Fri Mar 05 20:07:21 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.012261	103.117214	0.000000
-0.087199	81.157533	0.005005
-1.187427	52.687791	0.010010
-2.568508	4.946952	0.015014
-5.993089	-17.127983	0.020019
-11.502025	-25.322945	0.025024
-16.290414	-18.517889	0.030029
-21.177688	-25.487363	0.035034
-25.369729	-28.530769	0.040038
-29.303134	-26.559768	0.045043
-33.016711	-19.943479	0.050048
-36.424403	-25.765970	0.055053
-40.330612	-27.552397	0.060058
-43.741565	-24.453628	0.065062
-47.455343	-18.155827	0.070067
-51.523310	-24.407547	0.075072
-55.204606	-26.349677	0.080077
-59.018184	-17.388261	0.085082
-62.654422	-25.705237	0.090086
-66.543136	-20.811358	0.095091
-70.179093	-21.852384	0.100096
-73.873915	-20.991689	0.105101
-78.002677	-26.268578	0.110106
-81.330116	-31.255413	0.115110
-85.346306	-19.568230	0.120115
-89.075006	-23.384030	0.125120
-92.612710	-29.521582	0.130125
-96.623919	-24.865155	0.135130
-100.177700	-22.345910	0.140134
-104.306905	-22.019831	0.145139
-107.800445	-18.122483	0.150144
-111.536469	-14.810906	0.155149
-115.578643	-23.931922	0.160154
-118.528419	-33.394378	0.165158
-122.753987	-21.618540	0.170163
-126.727821	-27.896185	0.175168
-130.540767	-36.484468	0.180173
-134.293468	-25.400646	0.185178
-138.227114	-31.728836	0.190182
-142.413619	-24.030843	0.195187
-145.815195	-20.099232	0.200192
-149.379656	-22.789981	0.205197
-153.099332	-19.091448	0.210202
-156.533148	-23.741086	0.215206
-160.622106	-21.434396	0.220211
-164.248977	-13.879280	0.225216
-168.106348	-24.901514	0.230221
-172.051172	-21.386220	0.235226
-175.559895	-27.473077	0.240230
-179.372287	-18.773445	0.245235
-183.184211	-16.771121	0.250240
-186.982577	-15.456920	0.255245
-190.643544	-11.751929	0.260250
-194.274720	-22.270906	0.265254
-198.118322	-13.454300	0.270259
-201.793460	-19.799988	0.275264
-205.611356	-18.843760	0.280269
-209.845802	-16.485383	0.285274
-213.370214	-21.885293	0.290278
-216.781462	-21.454410	0.295283
-220.768168	-23.636121	0.300288
-224.399721	-28.637293	0.305293
-228.271164	-23.058377	0.310298
-231.859286	-27.128195	0.315302
-235.884751	-19.096208	0.320307
-239.535807	-19.748218	0.325312
-243.015669	-34.869092	0.330317
-247.408540	-25.573674	0.335322
-250.810622	-37.698160	0.340326
-254.823213	-29.851127	0.345331
-258.497363	-35.302754	0.350336
-261.902597	-28.689619	0.355341
-266.024916	-23.783375	0.360346
-269.394308	-25.685073	0.365350
-273.493875	-31.532393	0.370355
-277.322647	-25.715789	0.375360
-280.800592	-29.930848	0.380365
-284.711958	-22.837926	0.385370
-288.294690	-36.437912	0.390374
-292.339911	-31.525010	0.395379
-296.221167	-32.649535	0.400384
-299.800088	-28.189519	0.405389
-303.756730	-19.260098	0.410394
-307.114774	-33.205002	0.415398
-311.143209	-27.034780	0.420403
-315.164203	-29.493128	0.425408
-318.893365	-30.175125	0.430413
-322.013871	-24.838944	0.435418
-325.544942	-26.670598	0.440422
-329.788019	-26.302300	0.445427
-333.707423	-22.037033	0.450432
-337.127698	-29.027152	0.455437
-341.419362	-25.762141	0.460442
-345.022655	-34.134380	0.465446
-348.594249	-28.934306	0.470451
-352.534335	-24.437052	0.475456
-355.998172	-34.728586	0.480461
-359.868917	-23.130437	0.485466
-363.786511	-22.708390	0.490470
-367.716000	-27.433115	0.495475
-371.672424	-24.346152	0.500480
-374.772928	-24.075044	0.505485
-378.728414	-20.858910	0.510490
-382.510192	-32.466839	0.515494
-386.339045	-31.557461	0.520499
-390.049265	-32.079947	0.525504
-393.872598	-26.915305	0.530509
-397.879256	-22.691197	0.535514
-401.024924	-32.904155	0.540518
-405.102410	-16.852791	0.545523
-408.848455	-16.341369	0.550528
-412.728634	-21.259973	0.555533
-416.951093	-24.529637	0.560538
-420.219858	-25.641377	0.565542
-423.827536	-29.001311	0.570547
-427.375778	-26.463554	0.575552
-431.230187	-26.608143	0.580557
-435.071301	-22.161253	0.585562
-439.079450	-27.281722	0.590566
-442.848048	-18.147150	0.595571
-446.606554	-16.771100	0.600576
-450.295858	-31.664233	0.605581
-454.347519	-21.725941	0.610586
-457.616698	-29.392857	0.615590
-461.537820	-17.975739	0.620595
-465.291010	-26.297045	0.625600
-468.915362	-31.980215	0.630605
-472.645339	-22.355037	0.635610
-476.090429	-31.681145	0.640614
-480.001548	-24.759845	0.645619
-484.206286	-24.581898	0.650624
-487.805523	-34.375369	0.655629
-492.138994	-29.050257	0.660634
-495.529949	-31.232034	0.665638
-499.266121	-17.209351	0.670643
-502.897354	-15.948156	0.675648
-506.261943	-18.376978	0.680653
-510.743885	-19.157637	0.685658
-514.267176	-33.671904	0.690662
-518.107145	-23.585976	0.695667
-522.092361	-20.320708	0.700672
-525.508066	-20.642446	0.705677
-529.108984	-17.571009	0.710682
-532.789318	-24.110873	0.715686
-536.597732	-20.514281	0.720691
-540.655418	-29.308786	0.725696
-544.306860	-22.679594	0.730701
-548.261201	-25.714308	0.735706
-551.963455	-23.990693	0.740710
-555.592207	-19.359920	0.745715
-559.389524	-15.618410	0.750720
-562.716036	-24.450828	0.755725
-567.231275	-20.921050	0.760730
-570.788378	-26.053417	0.765734
-574.240455	-24.543194	0.770739
-578.285548	-23.649428	0.775744
-581.889745	-23.215588	0.780749
-585.921225	-21.732636	0.785754
-589.248797	-21.797130	0.790758
-592.748494	-23.448896	0.795763
-596.841907	-23.296419	0.800768
-600.671607	-28.771537	0.805773
-605.022473	-19.624130	0.810778
-608.631540	-19.277779	0.815782
-612.178465	-14.811379	0.820787
-615.629996	-21.051779	0.825792
-619.232268	-18.289069	0.830797
-623.291917	-16.522438	0.835802
-626.958018	-29.553472	0.840806
-630.826576	-18.955035	0.845811
-634.805532	-21.178285	0.850816
-638.135066	-22.505515	0.855821
-642.125632	-12.929911	0.860826
-645.812886	-22.532455	0.865830
-649.553714	-23.144261	0.870835
-653.598064	-22.278871	0.875840
-657.067027	-24.958875	0.880845
-661.161321	-24.080761	0.885850
-664.701586	-27.534670	0.890854
-668.241332	-24.272532	0.895859
-672.272295	-30.547987	0.900864
-675.690166	-25.296311	0.905869
-679.566793	-17.437205	0.910874
-683.645340	-24.632272	0.915878
-687.789454	-24.222383	0.920883
-691.399149	-23.115729	0.925888
-694.389792	-23.360068	0.930893
-698.223689	-20.566537	0.935898
-701.698748	-19.553920	0.940902
-705.998166	-29.309267	0.945907
-709.896960	-23.260037	0.950912
-713.758982	-27.403608	0.955917
-717.472066	-20.512003	0.960922
-721.025597	-30.946325	0.965926
-724.823312	-26.633649	0.970931
-728.993728	-27.264985	0.975936
-732.135204	-32.930288	0.980941
-736.330313	-28.874202	0.985946
-739.893114	-28.151854	0.990950
-743.650917	-27.111335	0.995955
-747.397818	-20.368819	1.000960
-751.095221	-34.550521	1.005965
-755.241161	-34.228530	1.010970
-758.497960	-35.710712	1.015974
-762.584100	-20.278726	1.020979
-766.024730	-32.060365	1.025984
-769.966877	-38.436569	1.030989
-773.927475	-36.273937	1.035994
-777.532778	-35.730816	1.040998
-781.389357	-21.784685	1.046003
-785.433704	-25.709763	1.051008
-788.835033	-33.648377	1.056013
-792.867256	-24.969460	1.061018
-796.156457	-22.459950	1.066022
-799.701592	-23.960643	1.071027
-803.631734	-20.022483	1.076032
-807.395043	-23.751175	1.081037
-811.282303	-18.301280	1.086042
-815.107470	-29.606646	1.091046
-818.898379	-31.419676	1.096051
-822.997105	-22.189195	1.101056
-826.287092	-29.571552	1.106061
-830.214887	-21.839650	1.111066
-833.926626	-30.288384	1.116070
-837.867396	-30.705505	1.121075
-841.562126	-31.532528	1.126080
-845.165403	-33.642008	1.131085
-849.157323	-29.495209	1.136090
-852.612977	-28.472858	1.141094
-856.412170	-28.300735	1.146099
-860.278845	-22.421978	1.151104
-864.102202	-24.467863	1.156109
-868.225322	-28.736586	1.161114
-871.559382	-30.012297	1.166118
-875.414356	-19.141276	1.171123
-878.837690	-19.508591	1.176128
-882.635530	-22.662371	1.181133
-886.753942	-17.251092	1.186138
-890.445818	-26.395178	1.191142
-894.176202	-22.312193	1.196147
-897.923204	-22.258733	1.201152
-901.616332	-22.898263	1.206157
-905.705461	-18.105057	1.211162
-909.007270	-19.049988	1.216166
-912.797276	-19.259282	1.221171
-916.648949	-21.306861	1.226176
-920.254717	-29.912740	1.231181
-924.308377	-22.901718	1.236186
-928.005496	-24.909336	1.241190
-931.761369	-19.705757	1.246195
-935.459610	-14.793654	1.251200
-938.880917	-24.370423	1.256205
-942.811922	-20.028207	1.261210
-946.905744	-20.814903	1.266214
-950.754673	-25.467936	1.271219
-954.536831	-23.467575	1.276224
-958.028708	-32.990446	1.281229
-961.867010	-26.327607	1.286234
-965.719809	-24.435778	1.291238
-968.852172	-26.588833	1.296243
-972.738781	-20.850209	1.301248
-976.484192	-28.291976	1.306253
-981.024510	-18.698886	1.311258
-984.699124	-20.527090	1.316262
-988.324196	-27.551276	1.321267
-991.925973	-24.469551	1.326272
-995.509631	-26.673397	1.331277
-999.948794	-18.917791	1.336282
-1003.151977	-32.331290	1.341286
-1006.998836	-25.329551	1.346291
-1010.639384	-31.177995	1.351296
-1014.406368	-33.592183	1.356301
-1018.282948	-27.505017	1.361306
-1021.757244	-26.793244	1.366310
-1025.576293	-10.952554	1.371315
-1029.574962	-22.311800	1.376320
-1033.108672	-31.357940	1.381325
-1037.069503	-25.116923	1.386330
-1040.796655	-23.136260	1.391334
-1044.609864	-26.285735	1.396339
-1048.466932	-28.817921	1.401344
-1052.071038	-30.638370	1.406349
-1056.300666	-22.037835	1.411354
-1059.675739	-29.537119	1.416358
-1063.163521	-36.017024	1.421363
-1067.130397	-17.982799	1.426368
-1070.872905	-30.513586	1.431373
-1075.115561	-30.558751	1.436378
-1078.451492	-33.060707	1.441382
-1082.095749	-26.532794	1.446387
-1085.879450	-15.086237	1.451392
-1089.739724	-27.975039	1.456397
-1093.541205	-19.794579	1.461402
-1097.272979	-27.859629	1.466406
-1100.554032	-36.875112	1.471411
-1104.819758	-29.792024	1.476416
-1108.370778	-37.546928	1.481421
-1112.500358	-28.653229	1.486426
-1116.083889	-24.697469	1.491430
-1119.695197	-34.697704	1.496435
-1123.526717	-30.957723	1.501440
-1127.417959	-35.504337	1.506445
-1131.226552	-27.059339	1.511450
-1135.205300	-25.702159	1.516454
-1138.438510	-20.219186	1.521459
-1142.453025	-26.621010	1.526464
-1146.056351	-41.473067	1.531469
-1149.939915	-38.286100	1.536474
-1153.725626	-34.178095	1.541478
-1157.464772	-30.836028	1.546483
-1161.249231	-23.400916	1.551488
-1164.878081	-28.079333	1.556493
-1168.567360	-32.631383	1.561498
-1172.141323	-29.787219	1.566502
-1176.061274	-37.423063	1.571507
-1180.338346	-28.850996	1.576512
-1183.868264	-32.409831	1.581517
-1187.553340	-21.734249	1.586522
-1191.248674	-28.322670	1.591526
-1194.807770	-42.153570	1.596531
-1198.857755	-28.737257	1.601536
-1202.367394	-29.274785	1.606541
-1206.437411	-15.664437	1.611546
-1210.351573	-28.020862	1.616550
-1214.006184	-28.159869	1.621555
-1217.782557	-32.865054	1.626560
-1221.260416	-42.919582	1.631565
-1224.827721	-36.927310	1.636570
-1228.792995	-39.334644	1.641574
-1232.657040	-31.371039	1.646579
-1236.918145	-27.014941	1.651584
-1240.059373	-45.908296	1.656589
-1243.844981	-34.221520	1.661594
-1247.787951	-26.803486	1.666598
-1251.617327	-22.896487	1.671603
-1255.558739	-23.574567	1.676608
-1258.876073	-29.985252	1.681613
-1262.601937	-27.428872	1.686618
-1266.289867	-27.270735	1.691622
-1270.060569	-33.320270	1.696627
-1274.166187	-25.926624	1.701632
-1277.719890	-28.525896	1.706637
-1281.638106	-28.953760	1.711642
-1285.121610	-26.568593	1.716646
-1288.936186	-32.393461	1.721651
-1293.058900	-32.328117	1.726656
-1296.710332	-28.783833	1.731661
-1300.029762	-26.721364	1.736666
-1304.018401	-24.308935	1.741670
-1307.923240	-29.129023	1.746675
-1311.671209	-34.802089	1.751680
-1315.348113	-32.102079	1.756685
-1319.504884	-29.137602	1.761690
-1322.852963	-30.326840	1.766694
-1326.588958	-32.736012	1.771699
-1330.640206	-24.442670	1.776704
-1334.087919	-36.430411	1.781709
-1338.128201	-38.289399	1.786714
-1341.899930	-28.552178	1.791718
-1345.487212	-31.041893	1.796723
-1349.113852	-24.959512	1.801728
-1353.006623	-32.533165	1.806733
-1356.704380	-30.553554	1.811738
-1360.513970	-33.332502	1.816742
-1364.075031	-29.630697	1.821747
-1367.924654	-21.405837	1.826752
-1371.731546	-28.977436	1.831757
-1375.851540	-28.931303	1.836762
-1379.453655	-31.863279	1.841766
-1382.746282	-26.878235	1.846771
-1386.920473	-23.409391	1.851776
-1390.707854	-31.633767	1.856781
-1394.418302	-24.593332	1.861786
-1398.281238	-21.611102	1.866790
-1401.843880	-30.961085	1.871795
-1405.956007	-24.274206	1.876800
-1409.580332	-28.812605	1.881805
-1413.233396	-22.557167	1.886810
-1416.847967	-26.929964	1.891814
-1420.335944	-30.389491	1.896819
-1424.445255	-25.835015	1.901824
-1428.133074	-32.075743	1.906829
-1432.211490	-26.417632	1.911834
-1435.975074	-28.410633	1.916838
-1439.688383	-27.199510	1.921843
-1443.331982	-30.302932	1.926848
-1446.775386	-39.255624	1.931853
-1450.626871	-25.594728	1.936858
-1454.581655	-31.914088	1.941862
-1458.303022	-24.969575	1.946867
-1462.495541	-21.606468	1.951872
-1465.746542	-25.225293	1.956877
-1469.738530	-20.747869	1.961882
-1473.495260	-27.764367	1.966886
-1476.997428	-24.388781	1.971891
-1480.811340	-18.742977	1.976896
-1484.479883	-26.095269	1.981901
-1488.561111	-30.456298	1.986906
-1492.426324	-24.505804	1.991910
-1495.571173	-27.003054	1.996915
-1499.733899	-24.027177	2.006912
-1500.839216	-26.104874	2.016909
-1498.396597	-25.600772	2.026906
-1495.314915	-32.259975	2.036902
-1493.306987	-26.687367	2.046899
-1491.759429	-22.387861	2.056896
-1489.619575	-26.351004	2.066893
-1487.371102	-26.516845	2.076890
-1485.550331	-26.247882	2.086886
-1483.882229	-26.368151	2.096883
-1482.223762	-28.931058	2.106880
-1479.933809	-35.635562	2.116877
-1478.180885	-31.206305	2.126874
-1476.154008	-38.069203	2.136870
-1474.286507	-31.509368	2.146867
-1472.422475	-26.968424	2.156864
-1470.551450	-31.761649	2.166861
-1468.744413	-37.150935	2.176858
-1466.574756	-33.219446	2.186854
-1464.737452	-36.804122	2.196851
-1463.228536	-30.755273	2.206848
-1461.087902	-35.162193	2.216845
-1459.339713	-28.038508	2.226842
-1457.521942	-32.365307	2.236838
-1455.319681	-34.840006	2.246835
-1453.585883	-30.189774	2.256832
-1451.283458	-31.818412	2.266829
-1449.661336	-32.343394	2.276826
-1447.729301	-32.676421	2.286822
-1446.141223	-37.673792	2.296819
-1444.465486	-40.026281	2.306816
-1442.532156	-39.759518	2.316813
-1440.410831	-35.119221	2.326810
-1438.585659	-35.604076	2.336806
-1436.327868	-33.857696	2.346803
-1434.659459	-37.110574	2.356800
-1433.094339	-38.797983	2.366797
-1430.850874	-35.940896	2.376794
-1428.854372	-32.232696	2.386790
-1427.245848	-38.559629	2.396787
-1425.408564	-31.480182	2.406784
-1423.427290	-31.415288	2.416781
-1421.453055	-36.501312	2.426778
-1419.577596	-38.318924	2.436774
-1417.740784	-40.117716	2.446771
-1416.103011	-35.628922	2.456768
-1414.255369	-35.452625	2.466765
-1412.189786	-35.939634	2.476762
-1410.178431	-39.640554	2.486758
-1408.513878	-37.745485	2.496755
-1406.536306	-37.768403	2.506752
-1404.740133	-37.506492	2.516749
-1402.609587	-34.882348	2.526746
-1400.742171	-32.632913	2.536742
-1398.966037	-37.279840	2.546739
-1397.061422	-32.723225	2.556736
-1395.651155	-29.761131	2.566733
-1393.543001	-36.918025	2.576730
-1391.317687	-34.782721	2.586726
-1389.593111	-29.464652	2.596723
-1387.586950	-33.292616	2.606720
-1385.703434	-33.126777	2.616717
-1384.097876	-28.021752	2.626714
-1382.236124	-33.863415	2.636710
-1380.071388	-42.180393	2.646707
-1378.250119	-34.201509	2.656704
-1376.569199	-32.048513	2.666701
-1374.241655	-34.195828	2.676698
-1372.646281	-34.192269	2.686694
-1371.097741	-35.224885	2.696691
-1369.071655	-37.055518	2.706688
-1366.999900	-38.443465	2.716685
-1365.245848	-40.653700	2.726682
-1363.265432	-42.734382	2.736678
-1361.260446	-41.705346	2.746675
-1359.540196	-37.752337	2.756672
-1357.972900	-33.994313	2.766669
-1355.672136	-35.336805	2.776666
-1353.878807	-36.991220	2.786662
-1352.027429	-31.322371	2.796659
-1350.219583	-34.134885	2.806656
-1348.473034	-40.496494	2.816653
-1346.675103	-35.535921	2.826650
-1344.354754	-38.155733	2.836646
-1342.545916	-32.536908	2.846643
-1340.547287	-37.250987	2.856640
-1338.850831	-31.009438	2.866637
-1337.066322	-33.590841	2.876634
-1335.229321	-28.964927	2.886630
-1333.411971	-32.380523	2.896627
-1331.247622	-32.736428	2.906624
-1329.254043	-36.854432	2.916621
-1327.442272	-35.350759	2.926618
-1325.791932	-35.907013	2.936614
-1323.953480	-43.000149	2.946611
-1322.310790	-35.561049	2.956608
-1320.465698	-39.203704	2.966605
-1317.970683	-39.489366	2.976602
-1316.398450	-41.206258	2.986598
-1314.376417	-39.226234	2.996595
-1312.446471	-38.131460	3.006592
-1310.930573	-36.218841	3.016589
-1308.887348	-36.902704	3.026586
-1307.008224	-38.068715	3.036582
-1305.167795	-37.973281	3.046579
-1303.010713	-38.798518	3.056576
-1301.250126	-34.904024	3.066573
-1299.668472	-40.806580	3.076570
-1297.884816	-35.147373	3.086566
-1295.616738	-35.388795	3.096563
-1294.096404	-41.112588	3.106560
-1291.855345	-33.295552	3.116557
-1289.885789	-34.277078	3.126554
-1288.086792	-35.772878	3.136550
-1286.157393	-39.346895	3.146547
-1284.707739	-31.875289	3.156544
-1282.728251	-31.855777	3.166541
-1280.658779	-27.634914	3.176538
-1278.754149	-33.824411	3.186534
-1276.747548	-27.095611	3.196531
-1275.248382	-30.948131	3.206528
-1273.285843	-30.679584	3.216525
-1271.469505	-33.656028	3.226522
-1269.123741	-36.035101	3.236518
-1267.673749	-37.331348	3.246515
-1265.866359	-35.179562	3.256512
-1263.859544	-37.018073	3.266509
-1261.725373	-31.386508	3.276506
-1260.115802	-33.628807	3.286502
-1258.141197	-30.515363	3.296499
-1256.283112	-30.430610	3.306496
-1254.487282	-31.291147	3.316493
-1252.483951	-33.686455	3.326490
-1250.705853	-32.036805	3.336486
-1249.099799	-32.405920	3.346483
-1246.940406	-32.838321	3.356480
-1244.994789	-27.039196	3.366477
-1243.294798	-32.756976	3.376474
-1241.215543	-38.713865	3.386470
-1239.177586	-37.039477	3.396467
-1237.625668	-28.486843	3.406464
-1235.617420	-33.039746	3.416461
-1233.703324	-30.548170	3.426458
-1231.816983	-31.178439	3.436454
-1230.188507	-38.267910	3.446451
-1228.222472	-34.905176	3.456448
-1226.402026	-29.681263	3.466445
-1224.618667	-35.447107	3.476442
-1222.669431	-32.166942	3.486438
-1220.187260	-38.178814	3.496435
-1218.773049	-36.969855	3.506432
-1217.053738	-32.313957	3.516429
-1215.136944	-32.262249	3.526426
-1212.823881	-29.960811	3.536422
-1211.242696	-32.258535	3.546419
-1209.366469	-31.726651	3.556416
-1207.551855	-25.811794	3.566413
-1205.735541	-33.434988	3.576410
-1203.750264	-35.423159	3.586406
-1201.832338	-31.891652	3.596403
-1199.816891	-30.602043	3.606400
-1198.455560	-27.166207	3.616397
-1196.468481	-32.934629	3.626394
-1194.246999	-27.058021	3.636390
-1192.535650	-29.395507	3.646387
-1190.525830	-27.912360	3.656384
-1188.725012	-32.471509	3.666381
-1186.845394	-30.460688	3.676378
-1185.158008	-24.457560	3.686374
-1182.899584	-24.125753	3.696371
-1181.015710	-33.321307	3.706368
-1179.321363	-24.298787	3.716365
-1177.516401	-26.337033	3.726362
-1175.693976	-32.788036	3.736358
-1173.890313	-32.779772	3.746355
-1171.963102	-29.181829	3.756352
-1169.748534	-30.518243	3.766349
-1168.235517	-28.985589	3.776346
-1166.216595	-34.596451	3.786342
-1164.184512	-35.644717	3.796339
-1162.630485	-26.444998	3.806336
-1160.506101	-31.520102	3.816333
-1158.843826	-29.739746	3.826330
-1156.869926	-26.831359	3.836326
-1154.857874	-29.098508	3.846323
-1153.216433	-26.211138	3.856320
-1151.186412	-23.818563	3.866317
-1149.245166	-25.063861	3.876314
-1147.876035	-26.508151	3.886310
-1145.609249	-24.387132	3.896307
-1143.558706	-18.659962	3.906304
-1141.838120	-19.281009	3.916301
-1139.925261	-16.437049	3.926298
-1138.189843	-26.001982	3.936294
-1135.833032	-21.812740	3.946291
-1134.175719	-24.255224	3.956288
-1132.698063	-17.425872	3.966285
-1130.844917	-25.418066	3.976282
-1128.517022	-29.805707	3.986278
-1126.944049	-24.185278	3.996275
-1124.857659	-20.942756	4.006272
-1123.208701	-26.410716	4.016269
-1121.350997	-26.420530	4.026266
-1119.083798	-30.324771	4.036262
-1117.138209	-26.398143	4.046259
-1115.594943	-25.708708	4.056256
-1113.937621	-26.542244	4.066253
-1111.867058	-25.907159	4.076250
-1109.708777	-32.124476	4.086246
-1108.053277	-23.964097	4.096243
-1106.204991	-19.158214	4.106240
-1104.499084	-26.133684	4.116237
-1102.228712	-29.496841	4.126234
-1100.780583	-27.525871	4.136230
-1098.510886	-33.435740	4.146227
-1097.178391	-25.034210	4.156224
-1094.948147	-27.350423	4.166221
-1092.906982	-24.528529	4.176218
-1090.978175	-17.813947	4.186214
-1089.581839	-22.821479	4.196211
-1087.609802	-25.247960	4.206208
-1085.300776	-25.543096	4.216205
-1083.497702	-30.040952	4.226202
-1081.571071	-23.485489	4.236198
-1079.880659	-29.733730	4.246195
-1078.129513	-22.736512	4.256192
-1076.063498	-20.447520	4.266189
-1074.000250	-21.255959	4.276186
-1072.760051	-26.806924	4.286182
-1070.598978	-22.791565	4.296179
-1068.651264	-20.960483	4.306176
-1066.814709	-24.434217	4.316173
-1064.712705	-22.548864	4.326170
-1063.008231	-24.065691	4.336166
-1060.912416	-32.289277	4.346163
-1059.244104	-27.891936	4.356160
-1057.659485	-22.707526	4.366157
-1055.511386	-21.900057	4.376154
-1053.563112	-35.255268	4.386150
-1051.615556	-30.342063	4.396147
-1049.976547	-31.542096	4.406144
-1048.158052	-26.826138	4.416141
-1046.159270	-27.191612	4.426138
-1044.487193	-28.205879	4.436134
-1042.405729	-25.241964	4.446131
-1040.227256	-26.000908	4.456128
-1038.670585	-27.074081	4.466125
-1036.869020	-17.271223	4.476122
-1034.727548	-26.700508	4.486118
-1032.839714	-28.789794	4.496115
-1031.245037	-24.882755	4.506112
-1029.479759	-23.594037	4.516109
-1027.541237	-28.918775	4.526106
-1025.111298	-30.818442	4.536102
-1023.513626	-31.302903	4.546099
-1021.726447	-23.862983	4.556096
-1019.985844	-25.387136	4.566093
-1018.027712	-23.478731	4.576090
-1016.117361	-27.480541	4.586086
-1014.308452	-27.097205	4.596083
-1012.316280	-26.438442	4.606080
-1010.540520	-22.271402	4.616077
-1008.590921	-25.580014	4.626074
-1006.879125	-29.709535	4.636070
-1004.564374	-27.896046	4.646067
-1002.988425	-26.910185	4.656064
-1001.092039	-29.003972	4.666061
-999.304170	-28.254104	4.676058
-997.270610	-16.484640	4.686054
-995.273102	-25.957186	4.696051
-993.691599	-27.091141	4.706048
-991.791663	-23.333943	4.716045
-989.763963	-28.218179	4.726042
-988.210460	-28.457132	4.736038
-986.206328	-35.507054	4.746035
-983.979872	-30.371551	4.756032
-982.196002	-31.771543	4.766029
-980.513756	-32.231605	4.776026
-978.653552	-26.756474	4.786022
-976.458800	-28.492167	4.796019
-974.895628	-33.339999	4.806016
-973.004438	-36.727661	4.816013
-971.047191	-36.061699	4.826010
-969.124886	-36.294879	4.836006
-967.409022	-38.441875	4.846003
-965.723170	-39.170922	4.856000
-963.355875	-32.557929	4.865997
-961.872824	-38.242408	4.875994
-959.816340	-34.582850	4.885990
-957.989379	-32.175001	4.895987
-955.993757	-31.739371	4.905984
-954.238623	-24.529532	4.915981
-952.465851	-28.086138	4.925978
-950.437710	-22.896781	4.935974
-948.472443	-30.185198	4.945971
-946.545209	-30.024413	4.955968
-944.786342	-28.273555	4.965965
-942.785440	-30.627164	4.975962
-941.441370	-33.616267	4.985958
-939.186731	-33.252040	4.995955
-937.338499	-34.452291	5.005952
-935.714186	-29.540982	5.015949
-933.432025	-35.196906	5.025946
-931.486199	-29.787531	5.035942
-929.493516	-31.623502	5.045939
-927.924223	-36.303337	5.055936
-926.170214	-35.380631	5.065933
-924.146619	-34.924184	5.075930
-922.400850	-34.915943	5.085926
-920.397591	-29.285216	5.095923
-918.322243	-33.594382	5.105920
-916.746435	-32.011601	5.115917
-914.937367	-34.642408	5.125914
-913.008431	-27.719271	5.135910
-910.991864	-34.677966	5.145907
-908.962447	-34.104016	5.155904
-907.694212	-33.154154	5.165901
-905.219105	-37.555645	5.175898
-903.273324	-32.653078	5.185894
-901.360014	-42.222608	5.195891
-899.883380	-26.074036	5.205888
-897.940814	-27.205656	5.215885
-896.142918	-39.466192	5.225882
-894.213516	-34.046265	5.235878
-892.174897	-31.081679	5.245875
-890.466054	-28.383312	5.255872
-888.739348	-28.207788	5.265869
-886.502190	-23.238104	5.275866
-884.973633	-32.802957	5.285862
-882.740686	-34.833616	5.295859
-881.171881	-37.909141	5.305856
-879.089299	-32.611584	5.315853
-877.151161	-35.136683	5.325850
-875.117648	-32.603894	5.335846
-873.498731	-35.480585	5.345843
-871.950005	-33.700813	5.355840
-869.725723	-27.162747	5.365837
-867.851924	-30.042288	5.375834
-865.942509	-25.560186	5.385830
-864.016332	-30.499142	5.395827
-862.278036	-36.314369	5.405824
-860.264515	-30.099442	5.415821
-858.665333	-33.434019	5.425818
-856.591623	-34.978147	5.435814
-854.574766	-38.587911	5.445811
-852.895650	-30.541632	5.455808
-850.958392	-32.360783	5.465805
-849.398953	-34.144797	5.475802
-847.160477	-36.261570	5.485798
-845.180568	-32.698612	5.495795
-843.348506	-33.094104	5.505792
-841.794298	-32.939918	5.515789
-839.681619	-33.047109	5.525786
-837.766891	-29.851091	5.535782
-836.270924	-33.298627	5.545779
-834.213790	-28.795902	5.555776
-832.112968	-32.816965	5.565773
-830.422504	-31.711924	5.575770
-828.557161	-30.721678	5.585766
-826.293316	-33.946167	5.595763
-824.749467	-30.046644	5.605760
-823.011682	-25.702859	5.615757
-820.989144	-26.087729	5.625754
-818.985133	-35.136443	5.635750
-817.189857	-29.502376	5.645747
-815.371957	-31.131894	5.655744
-813.419233	-38.364515	5.665741
-811.823390	-32.081201	5.675738
-809.615646	-39.371951	5.685734
-807.694317	-38.142745	5.695731
-805.952087	-35.280706	5.705728
-804.097484	-39.552912	5.715725
-802.328169	-31.056802	5.725722
-800.258333	-31.488688	5.735718
-798.416737	-31.871459	5.745715
-796.615086	-33.008893	5.755712
-794.623115	-28.148349	5.765709
-792.789274	-27.696195	5.775706
-791.076078	-35.724197	5.785702
-789.120018	-33.963686	5.795699
-787.080924	-30.421189	5.805696
-785.353942	-35.920347	5.815693
-783.592382	-36.132420	5.825690
-781.599332	-32.603085	5.835686
-779.625599	-31.645914	5.845683
-777.724984	-33.923358	5.855680
-776.032241	-32.738116	5.865677
-774.070611	-32.937949	5.875674
-772.210598	-33.675747	5.885670
-770.220578	-36.325894	5.895667
-768.501195	-28.745454	5.905664
-766.316881	-31.306652	5.915661
-764.729074	-34.042511	5.925658
-762.779350	-31.889387	5.935654
-760.913492	-35.103891	5.945651
-758.990252	-38.123880	5.955648
-757.349113	-33.207234	5.965645
-755.704213	-27.822239	5.975642
-753.392910	-38.454745	5.985638
-751.470201	-35.594666	5.995635
-749.600171	-37.521411	6.005632
-747.801181	-38.502068	6.015629
-746.050602	-36.021842	6.025626
-744.013867	-27.873155	6.035622
-741.935843	-34.386805	6.045619
-740.323365	-38.470269	6.055616
-738.379581	-34.121447	6.065613
-736.889846	-38.651081	6.075610
-734.332041	-37.010374	6.085606
-732.783187	-36.571051	6.095603
-730.968630	-37.470499	6.105600
-729.058309	-39.874192	6.115597
-727.108123	-37.605850	6.125594
-725.427062	-32.439770	6.135590
-723.594112	-34.057413	6.145587
-721.410570	-34.300560	6.155584
-719.631586	-33.823793	6.165581
-717.634639	-37.155528	6.175578
-715.827070	-33.282285	6.185574
-714.164889	-37.326308	6.195571
-712.041854	-35.232416	6.205568
-710.301223	-35.352669	6.215565
-708.441573	-36.605095	6.225562
-706.361221	-40.873829	6.235558
-704.768613	-35.043076	6.245555
-702.788052	-34.063247	6.255552
-700.893359	-34.247586	6.265549
-698.999712	-34.033862	6.275546
-696.906872	-33.676705	6.285542
-695.496419	-42.542052	6.295539
-693.486170	-44.601686	6.305536
-691.549843	-37.704800	6.315533
-689.572015	-38.413991	6.325530
-687.679227	-36.648021	6.335526
-685.835876	-32.349420	6.345523
-683.866827	-36.808772	6.355520
-682.002365	-31.275650	6.365517
-680.273781	-29.715539	6.375514
-678.591273	-36.865410	6.385510
-676.580072	-32.604674	6.395507
-674.656307	-32.067323	6.405504
-672.676591	-36.474687	6.415501
-670.878318	-35.977282	6.425498
-668.722497	-40.745937	6.435494
-667.079615	-42.870007	6.445491
-665.520507	-33.424409	6.455488
-663.362751	-39.762839	6.465485
-661.467231	-36.645709	6.475482
-659.499527	-37.279048	6.485478
-657.597463	-36.626111	6.495475
-655.817747	-37.158357	6.505472
-654.101205	-38.921558	6.515469
-652.464898	-39.396152	6.525466
-649.899674	-32.966024	6.535462
-648.197514	-42.285323	6.545459
-646.663668	-34.733564	6.555456
-644.542823	-42.378182	6.565453
-642.564044	-38.532236	6.575450
-640.762137	-40.452750	6.585446
-638.999163	-38.596526	6.595443
-637.174989	-32.433247	6.605440
-635.098018	-34.760861	6.615437
-633.298762	-39.875149	6.625434
-631.459567	-41.613719	6.635430
-629.627847	-36.899532	6.645427
-627.774217	-37.100936	6.655424
-625.915521	-36.343150	6.665421
-624.265858	-34.413548	6.675418
-621.782314	-27.405073	6.685414
-620.091982	-31.755111	6.695411
-618.569270	-33.845741	6.705408
-616.459916	-25.842743	6.715405
-614.458557	-26.085106	6.725402
-612.808923	-25.118647	6.735398
-610.726900	-29.599150	6.745395
-608.816429	-27.090678	6.755392
-607.034462	-25.109567	6.765389
-605.095004	-28.365713	6.775386
-603.323524	-32.523441	6.785382
-601.456355	-34.247511	6.795379
-599.698080	-34.289976	6.805376
-597.869881	-28.474672	6.815373
-595.830409	-24.619430	6.825370
-593.734327	-25.424803	6.835366
-592.198396	-24.967532	6.845363
-590.212458	-30.758983	6.855360
-588.043038	-31.997644	6.865357
-586.407825	-23.413609	6.875354
-584.395443	-28.602965	6.885350
-582.921892	-26.818883	6.895347
-580.945799	-23.621396	6.905344
-578.939643	-21.706077	6.915341
-576.980556	-25.816389	6.925338
-575.152168	-29.629505	6.935334
-573.003529	-29.713782	6.945331
-571.687749	-27.007649	6.955328
-569.720584	-22.308727	6.965325
-567.662759	-25.935858	6.975322
-565.760478	-32.173400	6.985318
-563.990531	-24.599290	6.995315
-561.654218	-27.421428	7.005312
-560.076364	-33.397141	7.015309
-558.604266	-30.221761	7.025306
-556.607591	-29.391223	7.035302
-554.249824	-23.974683	7.045299
