111.816426	63.578523	76.225370
111.117486	66.823379	76.230375
110.317495	62.822512	76.235380
109.296711	66.484540	76.240385
109.276641	61.268065	76.245390
108.620314	67.809829	76.250394
107.551200	62.073081	76.255399
106.979168	63.023746	76.260404
106.154542	61.849542	76.265409
106.128517	57.021947	76.270414
105.243680	64.442236	76.275418
104.521311	61.297892	76.280423
103.797014	61.082243	76.285428
103.307814	63.599800	76.290433
102.573680	51.161243	76.295438
101.784350	60.688869	76.300442
101.221755	59.712580	76.305447
100.756297	53.406497	76.310452
99.491141	58.645015	76.315457
99.197724	51.931456	76.320462
98.259570	58.798854	76.325466
97.620699	48.839838	76.330471
97.528578	59.055797	76.335476
96.218712	63.014661	76.340481
95.876074	50.718681	76.345486
95.380156	51.124204	76.350490
94.694054	52.313832	76.355495
93.423841	51.734234	76.360500
92.912829	63.923519	76.365505
92.433046	50.998131	76.370510
91.882842	57.207582	76.375514
91.625534	53.776196	76.380519
90.625925	55.168783	76.385524
90.027114	61.035905	76.390529
89.602963	57.569623	76.395534
88.730509	64.891749	76.400538
87.478545	57.714458	76.405543
87.243954	59.341442	76.410548
86.763299	58.869328	76.415553
86.014166	55.729259	76.420558
85.067873	61.501984	76.425562
84.644412	55.780562	76.430567
84.189106	51.445624	76.435572
83.347928	53.364879	76.440577
82.644183	56.713008	76.445582
81.767762	57.781604	76.450586
81.059674	60.323031	76.455591
80.888973	57.658422	76.460596
80.095648	63.564450	76.465601
79.673509	62.029607	76.470606
79.173063	64.454345	76.475610
78.198264	64.160380	76.480615
77.179469	66.410737	76.485620
76.336128	65.506031	76.490625
76.166346	60.225124	76.495630
75.388170	61.718023	76.500634
74.606642	49.797967	76.505639
73.769127	53.656282	76.510644
72.929855	54.018793	76.515649
72.731169	50.609602	76.520654
72.218354	59.482860	76.525658
71.992160	48.426722	76.530663
71.032450	50.013225	76.535668
70.019062	55.252606	76.540673
69.650235	50.678377	76.545678
68.563132	59.107058	76.550682
67.790798	59.214469	76.555687
67.404693	50.000473	76.560692
66.852378	50.930655	76.565697
66.535382	45.524998	76.570702
65.212174	51.659030	76.575706
64.344048	53.894823	76.580711
64.116641	43.466508	76.585716
63.897428	57.615127	76.590721
62.782088	54.640699	76.595726
61.845710	57.967586	76.600730
61.311688	59.576092	76.605735
61.129791	52.950411	76.610740
60.344220	59.615293	76.615745
59.486680	55.724550	76.620750
58.895149	61.868059	76.625754
58.571157	55.993586	76.630759
57.298165	47.813581	76.635764
56.228469	50.978804	76.640769
56.161552	42.775194	76.645774
55.506238	53.106194	76.650778
55.379932	52.274803	76.655783
54.482536	49.634627	76.660788
53.340051	52.152297	76.665793
52.996519	56.176266	76.670798
52.406534	60.020345	76.675802
51.542005	58.164977	76.680807
50.967070	55.244719	76.685812
50.241556	52.380016	76.690817
50.025862	51.365762	76.695822
48.836135	51.541323	76.700826
48.025968	51.194307	76.705831
47.531648	50.680226	76.710836
46.762392	53.704499	76.715841
46.638344	50.698143	76.720846
45.454428	55.677726	76.725850
44.593925	56.420522	76.730855
44.327247	50.063831	76.735860
43.831363	63.036024	76.740865
43.336281	53.836257	76.745870
42.196384	61.205777	76.750874
41.575359	65.302390	76.755879
41.319775	61.872311	76.760884
40.425366	63.479951	76.765889
39.769579	56.149262	76.770894
39.131196	59.439670	76.775898
38.721975	64.418709	76.780903
37.978645	62.758480	76.785908
36.858919	59.360565	76.790913
36.425155	49.756788	76.795918
35.655057	52.921546	76.800922
34.933903	59.601392	76.805927
34.222081	58.313029	76.810932
33.395913	76.180706	76.815937
33.196207	59.613650	76.820942
32.843025	57.378693	76.825946
32.248983	60.106947	76.830951
31.313496	56.242838	76.835956
30.890956	60.481260	76.840961
29.843887	51.872579	76.845966
28.877175	59.594525	76.850970
27.880115	62.765524	76.855975
27.736643	58.396632	76.860980
27.138106	63.038437	76.865985
26.792475	56.784224	76.870990
25.657097	55.054064	76.875994
25.079942	60.597625	76.880999
24.784020	55.462999	76.886004
23.819254	59.059353	76.891009
22.788819	58.615013	76.896014
22.075043	62.851001	76.901018
21.740171	62.503882	76.906023
21.521193	59.138931	76.911028
20.681916	66.168781	76.916033
20.090901	65.624395	76.921038
19.151714	63.798292	76.926042
18.643192	60.309212	76.931047
18.281578	58.583379	76.936052
17.042342	62.706057	76.941057
16.631545	56.615203	76.946062
15.848607	63.380602	76.951066
15.286872	71.509474	76.956071
14.514342	63.751134	76.961076
13.598265	63.946144	76.966081
12.986462	64.132048	76.971086
12.697960	67.518046	76.976090
12.301837	62.634366	76.981095
11.599565	60.617517	76.986100
10.336478	61.528614	76.991105
9.980379	61.340999	76.996110
9.834213	58.618868	77.001114
8.402507	54.963224	77.006119
8.156350	53.370365	77.011124
7.541691	49.291095	77.016129
6.882427	56.102999	77.021134
5.730017	57.016946	77.026139
4.978559	63.018817	77.031143
4.808250	61.141048	77.036148
4.456595	66.568223	77.041153
3.363831	56.022469	77.046158