Fri Mar 05 20:04:07 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.368856	106.438467	0.000000
-0.396492	95.686549	0.005005
-1.116466	59.411831	0.010010
-3.028483	24.051161	0.015014
-6.495265	-12.761354	0.020019
-12.382239	3.623824	0.025024
-17.170643	0.741803	0.030029
-22.018175	-0.998534	0.035034
-26.155656	0.932520	0.040038
-29.781173	-0.196922	0.045043
-33.894305	2.163918	0.050048
-37.012100	0.789493	0.055053
-40.684849	-3.472078	0.060058
-44.448705	2.348053	0.065062
-47.965262	-6.678694	0.070067
-52.049889	-1.080191	0.075072
-55.872376	-3.245756	0.080077
-59.468557	-9.416565	0.085082
-62.950045	-4.464616	0.090086
-67.113745	-6.452726	0.095091
-70.807727	-4.381043	0.100096
-74.654641	-3.204308	0.105101
-78.406873	-8.616916	0.110106
-82.374356	-7.919245	0.115110
-85.614093	-12.457982	0.120115
-89.624220	-12.087806	0.125120
-93.420837	-14.872441	0.130125
-97.144220	-6.549789	0.135130
-101.290172	-3.024553	0.140134
-104.612543	-10.946798	0.145139
-108.718275	0.940826	0.150144
-111.908274	-11.499947	0.155149
-115.343816	-10.063937	0.160154
-119.292184	-15.729030	0.165158
-123.341425	-21.035824	0.170163
-127.646520	-9.050136	0.175168
-131.099004	-14.565677	0.180173
-135.296977	-14.324723	0.185178
-139.159696	2.548285	0.190182
-142.577385	-9.688959	0.195187
-146.518577	2.081009	0.200192
-149.940886	-6.561654	0.205197
-153.632670	-4.332503	0.210202
-157.396077	5.646102	0.215206
-161.154043	-7.227514	0.220211
-164.923052	-8.130429	0.225216
-168.540976	-0.262887	0.230221
-172.389394	5.019003	0.235226
-176.179346	-1.817711	0.240230
-179.859140	-4.343312	0.245235
-183.740444	0.811379	0.250240
-187.443741	-5.162368	0.255245
-191.242432	-6.716508	0.260250
-195.070719	3.513774	0.265254
-198.623727	-4.524492	0.270259
-202.844647	1.734666	0.275264
-206.294469	-8.535645	0.280269
-210.238649	-6.597285	0.285274
-213.893204	-2.869590	0.290278
-217.336343	-4.374780	0.295283
-221.289714	4.607651	0.300288
-224.897626	-1.595724	0.305293
-228.807477	-2.854524	0.310298
-232.922358	-5.731642	0.315302
-236.524591	-7.757031	0.320307
-240.258761	-1.613345	0.325312
-243.666694	-7.449642	0.330317
-247.818705	-0.107016	0.335322
-251.349952	2.852011	0.340326
-255.296702	-1.578377	0.345331
-259.213453	2.831471	0.350336
-262.833096	-6.164295	0.355341
-265.886195	2.199848	0.360346
-269.904002	-4.587724	0.365350
-273.873738	-9.011254	0.370355
-278.097713	4.284789	0.375360
-281.733789	-2.388657	0.380365
-285.359825	-0.759575	0.385370
-289.227261	0.367160	0.390374
-292.691291	-7.084350	0.395379
-296.742640	-1.154874	0.400384
-300.184221	-2.977156	0.405389
-303.919520	-5.921052	0.410394
-308.078446	1.246161	0.415398
-311.372844	-11.682272	0.420403
-315.234131	-5.193337	0.425408
-319.125251	-4.963202	0.430413
-323.056355	-7.896308	0.435418
-326.815961	-4.987450	0.440422
-330.234136	-11.582062	0.445427
-334.307992	-5.448663	0.450432
-338.197141	-2.433952	0.455437
-341.864025	-15.220869	0.460442
-345.378419	-8.172267	0.465446
-349.140640	-13.854072	0.470451
-353.274267	-10.904384	0.475456
-356.768727	-12.705524	0.480461
-360.599460	-7.482941	0.485466
-364.957554	-6.738212	0.490470
-367.748942	-15.304655	0.495475
-371.728732	-4.937966	0.500480
-375.536230	-15.828982	0.505485
-379.125436	-23.083748	0.510490
-383.263091	-17.517244	0.515494
-387.196367	-15.482568	0.520499
-390.796356	-8.372928	0.525504
-394.190182	-18.621920	0.530509
-397.921770	-13.312612	0.535514
-401.988665	-12.093926	0.540518
-405.776628	-5.797906	0.545523
-409.726065	0.861369	0.550528
-413.317254	-3.199754	0.555533
-417.135321	-12.215621	0.560538
-420.778884	-7.857028	0.565542
-424.325554	-12.582819	0.570547
-428.295458	-15.829668	0.575552
-431.948860	-16.972968	0.580557
-435.426133	-8.480972	0.585562
-439.537978	-11.083827	0.590566
-443.232570	-18.119819	0.595571
-447.107887	-13.982795	0.600576
-451.068766	-10.208987	0.605581
-454.729149	-14.549147	0.610586
-458.606295	-3.443366	0.615590
-462.253059	-12.136435	0.620595
-465.889204	-10.978547	0.625600
-469.948497	-14.400282	0.630605
-473.081905	-14.603137	0.635610
-476.773094	-13.080056	0.640614
-480.505388	-15.420185	0.645619
-484.574044	-13.787923	0.650624
-488.708227	-20.720517	0.655629
-492.639264	-17.285718	0.660634
-496.513226	-9.304284	0.665638
-499.812063	-13.233769	0.670643
-503.459131	-6.218949	0.675648
-507.215715	-8.654503	0.680653
-510.966767	-5.805074	0.685658
-514.744142	-0.959774	0.690662
-518.371477	-8.484201	0.695667
-522.547107	-8.682947	0.700672
-525.838223	-11.039856	0.705677
-529.836656	-13.028319	0.710682
-533.703221	-5.994164	0.715686
-537.024198	-10.544523	0.720691
-540.967160	-7.702241	0.725696
-544.889622	-6.287191	0.730701
-548.912114	-11.433517	0.735706
-552.889790	-6.988243	0.740710
-555.850652	-16.514531	0.745715
-560.094307	-9.989371	0.750720
-563.562929	-6.994168	0.755725
-567.174555	-14.174098	0.760730
-571.445689	1.416493	0.765734
-574.937145	-8.381400	0.770739
-578.814952	-11.735745	0.775744
-582.422064	-15.298902	0.780749
-586.230528	-5.607366	0.785754
-589.886058	-4.197039	0.790758
-593.863374	-16.803054	0.795763
-597.785147	-7.886594	0.800768
-601.634203	-12.063918	0.805773
-605.063009	-6.389513	0.810778
-608.714942	-8.401660	0.815782
-612.073946	-5.176324	0.820787
-616.228089	-10.077576	0.825792
-620.302312	-8.318041	0.830797
-623.994276	-10.349000	0.835802
-627.962921	-8.754551	0.840806
-631.596678	-7.897986	0.845811
-635.133427	-9.163686	0.850816
-638.960422	-2.170381	0.855821
-642.330325	-8.225043	0.860826
-646.599440	-5.451900	0.865830
-650.010573	-10.046038	0.870835
-654.138052	-2.009658	0.875840
-658.016012	-13.811433	0.880845
-661.402356	-7.692735	0.885850
-665.234833	0.197181	0.890854
-668.965044	-8.152642	0.895859
-672.707134	-9.374437	0.900864
-676.612398	-3.483454	0.905869
-680.579530	-2.970929	0.910874
-684.185964	-0.828725	0.915878
-687.453082	-0.253007	0.920883
-691.641583	1.528065	0.925888
-695.438718	0.121139	0.930893
-699.044368	-13.006118	0.935898
-703.143064	-3.320065	0.940902
-706.666748	-5.492901	0.945907
-710.262033	4.144261	0.950912
-714.239534	-3.809587	0.955917
-717.722062	-0.476056	0.960922
-721.617874	0.501371	0.965926
-725.323797	-5.422200	0.970931
-729.252788	2.057469	0.975936
-733.124800	-0.639969	0.980941
-736.594678	-4.674244	0.985946
-740.621994	-0.865691	0.990950
-743.869084	-10.098407	0.995955
-748.286359	-4.447174	1.000960
-752.192884	-10.348101	1.005965
-755.558057	-6.851926	1.010970
-759.485762	-1.155916	1.015974
-763.056190	-4.909157	1.020979
-766.713568	-7.853726	1.025984
-770.438618	-4.886627	1.030989
-774.171052	-4.044034	1.035994
-778.412329	2.329742	1.040998
-781.773007	-3.625266	1.046003
-785.841673	6.172820	1.051008
-789.847355	1.574571	1.056013
-792.977236	-4.545040	1.061018
-797.091054	3.161395	1.066022
-799.989811	-2.596188	1.071027
-804.403551	9.177779	1.076032
-808.210800	4.844305	1.081037
-811.805358	0.506803	1.086042
-815.996636	2.799460	1.091046
-819.686192	-0.548306	1.096051
-823.455647	4.665205	1.101056
-826.908902	2.388254	1.106061
-830.642614	-0.928782	1.111066
-834.577822	0.004666	1.116070
-838.162307	2.334401	1.121075
-841.955707	6.690770	1.126080
-846.005527	3.050560	1.131085
-849.458319	3.438567	1.136090
-853.519251	5.973800	1.141094
-856.843404	1.514294	1.146099
-860.765576	5.943316	1.151104
-864.689694	0.037506	1.156109
-868.497838	-5.134643	1.161114
-872.331259	6.131934	1.166118
-875.738626	-1.258354	1.171123
-879.826069	9.654618	1.176128
-883.393264	2.382931	1.181133
-887.267107	-0.318687	1.186138
-891.167072	-2.427929	1.191142
-894.732147	-0.194251	1.196147
-898.626227	5.031417	1.201152
-902.358628	9.002820	1.206157
-905.866456	-1.605626	1.211162
-909.992224	3.967757	1.216166
-913.463357	-3.186777	1.221171
-917.108213	-1.498539	1.226176
-921.075209	3.883899	1.231181
-924.725917	-8.482010	1.236186
-928.558077	-3.931657	1.241190
-932.137847	-3.553186	1.246195
-936.135531	4.986448	1.251200
-939.970228	2.887351	1.256205
-943.683458	-5.688651	1.261210
-947.501969	-1.386450	1.266214
-950.988050	-8.816070	1.271219
-955.062121	1.361612	1.276224
-958.525751	3.039857	1.281229
-962.147003	-0.963562	1.286234
-966.173882	0.631302	1.291238
-969.775830	-2.936808	1.296243
-973.314665	-7.797039	1.301248
-977.344111	-9.120623	1.306253
-981.327295	-2.070272	1.311258
-985.226116	-0.355508	1.316262
-988.732163	-7.773992	1.321267
-992.641752	-0.408969	1.326272
-996.308285	6.959769	1.331277
-999.885935	-2.788975	1.336282
-1003.869872	0.349198	1.341286
-1007.809729	-5.640573	1.346291
-1011.690326	-2.192493	1.351296
-1015.187301	-5.137090	1.356301
-1018.496015	3.929564	1.361306
-1022.603904	3.798138	1.366310
-1025.950811	-8.445880	1.371315
-1030.155960	-1.446680	1.376320
-1034.097877	1.803092	1.381325
-1037.853804	-10.061681	1.386330
-1041.794284	-0.070801	1.391334
-1045.269052	-6.074972	1.396339
-1048.919929	-1.805730	1.401344
-1052.592208	-4.066232	1.406349
-1056.186132	-8.766137	1.411354
-1060.367585	-1.937829	1.416358
-1064.329624	-3.454967	1.421363
-1067.754316	-0.068680	1.426368
-1071.505149	-4.702464	1.431373
-1075.152909	-12.574369	1.436378
-1078.991084	1.801381	1.441382
-1082.639321	-8.688121	1.446387
-1086.643547	-3.892379	1.451392
-1090.685615	2.218266	1.456397
-1093.985558	-3.930487	1.461402
-1097.680959	-7.070292	1.466406
-1101.527743	-15.280889	1.471411
-1105.242651	-5.638227	1.476416
-1109.329018	-4.822061	1.481421
-1113.058120	-5.094345	1.486426
-1117.203360	-7.550311	1.491430
-1120.239946	-10.962625	1.496435
-1123.515774	-9.728913	1.501440
-1127.306353	-12.733595	1.506445
-1131.842170	-9.066960	1.511450
-1135.919768	-4.361898	1.516454
-1139.285226	-4.745932	1.521459
-1143.027117	-11.183441	1.526464
-1146.893075	0.746328	1.531469
-1150.101469	-7.545825	1.536474
-1154.209260	-2.621440	1.541478
-1157.980463	-3.061954	1.546483
-1162.081589	-2.965562	1.551488
-1165.597700	-6.077172	1.556493
-1169.192953	-16.138195	1.561498
-1173.167555	0.408857	1.566502
-1176.980596	-5.394331	1.571507
-1180.635789	-2.299001	1.576512
-1184.415420	-0.992477	1.581517
-1187.884057	-10.381465	1.586522
-1191.828887	1.013802	1.591526
-1195.771825	-11.028923	1.596531
-1199.189649	-10.248612	1.601536
-1202.937882	-3.177150	1.606541
-1206.595145	-10.463858	1.611546
-1210.782727	-6.398643	1.616550
-1214.617205	-6.084635	1.621555
-1218.280992	-9.079495	1.626560
-1221.931886	-11.915565	1.631565
-1225.642047	-13.904804	1.636570
-1229.852019	1.845813	1.641574
-1233.201169	-6.045234	1.646579
-1237.199079	-6.077187	1.651584
-1240.809690	-0.771756	1.656589
-1244.489078	-8.270900	1.661594
-1248.809963	0.729382	1.666598
-1251.799304	-9.691818	1.671603
-1255.726577	-8.462474	1.676608
-1259.663755	-7.908034	1.681613
-1263.011684	-17.671021	1.686618
-1266.962805	-9.068925	1.691622
-1270.672029	-3.154748	1.696627
-1274.596285	-4.388995	1.701632
-1278.936082	-4.224237	1.706637
-1282.412881	-15.619176	1.711642
-1286.066178	-5.907259	1.716646
-1289.784617	-4.703397	1.721651
-1293.240091	-11.353646	1.726656
-1297.070184	1.963027	1.731661
-1300.572252	-11.865750	1.736666
-1304.576121	-6.959318	1.741670
-1308.472439	-8.672629	1.746675
-1312.358446	-12.406031	1.751680
-1316.157218	-0.535643	1.756685
-1319.647463	-13.175709	1.761690
-1323.613978	-1.743650	1.766694
-1327.177413	-4.413784	1.771699
-1330.852112	-3.003974	1.776704
-1335.229344	4.367070	1.781709
-1338.856667	-7.110919	1.786714
-1342.477407	-4.011393	1.791718
-1346.071693	-17.664482	1.796723
-1349.816648	-15.068597	1.801728
-1353.404223	-12.963088	1.806733
-1356.912647	-25.759439	1.811738
-1361.040660	-16.613229	1.816742
-1364.885145	-13.738043	1.821747
-1368.514920	-12.887285	1.826752
-1372.747267	-8.466121	1.831757
-1376.113333	-17.894876	1.836762
-1380.006326	-16.415350	1.841766
-1383.583113	-18.379953	1.846771
-1387.244256	-3.319324	1.851776
-1391.132469	-4.904485	1.856781
-1395.029747	-10.857810	1.861786
-1398.884356	-3.259673	1.866790
-1402.480227	-7.190755	1.871795
-1406.126613	-1.467774	1.876800
-1409.938826	-7.617615	1.881805
-1413.484318	-5.734788	1.886810
-1417.682729	-5.343253	1.891814
-1421.249297	-5.322526	1.896819
-1425.417201	-6.884924	1.901824
-1429.289631	-6.217563	1.906829
-1432.640351	-7.350985	1.911834
-1436.393398	-9.306207	1.916838
-1439.994199	-7.794519	1.921843
-1443.563894	-11.822763	1.926848
-1447.584810	0.206394	1.931853
-1451.138140	-16.105439	1.936858
-1455.182851	-5.427030	1.941862
-1459.046726	-13.894454	1.946867
-1462.726776	-14.380602	1.951872
-1466.341504	-5.240706	1.956877
-1470.090844	-18.594370	1.961882
-1474.159938	-0.505278	1.966886
-1477.991705	-11.656983	1.971891
-1481.466731	-19.825518	1.976896
-1485.339723	-8.376644	1.981901
-1488.640064	-10.481542	1.986906
-1492.954874	-10.195806	1.991910
-1496.466372	-11.196156	1.996915
-1500.444464	-15.657523	2.006912
-1501.551291	-8.753963	2.016909
-1499.018518	-7.515824	2.026906
-1495.954963	-18.874111	2.036902
-1493.937542	-7.449876	2.046899
-1492.106704	-9.653491	2.056896
-1490.053745	-11.730045	2.066893
-1488.000844	-8.788752	2.076890
-1486.191939	-10.562539	2.086886
-1484.546234	-12.632293	2.096883
-1482.605059	-9.819944	2.106880
-1480.821702	-13.020146	2.116877
-1478.812648	-12.942316	2.126874
-1476.775577	-13.794223	2.136870
-1475.248830	-8.652900	2.146867
-1472.883389	-10.465270	2.156864
-1471.067198	-10.749704	2.166861
-1469.274773	-7.921418	2.176858
-1467.293709	-2.972835	2.186854
-1465.154460	-9.522082	2.196851
-1463.777369	-4.325207	2.206848
-1461.698192	-7.604342	2.216845
-1459.794426	-9.794347	2.226842
-1458.043849	-10.415629	2.236838
-1455.833245	-10.160054	2.246835
-1454.169768	-9.272140	2.256832
-1452.344672	-15.317918	2.266829
-1450.153091	-10.488292	2.276826
-1448.519330	-9.605089	2.286822
-1446.762671	-13.104145	2.296819
-1444.778069	-9.315044	2.306816
-1442.768937	-9.701400	2.316813
-1440.821797	-12.506222	2.326810
-1439.057862	-6.122338	2.336806
-1437.368997	-9.198432	2.346803
-1435.402326	-8.521679	2.356800
-1433.705015	-7.238119	2.366797
-1431.386493	-6.328754	2.376794
-1429.328014	-14.042919	2.386790
-1427.828529	-5.769335	2.396787
-1425.957638	-9.844029	2.406784
-1423.993482	-6.305842	2.416781
-1422.011690	-18.460304	2.426778
-1420.515485	-14.847193	2.436774
-1418.295722	-14.042002	2.446771
-1416.389450	-10.488227	2.456768
-1414.779855	-5.276440	2.466765
-1412.868885	-6.319678	2.476762
-1410.819211	-7.558805	2.486758
-1408.954581	-10.306181	2.496755
-1407.168546	-9.876797	2.506752
-1405.261103	-15.165207	2.516749
-1403.342556	-15.263871	2.526746
-1401.684771	-13.242915	2.536742
-1399.600310	-11.986575	2.546739
-1397.347133	-11.204081	2.556736
-1395.992545	-11.062453	2.566733
-1393.852581	-13.197062	2.576730
-1392.036806	-11.119287	2.586726
-1390.504809	-3.823501	2.596723
-1388.312494	-5.792805	2.606720
-1386.183189	-14.771945	2.616717
-1384.629597	-12.012724	2.626714
-1382.674748	-9.262476	2.636710
-1380.797373	-9.937156	2.646707
-1379.255529	-10.029177	2.656704
-1377.099727	-14.976803	2.666701
-1374.671660	-11.211265	2.676698
-1373.451640	-15.570138	2.686694
-1371.545454	-8.413189	2.696691
-1369.695328	-7.839300	2.706688
-1367.835847	-15.292613	2.716685
-1365.649182	-10.544219	2.726682
-1363.688272	-11.647516	2.736678
-1362.001933	-11.806868	2.746675
-1360.211766	-4.418179	2.756672
-1358.164130	-12.258445	2.766669
-1356.561362	-17.548570	2.776666
-1354.843931	-13.389781	2.786662
-1352.698929	-5.004741	2.796659
-1350.499800	-11.416634	2.806656
-1348.793244	-15.076544	2.816653
-1346.923728	-9.183164	2.826650
-1345.069983	-7.438267	2.836646
-1343.545508	-4.972773	2.846643
-1341.543397	-10.587339	2.856640
-1339.257760	-13.451000	2.866637
-1337.733938	-8.669106	2.876634
-1335.564906	-6.941512	2.886630
-1333.700676	-18.387098	2.896627
-1332.194264	-7.885103	2.906624
-1329.939321	-12.834347	2.916621
-1328.242762	-7.033264	2.926618
-1326.374793	-8.104285	2.936614
-1324.441764	-11.225699	2.946611
-1322.550314	-6.264219	2.956608
-1320.807205	-2.447401	2.966605
-1318.837246	-3.991053	2.976602
-1317.151956	-4.093362	2.986598
-1315.113858	-8.638415	2.996595
-1313.083837	-8.224326	3.006592
-1311.276195	-7.935693	3.016589
-1308.923855	-2.324818	3.026586
-1307.739566	-5.327956	3.036582
-1306.000567	1.363190	3.046579
-1303.863665	-8.476041	3.056576
-1301.855498	-12.542612	3.066573
-1299.959050	-18.304439	3.076570
-1298.449845	-10.198106	3.086566
-1296.275884	-8.807576	3.096563
-1294.621066	-12.369169	3.106560
-1292.543542	-13.798963	3.116557
-1290.569418	-12.434864	3.126554
-1288.587364	-12.043076	3.136550
-1286.929016	-12.249998	3.146547
-1285.158892	-10.745877	3.156544
-1283.107089	-13.284693	3.166541
-1281.135034	-6.117677	3.176538
-1279.606388	-11.244316	3.186534
-1277.694324	-8.395550	3.196531
-1275.857838	-11.946732	3.206528
-1273.507349	-12.305470	3.216525
-1271.602193	-13.511871	3.226522
-1270.138761	-10.070251	3.236518
-1268.380759	-8.171023	3.246515
-1266.315974	-7.972454	3.256512
-1264.443215	-8.804195	3.266509
-1262.617625	-7.774718	3.276506
-1260.550674	-10.715409	3.286502
-1258.862045	-9.810851	3.296499
-1256.991246	-11.172794	3.306496
-1255.000586	-15.691256	3.316493
-1253.085589	-11.834001	3.326490
-1251.148971	-15.031719	3.336486
-1249.312886	-13.726019	3.346483
-1247.418431	-9.164425	3.356480
-1245.911451	-10.177612	3.366477
-1243.935078	-7.451213	3.376474
-1241.905456	-12.031163	3.386470
-1240.276331	-11.030228	3.396467
-1237.950544	-14.511264	3.406464
-1236.308574	-13.340278	3.416461
-1234.306396	-20.153176	3.426458
-1232.170247	-14.798150	3.436454
-1230.971311	-10.794709	3.446451
-1228.973937	-11.423734	3.456448
-1226.827826	-12.469712	3.466445
-1224.738173	-12.256139	3.476442
-1222.738859	-13.229676	3.486438
-1221.334534	-12.268543	3.496435
-1219.799280	-7.981021	3.506432
-1217.717065	-15.878811	3.516429
-1215.459846	-16.298353	3.526426
-1213.458910	-18.285817	3.536422
-1212.004809	-15.576870	3.546419
-1209.873638	-9.442610	3.556416
-1208.123704	-13.609886	3.566413
-1206.369264	-11.121097	3.576410
-1204.343019	-6.007400	3.586406
-1202.075488	-8.242775	3.596403
-1200.709232	-5.488184	3.606400
-1198.876483	-7.799248	3.616397
-1196.544064	-6.732396	3.626394
-1195.365985	-4.847684	3.636390
-1193.346016	-0.961382	3.646387
-1191.059443	-4.852939	3.656384
-1189.444210	-2.596069	3.666381
-1187.281180	-5.034182	3.676378
-1185.504792	-2.351520	3.686374
-1183.690016	-5.218639	3.696371
-1181.784270	-11.386075	3.706368
-1179.971544	-11.068152	3.716365
-1177.953970	-11.739838	3.726362
-1176.268928	-6.178367	3.736358
-1174.473776	-8.459713	3.746355
-1172.686706	-4.570865	3.756352
-1170.316597	-8.523136	3.766349
-1168.804746	-11.858087	3.776346
-1166.664352	-12.483099	3.786342
-1164.916486	-7.724296	3.796339
-1163.116133	-7.859114	3.806336
-1160.998675	-17.611429	3.816333
-1159.248356	-4.220979	3.826330
-1157.410041	-10.391818	3.836326
-1155.681392	-6.894660	3.846323
-1153.679038	-9.603874	3.856320
-1151.854158	-13.639418	3.866317
-1150.129755	-15.825741	3.876314
-1148.021086	-11.934645	3.886310
-1145.943976	-10.316900	3.896307
-1144.455684	-9.318627	3.906304
-1142.651611	-9.758758	3.916301
-1140.470957	-8.339151	3.926298
-1138.546918	-9.442678	3.936294
-1136.581507	-7.140743	3.946291
-1135.212451	-13.675434	3.956288
-1133.116556	-9.624386	3.966285
-1131.026760	-7.288662	3.976282
-1129.319016	-8.269157	3.986278
-1127.473225	-10.433833	3.996275
-1125.664092	-12.060541	4.006272
-1123.480742	-14.283952	4.016269
-1121.809896	-11.805408	4.026266
-1119.821151	-12.660325	4.036262
-1118.051353	-8.347095	4.046259
-1116.389663	-7.790225	4.056256
-1114.217650	-8.500774	4.066253
-1112.422119	-10.028981	4.076250
-1110.522712	-8.646457	4.086246
-1108.394715	-12.245726	4.096243
-1106.615106	-9.100891	4.106240
-1104.958896	-11.025222	4.116237
-1103.005257	-13.344499	4.126234
-1101.101677	-7.061618	4.136230
-1099.301253	-10.829529	4.146227
-1097.435126	-6.441693	4.156224
-1095.543768	-9.654152	4.166221
-1093.797035	-7.812984	4.176218
-1091.852337	-11.008710	4.186214
-1090.064169	-5.796823	4.196211
-1087.961971	-8.945109	4.206208
-1085.838466	-12.510483	4.216205
-1084.312245	-6.732483	4.226202
-1082.332781	-7.322202	4.236198
-1080.629266	-5.800950	4.246195
-1078.439627	-5.371135	4.256192
-1076.775964	-2.125622	4.266189
-1075.027003	-4.494241	4.276186
-1073.182147	-7.721350	4.286182
-1070.977113	-3.501384	4.296179
-1068.999233	-2.600322	4.306176
-1067.278209	-5.310254	4.316173
-1065.779746	-9.760889	4.326170
-1063.522039	-4.384086	4.336166
-1061.632139	0.269979	4.346163
-1060.048591	-3.270585	4.356160
-1058.007590	-4.735384	4.366157
-1055.957857	-7.144203	4.376154
-1054.094569	-10.955294	4.386150
-1052.165471	-4.284874	4.396147
-1050.714565	2.390984	4.406144
-1048.839094	-6.299391	4.416141
-1046.463826	-9.682370	4.426138
-1044.716347	-9.175486	4.436134
-1043.040610	-6.419771	4.446131
-1041.302985	-4.376581	4.456128
-1039.551851	-8.076565	4.466125
-1037.116566	-7.878631	4.476122
-1035.315826	-7.086576	4.486118
-1033.723955	-5.605853	4.496115
-1031.628776	-13.851355	4.506112
-1029.866803	-9.290489	4.516109
-1027.845087	-10.185339	4.526106
-1025.885842	-9.417049	4.536102
-1024.390655	-8.168749	4.546099
-1022.655306	-8.413061	4.556096
-1020.347706	-6.468909	4.566093
-1018.534330	-6.100438	4.576090
-1016.650871	-5.368966	4.586086
-1014.772133	-1.115705	4.596083
-1013.137192	-6.961813	4.606080
-1011.084869	-9.754689	4.616077
-1008.978723	-7.121469	4.626074
-1007.447315	-7.806835	4.636070
-1005.455082	-5.123814	4.646067
-1003.567048	-6.133052	4.656064
-1001.670484	-2.885258	4.666061
-999.811948	-6.869232	4.676058
-997.825012	-5.773769	4.686054
-996.055472	-7.073523	4.696051
-994.119347	-4.822043	4.706048
-992.112840	-5.082855	4.716045
-990.387703	-0.209748	4.726042
-989.021630	-4.754429	4.736038
-986.931094	1.264975	4.746035
-984.623366	-3.354505	4.756032
-982.671326	-1.686609	4.766029
-981.220906	-7.770029	4.776026
-979.154881	-4.831945	4.786022
-977.341078	-7.899280	4.796019
-975.379364	-3.575572	4.806016
-973.771772	-2.739949	4.816013
-971.502665	-9.718489	4.826010
-969.608776	-10.269165	4.836006
-967.923774	-10.262229	4.846003
-966.200057	-10.092536	4.856000
-963.975389	-15.674495	4.865997
-962.340072	-6.413348	4.875994
-960.624868	-11.602785	4.885990
-958.510613	-12.646583	4.895987
-956.509695	-12.169107	4.905984
-954.568407	-3.359508	4.915981
-953.157197	-4.671404	4.925978
-951.136787	-7.877547	4.935974
-949.051411	-7.800409	4.945971
-947.272138	-2.002773	4.955968
-945.494796	-9.164759	4.965965
-943.323792	-7.617106	4.975962
-941.808720	-11.762429	4.985958
-939.645881	-16.123434	4.995955
-938.081682	-8.886148	5.005952
-936.204520	-10.296224	5.015949
-934.225350	-6.963687	5.025946
-931.894598	-14.406781	5.035942
-930.533152	-8.545482	5.045939
-928.644119	-6.947993	5.055936
-926.686841	-10.698227	5.065933
-924.544241	-13.412307	5.075930
-922.844492	-6.673522	5.085926
-921.254868	-7.017616	5.095923
-919.279196	-11.514466	5.105920
-917.034267	-9.806504	5.115917
-915.047207	-9.404144	5.125914
-913.351462	-9.885200	5.135910
-911.983507	-17.264332	5.145907
-909.909643	-8.583261	5.155904
-907.696273	-10.274437	5.165901
-905.955553	-15.035287	5.175898
-904.129432	-16.819279	5.185894
-902.202394	-13.397854	5.195891
-900.440270	-8.814803	5.205888
-898.499603	-12.480254	5.215885
-896.786192	-13.662013	5.225882
-894.654500	-12.573817	5.235878
-892.594134	-16.103664	5.245875
-891.202897	-6.955015	5.255872
-889.309626	-14.577598	5.265869
-887.130098	-11.022844	5.275866
-885.427190	-11.994496	5.285862
-883.481211	-11.110281	5.295859
-881.691716	-5.939487	5.305856
-879.585059	-9.434094	5.315853
-877.871882	-17.234716	5.325850
-875.946861	-11.386117	5.335846
-873.953368	-20.993646	5.345843
-872.178647	-14.072601	5.355840
-870.503864	-16.253950	5.365837
-868.444473	-11.592083	5.375834
-866.482742	-10.896687	5.385830
-864.902273	-8.572449	5.395827
-862.852174	-6.855392	5.405824
-860.783569	-15.968083	5.415821
-859.236704	-10.425327	5.425818
-857.297093	-12.776899	5.435814
-855.485026	-13.058615	5.445811
-853.320407	-14.241423	5.455808
-851.727551	-5.922342	5.465805
-849.553801	-8.584495	5.475802
-847.413428	-9.654475	5.485798
-846.025901	-8.853058	5.495795
-844.324858	-7.400709	5.505792
-841.974565	-8.884766	5.515789
-840.318606	-12.599395	5.525786
-838.351576	-11.926927	5.535782
-836.819334	-8.339703	5.545779
-834.762270	-5.464792	5.555776
-832.781659	-9.302366	5.565773
-830.940465	-2.927167	5.575770
-829.072905	-5.808777	5.585766
-827.472362	-6.228763	5.595763
-825.381650	-0.160286	5.605760
-823.161163	-4.301460	5.615757
-821.479346	-6.367060	5.625754
-819.649914	-7.673099	5.635750
-818.133214	-2.272331	5.645747
-815.936368	0.168151	5.655744
-813.968856	-7.909931	5.665741
-812.196304	-1.351639	5.675738
-810.216477	-2.250660	5.685734
-808.299038	-6.676537	5.695731
-806.684856	-4.073437	5.705728
-804.955073	-4.911960	5.715725
-802.545978	0.022494	5.725722
-801.025760	-6.957770	5.735718
-799.153403	-4.187512	5.745715
-797.074449	-9.040247	5.755712
-795.148532	-10.074323	5.765709
-793.047935	-3.470556	5.775706
-791.597647	-9.800164	5.785702
-789.782602	-9.515466	5.795699
-787.971830	-8.851138	5.805696
-785.732426	-7.565321	5.815693
-784.213915	-10.433736	5.825690
-782.277537	-13.534728	5.835686
-780.221357	-4.321755	5.845683
-778.443224	-9.194288	5.855680
-776.527412	-7.989373	5.865677
-774.689040	-3.478406	5.875674
-772.895259	-1.279776	5.885670
-770.600247	-5.349130	5.895667
-769.102743	-6.785237	5.905664
-767.100086	-9.382076	5.915661
-765.302941	-10.896071	5.925658
-763.309689	-2.833544	5.935654
-761.531314	-5.268218	5.945651
-759.843830	-6.117316	5.955648
-757.505617	-2.913059	5.965645
-755.731599	-7.213342	5.975642
-754.300332	-6.170966	5.985638
-752.286434	-8.276960	5.995635
-750.399959	-1.291563	6.005632
-748.368531	-7.783500	6.015629
-746.229949	-3.598382	6.025626
-744.590180	-3.006164	6.035622
-743.126722	-0.249456	6.045619
-740.763481	-1.383380	6.055616
-738.916868	-1.225266	6.065613
-736.829865	-3.309773	6.075610
-735.183276	-1.829693	6.085606
-733.548508	0.416486	6.095603
-731.750403	-5.524994	6.105600
-729.381386	-7.733511	6.115597
-727.686023	-11.296468	6.125594
-726.015204	-11.994458	6.135590
-724.102997	-5.376308	6.145587
-722.114031	-8.261448	6.155584
-719.903783	-5.245124	6.165581
-718.398597	-5.161905	6.175578
-716.891082	-9.806412	6.185574
-714.616607	-9.479813	6.195571
-712.525665	-4.668105	6.205568
-710.951936	-8.906349	6.215565
-708.942906	-8.752061	6.225562
-707.008812	-10.368423	6.235558
-705.159657	-4.741230	6.245555
-703.204269	-6.627834	6.255552
-701.850396	-2.803591	6.265549
-699.674902	-14.105866	6.275546
-697.668705	-5.712192	6.285542
-695.841560	-10.718814	6.295539
-694.097538	-2.655870	6.305536
-692.112654	-12.159264	6.315533
-689.943517	-6.220034	6.325530
-688.221476	-6.463552	6.335526
-686.785783	-6.086577	6.345523
-684.549996	-6.484818	6.355520
-682.484734	-0.078980	6.365517
-680.895098	-3.317119	6.375514
-678.914078	-5.433589	6.385510
-677.050870	-3.305977	6.395507
-675.489014	-3.632837	6.405504
-673.408564	-4.063088	6.415501
-671.398505	-3.357881	6.425498
-669.692601	-3.330387	6.435494
-667.835764	-2.397011	6.445491
-665.749490	-5.326075	6.455488
-663.852040	-6.917601	6.465485
-661.847320	-6.492585	6.475482
-660.342544	-7.220840	6.485478
-658.411223	0.144314	6.495475
-656.404301	-1.411014	6.505472
-654.514501	-3.481309	6.515469
-652.482225	-6.529629	6.525466
-650.688812	-6.118209	6.535462
-648.754635	-4.090335	6.545459
-647.580860	-12.598837	6.555456
-645.525934	-6.829209	6.565453
-643.026829	-3.620542	6.575450
-641.268966	-10.539211	6.585446
-639.592537	-2.088054	6.595443
-637.671425	-0.887029	6.605440
-635.673968	-8.491342	6.615437
-634.112908	-9.313837	6.625434
-632.212703	-0.871585	6.635430
-629.953963	-2.696071	6.645427
-628.236645	-6.857732	6.655424
-626.663318	-6.485342	6.665421
-624.301788	-4.266778	6.675418
-622.478436	-9.331163	6.685414
-621.084604	-0.915367	6.695411
-619.240692	-5.135143	6.705408
-616.843783	-2.282751	6.715405
-614.748261	-8.159561	6.725402
-613.357681	-8.200070	6.735398
-611.630474	-6.135941	6.745395
-609.475518	-6.143829	6.755392
-607.611788	-5.753084	6.765389
-605.659076	-3.816556	6.775386
-603.751272	-9.939682	6.785382
-601.908777	-6.727124	6.795379
-600.430335	-10.721129	6.805376
-598.264976	-10.242775	6.815373
-596.360016	-10.665450	6.825370
-594.574328	-7.203811	6.835366
-592.742264	-12.555355	6.845363
-590.821545	-9.710548	6.855360
-588.867232	-11.045836	6.865357
-587.054176	-10.814348	6.875354
-585.365694	-10.965589	6.885350
-583.432250	-7.581230	6.895347
-581.120460	-7.427831	6.905344
-579.623526	-7.144258	6.915341
-577.552189	-4.953499	6.925338
-575.654798	-6.961788	6.935334
-574.132399	-4.626492	6.945331
-572.101404	-2.604546	6.955328
-569.703743	-8.174322	6.965325
-568.287684	-8.005717	6.975322
-566.639513	-9.366293	6.985318
-564.627712	-8.798642	6.995315
-562.467181	-2.561069	7.005312
-560.857311	-4.750785	7.015309
-558.877938	-7.744788	7.025306
-557.017366	-3.928765	7.035302
-554.896615	-3.574298	7.045299
-553.091739	-8.662525	7.055296
-551.608794	1.016451	7.065293
-549.406714	-0.078910	7.075290
-547.558800	-7.597691	7.085286
-545.724974	-2.332651	7.095283
-544.000476	-5.862245	7.105280
-541.938650	-10.520981	7.115277
-540.323901	-9.888308	7.125274
-538.312682	-7.825279	7.135270
-536.274754	-4.402306	7.145267
-534.648645	-8.587229	7.155264
-532.690469	-9.585194	7.165261
-530.585677	-11.486049	7.175258
-528.679305	-10.091529	7.185254
-526.846269	-10.600554	7.195251
-525.354053	-7.139353	7.205248
-523.357540	-8.252382	7.215245
-521.483027	-12.500656	7.225242
-519.246050	-6.709463	7.235238
-517.403691	-7.625759	7.245235
-515.670067	-10.897843	7.255232
-514.096356	-12.732806	7.265229
-512.273359	-2.637591	7.275226
-509.956797	-6.572779	7.285222
-508.114722	-3.172182	7.295219
-506.590430	-2.509248	7.305216
-504.205128	-4.740673	7.315213
-502.389184	-5.872213	7.325210
-500.834749	-7.759352	7.335206
-498.841100	-2.736115	7.345203
-496.786472	-1.556299	7.355200
-495.031572	-5.921241	7.365197
-493.327346	-7.224404	7.375194
-491.075631	-9.510270	7.385190
-489.550507	-3.660617	7.395187
-487.571987	-8.643900	7.405184
-485.898310	-5.311128	7.415181
-483.813114	-4.652498	7.425178
-481.781180	-4.381676	7.435174
-480.109524	-12.625416	7.445171
-478.371426	-9.634506	7.455168
-476.170956	-10.109017	7.465165
-474.384128	-7.106939	7.475162
-472.607526	-7.016383	7.485158
-470.908222	-7.796114	7.495155
-468.486860	-7.121684	7.505152
-466.781485	-14.560800	7.515149
-465.242403	-13.447044	7.525146
-463.135143	-1.458236	7.535142
-461.330695	-2.752119	7.545139
-459.432214	-3.855756	7.555136
-457.787370	-4.243095	7.565133
-455.607588	-3.586914	7.575130
-453.751611	-7.792706	7.585126
-451.969163	-5.067805	7.595123
-450.036631	-3.453186	7.605120
-448.347985	-2.398040	7.615117
-446.238117	-3.784897	7.625114
-444.182498	-2.854667	7.635110
-442.535948	-7.994902	7.645107
-440.707084	-0.354244	7.655104
-438.996258	-3.207372	7.665101
-436.617646	-4.504505	7.675098
-434.732454	-5.836526	7.685094
-433.442474	-6.729286	7.695091
-431.584183	-0.438583	7.705088
-429.396665	-4.694143	7.715085
-427.364233	-2.667563	7.725082
-425.602003	-4.431521	7.735078
-423.867526	-5.925783	7.745075
-421.953204	-5.610866	7.755072
-420.008452	-9.541861	7.765069
-418.090076	-11.592852	7.775066
-416.138166	-9.063932	7.785062
-414.492380	-8.824550	7.795059
-412.342438	0.004337	7.805056
-410.616290	-2.134375	7.815053
-408.603774	-1.471969	7.825050
-406.718259	-5.144022	7.835046
-405.427756	-3.952639	7.845043
-403.466946	2.598035	7.855040
-401.266860	4.612080	7.865037
-399.380967	-8.083723	7.875034
-397.348663	-0.238670	7.885030
-395.423810	0.699851	7.895027
-393.630449	-3.296952	7.905024
-392.104960	0.031131	7.915021
-390.098257	-6.061842	7.925018
-387.873196	-0.952297	7.935014
-386.469142	-4.215881	7.945011
-384.341888	-7.062830	7.955008
-382.735269	-1.008219	7.965005
-380.354988	-8.209253	7.975002
-378.748367	-7.005171	7.984998
-377.132001	-3.311062	7.994995
-374.776963	0.820900	8.004992
-373.120641	0.646523	8.014989
-371.277637	-1.823452	8.024986
-369.391058	-3.836171	8.034982
-367.451362	2.302643	8.044979
-365.643819	2.003074	8.054976
-363.819766	-8.507039	8.064973
-361.768832	-4.673880	8.074970
-359.851241	-3.017328	8.084966
-357.927202	-0.014959	8.094963
-356.173071	-6.553897	8.104960
-354.334578	-4.291027	8.114957
-352.388071	-9.365410	8.124954
-351.052939	0.078363	8.134950
-349.005858	7.591107	8.144947
-346.826821	1.038018	8.154944
-344.720391	-2.512943	8.164941
-342.930571	-2.560191	8.174938
-341.096537	0.587614	8.184934
-339.304801	-2.287837	8.194931
-337.633370	2.396986	8.204928
-335.761165	-4.181316	8.214925
-333.862322	1.840891	8.224922
-331.613441	-3.081224	8.234918
-329.981508	2.520965	8.244915
-327.916279	2.725024	8.254912
-326.133208	-0.287983	8.264909
-324.666356	-0.468395	8.274906
-322.583928	-1.580764	8.284902
-320.631323	-2.876090	8.294899
-318.618799	-1.368870	8.304896
-316.855483	4.815515	8.314893
-314.830433	-10.106662	8.324890
-312.920879	2.300706	8.334886
-311.240537	3.840436	8.344883
-309.308058	1.288328	8.354880
-307.511231	3.663678	8.364877
-305.515682	5.344147	8.374874
-303.619242	3.359903	8.384870
-301.900685	2.572480	8.394867
-299.765060	0.191636	8.404864
-298.225255	3.176444	8.414861
-296.373231	-3.985979	8.424858
-294.395752	-1.754721	8.434854
-292.414494	2.181203	8.444851
-290.439590	-2.676615	8.454848
-288.757809	-5.346583	8.464845
-286.649164	-4.693102	8.474842
-285.103608	-5.263422	8.484838
-283.130997	0.904947	8.494835
-281.119629	1.338698	8.504832
-279.069358	0.741500	8.514829
-277.692831	0.310271	8.524826
-275.293428	-7.135300	8.534822
-273.684966	-0.619849	8.544819
-271.888649	3.265088	8.554816
-270.236152	4.689292	8.564813
-268.293365	4.666630	8.574810
-265.853397	0.048808	8.584807
-264.325551	0.821858	8.594803
-262.469983	7.479458	8.604800
-260.533577	0.058852	8.614797
-258.275059	0.898437	8.624794
-257.064571	3.618467	8.634791
-255.104026	0.381393	8.644787
-252.724675	3.003281	8.654784
-251.088674	6.386453	8.664781
-249.538874	3.710734	8.674778
-247.311191	-0.168974	8.684775
-245.707171	0.047191	8.694771
-243.612780	3.635100	8.704768
-241.974339	-0.202660	8.714765
-239.763098	1.317121	8.724762
-237.853430	2.888196	8.734759
-236.174113	-6.117678	8.744755
-234.275823	-0.775826	8.754752
-232.535036	0.609049	8.764749
-230.431622	-7.926086	8.774746
-228.791272	-7.019391	8.784743
-226.504318	-4.100099	8.794739
-224.994211	-2.858402	8.804736
-223.026278	-6.715578	8.814733
-221.187023	-8.951158	8.824730
-219.261877	1.603278	8.834727
-217.224119	-6.911895	8.844723
-215.133721	-15.067567	8.854720
-213.609103	-12.211334	8.864717
-211.694281	-11.716328	8.874714
-209.857152	-11.723659	8.884711
-208.053590	-7.645621	8.894707
-206.219342	-10.601971	8.904704
-204.132175	-6.209190	8.914701
-202.455723	-12.692996	8.924698
-200.517697	-11.383787	8.934695
-198.642736	-13.037678	8.944691
-196.787843	-12.582044	8.954688
-194.895967	-5.287553	8.964685
-192.954989	-10.747776	8.974682
-191.075337	-3.331330	8.984679
-189.352171	-1.492031	8.994675
-187.577727	-9.546736	9.004672
-185.356009	-7.739628	9.014669
-183.477691	-10.458257	9.024666
-181.820020	-10.269559	9.034663
-179.919729	-14.169590	9.044659
-178.090822	-9.677151	9.054656
-176.313862	-11.459071	9.064653
-174.200329	-9.333109	9.074650
-172.147592	-7.457969	9.084647
-170.154504	-10.040166	9.094643
-168.653236	-9.218604	9.104640
-166.952883	-15.502516	9.114637
-164.677151	-18.608234	9.124634
-162.877921	-15.658421	9.134631
-161.178525	-10.521615	9.144627
-159.451855	-8.472854	9.154624
-157.641248	-12.794348	9.164621
-155.349536	-6.594682	9.174618
-153.473325	-11.640329	9.184615
-151.707444	-13.390463	9.194611
-150.143855	-14.247787	9.204608
-147.903887	-10.793551	9.214605
-146.230777	-11.139400	9.224602
-144.173343	-8.330246	9.234599
-142.363734	-7.126814	9.244595
-140.494683	-10.906568	9.254592
-138.537355	-10.353549	9.264589
-136.512681	-8.262321	9.274586
-134.674261	-6.180846	9.284583
-133.240511	-13.385359	9.294579
-131.301096	-6.485243	9.304576
-129.198885	-9.536400	9.314573
-127.202175	-11.700718	9.324570
-125.465473	-11.854592	9.334567
-123.602056	-11.668683	9.344563
-121.522722	-11.924594	9.354560
-119.613298	-7.399165	9.364557
-118.031254	-12.222585	9.374554
-116.362705	-11.250838	9.384551
-114.071967	-6.192559	9.394547
-112.277249	-1.531976	9.404544
-110.313777	-8.424682	9.414541
-108.612748	-10.904967	9.424538
-106.748027	-7.405030	9.434535
-105.066339	-6.400634	9.444531
-102.992593	-0.216662	9.454528
-101.144384	-1.168314	9.464525
-99.104411	-5.365311	9.474522
-97.116517	-9.514523	9.484519
-95.700217	-5.695135	9.494515
-93.529330	-8.381429	9.504512
-91.448876	-0.990617	9.514509
-89.804037	-1.811918	9.524506
-87.764139	-8.097851	9.534503
-86.035207	-0.630424	9.544499
-84.261287	0.359272	9.554496
-82.299750	-1.744136	9.564493
-80.517307	-3.727390	9.574490
-78.716415	-8.966231	9.584487
-76.785387	-7.880016	9.594483
-74.760921	-10.212932	9.604480
-72.730522	-6.690451	9.614477
-71.211450	-4.047976	9.624474
-69.368065	-10.586753	9.634471
-67.177158	-3.493016	9.644467
-65.171869	-7.378135	9.654464
-63.599043	-8.356878	9.664461
-61.705112	-11.160013	9.674458
-59.747468	-9.328027	9.684455
-57.984896	-11.579674	9.694451
-56.198587	-10.295092	9.704448
-53.978014	-2.187648	9.714445
-52.404922	-4.601697	9.724442
-50.536669	-7.725992	9.734439
-48.516644	-8.891330	9.744435
-46.481412	0.248326	9.754432
-44.791251	-7.964949	9.764429
-42.887713	-6.418003	9.774426
-41.014871	-10.125657	9.784423
-39.063486	-9.451609	9.794419
-37.527098	-6.559241	9.804416
-35.408329	-6.552947	9.814413
-33.416630	-6.393748	9.824410
-31.426984	-5.547374	9.834407
-29.646336	-12.415591	9.844403
-28.055553	-2.958704	9.854400
-26.127818	-4.404567	9.864397
-24.001006	-2.740063	9.874394
-22.547442	-3.623966	9.884391
-20.682974	-6.548687	9.894387
-18.542932	-1.358902	9.904384
-16.739225	-7.128680	9.914381
-14.373037	-7.690785	9.924378
-12.771486	-9.337239	9.934375
-11.108331	-1.895577	9.944371
-9.088866	-0.074988	9.954368
-7.135751	-6.250700	9.964365
-5.671621	6.745906	9.974362
-4.153820	29.746143	9.984359
-2.887926	61.843529	9.994355
-1.503233	112.604383	10.004352
0.000000	140.470627	10.009357
0.288921	182.418886	10.014362
1.170162	205.514840	10.019367
1.627540	222.662331	10.024371
1.908682	244.363840	10.029376
2.469440	256.450175	10.034381
2.535789	275.814237	10.039386
2.845524	273.911933	10.044391
2.686671	275.899057	10.049395
2.763338	279.629010	10.054400
3.122174	288.360254	10.059405
2.672109	290.422216	10.064410
3.288179	304.966149	10.069415
3.664157	313.604787	10.074419
3.595172	307.583914	10.079424
3.461337	296.309464	10.084429
3.191492	300.105732	10.089434
3.703069	295.528229	10.094439
3.566225	294.972924	10.099443
3.657839	298.238446	10.104448
3.767533	301.220383	10.109453
3.491229	304.945142	10.114458
3.689652	305.342466	10.119463
3.593256	310.046214	10.124467
3.579317	310.578338	10.129472
3.960050	304.621353	10.134477
3.419523	314.352363	10.139482
3.723806	315.784642	10.144487
3.652118	311.394788	10.149491
3.511792	314.883392	10.154496
3.637244	311.241116	10.159501
3.759027	326.713901	10.164506
3.902114	338.250331	10.169511
4.190769	338.718420	10.174515
4.542001	344.188153	10.179520
4.369801	334.354838	10.184525
3.750242	328.278273	10.189530
4.147626	338.988809	10.194535
4.385359	351.301793	10.199539
4.232096	346.048142	10.204544
4.530804	351.001122	10.209549
4.332313	361.286319	10.214554
4.358667	356.221636	10.219559
4.540074	362.686727	10.224563
4.531688	357.271189	10.229568
4.595414	351.035162	10.234573
4.534761	364.428671	10.239578
4.608833	362.234359	10.244583
4.672480	365.977450	10.249587
4.468973	369.074015	10.254592
4.672211	364.643446	10.259597
4.940206	369.306437	10.264602
4.931852	368.771635	10.269607
4.567052	368.560198	10.274611
4.777732	370.105186	10.279616
4.953714	365.074982	10.284621
4.881840	370.823528	10.289626
4.980862	371.492179	10.294631
5.094005	375.411884	10.299635
5.271606	396.270683	10.304640
5.607158	388.535729	10.309645
5.340990	384.290416	10.314650
5.411577	377.518688	10.319655
5.280337	375.863332	10.324659
5.363044	385.231623	10.329664
5.324002	380.669381	10.334669
5.431871	397.508548	10.339674
5.657225	408.863175	10.344679
5.702051	406.619903	10.349683
5.722789	407.599093	10.354688
6.026626	406.019418	10.359693
5.517145	399.505787	10.364698
5.688699	399.953132	10.369703
5.767460	404.211072	10.374707
5.674727	410.756182	10.379712
5.954079	413.003016	10.384717
5.642954	425.116599	10.389722
5.422307	418.443346	10.394727
5.833247	423.411566	10.399731
5.839238	423.322338	10.404736
5.945838	423.600268	10.409741
5.811208	427.081682	10.414746
6.093345	421.411618	10.419751
6.140195	429.656538	10.424755
6.146788	448.372759	10.429760
6.350704	446.615049	10.434765
6.047126	455.918842	10.439770
6.330063	460.128461	10.444775
6.702659	452.955280	10.449779
6.562608	462.184107	10.454784
6.749911	457.256147	10.459789
6.672524	466.427672	10.464794
6.851002	452.688915	10.469799
6.760730	469.059865	10.474803
6.583430	460.788496	10.479808
7.068099	453.868681	10.484813
6.626090	465.884900	10.489818
6.929072	463.138385	10.494823
6.848347	463.812057	10.499827
6.152756	464.473414	10.504832
6.692498	465.298859	10.509837
6.768828	464.613348	10.514842
6.933062	463.831813	10.519847
6.904502	466.799567	10.524851
6.970114	490.980155	10.529856
7.465811	493.233496	10.534861
7.365263	504.223856	10.539866
7.352771	484.078250	10.544871
7.162469	485.646207	10.549875
7.253405	497.336165	10.554880
7.415657	498.325906	10.559885
7.356996	505.002822	10.564890
7.855296	502.080062	10.569895
7.585010	501.602805	10.574899
7.775530	515.216593	10.579904
8.079106	505.414509	10.584909
7.777572	498.058667	10.589914
7.580296	485.546788	10.594919
7.855393	489.316109	10.599923
7.484574	508.070528	10.604928
7.865304	504.598803	10.609933
7.755282	508.994121	10.614938
7.728665	509.017329	10.619943
7.805252	510.410251	10.624947
7.918863	517.319898	10.629952
7.894252	504.446139	10.634957
7.788958	511.535783	10.639962
7.905511	523.847743	10.644967
8.167045	517.360891	10.649971
8.153694	526.861294	10.654976
8.376455	532.293241	10.659981
8.118546	536.475607	10.664986
8.472712	546.142911	10.669991
8.278248	547.853469	10.674995
8.273211	545.988724	10.680000
8.797766	547.655559	10.685005
8.443951	549.268528	10.690010
8.529909	545.088430	10.695015
8.771919	543.539104	10.700019
8.698121	553.432375	10.705024
8.938305	549.719699	10.710029
8.773632	558.048895	10.715034
8.801705	554.078306	10.720039
9.016215	549.831969	10.725043
8.779846	557.112858	10.730048
9.097820	550.145467	10.735053
8.673095	544.589681	10.740058
8.837192	548.947595	10.745063
8.926464	553.303253	10.750067
8.927018	555.290220	10.755072
9.053850	547.099605	10.760077
8.860133	560.000418	10.765082
9.048516	559.601391	10.770087
9.107356	573.095884	10.775091
9.156176	583.287383	10.780096
9.349538	583.972538	10.785101
9.375938	594.860713	10.790106
9.502197	601.095003	10.795111
9.548391	595.547664	10.800115
9.986300	591.713550	10.805120
10.236164	585.662205	10.810125
9.866709	593.713416	10.815130
10.108823	573.524709	10.820135
9.766700	569.740901	10.825139
9.532633	563.673711	10.830144
9.626772	549.563528	10.835149
9.753154	581.491036	10.840154
9.803590	579.376157	10.845159
10.372798	591.034060	10.850163
9.891793	588.177598	10.855168
10.018655	582.407656	10.860173
9.861059	589.871545	10.865178
10.057963	585.191177	10.870183
10.312991	583.639770	10.875187
10.106333	598.890835	10.880192
10.040865	590.000717	10.885197
10.099718	602.243097	10.890202
10.024478	598.300014	10.895207
10.238256	598.863638	10.900211
10.182708	604.518205	10.905216
10.368258	587.466487	10.910221
10.277073	610.145747	10.915226
10.548519	629.315136	10.920231
10.728231	626.039455	10.925235
10.863672	624.524465	10.930240
10.884618	627.656249	10.935245
10.900217	637.656748	10.940250
11.129551	631.905136	10.945255
10.776745	620.889294	10.950259
10.389023	615.947340	10.955264
10.691506	629.991247	10.960269
10.824710	629.402316	10.965274
10.979876	631.276320	10.970279
11.003706	628.806120	10.975283
10.647993	636.982900	10.980288
10.996025	626.378833	10.985293
11.148417	625.061419	10.990298
11.182433	634.268899	10.995303
10.985094	636.631229	11.000307
10.982450	639.766778	11.005312
11.681841	647.666457	11.010317
11.699198	661.166072	11.015322
11.180158	643.222119	11.020327
11.678362	650.325961	11.025331
11.187107	665.458482	11.030336
11.703090	664.109880	11.035341
11.572591	662.555301	11.040346
11.853158	662.980536	11.045351
12.008652	656.964715	11.050355
11.571291	658.215694	11.055360
12.203848	658.936458	11.060365
11.779502	670.043247	11.065370
11.872059	662.029929	11.070375
12.300178	657.020912	11.075379
12.185905	655.528403	11.080384
11.839991	638.995072	11.085389
11.847800	647.241612	11.090394
12.126733	660.002467	11.095399
12.194769	663.262370	11.100403
12.130106	660.544496	11.105408
12.331203	655.678926	11.110413
11.971284	666.526269	11.115418
12.209321	663.611874	11.120423
12.359607	666.719882	11.125427
12.330691	664.064117	11.130432
12.497420	659.511545	11.135437
12.510094	662.852821	11.140442
12.387604	660.252984	11.145447
12.539157	656.511839	11.150451
12.533362	660.724992	11.155456
12.669607	660.460440	11.160461
12.399455	660.997172	11.165466
12.591154	670.371918	11.170471
12.496765	679.418552	11.175475
12.855695	689.280742	11.180480
12.904511	692.086384	11.185485
12.972743	688.888397	11.190490
13.374761	690.156887	11.195495
13.396723	694.214230	11.200499
12.973039	695.686965	11.205504
13.289823	696.699382	11.210509
13.301896	686.163051	11.215514
13.141265	679.732425	11.220519
13.229690	680.445362	11.225523
13.380699	696.016386	11.230528
13.455174	689.521446	11.235533
13.668567	690.676515	11.240538
12.998215	677.689548	11.245543
13.291875	679.230797	11.250547
13.262303	683.730034	11.255552
13.462389	691.490174	11.260557
13.747511	696.111115	11.265562
13.662057	702.710390	11.270567
13.528094	701.471762	11.275571
13.651897	701.575060	11.280576
13.557110	693.970090	11.285581
13.410852	701.501616	11.290586
13.450057	702.848478	11.295591
13.772865	705.826471	11.300595
13.496533	719.420295	11.305600
14.038911	718.761366	11.310605
14.011436	732.406976	11.315610
13.756652	730.605697	11.320615
14.327955	730.489378	11.325619
13.879826	730.791139	11.330624
14.525473	732.645272	11.335629
14.305478	737.285290	11.340634
13.988431	732.462915	11.345639
14.243312	726.215162	11.350643
13.897472	737.905593	11.355648
13.905518	729.773248	11.360653
13.828772	741.665198	11.365658
14.257564	755.364215	11.370663
14.645639	748.186844	11.375667
14.576176	756.437886	11.380672
14.917003	750.603786	11.385677
14.999369	749.407923	11.390682
14.975758	747.339524	11.395687
15.165171	749.091382	11.400691
14.789250	757.060131	11.405696
15.175890	755.757384	11.410701
14.961730	749.090828	11.415706
14.985618	750.230394	11.420711
15.241794	751.881713	11.425715
14.855974	762.525091	11.430720
14.882002	751.795668	11.435725
14.854826	760.058891	11.440730
14.749108	759.156389	11.445735
15.341781	753.780456	11.450739
15.145731	757.877321	11.455744
15.268837	743.017976	11.460749
15.260639	750.871297	11.465754
15.006828	758.683369	11.470759
15.331857	759.533620	11.475763
15.093406	761.325337	11.480768
15.473855	765.707159	11.485773
15.683296	785.178393	11.490778
15.751095	786.336191	11.495783
16.031074	779.038846	11.500787
15.954749	777.966067	11.505792
15.651712	761.769548	11.510797
15.670984	764.972594	11.515802
15.855989	773.405417	11.520807
16.060732	779.045345	11.525811
15.977723	788.099693	11.530816
16.342555	774.245750	11.535821
15.966332	758.018328	11.540826
15.775846	773.402620	11.545831
16.255321	780.566288	11.550835
16.097465	783.482186	11.555840
16.288972	773.437590	11.560845
16.437195	773.516492	11.565850
16.302341	784.714394	11.570855
16.462269	776.918936	11.575859
16.226417	782.163919	11.580864
16.348957	778.022076	11.585869
16.237328	792.236277	11.590874
15.930747	791.266458	11.595879
16.484148	786.246877	11.600883
16.172044	788.714272	11.605888
16.088912	790.561648	11.610893
16.608174	792.901170	11.615898
16.717366	805.287087	11.620903
17.269760	805.495498	11.625907
16.706211	808.122856	11.630912
16.894199	791.087858	11.635917
16.707833	791.600191	11.640922
16.549641	808.581625	11.645927
16.944471	813.363309	11.650931
17.092830	828.026531	11.655936
16.996123	823.328261	11.660941
17.094648	822.298555	11.665946
17.297445	817.333309	11.670951
17.336323	815.478871	11.675955
17.328237	817.000452	11.680960
17.620099	808.956841	11.685965
17.271513	821.098805	11.690970
17.443315	817.496322	11.695975
17.605957	815.448671	11.700979
17.141119	821.332616	11.705984
17.687533	818.279113	11.710989
17.628991	808.747484	11.715994
17.455384	810.877387	11.720999
17.917497	814.777822	11.726003
17.711190	820.853930	11.731008
17.728610	814.541509	11.736013
17.775014	816.073322	11.741018
17.612650	818.423794	11.746023
18.062122	804.504280	11.751027
17.825222	819.960683	11.756032
17.871291	815.838912	11.761037
17.783868	824.185901	11.766042
17.393983	821.258084	11.771047
17.529159	825.086084	11.776051
17.475568	838.863698	11.781056
18.047251	840.660255	11.786061
18.048206	846.969834	11.791066
18.114899	855.967229	11.796071
18.023856	856.241998	11.801075
17.873971	850.774725	11.806080
17.893645	843.510982	11.811085
18.370679	854.384248	11.816090
18.397919	866.467882	11.821095
19.027328	862.147394	11.826099
18.712009	869.477302	11.831104
18.845164	848.024256	11.836109
18.575987	849.529134	11.841114
18.638494	848.847388	11.846119
18.777535	848.054082	11.851123
18.587463	854.178079	11.856128
18.867959	865.823907	11.861133
19.165584	863.843033	11.866138
18.813694	862.497217	11.871143
18.837655	856.133269	11.876147
18.827938	872.450822	11.881152
19.239151	869.674353	11.886157
19.106285	869.228782	11.891162
18.939635	878.069434	11.896167
19.279648	874.719242	11.901171
19.252337	879.487851	11.906176
19.148056	875.170837	11.911181
19.179586	875.825045	11.916186
19.372559	874.657264	11.921191
19.467584	866.608745	11.926195
19.210327	875.932226	11.931200
19.162134	869.206024	11.936205
19.435722	869.137192	11.941210
19.247743	873.321115	11.946215
19.363379	863.622888	11.951219
19.225719	882.766398	11.956224
19.500069	892.634334	11.961229
19.833851	892.565364	11.966234
19.839819	893.744072	11.971239
20.356737	887.333024	11.976243
19.815430	894.446664	11.981248
20.315254	897.913731	11.986253
20.015500	881.656626	11.991258
19.802297	887.084124	11.996263
20.198390	891.200125	12.001267
19.936966	894.511052	12.006272
20.170523	895.940480	12.011277
20.401638	893.676883	12.016282
20.131667	891.450629	12.021287
20.480539	879.611427	12.026291
20.225777	870.361802	12.031296
20.131644	871.619556	12.036301
20.284364	875.982539	12.041306
20.043364	882.855877	12.046311
20.366869	867.548104	12.051315
20.405653	874.465126	12.056320
20.264074	872.431296	12.061325
20.368714	870.768223	12.066330
20.488900	868.965468	12.071335
20.494095	871.316032	12.076339
20.529755	873.108199	12.081344
20.171805	872.312156	12.086349
20.466662	870.831642	12.091354
19.904726	862.369068	12.096359
20.243253	851.413099	12.101363
19.963531	852.869195	12.106368
19.974765	859.626593	12.111373
20.173055	871.354927	12.116378
20.114571	882.685810	12.121383
20.403100	867.377308	12.126387
20.132482	874.758440	12.131392
20.259921	857.037551	12.136397
20.512773	841.556562	12.141402
20.007412	850.899098	12.146407
20.538458	841.569889	12.151411
20.110115	853.764027	12.156416
20.299835	850.131868	12.161421
19.994527	847.220519	12.166426
20.212534	853.724150	12.171431
20.287255	845.629993	12.176435
20.112649	854.199074	12.181440
19.959022	844.537499	12.186445
20.303988	843.545760	12.191450
20.340195	840.811763	12.196455
20.500276	840.183843	12.201459
20.011006	851.026721	12.206464
19.970019	845.706091	12.211469
20.185513	849.855617	12.216474
20.006089	852.167813	12.221479
20.333789	850.223147	12.226483
20.166226	855.515614	12.231488
20.106788	851.036905	12.236493
20.355073	843.708312	12.241498
20.305246	854.246124	12.246503
20.211617	843.647687	12.251507
20.424211	853.424517	12.256512
20.491088	849.819837	12.261517
20.292248	860.597474	12.266522
19.897644	854.950024	12.271527
20.557004	842.233389	12.276531
20.346127	834.276259	12.281536
20.350321	830.747817	12.286541
20.252273	826.844581	12.291546
20.147668	819.319961	12.296551
20.251765	828.338183	12.301555
20.457972	834.234955	12.306560
20.035814	822.269609	12.311565
20.198975	823.137797	12.316570
19.983441	823.470271	12.321575
19.936712	825.616210	12.326579
20.038465	825.861805	12.331584
19.599989	827.530886	12.336589
19.875960	820.155309	12.341594
20.088783	848.069491	12.346599
20.089938	849.146456	12.351603
20.093879	855.862436	12.356608
20.558306	850.107936	12.361613
20.173144	828.920525	12.366618
19.781532	839.689468	12.371623
20.254479	843.209697	12.376627
20.149623	837.296832	12.381632
20.024770	833.336365	12.386637
20.298590	836.617104	12.391642
19.837288	833.431003	12.396647
20.198776	851.772579	12.401651
20.296298	859.661138	12.406656
20.333673	850.227728	12.411661
20.191126	831.173187	12.416666
19.679608	844.916609	12.421671
20.230164	845.462799	12.426675
20.318867	856.853769	12.431680
20.172272	843.932929	12.436685
20.075948	834.952960	12.441690
20.103832	833.735816	12.446695
20.241961	831.862392	12.451699
20.072513	836.313020	12.456704
19.920683	843.648380	12.461709
20.218613	848.603234	12.466714
20.121340	857.082708	12.471719
20.686446	846.678836	12.476723
20.396426	837.855922	12.481728
20.067596	833.609430	12.486733
20.368575	821.620211	12.491738
20.087562	837.356494	12.496743
20.156801	830.173165	12.501747
20.115716	838.558506	12.506752
20.356173	830.765945	12.511757
20.066670	837.183352	12.516762
19.905101	835.859224	12.521767
20.173247	839.107751	12.526771
20.281839	838.850760	12.531776
20.196376	834.366745	12.536781
19.941757	829.830860	12.541786
19.854542	834.164288	12.546791
20.237403	827.516015	12.551795
20.253950	829.921535	12.556800
20.059932	834.626829	12.561805
20.288734	829.703164	12.566810
19.950300	833.847993	12.571815
20.328849	834.965692	12.576819
20.250543	825.799920	12.581824
20.031773	828.569417	12.586829
20.537307	827.083691	12.591834
20.180850	837.582085	12.596839
20.504401	832.064537	12.601843
19.926154	842.153588	12.606848
19.849602	838.956583	12.611853
20.252884	839.575151	12.616858
20.105434	842.738571	12.621863
20.066804	835.078835	12.626867
20.092024	842.829100	12.631872
20.237677	830.787374	12.636877
20.078323	838.429874	12.641882
20.343766	840.846162	12.646887
20.287940	835.824383	12.651891
20.162108	840.742742	12.656896
20.070840	841.356608	12.661901
20.541226	837.665493	12.666906
20.207494	844.542565	12.671911
20.171552	840.205198	12.676915
20.249772	848.992583	12.681920
20.093846	853.907860	12.686925
20.399258	842.596041	12.691930
20.259940	856.855724	12.696935
20.637188	845.158688	12.701939
20.289682	827.305421	12.706944
19.902629	828.702936	12.711949
20.223035	813.159161	12.716954
19.967758	823.179338	12.721959
20.081963	818.114675	12.726963
20.061900	829.155524	12.731968
19.777365	823.115198	12.736973
20.248073	830.026388	12.741978
19.981675	837.176582	12.746983
20.023722	850.241907	12.751987
19.946662	849.047808	12.756992
20.033119	855.214436	12.761997
20.341079	854.832601	12.767002
20.168841	848.720734	12.772007
20.209282	848.198633	12.777011
20.236181	847.241855	12.782016
20.042183	850.683951	12.787021
20.453285	839.454629	12.792026
20.188458	849.153056	12.797031
20.176374	824.689005	12.802035
20.259250	815.330366	12.807040
19.821781	821.634165	12.812045
20.076802	834.909946	12.817050
20.070358	846.268772	12.822055
20.276789	846.895083	12.827059
20.179567	849.135816	12.832064
20.206519	840.703912	12.837069
20.013512	831.553277	12.842074
20.002259	850.197166	12.847079
20.179337	844.769211	12.852083
20.196907	843.157877	12.857088
20.065112	852.180620	12.862093
20.440993	848.715898	12.867098
19.903882	843.310390	12.872103
20.289913	847.882168	12.877107
20.095460	848.316941	12.882112
20.075492	839.495109	12.887117
20.241708	828.339550	12.892122
20.005505	825.480263	12.897127
20.278076	824.490610	12.902131
20.168200	832.345999	12.907136
19.910821	833.226068	12.912141
19.992896	841.102888	12.917146
19.930464	851.019781	12.922151
20.252792	855.981787	12.927155
20.241852	855.665010	12.932160
20.308981	855.376783	12.937165
20.245871	852.764286	12.942170
19.780965	850.110216	12.947175
20.283791	850.260299	12.952179
20.097280	853.450453	12.957184
20.324714	860.460388	12.962189
20.432383	836.953398	12.967194
20.192707	830.729286	12.972199
20.323271	824.294729	12.977203
20.185881	827.005512	12.982208
20.147037	825.832130	12.987213
20.368544	822.103441	12.992218
20.294976	831.638880	12.997223
20.295798	823.360971	13.002227
20.341444	829.740688	13.007232
19.860954	838.374318	13.012237
20.357062	827.752796	13.017242
20.425827	829.915010	13.022247
19.924305	830.975952	13.027251
19.939621	831.547585	13.032256
20.085162	833.232330	13.037261
20.390671	826.703634	13.042266
20.157850	845.833887	13.047271
20.482692	828.499460	13.052275
20.369102	832.122700	13.057280
20.248584	838.849062	13.062285
20.268767	832.047313	13.067290
20.100245	830.166027	13.072295
20.319629	837.047917	13.077299
20.046961	841.373078	13.082304
19.913627	835.474218	13.087309
20.400982	836.882084	13.092314
20.188490	847.395371	13.097319
20.040076	837.229898	13.102323
20.240228	838.743499	13.107328
20.101045	844.171792	13.112333
20.270772	833.859378	13.117338
19.892493	837.985331	13.122343
20.255325	837.036476	13.127347
20.197627	833.618835	13.132352
19.957508	835.459715	13.137357
20.341745	834.122652	13.142362
20.080452	839.699735	13.147367
20.391084	826.642902	13.152371
20.353544	811.168837	13.157376
19.916322	810.935823	13.162381
19.987453	810.746312	13.167386
20.130643	822.153796	13.172391
20.407401	819.750459	13.177395
20.252778	806.668499	13.182400
19.681527	806.158806	13.187405
20.081051	814.934347	13.192410
19.982350	839.135417	13.197415
20.067202	831.711466	13.202419
20.504396	832.710996	13.207424
20.169307	829.320253	13.212429
20.417424	813.620842	13.217434
19.959374	815.367164	13.222439
20.297735	807.126894	13.227443
19.833620	806.972290	13.232448
19.962543	819.044397	13.237453
20.385912	817.574932	13.242458
20.086243	815.977929	13.247463
20.151122	809.238450	13.252467
20.181828	814.838340	13.257472
19.864178	818.301727	13.262477
19.931782	829.617190	13.267482
19.869850	840.010258	13.272487
20.323899	827.794760	13.277491
20.130762	841.025328	13.282496
20.077537	844.386619	13.287501
20.484637	834.290246	13.292506
20.250699	832.928774	13.297511
20.141016	831.864465	13.302515
20.322532	830.804175	13.307520
19.957301	825.019582	13.312525
20.153675	813.770910	13.317530
20.010253	820.691736	13.322535
20.316425	831.644280	13.327539
20.251569	829.213424	13.332544
19.884592	835.933361	13.337549
20.300358	827.496221	13.342554
20.071186	826.307462	13.347559
20.190239	821.292490	13.352563
20.053128	819.884034	13.357568
19.955989	834.321480	13.362573
20.422784	834.838449	13.367578
20.073205	833.684665	13.372583
20.066099	820.164406	13.377587
19.862574	824.484841	13.382592
19.920287	844.625361	13.387597
20.537381	841.719861	13.392602
20.316173	839.556804	13.397607
20.102049	836.518943	13.402611
20.310578	826.572525	13.407616
20.490908	831.006788	13.412621
20.046368	823.375530	13.417626
19.877787	820.350910	13.422631
19.787321	820.981995	13.427635
20.100655	822.315108	13.432640
19.943072	839.600848	13.437645
20.445403	844.199809	13.442650
20.386663	842.360938	13.447655
19.811996	829.771752	13.452659
20.264417	829.882564	13.457664
20.154353	836.791769	13.462669
20.147965	835.739371	13.467674
20.172737	820.752121	13.472679
20.002196	824.393906	13.477683
20.194797	832.418680	13.482688
20.065169	844.320726	13.487693
20.457642	840.366057	13.492698
20.303762	824.926305	13.497703
20.145476	817.394478	13.502707
20.258624	816.397136	13.507712
19.881297	826.474631	13.512717
20.118351	817.674898	13.517722
20.051094	827.508963	13.522727
20.224605	821.323036	13.527731
20.410129	812.955746	13.532736
20.039677	818.778901	13.537741
20.020413	812.587454	13.542746
20.171033	812.738518	13.547751
20.042211	820.954908	13.552755
20.098267	817.724140	13.557760
20.209073	816.577354	13.562765
20.155548	820.394448	13.567770
19.968166	824.904706	13.572775
19.983383	821.929622	13.577779
20.203871	822.208320	13.582784
20.195354	830.545882	13.587789
20.145516	830.008218	13.592794
20.070700	832.808374	13.597799
20.261288	826.629183	13.602803
20.233642	826.975846	13.607808
19.967134	826.896961	13.612813
20.230147	820.669949	13.617818
19.916487	824.250979	13.622823
20.033534	818.577130	13.627827
20.489013	823.915297	13.632832
20.241255	829.934940	13.637837
20.122438	816.829912	13.642842
20.381222	825.637370	13.647847
20.436933	813.070662	13.652851
20.395146	811.426219	13.657856
20.241884	828.326462	13.662861
20.340788	827.959048	13.667866
20.085690	837.706380	13.672871
19.777900	834.858510	13.677875
20.350784	824.991180	13.682880
20.085680	833.877472	13.687885
19.999452	829.319460	13.692890
20.155919	825.539640	13.697895
19.921055	824.350212	13.702899
20.250167	828.891637	13.707904
19.900681	838.688719	13.712909
20.104998	822.799156	13.717914
20.048412	826.324990	13.722919
20.314200	831.914200	13.727923
20.389880	823.599118	13.732928
19.898328	835.435876	13.737933
20.114381	826.413973	13.742938
19.970701	830.027819	13.747943
19.776754	833.394205	13.752947
19.920456	823.074912	13.757952
19.929228	831.097465	13.762957
20.210645	825.331162	13.767962
20.148541	843.377574	13.772967
20.042890	837.438027	13.777971
20.425962	840.330739	13.782976
20.180143	845.878547	13.787981
20.189508	830.819625	13.792986
20.363810	838.224394	13.797991