-552.604885	-25.795850	7.055296
-550.890475	-23.494431	7.065293
-548.953282	-20.824386	7.075290
-547.106418	-20.091489	7.085286
-545.008161	-25.461901	7.095283
-543.299036	-27.288577	7.105280
-541.515263	-30.369806	7.115277
-539.391241	-31.634330	7.125274
-537.565510	-33.081732	7.135270
-535.692944	-32.954511	7.145267
-533.954029	-28.122786	7.155264
-532.109591	-29.535278	7.165261
-530.136899	-21.245102	7.175258
-528.395592	-23.612171	7.185254
-526.123878	-23.444485	7.195251
-524.586409	-19.193206	7.205248
-522.584982	-27.232343	7.215245
-520.612320	-27.278991	7.225242
-518.898280	-21.322228	7.235238
-517.068427	-27.352378	7.245235
-515.189162	-28.325156	7.255232
-513.268583	-26.716639	7.265229
-511.389219	-36.361003	7.275226
-509.746533	-32.721785	7.285222
-507.493159	-28.854839	7.295219
-505.606179	-27.788844	7.305216
-504.120962	-23.893943	7.315213
-501.998185	-24.809288	7.325210
-500.134912	-35.638444	7.335206
-498.237751	-38.775644	7.345203
-496.348471	-32.388961	7.355200
-494.405273	-27.755621	7.365197
-492.532644	-28.015217	7.375194
-491.104897	-29.009023	7.385190
-488.701893	-28.874902	7.395187
-486.846485	-33.649110	7.405184
-485.143049	-29.391154	7.415181
-483.422661	-31.115377	7.425178
-481.163015	-28.687826	7.435174
-479.458007	-31.615905	7.445171
-477.588462	-30.566050	7.455168
-475.691760	-26.365794	7.465165
-473.874196	-31.301318	7.475162
-471.983199	-29.438569	7.485158
-470.042544	-32.697959	7.495155
-468.089648	-33.560881	7.505152
-466.386581	-30.832852	7.515149
-464.717647	-32.908844	7.525146
-462.457358	-34.652956	7.535142
-460.895880	-33.675470	7.545139
-458.836055	-32.820198	7.555136
-456.962028	-29.506832	7.565133
-455.167400	-26.348153	7.575130
-453.079553	-29.695772	7.585126
-451.193763	-29.325859	7.595123
-449.320940	-36.318083	7.605120
-447.417220	-34.751031	7.615117
-445.678273	-33.103980	7.625114
-443.951789	-33.441253	7.635110
-441.921036	-36.089744	7.645107
-440.027583	-29.871046	7.655104
-438.442530	-32.235204	7.665101
-436.330310	-35.217227	7.675098
-434.347539	-30.163840	7.685094
-432.430614	-33.517305	7.695091
-430.684100	-36.883030	7.705088
-428.793346	-23.869677	7.715085
-427.188002	-32.175493	7.725082
-425.221511	-29.301603	7.735078
-423.114186	-28.232831	7.745075
-421.113568	-30.238600	7.755072
-419.296474	-28.397165	7.765069
-417.513722	-24.909717	7.775066
-415.843022	-26.258063	7.785062
-413.882955	-28.153140	7.795059
-412.002874	-25.657019	7.805056
-410.272782	-17.260097	7.815053
-408.332166	-20.306277	7.825050
-406.063513	-27.099574	7.835046
-404.367800	-32.915592	7.845043
-402.517732	-31.480463	7.855040
-400.573793	-22.167155	7.865037
-398.700301	-29.080506	7.875034
-397.069408	-27.567744	7.885030
-394.959634	-19.683015	7.895027
-393.046089	-23.193807	7.905024
-391.479037	-24.487693	7.915021
-389.382117	-25.285127	7.925018
-387.688343	-27.837139	7.935014
-385.490266	-26.804929	7.945011
-383.746705	-25.982779	7.955008
-382.084028	-21.906130	7.965005
-380.016314	-18.822571	7.975002
-377.958254	-23.207480	7.984998
-376.278654	-24.975642	7.994995
-374.363970	-24.878702	8.004992
-372.561436	-22.141220	8.014989
-370.841014	-19.218520	8.024986
-368.796658	-23.538075	8.034982
-366.720787	-28.805292	8.044979
-364.696033	-26.706443	8.054976
-363.155198	-23.447170	8.064973
-361.251882	-25.524198	8.074970
-359.495046	-27.100995	8.084966
-357.492358	-22.161242	8.094963
-356.014317	-24.530370	8.104960
-353.673686	-14.734030	8.114957
-351.871918	-20.249583	8.124954
-349.993266	-25.316353	8.134950
-348.128662	-20.133494	8.144947
-346.084037	-15.712004	8.154944
-344.262871	-17.234324	8.164941
-342.495766	-16.798008	8.174938
-340.759383	-21.463112	8.184934
-338.769564	-24.897619	8.194931
-336.838278	-20.822766	8.204928
-334.925273	-19.773419	8.214925
-333.375181	-25.087726	8.224922
-331.314959	-29.182414	8.234918
-329.241241	-29.061879	8.244915
-327.535173	-25.683698	8.254912
-325.494319	-22.448961	8.264909
-323.707216	-21.160032	8.274906
-321.917290	-21.651030	8.284902
-320.074218	-25.087358	8.294899
-318.136084	-23.587272	8.304896
-316.322601	-27.653612	8.314893
-314.376899	-23.996306	8.324890
-312.295576	-18.993276	8.334886
-310.517509	-24.667647	8.344883
-308.942995	-21.006345	8.354880
-306.883426	-21.071427	8.364877
-304.691787	-21.778118	8.374874
-302.877435	-23.187214	8.384870
-301.632571	-20.932234	8.394867
-299.501410	-18.506101	8.404864
-297.495458	-19.587356	8.414861
-295.342252	-19.684744	8.424858
-293.644646	-15.130444	8.434854
-291.863453	-21.466884	8.444851
-290.036740	-17.948457	8.454848
-288.077883	-15.166386	8.464845
-286.278442	-20.722574	8.474842
-284.302278	-23.150646	8.484838
-282.363295	-24.601726	8.494835
-280.603457	-26.669999	8.504832
-278.807294	-22.180370	8.514829
-276.834579	-21.675772	8.524826
-275.054502	-24.746748	8.534822
-273.178269	-20.798844	8.544819
-271.279707	-23.552413	8.554816
-269.227259	-26.711071	8.564813
-267.328006	-21.808413	8.574810
-265.600189	-23.077353	8.584807
-263.547373	-14.346557	8.594803
-261.711804	-21.187447	8.604800
-260.034717	-21.827757	8.614797
-258.171173	-9.411469	8.624794
-256.279611	-20.934993	8.634791
-254.189192	-20.933902	8.644787
-252.496576	-15.402982	8.654784
-250.506863	-15.426866	8.664781
-248.993195	-25.626904	8.674778
-246.848576	-18.903385	8.684775
-244.909014	-25.323489	8.694771
-242.929624	-26.774671	8.704768
-241.204315	-21.297911	8.714765
-239.608646	-22.572583	8.724762
-237.366712	-21.430393	8.734759
-235.508506	-20.146429	8.744755
-233.694773	-25.335386	8.754752
-231.818705	-28.865338	8.764749
-229.833410	-19.261629	8.774746
-228.053931	-25.394066	8.784743
-226.148960	-29.487575	8.794739
-224.248217	-27.131968	8.804736
-222.250057	-26.992966	8.814733
-220.374649	-34.204918	8.824730
-218.537464	-30.269686	8.834727
-216.632085	-27.382707	8.844723
-214.916598	-31.139649	8.854720
-213.113093	-31.490628	8.864717
-211.179289	-23.511324	8.874714
-209.385025	-31.957691	8.884711
-207.468131	-31.535707	8.894707
-205.294069	-22.819475	8.904704
-203.645021	-31.631085	8.914701
-201.766257	-26.282997	8.924698
-199.868425	-30.073767	8.934695
-198.060108	-32.476561	8.944691
-196.151344	-31.806954	8.954688
-194.306399	-30.495580	8.964685
-192.688963	-25.701044	8.974682
-190.559072	-32.235164	8.984679
-188.805576	-29.003397	8.994675
-186.751109	-30.818621	9.004672
-184.931721	-26.316835	9.014669
-183.056324	-29.016114	9.024666
-181.038332	-33.340783	9.034663
-179.205821	-31.353200	9.044659
-177.473447	-27.925421	9.054656
-175.461613	-28.952251	9.064653
-173.568394	-33.808057	9.074650
-171.748212	-30.233233	9.084647
-169.982687	-28.830219	9.094643
-168.076883	-35.385403	9.104640
-166.052389	-33.196340	9.114637
-164.255288	-21.604641	9.124634
-162.489635	-27.638510	9.134631
-160.546511	-32.657008	9.144627
-158.469961	-29.066240	9.154624
-157.061657	-30.844646	9.164621
-155.014083	-25.168191	9.174618
-152.722558	-34.142291	9.184615
-151.028076	-22.073151	9.194611
-149.358599	-33.704842	9.204608
-147.275601	-22.364012	9.214605
-145.278433	-30.053238	9.224602
-143.780041	-23.919666	9.234599
-141.953815	-32.579511	9.244595
-139.524517	-34.272926	9.254592
-138.445933	-32.873962	9.264589
-136.446290	-24.391937	9.274586
-134.344937	-24.529856	9.284583
-132.206073	-32.150101	9.294579
-130.389822	-27.920930	9.304576
-128.544052	-22.774358	9.314573
-126.526249	-23.091571	9.324570
-125.041522	-25.513734	9.334567
-122.994614	-23.009261	9.344563
-121.046914	-26.689508	9.354560
-119.031385	-20.924221	9.364557
-117.483071	-25.878115	9.374554
-115.669208	-22.657502	9.384551
-113.588430	-26.872136	9.394547
-111.738011	-22.250504	9.404544
-110.022186	-21.998467	9.414541
-107.990475	-18.307339	9.424538
-106.045841	-19.474970	9.434535
-104.089034	-30.415109	9.444531
-102.319909	-22.005220	9.454528
-100.480464	-31.339782	9.464525
-98.456604	-31.560043	9.474522
-96.941862	-18.573227	9.484519
-94.814343	-20.422136	9.494515
-92.951597	-20.518792	9.504512
-91.239208	-22.091465	9.514509
-89.213065	-21.857344	9.524506
-87.123165	-23.237610	9.534503
-85.497366	-25.431204	9.544499
-83.731249	-26.884548	9.554496
-81.802186	-27.350198	9.564493
-79.871050	-23.516684	9.574490
-78.147980	-27.453168	9.584487
-75.980990	-25.765184	9.594483
-74.166293	-24.180467	9.604480
-72.436988	-27.587413	9.614477
-70.290728	-17.778708	9.624474
-68.635769	-18.214829	9.634471
-66.765828	-23.725272	9.644467
-64.627613	-20.084254	9.654464
-62.861876	-16.843288	9.664461
-61.110878	-25.765821	9.674458
-59.311325	-20.660766	9.684455
-57.283657	-30.633225	9.694451
-55.542247	-24.917311	9.704448
-53.512427	-24.497429	9.714445
-51.705529	-20.498808	9.724442
-49.917577	-28.457748	9.734439
-47.781736	-18.342621	9.744435
-46.066196	-21.343141	9.754432
-44.279410	-23.720286	9.764429
-42.273589	-18.746016	9.774426
-40.541404	-23.422881	9.784423
-38.629893	-25.949392	9.794419
-36.498407	-23.763073	9.804416
-34.874409	-27.225827	9.814413
-32.977179	-27.727413	9.824410
-30.923110	-24.055575	9.834407
-29.250267	-32.345087	9.844403
-27.571824	-24.418043	9.854400
-25.369876	-22.637693	9.864397
-23.645497	-25.023815	9.874394
-21.571976	-19.766641	9.884391
-19.611724	-26.649357	9.894387
-17.913564	-28.672869	9.904384
-16.045195	-22.089802	9.914381
-14.159215	-29.813302	9.924378
-12.288489	-23.020606	9.934375
-10.412705	-22.617170	9.944371
-8.508560	-26.899861	9.954368
-6.868699	-26.738266	9.964365
-5.247216	-1.169897	9.974362
-3.949507	31.362858	9.984359
-2.400071	67.447683	9.994355
-0.966714	122.746665	10.004352
0.000000	176.783490	10.009357
0.702409	208.011968	10.014362
1.183845	243.817422	10.019367
1.681216	269.035805	10.024371
2.011894	294.213010	10.029376
2.015419	327.112846	10.034381
2.831122	343.197209	10.039386
3.217393	366.708270	10.044391
3.408179	366.024973	10.049395
3.295900	373.530387	10.054400
3.463760	380.473871	10.059405
3.459301	383.574931	10.064410
3.351968	384.817370	10.069415
3.658828	383.245065	10.074419
3.650448	389.822419	10.079424
3.566161	398.042484	10.084429
4.130747	399.065784	10.089434
4.112955	422.368567	10.094439
4.111487	416.008825	10.099443
4.463568	426.018568	10.104448
4.246233	418.948919	10.109453
4.081026	409.297320	10.114458
3.716132	405.230137	10.119463
4.211353	420.165620	10.124467
4.226587	434.092711	10.129472
4.137988	446.382117	10.134477
4.637924	444.318529	10.139482
4.578145	447.444196	10.144487
4.434592	444.415626	10.149491
4.608280	444.996644	10.154496
4.615979	441.997566	10.159501
4.676774	443.577477	10.164506
4.378491	440.859023	10.169511
4.395728	448.053650	10.174515
4.598386	449.103144	10.179520
4.703664	455.987259	10.184525
4.631976	457.440066	10.189530
4.710542	461.668063	10.194535
4.411849	469.428769	10.199539
4.507636	464.814991	10.204544
4.542199	470.404644	10.209549
4.644837	472.662298	10.214554
4.799879	490.405540	10.219559
4.936087	487.393840	10.224563
5.149013	493.835015	10.229568
5.140876	511.134366	10.234573
5.394496	497.815624	10.239578
5.258005	518.589074	10.244583
5.214782	516.344022	10.249587
5.554825	510.095351	10.254592
5.162403	514.459991	10.259597
5.259041	517.183822	10.264602
5.250332	511.936975	10.269607
5.148657	503.371192	10.274611
5.469944	513.218746	10.279616
5.099304	526.475748	10.284621
5.676319	522.233062	10.289626
5.908443	548.878843	10.294631
5.687194	535.413454	10.299635
5.732141	527.734197	10.304640
5.813383	546.392898	10.309645
6.154040	555.235208	10.314650
5.870851	562.913064	10.319655
5.928189	551.247526	10.324659
5.952140	551.967553	10.329664
6.159880	560.107225	10.334669
6.443092	556.174750	10.339674
5.981124	557.467461	10.344679
6.028765	560.494015	10.349683
6.161559	558.960495	10.354688
6.047118	568.503838	10.359693
6.261440	569.135151	10.364698
6.159418	572.185580	10.369703
6.162162	577.927011	10.374707
6.641793	573.370249	10.379712
6.302639	570.956342	10.384717
6.375711	578.580535	10.389722
6.053328	580.331969	10.394727
6.114968	581.864450	10.399731
6.565409	591.959548	10.404736
6.571072	603.136456	10.409741
6.738639	605.602979	10.414746
6.514532	614.949371	10.419751
6.596007	616.004013	10.424755
7.085853	614.456116	10.429760
6.931852	619.859853	10.434765
6.963255	619.146772	10.439770
6.975921	624.642203	10.444775
6.691818	628.773550	10.449779
7.021318	626.182015	10.454784
6.827836	626.094605	10.459789
7.043951	625.243248	10.464794
6.888871	622.423067	10.469799
7.191943	638.927007	10.474803
7.392551	636.926907	10.479808
7.128317	642.990078	10.484813
7.287503	648.298138	10.489818
7.071840	652.241950	10.494823
7.296613	657.990577	10.499827
7.402421	659.147001	10.504832
7.272741	662.203437	10.509837
7.622621	658.310766	10.514842
7.471175	654.912812	10.519847
7.279904	658.868505	10.524851
7.734944	673.091542	10.529856
7.571852	683.642546	10.534861
7.873388	690.151679	10.539866
7.983461	691.007793	10.544871
8.047960	693.139095	10.549875
8.424333	689.773644	10.554880
7.651003	680.990022	10.559885
7.999950	689.603214	10.564890
7.928820	700.065442	10.569895
7.980594	698.063841	10.574899
8.188957	695.406458	10.579904
7.818935	695.392939	10.584909
8.161868	695.866544	10.589914
8.221304	703.204384	10.594919
8.201692	707.082245	10.599923
8.594456	702.298016	10.604928
8.116957	713.553652	10.609933
8.145534	703.568161	10.614938
8.102991	710.151109	10.619943
8.167798	722.906732	10.624947
8.508827	737.357761	10.629952
8.446328	739.671760	10.634957
8.697341	737.706186	10.639962
8.676215	746.342168	10.644967
8.713485	741.669824	10.649971
8.844448	737.987099	10.654976
8.569647	742.804575	10.659981
8.840648	738.897655	10.664986
8.748014	746.204576	10.669991
8.784632	762.237047	10.674995
9.142624	771.938568	10.680000
9.220890	784.018709	10.685005
9.556489	778.357286	10.690010
9.338290	770.119028	10.695015
9.135205	767.323822	10.700019
9.057464	764.388771	10.705024
9.170218	775.971373	10.710029
9.690625	773.729426	10.715034
9.456342	783.698897	10.720039
9.686730	782.178174	10.725043
9.774859	784.244217	10.730048
9.199206	775.386427	10.735053
9.520080	783.409614	10.740058
9.493882	787.408401	10.745063
9.357874	788.959814	10.750067
9.476413	789.313089	10.755072
9.457285	801.083911	10.760077
9.430645	789.732001	10.765082
9.646356	791.963784	10.770087
9.279148	802.468580	10.775091
9.716657	805.063976	10.780096
9.905048	820.348449	10.785101
10.148032	819.461255	10.790106
10.143126	822.005789	10.795111
10.245715	820.648956	10.800115
10.392445	821.421956	10.805120
10.191506	826.462655	10.810125
10.160339	824.434840	10.815130
10.536930	821.980847	10.820135
10.340901	823.280050	10.825139
10.521707	818.017057	10.830144
10.169202	827.190090	10.835149
10.368612	827.011624	10.840154
10.328390	835.005700	10.845159
10.465774	840.080754	10.850163
10.537751	830.883077	10.855168
10.416607	839.487756	10.860173
10.235940	829.833612	10.865178
10.369951	836.322221	10.870183
10.840080	851.113912	10.875187
10.797859	868.297692	10.880192
10.759325	866.340436	10.885197
10.910405	870.381936	10.890202
11.144625	863.058686	10.895207
10.834892	865.342750	10.900211
10.974660	869.269353	10.905216
10.832210	884.275486	10.910221
10.802576	865.136595	10.915226
10.823765	874.972335	10.920231
10.696142	876.139199	10.925235
10.938616	876.027985	10.930240
10.893162	889.484197	10.935245
11.381062	892.140961	10.940250
11.471566	899.237389	10.945255
11.561647	905.742498	10.950259
11.684308	896.156630	10.955264
11.565253	908.987476	10.960269
11.560029	900.923343	10.965274
11.559193	907.160664	10.970279
11.502587	907.937715	10.975283
11.643776	902.319869	10.980288
11.710496	906.018424	10.985293
12.076009	896.942629	10.990298
11.968790	909.091885	10.995303
11.970844	902.324492	11.000307
12.228028	905.806578	11.005312
12.034188	911.178928	11.010317
11.849775	914.591094	11.015322
12.168263	911.452458	11.020327
12.056751	905.460156	11.025331
12.696408	901.242066	11.030336
12.071796	907.392790	11.035341
12.067503	901.615213	11.040346
12.196561	909.449858	11.045351
12.123965	909.806813	11.050355
12.162576	899.407980	11.055360
12.160201	911.672987	11.060365
12.120972	904.606232	11.065370
12.434316	909.262139	11.070375
12.250649	907.846871	11.075379
12.333000	907.579838	11.080384
12.464728	923.691940	11.085389
12.987571	939.960885	11.090394
12.656379	941.477209	11.095399
12.509317	948.680943	11.100403
12.866259	956.291598	11.105408
12.805470	951.082862	11.110413
12.907387	953.211389	11.115418
12.842950	949.832606	11.120423
12.820049	959.924609	11.125427
12.971542	952.253367	11.130432
12.876700	957.972664	11.135437
13.149369	951.551614	11.140442
13.156706	942.939797	11.145447
12.859555	953.264783	11.150451
13.119336	949.118310	11.155456
12.876532	954.735042	11.160461
12.923949	948.247414	11.165466
13.243781	957.863679	11.170471
13.312020	969.119202	11.175475
13.284802	975.895380	11.180480
13.323786	978.486560	11.185485
13.567517	975.244710	11.190490
13.551536	979.782846	11.195495
13.557434	978.280562	11.200499
13.784845	982.514935	11.205504
13.459895	984.430838	11.210509
13.640317	988.382530	11.215514
13.588386	979.609823	11.220519
13.739911	979.284444	11.225523
13.892088	980.436652	11.230528
13.463301	991.798279	11.235533
13.562259	989.785958	11.240538
13.949998	1009.891408	11.245543
14.053076	1020.121064	11.250547
14.225305	1011.840895	11.255552
14.192600	1017.070882	11.260557
14.102022	1011.398492	11.265562
14.297690	1023.061113	11.270567
13.878900	1022.971787	11.275571
14.259551	1014.382390	11.280576
14.126500	1012.678324	11.285581
14.210846	1004.461066	11.290586
14.446643	1010.777390	11.295591
14.229518	1019.384869	11.300595
14.396597	1012.747231	11.305600
14.378410	1011.999461	11.310605
14.525058	1032.621243	11.315610
14.931603	1043.955337	11.320615
14.825165	1045.058907	11.325619
14.998349	1042.728792	11.330624
14.852195	1048.552509	11.335629
14.605898	1032.345003	11.340634
14.805158	1043.496102	11.345639
14.692111	1044.755278	11.350643
15.069391	1048.672435	11.355648
15.038389	1048.855591	11.360653
14.926693	1041.905990	11.365658
15.248365	1042.580132	11.370663
15.257035	1055.365503	11.375667
15.693151	1044.079942	11.380672
15.363099	1054.951177	11.385677
15.569843	1048.603682	11.390682
15.545776	1053.067433	11.395687
15.353119	1059.105165	11.400691
15.816682	1044.438754	11.405696
15.445084	1041.850156	11.410701
15.154992	1025.450934	11.415706
15.405872	1034.797533	11.420711
15.326810	1047.413952	11.425715
15.656206	1045.013185	11.430720
15.531317	1058.051688	11.435725
15.637145	1054.257768	11.440730
15.961491	1049.651508	11.445735
15.692799	1057.514979	11.450739
15.768772	1053.358367	11.455744
15.444177	1054.728562	11.460749
15.750497	1057.713960	11.465754
15.637441	1058.985755	11.470759
15.748063	1070.111587	11.475763
16.159658	1077.497532	11.480768
16.113481	1088.350323	11.485773
16.265315	1080.166416	11.490778
16.353216	1085.049162	11.495783
16.183737	1083.079644	11.500787
16.329737	1086.199436	11.505792
16.601149	1087.856219	11.510797
16.522664	1093.435756	11.515802
16.501333	1087.593009	11.520807
16.024101	1089.774503	11.525811
16.540200	1092.869962	11.530816
16.460483	1096.618732	11.535821
16.508625	1085.335094	11.540826
16.432898	1085.503305	11.545831
16.287369	1094.075752	11.550835
16.497504	1091.217729	11.555840
16.480778	1094.418675	11.560845
16.353945	1086.987310	11.565850
16.774350	1109.371268	11.570855
16.748348	1119.232048	11.575859
17.073649	1115.647551	11.580864
16.902078	1123.006677	11.585869
16.630178	1130.798154	11.590874
16.959108	1125.412071	11.595879
16.931717	1117.658880	11.600883
17.037146	1116.935545	11.605888
17.015285	1121.755381	11.610893
16.975553	1122.842009	11.615898
17.228312	1130.579768	11.620903
17.296760	1143.988083	11.625907
17.705592	1150.638018	11.630912
17.828321	1144.655568	11.635917
17.483376	1126.322039	11.640922
17.593520	1128.315229	11.645927
17.515941	1128.824382	11.650931
17.557141	1125.595877	11.655936
17.788219	1126.748129	11.660941
17.903534	1129.533757	11.665946
17.688612	1129.864529	11.670951
17.581687	1129.238147	11.675955
17.766346	1142.801403	11.680960
18.034520	1155.529700	11.685965
17.978183	1158.360060	11.690970
18.285183	1154.163417	11.695975
17.993510	1162.331829	11.700979
18.205779	1147.618656	11.705984
18.071457	1152.763967	11.710989
18.394333	1155.322515	11.715994
18.134008	1135.712248	11.720999
17.806465	1148.934553	11.726003
18.457077	1142.949914	11.731008
18.573984	1156.880406	11.736013
18.319926	1151.188302	11.741018
18.465840	1143.352257	11.746023
18.271643	1154.181395	11.751027
18.571515	1157.088990	11.756032
18.418031	1157.991900	11.761037
18.115541	1150.506512	11.766042
18.464106	1153.579817	11.771047
18.178844	1165.590516	11.776051
18.316655	1151.545275	11.781056
18.320731	1162.664515	11.786061
18.491008	1177.069096	11.791066
19.144943	1187.004413	11.796071
19.094075	1184.012947	11.801075
19.198131	1186.604825	11.806080
19.343600	1176.978861	11.811085
19.024857	1179.329069	11.816090
18.818369	1161.948038	11.821095
18.865282	1182.106513	11.826099
18.976089	1178.166676	11.831104
19.116822	1183.110420	11.836109
19.356310	1180.151497	11.841114
19.249588	1181.680931	11.846119
19.301506	1181.932871	11.851123
19.355078	1171.050452	11.856128
19.532261	1184.853077	11.861133
19.505075	1184.184010	11.866138
19.667832	1182.871167	11.871143
19.399369	1196.538287	11.876147
19.485493	1189.328389	11.881152
19.395754	1192.238204	11.886157
19.308465	1185.275180	11.891162
19.573386	1184.450704	11.896167
19.417772	1191.044019	11.901171
19.720843	1196.502809	11.906176
19.550665	1219.000059	11.911181
19.597490	1213.411338	11.916186
19.934275	1215.854130	11.921191
19.713058	1225.716154	11.926195
19.966337	1214.188369	11.931200
20.025228	1218.664172	11.936205
19.881868	1207.921953	11.941210
20.212524	1219.651518	11.946215
19.978893	1219.977391	11.951219
20.319768	1205.131676	11.956224
20.337495	1212.821804	11.961229
20.569671	1217.247889	11.966234
20.652636	1207.431586	11.971239
20.196921	1225.052351	11.976243
20.477658	1206.429676	11.981248
20.223684	1217.859797	11.986253
20.129748	1217.269188	11.991258
20.366866	1227.763061	11.996263
20.424959	1244.540172	12.001267
20.820914	1238.673389	12.006272
20.778205	1234.409490	12.011277
20.600776	1237.080969	12.016282
21.066285	1240.444747	12.021287
20.744911	1236.914475	12.026291
20.957260	1240.572540	12.031296
21.247618	1235.720889	12.036301
21.154046	1222.251844	12.041306
20.815533	1216.344508	12.046311
20.882680	1221.867748	12.051315
21.137864	1207.456777	12.056320
20.725514	1220.992316	12.061325
21.018491	1213.404035	12.066330
21.079290	1211.292106	12.071335
20.632360	1210.671060	12.076339
21.260251	1213.253516	12.081344
20.931893	1214.141740	12.086349
20.968324	1207.048577	12.091354
20.893672	1193.261127	12.096359
20.512979	1183.480943	12.101363
20.656058	1179.942843	12.106368
20.564030	1183.854460	12.111373
20.541567	1198.212528	12.116378
20.665947	1202.054938	12.121383
20.805122	1206.898006	12.126387
20.810092	1204.337632	12.131392
20.728602	1215.699236	12.136397
20.922709	1212.488905	12.141402
20.797590	1198.755234	12.146407
20.734614	1189.460575	12.151411
20.717410	1179.827437	12.156416
20.784037	1187.370970	12.161421
20.373329	1186.095973	12.166426
20.941855	1191.121310	12.171431
20.871137	1212.041387	12.176435
20.680080	1198.389202	12.181440
20.404139	1199.967707	12.186445
20.745631	1205.139655	12.191450
20.515644	1217.196777	12.196455
20.805928	1217.385465	12.201459
21.265850	1205.799494	12.206464
20.795664	1207.139303	12.211469
20.573960	1195.554817	12.216474
20.808689	1192.416865	12.221479
20.614377	1192.323273	12.226483
20.760694	1191.273268	12.231488
20.519828	1196.399315	12.236493
20.745210	1206.190094	12.241498
20.918885	1216.683039	12.246503
20.414463	1209.508970	12.251507
21.049782	1213.157917	12.256512
20.802095	1203.969986	12.261517
20.213410	1197.528506	12.266522
20.711936	1197.696597	12.271527
20.857603	1221.047134	12.276531
20.882259	1225.634064	12.281536
20.983138	1231.809566	12.286541
20.777138	1209.987362	12.291546
20.751218	1196.307263	12.296551
20.694450	1196.092378	12.301555
20.759722	1192.131413	12.306560
20.312114	1197.470222	12.311565
20.613894	1209.817864	12.316570
20.628526	1217.267197	12.321575
20.807738	1229.230675	12.326579
20.815401	1225.054946	12.331584
20.859745	1234.317912	12.336589
21.025059	1227.901249	12.341594
20.699367	1207.498580	12.346599
20.578238	1201.277437	12.351603
20.868981	1194.608954	12.356608
20.585191	1194.521748	12.361613
20.766049	1194.131757	12.366618
20.710838	1189.092370	12.371623
20.516728	1198.551053	12.376627
21.089870	1206.442772	12.381632
20.898212	1213.418765	12.386637
20.592936	1201.519573	12.391642
20.582491	1191.506853	12.396647
20.501789	1202.906171	12.401651
20.996676	1214.751474	12.406656
21.055591	1216.726037	12.411661
20.624843	1207.608306	12.416666
20.862977	1201.776172	12.421671
20.768555	1200.688865	12.426675
20.557455	1200.150062	12.431680
20.945267	1206.622013	12.436685
20.676488	1197.347558	12.441690
21.026851	1197.706449	12.446695
20.936149	1203.306902	12.451699
20.957056	1204.945302	12.456704
20.771212	1205.577388	12.461709
20.880279	1206.741223	12.466714
20.980715	1204.962043	12.471719
20.743098	1205.163962	12.476723
20.833603	1197.480240	12.481728
20.680235	1208.061613	12.486733
20.745923	1207.169558	12.491738
20.947250	1200.414401	12.496743
20.724431	1211.468935	12.501747
20.962331	1203.526717	12.506752
20.859721	1206.217799	12.511757
20.763734	1203.804425	12.516762
20.828408	1201.983637	12.521767
20.872883	1208.582896	12.526771
20.731739	1189.552833	12.531776
20.802862	1181.656152	12.536781
20.480269	1178.742722	12.541786
20.746082	1190.127766	12.546791
20.659222	1205.928091	12.551795
20.899444	1200.628674	12.556800
20.705613	1193.644789	12.561805
20.792809	1194.671751	12.566810
20.760906	1188.824341	12.571815
20.703621	1196.786642	12.576819
20.714954	1191.979508	12.581824
20.818372	1202.936268	12.586829
20.545907	1191.851927	12.591834
20.827963	1187.253947	12.596839
20.663857	1205.479507	12.601843
20.731700	1197.624344	12.606848
20.829429	1199.945978	12.611853
20.632512	1196.403751	12.616858
20.875276	1189.717688	12.621863
20.721895	1189.228032	12.626867
20.706375	1175.812818	12.631872
20.708181	1184.208843	12.636877
20.474844	1180.391710	12.641882
21.042236	1189.599610	12.646887
21.081777	1204.908230	12.651891
20.615901	1183.696838	12.656896
20.712372	1181.762163	12.661901
20.627925	1179.118278	12.666906
20.810768	1176.952193	12.671911
20.515062	1181.364685	12.676915
20.909007	1176.077031	12.681920
20.679202	1187.859690	12.686925
20.796938	1186.979836	12.691930
20.856613	1181.641410	12.696935
20.489540	1186.964214	12.701939
20.746595	1191.900448	12.706944
20.616428	1191.977988	12.711949
20.353222	1186.585395	12.716954
20.842741	1196.703072	12.721959
20.834865	1204.980796	12.726963
21.048937	1203.563565	12.731968
20.705184	1199.432854	12.736973
20.628160	1192.936578	12.741978
20.855761	1180.879865	12.746983
20.801981	1184.763303	12.751987
21.022069	1187.787717	12.756992
20.720707	1187.211268	12.761997
20.651129	1195.312733	12.767002
20.617389	1183.622578	12.772007
20.852860	1191.683272	12.777011
20.791541	1192.200873	12.782016
21.173405	1189.198737	12.787021
20.954689	1195.270646	12.792026
21.280264	1182.658948	12.797031
21.351971	1192.365411	12.802035
21.312753	1187.741396	12.807040
21.080010	1162.072329	12.812045
20.789550	1151.139133	12.817050
20.836643	1153.773210	12.822055
20.474851	1157.256304	12.827059
20.776273	1156.591600	12.832064
20.728741	1153.473443	12.837069
20.351903	1156.339151	12.842074
20.310018	1145.897783	12.847079
20.702338	1167.720146	12.852083
20.763136	1175.469622	12.857088
20.501728	1178.443088	12.862093
20.812977	1187.535712	12.867098
20.825680	1188.049392	12.872103
20.878379	1201.906584	12.877107
21.070325	1174.857635	12.882112
21.017197	1171.592122	12.887117
20.878661	1163.397707	12.892122
21.079479	1157.413836	12.897127
21.024708	1159.102151	12.902131
20.997009	1161.674036	12.907136
21.149013	1159.404054	12.912141
20.832343	1157.372841	12.917146
20.860880	1158.543207	12.922151
20.741379	1167.108391	12.927155
20.752160	1160.673824	12.932160
20.731592	1167.231395	12.937165
20.598027	1167.527112	12.942170
20.959326	1163.640373	12.947175
20.894299	1161.149523	12.952179
20.710641	1147.377926	12.957184
20.677867	1141.618989	12.962189
20.707210	1139.102051	12.967194
20.883181	1139.955567	12.972199
20.591599	1152.907193	12.977203
20.496157	1145.970721	12.982208
20.797701	1161.141305	12.987213
20.680201	1164.210095	12.992218
20.916138	1156.776031	12.997223
20.839025	1165.203556	13.002227
20.753621	1157.845978	13.007232
20.446562	1149.881891	13.012237
20.727987	1153.633003	13.017242
21.081470	1149.264933	13.022247
20.694240	1146.924831	13.027251
20.451170	1145.530053	13.032256
20.831410	1143.753565	13.037261
20.596679	1151.908157	13.042266
21.006153	1156.367451	13.047271
20.836855	1161.508881	13.052275
20.820830	1145.160433	13.057280
20.862492	1141.233212	13.062285
20.681142	1137.521348	13.067290
21.087180	1139.793797	13.072295
20.539514	1142.682018	13.077299
20.346428	1137.033814	13.082304
20.581410	1140.905879	13.087309
20.667236	1139.078571	13.092314
20.703995	1143.811789	13.097319
20.779102	1166.853350	13.102323
20.732688	1159.576290	13.107328
20.476548	1163.195510	13.112333
20.966308	1159.392369	13.117338
21.262506	1158.015665	13.122343
20.655589	1155.781569	13.127347
20.805341	1145.830067	13.132352
21.060573	1138.739888	13.137357
20.737902	1139.641395	13.142362
20.767127	1139.769211	13.147367
20.887393	1130.126796	13.152371
21.171817	1137.962018	13.157376
20.822016	1141.763340	13.162381
20.957595	1149.589190	13.167386
21.128436	1134.799053	13.172391
20.574748	1145.579859	13.177395
20.544708	1146.769030	13.182400
20.687539	1139.909682	13.187405
20.601074	1141.554161	13.192410
20.811043	1143.889425	13.197415
20.738046	1149.775636	13.202419
20.928923	1144.064611	13.207424
20.904083	1147.235322	13.212429
20.567478	1149.530022	13.217434
20.859735	1139.333429	13.222439
20.429908	1148.541075	13.227443
20.586156	1150.930643	13.232448
21.004858	1148.804220	13.237453
20.512598	1156.477882	13.242458
20.708736	1152.653762	13.247463
20.585829	1152.823190	13.252467
20.605665	1154.852868	13.257472
20.603916	1148.917080	13.262477
20.477066	1150.131154	13.267482
20.788746	1146.247603	13.272487
20.511380	1152.448706	13.277491
20.295946	1149.852528	13.282496
20.704314	1143.662081	13.287501
20.645156	1148.300204	13.292506
20.647153	1147.781036	13.297511
20.652079	1152.681771	13.302515
20.779989	1146.247453	13.307520
20.871841	1147.614315	13.312525
20.556772	1154.250394	13.317530
20.806874	1150.002899	13.322535
20.716192	1159.270007	13.327539
20.689771	1157.440098	13.332544
20.803285	1146.937672	13.337549
20.688005	1151.572130	13.342554
20.903194	1149.694224	13.347559
20.806838	1157.699007	13.352563
20.650532	1146.851658	13.357568
20.673371	1150.494192	13.362573
20.441089	1157.402517	13.367578
21.024105	1138.007843	13.372583
20.769441	1148.017085	13.377587
20.778586	1151.455208	13.382592
20.819938	1147.998000	13.387597
20.771964	1150.480070	13.392602
21.022254	1141.018774	13.397607
20.607937	1151.372049	13.402611
20.836574	1153.767420	13.407616
20.839368	1155.736733	13.412621
20.638784	1156.519413	13.417626
20.836419	1151.660499	13.422631
20.728670	1162.138363	13.427635
20.730040	1152.710453	13.432640
20.840390	1153.162822	13.437645
20.684248	1158.087671	13.442650
20.957674	1149.311857	13.447655
20.779803	1155.118596	13.452659
20.893834	1153.690517	13.457664
21.153855	1152.901520	13.462669
21.002545	1151.738128	13.467674
21.102702	1140.521849	13.472679
20.803138	1128.594996	13.477683
20.538268	1125.722836	13.482688
20.730804	1129.822456	13.487693
20.835345	1134.145862	13.492698
20.841401	1120.082240	13.497703
20.634120	1128.546276	13.502707
20.826719	1115.296633	13.507712
20.812114	1114.051512	13.512717
20.600811	1113.820272	13.517722
20.551808	1112.932322	13.522727
20.582939	1129.890233	13.527731
20.990935	1137.822448	13.532736
20.799347	1117.579878	13.537741
20.661390	1114.671707	13.542746
20.563430	1118.943823	13.547751
20.287321	1140.495840	13.552755
20.550686	1149.427332	13.557760
20.850487	1147.520160	13.562765
20.904144	1152.532979	13.567770
21.072575	1146.322450	13.572775
20.673540	1154.473286	13.577779
20.784074	1159.577968	13.582784
20.850177	1150.661743	13.587789
20.365923	1141.275024	13.592794
20.797905	1132.582748	13.597799
20.880207	1150.884064	13.602803
20.705425	1153.242847	13.607808
21.116692	1145.126342	13.612813
20.385673	1141.134691	13.617818
20.583592	1125.985405	13.622823
20.681487	1145.309318	13.627827
21.007502	1146.820194	13.632832
20.603744	1142.407312	13.637837
20.685001	1143.805828	13.642842
21.050590	1140.814184	13.647847
20.529484	1131.805536	13.652851
20.507963	1137.341309	13.657856
20.950667	1144.446341	13.662861
20.607972	1148.572984	13.667866
20.610378	1142.504063	13.672871
20.634558	1158.903258	13.677875
20.938371	1168.170533	13.682880
21.014779	1173.219157	13.687885
20.856133	1153.594225	13.692890
21.065692	1138.062997	13.697895
20.873325	1139.951464	13.702899
20.796691	1135.328703	13.707904
20.957976	1137.480907	13.712909
20.495248	1144.776089	13.717914
20.611534	1135.001832	13.722919
20.501052	1140.994950	13.727923
20.876206	1135.833319	13.732928
20.464764	1135.670273	13.737933
20.422722	1141.488461	13.742938
20.537449	1139.006794	13.747943
20.935353	1159.763737	13.752947
20.391770	1158.931012	13.757952
20.778745	1159.274600	13.762957
20.997477	1169.282474	13.767962
21.139215	1160.384144	13.772967
20.969095	1147.050388	13.777971
20.929666	1148.909732	13.782976
20.792644	1143.351939	13.787981
20.925633	1147.707084	13.792986
20.831155	1138.078413	13.797991
20.622917	1141.830346	13.802995
20.685780	1143.985633	13.808000
20.699941	1142.289612	13.813005
20.623020	1150.425342	13.818010
20.682495	1141.691542	13.823015
20.687570	1142.670093	13.828019
20.474137	1141.970805	13.833024
20.876726	1139.608816	13.838029
20.608763	1146.352503	13.843034
20.672419	1142.376039	13.848039
20.797051	1158.161505	13.853043
20.618987	1147.005367	13.858048
20.859989	1135.594728	13.863053
20.421984	1142.404961	13.868058
20.744761	1143.889543	13.873063
20.687396	1147.043362	13.878067
20.713319	1138.617712	13.883072
20.773161	1139.186954	13.888077
20.546237	1146.603810	13.893082
20.726781	1141.760243	13.898087
20.643420	1147.329539	13.903091
20.760153	1146.736873	13.908096
21.011474	1145.572345	13.913101
20.888713	1147.985913	13.918106
20.861860	1146.810556	13.923111
20.705780	1161.502158	13.928115
20.852380	1158.793038	13.933120
20.818655	1158.170749	13.938125
20.478699	1166.774249	13.943130
20.718515	1146.068565	13.948135
20.662309	1154.861784	13.953139
20.558076	1137.828774	13.958144
20.794982	1147.412657	13.963149
20.421388	1151.525304	13.968154
20.787330	1144.300762	13.973159
20.608984	1143.431863	13.978163
20.585392	1143.478211	13.983168
20.471414	1148.606082	13.988173
20.690374	1171.823416	13.993178
20.962409	1176.247863	13.998183
20.798985	1174.952350	14.003187
20.463812	1166.450227	14.008192
20.953138	1174.368688	14.013210
21.036712	1167.021833	14.018227
20.871142	1156.092004	14.023245
20.606584	1155.007907	14.028263
20.757835	1144.689805	14.033280
21.204641	1138.935150	14.038298
20.829898	1147.450018	14.043315
21.033033	1145.798964	14.048333
20.697908	1149.605696	14.053351
20.621195	1145.410051	14.058368
20.945247	1138.795645	14.063386
20.746036	1148.105216	14.068403
20.838367	1137.324605	14.073421
20.708520	1170.610433	14.078439
20.999918	1174.136342	14.083456
21.081023	1171.759125	14.088474
20.868109	1184.621265	14.093491
21.128733	1180.686415	14.098509
21.272567	1176.691541	14.103527
21.017706	1184.268652	14.108544
21.288309	1170.132592	14.113562
20.474684	1178.583770	14.118579
20.997990	1178.616714	14.123597
20.878548	1176.469687	14.128615
20.836768	1188.184527	14.133632
21.223227	1181.668689	14.138650
21.041583	1188.947830	14.143667
21.270300	1185.414474	14.148685
20.955422	1183.127156	14.153703
20.747029	1190.368092	14.158720
21.218607	1188.875567	14.163738
20.915410	1194.704874	14.168755
20.955069	1201.037930	14.173773
20.933610	1211.465941	14.178791
21.330423	1212.618621	14.183808
21.741332	1210.855768	14.188826
21.246872	1223.742399	14.193843
21.344096	1220.299222	14.198861
21.427237	1205.003804	14.203879
21.010421	1219.488847	14.208896
21.366928	1221.478526	14.213914
21.340369	1223.653574	14.218931
21.653311	1214.206272	14.223949
21.435537	1220.909164	14.228967
21.449577	1221.803567	14.233984
21.674277	1214.525416	14.239002
21.382204	1220.708468	14.244019
21.297470	1220.059734	14.249037
21.347526	1226.620808	14.254055
21.199438	1227.309832	14.259072
21.344937	1241.689479	14.264090
21.577829	1250.271087	14.269107
21.776973	1253.440490	14.274125
21.915038	1248.353245	14.279143
21.569284	1258.425594	14.284160
22.001204	1244.496545	14.289178
21.764611	1248.979730	14.294195
22.042923	1237.916119	14.299213
21.916251	1228.282518	14.304231
21.331049	1226.225502	14.309248
21.688463	1234.216223	14.314266
21.896403	1248.644121	14.319283
21.842837	1261.007424	14.324301
21.941321	1260.573288	14.329319
21.763349	1257.369055	14.334336
22.073641	1255.626963	14.339354
21.959721	1257.403811	14.344371
21.857876	1261.783708	14.349389
21.804806	1256.184243	14.354407
22.002992	1265.723093	14.359424
21.924887	1255.029355	14.364442
21.795153	1253.723968	14.369459
21.692635	1259.123311	14.374477
21.964719	1255.037173	14.379495
21.958597	1258.207855	14.384512
22.034119	1245.852072	14.389530
21.918677	1254.852617	14.394547
21.953273	1255.334749	14.399565
22.267361	1249.071101	14.404583
21.903080	1255.251527	14.409600
21.936274	1250.483034	14.414618
21.914233	1256.874720	14.419635
22.190581	1264.768274	14.424653
22.515456	1270.436086	14.429671
22.161017	1277.684629	14.434688
22.552338	1257.661736	14.439706
22.383194	1258.289625	14.444723
22.137445	1263.121919	14.449741
22.249631	1256.679681	14.454759
22.065998	1266.968428	14.459776
22.564784	1282.035821	14.464794
22.661520	1285.479546	14.469811
22.676264	1271.786900	14.474829
22.654141	1268.469715	14.479847
22.232149	1271.123127	14.484864
22.481070	1260.337899	14.489882
22.463051	1260.636511	14.494899
22.197443	1258.679529	14.499917
22.743853	1270.429611	14.504935
22.703855	1283.130548	14.509952
22.844407	1274.277004	14.514970
22.296788	1279.192057	14.519987
22.547677	1277.718992	14.525005
22.774589	1278.154721	14.530023
22.497587	1289.771878	14.535040
22.584375	1288.620720	14.540058
22.727970	1291.136734	14.545075
22.522630	1294.977860	14.550093
22.653118	1292.765784	14.555111
22.722330	1289.972012	14.560128
22.741324	1290.736638	14.565146
22.700838	1300.491334	14.570163
22.554807	1294.373415	14.575181
22.581188	1293.780888	14.580199
22.704336	1300.231235	14.585216
22.562865	1293.351229	14.590234
22.801722	1289.210605	14.595251
22.991072	1290.012555	14.600269
22.969734	1286.734568	14.605287
23.163408	1292.048927	14.610304
23.086547	1286.846509	14.615322
23.313367	1284.963568	14.620339
22.951797	1288.261737	14.625357
23.365315	1282.553235	14.630375
22.889879	1289.962657	14.635392
23.012246	1291.451706	14.640410
23.122328	1284.509559	14.645427
22.904277	1289.169127	14.650445
23.030613	1290.791252	14.655463
23.006435	1291.816026	14.660480
22.835256	1290.610057	14.665498
23.304776	1292.246660	14.670515
22.832523	1294.834158	14.675533
23.320916	1290.002488	14.680551
22.699957	1290.482213	14.685568
22.974983	1301.610203	14.690586
23.441900	1315.797083	14.695603
23.197882	1336.443098	14.700621
23.382268	1312.805207	14.705639
23.371195	1325.935732	14.710656
23.758176	1324.787030	14.715674
23.652067	1327.020400	14.720691
23.509318	1307.323301	14.725709
23.477400	1296.719695	14.730727
22.973563	1293.070341	14.735744
23.451452	1306.613655	14.740762
23.570766	1313.958117	14.745779
23.477036	1319.563724	14.750797
23.862962	1318.784859	14.755815
23.660800	1320.265895	14.760832
23.928955	1311.075791	14.765850
23.468881	1298.893480	14.770867
23.352042	1290.340533	14.775885
24.052675	1293.387486	14.780903
23.666575	1303.117082	14.785920
23.557290	1297.869494	14.790938
23.540989	1299.253243	14.795955
23.624063	1320.940340	14.800973
23.905772	1318.257392	14.805991
23.958240	1317.476655	14.811008
23.779860	1308.740026	14.816026
23.806686	1302.556780	14.821043
23.725384	1315.144781	14.826061
23.961354	1308.006362	14.831079
23.749371	1315.762322	14.836096
23.489462	1318.688772	14.841114
24.044869	1313.127518	14.846131
23.770174	1326.163234	14.851149
24.189876	1317.235252	14.856167
23.944076	1324.598626	14.861184
24.171980	1321.076380	14.866202
24.154132	1318.656719	14.871219
24.067876	1321.542888	14.876237
24.248736	1311.853889	14.881255
24.039786	1312.554197	14.886272
23.843403	1301.591419	14.891290
24.179404	1312.535083	14.896307
24.259952	1322.069138	14.901325
24.038999	1316.370581	14.906343
23.683788	1323.553200	14.911360
24.143466	1321.667723	14.916378
24.183930	1324.322891	14.921395
23.822195	1329.096625	14.926413
24.146314	1319.935343	14.931431
24.331126	1323.926611	14.936448
24.188200	1319.247536	14.941466
24.423123	1308.779117	14.946483
24.156119	1321.225278	14.951501
24.235275	1309.510670	14.956519
24.113986	1322.451128	14.961536
24.224782	1321.804237	14.966554
24.408165	1315.668376	14.971571
24.049307	1327.146031	14.976589
24.542480	1324.913856	14.981607
25.037624	1335.677995	14.986624
24.471424	1333.083090	14.991642
24.289142	1325.339675	14.996659
24.454725	1327.734210	15.001677
24.886439	1331.343173	15.006695
24.497190	1331.087503	15.011712
24.584377	1323.187850	15.016730
24.631279	1323.465097	15.021747
24.580983	1334.560055	15.026765
24.938319	1331.619645	15.031783
24.856419	1330.361678	15.036800
24.462275	1325.230301	15.041818
25.075027	1324.987853	15.046835
24.763407	1322.666958	15.051853
24.937647	1314.404205	15.056871
24.499692	1324.022533	15.061888
24.575708	1326.901698	15.066906
24.718507	1339.232175	15.071923
24.632911	1341.116202	15.076941
24.913918	1341.958594	15.081959
24.953632	1346.981344	15.086976
24.474908	1348.298849	15.091994
24.883627	1351.098212	15.097011
24.558480	1348.376766	15.102029
24.718292	1354.597915	15.107047
24.979284	1347.658410	15.112064
24.877327	1338.681480	15.117082
25.106672	1339.126262	15.122099
24.980367	1347.370380	15.127117
24.953035	1353.174627	15.132135
25.073147	1358.082309	15.137152
25.433462	1376.447006	15.142170
25.318849	1364.517861	15.147187
24.999170	1364.571999	15.152205
25.233032	1355.714534	15.157223
25.504755	1365.708921	15.162240
25.248863	1361.313697	15.167258
25.045989	1347.890075	15.172275
25.140303	1367.299227	15.177293
25.554993	1377.036433	15.182311
25.878117	1363.241031	15.187328
25.302606	1358.767795	15.192346
25.511632	1349.431364	15.197363
25.860587	1353.047241	15.202381
25.696900	1342.941256	15.207399
25.759591	1350.030492	15.212416
25.755585	1347.536258	15.217434
25.672418	1340.821540	15.222451
25.189055	1345.477823	15.227469
25.126042	1361.087945	15.232487
25.451051	1350.581532	15.237504
25.267669	1360.483331	15.242522
25.497516	1346.646192	15.247539
25.241365	1348.790236	15.252557
25.334250	1369.137164	15.257575
25.598942	1379.949104	15.262592
25.751806	1380.719125	15.267610
25.619661	1373.225671	15.272627
25.603334	1378.336024	15.277645
25.334644	1379.810373	15.282663
25.881310	1385.044870	15.287680
25.467412	1392.630150	15.292698
25.699284	1383.099713	15.297715
25.817951	1384.051372	15.302733
25.725859	1384.714168	15.307751
25.757308	1377.672831	15.312768
26.255923	1391.790235	15.317786
26.027855	1383.344638	15.322803
25.766049	1384.221698	15.327821
25.753296	1394.980369	15.332839
26.234693	1393.388729	15.337856
26.234251	1403.934653	15.342874
26.611464	1396.701302	15.347891
26.121457	1383.142540	15.352909
25.831178	1381.675553	15.357927
26.182292	1380.792123	15.362944
26.038392	1383.733117	15.367962
26.384218	1389.632022	15.372979
26.178360	1380.726695	15.377997
26.072987	1390.447754	15.383015
26.257841	1388.233285	15.388032
26.085773	1409.265913	15.393050
26.442989	1400.366723	15.398067
26.436507	1412.688037	15.403085
26.334036	1403.259678	15.408103
26.747999	1406.728343	15.413120
26.364833	1397.247227	15.418138
26.181264	1390.221301	15.423155
26.387791	1401.884125	15.428173
26.463560	1408.826582	15.433191
26.754835	1403.952381	15.438208
26.456938	1412.796502	15.443226
26.474309	1406.186844	15.448243
26.461021	1410.379624	15.453261
26.626954	1411.020144	15.458279
26.706248	1410.162763	15.463296
26.287029	1412.282487	15.468314
26.307208	1407.564784	15.473331
26.561409	1409.690361	15.478349
26.192167	1412.305495	15.483367
26.457807	1406.933572	15.488384
26.439996	1415.522231	15.493402
26.457875	1414.289243	15.498419
26.732455	1431.022253	15.503437
26.987479	1434.360540	15.508455
27.053242	1435.566040	15.513472
26.802278	1439.681903	15.518490
27.295540	1429.954010	15.523507
27.222460	1417.790102	15.528525
26.824735	1416.843630	15.533543
26.604153	1409.346959	15.538560
26.480910	1424.015048	15.543578
26.998063	1423.572336	15.548595
26.953409	1435.951670	15.553613
27.095459	1440.814981	15.558631
27.470472	1444.294587	15.563648
27.153697	1442.399224	15.568666
26.973085	1450.560824	15.573683
26.962440	1449.519578	15.578701
27.178705	1451.346822	15.583719
27.546020	1443.132642	15.588736
27.027202	1441.260066	15.593754
27.190697	1446.823909	15.598771
27.409558	1445.947412	15.603789
27.302043	1449.078463	15.608807
27.543443	1443.555445	15.613824
27.092455	1450.779358	15.618842
27.393083	1448.947548	15.623859
27.749961	1441.796072	15.628877
27.512061	1451.931578	15.633895
27.600685	1441.856857	15.638912
27.581556	1446.293619	15.643930
27.390038	1446.391811	15.648947
27.489122	1443.825274	15.653965
27.540352	1440.005552	15.658983
27.572364	1440.716985	15.664000
27.207678	1449.947745	15.669018
27.530836	1438.566148	15.674035
27.357548	1439.316618	15.679053
27.255441	1444.088307	15.684071
27.495418	1437.034132	15.689088
27.538657	1444.091910	15.694106
27.423499	1447.737788	15.699123
27.612919	1460.737354	15.704141
27.689617	1467.502720	15.709159
27.768698	1468.198782	15.714176
27.774151	1475.959474	15.719194
27.893705	1471.883446	15.724211
28.201825	1470.995858	15.729229
27.804443	1475.671502	15.734247
27.747759	1471.856398	15.739264
27.611289	1472.141659	15.744282
27.587587	1465.069750	15.749299
28.117143	1467.967844	15.754317
27.929021	1467.836612	15.759335
28.184422	1462.002245	15.764352
28.080755	1475.282172	15.769370
27.918816	1468.671197	15.774387
28.030783	1468.713906	15.779405
27.995620	1474.087641	15.784423
28.117278	1470.512303	15.789440
28.011191	1482.540453	15.794458
28.113461	1475.148776	15.799475
27.885136	1486.755965	15.804493
27.755753	1495.973606	15.809511
28.211457	1498.901576	15.814528
28.222560	1509.164940	15.819546
28.355260	1501.151748	15.824563
28.547522	1501.242215	15.829581
28.259211	1507.847945	15.834599
28.721824	1502.768626	15.839616
28.605023	1505.215308	15.844634
28.646000	1498.490155	15.849651
28.591671	1491.106142	15.854669
28.661796	1506.601587	15.859687
28.833291	1492.672153	15.864704
28.813348	1509.407395	15.869722
28.895883	1496.265315	15.874739
28.800600	1495.612745	15.879757
28.798585	1504.853337	15.884775
28.907418	1482.600520	15.889792
28.695145	1487.096415	15.894810
28.689682	1473.286461	15.899827
28.851078	1459.906099	15.904845
28.595830	1474.194159	15.909863
28.587790	1477.812736	15.914880
28.760453	1502.679948	15.919898
28.854691	1500.082712	15.924915
29.113661	1494.989469	15.929933
28.866673	1500.449697	15.934951
29.030701	1497.833465	15.939968
28.933376	1497.815171	15.944986
29.049763	1507.144636	15.950003
29.154259	1497.610058	15.955021
29.044783	1493.873370	15.960039
29.067807	1494.681411	15.965056
29.082901	1498.898792	15.970074
28.797054	1505.458509	15.975091
29.093615	1502.416856	15.980109
28.848312	1507.784792	15.985127
29.172383	1501.171794	15.990144
29.120898	1505.459573	15.995162
28.897975	1503.963739	16.000179
29.306090	1501.551617	16.005197
29.092462	1508.099817	16.010215
29.196613	1501.547064	16.015232
29.255267	1502.461111	16.020250
29.022868	1506.715608	16.025267
29.370055	1516.713008	16.030285
29.380896	1531.062507	16.035303
29.603523	1529.403583	16.040320
29.556657	1535.298324	16.045338
29.490343	1535.008446	16.050355
29.596001	1527.401475	16.055373
29.483322	1534.665069	16.060391
29.942395	1528.808416	16.065408
29.906925	1528.500248	16.070426
29.648430	1520.660341	16.075443
29.824584	1515.655021	16.080461
29.826827	1518.443740	16.085479
29.880942	1506.565435	16.090496
29.567971	1500.128763	16.095514
29.694598	1508.695226	16.100531
30.018405	1511.091298	16.105549
29.686130	1520.378283	16.110567
30.127069	1516.183342	16.115584
29.730806	1519.155174	16.120602
29.562774	1527.920447	16.125619
30.081811	1523.411016	16.130637
29.595602	1524.978276	16.135655
29.794639	1529.558025	16.140672
29.959728	1530.253744	16.145690
29.614702	1533.044368	16.150707
30.289677	1528.303204	16.155725
29.974315	1529.174655	16.160743
30.420948	1528.646444	16.165760
29.946297	1523.763798	16.170778
29.905464	1532.810818	16.175795
30.014120	1531.726942	16.180813
30.026162	1531.962562	16.185831
30.418885	1544.272229	16.190848
30.469103	1539.528455	16.195866
30.276667	1534.863499	16.200883
30.367225	1524.319633	16.205901
30.306596	1538.773351	16.210919
30.429386	1537.174396	16.215936
30.662085	1538.696998	16.220954
30.269998	1536.569020	16.225971
30.293564	1541.473285	16.230989
30.088815	1559.153595	16.236007
30.518258	1563.772901	16.241024
30.567661	1559.033970	16.246042
30.598195	1564.445239	16.251059
30.895918	1569.484333	16.256077
30.507615	1561.623421	16.261095
30.771354	1564.061330	16.266112
30.900617	1555.112671	16.271130
30.379937	1567.106339	16.276147
30.627697	1560.561330	16.281165
30.397178	1564.423846	16.286183
30.579538	1556.162808	16.291200
30.752329	1559.942120	16.296218
30.446519	1569.696840	16.301235
30.319248	1567.105033	16.306253
30.453261	1582.922292	16.311271
30.872982	1597.355299	16.316288
30.954979	1589.948706	16.321306
30.670936	1594.998797	16.326323
31.005465	1584.841497	16.331341
31.014791	1594.109439	16.336359
30.820680	1595.670232	16.341376
31.480768	1585.218751	16.346394
31.342899	1592.535944	16.351411
31.422304	1580.451403	16.356429
31.353889	1587.030748	16.361447
31.328359	1580.268186	16.366464
31.259353	1580.368076	16.371482
31.225973	1589.186631	16.376499
31.502510	1594.364398	16.381517
31.481509	1586.885355	16.386535
31.073250	1583.440127	16.391552
31.520256	1588.499465	16.396570
31.218346	1586.195855	16.401587
31.428993	1586.711270	16.406605
31.313795	1586.724142	16.411623
31.079505	1590.151520	16.416640
31.612142	1588.404604	16.421658
31.671942	1597.419097	16.426675
31.519304	1591.460200	16.431693
31.781889	1596.880877	16.436711
31.919763	1603.162263	16.441728
31.832961	1597.030835	16.446746
31.674427	1587.712762	16.451763
31.865150	1577.848188	16.456781
31.704786	1582.366508	16.461799
31.664339	1578.533842	16.466816
32.117096	1576.112229	16.471834
31.640567	1597.424144	16.476851
31.749521	1608.183225	16.481869
31.884801	1613.477915	16.486887
32.121174	1616.815287	16.491904
32.273427	1607.458645	16.496922
31.692705	1616.982739	16.501939
31.919319	1614.207061	16.506957
32.242555	1612.559610	16.511975
32.302072	1618.314716	16.516992
32.557745	1601.016348	16.522010
32.129152	1591.492796	16.527027
32.219206	1581.715064	16.532045
32.004926	1584.325963	16.537063
32.151028	1581.830557	16.542080
32.473813	1598.077853	16.547098
32.130953	1604.952673	16.552115
32.277084	1607.329907	16.557133
32.027119	1609.917399	16.562151
32.294093	1612.376038	16.567168
32.721481	1606.596771	16.572186
32.485982	1614.311020	16.577203
32.321379	1609.268777	16.582221
32.270686	1603.749813	16.587239
31.899514	1601.888273	16.592256
32.074857	1598.114785	16.597274
31.990254	1607.094110	16.602291
32.507063	1615.809986	16.607309
32.745507	1629.534945	16.612327
32.437311	1641.668611	16.617344
32.687093	1640.671548	16.622362
32.603845	1648.825595	16.627379
32.657972	1645.537064	16.632397
32.558092	1645.698510	16.637415
32.368663	1635.243267	16.642432
32.568438	1641.169502	16.647450
32.840626	1639.418501	16.652467
32.999716	1636.914722	16.657485
32.762378	1638.808831	16.662503
32.596356	1644.522051	16.667520
33.116199	1644.956692	16.672538
33.193657	1661.641180	16.677555
33.149249	1671.185954	16.682573
33.029655	1670.481408	16.687591
33.158319	1669.819854	16.692608
33.378182	1666.212288	16.697626
32.888061	1654.017165	16.702643
33.242119	1652.389177	16.707661
33.189002	1666.524058	16.712679
33.065083	1668.684812	16.717696
33.606581	1664.588627	16.722714
33.438303	1677.406327	16.727731
33.217423	1672.803280	16.732749
33.104918	1667.503372	16.737767
33.220880	1665.188947	16.742784
33.434557	1662.347680	16.747802
33.392629	1668.134716	16.752819
33.582991	1669.885105	16.757837
33.888014	1676.168179	16.762855
33.530980	1672.550371	16.767872
33.720292	1662.368199	16.772890
33.830850	1659.635406	16.777907
33.470186	1671.352728	16.782925
33.895410	1671.316374	16.787943
33.457860	1674.128074	16.792960
33.671587	1657.688948	16.797978
33.640627	1670.216528	16.802995
33.543129	1670.455462	16.808013
33.790210	1671.095637	16.813031
33.639660	1671.805523	16.818048
34.029746	1664.768199	16.823066
33.833165	1662.688460	16.828083
33.856063	1661.228912	16.833101
34.100718	1661.858462	16.838119
34.036287	1661.171074	16.843136
34.120087	1659.640461	16.848154
34.106233	1667.149493	16.853171
34.106623	1670.288551	16.858189
34.437774	1666.491768	16.863207
33.995876	1677.117736	16.868224
34.155509	1675.023657	16.873242
34.405073	1691.573758	16.878259
34.340161	1686.698069	16.883277
34.476774	1683.828975	16.888295
34.399423	1686.735819	16.893312
34.608837	1676.832802	16.898330
34.349472	1673.984391	16.903347
34.467988	1665.342560	16.908365
34.917287	1655.880305	16.913383
34.096218	1655.813840	16.918400
34.943005	1652.649793	16.923418
34.604053	1659.740315	16.928435
34.318579	1663.257675	16.933453
34.604650	1668.754074	16.938471
34.722359	1676.087964	16.943488
35.091494	1674.982984	16.948506
34.715476	1664.470172	16.953523
34.605764	1662.313655	16.958541
35.021422	1659.565235	16.963559
34.734760	1658.733959	16.968576
34.735895	1665.661700	16.973594
34.781921	1680.794643	16.978611
34.645668	1691.806050	16.983629
34.859652	1686.044270	16.988647
34.689017	1686.448247	16.993664
35.039849	1679.881240	16.998682
34.818735	1683.005290	17.003699
34.796978	1686.506550	17.008717
35.145049	1681.663313	17.013735
34.831684	1685.638178	17.018752
35.028803	1683.301367	17.023770
35.029059	1681.724299	17.028787
35.156809	1702.122764	17.033805
35.411786	1710.474598	17.038823
35.613152	1713.997697	17.043840
35.328598	1696.446374	17.048858
35.006079	1692.161567	17.053875
35.030369	1704.576539	17.058893
35.636648	1704.379169	17.063911
35.352031	1713.972508	17.068928
35.631978	1716.456625	17.073946
35.508046	1716.172787	17.078963
35.596214	1717.862399	17.083981
35.666177	1718.856458	17.088999
35.542244	1716.117793	17.094016
35.464543	1706.028516	17.099034
35.722927	1703.072354	17.104051
35.772742	1712.466055	17.109069
35.926530	1715.542902	17.114087
35.889644	1718.606114	17.119104
35.917744	1724.019404	17.124122
35.812079	1710.812760	17.129139
35.617641	1710.397801	17.134157
35.894155	1714.395790	17.139175
35.676790	1716.754721	17.144192
35.848307	1711.409498	17.149210
35.754400	1713.581202	17.154227
35.578738	1714.225093	17.159245
35.913886	1700.689377	17.164263
35.766298	1716.577651	17.169280
36.039404	1736.805896	17.174298
36.146831	1740.049027	17.179315
36.010950	1744.346403	17.184333
36.356858	1734.180893	17.189351
36.436030	1740.894079	17.194368
36.306874	1737.460931	17.199386
36.219179	1738.825432	17.204403
35.782936	1750.710609	17.209421
36.389188	1738.267403	17.214439
36.249705	1748.021670	17.219456
36.159564	1753.092801	17.224474
36.421211	1740.278243	17.229491
36.531064	1747.223291	17.234509
36.627668	1733.671319	17.239527
36.760453	1750.130782	17.244544
36.885367	1752.697837	17.249562
36.935162	1744.910891	17.254579
36.528594	1745.024505	17.259597
36.916865	1728.456783	17.264615
36.869963	1734.402736	17.269632
36.584822	1741.096158	17.274650
36.789562	1741.968831	17.279667
36.536975	1762.039483	17.284685
37.105637	1763.525045	17.289703
37.138316	1779.212380	17.294720
36.948396	1778.095878	17.299738
37.250792	1774.848736	17.304755
37.191102	1779.269258	17.309773
37.321978	1767.886612	17.314791
37.002668	1763.650038	17.319808
36.687382	1766.839464	17.324826
36.874200	1778.884854	17.329843
36.844692	1781.835212	17.334861
37.063022	1774.411501	17.339879
36.920946	1788.093474	17.344896
36.984904	1777.289387	17.349914
37.299971	1778.201883	17.354931
37.240257	1785.118149	17.359949
37.556498	1778.106706	17.364967
37.127752	1784.773499	17.369984
37.407702	1795.863330	17.375002
37.433029	1795.642992	17.380019
37.260255	1806.660310	17.385037
37.451498	1800.937507	17.390055
37.412711	1804.421848	17.395072
37.307655	1801.355309	17.400090
37.378271	1800.132755	17.405107
37.258055	1812.659747	17.410125
37.449750	1814.856706	17.415143
37.717500	1813.698670	17.420160
37.742684	1829.676707	17.425178
38.181206	1834.101947	17.430195
38.081332	1837.935045	17.435213
37.994576	1826.811232	17.440231
37.835692	1831.534684	17.445248
37.965098	1830.986269	17.450266
38.117865	1833.154044	17.455283
37.970684	1834.900084	17.460301
38.105324	1833.797884	17.465319
37.862655	1835.147783	17.470336
38.098834	1835.106973	17.475354
38.061508	1831.460157	17.480371
38.163864	1827.637686	17.485389
38.272593	1828.911090	17.490407
38.462136	1829.454264	17.495424
38.112350	1832.046703	17.500442
38.224195	1828.600266	17.505459
38.318204	1830.047487	17.510477
38.526420	1820.739201	17.515495
38.577920	1818.976184	17.520512
38.452897	1825.259481	17.525530
38.752782	1829.509405	17.530547
38.267290	1844.694255	17.535565
38.561374	1854.045156	17.540583
38.721424	1851.327244	17.545600
38.533277	1863.504084	17.550618
38.691951	1856.724599	17.555635
38.786890	1866.598083	17.560653
38.928492	1854.948587	17.565671
38.763612	1855.232880	17.570688
38.528364	1857.631653	17.575706
39.367818	1852.098048	17.580723
38.960382	1851.055559	17.585741
39.210930	1852.606812	17.590759
38.936892	1854.764006	17.595776
39.183544	1854.841082	17.600794
39.223340	1851.139487	17.605811
39.024332	1853.953289	17.610829
38.944310	1863.360715	17.615847
39.184232	1857.652151	17.620864
39.146256	1856.219596	17.625882
39.205876	1858.134801	17.630899
39.273562	1857.666233	17.635917
39.356747	1850.925534	17.640935
39.364331	1854.229447	17.645952
38.950043	1856.192706	17.650970
39.428461	1857.960102	17.655987
39.730955	1879.161551	17.661005
39.773661	1877.197783	17.666023
39.612124	1862.579386	17.671040
39.374272	1862.774637	17.676058
39.553733	1868.760052	17.681075
39.498176	1887.817826	17.686093
39.962202	1885.575276	17.691111
40.022062	1884.669841	17.696128
39.901265	1891.925468	17.701146
40.269797	1878.232458	17.706163
39.910768	1870.232993	17.711181
40.039004	1870.229849	17.716199
39.764078	1857.748532	17.721216
39.460125	1856.052427	17.726234
40.170015	1877.171594	17.731251
39.925281	1886.562831	17.736269
39.893745	1895.043843	17.741287
40.487311	1880.948402	17.746304
40.236814	1890.464838	17.751322
40.223078	1879.352936	17.756339
40.109202	1884.727577	17.761357
40.025722	1883.390371	17.766375
40.000985	1885.257682	17.771392
40.054824	1888.557373	17.776410
40.103215	1882.898223	17.781427
40.126591	1893.012027	17.786445
40.044193	1906.017589	17.791463
40.396878	1923.713260	17.796480