20.264402	832.684418	13.802995
20.136871	834.013731	13.808000
19.975930	834.203450	13.813005
20.240358	828.296346	13.818010
20.238243	838.025406	13.823015
20.199383	839.340576	13.828019
20.120766	830.646381	13.833024
19.858027	843.343978	13.838029
19.962993	832.559325	13.843034
20.188335	836.576383	13.848039
20.256488	837.201093	13.853043
20.326004	834.528019	13.858048
20.114341	833.924698	13.863053
20.465159	826.530872	13.868058
20.141805	832.474260	13.873063
19.886709	832.358860	13.878067
20.136164	831.883850	13.883072
20.122616	831.821391	13.888077
19.958939	826.297976	13.893082
20.267168	831.669095	13.898087
19.768256	833.707378	13.903091
20.057117	831.450350	13.908096
19.848411	827.599458	13.913101
20.146394	834.938765	13.918106
20.106207	845.659545	13.923111
19.959822	853.372528	13.928115
20.387975	856.978756	13.933120
20.180613	848.625223	13.938125
20.101840	841.399262	13.943130
20.078975	839.431661	13.948135
20.041097	840.492773	13.953139
20.453620	841.898381	13.958144
19.802292	843.170885	13.963149
20.250210	840.243481	13.968154
20.269975	834.075763	13.973159
19.832751	841.240589	13.978163
20.224870	846.446937	13.983168
20.273662	859.153209	13.988173
20.061196	844.976519	13.993178
20.103015	844.831108	13.998183
20.106776	845.656910	14.003187
20.042943	841.674092	14.008192
20.152731	868.314470	14.013210
20.510838	860.834364	14.018227
20.050689	844.171003	14.023245
20.282932	845.458469	14.028263
20.249747	830.948107	14.033280
20.386727	845.039301	14.038298
20.116657	839.097128	14.043315
20.065625	850.399490	14.048333
20.136402	849.243090	14.053351
20.361386	854.152777	14.058368
20.324063	869.269082	14.063386
20.407562	867.276957	14.068403
20.450040	851.222396	14.073421
20.330186	851.246270	14.078439
20.303709	851.159297	14.083456
20.332248	869.744589	14.088474
20.467190	867.255053	14.093491
20.497785	872.892594	14.098509
20.328241	870.758360	14.103527
20.462862	873.672161	14.108544
20.162103	885.953468	14.113562
20.681283	871.679003	14.118579
20.908198	877.351299	14.123597
20.350056	881.314684	14.128615
20.672578	876.121111	14.133632
20.837007	884.273001	14.138650
20.722412	867.722809	14.143667
20.717365	852.375815	14.148685
20.401035	848.912211	14.153703
20.542664	858.417363	14.158720
20.111284	871.922843	14.163738
20.410100	869.457506	14.168755
20.552303	875.634091	14.173773
20.515376	882.775192	14.178791
20.569408	877.487591	14.183808
20.434205	883.557417	14.188826
20.683869	874.430356	14.193843
20.453972	882.605815	14.198861
20.642282	890.223795	14.203879
20.791765	896.433835	14.208896
20.877813	916.395837	14.213914
21.055288	910.928087	14.218931
20.887616	909.644549	14.223949
20.515669	908.085283	14.228967
20.978278	902.079704	14.233984
20.778722	909.767424	14.239002
21.214473	908.807635	14.244019
21.210724	914.850215	14.249037
20.951483	918.312907	14.254055
21.143921	909.843034	14.259072
21.425751	910.988891	14.264090
20.848864	897.866064	14.269107
21.150392	890.063063	14.274125
20.767038	903.328106	14.279143
21.451551	905.311071	14.284160
20.888042	902.649790	14.289178
20.829938	909.915403	14.294195
21.184667	903.868830	14.299213
21.215165	913.341407	14.304231
21.419626	916.157561	14.309248
21.116714	918.176900	14.314266
21.196584	913.078646	14.319283
21.599087	918.241609	14.324301
21.426005	922.694143	14.329319
21.307286	914.851193	14.334336
21.368758	920.419333	14.339354
21.002453	913.996980	14.344371
21.269407	918.012814	14.349389
21.272930	916.725565	14.354407
21.565795	909.757632	14.359424
21.266043	914.364074	14.364442
20.924992	911.475401	14.369459
21.395486	913.193631	14.374477
21.069909	921.278981	14.379495
21.423342	918.425827	14.384512
21.255426	921.199130	14.389530
21.486173	923.526605	14.394547
21.780706	910.343427	14.399565
21.287213	915.921432	14.404583
21.484489	909.956598	14.409600
21.435555	924.225385	14.414618
21.253721	921.042330	14.419635
21.805293	921.618205	14.424653
21.673077	945.288049	14.429671
21.481951	937.742924	14.434688
21.725247	945.643171	14.439706
21.831417	948.640176	14.444723
21.647623	941.049835	14.449741
21.825656	951.947654	14.454759
22.347307	936.397014	14.459776
22.230464	922.022600	14.464794
21.732005	920.370253	14.469811
22.210145	909.278214	14.474829
22.056064	918.133726	14.479847
21.961702	916.409061	14.484864
22.263871	912.557357	14.489882
21.828638	922.057033	14.494899
22.038844	913.713310	14.499917
21.705161	910.721217	14.504935
21.782208	914.817677	14.509952
21.556259	913.321639	14.514970
21.801583	915.690832	14.519987
21.973112	910.628295	14.525005
21.783667	912.829308	14.530023
22.032173	926.358530	14.535040
21.951888	921.746710	14.540058
22.243227	933.073179	14.545075
22.186447	927.268409	14.550093
22.118010	944.041420	14.555111
22.296329	932.380562	14.560128
22.253920	930.616149	14.565146
22.014633	925.969914	14.570163
22.092603	924.980674	14.575181
22.324949	937.181713	14.580199
22.318547	937.409287	14.585216
22.135662	943.192589	14.590234
21.966369	946.821838	14.595251
22.420798	940.924514	14.600269
22.476535	952.724301	14.605287
22.598113	949.587227	14.610304
22.393621	948.768879	14.615322
22.515841	944.659579	14.620339
22.618691	934.247148	14.625357
22.210412	927.493284	14.630375
22.273464	928.209999	14.635392
22.685646	939.610006	14.640410
22.808767	936.593810	14.645427
22.489856	923.511610	14.650445
22.420617	920.601604	14.655463
22.131113	928.118064	14.660480
22.370089	935.190016	14.665498
22.369796	942.142833	14.670515
22.649978	933.496930	14.675533
22.386362	942.354197	14.680551
22.564884	942.679690	14.685568
22.487675	939.552302	14.690586
22.496166	940.571873	14.695603
22.676588	940.477068	14.700621
22.457841	951.422442	14.705639
22.737845	944.275647	14.710656
22.892922	945.701272	14.715674
22.525141	950.115656	14.720691
22.644957	943.500922	14.725709
22.536853	945.388520	14.730727
22.844391	969.052756	14.735744
23.070337	968.824848	14.740762
23.019670	982.030607	14.745779
23.312207	964.501442	14.750797
23.054869	955.239694	14.755815
22.661134	948.574736	14.760832
22.791288	948.425027	14.765850
22.786157	968.856246	14.770867
22.976166	971.445056	14.775885
23.370695	970.257458	14.780903
23.291510	971.353937	14.785920
23.315758	959.563475	14.790938
23.035170	954.796404	14.795955
23.112987	941.746863	14.800973
22.771643	954.047285	14.805991
22.891444	959.749282	14.811008
23.334034	969.337064	14.816026
23.217725	972.589782	14.821043
23.455579	965.383633	14.826061
23.366744	967.578045	14.831079
23.046009	967.091267	14.836096
22.852906	966.227057	14.841114
23.377263	971.167685	14.846131
23.396296	968.509431	14.851149
23.232632	966.065933	14.856167
23.527721	974.173438	14.861184
23.668411	964.207980	14.866202
23.670574	969.898857	14.871219
23.684516	977.412561	14.876237
23.491334	963.143090	14.881255
23.351301	947.023152	14.886272
23.148436	952.342459	14.891290
23.414729	969.659857	14.896307
23.733711	963.696039	14.901325
23.616481	967.115642	14.906343
23.633322	970.235438	14.911360
23.649299	963.601079	14.916378
23.446121	968.165392	14.921395
23.297564	963.731188	14.926413
23.518583	962.363627	14.931431
23.614507	964.906094	14.936448
23.646517	963.483737	14.941466
23.536342	957.442080	14.946483
23.950699	964.324052	14.951501
23.635824	967.249792	14.956519
23.230374	973.414669	14.961536
24.175574	950.466188	14.966554
23.781498	966.440162	14.971571
23.842704	962.578114	14.976589
24.045673	965.202608	14.981607
23.841790	958.541970	14.986624
23.905790	956.593842	14.991642
23.827687	960.966745	14.996659
23.793572	963.844556	15.001677
23.777848	970.821871	15.006695
23.709636	970.043133	15.011712
24.245172	965.427457	15.016730
24.130304	971.413853	15.021747
23.902884	962.306203	15.026765
24.148710	962.691747	15.031783
24.086033	973.195395	15.036800
24.248307	967.409153	15.041818
24.041469	972.600113	15.046835
24.286641	981.352657	15.051853
24.248685	965.464955	15.056871
24.375228	973.248560	15.061888
24.486113	960.498894	15.066906
23.982665	967.623210	15.071923
23.675452	984.755249	15.076941
24.178807	985.872072	15.081959
24.293117	994.978978	15.086976
24.334475	999.062278	15.091994
24.506492	995.723667	15.097011
24.516098	998.742376	15.102029
24.903361	990.131271	15.107047
24.205193	998.471145	15.112064
24.508997	998.296885	15.117082
24.341079	998.608423	15.122099
23.997185	990.180003	15.127117
24.257112	996.246628	15.132135
24.203111	996.063370	15.137152
24.407824	992.359323	15.142170
24.426082	998.250564	15.147187
24.661984	992.775038	15.152205
24.834697	992.071129	15.157223
24.590442	1009.698096	15.162240
24.786159	997.496436	15.167258
24.394789	999.533041	15.172275
24.468883	1003.189551	15.177293
24.735000	998.649871	15.182311
24.449940	996.966624	15.187328
25.141088	1004.907157	15.192346
25.029827	1012.802644	15.197363
24.854951	1002.756931	15.202381
25.150400	1000.490310	15.207399
25.170539	999.843770	15.212416
25.338186	993.293744	15.217434
25.238546	998.333908	15.222451
25.417806	1002.464427	15.227469
25.055555	993.570172	15.232487
24.955509	1002.914192	15.237504
24.982564	986.871379	15.242522
24.938194	990.535770	15.247539
24.874054	990.962889	15.252557
24.745739	989.048576	15.257575
24.775273	993.835329	15.262592
25.052126	987.782266	15.267610
25.047032	989.716360	15.272627
24.835896	992.812748	15.277645
25.088011	993.507175	15.282663
25.021285	995.392899	15.287680
25.159941	1010.640158	15.292698
25.485960	1017.377370	15.297715
25.265730	1015.811195	15.302733
25.307973	996.426419	15.307751
25.017717	1018.594184	15.312768
25.134603	1018.882319	15.317786
25.278644	1019.823647	15.322803
25.388490	1027.090846	15.327821
25.642419	1022.579844	15.332839
25.640620	1017.061998	15.337856
25.832065	1019.941597	15.342874
25.708662	1029.023518	15.347891
25.500846	1016.024187	15.352909
25.716159	1008.554198	15.357927
25.363119	1000.455992	15.362944
25.393858	1004.647953	15.367962
25.593939	1011.652214	15.372979
25.521069	1022.846508	15.377997
25.939992	1014.214608	15.383015
25.693142	1027.165409	15.388032
25.649277	1017.770471	15.393050
25.688070	1017.135112	15.398067
25.546576	1015.517053	15.403085
25.998057	1011.646227	15.408103
25.760041	1014.899490	15.413120
25.760331	1014.822404	15.418138
26.053792	1015.571586	15.423155
25.465034	1016.716311	15.428173
25.993878	1023.480951	15.433191
26.217967	1024.843667	15.438208
26.014769	1025.744425	15.443226
25.903020	1020.857593	15.448243
25.692254	1023.390785	15.453261
26.287317	1018.337737	15.458279
25.972166	1022.902623	15.463296
25.932378	1023.311702	15.468314
26.291365	1016.981259	15.473331
25.838993	1024.154084	15.478349
25.932441	1021.845747	15.483367
26.118365	1025.714088	15.488384
25.896258	1015.926009	15.493402
25.885689	1022.468371	15.498419
25.864117	1021.093880	15.503437
26.015868	1021.418926	15.508455
26.071989	1021.575180	15.513472
26.117659	1020.355132	15.518490
26.219510	1021.295324	15.523507
26.134178	1028.014781	15.528525
26.506585	1040.690644	15.533543
26.213577	1052.272430	15.538560
26.515884	1046.995505	15.543578
27.073194	1040.141062	15.548595
26.296219	1031.410458	15.553613
26.547281	1021.411626	15.558631
26.292061	1022.454389	15.563648
26.238247	1042.885612	15.568666
26.840639	1045.172707	15.573683
26.502757	1050.983920	15.578701
26.281340	1058.590261	15.583719
26.553319	1047.631674	15.588736
26.513031	1047.568924	15.593754
26.827701	1038.313416	15.598771
26.634088	1050.506985	15.603789
26.773049	1043.167134	15.608807
26.634580	1048.027891	15.613824
26.892818	1044.368776	15.618842
26.844988	1043.438919	15.623859
26.582714	1050.252675	15.628877
26.745547	1038.704313	15.633895
26.752348	1048.432442	15.638912
26.867398	1051.505131	15.643930
27.044938	1041.031947	15.648947
26.921882	1045.898110	15.653965
26.595391	1045.514494	15.658983
26.784179	1051.191367	15.664000
26.841549	1044.537784	15.669018
26.759500	1048.741456	15.674035
26.600569	1053.871320	15.679053
27.150601	1061.732146	15.684071
27.022990	1072.271390	15.689088
27.073622	1073.367620	15.694106
27.713207	1066.023414	15.699123
27.440759	1063.661745	15.704141
27.401326	1050.009461	15.709159
26.865845	1041.724826	15.714176
27.071409	1041.654324	15.719194
27.384304	1051.070938	15.724211
27.071636	1039.576395	15.729229
27.588530	1047.245870	15.734247
27.420874	1054.530602	15.739264
27.120384	1040.566034	15.744282
27.472399	1057.095936	15.749299
27.637156	1069.682248	15.754317
27.561827	1052.637942	15.759335
27.479999	1041.751520	15.764352
27.060288	1043.690404	15.769370
27.265321	1055.488486	15.774387
27.592917	1070.908594	15.779405
27.522496	1071.015819	15.784423
27.726995	1072.559417	15.789440
27.421654	1086.842518	15.794458
27.555711	1078.328376	15.799475
27.643977	1077.726022	15.804493
27.799460	1071.170037	15.809511
27.882361	1067.633264	15.814528
27.732762	1073.375129	15.819546
27.927129	1065.683508	15.824563
27.929487	1075.997532	15.829581
28.131487	1073.953445	15.834599
28.100219	1072.516001	15.839616
28.028078	1072.769792	15.844634
27.981946	1060.661710	15.849651
27.609485	1059.851269	15.854669
27.702070	1067.457870	15.859687
28.193833	1067.720821	15.864704
27.739973	1066.075499	15.869722
27.662805	1066.570766	15.874739
28.038779	1077.536209	15.879757
28.053233	1073.209680	15.884775
28.204161	1064.950831	15.889792
27.706023	1073.842438	15.894810
28.028200	1065.510657	15.899827
27.674593	1068.096527	15.904845
27.630842	1069.593203	15.909863
28.164240	1080.535114	15.914880
28.198869	1097.272987	15.919898
28.515854	1090.662919	15.924915
28.480253	1094.563465	15.929933
28.569850	1093.174381	15.934951
28.578785	1091.063557	15.939968
28.146687	1074.883095	15.944986
28.208748	1082.022662	15.950003
28.459008	1095.372437	15.955021
28.633096	1097.510776	15.960039
28.593326	1094.202776	15.965056
28.681642	1097.213671	15.970074
28.425271	1075.406754	15.975091
28.442952	1077.255430	15.980109
28.451681	1092.668218	15.985127
28.510090	1097.964781	15.990144
28.505239	1100.760874	15.995162
28.659669	1099.488865	16.000179
28.626322	1099.973997	16.005197
28.559804	1100.313409	16.010215
28.796671	1097.074544	16.015232
28.500357	1106.283193	16.020250
28.730447	1102.247880	16.025267
28.731025	1099.276365	16.030285
29.087773	1100.037480	16.035303
28.840511	1093.932687	16.040320
28.819703	1095.089078	16.045338
28.647254	1089.963365	16.050355
28.793482	1103.578280	16.055373
28.460178	1102.445411	16.060391
29.193302	1099.681103	16.065408
29.077373	1104.810418	16.070426
29.013893	1093.170695	16.075443
28.989755	1103.059525	16.080461
28.951142	1118.898319	16.085479
29.251446	1121.582823	16.090496
29.046120	1134.306870	16.095514
29.375425	1126.244481	16.100531
29.695174	1125.285878	16.105549
29.185352	1118.678681	16.110567
29.378847	1106.165825	16.115584
29.081231	1102.592207	16.120602
29.487616	1116.662719	16.125619
29.293674	1112.136606	16.130637
29.584347	1122.039733	16.135655
29.450440	1104.002686	16.140672
29.334870	1107.357563	16.145690
29.442756	1107.765113	16.150707
29.248553	1122.076141	16.155725
29.433771	1123.333381	16.160743
29.626045	1118.818026	16.165760
29.382033	1123.769575	16.170778
29.345556	1121.618799	16.175795
29.702168	1127.506463	16.180813
29.607754	1124.624026	16.185831
29.735231	1117.476306	16.190848
29.575317	1121.632642	16.195866
29.893865	1121.265693	16.200883
29.887102	1118.351974	16.205901
29.478165	1122.395445	16.210919
29.942774	1122.011491	16.215936
29.624668	1126.122273	16.220954
29.770881	1115.175829	16.225971
29.736939	1125.166913	16.230989
29.556061	1121.746132	16.236007
29.905941	1124.311044	16.241024
29.751543	1132.402240	16.246042
30.087536	1132.650712	16.251059
30.082644	1131.819394	16.256077
29.940812	1145.459843	16.261095
30.046792	1140.149704	16.266112
29.791404	1159.877060	16.271130
29.966963	1158.559204	16.276147
30.196812	1163.499682	16.281165
30.009269	1161.571197	16.286183
30.314827	1152.611229	16.291200
30.506013	1154.663478	16.296218
30.402564	1155.634851	16.301235
30.480313	1159.905876	16.306253
30.305754	1156.745204	16.311271
30.414619	1155.669223	16.316288
30.498905	1151.265464	16.321306
30.475791	1160.831698	16.326323
30.416125	1159.394056	16.331341
30.349028	1164.296951	16.336359
30.552364	1154.086988	16.341376
30.369755	1166.810587	16.346394
30.445899	1157.531699	16.351411
30.550874	1158.661740	16.356429
30.498252	1156.386118	16.361447
30.678316	1147.013583	16.366464
30.863683	1151.736207	16.371482
30.500196	1159.445485	16.376499
30.636585	1149.861262	16.381517
30.351617	1155.395086	16.386535
30.608774	1155.841750	16.391552
30.354432	1154.314035	16.396570
30.613590	1167.711222	16.401587
30.939690	1169.428920	16.406605
30.950323	1184.415206	16.411623
31.216532	1176.067121	16.416640
31.312671	1183.210742	16.421658
31.140175	1168.316416	16.426675
31.104784	1154.685412	16.431693
31.003315	1156.343888	16.436711
30.850824	1152.939021	16.441728
30.962235	1170.135071	16.446746
31.462403	1169.976682	16.451763
31.460686	1172.940604	16.456781
31.196250	1164.574914	16.461799
31.494378	1145.976544	16.466816
31.248023	1150.785329	16.471834
31.356531	1151.480648	16.476851
31.389822	1144.431308	16.481869
31.324059	1158.377390	16.486887
31.357863	1146.862107	16.491904
31.129030	1149.709664	16.496922
31.267926	1148.622601	16.501939
31.715431	1147.116653	16.506957
31.252225	1152.236880	16.511975
31.719338	1156.675466	16.516992
31.353713	1151.638745	16.522010
31.541731	1168.327066	16.527027
31.496911	1162.834902	16.532045
31.455211	1174.744794	16.537063
31.613767	1165.998602	16.542080
31.538804	1174.214007	16.547098
31.244061	1178.572764	16.552115
31.491179	1173.334484	16.557133
31.407020	1167.205219	16.562151
31.493064	1168.744125	16.567168
31.761098	1168.696694	16.572186
31.664848	1169.824223	16.577203
31.813572	1174.744610	16.582221
31.864237	1186.860006	16.587239
32.119127	1188.288613	16.592256
32.112700	1181.176376	16.597274
31.726885	1167.388890	16.602291
32.115311	1189.011363	16.607309
32.175274	1201.790686	16.612327
31.978887	1189.899945	16.617344
32.216656	1192.680955	16.622362
32.258790	1201.738154	16.627379
32.291614	1188.020732	16.632397
32.103017	1188.914451	16.637415
32.531012	1182.550908	16.642432
32.690313	1181.282835	16.647450
32.254367	1177.059572	16.652467
32.386759	1169.844974	16.657485
32.214698	1171.502126	16.662503
32.420577	1174.654737	16.667520
32.223264	1167.854527	16.672538
32.478025	1175.625656	16.677555
32.822045	1180.933325	16.682573
32.126258	1180.685685	16.687591
32.577380	1187.228416	16.692608
32.396105	1193.009987	16.697626
32.178680	1201.929258	16.702643
32.735817	1187.996075	16.707661
32.437991	1205.628676	16.712679
32.515915	1201.029287	16.717696
32.624322	1199.421686	16.722714
32.429040	1207.983494	16.727731
32.721969	1200.955637	16.732749
32.538166	1199.501610	16.737767
32.609191	1196.751650	16.742784
32.813858	1206.659115	16.747802
32.741811	1219.059954	16.752819
32.478029	1218.304529	16.757837
33.011701	1228.861113	16.762855
33.217590	1235.689949	16.767872
33.220856	1234.792828	16.772890
33.109624	1240.176276	16.777907
32.949283	1226.532099	16.782925
32.998437	1234.789091	16.787943
33.083039	1232.367299	16.792960
33.402958	1223.788821	16.797978
33.151240	1229.340965	16.802995
33.387521	1222.086176	16.808013
33.253491	1231.276885	16.813031
33.018959	1229.230042	16.818048
33.140612	1225.995368	16.823066
33.314120	1226.560771	16.828083
33.445850	1220.351432	16.833101
33.058299	1225.170176	16.838119
33.112368	1225.981149	16.843136
33.455866	1221.016920	16.848154
33.194159	1230.638558	16.853171
33.409710	1219.139848	16.858189
33.528034	1224.636117	16.863207
33.451617	1219.070319	16.868224
33.613821	1226.930171	16.873242
33.639301	1245.239576	16.878259
33.888800	1248.693564	16.883277
33.850994	1257.161069	16.888295
33.773016	1250.270999	16.893312
33.785165	1229.767553	16.898330
33.717432	1255.302690	16.903347
33.823867	1256.684195	16.908365
34.053122	1256.388115	16.913383
33.884237	1263.064376	16.918400
34.080997	1256.677906	16.923418
33.992789	1259.141253	16.928435
34.167085	1257.287180	16.933453
34.079652	1262.264139	16.938471
33.663883	1248.361801	16.943488
34.238056	1252.885591	16.948506
34.209995	1253.964498	16.953523
34.484849	1253.426760	16.958541
34.599448	1258.421833	16.963559
34.064030	1242.621035	16.968576
34.345449	1244.430814	16.973594
34.129233	1257.660081	16.978611
34.110573	1255.559927	16.983629
34.193974	1253.729790	16.988647
34.215476	1259.625338	16.993664
34.483371	1258.568031	16.998682
34.479865	1256.866587	17.003699
34.229692	1251.468491	17.008717
34.352038	1257.019188	17.013735
34.327211	1261.805261	17.018752
34.843520	1254.420848	17.023770
34.726881	1248.323471	17.028787
34.749607	1254.824447	17.033805
34.430525	1254.250876	17.038823
34.481302	1256.361714	17.043840
34.777619	1254.041434	17.048858
34.412842	1253.854256	17.053875
34.707114	1249.714283	17.058893
34.636780	1252.141744	17.063911
34.780265	1262.548223	17.068928
34.894421	1269.443617	17.073946
34.642276	1269.491736	17.078963
34.841760	1258.980288	17.083981
35.088879	1273.420853	17.088999
34.882059	1281.018690	17.094016
35.416136	1270.076336	17.099034
34.906060	1281.032242	17.104051
35.030345	1268.893659	17.109069
35.136260	1272.293474	17.114087
35.252900	1279.114542	17.119104
35.193013	1265.713860	17.124122
35.138510	1276.120467	17.129139
34.763844	1270.013896	17.134157
35.030395	1277.141395	17.139175
34.881279	1279.680528	17.144192
35.458848	1285.213686	17.149210
35.282140	1291.446034	17.154227
35.657269	1304.953842	17.159245
35.728389	1304.520958	17.164263
35.820493	1294.423022	17.169280
35.614316	1270.309573	17.174298
35.464642	1270.004715	17.179315
35.410072	1268.218604	17.184333
35.895405	1278.266974	17.189351
35.737496	1284.291823	17.194368
35.660779	1266.884111	17.199386
35.626512	1284.742191	17.204403
35.766080	1297.395641	17.209421
36.147775	1299.728991	17.214439
35.885685	1302.547274	17.219456
35.815505	1291.216779	17.224474
36.159227	1299.448849	17.229491
36.121250	1295.879389	17.234509
35.672320	1283.034681	17.239527
35.663140	1294.848247	17.244544
35.966778	1294.963454	17.249562
35.917588	1297.319909	17.254579
35.833043	1304.066109	17.259597
36.311582	1286.299248	17.264615
36.313248	1298.891323	17.269632
36.507419	1284.139748	17.274650
36.322310	1290.804452	17.279667
36.162168	1291.605548	17.284685
36.312219	1288.377342	17.289703
36.062875	1297.701318	17.294720
36.182589	1288.800795	17.299738
36.201130	1291.807129	17.304755
36.304199	1292.143093	17.309773
36.377844	1284.196900	17.314791
36.651604	1303.766122	17.319808
36.767753	1299.037907	17.324826
36.437527	1298.129477	17.329843
36.255170	1296.936336	17.334861
36.419796	1299.902069	17.339879
36.607951	1312.706662	17.344896
36.684746	1309.822050	17.349914
36.443314	1318.222966	17.354931
36.731679	1318.121955	17.359949
37.335988	1312.658339	17.364967
37.000272	1322.524653	17.369984
37.058388	1313.517534	17.375002
36.954995	1313.165967	17.380019
36.993116	1307.407258	17.385037
37.149239	1314.651490	17.390055
36.632668	1314.537286	17.395072
36.902455	1311.849986	17.400090
37.378677	1306.205451	17.405107
37.075554	1318.323899	17.410125
37.040896	1312.185104	17.415143
37.325577	1325.045101	17.420160
37.151644	1313.545515	17.425178
36.883251	1314.845232	17.430195
36.955779	1306.133127	17.435213
37.089433	1308.078168	17.440231
37.042708	1317.763104	17.445248
37.648574	1332.074150	17.450266
37.568089	1336.354734	17.455283
37.747612	1343.799747	17.460301
37.910194	1325.276252	17.465319
37.711497	1314.412984	17.470336
37.847034	1314.735905	17.475354
37.686181	1308.005319	17.480371
37.524776	1303.341821	17.485389
37.730019	1305.012743	17.490407
37.324980	1312.948957	17.495424
37.495415	1320.639230	17.500442
38.178680	1330.791351	17.505459
37.801925	1330.296189	17.510477
38.263731	1334.203985	17.515495
37.876918	1326.817284	17.520512
37.547576	1325.793878	17.525530
38.035740	1334.024953	17.530547
38.107043	1339.462697	17.535565
37.977698	1345.236045	17.540583
38.232526	1350.465193	17.545600
38.441780	1339.912802	17.550618
38.393931	1331.628876	17.555635
38.289666	1336.286068	17.560653
38.477699	1336.986016	17.565671
38.102144	1332.211942	17.570688
38.271147	1334.697201	17.575706
38.476441	1337.521172	17.580723
38.219005	1339.427918	17.585741
38.419733	1324.580873	17.590759
38.511621	1341.862039	17.595776
38.349659	1339.268765	17.600794
38.296384	1336.747820	17.605811
38.084150	1345.164544	17.610829
38.345764	1337.652395	17.615847
38.242919	1335.240033	17.620864
38.470716	1331.017829	17.625882
38.294856	1333.499887	17.630899
38.515763	1359.388728	17.635917
38.871631	1360.293149	17.640935
38.539311	1365.007173	17.645952
38.834993	1364.892410	17.650970
39.297897	1356.077114	17.655987
38.672087	1362.864050	17.661005
38.897652	1362.022704	17.666023
39.097779	1368.989378	17.671040
39.179288	1363.882840	17.676058
39.370940	1366.477752	17.681075
39.448436	1364.993044	17.686093
39.156557	1362.527454	17.691111
39.088762	1364.794076	17.696128
39.103861	1361.950756	17.701146
39.627143	1353.865170	17.706163
39.302541	1351.801212	17.711181
39.576173	1353.130891	17.716199
39.087062	1340.904459	17.721216
39.322179	1344.035141	17.726234
39.450317	1348.194363	17.731251
39.220628	1349.859153	17.736269
39.536017	1350.625308	17.741287
39.332444	1355.751386	17.746304
39.417809	1357.098508	17.751322
39.264394	1347.701951	17.756339
39.509353	1355.591148	17.761357
39.587206	1346.189169	17.766375
39.603491	1346.466614	17.771392
39.776610	1356.242357	17.776410
39.848483	1350.983200	17.781427
39.567585	1360.156515	17.786445
39.681656	1358.581028	17.791463
39.868911	1370.298831	17.796480
39.903141	1381.499915	17.801498
40.160988	1379.701716	17.806515
39.846625	1381.792156	17.811533
40.146837	1383.425919	17.816551
40.150603	1391.606867	17.821568
40.219148	1386.470927	17.826586
40.132334	1389.275428	17.831603
39.613471	1387.698637	17.836621
39.798911	1382.493717	17.841639
40.133545	1384.839307	17.846656
40.028499	1384.530475	17.851674
40.297933	1384.847772	17.856691
40.487902	1402.289550	17.861709
40.809465	1399.853533	17.866727
40.463078	1382.841059	17.871744
40.831987	1375.060088	17.876762
41.231221	1364.365692	17.881779
40.684014	1376.221090	17.886797
40.679402	1367.588893	17.891815
41.074349	1364.617347	17.896832
41.036081	1377.470696	17.901850
41.199496	1366.297945	17.906867
40.967113	1369.580274	17.911885
41.154736	1368.447671	17.916903
40.971005	1368.097905	17.921920
40.825893	1354.724890	17.926938
40.958434	1360.821426	17.931955
40.778037	1366.484946	17.936973
40.984183	1353.269846	17.941991
41.289697	1365.314857	17.947008
41.029447	1366.559796	17.952026
41.074998	1361.839674	17.957043
41.001463	1366.654000	17.962061
40.878449	1360.371970	17.967079
41.006248	1366.275778	17.972096
40.989703	1364.658201	17.977114
41.113793	1361.429401	17.982131
40.922727	1357.437593	17.987149
40.966983	1366.974341	17.992167
41.261419	1385.969355	17.997184
41.323742	1391.491923	18.002202
41.283158	1386.952276	18.007219
41.458582	1394.468756	18.012237
41.432735	1399.566504	18.017255
41.707525	1399.149899	18.022272
41.488631	1394.289468	18.027290
41.762811	1388.648810	18.032307
41.661409	1397.570145	18.037325
41.571478	1402.637216	18.042343
41.733547	1393.503353	18.047360
41.755201	1402.859680	18.052378
42.158484	1409.394414	18.057395
41.912615	1409.748280	18.062413
41.894755	1416.269959	18.067431
42.254669	1428.271738	18.072448
42.409468	1420.317247	18.077466
42.244300	1400.445899	18.082483
42.279733	1399.990389	18.087501
41.896876	1400.115985	18.092519
42.774269	1391.579061	18.097536
42.139511	1395.915030	18.102554
42.281618	1378.912741	18.107571
42.300257	1395.296423	18.112589
42.439670	1393.441605	18.117607
42.424519	1402.007831	18.122624
42.369509	1424.242516	18.127642
42.694996	1414.637397	18.132659
42.549217	1431.780393	18.137677
42.534980	1419.287815	18.142695
43.101759	1421.547621	18.147712
42.530190	1413.746737	18.152730
42.782276	1408.389602	18.157747
42.721053	1411.759476	18.162765
42.710381	1419.686333	18.167783
42.725108	1418.636359	18.172800
42.699030	1421.626240	18.177818
42.721901	1420.532494	18.182835
42.757771	1425.562204	18.187853
42.792782	1424.518433	18.192871
43.080894	1416.215483	18.197888
42.836353	1424.390434	18.202906
43.123658	1418.540026	18.207923
42.892109	1414.406791	18.212941
42.855283	1421.386114	18.217959
42.823313	1424.696268	18.222976
42.831971	1445.138544	18.227994
43.354127	1440.010465	18.233011
43.100065	1446.626460	18.238029
42.935687	1452.605218	18.243047
42.980975	1439.676826	18.248064
43.097712	1443.902390	18.253082
43.243815	1450.357034	18.258099
43.427245	1472.796018	18.263117
43.511891	1471.546119	18.268135
43.908215	1468.961310	18.273152
44.034950	1475.253095	18.278170
44.201009	1457.620024	18.283187
43.875823	1453.963408	18.288205
43.365545	1444.275270	18.293223
43.728250	1453.283071	18.298240
43.759475	1471.499820	18.303258
44.241152	1467.463609	18.308275
44.375284	1463.777780	18.313293
44.086115	1467.025142	18.318311
44.007042	1459.326587	18.323328
43.977090	1473.102874	18.328346
44.246974	1467.832543	18.333363
43.852641	1464.436286	18.338381
44.036180	1469.497517	18.343399
44.255918	1470.123200	18.348416
44.360374	1472.056403	18.353434
44.236536	1468.248117	18.358451
44.582322	1469.696865	18.363469
44.363719	1476.683183	18.368487
44.442232	1458.907552	18.373504
44.207283	1469.758367	18.378522
44.425125	1468.338570	18.383539
44.578385	1478.705893	18.388557
44.261088	1472.930656	18.393575
44.604020	1473.786023	18.398592
44.541333	1492.899485	18.403610
44.395882	1493.559031	18.408627
44.832444	1505.012231	18.413645
44.650518	1505.606806	18.418663
44.848725	1500.741165	18.423680
44.831737	1502.252494	18.428698
44.968693	1501.665954	18.433715
45.182309	1502.963532	18.438733
44.893535	1500.692484	18.443751
45.215432	1491.617229	18.448768
45.171981	1506.175159	18.453786
45.145041	1495.716171	18.458803
45.106116	1493.579101	18.463821
44.711980	1498.487076	18.468839
44.825473	1500.254455	18.473856
44.912650	1511.155389	18.478874
45.210670	1532.109292	18.483891
45.712817	1524.115864	18.488909
45.198297	1530.680625	18.493927
45.595081	1527.405937	18.498944
45.744982	1526.880255	18.503962
45.878902	1525.977223	18.508979
46.255344	1520.329644	18.513997
45.868832	1529.663846	18.519015
46.038253	1530.300703	18.524032
45.607412	1524.423213	18.529050
45.731164	1522.942910	18.534067
46.037604	1510.240228	18.539085
45.784172	1526.961616	18.544103
45.885868	1515.863877	18.549120
46.097284	1525.415755	18.554138
45.811600	1517.229433	18.559155
45.998216	1516.403730	18.564173
46.144304	1527.803385	18.569191
46.021402	1516.426064	18.574208
46.034445	1524.077053	18.579226
45.968727	1519.502046	18.584243
45.902841	1525.016797	18.589261
46.326188	1540.516521	18.594279
46.544545	1545.699646	18.599296
46.468224	1546.124004	18.604314
46.495557	1551.795364	18.609331
46.663779	1546.873140	18.614349
46.636497	1546.767414	18.619367
46.695173	1539.376408	18.624384
46.746977	1548.545543	18.629402
46.655174	1555.212789	18.634419
46.967948	1545.213197	18.639437
46.549573	1543.804411	18.644455
46.914154	1542.605818	18.649472
46.671190	1547.152272	18.654490
46.931437	1540.506220	18.659507
47.016735	1540.732549	18.664525
47.025896	1546.887382	18.669543
47.078490	1542.564855	18.674560
46.885920	1551.905106	18.679578
46.812917	1542.383123	18.684595
47.219251	1539.401075	18.689613
46.967957	1547.960217	18.694631
46.881604	1551.287725	18.699648
47.059916	1572.882934	18.704666
47.336788	1571.787207	18.709683
47.458012	1566.761570	18.714701
47.406649	1578.551419	18.719719
47.400843	1570.497401	18.724736
47.207874	1574.294181	18.729754
47.100974	1573.097634	18.734771
47.527930	1574.527940	18.739789
47.492708	1581.534613	18.744807
47.674603	1581.718008	18.749824
47.874044	1584.825330	18.754842
47.969853	1590.028803	18.759859
47.944271	1581.199255	18.764877
47.851815	1585.167204	18.769895
47.909141	1590.888854	18.774912
48.088642	1591.011280	18.779930
48.284559	1592.082019	18.784947
48.162586	1597.737095	18.789965
47.994564	1595.701614	18.794983
48.087044	1603.490204	18.800000
48.401034	1599.029226	18.805018
48.353538	1604.960302	18.810035
48.374544	1595.627006	18.815053
48.100306	1600.830510	18.820071
48.168548	1605.997484	18.825088
48.332635	1608.573241	18.830106
48.422487	1606.816753	18.835123
48.467237	1592.248366	18.840141
48.457977	1600.492860	18.845159
48.560522	1600.408900	18.850176
48.728498	1598.322190	18.855194
48.533322	1593.163741	18.860211
48.697128	1592.477744	18.865229
48.707917	1623.216575	18.870247
48.777937	1624.459985	18.875264
48.936983	1632.214378	18.880282
48.546009	1632.315313	18.885299
49.204138	1626.537821	18.890317
49.018275	1629.400639	18.895335
49.105236	1629.566927	18.900352
49.135658	1623.182444	18.905370
49.160030	1622.275641	18.910387
49.308974	1615.827425	18.915405
49.222838	1623.742832	18.920423
49.525169	1613.589909	18.925440
49.680646	1611.999927	18.930458
49.438659	1616.286687	18.935475
49.809155	1618.433894	18.940493
49.488082	1624.509288	18.945511
49.737248	1624.825892	18.950528
49.669222	1620.055372	18.955546
49.957327	1624.081405	18.960563
49.863379	1619.241083	18.965581
49.424826	1625.030035	18.970599
49.595594	1618.715196	18.975616
49.615335	1614.987796	18.980634
49.716477	1625.638041	18.985651
49.964829	1611.203124	18.990669
50.007354	1620.907849	18.995687
50.120329	1635.761871	19.000704
50.282947	1638.107409	19.005722
49.933972	1638.504466	19.010739
50.270910	1628.790411	19.015757
50.176086	1640.031941	19.020775
50.548322	1633.397875	19.025792
50.517114	1629.402519	19.030810
50.133362	1641.914782	19.035827
50.427987	1634.833750	19.040845
50.118647	1637.886157	19.045863
50.312939	1641.423767	19.050880
50.500860	1636.171169	19.055898
50.362218	1632.650716	19.060915
50.158577	1625.560276	19.065933
50.173272	1643.003557	19.070951
50.365876	1662.624749	19.075968
50.573047	1660.173899	19.080986
50.247798	1670.115858	19.086003
50.588617	1655.752671	19.091021
51.027669	1656.087757	19.096039
50.729649	1670.264863	19.101056
51.154486	1670.005227	19.106074
51.252538	1680.420827	19.111091
51.161935	1680.348008	19.116109
51.398505	1687.457682	19.121127
51.056842	1687.837056	19.126144
51.617078	1685.311016	19.131162
51.271180	1694.565695	19.136179
51.485681	1694.536243	19.141197
51.796417	1693.789053	19.146215
51.399717	1687.797507	19.151232
51.573098	1686.133872	19.156250
51.632146	1696.625707	19.161267
51.675730	1680.135879	19.166285
51.901860	1676.014521	19.171303
51.835072	1687.810852	19.176320
51.938307	1676.848032	19.181338
51.857753	1689.829528	19.186355
51.932027	1685.859021	19.191373
51.855565	1675.425106	19.196391
51.959043	1681.308538	19.201408
52.207451	1680.321954	19.206426
51.985732	1682.173494	19.211443
52.149323	1681.817878	19.216461
51.958056	1685.485421	19.221479
51.791769	1689.420340	19.226496
51.926038	1681.850457	19.231514
52.078821	1684.345443	19.236531
52.172388	1705.246471	19.241549
52.554903	1710.097507	19.246567
52.616460	1721.707433	19.251584
52.658153	1715.460332	19.256602
52.689486	1711.384976	19.261619
52.391684	1714.160265	19.266637
52.513585	1708.115889	19.271655
52.419821	1712.830517	19.276672
52.956003	1706.181283	19.281690
52.766152	1711.390244	19.286707
52.701127	1718.055653	19.291725
52.820199	1706.461044	19.296743
52.720991	1713.275842	19.301760
52.833245	1720.618515	19.306778
52.473953	1726.799938	19.311795
53.039258	1738.736184	19.316813
53.333263	1737.522090	19.321831
53.133180	1742.248965	19.326848
53.390712	1740.964392	19.331866
52.924960	1746.139499	19.336883
53.174402	1739.900155	19.341901
53.470415	1736.874313	19.346919
53.262983	1744.126403	19.351936
53.210898	1738.563603	19.356954
53.060448	1752.930409	19.361971
53.777640	1763.443961	19.366989
53.712938	1773.309042	19.372007
53.271860	1774.296547	19.377024
53.809890	1777.149340	19.382042
53.738485	1775.036286	19.387059
53.959920	1774.345023	19.392077
54.046858	1765.944179	19.397095
53.865436	1774.364101	19.402112
54.148517	1765.113174	19.407130
54.173044	1762.741776	19.412147
54.532780	1752.931191	19.417165
54.447549	1752.092986	19.422183
54.454079	1752.398738	19.427200
54.872527	1755.689831	19.432218
54.639168	1756.727582	19.437235
54.184785	1752.047739	19.442253
54.840065	1750.630513	19.447271
54.479186	1759.208041	19.452288
54.768135	1755.822294	19.457306
54.509558	1755.721993	19.462323
54.672492	1755.138380	19.467341
54.637723	1752.848017	19.472359
54.884548	1749.348647	19.477376
54.955548	1754.029932	19.482394
54.906277	1754.038615	19.487411
54.484911	1753.434926	19.492429
55.186088	1757.485571	19.497447
54.895220	1771.879509	19.502464
54.900425	1768.045057	19.507482
55.183012	1776.759870	19.512499
55.297888	1781.363376	19.517517
55.566927	1778.636786	19.522535
55.386838	1787.493039	19.527552
55.867100	1786.893424	19.532570
55.539783	1781.504285	19.537587
55.433943	1776.232416	19.542605
55.609538	1772.451017	19.547623
55.132166	1782.923854	19.552640
55.419919	1778.894892	19.557658
55.451321	1782.092768	19.562675
55.361243	1773.842068	19.567693
55.632307	1779.114404	19.572711
55.583505	1793.167720	19.577728
55.651541	1782.666635	19.582746
55.804033	1784.380637	19.587763
55.676829	1806.558203	19.592781
56.019082	1813.405679	19.597799
55.914315	1822.492200	19.602816
55.989264	1821.192693	19.607834
56.244083	1824.028527	19.612851
56.113088	1815.059910	19.617869
56.195249	1810.211102	19.622887
56.252756	1826.730651	19.627904
56.459163	1821.763704	19.632922
56.059316	1822.976671	19.637939
56.218386	1830.709930	19.642957
56.571692	1836.798201	19.647975
56.486305	1846.030305	19.652992
56.586392	1841.073229	19.658010
56.730351	1844.649593	19.663027
56.706189	1852.110835	19.668045
56.905619	1847.878063	19.673063
56.885942	1847.313345	19.678080
56.994552	1840.508860	19.683098
57.155824	1849.825118	19.688115
56.494893	1848.215870	19.693133
56.926466	1845.157374	19.698151
56.788914	1863.337820	19.703168
56.948937	1863.479874	19.708186
57.312613	1873.533120	19.713203
57.135963	1871.027826	19.718221
57.447132	1869.644234	19.723239
57.404943	1874.906786	19.728256
57.531552	1877.721390	19.733274
57.643050	1869.000373	19.738291
57.705694	1875.278171	19.743309
57.690971	1875.815417	19.748327
57.654930	1874.222916	19.753344
57.815203	1888.742444	19.758362
58.149012	1898.555065	19.763379
57.932546	1902.269941	19.768397
58.203490	1885.598893	19.773415
58.233259	1894.961322	19.778432
58.143681	1883.490304	19.783450
58.363093	1864.972005	19.788467
58.093736	1861.518750	19.793485
58.292466	1868.187784	19.798503
58.436581	1888.745940	19.803520
58.373206	1895.367120	19.808538
58.491519	1897.225808	19.813555
58.548747	1893.266616	19.818573
58.671876	1890.287192	19.823591
58.612530	1894.492991	19.828608
58.542330	1893.009762	19.833626
58.712780	1890.883288	19.838643
58.541929	1890.654156	19.843661
58.700093	1896.075109	19.848679
58.569899	1894.498408	19.853696
58.663250	1896.059824	19.858714
58.756485	1891.648124	19.863731
58.832093	1888.121755	19.868749
58.960405	1882.210000	19.873767
58.518118	1897.299145	19.878784
58.920795	1910.979318	19.883802
59.515420	1919.111951	19.888819
59.293387	1921.420562	19.893837
59.263032	1916.130311	19.898855
59.255299	1929.438628	19.903872
58.993776	1923.950847	19.908890
59.720460	1920.132647	19.913907
59.169536	1925.208921	19.918925
59.345391	1923.501604	19.923943
59.458804	1938.934775	19.928960
59.928022	1945.253160	19.933978
59.885634	1939.750089	19.938995
59.825147	1946.912773	19.944013
60.139989	1937.514304	19.949031
60.100352	1936.449366	19.954048
60.109462	1938.995626	19.959066
60.045842	1939.837207	19.964083
60.118785	1951.417972	19.969101
60.288786	1940.135973	19.974119
60.387939	1937.828156	19.979136
60.165228	1943.620562	19.984154
60.278263	1935.034550	19.989171
59.956138	1935.288109	19.994189
60.156755	1941.560448	19.999207
60.467500	1950.668876	20.004224
60.183422	1964.594702	20.009242
60.549874	1961.848609	20.014259
60.595456	1971.845682	20.019277
60.543325	1970.037858	20.024295
60.823573	1970.018372	20.029312
60.727412	1988.193945	20.034330
61.271311	1989.578117	20.039347
61.322324	1998.726425	20.044365
61.211578	1998.420060	20.049383
61.495101	1995.900347	20.054400
61.374498	1985.935749	20.059418
61.332060	1969.439649	20.064435
61.518525	1979.942830	20.069453
61.549793	1980.887264	20.074471
61.770805	1982.085388	20.079488
61.491913	1975.853907	20.084506
61.423089	1962.445355	20.089523
61.518759	1969.104915	20.094541
61.591613	1979.590820	20.099559
61.677080	1984.494043	20.104576
61.620901	1994.965928	20.109594
62.283979	1981.789081	20.114611
61.993658	1994.101900	20.119629
62.075066	1990.397604	20.124647
61.978986	1987.544363	20.129664
62.012948	1995.475427	20.134682
61.909781	1991.062770	20.139699
62.081831	1991.436517	20.144717
61.996302	1993.500771	20.149735
62.179150	1994.730939	20.154752
62.056317	1991.832410	20.159770
62.450454	2018.468781	20.164787
62.472555	2025.923520	20.169805
62.286551	2024.053664	20.174823
62.520507	2024.087967	20.179840
62.652852	2028.055580	20.184858
63.047835	2022.669927	20.189875
63.088835	2013.788596	20.194893
63.337900	2005.688970	20.199911
62.894196	2010.606591	20.204928
62.641203	2016.777475	20.209946
63.135850	2010.407668	20.214963
62.753011	2011.645465	20.219981
63.098593	2009.787580	20.224999
63.270810	2006.221392	20.230016
63.032286	2015.061932	20.235034
63.619411	2016.141891	20.240051
63.551127	2019.129974	20.245069
63.662835	2026.084324	20.250087
63.610714	2032.866591	20.255104
63.782469	2036.149899	20.260122
63.977014	2027.037205	20.265139
63.616151	2031.864538	20.270157
63.757705	2032.948701	20.275175
64.222804	2019.708220	20.280192
63.931023	2028.078242	20.285210
64.262473	2018.125690	20.290227
64.141893	2027.796920	20.295245
63.841847	2025.326223	20.300263
64.239922	2025.098382	20.305280
63.983983	2028.350005	20.310298
64.074934	2022.486626	20.315315
64.024460	2029.231660	20.320333
64.048492	2028.844021	20.325351
64.269191	2032.983174	20.330368
64.232361	2054.717238	20.335386
64.625800	2057.826760	20.340403
64.723687	2061.129721	20.345421
64.635979	2060.344593	20.350439
64.553706	2061.163985	20.355456
64.651878	2066.494676	20.360474
64.660041	2056.948399	20.365491
64.647127	2073.188429	20.370509
64.868337	2080.244114	20.375527
65.215662	2076.983488	20.380544
64.971197	2084.983388	20.385562
65.229834	2089.438214	20.390579
65.126767	2092.249374	20.395597
65.038298	2086.468857	20.400615
65.438181	2088.426607	20.405632
65.175629	2091.857063	20.410650
65.380734	2087.653208	20.415667
65.547496	2088.668070	20.420685
65.165970	2091.593644	20.425703
65.982945	2107.197167	20.430720
65.866045	2110.060091	20.435738
66.175781	2119.488135	20.440755
66.246444	2112.393038	20.445773
66.067358	2102.491960	20.450791
66.135109	2104.727641	20.455808
66.073097	2112.967465	20.460826
66.318508	2115.330555	20.465843
66.614442	2111.238846	20.470861
66.123674	2114.896053	20.475879
66.380400	2103.805393	20.480896
66.214049	2111.499458	20.485914
66.241425	2109.734784	20.490931
66.231336	2109.397418	20.495949
66.285861	2111.997819	20.500967
66.465821	2109.002995	20.505984
66.496484	2119.472919	20.511002
66.581705	2124.752996	20.516019
66.877776	2141.361494	20.521037
66.756166	2143.982125	20.526055
66.934750	2130.776225	20.531072
66.954645	2145.264125	20.536090
66.816429	2138.613706	20.541107
66.775203	2131.345306	20.546125
66.902106	2153.402643	20.551143
67.495395	2153.776861	20.556160
67.093270	2169.459249	20.561178
67.314106	2168.479392	20.566195
67.445451	2176.428846	20.571213
67.317493	2166.532943	20.576231
67.938522	2158.082093	20.581248
67.420614	2163.500847	20.586266
67.715949	2172.618165	20.591283
67.935044	2177.966582	20.596301
68.111549	2194.967046	20.601319
68.033478	2193.104337	20.606336
67.968890	2200.326793	20.611354
68.183114	2189.692768	20.616371
68.440198	2190.362084	20.621389
68.142194	2201.997487	20.626407
68.550780	2199.392509	20.631424
68.306257	2201.320900	20.636442
68.026208	2198.050181	20.641459
68.223297	2197.391100	20.646477
68.093571	2198.778896	20.651495
68.452855	2198.318909	20.656512
68.148622	2214.472623	20.661530
68.388890	2222.175838	20.666547
69.052667	2219.058998	20.671565
68.614191	2224.635007	20.676583
68.985854	2223.865493	20.681600
68.743634	2229.682360	20.686618
68.571204	2235.515631	20.691635
68.609141	2243.575194	20.696653
68.719159	2255.556162	20.701671
69.293216	2249.419789	20.706688
69.020448	2257.249676	20.711706
69.106238	2254.291866	20.716723
69.647089	2260.346474	20.721741
69.584319	2283.260952	20.726759
69.790102	2278.039099	20.731776
69.949600	2285.149561	20.736794
69.858399	2281.043247	20.741811
70.062556	2279.517796	20.746829
70.055096	2278.885040	20.751847
70.221403	2270.759924	20.756864
69.871545	2282.251851	20.761882
70.081941	2278.651979	20.766899
70.129368	2272.332145	20.771917
70.080409	2271.860178	20.776935
70.036631	2274.605283	20.781952
70.224385	2273.337301	20.786970
70.000390	2276.132386	20.791987
70.368324	2274.871065	20.797005
70.473162	2297.162606	20.802023
70.525223	2301.039268	20.807040
70.831587	2298.376637	20.812058
70.397028	2301.697707	20.817075
70.646623	2301.422752	20.822093
70.669978	2311.900271	20.827111
70.826346	2305.308198	20.832128
71.338153	2314.798533	20.837146
70.830033	2318.894323	20.842163
71.118297	2327.668344	20.847181
71.242034	2338.544403	20.852199
71.429347	2328.107282	20.857216
71.368129	2335.141274	20.862234
71.350669	2341.052913	20.867251
71.544226	2330.993928	20.872269
71.662468	2345.277562	20.877287
71.402160	2340.369927	20.882304
71.424063	2332.141167	20.887322
71.490285	2353.914302	20.892339
72.035970	2350.201947	20.897357
71.960197	2352.231658	20.902375
72.281747	2352.390434	20.907392
72.397480	2353.258496	20.912410
72.060946	2350.703104	20.917427
72.440312	2350.576568	20.922445
72.109731	2354.988578	20.927463
72.252964	2356.002493	20.932480
72.479005	2347.148870	20.937498
72.304914	2355.490870	20.942515
72.491270	2355.116664	20.947533
72.192117	2358.641115	20.952551
72.490659	2361.686395	20.957568
72.615110	2375.170684	20.962586
72.763049	2383.812947	20.967603
72.907983	2381.020301	20.972621
72.917740	2381.357802	20.977639
73.110492	2386.050550	20.982656
73.081663	2383.361915	20.987674
72.996416	2386.217484	20.992691
73.248245	2376.418188	20.997709
73.038866	2385.343973	21.002727
73.423003	2397.669129	21.007744
73.347771	2403.797667	21.012762
73.224725	2411.044494	21.017779
73.525747	2404.187038	21.022797
73.596415	2420.455813	21.027815
73.634374	2413.727616	21.032832
73.929415	2412.242719	21.037850
73.621591	2420.293021	21.042867
74.106771	2428.329343	21.047885
74.121459	2442.102572	21.052903
74.465948	2441.946988	21.057920
74.654827	2438.982926	21.062938
74.283748	2440.798597	21.067955
74.725011	2436.671823	21.072973
74.594225	2432.278382	21.077991
74.878579	2432.233072	21.083008
74.714258	2408.550761	21.088026
74.424605	2407.512288	21.093043
74.915249	2423.263375	21.098061
74.848539	2426.316576	21.103079
74.938281	2422.295421	21.108096
74.997534	2432.495142	21.113114
74.641248	2427.882810	21.118131
75.293402	2422.747037	21.123149
74.834389	2423.743733	21.128167
75.151150	2426.249667	21.133184
75.374432	2428.963224	21.138202
75.223008	2430.010763	21.143219
75.074901	2434.643831	21.148237
74.999892	2446.582885	21.153255
75.257214	2441.993039	21.158272
75.572324	2449.460261	21.163290
75.418483	2451.711669	21.168307
75.519981	2455.703983	21.173325
75.719270	2475.094735	21.178343
75.821950	2476.068716	21.183360
76.225391	2475.143884	21.188378
76.099047	2484.924097	21.193395
76.290928	2481.106096	21.198413
76.010955	2474.005389	21.203431
76.164838	2487.174384	21.208448
76.047058	2479.059849	21.213466
76.041446	2485.465997	21.218483
76.627120	2494.980067	21.223501
76.559285	2504.657359	21.228519
76.459489	2506.187503	21.233536
76.706714	2507.062135	21.238554
76.705143	2509.806060	21.243571
76.664514	2510.235765	21.248589
76.422241	2505.043597	21.253607
76.919440	2518.253048	21.258624
77.247708	2527.927753	21.263642
77.070680	2540.711436	21.268659
77.496952	2542.095548	21.273677
77.360758	2542.201471	21.278695
77.078445	2537.412908	21.283712
77.441678	2540.844353	21.288730
77.489266	2536.744937	21.293747
77.789662	2530.849527	21.298765
77.574178	2537.947547	21.303783
77.618317	2537.843795	21.308800
77.916667	2547.347087	21.313818
77.966170	2563.713002	21.318835
78.214184	2560.936134	21.323853
78.149025	2556.718612	21.328871
78.028647	2564.836637	21.333888
78.256375	2558.361285	21.338906
78.287322	2562.257116	21.343923
78.390420	2557.680817	21.348941
78.574586	2550.798666	21.353959
78.939051	2548.679702	21.358976
78.828171	2548.554262	21.363994
78.592880	2553.685028	21.369011
78.720136	2555.549454	21.374029
79.108300	2570.407740	21.379047
78.621183	2580.760773	21.384064
79.100211	2585.848426	21.389082
79.273369	2589.496619	21.394099
79.237741	2579.890123	21.399117
79.422221	2586.061485	21.404135
79.383403	2588.665844	21.409152
79.409879	2574.740468	21.414170
79.169641	2573.836476	21.419187
79.581414	2579.981813	21.424205
79.532416	2572.183481	21.429223
79.475165	2590.418885	21.434240
79.787074	2595.372728	21.439258
79.567327	2610.155737	21.444275
79.966706	2596.955109	21.449293
80.454032	2594.398862	21.454311
80.378421	2592.486941	21.459328
80.443690	2592.345995	21.464346
80.235599	2596.844733	21.469363
80.254938	2601.111340	21.474381
80.482686	2592.151107	21.479399
80.586098	2596.941551	21.484416
80.636155	2589.101455	21.489434
80.472283	2589.324276	21.494451
80.801005	2593.405461	21.499469
80.949079	2583.408618	21.504487
80.501846	2597.273750	21.509504
80.902340	2608.215999	21.514522
80.785981	2611.470660	21.519539
80.969682	2618.825204	21.524557
81.145518	2623.339810	21.529575
81.091724	2624.037488	21.534592
81.425790	2618.793484	21.539610
81.211352	2624.298516	21.544627
81.311164	2627.163163	21.549645
81.493235	2633.299532	21.554663
81.647858	2645.359448	21.559680
81.850644	2650.856161	21.564698
81.549638	2659.616593	21.569715
81.602581	2651.094807	21.574733
82.091233	2651.456627	21.579751
81.503418	2653.253398	21.584768
81.650887	2671.232860	21.589786
81.857382	2677.259949	21.594803
82.054677	2681.239407	21.599821
82.500317	2668.061230	21.604839
82.204266	2677.921338	21.609856
82.748700	2679.860054	21.614874
83.080252	2688.270273	21.619891
82.878885	2692.414783	21.624909
83.146293	2668.876368	21.629927
82.959356	2668.373689	21.634944
82.903218	2665.242566	21.639962
83.490519	2688.327747	21.644979
83.543134	2676.614752	21.649997
83.522887	2668.298132	21.655015
83.222566	2672.325481	21.660032
83.558046	2673.557326	21.665050
83.612312	2690.089383	21.670067
83.424819	2696.578905	21.675085
83.634871	2697.221137	21.680103
83.534473	2695.966036	21.685120
83.387729	2692.368742	21.690138
83.432469	2696.277355	21.695155
83.363964	2693.435309	21.700173
83.864486	2716.408516	21.705191
83.838940	2730.879072	21.710208
83.803016	2724.179034	21.715226
83.984394	2726.450179	21.720243
84.172046	2730.285667	21.725261
84.395856	2749.441612	21.730279
84.163036	2758.192802	21.735296
84.213114	2755.242160	21.740314
84.610340	2751.475509	21.745331
84.484098	2754.940228	21.750349
84.773955	2750.279024	21.755367
84.607594	2764.104240	21.760384
84.805574	2776.889681	21.765402
84.988839	2784.915355	21.770419
84.989917	2792.254274	21.775437
85.144756	2785.542664	21.780455
84.998814	2791.797485	21.785472
85.358734	2791.672477	21.790490
85.057694	2791.862899	21.795507
85.468944	2816.047718	21.800525
85.969974	2801.366817	21.805543
85.901001	2811.532190	21.810560
86.195821	2805.503837	21.815578
86.685097	2790.187669	21.820595
86.487839	2793.017129	21.825613
86.636464	2768.666052	21.830631
86.444829	2769.125352	21.835648
86.647399	2765.122294	21.840666
86.416278	2761.453486	21.845683
86.641049	2757.020549	21.850701
86.490696	2761.346515	21.855719
86.192246	2761.299755	21.860736
86.642671	2772.870531	21.865754
87.027419	2778.180954	21.870771
86.802976	2795.140654	21.875789
86.949344	2791.428158	21.880807
86.899812	2794.274964	21.885824
87.133808	2788.164285	21.890842
87.061773	2791.898827	21.895859
87.031614	2802.289266	21.900877
87.369097	2793.120265	21.905895
87.038761	2795.874983	21.910912
87.048613	2815.747912	21.915930
87.553062	2815.574684	21.920947
87.745566	2830.515569	21.925965
87.472021	2824.706064	21.930983
87.557218	2830.044611	21.936000
87.971947	2831.751531	21.941018
87.940818	2850.990742	21.946035
88.038299	2851.245042	21.951053
88.376375	2842.413373	21.956071
88.477449	2855.673718	21.961088
88.278671	2849.731928	21.966106
88.748405	2850.507384	21.971123
88.544131	2849.203545	21.976141
89.023111	2839.659549	21.981159
88.573147	2844.092315	21.986176
88.690865	2843.205162	21.991194
88.936091	2847.143199	21.996211
89.028533	2856.264987	22.001229
89.007324	2865.393105	22.006247
89.092049	2882.517561	22.011264
88.631278	2888.563833	22.016282
89.313629	2879.598578	22.021299
88.779130	2885.429276	22.026317
89.336358	2877.864482	22.031335
89.195940	2888.041301	22.036352
89.230819	2900.743521	22.041370
89.500103	2905.130828	22.046387
89.486517	2911.318968	22.051405
89.822445	2903.285232	22.056423
89.780251	2922.070852	22.061440
89.650977	2936.271038	22.066458
90.508577	2937.292999	22.071475
90.168545	2943.657497	22.076493
90.394505	2936.202924	22.081511
90.338400	2936.706691	22.086528
90.547105	2944.326436	22.091546
90.779609	2940.485320	22.096563
90.151491	2943.020888	22.101581
90.639702	2951.479434	22.106599
90.861516	2967.526488	22.111616
90.559724	2966.377421	22.116634
91.168493	2960.678876	22.121651
90.930534	2969.818813	22.126669
91.283340	2963.276926	22.131687
90.987052	2974.697133	22.136704
91.214016	2994.011793	22.141722
91.709792	2998.393687	22.146739
91.487172	3001.509627	22.151757
91.824277	2991.701043	22.156775
91.651812	2990.163212	22.161792
91.531134	2996.256767	22.166810
91.760657	2994.476269	22.171827
91.872614	3007.241805	22.176845
92.129242	3029.582628	22.181863
92.237895	3031.364341	22.186880
92.416755	3030.089062	22.191898
92.317026	3026.580943	22.196915
91.916684	3025.920346	22.201933
92.200304	3039.342109	22.206951
92.603565	3059.676521	22.211968
93.060145	3047.196356	22.216986
93.396480	3045.940800	22.222003
93.488402	3052.164092	22.227021
93.672662	3042.711016	22.232039
93.379250	3048.535582	22.237056
93.497620	3036.826759	22.242074
93.589780	3034.080164	22.247091
93.553172	3041.940455	22.252109
93.908851	3034.746757	22.257127
93.750646	3033.738404	22.262144
93.670320	3040.188174	22.267162
93.639504	3038.043290	22.272179
93.956647	3035.118439	22.277197
93.716000	3037.253986	22.282215
94.026244	3028.791636	22.287232
93.892682	3035.954707	22.292250
93.800879	3037.655114	22.297267
94.164538	3054.041490	22.302285
94.628689	3055.926199	22.307303
94.597309	3058.325720	22.312320
94.189053	3063.494471	22.317338
94.556680	3057.880755	22.322355
94.582820	3061.686237	22.327373
94.845687	3063.511799	22.332391
94.824674	3069.882901	22.337408
95.125518	3086.738718	22.342426
95.226517	3085.361004	22.347443
95.244910	3100.905740	22.352461
95.195330	3093.979588	22.357479
95.495841	3085.510892	22.362496
95.345052	3088.023068	22.367514
95.349961	3085.867760	22.372531
95.597848	3090.712417	22.377549
95.590079	3105.306368	22.382567
95.630649	3118.000004	22.387584
95.670603	3118.095145	22.392602
95.729863	3116.000389	22.397619
95.910658	3121.641594	22.402637
96.107779	3129.605466	22.407655
96.526571	3135.038025	22.412672
96.673744	3146.111540	22.417690
96.748966	3151.813644	22.422707
96.553738	3149.083753	22.427725
96.638976	3143.298714	22.432743
96.996686	3144.110932	22.437760
96.609502	3150.552261	22.442778
96.807399	3146.272166	22.447795
96.698187	3158.357274	22.452813
96.990220	3173.808893	22.457831
97.561513	3158.515449	22.462848
97.369551	3169.285147	22.467866
97.385246	3165.547771	22.472883
97.661531	3167.961964	22.477901
97.390113	3162.590136	22.482919
97.308457	3189.502755	22.487936
97.754909	3196.080979	22.492954
97.915750	3192.598917	22.497971
98.330709	3197.696221	22.502989
98.001931	3193.129598	22.508007
98.285329	3190.918065	22.513024
98.334670	3201.393652	22.518042
98.668561	3218.621934	22.523059
98.841829	3217.222457	22.528077
98.952393	3207.507280	22.533095
98.984782	3219.067986	22.538112
99.356191	3220.044003	22.543130
99.172269	3213.708739	22.548147
99.205394	3215.542638	22.553165
98.915178	3211.585792	22.558183
99.288220	3205.168007	22.563200
99.119258	3211.836511	22.568218
99.075704	3212.998269	22.573235
99.356590	3209.677198	22.578253
99.405181	3227.440271	22.583271
99.818656	3236.022604	22.588288
99.713376	3248.295950	22.593306
99.763282	3246.846132	22.598323
99.905010	3247.726624	22.603341
99.513280	3263.502913	22.608359
99.871559	3249.933819	22.613376
99.708627	3268.376499	22.618394
100.039200	3280.795905	22.623411
99.820597	3271.654715	22.628429
100.119315	3292.979191	22.633447
100.326562	3304.062125	22.638464
100.336636	3312.531839	22.643482
100.573873	3307.697140	22.648499
100.757643	3322.370891	22.653517
100.671473	3326.600257	22.658535
101.318554	3321.965293	22.663552
101.387842	3326.820417	22.668570
101.742328	3323.926528	22.673587
101.778520	3323.575461	22.678605
101.875352	3319.908490	22.683623
101.717651	3321.812165	22.688640
101.523241	3327.672970	22.693658
101.721451	3329.080946	22.698675
101.908088	3335.722692	22.703693
101.944089	3350.421610	22.708711
102.303903	3354.217224	22.713728
102.160122	3365.780181	22.718746
102.281330	3365.774263	22.723763
102.305608	3355.182272	22.728781
102.586071	3367.273062	22.733799
102.595160	3366.164850	22.738816
102.429988	3386.767359	22.743834
102.763549	3377.449161	22.748851
102.777193	3375.590554	22.753869
102.472058	3386.846509	22.758887
103.291942	3402.087546	22.763904
103.083394	3408.454089	22.768922
103.353634	3412.665976	22.773939
103.173555	3410.340313	22.778957
103.260747	3417.591082	22.783975
103.812291	3433.490884	22.788992
104.020607	3440.503663	22.794010
104.122539	3445.103468	22.799027
103.963888	3444.752004	22.804045
103.797664	3452.183224	22.809063
104.159950	3452.242700	22.814080
104.303083	3455.920285	22.819098
104.126978	3456.182039	22.824115
104.369042	3457.575169	22.829133
104.595913	3467.227339	22.834151
104.866290	3477.386256	22.839168
104.636605	3478.872708	22.844186
104.549842	3481.535216	22.849203
104.804810	3474.448616	22.854221
104.791337	3485.385170	22.859239
105.250959	3494.189998	22.864256
105.269465	3500.955388	22.869274
105.026044	3507.261455	22.874291
105.374458	3502.512014	22.879309
105.109845	3511.405596	22.884327
105.360251	3518.612295	22.889344
105.532245	3536.378090	22.894362
105.831565	3537.130418	22.899379
105.927591	3528.539108	22.904397
105.895381	3539.572301	22.909415
106.338954	3538.257127	22.914432
106.408202	3553.017811	22.919450
106.338403	3553.348359	22.924467
107.019127	3555.596647	22.929485
106.802262	3572.096631	22.934503
106.896237	3561.693186	22.939520
106.772636	3569.735188	22.944538
106.949698	3563.833864	22.949555
107.095276	3549.051575	22.954573
106.967651	3564.420278	22.959591
107.543105	3556.418792	22.964608
107.187408	3564.309006	22.969626
107.513290	3578.946194	22.974643
107.538674	3585.131551	22.979661
107.357776	3586.498529	22.984679
107.722342	3583.117620	22.989696
107.799446	3589.666817	22.994714
107.903440	3602.218600	22.999731
108.215583	3611.841535	23.004749
108.079057	3619.784148	23.009767
108.398043	3619.039491	23.014784
108.738223	3615.708089	23.019802
108.252439	3621.415664	23.024819
108.371551	3619.673153	23.029837
108.272845	3631.816759	23.034855
108.546913	3642.546314	23.039872
108.783913	3643.013591	23.044890
108.730922	3654.777839	23.049907
109.400665	3655.231963	23.054925
109.366718	3676.275718	23.059943
109.710852	3668.187554	23.064960
109.828594	3669.752354	23.069978
110.003840	3671.528247	23.074995
110.049866	3667.352460	23.080013
109.913308	3672.878501	23.085031
109.752813	3660.548140	23.090048
109.958765	3672.388322	23.095066
110.231516	3664.204558	23.100083
110.074496	3666.290672	23.105101
110.211759	3687.484139	23.110119
110.308154	3690.640604	23.115136
110.621847	3697.924619	23.120154
110.151843	3703.086129	23.125171
110.424456	3692.653319	23.130189
110.715361	3714.782047	23.135207
111.021225	3717.938155	23.140224
111.125322	3716.806899	23.145242
111.087774	3719.933597	23.150259
111.880260	3712.802862	23.155277
111.657072	3722.878605	23.160295
111.573158	3719.987683	23.165312
111.759156	3707.938719	23.170330
111.580727	3724.007162	23.175347
111.603660	3722.836142	23.180365
111.654512	3745.793000	23.185383
111.934838	3748.280594	23.190400
112.241425	3747.884826	23.195418
111.512754	3755.000758	23.200435
112.178456	3757.908336	23.205453
112.204316	3768.294459	23.210471
112.446973	3770.042309	23.215488
112.947446	3766.198370	23.220506
112.655932	3793.685210	23.225523
113.047182	3796.642067	23.230541
112.688108	3804.707587	23.235559
113.099902	3807.291439	23.240576
113.182300	3797.213779	23.245594
113.248868	3816.040625	23.250611
113.495009	3818.663482	23.255629
113.654330	3827.354346	23.260647
113.917285	3834.025843	23.265664
113.979159	3831.671756	23.270682
113.605166	3830.353983	23.275699
113.912552	3831.213602	23.280717
113.988445	3855.596007	23.285735
114.227502	3868.952480	23.290752
114.541447	3868.488670	23.295770
114.503961	3871.520203	23.300787
114.587017	3855.526671	23.305805
114.759094	3870.726756	23.310823
114.782994	3882.853379	23.315840
115.177350	3886.034747	23.320858
115.058195	3887.328972	23.325875
115.164790	3891.029015	23.330893
115.102856	3894.196611	23.335911
115.358677	3903.071159	23.340928
115.417931	3905.918927	23.345946
115.533030	3928.717932	23.350963
115.730495	3921.445981	23.355981
116.129387	3921.448492	23.360999
115.618531	3920.818056	23.366016
116.212960	3925.948361	23.371034
116.224004	3950.173704	23.376051
116.084496	3950.320282	23.381069
116.391852	3959.845090	23.386087
116.177027	3952.318693	23.391104
116.824425	3968.232902	23.396122
116.716013	3982.771399	23.401139
117.034742	3981.219643	23.406157
117.032776	3989.481626	23.411175