40.494230	1923.786620	17.801498
40.448421	1918.238441	17.806515
40.350261	1921.931279	17.811533
40.332725	1917.805415	17.816551
40.708363	1921.624834	17.821568
40.717981	1919.387894	17.826586
40.857973	1913.869863	17.831603
40.633446	1920.919451	17.836621
40.732744	1913.126092	17.841639
40.983223	1909.868324	17.846656
40.727225	1912.965736	17.851674
40.762050	1922.944019	17.856691
41.164647	1940.014298	17.861709
41.304511	1948.214731	17.866727
41.286967	1926.888300	17.871744
41.286870	1919.700713	17.876762
41.394120	1912.153854	17.881779
41.176061	1916.779798	17.886797
41.210395	1915.207495	17.891815
41.432567	1910.579331	17.896832
41.001289	1912.457998	17.901850
41.029435	1910.424970	17.906867
41.133388	1925.087217	17.911885
41.249652	1943.225699	17.916903
41.484368	1940.493502	17.921920
41.407126	1943.227335	17.926938
41.591141	1947.235422	17.931955
41.734984	1945.718801	17.936973
41.378693	1945.859792	17.941991
41.697653	1942.119943	17.947008
41.555982	1942.886631	17.952026
41.832855	1945.130590	17.957043
41.899273	1942.895600	17.962061
41.707070	1942.770519	17.967079
41.715860	1941.787491	17.972096
41.506829	1936.423436	17.977114
41.451390	1938.087998	17.982131
41.798464	1943.389931	17.987149
41.620097	1941.971892	17.992167
42.085397	1953.792890	17.997184
41.844531	1974.530543	18.002202
42.190648	1971.447857	18.007219
42.241063	1970.100301	18.012237
42.171991	1976.438451	18.017255
42.398375	1965.432128	18.022272
42.228838	1971.534598	18.027290
42.227163	1969.195626	18.032307
42.296457	1977.357776	18.037325
42.162015	1978.236579	18.042343
42.464356	1965.254088	18.047360
42.311811	1966.513328	18.052378
42.358839	1972.757450	18.057395
42.546112	1965.683111	18.062413
42.173060	1967.855326	18.067431
42.163732	1967.277120	18.072448
42.548200	1983.544113	18.077466
43.101071	1993.012717	18.082483
43.319622	2002.481947	18.087501
42.738422	1983.150395	18.092519
42.963165	1967.254254	18.097536
42.732760	1963.533586	18.102554
42.453496	1968.680575	18.107571
43.125739	1979.243907	18.112589
43.018440	1999.239800	18.117607
43.109219	1998.209869	18.122624
42.848057	2001.747814	18.127642
43.156698	2005.041502	18.132659
43.107740	1999.345133	18.137677
43.291803	2004.514200	18.142695
43.398943	2000.825424	18.147712
43.200733	2002.420735	18.152730
43.043453	2007.163651	18.157747
43.687344	2002.903170	18.162765
43.408358	2001.478363	18.167783
43.623386	2002.762359	18.172800
43.536529	2001.621536	18.177818
43.608804	1995.432320	18.182835
43.396752	2000.785693	18.187853
43.579393	2001.961588	18.192871
43.806362	1992.530645	18.197888
43.569996	1997.839914	18.202906
43.459520	1996.831069	18.207923
43.490543	1995.357606	18.212941
43.423528	1999.808466	18.217959
43.712856	1995.481045	18.222976
43.440956	2002.992076	18.227994
43.859234	1997.545255	18.233011
43.920414	1993.413895	18.238029
43.453684	2004.732305	18.243047
43.941035	2007.742644	18.248064
43.755166	2026.294383	18.253082
43.719627	2027.314728	18.258099
44.150369	2025.115221	18.263117
43.895641	2025.048092	18.268135
44.072779	2021.039812	18.273152
44.043108	2021.775270	18.278170
44.062925	2029.904439	18.283187
44.281613	2034.250751	18.288205
43.922667	2051.927932	18.293223
44.464772	2053.128305	18.298240
44.424541	2056.338423	18.303258
44.363327	2066.752936	18.308275
44.607122	2060.108443	18.313293
44.477094	2060.443027	18.318311
44.645921	2055.503192	18.323328
44.552796	2050.332983	18.328346
44.760765	2051.249994	18.333363
45.122538	2050.275947	18.338381
44.749406	2057.477512	18.343399
44.688641	2048.768086	18.348416
44.970111	2051.433717	18.353434
44.656114	2062.478470	18.358451
44.919074	2046.469175	18.363469
45.054184	2049.582895	18.368487
45.087643	2051.798048	18.373504
45.062730	2064.995159	18.378522
45.134292	2070.953818	18.383539
45.378147	2070.368265	18.388557
45.060438	2079.657211	18.393575
45.473134	2076.529275	18.398592
45.738763	2073.691443	18.403610
45.010066	2072.497239	18.408627
45.799060	2070.939851	18.413645
45.630604	2063.102594	18.418663
45.487056	2044.577398	18.423680
45.647338	2051.355662	18.428698
45.350125	2048.033406	18.433715
45.751822	2061.571491	18.438733
45.562689	2075.228202	18.443751
45.740936	2078.148632	18.448768
45.698865	2071.850983	18.453786
45.412668	2083.805313	18.458803
45.919311	2080.956571	18.463821
45.571680	2072.877304	18.468839
45.982422	2073.941315	18.473856
46.106116	2078.370436	18.478874
45.937055	2078.826871	18.483891
45.923534	2071.076592	18.488909
45.691538	2068.528926	18.493927
45.634465	2068.979299	18.498944
45.630930	2069.458889	18.503962
45.970385	2086.320744	18.508979
46.288502	2096.169802	18.513997
46.524091	2111.800750	18.519015
46.689718	2098.187090	18.524032
46.907670	2106.115590	18.529050
46.447890	2088.445437	18.534067
46.493291	2077.485199	18.539085
46.347699	2081.725229	18.544103
46.573666	2088.574839	18.549120
46.455255	2084.828412	18.554138
46.522697	2099.488792	18.559155
46.639996	2103.771851	18.564173
46.473915	2099.712888	18.569191
46.864054	2103.718820	18.574208
46.818219	2105.584018	18.579226
46.589559	2109.045227	18.584243
46.885590	2094.573860	18.589261
46.665670	2106.923510	18.594279
46.695762	2100.715807	18.599296
47.106736	2103.892517	18.604314
46.570600	2103.551705	18.609331
46.670591	2115.616729	18.614349
47.184906	2130.659722	18.619367
47.352848	2133.213690	18.624384
47.264705	2130.327655	18.629402
47.065624	2134.462965	18.634419
47.380227	2125.050996	18.639437
47.199142	2135.116560	18.644455
47.319217	2140.113396	18.649472
47.519530	2137.882979	18.654490
47.172298	2136.568937	18.659507
47.197917	2127.301377	18.664525
47.251203	2143.739356	18.669543
47.777092	2158.462756	18.674560
47.824752	2163.751957	18.679578
47.683252	2171.626912	18.684595
48.159694	2165.370806	18.689613
47.827249	2165.011665	18.694631
47.832573	2163.132479	18.699648
47.951820	2160.778123	18.704666
48.046964	2158.057134	18.709683
48.144263	2148.383269	18.714701
47.983019	2156.664092	18.719719
48.071574	2161.468532	18.724736
48.222054	2153.595305	18.729754
48.001571	2161.876926	18.734771
48.219962	2150.700265	18.739789
47.971104	2152.792919	18.744807
47.990225	2150.911533	18.749824
48.324057	2152.942719	18.754842
48.211719	2151.059489	18.759859
48.241368	2151.670653	18.764877
48.528478	2158.097592	18.769895
48.593203	2162.121617	18.774912
48.679027	2152.621052	18.779930
48.246029	2155.838773	18.784947
48.618435	2173.195736	18.789965
48.436371	2185.972032	18.794983
48.240064	2188.361501	18.800000
48.793055	2190.307398	18.805018
48.385795	2191.414569	18.810035
48.573678	2185.888011	18.815053
48.845488	2194.596119	18.820071
48.909181	2208.791553	18.825088
48.966926	2208.636044	18.830106
49.170740	2220.778199	18.835123
49.492865	2212.271113	18.840141
48.956419	2216.074041	18.845159
49.145650	2225.718781	18.850176
49.360682	2212.256812	18.855194
49.484059	2218.402339	18.860211
49.749628	2219.355797	18.865229
49.440356	2214.617224	18.870247
49.349840	2211.637162	18.875264
49.580253	2205.608269	18.880282
49.542853	2215.594338	18.885299
49.678823	2205.117464	18.890317
49.813185	2206.913821	18.895335
49.214574	2212.687600	18.900352
49.736672	2211.036688	18.905370
49.592542	2216.745852	18.910387
49.943993	2212.988955	18.915405
49.682444	2219.551405	18.920423
49.831060	2205.898671	18.925440
50.019691	2205.389565	18.930458
49.831338	2228.921781	18.935475
50.078963	2232.472239	18.940493
50.381583	2241.227375	18.945511
50.087686	2239.011263	18.950528
50.487113	2244.945233	18.955546
50.093864	2240.799754	18.960563
49.994295	2238.009910	18.965581
50.087577	2244.260143	18.970599
49.775499	2241.313837	18.975616
50.159438	2241.203054	18.980634
50.133491	2246.131186	18.985651
50.515884	2256.972991	18.990669
50.768648	2272.412593	18.995687
50.498625	2277.056376	19.000704
50.572130	2262.861027	19.005722
50.429477	2268.790218	19.010739
50.833404	2269.137971	19.015757
50.710915	2272.794662	19.020775
50.394620	2272.546210	19.025792
50.726870	2268.376259	19.030810
50.681291	2269.851293	19.035827
50.938906	2266.876265	19.040845
50.896509	2270.907179	19.045863
51.008939	2289.951272	19.050880
51.324563	2293.760698	19.055898
51.254124	2299.703556	19.060915
50.996127	2298.421675	19.065933
51.259429	2308.961586	19.070951
51.135988	2301.765952	19.075968
51.541364	2295.001980	19.080986
51.299596	2299.867800	19.086003
51.343225	2295.283722	19.091021
51.555893	2297.703947	19.096039
51.505678	2308.661980	19.101056
51.528016	2293.300393	19.106074
51.424271	2300.525186	19.111091
51.394067	2297.147702	19.116109
51.754962	2322.123946	19.121127
51.401879	2327.198668	19.126144
51.887844	2318.829787	19.131162
52.043050	2327.164853	19.136179
51.995162	2325.989472	19.141197
52.036817	2325.624937	19.146215
52.056998	2323.368946	19.151232
52.230757	2318.347218	19.156250
52.369914	2314.112088	19.161267
52.398920	2318.158371	19.166285
52.340985	2317.451038	19.171303
52.188375	2313.872828	19.176320
52.406131	2314.734023	19.181338
52.507696	2317.042970	19.186355
52.504516	2319.444135	19.191373
52.727137	2317.852772	19.196391
52.577903	2321.454746	19.201408
52.561258	2309.827767	19.206426
52.469667	2326.916751	19.211443
52.823813	2319.088039	19.216461
52.691108	2319.777804	19.221479
52.960247	2333.776199	19.226496
53.218570	2335.882380	19.231514
52.881541	2333.841461	19.236531
53.217895	2343.134809	19.241549
53.278995	2329.294551	19.246567
52.738485	2325.705050	19.251584
53.221963	2340.783857	19.256602
53.152086	2343.415907	19.261619
53.150482	2347.116264	19.266637
53.217310	2343.039751	19.271655
53.089009	2345.663815	19.276672
53.350961	2339.813111	19.281690
53.477346	2343.864323	19.286707
53.112430	2349.646506	19.291725
53.508612	2346.986021	19.296743
52.990456	2350.102523	19.301760
53.058759	2349.938250	19.306778
53.531951	2358.472754	19.311795
53.530018	2367.591172	19.316813
53.728604	2376.597385	19.321831
53.811213	2385.498606	19.326848
53.930716	2381.534817	19.331866
53.858577	2378.985199	19.336883
53.745781	2375.328258	19.341901
54.116710	2374.045963	19.346919
53.700016	2369.747655	19.351936
54.001048	2376.002568	19.356954
54.024972	2385.290710	19.361971
54.514356	2385.281098	19.366989
54.399479	2368.791325	19.372007
54.012207	2381.393646	19.377024
54.269188	2394.143364	19.382042
54.268002	2404.587874	19.387059
54.596332	2408.831074	19.392077
54.929666	2400.576161	19.397095
54.408765	2410.301240	19.402112
54.750665	2397.673890	19.407130
54.983302	2411.653010	19.412147
54.573344	2404.521111	19.417165
55.023797	2397.104116	19.422183
54.696121	2400.557586	19.427200
54.851335	2396.589670	19.432218
54.697712	2398.229040	19.437235
54.667633	2397.120819	19.442253
54.539412	2389.783531	19.447271
54.863915	2414.580891	19.452288
55.299344	2433.617707	19.457306
55.388375	2435.247486	19.462323
55.233560	2432.545073	19.467341
55.208131	2430.538610	19.472359
55.187328	2439.967639	19.477376
55.608777	2429.773084	19.482394
55.147592	2427.710262	19.487411
55.363860	2427.145614	19.492429
55.395240	2420.217054	19.497447
55.102980	2420.423347	19.502464
55.547096	2442.281858	19.507482
55.651860	2452.045622	19.512499
55.468632	2455.504385	19.517517
55.724894	2448.444770	19.522535
55.603082	2460.906498	19.527552
55.606727	2455.425740	19.532570
56.254873	2457.107938	19.537587
55.847806	2457.887087	19.542605
55.788137	2459.804878	19.547623
55.556787	2475.924433	19.552640
55.845449	2484.944665	19.557658
56.112627	2483.479113	19.562675
56.357809	2489.521950	19.567693
56.560146	2483.016027	19.572711
56.534337	2485.273735	19.577728
56.754048	2480.723658	19.582746
56.622043	2480.347486	19.587763
56.455092	2481.275551	19.592781
56.588444	2478.463458	19.597799
56.753434	2483.048941	19.602816
56.649734	2481.592983	19.607834
56.932134	2473.051180	19.612851
56.672172	2474.729541	19.617869
56.856807	2479.060180	19.622887
56.878436	2485.678271	19.627904
57.101801	2497.726295	19.632922
57.345180	2505.273393	19.637939
57.032938	2514.844128	19.642957
57.214925	2505.973792	19.647975
57.384674	2516.875662	19.652992
57.526768	2511.887236	19.658010
57.639460	2509.640060	19.663027
57.073146	2518.069853	19.668045
57.509252	2502.892195	19.673063
57.303581	2514.529620	19.678080
57.483767	2510.847945	19.683098
57.476448	2512.140704	19.688115
57.400579	2516.470424	19.693133
57.543756	2508.610757	19.698151
57.602052	2513.775680	19.703168
57.689605	2513.959943	19.708186
57.732206	2517.083798	19.713203
58.005983	2543.744257	19.718221
58.001493	2528.455136	19.723239
58.026907	2541.634425	19.728256
58.054229	2535.938267	19.733274
58.681452	2538.600764	19.738291
58.204141	2542.509971	19.743309
58.343350	2545.582242	19.748327
58.256154	2542.480447	19.753344
58.173866	2539.320448	19.758362
58.331656	2547.439700	19.763379
58.273795	2550.305063	19.768397
58.333932	2530.547993	19.773415
58.422643	2541.274810	19.778432
57.988528	2548.595675	19.783450
58.596693	2556.769748	19.788467
58.387102	2569.426485	19.793485
58.739826	2569.924000	19.798503
58.780820	2560.726868	19.803520
59.011135	2562.250749	19.808538
59.073001	2565.697194	19.813555
58.863291	2566.235638	19.818573
58.722451	2565.716139	19.823591
58.950297	2580.816300	19.828608
59.311133	2589.930491	19.833626
59.419437	2583.268042	19.838643
59.525646	2600.682915	19.843661
59.890168	2593.148164	19.848679
59.382912	2589.547000	19.853696
59.711287	2586.363973	19.858714
59.911780	2577.740781	19.863731
59.464206	2575.935343	19.868749
59.803597	2579.424843	19.873767
59.835396	2579.242005	19.878784
59.640701	2591.459823	19.883802
60.044304	2582.503755	19.888819
59.936765	2590.548144	19.893837
59.943905	2588.378358	19.898855
59.829414	2582.364201	19.903872
59.902516	2586.000788	19.908890
59.964441	2586.898651	19.913907
59.864547	2596.885508	19.918925
59.838033	2589.144893	19.923943
59.966376	2595.156852	19.928960
59.876767	2623.991361	19.933978
60.061975	2613.935040	19.938995
59.791171	2628.342335	19.944013
60.311850	2617.837636	19.949031
60.445289	2628.427594	19.954048
60.448039	2640.286739	19.959066
60.873261	2650.224497	19.964083
60.670493	2656.226359	19.969101
60.930943	2652.674223	19.974119
60.896951	2657.492078	19.979136
60.669481	2661.571494	19.984154
60.984306	2646.952638	19.989171
61.173742	2661.233864	19.994189
61.148919	2652.159654	19.999207
61.035056	2671.014580	20.004224
60.915145	2658.455150	20.009242
61.073670	2650.710162	20.014259
60.861187	2660.364981	20.019277
60.892634	2660.715514	20.024295
61.176854	2672.793307	20.029312
61.172091	2673.903181	20.034330
61.437997	2664.545045	20.039347
61.605606	2672.550317	20.044365
61.594827	2685.234442	20.049383
62.117815	2693.375768	20.054400
61.748766	2690.629599	20.059418
62.146281	2690.907594	20.064435
62.110246	2687.752771	20.069453
62.014028	2683.561365	20.074471
62.186742	2686.290870	20.079488
62.031293	2696.833344	20.084506
62.320973	2701.872547	20.089523
62.162702	2706.853400	20.094541
62.204092	2701.976935	20.099559
62.284546	2693.246176	20.104576
61.987469	2709.334779	20.109594
62.465554	2696.978071	20.114611
62.239223	2705.478033	20.119629
62.121096	2701.279103	20.124647
62.427879	2703.768554	20.129664
62.113143	2707.264080	20.134682
62.601513	2719.903241	20.139699
62.431445	2732.921160	20.144717
62.431221	2732.071666	20.149735
62.839833	2733.984032	20.154752
62.755400	2735.298548	20.159770
62.833288	2731.687409	20.164787
63.175975	2749.871017	20.169805
63.612730	2753.413467	20.174823
63.991442	2734.232242	20.179840
63.630096	2730.873644	20.184858
63.583776	2727.316138	20.189875
63.153443	2726.421967	20.194893
63.278948	2724.444094	20.199911
63.418919	2718.992626	20.204928
63.399058	2730.681610	20.209946
63.644927	2736.932891	20.214963
63.964357	2752.236514	20.219981
63.696885	2754.205576	20.224999
63.891926	2748.933312	20.230016
63.750079	2758.538386	20.235034
64.053871	2749.580043	20.240051
63.948753	2753.951468	20.245069
64.266144	2750.212455	20.250087
64.187206	2751.808488	20.255104
64.096407	2750.469222	20.260122
64.364808	2748.407202	20.265139
64.307856	2751.121430	20.270157
64.357383	2742.523790	20.275175
64.616048	2740.458605	20.280192
64.114560	2744.075955	20.285210
64.509452	2753.257973	20.290227
64.822854	2761.713581	20.295245
64.585462	2775.898588	20.300263
64.860397	2777.464147	20.305280
64.833867	2782.041724	20.310298
65.087926	2778.347414	20.315315
64.937360	2774.108801	20.320333
64.786275	2774.344497	20.325351
65.178322	2770.625037	20.330368
65.021498	2773.407900	20.335386
65.055396	2776.194957	20.340403
64.992103	2773.759490	20.345421
65.120467	2767.452452	20.350439
65.132156	2768.227761	20.355456
65.143077	2795.990949	20.360474
65.367028	2793.647326	20.365491
65.417971	2803.810854	20.370509
65.239272	2807.765327	20.375527
65.469114	2798.956404	20.380544
65.218249	2804.040157	20.385562
65.568209	2811.214083	20.390579
65.947543	2829.218106	20.395597
65.835501	2834.241973	20.400615
65.949943	2831.812762	20.405632
65.450783	2836.815773	20.410650
65.425687	2831.841316	20.415667
65.677532	2830.274344	20.420685
66.131623	2846.913495	20.425703
66.031694	2858.177994	20.430720
66.351230	2862.263836	20.435738
66.432655	2858.214744	20.440755
66.300968	2861.029799	20.445773
66.325477	2863.285833	20.450791
66.672836	2855.959779	20.455808
66.386683	2873.926825	20.460826
66.570603	2875.673671	20.465843
66.862684	2886.928378	20.470861
66.477281	2891.723691	20.475879
66.958722	2887.833409	20.480896
66.754645	2898.265004	20.485914
67.053786	2898.822209	20.490931
67.072841	2897.046931	20.495949
67.006403	2901.834643	20.500967
67.326134	2893.330695	20.505984
67.268518	2908.117237	20.511002
67.465318	2919.863067	20.516019
67.656515	2924.112558	20.521037
67.202605	2935.555493	20.526055
67.741015	2927.743484	20.531072
67.606161	2930.437131	20.536090
67.806572	2923.185609	20.541107
67.994759	2934.456134	20.546125
67.875248	2928.658168	20.551143
68.124883	2923.068783	20.556160
67.859511	2931.679721	20.561178
67.891166	2921.879729	20.566195
68.094972	2923.012996	20.571213
67.817041	2923.598516	20.576231
67.959921	2921.125425	20.581248
67.833517	2942.987574	20.586266
68.088927	2952.012613	20.591283
68.498442	2955.042650	20.596301
68.176944	2954.004460	20.601319
68.462600	2956.553961	20.606336
68.213947	2959.508040	20.611354
68.375090	2971.174643	20.616371
68.592924	2987.945241	20.621389
68.825732	2984.487895	20.626407
68.968099	2980.333870	20.631424
68.925659	2988.110870	20.636442
69.065090	2981.027155	20.641459
68.982057	2986.363455	20.646477
68.804990	2982.918773	20.651495
68.924979	2981.927380	20.656512
69.020566	2988.396245	20.661530
69.065903	2997.218828	20.666547
69.282784	3003.137388	20.671565
69.276777	3018.429474	20.676583
69.281547	3013.701911	20.681600
69.452532	3014.148193	20.686618
69.446107	3009.167551	20.691635
69.803138	3008.104529	20.696653
69.676839	3023.655724	20.701671
70.197719	3027.663093	20.706688
69.997699	3040.547615	20.711706
70.102330	3034.543951	20.716723
70.093961	3037.428260	20.721741
69.943528	3045.275216	20.726759
70.056957	3043.157635	20.731776
70.292517	3036.764951	20.736794
70.193441	3043.042270	20.741811
70.468825	3041.486468	20.746829
70.157050	3038.005832	20.751847
70.293394	3042.979146	20.756864
70.255722	3054.598859	20.761882
70.364023	3059.022867	20.766899
70.757222	3063.420322	20.771917
70.670419	3067.088037	20.776935
70.732011	3063.578529	20.781952
71.011000	3071.319258	20.786970
71.034517	3067.701761	20.791987
70.940054	3071.907963	20.797005
70.846459	3080.948623	20.802023
71.088277	3084.751152	20.807040
71.178977	3088.789383	20.812058
71.216876	3094.124529	20.817075
71.632329	3089.403030	20.822093
71.473565	3097.573859	20.827111
71.776404	3088.855383	20.832128
71.613966	3093.984917	20.837146
71.561459	3096.107744	20.842163
71.811541	3093.540439	20.847181
71.921462	3100.430273	20.852199
72.110602	3095.508089	20.857216
71.875643	3099.838966	20.862234
71.816948	3106.418230	20.867251
72.307543	3109.594269	20.872269
72.278824	3111.338084	20.877287
72.339394	3106.919389	20.882304
72.503658	3121.243623	20.887322
72.173792	3115.651400	20.892339
72.472736	3106.688894	20.897357
72.601007	3109.141595	20.902375
72.521379	3110.545840	20.907392
72.510531	3104.887013	20.912410
72.319606	3111.364653	20.917427
72.897724	3131.963108	20.922445
72.517822	3144.383979	20.927463
72.796213	3148.117762	20.932480
73.016460	3142.798074	20.937498
72.780790	3146.972540	20.942515
73.060792	3144.577446	20.947533
73.178238	3141.295787	20.952551
73.088420	3136.002738	20.957568
73.283254	3148.281612	20.962586
73.073543	3167.234269	20.967603
73.707952	3165.267216	20.972621
73.517049	3175.397987	20.977639
73.597917	3175.889325	20.982656
73.645574	3173.819973	20.987674
73.784258	3174.023623	20.992691
73.704843	3175.102962	20.997709
73.219094	3181.876225	21.002727
73.867632	3190.477655	21.007744
73.973012	3206.708717	21.012762
73.794839	3218.457948	21.017779
74.206915	3199.188987	21.022797
74.073073	3200.338365	21.027815
74.244156	3209.252724	21.032832
74.407487	3209.008784	21.037850
74.461115	3215.108431	21.042867
74.960804	3224.196945	21.047885
74.355032	3244.337748	21.052903
74.628674	3240.514340	21.057920
74.829266	3239.154518	21.062938
74.345702	3247.529048	21.067955
74.760072	3234.626689	21.072973
74.956967	3236.407696	21.077991
75.066899	3234.676096	21.083008
75.448538	3246.771868	21.088026
75.115204	3246.423848	21.093043
75.300389	3259.800922	21.098061
75.317284	3271.136782	21.103079
75.724368	3270.506277	21.108096
75.865619	3264.365311	21.113114
75.576737	3272.911759	21.118131
75.920782	3263.263100	21.123149
75.664498	3265.460927	21.128167
75.750876	3261.294513	21.133184
75.982864	3264.017822	21.138202
75.664384	3266.987816	21.143219
75.810292	3262.398138	21.148237
75.691108	3264.702323	21.153255
75.877895	3281.800730	21.158272
76.157360	3285.147352	21.163290
76.094072	3288.845984	21.168307
76.405392	3291.890180	21.173325
76.167721	3295.399512	21.178343
76.280658	3294.034785	21.183360
76.224325	3310.560780	21.188378
76.087090	3322.997380	21.193395
75.998405	3333.200849	21.198413
76.110130	3337.361658	21.203431
76.727588	3350.032701	21.208448
76.977318	3351.703820	21.213466
76.885149	3364.724821	21.218483
77.073018	3361.741033	21.223501
77.239460	3358.017288	21.228519
77.387792	3346.068186	21.233536
77.420934	3346.316990	21.238554
77.161719	3361.558564	21.243571
77.322243	3353.274041	21.248589
77.453486	3373.366709	21.253607
77.240969	3378.114154	21.258624
77.671827	3383.286835	21.263642
77.521996	3393.898137	21.268659
77.597307	3385.594932	21.273677
77.612258	3391.269742	21.278695
78.165123	3403.433522	21.283712
78.266219	3405.255000	21.288730
77.939392	3418.403147	21.293747
78.181877	3413.837353	21.298765
77.925983	3425.275047	21.303783
78.356242	3421.518654	21.308800
78.380590	3420.333238	21.313818
78.307052	3427.261922	21.318835
78.214712	3422.095034	21.323853
78.489124	3454.012615	21.328871
78.641750	3456.466997	21.333888
78.745895	3454.899130	21.338906
78.597304	3469.780197	21.343923
79.105453	3457.466832	21.348941
78.871623	3457.607177	21.353959
79.065773	3474.626757	21.358976
79.612924	3472.091464	21.363994
79.288586	3494.991332	21.369011
79.659060	3487.128721	21.374029
79.763623	3478.779893	21.379047
79.809344	3494.404844	21.384064
80.023047	3483.030472	21.389082
79.726509	3492.094308	21.394099
79.982977	3488.482824	21.399117
79.900451	3479.512488	21.404135
79.537823	3487.867080	21.409152
79.827081	3482.536265	21.414170
80.004899	3488.639034	21.419187
80.116278	3479.800612	21.424205
80.327648	3484.260231	21.429223
79.951994	3485.293224	21.434240
80.427593	3486.640426	21.439258
80.194503	3509.023097	21.444275
80.493132	3504.254807	21.449293
80.632145	3512.580547	21.454311
80.753587	3515.554380	21.459328
81.108625	3510.179239	21.464346
80.838884	3513.071498	21.469363
81.005972	3509.607206	21.474381
81.136623	3513.385097	21.479399
80.508417	3514.590523	21.484416
80.850707	3503.932718	21.489434
81.114599	3525.971060	21.494451
81.286368	3528.942377	21.499469
81.401541	3536.496296	21.504487
81.357532	3534.345541	21.509504
81.663782	3530.332783	21.514522
81.524691	3533.275796	21.519539
81.114562	3538.573994	21.524557
81.582384	3535.722522	21.529575
81.500111	3557.113637	21.534592
82.003231	3558.585468	21.539610
81.896132	3570.856209	21.544627
82.125051	3565.948765	21.549645
82.088371	3562.532689	21.554663
81.730832	3564.396647	21.559680
82.298243	3568.077368	21.564698
82.337483	3570.157313	21.569715
82.513068	3579.646222	21.574733
82.827948	3588.389991	21.579751
82.319975	3594.348867	21.584768
82.713303	3588.766209	21.589786
82.448650	3591.325704	21.594803
82.289770	3588.582817	21.599821
82.849546	3607.525034	21.604839
82.903179	3621.003656	21.609856
83.140577	3613.090615	21.614874
83.033741	3624.960951	21.619891
83.046082	3618.602826	21.624909
83.316550	3623.306366	21.629927
83.065148	3630.382295	21.634944
83.416188	3645.832853	21.639962
83.515133	3655.839065	21.644979
83.429277	3654.369916	21.649997
83.807807	3655.226796	21.655015
83.817639	3656.359589	21.660032
83.909135	3648.136255	21.665050
83.841770	3658.005367	21.670067
83.874329	3678.816674	21.675085
84.352518	3677.491210	21.680103
84.179942	3688.118151	21.685120
84.110107	3683.281911	21.690138
83.909176	3690.137422	21.695155
84.237089	3686.516856	21.700173
84.489632	3701.165056	21.705191
84.522002	3714.884726	21.710208
84.936080	3701.241761	21.715226
84.736707	3716.802195	21.720243
84.863420	3717.945461	21.725261
84.862276	3707.420157	21.730279
85.001938	3713.540118	21.735296
85.149861	3712.064361	21.740314
85.155210	3726.137626	21.745331
85.309358	3734.908688	21.750349
85.562474	3736.392875	21.755367
85.390499	3751.026224	21.760384
85.648178	3757.896737	21.765402
85.571975	3745.488309	21.770419
85.515006	3744.525086	21.775437
85.578999	3741.078754	21.780455
85.304783	3750.737837	21.785472
85.920231	3765.290469	21.790490
86.094873	3773.757781	21.795507
85.748068	3782.709452	21.800525
86.246651	3776.321703	21.805543
86.012520	3779.360160	21.810560
86.102874	3770.410064	21.815578
86.284595	3789.059594	21.820595
86.325824	3797.965914	21.825613
86.698492	3808.947309	21.830631
86.776301	3812.855638	21.835648
86.947989	3804.890827	21.840666
86.794755	3819.413482	21.845683
86.708153	3825.221080	21.850701
86.981540	3810.754786	21.855719
86.724962	3825.662873	21.860736
86.887462	3835.310581	21.865754
87.234599	3839.471753	21.870771
87.051816	3843.420073	21.875789
87.390113	3832.687148	21.880807
87.360786	3853.795705	21.885824
87.707320	3850.263384	21.890842
87.724087	3860.566828	21.895859
87.831758	3870.886463	21.900877
88.013247	3866.522991	21.905895
87.802730	3875.594583	21.910912
88.279290	3860.769374	21.915930
88.394387	3862.298397	21.920947
88.138601	3864.932831	21.925965
88.396021	3862.365012	21.930983
88.121305	3881.382447	21.936000
88.413740	3893.406449	21.941018
88.225719	3897.908646	21.946035
88.392216	3900.272785	21.951053
88.570165	3893.894425	21.956071
88.499805	3911.988803	21.961088
88.793597	3919.497129	21.966106
88.946349	3920.550511	21.971123
88.988826	3932.486179	21.976141
89.126047	3925.093202	21.981159
89.109227	3924.792234	21.986176
89.316602	3932.866590	21.991194
89.548246	3954.596838	21.996211
89.366062	3956.402199	22.001229
89.970616	3961.663030	22.006247
89.853615	3958.180217	22.011264
89.807799	3961.224080	22.016282
89.868816	3957.369889	22.021299
90.035976	3961.192422	22.026317
90.224636	3948.427703	22.031335
90.118283	3958.329193	22.036352
90.212404	3954.744273	22.041370
90.522753	3959.311762	22.046387
90.008796	3957.072258	22.051405
90.436127	3963.963802	22.056423
90.575410	3980.505769	22.061440
90.731983	3995.451197	22.066458
90.465768	3989.282080	22.071475
90.448997	3991.365510	22.076493
90.609003	3991.269198	22.081511
90.856633	3997.391727	22.086528
91.249889	4005.487616	22.091546
91.141295	4007.714705	22.096563
91.102732	4024.366897	22.101581
91.498309	4022.797336	22.106599
91.263409	4023.296578	22.111616
91.372007	4019.917015	22.116634
91.268651	4027.734959	22.121651
91.624258	4043.680028	22.126669
91.873795	4041.996086	22.131687
91.791802	4040.815778	22.136704
91.758180	4042.601392	22.141722
91.946616	4046.170391	22.146739
91.789336	4052.054643	22.151757
91.922326	4059.687019	22.156775
92.440200	4073.303640	22.161792
92.649617	4074.602881	22.166810
92.977108	4070.425323	22.171827
92.559323	4077.430449	22.176845
92.791506	4071.295101	22.181863
92.743607	4075.032383	22.186880
92.644600	4078.720389	22.191898
93.058969	4075.744393	22.196915
93.164389	4096.862491	22.201933
93.113929	4097.101039	22.206951
93.089641	4100.733868	22.211968
93.158289	4106.228107	22.216986
93.402816	4096.151090	22.222003
93.053673	4103.695957	22.227021
93.535060	4106.185345	22.232039
93.715330	4123.360507	22.237056
93.800698	4129.352418	22.242074
93.963939	4121.900913	22.247091
93.656433	4124.165246	22.252109
94.009640	4124.076672	22.257127
94.250346	4129.630018	22.262144
93.898197	4135.576846	22.267162
94.137091	4153.715820	22.272179
94.285150	4164.348613	22.277197
94.364787	4163.034745	22.282215
94.441860	4168.064308	22.287232
94.368895	4170.421837	22.292250
94.619192	4174.974583	22.297267
94.480462	4195.798203	22.302285
95.030761	4184.902201	22.307303
94.831893	4193.526081	22.312320
94.764389	4198.677832	22.317338
94.865940	4199.830656	22.322355
94.986287	4209.402730	22.327373
95.138888	4221.763974	22.332391
95.394573	4225.536272	22.337408
95.407231	4232.227383	22.342426
95.600657	4228.243444	22.347443
95.367095	4241.463985	22.352461
95.211332	4251.194973	22.357479
95.593337	4252.988283	22.362496
95.837036	4266.311317	22.367514
96.187567	4277.666339	22.372531
96.329703	4296.045911	22.377549
96.577996	4291.341252	22.382567
96.551362	4284.997708	22.387584
96.728305	4282.620442	22.392602
97.120583	4270.085730	22.397619
96.932377	4283.460347	22.402637
97.084505	4281.782472	22.407655
97.481367	4265.993287	22.412672
97.042126	4273.506193	22.417690
97.195616	4264.845457	22.422707
97.411578	4277.148656	22.427725
97.335236	4269.860365	22.432743
97.198399	4271.822164	22.437760
97.004792	4285.999280	22.442778
97.524696	4290.422534	22.447795
97.462772	4308.028305	22.452813
97.546101	4303.583596	22.457831
97.801137	4305.884907	22.462848
97.707190	4308.049917	22.467866
97.792836	4317.314493	22.472883
98.162279	4328.312528	22.477901
98.216930	4324.268877	22.482919
98.511992	4321.277245	22.487936
98.441169	4324.076576	22.492954
99.394502	4321.241941	22.497971
99.043981	4322.241083	22.502989
98.999920	4325.080989	22.508007
99.103438	4322.027858	22.513024
98.987315	4322.121902	22.518042
99.100596	4321.497303	22.523059
99.080193	4329.081118	22.528077
99.250483	4334.329521	22.533095
99.588066	4346.866700	22.538112
99.380713	4356.036419	22.543130
99.604755	4352.413377	22.548147
99.511644	4353.310898	22.553165
99.264340	4354.131525	22.558183
99.736347	4351.187192	22.563200
99.558187	4355.484989	22.568218
99.819986	4369.685540	22.573235
99.588327	4386.162819	22.578253
99.961657	4388.818173	22.583271
100.230853	4383.203093	22.588288
99.913060	4392.422700	22.593306
100.288643	4400.276965	22.598323
100.145799	4423.635508	22.603341
100.300337	4423.231681	22.608359
100.498852	4418.927481	22.613376
100.545037	4438.784215	22.618394
100.848641	4444.998704	22.623411
101.081395	4455.239014	22.628429
101.070015	4449.152577	22.633447
101.087599	4455.762762	22.638464
101.052127	4457.888574	22.643482
101.262573	4465.028924	22.648499
101.086777	4480.503013	22.653517
101.664911	4486.514828	22.658535
101.730024	4480.152636	22.663552
101.566111	4484.999674	22.668570
101.554108	4490.927803	22.673587
101.665328	4508.188377	22.678605
101.851630	4519.932445	22.683623
102.229197	4517.409078	22.688640
102.096627	4525.198902	22.693658
102.436451	4524.510635	22.698675
102.600851	4542.380330	22.703693
102.192328	4538.996574	22.708711
102.497236	4537.089765	22.713728
102.646619	4543.271459	22.718746
102.913351	4554.928780	22.723763
102.861368	4566.079159	22.728781
102.986720	4576.690698	22.733799
103.009051	4578.568152	22.738816
102.930088	4578.935552	22.743834
103.502374	4588.901536	22.748851
103.475120	4604.406349	22.753869
103.275503	4599.385172	22.758887
103.657734	4593.490802	22.763904
103.562687	4599.776794	22.768922
103.509601	4601.529391	22.773939
103.925387	4627.208856	22.778957
104.078318	4632.937666	22.783975
104.386981	4631.499124	22.788992
104.114346	4644.855276	22.794010
104.308984	4636.594489	22.799027
104.488030	4659.337219	22.804045
104.685579	4665.117930	22.809063
104.772072	4659.575149	22.814080
104.810484	4662.920410	22.819098
104.704252	4657.859933	22.824115
105.228305	4665.884196	22.829133
104.912131	4673.861505	22.834151
105.150656	4685.210316	22.839168
105.401188	4693.129522	22.844186
105.615603	4694.268321	22.849203
105.610355	4691.190763	22.854221
105.799586	4684.974686	22.859239
106.122772	4688.598666	22.864256
105.903694	4695.836730	22.869274
105.946894	4677.167498	22.874291
106.028205	4688.087450	22.879309
106.026001	4695.158763	22.884327
106.436512	4700.552295	22.889344
106.305054	4717.720431	22.894362
106.372087	4707.222876	22.899379
106.690373	4710.893272	22.904397
106.168760	4716.468491	22.909415
106.382995	4722.801195	22.914432
106.521610	4740.384945	22.919450
106.642505	4749.143822	22.924467
107.116600	4759.068149	22.929485
106.678883	4764.223276	22.934503
107.411060	4766.900937	22.939520
107.331761	4786.225088	22.944538
107.442388	4782.251844	22.949555
107.489777	4783.067197	22.954573
107.288525	4789.124750	22.959591
107.618859	4797.915556	22.964608
107.640339	4804.773877	22.969626
108.150897	4814.811223	22.974643
108.047445	4817.836918	22.979661
108.202748	4817.518712	22.984679
108.469375	4821.971505	22.989696
108.481834	4844.958220	22.994714
108.614736	4845.369727	22.999731
108.701897	4847.429624	23.004749
108.675952	4844.958747	23.009767
108.864367	4847.365176	23.014784
108.870338	4845.741226	23.019802
108.991253	4868.004996	23.024819
109.231477	4870.641543	23.029837
109.018727	4878.123356	23.034855
109.576799	4871.533698	23.039872
109.598398	4879.443094	23.044890
109.372753	4874.479470	23.049907
109.624355	4878.329687	23.054925
109.807772	4894.462844	23.059943
110.184286	4898.489828	23.064960
110.142215	4905.690328	23.069978
110.159469	4901.731942	23.074995
110.594870	4906.337220	23.080013
110.520943	4903.988060	23.085031
110.612683	4904.031652	23.090048
110.726159	4920.348283	23.095066
110.737895	4938.280564	23.100083
110.828052	4937.033395	23.105101
110.686813	4941.953279	23.110119
110.671404	4935.818506	23.115136
110.627732	4945.443963	23.120154
111.072372	4970.497915	23.125171
111.304833	4976.290489	23.130189
111.491576	4971.396390	23.135207
111.727460	4972.004682	23.140224
111.474745	4967.456800	23.145242
111.468565	4969.481248	23.150259
111.910707	4979.871843	23.155277
111.913607	4996.431193	23.160295
112.282056	4996.696577	23.165312
112.232174	4999.738155	23.170330
112.173274	5000.452459	23.175347
112.527475	4996.474148	23.180365
112.284271	5009.497082	23.185383
112.675519	5008.433194	23.190400
112.381580	5015.909141	23.195418
112.867646	5023.718589	23.200435
113.071231	5019.142774	23.205453
112.976297	5024.018324	23.210471
113.060603	5032.867384	23.215488
113.106495	5045.795475	23.220506
113.429407	5048.633646	23.225523
113.431682	5048.918084	23.230541
113.873612	5055.948644	23.235559
113.590823	5058.827544	23.240576
113.795604	5072.122900	23.245594
113.590414	5081.672712	23.250611
114.135200	5082.939811	23.255629
114.064585	5085.411972	23.260647
114.304201	5087.753632	23.265664
114.570562	5090.167340	23.270682
114.627079	5098.069712	23.275699
114.736403	5102.229046	23.280717
114.916028	5114.277547	23.285735
115.008385	5106.011567	23.290752
114.945040	5106.077530	23.295770
115.089850	5108.138499	23.300787
115.181682	5110.508448	23.305805
115.566957	5123.428906	23.310823
115.535890	5137.326803	23.315840
115.858452	5139.474296	23.320858
115.656846	5142.358361	23.325875
115.913245	5140.188577	23.330893
115.918960	5148.793763	23.335911
115.800135	5138.196515	23.340928
115.584321	5149.075286	23.345946
115.748197	5168.996056	23.350963
115.707682	5170.146435	23.355981
116.091230	5184.455025	23.360999
116.327832	5195.059498	23.366016
116.651743	5198.855786	23.371034
116.520269	5201.273159	23.376051
116.742490	5217.675840	23.381069
116.716954	5241.646361	23.386087
116.953613	5237.403503	23.391104
117.224015	5236.164545	23.396122
117.014190	5247.807931	23.401139
117.067547	5261.728673	23.406157
116.840562	5266.158035	23.411175
117.189171	5273.131201	23.416192
117.417288	5300.285437	23.421210
117.563769	5312.121456	23.426227
117.684894	5303.325235	23.431245
117.876781	5331.247660	23.436263
118.068474	5333.630044	23.441280
117.960270	5332.770868	23.446298
118.243358	5334.456571	23.451315
118.631850	5356.049014	23.456333
118.648024	5363.570095	23.461351
118.886273	5358.153910	23.466368
118.927061	5368.976191	23.471386
118.877669	5371.272718	23.476403
119.349627	5373.431827	23.481421
118.910852	5388.738736	23.486439
119.242304	5388.501002	23.491456
119.684432	5395.261840	23.496474
119.518385	5394.698260	23.501491
119.853318	5406.412256	23.506509
120.095023	5420.367627	23.511527
120.760465	5401.252091	23.516544
120.838127	5410.335315	23.521562
120.899189	5410.125749	23.526579
121.248344	5390.454077	23.531597
121.001425	5379.556087	23.536615
120.976235	5373.476191	23.541632
121.052678	5359.803722	23.546650
120.882067	5362.461025	23.551667
120.968993	5374.731434	23.556685
121.087536	5393.227856	23.561703
121.117819	5392.903612	23.566720
121.069308	5390.172681	23.571738
121.208944	5406.233918	23.576755
121.772386	5406.348633	23.581773
121.769897	5418.771804	23.586791
121.554530	5428.960730	23.591808
121.646135	5439.062950	23.596826
121.751751	5435.317702	23.601843
122.329171	5446.243291	23.606861
122.286230	5458.446361	23.611879
122.030223	5472.388308	23.616896
122.313484	5467.674557	23.621914
122.399105	5477.002807	23.626931
122.792324	5485.300933	23.631949
122.933599	5487.811755	23.636967
122.856334	5490.509269	23.641984
123.254580	5488.731435	23.647002
123.068615	5498.656092	23.652019
122.930333	5512.608414	23.657037
123.238606	5526.591823	23.662055
123.351820	5528.559545	23.667072
123.528068	5533.442374	23.672090
123.236392	5559.595035	23.677107
123.553040	5554.739824	23.682125
124.080071	5563.288876	23.687143
123.794540	5571.518260	23.692160
124.338199	5583.170004	23.697178
124.372427	5595.323904	23.702195
124.469780	5594.259636	23.707213
124.477960	5599.130734	23.712231
124.605588	5590.333306	23.717248
124.743697	5608.715944	23.722266
124.693559	5629.361449	23.727283
124.857040	5627.754783	23.732301
124.806700	5632.714687	23.737319
124.819159	5652.016682	23.742336
125.160742	5658.596198	23.747354
125.098771	5667.644411	23.752371
125.464296	5687.160014	23.757389
125.998541	5686.020568	23.762407
126.054845	5684.411317	23.767424
126.366681	5681.934432	23.772442
126.059418	5703.400722	23.777459
126.481669	5705.866780	23.782477
126.813234	5714.097763	23.787495
126.648790	5722.164732	23.792512
127.025296	5718.897058	23.797530
127.002425	5721.604035	23.802547
127.152366	5706.069055	23.807565
126.948949	5722.742366	23.812583
126.906034	5734.904748	23.817600
127.466923	5736.464379	23.822618
126.949783	5744.977834	23.827635
127.523836	5761.040997	23.832653
127.569329	5772.121668	23.837671
127.486287	5786.028461	23.842688
127.923585	5781.696810	23.847706
127.914433	5809.137648	23.852723
128.105406	5805.252027	23.857741
128.317312	5807.787834	23.862759
128.216755	5812.554391	23.867776
128.534090	5823.899383	23.872794
128.682921	5848.187688	23.877811
128.954463	5844.027215	23.882829
129.119275	5850.254992	23.887847
128.917167	5855.098337	23.892864
129.303519	5855.377410	23.897882
129.179131	5874.104354	23.902899
129.244019	5868.103519	23.907917
129.232799	5887.604716	23.912935
129.338956	5903.965299	23.917952
129.799213	5910.377304	23.922970
129.363711	5919.441958	23.927987
129.681735	5935.899398	23.933005
130.304526	5940.881104	23.938023
130.310180	5947.119352	23.943040
130.738639	5961.114693	23.948058
130.613549	5978.443776	23.953075
131.060605	5971.646323	23.958093
131.429982	5977.969781	23.963111
131.073444	5984.264223	23.968128
131.370832	5970.478070	23.973146
131.307056	5973.645587	23.978163
131.755971	5977.567702	23.983181
131.883814	5969.685826	23.988199
131.694820	5973.108556	23.993216
131.720667	5972.128047	23.998234
131.606840	5985.923493	24.003251
131.905650	5995.821536	24.008269
132.102471	5999.077325	24.013287
132.062276	6002.196242	24.018304
132.445159	6016.357833	24.023322
132.390675	6031.281544	24.028339
132.333152	6034.817078	24.033357
132.919395	6032.446658	24.038375
132.894374	6054.405036	24.043392
133.088339	6060.759647	24.048410
133.265110	6059.948615	24.053427
133.520291	6063.367419	24.058445
133.701798	6055.380953	24.063463
133.277567	6065.804247	24.068480
133.968217	6083.646972	24.073498
133.528899	6096.012904	24.078515
133.371833	6100.269285	24.083533
133.660603	6109.390875	24.088551
133.985449	6121.680615	24.093568
134.254990	6126.720285	24.098586
134.702697	6149.714371	24.103603
134.742058	6146.713583	24.108621
134.964037	6152.458726	24.113639
134.849398	6166.250535	24.118656
134.905116	6155.691603	24.123674
134.712057	6171.418832	24.128691
135.047729	6182.071948	24.133709
135.567883	6177.736415	24.138727
135.283277	6199.291074	24.143744
135.767262	6206.693931	24.148762
135.682062	6216.481832	24.153779
136.029469	6217.972489	24.158797
136.201223	6219.846783	24.163815
135.938680	6242.420817	24.168832
136.523488	6242.248895	24.173850
136.554353	6261.964963	24.178867
136.554694	6251.646110	24.183885
136.986616	6257.967585	24.188903
136.861198	6275.784092	24.193920
137.165698	6283.231342	24.198938
137.235519	6280.835437	24.203955
137.428730	6282.190967	24.208973
137.290767	6285.794462	24.213991
137.688491	6310.714976	24.219008
137.594776	6312.486054	24.224026
137.708974	6308.061000	24.229043
137.395285	6317.076573	24.234061
138.010493	6331.143200	24.239079
138.235173	6348.800114	24.244096
138.677719	6342.722347	24.249114
138.292605	6341.839599	24.254131
138.663116	6355.088442	24.259149
138.736539	6373.073208	24.264167
138.667074	6373.781393	24.269184
138.768184	6376.884939	24.274202
138.963954	6390.361522	24.279219
138.678727	6405.465599	24.284237
138.909122	6409.543841	24.289255
138.980227	6419.966294	24.294272
139.598750	6432.713021	24.299290
139.886995	6445.112725	24.304307
140.139977	6462.958031	24.309325
140.574907	6463.507902	24.314343
140.256868	6468.031603	24.319360
140.743557	6467.675478	24.324378
140.969429	6463.847067	24.329395
140.973774	6467.148599	24.334413
140.852804	6464.686309	24.339431
140.864634	6468.951271	24.344448
141.134388	6476.151594	24.349466
141.066298	6483.387693	24.354483
141.189529	6489.889098	24.359501
141.336848	6501.727510	24.364519
141.244306	6523.865724	24.369536
141.798606	6514.585070	24.374554
142.120801	6528.460990	24.379571
142.202907	6534.523638	24.384589
142.554203	6546.143875	24.389607
142.540440	6547.351466	24.394624
142.755249	6550.447148	24.399642
142.667026	6553.733560	24.404659
142.483672	6557.200372	24.409677
142.706269	6575.565231	24.414695
142.871833	6584.371578	24.419712
143.145127	6602.210666	24.424730
143.360927	6612.418987	24.429747
143.217526	6621.791556	24.434765
143.431739	6618.410301	24.439783
143.813741	6633.957417	24.444800
144.060616	6647.532306	24.449818
143.880756	6658.007531	24.454835
144.066046	6661.535970	24.459853
143.940840	6669.179394	24.464871
144.013107	6688.920113	24.469888
144.258867	6695.572811	24.474906
144.839834	6712.350340	24.479923
144.639407	6724.454456	24.484941
144.762678	6718.596612	24.489959
145.091179	6743.847553	24.494976
145.385317	6757.182108	24.499994
145.638299	6754.125893	24.505011
145.421412	6765.327037	24.510029
145.794815	6755.769792	24.515047
146.000188	6785.474957	24.520064
146.132907	6783.761346	24.525082
146.444458	6789.171433	24.530099
146.430372	6794.560269	24.535117
146.691610	6783.919339	24.540135
146.633193	6791.261052	24.545152
146.935357	6808.436428	24.550170
147.286849	6814.856731	24.555187
147.302649	6822.950633	24.560205
147.459684	6820.078870	24.565223
147.407663	6825.111826	24.570240
147.220851	6825.195121	24.575258
147.357396	6828.759698	24.580275
147.288841	6851.461088	24.585293
147.966885	6845.451793	24.590311
148.083381	6851.093644	24.595328
148.138358	6867.504364	24.600346
148.489960	6878.685765	24.605363
148.629832	6874.751365	24.610381
148.795339	6873.811475	24.615399
148.821119	6880.319147	24.620416
149.148973	6899.184570	24.625434
149.338316	6897.813630	24.630451
149.320590	6906.255979	24.635469
149.532063	6905.809181	24.640487
149.788004	6898.282494	24.645504
149.564003	6911.640004	24.650522
149.851552	6923.897805	24.655539
149.716727	6944.876519	24.660557
149.965172	6940.094684	24.665575
149.879554	6960.346411	24.670592
149.814884	6968.546855	24.675610
150.347864	6978.089554	24.680627
150.577429	6994.531591	24.685645
150.838483	7003.869811	24.690663
150.899362	7006.418892	24.695680
150.932626	7031.120976	24.700698
151.102113	7025.385470	24.705715
151.205509	7039.805838	24.710733
151.681201	7050.021807	24.715751
151.185133	7068.299645	24.720768
151.228252	7073.148346	24.725786
151.800971	7093.858663	24.730803
151.460060	7112.075621	24.735821
151.959250	7124.836468	24.740839
152.515976	7136.559752	24.745856
152.230459	7144.674331	24.750874
152.118972	7163.513358	24.755891
152.301567	7173.605794	24.760909
152.738271	7183.835153	24.765927
152.972124	7192.557010	24.770944
153.320978	7209.152583	24.775962
154.075464	7217.805608	24.780979
154.013186	7224.838920	24.785997
154.315756	7222.969136	24.791015
154.386617	7228.852886	24.796032
154.446177	7233.403164	24.801050
154.618518	7223.350493	24.806067
154.516648	7233.768836	24.811085
154.587525	7231.016169	24.816103
154.776175	7230.708339	24.821120
155.083144	7256.628470	24.826138
155.425452	7258.540227	24.831155
154.997139	7262.737895	24.836173
155.104472	7261.354033	24.841191
155.360236	7266.415962	24.846208
155.383325	7280.695932	24.851226
155.846824	7282.337365	24.856243
155.615181	7294.952863	24.861261
156.183307	7311.578112	24.866279
156.364579	7318.760694	24.871296
156.006153	7322.889796	24.876314
156.582160	7331.268407	24.881331
156.414382	7356.635713	24.886349
156.975915	7353.722175	24.891367
157.157291	7360.748177	24.896384
156.865305	7378.649999	24.901402
156.933248	7376.653940	24.906419
156.911834	7405.449131	24.911437
157.283849	7416.501787	24.916455
157.512169	7421.313204	24.921472
157.524909	7452.504523	24.926490
157.876717	7446.185054	24.931507
158.076725	7465.593266	24.936525
158.299132	7480.597032	24.941543
158.542052	7492.823076	24.946560
158.790037	7497.378014	24.951578
158.938943	7503.151859	24.956595
158.965473	7526.986358	24.961613
159.378809	7524.664530	24.966631
159.540240	7526.229042	24.971648
159.269939	7549.414531	24.976666
159.665842	7547.665954	24.981683
159.876707	7558.011054	24.986701
160.051513	7563.923216	24.991719
160.470540	7575.133736	24.996736
160.427998	7583.026473	25.001754
160.662318	7577.525134	25.006771
160.172969	7589.263699	25.011789
160.651237	7603.011088	25.016807
160.973702	7601.784103	25.021824
160.846287	7623.826430	25.026842
161.444591	7640.293011	25.031859
161.546225	7641.399670	25.036877
161.617554	7644.120305	25.041895
161.878704	7654.578632	25.046912
161.840753	7670.281922	25.051930
162.471065	7666.562622	25.056947
162.439184	7681.683460	25.061965
162.498298	7688.145254	25.066983
162.558763	7682.715661	25.072000
162.631443	7687.082219	25.077018
162.631217	7708.386767	25.082035
162.595324	7712.355962	25.087053
162.869361	7718.059580	25.092071
163.019844	7742.371176	25.097088
163.111047	7750.669949	25.102106
163.596600	7748.473489	25.107123
163.613532	7770.853407	25.112141
163.643165	7785.065932	25.117159
164.148724	7784.556484	25.122176
163.777209	7813.409068	25.127194
164.126727	7821.659613	25.132211
164.495556	7824.036196	25.137229
164.513558	7844.795874	25.142247
165.100231	7844.454474	25.147264
164.961051	7848.627450	25.152282
165.285265	7857.073261	25.157299
165.407706	7873.423186	25.162317
165.706219	7883.891456	25.167335
166.235849	7882.612534	25.172352
165.957890	7898.921670	25.177370
166.257010	7897.396222	25.182387
166.417624	7901.443513	25.187405
166.313650	7900.267970	25.192423
166.374497	7912.720896	25.197440
166.735462	7930.714420	25.202458
166.816554	7938.336617	25.207475
167.075961	7950.222836	25.212493
166.963918	7968.655361	25.217511
167.429762	7960.654022	25.222528
167.329532	7982.108674	25.227546
167.634367	7994.082112	25.232563
167.718543	8004.417820	25.237581
167.834623	8009.487324	25.242599
167.994386	8027.132977	25.247616
168.047419	8042.812709	25.252634
168.881545	8052.767242	25.257651
168.681743	8063.869450	25.262669
168.761155	8072.810024	25.267687
169.123171	8076.912597	25.272704
169.092168	8093.162111	25.277722
169.181928	8096.269401	25.282739
169.719403	8111.430129	25.287757
169.321306	8121.462740	25.292775
169.843548	8132.630079	25.297792
169.708648	8151.232900	25.302810
170.150913	8154.357969	25.307827
170.448023	8165.738278	25.312845
170.378285	8171.757736	25.317863
170.841345	8188.914170	25.322880
170.616344	8195.118919	25.327898
170.828681	8194.647556	25.332915
170.903160	8215.986950	25.337933
171.238798	8224.376066	25.342951
171.479840	8224.718105	25.347968
171.352269	8256.828176	25.352986
171.991866	8263.726073	25.358003
172.274301	8255.503586	25.363021
172.581636	8264.937519	25.368039
172.682717	8250.896103	25.373056
172.750283	8282.711114	25.378074
172.743238	8281.119554	25.383091
172.834320	8285.920084	25.388109
172.996896	8294.391521	25.393127
173.388023	8311.017389	25.398144
173.317303	8329.598789	25.403162
173.534725	8330.044140	25.408179
173.724720	8338.816550	25.413197
173.805261	8355.898422	25.418215
173.871779	8356.073137	25.423232
174.203453	8372.941083	25.428250
174.171516	8386.912187	25.433267
174.293677	8395.083625	25.438285
174.713569	8411.208874	25.443303
174.877121	8423.126885	25.448320
175.066865	8417.515492	25.453338
175.112505	8438.247194	25.458355
175.247309	8458.034187	25.463373
175.406134	8469.731080	25.468391
175.925111	8476.037272	25.473408
175.758516	8492.193554	25.478426
176.136445	8490.676730	25.483443
176.006423	8517.880177	25.488461
176.215535	8525.999659	25.493479
176.430319	8530.448860	25.498496
176.269601	8554.931005	25.503514
176.485926	8565.660736	25.508531
176.705361	8577.833578	25.513549
176.686217	8600.727262	25.518567
177.289608	8600.984786	25.523584
177.545115	8621.273690	25.528602
177.675269	8648.108927	25.533619
177.991379	8656.575372	25.538637
178.044888	8664.155908	25.543655
178.206005	8679.770680	25.548672
178.342128	8698.794860	25.553690
178.674055	8716.528770	25.558707
179.198644	8719.274916	25.563725
179.060028	8736.108869	25.568743
179.666232	8738.276208	25.573760
179.793979	8745.376730	25.578778
179.834757	8752.556829	25.583795
180.079799	8753.016283	25.588813
180.112927	8786.556499	25.593831
180.233323	8781.412446	25.598848
180.294007	8789.201224	25.603866
180.467593	8799.467355	25.608883
181.153188	8819.201244	25.613901
180.676094	8822.103174	25.618919
180.950102	8825.447224	25.623936
181.105021	8833.228084	25.628954
181.704055	8845.042771	25.633971
182.497498	8844.154528	25.638989
181.967398	8854.743783	25.644007
182.429628	8847.374853	25.649024
182.200170	8846.764189	25.654042
182.675525	8862.587953	25.659059
182.874377	8870.269757	25.664077
182.613945	8875.971683	25.669095
182.910724	8879.284179	25.674112
183.006952	8891.068107	25.679130
183.153117	8908.423049	25.684148
183.262247	8904.350980	25.689165
183.382647	8918.897148	25.694183
183.724871	8933.358388	25.699200
183.833726	8943.243832	25.704218
183.902921	8959.062808	25.709236
184.422577	8971.777129	25.714253
184.165474	8982.277700	25.719271
184.504498	9001.589020	25.724288
184.819023	9006.328582	25.729306
184.855972	9027.928511	25.734324
185.261385	9036.504878	25.739341
185.203429	9046.815176	25.744359
185.662841	9057.273178	25.749376
185.473870	9071.620930	25.754394
185.706612	9080.886276	25.759412
186.208006	9096.665610	25.764429
185.950308	9121.600105	25.769447
186.322491	9123.911838	25.774464
186.948621	9127.940334	25.779482
187.004582	9120.735985	25.784500
187.938980	9115.573396	25.789517
187.689216	9121.096650	25.794535
188.098784	9134.468841	25.799552
188.462078	9141.641384	25.804570
188.407481	9144.400075	25.809588
188.545228	9140.055031	25.814605
188.706236	9150.932899	25.819623
188.767804	9156.158643	25.824640
189.046591	9154.749636	25.829658
188.950391	9157.767572	25.834676
188.941638	9162.455634	25.839693
189.009302	9186.754452	25.844711
189.004885	9189.795142	25.849728
189.260015	9209.460461	25.854746
189.308795	9218.060738	25.859764
189.913677	9227.225925	25.864781
189.961091	9246.512046	25.869799
189.922843	9251.577460	25.874816
190.111752	9271.879832	25.879834
189.972365	9294.790203	25.884852
190.434215	9304.042377	25.889869
190.839504	9322.680145	25.894887
191.055187	9339.344574	25.899904
191.145245	9355.562776	25.904922
191.022404	9362.017708	25.909940
191.546051	9378.576815	25.914957
191.592022	9393.895906	25.919975
191.720776	9400.721143	25.924992
192.056498	9425.067323	25.930010
192.242957	9431.853470	25.935028
192.450826	9449.284193	25.940045
192.324328	9467.432045	25.945063
192.778589	9483.271635	25.950080
193.040350	9495.363715	25.955098
192.856120	9507.436012	25.960116
193.362778	9518.973605	25.965133
193.459766	9539.466487	25.970151
193.248708	9563.876061	25.975168
193.649232	9574.976931	25.980186
193.797531	9598.965691	25.985204
194.293717	9616.528892	25.990221
194.379404	9631.988663	25.995239
194.531371	9647.960433	26.000256
194.966157	9662.546129	26.005274
194.914107	9682.366101	26.010292
195.572799	9691.284149	26.015309
195.410926	9711.327461	26.020327
195.842922	9728.915586	26.025344
196.191443	9735.117674	26.030362
196.355433	9743.952504	26.035380
196.737268	9757.535862	26.040397
196.728315	9769.911350	26.045415
197.000054	9779.207113	26.050432
197.518955	9795.608076	26.055450
197.239973	9817.061579	26.060468
197.364427	9804.561012	26.065485
197.560108	9830.623759	26.070503
197.705131	9849.735334	26.075520
197.857745	9858.577948	26.080538
197.821211	9873.353102	26.085556
198.160237	9886.563682	26.090573
198.546985	9907.481881	26.095591
198.561432	9917.638394	26.100608
198.985450	9931.327330	26.105626
198.984740	9953.370582	26.110644
199.329978	9969.483839	26.115661
199.597941	9978.354173	26.120679
199.712267	9992.281021	26.125696
200.093723	10010.146291	26.130714
199.913034	10027.917437	26.135732
200.692125	10042.788989	26.140749
200.347328	10043.319305	26.145767
200.688192	10061.141526	26.150784
201.130764	10070.117080	26.155802
201.007750	10089.130032	26.160820
201.331476	10097.223832	26.165837
201.557745	10115.110426	26.170855
201.597868	10129.449024	26.175872
201.884962	10133.960370	26.180890
201.557010	10148.353731	26.185908
201.997156	10163.472252	26.190925
202.270883	10179.620351	26.195943
202.313396	10190.339608	26.200960
203.144341	10195.602033	26.205978
202.970954	10212.151987	26.210996
203.624088	10230.784033	26.216013
203.830896	10240.002289	26.221031
203.824716	10246.944256	26.226048
204.349826	10252.749697	26.231066
204.218032	10277.675867	26.236084
204.587008	10268.922611	26.241101
204.613715	10285.125550	26.246119
205.119289	10299.607716	26.251136
205.331847	10309.966651	26.256154
205.199906	10324.034590	26.261172
205.273189	10325.063336	26.266189
205.695281	10342.935116	26.271207
205.387676	10349.875208	26.276224
206.102261	10368.976131	26.281242
206.279764	10383.209254	26.286260
206.656048	10389.243491	26.291277
206.646581	10403.629607	26.296295
206.680062	10425.571689	26.301312
207.086140	10433.246444	26.306330
206.981816	10449.784468	26.311348
206.878651	10467.030441	26.316365
207.463396	10480.980337	26.321383
207.288878	10499.236249	26.326400
207.930108	10517.471926	26.331418
208.187760	10537.069716	26.336436
208.701503	10546.582370	26.341453
208.828106	10552.999223	26.346471
208.852964	10581.854515	26.351488
208.979575	10580.874170	26.356506
208.994792	10602.177211	26.361524
209.374362	10618.018103	26.366541
210.014645	10631.550034	26.371559
209.664925	10659.196899	26.376576
210.269133	10658.450893	26.381594
209.997144	10677.886962	26.386612
210.754156	10681.987107	26.391629
210.806763	10698.343766	26.396647
211.013598	10721.081479	26.401664
211.539942	10715.211343	26.406682
211.639094	10731.218654	26.411700
211.806713	10744.435672	26.416717
211.759750	10750.385631	26.421735
211.955565	10767.663184	26.426752
212.496544	10776.557758	26.431770
212.485680	10786.904237	26.436788
212.658851	10785.555602	26.441805
213.251888	10801.755780	26.446823
212.997041	10812.446147	26.451840
213.402324	10806.581503	26.456858
213.612900	10821.195413	26.461876
213.985064	10840.891431	26.466893
214.233414	10845.055397	26.471911
214.269535	10844.536497	26.476928
214.428377	10861.208132	26.481946
214.511178	10892.143572	26.486964
214.511960	10888.537641	26.491981
214.554057	10903.587355	26.496999
214.739855	10923.736618	26.502016
215.372078	10933.516719	26.507034
215.284928	10954.803914	26.512052
215.371104	10976.933583	26.517069
215.751510	10991.536325	26.522087
215.707140	11008.329453	26.527104
216.015090	11029.301520	26.532122
216.023280	11052.636891	26.537140
216.594649	11058.601341	26.542157
216.742929	11086.357306	26.547175
216.809024	11113.061153	26.552192
217.216797	11124.370978	26.557210
217.432020	11143.033435	26.562228
217.486606	11165.014546	26.567245
217.709509	11180.659844	26.572263
217.810401	11198.963205	26.577280
218.485365	11211.719213	26.582298
218.889131	11226.646662	26.587316
218.897525	11259.522604	26.592333
219.526193	11264.871576	26.597351
219.338666	11278.190145	26.602368
219.983411	11289.962887	26.607386
220.634902	11295.211030	26.612404
220.720042	11295.523698	26.617421
221.127400	11305.019557	26.622439
220.725374	11317.075675	26.627456
221.113197	11324.159175	26.632474
220.900609	11328.662782	26.637492
220.834444	11347.697766	26.642509
221.500899	11361.058541	26.647527
221.316382	11395.669520	26.652544
221.840707	11396.615026	26.657562
222.265157	11413.460977	26.662580
222.159326	11432.267058	26.667597
222.662089	11438.802202	26.672615
222.549408	11461.830642	26.677632
222.919835	11463.270368	26.682650
222.871261	11496.279475	26.687668
222.923276	11512.311262	26.692685
223.323603	11525.083771	26.697703
223.260624	11542.981569	26.702720
223.600292	11565.174006	26.707738
224.499665	11576.542559	26.712756
224.343059	11602.099405	26.717773
225.022761	11599.111744	26.722791
224.988703	11626.132532	26.727808
225.324994	11631.285629	26.732826
225.306809	11642.875078	26.737844
225.586768	11655.815250	26.742861
226.024665	11658.461258	26.747879
225.939897	11671.205752	26.752896
226.105576	11691.085145	26.757914
226.184941	11711.234124	26.762932
226.673308	11722.368627	26.767949
227.002452	11735.896060	26.772967
227.325458	11752.568482	26.777984
227.480371	11764.138300	26.783002
228.084851	11765.567703	26.788020
228.100077	11765.933242	26.793037
228.668694	11776.148470	26.798055
228.631696	11801.465611	26.803072
228.873906	11802.663908	26.808090
228.893049	11810.637571	26.813108
229.046772	11836.325978	26.818125
229.014302	11844.933227	26.823143
229.026949	11862.749295	26.828160
229.654348	11873.790123	26.833178
229.850116	11903.493568	26.838196
229.536094	11911.451721	26.843213
229.940069	11928.577584	26.848231
230.113970	11945.858993	26.853248
230.556752	11964.520821	26.858266