117.017793	3989.171744	23.416192
117.825379	3987.509780	23.421210
117.401111	3989.767568	23.426227
117.520674	3976.281502	23.431245
117.423999	3977.957620	23.436263
117.450788	3986.937967	23.441280
118.023381	3993.181773	23.446298
117.698546	4007.167948	23.451315
118.254843	4011.039394	23.456333
118.415114	4007.228402	23.461351
118.209924	4012.162923	23.466368
118.625286	4005.676685	23.471386
118.327299	4001.125349	23.476403
118.359934	4022.163702	23.481421
118.510467	4028.186115	23.486439
118.622489	4043.350329	23.491456
119.112431	4039.506427	23.496474
118.903960	4049.409337	23.501491
119.049770	4055.208312	23.506509
119.569604	4057.745875	23.511527
119.000339	4065.627930	23.516544
119.331529	4063.656453	23.521562
119.743850	4075.314585	23.526579
120.014781	4088.374319	23.531597
119.936274	4100.656693	23.536615
120.197350	4099.122772	23.541632
120.472258	4091.393915	23.546650
120.237691	4091.625667	23.551667
120.335899	4087.124408	23.556685
120.544092	4080.830869	23.561703
120.443100	4093.965648	23.566720
120.681404	4102.330983	23.571738
120.701354	4122.905789	23.576755
120.953393	4122.764943	23.581773
120.863204	4120.759956	23.586791
120.816483	4135.321808	23.591808
121.321925	4143.681543	23.596826
121.179628	4156.656974	23.601843
121.514538	4152.748870	23.606861
121.626230	4154.884245	23.611879
121.569183	4162.945851	23.616896
122.036132	4159.509153	23.621914
122.314156	4169.210272	23.626931
122.338169	4160.255616	23.631949
122.523764	4164.831294	23.636967
122.529514	4166.324324	23.641984
122.821021	4164.208906	23.647002
122.771738	4187.572616	23.652019
123.105274	4194.363613	23.657037
123.541758	4187.883369	23.662055
123.270487	4194.508055	23.667072
123.747470	4183.259562	23.672090
123.967556	4184.790004	23.677107
123.831100	4164.305353	23.682125
123.778425	4149.747598	23.687143
123.808713	4152.199612	23.692160
123.946053	4152.387007	23.697178
123.897177	4164.059752	23.702195
123.812333	4178.560857	23.707213
124.124599	4173.293038	23.712231
124.115047	4184.437958	23.717248
124.041614	4169.345402	23.722266
124.034691	4182.657997	23.727283
124.200753	4203.299299	23.732301
124.457305	4195.098946	23.737319
124.181118	4204.248101	23.742336
124.991616	4225.306672	23.747354
124.970114	4237.333838	23.752371
124.756631	4243.746366	23.757389
125.098770	4233.818942	23.762407
125.075743	4262.919030	23.767424
125.282367	4268.857076	23.772442
125.387553	4267.322035	23.777459
125.299020	4273.876710	23.782477
125.523086	4289.065006	23.787495
125.548169	4305.556337	23.792512
126.019470	4311.540306	23.797530
126.354286	4322.555682	23.802547
126.254783	4324.816014	23.807565
126.700106	4322.184366	23.812583
126.581060	4325.758441	23.817600
126.572929	4337.210058	23.822618
127.093140	4349.063613	23.827635
127.109756	4363.618738	23.832653
127.552539	4359.918373	23.837671
127.020109	4366.071856	23.842688
127.354519	4360.482616	23.847706
127.491549	4377.137902	23.852723
127.654542	4388.903698	23.857741
127.451661	4387.856743	23.862759
127.568468	4403.165317	23.867776
127.899179	4414.256154	23.872794
128.141004	4409.926210	23.877811
128.478461	4409.567201	23.882829
128.973332	4405.691741	23.887847
128.698895	4413.405028	23.892864
128.818729	4415.517115	23.897882
128.899942	4422.012534	23.902899
128.557646	4437.808939	23.907917
129.247930	4436.820168	23.912935
129.316716	4444.920866	23.917952
129.334471	4440.526732	23.922970
129.541551	4444.553892	23.927987
129.399437	4460.929665	23.933005
129.958649	4471.533332	23.938023
129.793160	4481.493399	23.943040
129.769164	4476.382936	23.948058
130.212768	4482.525585	23.953075
129.904901	4480.600100	23.958093
130.512414	4485.691546	23.963111
130.268107	4498.191857	23.968128
130.393505	4499.257545	23.973146
130.208809	4507.561543	23.978163
130.413283	4516.769559	23.983181
130.888346	4524.462517	23.988199
130.847664	4542.172972	23.993216
130.960297	4540.434533	23.998234
131.324195	4549.237172	24.003251
131.348388	4563.387707	24.008269
131.603238	4565.168326	24.013287
131.618992	4568.729618	24.018304
131.857357	4563.500193	24.023322
131.832310	4577.207026	24.028339
131.705623	4584.967646	24.033357
132.295123	4600.140476	24.038375
132.108921	4608.259895	24.043392
132.303717	4609.989519	24.048410
132.625581	4619.739016	24.053427
132.438050	4626.182186	24.058445
132.804255	4624.113010	24.063463
132.928794	4640.018494	24.068480
133.074890	4646.637407	24.073498
132.932875	4657.936760	24.078515
132.983385	4661.741919	24.083533
133.638017	4669.284380	24.088551
133.457639	4690.724260	24.093568
133.169394	4692.276810	24.098586
133.897706	4695.224952	24.103603
133.959786	4723.332923	24.108621
134.301663	4712.608283	24.113639
134.138418	4716.699287	24.118656
134.541480	4721.543348	24.123674
134.919275	4733.912406	24.128691
134.801727	4738.897703	24.133709
135.176735	4734.573964	24.138727
135.513143	4741.983902	24.143744
135.341409	4747.862893	24.148762
135.591717	4731.929853	24.153779
135.383265	4734.383842	24.158797
135.621399	4744.280515	24.163815
136.042451	4760.015335	24.168832
136.052969	4762.896215	24.173850
136.199834	4768.356231	24.178867
136.238396	4776.731774	24.183885
136.391872	4768.484602	24.188903
136.458952	4773.023512	24.193920
136.503061	4770.535221	24.198938
137.054551	4771.967255	24.203955
136.874211	4785.961019	24.208973
137.385440	4788.109878	24.213991
137.507916	4791.151495	24.219008
137.332691	4792.473620	24.224026
137.542280	4789.026682	24.229043
137.280774	4788.193590	24.234061
137.657779	4785.778090	24.239079
137.513277	4784.842950	24.244096
137.701315	4806.666388	24.249114
137.805688	4814.992123	24.254131
137.932570	4817.511451	24.259149
138.222133	4822.084918	24.264167
138.140314	4824.606843	24.269184
138.209082	4837.662505	24.274202
138.422330	4847.130520	24.279219
138.135923	4865.568135	24.284237
138.726084	4868.709061	24.289255
138.974941	4882.054668	24.294272
138.502172	4890.020894	24.299290
139.143138	4893.703643	24.304307
139.530168	4906.865962	24.309325
139.649058	4906.731395	24.314343
139.658191	4912.943504	24.319360
139.629752	4924.404323	24.324378
140.034877	4935.991913	24.329395
140.068967	4949.914665	24.334413
140.271474	4946.130528	24.339431
140.372273	4943.878626	24.344448
140.532858	4961.780135	24.349466
140.714383	4963.949337	24.354483
140.935793	4973.361061	24.359501
141.130774	4964.986007	24.364519
141.121836	4966.586881	24.369536
140.980161	4977.357745	24.374554
141.426364	4989.463573	24.379571
141.408481	4997.235381	24.384589
141.710971	4996.999947	24.389607
142.127084	5014.095291	24.394624
142.098805	5027.774735	24.399642
142.263940	5030.172351	24.404659
142.395383	5036.862222	24.409677
142.382642	5033.150934	24.414695
142.420940	5037.008488	24.419712
142.572187	5051.835488	24.424730
142.864955	5058.951228	24.429747
142.666026	5072.798748	24.434765
143.028985	5057.234468	24.439783
143.431552	5067.791168	24.444800
143.400058	5088.803507	24.449818
143.560561	5085.915825	24.454835
143.438114	5097.081009	24.459853
143.604273	5097.930185	24.464871
143.843541	5104.899492	24.469888
143.902864	5123.659147	24.474906
144.072345	5129.318668	24.479923
143.870680	5132.542639	24.484941
143.885970	5150.344813	24.489959
144.295395	5157.896733	24.494976
143.954740	5178.531297	24.499994
144.758180	5180.942811	24.505011
145.063287	5195.209655	24.510029
145.119116	5208.189821	24.515047
145.199830	5224.069880	24.520064
145.263841	5217.270949	24.525082
145.603310	5205.315880	24.530099
145.503222	5229.359640	24.535117
145.864426	5248.459181	24.540135
146.355510	5236.885869	24.545152
146.218939	5255.912162	24.550170
145.988025	5238.233219	24.555187
146.610958	5256.988144	24.560205
146.713453	5270.631226	24.565223
146.771355	5270.627539	24.570240
147.057442	5281.728509	24.575258
147.106543	5274.142041	24.580275
147.205694	5286.699182	24.585293
147.096637	5300.950345	24.590311
147.542995	5304.240176	24.595328
147.035004	5320.000212	24.600346
147.682552	5322.385470	24.605363
147.744660	5335.698326	24.610381
147.598763	5333.167855	24.615399
148.234643	5348.315972	24.620416
148.006575	5368.154757	24.625434
148.333030	5355.011296	24.630451
148.868565	5370.851251	24.635469
149.707962	5375.430847	24.640487
149.907594	5360.029186	24.645504
149.924471	5349.587210	24.650522
149.970316	5333.398964	24.655539
150.257949	5338.476418	24.660557
150.058379	5337.282530	24.665575
150.332255	5333.671014	24.670592
149.744134	5336.698595	24.675610
150.377376	5349.706404	24.680627
150.491657	5361.493334	24.685645
150.351364	5364.002644	24.690663
150.418280	5367.570920	24.695680
150.525434	5375.389864	24.700698
150.504823	5389.755250	24.705715
150.971315	5400.702452	24.710733
150.953756	5396.906872	24.715751
151.324581	5395.298678	24.720768
151.130379	5403.196371	24.725786
151.413464	5423.782174	24.730803
151.513243	5428.010027	24.735821
151.554029	5436.716812	24.740839
151.742573	5449.192964	24.745856
151.647835	5463.892808	24.750874
151.998132	5468.780938	24.755891
152.164315	5488.067662	24.760909
152.431006	5501.503825	24.765927
152.571422	5495.844390	24.770944
152.528181	5517.424098	24.775962
153.190235	5524.943795	24.780979
153.366459	5533.942170	24.785997
153.338996	5535.307673	24.791015
153.225096	5526.126351	24.796032
153.103482	5543.399312	24.801050
153.422104	5553.216822	24.806067
153.708468	5555.307243	24.811085
153.680281	5561.461061	24.816103
154.199346	5575.216599	24.821120
153.883154	5587.049529	24.826138
154.209170	5578.285034	24.831155
154.263668	5609.285661	24.836173
154.359497	5619.501434	24.841191
154.914541	5625.507999	24.846208
154.782770	5648.323851	24.851226
154.787139	5650.681902	24.856243
155.341853	5664.575029	24.861261
155.271812	5678.767621	24.866279
155.483938	5681.364771	24.871296
155.659525	5680.257375	24.876314
156.108469	5691.979407	24.881331
156.399549	5712.775191	24.886349
156.209991	5712.393976	24.891367
156.703613	5706.877195	24.896384
156.673405	5708.709703	24.901402
156.704278	5729.976573	24.906419
157.146787	5729.303394	24.911437
157.094320	5737.788408	24.916455
157.172157	5738.350374	24.921472
157.466116	5760.940380	24.926490
158.041002	5760.285432	24.931507
158.144832	5760.845615	24.936525
158.286572	5764.264372	24.941543
158.847665	5743.903123	24.946560
158.678202	5749.986706	24.951578
159.028844	5756.842580	24.956595
159.029129	5746.929317	24.961613
158.976810	5740.421702	24.966631
159.034135	5741.299285	24.971648
159.185253	5758.814609	24.976666
159.344620	5768.754427	24.981683
159.549221	5776.609974	24.986701
158.996831	5785.734903	24.991719
159.406588	5786.704995	24.996736
159.631154	5802.459674	25.001754
159.484378	5813.546665	25.006771
159.595373	5815.558084	25.011789
159.919335	5841.920713	25.016807
160.210805	5842.449408	25.021824
160.202224	5866.888733	25.026842
160.499878	5875.277089	25.031859
160.822142	5882.065163	25.036877
160.783828	5904.792552	25.041895
161.428261	5909.539519	25.046912
161.379664	5915.850159	25.051930
161.417034	5911.278584	25.056947
161.469646	5921.761093	25.061965
161.567248	5934.222258	25.066983
161.360592	5941.275650	25.072000
162.012802	5958.857655	25.077018
162.069221	5974.647195	25.082035
162.448428	5973.925878	25.087053
162.273342	5978.677649	25.092071
162.540935	5990.778164	25.097088
163.051100	6004.535524	25.102106
162.923188	6000.572491	25.107123
163.312325	5995.884222	25.112141
163.523630	6019.435871	25.117159
163.571610	6025.861765	25.122176
163.797177	6026.573280	25.127194
163.677073	6031.700250	25.132211
164.420369	6034.354394	25.137229
163.950947	6053.110625	25.142247
164.574968	6053.121319	25.147264
164.636454	6050.161120	25.152282
164.625602	6069.428049	25.157299
164.938366	6075.858168	25.162317
165.056499	6080.598625	25.167335
165.087181	6080.006831	25.172352
165.256104	6101.322247	25.177370
165.274103	6107.642020	25.182387
165.814117	6115.570155	25.187405
165.687150	6132.323016	25.192423
165.666924	6142.410525	25.197440
166.284197	6146.504935	25.202458
166.118665	6155.232448	25.207475
166.594478	6164.450163	25.212493
166.591445	6182.945727	25.217511
166.788110	6181.921481	25.222528
166.765054	6207.371551	25.227546
166.718402	6215.655279	25.232563
167.139211	6210.992579	25.237581
167.257264	6245.392780	25.242599
167.378826	6251.094993	25.247616
168.076447	6250.376399	25.252634
167.928893	6274.935329	25.257651
168.328321	6273.136802	25.262669
168.408263	6280.366535	25.267687
168.545645	6286.713771	25.272704
168.891851	6292.946675	25.277722
168.908071	6304.423471	25.282739
169.249391	6300.831657	25.287757
168.974717	6310.010187	25.292775
169.393316	6327.165670	25.297792
169.448642	6334.773083	25.302810
169.334441	6350.638221	25.307827
169.509746	6357.371266	25.312845
169.727348	6371.397492	25.317863
170.108977	6368.269741	25.322880
170.327087	6388.912097	25.327898
170.047667	6408.968172	25.332915
170.594408	6398.120750	25.337933
170.769119	6421.754406	25.342951
170.883163	6431.468217	25.347968
171.285572	6432.552041	25.352986
171.621747	6442.918108	25.358003
171.668503	6442.589676	25.363021
171.309109	6458.281585	25.368039
171.785139	6467.198896	25.373056
172.134396	6471.284988	25.378074
172.117325	6474.128899	25.383091
172.753732	6488.661257	25.388109
172.840984	6498.357352	25.393127
173.068544	6497.305343	25.398144
173.065180	6496.610381	25.403162
172.805260	6506.805592	25.408179
173.285267	6509.704802	25.413197
173.842155	6517.964858	25.418215
173.983782	6514.195541	25.423232
174.015815	6514.022095	25.428250
173.909233	6518.339813	25.433267
174.295938	6514.924039	25.438285
174.182334	6527.417803	25.443303
174.421316	6545.983813	25.448320
174.802399	6544.934861	25.453338
174.459680	6550.119533	25.458355
174.646965	6559.632916	25.463373
174.878187	6583.805440	25.468391
174.916004	6589.637583	25.473408
175.343832	6602.685551	25.478426
175.172425	6614.146079	25.483443
175.428529	6622.772809	25.488461
175.662727	6644.899245	25.493479
175.432397	6654.559527	25.498496
176.012603	6676.733131	25.503514
176.167350	6683.857503	25.508531
176.485295	6698.480970	25.513549
176.707152	6712.233028	25.518567
176.658941	6729.026721	25.523584
177.191829	6736.749396	25.528602
177.255803	6749.720172	25.533619
177.691394	6760.864514	25.538637
177.890031	6765.493217	25.543655
178.033184	6776.650361	25.548672
178.392135	6767.303969	25.553690
178.705886	6783.366496	25.558707
178.926542	6787.866591	25.563725
179.154835	6793.105082	25.568743
179.340459	6795.299870	25.573760
179.690586	6787.019441	25.578778
179.715202	6789.471224	25.583795
179.725580	6793.802633	25.588813
180.072442	6789.241244	25.593831
179.910600	6798.506731	25.598848
179.885727	6802.093921	25.603866
180.143302	6812.198179	25.608883
180.081162	6823.019070	25.613901
180.056498	6832.442890	25.618919
180.285733	6833.793550	25.623936
180.399008	6848.378196	25.628954
180.557147	6867.603480	25.633971
180.682454	6872.573588	25.638989
181.155465	6881.193426	25.644007
180.554024	6895.578124	25.649024
181.299194	6910.309149	25.654042
181.592846	6914.988057	25.659059
181.748462	6934.346804	25.664077
182.061247	6949.423769	25.669095
182.123771	6954.748546	25.674112
182.555213	6963.589864	25.679130
182.699510	6985.329071	25.684148
182.868573	6979.391476	25.689165
183.206827	6981.731127	25.694183
183.167057	6999.272843	25.699200
183.493767	7000.641812	25.704218
183.271760	7009.979969	25.709236
183.701744	7023.497705	25.714253
184.084196	7038.876813	25.719271
184.137337	7037.496139	25.724288
184.300953	7044.738083	25.729306
184.361638	7065.160200	25.734324
184.388262	7065.801199	25.739341
184.930763	7076.236319	25.744359
185.006727	7095.663840	25.749376
185.330870	7099.699034	25.754394
185.541424	7110.907058	25.759412
185.747952	7119.598635	25.764429
185.899104	7124.803906	25.769447
185.873397	7127.190591	25.774464
186.499173	7143.163634	25.779482
186.498395	7153.321904	25.784500
186.652906	7148.514892	25.789517
187.081191	7154.776780	25.794535
187.164825	7157.661419	25.799552
187.231249	7176.775044	25.804570
187.499756	7190.032660	25.809588
187.469486	7183.332054	25.814605
187.833731	7191.851389	25.819623
188.048337	7216.618511	25.824640
188.236162	7211.806168	25.829658
188.191062	7220.188562	25.834676
188.559267	7232.558892	25.839693
188.509912	7242.465309	25.844711
188.514147	7246.258053	25.849728
188.694251	7269.145482	25.854746
189.306564	7273.534499	25.859764
189.377401	7278.579523	25.864781
189.615542	7291.079222	25.869799
189.451998	7312.753894	25.874816
189.710672	7315.068518	25.879834
189.985423	7321.335283	25.884852
190.402378	7341.086449	25.889869
190.780965	7336.504100	25.894887
190.846227	7338.918806	25.899904
190.972009	7338.260656	25.904922
191.026905	7351.456870	25.909940
191.324833	7370.616455	25.914957
191.479819	7373.714800	25.919975
191.402930	7381.026726	25.924992
191.890203	7389.023762	25.930010
191.842690	7404.754280	25.935028
191.772621	7406.655512	25.940045
192.239299	7417.546748	25.945063
192.577534	7435.954054	25.950080
192.426475	7437.475561	25.955098
192.588451	7457.065310	25.960116
192.891212	7472.600782	25.965133
193.120982	7471.945719	25.970151
193.319678	7498.676696	25.975168
193.792211	7497.014305	25.980186
193.850545	7502.542168	25.985204
194.230790	7525.005440	25.990221
194.194335	7535.058711	25.995239
193.926366	7540.153117	26.000256
194.200353	7556.207084	26.005274
194.494618	7567.388731	26.010292
194.841824	7589.444264	26.015309
195.148738	7598.695315	26.020327
195.136185	7610.693101	26.025344
195.723168	7617.808814	26.030362
196.001752	7620.749018	26.035380
196.505990	7630.149609	26.040397
196.731797	7639.200375	26.045415
196.912682	7657.230165	26.050432
196.816318	7649.730201	26.055450
196.715107	7653.266817	26.060468
196.894867	7661.922849	26.065485
197.088876	7669.914859	26.070503
197.312086	7682.902766	26.075520
197.318141	7688.862369	26.080538
197.511069	7707.110622	26.085556
197.456488	7728.624528	26.090573
197.972224	7734.151161	26.095591
198.034557	7749.625321	26.100608
198.185231	7774.041602	26.105626
198.462451	7779.057827	26.110644
198.768444	7795.871791	26.115661
199.399828	7804.673870	26.120679
200.086226	7795.367488	26.125696
200.241210	7792.329876	26.130714
200.568445	7790.507278	26.135732
200.625459	7794.346829	26.140749
200.925938	7792.441939	26.145767
200.861976	7790.005783	26.150784
200.945576	7795.417991	26.155802
201.122814	7804.210638	26.160820
201.143212	7814.290443	26.165837
201.451115	7817.141816	26.170855
201.216924	7832.584648	26.175872
201.688728	7832.068818	26.180890
201.888594	7834.891781	26.185908
201.914580	7857.431705	26.190925
202.165538	7861.626710	26.195943
202.301303	7855.706669	26.200960
202.180324	7876.879639	26.205978
202.112239	7883.152514	26.210996
202.311895	7899.834829	26.216013
202.792512	7921.672080	26.221031
202.899000	7936.723134	26.226048
203.082898	7948.970791	26.231066
203.180918	7962.079621	26.236084
203.332343	7986.598425	26.241101
203.738842	7993.946898	26.246119
203.857904	8012.106580	26.251136
203.691816	8025.300850	26.256154
204.362651	8043.302178	26.261172
204.612178	8058.289239	26.266189
205.166849	8073.804852	26.271207
205.345344	8073.315711	26.276224
205.523069	8099.846124	26.281242
205.972272	8100.359996	26.286260
205.991772	8103.184616	26.291277
206.364697	8110.942175	26.296295
206.493599	8127.738321	26.301312
206.631791	8140.306604	26.306330
206.747731	8144.733709	26.311348
207.143217	8163.861058	26.316365
207.254146	8169.726625	26.321383
207.007898	8175.109326	26.326400
207.328430	8189.622899	26.331418
207.752062	8195.652266	26.336436
207.740661	8223.136865	26.341453
208.022321	8231.304846	26.346471
208.174464	8242.435690	26.351488
208.656315	8256.280715	26.356506
208.792029	8263.989612	26.361524
208.806269	8292.019899	26.366541
209.076784	8302.303310	26.371559
209.312096	8316.684230	26.376576
209.490250	8338.879565	26.381594
210.167850	8336.829109	26.386612
210.163847	8350.643085	26.391629
210.212633	8359.569459	26.396647
210.503648	8374.499469	26.401664
210.525842	8384.322054	26.406682
210.997927	8403.130606	26.411700
210.769522	8413.474747	26.416717
211.217218	8427.380067	26.421735
210.961846	8437.957907	26.426752
211.372826	8466.868382	26.431770
211.717451	8471.977575	26.436788
211.711323	8481.625323	26.441805
212.176281	8500.158141	26.446823
212.297019	8503.479764	26.451840
212.264635	8520.901297	26.456858
212.886956	8527.529835	26.461876
213.016322	8546.095751	26.466893
213.391228	8557.037869	26.471911
213.818061	8561.941981	26.476928
213.918578	8576.205356	26.481946
214.243802	8581.174462	26.486964
214.159457	8599.763498	26.491981
214.343500	8601.967466	26.496999
214.768112	8610.239953	26.502016
214.645865	8632.086613	26.507034
215.020512	8634.810255	26.512052
215.397308	8658.903529	26.517069
215.627821	8657.181237	26.522087
215.726604	8672.844124	26.527104
215.677839	8692.923145	26.532122
216.103591	8692.089242	26.537140
216.443184	8710.997997	26.542157
216.552084	8719.950807	26.547175
216.570154	8724.943746	26.552192
216.987784	8751.192730	26.557210
217.584962	8746.706529	26.562228
217.420502	8761.102425	26.567245
217.741041	8780.570268	26.572263
217.949817	8787.166485	26.577280
217.658676	8805.137166	26.582298
218.477180	8810.035188	26.587316
218.017527	8827.246225	26.592333
218.209401	8845.909963	26.597351
218.583371	8865.680236	26.602368
218.490570	8893.384430	26.607386
219.243639	8906.329068	26.612404
219.369869	8929.657690	26.617421
219.646349	8939.555780	26.622439
220.063995	8957.178750	26.627456
219.902331	8972.257856	26.632474
220.603954	8980.675254	26.637492
220.716836	8983.600834	26.642509
220.941991	8999.860482	26.647527
221.149622	9013.124312	26.652544
221.431610	9018.378248	26.657562
221.640896	9038.984763	26.662580
221.455100	9054.920055	26.667597
221.895594	9063.789519	26.672615
222.247126	9080.637413	26.677632
221.935155	9100.605878	26.682650
222.240643	9113.346619	26.687668
222.626378	9137.472684	26.692685
222.847719	9150.898135	26.697703
223.137546	9162.747051	26.702720
222.958275	9186.030733	26.707738
223.453608	9196.771158	26.712756
223.578761	9216.812924	26.717773
224.059626	9232.239602	26.722791
224.464335	9253.481019	26.727808
224.333375	9271.279561	26.732826
224.487879	9280.093228	26.737844
224.894396	9302.291360	26.742861
224.880621	9308.750155	26.747879
225.564197	9321.158908	26.752896
225.979623	9326.169759	26.757914
226.341717	9333.189160	26.762932
226.111537	9352.339471	26.767949
226.475105	9355.895254	26.772967
226.902913	9370.467636	26.777984
226.926752	9379.033839	26.783002
227.263808	9390.750281	26.788020
227.091047	9399.237269	26.793037
227.254934	9427.084494	26.798055
227.266242	9439.863359	26.803072
227.435684	9458.061227	26.808090
228.084723	9467.413540	26.813108
228.280635	9494.758031	26.818125
228.374666	9512.713011	26.823143
229.118253	9521.643819	26.828160
228.804499	9536.901586	26.833178
228.971535	9548.898265	26.838196
229.681843	9559.007374	26.843213
229.594999	9581.369954	26.848231
229.895020	9585.184212	26.853248
230.090722	9612.850821	26.858266
230.254180	9614.266137	26.863284
230.556567	9646.512494	26.868301
230.896437	9657.673094	26.873319
231.295418	9671.619607	26.878336
231.580029	9690.169274	26.883354
231.982759	9692.282669	26.888372
232.652329	9708.731549	26.893389
232.149567	9711.151016	26.898407
232.771300	9717.585410	26.903424
233.093875	9735.258686	26.908442
233.018343	9746.635099	26.913460
233.085348	9751.367172	26.918477
232.830462	9761.144718	26.923495
233.364966	9765.537453	26.928512
233.766018	9783.746013	26.933530
234.050218	9802.927435	26.938548
234.781415	9804.822826	26.943565
234.469129	9826.456764	26.948583
234.910302	9833.132476	26.953600
235.062667	9840.281955	26.958618
235.274591	9854.465434	26.963636
235.459747	9875.959940	26.968653
235.377391	9889.054746	26.973671
235.892164	9902.426619	26.978688
235.849612	9919.241873	26.983706
236.103073	9946.833390	26.988724
236.571124	9949.734021	26.993741
236.525577	9963.697367	26.998759
237.203436	9968.855086	27.003776
237.111503	9980.451105	27.008794
237.218219	10000.128937	27.013812
237.585784	10007.525933	27.018829
237.535025	10031.849331	27.023847
237.871173	10042.520516	27.028864
238.014789	10062.932715	27.033882
238.315844	10076.292379	27.038900
238.413876	10093.122405	27.043917
238.529582	10110.261677	27.048935
238.891488	10128.701583	27.053952
239.200690	10159.274011	27.058970
239.119250	10179.596323	27.063988
239.658015	10189.887855	27.069005
239.697175	10214.648951	27.074023
240.382665	10229.203523	27.079040
240.573857	10257.573256	27.084058
240.559753	10278.074634	27.089076
240.891259	10294.559949	27.094093
241.081920	10326.199510	27.099111
241.260668	10329.095966	27.104128
241.433601	10354.348309	27.109146
241.713691	10371.164184	27.114164
242.147269	10391.848163	27.119181
242.399168	10423.058689	27.124199
243.010817	10426.376858	27.129216
242.974508	10448.506008	27.134234
243.501864	10458.868014	27.139252
243.770816	10469.170480	27.144269
244.093598	10487.804177	27.149287
244.574216	10491.410440	27.154304
244.793439	10509.336027	27.159322
244.988904	10518.927761	27.164340
245.374472	10521.247851	27.169357
245.172965	10535.078789	27.174375
245.761645	10547.358488	27.179392
245.711647	10554.516561	27.184410
245.937493	10582.112464	27.189428
246.129096	10587.707582	27.194445
246.560551	10600.549135	27.199463
246.875565	10616.187056	27.204480
246.985479	10627.338995	27.209498
247.503849	10639.026331	27.214516
247.346816	10647.040084	27.219533
247.234746	10674.359864	27.224551
247.604669	10684.386271	27.229568
248.075065	10697.341722	27.234586
247.955075	10720.652950	27.239604
248.326118	10738.835577	27.244621
248.579051	10753.720906	27.249639
248.995086	10762.846344	27.254656
249.377994	10782.760173	27.259674
249.647584	10789.652161	27.264692
250.154168	10805.667817	27.269709
250.340367	10819.460036	27.274727
250.758327	10814.593731	27.279744
250.906698	10817.973247	27.284762
251.165243	10841.603671	27.289780
251.145884	10842.974660	27.294797
251.632007	10845.667568	27.299815
251.764928	10855.215968	27.304832
251.977522	10873.352790	27.309850
252.082459	10878.506925	27.314868
252.616860	10894.260094	27.319885
252.522652	10905.593920	27.324903
253.022861	10916.506776	27.329920
253.282934	10923.052865	27.334938
253.270464	10943.540326	27.339956
253.579989	10942.890121	27.344973
253.755478	10970.454622	27.349991
253.860007	10983.618178	27.355008
254.051295	10988.476826	27.360026
253.962868	11014.448397	27.365044
254.541371	11033.588412	27.370061
254.413745	11058.608475	27.375079
254.832852	11081.580109	27.380096
255.350104	11107.324644	27.385114
255.553661	11129.311877	27.390132
255.949208	11133.799581	27.395149
255.536369	11158.699599	27.400167
256.227545	11178.313744	27.405184
256.551722	11208.430603	27.410202
256.609923	11225.288705	27.415220
257.182505	11237.408224	27.420237
257.090545	11256.414162	27.425255
257.583593	11270.816254	27.430272
258.286181	11295.324223	27.435290
258.414667	11310.372002	27.440308
259.127505	11329.207639	27.445325
259.043208	11350.149820	27.450343
259.133458	11349.239010	27.455360
259.626737	11370.692829	27.460378
259.613282	11387.745919	27.465396
260.295501	11396.334645	27.470413
260.208674	11421.107961	27.475431
260.273583	11427.805604	27.480448
260.765594	11431.481316	27.485466
260.678801	11454.971374	27.490484
260.937174	11486.284597	27.495501
261.048593	11513.648776	27.500519
261.408498	11530.292464	27.505536
261.673796	11546.187595	27.510554
262.230484	11563.949863	27.515572
263.042342	11570.724683	27.520589
263.014852	11581.950586	27.525607
263.203685	11594.243721	27.530624
263.453199	11602.040087	27.535642
263.582188	11613.870533	27.540660
264.142064	11618.192878	27.545677
264.152486	11639.712633	27.550695
264.558446	11645.706082	27.555712
264.842041	11654.826611	27.560730
264.783164	11674.195364	27.565748
265.521077	11660.019606	27.570765
265.830563	11679.179711	27.575783
265.899871	11690.300341	27.580800
266.436518	11690.422627	27.585818
266.052881	11712.903552	27.590836
266.329675	11732.332606	27.595853
266.476850	11741.245499	27.600871
266.801956	11760.142496	27.605888
267.027360	11773.688294	27.610906
266.931719	11795.801322	27.615924
267.617709	11823.366090	27.620941
267.868852	11832.401384	27.625959
268.035637	11860.868927	27.630976
268.535182	11867.954388	27.635994
268.418976	11892.897069	27.641012
268.854819	11900.434453	27.646029
269.317413	11920.404773	27.651047
269.515794	11929.330275	27.656064
270.203698	11954.016982	27.661082
270.076477	11977.171710	27.666100
270.432447	11981.342090	27.671117
270.991116	11999.853673	27.676135
270.818936	12033.240597	27.681152
271.204233	12044.708209	27.686170
271.565005	12063.776407	27.691188
271.752586	12074.292079	27.696205
272.095782	12095.360773	27.701223
272.064752	12115.641636	27.706240
272.336067	12129.845731	27.711258
272.650549	12155.009451	27.716276
273.003808	12165.760096	27.721293
273.386089	12185.502911	27.726311
273.226147	12211.427519	27.731328
273.677893	12235.540747	27.736346
273.711989	12260.606868	27.741364
273.737480	12281.467699	27.746381
274.192043	12307.473195	27.751399
274.402651	12332.373751	27.756416
274.825601	12354.549759	27.761434
275.242024	12380.460512	27.766452
275.564698	12401.844993	27.771469
275.701742	12426.124982	27.776487
276.015214	12449.135801	27.781504
276.786822	12470.222132	27.786522
276.909767	12487.537881	27.791540
277.471775	12498.571518	27.796557
277.843118	12516.431946	27.801575
277.962749	12537.537480	27.806592
278.542654	12547.327206	27.811610
278.398294	12563.183227	27.816628
278.459577	12577.852367	27.821645
279.275909	12586.625252	27.826663
279.187416	12596.663230	27.831680
279.509044	12607.330287	27.836698
279.837812	12615.802689	27.841716
280.166343	12634.491053	27.846733
280.624225	12649.343615	27.851751
280.755578	12656.387975	27.856768
280.907004	12666.277363	27.861786
281.340737	12693.088138	27.866804
281.412533	12694.295800	27.871821
281.500834	12713.606603	27.876839
281.486464	12735.741100	27.881856
281.799623	12749.395592	27.886874
282.165392	12780.647338	27.891892
282.442893	12794.134581	27.896909
282.398940	12814.285212	27.901927
282.641615	12844.818179	27.906944
283.529238	12867.559438	27.911962
283.785291	12886.448381	27.916980
283.960351	12904.876201	27.921997
284.589155	12913.294454	27.927015
284.567432	12945.338178	27.932032
285.149531	12958.008175	27.937050
285.576893	12974.788027	27.942068
285.708174	12994.266982	27.947085
286.072985	13003.583384	27.952103
286.443215	13031.791043	27.957120
286.692515	13039.979891	27.962138
286.416874	13055.182762	27.967156
286.823082	13070.760672	27.972173
287.509955	13090.992363	27.977191
287.435069	13116.127935	27.982208
287.780517	13122.762621	27.987226
288.134495	13157.124795	27.992244
288.029385	13172.623433	27.997261
288.582577	13203.247150	28.002279
288.613730	13225.390255	28.007296
288.736912	13246.060611	28.012314
288.833285	13282.712743	28.017332
288.883183	13312.177120	28.022349
289.473784	13336.632749	28.027367
289.563146	13366.663824	28.032384
290.220405	13393.600985	28.037402
290.967874	13426.754541	28.042420
291.141289	13437.836634	28.047437
291.630541	13464.349652	28.052455
291.806990	13491.777280	28.057472
292.262165	13500.940945	28.062490
292.557758	13533.859466	28.067508
292.377173	13557.769664	28.072525
293.469605	13570.872269	28.077543
293.522253	13593.711494	28.082560
294.552786	13576.195563	28.087578
294.800860	13592.425312	28.092596
294.739543	13613.011628	28.097613
295.240284	13619.674326	28.102631
295.495953	13620.703880	28.107648
296.159043	13605.590205	28.112666
296.403027	13605.849106	28.117684
296.329934	13620.870493	28.122701
296.347053	13627.324826	28.127719
296.499323	13642.122082	28.132736
296.799488	13655.809668	28.137754
297.132778	13678.440753	28.142772
297.288219	13679.811589	28.147789
297.715854	13696.238653	28.152807
297.812035	13720.875447	28.157824
298.332196	13728.929888	28.162842
298.647309	13738.454117	28.167860
298.559641	13762.006611	28.172877
299.174410	13765.925769	28.177895
299.346205	13791.799398	28.182912
299.550300	13801.994628	28.187930
299.752303	13820.287702	28.192948
299.801552	13839.658109	28.197965
300.063460	13860.813940	28.202983
300.106051	13887.806355	28.208000
300.893997	13913.925202	28.213018
301.056057	13934.841113	28.218036
301.091143	13969.511191	28.223053
301.500530	13990.198537	28.228071
301.846717	14013.019449	28.233088
302.143135	14043.491147	28.238106
302.347170	14067.335820	28.243124
302.649817	14101.923406	28.248141
303.455550	14108.507895	28.253159
303.927325	14138.165712	28.258176
304.167242	14142.143927	28.263194
304.610241	14168.590562	28.268212
304.741467	14183.257256	28.273229
305.351956	14203.562926	28.278247
305.657570	14211.490343	28.283264
305.923508	14235.182041	28.288282
306.611056	14252.081836	28.293300
306.258597	14261.646763	28.298317
306.649592	14273.268170	28.303335
306.713968	14302.985827	28.308352
307.242556	14324.197017	28.313370
307.516864	14340.141362	28.318388
307.648304	14356.952487	28.323405
307.669525	14367.050696	28.328423
308.041574	14398.760065	28.333440
308.093467	14431.376331	28.338458
308.589857	14452.102589	28.343476
308.558686	14479.981028	28.348493
309.417285	14505.082575	28.353511
309.606941	14531.020930	28.358528
310.099476	14546.508363	28.363546
310.240672	14568.254265	28.368564
310.409957	14599.185718	28.373581
310.921374	14621.797979	28.378599
310.815657	14643.117693	28.383616
310.872290	14664.859693	28.388634
311.609268	14691.917816	28.393652
311.818911	14715.915132	28.398669
312.195083	14736.467867	28.403687
312.736001	14763.674072	28.408704
312.949358	14779.582831	28.413722
313.210889	14797.655033	28.418740
313.484861	14840.002169	28.423757
314.001239	14855.116014	28.428775
314.101215	14876.487406	28.433792
314.783503	14902.657851	28.438810
314.970532	14926.427651	28.443828
315.271356	14939.183989	28.448845
315.817128	14959.055202	28.453863
316.065226	14992.562665	28.458880
316.510805	15011.468315	28.463898
316.821709	15016.349048	28.468916
316.834791	15046.174824	28.473933
317.294574	15058.348849	28.478951
317.794317	15081.440331	28.483968
317.835129	15103.749835	28.488986
318.070795	15117.903751	28.494004
318.201405	15147.080203	28.499021
318.488768	15183.938684	28.504039
318.559362	15207.944858	28.509056
318.713972	15245.112485	28.514074
319.374504	15271.016309	28.519092
319.352905	15310.266243	28.524109
319.787551	15332.201259	28.529127
320.495586	15361.299277	28.534144
320.603758	15397.368662	28.539162
320.889245	15421.062324	28.544180
321.146606	15454.103843	28.549197
321.774536	15483.835328	28.554215
321.914382	15510.111371	28.559232
322.408210	15538.498020	28.564250
322.970920	15556.164215	28.569268
323.020804	15589.374306	28.574285
323.388666	15611.480182	28.579303
323.950394	15639.265146	28.584320
324.212060	15671.955909	28.589338
324.672124	15689.904129	28.594356
324.899132	15709.804190	28.599373
324.975204	15737.838557	28.604391
325.257884	15762.102400	28.609408
325.675872	15796.987879	28.614426
326.364899	15826.595347	28.619444
326.729647	15848.506222	28.624461
326.864439	15867.664005	28.629479
327.412325	15890.569234	28.634496
327.250624	15921.532576	28.639514
327.778793	15938.582164	28.644532
328.039973	15965.858999	28.649549
328.443618	15985.523812	28.654567
328.517329	16006.048607	28.659584
328.733678	16042.109543	28.664602
329.477078	16064.524284	28.669620
329.548508	16086.041945	28.674637
329.693789	16106.563145	28.679655
329.938483	16129.252122	28.684672
330.336177	16155.479117	28.689690
330.483671	16175.113153	28.694708
330.790070	16215.213009	28.699725
331.103274	16246.235157	28.704743
331.693008	16269.838927	28.709760
331.967263	16309.357011	28.714778
332.363883	16327.362735	28.719796
332.538093	16360.740281	28.724813
332.676816	16391.202992	28.729831
333.274309	16421.546591	28.734848
333.553541	16458.458427	28.739866
334.036118	16485.478084	28.744884
334.350121	16522.696117	28.749901
335.154282	16546.751918	28.754919
335.659548	16568.978007	28.759936
335.477581	16599.826655	28.764954
335.816819	16627.158748	28.769972
336.190764	16648.731137	28.774989
337.025451	16662.287903	28.780007
337.980009	16676.609369	28.785024
337.892057	16689.467995	28.790042
338.608432	16704.852162	28.795060
338.344219	16709.970653	28.800077
338.909397	16736.326657	28.805095
339.026228	16746.983385	28.810112
339.175550	16774.954027	28.815130
339.710458	16795.422906	28.820148
339.841401	16819.203383	28.825165
340.099692	16847.201078	28.830183
340.170128	16869.002249	28.835200
340.482633	16904.818197	28.840218
341.210741	16925.860157	28.845236
341.242552	16964.286349	28.850253
341.812747	16976.900573	28.855271
342.265243	17000.252549	28.860288
342.238174	17039.163672	28.865306
342.766761	17056.906517	28.870324
343.317786	17087.483622	28.875341
343.145771	17111.865945	28.880359
343.699737	17135.525951	28.885376
343.986392	17185.875977	28.890394
344.325554	17217.054984	28.895412
344.452781	17246.472642	28.900429
344.765519	17264.698725	28.905447
345.613759	17291.079657	28.910464
345.560367	17321.812403	28.915482
346.231447	17344.272229	28.920500
346.541499	17373.968066	28.925517
346.755579	17392.567488	28.930535
347.528847	17400.696726	28.935552
347.916368	17427.633972	28.940570
348.089441	17439.354418	28.945588
348.237003	17471.243187	28.950605
348.803302	17494.736036	28.955623
349.454922	17503.571701	28.960640
349.637490	17537.880539	28.965658
349.974602	17545.076636	28.970676
350.350379	17560.241538	28.975693
350.808986	17580.541932	28.980711
351.276833	17589.310478	28.985728
351.582981	17610.154090	28.990746
351.885517	17616.750628	28.995764
352.209138	17643.164982	29.000781
352.616759	17658.154044	29.005799
353.094989	17672.151968	29.010816
353.132352	17700.941909	29.015834
353.554475	17719.846359	29.020852
353.870195	17742.215761	29.025869
354.133641	17761.214444	29.030887
354.788415	17772.707594	29.035904
355.087123	17791.278261	29.040922
355.298695	17810.002598	29.045940
355.401928	17836.354372	29.050957
355.756946	17859.579088	29.055975
356.373115	17867.953295	29.060992
356.284846	17904.691123	29.066010
356.563184	17929.482090	29.071028
357.037410	17953.266686	29.076045
357.029136	17985.885674	29.081063
357.556341	18010.744591	29.086080
357.676751	18057.908978	29.091098
358.278549	18076.978539	29.096116
358.738778	18110.889670	29.101133
358.843863	18147.996868	29.106151
359.554891	18175.357880	29.111168
359.995255	18203.630982	29.116186
360.024689	18239.508706	29.121204
360.640199	18257.539675	29.126221
360.786412	18298.891140	29.131239
361.334576	18326.529558	29.136256
361.536066	18361.778164	29.141274
361.720227	18385.075383	29.146292
361.765689	18422.552980	29.151309
362.124370	18451.347830	29.156327
362.941768	18491.355411	29.161344
363.142241	18528.149879	29.166362
363.596041	18550.875225	29.171380
364.307796	18587.034793	29.176397
364.617502	18619.790662	29.181415
364.931553	18648.428810	29.186432
365.161351	18676.539862	29.191450
365.357207	18701.846012	29.196468
366.073943	18728.010187	29.201485
365.965477	18764.529625	29.206503
366.558962	18788.859122	29.211520
366.941550	18815.963745	29.216538
367.255488	18846.016126	29.221556
367.593146	18882.037559	29.226573
367.933112	18905.934384	29.231591
368.239641	18933.657667	29.236608
368.785023	18961.862259	29.241626
369.320563	18984.029904	29.246644
369.834430	19000.826283	29.251661
370.054785	19029.701335	29.256679
370.959637	19035.889881	29.261696
371.270415	19063.348526	29.266714
371.402499	19094.082377	29.271732
372.042564	19105.808410	29.276749
372.297365	19131.801190	29.281767
372.729013	19158.558410	29.286784
372.955806	19188.779681	29.291802
373.357499	19209.770461	29.296820
373.585236	19221.923733	29.301837
373.644637	19258.628615	29.306855
373.982001	19277.249625	29.311872
374.568321	19311.259824	29.316890
375.020817	19344.651997	29.321908
375.274554	19363.022240	29.326925
375.643206	19397.724457	29.331943
375.907863	19419.273624	29.336960
376.501798	19449.156554	29.341978
376.985118	19483.929280	29.346996
377.397616	19505.210890	29.352013
377.652218	19542.616899	29.357031
377.841231	19560.448816	29.362048
378.375127	19583.932669	29.367066
378.555949	19616.642264	29.372084
379.055419	19644.215972	29.377101
379.463334	19679.847696	29.382119
380.079185	19689.491981	29.387136
380.694441	19719.765381	29.392154
381.125934	19742.486572	29.397172
381.529132	19766.784923	29.402189
381.824043	19798.601817	29.407207
382.389912	19809.414904	29.412224
382.460097	19831.021616	29.417242
382.859690	19850.927247	29.422260
383.396697	19875.892322	29.427277
383.498262	19905.427762	29.432295
384.031634	19925.425177	29.437312
384.464153	19955.237935	29.442330
384.541349	19985.948028	29.447348
384.859131	20010.243831	29.452365
384.908817	20048.736592	29.457383
385.524647	20064.616574	29.462400
385.600155	20097.269929	29.467418
386.056402	20121.957281	29.472436
386.586656	20154.092562	29.477453
387.009713	20174.832778	29.482471
387.720356	20206.714588	29.487488
387.853535	20225.955176	29.492506
387.994986	20253.004249	29.497524
388.738354	20271.678303	29.502541
388.830198	20302.389043	29.507559
389.467385	20327.237286	29.512576
389.992578	20358.432709	29.517594
390.187252	20376.346163	29.522612
390.613553	20410.681149	29.527629
390.756490	20443.495765	29.532647
391.311089	20463.431028	29.537664
391.736272	20490.836150	29.542682
391.748919	20521.348487	29.547700
392.617267	20548.557089	29.552717
393.090553	20588.767035	29.557735
393.291478	20610.160648	29.562752
393.909967	20639.332376	29.567770
394.069594	20661.043714	29.572788
394.537912	20683.514694	29.577805
394.564650	20715.485254	29.582823
394.799186	20745.133391	29.587840
395.333985	20787.699026	29.592858
395.636488	20826.557022	29.597876
396.128345	20862.070165	29.602893
396.533494	20890.882582	29.607911
396.922451	20931.902266	29.612928
397.568709	20962.792539	29.617946
398.162869	20993.721890	29.622964
398.626944	21016.482267	29.627981
399.049274	21048.863789	29.632999
399.325752	21076.003807	29.638016
399.596528	21116.099311	29.643034
399.702338	21150.322382	29.648052
400.320521	21172.607158	29.653069
400.480083	21211.074623	29.658087
401.630682	21233.603065	29.663104
402.331634	21253.786150	29.668122
402.382723	21283.386563	29.673140
402.946583	21297.998257	29.678157
403.446820	21325.172358	29.683175
403.748514	21349.876821	29.688192
403.905296	21368.520431	29.693210
404.184560	21412.415364	29.698228
404.464059	21428.213682	29.703245
404.729184	21459.628756	29.708263
405.403946	21500.408276	29.713280
405.768353	21517.021685	29.718298
405.991407	21555.468848	29.723316
406.573251	21584.158297	29.728333
407.220161	21620.917242	29.733351
407.556388	21648.794568	29.738368
408.052162	21672.896828	29.743386
407.980597	21708.945856	29.748404
408.449529	21726.251659	29.753421
408.684251	21761.822769	29.758439
408.862768	21790.699725	29.763456
409.941807	21818.195938	29.768474
409.914841	21849.553579	29.773492
410.352098	21872.939307	29.778509
410.871713	21913.336643	29.783527
411.297829	21924.017130	29.788544
411.782631	21957.367188	29.793562
411.977125	21987.935297	29.798580
412.191090	22021.676765	29.803597
412.754086	22050.608711	29.808615
412.847460	22093.830252	29.813632
413.388335	22124.224505	29.818650
413.656278	22156.947947	29.823668
414.199920	22199.184405	29.828685
414.613344	22231.578440	29.833703
414.740214	22272.138511	29.838720
415.328232	22310.030798	29.843738
415.497438	22362.277322	29.848756
416.178435	22393.699665	29.853773
416.311696	22438.758825	29.858791
416.667351	22480.393524	29.863808
417.330274	22510.850201	29.868826
417.881172	22563.079102	29.873844
418.290338	22601.944166	29.878861
419.029727	22636.779161	29.883879
419.382107	22671.674321	29.888896
420.242864	22699.573107	29.893914
420.552729	22742.169619	29.898932
420.975903	22765.988964	29.903949
421.477830	22794.412162	29.908967
421.714912	22833.845536	29.913984
422.130253	22857.207071	29.919002
422.550256	22903.103237	29.924020
423.260716	22928.783947	29.929037
423.619899	22963.871640	29.934055
423.637992	22991.076597	29.939072
424.287960	23017.788673	29.944090
424.752983	23058.988437	29.949108
425.416359	23094.371369	29.954125
425.988311	23118.455823	29.959143
425.841176	23148.149592	29.964160
425.922159	23186.116886	29.969178
426.364961	23232.631837	29.974196
426.786170	23274.872556	29.979213
427.291116	23317.253640	29.984231
427.632824	23352.941242	29.989248
428.165084	23389.704453	29.994266
428.470453	23440.377968	29.999284
428.981162	23477.121185	30.004301
429.615018	23503.622400	30.009319
429.942020	23551.736814	30.014336
430.497698	23592.495021	30.019354
430.767481	23619.405743	30.024372
431.184167	23646.941367	30.029389
431.641254	23689.723337	30.034407
432.086574	23729.988272	30.039424
432.358790	23755.683434	30.044442
432.407670	23800.989118	30.049460
432.908668	23836.438174	30.054477
433.734114	23872.967532	30.059495
433.794138	23912.487718	30.064512
434.682675	23950.240735	30.069530
435.109466	23984.682663	30.074548
435.920595	24016.412814	30.079565
436.414253	24047.590230	30.084583
436.354323	24088.193362	30.089600
437.108233	24116.603201	30.094618
437.367940	24158.186692	30.099636
437.803142	24192.231511	30.104653
438.733907	24220.307727	30.109671
438.797005	24255.791251	30.114688
439.567790	24280.238072	30.119706
439.580328	24326.966563	30.124724
439.733729	24355.120395	30.129741
439.978155	24393.966463	30.134759
440.380872	24445.798218	30.139776
441.173237	24481.343291	30.144794
441.085715	24534.153021	30.149812
441.182785	24579.829769	30.154829
442.157097	24627.677300	30.159847
442.434720	24669.263206	30.164864
443.316848	24709.420060	30.169882
443.882292	24757.055051	30.174900
444.432904	24793.251410	30.179917
445.126368	24839.321492	30.184935
445.303648	24873.856296	30.189952
445.857789	24906.564220	30.194970
446.105481	24949.731115	30.199988
446.470242	24996.203779	30.205005
447.271099	25031.891310	30.210023
447.562082	25079.153481	30.215040
448.044496	25110.170913	30.220058
448.367131	25146.480018	30.225076
448.698227	25186.618729	30.230093
449.290078	25235.599583	30.235111
449.497220	25275.465218	30.240128
450.448066	25306.547835	30.245146
450.499010	25352.442106	30.250164
450.892919	25394.855857	30.255181
451.853561	25428.378449	30.260199
451.830983	25471.583507	30.265216
452.488281	25509.611031	30.270234
452.422865	25562.220529	30.275252
452.813943	25599.065684	30.280269
453.730443	25653.240341	30.285287
453.662134	25703.449602	30.290304
454.252102	25746.069382	30.295322
454.759134	25791.013073	30.300340
455.381629	25836.159076	30.305357
455.674577	25859.508277	30.310375
456.057545	25911.740244	30.315392
456.301471	25947.078958	30.320410
456.650342	25991.772680	30.325428
457.063972	26044.424028	30.330445
457.764124	26082.319248	30.335463
458.163877	26133.181634	30.340480
458.664681	26174.635837	30.345498
459.091065	26215.990134	30.350516
459.694107	26270.293232	30.355533
460.394981	26308.348796	30.360551
461.243825	26363.974393	30.365568
461.590149	26394.663839	30.370586
462.020585	26441.612370	30.375604
462.508153	26482.792164	30.380621
463.013542	26511.775278	30.385639
463.569145	26557.806876	30.390656
463.988422	26593.303425	30.395674
464.264424	26633.107097	30.400692
464.665898	26678.928822	30.405709
465.067948	26706.611496	30.410727
465.385564	26748.743174	30.415744
465.698491	26792.430902	30.420762
466.649971	26836.923034	30.425780
467.023280	26887.191681	30.430797
467.404938	26934.065119	30.435815
467.331498	26982.790943	30.440832
468.032973	27024.936247	30.445850
468.749798	27073.435600	30.450868
469.454824	27121.930677	30.455885
470.015608	27166.325240	30.460903
470.480381	27205.084703	30.465920
471.168950	27248.308862	30.470938
471.676351	27277.380487	30.475956
472.430117	27314.348273	30.480973
473.071558	27345.727592	30.485991
473.314888	27372.770950	30.491008
474.150134	27397.321788	30.496026
474.311004	27426.565493	30.501044
474.296856	27477.353879	30.506061
474.976969	27506.283374	30.511079
475.460240	27544.181924	30.516096
475.728348	27585.501133	30.521114
475.777365	27628.172683	30.526132
476.164520	27682.794629	30.531149
476.595027	27729.097681	30.536167
477.246177	27779.722724	30.541184
477.985437	27824.535032	30.546202
478.669364	27860.667429	30.551220
479.006662	27911.892832	30.556237
479.780461	27935.229895	30.561255
480.715203	27958.982574	30.566272
481.408336	27997.843078	30.571290
482.191254	28010.468138	30.576308
482.271811	28042.366781	30.581325
482.880311	28062.665437	30.586343
482.887130	28090.322840	30.591360
483.039992	28108.278435	30.596378
483.548946	28146.172730	30.601396
483.597635	28178.861470	30.606413
484.134014	28215.300235	30.611431
484.784502	28264.521275	30.616448
484.944265	28297.933195	30.621466
485.192902	28344.728697	30.626484
485.238125	28393.772357	30.631501
485.904640	28441.543193	30.636519
486.485201	28504.818382	30.641536
486.881572	28548.614171	30.646554
487.557254	28592.378189	30.651572
487.617245	28648.041989	30.656589
488.215075	28704.903049	30.661607
488.832848	28759.928399	30.666624
489.425554	28808.523644	30.671642
490.222078	28861.062502	30.676660
490.647337	28912.308567	30.681677
491.246583	28963.963597	30.686695
491.949872	29006.031831	30.691712
492.535865	29048.166137	30.696730
493.266575	29084.478192	30.701748
493.671731	29132.270633	30.706765
494.107996	29160.074189	30.711783
494.398351	29205.997199	30.716800
494.892982	29249.626361	30.721818
495.139468	29300.947830	30.726836
495.287961	29350.839948	30.731853
496.071583	29395.224032	30.736871
496.852950	29454.753315	30.741888
497.118093	29503.722732	30.746906
497.820204	29544.542828	30.751924
498.975683	29591.240005	30.756941
499.285757	29627.045059	30.761959
500.796399	29642.127428	30.766976
501.416852	29662.958861	30.771994
502.174872	29697.454014	30.777012
502.542107	29721.312298	30.782029
503.153646	29737.154183	30.787047
503.151373	29763.170570	30.792064
503.586462	29805.144913	30.797082
504.182177	29817.207074	30.802100
504.365125	29837.739648	30.807117
504.692630	29878.620258	30.812135
504.979581	29903.828025	30.817152
505.460156	29959.563261	30.822170
505.782025	29992.946531	30.827188
505.706154	30039.784411	30.832205
506.655905	30079.953343	30.837223
507.114373	30123.540173	30.842240
507.188688	30174.795680	30.847258
507.779553	30212.125412	30.852276
508.021234	30260.281313	30.857293
508.419894	30298.864846	30.862311
509.070422	30350.071665	30.867328
509.164822	30397.427171	30.872346
509.827658	30445.415663	30.877364
510.298565	30491.767424	30.882381
511.190490	30543.098727	30.887399
511.724823	30589.606146	30.892416
511.977100	30654.420301	30.897434
512.633882	30687.542025	30.902452
513.589835	30734.433446	30.907469
514.015531	30777.738821	30.912487
514.845169	30820.447256	30.917504
515.106435	30863.630900	30.922522
515.667673	30903.334187	30.927540
515.908771	30948.080003	30.932557
516.494613	31001.721596	30.937575
516.965478	31037.069126	30.942592
517.388023	31088.251527	30.947610
518.269873	31133.947036	30.952628
518.647318	31183.748379	30.957645
519.206092	31240.783682	30.962663
519.508185	31285.058901	30.967680
519.987149	31344.556552	30.972698
520.295015	31386.258903	30.977716
520.637993	31447.569060	30.982733
521.291944	31499.856997	30.987751
521.639730	31555.738599	30.992768
522.233142	31619.547083	30.997786
522.798832	31671.682555	31.002804
523.262301	31728.763102	31.007821
523.843497	31774.071690	31.012839
524.972303	31820.202621	31.017856
525.435134	31878.878865	31.022874
526.059387	31929.308294	31.027892
526.411013	31983.712288	31.032909
527.149975	32028.801002	31.037927
527.594726	32076.010964	31.042944
527.802119	32127.435773	31.047962
528.865718	32174.306285	31.052980
529.345071	32230.186556	31.057997
529.600305	32275.772267	31.063015
530.557840	32309.356898	31.068032
530.443772	32370.861506	31.073050
531.148361	32410.679579	31.078068
532.147285	32462.408084	31.083085
532.500224	32512.999156	31.088103
533.293546	32560.935216	31.093120
533.423780	32612.038087	31.098138
533.890343	32662.026733	31.103156
534.266576	32710.653855	31.108173
534.560113	32775.972608	31.113191
535.235598	32834.006790	31.118208
535.444897	32889.970138	31.123226
536.170341	32921.682557	31.128244
536.731257	32978.063075	31.133261
536.794805	33038.882990	31.138279
537.647673	33091.673922	31.143296
537.931990	33149.995351	31.148314
538.475620	33193.702856	31.153332
539.047005	33250.282823	31.158349
539.461280	33311.028956	31.163367
540.325723	33380.866692	31.168384
540.439682	33435.661683	31.173402
541.046490	33495.359524	31.178420
541.610543	33562.451056	31.183437
542.230230	33623.625902	31.188455
542.697164	33679.891365	31.193472
542.936486	33745.928773	31.198490
543.189015	33804.916477	31.203508
544.057311	33864.637051	31.208525
544.426215	33945.401422	31.213543
545.555289	34001.899852	31.218560
545.954788	34067.172129	31.223578
547.027888	34121.482417	31.228596
547.521026	34181.891286	31.233613
547.968828	34248.045660	31.238631
549.086451	34291.084520	31.243648
549.365963	34350.558544	31.248666
549.637728	34406.960020	31.253684
550.726041	34460.485521	31.258701
551.035583	34515.815694	31.263719
551.762824	34578.271162	31.268736
551.871353	34640.694566	31.273754
552.557012	34693.950748	31.278772
553.330835	34753.730551	31.283789
554.127693	34800.215897	31.288807
554.773830	34841.162093	31.293824
555.039570	34900.539379	31.298842
555.801365	34942.151584	31.303860
556.640348	34998.898244	31.308877
556.841564	35054.209622	31.313895
557.583161	35099.285783	31.318912
557.683427	35152.638245	31.323930
558.473147	35207.512725	31.328948
558.798438	35259.995730	31.333965
559.031714	35325.371924	31.338983
559.639695	35376.028831	31.344000
560.073084	35448.660210	31.349018
560.561364	35506.019381	31.354036
561.636071	35567.961294	31.359053
562.045889	35631.261093	31.364071
562.803207	35683.425949	31.369088
563.246429	35748.582750	31.374106
563.935798	35800.017822	31.379124
564.464770	35864.876064	31.384141
564.997409	35931.587997	31.389159
565.480152	35978.850291	31.394176
565.671827	36043.704614	31.399194
566.562847	36103.801660	31.404212
567.058865	36148.243417	31.409229
567.252906	36205.814235	31.414247
568.200309	36254.568840	31.419264
568.643788	36316.899422	31.424282
569.057655	36372.250650	31.429300
569.587476	36430.301645	31.434317
569.779409	36500.948533	31.439335
570.625840	36558.284217	31.444352
571.105695	36617.980338	31.449370
571.401548	36690.430884	31.454388
571.969202	36754.753504	31.459405
572.651221	36824.806563	31.464423
573.402049	36884.435246	31.469440
574.131440	36951.859338	31.474458
575.096785	37009.311637	31.479476
575.763548	37067.938997	31.484493
576.138879	37140.974798	31.489511
576.964131	37194.662898	31.494528
577.289647	37252.440241	31.499546
577.675063	37319.463352	31.504564
578.360511	37381.283181	31.509581
578.873378	37440.392009	31.514599
579.861477	37499.229846	31.519616
581.046606	37529.927081	31.524634
582.071252	37576.626669	31.529652
582.836835	37616.453779	31.534669
583.358296	37669.978923	31.539687
584.194029	37696.128108	31.544704
584.629305	37743.199524	31.549722
584.799145	37788.717701	31.554740
585.647971	37835.788159	31.559757
586.094307	37869.812321	31.564775
586.570065	37912.969047	31.569792
587.118536	37966.954391	31.574810
587.674304	38011.740013	31.579828
588.227079	38059.829520	31.584845
588.401437	38127.524881	31.589863
588.958282	38174.392080	31.594880
589.402067	38220.943141	31.599898
589.550154	38281.528943	31.604916
590.060162	38345.042157	31.609933
590.481319	38412.920101	31.614951
591.092535	38483.606267	31.619968
591.428553	38561.337527	31.624986
592.116860	38623.265513	31.630004
592.725896	38693.563431	31.635021
593.064755	38778.110197	31.640039
593.501362	38841.734723	31.645056
594.114810	38925.114215	31.650074
594.390927	39003.484616	31.655092
595.462394	39069.546019	31.660109
595.860916	39155.080145	31.665127
596.667953	39225.454379	31.670144
597.528766	39300.790617	31.675162
597.881361	39363.932187	31.680180
598.774284	39436.316741	31.685197
599.632832	39489.177387	31.690215
600.817626	39541.655094	31.695232
601.246944	39587.966213	31.700250
601.703925	39648.550267	31.705268
602.609685	39699.057625	31.710285
603.195564	39748.338783	31.715303
603.577624	39799.584257	31.720320
604.358667	39867.434347	31.725338
604.859963	39912.139045	31.730356
605.932359	39958.407104	31.735373
606.449764	40021.933290	31.740391
606.690688	40069.701266	31.745408
607.417587	40125.768689	31.750426
607.768377	40183.045786	31.755444
608.405759	40224.717665	31.760461
608.903371	40287.375938	31.765479
609.472324	40351.234185	31.770496
610.041768	40414.351418	31.775514
610.263699	40483.500954	31.780532
610.990720	40546.823820	31.785549
611.429024	40621.562966	31.790567
611.934253	40691.841505	31.795584
612.774480	40749.135597	31.800602
613.364014	40825.677714	31.805620
614.179849	40898.333071	31.810637
614.336481	40967.636890	31.815655
614.770363	41042.302878	31.820672
615.468494	41117.949025	31.825690
615.961656	41201.598503	31.830708
616.944300	41275.323360	31.835725
617.514041	41345.455525	31.840743
618.409581	41407.300694	31.845760
619.204281	41480.539088	31.850778
620.284147	41531.114034	31.855796
620.843129	41584.226007	31.860813
621.798208	41650.992509	31.865831
622.504143	41704.996161	31.870848
623.145034	41768.018685	31.875866
623.698085	41827.049601	31.880884
624.661341	41874.666573	31.885901
625.069923	41923.501215	31.890919
625.481634	41983.652842	31.895936
626.192626	42041.760391	31.900954
626.360561	42110.022963	31.905972
627.133401	42163.351855	31.910989
627.439521	42226.031931	31.916007
628.094164	42281.843495	31.921024
628.774279	42344.145861	31.926042
629.201455	42417.320600	31.931060
630.232186	42474.542803	31.936077
631.052849	42536.965430	31.941095
631.546909	42606.386139	31.946112
632.502012	42653.479793	31.951130
633.084500	42716.761128	31.956148
634.001284	42755.234001	31.961165
634.610220	42803.774266	31.966183
635.080544	42840.012578	31.971200
635.933851	42888.842223	31.976218
636.158000	42937.418902	31.981236
636.918649	42983.374143	31.986253
637.578630	43038.584816	31.991271
637.839128	43088.909987	31.996288
638.435564	43147.771333	32.001306
638.766093	43219.214147	32.006324
639.200817	43276.067062	32.011341
639.947908	43338.885994	32.016359
640.358090	43412.550286	32.021376
640.894937	43474.636650	32.026394
641.365387	43552.717696	32.031412
641.950955	43621.279343	32.036429
642.353270	43700.078514	32.041447
643.059608	43772.179842	32.046464
644.334347	43831.667356	32.051482
645.196461	43905.542533	32.056500
645.768987	43971.041395	32.061517
646.558082	44048.099163	32.066535
647.319875	44108.476885	32.071552
648.176788	44161.852189	32.076570
648.572194	44228.301374	32.081588
649.196637	44297.307458	32.086605
649.880453	44357.269431	32.091623
650.225084	44437.043298	32.096640
650.663999	44501.814625	32.101658
651.358038	44579.653318	32.106676
652.064014	44657.323259	32.111693
652.599651	44723.793016	32.116711
653.286037	44797.185745	32.121728
654.331423	44865.858903	32.126746
654.987192	44950.447040	32.131764
655.772183	45012.814862	32.136781
656.499987	45079.069243	32.141799
657.046516	45148.832482	32.146816
658.036061	45213.834256	32.151834
658.805242	45279.183688	32.156852
659.233595	45339.006738	32.161869
659.736165	45407.446670	32.166887
660.454924	45471.382016	32.171904
661.217862	45535.096031	32.176922
661.418146	45612.497400	32.181940
661.797654	45679.629787	32.186957
662.638929	45754.998926	32.191975
663.051005	45829.004398	32.196992
663.630372	45910.211497	32.202010
663.970418	45998.849126	32.207028
665.203255	46070.260911	32.212045
665.945072	46153.667520	32.217063
666.535022	46232.451404	32.222080
667.384942	46302.801932	32.227098
667.711904	46376.072373	32.232116
667.883462	46459.334609	32.237133
668.586530	46529.204621	32.242151
669.026998	46606.553198	32.247168
669.996713	46688.156071	32.252186
670.558039	46779.453681	32.257204
670.779011	46857.658634	32.262221
671.685261	46934.133090	32.267239
672.125741	47025.072601	32.272256
673.243660	47107.022971	32.277274
673.931553	47196.844914	32.282292
674.136769	47281.017515	32.287309
675.496338	47357.633029	32.292327
675.852221	47451.983200	32.297344
676.489049	47538.890136	32.302362
677.218543	47628.101847	32.307380
678.021043	47703.078489	32.312397
678.658449	47785.420892	32.317415
679.584215	47875.659618	32.322432
681.023471	47946.535007	32.327450
681.652341	48030.713141	32.332468
682.152625	48110.794445	32.337485
683.079531	48181.430511	32.342503
683.384794	48256.756877	32.347520
684.027241	48329.650729	32.352538
684.291392	48414.141185	32.357556
685.134254	48499.082629	32.362573
685.826802	48584.427063	32.367591
686.467611	48684.534929	32.372608
687.177083	48752.898120	32.377626
688.138797	48847.462187	32.382644
688.510011	48931.622513	32.387661
689.330959	49002.856176	32.392679
689.843690	49094.403823	32.397696
690.545361	49178.941853	32.402714
691.186425	49275.613495	32.407732
691.682462	49369.607600	32.412749
692.601725	49459.347377	32.417767
693.233655	49553.813086	32.422784
694.314010	49625.626437	32.427802
695.296795	49712.447918	32.432820
695.985573	49791.238229	32.437837
697.633852	49851.545020	32.442855
698.093397	49925.490653	32.447872
698.846915	49985.918270	32.452890
699.779565	50062.253716	32.457908
700.470607	50130.236986	32.462925
701.221633	50198.169941	32.467943
701.448805	50270.169064	32.472960
702.330998	50329.065772	32.477978
703.011280	50399.162956	32.482996
703.647425	50473.114297	32.488013
704.032917	50536.335247	32.493031
704.568931	50617.419360	32.498048
705.244926	50696.502875	32.503066
705.995472	50771.387126	32.508084
706.550200	50840.196371	32.513101
707.036596	50903.172177	32.518119
707.643757	50983.378767	32.523136
707.995856	51056.434144	32.528154
708.957346	51128.726910	32.533172
709.762291	51211.440344	32.538189