230.680075	11988.253879	26.863284
230.967270	12007.486805	26.868301
231.585162	12015.706926	26.873319
232.082032	12027.534124	26.878336
232.371416	12033.604524	26.883354
233.322359	12032.187880	26.888372
233.816089	12042.625579	26.893389
234.289735	12024.392944	26.898407
233.876765	12028.345066	26.903424
234.133814	12015.693834	26.908442
234.403110	12014.036774	26.913460
234.198501	12037.200379	26.918477
234.291264	12048.141003	26.923495
234.407812	12036.587325	26.928512
234.503370	12050.680221	26.933530
234.803725	12065.993742	26.938548
234.588022	12080.108931	26.943565
234.963866	12093.092832	26.948583
234.941086	12115.335393	26.953600
235.198900	12138.467155	26.958618
235.978377	12148.154134	26.963636
235.489428	12167.481667	26.968653
235.749187	12182.742153	26.973671
235.859075	12207.137879	26.978688
236.100276	12236.973660	26.983706
236.220368	12256.993099	26.988724
236.470945	12282.473193	26.993741
236.751126	12295.114776	26.998759
237.070006	12316.844086	27.003776
237.245020	12341.073798	27.008794
237.634758	12356.413506	27.013812
237.864966	12374.589444	27.018829
238.113484	12395.807046	27.023847
238.337722	12413.180338	27.028864
238.554620	12428.128924	27.033882
238.817384	12438.847328	27.038900
238.750999	12471.748442	27.043917
239.161048	12489.566244	27.048935
239.366133	12511.335422	27.053952
239.335147	12541.086099	27.058970
239.571443	12561.125590	27.063988
239.610254	12589.787664	27.069005
240.197213	12612.924944	27.074023
240.764788	12632.188746	27.079040
241.216672	12648.199118	27.084058
241.838886	12664.723703	27.089076
242.019297	12688.174046	27.094093
242.475453	12679.248485	27.099111
242.604681	12700.211213	27.104128
242.732674	12710.731290	27.109146
243.284054	12705.295041	27.114164
243.425217	12731.571605	27.119181
243.871492	12735.162213	27.124199
243.740877	12736.083124	27.129216
244.134138	12748.577971	27.134234
244.480779	12765.216452	27.139252
244.440409	12788.251902	27.144269
244.962517	12782.848236	27.149287
245.016582	12806.872652	27.154304
245.153827	12819.385933	27.159322
245.295466	12825.242882	27.164340
245.240416	12838.504307	27.169357
245.629534	12843.738151	27.174375
245.736788	12865.983120	27.179392
246.000991	12886.856896	27.184410
246.170777	12901.786893	27.189428
246.294730	12934.442988	27.194445
246.193114	12950.529512	27.199463
246.808266	12982.715709	27.204480
246.785431	13002.579246	27.209498
247.152130	13019.622354	27.214516
247.361724	13051.819228	27.219533
247.702505	13063.804657	27.224551
248.369407	13089.016262	27.229568
248.243526	13099.997611	27.234586
249.020658	13115.821931	27.239604
248.958908	13142.925885	27.244621
249.279462	13156.009936	27.249639
249.656800	13166.796588	27.254656
249.543942	13191.294042	27.259674
249.780476	13196.224677	27.264692
250.336459	13215.877564	27.269709
250.538719	13227.177744	27.274727
250.684217	13244.436525	27.279744
250.835022	13254.887221	27.284762
251.320061	13267.512998	27.289780
251.497736	13290.204898	27.294797
251.889500	13298.847184	27.299815
252.159217	13323.700768	27.304832
252.208042	13324.883279	27.309850
252.390028	13345.972329	27.314868
252.751226	13363.987175	27.319885
252.653192	13379.565464	27.324903
252.850327	13388.784725	27.329920
252.930524	13416.323881	27.334938
253.452411	13435.936044	27.339956
253.763936	13463.948793	27.344973
254.075678	13489.172314	27.349991
254.236764	13500.059796	27.355008
254.415705	13529.460920	27.360026
254.656038	13545.890988	27.365044
255.208579	13564.633818	27.370061
255.603423	13580.942276	27.375079
255.939707	13607.163861	27.380096
256.004658	13619.629103	27.385114
256.325211	13630.278525	27.390132
256.198614	13650.955282	27.395149
256.639265	13671.753498	27.400167
257.106049	13698.525735	27.405184
257.254996	13717.960078	27.410202
257.297610	13733.482752	27.415220
257.510319	13753.598715	27.420237
258.008725	13775.566383	27.425255
258.192661	13786.323100	27.430272
258.546744	13818.839315	27.435290
259.135849	13825.311162	27.440308
259.375064	13842.217092	27.445325
259.669929	13870.864471	27.450343
260.106708	13872.917515	27.455360
259.793415	13880.893296	27.460378
260.295041	13895.532164	27.465396
260.892866	13920.825237	27.470413
261.012354	13922.093651	27.475431
261.350639	13941.609486	27.480448
261.326967	13955.350609	27.485466
261.813268	13967.356065	27.490484
261.717480	13980.754565	27.495501
261.808303	13994.665318	27.500519
262.367168	14007.568748	27.505536
262.285481	14034.085976	27.510554
262.699859	14042.997946	27.515572
263.136930	14071.718876	27.520589
263.181097	14087.356005	27.525607
263.847654	14107.055691	27.530624
263.592970	14114.889312	27.535642
264.488069	14130.695203	27.540660
264.289149	14151.330927	27.545677
264.565801	14162.023611	27.550695
265.035830	14181.459713	27.555712
265.190930	14195.281781	27.560730
265.370311	14196.946477	27.565748
265.581108	14216.284609	27.570765
265.596318	14233.923849	27.575783
265.719217	14255.892530	27.580800
265.702628	14281.069619	27.585818
266.348022	14289.747616	27.590836
266.639031	14335.347838	27.595853
266.717028	14341.604399	27.600871
267.106822	14368.082577	27.605888
267.226032	14403.032677	27.610906
267.844163	14414.851962	27.615924
267.881656	14436.908218	27.620941
268.130125	14464.450877	27.625959
268.686867	14480.613555	27.630976
268.733967	14502.894702	27.635994
269.293226	14518.941200	27.641012
269.555625	14546.320404	27.646029
269.566682	14560.399370	27.651047
269.868725	14576.977369	27.656064
270.027898	14609.270286	27.661082
270.328813	14620.168851	27.666100
270.662979	14644.733959	27.671117
270.706529	14671.163541	27.676135
271.174115	14689.410286	27.681152
271.565612	14726.876035	27.686170
272.038643	14741.804074	27.691188
272.188517	14762.326768	27.696205
272.584090	14791.158792	27.701223
272.931077	14797.539854	27.706240
272.992530	14827.637059	27.711258
273.520460	14838.219535	27.716276
273.911119	14853.565060	27.721293
274.057203	14871.210545	27.726311
274.666950	14885.929373	27.731328
274.495745	14903.963786	27.736346
275.025682	14920.136419	27.741364
275.514321	14936.069539	27.746381
275.456646	14964.375235	27.751399
275.849175	14968.275284	27.756416
275.900131	14984.719076	27.761434
276.014968	14999.213314	27.766452
276.365917	15015.617195	27.771469
276.958150	15031.022288	27.776487
277.518115	15026.348387	27.781504
277.860799	15058.974545	27.786522
277.788401	15052.930448	27.791540
277.787684	15070.069247	27.796557
277.961119	15089.391408	27.801575
278.117678	15108.417816	27.806592
278.464948	15137.795197	27.811610
278.617034	15158.672531	27.816628
279.327359	15171.302460	27.821645
279.634798	15189.594911	27.826663
279.507175	15199.477548	27.831680
279.612052	15213.054549	27.836698
280.205086	15238.356079	27.841716
280.043228	15250.840200	27.846733
280.159216	15282.072509	27.851751
280.599459	15302.385007	27.856768
280.886272	15329.761817	27.861786
282.082992	15327.251596	27.866804
282.536923	15341.616041	27.871821
282.933783	15361.159090	27.876839
283.312398	15350.453416	27.881856
283.133717	15368.713542	27.886874
283.431971	15378.764595	27.891892
283.440398	15388.209695	27.896909
283.700873	15405.000202	27.901927
284.226444	15426.612628	27.906944
284.350352	15443.389320	27.911962
284.700936	15460.379466	27.916980
284.765050	15472.906969	27.921997
284.777600	15505.667981	27.927015
285.117064	15512.409837	27.932032
285.634155	15548.112676	27.937050
285.835791	15566.603219	27.942068
285.947122	15580.265624	27.947085
285.946097	15607.727482	27.952103
286.089376	15622.255170	27.957120
286.234907	15655.543056	27.962138
286.626868	15682.525544	27.967156
286.857943	15713.076704	27.972173
287.113162	15746.465594	27.977191
287.518474	15770.468194	27.982208
287.869098	15804.658027	27.987226
288.143926	15832.974617	27.992244
288.646920	15849.406331	27.997261
288.801181	15881.791273	28.002279
289.618032	15901.862477	28.007296
289.365449	15933.538068	28.012314
289.668084	15956.681850	28.017332
289.995671	15980.208647	28.022349
290.453359	16008.633011	28.027367
290.891824	16030.462113	28.032384
290.773740	16060.367338	28.037402
291.173780	16086.218088	28.042420
291.752037	16108.121661	28.047437
292.027400	16130.714607	28.052455
292.367334	16161.410506	28.057472
292.644519	16175.085386	28.062490
292.942754	16193.822869	28.067508
293.810727	16215.316682	28.072525
293.782945	16224.191753	28.077543
294.468841	16238.239293	28.082560
294.618346	16249.508879	28.087578
294.706865	16266.949908	28.092596
295.297749	16274.673765	28.097613
295.448799	16292.225315	28.102631
295.776070	16297.776481	28.107648
295.613906	16318.086347	28.112666
295.610574	16342.885797	28.117684
296.377931	16357.943977	28.122701
296.502840	16368.294439	28.127719
296.564668	16392.917854	28.132736
296.927236	16421.368375	28.137754
296.890897	16437.047984	28.142772
297.390574	16462.255202	28.147789
297.999783	16489.044848	28.152807
297.831343	16509.004817	28.157824
298.146715	16532.592863	28.162842
298.549038	16567.338891	28.167860
298.538194	16581.347216	28.172877
298.822955	16620.520951	28.177895
299.307378	16640.516590	28.182912
299.713044	16675.131630	28.187930
299.605098	16704.447950	28.192948
299.955217	16723.441369	28.197965
300.357439	16757.119029	28.202983
300.735109	16793.503419	28.208000
300.986198	16814.715515	28.213018
301.368576	16846.432902	28.218036
301.743670	16873.174709	28.223053
302.072041	16899.257126	28.228071
302.644881	16931.908832	28.233088
303.013968	16943.118536	28.238106
303.147920	16969.344058	28.243124
304.048758	16978.107383	28.248141
304.202818	17002.203518	28.253159
305.009829	17011.464463	28.258176
305.209216	17034.643639	28.263194
305.447528	17046.892309	28.268212
305.997252	17059.151983	28.273229
305.867015	17084.046463	28.278247
305.914548	17082.290175	28.283264
306.132595	17101.838542	28.288282
306.269186	17128.999884	28.293300
306.510325	17148.056073	28.298317
306.833705	17178.024978	28.303335
307.069695	17212.276552	28.308352
307.348500	17230.938670	28.313370
307.716275	17266.331507	28.318388
308.084977	17278.148181	28.323405
308.177311	17314.464120	28.328423
308.797116	17328.975339	28.333440
309.005304	17352.381334	28.338458
309.226077	17377.664418	28.343476
309.617957	17399.952670	28.348493
309.593502	17444.438003	28.353511
309.873297	17457.912233	28.358528
310.518993	17482.487237	28.363546
310.530477	17518.105143	28.368564
310.792180	17536.818386	28.373581
311.141901	17573.710034	28.378599
311.600539	17600.814183	28.383616
311.913541	17620.654362	28.388634
312.131798	17649.757490	28.393652
312.706673	17676.932221	28.398669
312.813083	17691.927958	28.403687
312.932455	17715.621879	28.408704
313.447303	17731.491520	28.413722
313.549465	17760.316512	28.418740
314.064498	17788.230886	28.423757
314.302430	17815.866643	28.428775
314.546270	17841.942860	28.433792
315.201930	17869.938905	28.438810
315.498023	17894.468313	28.443828
315.800901	17911.182152	28.448845
316.314492	17931.437608	28.453863
316.154716	17959.182279	28.458880
316.944677	17973.445334	28.463898
317.091220	18000.332205	28.468916
317.676381	18023.045668	28.473933
317.984982	18045.881193	28.478951
318.192997	18059.716601	28.483968
318.692833	18083.578007	28.488986
319.069233	18097.332282	28.494004
319.367166	18110.462061	28.499021
319.820018	18130.360527	28.504039
320.025830	18162.324891	28.509056
320.271436	18174.653213	28.514074
320.432238	18193.495929	28.519092
320.768289	18200.625541	28.524109
320.764236	18245.003611	28.529127
321.235933	18265.927610	28.534144
321.570864	18285.846643	28.539162
321.681733	18317.507947	28.544180
322.253266	18338.724014	28.549197
322.544362	18370.848840	28.554215
322.498295	18395.100097	28.559232
323.014348	18416.595591	28.564250
323.449391	18442.551397	28.569268
324.007425	18480.535654	28.574285
324.393597	18497.988055	28.579303
324.658787	18515.158959	28.584320
324.960638	18530.998797	28.589338
325.058580	18544.054907	28.594356
325.432373	18580.269100	28.599373
326.119471	18607.539787	28.604391
325.989341	18639.638594	28.609408
326.445029	18651.579075	28.614426
326.776414	18675.659585	28.619444
327.567830	18693.977585	28.624461
327.420387	18722.733897	28.629479
327.154895	18764.007324	28.634496
327.728452	18782.192817	28.639514
327.980498	18808.199264	28.644532
328.250233	18841.906108	28.649549
328.622057	18870.029906	28.654567
328.936883	18893.333426	28.659584
329.490935	18918.904111	28.664602
329.485250	18952.203090	28.669620
330.250610	18963.202673	28.674637
330.877810	18983.922532	28.679655
331.020220	19010.937797	28.684672
331.997674	19018.509305	28.689690
332.202210	19041.348308	28.694708
332.245619	19058.177965	28.699725
332.846857	19075.121905	28.704743
332.568953	19101.915709	28.709760
333.078173	19112.878261	28.714778
333.212989	19146.473791	28.719796
333.547001	19164.138023	28.724813
333.826464	19188.054358	28.729831
333.947492	19219.128820	28.734848
334.630028	19241.060772	28.739866
334.567065	19272.422949	28.744884
335.019374	19298.156940	28.749901
335.637042	19332.122413	28.754919
335.661797	19359.966944	28.759936
335.813520	19383.970871	28.764954
335.780161	19423.465185	28.769972
336.465425	19451.136106	28.774989
337.121820	19476.958745	28.780007
337.451013	19516.727439	28.785024
337.885266	19530.401709	28.790042
338.289143	19565.456982	28.795060
338.624078	19591.600752	28.800077
339.364918	19606.561801	28.805095
339.401295	19635.282225	28.810112
339.983234	19644.549530	28.815130
340.351480	19671.985114	28.820148
340.805092	19693.312778	28.825165
341.152867	19711.102222	28.830183
341.021208	19735.638517	28.835200
341.583895	19753.137827	28.840218
341.808793	19774.724910	28.845236
342.400636	19801.042288	28.850253
342.614654	19825.563010	28.855271
342.917756	19848.197699	28.860288
342.885762	19865.906485	28.865306
342.807323	19900.997242	28.870324
343.398668	19933.006167	28.875341
344.032651	19959.568308	28.880359
344.318631	19998.293405	28.885376
344.560479	20023.782568	28.890394
344.627052	20051.120022	28.895412
345.148948	20084.850787	28.900429
345.635463	20113.038478	28.905447
345.755996	20159.671723	28.910464
346.247726	20188.588348	28.915482
346.278821	20217.922577	28.920500
346.848420	20245.935040	28.925517
347.190544	20262.454176	28.930535
347.369261	20294.875711	28.935552
347.902690	20322.240829	28.940570
348.220110	20347.849597	28.945588
348.277141	20383.486069	28.950605
348.831771	20399.685221	28.955623
349.074132	20440.432449	28.960640
349.906343	20452.608847	28.965658
350.106855	20490.218285	28.970676
350.538302	20513.138255	28.975693
350.613851	20535.507788	28.980711
350.734414	20572.245767	28.985728
351.019905	20606.806797	28.990746
351.705462	20645.252061	28.995764
351.736414	20673.573999	29.000781
352.523312	20705.135946	29.005799
352.500113	20739.093590	29.010816
352.799616	20773.382627	29.015834
353.483129	20811.241117	29.020852
353.624315	20845.083802	29.025869
353.900739	20871.208317	29.030887
354.536101	20908.087132	29.035904
354.910548	20932.356416	29.040922
355.407534	20958.294719	29.045940
355.550264	20998.427654	29.050957
356.073470	21025.314040	29.055975
356.248598	21063.194298	29.060992
356.674852	21090.318336	29.066010
357.290573	21123.700884	29.071028
357.310057	21159.541198	29.076045
358.028269	21185.535979	29.081063
357.947063	21222.343856	29.086080
358.471586	21252.179059	29.091098
359.045089	21281.754493	29.096116
359.223269	21323.645180	29.101133
359.714419	21349.824480	29.106151
359.628380	21389.024578	29.111168
360.618895	21407.949620	29.116186
361.096754	21435.787448	29.121204
361.078651	21471.885696	29.126221
361.675679	21501.579081	29.131239
361.747088	21531.465755	29.136256
362.097251	21558.052208	29.141274
362.580593	21581.288374	29.146292
362.988878	21618.416113	29.151309
363.384990	21634.550444	29.156327
363.785160	21659.327106	29.161344
364.134135	21692.651770	29.166362
364.641414	21719.074054	29.171380
364.575622	21751.011047	29.176397
365.621394	21771.317034	29.181415
366.310473	21790.989168	29.186432
366.591353	21812.871779	29.191450
367.203850	21814.237529	29.196468
367.575783	21830.047488	29.201485
368.016032	21840.957190	29.206503
368.116363	21852.913435	29.211520
368.721162	21863.486619	29.216538
369.094251	21881.249683	29.221556
368.887888	21885.818340	29.226573
369.535875	21909.845495	29.231591
369.471736	21929.414940	29.236608
369.775268	21956.429286	29.241626
370.484635	21971.280664	29.246644
370.248104	21991.972422	29.251661
370.641920	22020.246043	29.256679
370.815539	22046.889019	29.261696
371.487607	22060.329525	29.266714
371.467337	22093.548478	29.271732
371.742946	22148.086617	29.276749
372.142369	22172.802772	29.281767
372.163320	22205.196276	29.286784
372.426275	22248.095865	29.291802
372.701761	22285.567681	29.296820
373.123668	22336.620007	29.301837
373.388195	22368.512697	29.306855
374.069900	22421.609518	29.311872
374.518996	22450.580023	29.316890
375.020542	22478.355271	29.321908
375.258971	22522.678027	29.326925
376.042062	22558.998430	29.331943
376.422994	22588.949624	29.336960
376.699974	22621.089730	29.341978
377.268587	22654.503508	29.346996
377.820267	22684.610405	29.352013
378.505666	22700.713910	29.357031
378.843453	22731.331501	29.362048
379.064223	22761.127384	29.367066
379.464202	22786.886460	29.372084
379.523884	22820.384834	29.377101
380.093549	22850.374973	29.382119
381.294769	22862.778799	29.387136
381.945012	22863.761353	29.392154
382.783947	22883.332213	29.397172
382.927618	22913.463604	29.402189
383.321378	22910.450337	29.407207
383.490858	22909.492336	29.412224
383.624945	22928.876260	29.417242
384.006882	22939.464417	29.422260
384.089365	22968.621889	29.427277
384.346338	22984.875869	29.432295
384.860430	23010.343023	29.437312
384.632475	23038.343406	29.442330
385.116586	23064.860642	29.447348
385.135759	23099.337239	29.452365
385.516114	23124.041380	29.457383
385.366606	23158.919910	29.462400
385.646631	23204.969222	29.467418
386.262913	23235.251974	29.472436
386.146424	23275.572982	29.477453
386.594592	23310.948146	29.482471
387.247884	23354.196542	29.487488
387.730668	23398.148835	29.492506
387.747659	23438.398575	29.497524
388.252555	23490.148722	29.502541
388.564328	23523.857316	29.507559
389.029327	23570.109787	29.512576
389.442547	23614.070611	29.517594
389.872045	23648.780760	29.522612
390.066066	23700.645717	29.527629
390.503578	23747.255967	29.532647
390.765792	23780.861150	29.537664
391.554285	23820.855803	29.542682
392.347728	23846.576748	29.547700
393.045360	23895.425571	29.552717
393.649571	23917.548655	29.557735
394.045124	23947.619814	29.562752
394.285806	23980.575060	29.567770
395.133024	23986.486459	29.572788
395.295534	24031.247728	29.577805
395.490969	24050.164012	29.582823
396.033760	24087.078391	29.587840
396.059983	24118.893626	29.592858
396.784923	24146.122616	29.597876
397.127891	24186.844555	29.602893
397.411857	24212.171495	29.607911
397.909233	24241.473933	29.612928
398.033707	24282.845347	29.617946
398.464530	24310.045862	29.622964
398.652923	24350.733770	29.627981
398.888067	24388.395786	29.632999
398.893473	24424.014122	29.638016
399.323278	24463.857224	29.643034
400.133722	24498.413999	29.648052
400.050585	24558.460755	29.653069
400.542193	24597.752386	29.658087
401.084584	24645.786949	29.663104
401.327405	24696.483096	29.668122
401.878759	24732.792625	29.673140
402.372325	24778.376050	29.678157
402.583317	24826.135471	29.683175
402.968049	24865.248641	29.688192
403.344963	24909.428361	29.693210
404.238872	24951.950329	29.698228
404.607784	24998.396346	29.703245
404.889369	25032.906204	29.708263
405.659244	25071.038416	29.713280
405.811188	25110.257812	29.718298
406.804199	25135.809613	29.723316
406.901303	25174.280868	29.728333
407.522126	25205.857787	29.733351
408.073444	25242.264587	29.738368
408.302021	25274.493386	29.743386
408.620999	25310.308724	29.748404
408.914955	25336.569358	29.753421
409.555771	25358.213590	29.758439
410.000180	25387.699092	29.763456
410.127385	25424.339313	29.768474
411.247547	25417.575858	29.773492
412.347631	25428.918591	29.778509
413.161413	25432.036129	29.783527
413.374955	25456.851608	29.788544
413.454785	25464.786739	29.793562
413.690078	25472.675834	29.798580
413.829101	25498.813319	29.803597
414.202890	25512.638312	29.808615
414.599845	25536.985113	29.813632
414.652688	25569.782922	29.818650
415.072548	25589.020559	29.823668
415.412018	25617.857533	29.828685
415.548417	25650.440522	29.833703
415.866849	25666.150179	29.838720
415.803253	25714.460968	29.843738
416.174845	25749.502390	29.848756
416.218272	25803.348722	29.853773
416.541876	25845.751235	29.858791
417.130927	25898.411980	29.863808
417.517096	25955.762682	29.868826
417.872594	25998.552052	29.873844
418.352868	26042.175632	29.878861
418.891936	26092.284620	29.883879
419.263442	26134.251697	29.888896
419.680352	26185.111522	29.893914
419.988716	26233.355150	29.898932
420.729531	26284.215677	29.903949
421.084743	26332.383598	29.908967
421.392231	26368.396931	29.913984
421.798418	26429.348822	29.919002
422.330790	26471.128855	29.924020
422.870054	26513.568096	29.929037
423.386301	26564.374690	29.934055
423.890693	26594.919573	29.939072
424.433257	26646.549454	29.944090
424.958834	26692.477501	29.949108
425.178757	26737.251354	29.954125
425.665143	26782.758108	29.959143
426.268944	26813.138666	29.964160
426.371300	26865.260090	29.969178
426.971343	26895.174999	29.974196
427.254937	26943.367974	29.979213
427.531287	26995.139079	29.984231
427.894571	27029.259677	29.989248
428.626539	27081.881829	29.994266
429.132728	27117.134837	29.999284
429.532770	27168.324261	30.004301
429.710250	27219.461067	30.009319
430.437418	27260.876484	30.014336
430.397465	27302.954703	30.019354
431.145635	27333.518086	30.024372
431.810824	27380.063231	30.029389
431.799349	27417.222496	30.034407
432.353146	27455.587044	30.039424
432.761257	27495.183491	30.044442
433.088544	27538.856770	30.049460
433.283195	27579.399792	30.054477
433.727220	27623.163426	30.059495
434.246523	27669.409617	30.064512
434.643889	27725.297004	30.069530
435.192313	27773.672443	30.074548
436.197808	27820.122092	30.079565
436.079026	27858.931970	30.084583
436.901359	27890.636489	30.089600
437.059242	27932.637550	30.094618
437.732494	27969.482560	30.099636
438.169812	28022.198841	30.104653
438.395997	28056.291449	30.109671
439.445943	28089.077337	30.114688
439.706691	28134.318141	30.119706
440.091334	28171.278928	30.124724
440.833666	28210.158884	30.129741
441.330499	28243.015873	30.134759
441.636766	28282.190818	30.139776
441.595471	28320.751506	30.144794
442.261684	28357.199837	30.149812
442.531164	28400.318925	30.154829
442.671485	28450.441243	30.159847
443.469049	28492.608156	30.164864
444.113376	28528.314986	30.169882
444.776161	28563.193209	30.174900
445.201072	28602.064795	30.179917
445.285865	28640.128667	30.184935
446.110041	28674.682005	30.189952
446.553878	28716.951557	30.194970
447.062581	28743.575129	30.199988
447.511456	28783.149319	30.205005
447.718861	28832.773608	30.210023
448.541326	28858.225358	30.215040
448.830380	28898.843309	30.220058
448.917360	28953.331412	30.225076
449.430932	28980.608590	30.230093
450.121837	29017.325526	30.235111
450.552704	29057.684896	30.240128
450.981563	29102.323258	30.245146
451.296151	29143.728855	30.250164
451.819820	29179.156918	30.255181
451.977115	29228.248283	30.260199
452.484446	29265.617511	30.265216
452.859129	29317.114029	30.270234
453.248418	29355.116878	30.275252
453.471858	29390.944665	30.280269
453.897253	29447.014741	30.285287
454.785417	29480.907165	30.290304
455.230040	29531.285334	30.295322
455.848427	29573.084886	30.300340
455.926675	29604.429066	30.305357
456.401769	29641.946129	30.310375
456.795988	29685.447465	30.315392
457.418687	29725.043531	30.320410
457.541639	29761.427119	30.325428
457.965148	29809.275358	30.330445
458.395857	29853.001419	30.335463
459.319830	29894.357542	30.340480
459.291066	29944.147338	30.345498
460.163733	29979.376552	30.350516
460.787685	30012.782647	30.355533
461.094106	30054.269079	30.360551
461.716308	30092.800747	30.365568
462.444775	30134.998690	30.370586
462.627694	30167.491938	30.375604
463.134873	30195.906896	30.380621
463.485986	30251.096395	30.385639
464.120175	30276.418036	30.390656
464.377171	30324.344743	30.395674
464.922969	30357.781331	30.400692
465.638554	30397.939482	30.405709
465.797175	30433.951669	30.410727
466.580189	30465.699009	30.415744
466.872322	30513.436277	30.420762
467.072998	30560.359255	30.425780
467.674742	30602.796089	30.430797
467.950847	30642.134387	30.435815
468.281959	30697.427867	30.440832
468.525324	30746.284700	30.445850
469.223931	30793.696403	30.450868
469.609111	30828.752943	30.455885
470.078590	30895.829799	30.460903
470.596348	30940.950758	30.465920
471.190740	30986.535610	30.470938
471.315657	31039.702283	30.475956
471.899605	31093.714863	30.480973
472.217751	31145.235600	30.485991
472.619710	31191.274071	30.491008
473.161984	31245.525476	30.496026
473.292364	31299.054622	30.501044
473.949332	31358.402614	30.506061
474.427441	31422.299639	30.511079
475.110356	31483.051427	30.516096
475.624651	31542.088672	30.521114
475.801692	31589.071941	30.526132
476.192893	31654.512567	30.531149
476.568006	31717.193021	30.536167
477.346194	31769.309137	30.541184
478.025769	31824.044949	30.546202
478.567197	31870.980430	30.551220
479.285107	31914.521229	30.556237
479.860452	31964.974319	30.561255
480.498211	32009.068765	30.566272
480.895910	32060.987925	30.571290
481.189946	32100.345769	30.576308
481.965535	32138.556759	30.581325
482.271962	32190.602777	30.586343
482.962573	32221.257020	30.591360
483.670696	32248.822325	30.596378
483.964449	32288.002551	30.601396
484.352793	32323.887707	30.606413
484.435084	32375.046353	30.611431
484.925571	32416.551986	30.616448
485.981383	32452.758249	30.621466
486.502591	32491.522855	30.626484
487.077890	32519.272124	30.631501
487.631741	32565.334374	30.636519
487.791857	32598.512263	30.641536
488.268578	32639.921348	30.646554
488.805812	32682.176798	30.651572
489.333668	32717.055433	30.656589
489.683600	32769.835606	30.661607
489.791744	32819.459390	30.666624
490.469291	32860.715665	30.671642
490.621868	32917.659130	30.676660
491.079359	32964.165010	30.681677
491.567170	33011.615109	30.686695
491.741602	33058.271954	30.691712
492.248353	33113.425764	30.696730
492.844036	33168.936019	30.701748
493.263184	33214.944299	30.706765
493.854609	33277.530010	30.711783
494.598335	33325.272841	30.716800
495.597686	33378.057114	30.721818
495.961055	33437.033751	30.726836
496.522468	33463.063906	30.731853
496.779233	33526.257155	30.736871
497.593563	33563.287760	30.741888
498.213407	33601.969899	30.746906
498.627219	33659.176951	30.751924
499.205516	33701.592402	30.756941
499.506225	33743.864596	30.761959
500.017835	33785.537392	30.766976
500.454785	33841.008976	30.771994
500.797817	33887.021787	30.777012
501.588386	33935.416257	30.782029
501.858305	33977.462223	30.787047
502.529233	34028.849053	30.792064
502.967011	34081.230042	30.797082
503.488062	34132.680476	30.802100
504.022593	34175.431998	30.807117
504.290036	34230.492071	30.812135
504.681652	34281.876884	30.817152
505.495577	34330.703870	30.822170
505.785548	34382.483521	30.827188
506.294301	34433.460770	30.832205
506.746910	34475.731120	30.837223
507.231608	34532.313505	30.842240
507.730745	34575.041740	30.847258
508.088165	34633.218013	30.852276
508.753882	34667.873857	30.857293
508.991918	34726.788327	30.862311
509.445020	34782.515859	30.867328
510.182585	34829.248768	30.872346
510.697479	34886.372996	30.877364
510.934686	34926.189580	30.882381
511.435633	34982.239637	30.887399
511.896885	35037.973030	30.892416
512.802282	35084.632627	30.897434
512.796661	35143.164883	30.902452
513.573241	35195.597877	30.907469
514.018958	35249.584555	30.912487
514.418981	35308.025972	30.917504
514.956449	35350.102148	30.922522
515.172108	35423.196927	30.927540
515.829654	35474.609265	30.932557
516.217267	35540.756295	30.937575
516.480060	35604.757328	30.942592
517.299929	35672.462995	30.947610
517.702531	35740.586968	30.952628
518.389902	35791.872561	30.957645
519.118602	35850.884675	30.962663
519.671717	35909.390515	30.967680
520.378712	35953.172255	30.972698
521.041080	36016.449061	30.977716
521.736942	36072.793343	30.982733
522.093720	36120.284206	30.987751
522.750441	36169.302425	30.992768
523.350899	36217.804748	30.997786
523.715673	36290.827529	31.002804
524.463287	36339.123879	31.007821
525.084567	36375.835184	31.012839
524.972192	36436.927271	31.017856
526.108294	36491.444929	31.022874
526.371460	36543.809419	31.027892
526.883972	36604.649649	31.032909
527.196840	36659.458219	31.037927
527.773094	36713.815091	31.042944
528.079929	36769.747537	31.047962
528.742138	36838.883073	31.052980
529.808560	36876.852099	31.057997
530.151615	36936.534888	31.063015
530.730120	36993.671933	31.068032
531.265975	37041.385985	31.073050
531.901708	37100.680603	31.078068
532.207009	37147.230263	31.083085
533.041242	37202.588222	31.088103
533.586964	37262.520532	31.093120
533.914623	37304.203018	31.098138
533.953084	37370.619408	31.103156
534.283064	37425.448239	31.108173
535.170135	37484.694714	31.113191
535.737165	37545.062955	31.118208
536.353212	37592.874589	31.123226
536.709013	37656.108637	31.128244
537.129942	37709.525360	31.133261
537.796978	37769.572592	31.138279
537.825221	37814.449591	31.143296
538.668097	37866.027360	31.148314
539.053607	37942.265795	31.153332
539.589913	37992.439026	31.158349
540.177161	38057.998098	31.163367
540.637860	38122.144310	31.168384
541.632376	38161.836896	31.173402
541.810193	38219.532284	31.178420
542.487844	38280.814247	31.183437
543.200952	38335.280688	31.188455
543.319224	38399.887724	31.193472