710.695936	51285.776873	32.543207
711.176711	51379.540969	32.548224
711.539704	51445.375483	32.553242
712.602471	51524.306394	32.558260
713.292020	51616.290100	32.563277
713.887149	51697.473827	32.568295
714.555354	51792.766124	32.573312
715.327806	51867.916564	32.578330
716.095664	51945.709625	32.583348
716.304950	52051.655285	32.588365
717.187970	52139.122996	32.593383
717.607978	52236.631665	32.598400
718.062859	52327.034148	32.603418
718.958957	52420.661794	32.608436
719.477271	52528.050722	32.613453
720.174014	52625.264942	32.618471
720.820675	52723.592308	32.623488
721.749418	52830.823008	32.628506
722.501092	52930.728642	32.633524
723.222635	53028.092576	32.638541
724.178867	53112.861114	32.643559
724.875444	53213.458820	32.648576
725.997096	53309.643266	32.653594
727.008859	53402.389614	32.658612
727.217673	53504.142871	32.663629
728.074201	53597.880753	32.668647
728.802582	53703.475681	32.673664
729.571012	53792.894981	32.678682
730.414704	53875.825928	32.683700
731.236054	53972.838159	32.688717
732.040419	54059.131412	32.693735
732.952968	54157.657794	32.698752
733.539158	54245.738462	32.703770
734.806758	54337.845986	32.708788
735.215290	54426.268295	32.713805
736.160705	54507.790785	32.718823
736.709592	54599.262815	32.723840
737.417638	54681.360470	32.728858
738.241250	54766.366166	32.733876
738.832933	54860.998660	32.738893
740.024536	54946.574759	32.743911
740.719110	55030.573201	32.748928
741.447412	55120.336844	32.753946
742.004447	55212.479837	32.758964
742.761630	55282.602658	32.763981
743.647153	55370.899943	32.768999
744.452203	55451.953410	32.774016
745.085002	55531.311141	32.779034
746.208609	55609.981850	32.784052
746.462539	55686.089249	32.789069
747.118181	55758.048288	32.794087
747.962333	55836.758146	32.799104
748.497070	55922.557024	32.804122
749.467314	55998.141315	32.809140
750.194921	56081.002904	32.814157
751.187425	56150.078278	32.819175
751.428105	56244.423398	32.824192
751.982664	56313.193450	32.829210
752.733295	56395.190995	32.834228
753.223050	56498.491420	32.839245
754.204587	56587.928353	32.844263
754.910021	56685.267008	32.849280
755.621101	56772.203490	32.854298
756.784493	56850.702718	32.859316
757.755977	56947.997253	32.864333
758.347701	57032.207486	32.869351
758.964532	57117.945202	32.874368
759.722661	57209.665273	32.879386
760.758167	57277.993008	32.884404
761.511320	57374.797343	32.889421
762.336238	57459.310196	32.894439
763.311008	57534.385496	32.899456
764.090597	57628.869739	32.904474
764.937909	57715.334373	32.909492
765.446012	57796.477012	32.914509
766.195395	57885.439443	32.919527
767.045629	57969.353919	32.924544
767.496570	58058.607781	32.929562
768.298155	58143.916741	32.934580
768.733095	58240.113272	32.939597
769.569280	58337.922852	32.944615
770.140551	58431.576145	32.949632
770.652363	58539.282330	32.954650
771.410572	58639.650567	32.959668
772.191237	58735.059009	32.964685
773.146725	58830.812659	32.969703
774.376886	58934.517128	32.974720
775.101530	59028.281614	32.979738
775.895332	59110.622148	32.984756
776.637894	59218.674403	32.989773
777.666222	59315.404016	32.994791
778.570259	59401.387567	32.999808
779.400666	59500.018757	33.004826
780.054732	59592.569126	33.009844
780.622170	59688.398427	33.014861
781.858378	59773.781444	33.019879
782.406510	59869.816819	33.024896
783.048250	59974.267997	33.029914
784.250379	60049.494087	33.034932
784.985332	60149.987822	33.039949
785.722209	60237.681575	33.044967
786.215618	60326.386985	33.049984
786.890468	60423.983753	33.055002
787.775961	60511.582511	33.060020
788.220426	60592.842178	33.065037
788.884813	60693.943670	33.070055
789.732036	60779.573173	33.075072
790.266098	60886.471547	33.080090
791.293125	60968.034801	33.085108
791.856369	61072.776141	33.090125
791.911037	61169.004070	33.095143
792.999535	61273.697654	33.100160
793.678689	61383.382864	33.105178
794.777867	61481.192293	33.110196
795.248420	61591.603440	33.115213
796.549076	61689.009276	33.120231
797.368073	61791.516163	33.125248
797.972599	61900.537357	33.130266
799.386412	61985.453779	33.135284
800.199138	62090.072643	33.140301
801.500024	62179.788732	33.145319
802.628289	62260.223626	33.150336
803.433950	62355.172848	33.155354
804.363759	62435.791652	33.160372
804.864920	62515.964304	33.165389
805.405822	62608.279116	33.170407
806.037268	62700.074711	33.175424
806.688711	62799.298001	33.180442
807.731722	62892.718474	33.185460
808.393896	62997.341053	33.190477
809.190554	63091.149083	33.195495
810.472129	63175.637164	33.200512
811.541342	63276.406993	33.205530
812.385551	63371.172008	33.210548
812.822489	63467.072870	33.215565
813.157472	63562.848334	33.220583
814.139886	63662.825582	33.225600
814.532866	63770.918535	33.230618
815.566250	63866.660157	33.235636
815.840901	63982.121884	33.240653
816.422503	64088.917079	33.245671
817.119950	64207.581477	33.250688
817.731426	64332.822847	33.255706
818.794669	64448.922983	33.260724
819.624679	64570.846676	33.265741
820.436666	64685.453379	33.270759
821.197405	64801.648018	33.275776
822.101447	64935.121216	33.280794
822.931510	65037.211168	33.285812
824.214924	65167.991647	33.290829
824.740454	65278.788112	33.295847
826.011716	65384.097445	33.300864
826.513914	65492.530145	33.305882
827.747791	65605.650807	33.310900
828.688023	65718.386179	33.315917
830.094831	65811.977807	33.320935
831.257174	65907.361694	33.325952
831.766608	66013.525313	33.330970
833.108861	66090.553369	33.335988
834.080793	66167.691208	33.341005
834.651778	66245.559597	33.346023
835.574381	66316.430096	33.351040
836.447776	66417.951967	33.356058
837.166367	66492.393050	33.361076
837.781543	66578.789924	33.366093
838.174919	66668.475732	33.371111
839.255194	66759.660314	33.376128
839.917442	66857.639513	33.381146
840.552187	66950.285653	33.386164
841.633645	67041.566133	33.391181
841.996419	67149.802922	33.396199
842.932686	67248.302713	33.401216
843.295387	67353.565261	33.406234
844.058748	67457.968641	33.411252
844.552992	67579.194110	33.416269
845.204367	67693.073552	33.421287
846.482163	67806.746570	33.426304
847.126118	67923.224976	33.431322
847.976805	68040.107080	33.436340
849.392818	68162.768845	33.441357
850.136729	68274.432166	33.446375
851.247324	68380.465696	33.451392
852.185901	68486.091267	33.456410
853.264945	68594.177877	33.461428
854.106981	68703.819042	33.466445
854.785711	68817.163703	33.471463
855.828878	68922.730770	33.476480
856.631456	69023.516252	33.481498
857.190295	69131.707580	33.486516
858.556865	69236.649956	33.491533
859.060345	69350.783739	33.496551
859.878056	69467.028897	33.501568
860.733254	69582.163141	33.506586
861.911498	69691.017135	33.511604
862.594702	69808.170237	33.516621
863.130721	69922.523297	33.521639
864.071036	70029.369988	33.526656
864.797013	70163.400303	33.531674
865.482452	70275.337069	33.536692
866.436806	70391.256363	33.541709
867.167209	70517.365373	33.546727
867.945789	70643.492797	33.551744
869.043725	70764.622967	33.556762
869.710665	70882.972896	33.561780
870.677230	71010.140549	33.566797
871.568730	71136.594347	33.571815
872.342553	71253.886947	33.576832
873.423015	71371.238860	33.581850
874.187526	71498.947292	33.586868
875.325573	71612.601443	33.591885
876.485237	71736.210949	33.596903
877.367984	71856.813383	33.601920
878.023574	71982.532931	33.606938
878.806554	72087.254804	33.611956
879.914851	72189.745485	33.616973
880.569976	72306.911556	33.621991
881.582575	72403.447303	33.627008
882.393962	72507.238001	33.632026
883.186087	72629.704657	33.637044
884.288210	72736.041032	33.642061
885.025803	72860.710457	33.647079
885.876384	72958.367863	33.652096
886.831675	73075.591794	33.657114
887.729699	73185.539627	33.662132
888.563131	73292.503085	33.667149
889.247780	73417.607794	33.672167
890.421680	73524.802678	33.677184
891.222211	73640.803355	33.682202
891.901006	73757.474960	33.687220
893.198839	73865.669351	33.692237
893.994410	73990.450344	33.697255
894.922565	74118.566603	33.702272
895.615216	74230.366518	33.707290
896.815660	74353.132643	33.712308
897.975800	74452.201554	33.717325
898.856161	74568.618301	33.722343
899.752171	74675.566545	33.727360
900.714442	74789.810252	33.732378
901.697685	74905.707012	33.737396
902.648810	75023.865667	33.742413
903.305493	75138.248453	33.747431
904.040928	75257.087406	33.752448
904.786787	75379.325434	33.757466
905.529380	75507.758135	33.762484
906.917324	75612.079866	33.767501
907.490053	75743.543019	33.772519
908.371170	75854.588850	33.777536
909.652556	75979.304858	33.782554
910.428127	76095.570130	33.787572
911.537428	76218.640197	33.792589
912.276691	76341.043085	33.797607
913.108655	76462.250100	33.802624
913.941956	76582.680248	33.807642
914.949716	76701.825634	33.812660
915.855039	76829.507674	33.817677
916.549337	76954.474781	33.822695
917.469634	77081.151095	33.827712
918.559157	77222.527662	33.832730
919.370018	77344.830392	33.837748
920.386147	77464.364452	33.842765
921.318819	77583.476381	33.847783
922.507410	77711.592908	33.852800
923.492478	77826.855059	33.857818
924.259018	77956.323344	33.862836
925.585854	78068.757749	33.867853
926.001232	78196.140741	33.872871
927.016672	78314.327264	33.877888
928.294608	78429.097439	33.882906
929.001824	78553.174724	33.887924
930.184566	78647.557890	33.892941
931.223513	78754.941000	33.897959
931.958005	78860.622240	33.902976
932.711048	78972.249020	33.907994
933.642094	79072.306094	33.913012
934.777803	79183.544446	33.918029
935.629830	79302.451640	33.923047
936.049016	79408.647295	33.928064
937.144992	79530.601646	33.933082
937.859396	79656.252059	33.938100
938.646732	79780.975067	33.943117
939.499165	79906.118310	33.948135
940.525768	80031.089211	33.953152
941.047797	80159.775865	33.958170
941.858482	80291.249325	33.963188
943.085684	80428.649965	33.968205
943.759803	80568.965168	33.973223
944.779938	80698.840189	33.978240
945.911195	80835.557114	33.983258
946.460129	80971.804979	33.988276
947.335537	81113.608991	33.993293
948.390474	81267.567090	33.998311
949.288375	81408.124178	34.003328
950.549700	81554.611011	34.008346
951.311123	81700.154293	34.013364
952.341202	81839.207654	34.018381
953.203698	81982.688576	34.023399
954.071800	82127.592004	34.028416
955.735914	82243.978220	34.033434
957.332217	82375.226050	34.038452
959.234859	82486.271580	34.043469
960.205061	82606.563390	34.048487
961.250261	82719.105805	34.053504
962.242648	82828.097910	34.058522
962.978901	82943.788490	34.063540
964.018892	83053.735151	34.068557
964.722111	83175.533110	34.073575
965.674117	83288.788843	34.078592
966.982911	83411.907995	34.083610
967.606525	83526.797813	34.088628
968.458141	83643.592927	34.093645
968.921911	83759.824484	34.098663
970.045059	83898.029491	34.103680
970.928184	84021.599270	34.108698
971.278784	84166.902566	34.113716
972.289000	84294.209257	34.118733
973.312369	84430.081651	34.123751
974.128340	84566.892041	34.128768
975.399984	84703.093396	34.133786
976.434304	84845.946882	34.138804
977.459544	84968.513243	34.143821
978.595371	85109.303800	34.148839
979.486668	85241.642706	34.153856
980.166246	85374.635755	34.158874
980.766471	85513.927175	34.163892
982.304764	85625.818601	34.168909
982.917315	85748.929333	34.173927
983.896109	85884.982519	34.178944
984.789611	86001.037842	34.183962
985.653021	86137.926664	34.188980
986.759980	86277.989741	34.193997
987.485511	86423.166592	34.199015
988.347961	86557.206521	34.204032
989.146518	86687.741753	34.209050
989.992729	86840.831531	34.214068
990.725905	86981.888192	34.219085
991.754117	87137.916756	34.224103
992.872056	87292.395597	34.229120
994.082073	87435.573589	34.234138
994.774998	87590.590118	34.239156
995.632707	87739.947299	34.244173
996.665304	87899.306850	34.249191
997.882046	88058.366369	34.254208
998.929271	88203.643180	34.259226
1000.125466	88362.284522	34.264244
1001.138420	88508.732394	34.269261
1002.173495	88675.559284	34.274279
1003.237108	88823.316572	34.279296
1004.823696	88966.514371	34.284314
1005.854259	89113.595917	34.289332
1006.664169	89254.364312	34.294349
1007.568707	89404.750008	34.299367
1008.254723	89559.832323	34.304384
1009.577597	89708.774929	34.309402
1010.430418	89858.893729	34.314420
1011.834475	90002.551107	34.319437
1012.656950	90159.652363	34.324455
1013.886102	90311.308109	34.329472
1015.744143	90437.985075	34.334490
1016.905406	90576.100500	34.339508
1017.893825	90715.964522	34.344525
1019.262372	90849.754449	34.349543
1020.170629	90982.884778	34.354560
1021.661710	91098.922979	34.359578
1022.332252	91239.795906	34.364596
1023.538825	91360.149802	34.369613
1024.617375	91496.715692	34.374631
1025.435740	91624.254288	34.379648
1026.578966	91755.150945	34.384666
1027.445193	91877.712202	34.389684
1028.416167	92015.645586	34.394701
1029.208939	92153.506982	34.399719
1030.053285	92281.374134	34.404736
1031.264041	92414.711669	34.409754
1031.982974	92563.504082	34.414772
1032.941894	92694.359726	34.419789
1034.103421	92837.903452	34.424807
1034.820648	92983.112688	34.429824
1035.794932	93114.885498	34.434842
1036.549057	93262.437289	34.439860
1037.601259	93401.935011	34.444877
1038.687533	93535.665948	34.449895
1039.623969	93673.412736	34.454912
1040.733999	93806.490023	34.459930
1041.157783	93957.128763	34.464948
1042.153813	94104.356687	34.469965
1043.168193	94244.238893	34.474983
1044.000882	94406.650412	34.480000
1045.165174	94561.660163	34.485018
1046.111285	94708.368665	34.490036
1047.074880	94867.631575	34.495053
1048.195197	95030.457304	34.500071
1049.094101	95191.111782	34.505088
1050.827066	95334.005036	34.510106
1051.892370	95494.116505	34.515124
1053.037735	95648.181586	34.520141
1054.385787	95796.281862	34.525159
1055.468823	95949.403718	34.530176
1056.625413	96090.230011	34.535194
1057.778489	96240.116490	34.540212
1058.507014	96390.122100	34.545229
1059.596747	96536.870281	34.550247
1060.733514	96691.683996	34.555264
1061.866966	96842.241822	34.560282
1062.636340	97001.651911	34.565300
1063.739771	97156.208400	34.570317
1065.023086	97312.730095	34.575335
1065.858652	97468.545951	34.580352
1067.253063	97632.137614	34.585370
1067.926004	97794.573604	34.590388
1068.904713	97952.280566	34.595405
1069.956057	98104.669162	34.600423
1071.153415	98272.554469	34.605440
1071.936610	98437.767485	34.610458
1073.037504	98596.920893	34.615476
1074.380675	98763.293530	34.620493
1075.841421	98923.821795	34.625511
1076.616870	99087.187003	34.630528
1077.762753	99247.647403	34.635546
1079.089451	99413.654094	34.640564
1079.947445	99575.307724	34.645581
1081.208133	99724.858331	34.650599
1082.359787	99903.910848	34.655616
1083.465370	100056.107633	34.660634
1084.742330	100208.328779	34.665652
1085.158466	100381.364751	34.670669
1086.385986	100534.772746	34.675687
1087.357149	100706.008213	34.680704
1088.400810	100879.587140	34.685722
1090.016470	101039.308256	34.690740
1090.627378	101201.120102	34.695757
1091.825197	101365.528852	34.700775
1093.105052	101528.375503	34.705792
1094.494814	101676.564114	34.710810
1095.804834	101819.160205	34.715828
1096.976981	101960.564213	34.720845
1097.954341	102109.529846	34.725863
1099.049336	102263.735953	34.730880
1099.903046	102398.637866	34.735898
1101.257244	102529.550456	34.740916
1102.110408	102696.295023	34.745933
1103.145202	102837.023794	34.750951
1103.900497	102999.597107	34.755968
1104.616412	103148.085712	34.760986
1106.021552	103307.887458	34.766004
1106.575394	103481.297827	34.771021
1107.781831	103634.134703	34.776039
1108.599484	103804.550331	34.781056
1109.468761	103980.439075	34.786074
1111.233622	104140.777763	34.791092
1112.327302	104305.223670	34.796109
1114.018614	104472.923285	34.801127
1115.094849	104637.804591	34.806144
1116.141227	104804.545977	34.811162
1117.048874	104974.455771	34.816180
1117.930654	105143.896265	34.821197
1119.499179	105306.204210	34.826215
1120.620989	105485.797707	34.831232
1121.620082	105650.489458	34.836250
1122.937796	105818.454160	34.841268
1123.873679	105994.018120	34.846285
1125.017073	106149.032925	34.851303
1126.198038	106338.888470	34.856320
1126.886973	106504.293603	34.861338
1128.300407	106692.842904	34.866356
1129.168188	106871.847987	34.871373
1130.263087	107056.400347	34.876391
1131.118908	107241.770599	34.881408
1132.294121	107419.977721	34.886426
1133.649737	107604.473827	34.891444
1134.985832	107793.151630	34.896461
1136.269342	107968.529141	34.901479
1137.462722	108136.650055	34.906496
1139.106442	108321.194418	34.911514
1140.705894	108489.145604	34.916532
1141.568865	108656.360617	34.921549
1143.028801	108819.361450	34.926567
1143.755065	108994.708404	34.931584
1145.255777	109157.970854	34.936602
1146.693032	109323.782604	34.941620
1147.758043	109486.907670	34.946637
1148.967226	109636.218816	34.951655
1150.253371	109814.033425	34.956672
1151.148464	109973.612538	34.961690
1152.636357	110129.775344	34.966708
1153.728133	110296.452493	34.971725
1154.228300	110459.173804	34.976743
1155.183860	110632.597094	34.981760
1156.278252	110800.308998	34.986778
1157.464518	110965.253933	34.991796
1158.465062	111126.988580	34.996813
1159.741396	111279.520967	35.001831
1160.317907	111440.090748	35.006848
1160.803305	111614.076776	35.011866
1162.390304	111786.451921	35.016884
1163.304388	111963.290406	35.021901
1164.603532	112137.771062	35.026919
1165.441226	112316.896748	35.031936
1166.555815	112501.284465	35.036954
1167.780741	112690.289800	35.041972
1168.678618	112894.231287	35.046989
1169.979664	113072.123929	35.052007
1171.196950	113265.939628	35.057024
1172.171572	113465.271315	35.062042
1173.899114	113642.612746	35.067060
1175.111867	113842.738873	35.072077
1176.433962	114015.513399	35.077095
1178.003698	114201.955715	35.082112
1178.967363	114383.868001	35.087130
1180.475054	114561.415476	35.092148
1181.542090	114736.824805	35.097165
1183.152967	114918.093580	35.102183
1184.661157	115103.026601	35.107200
1185.979448	115271.802859	35.112218
1187.473578	115448.320442	35.117236
1187.913760	115629.603189	35.122253
1189.321055	115798.172534	35.127271
1190.764344	115963.710986	35.132288
1192.278399	116130.600469	35.137306
1193.683369	116299.046880	35.142324
1194.890315	116471.685536	35.147341
1196.245820	116622.085160	35.152359
1197.314933	116797.666670	35.157376
1198.469312	116963.168906	35.162394
1200.061939	117118.465904	35.167412
1200.955203	117282.023647	35.172429
1202.016778	117459.788919	35.177447
1203.234966	117622.967931	35.182464
1204.302267	117802.634129	35.187482
1205.605924	117960.413499	35.192500
1206.291269	118146.892355	35.197517
1207.385407	118330.603911	35.202535
1208.454646	118504.911714	35.207552
1209.315967	118704.562031	35.212570
1210.748667	118869.759996	35.217588
1211.711844	119059.031590	35.222605
1213.489302	119253.411624	35.227623
1214.270379	119428.296999	35.232640
1216.101757	119613.002189	35.237658
1217.184021	119795.611562	35.242676
1218.172194	119984.936568	35.247693
1219.503011	120160.113042	35.252711
1220.598962	120340.647094	35.257728
1221.555009	120540.226759	35.262746
1222.649760	120708.339628	35.267764
1224.090458	120882.135681	35.272781
1225.519631	121056.048699	35.277799
1226.830409	121230.070346	35.282816
1227.477402	121394.826613	35.287834
1228.741873	121571.416195	35.292852
1230.014413	121756.275997	35.297869
1231.176006	121936.772570	35.302887
1232.347683	122111.316084	35.307904
1233.392426	122300.750080	35.312922
1234.560095	122479.539557	35.317940
1235.936451	122671.000610	35.322957
1237.131348	122861.934603	35.327975
1238.839603	123044.466960	35.332992
1239.674394	123237.512744	35.338010
1241.157345	123430.748192	35.343028
1242.280825	123622.002960	35.348045
1243.816368	123800.755480	35.353063
1245.151083	123982.251684	35.358080
1246.000353	124172.667343	35.363098
1247.372455	124363.330558	35.368116
1248.512499	124559.364590	35.373133
1249.664189	124762.592794	35.378151
1250.946563	124945.927804	35.383168
1251.971706	125161.592429	35.388186
1253.486634	125353.151940	35.393204
1254.548373	125552.499003	35.398221
1255.792558	125755.922637	35.403239
1257.122524	125965.921051	35.408256
1258.243495	126187.899488	35.413274
1259.263333	126389.982803	35.418292
1260.685052	126596.310642	35.423309
1262.005456	126811.574063	35.428327
1263.016211	127026.850402	35.433344
1264.242272	127234.911621	35.438362
1265.460896	127446.813940	35.443380
1267.101363	127666.264235	35.448397
1268.662471	127876.278577	35.453415
1270.226132	128079.352005	35.458432
1271.620269	128290.434829	35.463450
1273.275584	128480.068370	35.468468
1274.838451	128670.782051	35.473485
1276.059219	128874.637929	35.478503
1277.662312	129057.214735	35.483520
1278.585976	129253.836225	35.488538
1280.031870	129444.991888	35.493556
1281.162455	129652.123662	35.498573
1282.358629	129846.793028	35.503591
1283.840212	130027.393830	35.508608
1284.456883	130229.911395	35.513626
1285.995405	130431.663094	35.518644
1287.419661	130629.050852	35.523661
1289.212032	130816.816139	35.528679
1290.808695	130989.537199	35.533696
1292.148935	131187.056257	35.538714
1293.687429	131344.306627	35.543732
1294.603889	131522.244913	35.548749
1295.772121	131688.070056	35.553767
1296.972943	131857.299164	35.558784
1297.683633	132032.321304	35.563802
1299.092619	132215.811081	35.568820
1299.843810	132403.359655	35.573837
1301.208072	132601.264864	35.578855
1302.452239	132783.745555	35.583872
1303.882912	132967.363435	35.588890
1305.369707	133159.716130	35.593908
1306.388562	133365.790586	35.598925
1307.062467	133553.181613	35.603943
1308.640672	133756.711883	35.608960
1309.435434	133962.154700	35.613978
1310.984399	134175.892523	35.618996
1312.481246	134384.812600	35.624013
1313.314044	134591.026781	35.629031
1314.621749	134807.189780	35.634048
1316.189378	135029.382580	35.639066
1317.440392	135252.020221	35.644084
1318.580350	135472.206301	35.649101
1319.642738	135685.766522	35.654119
1321.108392	135907.348675	35.659136
1322.266817	136145.555895	35.664154
1323.280291	136369.950514	35.669172
1325.080389	136598.352853	35.674189
1326.177543	136834.459215	35.679207
1327.421841	137059.367317	35.684224
1329.194012	137292.924362	35.689242
1330.724092	137523.252293	35.694260
1332.364887	137744.199545	35.699277
1333.391752	137979.489878	35.704295
1334.856539	138211.341573	35.709312
1336.267140	138435.283279	35.714330
1337.499310	138666.313759	35.719348
1339.025352	138889.885704	35.724365
1340.383074	139133.788151	35.729383
1341.885437	139359.762570	35.734400
1342.858166	139595.239027	35.739418
1344.373482	139830.200205	35.744436
1345.838868	140052.041569	35.749453
1346.768923	140282.055310	35.754471
1348.670600	140508.000256	35.759488
1349.804882	140753.408832	35.764506
1351.226051	140979.002770	35.769524
1352.841424	141212.197169	35.774541
1354.386243	141438.674720	35.779559
1355.983060	141664.651409	35.784576
1357.184588	141887.777554	35.789594
1358.690951	142110.502006	35.794612
1360.089215	142332.459457	35.799629
1360.992690	142563.800159	35.804647
1363.314094	142769.010610	35.809664
1364.319171	142981.846260	35.814682
1365.688750	143187.743117	35.819700
1367.175168	143388.058573	35.824717
1367.996097	143595.490270	35.829735
1369.501494	143806.845198	35.834752
1370.765563	144019.279273	35.839770
1372.129113	144221.381482	35.844788
1373.159304	144431.067031	35.849805
1374.206231	144642.120260	35.854823
1375.766669	144862.751914	35.859840
1376.890097	145094.583605	35.864858
1378.064844	145313.277021	35.869876
1379.389950	145538.970355	35.874893
1380.554355	145783.932571	35.879911
1381.960171	146015.345924	35.884928
1383.474156	146246.883224	35.889946
1385.174714	146473.436263	35.894964
1387.169892	146687.851135	35.899981
1389.035729	146909.437370	35.904999
1390.837466	147119.474607	35.910016
1392.181353	147338.674924	35.915034
1393.961377	147541.302751	35.920052
1395.778003	147736.345511	35.925069
1397.462247	147936.937487	35.930087
1398.839401	148130.074949	35.935104
1399.750970	148338.448928	35.940122
1401.092022	148545.944694	35.945140
1403.000468	148736.846329	35.950157
1404.129364	148948.371628	35.955175
1405.570861	149151.000060	35.960192
1406.852452	149351.766284	35.965210
1407.991503	149563.496836	35.970228
1409.630682	149774.223856	35.975245
1410.916485	149986.073300	35.980263
1412.166345	150195.863412	35.985280
1413.007099	150424.710843	35.990298
1414.312681	150630.881802	35.995316
1415.978519	150851.677601	36.000333
1416.974530	151087.655233	36.005351
1418.230966	151312.436637	36.010368
1420.007260	151541.181246	36.015386
1421.229669	151770.345091	36.020404
1422.888149	151989.387463	36.025421
1424.009917	152230.031541	36.030439
1425.611617	152457.491714	36.035456
1427.135005	152686.195699	36.040474
1428.818785	152909.284554	36.045492
1431.040942	153116.441132	36.050509
1432.259357	153341.888980	36.055527
1433.940617	153549.020090	36.060544
1435.156105	153770.870535	36.065562
1436.185555	153996.834619	36.070580
1437.567093	154215.707435	36.075597
1438.665177	154453.924276	36.080615
1440.122773	154677.542666	36.085632
1441.336584	154911.978641	36.090650
1442.563990	155128.941949	36.095668
1444.384184	155337.710308	36.100685
1445.379637	155555.030183	36.105703
1446.734288	155779.382257	36.110720
1448.413661	156000.869326	36.115738
1449.276854	156232.808831	36.120756
1450.685104	156457.435798	36.125773
1451.684071	156696.863332	36.130791
1453.185914	156944.429276	36.135808
1454.586142	157192.469631	36.140826
1455.481106	157437.257161	36.145844
1457.220843	157679.350781	36.150861
1458.321328	157937.220603	36.155879
1459.674078	158199.490421	36.160896
1461.324587	158447.588760	36.165914
1462.887809	158717.957281	36.170932
1464.264330	158978.479251	36.175949
1465.415580	159244.073247	36.180967
1466.915977	159501.561379	36.185984
1468.509768	159776.079870	36.191002
1469.825974	160049.148227	36.196020
1471.377390	160321.420447	36.201037
1472.836827	160605.033804	36.206055
1474.480553	160884.207005	36.211072
1476.465549	161150.481782	36.216090
1477.851436	161421.304984	36.221108
1479.354375	161690.729330	36.226125
1480.797104	161956.918722	36.231143
1482.658934	162231.553059	36.236160
1484.101000	162501.918936	36.241178
1485.368225	162776.740667	36.246196
1487.582563	163034.001355	36.251213
1489.260214	163296.282543	36.256231
1491.166712	163558.148793	36.261248
1492.797418	163813.922429	36.266266
1494.304462	164066.229799	36.271284
1495.842504	164316.365252	36.276301
1497.091252	164571.507315	36.281319
1498.857443	164836.626410	36.286336
1500.449714	165088.622870	36.291354
1501.899858	165348.950986	36.296372
1503.374902	165602.047619	36.301389
1504.627306	165864.211761	36.306407
1505.935204	166125.011823	36.311424
1507.615030	166384.397500	36.316442
1509.191989	166646.718508	36.321460
1510.543157	166908.569879	36.326477
1512.001832	167171.712406	36.331495
1513.414950	167439.239883	36.336512
1515.220891	167696.115885	36.341530
1516.896103	167957.720115	36.346548
1518.505361	168211.092053	36.351565
1520.145903	168471.195933	36.356583
1521.337638	168727.313964	36.361600
1523.237137	168978.805694	36.366618
1524.807643	169215.777087	36.371636
1526.847392	169436.439411	36.376653
1528.423612	169666.068427	36.381671
1529.840819	169897.233529	36.386688
1531.162337	170126.017825	36.391706
1532.508963	170364.668152	36.396724
1533.866584	170593.525577	36.401741
1535.353555	170847.200674	36.406759
1536.276206	171088.979832	36.411776
1537.727488	171333.340352	36.416794
1539.073272	171589.554315	36.421812
1540.326100	171843.590184	36.426829
1541.423082	172118.583075	36.431847
1542.760979	172389.302711	36.436864
1544.298696	172661.425904	36.441882
1545.626026	172952.561883	36.446900
1547.104585	173223.569308	36.451917
1548.935250	173503.478723	36.456935
1550.513123	173782.681790	36.461952
1552.167542	174067.228068	36.466970
1554.174531	174345.072917	36.471988
1556.238847	174618.216744	36.477005
1557.870913	174887.612556	36.482023
1559.992609	175152.289234	36.487040
1561.895149	175411.927937	36.492058
1563.152824	175675.793789	36.497076
1564.898875	175939.964359	36.502093
1566.651023	176196.802855	36.507111
1567.777546	176461.646078	36.512128
1569.666378	176721.092256	36.517146
1571.133536	176989.931807	36.522164
1572.574804	177248.881478	36.527181
1574.152217	177524.913099	36.532199
1575.474680	177803.422948	36.537216
1577.512425	178063.881495	36.542234
1578.579016	178337.576383	36.547252
1580.221966	178611.485996	36.552269
1581.739181	178892.408078	36.557287
1582.704717	179176.185507	36.562304
1584.448514	179455.413278	36.567322
1586.349853	179745.465743	36.572340
1587.938540	180019.634125	36.577357
1589.562457	180312.005589	36.582375
1590.844365	180591.263390	36.587392
1592.759400	180868.811073	36.592410
1593.899111	181171.314106	36.597428
1595.933440	181450.496012	36.602445
1597.355018	181737.884777	36.607463
1598.714174	182020.945965	36.612480
1600.239524	182319.157839	36.617498
1602.119066	182613.382072	36.622516
1603.797465	182893.822433	36.627533
1605.372454	183195.331368	36.632551
1606.830008	183477.548842	36.637568
1609.144165	183758.096719	36.642586
1610.181654	184038.392332	36.647604
1611.593117	184302.172789	36.652621
1613.561254	184566.983015	36.657639
1615.285118	184829.194274	36.662656
1617.038187	185090.755274	36.667674
1619.060440	185357.096930	36.672692
1620.957957	185607.737951	36.677709
1622.421089	185865.618821	36.682727
1624.487634	186115.398295	36.687744
1626.452551	186361.756424	36.692762
1628.206794	186628.008484	36.697780
1629.688812	186889.775121	36.702797
1631.548615	187133.704981	36.707815
1632.909336	187389.491487	36.712832
1634.252049	187635.244604	36.717850
1635.501061	187899.135075	36.722868
1637.247351	188164.572379	36.727885
1638.502011	188428.667978	36.732903
1639.963545	188702.998511	36.737920
1641.429323	188977.774122	36.742938
1642.786200	189263.215757	36.747956
1644.231622	189553.949611	36.752973
1646.131820	189827.277902	36.757991
1647.333409	190124.627593	36.763008
1648.941856	190412.447345	36.768026
1650.890385	190701.052395	36.773044
1652.388977	191007.865673	36.778061
1654.212754	191310.657028	36.783079
1655.464153	191610.482662	36.788096
1657.554249	191895.785396	36.793114
1659.264715	192191.721714	36.798132
1660.940009	192499.277768	36.803149
1663.067421	192794.174278	36.808167
1664.505156	193101.924102	36.813184
1666.385949	193383.981647	36.818202
1668.021090	193684.050842	36.823220
1669.726036	193984.224974	36.828237
1671.643060	194273.769762	36.833255
1672.880716	194566.698540	36.838272
1675.119985	194859.292275	36.843290
1676.546698	195161.560952	36.848308
1678.494242	195455.460928	36.853325
1680.651567	195732.905921	36.858343
1682.227974	196025.763905	36.863360
1683.915574	196305.837671	36.868378
1685.794931	196592.406265	36.873396
1687.601253	196880.092261	36.878413
1689.777224	197170.627682	36.883431
1690.899873	197446.951542	36.888448
1692.893466	197727.479366	36.893466
1694.393381	198008.213999	36.898484
1695.996991	198288.781347	36.903501
1697.928715	198574.755903	36.908519
1699.556991	198865.349547	36.913536
1700.913972	199142.343137	36.918554
1702.610263	199415.260654	36.923572
1704.408231	199678.009106	36.928589
1706.061248	199937.481687	36.933607
1707.378194	200214.220584	36.938624
1709.078177	200471.098883	36.943642
1710.915426	200736.130968	36.948660
1712.417224	201005.647522	36.953677
1714.607277	201261.829749	36.958695
1716.474036	201533.969214	36.963712
1718.495553	201789.647530	36.968730
1720.244014	202057.391055	36.973748
1721.992031	202317.748324	36.978765
1723.944257	202586.375961	36.983783
1725.487591	202852.378760	36.988800
1726.832385	203109.681093	36.993818
1728.507039	203378.572367	36.998836
1730.014036	203655.501312	37.003853
1731.859801	203929.293209	37.008871
1733.599881	204210.656071	37.013888
1735.083257	204491.083631	37.018906
1737.323706	204773.677277	37.023924
1738.765307	205053.936482	37.028941
1740.594437	205335.074875	37.033959
1742.199174	205624.234911	37.038976
1743.738057	205907.313572	37.043994
1745.301625	206204.099563	37.049012
1746.530139	206500.267434	37.054029
1748.614828	206797.417961	37.059047
1750.153343	207101.740231	37.064064
1752.198445	207400.410689	37.069082
1754.344955	207699.980544	37.074100
1755.880082	207992.108284	37.079117
1758.214735	208287.677727	37.084135
1759.921229	208588.121593	37.089152
1761.546482	208877.751073	37.094170
1763.474263	209177.540639	37.099188
1764.997300	209475.085420	37.104205
1767.439483	209769.984771	37.109223
1769.075728	210058.069221	37.114240
1771.102124	210355.665240	37.119258
1773.106576	210641.078696	37.124276
1774.864261	210920.362691	37.129293
1777.239131	211192.935643	37.134311
1778.870107	211485.470813	37.139328
1780.382145	211764.467419	37.144346
1782.434263	212041.449772	37.149364
1783.642849	212331.034300	37.154381
1785.509107	212624.260929	37.159399
1787.157356	212913.232335	37.164416
1788.788287	213188.597903	37.169434
1790.880481	213477.983755	37.174452
1792.251290	213783.634545	37.179469
1793.865743	214065.379707	37.184487
1795.593506	214366.164744	37.189504
1797.766385	214660.608622	37.194522
1799.638540	214937.758657	37.199540
1801.382241	215193.956185	37.204557
1803.540866	215459.052324	37.209575
1805.457199	215721.750275	37.214592
1807.329172	215994.994194	37.219610
1809.396814	216243.539149	37.224628
1811.427179	216504.990440	37.229645
1812.865172	216763.438817	37.234663
1814.421001	217024.116721	37.239680
1815.953596	217293.229773	37.244698
1818.073330	217558.428982	37.249716
1819.570067	217840.182900	37.254733
1821.398577	218106.687350	37.259751
1823.111884	218386.352185	37.264768
1824.862827	218670.113190	37.269786
1826.575190	218949.412153	37.274804
1828.305932	219247.653002	37.279821
1830.229569	219525.435104	37.284839
1831.840012	219817.780606	37.289856
1833.535404	220111.726304	37.294874
1835.823676	220393.186719	37.299892
1837.122908	220695.895100	37.304909
1839.089375	221006.866228	37.309927
1840.937870	221308.372539	37.314944
1842.724434	221613.991098	37.319962
1844.711398	221905.891358	37.324980
1846.295686	222266.219314	37.329997
1848.433841	222567.900467	37.335015
1850.532024	222875.963272	37.340032
1852.215656	223179.407703	37.345050
1854.135397	223473.025997	37.350068
1855.953871	223781.720839	37.355085
1858.102398	224084.155331	37.360103
1859.993482	224390.161795	37.365120
1861.942331	224697.226867	37.370138
1864.284076	224987.634698	37.375156
1866.177571	225290.761782	37.380173
1868.063620	225589.002474	37.385191
1870.077124	225887.465278	37.390208
1872.143529	226188.130213	37.395226
1874.459404	226467.525508	37.400244
1875.946953	226772.398582	37.405261
1878.004440	227058.668422	37.410279
1879.908721	227350.144399	37.415296
1881.823202	227628.083452	37.420314
1883.852490	227916.697116	37.425332
1885.707349	228212.729839	37.430349
1887.637542	228500.675466	37.435367
1889.733599	228788.671907	37.440384
1891.150333	229074.542180	37.445402
1893.377425	229363.027635	37.450420
1895.053868	229647.106143	37.455437
1897.275787	229940.419714	37.460455
1899.321783	230215.958737	37.465472
1901.099114	230505.712901	37.470490
1903.249929	230764.728735	37.475508
1904.740569	231023.062750	37.480525
1906.612107	231273.108257	37.485543
1908.628069	231537.633510	37.490560
1910.107440	231795.057144	37.495578
1912.448498	232051.100247	37.500596
1914.049271	232312.391869	37.505613
1916.290154	232567.512546	37.510631
1917.890444	232826.494448	37.515648
1919.791489	233099.499782	37.520666
1921.592901	233361.956117	37.525684
1923.459696	233635.171571	37.530701
1925.035185	233906.300567	37.535719
1927.334933	234187.931831	37.540736
1928.882232	234475.651901	37.545754
1930.632562	234754.578135	37.550772
1932.519308	235053.294279	37.555789
1934.415375	235330.446476	37.560807
1936.545604	235625.900044	37.565824
1938.276445	235918.928765	37.570842
1940.178587	236208.222913	37.575860
1941.570847	236523.988129	37.580877
1943.612983	236828.958230	37.585895
1945.728577	237147.455191	37.590912
1947.299523	237463.347224	37.595930
1949.507618	237770.935162	37.600948
1951.513468	238084.296272	37.605965
1953.051498	238397.148324	37.610983
1954.896380	238728.011480	37.616000
1957.195511	239056.974774	37.621018
1958.897732	239367.619129	37.626036
1960.715186	239703.366183	37.631053
1962.903926	240023.180544	37.636071
1964.821839	240362.799709	37.641088
1966.824965	240698.774169	37.646106
1969.224812	241025.237895	37.651124
1971.409044	241343.380161	37.656141
1973.171825	241676.144313	37.661159
1975.343519	241994.671273	37.666176
1977.630598	242321.892979	37.671194
1979.789640	242638.493196	37.676212
1981.864991	242967.756799	37.681229
1983.795104	243291.227635	37.686247
1986.171556	243598.727848	37.691264
1987.894915	243926.652743	37.696282
1990.113499	244243.806284	37.701300
1992.082966	244560.898510	37.706317
1993.689073	244880.004986	37.711335
1995.857971	245199.581734	37.716352
1997.760314	245525.526301	37.721370
1999.887297	245840.691469	37.726388
2001.967915	246168.742926	37.731405
2004.036451	246482.699570	37.736423
2006.169124	246801.269701	37.741440
2008.181085	247118.665841	37.746458
2010.641344	247399.769650	37.751476
2012.208427	247689.753683	37.756493
2014.205316	247984.572508	37.761511
2016.177546	248264.993348	37.766528
2018.047261	248560.341496	37.771546
2019.930498	248845.857768	37.776564
2021.485392	249148.877373	37.781581
2023.101196	249464.512386	37.786599
2025.457247	249772.867378	37.791616
2027.287038	250094.591429	37.796634
2028.985467	250398.149455	37.801652
2031.123493	250720.511671	37.806669
2033.073969	251041.176951	37.811687
2034.967008	251367.135497	37.816704
2036.679583	251708.110309	37.821722
2038.783333	252031.420298	37.826740
2040.920832	252381.067213	37.831757
2043.067021	252714.481633	37.836775
2045.265128	253046.084890	37.841792
2047.234829	253392.915349	37.846810
2049.509858	253720.468690	37.851828
2051.901336	254060.832155	37.856845
2053.628158	254401.200049	37.861863
2055.759263	254738.456138	37.866880
2057.946645	255088.531968	37.871898
2060.320872	255419.069850	37.876916
2062.363551	255761.853941	37.881933
2064.590138	256103.288494	37.886951
2066.711226	256437.907095	37.891968
2068.621261	256774.515671	37.896986
2071.026739	257118.590680	37.902004
2073.138150	257454.304645	37.907021
2074.822591	257796.285037	37.912039
2077.162535	258137.425267	37.917056
2079.119313	258487.771686	37.922074
2081.586206	258819.671604	37.927092
2083.679141	259177.414956	37.932109
2085.433494	259516.744774	37.937127
2087.563291	259861.832693	37.942144
2089.289341	260219.153011	37.947162
2091.459336	260570.890972	37.952180
2094.038316	260920.710094	37.957197
2095.615880	261275.184789	37.962215
2097.717560	261626.299803	37.967232
2099.743216	261998.968932	37.972250
2101.828341	262353.415180	37.977268
2103.899523	262705.933407	37.982285
2105.923004	263082.058938	37.987303
2108.175416	263430.560915	37.992320
2110.117916	263793.947761	37.997338
2112.022106	264161.710373	38.002356
2114.412274	264529.040620	38.007373
2116.914468	264886.624061	38.012391
2119.641270	265231.927893	38.017408
2122.255418	265573.718846	38.022426
2124.314231	265897.409493	38.027444
2126.312794	266205.613995	38.032461
2127.681138	266536.654518	38.037479
2130.349715	266842.466882	38.042496
2132.034275	267171.145990	38.047514
2134.268336	267503.828074	38.052532
2136.513190	267818.345325	38.057549
2138.566488	268145.137509	38.062567
2140.783634	268464.892582	38.067584
2142.610379	268803.914632	38.072602
2144.772559	269132.087251	38.077620
2147.022483	269454.835203	38.082637
2149.010051	269800.259277	38.087655
2151.312586	270127.139919	38.092672
2153.181526	270472.456082	38.097690
2155.467520	270813.895731	38.102708
2157.737893	271152.823046	38.107725
2159.676592	271505.698721	38.112743
2162.163261	271838.215699	38.117760
2164.172639	272190.343668	38.122778
2166.421202	272538.191424	38.127796
2168.696926	272894.316458	38.132813
2170.383505	273245.759152	38.137831
2172.598989	273593.282107	38.142848
2174.808672	273953.406118	38.147866
2176.634836	274323.472915	38.152884
2179.140145	274684.515434	38.157901
2180.976589	275057.857678	38.162919
2183.668685	275414.145554	38.167936
2185.841903	275788.577533	38.172954
2188.048525	276150.581922	38.177972
2190.428303	276513.422533	38.182989
2192.817285	276874.889854	38.188007
2195.560991	277225.250386	38.193024
2198.163538	277578.935681	38.198042
2200.198507	277938.833123	38.203060
2202.863340	278290.806350	38.208077
2205.101251	278638.376186	38.213095
2207.836996	278975.578608	38.218112
2209.515463	279321.407899	38.223130
2211.618860	279664.807170	38.228148
2214.502180	280006.177384	38.233165
2216.284417	280356.206771	38.238183
2218.880316	280694.370643	38.243200
2221.124084	281029.135347	38.248218
2223.062560	281375.151149	38.253236
2225.334074	281711.130469	38.258253
2227.355327	282067.497302	38.263271
2229.750024	282400.763957	38.268288
2231.860557	282753.889992	38.273306
2233.882193	283102.965374	38.278324
2236.173895	283447.425118	38.283341
2237.845218	283806.564412	38.288359
2239.935960	284160.505487	38.293376
2242.145522	284510.794794	38.298394
2244.071943	284856.835587	38.303412
2246.322921	285190.758161	38.308429
2248.193772	285530.431020	38.313447
2250.017710	285875.572677	38.318464
2252.247895	286221.157665	38.323482
2253.880666	286585.279630	38.328500
2256.651361	286923.690806	38.333517
2258.762113	287289.082608	38.338535
2261.059386	287645.197774	38.343552
2263.463644	288003.124594	38.348570
2265.763069	288369.247353	38.353588
2268.512540	288721.453776	38.358605
2270.781764	289087.199413	38.363623
2273.262560	289440.768522	38.368640
2275.641961	289801.694659	38.373658
2277.877665	290160.890323	38.378676
2280.606489	290509.134985	38.383693
2282.982732	290873.184722	38.388711
2285.240770	291231.892740	38.393728
2287.646715	291584.226158	38.398746
2289.711627	291947.333007	38.403764
2292.359758	292303.767603	38.408781
2294.503864	292669.604270	38.413799
2296.865744	293023.923946	38.418816
2298.557628	293390.745645	38.423834
2300.760337	293772.422321	38.428852
2303.219198	294132.618196	38.433869
2305.383750	294528.448654	38.438887
2307.339433	294899.874576	38.443904
2310.020380	295285.359242	38.448922
2312.115446	295680.309425	38.453940
2314.398725	296064.153693	38.458957
2316.773534	296457.025801	38.463975
2318.896898	296838.683904	38.468992
2321.568302	297234.631815	38.474010
2323.759866	297630.705746	38.479028
2326.568661	298016.977486	38.484045
2328.566071	298412.674041	38.489063
2330.811929	298807.390454	38.494080
2333.459800	299202.474058	38.499098
2335.596123	299605.613914	38.504116
2338.169343	300002.587181	38.509133
2340.485652	300401.581522	38.514151
2342.707782	300799.421341	38.519168
2344.953424	301204.876821	38.524186
2347.455163	301597.818653	38.529204
2350.412202	301986.826334	38.534221
2352.668263	302380.465527	38.539239
2355.241937	302776.669641	38.544256
2357.590305	303156.372385	38.549274
2360.061635	303553.225643	38.554292
2362.298534	303929.235493	38.559309
2364.873886	304326.959134	38.564327
2367.180933	304705.089449	38.569344
2369.615436	305080.429858	38.574362
2371.945611	305454.947550	38.579380
2374.542752	305803.691209	38.584397
2376.851955	306165.687801	38.589415
2379.054449	306515.431950	38.594432
2381.482015	306866.587295	38.599450
2384.085112	307209.738198	38.604468
2386.095918	307562.811901	38.609485
2388.487382	307924.434892	38.614503
2390.753992	308280.006027	38.619520
2393.300442	308644.802741	38.624538
2395.106393	309016.167284	38.629556
2397.215384	309381.005713	38.634573
2399.642936	309758.390764	38.639591
2402.041648	310140.732094	38.644608
2404.452536	310523.476629	38.649626
2406.701707	310920.316795	38.654644
2409.362972	311299.463135	38.659661
2411.835795	311696.265134	38.664679
2414.522636	312076.268365	38.669696
2417.108642	312455.752887	38.674714
2419.492623	312850.913872	38.679732
2422.340891	313227.001471	38.684749
2424.536765	313617.439860	38.689767
2426.743995	314008.890956	38.694784
2429.381907	314399.027803	38.699802
2431.702339	314797.544203	38.704820
2434.256744	315185.380049	38.709837
2436.624750	315587.720986	38.714855
2438.781699	315989.941375	38.719872
2441.486332	316391.463790	38.724890
2443.599258	316804.786816	38.729908
2446.361102	317203.071303	38.734925
2448.888563	317597.124469	38.739943
2451.080760	318006.391557	38.744960
2453.979957	318419.760834	38.749978
2456.341287	318835.931060	38.754996
2458.773872	319223.744711	38.760013
2461.370901	319629.892870	38.765031
2464.193533	320034.378061	38.770048
2467.046968	320426.107272	38.775066
2469.072830	320839.248515	38.780084
2471.601460	321246.644690	38.785101
2474.068599	321651.458272	38.790119
2476.237672	322062.006040	38.795136
2478.712652	322466.357458	38.800154
2480.861847	322884.599580	38.805172
2483.188270	323303.090924	38.810189
2485.675146	323723.459475	38.815207
2488.260567	324159.962098	38.820224
2490.555451	324578.223511	38.825242
2493.121255	325015.791349	38.830260
2495.241558	325439.993214	38.835277
2498.030195	325865.839235	38.840295
2500.333201	326307.784341	38.845312
2503.149260	326713.559265	38.850330
2505.668848	327118.185518	38.855348
2508.335151	327506.711497	38.860365
2510.901179	327892.508795	38.865383
2512.959470	328288.974161	38.870400
2515.710713	328679.359979	38.875418
2517.995265	329074.591875	38.880436
2520.578943	329467.158703	38.885453
2523.121935	329870.700156	38.890471
2525.163918	330278.407224	38.895488
2527.892503	330680.975285	38.900506
2530.129849	331092.938434	38.905524
2532.901175	331513.626186	38.910541
2535.350202	331927.709499	38.915559
2537.455023	332347.050563	38.920576
2540.617235	332769.167215	38.925594
2542.895881	333201.629278	38.930612
2545.219379	333630.120303	38.935629
2548.075662	334047.935574	38.940647
2550.009452	334489.864919	38.945664
2553.121210	334921.854161	38.950682
2555.442051	335367.830052	38.955700
2558.004925	335811.911046	38.960717
2560.710510	336254.189069	38.965735
2563.307831	336698.893509	38.970752
2566.127816	337143.508900	38.975770
2568.340634	337594.336762	38.980788
2571.116228	338032.427599	38.985805
2573.752826	338488.158768	38.990823
2576.222679	338942.135773	38.995840
2579.014136	339391.564477	39.000858
2581.624415	339847.315502	39.005876
2584.613385	340296.046329	39.010893
2587.595732	340737.995859	39.015911
2589.842553	341189.935395	39.020928
2592.648507	341634.166159	39.025946
2595.008519	342089.026345	39.030964
2597.744720	342542.579462	39.035981
2600.378687	342986.243643	39.040999
2603.237059	343437.307929	39.046016
2605.950558	343886.665324	39.051034
2608.490096	344335.742205	39.056052
2611.281327	344784.115693	39.061069
2614.119840	345236.184911	39.066087
2616.737066	345688.818809	39.071104
2619.326960	346130.282908	39.076122
2621.648933	346586.510790	39.081140
2624.047257	347026.195806	39.086157
2627.639080	347476.046281	39.091175
2630.093598	347934.857174	39.096192
2632.693886	348380.440145	39.101210
2635.349552	348831.875046	39.106228
2637.804572	349268.842486	39.111245
2640.624831	349709.988067	39.116263
2642.936131	350165.452164	39.121280
2645.562378	350607.865105	39.126298
2648.035799	351027.299420	39.131316
2650.549725	351442.510090	39.136333
2653.968250	351853.157246	39.141351
2656.295003	352269.914208	39.146368
2658.730909	352680.659813	39.151386
2661.377891	353095.303362	39.156404
2663.739574	353517.680232	39.161421
2666.464405	353940.605366	39.166439
2668.694391	354370.738269	39.171456
2671.551670	354790.107099	39.176474
2674.194113	355231.488539	39.181492
2676.413726	355658.109340	39.186509
2679.384656	356105.650019	39.191527
2681.683152	356541.490245	39.196544
2684.118657	357009.439226	39.201562
2686.943944	357461.508919	39.206580
2689.438487	357923.601999	39.211597
2692.194308	358390.141932	39.216615
2694.861193	358866.057287	39.221632
2697.456727	359320.303656	39.226650
2700.732201	359791.519523	39.231668
2703.174783	360268.776407	39.236685
2705.956031	360736.787131	39.241703
2708.992989	361210.844023	39.246720
2711.829493	361685.054808	39.251738
2714.852440	362154.206085	39.256756
2717.572520	362621.801709	39.261773
2720.611139	363079.342749	39.266791
2723.445067	363549.702712	39.271808
2726.207626	364019.739246	39.276826
2729.028813	364481.361383	39.281844
2731.731777	364953.402645	39.286861
2734.691899	365425.601289	39.291879
2737.132495	365885.569063	39.296896
2740.072386	366355.984696	39.301914
2742.622977	366835.846574	39.306932
2745.401933	367314.956546	39.311949
2748.249053	367776.236125	39.316967
2750.649473	368264.226780	39.321984
2753.334052	368747.903806	39.327002
2756.287645	369227.015958	39.332020
2758.923273	369719.774425	39.337037
2761.743398	370206.737857	39.342055
2764.311909	370698.429953	39.347072
2766.883386	371191.359256	39.352090
2769.485676	371692.296232	39.357108
2772.187039	372180.676792	39.362125
2774.899275	372675.900849	39.367143
2777.889611	373189.267738	39.372160
2780.714276	373691.363472	39.377178
2783.497288	374193.891030	39.382196
2785.868807	374711.675716	39.387213
2788.948671	375212.849770	39.392231
2791.410914	375727.689379	39.397248
2794.148794	376226.773811	39.402266
2797.098032	376707.069249	39.407284
2799.571597	377191.823411	39.412301
2802.652745	377659.553270	39.417319
2804.827398	378153.476460	39.422336
2807.359558	378635.083156	39.427354
2810.091593	379120.965150	39.432372
2812.767248	379633.969881	39.437389
2815.642814	380125.474002	39.442407
2818.063536	380633.102289	39.447424
2820.742991	381146.898175	39.452442
2823.435284	381659.543585	39.457460
2826.256928	382182.892157	39.462477
2829.175600	382709.414437	39.467495
2831.341449	383250.076500	39.472512
2833.962682	383778.431996	39.477530
2837.557605	384310.557644	39.482548
2841.367948	384834.854257	39.487565
2844.586463	385358.552278	39.492583
2847.618089	385891.708287	39.497600
2850.498203	386410.219690	39.502618
2853.406878	386937.064109	39.507636
2855.671977	387463.064309	39.512653
2859.138970	387992.113143	39.517671
2862.156904	388530.229269	39.522688
2864.947513	389059.876722	39.527706
2868.405392	389586.164271	39.532724
2870.674752	390128.128457	39.537741
2873.567625	390649.493305	39.542759
2876.433401	391193.172755	39.547776
2879.415808	391730.485049	39.552794
2882.435340	392271.967683	39.557812
2884.908334	392817.408497	39.562829
2887.947214	393349.259690	39.567847
2891.107433	393902.816472	39.572864
2893.708099	394449.225555	39.577882
2896.974627	394986.442086	39.582900
2899.677228	395551.379805	39.587917
2902.608093	396097.278963	39.592935
2905.649815	396652.508565	39.597952
2908.666452	397201.875464	39.602970
2911.544374	397757.315459	39.607988
2913.948306	398316.573869	39.613005
2916.990746	398869.889926	39.618023
2919.742158	399437.593780	39.623040
2922.674449	399997.779481	39.628058
2925.846153	400561.695436	39.633076
2928.353784	401137.724428	39.638093
2931.284817	401702.647363	39.643111
2934.438085	402277.869199	39.648128
2937.506795	402838.668463	39.653146
2940.517753	403418.582453	39.658164
2942.796309	403995.863768	39.663181
2946.217845	404572.978952	39.668199
2949.190636	405153.855743	39.673216
2951.783765	405709.203446	39.678234
2954.627953	406263.893101	39.683252
2957.699221	406804.620095	39.688269
2960.865035	407336.729367	39.693287
2963.717679	407877.041184	39.698304
2966.683351	408409.011420	39.703322
2969.553785	408946.462511	39.708340
2972.089827	409497.821869	39.713357
2975.074138	410050.266165	39.718375
2978.215145	410597.378166	39.723392
2980.619463	411168.168267	39.728410
2983.914896	411719.163880	39.733428
2987.238361	412276.227578	39.738445
2990.289487	412839.279789	39.743463
2992.953095	413402.990819	39.748480
2996.095207	413967.983834	39.753498
2999.214326	414540.901859	39.758516
3001.738501	415114.967135	39.763533
3004.878777	415698.806837	39.768551
3008.095230	416275.501778	39.773568
3010.908136	416862.613379	39.778586
3014.197805	417438.031661	39.783604
3016.993052	418032.622720	39.788621
3020.118852	418626.414179	39.793639
3022.989494	419215.773940	39.798656
3025.721006	419825.489884	39.803674
3028.791876	420434.302727	39.808692
3031.648681	421046.201942	39.813709
3034.755918	421655.489078	39.818727
3037.777259	422271.769095	39.823744
3040.433098	422911.122953	39.828762
3043.432543	423532.495911	39.833780
3046.466916	424157.041311	39.838797
3049.794368	424782.970013	39.843815
3053.157002	425422.406484	39.848832
3056.423438	426059.917759	39.853850
3059.763954	426684.077680	39.858868
3062.559540	427330.727333	39.863885
3065.525834	427961.021410	39.868903
3068.973248	428585.271846	39.873920
3071.794159	429232.884317	39.878938
3075.049128	429856.451202	39.883956
3078.349655	430496.054056	39.888973
3081.297733	431135.038477	39.893991
3084.383196	431779.886601	39.899008
3087.084222	432428.502431	39.904026
3090.644062	433066.430607	39.909044
3093.576843	433716.471482	39.914061
3096.784483	434358.525824	39.919079
3100.021908	434996.482140	39.924096
3103.269941	435648.069828	39.929114
3106.575368	436284.564798	39.934132
3109.147668	436929.515812	39.939149
3112.515617	437570.323601	39.944167
3115.735550	438218.430620	39.949184
3118.631299	438852.519541	39.954202
3121.817711	439450.972826	39.959220
3124.786480	440061.497633	39.964237
3127.917817	440670.006743	39.969255
3130.739356	441269.081062	39.974272
3133.208265	441895.892852	39.979290
3136.184837	442519.570232	39.984308
3139.284391	443141.440001	39.989325
3142.021278	443775.400874	39.994343
3145.115209	444405.390166	39.999360
3147.919040	445059.608283	40.004378
3151.294376	445695.897941	40.009396
3154.094273	446355.042307	40.014413
3157.230931	447007.635346	40.019431
3160.867993	447667.015599	40.024448
3164.253547	448321.102037	40.029466
3167.101110	448983.404792	40.034484
3170.519521	449649.040337	40.039501
3173.792172	450327.283024	40.044519
3176.899363	451005.785030	40.049536
3179.780894	451683.189247	40.054554
3183.233628	452364.734386	40.059572
3186.241842	453060.095193	40.064589
3189.158117	453755.095018	40.069607
3192.595464	454449.029573	40.074624
3195.657590	455144.925096	40.079642
3198.803179	455849.236555	40.084660
3202.376256	456550.776354	40.089677
3205.357574	457252.994863	40.094695
3208.480730	457965.237757	40.099712
3211.677147	458687.514824	40.104730
3214.603185	459399.540216	40.109748
3218.139897	460124.144798	40.114765
3221.317575	460849.389231	40.119783
3224.828292	461568.334272	40.124800
3227.794396	462300.140397	40.129818
3231.482861	463041.671811	40.134836
3234.854097	463781.558531	40.139853
3237.653174	464512.354678	40.144871
3241.234136	465244.013755	40.149888
3244.432325	465989.516349	40.154906
3247.988112	466706.713810	40.159924
3251.215614	467442.095544	40.164941
3254.504024	468186.747531	40.169959
3257.856201	468921.855330	40.174976
3260.890073	469662.499722	40.179994
3263.861723	470399.891130	40.185012
3267.454318	471146.614051	40.190029
3270.610202	471888.625845	40.195047
3274.125323	472625.143724	40.200064
3277.291235	473367.353164	40.205082
3280.925629	474104.911099	40.210100
3284.722661	474845.096050	40.215117
3288.070880	475576.780912	40.220135
3291.555309	476312.057530	40.225152
3295.013405	477019.962599	40.230170
3298.096986	477701.868304	40.235188
3301.710944	478384.374472	40.240205
3304.626777	479059.183311	40.245223
3307.826170	479724.169033	40.250240
3310.762565	480409.644083	40.255258
3313.951890	481092.022709	40.260276
3316.713700	481778.185119	40.265293
3320.324968	482478.845183	40.270311
3323.460112	483173.743591	40.275328
3326.252400	483892.220423	40.280346
3329.609865	484597.796381	40.285364
3332.674985	485322.897601	40.290381
3335.758804	486039.327999	40.295399
3338.984878	486771.675583	40.300416
3342.173598	487515.369039	40.305434
3345.551788	488247.585175	40.310452
3349.069209	489000.969790	40.315469
3352.168706	489750.399348	40.320487
3355.788965	490498.302170	40.325504
3359.654959	491252.299057	40.330522
3363.260366	492016.106141	40.335540
3366.756089	492763.432607	40.340557
3369.910544	493518.561202	40.345575
3373.536166	494281.210894	40.350592
3376.651217	495043.354096	40.355610
3380.129509	495800.660904	40.360628
3383.500077	496558.660307	40.365645
3386.572482	497350.509085	40.370663
3390.198326	498123.047252	40.375680
3393.514671	498904.993140	40.380698
3396.375065	499690.562018	40.385716
3399.821409	500485.798775	40.390733
3403.122457	501274.308283	40.395751
3406.899966	502063.767698	40.400768
3410.413053	502874.385987	40.405786
3413.856302	503674.932521	40.410804
3417.079487	504470.379138	40.415821
3420.269843	505279.120457	40.420839
3424.214790	506077.458949	40.425856
3427.702884	506888.248929	40.430874
3430.771632	507698.764487	40.435892
3434.662795	508515.723119	40.440909
3438.256548	509311.343750	40.445927
3441.663980	510120.076965	40.450944
3444.980998	510930.955967	40.455962
3448.684720	511751.574325	40.460980
3452.331650	512561.263854	40.465997
3455.134036	513373.217559	40.471015
3458.668883	514190.263133	40.476032
3462.260051	515017.399916	40.481050
3465.551991	515835.614442	40.486068
3468.851634	516663.119396	40.491085
3472.072453	517492.209677	40.496103
3475.691447	518326.390529	40.501120
3478.955819	519147.202086	40.506125
3482.494280	519913.015079	40.511130
3485.761781	520632.776061	40.516135
3488.640202	521294.679389	40.521140
3491.397997	521907.587265	40.526144
3494.348296	522469.332437	40.531149
3496.752877	522959.310686	40.536154
3499.295779	523389.097502	40.541159
3501.143228	523770.202991	40.546164
3504.029654	524093.106163	40.551168
3505.996320	524376.569819	40.556173
3507.605121	524593.616511	40.561178
3509.681922	524780.208229	40.566183
3511.076033	524921.768624	40.571188
3512.305324	525016.953411	40.576192
3513.820977	525056.341273	40.581197
3514.774526	525083.080550	40.586202
3516.211060	525067.740593	40.591207
3516.773738	525028.024357	40.596212
3517.739485	524946.140055	40.601216
3518.465204	524849.230661	40.606221
3518.833512	524723.414283	40.611226
3519.990364	524580.741396	40.616231
3520.273742	524416.874452	40.621236
3520.804044	524228.805056	40.626240
3520.993709	524031.334780	40.631245
3521.287787	523827.526973	40.636250
3521.380715	523614.952762	40.641255
3521.548439	523372.893117	40.646260
3521.609159	523132.868805	40.651264
3521.923147	522887.189654	40.656269
3521.842702	522633.885119	40.661274
3522.117137	522357.013182	40.666279
3521.952745	522112.257315	40.671284
3522.226622	521840.027651	40.676288
3522.181591	521558.693209	40.681293
3521.939981	521286.030198	40.686298
3522.068564	520990.957617	40.691303
3521.563092	520716.911185	40.696308
3522.137934	520424.336334	40.701312
3522.026508	520139.195977	40.706317
3521.216628	519847.689208	40.711322
3521.537755	519549.425423	40.716327
3521.119610	519280.700767	40.721332
3520.962190	518983.311355	40.726336
3520.774045	518713.175857	40.731341
3520.328395	518416.529680	40.736346
3520.537508	518135.804283	40.741351
3520.199193	517868.257588	40.746356
3520.070914	517572.911429	40.751360
3519.620395	517299.153377	40.756365
3519.419678	517029.093500	40.761370
3519.371498	516753.492913	40.766375
3518.616767	516484.776019	40.771380
3518.706000	516230.031083	40.776384
3518.705438	515974.032118	40.781389
3518.197232	515709.865915	40.786394
3518.363829	515450.848649	40.791399
3517.696126	515209.104310	40.796404
3517.521710	514954.887352	40.801408
3517.414483	514722.252263	40.806413
3516.689691	514473.374986	40.811418
3516.785903	514233.367209	40.816423
3516.287444	514004.122177	40.821428
3515.918211	513779.658671	40.826432
3515.966906	513563.876525	40.831437
3515.850751	513332.437550	40.836442
3515.554442	513112.961166	40.841447
3515.185232	512911.247857	40.846452
3515.203567	512683.572409	40.851456
3515.227807	512486.496070	40.856461
3514.735982	512276.954120	40.861466
3514.518505	512060.790186	40.866471
3514.373538	511858.775975	40.871476
3514.155212	511679.332329	40.876480
3513.782511	511474.061447	40.881485
3513.703387	511295.350546	40.886490
3513.860990	511098.995834	40.891495
3513.222708	510919.661139	40.896500
3513.221903	510737.441418	40.901504
3513.328096	510555.708735	40.906509
3512.697182	510380.717892	40.911514
3512.948515	510204.321056	40.916519
3512.787659	510037.144501	40.921524
3512.579800	509856.718798	40.926528
3512.287447	509696.440129	40.931533
3512.081600	509525.623077	40.936538
3512.144188	509354.913676	40.941543
3511.714544	509204.618907	40.946548
3511.780979	509042.000718	40.951552
3512.082644	508899.429733	40.956557
3511.333193	508736.077504	40.961562
3511.568135	508578.184202	40.966567
3511.454400	508435.472651	40.971572
3511.206566	508288.733433	40.976576
3511.103941	508145.005802	40.981581
3510.794820	507995.592166	40.986586
3510.945352	507854.554336	40.991591
3510.040871	507727.444676	40.996596
3510.024767	507588.657311	41.001600
3510.316648	507448.251603	41.006605
3510.024220	507332.072764	41.011610
3509.981965	507186.404868	41.016615
3509.716643	507071.231980	41.021620
3509.781632	506957.625317	41.026624
3509.357766	506832.760718	41.031629
3509.525338	506717.466461	41.036634
3509.418912	506591.841548	41.041639
3509.376384	506478.855959	41.046644
3509.109767	506375.772371	41.051648
3509.218564	506251.780837	41.056653
3509.052509	506145.643873	41.061658
3509.065186	506050.559974	41.066663
3508.650081	505917.489803	41.071668
3508.949690	505812.188060	41.076672
3508.665388	505713.758846	41.081677
3508.623542	505610.179769	41.086682
3508.648557	505506.842530	41.091687
3508.275973	505404.883238	41.096692
3508.386925	505308.312234	41.101696
3508.675769	505197.492574	41.106701
3508.291044	505101.909665	41.111706
3508.286896	505007.328799	41.116711
3507.747650	504913.995931	41.121716
3507.887017	504816.759847	41.126720
3507.585243	504733.104854	41.131725
3507.674532	504639.620574	41.136730
3507.906234	504555.273133	41.141735
3507.600560	504470.251116	41.146740
3507.479160	504382.821015	41.151744
3507.490784	504293.446363	41.156749
3507.488344	504213.992623	41.161754
3507.654667	504133.803336	41.166759