544.399580	38447.788654	31.198490
544.543726	38512.691588	31.203508
545.210415	38573.326718	31.208525
546.229533	38633.191639	31.213543
546.595660	38691.934020	31.218560
547.022856	38736.527586	31.223578
547.691403	38810.413236	31.228596
548.207585	38862.129649	31.233613
548.994090	38912.207412	31.238631
549.278115	38972.545400	31.243648
550.064349	39030.449391	31.248666
550.535400	39098.102962	31.253684
550.741848	39146.383164	31.258701
551.563544	39201.180423	31.263719
551.662342	39262.597551	31.268736
552.286435	39333.521748	31.273754
552.643524	39394.259580	31.278772
553.290668	39462.976175	31.283789
553.845698	39523.140493	31.288807
553.996355	39595.478386	31.293824
554.906776	39654.742928	31.298842
555.414313	39728.863208	31.303860
555.772444	39797.296033	31.308877
556.535250	39866.691252	31.313895
557.020839	39940.129987	31.318912
557.810957	40009.507245	31.323930
558.254356	40078.987316	31.328948
558.956381	40144.216038	31.333965
559.747620	40213.765835	31.338983
560.099053	40275.703034	31.344000
561.248435	40325.402310	31.349018
561.911266	40389.554841	31.354036
562.020518	40451.815104	31.359053
563.122430	40501.251214	31.364071
563.862851	40550.316104	31.369088
564.309894	40602.581831	31.374106
564.880938	40660.164505	31.379124
565.433337	40714.520655	31.384141
566.371276	40756.291036	31.389159
566.633409	40819.004539	31.394176
567.477371	40860.594594	31.399194
568.104585	40894.816773	31.404212
568.496115	40948.505401	31.409229
569.113170	40998.127411	31.414247
569.129862	41037.689132	31.419264
569.432819	41081.766122	31.424282
570.082433	41136.382532	31.429300
570.672758	41182.691252	31.434317
570.817818	41236.391649	31.439335
571.298072	41308.127589	31.444352
571.924545	41364.489474	31.449370
571.940877	41431.757897	31.454388
572.299451	41502.684493	31.459405
573.416863	41559.019295	31.464423
573.863326	41632.588222	31.469440
574.432375	41702.520103	31.474458
575.153125	41766.062963	31.479476
575.893970	41835.583214	31.484493
576.721911	41894.753531	31.489511
577.083455	41966.142080	31.494528
578.001763	42023.592015	31.499546
578.594103	42081.103519	31.504564
578.775545	42146.364418	31.509581
579.679328	42215.964347	31.514599
580.480811	42270.197434	31.519616
580.913411	42338.267371	31.524634
581.668205	42386.707523	31.529652
582.693654	42430.647672	31.534669
583.956145	42466.084004	31.539687
584.137401	42522.996893	31.544704
585.152130	42564.071811	31.549722
585.863637	42610.229443	31.554740
585.938980	42660.942453	31.559757
586.395805	42707.771776	31.564775
586.485490	42755.274797	31.569792
587.280447	42810.201430	31.574810
587.906359	42864.451732	31.579828
587.649483	42933.299396	31.584845
588.453014	42989.445986	31.589863
589.161040	43051.402636	31.594880
589.878455	43108.399249	31.599898
590.591895	43162.781652	31.604916
591.008853	43230.532689	31.609933
591.312377	43294.207562	31.614951
592.042829	43354.931488	31.619968
592.909929	43427.781794	31.624986
593.235753	43491.015365	31.630004
593.573657	43558.789738	31.635021
594.146505	43615.082351	31.640039
594.323886	43689.005725	31.645056
595.023221	43757.392076	31.650074
595.745646	43825.989530	31.655092
596.197620	43909.242312	31.660109
596.745899	43975.615724	31.665127
597.372937	44057.251424	31.670144
597.773996	44132.459686	31.675162
598.331635	44204.419306	31.680180
598.864934	44283.007849	31.685197
599.854129	44337.640250	31.690215
600.284619	44410.870216	31.695232
600.732769	44479.570712	31.700250
601.406996	44546.541407	31.705268
601.709159	44631.461942	31.710285
602.354901	44700.851117	31.715303
602.758832	44776.055390	31.720320
603.401191	44849.344945	31.725338
604.177781	44938.444018	31.730356
604.667273	45017.383563	31.735373
605.440027	45088.845672	31.740391
606.063547	45174.029993	31.745408
606.438934	45252.370429	31.750426
607.565167	45319.268956	31.755444
607.806105	45405.600593	31.760461
608.383672	45476.458092	31.765479
609.351614	45549.824932	31.770496
610.566087	45622.610181	31.775514
611.092471	45688.299524	31.780532
611.491944	45761.044772	31.785549
612.668398	45813.049181	31.790567
613.889873	45882.685790	31.795584
614.017074	45930.809862	31.800602
615.122127	45987.915082	31.805620
615.648046	46055.574568	31.810637
616.512583	46107.866149	31.815655
617.065629	46143.694324	31.820672
617.872311	46196.594829	31.825690
618.602092	46251.167270	31.830708
618.682703	46303.820897	31.835725
619.527844	46351.569930	31.840743
620.144071	46410.249850	31.845760
620.494274	46464.451161	31.850778
621.042552	46515.557548	31.855796
621.528885	46577.161353	31.860813
622.036876	46646.091147	31.865831
622.413420	46704.232839	31.870848
622.843307	46779.738161	31.875866
623.349049	46853.319732	31.880884
623.819283	46923.275724	31.885901
624.752896	46988.939795	31.890919
625.159719	47065.440725	31.895936
625.401323	47139.090793	31.900954
626.514084	47212.460462	31.905972
627.091469	47293.611184	31.910989
627.874946	47361.392440	31.916007
628.384954	47439.658093	31.921024
628.840733	47517.342701	31.926042
629.656192	47585.469956	31.931060
630.340842	47664.683765	31.936077
630.526827	47734.931193	31.941095
631.127963	47815.326423	31.946112
631.439270	47893.928635	31.951130
632.398806	47966.104742	31.956148
632.378488	48043.864321	31.961165
633.062401	48122.367195	31.966183
633.849153	48201.302101	31.971200
634.307845	48288.193778	31.976218
635.186191	48366.079874	31.981236
635.450124	48455.956818	31.986253
636.261887	48526.047783	31.991271
636.887530	48608.263378	31.996288
637.047376	48702.077172	32.001306
638.247056	48779.781390	32.006324
638.584524	48876.830557	32.011341
639.324186	48954.911718	32.016359
640.447240	49048.700184	32.021376
640.729907	49131.827956	32.026394
641.641983	49195.118087	32.031412
641.943572	49293.431137	32.036429
642.797715	49368.548612	32.041447
643.656292	49457.954110	32.046464
644.176498	49544.962048	32.051482
645.214293	49619.770493	32.056500
645.982333	49700.621025	32.061517
646.309279	49790.179111	32.066535
647.281919	49856.267304	32.071552
647.927351	49939.470460	32.076570
648.663768	50008.351718	32.081588
649.318700	50103.113333	32.086605
650.185480	50169.661341	32.091623
650.868737	50245.608115	32.096640
651.270555	50326.128486	32.101658
652.056117	50397.165089	32.106676
653.038158	50484.902470	32.111693
653.518550	50555.092060	32.116711
654.226163	50623.194491	32.121728
654.507868	50705.364073	32.126746
655.064683	50775.274114	32.131764
655.429862	50854.505661	32.136781
656.367986	50935.322073	32.141799
657.155538	51012.659840	32.146816
657.541014	51100.062874	32.151834
658.470955	51172.919432	32.156852
658.973350	51268.484691	32.161869
659.422062	51347.178077	32.166887
660.453766	51428.941208	32.171904
660.971504	51514.245449	32.176922
661.914164	51591.343253	32.181940
662.347265	51668.999072	32.186957
663.251216	51761.523788	32.191975
663.817194	51831.202939	32.196992
664.192862	51921.764359	32.202010
665.351997	51992.738332	32.207028
665.896464	52072.786199	32.212045
666.156215	52159.851456	32.217063
666.815268	52236.163983	32.222080
667.653838	52319.082313	32.227098
668.615599	52385.232066	32.232116
669.300793	52460.875449	32.237133
670.013982	52529.937360	32.242151
670.629309	52601.492671	32.247168
671.160317	52678.496555	32.252186
671.462816	52740.965220	32.257204
672.143300	52825.006227	32.262221
673.011675	52903.592244	32.267239
674.135901	52968.897665	32.272256
674.779272	53049.268668	32.277274
675.348467	53117.244767	32.282292
675.896582	53196.160795	32.287309
676.247932	53271.737632	32.292327
677.182156	53347.588104	32.297344
677.562688	53430.849587	32.302362
678.571537	53506.701469	32.307380
678.994610	53588.527108	32.312397
679.626801	53669.199331	32.317415
680.286764	53748.570242	32.322432
680.339050	53835.575582	32.327450
681.421462	53932.211483	32.332468
681.880436	54022.056807	32.337485
682.424324	54096.302838	32.342503
683.265495	54194.597767	32.347520
684.173467	54278.798672	32.352538
685.217445	54352.786212	32.357556
686.133222	54450.515114	32.362573
686.853740	54518.507086	32.367591
687.654355	54601.069437	32.372608
688.047891	54696.190337	32.377626
688.543753	54770.961271	32.382644
689.393181	54856.193715	32.387661
689.763178	54929.530186	32.392679
691.013495	55014.087175	32.397696
691.568128	55104.863252	32.402714
691.887422	55186.453750	32.407732
692.621207	55273.322716	32.412749
693.270650	55363.182196	32.417767
694.105791	55458.372485	32.422784
694.454527	55549.735957	32.427802
695.460295	55641.591883	32.432820
696.366422	55727.491727	32.437837
696.427019	55820.461813	32.442855
697.633501	55906.043200	32.447872
698.104664	55999.763254	32.452890
698.957037	56092.375061	32.457908
699.810992	56187.544044	32.462925
699.993084	56272.532615	32.467943
701.089402	56357.634881	32.472960
701.868151	56458.025910	32.477978
702.567117	56550.165675	32.482996
703.149704	56640.689198	32.488013
703.481597	56735.372747	32.493031
704.463838	56814.175305	32.498048
705.149185	56910.290355	32.503066
705.939185	56989.967155	32.508084
706.905855	57065.821587	32.513101
707.368728	57144.354673	32.518119
707.936540	57227.641490	32.523136
708.450634	57323.732291	32.528154
709.064796	57401.064844	32.533172
709.945434	57492.372214	32.538189
710.833530	57582.277149	32.543207
711.799589	57656.025243	32.548224
711.920568	57742.188925	32.553242
712.594789	57833.600296	32.558260
713.609720	57918.599603	32.563277
714.320100	58017.652472	32.568295
715.488073	58098.817678	32.573312
715.703104	58188.324423	32.578330
716.787905	58260.193342	32.583348
718.030639	58338.736780	32.588365
718.167526	58437.270713	32.593383
719.381034	58502.644819	32.598400
719.897646	58585.112408	32.603418
720.707858	58678.189054	32.608436
721.496983	58763.054538	32.613453
721.996301	58844.547304	32.618471
722.299908	58930.264357	32.623488
723.006952	59026.418505	32.628506
723.728192	59104.776685	32.633524
724.366754	59191.609794	32.638541
724.825770	59291.542984	32.643559
725.779595	59391.413723	32.648576
726.522558	59494.359049	32.653594
727.358786	59587.022488	32.658612
728.331301	59677.145137	32.663629
729.204434	59768.913235	32.668647
729.520288	59862.680708	32.673664
729.964482	59959.765572	32.678682
730.475414	60060.799694	32.683700
731.607322	60149.873093	32.688717
731.705012	60263.329061	32.693735
732.552206	60371.570269	32.698752
733.349425	60469.015198	32.703770
733.890429	60575.806531	32.708788
735.010681	60675.174535	32.713805
736.150801	60779.064629	32.718823
736.660980	60872.010517	32.723840
737.414149	60992.357326	32.728858
738.318312	61083.568035	32.733876
739.471985	61173.770088	32.738893
740.190499	61274.335633	32.743911
741.152226	61357.473989	32.748928
742.253311	61441.480981	32.753946
742.694466	61522.849410	32.758964
743.735328	61606.026790	32.763981
744.577202	61680.429467	32.768999
745.930480	61747.671501	32.774016
746.899844	61822.398632	32.779034
747.389819	61891.016423	32.784052
748.451362	61953.426978	32.789069
748.775162	62011.752246	32.794087
749.415931	62070.721937	32.799104
750.245763	62141.174864	32.804122
750.730398	62199.361428	32.809140
751.165688	62272.356491	32.814157
751.639793	62367.519618	32.819175
752.362609	62441.281113	32.824192
753.113052	62517.694216	32.829210
753.332431	62610.625490	32.834228
754.482773	62681.979917	32.839245
754.695464	62783.192955	32.844263
755.374651	62871.779734	32.849280
756.235874	62956.548489	32.854298
756.740518	63064.815478	32.859316
757.296011	63160.332785	32.864333
758.174694	63260.084443	32.869351
758.832724	63351.086331	32.874368
759.272320	63464.586041	32.879386
760.077471	63563.883618	32.884404
761.127622	63675.866305	32.889421
761.928168	63779.688002	32.894439
762.359781	63889.847173	32.899456
763.051178	63985.346986	32.904474
764.030597	64109.956757	32.909492
764.657715	64206.424805	32.914509
765.432391	64327.225189	32.919527
766.511181	64428.034341	32.924544
767.323074	64547.484830	32.929562
767.763343	64658.161829	32.934580
769.127648	64752.358260	32.939597
770.192308	64848.042990	32.944615
771.186620	64938.430442	32.949632
772.412160	65018.514123	32.954650
773.689000	65111.150291	32.959668
774.612507	65196.958154	32.964685
775.100203	65292.699048	32.969703
775.922213	65367.233016	32.974720
776.452808	65449.298821	32.979738
777.157364	65535.496780	32.984756
777.914223	65618.500050	32.989773
778.685285	65715.849751	32.994791
779.170215	65813.952960	32.999808
779.773966	65910.708082	33.004826
780.037651	66002.751813	33.009844
781.147000	66099.500047	33.014861
781.497167	66205.194232	33.019879
782.509726	66306.409126	33.024896
783.145496	66405.375697	33.029914
783.802313	66516.976462	33.034932
785.076852	66615.753999	33.039949
785.898463	66711.401415	33.044967
786.566092	66816.536736	33.049984
787.436247	66920.882343	33.055002
787.923422	67008.839732	33.060020
789.062929	67095.866145	33.065037
789.178546	67201.445179	33.070055
790.126961	67289.886339	33.075072
791.097525	67384.970096	33.080090
791.438210	67497.040608	33.085108
792.236487	67591.009374	33.090125
793.096476	67702.783627	33.095143
793.756021	67802.915943	33.100160
794.485320	67910.523784	33.105178
794.967438	68018.556927	33.110196
795.806771	68125.794668	33.115213
796.736163	68236.335353	33.120231
797.435497	68348.562161	33.125248
798.283970	68457.436515	33.130266
798.877889	68585.936586	33.135284
799.776483	68706.694106	33.140301
800.580476	68806.928626	33.145319
801.375532	68928.133598	33.150336
802.229590	69039.720615	33.155354
803.077460	69152.035800	33.160372
804.167368	69264.957524	33.165389
804.858453	69384.804586	33.170407
805.528144	69490.693210	33.175424
806.844811	69606.998803	33.180442
807.099845	69728.332587	33.185460
807.836203	69845.780745	33.190477
808.725158	69964.551063	33.195495
809.610804	70082.779270	33.200512
811.187867	70184.325684	33.205530
811.821651	70292.107147	33.210548
812.846306	70399.504760	33.215565
813.509877	70518.446979	33.220583
814.844298	70617.260545	33.225600
816.687476	70702.232385	33.230618
817.058794	70794.610150	33.235636
817.990748	70887.297172	33.240653
818.995590	70974.697181	33.245671
819.534130	71072.237021	33.250688
820.625565	71166.372162	33.255706
821.159051	71257.974389	33.260724
822.233731	71350.305991	33.265741
822.547642	71452.382231	33.270759
823.234923	71547.853538	33.275776
824.092960	71646.229957	33.280794
824.252645	71755.623964	33.285812
825.049902	71858.895414	33.290829
825.934658	71971.852676	33.295847
826.367794	72086.891816	33.300864
827.421818	72195.747828	33.305882
828.031583	72311.606873	33.310900
828.647946	72426.132266	33.315917
829.508241	72544.650941	33.320935
830.109400	72676.658227	33.325952
830.945506	72783.599592	33.330970
831.657904	72899.850137	33.335988
832.443588	73014.547853	33.341005
833.028839	73131.098019	33.346023
834.008556	73242.530802	33.351040
835.190072	73353.161157	33.356058
835.981194	73472.644225	33.361076
836.975707	73580.253439	33.366093
837.787658	73700.360154	33.371111
838.495110	73820.458944	33.376128
839.384935	73918.468689	33.381146
840.377498	74038.972085	33.386164
840.991029	74155.416285	33.391181
841.809033	74273.819238	33.396199
842.535522	74404.699440	33.401216
843.508968	74522.042725	33.406234
843.958191	74654.257856	33.411252
844.755567	74765.595417	33.416269
845.456066	74896.293365	33.421287
846.229973	75035.164442	33.426304
847.533127	75157.154469	33.431322
848.041412	75301.359244	33.436340
849.170704	75425.754791	33.441357
850.371487	75551.959837	33.446375
850.609215	75686.699081	33.451392
851.781479	75812.215105	33.456410
852.669641	75951.870608	33.461428
853.756141	76070.026498	33.466445
854.586941	76193.305071	33.471463
855.288774	76335.065836	33.476480
855.964466	76469.424577	33.481498
857.071153	76599.108225	33.486516
858.106855	76718.198717	33.491533
858.864457	76849.115070	33.496551
859.529281	76982.650981	33.501568
860.514546	77100.860581	33.506586
861.384469	77239.794684	33.511604
862.676036	77364.125731	33.516621
863.708367	77493.346560	33.521639
864.678366	77612.465378	33.526656
865.748257	77734.299452	33.531674
866.535208	77849.902982	33.536692
867.292946	77978.841912	33.541709
868.093468	78108.545961	33.546727
869.099285	78228.515952	33.551744
870.009869	78351.105926	33.556762
870.751119	78477.838377	33.561780
871.527617	78598.194663	33.566797
872.376591	78711.454498	33.571815
872.871009	78849.624937	33.576832
873.852514	78981.126103	33.581850
874.857133	79108.553755	33.586868
875.688214	79232.874612	33.591885
876.852019	79345.594803	33.596903
877.480728	79483.893509	33.601920
878.592686	79600.327474	33.606938
879.321657	79719.142891	33.611956
880.157266	79834.794090	33.616973
881.397315	79952.100939	33.621991
881.983992	80055.738490	33.627008
882.957606	80166.514890	33.632026
883.686508	80277.431964	33.637044
884.585302	80401.970328	33.642061
885.452464	80510.091586	33.647079
886.175536	80640.386493	33.652096
887.166857	80763.989383	33.657114
887.712826	80877.372527	33.662132
888.640624	81011.227775	33.667149
889.299970	81141.573893	33.672167
889.578446	81274.750289	33.677184
890.812247	81403.527383	33.682202
891.653489	81536.141775	33.687220
892.617053	81681.450502	33.692237
893.870264	81806.237998	33.697255
894.479596	81952.382552	33.702272
895.746883	82080.007930	33.707290
896.465508	82210.951868	33.712308
897.449909	82338.364639	33.717325
899.000765	82469.582370	33.722343
899.614062	82608.523854	33.727360
900.498163	82740.658594	33.732378
901.842876	82865.557968	33.737396
902.539516	82998.925355	33.742413
903.526916	83110.113495	33.747431
904.005460	83242.846986	33.752448
905.446969	83371.533598	33.757466
906.298743	83502.584527	33.762484
906.822883	83632.474523	33.767501
908.208369	83761.924789	33.772519
908.789223	83900.589138	33.777536
909.850548	84020.533139	33.782554
910.736298	84150.286589	33.787572
911.500878	84285.396300	33.792589
912.400087	84415.819422	33.797607
913.382831	84556.466299	33.802624
914.470540	84679.204414	33.807642
915.350337	84819.888388	33.812660
915.904817	84944.103865	33.817677
917.183639	85086.161362	33.822695
917.877868	85225.183055	33.827712
918.763919	85358.288596	33.832730
919.943171	85483.520628	33.837748
921.009100	85622.017879	33.842765
921.958493	85751.410586	33.847783
923.029727	85883.136835	33.852800
924.164459	85997.895497	33.857818
925.086927	86122.318536	33.862836
925.969197	86243.903312	33.867853
927.360690	86347.873780	33.872871
928.141408	86485.315470	33.877888
929.325761	86596.149102	33.882906
930.000688	86711.294591	33.887924
930.817209	86816.180838	33.892941
931.795434	86919.960589	33.897959
932.601206	87042.390419	33.902976
933.581595	87147.245887	33.907994
934.449016	87249.331236	33.913012
935.075750	87366.972994	33.918029
936.167317	87485.401425	33.923047
936.548336	87605.790015	33.928064
937.267199	87736.761670	33.933082
938.286738	87836.833696	33.938100
939.241678	87983.413736	33.943117
940.289115	88105.621454	33.948135
941.228875	88236.845561	33.953152
942.111086	88354.989571	33.958170
942.945708	88493.244939	33.963188
943.565993	88628.158396	33.968205
944.890889	88749.762794	33.973223
945.550887	88904.382973	33.978240
946.366522	89031.824686	33.983258
947.831865	89160.453858	33.988276
948.552776	89305.764706	33.993293
949.662634	89435.052840	33.998311
950.573086	89573.031089	34.003328
951.827507	89698.142887	34.008346
952.464986	89845.462698	34.013364
953.090499	89983.678604	34.018381
954.057697	90134.160581	34.023399
954.788518	90274.423264	34.028416
955.681294	90418.816140	34.033434
956.737323	90567.231570	34.038452
957.715384	90722.971393	34.043469
958.729413	90869.422345	34.048487
959.799016	91013.411542	34.053504
960.603289	91152.649922	34.058522
961.679638	91303.160510	34.063540
962.336836	91467.747787	34.068557
963.559674	91612.418559	34.073575
964.397201	91768.181823	34.078592
965.557783	91919.290392	34.083610
967.087559	92046.003568	34.088628
967.808434	92205.178549	34.093645
968.451867	92353.526203	34.098663
969.465582	92508.026985	34.103680
970.433485	92652.694535	34.108698
971.477041	92799.159937	34.113716
972.584647	92950.144830	34.118733
973.713506	93096.807352	34.123751
974.689249	93255.038517	34.128768
975.381680	93394.226585	34.133786
976.711055	93536.824670	34.138804
977.267875	93701.925234	34.143821
978.544632	93841.301446	34.148839
979.601725	93998.329475	34.153856
980.149529	94148.007333	34.158874
981.349135	94278.618956	34.163892
982.347277	94419.112094	34.168909
983.699547	94546.335864	34.173927
984.743796	94683.262086	34.178944
985.542849	94814.573113	34.183962
986.957181	94943.187213	34.188980
987.666950	95079.751579	34.193997
988.573545	95211.642430	34.199015
989.645422	95348.884603	34.204032
990.290301	95487.182357	34.209050
991.365471	95623.793109	34.214068
992.071543	95769.098143	34.219085
992.769442	95909.452268	34.224103
994.163262	96055.029286	34.229120
995.147021	96197.661331	34.234138
996.434956	96337.114531	34.239156
996.971384	96488.675939	34.244173
998.134638	96630.649560	34.249191
999.180133	96785.699867	34.254208
1000.195682	96927.300299	34.259226
1001.269081	97082.835311	34.264244
1002.018845	97232.640703	34.269261
1003.163171	97377.354936	34.274279
1004.110319	97521.690247	34.279296
1004.677792	97680.776643	34.284314
1006.045927	97830.177606	34.289332
1007.257388	97994.009757	34.294349
1008.268802	98134.549191	34.299367
1009.460111	98284.974517	34.304384
1010.150468	98445.590361	34.309402
1010.743747	98604.647449	34.314420
1011.906485	98761.856246	34.319437
1013.046728	98921.575068	34.324455
1014.084538	99089.093180	34.329472
1014.922506	99262.718014	34.334490
1016.081713	99411.093302	34.339508
1017.213002	99573.291865	34.344525
1018.331012	99737.043776	34.349543
1019.581947	99884.622985	34.354560
1020.025540	100048.794409	34.359578
1021.189828	100200.078059	34.364596
1022.131995	100373.865509	34.369613
1023.166843	100536.086174	34.374631
1024.309099	100702.833802	34.379648
1025.351651	100863.321884	34.384666
1026.696501	101024.205899	34.389684
1027.682511	101192.342259	34.394701
1028.696635	101353.825311	34.399719
1029.865050	101499.605654	34.404736
1030.646558	101665.411514	34.409754
1031.768086	101825.887344	34.414772
1032.764971	101996.818197	34.419789
1033.647487	102154.575502	34.424807
1034.706150	102326.093726	34.429824
1035.699079	102475.179449	34.434842
1036.891404	102618.912811	34.439860
1038.017861	102773.870281	34.444877
1039.053246	102915.668826	34.449895
1040.419235	103064.585055	34.454912
1040.986140	103210.572977	34.459930
1042.687363	103347.851377	34.464948
1043.287961	103496.708577	34.469965
1043.931217	103646.610374	34.474983
1045.484118	103795.552120	34.480000
1045.935483	103967.944603	34.485018
1047.352767	104110.512240	34.490036
1047.732755	104268.388960	34.495053
1048.689811	104431.104595	34.500071
1049.962115	104597.599780	34.505088
1051.016526	104769.592090	34.510106
1052.509062	104909.760479	34.515124
1053.801321	105073.964983	34.520141
1054.970593	105225.640975	34.525159
1055.946998	105365.944776	34.530176
1056.697398	105540.123689	34.535194
1058.009897	105694.178374	34.540212
1059.263206	105861.103101	34.545229
1060.572767	106004.781418	34.550247
1061.629168	106152.835981	34.555264
1062.441638	106313.581287	34.560282
1063.825465	106474.913968	34.565300
1064.786262	106624.727050	34.570317
1065.288462	106785.290699	34.575335
1066.771832	106930.320268	34.580352
1067.542345	107109.456537	34.585370
1068.663345	107268.792117	34.590388
1069.295954	107436.288528	34.595405
1070.486903	107601.830236	34.600423
1071.407390	107766.327496	34.605440
1072.336198	107951.071365	34.610458
1073.420007	108115.393121	34.615476
1074.888658	108283.496605	34.620493
1075.681285	108463.297617	34.625511
1077.406659	108624.837186	34.630528
1078.300102	108797.548494	34.635546
1079.450223	108961.257811	34.640564
1080.835786	109123.981369	34.645581
1081.520394	109295.843304	34.650599
1083.323904	109452.533902	34.655616
1084.482910	109612.771282	34.660634
1085.996525	109768.731481	34.665652
1086.852235	109912.568484	34.670669
1087.622415	110084.365380	34.675687
1089.089168	110233.297406	34.680704
1089.559887	110396.491412	34.685722
1090.391412	110550.362313	34.690740
1091.478955	110721.676433	34.695757
1092.441602	110883.909256	34.700775
1093.929521	111051.686898	34.705792
1094.711501	111228.610800	34.710810
1095.790296	111375.433930	34.715828
1097.160498	111528.870782	34.720845
1098.118342	111684.197228	34.725863
1099.205995	111838.098717	34.730880
1099.979388	111993.380472	34.735898
1100.954288	112153.271182	34.740916
1101.762164	112321.406127	34.745933
1102.556705	112486.822309	34.750951
1103.908903	112648.441335	34.755968
1104.793344	112818.991973	34.760986
1106.423249	112990.684972	34.766004
1107.588125	113159.731016	34.771021
1108.301064	113332.312853	34.776039
1109.545445	113498.702397	34.781056
1110.437917	113678.848380	34.786074
1111.540846	113855.030868	34.791092
1112.661377	114038.036253	34.796109
1113.787169	114220.523014	34.801127
1115.093344	114382.021271	34.806144
1115.885057	114574.800561	34.811162
1117.006696	114762.388202	34.816180
1118.207225	114931.510130	34.821197
1119.461984	115131.310627	34.826215
1120.708592	115299.465383	34.831232
1122.394789	115469.887497	34.836250
1123.930512	115640.195403	34.841268
1125.022449	115809.669677	34.846285
1125.974993	115977.717413	34.851303
1127.425642	116149.283165	34.856320
1128.439912	116326.750540	34.861338
1129.673334	116488.368755	34.866356
1130.818473	116662.253140	34.871373
1131.693513	116828.767631	34.876391
1132.903164	117006.613863	34.881408
1133.693427	117180.703825	34.886426
1134.893823	117367.645998	34.891444
1136.017720	117534.733321	34.896461
1136.936403	117724.464444	34.901479
1138.187757	117902.449541	34.906496
1139.207926	118090.964213	34.911514
1140.231350	118270.222770	34.916532
1141.321331	118451.574131	34.921549
1142.412765	118654.923242	34.926567
1143.543910	118835.941495	34.931584
1144.675661	119020.399138	34.936602
1145.662720	119207.705148	34.941620
1146.951763	119391.975786	34.946637
1148.104294	119589.642701	34.951655
1149.631203	119769.471087	34.956672
1150.546676	119972.294923	34.961690
1151.664498	120143.237300	34.966708
1153.235477	120325.810672	34.971725
1155.007534	120496.436029	34.976743
1156.450410	120674.118369	34.981760
1158.047689	120832.438385	34.986778
1159.209964	120977.682512	34.991796
1161.106568	121104.218724	34.996813
1161.933105	121249.695048	35.001831
1163.370692	121384.664423	35.006848
1164.617659	121522.590419	35.011866
1165.372051	121667.029321	35.016884
1166.751017	121796.614803	35.021901
1167.404996	121946.859172	35.026919
1168.509732	122090.117474	35.031936
1169.134574	122237.391782	35.036954
1170.406716	122383.158119	35.041972
1171.238745	122545.840351	35.046989
1171.736244	122704.992412	35.052007
1173.019965	122871.708462	35.057024
1174.110241	123046.258409	35.062042
1175.272130	123227.055029	35.067060
1176.487985	123403.626545	35.072077
1177.208922	123585.850958	35.077095
1177.979714	123770.069925	35.082112
1179.349343	123957.437480	35.087130
1180.555613	124155.421312	35.092148
1181.591172	124346.619248	35.097165
1182.771961	124531.766224	35.102183
1183.890244	124727.285634	35.107200
1184.696589	124927.175377	35.112218
1185.938160	125127.580068	35.117236
1187.493376	125326.657025	35.122253
1188.240134	125532.514118	35.127271
1189.227115	125737.257881	35.132288
1190.775040	125947.449522	35.137306
1192.026722	126149.380208	35.142324
1193.562620	126351.178531	35.147341
1194.878220	126550.593906	35.152359
1196.880809	126740.071550	35.157376
1198.142173	126934.874728	35.162394
1199.233131	127126.121442	35.167412
1201.124857	127302.547602	35.172429
1201.826289	127494.099500	35.177447
1203.223007	127674.964487	35.182464
1204.168517	127863.338511	35.187482
1205.325693	128056.696726	35.192500
1206.478409	128248.144113	35.197517
1207.309767	128439.542574	35.202535
1208.984061	128624.879557	35.207552
1210.387749	128817.646496	35.212570
1211.360685	129019.148524	35.217588
1212.803194	129205.869107	35.222605
1213.817048	129409.926520	35.227623
1214.906072	129597.504059	35.232640
1216.137016	129792.167530	35.237658
1217.165887	129984.064646	35.242676
1218.440493	130182.714617	35.247693
1219.568280	130384.214557	35.252711
1220.837575	130572.960878	35.257728
1222.059961	130767.657831	35.262746
1223.048495	130963.052119	35.267764
1224.077059	131146.202681	35.272781
1225.130242	131336.736873	35.277799
1226.225282	131527.772482	35.282816
1227.562550	131722.837858	35.287834
1228.708951	131921.710530	35.292852
1229.829237	132118.599573	35.297869
1231.069479	132318.030252	35.302887
1232.129905	132521.887438	35.307904
1233.188652	132723.959856	35.312922
1234.286773	132932.780701	35.317940
1235.804048	133138.812308	35.322957
1236.724027	133358.219000	35.327975
1237.974125	133561.445272	35.332992
1239.290043	133787.824464	35.338010
1240.599094	133996.708229	35.343028
1242.067571	134203.578844	35.348045
1243.109261	134424.811603	35.353063
1244.346273	134631.836127	35.358080
1246.075202	134849.985199	35.363098
1247.271246	135067.004195	35.368116
1249.057042	135264.214512	35.373133
1250.422947	135474.620480	35.378151
1251.289815	135683.460012	35.383168
1253.133609	135900.863780	35.388186
1254.277624	136096.293701	35.393204
1255.789281	136304.401593	35.398221
1256.682077	136514.978982	35.403239
1257.959783	136708.351573	35.408256
1259.545917	136909.190911	35.413274
1260.270143	137118.912389	35.418292
1261.771214	137327.041893	35.423309
1262.871049	137548.580566	35.428327
1264.073822	137755.049752	35.433344
1265.820560	137964.652714	35.438362
1267.060355	138177.138382	35.443380
1268.393804	138381.183376	35.448397
1269.417079	138584.759497	35.453415
1270.811031	138799.582241	35.458432
1272.302523	139005.672067	35.463450