3507.040621	504064.921462	41.171764
3507.154909	503965.508471	41.176768
3507.460237	503890.761831	41.181773
3507.067756	503812.633145	41.186778
3507.004974	503724.330150	41.191783
3506.988763	503650.240622	41.196788
3506.667788	503585.561743	41.201792
3506.819195	503504.562193	41.206797
3506.582292	503447.258562	41.211802
3506.899212	503371.394466	41.216807
3506.388630	503317.524559	41.221812
3506.509302	503235.010315	41.226816
3506.820326	503164.915879	41.231821
3506.608931	503105.025950	41.236826
3506.833562	503029.174971	41.241831
3506.566518	502967.876256	41.246836
3506.323879	502899.336009	41.251840
3506.630427	502827.165864	41.256845
3506.599411	502770.131164	41.261850
3506.528373	502695.287113	41.266855
3506.524619	502646.295046	41.271860
3506.528240	502570.628869	41.276864
3506.665911	502498.737140	41.281869
3506.261930	502432.346321	41.286874
3506.253817	502362.754666	41.291879
3506.704897	502299.669896	41.296884
3506.550223	502233.238926	41.301888
3506.212291	502174.327502	41.306893
3506.138691	502111.274378	41.311898
3506.046049	502053.032375	41.316903
3506.070852	501993.354420	41.321908
3506.046512	501934.746934	41.326912
3506.246189	501863.804505	41.331917
3505.574415	501818.509371	41.336922
3506.102949	501756.372109	41.341927
3505.752007	501706.420022	41.346932
3505.567370	501639.839720	41.351936
3505.531255	501593.380621	41.356941
3505.549185	501538.105759	41.361946
3505.815793	501492.914553	41.366951
3505.541841	501442.089088	41.371956
3505.710799	501385.423254	41.376960
3505.913149	501330.675375	41.381965
3505.496194	501295.968011	41.386970
3505.810727	501229.408508	41.391975
3505.663524	501180.131369	41.396980
3505.278408	501146.532246	41.401984
3505.361760	501083.551901	41.406989
3505.133361	501042.790839	41.411994
3505.470084	500973.291090	41.416999
3505.149278	500957.397431	41.422004
3505.461806	500898.935757	41.427008
3505.279175	500858.420125	41.432013
3505.555037	500806.797300	41.437018
3505.318528	500763.455383	41.442023
3505.466232	500713.371076	41.447028
3505.792999	500669.079395	41.452032
3505.585321	500622.543645	41.457037
3505.155961	500565.514212	41.462042
3505.141621	500523.705764	41.467047
3505.095293	500482.914644	41.472052
3505.084102	500436.651064	41.477056
3505.399443	500398.282900	41.482061
3505.000492	500358.762082	41.487066
3505.306923	500302.577270	41.492071
3504.976156	500273.624860	41.497076
3504.979865	500225.029898	41.502080
3505.089483	500188.364236	41.507085
3504.907154	500152.453316	41.512090
3504.951027	500107.850624	41.517095
3504.911482	500070.702101	41.522100
3504.921587	500038.354533	41.527104
3505.115118	499990.640088	41.532109
3504.526057	499944.669052	41.537114
3504.859753	499915.813520	41.542119
3504.856955	499883.720812	41.547124
3504.829412	499846.418067	41.552128
3505.292554	499813.441663	41.557133
3505.126621	499770.086182	41.562138
3505.146693	499722.955267	41.567143
3504.739183	499694.823981	41.572148
3504.838471	499645.655512	41.577152
3505.220903	499603.377235	41.582157
3504.803062	499569.071620	41.587162
3505.188927	499516.212781	41.592167
3505.363798	499486.014888	41.597172
3505.076530	499446.828752	41.602176
3505.127278	499399.084680	41.607181
3505.046092	499358.600239	41.612186
3505.019952	499322.966700	41.617191
3505.016324	499264.296553	41.622196
3505.103392	499231.429146	41.627200
3505.042300	499197.825765	41.632205
3504.808302	499155.745111	41.637210
3504.933623	499110.468977	41.642215
3504.855041	499083.752791	41.647220
3504.884059	499037.934849	41.652224
3504.825775	498992.484948	41.657229
3504.951945	498966.799302	41.662234
3504.832543	498922.219472	41.667239
3504.895092	498884.748620	41.672244
3504.615016	498852.697897	41.677248
3505.051134	498802.461421	41.682253
3504.959583	498771.038856	41.687258
3504.867591	498728.580394	41.692263
3504.974269	498700.163782	41.697268
3504.936390	498648.786832	41.702272
3504.797577	498614.637785	41.707277
3504.867316	498583.037528	41.712282
3505.090571	498541.845020	41.717287
3504.639086	498498.734100	41.722292
3504.568941	498473.787520	41.727296
3505.000447	498428.005658	41.732301
3504.836162	498393.860219	41.737306
3504.860986	498358.824208	41.742311
3504.669666	498322.303555	41.747316
3504.358207	498289.092422	41.752320
3504.770711	498254.703680	41.757325
3504.434669	498238.810013	41.762330
3504.580339	498180.416487	41.767335
3504.142324	498160.235743	41.772340
3504.244485	498129.490193	41.777344
3504.783908	498100.497987	41.782349
3504.486562	498078.168657	41.787354
3504.719788	498036.416541	41.792359
3504.484658	497996.054620	41.797364
3504.525224	497966.584167	41.802368
3504.813204	497930.442594	41.807373
3504.446730	497912.579047	41.812378
3504.568560	497874.489219	41.817383
3504.278364	497850.184068	41.822388
3504.381703	497814.172698	41.827392
3504.468064	497778.265193	41.832397
3504.352269	497752.261682	41.837402
3504.331733	497730.596936	41.842407
3504.177240	497686.677740	41.847412
3504.489176	497667.694194	41.852416
3504.688075	497640.628253	41.857421
3504.125638	497617.277096	41.862426
3504.410969	497582.299658	41.867431
3504.622429	497551.383971	41.872436
3504.127001	497519.820558	41.877440
3503.992523	497495.237182	41.882445
3504.218689	497468.926079	41.887450
3504.433022	497439.984201	41.892455
3504.172985	497415.218054	41.897460
3504.242935	497377.287262	41.902464
3504.383327	497361.368144	41.907469
3504.050889	497339.701603	41.912474
3504.453411	497304.300087	41.917479
3504.534818	497276.847155	41.922484
3504.374059	497244.319068	41.927488
3504.561609	497209.457622	41.932493
3504.382694	497177.236051	41.937498
3504.227749	497146.023192	41.942503
3504.031794	497129.498871	41.947508
3504.301684	497089.763897	41.952512
3504.185270	497071.657482	41.957517
3504.029890	497043.634086	41.962522
3503.939644	497020.359408	41.967527
3504.197655	496992.928760	41.972532
3503.955648	496978.487342	41.977536
3504.359487	496954.375059	41.982541
3504.234641	496925.637857	41.987546
3504.435558	496907.531749	41.992551
3504.222720	496872.935456	41.997556
3504.135975	496841.508779	42.002560
3504.604054	496822.550300	42.007565
3503.991727	496802.041187	42.012570
3504.347796	496773.126473	42.017575
3504.332851	496739.511226	42.022580
3504.320661	496709.945812	42.027584
3504.257301	496678.515156	42.032589
3504.097856	496643.049290	42.037594
3504.495614	496624.354866	42.042599
3504.532021	496601.819073	42.047604
3504.000576	496565.044859	42.052608
3504.562595	496542.932210	42.057613
3504.039851	496513.852211	42.062618
3504.652366	496486.719176	42.067623
3504.534104	496448.006117	42.072628
3504.135849	496421.994714	42.077632
3504.415963	496379.421298	42.082637
3504.201258	496368.215401	42.087642
3503.951725	496331.649305	42.092647
3504.040086	496315.484346	42.097652
3504.037883	496294.827594	42.102656
3504.212793	496275.003539	42.107661
3503.772388	496251.175658	42.112666
3504.042155	496235.032585	42.117671
3504.399169	496201.205661	42.122676
3503.788724	496180.695548	42.127680
3504.124659	496139.581036	42.132685
3503.963650	496115.658185	42.137690
3504.093578	496098.828264	42.142695
3503.872587	496077.851431	42.147700
3503.781429	496064.499322	42.152704
3504.055610	496031.545902	42.157709
3504.006294	496017.427680	42.162714
3504.094699	495993.920927	42.167719
3504.355741	495970.437487	42.172724
3503.735636	495942.739005	42.177728
3504.053210	495916.158054	42.182733
3504.140326	495902.828280	42.187738
3504.223563	495876.081785	42.192743
3504.036774	495848.517194	42.197748
3503.730715	495826.743414	42.202752
3504.226932	495795.830369	42.207757
3503.848009	495787.029757	42.212762
3503.849476	495755.435368	42.217767
3503.936794	495735.472677	42.222772
3504.040832	495717.380701	42.227776
3504.056863	495687.758535	42.232781
3503.888005	495665.608453	42.237786
3503.970231	495637.545336	42.242791
3503.984071	495619.467520	42.247796
3503.715861	495601.079841	42.252800
3503.966637	495578.913959	42.257805
3503.503801	495564.405057	42.262810
3503.693193	495540.983023	42.267815
3504.011314	495528.122787	42.272820
3504.249328	495512.642317	42.277824
3504.425427	495484.057802	42.282829
3503.997668	495463.214209	42.287834
3504.045319	495431.865124	42.292839
3503.767406	495407.301597	42.297844
3503.383026	495392.223197	42.302848
3504.022300	495374.198181	42.307853
3503.806789	495353.776610	42.312858
3503.842943	495343.644355	42.317863
3503.953168	495302.259839	42.322868
3503.725561	495293.840135	42.327872
3503.937553	495269.705320	42.332877
3504.012358	495259.212477	42.337882
3504.464615	495220.254738	42.342887
3504.112804	495202.639370	42.347892
3503.858559	495182.071830	42.352896
3504.284485	495162.763862	42.357901
3503.983107	495128.836487	42.362906
3503.925142	495108.845443	42.367911
3504.080189	495098.238558	42.372916
3503.940364	495067.526084	42.377920
3503.947862	495032.486402	42.382925
3503.755968	495019.301353	42.387930
3504.041905	494996.369702	42.392935
3504.051053	494975.912200	42.397940
3503.717988	494948.875712	42.402944
3504.046434	494929.228468	42.407949
3503.661758	494895.617631	42.412954
3503.633856	494885.748418	42.417959
3503.811772	494865.162849	42.422964
3503.929239	494846.966622	42.427968
3504.133581	494825.566683	42.432973
3503.978102	494807.818634	42.437978
3504.285420	494780.326239	42.442983
3504.146313	494754.220862	42.447988
3503.887675	494733.349704	42.452992
3504.162157	494702.469864	42.457997
3504.124167	494686.374072	42.463002
3504.079948	494666.431007	42.468007
3504.125261	494639.891240	42.473012
3503.951547	494604.221130	42.478016
3504.104960	494584.702453	42.483021
3503.756639	494578.883885	42.488026
3503.932473	494543.107772	42.493031
3504.026957	494524.307237	42.498036
3503.684019	494505.272011	42.503040
3503.789980	494482.368165	42.508045
3503.581419	494464.071186	42.513050
3503.993076	494452.461297	42.518055
3504.047274	494427.641421	42.523060
3503.604885	494412.520745	42.528064
3504.162836	494377.899165	42.533069
3503.627090	494370.742994	42.538074
3503.722946	494344.802439	42.543079
3503.893248	494318.039908	42.548084
3503.670348	494323.999558	42.553088
3503.802118	494292.989680	42.558093
3503.666651	494270.225002	42.563098
3503.637045	494259.140461	42.568103
3503.785217	494227.317705	42.573108
3503.577373	494214.894138	42.578112
3503.802206	494202.300901	42.583117
3503.519835	494183.863400	42.588122
3503.421029	494170.713662	42.593127
3503.820378	494150.548019	42.598132
3503.581350	494134.129065	42.603136
3503.763509	494115.972526	42.608141
3503.829594	494106.037402	42.613146
3503.900275	494091.037911	42.618151
3503.711394	494064.433057	42.623156
3503.664971	494045.299849	42.628160
3503.832829	494033.626959	42.633165
3503.803229	494006.085387	42.638170
3503.729610	493995.260826	42.643175
3503.980790	493966.155716	42.648180
3503.486708	493946.485522	42.653184
3503.865609	493937.057868	42.658189
3503.750053	493911.960307	42.663194
3503.981003	493890.099343	42.668199
3503.537497	493873.509929	42.673204
3503.807881	493854.528997	42.678208
3503.951856	493836.023758	42.683213
3503.638167	493818.856768	42.688218
3503.773871	493808.454746	42.693223
3504.335498	493772.059148	42.698228
3503.960922	493761.737754	42.703232
3503.981281	493733.782780	42.708237
3503.782108	493716.445682	42.713242
3504.045531	493687.135647	42.718247
3503.797803	493665.552627	42.723252
3503.817626	493642.205614	42.728256
3503.970873	493621.673192	42.733261
3503.386993	493609.004824	42.738266
3503.839191	493588.475751	42.743271
3504.019965	493565.457665	42.748276
3504.057059	493542.512899	42.753280
3503.649815	493527.284663	42.758285
3503.704981	493506.058684	42.763290
3503.968252	493481.407039	42.768295
3504.131769	493467.455766	42.773300
3503.429753	493443.361748	42.778304
3503.852823	493413.823493	42.783309
3503.668427	493411.422041	42.788314
3503.558567	493392.247545	42.793319
3503.512195	493371.138736	42.798324
3503.439329	493359.807299	42.803329
3503.554776	493340.242668	42.808333
3503.090984	493308.211223	42.813338
3503.393587	493289.123341	42.818343
3503.503862	493298.271527	42.823348
3503.403956	493280.462581	42.828353
3503.602036	493251.466015	42.833357
3503.354217	493255.961425	42.838362
3503.376610	493240.108017	42.843367
3503.635856	493212.063856	42.848372
3503.122277	493211.182934	42.853377
3503.454023	493204.243660	42.858381
3503.507733	493190.917200	42.863386
3503.349650	493175.851846	42.868391
3503.653636	493167.954808	42.873396
3502.939972	493168.472759	42.878401
3503.379513	493130.424112	42.883405
3503.184534	493113.693451	42.888410
3503.467402	493118.813961	42.893415
3503.564842	493102.492822	42.898420
3503.680389	493084.041963	42.903425
3503.855578	493077.076749	42.908429
3503.719510	493059.020110	42.913434
3503.718656	493032.839800	42.918439
3503.946678	493022.372105	42.923444
3503.524739	493002.841417	42.928449
3503.806796	492989.579998	42.933453
3503.717631	492970.047316	42.938458
3503.786244	492946.792991	42.943463
3503.518019	492936.656882	42.948468
3503.746095	492916.618245	42.953473
3503.843634	492903.942965	42.958477
3503.617053	492883.216561	42.963482
3503.850914	492849.352300	42.968487
3504.046547	492841.776088	42.973492
3503.545099	492830.106950	42.978497
3503.963543	492799.353091	42.983501
3503.964924	492782.439175	42.988506
3503.597721	492762.848941	42.993511
3503.836488	492740.529623	42.998516
3503.748195	492712.083877	43.003521
3503.645699	492697.566388	43.008525
3503.634623	492674.223037	43.013530
3503.675789	492660.290495	43.018535
3503.952348	492655.993035	43.023540
3503.600660	492641.362969	43.028545
3503.527678	492627.043321	43.033549
3503.701387	492602.708506	43.038554
3503.655081	492586.561554	43.043559
3503.996403	492567.011045	43.048564
3503.658542	492561.797868	43.053569
3503.547784	492533.861805	43.058573
3503.619605	492508.276954	43.063578
3503.675371	492492.468272	43.068583
3503.820466	492474.164058	43.073588
3503.409527	492474.026486	43.078593
3503.648461	492450.187569	43.083597
3503.640573	492431.502367	43.088602
3503.423798	492411.736061	43.093607
3503.687814	492401.768737	43.098612
3503.609154	492387.196596	43.103617
3503.596077	492355.497388	43.108621
3503.912323	492346.737166	43.113626
3503.397968	492326.156905	43.118631
3503.550928	492313.016691	43.123636
3503.736989	492307.923196	43.128641
3503.658264	492288.388145	43.133645
3503.633157	492266.059324	43.138650
3503.287050	492249.301127	43.143655
3503.569977	492230.924247	43.148660
3503.470065	492230.838794	43.153665
3503.592294	492211.119974	43.158669
3503.371283	492177.528951	43.163674
3503.362222	492168.212363	43.168679
3504.009971	492160.108639	43.173684
3503.655126	492148.365255	43.178689
3503.498650	492127.069864	43.183693
3503.848705	492111.366268	43.188698
3503.288767	492097.224463	43.193703
3503.600050	492091.554056	43.198708
3503.344891	492075.540955	43.203713
3503.795889	492041.640900	43.208717
3503.654219	492044.094144	43.213722
3503.655334	492025.052616	43.218727
3503.692415	491996.434030	43.223732
3503.701638	492000.534620	43.228737
3503.639759	491959.271092	43.233741
3503.795822	491955.347013	43.238746
3503.673440	491926.044532	43.243751
3503.940195	491915.722019	43.248756
3503.644155	491919.263169	43.253761
3503.607963	491885.895617	43.258765
3503.732663	491867.492745	43.263770
3503.252133	491848.172667	43.268775
3503.666333	491818.785205	43.273780
3503.353173	491822.329079	43.278785
3503.544535	491803.510467	43.283789
3503.344227	491790.425721	43.288794
3503.292792	491780.153427	43.293799
3503.478772	491768.223033	43.298804
3503.295685	491756.249682	43.303809
3503.409461	491739.215764	43.308813
3503.361102	491720.485601	43.313818
3503.278943	491727.031551	43.318823
3503.280025	491708.040346	43.323828
3503.263084	491690.419330	43.328833
3503.615410	491673.803434	43.333837
3503.494554	491672.556500	43.338842
3503.446112	491653.319852	43.343847
3503.763784	491627.846860	43.348852
3503.486218	491632.499291	43.353857
3503.724972	491599.442269	43.358861
3503.859103	491596.483801	43.363866
3503.686976	491576.760193	43.368871
3503.881928	491559.460064	43.373876
3503.706690	491549.511070	43.378881
3503.806072	491523.920508	43.383885
3503.619180	491505.060095	43.388890
3503.602155	491489.464640	43.393895
3503.476549	491463.149904	43.398900
3503.498119	491459.297623	43.403905
3503.565362	491439.384103	43.408909
3503.404590	491426.495426	43.413914
3503.559876	491402.870965	43.418919
3503.767064	491401.825380	43.423924
3503.591449	491376.632589	43.428929
3503.811486	491366.874239	43.433933
3503.536289	491340.734906	43.438938
3503.565782	491323.612643	43.443943
3503.504209	491310.353699	43.448948
3503.704368	491302.877436	43.453953
3503.379384	491269.301205	43.458957
3503.364504	491275.127663	43.463962
3502.976679	491253.260110	43.468967
3503.612740	491226.166277	43.473972
3503.263468	491235.084252	43.478977
3503.293530	491214.568639	43.483981
3503.336111	491214.308725	43.488986
3503.428375	491193.175527	43.493991
3503.574863	491196.798798	43.498996
3503.332795	491192.582978	43.504001
3503.563012	491162.970343	43.509005
3503.729120	491141.926703	43.514010
3503.347046	491144.873863	43.519015
3503.769752	491104.494092	43.524020
3503.717913	491099.893672	43.529025
3503.706312	491093.159819	43.534029
3503.873557	491071.660119	43.539034
3503.991294	491049.256616	43.544039
3503.950223	491019.484055	43.549044
3503.808878	491005.629766	43.554049
3503.658581	490988.890127	43.559053
3503.851345	490973.007857	43.564058
3503.727459	490948.515339	43.569063
3503.907328	490931.926042	43.574068
3503.632557	490926.651786	43.579073
3503.549986	490883.211410	43.584077
3503.481797	490876.182553	43.589082
3503.516679	490871.770949	43.594087
3503.723599	490836.337286	43.599092
3503.360721	490828.544665	43.604097
3503.793705	490811.813964	43.609101
3503.609902	490797.763651	43.614106
3503.585980	490779.332552	43.619111
3503.802375	490770.030275	43.624116
3503.290433	490744.535272	43.629121
3503.487247	490745.922275	43.634125
3503.376837	490729.479972	43.639130
3503.363876	490704.564437	43.644135
3503.641192	490680.767838	43.649140
3503.607217	490694.650154	43.654145
3503.610177	490662.692302	43.659149
3503.447082	490656.488695	43.664154
3503.255062	490639.704691	43.669159
3503.430279	490606.757247	43.674164
3503.619213	490599.839582	43.679169
3503.617972	490583.734416	43.684173
3503.284109	490574.367079	43.689178
3503.825661	490557.618991	43.694183
3503.812944	490545.617932	43.699188
3503.589395	490518.405717	43.704193
3503.505423	490506.821065	43.709197
3503.519835	490487.877158	43.714202
3503.399871	490471.993247	43.719207
3503.675145	490458.883041	43.724212
3503.689668	490453.056462	43.729217
3503.750917	490427.673012	43.734221
3503.733703	490425.649916	43.739226
3503.865492	490393.975121	43.744231
3503.870531	490379.742706	43.749236
3503.367110	490350.194098	43.754241
3503.568291	490335.474827	43.759245
3503.784220	490321.816794	43.764250
3503.685669	490307.651344	43.769255
3503.533971	490289.239959	43.774260
3503.669023	490279.190595	43.779265
3503.466718	490256.482202	43.784269
3503.607001	490240.405018	43.789274
3503.694751	490229.907283	43.794279
3503.696543	490194.656769	43.799284
3503.541852	490183.944094	43.804289
3503.628416	490174.611396	43.809293
3504.028367	490147.198797	43.814298
3503.550178	490130.662157	43.819303
3503.689714	490104.962013	43.824308
3503.432286	490089.859213	43.829313
3503.889671	490076.010894	43.834317
3503.670326	490058.876158	43.839322
3503.572293	490043.292300	43.844327
3503.575496	490028.046960	43.849332
3503.399579	490010.905315	43.854337
3503.593992	490002.011312	43.859341
3503.568547	489992.848172	43.864346
3503.272877	489963.570001	43.869351
3503.348948	489960.012682	43.874356
3503.154346	489966.121191	43.879361
3503.437911	489937.916321	43.884365
3503.456278	489927.530679	43.889370
3503.393968	489920.449885	43.894375
3503.662047	489898.629016	43.899380
3503.378812	489886.568998	43.904385
3503.617258	489869.159137	43.909389
3503.806644	489859.658088	43.914394
3503.242657	489838.373849	43.919399
3503.429428	489814.489167	43.924404
3503.498696	489820.606665	43.929409
3503.709353	489793.426061	43.934413
3503.391394	489780.206558	43.939418
3503.163628	489773.303805	43.944423
3503.668360	489766.791752	43.949428
3503.660640	489750.383006	43.954433
3503.687915	489728.397408	43.959437
3503.560221	489707.145355	43.964442
3502.913234	489697.117993	43.969447
3503.586017	489680.804219	43.974452
3503.673641	489686.311078	43.979457
3503.419677	489661.533547	43.984461
3503.483281	489638.275891	43.989466
3503.408058	489636.211230	43.994471
3503.813371	489605.099653	43.999476
3503.431448	489610.984643	44.004481
3503.339447	489591.955355	44.009485
3503.792928	489566.306149	44.014490
3503.184719	489567.111403	44.019495
3503.504826	489545.535144	44.024500
3503.069193	489540.437866	44.029505
3503.521990	489512.661448	44.034509
3503.534959	489507.290660	44.039514
3503.288101	489500.846664	44.044519
3503.475456	489477.974440	44.049524
3503.350646	489469.434537	44.054529
3503.546664	489455.576426	44.059533
3503.506318	489451.277677	44.064538
3503.475003	489421.906228	44.069543
3503.326324	489416.003824	44.074548
3503.408105	489416.446777	44.079553
3503.133385	489381.998180	44.084557
3503.212513	489376.971442	44.089562
3502.836377	489370.294589	44.094567
3503.159300	489360.265688	44.099572
3503.530087	489365.018796	44.104577
3503.430373	489338.696981	44.109581
3503.772479	489316.053347	44.114586
3503.547201	489308.542238	44.119591
3503.570273	489276.477548	44.124596
3503.279818	489275.358558	44.129601
3503.480730	489262.309923	44.134605
3503.339955	489248.859441	44.139610
3503.314310	489237.467383	44.144615
3503.556248	489217.929088	44.149620
3503.826555	489214.239627	44.154625
3503.666166	489177.999849	44.159629
3503.407480	489175.558938	44.164634
3503.206552	489175.438786	44.169639
3503.249436	489137.394058	44.174644
3503.007686	489138.394654	44.179649
3503.064785	489130.686891	44.184653
3503.502971	489125.046184	44.189658
3503.193524	489126.766579	44.194663
3503.195649	489098.604936	44.199668
3503.413394	489090.415915	44.204673
3503.364879	489089.005423	44.209677
3503.488992	489075.918148	44.214682
3503.251946	489056.506044	44.219687
3503.545275	489040.707545	44.224692
3503.417422	489038.043336	44.229697
3503.403190	489020.115480	44.234701
3503.812118	489005.666234	44.239706
3503.410122	489006.540215	44.244711
3503.438916	488986.680818	44.249716
3503.426609	488958.875800	44.254721
3503.523163	488945.792791	44.259725
3503.568848	488948.419426	44.264730
3503.379323	488925.960655	44.269735
3503.634103	488910.370742	44.274740
3503.410833	488897.287601	44.279745
3503.298437	488881.958303	44.284749
3503.621449	488863.571788	44.289754
3503.411646	488873.735099	44.294759
3503.692690	488843.654919	44.299764
3503.365845	488833.779094	44.304769
3503.301886	488820.974623	44.309773
3503.434402	488804.644188	44.314778
3503.456682	488785.798624	44.319783
3503.666780	488772.748199	44.324788
3503.694199	488765.095629	44.329793
3503.335071	488749.096110	44.334797
3503.397993	488721.177548	44.339802
3503.213879	488731.640780	44.344807
3503.481160	488700.904087	44.349812
3503.371655	488684.358547	44.354817
3503.391924	488677.416186	44.359821
3503.193660	488661.239213	44.364826
3502.948826	488652.363352	44.369831
3503.315850	488631.183842	44.374836
3503.207785	488638.393428	44.379841
3503.240563	488633.373818	44.384845
3503.578885	488626.583772	44.389850
3503.347506	488599.218060	44.394855
3503.589273	488584.997520	44.399860
3503.736577	488589.279636	44.404865
3503.696896	488559.300350	44.409869
3503.575295	488547.163272	44.414874
3503.144377	488536.189409	44.419879
3503.409707	488501.451235	44.424884
3503.339778	488500.854507	44.429889
3503.020396	488499.284178	44.434893
3503.392805	488494.616061	44.439898
3503.822896	488479.099386	44.444903
3503.678793	488445.388205	44.449908
3503.488154	488443.594915	44.454913
3503.634306	488416.726434	44.459917
3503.558105	488401.593632	44.464922
3503.231980	488389.995298	44.469927
3503.560341	488362.236859	44.474932
3503.592399	488362.738348	44.479937
3503.360209	488351.783618	44.484941
3503.479180	488335.100355	44.489946
3503.617156	488322.516888	44.494951
3503.391495	488314.954789	44.499956
3503.356798	488304.627293	44.504961
3503.431627	488282.075319	44.509965
3503.771817	488278.779850	44.514970
3503.557606	488255.767010	44.519975
3503.611839	488237.219762	44.524980
3503.872446	488224.819456	44.529985
3503.440960	488214.706583	44.534989
3503.522613	488175.488788	44.539994
3503.387270	488186.704398	44.544999
3503.367667	488154.138024	44.550004
3503.238250	488142.457793	44.555009
3503.340262	488135.654271	44.560013
3503.592683	488126.800870	44.565018
3503.630211	488109.522451	44.570023
3503.245896	488096.261598	44.575028
3503.792882	488091.515137	44.580033
3503.341861	488070.514955	44.585037
3503.401403	488054.043448	44.590042
3503.250213	488059.537878	44.595047
3503.267120	488031.119045	44.600052
3503.452882	488020.148713	44.605057
3503.478833	488007.126868	44.610061
3503.467384	488000.797106	44.615066
3503.263443	487983.100863	44.620071
3503.469186	487962.098057	44.625076
3503.481472	487954.599510	44.630081
3503.012890	487945.657375	44.635085
3503.533617	487914.271509	44.640090
3503.445317	487912.411339	44.645095
3503.581149	487909.401373	44.650100
3503.335951	487894.750755	44.655105
3503.140971	487864.744262	44.660109
3503.415935	487862.218829	44.665114
3503.234180	487865.945282	44.670119
3503.524475	487840.826065	44.675124
3503.400626	487817.545143	44.680129
3503.223029	487823.195775	44.685133
3503.474130	487814.443744	44.690138
3503.442878	487796.365457	44.695143
3503.841441	487767.885904	44.700148
3503.639747	487763.865541	44.705153
3503.306786	487734.792415	44.710157
3503.560587	487734.600376	44.715162
3503.051063	487732.654806	44.720167
3503.105543	487719.425639	44.725172
3503.251645	487691.998949	44.730177
3503.279366	487681.357324	44.735181
3503.227695	487677.769114	44.740186
3503.261055	487677.561264	44.745191
3503.507637	487656.045127	44.750196
3503.200488	487643.531566	44.755201
3502.965779	487630.702624	44.760205
3503.290187	487621.584341	44.765210
3502.951411	487625.994160	44.770215
3503.126263	487618.267169	44.775220
3503.041732	487597.411149	44.780225
3503.031743	487579.379948	44.785229
3503.154317	487569.888310	44.790234
3503.197538	487587.002571	44.795239
3503.221339	487566.483972	44.800244
3502.848587	487576.825695	44.805249
3502.853750	487554.182559	44.810253
3503.025713	487545.138989	44.815258
3502.886037	487541.412701	44.820263
3503.055645	487531.508376	44.825268
3503.241710	487543.484030	44.830273
3503.140735	487536.155182	44.835277
3503.134532	487526.937148	44.840282
3503.262039	487508.073680	44.845287
3503.518184	487498.003698	44.850292
3503.206287	487495.216398	44.855297
3503.177178	487497.297860	44.860301
3503.304952	487478.029087	44.865306
3503.073336	487461.147198	44.870311
3503.075303	487447.774180	44.875316
3503.193772	487459.051410	44.880321
3503.264923	487443.337354	44.885325
3503.214196	487425.667027	44.890330
3503.225587	487406.872467	44.895335
3503.124666	487393.768945	44.900340
3503.326674	487389.178148	44.905345
3503.125360	487394.072838	44.910349
3503.185637	487379.018956	44.915354
3502.906800	487367.260556	44.920359
3502.979288	487349.520028	44.925364
3503.093019	487352.794639	44.930369
3503.397695	487352.695864	44.935373
3503.621369	487345.011700	44.940378
3502.897978	487329.929683	44.945383
3503.013475	487312.182322	44.950388
3503.080724	487313.134170	44.955393
3503.001199	487299.875237	44.960397
3503.075950	487296.418937	44.965402
3503.182145	487305.418734	44.970407
3503.499963	487282.877821	44.975412
3503.532391	487276.490228	44.980417
3503.507938	487258.866248	44.985421
3503.501490	487240.530236	44.990426
3503.232556	487230.847037	44.995431
3503.571151	487209.721092	45.000436
3503.272762	487214.935102	45.005441
3503.442089	487201.028907	45.010445
3503.659611	487174.198041	45.015450
3503.483402	487177.113270	45.020455
3503.442298	487156.249902	45.025460
3503.408804	487145.364377	45.030465
3503.198851	487129.187941	45.035469
3503.350083	487125.618210	45.040474
3503.377811	487103.578834	45.045479
3503.669438	487084.030487	45.050484
3503.732014	487079.410998	45.055489
3503.588825	487055.068436	45.060493
3503.580770	487044.229488	45.065498
3503.460023	487031.432782	45.070503
3503.548297	487010.650115	45.075508
3503.617474	486999.191068	45.080513
3503.491381	486989.434512	45.085517
3503.274803	486962.418685	45.090522
3503.264378	486947.578259	45.095527
3503.710114	486938.085883	45.100532
3503.319437	486924.977182	45.105537
3502.936463	486909.689055	45.110541
3503.531723	486892.523996	45.115546
3503.201588	486888.270469	45.120551
3503.215437	486892.320785	45.125556
3503.242267	486864.050605	45.130561
3503.071344	486855.162217	45.135565
3503.310564	486852.389022	45.140570
3502.834183	486847.044171	45.145575
3503.162628	486844.459496	45.150580
3503.178991	486833.312633	45.155585
3503.187001	486825.966284	45.160589
3503.336767	486815.760788	45.165594
3503.206850	486804.839653	45.170599
3503.097484	486808.960119	45.175604
3503.258275	486797.233189	45.180609
3503.345615	486774.069575	45.185613
3503.298763	486758.120324	45.190618
3503.061681	486776.090119	45.195623
3503.421086	486756.328098	45.200628
3503.131868	486733.730517	45.205633
3503.028575	486721.690688	45.210637
3503.276183	486713.799862	45.215642
3503.271490	486720.639242	45.220647
3503.050541	486714.798073	45.225652
3502.762325	486693.213411	45.230657
3503.026326	486672.503912	45.235661
3503.115408	486667.576196	45.240666
3502.863952	486675.062474	45.245671
3502.953121	486665.575666	45.250676
3503.141198	486663.114467	45.255681
3502.984795	486671.446881	45.260685
3503.167514	486662.553162	45.265690
3502.934982	486643.897716	45.270695
3502.995207	486632.085267	45.275700
3502.839390	486612.961757	45.280705
3502.705401	486624.026104	45.285709
3503.073935	486615.102992	45.290714
3502.823910	486631.808555	45.295719
3503.185295	486622.329354	45.300724
3503.044995	486629.038232	45.305729
3502.862416	486617.568092	45.310733
3503.069797	486620.017522	45.315738
3503.422327	486590.429041	45.320743
3503.404934	486580.452468	45.325748
3503.439931	486580.295004	45.330753
3503.342484	486568.254154	45.335757
3503.545340	486544.666750	45.340762
3503.099227	486533.947408	45.345767
3503.233287	486533.622316	45.350772
3503.288817	486523.228932	45.355777
3503.072704	486504.368127	45.360781
3503.310197	486485.232978	45.365786
3503.178356	486479.124367	45.370791
3503.206752	486484.540207	45.375796
3503.415615	486469.563435	45.380801
3503.212895	486453.182653	45.385805
3503.371702	486434.971717	45.390810
3503.209533	486422.941006	45.395815
3503.287806	486422.371444	45.400820
3503.344799	486397.743115	45.405825
3503.060504	486382.236338	45.410829
3503.320030	486386.653186	45.415834
3503.239376	486389.654746	45.420839
3503.177260	486371.529326	45.425844
3502.863080	486362.714008	45.430849
3503.156677	486342.708676	45.435853
3503.481139	486351.218509	45.440858
3503.201984	486343.106848	45.445863
3503.091794	486330.763919	45.450868
3503.287484	486306.012234	45.455873
3503.082427	486288.111958	45.460877
3503.242895	486285.097843	45.465882
3503.235813	486292.393671	45.470887
3503.233909	486274.765217	45.475892
3502.940712	486259.462377	45.480897
3502.933092	486245.431482	45.485901
3503.234732	486238.545071	45.490906
3503.302422	486253.377072	45.495911
3503.459554	486244.031285	45.500916
3503.545789	486225.071757	45.505921
3503.214354	486218.994610	45.510925
3503.220572	486192.854314	45.515930
3503.162911	486205.933145	45.520935
3503.266687	486183.171478	45.525940
3503.487627	486165.710331	45.530945
3503.120614	486161.665100	45.535949
3503.457975	486162.017076	45.540954
3503.291592	486132.965828	45.545959
3502.991022	486129.467325	45.550964
3503.082395	486120.435819	45.555969
3503.282196	486119.188486	45.560973
3503.539608	486110.991915	45.565978
3503.247818	486088.495291	45.570983
3503.369756	486081.231964	45.575988
3503.388639	486074.491504	45.580993
3503.242661	486079.681731	45.585997
3503.379415	486044.908739	45.591002
3503.256693	486040.166314	45.596007
3503.052858	486019.783346	45.601012
3503.552849	486023.605031	45.606017
3503.119959	485998.547038	45.611021
3503.167152	485992.561947	45.616026
3502.878113	485979.183237	45.621031
3503.221985	485983.586848	45.626036
3503.224969	485974.366611	45.631041
3502.955679	485977.246076	45.636045
3503.162932	485945.095989	45.641050
3503.084941	485938.370793	45.646055
3503.094204	485929.757442	45.651060
3503.084020	485930.366990	45.656065
3503.150992	485919.718178	45.661069
3503.105131	485922.511677	45.666074
3502.922461	485897.262026	45.671079
3503.051547	485889.288277	45.676084
3503.294659	485885.045233	45.681089
3502.874809	485893.368968	45.686093
3503.303539	485883.068223	45.691098
3503.153727	485877.620820	45.696103
3503.256880	485861.495135	45.701108
3503.440776	485840.696081	45.706113
3503.264235	485841.585219	45.711117
3503.425356	485835.683389	45.716122
3503.391498	485821.555013	45.721127
3503.553168	485793.312594	45.726132
3503.219288	485797.266129	45.731137
3503.138981	485782.030573	45.736141
3503.166988	485767.791061	45.741146
3503.196834	485752.031483	45.746151
3503.088881	485742.626034	45.751156
3503.137705	485745.556569	45.756161
3503.080769	485749.314363	45.761165
3503.285845	485725.522963	45.766170
3503.177306	485718.903836	45.771175
3502.860328	485699.146317	45.776180
3503.057673	485698.456595	45.781185
3502.920809	485712.612122	45.786189
3503.160284	485701.226696	45.791194
3503.212683	485702.535586	45.796199
3503.264067	485673.753173	45.801204
3503.212989	485659.779377	45.806209
3503.181429	485654.819811	45.811213
3503.338125	485647.398848	45.816218
3503.120300	485642.519379	45.821223
3503.182491	485613.177917	45.826228
3503.088796	485611.267714	45.831233
3502.857919	485617.940602	45.836237
3503.412353	485605.694790	45.841242
3503.378140	485597.797392	45.846247
3503.301458	485581.497259	45.851252
3503.230323	485563.119202	45.856257
3502.982816	485560.828030	45.861261
3503.144057	485549.049606	45.866266
3502.876064	485561.351573	45.871271
3503.249614	485542.295296	45.876276
3503.425180	485514.506204	45.881281
3503.211959	485519.099298	45.886285
3503.310307	485519.742363	45.891290
3503.293787	485504.648483	45.896295
3502.980049	485486.308699	45.901300
3503.201788	485472.696921	45.906305
3502.853496	485475.082352	45.911309
3503.003279	485464.217559	45.916314
3503.048414	485463.247930	45.921319
3502.957612	485457.588441	45.926324
3503.134436	485446.871343	45.931329
3502.841002	485438.254957	45.936333
3503.068752	485426.921882	45.941338
3503.275012	485430.435498	45.946343
3502.970024	485416.552318	45.951348
3503.272541	485419.088186	45.956353
3503.019128	485408.033792	45.961357
3503.306311	485387.623200	45.966362
3503.031513	485384.931042	45.971367
3503.108486	485380.004909	45.976372
3503.332427	485370.648137	45.981377
3503.245159	485374.816077	45.986381
3503.258970	485359.312010	45.991386
3503.215654	485351.922548	45.996391
3503.408224	485348.345953	46.001396
3503.394627	485331.984977	46.006401
3503.041483	485322.111477	46.011405
3503.120559	485294.387978	46.016410
3503.257103	485298.520558	46.021415
3502.681677	485299.016830	46.026420
3503.225139	485282.517101	46.031425
3502.973080	485294.715400	46.036429
3503.189537	485285.309109	46.041434
3503.126187	485265.257753	46.046439
3503.443815	485249.958876	46.051444
3503.279291	485240.866084	46.056449
3502.934116	485253.079127	46.061453
3503.293147	485241.471891	46.066458
3503.326671	485220.138671	46.071463
3503.114163	485207.203266	46.076468
3503.455676	485192.407171	46.081473
3503.134423	485197.473359	46.086477
3503.248159	485167.211183	46.091482
3503.178995	485173.048098	46.096487
3503.495628	485147.870519	46.101492
3503.252043	485150.391420	46.106497
3502.885075	485158.301830	46.111501
3503.206104	485127.094937	46.116506
3503.268668	485114.267972	46.121511
3503.315558	485112.538140	46.126516
3503.494219	485102.833771	46.131521
3503.362351	485089.176292	46.136525
3503.382212	485068.301008	46.141530
3503.564943	485066.347058	46.146535
3503.459585	485048.581846	46.151540
3503.356065	485029.296503	46.156545
3503.059141	485020.275194	46.161549
3503.315935	485009.849177	46.166554
3503.257804	485002.765887	46.171559
3503.185460	484993.810389	46.176564
3503.517660	484969.086064	46.181569
3503.161975	484961.796486	46.186573
3503.237923	484966.647970	46.191578
3503.346441	484945.555895	46.196583
3503.375406	484924.172406	46.201588
3503.290586	484914.509589	46.206593
3503.297766	484924.235414	46.211597
3503.222347	484894.002706	46.216602
3502.983201	484879.044845	46.221607
3502.809653	484877.299173	46.226612
3503.132648	484877.906753	46.231617
3503.035532	484872.957346	46.236621
3503.229356	484866.847405	46.241626
3503.127031	484858.403195	46.246631
3503.174506	484831.747910	46.251636
3503.176842	484817.815719	46.256641
3503.059122	484827.004061	46.261645
3503.063310	484817.225804	46.266650
3503.254038	484818.968841	46.271655
3503.192393	484796.332998	46.276660
3503.060176	484781.307499	46.281665
3503.082011	484780.848132	46.286669
3503.121070	484775.167916	46.291674
3502.785627	484772.637241	46.296679
3502.836155	484774.250459	46.301684
3502.925114	484778.998610	46.306689
3502.733812	484775.685231	46.311693
3502.886596	484772.925402	46.316698
3503.338835	484746.611312	46.321703
3502.951960	484727.117147	46.326708
3503.257332	484731.020518	46.331713
3503.219610	484724.643161	46.336717
3503.197187	484720.391171	46.341722
3503.089136	484708.604136	46.346727
3502.832501	484696.739255	46.351732
3503.063280	484676.387486	46.356737
3502.889342	484682.190449	46.361741
3503.101240	484672.733919	46.366746
3503.148473	484681.237656	46.371751
3503.156797	484679.108587	46.376756
3502.970681	484665.408720	46.381761
3503.237053	484644.899306	46.386765
3503.340387	484632.926827	46.391770
3503.177448	484627.126510	46.396775
3503.080609	484631.245462	46.401780
3502.901537	484623.319897	46.406785
3503.092059	484609.560458	46.411789
3503.025444	484601.414462	46.416794
3503.398418	484593.350966	46.421799
3503.168746	484596.933640	46.426804
3502.998461	484587.081519	46.431809
3503.011939	484595.489305	46.436813
3502.842983	484571.603612	46.441818
3502.766547	484564.421730	46.446823
3502.891643	484553.003043	46.451828
3503.078083	484547.958071	46.456833
3502.917746	484547.071536	46.461837
3503.171514	484541.863934	46.466842
3503.357433	484542.037233	46.471847
3503.345647	484540.012651	46.476852
3503.165353	484512.430347	46.481857
3502.826891	484503.719333	46.486861
3503.200748	484498.746048	46.491866
3503.302519	484501.161784	46.496871
3503.138914	484491.308558	46.501876
3503.444219	484470.640819	46.506881
3503.144196	484452.399202	46.511885
3503.392788	484443.646032	46.516890
3503.565742	484449.546221	46.521895
3502.972599	484422.485004	46.526900
3502.867628	484425.642701	46.531905
3502.935666	484418.437928	46.536909
3503.457001	484419.014173	46.541914
3503.405789	484406.508695	46.546919
3502.912662	484399.341952	46.551924
3503.108974	484369.217457	46.556929
3503.327866	484364.977907	46.561933
3502.934605	484355.160912	46.566938
3503.281578	484363.718736	46.571943
3503.159245	484355.226805	46.576948
3503.270833	484338.338572	46.581953
3503.206911	484325.480412	46.586957
3503.222308	484312.001755	46.591962
3503.353695	484310.663796	46.596967
3503.226850	484303.945748	46.601972
3503.300780	484280.223954	46.606977
3502.654077	484272.321497	46.611981
3502.809663	484272.904895	46.616986
3502.962763	484270.296933	46.621991
3502.969769	484267.002783	46.626996
3503.030779	484255.898027	46.632001
3503.064482	484265.923970	46.637005
3503.006058	484247.897286	46.642010
3503.248935	484242.741988	46.647015
3503.025689	484230.263588	46.652020
3503.537931	484217.415612	46.657025
3503.359454	484217.443860	46.662029
3503.127993	484200.964370	46.667034
3503.175764	484181.451613	46.672039
3503.197799	484181.954798	46.677044
3503.470442	484174.717594	46.682049
3503.198622	484166.249208	46.687053
3503.340058	484149.052113	46.692058
3503.499794	484139.552903	46.697063
3503.261209	484135.132298	46.702068
3503.600065	484121.197076	46.707073
3503.365033	484100.006390	46.712077
3503.301510	484089.073212	46.717082
3503.246169	484080.925213	46.722087
3503.201599	484076.068622	46.727092
3503.289309	484051.077786	46.732097
3503.043773	484052.129901	46.737101
3503.417633	484042.090165	46.742106
3503.171383	484035.998858	46.747111
3503.262992	484024.078518	46.752116
3503.477226	483995.267855	46.757121
3503.076395	483989.960919	46.762125
3503.268343	483990.487915	46.767130
3503.462201	483981.793851	46.772135
3502.927195	483963.436923	46.777140
3503.173330	483955.241219	46.782145
3503.274689	483950.057549	46.787149
3503.544493	483940.794163	46.792154
3503.267127	483912.263734	46.797159
3503.006663	483906.833261	46.802164
3502.919906	483897.575549	46.807169
3503.526134	483903.002112	46.812173
3503.494144	483894.901008	46.817178
3503.272990	483876.089078	46.822183
3503.081207	483870.343756	46.827188
3503.215701	483866.826732	46.832193
3503.064112	483871.663792	46.837197
3503.313252	483844.367302	46.842202
3503.202676	483838.305151	46.847207
3502.968574	483825.828204	46.852212
3503.139237	483811.159385	46.857217
3503.133779	483812.832197	46.862221
3502.992299	483811.841318	46.867226
3503.030312	483798.257399	46.872231
3503.037997	483778.750571	46.877236
3503.504839	483768.898654	46.882241
3502.962160	483781.143844	46.887245
3503.145787	483763.281105	46.892250
3503.215337	483767.069956	46.897255
3502.835902	483740.733962	46.902260
3503.273063	483730.937382	46.907265
3503.173648	483719.351033	46.912269
3503.088928	483712.068814	46.917274
3502.978557	483721.509841	46.922279
3502.885609	483727.958924	46.927284
3503.031381	483719.373671	46.932289
3503.169310	483701.163448	46.937293
3503.366318	483678.840060	46.942298
3503.050400	483677.724753	46.947303
3502.934755	483682.505515	46.952308
3503.104458	483678.780235	46.957313
3503.166851	483672.538699	46.962317
3502.919699	483644.408413	46.967322
3503.047880	483640.335038	46.972327
3503.057829	483632.581846	46.977332
3503.129327	483622.032377	46.982337
3503.034776	483628.380416	46.987341
3503.222067	483623.943043	46.992346
3503.047813	483606.187390	46.997351
3502.992326	483593.834055	47.002356
3503.006394	483594.389180	47.007361
3502.777150	483585.305833	47.012365
3502.744989	483582.524404	47.017370
3502.944289	483576.970501	47.022375
3502.669081	483590.085496	47.027380
3503.433771	483583.783590	47.032385
3503.227103	483582.245692	47.037389
3503.125004	483563.971950	47.042394
3503.429176	483538.692915	47.047399
3502.910410	483536.849692	47.052404
3502.921131	483522.864577	47.057409
3503.158672	483527.690881	47.062413
3503.133179	483519.233940	47.067418
3503.405061	483500.495708	47.072423
3502.938345	483490.639216	47.077428
3503.123411	483490.204683	47.082433
3503.022073	483480.898412	47.087437
3503.035370	483485.152193	47.092442
3503.407830	483470.907204	47.097447
3502.961405	483463.834058	47.102452
3503.183182	483442.570446	47.107457
3502.894452	483445.808011	47.112461
3503.157405	483440.598663	47.117466
3503.195077	483435.120932	47.122471
3502.987451	483441.993555	47.127476
3503.644287	483402.371082	47.132481
3503.165202	483403.662806	47.137485
3503.084831	483387.260069	47.142490
3503.611846	483384.288896	47.147495
3503.218702	483374.927367	47.152500
3503.260799	483350.094831	47.157505
3503.109740	483339.580386	47.162509
3503.066156	483333.862144	47.167514
3503.168553	483346.714958	47.172519
3502.762665	483317.443988	47.177524
3503.359352	483303.163433	47.182529
3503.153522	483297.825483	47.187533
3503.111740	483295.704182	47.192538
3503.264338	483293.856148	47.197543
3503.381862	483290.747024	47.202548
3503.252777	483266.549423	47.207553
3502.892885	483261.843798	47.212557
3503.290779	483251.445199	47.217562
3503.204357	483241.680465	47.222567
3502.881615	483232.561066	47.227572
3503.164086	483212.959570	47.232577
3502.982654	483214.305589	47.237581
3502.775623	483206.991848	47.242586
3502.880641	483199.426118	47.247591
3503.003188	483201.990729	47.252596
3503.114136	483193.664076	47.257601
3503.125644	483199.995492	47.262605
3503.217641	483183.058682	47.267610
3503.219596	483165.274772	47.272615
3502.799791	483164.682512	47.277620
3503.149203	483147.400989	47.282625
3502.988202	483164.602141	47.287629
3503.107055	483149.991677	47.292634
3503.299050	483152.342655	47.297639
3503.203042	483141.920733	47.302644
3503.452391	483125.060332	47.307649
3503.452880	483125.313621	47.312653
3503.528791	483110.608584	47.317658
3503.380302	483080.384586	47.322663
3502.988174	483077.710646	47.327668
3503.279960	483065.504747	47.332673
3503.121539	483071.204407	47.337677
3502.954955	483051.319066	47.342682
3503.106342	483038.020690	47.347687
3503.029968	483037.070145	47.352692
3503.024810	483018.679235	47.357697
3502.964434	483021.323449	47.362701
3502.828080	483024.587666	47.367706
3503.172827	483013.741345	47.372711
3502.853426	483025.495723	47.377716
3503.022529	482996.741376	47.382721
3502.894761	482976.241828	47.387725
3502.833153	482974.427622	47.392730
3503.106934	482961.667176	47.397735
3502.916949	482964.585216	47.402740
3503.110361	482970.482625	47.407745
3502.980357	482969.185891	47.412749
3503.023460	482961.173859	47.417754
3503.254171	482963.062745	47.422759
3503.250011	482949.484898	47.427764
3502.998454	482940.050112	47.432769
3503.030901	482931.735755	47.437773
3502.854971	482924.112993	47.442778
3503.157171	482921.430617	47.447783
3502.870347	482924.313303	47.452788
3503.249910	482901.200172	47.457793
3503.263083	482892.990177	47.462797
3503.060702	482877.366290	47.467802
3503.455674	482865.701286	47.472807
3502.939624	482873.028192	47.477812
3503.249485	482856.208659	47.482817
3503.077258	482833.486664	47.487821
3503.122212	482828.362276	47.492826
3503.031958	482828.832579	47.497831
3503.268550	482828.136555	47.502836
3503.416509	482821.931888	47.507841
3503.068085	482804.912362	47.512845
3502.848076	482776.776526	47.517850
3503.275274	482777.013040	47.522855
3502.855702	482777.332729	47.527860
3503.112610	482768.628157	47.532865
3503.074052	482786.924957	47.537869
3503.052205	482772.944449	47.542874
3503.137524	482752.208317	47.547879
3502.895703	482745.102566	47.552884
3503.064261	482731.091932	47.557889
3502.660829	482746.811770	47.562893
3502.669809	482739.261041	47.567898
3503.013328	482738.497446	47.572903
3502.907706	482742.010186	47.577908
3502.955713	482741.749301	47.582913
3503.096639	482735.444384	47.587917
3502.952413	482724.067190	47.592922
3503.002042	482699.840634	47.597927
3502.817832	482707.925819	47.602932
3502.902351	482685.872405	47.607937
3502.801365	482697.541790	47.612941
3502.944630	482690.223151	47.617946
3503.172636	482691.149821	47.622951
3503.185331	482675.441108	47.627956
3503.178740	482672.503505	47.632961
3503.074715	482640.701119	47.637965
3503.020105	482639.037777	47.642970
3503.015953	482637.467793	47.647975
3502.787390	482635.578610	47.652980
3503.238024	482630.035378	47.657985
3503.201745	482638.553214	47.662989
3502.947061	482613.614645	47.667994
3503.243108	482598.114418	47.672999
3503.224075	482594.418763	47.678004
3503.167763	482590.272995	47.683009
3503.155887	482597.874982	47.688013
3502.966850	482584.174100	47.693018
3502.924219	482578.911489	47.698023
3502.991249	482558.684714	47.703028
3503.321963	482551.387061	47.708033
3503.283622	482547.846451	47.713037
3503.240816	482552.970648	47.718042
3503.610645	482526.261236	47.723047
3503.371167	482513.074950	47.728052
3502.997995	482512.677966	47.733057
3503.213517	482502.155791	47.738061
3502.929338	482497.235343	47.743066
3503.413092	482471.875868	47.748071
3502.837643	482467.356123	47.753076
3503.075669	482447.406209	47.758081
3502.903531	482460.607008	47.763085
3502.854683	482459.702752	47.768090
3503.039968	482455.772105	47.773095
3503.017081	482447.162282	47.778100
3503.277309	482444.182471	47.783105
3503.169181	482425.553937	47.788109
3503.119500	482422.116431	47.793114
3503.227561	482409.939162	47.798119
3503.170655	482418.713692	47.803124
3503.292996	482407.040839	47.808129
3503.291677	482390.422094	47.813133
3503.075582	482378.498713	47.818138
3503.328124	482378.306830	47.823143
3503.202963	482378.529322	47.828148
3503.339657	482359.659357	47.833153
3502.956840	482347.306299	47.838157
3502.915769	482333.987195	47.843162
3503.155224	482323.258470	47.848167
3503.044037	482330.774923	47.853172
3503.170719	482321.381386	47.858177
3503.027537	482320.441366	47.863181
3502.558357	482305.467203	47.868186
3503.202868	482280.082070	47.873191
3502.994610	482284.117794	47.878196
3503.286629	482271.556686	47.883201
3503.081026	482277.264036	47.888205
3502.985449	482271.249691	47.893210
3503.158538	482271.881053	47.898215
3502.912903	482252.210060	47.903220
3502.824629	482240.823739	47.908225
3503.027573	482231.012760	47.913229
3502.957465	482227.527780	47.918234
3503.027975	482220.372469	47.923239
3502.594970	482229.662545	47.928244
3502.674487	482217.084322	47.933249
3502.972886	482224.586743	47.938253
3502.847620	482231.294770	47.943258
3503.116834	482226.084109	47.948263
3502.861606	482235.498086	47.953268
3502.976925	482211.057866	47.958273
3502.929125	482194.648974	47.963277
3503.062218	482188.193114	47.968282
3503.116220	482189.603325	47.973287
3502.877267	482189.539796	47.978292
3503.124789	482179.873749	47.983297
3502.911538	482183.251597	47.988301
3502.650303	482185.319655	47.993306
3502.859238	482182.246575	47.998311
3502.493991	482194.515381	48.003316
3502.875143	482187.969644	48.008321
3503.151497	482173.840235	48.013325
3502.906248	482151.686335	48.018330
3502.862300	482142.725028	48.023335
3502.757117	482140.512285	48.028340
3502.900075	482141.249752	48.033345
3502.884663	482141.556235	48.038349
3502.983579	482141.337965	48.043354
3503.267093	482132.172889	48.048359
3502.837000	482133.254275	48.053364
3502.908731	482124.882696	48.058369
3502.932297	482131.921911	48.063373
3502.828664	482112.177662	48.068378
3503.123776	482095.562480	48.073383
3503.191806	482098.490534	48.078388
3503.086440	482094.656424	48.083393
3503.055945	482096.941362	48.088397
3502.803311	482100.528123	48.093402
3502.907664	482087.641880	48.098407
3502.923180	482094.226365	48.103412
3503.272029	482070.205072	48.108417
3503.152230	482048.385905	48.113421
3502.841586	482055.731316	48.118426
3503.205634	482051.062973	48.123431
3502.996779	482050.944018	48.128436
3503.005673	482046.686490	48.133441
3503.291219	482045.830696	48.138445
3503.213362	482019.292690	48.143450
3503.153575	481997.007962	48.148455
3503.091324	482005.023492	48.153460
3503.068402	481998.997579	48.158465
3503.256658	481998.157162	48.163469
3503.243079	481983.668093	48.168474
3503.340486	481968.654783	48.173479
3502.950065	481963.396310	48.178484
3503.177779	481953.378601	48.183489
3503.175222	481960.776688	48.188493
3503.058455	481928.671140	48.193498
3503.402795	481924.765915	48.198503
3503.250965	481919.216373	48.203508
3503.294608	481924.935098	48.208513
3503.346107	481902.936686	48.213517
3503.340615	481883.784721	48.218522
3503.460298	481875.506794	48.223527
3503.076747	481864.268263	48.228532
3502.875420	481869.823048	48.233537
3503.157379	481841.505179	48.238541
3502.930448	481826.391018	48.243546
3503.252797	481814.686198	48.248551
3503.145665	481825.546369	48.253556
3503.004792	481819.843060	48.258561
3502.781640	481819.878369	48.263565
3502.855839	481816.623853	48.268570
3503.184517	481806.083418	48.273575
3503.085914	481783.145882	48.278580
3503.027611	481783.915174	48.283585
3503.185972	481780.292663	48.288589
3503.152282	481768.441415	48.293594
3503.189789	481760.683121	48.298599
3502.989669	481760.613451	48.303604
3502.855429	481732.209202	48.308609
3503.074926	481740.332315	48.313613
3502.921334	481724.801128	48.318618
3503.207632	481723.438508	48.323623
3502.633347	481728.545590	48.328628
3502.916492	481721.204478	48.333633
3503.006891	481718.707426	48.338637
3502.761753	481725.485243	48.343642
3503.103307	481716.310798	48.348647
3502.924167	481713.552333	48.353652
3502.704731	481683.286709	48.358657
3503.134079	481684.688298	48.363661
3502.688645	481676.752958	48.368666
3503.101795	481674.863589	48.373671
3502.848626	481679.261223	48.378676
3503.203010	481667.095226	48.383681
3503.168875	481667.303337	48.388685
3502.654749	481676.150471	48.393690
3503.142116	481662.392695	48.398695
3503.010979	481657.751860	48.403700
3503.123484	481643.901314	48.408705
3503.370740	481633.373656	48.413709
3502.961326	481632.222336	48.418714
3503.101246	481631.237534	48.423719
3502.925473	481636.028301	48.428724
3502.970378	481610.737076	48.433729
3503.348348	481594.463059	48.438733
3502.912798	481590.529031	48.443738
3503.439407	481588.165692	48.448743
3503.193951	481596.058339	48.453748
3502.906799	481572.238302	48.458753
3503.177092	481554.005149	48.463757
3502.975908	481547.956604	48.468762
3503.042759	481543.183107	48.473767
3502.494487	481539.874924	48.478772
3502.830005	481537.947143	48.483777
3503.042493	481538.977662	48.488781
3502.888189	481537.177973	48.493786
3502.897740	481545.841051	48.498791
3503.060185	481551.845126	48.503796
3502.830942	481525.685066	48.508801
3502.977856	481507.775391	48.513805
3502.872675	481503.029076	48.518810
3503.183914	481494.872720	48.523815
3502.991649	481508.837393	48.528820
3502.726987	481495.857079	48.533825
3503.016497	481485.829363	48.538829
3503.079510	481497.625553	48.543834
3503.375379	481493.778575	48.548839
3503.229359	481471.202857	48.553844
3503.290808	481454.370714	48.558849
3503.082857	481451.616765	48.563853
3502.897154	481449.315330	48.568858
3503.021947	481440.884401	48.573863
3502.915799	481454.683490	48.578868
3503.351934	481428.722149	48.583873
3503.137934	481409.197316	48.588877
3502.979371	481406.891586	48.593882
3502.948818	481397.877150	48.598887
3503.031524	481407.035429	48.603892
3502.942695	481402.185164	48.608897
3502.940369	481393.419616	48.613901
3503.061281	481372.524381	48.618906
3503.097382	481348.551637	48.623911
3502.872032	481361.406896	48.628916
3503.147776	481355.789610	48.633921
3503.213493	481348.938760	48.638925
3503.027764	481356.163347	48.643930
3503.133809	481338.817352	48.648935
3503.121167	481321.642112	48.653940
3502.918083	481312.148203	48.658945
3503.252034	481306.268350	48.663949
3503.266622	481304.137921	48.668954
3503.385264	481302.497750	48.673959
3502.948533	481292.128693	48.678964
3502.955737	481271.454005	48.683969
3502.981891	481259.390307	48.688973
3502.805613	481270.008363	48.693978
3502.981913	481264.508110	48.698983
3502.910682	481267.154278	48.703988
3503.157670	481255.765060	48.708993
3503.263199	481255.647076	48.713997
3503.154262	481228.758214	48.719002
3503.489541	481213.909409	48.724007
3503.255234	481210.602214	48.729012
3503.085056	481216.405614	48.734017
3503.035874	481196.398479	48.739021
3502.538515	481188.065780	48.744026
3503.048762	481175.064109	48.749031
3502.801867	481166.793154	48.754036
3502.771212	481160.464180	48.759041
3502.983196	481164.788405	48.764045
3502.863242	481169.773146	48.769050
3502.843548	481159.490113	48.774055
3502.613179	481161.604069	48.779060
3502.937440	481159.019309	48.784065
3503.146873	481158.986244	48.789069
3503.073840	481158.035079	48.794074
3502.905547	481147.066134	48.799079
3503.004423	481133.622750	48.804084
3502.509625	481119.513129	48.809089
3502.978056	481118.628389	48.814093
3502.750132	481113.242658	48.819098
3502.895586	481104.504293	48.824103
3502.940296	481112.401940	48.829108
3503.041777	481119.682559	48.834113
3502.877370	481114.844169	48.839117
3503.002586	481120.955603	48.844122
3502.967936	481118.782266	48.849127
3502.803423	481121.696553	48.854132
3503.077442	481100.979512	48.859137
3503.185256	481084.747774	48.864141
3502.862954	481073.701790	48.869146
3503.314125	481062.280186	48.874151
3502.957977	481059.498935	48.879156
3503.012391	481067.243053	48.884161
3503.134393	481061.143273	48.889165
3502.793862	481037.229679	48.894170
3503.012608	481024.983381	48.899175
3503.170695	481028.100046	48.904180
3503.085712	481017.421888	48.909185
3503.122680	481015.541247	48.914189
3502.941860	481025.450755	48.919194
3503.260735	481012.681911	48.924199
3502.999308	481006.186678	48.929204
3502.831702	480993.545388	48.934209
3503.349350	480978.819593	48.939213
3503.234288	480985.881133	48.944218
3503.472178	480969.932768	48.949223
3503.442177	480960.715358	48.954228
3503.027923	480937.167994	48.959233
3503.149879	480925.443648	48.964237
3502.634462	480941.942705	48.969242
3503.199489	480931.972501	48.974247
3503.242092	480922.186211	48.979252
3502.900298	480912.207317	48.984257
3502.737776	480890.596297	48.989261
3502.550013	480895.845184	48.994266
3503.048580	480888.520383	48.999271
3502.914087	480904.148517	49.004276
3502.692499	480892.326438	49.009281
3502.928450	480896.393576	49.014285
3502.629693	480891.424352	49.019290
3502.891623	480887.126577	49.024295
3502.828623	480893.115817	49.029300
3503.076838	480892.519234	49.034305
3502.766103	480889.882795	49.039309
3502.706976	480897.594255	49.044314
3503.061075	480885.225133	49.049319
3502.994537	480887.718595	49.054324
3502.828989	480870.060413	49.059329
3503.125275	480846.603317	49.064333
3502.893639	480846.842654	49.069338
3502.692825	480838.969650	49.074343
3503.178422	480843.706743	49.079348
3502.788817	480844.173737	49.084353
3503.102871	480843.769432	49.089357
3502.941535	480843.136240	49.094362
3503.057537	480841.699134	49.099367
3502.915181	480832.550095	49.104372
3502.771468	480809.010486	49.109377
3502.686836	480798.433497	49.114381
3502.530925	480801.599830	49.119386
3502.877797	480802.710492	49.124391
3502.833378	480798.258432	49.129396
3502.941665	480794.592983	49.134401
3503.177286	480795.366527	49.139405
3502.825181	480791.520490	49.144410
3503.028816	480793.312526	49.149415
3502.776400	480797.203519	49.154420
3502.945472	480785.572985	49.159425
3503.063424	480789.405438	49.164429
3502.479427	480787.724271	49.169434
3503.032157	480782.468414	49.174439
3502.746633	480771.365774	49.179444
3502.693208	480751.460200	49.184449
3502.920079	480749.042797	49.189453
3502.723873	480743.043887	49.194458
3502.971269	480743.055492	49.199463
3502.774893	480741.110364	49.204468
3502.608707	480747.825366	49.209473
3502.843149	480739.630164	49.214477
3502.772467	480743.340426	49.219482
3503.057110	480741.319266	49.224487
3503.442696	480745.768160	49.229492
3503.190352	480741.957016	49.234497
3503.080123	480722.719127	49.239501
3502.816111	480711.917085	49.244506
3503.044944	480699.567646	49.249511
3502.916653	480708.962290	49.254516
3503.025922	480709.502449	49.259521
3503.089552	480701.384902	49.264525
3502.806408	480701.227006	49.269530
3503.041218	480691.207532	49.274535
3503.114508	480676.045027	49.279540
3502.782156	480659.983857	49.284545
3502.947949	480655.853243	49.289549
3502.578916	480643.496925	49.294554
3503.038696	480641.802778	49.299559
3502.877258	480642.588417	49.304564
3502.929318	480649.471644	49.309569
3503.138404	480643.003264	49.314573
3502.571022	480645.879955	49.319578
3502.654707	480642.167695	49.324583
3502.634789	480639.181220	49.329588
3502.607763	480647.597116	49.334593
3502.811435	480644.271268	49.339597
3502.743162	480644.332769	49.344602
3502.792186	480646.960012	49.349607
3502.786496	480646.454228	49.354612
3502.794514	480651.114839	49.359617
3503.174704	480634.636988	49.364621
3503.164816	480621.514478	49.369626
3503.011438	480611.353632	49.374631
3502.758392	480609.873499	49.379636
3502.823309	480600.438227	49.384641
3502.763142	480593.911045	49.389645
3502.587277	480591.253247	49.394650
3502.787467	480596.998288	49.399655
3502.739768	480601.313012	49.404660
3502.536680	480596.885987	49.409665
3503.232813	480591.962120	49.414669
3503.167627	480595.570197	49.419674
3503.110916	480590.765327	49.424679
3502.914587	480572.300984	49.429684
3502.912213	480561.710865	49.434689
3502.985483	480549.740628	49.439693
3502.684653	480547.913336	49.444698
3502.773144	480548.304766	49.449703
3503.309221	480544.875687	49.454708
3503.120407	480547.287175	49.459713
3503.399421	480546.837731	49.464717
3503.160302	480527.417333	49.469722
3503.144403	480512.015437	49.474727
3503.328141	480499.673001	49.479732
3502.938754	480500.444003	49.484737
3503.140799	480505.276671	49.489741
3502.916899	480502.018382	49.494746
3503.068387	480468.955933	49.499751
3503.312093	480466.333144	49.504756
3502.934635	480462.947103	49.509761
3503.071786	480456.033978	49.514765
3503.190488	480461.893284	49.519770
3503.201528	480448.057932	49.524775
3503.280819	480426.965579	49.529780
3503.007868	480420.218609	49.534785
3503.258269	480401.126093	49.539789
3503.237259	480405.487315	49.544794
3503.493625	480405.193467	49.549799
3503.146614	480382.242881	49.554804
3502.951879	480375.280841	49.559809
3503.334255	480362.450865	49.564813
3503.086141	480373.739508	49.569818
3503.187588	480361.460665	49.574823
3503.378549	480340.705279	49.579828
3503.166433	480326.550404	49.584833
3503.247328	480323.902658	49.589837
3503.007303	480330.528127	49.594842
3503.149741	480313.074128	49.599847
3503.491123	480289.609240	49.604852
3503.229176	480285.799525	49.609857
3502.963159	480276.771118	49.614861
3503.185582	480279.827061	49.619866
3502.995253	480257.966374	49.624871
3503.075540	480242.954449	49.629876
3503.277147	480233.902782	49.634881
3503.198129	480221.145644	49.639885
3503.325311	480230.601482	49.644890
3503.221992	480217.341450	49.649895
3503.081485	480195.270125	49.654900
3503.135052	480197.339303	49.659905
3503.247622	480185.920040	49.664909
3503.302129	480181.502877	49.669914
3503.289130	480174.360020	49.674919
3503.127540	480157.663366	49.679924
3502.940538	480151.004064	49.684929
3503.236386	480151.616095	49.689933
3502.834762	480146.257552	49.694938
3503.086734	480145.660354	49.699943
3503.224885	480141.027267	49.704948
3502.873945	480124.664556	49.709953
3503.280623	480109.803633	49.714957
3503.258195	480093.540990	49.719962
3503.198474	480093.297100	49.724967
3503.155100	480096.749799	49.729972
3502.917363	480084.727091	49.734977
3502.883358	480051.845282	49.739981
3502.491208	480062.498111	49.744986
3502.814337	480052.768394	49.749991
3502.814329	480048.714535	49.754996
3502.622364	480046.413923	49.760001
3503.032603	480046.399791	49.765005
3503.076533	480047.254338	49.770010
3503.114627	480037.975058	49.775015
3502.774004	480045.832694	49.780020
3502.907991	480048.142546	49.785025
3503.225462	480034.967900	49.790029
3502.934411	480024.017731	49.795034
3502.863202	480001.327149	49.800039
3503.098758	479997.134697	49.805044
3502.574515	480004.869352	49.810049
3502.903746	479989.057777	49.815053
3503.104256	479992.421271	49.820058
3503.220709	479989.666512	49.825063
3502.824219	479996.772890	49.830068
3502.923846	480003.699499	49.835073
3503.082716	479989.181698	49.840077
3503.030628	479988.125818	49.845082
3502.924901	479960.170559	49.850087
3503.293207	479953.474090	49.855092
3502.847754	479952.531058	49.860097
3503.464248	479950.609387	49.865101
3503.181647	479960.383498	49.870106
3503.082547	479935.670290	49.875111
3503.175607	479925.976877	49.880116
3503.008475	479925.901984	49.885121
3503.104481	479909.215076	49.890125
3503.017712	479917.691401	49.895130
3503.226891	479900.327835	49.900135
3503.252220	479876.861739	49.905140
3503.130852	479875.766128	49.910145
3502.869609	479870.892063	49.915149
3502.792935	479871.664333	49.920154
3503.058303	479868.480626	49.925159
3502.953836	479869.612008	49.930164
3502.670097	479864.032058	49.935169
3503.366452	479851.810887	49.940173
3503.036984	479842.133545	49.945178
3503.013969	479828.657861	49.950183
3503.127780	479811.562662	49.955188
3502.842007	479819.817113	49.960193
3503.078667	479813.952195	49.965197
3502.665793	479821.213248	49.970202
3502.779267	479807.158558	49.975207
3502.800061	479812.070721	49.980212
3502.938946	479808.856322	49.985217
3502.996660	479804.641265	49.990221
3502.892877	479787.023021	49.995226
3502.988498	479771.552244	50.000231
3502.976849	479766.790724	50.005236
3502.692939	479765.264729	50.010241
3502.686599	479762.580022	50.015245
3502.642495	479762.080287	50.020250
3502.920392	479756.360857	50.025255
3503.133911	479760.887849	50.030260
3502.956124	479760.510592	50.035265
3502.815500	479758.860600	50.040269
3503.027712	479767.897825	50.045274
3502.934946	479757.625608	50.050279
3502.938501	479729.196678	50.055284
3502.690064	479729.590706	50.060289
3502.756414	479723.043237	50.065293
3502.799681	479718.577073	50.070298
3502.914767	479714.099556	50.075303
3503.147510	479717.964749	50.080308
3502.711340	479721.935672	50.085313
3503.133363	479711.024641	50.090317
3502.604162	479715.517016	50.095322
3502.785246	479719.846446	50.100327
3503.099990	479711.435426	50.105332
3502.968348	479713.888653	50.110337
3502.957968	479691.390798	50.115341
3502.846798	479679.905257	50.120346
3503.305117	479666.505405	50.125351
3503.077053	479670.190071	50.130356
3503.039875	479675.010082	50.135361
3502.929886	479668.693167	50.140365
3502.703227	479671.516140	50.145370
3502.599753	479664.184700	50.150375
3502.794211	479672.920726	50.155380
3502.586314	479668.190202	50.160385
3503.120574	479658.021522	50.165389
3502.844129	479655.936917	50.170394
3502.825099	479631.362696	50.175399
3503.195502	479614.530818	50.180404
3502.766609	479623.922818	50.185409
3503.379731	479618.251712	50.190413
3502.672336	479623.887120	50.195418
3503.320415	479619.021286	50.200423
3503.218038	479617.618610	50.205428
3502.995237	479600.677784	50.210433
3503.210513	479582.299477	50.215437
3503.037050	479583.593806	50.220442
3503.118586	479573.648667	50.225447
3503.271065	479572.611105	50.230452
3503.067805	479574.771619	50.235457
3503.173747	479540.498612	50.240461
3502.880358	479530.562039	50.245466
3502.727794	479526.126785	50.250471
3503.013285	479527.247224	50.255476
3502.529279	479532.847347	50.260481
3503.230742	479521.740018	50.265485
3502.767797	479527.691540	50.270490
3502.772669	479520.038870	50.275495
3503.292325	479516.814913	50.280500
3502.662082	479516.255793	50.285505
3503.103682	479502.250371	50.290509
3502.899602	479487.941597	50.295514
3502.712146	479486.400334	50.300519
3502.871175	479480.496913	50.305524
3502.609226	479481.754560	50.310529
3502.981123	479474.043859	50.315533
3503.013320	479485.086001	50.320538
3502.956862	479478.000436	50.325543
3503.443366	479473.768208	50.330548
3503.319362	479469.075051	50.335553
3503.216067	479448.821315	50.340557
3502.905808	479439.140738	50.345562
3503.128957	479432.872441	50.350567
3503.020651	479430.963936	50.355572
3503.205192	479435.748960	50.360577
3503.247228	479425.556613	50.365581
3502.786558	479408.450519	50.370586
3502.999515	479406.237855	50.375591
3503.051910	479391.736445	50.380596
3503.017038	479395.593327	50.385601
3502.785235	479397.352968	50.390605
3503.075234	479399.232833	50.395610
3503.105625	479393.400395	50.400615
3503.252728	479370.775931	50.405620
3502.979551	479356.782036	50.410625
3503.049519	479339.693360	50.415629
3503.007416	479342.487208	50.420634
3502.984389	479342.946965	50.425639
3502.859786	479336.632253	50.430644
3503.221637	479338.450092	50.435649
3502.921753	479326.335392	50.440653
3502.805760	479311.404459	50.445658
3502.927333	479298.361640	50.450663
3503.002831	479298.197717	50.455668
3502.789379	479304.413924	50.460673
3503.108904	479291.289135	50.465677
3503.066527	479302.089788	50.470682
3502.909802	479300.797031	50.475687
3503.368865	479295.758293	50.480692
3502.950770	479276.770355	50.485697
3502.918442	479255.897096	50.490701
3502.916509	479256.657576	50.495706
3502.956436	479250.924940	50.500711
3503.010708	479248.129231	50.505716
3503.043910	479255.117279	50.510721
3503.128136	479244.259385	50.515725
3502.997675	479233.536771	50.520730
3503.105908	479216.036533	50.525735
3503.097561	479179.703255	50.530740
3503.113072	479154.666898	50.535745
3502.756249	479089.655207	50.540749
3502.572082	479033.788430	50.545754
3502.459502	478976.998004	50.550759
3502.762407	478891.002658	50.555764
3502.490042	478813.155498	50.560769
3502.275820	478714.267832	50.565773
3502.260648	478618.692919	50.570778
3502.032143	478506.022215	50.575783
3501.959248	478377.717451	50.580788
3501.419090	478248.269436	50.585793
3501.457110	478104.995261	50.590797
3501.304143	477965.804569	50.595802
3500.991854	477814.981816	50.600807
3500.970061	477644.042779	50.605812
3500.538133	477485.989221	50.610817
3500.324675	477298.657100	50.615821
3500.077866	477110.618955	50.620826
3499.831433	476916.953310	50.625831
3499.859769	476711.179988	50.630836
3499.290951	476503.725044	50.635841
3499.312864	476294.400663	50.640845
3498.522386	476076.788992	50.645850
3498.273066	475844.492311	50.650855
3498.072084	475609.803111	50.655860
3497.409479	475381.266417	50.660865
3497.271932	475133.332694	50.665869
3496.741776	474873.647945	50.670874
3496.130495	474626.188374	50.675879
3495.673627	474357.310972	50.680884
3495.117335	474111.306374	50.685889
3495.230523	473840.862042	50.690893
3494.564435	473577.785981	50.695898
3494.411755	473292.067957	50.700903
3493.887385	473011.625909	50.705908
3493.129958	472723.765088	50.710913
3492.663147	472445.942169	50.715917
3492.134208	472147.138132	50.720922
3491.723879	471849.527656	50.725927
3491.838793	471551.170805	50.730932
3491.095012	471246.456288	50.735937
3490.745877	470929.507683	50.740941
3489.857705	470613.349179	50.745946
3489.306705	470303.723307	50.750951
3489.164633	469973.495073	50.755956
3488.373091	469646.304833	50.760961
3488.084481	469322.426878	50.765965
3487.786891	468986.224860	50.770970
3486.726091	468648.312781	50.775975
3486.485058	468312.445880	50.780980
3485.486860	467968.884876	50.785985
3485.135934	467626.230014	50.790989
3484.824421	467285.845080	50.795994
3484.128085	466943.487212	50.800999
3483.951752	466587.401344	50.806004
3482.972868	466234.225276	50.811009
3482.468475	465871.130773	50.816013
3481.819118	465514.543816	50.821018
3481.187700	465161.142803	50.826023
3480.610650	464792.412453	50.831028
3480.231002	464434.496966	50.836033
3479.547185	464063.742404	50.841037
3478.807067	463706.835265	50.846042
3478.280605	463332.949616	50.851047
3478.024312	462968.397182	50.856052
3477.206991	462589.980167	50.861057
3476.248489	462209.195100	50.866061
3475.853433	461839.878070	50.871066
3474.955722	461465.663705	50.876071
3474.384719	461087.840822	50.881076
3473.852100	460717.004820	50.886081
3473.113404	460329.558272	50.891085
3472.558098	459956.430434	50.896090
3471.781602	459579.476195	50.901095
3471.177417	459201.372293	50.906100
3470.164817	458831.188895	50.911105
3469.687992	458447.319917	50.916109
3469.238519	458075.766650	50.921114
3468.495247	457691.520839	50.926119
3467.936322	457313.174508	50.931124
3467.197248	456935.864805	50.936129
3466.472112	456548.197440	50.941133
3465.646122	456160.945130	50.946138
3465.123177	455793.880440	50.951143
3464.811057	455403.337639	50.956148
3463.587594	455017.599653	50.961153
3462.963210	454635.413266	50.966157
3462.386166	454262.446843	50.971162
3461.313385	453888.740841	50.976167
3460.616390	453496.450055	50.981172
3459.781921	453131.928132	50.986177
3459.509403	452744.022222	50.991181
3458.930004	452377.824241	50.996186
3457.772132	451998.417720	51.001191
3457.466668	451624.401002	51.006196
3456.933498	451246.354775	51.011201
3456.260898	450868.375115	51.016205
3455.796820	450486.195259	51.021210
3454.889056	450101.592707	51.026215
3454.378538	449717.073197	51.031220
3453.196242	449346.304388	51.036225
3452.846531	448960.326010	51.041229
3452.135389	448583.888328	51.046234
3451.301589	448206.144484	51.051239
3451.100632	447811.039471	51.056244
3450.241758	447442.219281	51.061249
3449.385964	447051.671084	51.066253
3448.793201	446681.172835	51.071258
3447.758271	446298.405612	51.076263
3447.412244	445912.579542	51.081268
3446.605365	445540.270122	51.086273
3446.105209	445159.734698	51.091277
3444.913192	444776.663228	51.096282
3444.265929	444406.594895	51.101287
3443.609666	444019.822818	51.106292
3443.020064	443649.023048	51.111297
3442.129049	443276.539377	51.116301
3441.470726	442904.926846	51.121306
3441.065365	442543.928480	51.126311
3440.506757	442167.923380	51.131316
3439.434187	441801.232547	51.136321
3438.755979	441411.731717	51.141325
3438.206811	441043.576097	51.146330
3437.287792	440671.869068	51.151335
3436.598950	440301.033788	51.156340
3435.416759	439941.185747	51.161345
3434.733636	439574.983751	51.166349
3434.019299	439225.737830	51.171354
3433.309376	438864.124037	51.176359
3432.954569	438498.666473	51.181364
3432.055692	438145.829837	51.186369
3431.953628	437772.325285	51.191373
3430.981263	437418.322213	51.196378
3430.101905	437061.227673	51.201383
3429.551430	436695.139930	51.206388
3428.641985	436343.193406	51.211393
3428.119013	435984.757841	51.216397
3427.239364	435620.559769	51.221402
3426.299716	435277.742726	51.226407
3425.711743	434906.557298	51.231412
3424.985504	434576.721315	51.236417
3424.465166	434215.594448	51.241421
3423.650886	433866.822854	51.246426
3422.902511	433516.817362	51.251431
3422.323618	433154.669154	51.256436
3421.384340	432818.318847	51.261441
3421.035978	432464.681075	51.266445
3419.989063	432118.867834	51.271450
3419.364438	431769.149064	51.276455
3418.681497	431411.080841	51.281460
3417.895927	431087.785924	51.286465
3417.377747	430734.836954	51.291469
3416.540004	430394.528624	51.296474
3415.802065	430050.924348	51.301479
3415.160450	429706.767065	51.306484
3414.216996	429377.483041	51.311489
3413.740067	429033.494046	51.316493
3413.271453	428690.184899	51.321498
3412.285373	428354.089073	51.326503
3411.551833	428007.663980	51.331508
3410.969202	427672.155989	51.336513
3410.287617	427341.840168	51.341517
3409.628729	427002.424826	51.346522
3408.755226	426667.102544	51.351527
3407.972099	426320.637956	51.356532
3407.430961	425989.927666	51.361537
3406.423628	425667.160230	51.366541
3405.663346	425336.044796	51.371546
3405.245761	425002.712280	51.376551
3405.006523	424663.353438	51.381556
3404.066133	424349.804702	51.386561
3403.379186	424003.041179	51.391565
3402.831985	423668.290431	51.396570
3401.516354	423334.901660	51.401575
3401.383625	423006.731984	51.406580
3400.489014	422695.290601	51.411585
3399.749045	422353.696207	51.416589
3399.148149	422023.861585	51.421594
3398.453184	421698.152884	51.426599
3397.793255	421371.825176	51.431604
3396.737311	421045.124414	51.436609
3396.022347	420730.152445	51.441613
3395.530993	420398.071193	51.446618
3394.691014	420082.933866	51.451623
3394.664446	419746.884790	51.456628
3393.790483	419433.955592	51.461633
3392.973656	419112.833951	51.466637
3392.237254	418784.887717	51.471642
3391.256159	418463.047941	51.476647
3390.621391	418134.697034	51.481652
3389.891976	417820.837952	51.486657
3389.176041	417499.834485	51.491661
3388.581091	417181.323391	51.496666
3387.759684	416865.944025	51.501671
3386.964352	416544.561294	51.506676
3386.302517	416240.836480	51.511681
3385.692516	415926.200945	51.516685
3385.195928	415621.732094	51.521690
3384.316811	415302.838597	51.526695
3383.917934	414985.567931	51.531700
3382.944485	414670.595096	51.536705
3381.989033	414360.595916	51.541709
3381.543046	414051.529200	51.546714
3381.041675	413746.761967	51.551719
3380.260911	413428.035647	51.556724
3379.170684	413128.284347	51.561729
3378.483827	412812.636373	51.566733
3377.803619	412520.411356	51.571738
3377.147788	412205.793767	51.576743
3376.618140	411901.570917	51.581748
3375.865274	411605.714756	51.586753
3375.349086	411305.752571	51.591757
3374.774541	410997.538151	51.596762
3373.853051	410699.387292	51.601767
3373.139031	410400.311268	51.606772
3372.234578	410106.700409	51.611777
3371.564208	409795.846003	51.616781
3371.322543	409491.324397	51.621786
3370.527343	409200.279444	51.626791
3369.786721	408890.367079	51.631796
3368.676919	408598.959501	51.636801
3367.879983	408306.152776	51.641805
3367.379561	408006.383982	51.646810
3366.686441	407726.261835	51.651815
3365.876892	407430.475349	51.656820
3365.281415	407144.588972	51.661825
3364.773888	406846.131477	51.666829
3364.299627	406557.297861	51.671834
3363.214402	406271.074197	51.676839
3363.052116	405970.164679	51.681844
3362.122421	405677.658900	51.686849
3361.576858	405382.522683	51.691853
3360.952810	405079.313945	51.696858
3360.055738	404799.960013	51.701863
3359.476127	404483.141038	51.706868
3358.615242	404206.470192	51.711873
3357.846436	403910.338753	51.716877
3357.062502	403628.923200	51.721882
3356.294511	403341.682143	51.726887
3355.501555	403055.001606	51.731892
3355.052209	402769.560430	51.736897
3354.527038	402488.449680	51.741901
3354.016485	402206.673277	51.746906
3353.021981	401925.936805	51.751911
3352.696444	401631.086607	51.756916
3351.576331	401342.942751	51.761921
3350.926956	401056.729954	51.766925
3350.543571	400774.361659	51.771930
3349.339386	400499.288907	51.776935
3348.864429	400214.794998	51.781940
3347.950868	399937.841328	51.786945
3347.315338	399659.748281	51.791949
3347.057578	399381.008461	51.796954
3346.191688	399105.133244	51.801959
3345.585183	398817.826304	51.806964
3344.825809	398545.462985	51.811969
3344.054517	398260.210888	51.816973
3343.597495	397993.438638	51.821978
3342.640555	397709.634727	51.826983
3342.178227	397429.436295	51.831988
3341.486993	397151.152910	51.836993
3340.420286	396870.079314	51.841997
3339.761377	396595.268988	51.847002
3339.308746	396326.931921	51.852007
3338.787307	396040.934870	51.857012
3337.747363	395778.101310	51.862017
3337.321709	395503.016349	51.867021
3336.817037	395232.060206	51.872026
3335.892320	394955.117541	51.877031
3335.339384	394682.130756	51.882036
3334.480736	394411.224031	51.887041
3333.686654	394132.830271	51.892045
3332.944209	393872.223052	51.897050
3332.239066	393614.480911	51.902055
3331.459273	393334.044436	51.907060
3330.934156	393073.269653	51.912065
3330.112826	392802.725678	51.917069
3329.897787	392533.253262	51.922074
3329.165669	392280.412476	51.927079
3328.530112	392008.866750	51.932084
3327.834912	391736.107895	51.937089
3326.908521	391456.137052	51.942093
3326.355015	391201.149819	51.947098
3325.512927	390928.636724	51.952103
3325.145825	390650.198276	51.957108
3324.189291	390391.302346	51.962113
3323.675413	390124.299582	51.967117
3322.833901	389852.210324	51.972122
3322.070392	389588.268828	51.977127
3321.305066	389329.614589	51.982132
3320.786744	389069.368315	51.987137
3320.317056	388808.705604	51.992141
3319.458537	388540.321482	51.997146
3318.558784	388272.526722	52.002151
3318.339805	388014.132558	52.007156
3317.474952	387765.476151	52.012161
3316.608057	387500.976181	52.017165
3316.090065	387230.163554	52.022170
3315.347026	386978.863282	52.027175
3314.469153	386708.917416	52.032180
3313.986779	386457.419742	52.037185
3313.509383	386197.120851	52.042189
3312.765066	385938.311829	52.047194
3311.797089	385680.502698	52.052199
3311.753418	385421.146911	52.057204
3310.249844	385167.106284	52.062209
3309.629882	384919.485269	52.067213
3309.439338	384654.679741	52.072218
3308.484319	384401.284595	52.077223
3307.827002	384138.914296	52.082228
3307.221212	383877.424100	52.087233
3306.313171	383619.820039	52.092237
3305.915539	383368.822021	52.097242
3304.802192	383125.488786	52.102247
3304.391074	382860.832595	52.107252
3303.480547	382613.979789	52.112257
3303.181237	382363.697062	52.117261
3302.767903	382104.936244	52.122266
3301.652463	381849.667260	52.127271
3300.781955	381604.734447	52.132276
3300.232052	381355.883533	52.137281
3299.569859	381118.035909	52.142285
3298.778416	380858.792349	52.147290
3298.200241	380623.115642	52.152295
3297.638383	380356.405794	52.157300
3296.774975	380113.395308	52.162305
3296.323638	379871.844167	52.167309
3295.553594	379625.051616	52.172314
3294.787889	379371.694750	52.177319
3294.057752	379125.706623	52.182324
3293.027588	378871.447260	52.187329
3292.552488	378632.461104	52.192333
3292.181078	378392.973830	52.197338
3291.201464	378154.344348	52.202343
3290.687292	377912.689312	52.207348
3289.819150	377669.359173	52.212353
3289.095174	377434.296750	52.217357
3288.864141	377195.568528	52.222362
3287.792099	376960.634665	52.227367
3287.384774	376709.925666	52.232372
3286.721249	376472.329841	52.237377
3285.652939	376228.615591	52.242381
3285.615155	375987.560327	52.247386
3284.357475	375746.645693	52.252391
3283.827823	375502.612927	52.257396
3283.093920	375265.606167	52.262401
3282.610696	375027.006711	52.267405
3281.845648	374786.059326	52.272410
3281.373193	374549.464916	52.277415
3280.614183	374299.381667	52.282420
3279.783744	374067.241794	52.287425
3279.359471	373829.007591	52.292429
3278.964296	373593.412963	52.297434
3278.029435	373350.296339	52.302439
3277.482056	373102.868801	52.307444
3276.733052	372859.134817	52.312449
3275.758039	372626.373760	52.317453
3275.262995	372380.485403	52.322458
3274.429617	372152.863373	52.327463
3273.820798	371909.534136	52.332468
3273.072129	371675.434598	52.337473
3272.534110	371440.384625	52.342477
3271.873093	371194.083109	52.347482
3270.961359	370967.789920	52.352487
3270.236068	370733.656030	52.357492
3269.577686	370494.117009	52.362497
3268.958386	370264.186796	52.367501
3268.256829	370030.732173	52.372506
3267.274343	369806.250263	52.377511
3267.119294	369575.606916	52.382516
3266.172371	369338.294951	52.387521
3265.514505	369108.746262	52.392525
3265.040116	368879.625271	52.397530
3263.839506	368658.021265	52.402535
3263.533240	368419.763381	52.407540
3262.893775	368194.557382	52.412545
3262.280120	367965.606256	52.417549
3261.641902	367725.896054	52.422554
3260.805628	367505.348000	52.427559
3260.092629	367272.898028	52.432564
3259.672291	367047.778697	52.437569
3259.072384	366813.807349	52.442573
3258.536001	366577.026077	52.447578
3257.273020	366367.963390	52.452583
3256.890422	366124.820253	52.457588
3256.140619	365895.778183	52.462593
3255.189038	365675.137508	52.467597
3254.712713	365452.181606	52.472602
3253.984311	365226.720177	52.477607
3253.842848	364991.954385	52.482612
3253.060342	364775.251683	52.487617
3252.089584	364545.830613	52.492621
3251.755238	364311.677009	52.497626
3250.673228	364091.761662	52.502631
3250.135361	363869.291144	52.507636
3249.454785	363642.745663	52.512641
3248.695235	363415.295573	52.517645
3248.178647	363189.637904	52.522650
3247.302790	362966.096943	52.527655
3246.341504	362740.074870	52.532660
3246.133235	362521.973034	52.537665
3245.338296	362288.212780	52.542669
3244.973751	362067.029295	52.547674
3244.035195	361849.523283	52.552679
3242.998513	361626.688346	52.557684
3242.416164	361404.136716	52.562689
3241.530508	361184.151086	52.567693
3241.389242	360968.067041	52.572698
3240.188103	360753.956288	52.577703
3239.907494	360539.444503	52.582708
3239.134760	360311.243502	52.587713
3238.098824	360098.706747	52.592717
3238.048175	359873.468372	52.597722
3237.536844	359662.653356	52.602727
3236.528996	359442.297330	52.607732
3236.097329	359225.666087	52.612737
3235.051498	358995.975267	52.617741
3234.930836	358779.623636	52.622746
3233.951721	358563.737643	52.627751
3233.133526	358338.842558	52.632756
3232.247544	358127.036818	52.637761
3231.739372	357911.480596	52.642765
3231.286597	357695.303936	52.647770
3230.270390	357479.495375	52.652775
3229.523199	357260.665987	52.657780
3229.068694	357052.808038	52.662785
3228.256620	356834.470533	52.667789
3228.089981	356622.162836	52.672794
3227.164308	356412.493627	52.677799
3226.791202	356185.457079	52.682804
3226.159500	355979.760308	52.687809
3225.091744	355759.448175	52.692813
3224.422516	355524.159435	52.697818
3223.798218	355317.364522	52.702823
3223.072754	355105.444206	52.707828
3222.364242	354887.412698	52.712833
3221.984011	354679.405953	52.717837
3221.446881	354459.207827	52.722842
3220.323834	354236.276630	52.727847
3219.763776	354021.170007	52.732852
3219.172189	353810.292005	52.737857
3218.057718	353605.323699	52.742861
3217.595039	353385.949031	52.747866
3216.933680	353172.890844	52.752871
3215.942919	352970.470842	52.757876
3215.510452	352758.978067	52.762881
3214.786320	352562.164095	52.767885
3214.457584	352346.861260	52.772890
3213.460355	352143.548352	52.777895
3212.913753	351925.147937	52.782900
3212.577451	351718.165853	52.787905
3211.686845	351514.248312	52.792909
3211.034590	351301.333815	52.797914
3210.396663	351095.745889	52.802919
3209.634220	350876.255504	52.807924
3209.112356	350663.317844	52.812929
3208.292077	350455.745725	52.817933
3207.550576	350251.876147	52.822938
3206.833989	350041.817318	52.827943
3206.144707	349830.149950	52.832948
3205.569681	349629.636668	52.837953
3204.858586	349426.420910	52.842957
3204.301823	349208.341947	52.847962
3203.462976	348997.407651	52.852967
3202.807440	348800.899925	52.857972
3202.138625	348599.277857	52.862977
3201.242480	348391.888064	52.867981
3200.840010	348189.942406	52.872986
3199.972623	347981.273949	52.877991
3199.372238	347778.849077	52.882996
3198.790601	347570.108428	52.888001
3198.107334	347380.955685	52.893005
3197.579485	347168.972632	52.898010
3196.613870	346959.628711	52.903015
3195.904578	346767.652836	52.908020
3195.321470	346563.693730	52.913025
3194.505924	346364.250302	52.918029
3194.201143	346159.456691	52.923034
3193.627790	345971.019987	52.928039
3192.878422	345754.612500	52.933044
3192.089230	345549.969711	52.938049
3191.516409	345351.909725	52.943053
3190.743997	345148.357335	52.948058
3189.952126	344957.890202	52.953063
3189.332438	344748.203508	52.958068
3188.687466	344553.486586	52.963073
3187.783619	344350.359458	52.968077
3187.600112	344144.826856	52.973082
3186.867438	343954.296188	52.978087
3186.120643	343742.895176	52.983092
3185.332085	343544.303232	52.988097
3184.506832	343346.429136	52.993101
3183.871841	343147.989751	52.998106
3183.182313	342947.012940	53.003111
3182.482331	342748.633422	53.008116
3181.858000	342549.834015	53.013121
3181.241738	342365.312486	53.018125
3180.918942	342153.813330	53.023130
3179.818994	341963.996247	53.028135
3179.176200	341769.218991	53.033140
3178.683346	341556.726486	53.038145
3177.652433	341384.103946	53.043149
3177.139729	341172.045977	53.048154
3176.436139	340991.810503	53.053159
3175.788425	340793.161802	53.058164
3175.263955	340595.791168	53.063169
3174.635565	340401.312765	53.068173
3173.894832	340200.411390	53.073178
3173.151342	340010.633718	53.078183
3172.373456	339818.722672	53.083188
3172.252213	339618.586900	53.088193
3171.070011	339424.193086	53.093197
3170.664266	339222.981034	53.098202
3169.992387	339030.719901	53.103207
3169.311856	338834.539386	53.108212
3168.860717	338644.711363	53.113217
3167.835560	338463.501288	53.118221
3167.545633	338252.110988	53.123226
3166.777794	338067.117070	53.128231
3166.049680	337868.624641	53.133236
3165.514980	337664.118818	53.138241
3164.868627	337470.448897	53.143245
3164.056204	337271.026105	53.148250
3163.405590	337081.301426	53.153255
3162.842142	336882.525381	53.158260
3161.846300	336684.733582	53.163265
3161.127703	336493.948794	53.168269
3160.957409	336287.420872	53.173274
3159.800949	336086.368792	53.178279
3159.242274	335898.051752	53.183284
3158.450746	335701.726653	53.188289
3157.668845	335514.793068	53.193293
3157.419771	335319.144734	53.198298
3156.648049	335133.201305	53.203303
3156.103459	334937.445882	53.208308
3155.442105	334747.665361	53.213313
3154.757094	334557.149793	53.218317
3154.207989	334355.003631	53.223322
3153.338974	334158.813617	53.228327
3152.503463	333956.024246	53.233332
3151.984809	333763.265354	53.238337
3151.187270	333581.802338	53.243341
3150.456046	333370.517354	53.248346
3149.679973	333196.916379	53.253351
3148.974799	332997.896805	53.258356
3148.522184	332812.965865	53.263361
3147.531122	332628.934289	53.268365
3147.023638	332433.165925	53.273370
3146.536199	332261.273584	53.278375
3145.969235	332071.114424	53.283380
3145.245064	331873.163940	53.288385
3144.511926	331685.652250	53.293389
3143.900197	331497.738984	53.298394
3142.682801	331318.627858	53.303399
3142.429489	331130.096839	53.308404
3141.584028	330943.135623	53.313409
3140.863996	330765.446494	53.318413
3140.319152	330577.138383	53.323418
3139.549282	330389.196358	53.328423
3139.129771	330200.841993	53.333428
3138.516735	330014.325352	53.338433
3137.816543	329830.571602	53.343437
3136.702317	329644.082414	53.348442
3136.228875	329459.884527	53.353447
3135.501445	329275.166272	53.358452
3134.982576	329086.646596	53.363457
3133.904029	328916.774835	53.368461
3133.493535	328736.867838	53.373466
3132.935251	328550.058837	53.378471
3132.351562	328373.997298	53.383476
3131.751039	328190.020100	53.388481
3130.981248	328007.724118	53.393485
3130.475241	327827.499117	53.398490
3129.753772	327649.573703	53.403495
3128.740851	327459.804280	53.408500
3128.360181	327283.300767	53.413505
3127.322378	327104.762203	53.418509
3127.333005	326915.593295	53.423514
3126.605413	326734.993466	53.428519
3125.815004	326548.674646	53.433524
3125.424972	326358.625775	53.438529
3124.684214	326174.029507	53.443533
3124.197435	325980.481533	53.448538
3123.137596	325798.811895	53.453543
3122.586052	325603.134590	53.458548
3121.926551	325410.223620	53.463553
3121.167809	325235.252083	53.468557
3120.141717	325058.616616	53.473562
3119.322658	324879.198261	53.478567
3118.888620	324696.586926	53.483572
3118.336631	324506.661162	53.488577
3117.276544	324333.644932	53.493581
3117.125801	324157.556454	53.498586
3116.485053	323982.945487	53.503591
3115.587633	323796.178979	53.508596
3114.987645	323617.206976	53.513601
3114.091282	323436.422831	53.518605
3113.833250	323264.626904	53.523610
3113.068581	323085.476139	53.528615
3112.403612	322892.738394	53.533620
3111.771402	322717.843378	53.538625
3111.112358	322535.059241	53.543629
3110.440148	322349.526969	53.548634
3109.619028	322181.535322	53.553639
3109.039720	321997.133355	53.558644
3108.489858	321803.432877	53.563649
3107.774167	321633.361101	53.568653
3107.443060	321455.029491	53.573658
3106.418854	321265.629513	53.578663
3105.633047	321083.269768	53.583668
3105.339629	320903.963532	53.588673
3104.185030	320729.299955	53.593677
3103.993080	320548.220078	53.598682
3102.842925	320373.147711	53.603687
3102.351081	320198.149064	53.608692
3101.924216	320012.343887	53.613697
3100.711486	319840.055750	53.618701
3100.403490	319651.964898	53.623706
3099.519382	319481.788364	53.628711
3098.814245	319292.028187	53.633716
3097.992489	319114.406128	53.638721
3097.107030	318958.284027	53.643725
3096.799835	318779.714180	53.648730
3096.149399	318614.285999	53.653735
3095.444582	318435.421940	53.658740
3094.763656	318256.935698	53.663745
3094.017838	318095.442926	53.668749
3093.712887	317916.641918	53.673754
3093.055565	317745.280510	53.678759
3092.239894	317567.960113	53.683764
3091.917123	317394.100712	53.688769
3091.071443	317220.018191	53.693773
3090.214059	317031.525232	53.698778
3089.719605	316860.569341	53.703783
3088.611748	316697.272715	53.708788
3088.362991	316514.055122	53.713793
3087.461791	316347.847892	53.718797
3086.915291	316159.940632	53.723802
3086.256612	315993.847206	53.728807
3085.725541	315822.920770	53.733812
3085.098146	315649.157405	53.738817
3083.907066	315476.476008	53.743821
3083.809269	315300.336537	53.748826
3083.007694	315126.345200	53.753831
3082.518148	314956.200085	53.758836
3081.888605	314772.479367	53.763841
3081.116371	314601.334396	53.768845
3080.839838	314421.147536	53.773850
3079.996470	314239.904203	53.778855
3079.207124	314063.184528	53.783860
3078.739505	313879.385671	53.788865
3077.790237	313704.167588	53.793869
3077.479123	313519.655815	53.798874
3076.739515	313347.663320	53.803879
3075.745927	313179.734025	53.808884
3075.234717	312995.813212	53.813889
3074.804414	312820.435153	53.818893
3073.977050	312639.593968	53.823898
3073.262742	312455.780765	53.828903
3072.387925	312276.881748	53.833908
3071.880592	312098.459029	53.838913
3070.938474	311930.774292	53.843917
3070.739687	311747.565849	53.848922
3069.798459	311569.720223	53.853927
3068.941567	311400.264166	53.858932
3068.744800	311224.719279	53.863937
3067.687170	311051.805858	53.868941
3067.151109	310874.709869	53.873946
3066.391767	310697.419760	53.878951
3065.808650	310522.291429	53.883956
3064.962959	310347.255313	53.888961
3064.085742	310181.543932	53.893965
3063.498002	310005.244179	53.898970
3063.023428	309832.720473	53.903975
3062.207434	309662.516897	53.908980
3061.763534	309498.365706	53.913985
3060.901182	309336.012110	53.918989
3060.633024	309157.725192	53.923994
3059.886681	308984.759428	53.928999
3058.807034	308811.285936	53.934004
3058.575564	308640.453631	53.939009
3057.574501	308473.995515	53.944013
3057.017720	308294.963586	53.949018
3056.343259	308124.684498	53.954023
3055.513282	307965.023220	53.959028
3055.070441	307781.032305	53.964033
3054.390555	307622.772873	53.969037
3053.768881	307452.586368	53.974042
3052.981480	307282.018418	53.979047
3052.021905	307107.606783	53.984052
3051.756440	306939.145771	53.989057
3050.781238	306776.450142	53.994061
3050.496871	306603.229683	53.999066
3049.709527	306440.172849	54.004071
3048.926118	306264.229734	54.009076
3048.534809	306092.960882	54.014081
3047.445011	305925.571230	54.019085
3047.098054	305767.154956	54.024090
3046.411351	305607.951902	54.029095
3045.667301	305427.239399	54.034100
3045.250663	305245.838197	54.039105
3044.275113	305093.836057	54.044109
3043.973496	304922.831626	54.049114
3043.353181	304747.522799	54.054119
3042.575712	304568.316910	54.059124
3041.934858	304387.586692	54.064129
3041.123370	304220.863919	54.069133
3040.228051	304050.079696	54.074138
3039.728143	303890.259364	54.079143
3038.739614	303720.177069	54.084148
3038.547187	303546.989069	54.089153
3037.427719	303388.768713	54.094157
3036.894005	303210.235558	54.099162
3036.448481	303046.814983	54.104167
3035.776110	302886.791632	54.109172
3035.136127	302713.622534	54.114177
3034.503597	302553.745310	54.119181
3033.894266	302378.890212	54.124186
3033.033957	302211.230595	54.129191
3032.184788	302055.690888	54.134196
3031.631012	301880.495355	54.139201
3030.664177	301723.649690	54.144205
3030.121023	301548.757688	54.149210
3029.729239	301385.250388	54.154215
3029.454930	301225.875318	54.159220
3028.458498	301054.034045	54.164225
3027.910287	300888.080753	54.169229
3027.291211	300717.962026	54.174234
3026.747326	300545.462846	54.179239
3025.771933	300383.371121	54.184244
3025.179167	300209.325867	54.189249
3024.281913	300045.438786	54.194253
3023.680173	299868.618747	54.199258
3023.083909	299704.301688	54.204263
3022.315635	299537.210376	54.209268
3021.588685	299376.198854	54.214273
3020.838976	299220.691553	54.219277
3020.145547	299049.233126	54.224282
3019.902214	298892.117382	54.229287
3018.722782	298728.604732	54.234292
3018.556717	298559.023273	54.239297
3017.880772	298409.615552	54.244301
3017.248928	298236.873233	54.249306
3016.961003	298076.758734	54.254311
3016.176475	297903.479986	54.259316
3015.735998	297728.134739	54.264321
3014.646745	297562.263786	54.269325
3013.976544	297378.983452	54.274330
3013.261090	297211.346737	54.279335
3012.732970	297052.873755	54.284340
3012.363962	296872.601266	54.289345
3011.528413	296706.103643	54.294349
3010.556741	296536.673254	54.299354
3009.993489	296374.741754	54.304359
3009.203645	296205.180422	54.309364
3008.572571	296026.935030	54.314369
3007.595566	295859.949717	54.319373
3007.336304	295684.803071	54.324378
3006.639102	295522.968461	54.329383
3005.810727	295364.567071	54.334388
3005.393337	295188.961141	54.339393
3004.505021	295024.991673	54.344397
3003.942185	294858.067301	54.349402
3003.345974	294699.501306	54.354407
3002.587237	294529.500680	54.359412
3001.909481	294364.707876	54.364417
3000.908854	294208.395700	54.369421
3000.210056	294037.697574	54.374426
2999.868238	293882.452373	54.379431
2998.806741	293719.477050	54.384436
2998.521468	293549.757241	54.389441
2997.732278	293395.703066	54.394445
2997.134387	293225.243003	54.399450
2996.507477	293065.993042	54.404455
2995.919791	292909.690976	54.409460
2995.305906	292737.017412	54.414465
2994.625494	292582.614387	54.419469
2994.010911	292411.010321	54.424474
2993.383480	292243.126410	54.429479
2992.438864	292084.588214	54.434484
2992.242253	291914.751284	54.439489
2991.610942	291751.502724	54.444493
2990.811127	291572.669134	54.449498
2990.102250	291399.067333	54.454503
2989.480861	291231.512842	54.459508
2988.898625	291069.529440	54.464513
2987.831792	290917.937015	54.469517
2987.371402	290746.485644	54.474522
2986.512498	290577.847743	54.479527
2986.112524	290413.772200	54.484532
2985.466680	290240.465246	54.489537
2984.762292	290081.531214	54.494541
2983.854662	289921.865229	54.499546
2983.275862	289757.868526	54.504551
2982.731392	289589.740520	54.509556
2982.148243	289415.964699	54.514561
2981.333705	289261.428080	54.519565
2980.868308	289089.416161	54.524570
2980.161184	288923.962155	54.529575
2979.255197	288767.529664	54.534580
2978.734383	288591.935265	54.539585
2978.190558	288432.312730	54.544589
2977.655889	288267.009333	54.549594
2976.716376	288100.929493	54.554599
2975.980544	287941.846452	54.559604
2975.525628	287770.366944	54.564609
2974.620659	287606.777226	54.569613
2974.344010	287434.810897	54.574618
2973.689491	287272.862247	54.579623
2972.869365	287107.985454	54.584628
2972.244743	286929.095732	54.589633
2971.656489	286775.107818	54.594637
2970.783332	286597.377855	54.599642
2970.144623	286439.221032	54.604647
2969.432271	286272.340276	54.609652
2969.015211	286102.127327	54.614657
2968.159503	285940.821136	54.619661
2967.709529	285776.394485	54.624666
2967.023365	285600.722811	54.629671
2965.793717	285446.683055	54.634676
2965.529888	285281.157066	54.639681
2964.931536	285118.587322	54.644685
2964.178415	284950.540907	54.649690
2963.724770	284778.473995	54.654695
2962.894477	284612.731786	54.659700
2962.547958	284442.124926	54.664705
2961.906077	284283.178216	54.669709
2961.319149	284114.035498	54.674714
2960.623362	283938.517446	54.679719
2959.252417	283764.990848	54.684724
2958.726702	283602.638244	54.689729
2958.081812	283446.391340	54.694733
2957.882533	283273.162979	54.699738
2957.014906	283104.217138	54.704743
2956.520052	282939.210736	54.709748
2955.839795	282760.990166	54.714753
2954.938138	282604.579901	54.719757
2954.440626	282433.537794	54.724762
2953.928621	282275.639530	54.729767
2953.275600	282097.745516	54.734772
2952.606410	281923.572369	54.739777
2951.996445	281762.327662	54.744781
2951.237049	281586.284045	54.749786
2950.795303	281413.908458	54.754791
2949.989631	281234.306511	54.759796
2949.144780	281058.021592	54.764801
2948.482757	280898.847835	54.769805
2947.966809	280733.742275	54.774810
2947.390962	280558.000412	54.779815
2946.510624	280389.539706	54.784820
2946.168954	280211.672289	54.789825
2945.313461	280046.518453	54.794829
2944.843971	279869.613520	54.799834
2943.956998	279699.269061	54.804839
2943.420963	279535.032347	54.809844
2943.027746	279352.155644	54.814849
2942.406758	279184.392217	54.819853
2941.586862	279009.427241	54.824858
2941.011189	278818.989756	54.829863
2940.101204	278652.698217	54.834868
2939.284323	278470.041233	54.839873
2938.770891	278301.190966	54.844877
2938.039275	278131.050861	54.849882
2937.890724	277964.791493	54.854887
2936.790400	277792.213816	54.859892
2936.318166	277606.929841	54.864897
2935.340578	277434.179881	54.869901
2934.588112	277260.400997	54.874906
2933.839790	277093.574305	54.879911
2933.115085	276926.234493	54.884916
2932.585326	276750.051745	54.889921
2931.915166	276580.054559	54.894925
2931.664458	276416.205242	54.899930
2930.695100	276237.341466	54.904935
2929.737750	276077.449727	54.909940
2929.508188	275905.498088	54.914945
2928.911407	275734.546908	54.919949
2928.217429	275566.667316	54.924954
2927.770981	275380.156608	54.929959
2926.794015	275207.202663	54.934964
2926.372892	275027.666278	54.939969
2925.454950	274853.455035	54.944973
2924.609631	274670.598510	54.949978
2924.097730	274495.125972	54.954983
2923.378061	274332.216779	54.959988
2922.901628	274152.128855	54.964993
2922.002295	273983.135701	54.969997
2921.528868	273818.022725	54.975002
2920.666134	273647.113662	54.980007
2919.536346	273472.197415	54.985012
2919.450556	273303.457522	54.990017
2918.657001	273145.500945	54.995021
2917.903494	272967.800044	55.000026
2917.472954	272798.809148	55.005031
2916.370967	272638.481943	55.010036
2916.312025	272459.295833	55.015041
2915.377300	272294.892709	55.020045
2914.620853	272131.123555	55.025050
2913.846601	271959.080019	55.030055
2913.299891	271786.058152	55.035060
2912.633314	271617.104753	55.040065
2912.165777	271461.388878	55.045069
2911.609570	271290.176836	55.050074
2910.598566	271109.817283	55.055079
2910.015121	270940.850822	55.060084
2909.499065	270763.596510	55.065089
2908.976801	270594.493079	55.070093
2908.128695	270443.116287	55.075098
2907.441911	270268.308589	55.080103
2907.065571	270097.221087	55.085108
2906.299582	269913.995987	55.090113
2905.610841	269744.689863	55.095117
2905.188413	269569.152814	55.100122
2904.980602	269395.823036	55.105127
2903.803952	269234.846000	55.110132
2903.544272	269038.119160	55.115137
2902.686938	268861.123041	55.120141
2901.845046	268687.180716	55.125146
2901.056481	268518.068964	55.130151
2899.898951	268341.400665	55.135156
2899.778150	268168.464917	55.140161
2899.442969	267998.644818	55.145165
2898.414981	267809.553130	55.150170
2898.224840	267638.436761	55.155175
2897.086671	267461.434573	55.160180
2896.579893	267292.253091	55.165185
2896.091912	267119.146582	55.170189
2895.279331	266930.454052	55.175194
2894.574922	266751.626122	55.180199
2893.968320	266590.177533	55.185204
2893.229695	266400.251022	55.190209
2892.530855	266227.483824	55.195213
2891.908298	266056.232701	55.200218
2891.292760	265878.129601	55.205223
2890.498768	265711.057058	55.210228
2889.791753	265526.779826	55.215233
2889.270415	265353.271751	55.220237
2888.474020	265184.824512	55.225242
2887.685379	265007.156666	55.230247
2886.985059	264832.276401	55.235252
2886.803897	264655.149226	55.240257
2886.228422	264497.593092	55.245261
2885.257979	264303.323703	55.250266
2884.818586	264122.774001	55.255271
2883.888890	263953.024052	55.260276
2883.066472	263778.112658	55.265281
2882.701640	263604.835252	55.270285
2882.027381	263425.138054	55.275290
2881.177198	263248.881509	55.280295
2880.610404	263070.033388	55.285300
2880.250538	262891.763826	55.290305
2879.227944	262721.825431	55.295309
2878.551410	262546.866086	55.300314
2878.283205	262364.431021	55.305319
2877.273736	262192.886343	55.310324
2876.713680	262011.414531	55.315329
2876.168595	261843.769501	55.320333
2875.383305	261660.525336	55.325338
2875.108613	261495.486337	55.330343
2874.028357	261311.015694	55.335348
2873.518092	261122.736615	55.340353
2872.744621	260956.860046	55.345357
2872.009676	260782.343897	55.350362
2871.630909	260595.623337	55.355367
2870.772633	260418.529226	55.360372
2870.207058	260237.288578	55.365377
2869.260675	260063.417575	55.370381
2868.721296	259884.668845	55.375386
2868.089708	259707.793972	55.380391
2867.289700	259531.200560	55.385396
2866.911660	259354.107502	55.390401
2866.120929	259177.945807	55.395405
2865.020002	259004.150901	55.400410
2864.722203	258824.447802	55.405415
2863.873849	258653.796590	55.410420
2863.004246	258472.554358	55.415425
2862.306485	258309.137789	55.420429
2861.771687	258139.863463	55.425434
2861.306060	257965.230127	55.430439
2860.825863	257796.940628	55.435444
2860.314316	257615.107521	55.440449
2859.523888	257437.928320	55.445453
2859.140476	257265.243474	55.450458
2858.340960	257082.335813	55.455463
2857.457540	256912.022472	55.460468
2857.075704	256731.926769	55.465473
2856.323213	256559.606507	55.470477
2855.773439	256370.904258	55.475482
2855.212013	256191.677851	55.480487
2853.839223	256018.997822	55.485492
2853.695739	255832.727498	55.490497
2853.197878	255656.012729	55.495501
2852.414082	255482.705056	55.500506
2851.847019	255286.875675	55.505511
2850.966253	255121.427552	55.510516
2850.459985	254931.038855	55.515521
2849.994727	254751.518305	55.520525
2849.109515	254573.948977	55.525530
2848.639591	254392.697722	55.530535
2847.562460	254224.632850	55.535540
2847.223068	254039.439320	55.540545
2846.692288	253862.935056	55.545549
2845.756383	253677.887261	55.550554
2845.531693	253483.788120	55.555559
2844.569009	253301.571762	55.560564
2843.948282	253117.264078	55.565569
2843.250103	252937.043542	55.570573
2842.513197	252756.982115	55.575578
2841.995631	252576.223993	55.580583
2840.913620	252398.025711	55.585588
2840.181945	252213.838366	55.590593
2839.938870	252029.370106	55.595597
2839.256351	251842.450415	55.600602
2838.399884	251668.648356	55.605607
2837.908680	251488.880358	55.610612
2837.547569	251306.443411	55.615617
2836.798352	251135.655433	55.620621
2836.105409	250945.682358	55.625626
2835.025192	250752.893099	55.630631
2834.021709	250579.140886	55.635636
2834.028548	250392.954002	55.640641
2833.229909	250209.619790	55.645645
2832.352692	250035.236955	55.650650
2831.878621	249854.092792	55.655655
2831.398934	249683.976674	55.660660
2830.713328	249490.489738	55.665665
2829.799319	249313.363136	55.670669
2829.081360	249134.932368	55.675674
2828.697242	248952.170598	55.680679
2828.040857	248777.983354	55.685684
2827.200270	248591.576214	55.690689
2826.309113	248408.182318	55.695693
2825.924780	248230.794798	55.700698
2825.221730	248052.464775	55.705703
2824.659123	247872.126363	55.710708
2824.171140	247685.689955	55.715713
2823.327610	247503.155456	55.720717
2822.512823	247327.416058	55.725722
2822.298637	247133.857427	55.730727
2821.388703	246958.209934	55.735732
2820.710095	246765.540246	55.740737
2820.017345	246584.867489	55.745741
2819.375497	246401.945901	55.750746
2818.939791	246220.647181	55.755751
2818.326677	246047.678637	55.760756
2817.539896	245857.242825	55.765761
2816.961335	245676.604069	55.770765
2816.142701	245492.922215	55.775770
2815.594155	245298.273063	55.780775
2814.559273	245120.763174	55.785780
2814.284442	244931.673634	55.790785
2813.618339	244742.773646	55.795789
2812.812977	244564.184047	55.800794
2812.108136	244383.032218	55.805799
2811.466238	244210.325198	55.810804
2810.967826	244007.699273	55.815809
2810.099802	243830.342921	55.820813
2809.543132	243656.859165	55.825818
2808.927856	243465.228150	55.830823
2808.388660	243279.747967	55.835828
2807.601636	243091.047747	55.840833
2807.301511	242908.229553	55.845837
2806.593471	242726.316572	55.850842
2805.738593	242541.676872	55.855847
2805.070848	242344.020609	55.860852
2804.715794	242143.157472	55.865857
2803.638137	241948.826277	55.870861
2802.951301	241787.665284	55.875866
2802.331726	241598.202301	55.880871
2801.561036	241413.754663	55.885876
2801.109155	241224.367561	55.890881
2800.391621	241031.737864	55.895885
2799.328766	240854.671215	55.900890
2798.853706	240667.707813	55.905895
2798.071230	240485.427964	55.910900
2797.726438	240292.332993	55.915905
2797.209056	240117.294622	55.920909
2796.290349	239928.823841	55.925914
2796.006346	239740.507491	55.930919
2794.738796	239557.236396	55.935924
2794.256147	239374.885329	55.940929
2793.678573	239185.394083	55.945933
2792.762852	238998.732320	55.950938
2792.516161	238816.803133	55.955943
2791.521545	238636.469618	55.960948
2791.218795	238445.128118	55.965953
2790.638783	238265.646250	55.970957
2789.626438	238075.716438	55.975962
2789.289698	237888.710185	55.980967
2788.457034	237714.642152	55.985972
2787.598260	237524.790825	55.990977
2787.055380	237331.222982	55.995981
2786.276145	237146.045093	56.000986
2786.019383	236958.645806	56.005991
2785.139693	236784.790422	56.010996
2784.328003	236593.456368	56.016001
2784.014221	236405.659658	56.021005
2782.961799	236219.304376	56.026010
2782.801693	236021.960573	56.031015
2781.670247	235840.252869	56.036020
2781.063498	235658.589700	56.041025
2780.534911	235471.719904	56.046029
2780.005119	235288.568308	56.051034
2779.209134	235108.718519	56.056039
2778.093529	234912.495765	56.061044
2777.944305	234732.646059	56.066049
2777.613695	234539.559008	56.071053
2776.337077	234343.286464	56.076058
2776.213702	234151.949762	56.081063
2775.172212	233979.958067	56.086068
2774.579840	233782.228705	56.091073
2774.224916	233595.182084	56.096077
2773.432590	233409.223615	56.101082
2772.899833	233216.782251	56.106087
2771.855049	233036.619105	56.111092
2771.100972	232839.273730	56.116097
2770.982582	232661.154364	56.121101
2769.983465	232470.316110	56.126106
2769.604208	232262.931136	56.131111
2768.855315	232081.653473	56.136116
2768.376293	231887.703948	56.141121
2767.520453	231700.562083	56.146125
2766.994352	231511.917000	56.151130
2766.304046	231309.192091	56.156135
2765.335844	231125.659375	56.161140
2764.733378	230936.390986	56.166145
2764.131001	230748.879868	56.171149
2763.056906	230562.309560	56.176154
2762.574657	230370.146052	56.181159
2761.755870	230182.899523	56.186164
2761.258116	229997.257568	56.191169
2760.566228	229813.963788	56.196173
2759.767597	229630.789133	56.201178
2759.370166	229433.394460	56.206183
2758.552232	229258.727913	56.211188
2757.848863	229078.391030	56.216193
2757.573670	228883.829935	56.221197
2756.570824	228700.078449	56.226202
2756.215665	228514.747982	56.231207
2755.498137	228329.475300	56.236212
2754.710676	228140.751311	56.241217
2753.969094	227947.921157	56.246221
2753.343569	227767.905631	56.251226
2752.950685	227571.838399	56.256231
2752.208110	227392.478729	56.261236
2751.620650	227201.968274	56.266241
2751.045570	227002.137466	56.271245
2749.836338	226816.767679	56.276250
2749.328909	226628.893793	56.281255
2748.556824	226447.121979	56.286260
2748.018479	226258.311754	56.291265
2747.591814	226077.619043	56.296269
2747.265855	225883.938438	56.301274
2746.534336	225694.803630	56.306279
2745.326453	225515.636223	56.311284
2744.865954	225310.138998	56.316289
2744.403222	225125.634964	56.321293
2743.565533	224935.793083	56.326298
2742.936242	224737.682146	56.331303
2742.519835	224550.282300	56.336308
2741.978799	224354.908051	56.341313
2741.092582	224161.282064	56.346317
2740.293646	223981.925953	56.351322
2739.965248	223783.807887	56.356327
2738.740339	223587.156243	56.361332
2738.159998	223400.434281	56.366337
2737.637338	223206.803943	56.371341
2736.735687	223025.925925	56.376346
2736.389814	222833.554232	56.381351
2735.605985	222639.533839	56.386356
2735.194034	222448.573853	56.391361
2734.742093	222259.733829	56.396365
2733.853783	222081.312752	56.401370
2733.422487	221861.829684	56.406375
2732.442813	221677.873814	56.411380
2731.390585	221490.060033	56.416385
2731.318478	221292.225932	56.421389
2730.283248	221105.708836	56.426394
2729.823726	220911.412296	56.431399
2728.956180	220722.336383	56.436404
2728.155887	220533.224833	56.441409
2727.537538	220338.165695	56.446413
2727.059258	220162.879293	56.451418
2726.605797	219955.651065	56.456423
2725.951558	219769.089673	56.461428
2724.988974	219586.370963	56.466433
2724.400112	219392.557120	56.471437
2723.592154	219200.649710	56.476442
2723.103020	219009.774293	56.481447
2722.514296	218819.538886	56.486452
2722.049478	218618.235348	56.491457
2721.273203	218431.785797	56.496461
2720.447851	218242.378599	56.501466
2720.176142	218050.261992	56.506471
2719.408706	217862.386848	56.511476
2718.401173	217666.760025	56.516481
2717.704016	217474.890563	56.521485
2717.189962	217279.695797	56.526490
2716.532244	217094.720246	56.531495
2715.509670	216905.576962	56.536500
2715.327670	216703.292078	56.541505
2714.391323	216514.276207	56.546509
2713.993676	216324.411783	56.551514
2713.354284	216134.331594	56.556519
2712.859914	215945.807321	56.561524
2711.801449	215758.289388	56.566529
2711.273941	215558.379194	56.571533
2710.719621	215360.752260	56.576538
2710.092921	215170.329042	56.581543
2709.132393	214985.330707	56.586548
2708.651946	214783.913344	56.591553
2707.964076	214590.013811	56.596557
2706.814648	214398.950032	56.601562
2706.550046	214206.817453	56.606567
2706.266194	214028.766108	56.611572
2705.151317	213835.038218	56.616577
2704.739522	213644.037938	56.621581
2703.889562	213448.729075	56.626586
2703.276336	213249.895738	56.631591
2702.661158	213060.940420	56.636596
2701.781171	212869.036464	56.641601
2701.453413	212686.502616	56.646605
2700.585658	212487.393695	56.651610
2699.815797	212293.972059	56.656615
2699.407701	212105.572181	56.661620
2698.385114	211913.540883	56.666625
2698.081100	211719.563496	56.671629
2697.317529	211526.066784	56.676634
2696.733394	211342.928197	56.681639
2696.341514	211152.606616	56.686644
2695.670449	210957.251424	56.691649
2694.753612	210755.266403	56.696653
2693.890176	210559.751988	56.701658
2693.214594	210372.519611	56.706663
2692.516996	210185.965842	56.711668
2691.644813	209998.702080	56.716673
2691.387318	209809.699640	56.721677
2690.644490	209617.529126	56.726682
2690.105566	209419.370424	56.731687
2689.668431	209244.232962	56.736692
2689.015337	209042.453487	56.741697
2688.563590	208837.295466	56.746701
2687.184572	208649.339680	56.751706
2686.753158	208451.727045	56.756711
2686.258309	208257.841459	56.761716
2685.449879	208075.244316	56.766721
2684.889741	207872.817590	56.771725
2684.057155	207684.727294	56.776730
2683.618755	207489.549766	56.781735
2682.991184	207298.806404	56.786740
2682.281625	207104.080344	56.791745
2682.096633	206910.226337	56.796749
2680.946155	206707.324321	56.801754
2680.315620	206502.240684	56.806759
2679.739910	206315.908468	56.811764
2678.724396	206123.486725	56.816769
2678.550309	205926.948823	56.821773
2677.430175	205732.801354	56.826778
2677.017719	205528.526500	56.831783
2676.149122	205343.554597	56.836788
2675.795877	205150.127519	56.841793
2674.931518	204954.351277	56.846797
2674.144086	204767.090283	56.851802
2673.392095	204568.243169	56.856807
2672.917660	204378.719432	56.861812
2672.331812	204192.726453	56.866817
2671.538330	203997.693070	56.871821
2670.544095	203807.706324	56.876826
2670.386656	203611.109961	56.881831
2669.646559	203420.676995	56.886836
2668.740487	203230.360043	56.891841
2668.371043	203036.382663	56.896845
2667.505710	202841.542776	56.901850
2667.009798	202650.666470	56.906855
2666.189036	202454.293728	56.911860
2665.338749	202260.560627	56.916865
2665.054273	202068.571088	56.921869
2663.947848	201880.873792	56.926874
2663.720061	201682.806347	56.931879
2662.760525	201493.763594	56.936884
2662.207374	201312.356187	56.941889
2661.721433	201118.352992	56.946893
2660.874333	200929.268901	56.951898
2660.330234	200734.792692	56.956903
2659.568197	200545.658265	56.961908
2659.107169	200351.628372	56.966913
2658.646038	200155.244967	56.971917
2657.551554	199967.145073	56.976922
2657.203308	199768.136461	56.981927
2656.362348	199576.714600	56.986932
2655.651206	199382.142421	56.991937
2655.414895	199180.687699	56.996941
2654.461855	198989.451105	57.001946
2653.745730	198784.854402	57.006951
2653.102333	198598.253008	57.011956
2652.785641	198404.868937	57.016961
2651.756039	198212.171142	57.021965
2650.811134	198033.788964	57.026970
2650.441502	197831.406072	57.031975
2649.497353	197638.073303	57.036980
2648.732921	197443.885653	57.041985
2648.409918	197251.919247	57.046989
2647.925597	197060.589889	57.051994
2647.066298	196861.876683	57.056999
2646.487862	196676.811471	57.062004
2645.766342	196485.496349	57.067009
2645.458545	196286.214425	57.072013
2644.458595	196102.096035	57.077018
2643.942705	195897.682420	57.082023
2643.290899	195698.151876	57.087028
2642.391578	195511.754702	57.092033
2641.999188	195310.606739	57.097037
2641.183440	195121.372943	57.102042
2640.686154	194929.633614	57.107047
2639.998815	194732.453719	57.112052
2639.029613	194536.375350	57.117057
2638.595819	194337.668092	57.122061
2637.901976	194154.131694	57.127066
2637.352259	193952.645028	57.132071
2636.977258	193755.966582	57.137076
2635.892776	193572.506920	57.142081
2635.504877	193366.479984	57.147085
2634.775378	193164.121575	57.152090
2634.176880	192973.118251	57.157095
2633.092960	192778.795346	57.162100
2632.630788	192577.262178	57.167105
2632.251086	192373.286558	57.172109
2631.420623	192193.265275	57.177114
2630.951482	191987.854935	57.182119
2630.134264	191792.806584	57.187124
2629.399257	191592.567566	57.192129
2628.525735	191391.753317	57.197133
2628.040770	191205.942694	57.202138
2627.423813	190997.735361	57.207143
2626.659989	190812.288505	57.212148
2626.116917	190615.903660	57.217153
2625.539636	190414.817495	57.222157
2624.522857	190225.685107	57.227162
2624.006022	190024.743669	57.232167
2623.626066	189828.743320	57.237172
2622.912349	189637.147877	57.242177
2622.174954	189433.063148	57.247181
2621.510556	189243.395338	57.252186
2620.472475	189043.876500	57.257191
2620.019563	188852.904467	57.262196
2619.145115	188654.862613	57.267201
2618.857125	188450.838125	57.272205
2617.784006	188272.409364	57.277210
2617.300025	188075.135039	57.282215
2616.722610	187884.377491	57.287220
2615.884863	187695.468542	57.292225
2615.382557	187493.937581	57.297229
2614.692377	187298.798378	57.302234
2614.313170	187109.259370	57.307239
2613.696861	186916.527282	57.312244
2612.597542	186711.913774	57.317249
2612.343477	186516.823257	57.322253
2611.835773	186329.152497	57.327258
2610.839856	186121.789999	57.332263
2610.261591	185924.208981	57.337268
2609.407616	185736.722727	57.342273
2608.980574	185529.870696	57.347277
2608.230089	185343.883546	57.352282
2607.499576	185142.717070	57.357287
2606.730912	184950.996948	57.362292
2605.970400	184753.844250	57.367297
2605.493176	184551.444441	57.372301
2604.729843	184370.513749	57.377306
2604.274275	184178.022176	57.382311
2603.746535	183981.828239	57.387316
2602.916203	183782.464629	57.392321
2602.521706	183585.386270	57.397325
2601.384632	183395.435797	57.402330
2601.193206	183189.651187	57.407335
2600.654879	182986.911940	57.412340
2599.874150	182786.539966	57.417345
2599.428384	182586.141266	57.422349
2598.338916	182386.914026	57.427354
2597.969192	182179.966601	57.432359
2597.496337	181980.427241	57.437364
2596.453776	181783.014372	57.442369
2596.037158	181580.554885	57.447373
2595.200015	181392.855228	57.452378
2594.561852	181183.792551	57.457383
2593.576244	180988.053363	57.462388
2593.010867	180789.933358	57.467393
2592.693444	180579.766974	57.472397
2591.596832	180386.439519	57.477402
2591.013576	180184.025672	57.482407
2590.655039	179983.408871	57.487412
2589.749862	179795.230843	57.492417
2589.175083	179591.292035	57.497421
2588.404913	179398.286184	57.502426
2587.761419	179195.479513	57.507431
2587.014466	178998.083423	57.512436
2586.242330	178806.823187	57.517441
2585.809166	178604.380322	57.522445
2584.878002	178411.048315	57.527450
2584.312183	178216.183823	57.532455
2583.857894	178013.734416	57.537460
2582.996019	177825.342029	57.542465
2582.171096	177622.419020	57.547469
2581.532722	177442.057070	57.552474
2581.195601	177243.586703	57.557479
2580.759662	177046.010569	57.562484
2579.728501	176848.516974	57.567489
2579.373064	176636.989770	57.572493
2578.399064	176447.731034	57.577498
2577.818517	176240.069975	57.582503
2577.179811	176046.435475	57.587508
2576.413831	175856.001780	57.592513
2575.808723	175667.362269	57.597517
2574.950771	175467.469408	57.602522
2574.454822	175269.809527	57.607527
2574.036398	175073.372027	57.612532
2573.433348	174879.750104	57.617537
2572.975398	174665.972657	57.622541
2571.901032	174468.115796	57.627546
2571.041785	174270.861733	57.632551
2570.710413	174074.415264	57.637556
2570.126307	173871.587064	57.642561
2569.358697	173678.047832	57.647565
2568.672456	173481.164478	57.652570
2568.130255	173280.164033	57.657575
2567.641889	173072.949663	57.662580
2566.619119	172879.251231	57.667585
2566.216083	172672.737620	57.672589
2565.117611	172468.179372	57.677594
2564.440091	172281.983532	57.682599
2564.103782	172072.333889	57.687604
2563.341785	171884.169341	57.692609
2562.844967	171675.984328	57.697613
2562.053658	171482.014403	57.702618
2561.367797	171282.115103	57.707623
2560.609796	171075.996727	57.712628
2559.941177	170878.869140	57.717633
2559.095481	170673.784164	57.722637
2558.313068	170481.445587	57.727642
2557.622499	170288.088750	57.732647
2557.474204	170089.331200	57.737652
2556.682073	169894.784291	57.742657
2556.401783	169695.108617	57.747661
2555.134975	169506.539544	57.752666
2554.742776	169298.121723	57.757671
2554.188585	169099.077507	57.762676
2553.645237	168911.236002	57.767681
2553.045845	168705.346694	57.772685
2552.116101	168501.494626	57.777690
2551.723007	168300.101894	57.782695
2551.008241	168102.665142	57.787700
2550.420659	167898.367859	57.792705
2549.798412	167691.978979	57.797709
2548.911667	167493.962258	57.802714
2548.335544	167287.390242	57.807719
2547.699691	167070.872133	57.812724
2546.690079	166881.372428	57.817729
2546.407846	166685.947215	57.822733
2545.746436	166486.196130	57.827738
2545.085218	166274.861979	57.832743
2544.600859	166071.168577	57.837748
2543.663281	165866.111240	57.842753
2543.130645	165660.240634	57.847757
2542.519104	165458.414491	57.852762
2541.840078	165260.910678	57.857767
2541.141443	165049.805558	57.862772
2540.448968	164851.975453	57.867777
2540.108224	164647.300720	57.872781
2539.359330	164438.915398	57.877786
2538.334637	164233.461292	57.882791
2537.668853	164024.721835	57.887796
2537.011191	163819.377172	57.892801
2536.610512	163611.996693	57.897805
2535.678536	163424.295132	57.902810
2534.945767	163205.335529	57.907815
2534.329839	163002.697081	57.912820
2533.507424	162802.190396	57.917825
2532.712459	162615.971612	57.922829
2532.452204	162350.279932	57.927834
2531.747672	162145.066569	57.932839
2531.389699	161936.417443	57.937844
2530.350707	161733.281004	57.942849
2529.860466	161534.216275	57.947853
2529.013424	161342.201947	57.952858
2528.230394	161139.206301	57.957863
2528.000367	160925.660584	57.962868
2526.967617	160730.691194	57.967873
2526.460487	160516.441724	57.972877
2525.826307	160316.427624	57.977882
2525.030086	160114.622280	57.982887
2524.236160	159917.509033	57.987892
2523.513492	159716.635103	57.992897
2523.374366	159507.240821	57.997901
2522.468620	159318.882768	58.002906
2521.639239	159121.538031	58.007911
2521.215512	158916.540313	58.012916
2520.207779	158715.145182	58.017921
2519.708781	158508.712479	58.022925
2519.088101	158319.691671	58.027930
2518.165813	158104.353062	58.032935
2517.617582	157911.648946	58.037940
2516.871980	157716.091376	58.042945
2516.346008	157504.736333	58.047949
2516.007306	157323.469138	58.052954
2515.233026	157116.147591	58.057959
2514.758528	156912.174010	58.062964
2513.912269	156710.993727	58.067969
2513.064451	156506.535081	58.072973
2512.545985	156302.038164	58.077978
2511.852602	156095.828619	58.082983
2511.010236	155900.080576	58.087988
2510.185600	155700.072309	58.092993
2509.885196	155498.469401	58.097997
2509.157233	155309.532940	58.103002
2508.351377	155114.355655	58.108007
2507.845122	154906.458392	58.113012
2506.813603	154709.908197	58.118017
2506.352930	154505.133243	58.123021
2505.628291	154312.451891	58.128026
2505.071586	154106.957303	58.133031
2504.849089	153901.563535	58.138036
2503.784959	153706.142958	58.143041
2503.477458	153500.892223	58.148045
2502.454547	153302.658286	58.153050
2501.577094	153102.444965	58.158055
2501.615968	152903.956123	58.163060
2500.905422	152707.544724	58.168065
2500.152215	152499.841310	58.173069
2499.162252	152296.917832	58.178074
2498.683966	152089.389494	58.183079
2497.887524	151886.971701	58.188084
2496.762729	151693.199508	58.193089
2496.228811	151490.907769	58.198093
2495.960468	151299.162919	58.203098
2495.097116	151103.395358	58.208103
2494.525988	150905.409196	58.213108
2493.404613	150708.388445	58.218113
2493.374824	150514.792811	58.223117
2492.565191	150311.713173	58.228122
2491.568289	150122.543710	58.233127
2491.130950	149912.645871	58.238132
2490.566713	149723.079694	58.243137
2490.001745	149513.916403	58.248141
2488.958179	149315.163227	58.253146
2488.558784	149118.075792	58.258151
2487.937170	148920.084280	58.263156
2487.198516	148731.886042	58.268161
2486.399932	148534.725638	58.273165
2485.897571	148341.179743	58.278170
2484.995412	148142.208035	58.283175
2484.345000	147942.702004	58.288180
2483.416091	147757.297498	58.293185
2483.215523	147552.028972	58.298189
2482.592304	147355.890151	58.303194
2481.647943	147159.409469	58.308199
2481.002518	146964.928713	58.313204
2480.537432	146777.067158	58.318209
2479.982995	146563.956343	58.323213
2479.240509	146377.882188	58.328218
2478.596696	146177.216998	58.333223
2477.736302	145966.509750	58.338228
2477.155226	145786.882004	58.343233
2476.553460	145583.392706	58.348237
2475.658307	145394.629015	58.353242
2475.045802	145197.383569	58.358247
2474.744571	145000.356889	58.363252
2474.002824	144808.827506	58.368257
2473.499768	144603.880229	58.373261
2472.555164	144407.886928	58.378266
2471.721168	144213.097254	58.383271
2471.087332	144017.463794	58.388276
2470.386595	143832.224119	58.393281
2469.990398	143639.821173	58.398285
2469.044447	143434.621417	58.403290
2468.644257	143245.766874	58.408295
2468.147189	143047.474769	58.413300
2467.535329	142853.713122	58.418305
2466.915843	142653.943528	58.423309
2466.062402	142454.174197	58.428314
2465.280824	142259.718907	58.433319
2464.603514	142064.765469	58.438324
2464.281180	141863.378292	58.443329
2463.363620	141665.428608	58.448333
2462.588827	141467.622760	58.453338
2462.025732	141267.154426	58.458343
2461.646650	141073.341739	58.463348
2460.924701	140876.420798	58.468353
2460.562336	140662.303611	58.473357
2459.829889	140473.772973	58.478362
2459.216453	140269.926703	58.483367
2458.492080	140052.237324	58.488372
2457.746152	139852.785684	58.493377
2456.932694	139649.636015	58.498381
2456.492565	139445.462916	58.503386
2455.916423	139238.466736	58.508391
2455.161122	139032.542229	58.513396
2454.120989	138839.750772	58.518401
2453.525800	138635.912701	58.523405
2452.846058	138440.995738	58.528410
2452.069998	138235.816918	58.533415
2451.374444	138024.096394	58.538420
2450.621381	137841.175781	58.543425
2450.434335	137645.665031	58.548429
2449.888725	137455.192665	58.553434
2448.870923	137244.951722	58.558439
2448.389216	137041.729138	58.563444
2447.726613	136851.634940	58.568449
2447.155345	136633.565141	58.573453
2446.730142	136441.974953	58.578458
2445.147339	136247.888933	58.583463
2445.087063	136046.003890	58.588468
2444.396100	135844.334553	58.593473
2443.543889	135631.055354	58.598477
2443.167401	135437.190016	58.603482
2442.174582	135242.508998	58.608487
2441.746760	135041.121097	58.613492
2441.333134	134839.554490	58.618497
2440.781546	134634.377950	58.623501
2439.882450	134433.843886	58.628506
2438.924090	134230.906975	58.633511
2438.550698	134020.460066	58.638516
2437.746807	133820.601143	58.643521
2437.153417	133625.473887	58.648525
2436.579386	133421.719565	58.653530
2435.755503	133222.693662	58.658535
2435.205944	133018.252369	58.663540
2434.268497	132821.952948	58.668545
2434.144231	132607.907432	58.673549
2433.276589	132412.488942	58.678554
2432.579849	132222.201891	58.683559
2432.176657	132008.649675	58.688564
2431.169270	131808.595724	58.693569
2430.743014	131601.147311	58.698573
2430.064609	131395.023299	58.703578
2429.075139	131196.075912	58.708583
2428.839679	130990.583236	58.713588
2427.897294	130794.324016	58.718593
2427.314652	130579.236006	58.723597
2426.759378	130374.116065	58.728602
2425.696917	130179.810814	58.733607
2425.659905	129973.455799	58.738612
2424.678070	129772.408831	58.743617
2423.758167	129557.191600	58.748621
2423.407847	129353.278659	58.753626
2422.747443	129152.566229	58.758631
2421.971525	128946.882077	58.763636
2420.775462	128755.630743	58.768641
2420.427568	128545.550705	58.773645
2420.217896	128343.045355	58.778650
2419.406261	128150.111562	58.783655
2418.595786	127928.463088	58.788660
2417.804227	127738.996218	58.793665
2417.393979	127538.116111	58.798669
2416.943608	127323.400584	58.803674
2415.831873	127129.264185	58.808679
2415.261686	126919.244458	58.813684
2414.444566	126734.678071	58.818689
2414.013038	126527.179353	58.823693
2413.573149	126319.810531	58.828698
2412.512445	126124.288892	58.833703
2411.931442	125914.380188	58.838708
2410.932281	125706.533211	58.843713
2410.494165	125505.278747	58.848717
2409.898838	125315.835633	58.853722
2409.516611	125117.076943	58.858727
2408.964125	124914.156000	58.863732
2407.987964	124716.027777	58.868737
2407.285059	124500.218900	58.873741
2407.098077	124296.000157	58.878746
2405.953781	124099.299987	58.883751
2405.439767	123890.793202	58.888756
2404.630114	123692.519120	58.893761
2403.889959	123488.660874	58.898765
2403.403792	123289.398801	58.903770
2402.763342	123089.375381	58.908775
2402.417053	122884.494224	58.913780
2401.582356	122684.695101	58.918785
2400.761461	122477.162236	58.923789
2400.337017	122274.075871	58.928794
2399.436865	122065.619141	58.933799
2398.907976	121862.146155	58.938804
2398.151672	121664.005666	58.943809
2397.690812	121460.931295	58.948813
2396.553021	121261.419490	58.953818
2395.751553	121052.726536	58.958823
2395.534677	120844.310766	58.963828
2394.562408	120657.398274	58.968833
2393.855517	120457.798842	58.973837
2393.260479	120256.151692	58.978842
2392.696780	120057.814983	58.983847
2392.156049	119851.020139	58.988852
2391.837397	119657.624710	58.993857
2390.939098	119457.130047	58.998861
2390.494040	119253.365572	59.003866
2389.746019	119050.291886	59.008871
2389.115129	118829.642379	59.013876
2388.058735	118630.455112	59.018881
2387.721276	118423.569533	59.023885
2387.051401	118218.744258	59.028890
2386.304040	118025.993892	59.033895
2385.647786	117811.203486	59.038900
2384.991260	117618.149759	59.043905
2384.299392	117405.920186	59.048909
2383.858786	117207.369893	59.053914
2382.788385	116997.507918	59.058919
2382.325446	116787.037190	59.063924
2381.518259	116593.443756	59.068929
2380.928092	116382.019002	59.073933
2380.559175	116180.831075	59.078938
2379.642817	115984.016018	59.083943
2379.235885	115773.976362	59.088948
2378.430530	115566.984832	59.093953
2378.048878	115368.807595	59.098957
2377.428154	115153.557785	59.103962
2376.614481	114944.770039	59.108967
2375.858111	114732.553850	59.113972
2374.959376	114534.801506	59.118977
2374.137706	114323.113214	59.123981
2373.724383	114112.136276	59.128986
2373.201920	113916.061827	59.133991
2372.721957	113712.023245	59.138996
2371.841637	113503.962475	59.144001
2371.370774	113294.296253	59.149005
2370.600764	113090.892601	59.154010
2369.679208	112888.288916	59.159015
2369.092246	112671.487328	59.164020
2368.390148	112463.635414	59.169025
2368.016577	112267.696212	59.174029
2367.317300	112061.852678	59.179034
2366.533048	111860.638118	59.184039
2365.939855	111652.052221	59.189044
2365.032106	111441.753693	59.194049
2364.623102	111229.937281	59.199053
2363.989733	111030.837847	59.204058
2362.957731	110827.030960	59.209063
2362.563881	110611.701703	59.214068
2361.684465	110409.295582	59.219073
2360.931968	110205.792192	59.224077
2360.578664	110004.892458	59.229082
2359.996023	109803.567482	59.234087
2359.527114	109591.654063	59.239092
2358.786507	109385.833025	59.244097
2358.177290	109176.521805	59.249101
2357.753974	108969.511737	59.254106
2356.848402	108754.768510	59.259111
2356.452334	108536.570579	59.264116
2355.570123	108329.073959	59.269121
2354.773031	108123.627863	59.274125
2354.135892	107903.379854	59.279130
2353.393613	107702.655903	59.284135
2352.832574	107486.841306	59.289140
2351.880755	107277.042365	59.294145
2351.572285	107073.456624	59.299149
2351.145172	106860.963907	59.304154
2350.057904	106648.311249	59.309159
2349.528957	106439.061661	59.314164
2348.949167	106229.752161	59.319169
2348.155810	106017.470894	59.324173
2347.348712	105805.333270	59.329178
2346.861278	105597.765797	59.334183
2346.479936	105381.142143	59.339188
2345.428391	105174.606802	59.344193
2344.670620	104966.110608	59.349197
2344.367528	104755.044405	59.354202
2343.551841	104553.457482	59.359207
2343.016211	104331.195890	59.364212
2342.137754	104128.207728	59.369217
2341.271746	103914.516526	59.374221
2340.826356	103727.907498	59.379226
2340.393059	103505.428058	59.384231
2339.817055	103286.703677	59.389236
2338.966690	103079.425093	59.394241
2338.070953	102863.185112	59.399245
2337.876143	102652.926153	59.404250
2337.275476	102447.148772	59.409255
2336.629879	102228.603849	59.414260
2335.873782	102013.910119	59.419265
2335.175419	101795.104821	59.424269
2334.570198	101573.064225	59.429274
2333.444374	101370.824174	59.434279
2333.445651	101152.402404	59.439284
2332.415738	100942.113604	59.444289
2331.833819	100723.648774	59.449293
2331.277930	100505.860608	59.454298
2330.508839	100292.738901	59.459303
2330.023353	100078.590977	59.464308
2329.737461	99865.358514	59.469313
2328.764491	99655.332415	59.474317
2328.176555	99437.870180	59.479322
2327.263102	99217.277424	59.484327
2326.738270	98975.033780	59.489332
2325.972236	98769.239047	59.494337
2325.624501	98551.341144	59.499341
2324.986703	98334.880370	59.504346
2323.985903	98117.578539	59.509351
2323.409607	97896.310728	59.514356
2322.911601	97678.000969	59.519361
2322.181518	97456.007039	59.524365
2321.502120	97246.210122	59.529370
2320.793191	97029.151426	59.534375
2320.373149	96795.508174	59.539380
2319.396611	96582.244500	59.544385
2318.662998	96363.756375	59.549389
2318.021962	96148.509199	59.554394
2317.249042	95935.701321	59.559399
2317.096085	95699.712134	59.564404
2316.119175	95488.938549	59.569409
2315.316474	95267.383430	59.574413
2314.485980	95056.616035	59.579418
2314.016256	94840.643871	59.584423
2313.587087	94609.599413	59.589428
2312.891376	94387.636463	59.594433
2312.309392	94185.113700	59.599437
2311.725537	93962.870870	59.604442
2310.953393	93738.307420	59.609447
2310.139784	93519.555194	59.614452
2309.342575	93299.775214	59.619457
2308.894837	93086.873009	59.624461
2308.231507	92870.411552	59.629466
2307.310326	92654.899880	59.634471
2307.079875	92429.217429	59.639476
2306.250832	92213.219852	59.644481
2305.613065	91993.142162	59.649485
2304.947181	91766.172206	59.654490
2304.090902	91552.620308	59.659495
2303.481992	91334.580013	59.664500
2302.894105	91117.274065	59.669505
2301.974855	90892.014553	59.674509
2301.346974	90672.037244	59.679514
2300.747283	90470.755912	59.684519
2300.058263	90239.417708	59.689524
2299.405457	90034.667882	59.694529
2298.834784	89810.740062	59.699533
2298.197630	89593.564802	59.704538
2297.597114	89376.645841	59.709543
2297.182154	89154.266093	59.714548
2296.087243	88945.874917	59.719553
2295.671547	88719.606905	59.724557
2294.958088	88491.518181	59.729562
2294.177914	88269.287821	59.734567
2293.863910	88053.103751	59.739572
2293.008773	87845.477597	59.744577
2292.543870	87621.111764	59.749581
2292.213778	87397.988470	59.754586
2291.245425	87175.222288	59.759591
2290.581570	86954.096430	59.764596
2289.765836	86720.013742	59.769601
2289.112844	86502.491610	59.774605
2288.427633	86281.166861	59.779610
2287.665289	86065.828204	59.784615
2287.436213	85835.649513	59.789620
2286.702981	85615.683163	59.794625
2285.858021	85392.725747	59.799629
2285.293028	85158.436526	59.804634
2284.518224	84938.832390	59.809639
2283.898207	84709.615289	59.814644
2283.152771	84500.032748	59.819649
2282.491298	84283.523412	59.824653
2281.502423	84051.893468	59.829658
2280.816629	83841.553675	59.834663
2280.585239	83613.662253	59.839668
2279.798629	83400.725023	59.844673
2279.015873	83180.703005	59.849677
2278.414816	82958.518449	59.854682
2277.653218	82735.899006	59.859687
2277.282301	82510.196639	59.864692
2276.403431	82292.379486	59.869697
2275.623240	82074.149646	59.874701
2275.238791	81847.664290	59.879706
2274.307982	81637.157211	59.884711
2273.702908	81414.837519	59.889716
2273.079289	81193.061846	59.894721
2272.401842	80982.064865	59.899725
2271.937763	80754.729374	59.904730
2271.219874	80537.367626	59.909735
2270.577502	80321.479153	59.914740
2269.681679	80104.378305	59.919745
2268.951417	79883.862964	59.924750
2268.487902	79661.336755	59.929754
2267.693919	79445.931393	59.934759
2267.133327	79220.795354	59.939764
2266.488098	79017.417869	59.944769
2265.492897	78791.842132	59.949774
2264.933646	78566.573604	59.954778
2264.494327	78351.890189	59.959783
2263.648242	78132.166024	59.964788
2263.200576	77923.248613	59.969793
2262.655493	77702.841287	59.974798
2262.172951	77480.379671	59.979802
2261.009889	77266.177259	59.984807
2260.704983	77036.398885	59.989812
2259.954845	76819.791149	59.994817
2259.188443	76601.528161	59.999822
2258.379087	76378.832568	60.004826
2257.461566	76162.822298	60.009831
2257.116379	75949.625517	60.014836
2256.297758	75736.607441	60.019841
2255.929857	75517.747977	60.024846
2255.329052	75302.913146	60.029850
2254.726430	75078.310912	60.034855
2253.925144	74852.836658	60.039860
2253.351818	74635.216795	60.044865
2252.486606	74419.558957	60.049870
2251.848986	74194.148472	60.054874
2251.272275	73987.313052	60.059879
2250.936787	73760.712764	60.064884
2250.334794	73545.846158	60.069889
2249.562647	73325.750495	60.074894
2248.920249	73095.709280	60.079898
2247.943552	72884.938434	60.084903
2247.099120	72652.267239	60.089908
2246.659226	72434.827452	60.094913
2245.736701	72216.535340	60.099918
2245.350135	71995.962387	60.104922
2244.476293	71781.582312	60.109927
2244.166520	71554.261779	60.114932
2243.210605	71342.129311	60.119937
2242.935167	71125.418910	60.124942
2242.665230	70893.487999	60.129946
2241.367806	70676.520194	60.134951
2241.046410	70452.425739	60.139956
2240.136179	70229.358375	60.144961
2239.268975	69999.350656	60.149966
2238.777207	69783.538075	60.154970
2238.010624	69572.680423	60.159975
2237.224421	69352.105317	60.164980
2236.645857	69138.815545	60.169985
2236.192864	68921.885153	60.174990
2235.831241	68689.259992	60.179994
2234.742668	68482.860835	60.184999
2234.183921	68257.726963	60.190004
2233.350640	68035.261367	60.195009
2232.713788	67816.389964	60.200014
2232.380470	67594.128774	60.205018
2231.663176	67374.413737	60.210023
2230.893720	67147.951746	60.215028
2230.139708	66930.660564	60.220033
2229.513723	66712.262193	60.225038
2229.005221	66477.422603	60.230042
2228.517795	66262.002910	60.235047
2227.549114	66037.491751	60.240052
2226.900943	65818.296360	60.245057
2225.887201	65604.474722	60.250062
2225.657304	65370.826630	60.255066
2224.666559	65157.870727	60.260071
2224.390979	64937.090573	60.265076
2223.629173	64719.784342	60.270081
2222.254395	64501.393624	60.275086
2221.962327	64279.309654	60.280090
2221.161264	64072.044399	60.285095
2220.492479	63858.472440	60.290100
2220.224490	63641.866312	60.295105
2219.521509	63418.128822	60.300110
2218.610682	63205.641030	60.305114
2217.780564	63000.487933	60.310119
2217.291759	62778.477946	60.315124
2216.751534	62566.134795	60.320129
2215.849745	62357.520646	60.325134
2215.281948	62138.753547	60.330138
2214.295190	61928.042806	60.335143
2213.867284	61719.601109	60.340148
2213.173251	61509.921792	60.345153
2212.575985	61296.383102	60.350158
2211.858387	61094.246551	60.355162
2211.124960	60872.275547	60.360167
2210.649328	60662.289260	60.365172
2210.130517	60448.861685	60.370177
2209.096509	60243.447940	60.375182
2208.753117	60027.825756	60.380186
2207.913159	59818.292881	60.385191
2207.340035	59603.284969	60.390196
2206.635469	59391.475270	60.395201
2205.952436	59184.612017	60.400206
2205.543849	58976.384410	60.405210
2204.030350	58765.675551	60.410215
2203.714878	58546.596842	60.415220
2203.047043	58346.786326	60.420225
2202.242798	58149.572891	60.425230
2201.699501	57934.497174	60.430234
2201.219095	57733.694976	60.435239
2200.306130	57520.929923	60.440244
2199.602685	57315.008555	60.445249
2199.061757	57121.407242	60.450254
2198.290587	56906.053603	60.455258
2197.387082	56705.912017	60.460263
2196.949309	56503.774454	60.465268
2196.430292	56298.908049	60.470273
2195.363991	56107.565476	60.475278
2194.881522	55895.538891	60.480282
2194.323784	55704.911029	60.485287
2193.506372	55497.698813	60.490292
2192.799840	55299.028694	60.495297
2191.895869	55106.550488	60.500302
2191.303783	54903.511916	60.505306
2190.406228	54719.483165	60.510311
2190.021280	54518.735652	60.515316
2189.282851	54318.976789	60.520321
2188.074281	54134.221631	60.525326
2187.581805	53943.044798	60.530330
2186.760145	53752.988604	60.535335
2186.248263	53568.065374	60.540340
2185.214858	53385.242459	60.545345
2184.686542	53202.695662	60.550350
2184.107753	53022.139562	60.555354
2182.848203	52845.854274	60.560359
2182.249430	52671.177731	60.565364
2181.473967	52495.689221	60.570369
2180.652012	52331.812852	60.575374
2180.147990	52155.056879	60.580378
2179.405177	51995.217959	60.585383
2178.597105	51826.604107	60.590388
2177.832060	51662.284972	60.595393
2177.176202	51508.422986	60.600398
2176.445272	51343.753298	60.605402
2175.427809	51179.472282	60.610407
2174.827040	51026.035980	60.615412
2174.161732	50871.497522	60.620417
2173.320717	50722.809850	60.625422
2172.962258	50564.026857	60.630426
2171.875946	50410.223574	60.635431
2171.353430	50269.689824	60.640436
2170.542848	50116.857739	60.645441
2169.804483	49968.527037	60.650446
2169.234489	49824.210955	60.655450
2168.484198	49680.193557	60.660455
2167.607758	49535.798707	60.665460
2167.273372	49390.642005	60.670465
2166.041773	49246.131843	60.675470
2165.502553	49102.784783	60.680474
2164.836486	48971.385743	60.685479
2163.833636	48842.695339	60.690484
2163.287650	48703.357648	60.695489
2162.465914	48570.015379	60.700494
2162.236470	48436.111946	60.705498
2161.432392	48301.060605	60.710503
2160.785975	48177.474935	60.715508
2160.308044	48043.316520	60.720513
2159.410998	47922.100675	60.725518
2158.557049	47788.791530	60.730522
2158.052370	47656.373821	60.735527
2157.551517	47531.304926	60.740532
2156.799814	47395.173481	60.745537
2155.738624	47265.488356	60.750542
2155.375164	47138.783998	60.755546
2154.493442	47013.804496	60.760551
2153.830770	46886.744522	60.765556
2153.085500	46760.302739	60.770561
2152.565422	46646.874244	60.775566
2152.219356	46521.367240	60.780570
2151.312919	46401.330527	60.785575
2150.669845	46269.634737	60.790580
2149.963805	46146.363739	60.795585
2149.379649	46028.666571	60.800590
2148.933295	45891.796089	60.805594
2148.527684	45773.297358	60.810599
2147.528936	45641.102854	60.815604
2147.110015	45524.005963	60.820609
2145.863400	45406.313693	60.825614
2145.303578	45274.305353	60.830618
2144.362629	45160.956388	60.835623
2143.898126	45040.352804	60.840628
2143.341446	44916.114726	60.845633
2142.406088	44807.457698	60.850638
2142.367347	44680.668934	60.855642
2141.568785	44560.618223	60.860647
2140.761538	44439.968788	60.865652
2140.142099	44320.735771	60.870657
2139.537845	44205.407142	60.875662
2139.070413	44086.142124	60.880666
2138.304188	43965.312353	60.885671
2137.663351	43846.607820	60.890676
2137.059622	43710.478330	60.895681
2136.140333	43597.572535	60.900686
2135.753689	43464.174667	60.905690
2134.962239	43350.310903	60.910695
2134.432246	43231.381092	60.915700
2133.902655	43108.090889	60.920705
2133.010812	42990.554732	60.925710
2132.418051	42866.001778	60.930714
2131.537024	42745.233499	60.935719
2131.074389	42626.885367	60.940724
2130.320225	42494.742348	60.945729
2129.307506	42382.068016	60.950734
2129.057750	42265.298247	60.955738
2128.172373	42143.023244	60.960743
2127.959731	42038.224994	60.965748
2127.109861	41914.096008	60.970753
2126.383068	41795.580442	60.975758
2125.837948	41667.094667	60.980762
2125.241115	41550.021142	60.985767
2124.750071	41427.204823	60.990772
2123.912763	41299.719980	60.995777
2122.706862	41183.261028	61.000782
2122.354742	41068.327536	61.005786
2121.662855	40956.405328	61.010791
2121.011072	40834.402959	61.015796
2120.308068	40718.689517	61.020801
2119.529293	40613.929680	61.025806
2119.292029	40483.275821	61.030810
2118.425454	40374.540861	61.035815
2117.939846	40253.543919	61.040820
2117.548644	40127.777213	61.045825
2116.542279	40013.770387	61.050830
2115.965597	39891.886127	61.055834
2115.289454	39776.185857	61.060839
2114.804865	39655.543955	61.065844
2113.907748	39526.817026	61.070849
2113.403610	39419.537269	61.075854
2113.036419	39286.193962	61.080858
2111.715111	39175.842457	61.085863
2111.094921	39055.479258	61.090868
2110.478574	38928.672608	61.095873
2109.904095	38823.516665	61.100878
2109.467236	38695.028099	61.105882
2108.577683	38583.053201	61.110887
2107.903418	38463.946897	61.115892
2107.320534	38342.142677	61.120897
2106.660638	38224.422162	61.125902
2106.061380	38108.042853	61.130906
2105.408127	37994.657457	61.135911
2104.982429	37866.174969	61.140916
2104.398323	37753.752396	61.145921
2103.235520	37629.836965	61.150926
2102.873118	37509.307872	61.155930
2102.253407	37397.675786	61.160935
2101.678314	37278.497264	61.165940
2101.027593	37151.303103	61.170945
2099.729545	37032.802186	61.175950
2099.547764	36911.989454	61.180954
2098.429484	36798.252755	61.185959
2097.711157	36692.197097	61.190964
2097.353203	36571.214012	61.195969
2096.540221	36470.967907	61.200974
2096.115254	36341.429949	61.205978
2095.133027	36222.394620	61.210983
2094.903167	36110.013716	61.215988
2094.280353	35990.635322	61.220993
2093.911362	35876.382902	61.225998
2093.127121	35742.634200	61.231002
2091.931808	35633.735234	61.236007
2091.196346	35517.422272	61.241012
2090.725821	35393.767491	61.246017
2089.855511	35283.496305	61.251022
2089.308834	35175.150159	61.256026
2088.581434	35057.906591	61.261031
2087.933142	34945.282194	61.266036
2087.203605	34826.908937	61.271041
2086.752684	34713.608355	61.276046
2086.465453	34592.482897	61.281050
2085.384188	34486.016727	61.286055
2084.644886	34368.704019	61.291060
2084.545682	34257.923701	61.296065
2083.568377	34145.333198	61.301070
2082.734052	34025.651520	61.306074
2082.414890	33912.267509	61.311079
2081.637919	33790.135100	61.316084
2080.750800	33674.157729	61.321089
2079.876186	33561.134497	61.326094
2079.498476	33441.403527	61.331098
2078.718476	33341.401677	61.336103
2078.152430	33224.330296	61.341108
2077.728799	33104.760750	61.346113
2077.007225	32993.183651	61.351118
2076.389335	32877.121712	61.356122
2075.202253	32762.250801	61.361127
2074.897479	32648.365847	61.366132
2074.063649	32541.784370	61.371137
2073.385489	32432.007265	61.376142
2073.022830	32313.897080	61.381146
2072.137609	32196.390564	61.386151
2071.480536	32089.077582	61.391156
2070.847694	31970.698253	61.396161
2070.158121	31868.235270	61.401166
2069.599406	31750.127038	61.406170
2069.066148	31631.601600	61.411175
2068.487804	31512.597469	61.416180
2067.558387	31397.063088	61.421185
2066.579748	31302.335469	61.426190
2065.993739	31183.080528	61.431194
2065.238917	31083.837329	61.436199
2064.513745	30969.694087	61.441204
2064.425108	30848.572348	61.446209
2063.752566	30750.378367	61.451214
2062.967417	30624.562102	61.456218
2062.375117	30522.371735	61.461223
2061.724327	30408.122623	61.466228
2061.192383	30284.534618	61.471233
2060.493068	30183.158120	61.476238
2059.978727	30060.423822	61.481242
2059.250346	29943.689044	61.486247
2058.154840	29831.020302	61.491252
2057.773154	29716.802825	61.496257
2056.834626	29607.694183	61.501262
2056.340416	29490.127577	61.506266
2055.422211	29384.011289	61.511271
2054.773434	29272.398872	61.516276
2054.157344	29168.171508	61.521281
2053.347753	29063.850701	61.526286
2052.882431	28951.313953	61.531290
2052.281338	28845.639044	61.536295
2051.424447	28740.466750	61.541300
2050.960606	28626.949296	61.546305
2050.122820	28514.104976	61.551310
2049.408507	28409.912266	61.556314
2048.893883	28302.064295	61.561319
2047.740804	28200.479841	61.566324
2047.431332	28096.335484	61.571329
2046.258516	28001.539317	61.576334
2045.932496	27894.335555	61.581338
2045.354084	27801.871275	61.586343
2044.431180	27690.493307	61.591348
2044.168468	27581.793372	61.596353
2043.383731	27479.309783	61.601358
2042.758920	27372.126871	61.606362
2041.851660	27277.719338	61.611367
2040.948435	27181.583448	61.616372
2040.568197	27072.764979	61.621377
2039.612767	26986.338251	61.626382
2038.872778	26884.876582	61.631386
2038.395983	26796.063753	61.636391
2037.560158	26696.011012	61.641396
2036.967619	26602.503729	61.646401
2036.316861	26509.676021	61.651406
2035.667935	26412.201098	61.656410
2034.849648	26321.867750	61.661415
2034.527747	26226.605736	61.666420
2034.109994	26119.639961	61.671425
2032.766784	26029.359176	61.676430
2032.291092	25933.912416	61.681434
2031.872333	25846.614433	61.686439
2030.970256	25750.725414	61.691444
2030.191768	25657.656719	61.696449
2029.206490	25575.932975	61.701454
2028.634643	25470.517923	61.706458
2027.882577	25389.957031	61.711463
2027.256292	25303.885943	61.716468
2026.901168	25206.477526	61.721473
2025.687043	25135.797247	61.726478
2025.400901	25047.039624	61.731482
2024.947558	24968.414996	61.736487
2024.268073	24867.944447	61.741492
2023.557347	24785.430086	61.746497
2022.887080	24703.513108	61.751502
2022.674507	24617.707005	61.756506
2021.685014	24523.078331	61.761511
2020.707164	24430.826305	61.766516
2020.388720	24339.140650	61.771521
2019.681490	24248.861363	61.776526
2019.360304	24157.584690	61.781530
2018.541214	24066.753995	61.786535
2017.756126	23981.303569	61.791540
2017.335135	23880.587338	61.796545
2016.199980	23791.668168	61.801550
2015.710760	23704.314062	61.806554
2015.060491	23625.921557	61.811559
2014.153566	23530.058456	61.816564
2013.626784	23443.367197	61.821569
2012.741316	23361.270143	61.826574
2012.369918	23277.961873	61.831578
2011.743766	23192.435174	61.836583
2010.828976	23104.150577	61.841588
2010.353017	23012.366456	61.846593
2009.605887	22928.242316	61.851598
2008.647185	22844.002954	61.856602
2007.954936	22766.133054	61.861607
2007.097622	22687.698277	61.866612
2006.830477	22605.235348	61.871617
2005.821070	22534.715741	61.876622
2005.004272	22446.172878	61.881626
2004.603451	22375.600029	61.886631
2003.952289	22294.272006	61.891636
2003.657098	22213.682279	61.896641
2002.785657	22137.318164	61.901646
2002.123000	22055.918173	61.906650
2001.257068	21967.471064	61.911655
2000.661804	21899.613559	61.916660
2000.224373	21819.524556	61.921665
1999.365396	21747.437717	61.926670
1998.889289	21661.571713	61.931674
1998.337556	21577.782213	61.936679
1997.501072	21506.637273	61.941684
1997.073569	21432.775473	61.946689
1995.881351	21356.205478	61.951694
1995.439147	21272.122276	61.956698
1994.731555	21193.233710	61.961703
1993.963908	21118.460911	61.966708
1993.560845	21026.339571	61.971713
1992.983218	20963.692150	61.976718
1992.334244	20879.764663	61.981722
1991.772929	20798.036081	61.986727
1990.924069	20726.958211	61.991732
1990.321912	20637.116269	61.996737
1989.489178	20560.371494	62.001742
1988.959113	20485.690319	62.006746
1988.366318	20409.805128	62.011751
1987.287946	20332.119045	62.016756
1986.755974	20256.592868	62.021761
1985.943212	20186.496271	62.026766
1985.579157	20100.315037	62.031770
1984.731811	20032.005808	62.036775
1984.229966	19966.473676	62.041780
1983.233929	19874.714922	62.046785
1982.555319	19808.893328	62.051790
1982.436906	19731.168385	62.056794
1981.626944	19656.872304	62.061799
1980.503343	19581.549075	62.066804
1980.232165	19500.294370	62.071809
1979.676155	19421.860387	62.076814
1978.954455	19358.231676	62.081818
1978.301905	19290.458462	62.086823
1977.682708	19210.280525	62.091828
1977.047310	19132.778371	62.096833
1976.293272	19058.796784	62.101838
1975.638364	18979.618075	62.106842
1974.775479	18908.703044	62.111847
1974.278180	18835.719130	62.116852
1973.558150	18751.482725	62.121857
1972.724770	18687.131192	62.126862
1972.266525	18608.109463	62.131866
1971.526739	18537.574071	62.136871
1970.920825	18461.692897	62.141876
1970.070142	18389.836866	62.146881
1969.130072	18332.184437	62.151886
1968.994061	18255.526283	62.156890
1968.089974	18188.362228	62.161895
1967.408453	18110.199477	62.166900
1966.802889	18036.943209	62.171905
1966.006005	17975.478531	62.176910
1965.420174	17900.454614	62.181914
1964.910867	17828.849729	62.186919
1964.201950	17760.978429	62.191924
1963.601237	17686.643908	62.196929
1962.501771	17616.233725	62.201934
1962.091440	17540.910944	62.206938
1961.631533	17473.216882	62.211943
1960.748753	17409.466183	62.216948
1960.487954	17335.053732	62.221953
1959.645994	17271.331460	62.226958
1959.103187	17201.777330	62.231962
1958.317941	17125.250687	62.236967
1957.660876	17061.355471	62.241972
1956.907258	16975.038996	62.246977
1956.343746	16913.754215	62.251982
1955.761399	16839.144555	62.256986
1955.065068	16773.524290	62.261991
1954.131319	16708.334304	62.266996
1953.735316	16629.467460	62.272001
1952.939225	16564.423967	62.277006
1952.414710	16489.070148	62.282010
1951.785046	16418.694830	62.287015
1951.121896	16352.198067	62.292020
1950.483862	16276.395221	62.297025
1949.922624	16207.334715	62.302030
1948.586470	16140.804598	62.307034
1948.345525	16065.719022	62.312039
1947.384073	16008.210452	62.317044
1947.023756	15942.790592	62.322049
1946.186227	15876.859901	62.327054
1945.536746	15810.941475	62.332058
1945.153144	15733.947316	62.337063
1944.262534	15677.231861	62.342068
1943.987812	15592.105048	62.347073
1943.365339	15531.517263	62.352078
1942.532350	15458.745177	62.357082
1942.077121	15375.951581	62.362087
1941.273999	15313.546775	62.367092
1940.437723	15232.654670	62.372097
1939.662736	15167.000246	62.377102
1938.961607	15100.660628	62.382106
1938.398515	15039.485626	62.387111
1937.652903	14972.452646	62.392116
1937.013185	14898.054153	62.397121
1936.318249	14842.346239	62.402126
1935.687828	14766.993272	62.407130
1934.982838	14706.535489	62.412135
1934.251493	14644.781037	62.417140
1933.692143	14573.594585	62.422145
1932.850815	14508.554129	62.427150
1932.643241	14444.809817	62.432154
1931.828956	14380.666140	62.437159
1931.025594	14308.100595	62.442164
1930.840456	14237.856361	62.447169
1930.195644	14178.102111	62.452174
1929.176756	14114.105087	62.457178
1928.499445	14037.380613	62.462183
1927.980121	13969.312099	62.467188
1927.568192	13897.213389	62.472193
1926.636313	13835.111854	62.477198
1925.974126	13757.356948	62.482202
1925.389106	13683.264344	62.487207
1924.582784	13625.864867	62.492212
1923.782874	13549.387422	62.497217
1923.274615	13486.449695	62.502222
1922.423266	13414.830118	62.507226
1922.024319	13357.448958	62.512231
1921.271973	13285.145234	62.517236
1920.653872	13218.101265	62.522241
1920.121318	13152.636281	62.527246
1919.322200	13089.369506	62.532250
1918.990944	13011.904019	62.537255
1918.111442	12951.748106	62.542260
1917.479248	12871.722700	62.547265
1916.563995	12808.902983	62.552270
1915.757093	12743.095336	62.557274
1915.778449	12676.116774	62.562279
1914.739476	12602.743061	62.567284
1914.045100	12530.753022	62.572289
1913.329738	12473.696488	62.577294
1912.532803	12390.945248	62.582298
1912.087504	12322.635676	62.587303
1911.256508	12270.263447	62.592308
1910.830070	12195.872154	62.597313
1909.966503	12133.518921	62.602318
1909.360797	12069.642637	62.607322
1908.772035	12002.584563	62.612327
1908.050412	11935.071645	62.617332
1907.321071	11861.143179	62.622337
1906.633091	11804.508565	62.627342
1905.950816	11726.116388	62.632346
1905.504559	11657.420137	62.637351
1904.480382	11601.731143	62.642356
1903.988819	11529.229142	62.647361
1903.312592	11476.675882	62.652366
1902.386972	11409.102408	62.657370
1902.105661	11342.858547	62.662375
1901.189564	11283.354507	62.667380
1900.478933	11211.118824	62.672385
1899.731249	11157.553396	62.677390
1899.148510	11089.558611	62.682394
1899.179213	11030.282629	62.687399
1898.111965	10976.215833	62.692404
1897.730472	10906.249998	62.697409
1897.020477	10834.329270	62.702414
1896.280172	10763.368059	62.707418
1895.489694	10702.224261	62.712423
1895.071040	10636.108265	62.717428
1894.490969	10557.233664	62.722433
1893.634814	10499.430493	62.727438
1892.790540	10423.633193	62.732442
1892.293711	10363.553930	62.737447
1891.131259	10291.429089	62.742452
1891.110992	10230.685287	62.747457
1890.280556	10162.677382	62.752462
1889.435511	10086.208467	62.757466
1888.856820	10023.394210	62.762471
1887.759679	9961.658261	62.767476
1887.571258	9892.753727	62.772481
1886.725925	9837.983151	62.777486
1886.092507	9770.669454	62.782490
1885.663240	9699.449256	62.787495
1884.811326	9643.427105	62.792500
1884.381864	9565.012701	62.797505
1883.392217	9504.720018	62.802510
1882.734535	9442.342835	62.807514
1882.192010	9383.484251	62.812519
1881.204306	9320.272758	62.817524
1880.764922	9247.543827	62.822529
1879.915888	9202.195366	62.827534
1879.075332	9136.514278	62.832538
1878.927992	9077.833602	62.837543
1877.779215	9020.766607	62.842548
1877.615414	8956.426613	62.847553
1876.950612	8894.267039	62.852558
1876.589336	8827.492664	62.857562
1875.932927	8765.114146	62.862567
1874.888180	8694.101752	62.867572
1874.452921	8627.022857	62.872577
1873.744357	8567.494039	62.877582
1873.035355	8497.394542	62.882586
1872.406813	8430.914063	62.887591
1871.426750	8365.604450	62.892596
1870.851507	8300.812684	62.897601
1870.224460	8242.075740	62.902606
1869.862556	8176.909032	62.907610
1869.218546	8110.783501	62.912615
1868.359838	8050.229739	62.917620
1867.767955	7981.945920	62.922625
1866.999789	7921.606694	62.927630
1866.122171	7852.260024	62.932634
1865.859794	7787.433823	62.937639
1865.072976	7733.515238	62.942644
1864.553971	7660.366834	62.947649
1864.028172	7595.018048	62.952654
1863.058886	7529.709983	62.957658
1862.640372	7456.680732	62.962663
1861.704654	7399.851560	62.967668
1861.054950	7333.048387	62.972673
1860.169795	7268.938244	62.977678
1859.374929	7217.275038	62.982682
1858.958496	7155.474930	62.987687
1858.100679	7105.538682	62.992692
1857.781306	7024.690777	62.997697
1856.849969	6976.886302	63.002702
1856.390309	6906.287283	63.007706
1855.776904	6852.589291	63.012711
1854.655799	6788.867352	63.017716
1854.636519	6718.536138	63.022721
1853.699362	6660.850965	63.027726
1852.968745	6598.068094	63.032730
1852.614313	6539.765503	63.037735
1851.696309	6475.562235	63.042740
1850.850549	6415.546706	63.047745
1850.608881	6355.609834	63.052750
1849.747937	6289.264540	63.057754
1849.310431	6225.100441	63.062759
1848.216588	6175.103039	63.067764
1847.875361	6109.925510	63.072769
1847.239121	6047.181255	63.077774
1846.139090	5992.224636	63.082778
1845.756532	5919.748587	63.087783
1845.114035	5870.246910	63.092788
1844.705052	5804.723363	63.097793
1843.861590	5740.669988	63.102798
1843.343940	5680.587983	63.107802
1842.924608	5607.652332	63.112807
1841.976834	5544.952569	63.117812
1841.562729	5472.221049	63.122817
1840.707116	5417.245110	63.127822
1839.828161	5354.563622	63.132826
1839.402491	5283.757890	63.137831
1838.584190	5235.952127	63.142836
1837.892901	5168.654169	63.147841
1837.386647	5110.695224	63.152846
1836.779374	5038.479227	63.157850
1835.893069	4975.737412	63.162855
1834.968094	4916.030010	63.167860
1834.850303	4860.741800	63.172865
1833.850290	4794.247031	63.177870
1833.119011	4737.009122	63.182874
1832.711572	4676.697577	63.187879
1832.277241	4615.305253	63.192884
1831.800985	4542.521917	63.197889
1830.796212	4480.153583	63.202894
1830.250196	4415.059408	63.207898
1829.580438	4343.923868	63.212903
1828.786742	4292.642953	63.217908
1828.018660	4221.914029	63.222913
1827.609819	4158.758363	63.227918
1826.444957	4101.146150	63.232922
1825.823883	4045.548919	63.237927
1824.903556	3980.157241	63.242932
1824.509968	3922.623588	63.247937
1823.772082	3864.237834	63.252942
1823.086762	3811.114777	63.257946
1822.832591	3744.613578	63.262951
1821.973169	3694.347605	63.267956
1821.343737	3623.979684	63.272961
1820.586446	3566.932638	63.277966
1819.796326	3517.807734	63.282970
1819.126493	3444.372048	63.287975
1818.631247	3390.448222	63.292980
1818.274850	3327.159243	63.297985
1817.352350	3278.874004	63.302990
1816.661878	3224.869008	63.307994
1816.340143	3155.887460	63.312999
1815.130632	3098.033119	63.318004
1814.485321	3045.534245	63.323009
1813.919798	2984.509460	63.328014
1813.192052	2929.578503	63.333018
1812.798898	2862.080495	63.338023
1811.873392	2808.419557	63.343028
1811.381602	2752.424203	63.348033
1810.614087	2695.974433	63.353038
1809.887164	2637.329206	63.358042
1809.252854	2570.073513	63.363047
1808.494548	2529.027896	63.368052
1807.815863	2467.221208	63.373057
1807.588578	2414.964198	63.378062
1806.438269	2353.669773	63.383066
1806.116711	2298.818633	63.388071
1805.312689	2248.419495	63.393076
1804.971278	2184.327901	63.398081
1804.187046	2128.297781	63.403086
1803.334866	2071.612302	63.408090
1802.713947	2005.961870	63.413095
1801.794430	1954.570323	63.418100
1801.207433	1894.959546	63.423105
1800.189200	1837.735140	63.428110
1799.440101	1784.691070	63.433114
1799.399262	1730.211489	63.438119
1798.558437	1686.328273	63.443124
1798.257361	1627.312720	63.448129
1797.244027	1574.561353	63.453134
1796.446151	1524.916824	63.458138
1796.306135	1474.658583	63.463143
1795.140872	1419.943933	63.468148
1794.717259	1369.347850	63.473153
1793.605865	1314.795370	63.478158
1793.174656	1261.986602	63.483162
1792.579191	1213.392887	63.488167
1791.839825	1158.148710	63.493172
1791.187267	1096.208838	63.498177
1790.593520	1056.260970	63.503182
1789.730750	1005.769008	63.508186
1789.333796	937.899623	63.513191
1788.781258	892.320254	63.518196
1787.993570	845.417366	63.523201
1787.343641	780.772972	63.528206
1786.456095	732.277714	63.533210
1785.944613	678.807256	63.538215
1784.986737	635.784787	63.543220
1784.376282	589.363965	63.548225
1783.823575	537.207935	63.553230
1783.042563	497.084754	63.558234
1782.506132	430.884719	63.563239
1781.439816	401.798911	63.568244
1780.941021	359.092306	63.573249
1780.381951	309.109646	63.578254
1779.478296	270.738905	63.583258
1778.668961	226.139146	63.588263
1777.758071	181.899435	63.593268
1777.175836	143.945565	63.598273
1776.489381	111.635011	63.603278
1775.569726	81.320170	63.608282
1775.140392	32.002272	63.613287
1774.287300	16.923169	63.618292
1773.227621	-25.866695	63.623297
1772.283967	-44.123129	63.628302
1771.310415	-57.631289	63.633306
1770.369999	-60.804563	63.638311
1766.363885	25.065153	63.643316
1764.425260	69.211355	63.648321
1765.552628	78.082621	63.653326
1766.224092	71.970896	63.658330
1766.683090	68.911247	63.663335
1766.490232	66.324133	63.668340
1766.410840	54.686088	63.673345
1765.704793	60.253010	63.678350
1763.490546	75.237455	63.683354
1762.769747	68.856400	63.688359
1761.743924	75.989587	63.693364
1761.551010	74.120006	63.698369
1761.586009	75.740348	63.703374
1760.878556	77.857076	63.708378
1760.282845	76.653869	63.713383
1759.289568	85.043474	63.718388
1758.851009	81.604387	63.723393
1758.255290	78.554541	63.728398
1757.181223	82.707024	63.733402
1756.636854	71.123889	63.738407
1755.902341	74.344068	63.743412
1755.755449	77.008870	63.748417
1755.175000	82.040184	63.753422
1754.257367	84.439457	63.758426
1753.763046	81.277313	63.763431
1752.855665	86.876223	63.768436
1752.061133	82.478097	63.773441
1751.663856	81.415268	63.778446
1751.288429	78.445558	63.783450
1750.663720	78.809742	63.788455
1749.980077	84.240652	63.793460
1749.206550	91.094080	63.798465
1748.745774	85.176360	63.803470
1747.721227	84.910177	63.808474
1746.964785	78.996838	63.813479
1745.991065	82.226626	63.818484
1745.646780	78.264783	63.823489
1744.956911	77.565397	63.828494
1744.547303	84.610188	63.833498
1744.493764	76.246559	63.838503
1743.138616	82.799691	63.843508
1742.679269	80.360558	63.848513
1742.382972	81.066831	63.853518
1741.028006	82.381218	63.858522
1740.953996	75.090032	63.863527
1740.147474	88.335456	63.868532
1739.081836	74.307219	63.873537
1738.683909	77.402981	63.878542
1737.511480	87.938927	63.883546
1737.399675	78.023344	63.888551
1736.392864	77.210292	63.893556
1735.713112	81.214999	63.898561
1734.931188	82.189215	63.903566
1734.298631	80.203378	63.908570
1734.494888	83.914412	63.913575
1733.872111	90.819595	63.918580
1732.608034	85.557750	63.923585
1732.107506	75.692869	63.928590
1731.615228	85.147795	63.933594
1730.944919	82.989756	63.938599
1729.772080	83.013642	63.943604
1729.671636	85.213746	63.948609
1729.082703	83.295099	63.953614
1727.981939	88.924731	63.958618
1727.930106	84.850207	63.963623
1726.541972	87.966047	63.968628
1726.058643	88.881803	63.973633
1725.872747	72.709509	63.978638
1724.665729	84.656035	63.983642
1724.601888	78.191147	63.988647
1723.448129	74.337376	63.993652
1722.750428	80.677284	63.998657
1722.379945	77.192699	64.003662
1721.530050	83.324966	64.008666
1721.127368	81.222195	64.013671
1719.992496	75.618135	64.018676
1719.711823	82.040044	64.023681
1719.367740	75.373660	64.028686
1717.609391	88.106359	64.033690
1717.673416	76.297290	64.038695
1717.170181	83.090444	64.043700
1716.596609	87.292761	64.048705
1715.590693	76.610856	64.053710
1714.907295	87.535920	64.058714
1714.532924	85.608429	64.063719
1713.770567	87.675543	64.068724
1712.855826	78.606597	64.073729
1712.340065	76.958612	64.078734
1711.462156	80.712519	64.083738
1711.480009	85.213566	64.088743
1710.240562	84.101578	64.093748
1709.637025	82.598423	64.098753
1709.178156	85.211854	64.103758
1708.414356	82.647618	64.108762
1707.897474	80.227093	64.113767
1706.746425	84.945340	64.118772
1706.431629	86.971330	64.123777
1706.309539	80.201877	64.128782
1705.150861	82.152166	64.133786
1704.761623	84.076438	64.138791
1703.954203	90.254005	64.143796
1703.276920	92.619851	64.148801
1702.641086	81.465999	64.153806
1702.051614	85.521031	64.158810
1701.628228	78.070873	64.163815
1700.625234	83.705483	64.168820
1700.120291	77.583478	64.173825
1699.067247	91.703866	64.178830
1698.234943	88.855618	64.183834
1698.022019	81.258487	64.188839
1697.297478	77.931071	64.193844
1696.418996	80.820891	64.198849
1695.667245	79.439055	64.203854
1695.583903	81.959723	64.208858
1694.669352	72.155888	64.213863
1693.685875	84.467469	64.218868
1692.984629	78.308836	64.223873
1693.056292	79.860274	64.228878
1692.025420	84.165194	64.233882
1691.212527	78.163069	64.238887
1690.568059	78.300168	64.243892
1690.152709	78.060247	64.248897
1689.630553	74.374254	64.253902
1688.844418	81.486741	64.258906
1688.284632	81.186182	64.263911
1687.900394	75.603258	64.268916
1687.049559	74.112582	64.273921
1686.010664	75.047204	64.278926
1685.022005	87.815359	64.283930
1684.441989	86.384169	64.288935
1684.177345	78.602866	64.293940
1683.592636	81.168478	64.298945
1682.940695	72.724867	64.303950
1681.866777	88.728326	64.308954
1681.786064	80.416327	64.313959
1680.997715	81.591855	64.318964
1680.405779	78.913596	64.323969
1680.399185	74.298875	64.328974
1678.988655	79.613444	64.333978
1678.020175	74.976469	64.338983
1677.141648	71.876951	64.343988
1676.550445	85.573888	64.348993
1676.047461	75.988540	64.353998
1675.017239	85.106292	64.359002
1675.022578	74.260621	64.364007
1674.342383	80.622989	64.369012
1673.837646	71.211390	64.374017
1673.246099	69.234826	64.379022
1672.726117	79.186170	64.384026
1672.507202	67.630218	64.389031
1671.006603	70.469053	64.394036
1669.970238	67.747853	64.399041
1669.342455	77.047683	64.404046
1668.739009	76.290434	64.409050
1668.200865	68.886903	64.414055
1667.878963	71.828668	64.419060
1667.559388	74.364783	64.424065
1667.214431	76.073863	64.429070
1665.633903	76.009573	64.434074
1664.466416	69.978632	64.439079
1663.984787	74.246775	64.444084
1663.395102	79.489308	64.449089
1663.195519	69.218675	64.454094
1662.394951	67.861951	64.459098
1661.862837	68.818583	64.464103
1661.561612	67.890324	64.469108
1660.695788	71.262273	64.474113
1660.531311	66.421897	64.479118
1658.875862	73.983143	64.484122
1658.007895	71.274621	64.489127
1657.486944	67.812376	64.494132
1656.725747	72.944956	64.499137
1656.228096	68.480785	64.504142
1655.704161	74.537630	64.509146
1655.268341	68.054572	64.514151
1654.547605	71.759872	64.519156
1654.199814	72.821267	64.524161
1653.975692	71.694678	64.529166
1652.771376	73.598621	64.534170
1651.709233	76.465589	64.539175
1650.806962	68.435500	64.544180
1649.917465	79.716587	64.549185
1649.606268	69.618230	64.554190
1648.699417	71.042830	64.559194
1648.688451	70.562056	64.564199
1648.133001	70.164622	64.569204
1647.562787	78.425547	64.574209
1646.970251	68.759819	64.579214
1646.450853	75.475121	64.584218
1645.434711	66.698292	64.589223
1644.477671	61.282070	64.594228
1643.946597	66.373364	64.599233
1643.650876	66.514998	64.604238
1642.783318	72.055567	64.609242
1642.266887	68.064321	64.614247
1641.059321	63.820166	64.619252
1640.003345	74.930576	64.624257
1639.997938	69.145555	64.629262
1639.106242	78.872097	64.634266
1638.642782	78.806987	64.639271
1637.778390	72.114466	64.644276
1637.301055	79.363991	64.649281
1637.039217	66.218967	64.654286
1636.481388	74.484232	64.659290
1635.988240	75.772151	64.664295
1634.546954	66.004717	64.669300
1633.747323	69.082303	64.674305
1633.408765	69.946689	64.679310
1632.770771	78.125342	64.684314
1632.272047	72.295686	64.689319
1631.660228	76.359009	64.694324
1631.284374	71.397671	64.699329
1630.331577	65.307413	64.704334
1629.600916	73.018230	64.709338
1628.789729	75.567792	64.714343
1628.014431	72.371466	64.719348
1627.659925	70.614303	64.724353
1627.261567	69.217348	64.729358
1626.066168	67.926515	64.734362
1625.474477	77.066074	64.739367
1624.553740	76.070656	64.744372
1623.662465	79.694247	64.749377
1623.372334	73.922918	64.754382
1622.812697	80.020136	64.759386
1622.561409	67.139948	64.764391
1622.114685	66.734709	64.769396
1620.791795	68.545538	64.774401
1620.304816	71.791081	64.779406
1619.561411	76.446176	64.784410
1618.762869	66.780070	64.789415
1618.291744	73.441973	64.794420
1617.689862	70.642307	64.799425
1617.488960	71.197817	64.804430
1616.017925	70.009126	64.809434
1615.436771	68.232778	64.814439
1614.777088	71.370140	64.819444
1613.841484	76.174043	64.824449
1613.562661	72.001550	64.829454
1613.410969	72.183384	64.834458
1612.825995	77.458293	64.839463
1611.710980	72.366804	64.844468
1610.429594	75.642362	64.849473
1610.221038	68.487688	64.854478
1609.818879	69.808465	64.859482
1609.558552	61.308977	64.864487
1609.170200	61.036395	64.869492
1607.624271	69.982196	64.874497
1606.956693	68.304737	64.879502
1606.208340	77.445533	64.884506
1605.763848	68.126889	64.889511
1605.046290	73.626291	64.894516
1604.616330	82.185066	64.899521
1604.179748	68.992116	64.904526
1603.017324	73.505624	64.909530
1602.009520	67.523465	64.914535
1601.310718	68.318931	64.919540
1600.803809	75.681967	64.924545
1600.551661	67.282104	64.929550
1600.169758	72.857492	64.934554
1599.491590	69.202616	64.939559
1598.259519	67.108635	64.944564
1597.561987	72.240576	64.949569
1597.041751	62.419878	64.954574
1596.204296	69.521610	64.959578
1595.890078	72.283963	64.964583
1595.786600	66.134478	64.969588
1594.751662	70.178296	64.974593
1593.911075	62.725069	64.979598
1592.823439	76.830464	64.984602
1592.363557	74.066592	64.989607
1591.962316	67.838256	64.994612
1591.168545	73.616278	64.999617
1591.221153	68.435486	65.004622
1589.905589	67.681009	65.009626
1589.058699	76.053707	65.014631
1589.062405	75.162166	65.019636
1588.392230	73.190231	65.024641
1587.650389	67.623144	65.029646
1586.154803	64.836168	65.034650
1585.449186	72.334855	65.039655
1585.180149	64.013375	65.044660
1584.149941	74.096252	65.049665
1584.023400	64.263469	65.054670
1583.755839	70.536636	65.059674
1583.205958	67.071120	65.064679
1582.196244	67.312009	65.069684
1581.008664	72.195380	65.074689
1580.634523	69.826324	65.079694
1580.087978	70.671722	65.084698
1579.574752	69.024941	65.089703
1578.520841	66.472150	65.094708
1577.183511	73.946627	65.099713
1577.264400	68.285097	65.104718
1576.046700	69.011624	65.109722
1575.914981	62.049757	65.114727
1575.757168	58.480951	65.119732
1575.104858	68.795525	65.124737
1574.772016	59.962209	65.129742
1573.710269	69.335728	65.134746
1572.868469	64.532015	65.139751
1572.188422	65.168389	65.144756
1571.617214	68.534555	65.149761
1570.894874	59.726855	65.154766
1569.722222	67.682952	65.159770
1568.988424	68.774150	65.164775
1568.586041	63.131059	65.169780
1568.137065	68.887419	65.174785
1567.568990	58.181767	65.179790
1567.134078	65.066579	65.184794
1566.635933	73.043244	65.189799
1565.487244	62.191720	65.194804
1564.740790	65.666157	65.199809
1564.145630	61.126039	65.204814
1563.659879	72.147444	65.209818
1563.100515	78.806028	65.214823
1562.183190	68.266252	65.219828
1561.240294	62.830471	65.224833
1560.650261	61.758878	65.229838
1560.142076	65.665395	65.234842
1559.590270	63.384498	65.239847
1559.462175	66.533601	65.244852
1558.090301	69.915023	65.249857
1557.696087	63.157295	65.254862
1557.049006	80.004442	65.259866
1556.592151	67.220012	65.264871
1555.689589	77.369351	65.269876
1554.509498	69.369254	65.274881
1553.831864	60.874582	65.279886
1553.221846	69.567621	65.284890
1552.516416	60.828204	65.289895
1552.311996	60.622601	65.294900
1551.494046	69.720844	65.299905
1551.122633	65.829582	65.304910
1550.839247	69.380257	65.309914
1550.076964	63.307072	65.314919
1548.972007	65.529591	65.319924
1548.397036	74.112984	65.324929
1548.154064	61.922211	65.329934
1546.965542	66.791551	65.334938
1545.652530	70.266130	65.339943
1545.168100	60.688921	65.344948
1544.560191	71.851164	65.349953
1544.170256	64.898790	65.354958
1543.670200	66.544218	65.359962
1543.195259	66.898847	65.364967
1543.156070	56.235325	65.369972
1541.991684	66.341106	65.374977
1541.088818	60.268186	65.379982
1540.386343	65.833013	65.384986
1539.923162	69.569955	65.389991
1539.308504	64.200300	65.394996
1538.056845	68.275421	65.400001
1537.511383	65.234997	65.405006
1536.576134	69.020142	65.410010
1536.290988	69.674201	65.415015
1536.021768	64.888331	65.420020
1535.355542	62.917361	65.425025
1534.913536	64.499949	65.430030
1533.625798	62.865860	65.435034
1533.168274	58.687085	65.440039
1532.706840	64.174187	65.445044
1531.986966	67.505635	65.450049
1531.348967	62.043497	65.455054
1530.255386	69.676382	65.460058
1529.387450	68.104899	65.465063
1529.211424	65.422094	65.470068
1528.529266	68.326499	65.475073
1528.577493	65.390438	65.480078
1527.573488	66.289615	65.485082
1526.589254	62.161420	65.490087
1525.738623	56.209519	65.495092
1525.404521	68.153008	65.500097
1524.859654	58.053971	65.505102
1523.555839	65.967848	65.510106
1522.848967	60.882515	65.515111
1522.642722	59.145965	65.520116
1521.854268	66.168963	65.525121
1521.389762	50.824773	65.530126
1520.973641	61.841416	65.535130
1520.309961	68.578080	65.540135
1519.345596	59.338922	65.545140
1518.512547	65.435440	65.550145
1518.249264	59.804952	65.555150
1517.540733	62.880708	65.560154
1516.379768	60.643004	65.565159
1515.937599	65.676033	65.570164
1515.149577	66.493584	65.575169
1514.671538	60.474594	65.580174
1514.371999	61.200328	65.585178
1513.320585	65.562187	65.590183
1511.993123	60.253772	65.595188
1511.237446	70.649438	65.600193
1511.214170	60.183664	65.605198
1510.813983	65.167444	65.610202
1510.284961	60.422864	65.615207
1510.121062	58.712703	65.620212
1509.015688	60.788645	65.625217
1508.269805	56.993171	65.630222
1507.306307	54.038111	65.635226
1506.866902	56.795132	65.640231
1506.510163	52.024755	65.645236
1505.140719	58.723759	65.650241
1504.563581	54.661772	65.655246
1504.042204	62.662631	65.660250
1503.469615	64.172933	65.665255
1503.291762	54.963343	65.670260
1501.904675	59.790136	65.675265
1501.281426	53.983463	65.680270
1500.615499	59.903614	65.685274
1499.845453	62.265321	65.690279
1499.684912	61.090796	65.695284
1499.150265	67.423755	65.700289
1498.439504	57.204432	65.705294
1497.579186	62.448993	65.710298
1496.780394	52.958031	65.715303
1496.351186	60.865394	65.720308
1495.514498	58.976718	65.725313
1494.860441	51.935447	65.730318
1493.742419	59.028168	65.735322
1493.338103	62.244821	65.740327
1493.262845	55.184109	65.745332
1492.480271	62.885851	65.750337
1491.694114	49.242300	65.755342
1491.024770	62.898032	65.760346
1490.069969	56.909083	65.765351
1489.841471	49.101587	65.770356
1489.207999	59.488867	65.775361
1488.282664	51.222825	65.780366
1487.566175	56.616419	65.785370
1486.727310	62.464708	65.790375
1486.513174	55.325140	65.795380
1485.976195	58.416218	65.800385
1485.001246	56.226240	65.805390
1483.962967	60.319512	65.810394
1483.381502	58.585826	65.815399
1483.202392	51.320844	65.820404
1482.769197	59.104260	65.825409
1481.533665	49.458784	65.830414
1480.754875	54.015447	65.835418
1480.095414	55.265167	65.840423
1479.883009	61.710920	65.845428
1479.083772	61.763856	65.850433
1479.036762	58.622156	65.855438
1477.795999	58.820956	65.860442
1476.742752	66.367021	65.865447
1476.752983	61.191394	65.870452
1475.793385	57.634901	65.875457
1474.634339	58.610777	65.880462
1474.156901	59.984537	65.885466
1473.451203	60.967214	65.890471
1472.871280	58.829580	65.895476
1472.124583	60.291865	65.900481
1472.289176	63.476456	65.905486
1471.740389	55.270426	65.910490
1470.738491	61.679220	65.915495
1470.259291	62.006153	65.920500
1469.239582	61.789776	65.925505
1468.002543	53.984868	65.930510
1467.170300	62.426223	65.935514
1466.613089	63.900974	65.940519
1466.739305	57.347567	65.945524
1466.067072	55.006984	65.950529
1465.679067	55.423505	65.955534
1464.247678	53.203573	65.960538
1463.605384	57.202380	65.965543
1463.262614	54.473543	65.970548
1462.657282	67.236005	65.975553
1462.529247	57.971193	65.980558
1461.156313	57.520794	65.985562
1460.341367	52.891058	65.990567
1460.272144	54.772382	65.995572
1459.443580	61.443795	66.000577
1458.807178	53.434623	66.005582
1457.688784	65.256749	66.010586
1457.123756	65.554747	66.015591
1456.830664	59.809156	66.020596
1456.039478	67.162191	66.025601
1455.052760	60.700506	66.030606
1454.282391	66.414914	66.035610
1453.572255	62.441886	66.040615
1453.389070	54.560960	66.045620
1452.586297	62.686972	66.050625
1452.009961	51.509587	66.055630
1451.805735	51.851169	66.060634
1450.326433	59.553264	66.065639
1449.994816	58.653517	66.070644
1449.145243	60.512208	66.075649
1448.958598	54.147300	66.080654
1448.208358	59.921587	66.085658
1446.962470	62.690099	66.090663
1446.862348	57.850561	66.095668
1446.036042	68.068225	66.100673
1445.847610	58.813014	66.105678
1444.958373	62.281788	66.110682
1443.857683	59.271286	66.115687
1443.537794	51.210238	66.120692
1442.925347	54.955144	66.125697
1441.824211	63.852408	66.130702
1440.868508	66.581111	66.135706
1440.071299	69.497514	66.140711
1439.721756	65.910307	66.145716
1439.092444	63.480906	66.150721
1438.433496	58.643454	66.155726
1438.499442	66.170924	66.160730
1437.954780	64.989646	66.165735
1437.506405	67.339669	66.170740
1436.472933	60.939040	66.175745
1435.717427	57.361165	66.180750
1434.765784	61.470647	66.185754
1433.656483	72.873445	66.190759
1433.142077	59.495806	66.195764
1432.282018	69.925421	66.200769
1432.166980	61.555842	66.205774
1432.158317	61.968845	66.210778
1431.398538	57.428122	66.215783
1430.358293	60.736396	66.220788
1429.361162	67.209104	66.225793
1429.264360	54.247649	66.230798
1428.139432	62.000666	66.235802
1427.174119	66.979659	66.240807
1426.977657	56.233915	66.245812
1426.110890	58.830213	66.250817
1425.869615	54.978218	66.255822
1424.721780	60.128147	66.260826
1423.885547	60.678995	66.265831
1423.775499	65.302852	66.270836
1422.908631	66.834713	66.275841
1422.578974	56.838701	66.280846
1421.313496	68.463443	66.285850
1420.474912	58.289698	66.290855
1419.975227	59.408381	66.295860
1419.621575	65.234760	66.300865
1419.135829	63.291907	66.305870
1418.635159	67.154673	66.310874
1417.528616	68.965908	66.315879
1417.157979	71.279924	66.320884
1416.636621	70.394570	66.325889
1416.158536	66.197010	66.330894
1415.036834	61.748511	66.335898
1414.086818	68.584323	66.340903
1413.764456	62.504343	66.345908
1413.309928	64.956273	66.350913
1412.472676	61.552248	66.355918
1411.652710	61.841892	66.360922
1410.706655	64.576955	66.365927
1410.659380	64.360578	66.370932
1410.124594	60.205150	66.375937
1409.092080	64.483616	66.380942
1408.234737	64.168914	66.385946
1407.432964	71.165672	66.390951
1407.234159	62.768409	66.395956
1406.462226	73.734388	66.400961
1405.309303	70.024144	66.405966
1404.471142	62.466529	66.410970
1403.923003	66.750008	66.415975
1404.050147	67.423703	66.420980
1403.364326	73.050570	66.425985
1402.727052	69.859190	66.430990
1401.853784	68.212906	66.435994
1400.983373	69.092473	66.440999
1400.732993	64.163279	66.446004
1400.180977	64.385103	66.451009
1399.192726	67.060646	66.456014
1397.985938	67.876986	66.461018
1397.596622	67.448469	66.466023
1397.202816	66.356762	66.471028
1396.415769	74.164900	66.476033
1396.450188	63.454999	66.481038
1395.663081	66.379270	66.486042
1394.358856	69.855677	66.491047
1393.964971	62.050826	66.496052
1393.143111	61.637449	66.501057
1392.287137	68.731135	66.506062
1391.770978	68.821104	66.511066
1390.890273	71.698754	66.516071
1390.607147	67.244702	66.521076
1390.090544	64.906210	66.526081
1389.672157	68.725940	66.531086
1388.443139	66.003945	66.536090
1387.634213	69.070461	66.541095
1387.456989	62.871220	66.546100
1386.964877	66.384120	66.551105
1385.890487	65.906806	66.556110
1385.226560	50.939720	66.561114
1384.479138	68.512450	66.566119
1384.353944	61.901235	66.571124
1382.840458	63.335620	66.576129
1382.168685	66.503338	66.581134
1381.576242	57.764951	66.586138
1381.000790	61.246943	66.591143
1380.689169	60.168984	66.596148
1380.224049	68.872130	66.601153
1379.829567	65.143841	66.606158
1379.085480	64.014777	66.611162
1378.015388	65.828119	66.616167
1377.809225	56.820170	66.621172
1376.656002	66.365986	66.626177
1375.819563	57.079754	66.631182
1375.065703	62.698514	66.636186
1374.660752	61.786781	66.641191
1374.494781	56.609208	66.646196
1373.416589	61.413769	66.651201
1372.454998	60.070121	66.656206
1371.734150	62.993328	66.661210
1370.925802	66.572270	66.666215
1370.823337	59.145306	66.671220
1370.455128	66.054226	66.676225
1369.763945	72.583978	66.681230
1368.707821	60.185038	66.686234
1367.740519	66.299783	66.691239
1367.850271	57.183268	66.696244
1367.360712	60.664226	66.701249
1366.347929	59.164713	66.706254
1365.741226	60.309880	66.711258
1364.908455	74.810061	66.716263
1364.121497	62.218523	66.721268
1363.131651	69.557427	66.726273
1362.796345	73.934817	66.731278
1362.319580	63.657845	66.736282
1361.616618	66.937760	66.741287
1361.099156	58.592740	66.746292
1360.058710	73.562754	66.751297
1359.621307	73.350048	66.756302
1359.388195	69.749076	66.761306
1358.020533	67.178448	66.766311
1357.585703	61.210976	66.771316
1356.625374	62.475438	66.776321
1356.069997	61.205995	66.781326
1355.933581	59.814755	66.786330
1354.742079	62.916866	66.791335
1354.295784	61.268956	66.796340
1353.621420	69.188498	66.801345
1353.181360	64.321004	66.806350
1352.010102	69.763274	66.811354
1351.035066	72.834129	66.816359
1350.682352	66.298510	66.821364
1350.300933	68.413972	66.826369
1349.771283	64.910606	66.831374
1349.813428	65.503193	66.836378
1348.400070	73.201169	66.841383
1347.478119	56.231360	66.846388
1347.044311	65.563470	66.851393
1346.402465	63.462519	66.856398
1345.681495	56.193810	66.861402
1344.705565	70.019729	66.866407
1344.275469	52.586954	66.871412
1343.651326	67.233740	66.876417
1343.154641	56.751785	66.881422
1342.736001	59.297369	66.886426
1341.573348	54.320825	66.891431
1341.014732	58.047732	66.896436
1340.100682	60.910196	66.901441
1339.483333	60.935837	66.906446
1339.269942	57.989331	66.911450
1338.349686	61.562418	66.916455
1337.915424	56.692431	66.921460
1336.899496	55.921990	66.926465
1336.617396	61.899426	66.931470
1335.668474	57.917090	66.936474
1334.285590	63.828250	66.941479
1334.315367	60.754775	66.946484
1333.644693	65.094017	66.951489
1333.680126	67.138480	66.956494
1333.008625	51.581256	66.961498
1331.880684	61.320186	66.966503
1331.378945	58.559872	66.971508
1330.805386	65.703292	66.976513
1329.711969	64.841093	66.981518
1328.974272	63.759914	66.986522
1328.075686	70.682195	66.991527
1328.065363	64.289268	66.996532
1327.409732	68.276034	67.001537
1326.604297	63.469788	67.006542
1325.475845	68.460557	67.011546
1324.884796	64.815569	67.016551
1324.828671	56.901847	67.021556
1324.199804	59.550241	67.026561
1323.437811	69.820786	67.031566
1322.349984	63.062995	67.036570
1321.880792	63.293746	67.041575
1321.611621	57.814039	67.046580
1320.282758	60.463334	67.051585
1319.539507	62.273622	67.056590
1319.402296	53.431344	67.061594
1318.478366	68.365493	67.066599
1318.244043	64.835683	67.071604
1317.233700	66.391966	67.076609
1316.511311	65.855565	67.081614
1316.014674	61.667287	67.086618
1315.349955	73.286447	67.091623
1315.064341	69.723790	67.096628
1313.814347	61.823253	67.101633
1313.051513	64.743688	67.106638
1312.993655	61.952230	67.111642
1311.874900	65.478036	67.116647
1310.706198	59.477440	67.121652
1310.117030	58.675431	67.126657
1309.789269	61.761663	67.131662
1309.616612	62.478286	67.136666
1308.648833	60.594747	67.141671
1308.635460	58.825977	67.146676
1307.931206	63.843927	67.151681
1306.760559	65.193886	67.156686
1306.220240	59.445051	67.161690
1304.977439	68.133072	67.166695
1304.565317	63.462999	67.171700
1303.647789	70.085520	67.176705
1303.149472	64.158116	67.181710
1303.306696	58.924435	67.186714
1302.532896	66.106004	67.191719
1301.437454	59.313166	67.196724
1300.745902	62.556587	67.201729
1300.242809	64.502164	67.206734
1299.703370	59.324053	67.211738
1298.478064	72.068410	67.216743
1297.880809	61.205060	67.221748
1297.161114	66.064617	67.226753
1296.615341	69.258055	67.231758
1296.605443	57.872387	67.236762
1295.599749	61.326606	67.241767
1294.916920	56.994471	67.246772
1294.289424	56.523415	67.251777
1293.754307	65.354390	67.256782
1292.912012	57.605091	67.261786
1292.085138	64.435552	67.266791
1291.255106	62.375576	67.271796
1291.069608	65.789278	67.276801
1290.171832	65.006378	67.281806
1289.141297	65.121380	67.286810
1288.270171	55.695620	67.291815
1288.075744	62.693609	67.296820
1287.857274	64.452008	67.301825
1287.323562	66.216373	67.306830
1286.600214	64.877457	67.311834
1285.579180	68.048689	67.316839
1285.268784	64.811679	67.321844
1284.515397	66.090574	67.326849
1283.469310	66.821492	67.331854
1282.686181	62.803353	67.336858
1282.119565	68.431790	67.341863
1281.866142	64.706324	67.346868
1281.037218	72.874385	67.351873
1280.156147	66.777606	67.356878
1279.574597	65.819849	67.361882
1279.047032	73.242976	67.366887
1278.692942	67.824083	67.371892
1277.255024	66.548322	67.376897
1276.435841	74.922996	67.381902
1276.244832	65.572026	67.386906
1275.577740	70.497343	67.391911
1275.189139	57.060334	67.396916
1274.626480	61.713575	67.401921
1273.400480	62.777457	67.406926
1273.128392	73.673445	67.411930
1272.492285	70.228025	67.416935
1272.112308	61.149957	67.421940
1271.198255	65.311865	67.426945
1270.255893	62.629509	67.431950
1269.973160	52.974585	67.436954
1268.756846	64.919571	67.441959
1268.161585	60.556173	67.446964
1267.633674	65.459361	67.451969
1266.979325	56.734008	67.456974
1266.645797	63.112290	67.461978
1266.049160	61.469378	67.466983
1265.460635	64.327417	67.471988
1264.470809	67.705008	67.476993
1263.719777	64.962269	67.481998
1263.474179	70.571205	67.487002
1262.303498	68.179047	67.492007
1261.544086	63.848058	67.497012
1261.396070	62.140123	67.502017
1260.931206	60.473106	67.507022
1259.705951	51.882692	67.512026
1258.609367	64.737477	67.517031
1258.417243	63.954349	67.522036
1257.974755	66.327117	67.527041
1257.290828	62.692186	67.532046
1256.725885	59.721163	67.537050
1255.858606	63.426203	67.542055
1255.472907	59.977243	67.547060
1254.647044	54.414178	67.552065
1253.280449	64.825024	67.557070
1252.949632	56.574939	67.562074
1252.365396	63.587602	67.567079
1252.214251	56.687216	67.572084
1251.696760	70.761962	67.577089
1250.554065	72.124848	67.582094
1250.047121	60.280475	67.587098
1249.266704	69.223003	67.592103
1248.834630	64.567154	67.597108
1247.555237	60.446588	67.602113
1246.701460	64.917467	67.607118
1246.496014	63.827373	67.612122
1245.820536	64.261252	67.617127
1245.497533	58.498378	67.622132
1244.992891	59.982160	67.627137
1243.912942	59.616178	67.632142
1243.526011	56.840782	67.637146
1242.815862	71.903382	67.642151
1242.018992	60.450469	67.647156
1241.422574	69.824215	67.652161
1240.661578	59.360665	67.657166
1240.098857	52.503652	67.662170
1239.422978	62.295309	67.667175
1238.591896	64.783488	67.672180
1237.893991	60.710813	67.677185
1237.126539	56.327497	67.682190
1236.839640	53.711239	67.687194
1236.030464	59.089666	67.692199
1235.247328	56.727361	67.697204
1234.532736	59.933460	67.702209
1234.053705	66.811126	67.707214
1233.551162	55.850740	67.712218
1232.760488	54.983020	67.717223
1231.896264	64.850362	67.722228
1231.280160	58.112225	67.727233
1230.448013	59.801054	67.732238
1230.261613	56.620032	67.737242
1229.494933	62.321290	67.742247
1228.847936	53.918061	67.747252
1228.267337	58.056918	67.752257
1227.472209	62.739249	67.757262
1227.118909	57.566252	67.762266
1225.764597	65.931410	67.767271
1225.269105	55.521844	67.772276
1224.900654	68.961026	67.777281
1223.959193	59.166429	67.782286
1224.195593	57.545602	67.787290
1222.968888	65.937778	67.792295
1222.274048	61.689577	67.797300
1221.591987	57.977090	67.802305
1220.535488	67.731508	67.807310
1220.140225	61.516501	67.812314
1219.301244	65.576600	67.817319
1218.721848	56.142327	67.822324
1218.680836	55.238978	67.827329
1217.801109	63.861409	67.832334
1217.011657	57.548239	67.837338
1216.003285	66.541215	67.842343
1215.702913	60.782632	67.847348
1214.936295	59.671393	67.852353
1213.795960	59.154177	67.857358
1213.369042	49.959015	67.862362
1212.460598	65.467888	67.867367
1212.417302	50.622955	67.872372
1212.201064	52.284807	67.877377
1211.345709	60.715703	67.882382
1210.604243	53.854007	67.887386
1209.705027	57.272399	67.892391
1208.702848	56.340550	67.897396
1207.920537	59.174222	67.902401
1207.257923	57.180693	67.907406
1207.063511	53.133618	67.912410
1206.301425	63.874130	67.917415
1206.065391	63.222570	67.922420
1205.262031	54.462590	67.927425
1204.022613	63.719394	67.932430
1204.014285	52.458073	67.937434
1203.004840	52.030434	67.942439
1201.812166	49.539303	67.947444
1201.402125	51.500060	67.952449
1201.004415	55.289713	67.957454
1200.648338	52.559881	67.962458
1200.118120	61.960947	67.967463
1199.195847	50.693585	67.972468
1198.313869	53.588840	67.977473
1197.500443	63.255721	67.982478
1197.538155	55.577827	67.987482
1196.354801	58.301814	67.992487
1195.435080	54.393741	67.997492
1195.145273	67.500292	68.002497
1194.450195	60.714800	68.007502
1194.137093	58.776079	68.012506
1193.134131	61.062946	68.017511
1192.296007	50.395644	68.022516
1191.701487	54.103055	68.027521
1191.265524	59.959885	68.032526
1190.880958	57.549978	68.037530
1189.802583	50.458017	68.042535
1189.130256	55.852538	68.047540
1188.634704	56.918566	68.052545
1187.481290	62.247672	68.057550
1186.949433	51.832865	68.062554
1185.960559	55.845846	68.067559
1185.516895	51.024700	68.072564
1185.015561	51.549172	68.077569
1184.767068	57.399842	68.082574
1184.608769	49.644314	68.087578
1183.186942	55.274730	68.092583
1182.914238	53.069387	68.097588
1182.421556	54.171229	68.102593
1180.918304	55.809107	68.107598
1180.551967	50.059448	68.112602
1179.882730	59.539394	68.117607
1179.395953	58.546089	68.122612
1178.473571	48.895144	68.127617
1177.524749	53.213996	68.132622
1177.465044	53.308686	68.137626
1176.542097	67.526764	68.142631
1176.260341	57.926895	68.147636
1175.157726	54.175651	68.152641
1174.315844	61.795432	68.157646
1173.735678	51.948134	68.162650
1173.527681	47.426982	68.167655
1173.098277	57.721922	68.172660
1172.184084	61.825534	68.177665
1171.440212	60.789540	68.182670
1171.285183	53.695818	68.187674
1169.875219	62.683289	68.192679
1168.989891	54.153982	68.197684
1168.720477	51.355179	68.202689
1168.276296	54.855757	68.207694
1167.572866	46.634995	68.212698
1166.130212	58.606548	68.217703
1165.679655	53.759694	68.222708
1165.517451	55.061293	68.227713
1164.935607	60.860902	68.232718
1164.197649	59.620542	68.237722
1163.165494	59.858855	68.242727
1162.997031	58.841736	68.247732
1162.376876	63.053129	68.252737
1161.352638	56.286886	68.257742
1160.781768	56.669456	68.262746
1160.177549	60.982395	68.267751
1159.623044	69.508963	68.272756
1158.421728	58.301765	68.277761
1157.535567	64.813680	68.282766
1157.579267	51.777890	68.287770
1156.909195	55.852141	68.292775
1156.317560	55.414840	68.297780
1155.862715	48.414540	68.302785
1154.445133	66.071799	68.307790
1154.106716	51.056193	68.312794
1153.368743	61.729800	68.317799
1153.034524	55.270134	68.322804
1152.143947	46.777943	68.327809
1151.254576	68.154830	68.332814
1150.849858	56.682166	68.337818
1150.304358	59.074487	68.342823
1149.917956	55.890590	68.347828
1148.993938	62.682919	68.352833
1148.019576	57.537753	68.357838
1147.617569	51.290723	68.362842
1147.186053	64.903936	68.367847
1145.896410	64.050950	68.372852
1145.662580	51.516623	68.377857
1144.653806	63.133750	68.382862
1144.612635	56.291581	68.387866
1143.472754	60.300211	68.392871
1142.445160	62.557898	68.397876
1142.056788	58.041781	68.402881
1141.313004	64.568902	68.407886
1141.362295	57.966236	68.412890
1140.745202	60.787841	68.417895
1139.609827	56.153994	68.422900
1139.071478	52.748262	68.427905
1138.596736	57.343386	68.432910
1137.935054	52.569543	68.437914
1136.778034	61.507335	68.442919
1136.265148	56.812326	68.447924
1136.124416	53.587781	68.452929
1134.676642	55.166398	68.457934
1133.961309	52.813844	68.462938
1133.212291	57.395823	68.467943
1132.767370	55.974821	68.472948
1132.627326	56.063367	68.477953
1131.934941	61.820640	68.482958
1131.230239	53.942291	68.487962
1130.215937	54.833795	68.492967
1129.765727	56.471367	68.497972
1129.439029	51.746747	68.502977
1128.283529	59.728660	68.507982
1127.700547	53.817926	68.512986
1127.190263	55.791485	68.517991
1126.571161	49.328254	68.522996
1125.622512	56.400473	68.528001
1124.632256	58.811501	68.533006
1124.359656	53.516878	68.538010
1124.069014	60.648441	68.543015
1123.108972	51.463984	68.548020
1122.458395	52.340215	68.553025
1121.651011	57.861889	68.558030
1121.357176	44.993341	68.563034
1120.912302	59.709394	68.568039
1119.863839	57.187479	68.573044
1119.123063	43.804970	68.578049
1118.294814	53.016899	68.583054
1118.037924	46.298938	68.588058
1116.914737	57.019627	68.593063
1116.073703	56.428039	68.598068
1115.656564	49.022779	68.603073
1114.923527	60.597629	68.608078
1114.918306	53.341313	68.613082
1114.268755	57.689855	68.618087
1113.191451	60.430126	68.623092
1112.735879	47.913735	68.628097
1112.083000	56.698802	68.633102
1111.470164	48.916238	68.638106
1110.755717	57.203317	68.643111
1109.922409	56.142144	68.648116
1109.554068	52.469678	68.653121
1107.996283	48.475477	68.658126
1107.637585	61.257085	68.663130
1107.008252	56.140634	68.668135
1106.914256	51.714897	68.673140
1106.241041	52.220992	68.678145
1104.746071	63.666307	68.683150
1104.177704	56.878040	68.688154
1103.823551	48.502393	68.693159
1103.321527	56.727298	68.698164
1103.481286	53.533806	68.703169
1101.915160	52.962944	68.708174
1101.302046	50.639871	68.713178
1100.656629	48.818681	68.718183
1100.296212	53.053423	68.723188
1099.474141	56.798626	68.728193
1098.283677	55.400029	68.733198
1097.693152	54.897910	68.738202
1097.576098	58.712317	68.743207
1096.818689	52.080282	68.748212
1095.911533	46.894490	68.753217
1095.064419	56.948372	68.758222
1094.793497	54.788489	68.763226
1094.329218	65.492688	68.768231
1093.573602	55.550321	68.773236
1092.628816	58.969692	68.778241
1091.821108	68.347104	68.783246
1091.538364	51.813506	68.788250
1090.993955	52.903093	68.793255
1089.527319	61.409179	68.798260
1089.269296	52.141451	68.803265
1088.540162	58.010234	68.808270
1088.234535	50.074729	68.813274
1087.840957	54.298978	68.818279
1086.646434	54.851735	68.823284
1085.860833	59.974136	68.828289
1085.228636	55.621398	68.833294
1085.419358	59.513004	68.838298
1084.207574	53.336454	68.843303
1083.490335	56.126692	68.848308
1083.397289	56.496348	68.853313
1082.010470	55.969515	68.858318
1081.188980	55.892074	68.863322
1080.352779	54.512825	68.868327
1080.105217	56.124476	68.873332
1079.937477	57.269264	68.878337
1079.207494	55.182409	68.883342
1078.582893	48.059321	68.888346
1077.773971	57.534694	68.893351
1077.299595	51.953632	68.898356
1075.803950	45.636165	68.903361
1075.253971	55.877749	68.908366
1074.964191	52.541302	68.913370
1074.581557	58.247733	68.918375
1073.343118	55.964219	68.923380
1072.911590	48.823035	68.928385
1072.111476	51.211718	68.933390
1071.970443	57.857432	68.938394
1071.235891	56.547172	68.943399
1069.862190	58.060425	68.948404
1069.524188	50.806591	68.953409
1068.768482	58.592460	68.958414
1068.529828	47.979662	68.963418
1067.812113	61.548516	68.968423
1066.704862	54.940605	68.973428
1066.184253	56.130490	68.978433
1065.785803	64.723706	68.983438
1065.148052	55.883821	68.988442
1064.109793	60.267402	68.993447
1063.477819	54.482753	68.998452
1062.984935	56.527673	69.003457
1062.350047	57.650583	69.008462
1061.931085	56.357929	69.013466
1060.358958	50.062100	69.018471
1060.108347	59.451813	69.023476
1059.698099	49.933918	69.028481
1059.061951	59.818629	69.033486
1058.877311	54.320788	69.038490
1058.265132	54.593258	69.043495
1057.186951	63.040717	69.048500
1056.941582	53.319970	69.053505
1055.354931	62.285139	69.058510
1054.947819	59.213365	69.063514
1054.274581	57.650503	69.068519
1053.644397	59.155868	69.073524
1053.543515	59.632428	69.078529
1052.453661	53.535848	69.083534
1051.711924	52.712441	69.088538
1051.163324	54.797765	69.093543
1050.511297	57.755834	69.098548
1049.640170	60.524831	69.103553
1048.745236	54.671634	69.108558
1048.490371	58.121610	69.113562
1047.929082	55.859692	69.118567
1047.303436	55.500368	69.123572
1046.410209	43.357983	69.128577
1045.353325	52.579493	69.133582
1045.031921	53.794461	69.138586
1044.880599	48.132051	69.143591
1044.073406	52.797423	69.148596
1043.252426	51.043603	69.153601
1042.380582	54.347305	69.158606
1042.035701	55.755244	69.163610
1041.543871	56.937402	69.168615
1040.352133	51.388473	69.173620
1039.777923	45.162558	69.178625
1039.404990	50.593056	69.183630
1038.543764	49.640429	69.188634
1037.874863	48.455353	69.193639
1036.786103	53.924041	69.198644
1036.819946	52.672896	69.203649
1035.991137	54.154671	69.208654
1035.459343	47.631848	69.213658
1035.006134	49.929080	69.218663
1033.772540	52.011422	69.223668
1033.652668	54.588363	69.228673
1032.596714	56.959413	69.233678
1032.041766	48.912198	69.238682
1031.365045	50.311430	69.243687
1030.716861	51.311883	69.248692
1030.261031	49.533089	69.253697
1029.008371	50.770062	69.258702
1028.561234	57.555939	69.263706
1028.140985	54.642380	69.268711
1027.258269	54.696123	69.273716
1026.399707	46.717716	69.278721
1025.654053	59.488345	69.283726
1025.286184	59.785031	69.288730
1024.902243	49.053431	69.293735
1024.373019	52.357822	69.298740
1023.742604	44.486622	69.303745
1022.747034	52.316968	69.308750
1022.458734	51.870862	69.313754
1021.368269	60.725566	69.318759
1020.287306	55.816615	69.323764
1019.814236	51.657778	69.328769
1019.014080	54.570034	69.333774
1018.426820	50.870915	69.338778
1018.476528	51.025471	69.343783
1017.665900	56.782655	69.348788
1017.130792	47.317754	69.353793
1016.145928	55.758261	69.358798
1015.311833	58.606533	69.363802
1014.204717	52.427562	69.368807
1013.653905	59.950608	69.373812
1013.535787	56.170539	69.378817
1012.870177	55.147374	69.383822
1012.546848	52.563752	69.388826
1011.906149	60.356568	69.393831
1010.777136	65.051078	69.398836
1010.286025	53.516509	69.403841
1009.803873	57.584548	69.408846
1009.013178	45.629294	69.413850
1008.064224	57.468747	69.418855
1007.260420	49.874297	69.423860
1007.344026	42.110275	69.428865
1006.242069	59.865597	69.433870
1005.227582	56.202915	69.438874
1004.646272	49.782595	69.443879
1004.344534	58.582774	69.448884
1004.092957	53.448830	69.453889
1002.624844	54.398396	69.458894
1001.915904	58.280168	69.463898
1001.757689	57.548438	69.468903
1000.926190	65.283306	69.473908
1000.436625	56.426174	69.478913
999.419373	52.672471	69.483918
998.879116	46.772327	69.488922
998.355088	51.042572	69.493927
997.649527	56.045026	69.498932
996.837538	51.012867	69.503937
995.956794	54.586083	69.508942
995.963720	45.074372	69.513946
995.346409	50.438100	69.518951
994.168562	47.403816	69.523956
993.651145	46.648815	69.528961
993.052301	49.492777	69.533966
992.559439	48.776447	69.538970
991.481646	51.195142	69.543975
990.538242	51.083512	69.548980
990.340824	45.847915	69.553985
989.545758	51.854942	69.558990
989.615101	59.479590	69.563994
988.745428	48.830017	69.568999
987.245200	52.760424	69.574004
987.080570	41.913519	69.579009
986.453442	55.384385	69.584014
985.855761	45.962568	69.589018
985.033490	46.684801	69.594023
984.466826	55.437245	69.599028
984.397193	50.220739	69.604033
983.036218	48.641171	69.609038
982.482586	48.830225	69.614042
981.967601	45.698362	69.619047
981.233406	48.909216	69.624052
980.377095	43.537187	69.629057
979.293847	51.261648	69.634062
978.701911	49.316863	69.639066
978.455894	46.377170	69.644071
977.973944	56.510169	69.649076
977.533568	49.575421	69.654081
976.466774	54.121268	69.659086
975.708852	48.648428	69.664090
975.378955	43.736690	69.669095
974.172545	56.314133	69.674100
973.594626	45.573990	69.679105
972.909481	52.099697	69.684110
972.564444	51.523853	69.689114
972.391407	50.340319	69.694119
971.298641	49.620101	69.699124
970.374688	46.305732	69.704129
969.962803	53.325702	69.709134
969.503376	54.196786	69.714138
968.721033	43.588523	69.719143
967.515599	52.910967	69.724148
967.278298	46.104759	69.729153
966.818273	49.756118	69.734158
966.256643	48.511416	69.739162
965.204028	42.252839	69.744167
964.238454	51.802045	69.749172
964.060766	37.826960	69.754177
963.382664	47.402961	69.759182
962.327222	52.286053	69.764186
961.714891	49.707426	69.769191
961.034159	51.496824	69.774196
961.117227	47.610631	69.779201
960.640526	45.537128	69.784206
959.355729	46.776093	69.789210
958.772178	45.285722	69.794215
958.010727	46.547067	69.799220
957.088914	50.051135	69.804225
956.486237	45.909784	69.809230
955.655116	54.098761	69.814234
955.354843	46.567713	69.819239
954.784891	53.658569	69.824244
954.360507	44.319574	69.829249
953.336350	49.058918	69.834254
952.678242	51.995898	69.839258
952.438419	51.531048	69.844263
951.516547	52.698074	69.849268
950.800343	46.885866	69.854273
949.886335	51.664455	69.859278
949.205948	50.536426	69.864282
948.984308	44.866294	69.869287
947.904502	44.642344	69.874292
947.320973	49.395152	69.879297
946.867205	52.972979	69.884302
946.131764	48.425401	69.889306
945.546656	45.654789	69.894311
944.170206	55.690435	69.899316
944.144706	43.816873	69.904321
943.447839	43.505179	69.909326
942.975248	52.047114	69.914330
942.103642	44.151245	69.919335
941.539439	54.399836	69.924340
940.995596	53.035614	69.929345
940.581559	51.040452	69.934350
939.194664	55.261936	69.939354
938.774197	52.469856	69.944359
938.085588	53.956160	69.949364
937.873813	51.977698	69.954369
936.638619	51.582936	69.959374
935.881975	50.706743	69.964378
935.226822	46.808716	69.969383
934.668560	61.126499	69.974388
934.665273	44.135322	69.979393
934.077451	55.477352	69.984398
933.110251	54.787632	69.989402
932.782931	34.960617	69.994407
931.307223	56.623207	69.999412
930.359123	44.393415	70.004417
930.043100	50.262722	70.009422
929.457640	46.888195	70.014426
929.537930	50.284841	70.019431
928.270446	55.504467	70.024436
927.703105	48.880096	70.029441
926.869022	63.057271	70.034446
926.556581	47.384743	70.039450
925.474366	49.212808	70.044455
924.261811	56.864828	70.049460
924.297598	49.526310	70.054465
923.543098	52.948570	70.059470
923.032982	51.454405	70.064474
922.903963	43.219596	70.069479
921.712910	43.759262	70.074484
921.124537	47.333280	70.079489
920.447838	53.856077	70.084494
919.592932	43.823934	70.089498
918.937600	45.276561	70.094503
918.188972	37.364289	70.099508
917.964575	50.212823	70.104513
917.384303	40.296252	70.109518
916.292302	41.555019	70.114522
915.871996	49.169268	70.119527
914.853695	52.906326	70.124532
914.511363	43.488053	70.129537
913.502188	55.122645	70.134542
912.505736	51.212706	70.139546
912.564233	45.436497	70.144551
911.503429	52.204927	70.149556
911.434237	43.895943	70.154561
910.725370	54.572838	70.159566
909.735180	52.989496	70.164570
909.281089	43.596895	70.169575
908.423042	49.591886	70.174580
907.621037	47.592242	70.179585
906.485979	43.497785	70.184590
906.105141	49.036784	70.189594
905.857269	47.245421	70.194599
905.431992	49.413649	70.199604
905.347350	47.774505	70.204609
904.179130	49.919043	70.209614
903.388555	53.585170	70.214618
902.095358	46.026072	70.219623
901.504947	49.712384	70.224628
900.820031	52.705682	70.229633
900.804623	55.945669	70.234638
900.222893	56.410450	70.239642
899.672318	49.367103	70.244647
898.068143	50.377806	70.249652
897.753024	50.645614	70.254657
897.389181	49.697458	70.259662
896.791851	59.557091	70.264666
895.840831	49.630138	70.269671
895.030680	56.361838	70.274676
894.863150	43.881680	70.279681
894.032957	47.498920	70.284686
893.174755	48.289979	70.289690
892.814183	48.604447	70.294695
892.150723	50.782198	70.299700
891.610674	53.265163	70.304705
890.529985	47.613486	70.309710
889.642916	47.524467	70.314714
889.812515	38.359043	70.319719
888.490015	56.786580	70.324724
887.921216	48.279565	70.329729
887.151915	43.418853	70.334734
886.513801	53.743868	70.339738
886.441682	45.550470	70.344743
885.015539	53.004683	70.349748
884.229511	52.428074	70.354753
883.826264	44.883468	70.359758
883.167524	53.615885	70.364762
883.139678	47.798225	70.369767
882.370288	44.973380	70.374772
881.423923	49.850180	70.379777
880.682999	51.037318	70.384782
880.193147	48.224754	70.389786
879.771779	39.628050	70.394791
878.775888	47.018517	70.399796
878.145587	48.044546	70.404801
877.381256	48.757592	70.409806
876.530930	50.793199	70.414810
876.108242	40.493591	70.419815
875.315238	49.942815	70.424820
875.019689	38.620028	70.429825
874.291814	47.992653	70.434830
873.235864	41.026598	70.439834
872.841039	48.053321	70.444839
872.113536	56.878688	70.449844
871.583986	36.131397	70.454849
870.631813	36.278252	70.459854
869.723258	47.854258	70.464858
869.550289	46.142441	70.469863
869.140683	55.738807	70.474868
868.608900	40.873923	70.479873
867.265782	49.300527	70.484878
866.368457	50.714412	70.489882
866.235467	46.720682	70.494887
866.057314	51.631337	70.499892
864.952424	45.746982	70.504897
863.607868	53.306492	70.509902
863.143794	48.111776	70.514906
862.884097	34.591318	70.519911
862.262989	47.838880	70.524916
862.117912	35.503397	70.529921
860.893799	45.382361	70.534926
860.351996	46.367500	70.539930
860.052866	35.560954	70.544935
858.832245	42.036289	70.549940
857.969093	38.876293	70.554945
857.793116	38.645719	70.559950
856.973517	42.668138	70.564954
855.879821	43.493537	70.569959
855.150089	50.250291	70.574964
854.935986	42.691357	70.579969
854.228579	47.869177	70.584974
853.824848	51.111045	70.589978
853.448751	37.285837	70.594983
852.052169	44.483044	70.599988
851.709022	39.638095	70.604993
851.238478	37.486365	70.609998
850.634546	41.526498	70.615002
849.645277	31.760209	70.620007
849.040631	48.051832	70.625012
848.703293	41.236338	70.630017
847.363201	34.211447	70.635022
846.655520	44.823502	70.640026
846.402403	39.979993	70.645031
845.692013	51.603313	70.650036
845.230190	38.748965	70.655041
844.255305	44.444024	70.660046
843.814078	46.887613	70.665050
843.222803	44.818179	70.670055
842.622794	52.267073	70.675060
841.516616	47.999316	70.680065
840.959623	42.357349	70.685070
840.271519	50.632398	70.690074
840.094731	42.985525	70.695079
839.140270	45.685848	70.700084
838.182307	36.345089	70.705089
837.687387	35.860931	70.710094
837.166452	34.502550	70.715098
836.782894	31.430229	70.720103
835.757035	46.259249	70.725108
834.895077	37.169715	70.730113
834.889615	37.128045	70.735118
833.973910	37.573461	70.740122
833.320509	41.052189	70.745127
832.305857	45.137202	70.750132
831.864360	41.228854	70.755137
831.471823	41.865386	70.760142
830.238366	39.035580	70.765146
829.849222	40.737595	70.770151
829.215254	48.277050	70.775156
828.696906	46.145549	70.780161
828.031476	36.893848	70.785166
826.902712	39.131487	70.790170
826.819281	33.871465	70.795175
825.935309	43.344636	70.800180
825.468674	44.701018	70.805185
824.296326	40.481651	70.810190
823.517217	39.243216	70.815194
823.430326	36.748148	70.820199
822.883801	33.332762	70.825204
822.007000	38.178004	70.830209
821.286597	34.787142	70.835214
820.608200	45.238422	70.840218
820.351463	36.036787	70.845223
818.598599	44.303128	70.850228
818.153678	41.309962	70.855233
817.705626	43.062357	70.860238
817.194931	43.657775	70.865242
817.320318	38.127969	70.870247
816.114686	39.816452	70.875252
815.382583	38.704578	70.880257
814.800916	37.138249	70.885262
814.228828	48.954023	70.890266
813.432742	37.573734	70.895271
812.403001	47.387083	70.900276
811.896125	33.548016	70.905281
811.523701	42.225401	70.910286
810.833674	38.139000	70.915290
810.125229	38.412660	70.920295
809.147828	37.136408	70.925300
808.997558	35.238058	70.930305
808.286034	32.752537	70.935310
807.346559	39.730342	70.940314
806.675298	38.851637	70.945319
805.843099	40.729838	70.950324
805.743044	35.265883	70.955329
804.941231	35.737334	70.960334
803.778246	43.006188	70.965338
803.555957	35.579456	70.970343
803.012298	40.336980	70.975348
802.198897	39.796294	70.980353
801.455680	33.944289	70.985358
800.709523	39.369560	70.990362
800.592843	38.030413	70.995367
799.245111	33.993522	71.000372
798.412093	38.420216	71.005377
798.060845	39.236261	71.010382
797.362798	42.446138	71.015386
797.345543	39.823291	71.020391
796.132683	45.911064	71.025396
795.673957	39.155907	71.030401
795.386212	42.302046	71.035406
794.147790	44.385267	71.040410
793.297500	31.646398	71.045415
792.288818	40.764114	71.050420
792.175331	40.794834	71.055425
792.197079	38.571057	71.060430
791.005989	42.108582	71.065434
790.380019	38.415690	71.070439
789.671929	41.409548	71.075444
789.134782	41.338977	71.080449
788.283193	38.052587	71.085454
787.002820	44.923819	71.090458
787.182396	37.190265	71.095463
786.340791	49.159334	71.100468
785.598579	43.154206	71.105473
784.799572	44.508312	71.110478
784.010593	48.025983	71.115482
783.916734	43.114553	71.120487
783.109827	45.919140	71.125492
782.037011	44.498815	71.130497
781.478661	36.321339	71.135502
780.648127	47.060197	71.140506
780.428679	42.201876	71.145511
780.086770	48.146274	71.150516
778.894090	41.858047	71.155521
778.730854	37.966914	71.160526
777.718226	47.646663	71.165530
777.179970	32.596772	71.170535
775.825286	36.341696	71.175540
775.334355	36.968669	71.180545
775.208544	27.809284	71.185550
774.701818	36.260465	71.190554
773.856042	38.554000	71.195559
773.022958	34.637043	71.200564
772.442439	36.558766	71.205569
772.129942	28.331120	71.210574
770.782115	37.253672	71.215578
770.420339	34.919064	71.220583
769.710789	45.234962	71.225588
769.288402	33.743163	71.230593
768.555638	34.629411	71.235598
767.391905	33.581537	71.240602
766.902237	33.579105	71.245607
766.377430	29.198336	71.250612
765.883630	34.222315	71.255617
765.205749	29.429099	71.260622
764.146388	39.433254	71.265626
763.826740	34.015302	71.270631
763.328205	48.085454	71.275636
762.578349	43.317885	71.280641
761.986069	37.724138	71.285646
760.980880	35.698546	71.290650
760.366577	36.840326	71.295655
759.954227	44.260930	71.300660
759.263004	39.901922	71.305665
758.767249	39.872076	71.310670
757.753901	43.428628	71.315674
757.555436	39.051096	71.320679
756.658432	40.438158	71.325684
755.937704	39.917427	71.330689
755.678580	37.616941	71.335694
754.625917	45.636228	71.340698
753.937594	27.629797	71.345703
752.796351	24.908356	71.350708
752.693997	38.478609	71.355713
752.296109	32.074903	71.360718
750.994270	34.802175	71.365722
750.721617	34.429306	71.370727
749.694137	32.847238	71.375732
749.412941	36.747697	71.380737
748.841461	31.319380	71.385742
747.664977	43.649273	71.390746
747.500147	35.415465	71.395751
746.962015	42.662129	71.400756
746.031653	41.417837	71.405761
745.182272	36.429579	71.410766
744.083880	40.135292	71.415770
744.089622	45.426677	71.420775
743.810980	38.040466	71.425780
742.774894	37.806490	71.430785
742.127601	32.683557	71.435790
741.211904	41.482133	71.440794
740.800977	40.637692	71.445799
739.591779	36.971440	71.450804
738.956636	31.427105	71.455809
738.987015	32.839987	71.460814
737.970440	42.124557	71.465818
737.844792	29.055880	71.470823
736.685171	36.418838	71.475828
735.914698	40.189041	71.480833
735.634182	35.048715	71.485838
734.890760	38.106558	71.490842
733.911087	29.931525	71.495847
733.095038	36.498615	71.500852
732.504927	48.252611	71.505857
732.486752	39.605945	71.510862
731.744495	45.259272	71.515866
730.823221	41.551913	71.520871
729.854471	39.170447	71.525876
729.612085	37.600584	71.530881
729.253858	35.008374	71.535886
727.936391	35.727529	71.540890
727.633094	44.069061	71.545895
726.921583	31.670828	71.550900
726.050267	27.267969	71.555905
725.406637	35.915994	71.560910
724.608307	43.585713	71.565914
724.094663	34.924898	71.570919
723.680845	39.157135	71.575924
723.052350	38.517649	71.580929
722.470450	33.559353	71.585934
721.426886	49.234893	71.590938
721.257182	35.427328	71.595943
719.843771	38.552427	71.600948
719.129386	38.623631	71.605953
718.840557	29.408207	71.610958
718.056083	35.960812	71.615962
718.155751	25.910827	71.620967
716.755919	27.710699	71.625972
715.909362	34.203802	71.630977
715.526755	31.443589	71.635982
715.009582	38.090830	71.640986
714.595159	32.132890	71.645991
713.469432	34.269167	71.650996
712.750902	30.761349	71.656001
712.570710	22.952622	71.661006
711.775609	32.654516	71.666010
711.221961	25.220642	71.671015
710.573793	34.036548	71.676020
710.141842	30.502025	71.681025
708.856235	41.444239	71.686030
707.823564	48.201950	71.691034
707.809078	33.350963	71.696039
707.565441	44.264469	71.701044
705.995060	39.562913	71.706049
705.543957	44.010826	71.711054
704.528325	38.615392	71.716058
704.121217	31.531921	71.721063
703.939642	43.796455	71.726068
703.029453	40.915243	71.731073
702.231505	32.719174	71.736078
701.309551	37.773491	71.741082
701.095307	33.275478	71.746087
700.653311	34.478146	71.751092
700.266243	36.684472	71.756097
699.455988	33.535039	71.761102
698.401424	33.316639	71.766106
697.887347	31.652845	71.771111
696.940246	35.217792	71.776116
696.169378	30.634946	71.781121
695.746863	35.166615	71.786126
695.186385	43.752524	71.791130
694.895930	31.504881	71.796135
693.953436	33.075826	71.801140
693.071197	39.965704	71.806145
692.852837	29.958473	71.811150
691.419234	38.110974	71.816154
690.756217	38.601361	71.821159
690.149673	35.892579	71.826164
689.837630	35.316254	71.831169
689.374880	30.864121	71.836174
688.589315	31.892840	71.841178
687.400550	38.834681	71.846183
687.231444	38.431138	71.851188
686.676915	35.578456	71.856193
686.767345	30.823774	71.861198
685.237229	36.687718	71.866202
684.561865	31.780585	71.871207
684.268323	34.773113	71.876212
683.047489	36.487732	71.881217
682.831243	33.209025	71.886222
681.701439	39.439736	71.891226
681.284273	36.552568	71.896231
680.071000	37.997902	71.901236
679.161085	38.038752	71.906241
678.978146	29.506643	71.911246
678.629132	38.544580	71.916250
678.598528	31.404317	71.921255
677.785132	33.828343	71.926260
676.768631	35.631853	71.931265
676.245005	27.508810	71.936270
675.097988	40.086345	71.941274
674.385200	26.325855	71.946279
673.708927	34.023453	71.951284
672.780082	33.707774	71.956289
673.051125	33.913810	71.961294
672.545850	33.300448	71.966298
671.750164	30.615483	71.971303
670.772074	42.398146	71.976308
670.089494	28.101412	71.981313
669.329051	28.383392	71.986318
668.110848	33.122192	71.991322
667.776561	25.461012	71.996327
667.389630	36.886184	72.001332
667.206823	38.085432	72.006337
666.672221	25.595981	72.011342
665.640200	39.276419	72.016346
665.006291	29.286480	72.021351
663.866536	38.432990	72.026356
662.775243	33.603136	72.031361
662.677494	30.381257	72.036366
661.843308	33.489842	72.041370
661.639214	31.663153	72.046375
661.126067	29.420478	72.051380
659.756847	36.485683	72.056385
659.412762	25.126534	72.061390
658.931144	33.321415	72.066394
658.316431	31.440267	72.071399
657.327774	40.803993	72.076404
656.619977	32.623549	72.081409
656.463729	18.367595	72.086414
655.724573	38.515783	72.091418
654.868221	31.317784	72.096423
653.988787	36.193456	72.101428
653.223950	34.601144	72.106433
652.957340	32.175708	72.111438
652.253748	30.039056	72.116442
651.424075	33.216311	72.121447
650.533781	27.340477	72.126452
650.085523	35.181541	72.131457
650.090094	29.857061	72.136462
648.999382	38.551066	72.141466
648.254712	28.730160	72.146471
647.842678	31.842485	72.151476
646.915093	31.122915	72.156481
646.356784	28.674548	72.161486
645.336050	29.196681	72.166490
645.047834	37.244073	72.171495
644.699976	37.230121	72.176500
643.359060	32.611917	72.181505
642.807051	26.830448	72.186510
642.309369	24.165846	72.191514
641.868207	36.772907	72.196519
641.016471	32.616120	72.201524
640.106329	30.917642	72.206529
639.824105	28.045264	72.211534
638.883447	36.071978	72.216538
638.501712	30.460511	72.221543
637.245048	24.557873	72.226548
636.532547	32.329056	72.231553
636.484937	32.402908	72.236558
635.676822	30.297099	72.241562
635.205204	22.845455	72.246567
634.351662	22.727533	72.251572
633.327867	19.976409	72.256577
633.480908	19.344949	72.261582
632.604828	37.915916	72.266586
631.498482	32.749430	72.271591
630.965457	29.227866	72.276596
630.335226	35.574578	72.281601
629.894673	28.745612	72.286606
628.828300	26.184195	72.291610
628.280812	19.212992	72.296615
627.736304	26.298254	72.301620
627.162091	27.020519	72.306625
626.997435	27.415787	72.311630
625.666443	35.876828	72.316634
625.049576	25.106756	72.321639
624.903385	30.332439	72.326644
623.760651	27.163444	72.331649
623.056964	21.685258	72.336654
622.496809	26.514820	72.341658
621.572569	23.460840	72.346663
621.706835	26.498780	72.351668
620.422011	31.312866	72.356673
620.007392	27.945913	72.361678
619.310932	36.304326	72.366682
618.389075	32.149254	72.371687
617.546144	40.250299	72.376692
616.932632	35.593534	72.381697
616.744984	25.661854	72.386702
615.962898	31.332585	72.391706
614.970998	32.452534	72.396711
614.443847	30.650493	72.401716
613.497570	30.123147	72.406721
613.209634	29.181871	72.411726
612.877053	29.042489	72.416730
611.930447	22.841327	72.421735
611.358106	26.398655	72.426740
610.451764	36.569297	72.431745
610.387196	30.785898	72.436750
608.868641	37.130589	72.441754
608.357341	31.150256	72.446759
608.281572	30.582043	72.451764
607.360442	39.053512	72.456769
606.478016	27.261297	72.461774
605.623171	31.245242	72.466778
605.260997	35.127069	72.471783
604.813795	28.592481	72.476788
603.830943	30.980440	72.481793
603.559092	26.739198	72.486798
602.469933	31.164162	72.491802
601.912610	30.590643	72.496807
601.559321	22.882043	72.501812
600.720540	27.945218	72.506817
600.100135	29.515362	72.511822
599.225464	40.081510	72.516826
598.796139	33.102528	72.521831
598.238562	23.655548	72.526836
597.081729	27.952520	72.531841
596.936208	24.162668	72.536846
596.400303	30.160047	72.541850
595.419914	32.000414	72.546855
594.827780	35.327511	72.551860
593.698601	24.377273	72.556865
593.681861	23.493731	72.561870
592.699568	23.298559	72.566874
592.051766	25.592156	72.571879
591.418026	33.812851	72.576884
590.535536	30.320148	72.581889
590.477498	30.747322	72.586894
589.062759	29.258541	72.591898
588.256939	31.525269	72.596903
588.434124	31.982787	72.601908
587.552528	32.115354	72.606913
587.152377	20.591693	72.611918
585.994090	29.091473	72.616922
585.190156	20.483251	72.621927
585.115678	22.928385	72.626932
584.361804	38.103646	72.631937
583.118012	28.303916	72.636942
582.334857	34.646608	72.641946
581.917419	39.437680	72.646951
581.564135	29.325806	72.651956
581.066396	36.367360	72.656961
580.866128	38.827801	72.661966
579.889097	31.417243	72.666970
578.978538	28.490411	72.671975
577.876844	24.359270	72.676980
577.161730	29.748108	72.681985
576.848969	25.699467	72.686990
576.269198	38.259223	72.691994
575.986329	37.802845	72.696999
575.080126	28.316780	72.702004
574.138070	38.512045	72.707009
574.051001	28.487080	72.712014
572.966497	37.970174	72.717018
571.853452	37.497792	72.722023
571.145633	43.017938	72.727028
570.487762	37.210769	72.732033
570.449160	34.807374	72.737038
570.046738	35.464443	72.742042
569.204931	36.123688	72.747047
568.502564	30.310994	72.752052
567.582424	33.354451	72.757057
567.134985	29.224760	72.762062
565.995368	33.200460	72.767066
565.530814	32.118588	72.772071
565.304130	23.904128	72.777076
564.679917	37.056011	72.782081
563.582381	31.129643	72.787086
562.710018	38.550993	72.792090
562.441512	36.173179	72.797095
561.957280	34.608740	72.802100
560.887148	37.926826	72.807105
560.051344	30.812327	72.812110
559.360527	39.122546	72.817114
558.985056	34.259149	72.822119
558.565903	31.239858	72.827124
557.776600	41.540108	72.832129
556.942746	28.407655	72.837134
556.274450	23.653982	72.842138
555.952154	33.506102	72.847143
555.489390	35.331844	72.852148
554.394096	34.782526	72.857153
553.898133	26.290838	72.862158
553.433842	31.677576	72.867162
552.472064	36.099618	72.872167
551.901502	30.530862	72.877172
550.882930	34.411595	72.882177
550.756124	22.137928	72.887182
549.603662	37.122793	72.892186
548.873225	36.874905	72.897191
548.542722	27.639350	72.902196
547.918922	40.896828	72.907201
547.334567	29.656402	72.912206
546.563617	41.322523	72.917210
545.414295	37.374023	72.922215
545.405726	34.636262	72.927220
544.779453	32.485750	72.932225
543.880511	23.447978	72.937230
543.139587	31.714137	72.942234
542.527679	36.887850	72.947239
542.369814	26.528817	72.952244
541.011820	36.317258	72.957249
540.413189	28.811752	72.962254
539.940261	27.559331	72.967258
539.433324	33.301371	72.972263
538.681512	32.739924	72.977268
537.635403	37.665835	72.982273
537.309789	24.775711	72.987278
536.964473	36.790345	72.992282
535.964889	34.956343	72.997287
535.163700	23.875045	73.002292
534.356517	30.543272	73.007297
534.079862	35.029648	73.012302
533.719480	35.862953	73.017306
532.665778	40.599265	73.022311
531.903699	31.527077	73.027316
531.427821	39.736830	73.032321
530.861387	28.667020	73.037326
529.722618	37.382913	73.042330
528.989275	37.988624	73.047335
528.843402	32.989312	73.052340
528.150836	39.238741	73.057345
527.680529	38.408527	73.062350
526.653480	42.418354	73.067354
525.924333	40.402505	73.072359
525.735705	30.295953	73.077364
524.313589	33.578659	73.082369
523.868957	21.700980	73.087374
523.182771	32.546197	73.092378
522.433528	30.702286	73.097383
522.824606	26.096834	73.102388
521.552413	28.638146	73.107393
520.794114	21.353627	73.112398
520.422561	23.704160	73.117402
519.345382	30.768637	73.122407
518.625396	34.105078	73.127412
517.371423	35.076002	73.132417
517.012817	26.480443	73.137422
517.119331	34.300953	73.142426
516.450053	29.476485	73.147431
516.019237	30.719980	73.152436
514.807063	40.138278	73.157441
514.486671	29.314706	73.162446
513.325586	36.178090	73.167450
512.263188	35.774937	73.172455
512.101059	35.643108	73.177460
511.202404	38.247923	73.182465
511.494541	29.510852	73.187470
510.250759	36.168214	73.192474
509.421524	37.508296	73.197479
509.391868	28.999106	73.202484
508.313890	23.181617	73.207489
507.799373	26.978911	73.212494
506.865963	23.536933	73.217498
506.244765	25.715926	73.222503
505.325500	24.357998	73.227508
503.810541	33.200059	73.232513
503.867172	19.493696	73.237518
503.293597	39.207088	73.242522
502.587223	31.324520	73.247527
502.435622	32.572422	73.252532
502.391617	34.675236	73.257537
501.485120	35.037304	73.262542
500.503154	32.257496	73.267546
499.743660	26.963282	73.272551
498.879617	27.339088	73.277556
497.880663	37.961328	73.282561
497.452824	20.560081	73.287566
497.033199	24.728612	73.292570
496.366424	33.574325	73.297575
495.609062	25.084875	73.302580
494.796017	33.567538	73.307585
494.294534	31.297812	73.312590
494.081497	31.653487	73.317594
492.975041	36.395064	73.322599
492.528707	27.871833	73.327604
491.728151	40.337462	73.332609
491.463014	33.068999	73.337614
490.064647	34.299483	73.342618
489.263707	26.963419	73.347623
488.691419	31.214621	73.352628
488.396063	36.968693	73.357633
487.868781	36.723151	73.362638
487.169187	32.911192	73.367642
486.488001	36.459079	73.372647
486.081417	25.863714	73.377652
485.119722	32.113447	73.382657
484.240151	33.278629	73.387662
484.015951	32.641028	73.392666
483.221912	35.308033	73.397671
482.899152	29.423854	73.402676
481.903160	32.023685	73.407681
481.097215	38.527729	73.412686
480.593388	31.849229	73.417690
479.723976	43.635129	73.422695
478.953241	27.106946	73.427700
478.237785	38.122418	73.432705
477.626407	31.185087	73.437710
477.538465	38.659683	73.442714
476.158927	43.112039	73.447719
475.638013	28.343356	73.452724
475.291701	39.006706	73.457729
474.618758	35.100618	73.462734
474.254056	36.533860	73.467738
473.264540	27.561010	73.472743
472.608603	23.871413	73.477748
471.966119	37.516647	73.482753
470.992410	34.297144	73.487758
470.036629	25.564926	73.492762
469.651732	29.174420	73.497767
469.308085	30.875542	73.502772
468.800506	42.313638	73.507777
468.259644	39.264869	73.512782
467.111814	35.913836	73.517786
466.498949	42.434432	73.522791
466.408123	37.596666	73.527796
465.067331	42.244703	73.532801
464.440254	47.436621	73.537806
463.776673	43.647314	73.542810
463.231829	46.662554	73.547815
463.250260	40.736631	73.552820
461.873188	41.052261	73.557825
461.397595	42.397517	73.562830
460.953080	44.259791	73.567834
460.134780	42.467901	73.572839
458.928125	39.944680	73.577844
458.395278	39.649568	73.582849
458.270829	38.780035	73.587854
457.566984	34.839452	73.592858
456.179601	39.119602	73.597863
455.700286	36.242381	73.602868
455.226266	40.801209	73.607873
454.536310	38.712907	73.612878
454.367305	37.356887	73.617882
453.325638	34.676496	73.622887
452.608233	34.629987	73.627892
451.536161	48.983921	73.632897
451.399007	37.082493	73.637902
450.803203	30.841278	73.642906
449.972210	41.575545	73.647911
449.553836	34.795127	73.652916
449.006331	42.546372	73.657921
448.518370	28.081532	73.662926
447.423899	28.205487	73.667930
446.195910	34.068732	73.672935
445.860500	38.834135	73.677940
445.769610	35.969145	73.682945
445.232288	41.914738	73.687950
444.246476	31.979370	73.692954
443.722249	40.345069	73.697959
443.043834	38.786364	73.702964
441.788312	37.593998	73.707969
441.395662	33.291603	73.712974
440.911411	36.737160	73.717978
440.383511	48.214770	73.722983
439.748752	38.021617	73.727988
438.913005	48.641532	73.732993
438.431134	39.221956	73.737998
437.266006	40.826891	73.743002
436.322157	35.391761	73.748007
435.933272	32.826565	73.753012
435.369487	37.511661	73.758017
435.351069	36.729313	73.763022
434.977280	36.019357	73.768026
433.415177	53.190538	73.773031
433.172479	39.293740	73.778036
432.095373	43.581236	73.783041
431.202465	43.222075	73.788046
430.558321	41.132788	73.793050
430.020738	43.855142	73.798055
429.649261	35.955507	73.803060
429.087486	48.761576	73.808065
428.702272	41.282018	73.813070
427.857907	33.541312	73.818074
426.958136	45.477141	73.823079
426.447144	41.307143	73.828084
424.995725	39.874765	73.833089
424.400862	41.655345	73.838094
424.167357	34.869132	73.843098
423.877410	45.616546	73.848103
423.568535	38.689376	73.853108
422.574165	36.397276	73.858113
421.560320	37.049290	73.863118
421.284736	37.783943	73.868122
420.283247	35.180743	73.873127
419.596892	34.086933	73.878132
418.822020	37.946230	73.883137
418.364416	32.039394	73.888142
418.072346	33.043178	73.893146
416.851609	43.152006	73.898151
416.228687	31.260183	73.903156
415.712104	46.747747	73.908161
415.311926	36.042565	73.913166
414.789018	36.398736	73.918170
413.757129	40.992846	73.923175
412.942237	35.087748	73.928180
412.619815	35.746286	73.933185
411.688837	41.350911	73.938190
410.822629	28.550112	73.943194
409.970346	41.009807	73.948199
409.778245	30.236782	73.953204
409.429857	44.294059	73.958209
408.817838	39.417921	73.963214
407.914099	34.690771	73.968218
407.152195	46.193054	73.973223
406.513928	40.316582	73.978228
405.396206	45.900505	73.983233
404.631587	42.999370	73.988238
404.261766	40.112597	73.993242
403.724822	45.731709	73.998247
403.906913	40.866229	74.003252
402.746461	48.811348	74.008257
401.580699	40.716585	74.013262
401.301020	37.213055	74.018266
400.775932	42.190036	74.023271
399.675176	38.205486	74.028276
399.008455	40.890075	74.033281
398.524720	46.253129	74.038286
398.257546	43.584965	74.043290
397.416327	47.431188	74.048295
396.580378	36.503714	74.053300
395.744203	41.992313	74.058305
395.243757	39.943216	74.063310
395.044379	38.992586	74.068314
393.977015	42.570494	74.073319
393.357667	37.782262	74.078324
392.992042	42.178748	74.083329
391.542027	47.194310	74.088334
390.872932	43.032168	74.093338
390.330008	41.726276	74.098343
390.160152	34.985118	74.103348
389.543148	35.323173	74.108353
388.585973	41.931765	74.113358
387.493827	34.938609	74.118362
386.929482	54.369856	74.123367
386.791895	39.522765	74.128372
386.408064	43.726611	74.133377
385.606423	43.326115	74.138382
384.903705	40.722628	74.143386
384.147412	51.949637	74.148391
383.777362	32.195862	74.153396
382.601808	41.039097	74.158401
382.241004	35.085304	74.163406
381.646841	41.032079	74.168410
380.385155	42.624042	74.173415
379.705836	34.883862	74.178420
379.282186	37.045598	74.183425
378.843992	48.890540	74.188430
378.440884	32.907789	74.193434
377.609167	41.696234	74.198439
376.881773	34.529841	74.203444
376.134769	42.252963	74.208449
375.509701	43.167893	74.213454
374.345024	36.873850	74.218458
373.630898	40.523208	74.223463
373.543576	39.740802	74.228468
373.355954	38.944419	74.233473
372.445231	36.508124	74.238478
371.497546	37.570660	74.243482
370.715874	42.262106	74.248487
370.246768	37.968755	74.253492
369.078324	43.011996	74.258497
367.989096	41.722205	74.263502
368.021141	38.011309	74.268506
367.225183	43.375236	74.273511
367.364870	34.727108	74.278516
366.786554	40.236122	74.283521
365.707526	39.581795	74.288526
365.286634	36.395663	74.293530
364.251561	39.588392	74.298535
363.220664	40.170607	74.303540
362.711171	39.037589	74.308545
362.090463	37.146437	74.313550
361.898820	32.581791	74.318554
361.036124	41.510794	74.323559
360.205672	41.129091	74.328564
359.713201	45.110558	74.333569
359.410632	34.413491	74.338574
358.296944	36.942240	74.343578
357.185638	49.466885	74.348583
356.973177	33.214063	74.353588
356.341645	40.347931	74.358593
355.602032	38.278611	74.363598
354.818441	34.897972	74.368602
354.041770	45.749761	74.373607
353.954464	33.843564	74.378612
353.434246	31.715628	74.383617
352.201909	36.185586	74.388622
351.364293	39.329505	74.393626
350.986853	39.560005	74.398631
350.715906	32.869658	74.403636
349.866013	43.509189	74.408641
349.087058	34.389300	74.413646
348.867525	42.460450	74.418650
347.286611	42.679320	74.423655
346.644425	41.316717	74.428660
346.204500	43.586708	74.433665
345.777363	37.602493	74.438670
345.515781	37.738836	74.443674
344.225505	43.627825	74.448679
343.444053	29.693918	74.453684
342.866458	33.029787	74.458689
342.592139	43.826748	74.463694
342.350681	34.482430	74.468698
340.734530	42.498617	74.473703
340.562519	41.589362	74.478708
340.155702	39.433892	74.483713
338.736040	36.373826	74.488718
338.185064	33.996906	74.493722
337.547093	41.136535	74.498727
337.334265	40.312633	74.503732
336.724408	46.862737	74.508737
335.738398	41.517947	74.513742
334.964028	40.398764	74.518746
334.660500	41.122110	74.523751
334.068585	30.387589	74.528756
333.384781	42.766833	74.533761
332.107982	35.822058	74.538766
331.892724	36.222254	74.543770
331.493134	36.743292	74.548775
330.486889	36.175151	74.553780
329.484018	30.506627	74.558785
328.992399	32.128848	74.563790
328.655115	33.374813	74.568794
328.030219	30.653287	74.573799
327.213204	33.689851	74.578804
326.650668	39.016585	74.583809
325.569949	40.174457	74.588814
325.148987	38.519561	74.593818
325.044274	36.960917	74.598823
324.003513	36.883980	74.603828
323.430582	34.513717	74.608833
322.558987	41.236422	74.613838
321.488260	33.479799	74.618842
320.656304	43.156117	74.623847
320.382215	41.320118	74.628852
319.887828	41.011023	74.633857
319.503703	36.682062	74.638862
319.331163	36.614982	74.643866
317.843057	41.248724	74.648871
317.282340	32.762692	74.653876
316.384569	35.977710	74.658881
315.918206	41.401082	74.663886
315.609932	30.853171	74.668890
314.460235	40.316781	74.673895
314.061669	35.660541	74.678900
313.744666	39.579354	74.683905
312.584348	42.929260	74.688910
311.908817	30.585395	74.693914
311.419874	48.011356	74.698919
311.114644	35.337232	74.703924
310.225214	48.208149	74.708929
309.134017	44.442891	74.713934
308.511731	39.139490	74.718938
308.285488	41.419584	74.723943
307.380481	35.926281	74.728948
306.646972	32.425714	74.733953
305.622484	49.897612	74.738958
305.397633	29.081519	74.743962
305.206693	44.570798	74.748967
304.468542	39.475099	74.753972
303.498958	44.180745	74.758977
302.843632	45.751795	74.763982
302.110419	43.074346	74.768986
301.039032	37.798375	74.773991
300.661333	47.279296	74.778996
300.039118	41.928577	74.784001
299.391090	48.522619	74.789006
299.338340	42.360469	74.794010
298.025802	46.830622	74.799015
297.562368	41.735293	74.804020
297.372979	36.367629	74.809025
295.973412	40.589880	74.814030
295.318415	39.248257	74.819034
294.761804	41.973669	74.824039
294.560835	36.866470	74.829044
293.462856	47.274324	74.834049
292.354243	39.230440	74.839054
292.038297	29.276690	74.844058
291.237257	46.719280	74.849063
291.028140	42.851282	74.854068
290.723328	41.966352	74.859073
289.506747	49.359068	74.864078
289.122292	35.781370	74.869082
288.296085	39.516422	74.874087
287.874187	33.283807	74.879092
286.683901	30.510487	74.884097
285.797069	38.449879	74.889102
286.202063	29.024612	74.894106
284.769716	34.929962	74.899111
283.989083	36.334909	74.904116
283.637228	37.600549	74.909121
283.012694	35.881915	74.914126
283.123820	29.632150	74.919130
281.558931	32.664933	74.924135
281.134898	32.168013	74.929140
280.610417	31.986724	74.934145
279.482710	34.511433	74.939150
278.547544	28.086247	74.944154
277.727370	31.422948	74.949159
277.494325	20.624943	74.954164
277.362524	37.940350	74.959169
276.826283	38.312867	74.964174
276.018912	34.612773	74.969178
274.977128	34.187514	74.974183
274.626709	34.547759	74.979188
273.448246	32.559457	74.984193
272.533455	38.541589	74.989198
272.396815	31.091838	74.994202
271.626401	35.642743	74.999207
271.433758	20.443352	75.004212
270.782083	25.361678	75.009217
269.696509	33.316982	75.014222
269.152797	26.534514	75.019226
268.445962	31.086322	75.024231
267.646362	30.504192	75.029236
266.913307	26.642447	75.034241
266.245144	31.881948	75.039246
266.019885	27.839912	75.044250
265.381812	35.646615	75.049255
264.399081	28.593508	75.054260
263.809677	30.576679	75.059265
263.213861	28.698934	75.064270
262.700950	29.611781	75.069274
261.703519	34.984194	75.074279
261.035897	23.392875	75.079284
260.485929	27.377210	75.084289
259.975878	28.912496	75.089294
259.265842	23.571065	75.094298
258.544637	30.220925	75.099303
257.875701	26.817316	75.104308
257.802736	16.742850	75.109313
256.409050	32.428566	75.114318
256.076226	27.189431	75.119322
255.355938	30.005593	75.124327
254.317508	27.209661	75.129332
253.491460	33.494616	75.134337
252.688168	28.765714	75.139342
252.593026	25.136599	75.144346
252.095743	30.826677	75.149351
251.870499	23.093014	75.154356
250.570383	31.661261	75.159361
249.948605	32.171998	75.164366
249.687095	21.370652	75.169370
248.144765	34.017644	75.174375
247.311792	28.631158	75.179380
246.884254	21.264057	75.184385
246.395321	32.850577	75.189390
246.060729	31.563549	75.194394
245.769877	26.962695	75.199399
245.139988	32.390064	75.204404
244.116358	31.979271	75.209409
243.530523	36.095484	75.214414
243.023795	21.581677	75.219418
241.554644	28.393349	75.224423
241.029009	25.255482	75.229428
240.734802	18.348098	75.234433
240.352543	30.051651	75.239438
239.674715	29.148921	75.244442
238.750662	23.587727	75.249447
238.037671	31.535685	75.254452
237.474652	31.981865	75.259457
236.527822	31.328598	75.264462
235.960404	22.402123	75.269466
235.227123	29.020797	75.274471
235.120117	34.746434	75.279476
234.554804	22.640502	75.284481
233.202012	26.101546	75.289486
232.766564	25.849304	75.294490
232.278757	28.399755	75.299495
231.539290	24.671508	75.304500
230.671512	35.146756	75.309505
230.009637	31.128596	75.314510
229.789835	21.380313	75.319514
228.499552	25.244553	75.324519
227.733222	35.094928	75.329524
227.383698	29.345953	75.334529
226.597393	31.207557	75.339534
226.709693	24.345755	75.344538
225.551360	33.224146	75.349543
224.966494	31.056084	75.354548
224.275702	32.632805	75.359553
223.715925	31.957264	75.364558
223.328735	27.753393	75.369562
221.790360	37.331036	75.374567
221.193658	33.373452	75.379572
221.041166	30.275450	75.384577
220.114971	26.919172	75.389582
219.329594	29.906569	75.394586
218.233093	37.762710	75.399591
218.148092	32.383147	75.404596
218.190409	31.573774	75.409601
216.811988	34.621024	75.414606
216.477793	26.671347	75.419610
215.354141	34.971783	75.424615
214.962294	31.689591	75.429620
214.661273	33.959534	75.434625
213.408011	41.192545	75.439630
212.885452	29.858810	75.444634
212.258426	39.817870	75.449639
211.872790	29.607169	75.454644
211.009893	27.939173	75.459649
209.954084	33.483335	75.464654
209.752909	25.181296	75.469658
209.166434	32.960858	75.474663
208.325256	31.734098	75.479668
207.596907	29.871188	75.484673
206.771260	35.981052	75.489678
206.896127	31.034808	75.494682
205.972936	31.913729	75.499687
204.922736	27.784023	75.504692
204.370258	22.341800	75.509697
203.897926	32.454388	75.514702
203.220438	27.610831	75.519706
202.161514	40.434671	75.524711
201.248265	37.405915	75.529716
201.426995	28.587571	75.534721
200.386654	33.020679	75.539726
199.494220	29.324715	75.544730
198.858678	36.238476	75.549735
198.581735	35.399578	75.554740
198.174194	31.290418	75.559745
197.018489	30.386618	75.564750
196.320916	30.113096	75.569754
195.529797	34.607397	75.574759
195.292545	37.810189	75.579764
194.782696	27.070521	75.584769
193.508048	36.136203	75.589774
192.645790	29.976973	75.594778
192.383400	31.788176	75.599783
191.871633	31.376222	75.604788
191.689308	27.874552	75.609793
190.606030	35.779056	75.614798
190.167155	31.055154	75.619802
189.189924	35.014584	75.624807
187.940362	22.191443	75.629812
187.297780	26.280442	75.634817
186.573670	35.442855	75.639822
186.407004	23.033687	75.644826
186.099237	33.153156	75.649831
185.683859	36.038995	75.654836
185.317253	27.958875	75.659841
183.933049	36.575253	75.664846
183.698884	21.559121	75.669850
182.412139	25.667246	75.674855
181.543106	32.350155	75.679860
181.282525	19.113877	75.684865
180.727373	21.572571	75.689870
179.859813	24.806469	75.694874
178.980592	30.909110	75.699879
178.319055	25.533166	75.704884
178.028147	28.645164	75.709889
177.376660	35.192466	75.714894
176.810985	32.644467	75.719898
175.869970	28.763870	75.724903
175.219605	26.224644	75.729908
175.148730	26.628641	75.734913
173.954366	26.609374	75.739918
173.414401	25.845531	75.744922
172.822425	27.392318	75.749927
172.011539	29.964329	75.754932
171.391846	27.864912	75.759937
170.424603	34.169248	75.764942
169.616892	28.252066	75.769946
169.586775	24.894863	75.774951
169.188893	34.661273	75.779956
168.360541	25.483110	75.784961
167.691729	34.911097	75.789966
166.940444	20.018423	75.794970
165.523285	23.332069	75.799975
165.224244	32.639597	75.804980
164.755847	22.189799	75.809985
164.625686	31.003625	75.814990
163.587247	31.752704	75.819994
162.486630	26.790547	75.824999
162.356956	32.401525	75.830004
161.764628	20.984322	75.835009
160.144293	34.903772	75.840014
159.895987	27.807732	75.845018
159.497788	30.695566	75.850023
158.648176	31.614811	75.855028
158.420125	28.377477	75.860033
157.200722	31.978141	75.865038
156.722148	27.123384	75.870042
156.334131	31.867234	75.875047
155.847789	33.851343	75.880052
154.896875	26.685984	75.885057
153.934265	29.851468	75.890062
153.585259	29.780999	75.895066
153.005051	37.067566	75.900071
152.072816	33.705970	75.905076
151.466630	34.720445	75.910081
150.783606	41.135589	75.915086
150.659229	28.869491	75.920090
149.382704	25.371984	75.925095
148.306115	29.823506	75.930100
148.106102	29.773435	75.935105
147.375159	24.935268	75.940110
147.366955	36.494031	75.945114
146.722806	27.213966	75.950119
145.769043	26.930845	75.955124
145.329480	19.773845	75.960129
143.870376	35.176728	75.965134
142.992153	26.555304	75.970138
142.563980	31.758141	75.975143
142.104786	30.923080	75.980148
141.602537	27.481889	75.985153
141.374216	41.967867	75.990158
140.682696	23.093349	75.995162
139.821595	25.566144	76.000167
139.053207	35.591906	76.005172
138.453514	20.689265	76.010177
136.979391	29.357845	76.015182
136.664908	27.619776	76.020186
136.226762	20.826825	76.025191
136.259276	28.665390	76.030196
135.632834	25.941013	76.035201
134.444076	30.295310	76.040206
133.856692	21.444592	76.045210
133.031815	25.835482	76.050215
131.726145	28.516363	76.055220
131.583017	21.253750	76.060225
130.835771	26.453849	76.065230
130.315733	32.761004	76.070234
130.322895	24.737993	76.075239
129.274895	20.639514	76.080244
128.729652	21.977009	76.085249
127.930052	32.520255	76.090254
126.990329	24.734964	76.095258
125.992406	27.437737	76.100263
125.627953	24.980668	76.105268
125.857037	24.824329	76.110273
124.563281	34.227397	76.115278
123.698506	31.321832	76.120282
123.453099	28.571391	76.125287
122.514773	37.217623	76.130292
121.486089	28.610738	76.135297
120.442947	34.523496	76.140302
120.129636	22.434192	76.145306
120.100814	28.232511	76.150311
119.723356	35.638139	76.155316
118.858975	30.948990	76.160321
117.710161	29.273005	76.165326
117.374447	26.470734	76.170330
116.683123	29.690742	76.175335
115.359350	25.508511	76.180340
114.729533	30.511695	76.185345
114.068395	28.713791	76.190350
113.970346	30.875683	76.195354
113.751710	19.654374	76.200359
112.626383	34.254997	76.205364
112.191947	34.294350	76.210369
111.603982	35.104080	76.215374
110.481587	37.889787	76.220378
109.730330	33.311911	76.225383
108.867213	31.738604	76.230388
108.983972	27.843898	76.235393
108.122156	35.407189	76.240398
107.434966	26.268043	76.245402
106.525241	18.878525	76.250407
105.933368	23.181803	76.255412
105.551372	25.190280	76.260417
104.291489	26.726898	76.265422
103.526423	24.625451	76.270426
103.158171	20.618858	76.275431
102.824190	28.812329	76.280436
102.529977	26.079136	76.285441
101.034617	37.925511	76.290446
100.274674	33.022596	76.295450
100.059712	22.437786	76.300455
99.685795	33.193850	76.305460
98.671301	23.085046	76.310465
97.596393	35.468339	76.315470
97.237513	30.851550	76.320474
96.698464	34.099320	76.325479
96.654913	31.392385	76.330484
95.710420	32.400899	76.335489
94.623506	35.884271	76.340494
94.362168	33.924845	76.345498
93.469999	29.662759	76.350503
92.369291	30.645724	76.355508
92.110916	21.736244	76.360513
91.453892	24.971288	76.365518
90.891871	33.467631	76.370522
89.932534	28.667482	76.375527
89.223880	34.930607	76.380532
88.874683	30.471546	76.385537
88.222675	34.762345	76.390542
87.889242	31.082934	76.395546
86.814962	31.549180	76.400551
85.793105	30.278739	76.405556
85.814895	18.587012	76.410561
84.551837	32.611946	76.415566
83.622086	20.043800	76.420570
82.992022	31.812108	76.425575
82.771751	35.478973	76.430580
82.664146	27.493190	76.435585
81.361226	31.681214	76.440590
80.647401	31.052351	76.445594
80.073260	23.456361	76.450599
79.553326	29.902276	76.455604
79.569661	22.776665	76.460609
78.326423	37.683109	76.465614
78.150715	28.090244	76.470618
77.189651	29.744800	76.475623
76.015588	32.344797	76.480628
75.600744	26.303498	76.485633
75.070513	32.350514	76.490638
74.382966	40.040565	76.495642
73.730544	26.570333	76.500647
72.789983	34.195076	76.505652
72.778820	26.812075	76.510657
71.290037	31.660523	76.515662
69.888301	30.395478	76.520666
69.760287	33.623432	76.525671
69.273419	31.947557	76.530676
69.219032	30.879218	76.535681
69.014702	38.782362	76.540686
68.177771	32.451989	76.545690
67.609413	34.668388	76.550695
66.525878	39.540519	76.555700
65.365933	30.752748	76.560705
64.674048	32.761768	76.565710
64.283553	31.799071	76.570714
63.872515	26.211328	76.575719
63.423148	31.854367	76.580724
62.662590	34.374231	76.585729
61.618789	40.742854	76.590734
60.921483	32.502615	76.595738
60.098992	33.956883	76.600743
59.002128	35.694605	76.605748
58.866844	21.601017	76.610753
58.407577	33.638555	76.615758
58.174252	39.885803	76.620762
57.547955	28.868286	76.625767
56.405630	36.646639	76.630772
56.071748	36.234729	76.635777
55.359081	37.753484	76.640782
54.115188	35.499762	76.645786
53.812567	30.877163	76.650791
53.136411	37.496233	76.655796
52.696978	25.676216	76.660801
51.385552	28.400633	76.665806
50.746149	28.660343	76.670810
50.156899	31.826242	76.675815
49.687671	33.115362	76.680820
49.438175	26.907351	76.685825
49.100099	25.478984	76.690830
48.139602	25.359401	76.695834
47.378104	22.036853	76.700839
46.361887	38.564466	76.705844
45.779437	25.292820	76.710849
44.845228	30.984804	76.715854
44.560262	27.994680	76.720858
44.558669	30.770389	76.725863
42.792012	38.023854	76.730868
42.738797	35.197038	76.735873
41.605715	36.558924	76.740878
41.256212	29.056425	76.745882
40.441848	18.379575	76.750887
39.478191	30.536982	76.755892
39.165579	20.147533	76.760897
38.522694	34.399998	76.765902
38.135064	30.443814	76.770906
37.568376	25.393408	76.775911
36.347655	36.352346	76.780916
35.883183	26.811854	76.785921
35.484035	31.691533	76.790926
34.532899	29.861058	76.795930
34.000619	30.628808	76.800935
33.414271	34.439217	76.805940
33.312962	33.001473	76.810945
32.245713	30.872554	76.815950
30.892832	27.691642	76.820954
30.497378	26.996245	76.825959
29.677550	24.700132	76.830964
29.529369	21.566771	76.835969
28.355986	38.557845	76.840974
27.773532	34.041383	76.845978
27.544837	32.120913	76.850983
26.886715	42.427157	76.855988
26.361988	31.798724	76.860993
24.991499	33.201637	76.865998
24.712811	31.855264	76.871002
24.331728	34.063879	76.876007
23.186759	40.114340	76.881012
22.832704	40.815819	76.886017
22.253454	32.712882	76.891022
21.655849	38.868425	76.896026
20.950182	28.825516	76.901031
19.787869	34.087119	76.906036
19.378181	32.826295	76.911041
18.379215	32.160931	76.916046
18.274299	30.042525	76.921050
17.470678	26.718820	76.926055
16.514633	34.986288	76.931060
16.306660	28.809505	76.936065
16.289925	31.112969	76.941070
14.902101	36.754317	76.946074
14.062650	23.667179	76.951079
13.749834	30.933192	76.956084
12.588678	33.304080	76.961089
11.565906	36.744140	76.966094
11.013012	28.217539	76.971098
10.720898	30.005113	76.976103
10.208623	27.718298	76.981108
9.886759	25.292302	76.986113
8.883591	27.404603	76.991118
7.837305	25.849512	76.996122
7.519175	26.400184	77.001127
6.923581	39.467140	77.006132
6.624689	35.518884	77.011137
5.416651	35.079260	77.016142
5.081597	32.940794	77.021147
4.529727	24.134916	77.026151
3.458174	27.645835	77.031156
2.977064	31.166652	77.036161