1273.301999	139216.188367	35.468468
1274.643199	139421.633287	35.473485
1276.131511	139623.304973	35.478503
1277.320452	139849.079453	35.483520
1278.687414	140057.148000	35.488538
1279.705420	140269.468366	35.493556
1281.608886	140475.338058	35.498573
1282.697793	140675.242630	35.503591
1283.960520	140879.949573	35.508608
1285.448592	141082.163367	35.513626
1286.624551	141289.890561	35.518644
1287.794275	141496.530207	35.523661
1289.198087	141700.472500	35.528679
1290.976672	141894.660883	35.533696
1292.275226	142086.810216	35.538714
1293.530763	142279.601311	35.543732
1295.225406	142453.324964	35.548749
1296.138994	142635.361434	35.553767
1297.054998	142817.474648	35.558784
1298.610252	142988.916735	35.563802
1299.786213	143188.773260	35.568820
1300.932653	143368.191430	35.573837
1302.140381	143568.995977	35.578855
1303.110762	143755.085983	35.583872
1304.604072	143955.936375	35.588890
1305.631479	144156.228373	35.593908
1307.067886	144346.494000	35.598925
1308.056299	144546.300382	35.603943
1309.449829	144745.080333	35.608960
1310.921029	144934.228600	35.613978
1312.204665	145153.664129	35.618996
1313.583581	145345.478727	35.624013
1314.962466	145552.264407	35.629031
1316.650164	145757.455932	35.634048
1318.067017	145952.716007	35.639066
1319.036054	146159.672237	35.644084
1320.165237	146361.179067	35.649101
1321.433429	146574.986187	35.654119
1322.475585	146791.657453	35.659136
1324.149980	146983.016755	35.664154
1325.015410	147214.157185	35.669172
1326.217964	147440.568130	35.674189
1327.842528	147651.625798	35.679207
1329.318282	147862.784575	35.684224
1330.544192	148078.091686	35.689242
1331.826843	148303.076238	35.694260
1333.562792	148506.934156	35.699277
1334.946814	148729.889980	35.704295
1335.827279	148959.494057	35.709312
1337.861272	149169.520527	35.714330
1338.500423	149396.541916	35.719348
1340.332029	149605.893472	35.724365
1341.751706	149824.008489	35.729383
1342.733894	150051.715233	35.734400
1344.227910	150270.886339	35.739418
1345.056131	150503.995973	35.744436
1346.877124	150719.023269	35.749453
1348.507611	150935.819110	35.754471
1349.695302	151165.871707	35.759488
1351.733435	151377.433129	35.764506
1352.739868	151590.896769	35.769524
1354.101542	151810.175286	35.774541
1355.627028	152022.253386	35.779559
1356.853726	152240.516606	35.784576
1358.110733	152454.491173	35.789594
1359.501231	152674.911897	35.794612
1360.905600	152891.731186	35.799629
1362.396045	153106.103923	35.804647
1363.357576	153328.739833	35.809664
1364.780665	153534.656683	35.814682
1366.198690	153755.105537	35.819700
1367.598905	153949.148518	35.824717
1368.672867	154145.602759	35.829735
1369.985888	154356.271407	35.834752
1371.373131	154573.142352	35.839770
1372.641088	154785.050718	35.844788
1373.778419	154984.327242	35.849805
1375.176174	155190.308973	35.854823
1376.121880	155427.149489	35.859840
1377.775193	155644.137167	35.864858
1379.054845	155873.218564	35.869876
1380.549676	156091.235966	35.874893
1381.505374	156319.217985	35.879911
1382.840980	156554.279915	35.884928
1384.272307	156784.725420	35.889946
1385.669240	157018.855147	35.894964
1386.844822	157254.796860	35.899981
1388.529758	157489.327820	35.904999
1389.643708	157731.102799	35.910016
1391.267976	157970.021362	35.915034
1392.527374	158206.412736	35.920052
1393.597389	158463.872867	35.925069
1395.288777	158705.550181	35.930087
1396.739363	158944.946856	35.935104
1398.077409	159193.353761	35.940122
1399.380404	159440.842288	35.945140
1400.948734	159689.545812	35.950157
1402.600835	159940.583783	35.955175
1403.606647	160187.985288	35.960192
1405.293711	160433.948732	35.965210
1406.746313	160689.119767	35.970228
1408.288589	160945.762116	35.975245
1409.937049	161181.972148	35.980263
1411.112981	161433.920644	35.985280
1412.949920	161679.754741	35.990298
1413.981915	161941.684830	35.995316
1415.498285	162173.103300	36.000333
1416.975074	162421.650217	36.005351
1418.308763	162688.826183	36.010368
1420.034247	162933.443706	36.015386
1421.644659	163172.247331	36.020404
1422.901884	163419.897501	36.025421
1424.776674	163661.477806	36.030439
1425.737552	163912.640709	36.035456
1427.792814	164149.300120	36.040474
1429.350707	164396.376463	36.045492
1430.901069	164629.415859	36.050509
1432.712986	164855.211325	36.055527
1433.803667	165091.890560	36.060544
1435.288837	165322.496892	36.065562
1436.698682	165564.100163	36.070580
1438.019183	165801.888890	36.075597
1439.452082	166032.228905	36.080615
1440.770101	166269.475632	36.085632
1442.044258	166509.812896	36.090650
1443.290031	166736.622951	36.095668
1444.858049	166966.807731	36.100685
1446.207891	167177.686069	36.105703
1447.477358	167407.819512	36.110720
1448.812267	167638.882557	36.115738
1450.307222	167867.384815	36.120756
1451.456820	168109.527803	36.125773
1452.553749	168349.448316	36.130791
1453.813888	168588.228207	36.135808
1455.206849	168834.002829	36.140826
1456.709878	169073.394049	36.145844
1458.126501	169331.230819	36.150861
1459.746663	169577.189735	36.155879
1461.616434	169820.421449	36.160896
1463.621679	170053.612362	36.165914
1465.467007	170292.322539	36.170932
1466.914117	170529.613342	36.175949
1468.613012	170749.703056	36.180967
1469.856452	170994.779461	36.185984
1471.623091	171228.535410	36.191002
1472.719247	171459.976439	36.196020
1474.015025	171707.256179	36.201037
1475.787049	171938.541904	36.206055
1477.056070	172183.520180	36.211072
1478.495754	172423.576320	36.216090
1480.140226	172665.453448	36.221108
1481.469538	172912.405573	36.226125
1482.695741	173155.836336	36.231143
1484.086026	173422.977362	36.236160
1485.515625	173656.687024	36.241178
1487.149808	173919.276491	36.246196
1488.408062	174178.895468	36.251213
1489.582629	174435.395977	36.256231
1490.928505	174707.779205	36.261248
1492.664679	174973.873362	36.266266
1494.150983	175236.850088	36.271284
1495.388632	175501.694842	36.276301
1497.389843	175755.535089	36.281319
1499.075509	176010.632253	36.286336
1500.555324	176273.616672	36.291354
1502.450203	176528.899485	36.296372
1503.548478	176789.296302	36.301389
1505.462776	177040.722435	36.306407
1506.740704	177309.391127	36.311424
1508.374474	177564.975539	36.316442
1510.083031	177812.988176	36.321460
1511.617166	178069.746021	36.326477
1513.502641	178327.731027	36.331495
1515.145857	178586.555397	36.336512
1516.398947	178835.813654	36.341530
1518.233940	179093.291183	36.346548
1519.493379	179348.527213	36.351565
1521.182292	179578.664025	36.356583
1522.564538	179840.036948	36.361600
1524.105528	180081.060570	36.366618
1525.545060	180312.281339	36.371636
1526.896951	180558.780732	36.376653
1528.576764	180777.366819	36.381671
1529.977680	181016.806574	36.386688
1531.713575	181247.503138	36.391706
1533.382999	181471.981634	36.396724
1534.721445	181711.625468	36.401741
1536.542543	181936.475599	36.406759
1538.047380	182180.929795	36.411776
1539.265311	182402.985204	36.416794
1540.974171	182625.090635	36.421812
1542.304909	182869.703204	36.426829
1543.920422	183112.026015	36.431847
1545.053840	183344.047426	36.436864
1546.887284	183584.637926	36.441882
1548.738426	183825.201539	36.446900
1549.807429	184083.363228	36.451917
1551.204827	184331.005883	36.456935
1553.030216	184565.905625	36.461952
1554.314713	184830.407250	36.466970
1556.172428	185078.602666	36.471988
1558.146384	185320.537896	36.477005
1559.722720	185563.451203	36.482023
1560.692273	185825.648461	36.487040
1562.255531	186078.476963	36.492058
1563.995930	186325.454256	36.497076
1565.082286	186596.735729	36.502093
1566.636881	186865.266915	36.507111
1568.227352	187126.129389	36.512128
1569.839919	187389.629294	36.517146
1571.669824	187654.821991	36.522164
1573.108757	187933.872233	36.527181
1574.780546	188199.816467	36.532199
1576.104069	188467.149982	36.537216
1577.950899	188739.820584	36.542234
1580.106072	188990.185175	36.547252
1581.329286	189265.876610	36.552269
1582.807935	189524.752440	36.557287
1584.559814	189793.992418	36.562304
1586.102892	190066.058984	36.567322
1587.877224	190321.262691	36.572340
1589.525155	190596.297889	36.577357
1591.128312	190858.321115	36.582375
1592.489883	191126.780276	36.587392
1593.709635	191399.210294	36.592410
1595.314542	191664.270703	36.597428
1596.760571	191945.462631	36.602445
1598.895390	192211.622103	36.607463
1600.565948	192478.745132	36.612480
1602.142433	192757.141629	36.617498
1603.798575	193023.153067	36.622516
1605.619995	193296.399117	36.627533
1607.120083	193561.219851	36.632551
1608.875618	193825.468378	36.637568
1610.383270	194082.625030	36.642586
1612.240712	194344.385256	36.647604
1613.532874	194593.303824	36.652621
1615.053096	194823.416358	36.657639
1616.826511	195074.443831	36.662656
1618.487336	195321.847868	36.667674
1620.002418	195562.955688	36.672692
1621.495664	195822.864893	36.677709
1622.874089	196065.710191	36.682727
1624.785750	196324.032434	36.687744
1625.928643	196582.122678	36.692762
1627.851231	196835.787722	36.697780
1628.935178	197106.061751	36.702797
1630.428643	197367.057506	36.707815
1632.106592	197637.354174	36.712832
1633.632792	197911.052524	36.717850
1635.702633	198183.917099	36.722868
1637.191648	198452.407527	36.727885
1639.028100	198720.463355	36.732903
1640.816553	198993.440236	36.737920
1642.438919	199266.635276	36.742938
1644.073347	199522.212116	36.747956
1645.602707	199809.412197	36.752973
1647.427276	200076.372393	36.757991
1649.273741	200344.434718	36.763008
1650.693673	200636.936854	36.768026
1652.198730	200905.690804	36.773044
1653.925405	201191.648285	36.778061
1655.531970	201476.610857	36.783079
1657.340966	201749.344428	36.788096
1658.993404	202045.180848	36.793114
1660.860758	202314.861500	36.798132
1662.431832	202600.203568	36.803149
1664.246953	202874.401416	36.808167
1666.384047	203150.136178	36.813184
1667.786103	203435.179270	36.818202
1669.531924	203702.435961	36.823220
1671.319001	203985.046924	36.828237
1673.151909	204262.384023	36.833255
1674.818891	204539.634561	36.838272
1676.633032	204805.641527	36.843290
1678.446692	205078.644240	36.848308
1680.199424	205344.384153	36.853325
1681.357640	205635.519260	36.858343
1683.302652	205910.104471	36.863360
1684.635630	206189.916660	36.868378
1686.891064	206462.487526	36.873396
1688.306031	206743.292165	36.878413
1690.340419	207018.376098	36.883431
1692.074719	207288.024887	36.888448
1693.554529	207569.064298	36.893466
1695.723680	207825.037797	36.898484
1697.340759	208103.658599	36.903501
1698.951969	208368.164987	36.908519
1700.921717	208638.087074	36.913536
1702.473455	208901.856215	36.918554
1704.306483	209143.619533	36.923572
1705.831205	209388.606504	36.928589
1707.504826	209634.078602	36.933607
1709.462055	209887.060229	36.938624
1711.033022	210119.373010	36.943642
1713.225748	210353.174832	36.948660
1714.955669	210585.743395	36.953677
1715.974590	210834.371002	36.958695
1718.166485	211074.548671	36.963712
1720.043599	211319.004793	36.968730
1721.598133	211564.592181	36.973748
1723.201664	211806.351385	36.978765
1724.770062	212060.266711	36.983783
1726.631589	212296.730834	36.988800
1728.274549	212554.838501	36.993818
1729.830744	212806.790859	36.998836
1731.214453	213062.872296	37.003853
1732.965639	213331.503307	37.008871
1734.721470	213584.417222	37.013888
1736.130410	213864.023157	37.018906
1737.597406	214132.308960	37.023924
1739.168119	214423.495648	37.028941
1740.869340	214699.491093	37.033959
1742.920929	214975.393952	37.038976
1744.208975	215261.411031	37.043994
1745.762474	215554.522436	37.049012
1747.460943	215841.682923	37.054029
1748.977244	216138.268804	37.059047
1750.930568	216443.039217	37.064064
1752.591291	216743.274008	37.069082
1754.419717	217041.756742	37.074100
1756.084551	217342.691755	37.079117
1757.636439	217643.468227	37.084135
1759.795165	217950.612226	37.089152
1761.745478	218252.115210	37.094170
1763.590007	218561.305093	37.099188
1765.616669	218860.614664	37.104205
1767.552658	219173.373143	37.109223
1769.661503	219456.051930	37.114240
1771.667156	219746.848850	37.119258
1773.580236	220034.652423	37.124276
1775.484169	220328.883278	37.129293
1777.181906	220617.802546	37.134311
1779.117112	220946.363857	37.139328
1781.067248	221233.036117	37.144346
1782.870538	221519.796261	37.149364
1784.892053	221801.850233	37.154381
1786.883089	222085.268701	37.159399
1788.756958	222362.434297	37.164416
1790.632225	222631.918712	37.169434
1792.382604	222903.099954	37.174452
1794.405183	223179.419521	37.179469
1796.302036	223443.125930	37.184487
1798.125633	223700.089718	37.189504
1799.968913	223960.924000	37.194522
1801.620081	224204.393785	37.199540
1803.729111	224440.325364	37.204557
1805.337138	224679.435419	37.209575
1807.191100	224921.135588	37.214592
1808.995385	225161.485692	37.219610
1810.834715	225401.754753	37.224628
1812.418411	225639.855659	37.229645
1813.825167	225884.308920	37.234663
1815.827371	226129.087419	37.239680
1817.503489	226383.695882	37.244698
1819.069232	226633.548164	37.249716
1820.939823	226891.504985	37.254733
1822.612422	227157.163701	37.259751
1824.318120	227410.729318	37.264768
1825.973006	227683.351090	37.269786
1827.310134	227956.252731	37.274804
1829.383056	228230.105098	37.279821
1830.915672	228512.932931	37.284839
1832.840989	228784.245400	37.289856
1834.569504	229073.901073	37.294874
1836.236495	229360.189665	37.299892
1838.610311	229640.297098	37.304909
1840.150150	229931.687103	37.309927
1841.955387	230219.962864	37.314944
1843.993444	230507.745435	37.319962
1845.829392	230784.487752	37.324980
1847.798249	231080.588031	37.329997
1849.634977	231378.056295	37.335015
1851.514097	231664.953387	37.340032
1853.355966	231951.603291	37.345050
1855.596521	232251.448401	37.350068
1857.857703	232526.960082	37.355085
1859.747611	232817.033671	37.360103
1861.481760	233102.485028	37.365120
1863.317100	233395.515173	37.370138
1864.899446	233681.601871	37.375156
1866.798798	233961.899097	37.380173
1868.639967	234257.445300	37.385191
1870.503313	234552.480890	37.390208
1872.382471	234853.534258	37.395226
1873.904823	235155.254710	37.400244
1875.843071	235453.532039	37.405261
1877.626092	235761.943521	37.410279
1879.274610	236067.786599	37.415296
1881.110472	236378.528200	37.420314
1883.225081	236677.289019	37.425332
1885.156923	236979.889522	37.430349
1886.997912	237294.849209	37.435367
1889.135294	237597.926812	37.440384
1891.032143	237903.176959	37.445402
1892.885372	238208.460278	37.450420
1895.008299	238507.402616	37.455437
1897.319380	238816.932822	37.460455
1899.125855	239108.383382	37.465472
1901.038510	239406.142309	37.470490
1903.068659	239672.489536	37.475508
1905.027507	239941.515652	37.480525
1906.764700	240217.740270	37.485543
1908.722163	240493.320991	37.490560
1910.516890	240766.032607	37.495578
1912.230055	241030.756847	37.500596
1914.290989	241298.144270	37.505613
1916.180805	241589.079787	37.510631
1917.663180	241867.406055	37.515648
1919.658654	242149.283737	37.520666
1921.685905	242436.084641	37.525684
1924.065802	242710.104755	37.530701
1925.387236	243002.251394	37.535719
1927.390439	243283.215989	37.540736
1929.232700	243583.511001	37.545754
1930.614149	243886.496074	37.550772
1932.933693	244174.245112	37.555789
1934.741203	244483.031457	37.560807
1936.881204	244780.919709	37.565824
1938.751053	245079.562707	37.570842
1940.367936	245395.950781	37.575860
1942.167973	245692.523338	37.580877
1943.830490	246020.945554	37.585895
1946.136954	246334.508455	37.590912
1948.355744	246638.103402	37.595930
1950.191668	246954.104615	37.600948
1952.404604	247276.041334	37.605965
1954.287064	247584.644830	37.610983
1956.247888	247908.705822	37.616000
1958.255259	248229.051554	37.621018
1960.222447	248535.459057	37.626036
1962.733648	248847.521541	37.631053
1964.295320	249172.562993	37.636071
1966.359344	249489.015940	37.641088
1968.554065	249802.807026	37.646106
1970.058169	250133.447886	37.651124
1972.608494	250443.322760	37.656141
1974.512791	250758.635051	37.661159
1976.689142	251069.281672	37.666176
1978.860281	251386.635731	37.671194
1980.821580	251706.843262	37.676212
1982.989009	252014.952831	37.681229
1984.851732	252327.353386	37.686247
1986.981283	252629.932434	37.691264
1989.381037	252942.553669	37.696282
1991.016952	253259.868977	37.701300
1993.215312	253561.956001	37.706317
1994.971630	253874.172842	37.711335
1996.848025	254182.992664	37.716352
1998.739714	254498.643714	37.721370
2000.529253	254813.701821	37.726388
2002.955704	255129.345230	37.731405
2004.577660	255448.749282	37.736423
2006.184518	255771.712537	37.741440
2008.599722	256078.976425	37.746458
2010.403479	256395.812834	37.751476
2012.359709	256692.024185	37.756493
2014.570812	256985.375829	37.761511
2016.218600	257284.608982	37.766528
2018.293994	257585.806882	37.771546
2019.959307	257889.153236	37.776564
2022.130821	258190.260453	37.781581
2023.820597	258505.314275	37.786599
2025.937530	258811.816264	37.791616
2027.799659	259126.132256	37.796634
2029.372205	259446.006952	37.801652
2031.406986	259764.132131	37.806669
2033.124190	260098.387995	37.811687
2035.061765	260440.280941	37.816704
2037.269846	260778.168557	37.821722
2039.392545	261120.617222	37.826740
2041.365958	261450.820397	37.831757
2043.723070	261793.461279	37.836775
2045.412226	262147.385783	37.841792
2047.935075	262486.901982	37.846810
2049.869468	262829.611048	37.851828
2052.079542	263171.133599	37.856845
2053.651920	263520.480164	37.861863
2056.110872	263864.656633	37.866880
2058.369188	264213.183774	37.871898
2060.930234	264557.674933	37.876916
2063.184334	264884.001068	37.881933
2065.642001	265222.920528	37.886951
2067.759930	265552.749027	37.891968
2070.834621	265886.134873	37.896986
2072.568678	266211.960259	37.902004
2074.847612	266525.963168	37.907021
2077.226886	266849.120926	37.912039
2079.458508	267159.372074	37.917056
2082.051785	267461.309991	37.922074
2084.239552	267763.820466	37.927092
2086.325274	268070.488025	37.932109
2088.737006	268378.526617	37.937127
2090.414672	268692.753189	37.942144
2093.035192	268991.232732	37.947162
2094.617753	269294.754485	37.952180
2096.756645	269596.079647	37.957197
2098.712873	269903.149656	37.962215
2100.439271	270221.205080	37.967232
2102.081126	270536.225631	37.972250
2103.785212	270855.682009	37.977268
2105.915486	271172.809994	37.982285
2107.918376	271503.726909	37.987303
2109.783264	271847.646939	37.992320
2112.216661	272172.907011	37.997338
2113.913108	272506.032082	38.002356
2116.217490	272840.737422	38.007373
2118.184561	273182.456858	38.012391
2120.030648	273521.375757	38.017408
2122.450995	273847.349492	38.022426
2124.352771	274178.206753	38.027444
2126.435301	274488.255375	38.032461
2128.513405	274794.443394	38.037479
2130.170042	275116.397576	38.042496
2132.615570	275426.388645	38.047514
2134.967077	275755.828230	38.052532
2136.618952	276070.136712	38.057549
2138.586258	276395.140784	38.062567
2140.632608	276732.884795	38.067584
2142.904589	277065.588505	38.072602
2144.802282	277410.621363	38.077620
2146.849456	277752.277198	38.082637
2149.182601	278084.335928	38.087655
2151.055996	278433.843403	38.092672
2153.556095	278775.503356	38.097690
2155.981241	279115.828713	38.102708
2158.074264	279464.538928	38.107725
2160.091238	279811.050981	38.112743
2162.235694	280158.177761	38.117760
2164.634822	280500.691403	38.122778
2167.004810	280861.804734	38.127796
2169.244940	281207.264640	38.132813
2171.638983	281548.940272	38.137831
2174.030797	281910.938687	38.142848
2176.135656	282249.687607	38.147866
2178.305011	282595.767632	38.152884
2180.432730	282953.742746	38.157901
2182.865496	283293.328125	38.162919
2184.989572	283644.444464	38.167936
2187.413000	283984.564308	38.172954
2189.302028	284343.795600	38.177972
2191.640927	284693.987956	38.182989
2194.242357	285037.127135	38.188007
2196.497758	285390.837774	38.193024
2198.877148	285745.519155	38.198042
2200.826309	286083.299203	38.203060
2203.064979	286435.665168	38.208077
2205.073074	286778.642843	38.213095
2207.015783	287138.853755	38.218112
2209.573597	287484.182239	38.223130
2211.915140	287844.710188	38.228148
2214.299641	288202.106364	38.233165
2216.946881	288544.701415	38.238183
2218.483086	288899.081339	38.243200
2221.112742	289247.825853	38.248218
2223.040076	289600.466320	38.253236
2225.383326	289951.922674	38.258253
2227.721126	290296.698534	38.263271
2229.753243	290653.918917	38.268288
2232.294914	290990.659712	38.273306
2234.360344	291353.792657	38.278324
2236.538662	291710.378721	38.283341
2238.871737	292062.011642	38.288359
2240.491822	292424.172111	38.293376
2242.951006	292759.297800	38.298394
2245.406828	293105.219553	38.303412
2247.340745	293435.347055	38.308429
2249.782068	293765.850857	38.313447
2251.723947	294092.775418	38.318464
2254.029396	294424.798491	38.323482
2256.024121	294752.424921	38.328500
2258.279223	295091.440524	38.333517
2260.715926	295413.635969	38.338535
2262.829292	295768.041190	38.343552
2265.124050	296100.317249	38.348570
2267.465788	296444.651234	38.353588
2269.513455	296792.460483	38.358605
2271.527112	297134.940083	38.363623
2273.820815	297496.578442	38.368640
2276.206829	297854.137161	38.373658
2278.121414	298218.679180	38.378676
2280.131103	298591.156094	38.383693
2282.303987	298951.591364	38.388711
2284.650872	299326.782004	38.393728
2286.941270	299700.685286	38.398746
2289.187034	300078.481222	38.403764
2291.601000	300464.200256	38.408781
2294.093261	300835.198575	38.413799
2296.440129	301227.022722	38.418816
2299.586966	301580.972856	38.423834
2301.886066	301957.130177	38.428852
2303.616037	302334.900856	38.433869
2306.676583	302699.759129	38.438887
2308.668475	303078.654842	38.443904
2311.131761	303462.174005	38.448922
2313.420063	303836.880396	38.453940
2316.274985	304212.105590	38.458957
2318.495447	304576.508058	38.463975
2320.750492	304959.268737	38.468992
2323.176077	305329.580436	38.474010
2325.866250	305706.377099	38.479028
2327.857104	306081.073718	38.484045
2330.548124	306451.111617	38.489063
2332.929389	306822.543779	38.494080
2335.235132	307194.596444	38.499098
2337.367669	307568.224883	38.504116
2339.717741	307940.192123	38.509133
2342.084686	308306.059581	38.514151
2344.293037	308694.531589	38.519168
2346.599871	309072.141025	38.524186
2348.961568	309449.918373	38.529204
2351.196076	309823.980932	38.534221
2353.870686	310210.265926	38.539239
2356.013729	310584.746938	38.544256
2358.426567	310959.158563	38.549274
2360.635825	311348.586817	38.554292
2363.499808	311726.124705	38.559309
2366.056425	312095.074326	38.564327
2368.411872	312464.740372	38.569344
2371.037289	312822.856642	38.574362
2373.706065	313174.818323	38.579380
2375.686605	313507.508649	38.584397
2378.084915	313843.179561	38.589415
2380.192517	314189.385118	38.594432
2382.428353	314520.990429	38.599450
2384.949230	314855.800502	38.604468
2386.789047	315211.696499	38.609485
2389.401476	315556.903100	38.614503
2391.403452	315913.837653	38.619520
2393.525967	316270.345455	38.624538
2395.648041	316635.715954	38.629556
2397.540131	317022.836771	38.634573
2400.235701	317387.021452	38.639591
2402.411616	317769.903654	38.644608
2404.859536	318154.519045	38.649626
2407.280534	318540.559400	38.654644
2409.743114	318932.534572	38.659661
2412.515146	319313.995356	38.664679
2414.990873	319704.365145	38.669696
2417.216398	320087.610940	38.674714
2420.042416	320477.058396	38.679732
2422.192534	320878.903369	38.684749
2424.680777	321267.512024	38.689767
2427.217914	321666.015910	38.694784
2429.214370	322060.438639	38.699802
2431.941579	322456.623100	38.704820
2434.343939	322863.574453	38.709837
2437.181723	323270.226295	38.714855
2439.286478	323669.881457	38.719872
2441.898509	324073.720840	38.724890
2444.348941	324476.390269	38.729908
2446.617133	324897.879414	38.734925
2449.300658	325291.949566	38.739943
2451.707542	325703.838441	38.744960
2454.314188	326122.499490	38.749978
2457.166888	326524.155387	38.754996
2459.201610	326935.258849	38.760013
2461.849834	327340.015796	38.765031
2463.819114	327757.702587	38.770048
2466.480071	328179.645390	38.775066
2469.346824	328595.509376	38.780084
2471.856707	329011.656192	38.785101
2474.442543	329423.039965	38.790119
2476.774777	329829.154309	38.795136
2479.259011	330257.462033	38.800154
2481.816535	330660.615823	38.805172
2484.432675	331086.536199	38.810189
2486.894156	331489.421304	38.815207
2489.251414	331919.999422	38.820224
2491.769056	332329.397013	38.825242
2494.627410	332743.842265	38.830260
2497.080599	333162.107436	38.835277
2499.984943	333569.075033	38.840295
2502.351993	333961.397681	38.845312
2504.884423	334366.337343	38.850330
2507.693374	334752.719814	38.855348
2510.187321	335112.132741	38.860365
2512.661089	335473.375190	38.865383
2515.222437	335841.711561	38.870400
2517.187168	336213.746070	38.875418
2519.838033	336583.181410	38.880436
2522.122042	336962.804015	38.885453
2524.588808	337335.641382	38.890471
2526.901726	337717.337133	38.895488
2528.862167	338113.076947	38.900506
2531.526761	338505.325787	38.905524
2533.732920	338908.613655	38.910541
2536.396175	339305.555087	38.915559
2538.502974	339716.648476	38.920576
2540.653453	340134.308331	38.925594
2543.423547	340551.334040	38.930612
2545.938259	340983.148935	38.935629
2548.427695	341396.938132	38.940647
2551.222060	341833.856869	38.945664
2553.309020	342275.403855	38.950682
2555.904400	342716.917856	38.955700
2558.377323	343156.036070	38.960717
2560.936112	343595.492901	38.965735
2563.347100	344049.009789	38.970752
2565.890758	344506.538931	38.975770
2568.911667	344948.679818	38.980788
2571.427360	345402.372766	38.985805
2573.853941	345862.042410	38.990823
2576.443592	346319.169178	38.995840
2579.170737	346779.926295	39.000858
2582.005674	347232.284828	39.005876
2584.588997	347704.278342	39.010893
2587.258701	348150.791278	39.015911
2590.169415	348618.384075	39.020928
2592.495713	349081.369033	39.025946
2595.503597	349539.215670	39.030964
2597.936624	350005.526892	39.035981
2600.670371	350458.890542	39.040999
2603.285770	350917.371619	39.046016
2606.027182	351379.992005	39.051034
2608.673073	351836.962647	39.056052
2611.152295	352303.906608	39.061069
2614.062208	352763.543600	39.066087
2617.066171	353221.232451	39.071104
2619.774952	353682.974738	39.076122
2622.805577	354130.573846	39.081140
2625.370724	354570.602300	39.086157
2627.888217	355016.447344	39.091175
2630.875362	355467.519198	39.096192
2633.403249	355918.482100	39.101210
2636.298652	356359.508835	39.106228
2638.663620	356807.900511	39.111245
2641.579877	357253.891036	39.116263
2644.207658	357689.922676	39.121280
2646.451450	358134.006584	39.126298
2649.181458	358546.383871	39.131316
2651.710919	358958.535621	39.136333
2654.178919	359381.099926	39.141351
2656.972889	359795.918448	39.146368
2659.250828	360207.439473	39.151386
2661.656450	360624.393564	39.156404
2664.192080	361048.912145	39.161421
2666.749930	361472.458955	39.166439
2669.520088	361893.049642	39.171456
2671.621980	362339.578921	39.176474
2674.777957	362769.161167	39.181492
2677.630230	363199.218986	39.186509
2680.150958	363653.714499	39.191527
2682.998556	364077.242470	39.196544
2685.741399	364522.202552	39.201562
2687.920565	364959.354926	39.206580
2691.031831	365411.506117	39.211597
2693.878100	365859.380525	39.216615
2696.740387	366307.552453	39.221632
2699.085121	366750.117348	39.226650
2701.843261	367211.340558	39.231668
2704.330151	367678.337044	39.236685
2707.059283	368136.636845	39.241703
2710.093841	368587.778150	39.246720
2712.563370	369065.648944	39.251738
2715.098587	369525.639635	39.256756
2717.673711	370009.954042	39.261773
2720.493130	370482.501020	39.266791
2723.179450	370952.247242	39.271808
2725.574434	371436.167988	39.276826
2728.486757	371925.735829	39.281844
2731.372765	372414.490169	39.286861
2733.797153	372900.546174	39.291879
2736.865220	373382.866189	39.296896
2739.452390	373885.402893	39.301914
2742.462427	374377.412957	39.306932
2745.020171	374878.901887	39.311949
2747.566573	375378.204447	39.316967
2750.340612	375875.993254	39.321984
2752.977707	376390.568122	39.327002
2755.851602	376881.605257	39.332020
2758.955698	377387.999978	39.337037
2761.420027	377902.887180	39.342055
2763.926744	378414.513592	39.347072
2766.621348	378934.678598	39.352090
2769.670839	379439.482715	39.357108
2772.538366	379970.895956	39.362125
2774.926362	380480.712906	39.367143
2778.039862	380998.703729	39.372160
2780.539558	381523.380459	39.377178
2783.313159	382048.716914	39.382196
2786.157584	382569.798541	39.387213
2788.999979	383090.289871	39.392231
2791.457120	383613.244842	39.397248
2794.473589	384133.237558	39.402266
2797.280122	384633.648345	39.407284
2800.495163	385114.177118	39.412301
2803.676621	385594.857152	39.417319
2806.761843	386065.755245	39.422336
2809.107332	386533.644548	39.427354
2812.314570	387006.362830	39.432372
2815.086531	387476.886475	39.437389
2817.595003	387959.924658	39.442407
2820.104602	388438.821958	39.447424
2822.806621	388935.208242	39.452442
2825.806004	389420.710692	39.457460
2828.695192	389921.314533	39.462477
2830.942806	390425.107025	39.467495
2833.763750	390916.881603	39.472512
2836.675459	391441.426980	39.477530
2838.818603	391946.101818	39.482548
2842.167005	392459.201085	39.487565
2844.958841	392972.862701	39.492583
2847.639168	393496.044210	39.497600
2850.353823	394026.972260	39.502618
2853.323604	394557.090904	39.507636
2856.411125	395089.819933	39.512653
2859.061354	395622.559092	39.517671
2862.410982	396158.500975	39.522688
2864.980875	396698.209187	39.527706
2867.440845	397239.346071	39.532724
2870.319704	397794.784964	39.537741
2873.292705	398343.378861	39.542759
2876.528513	398883.377176	39.547776
2879.512064	399436.946221	39.552794
2882.188265	399991.416602	39.557812
2885.200200	400544.911630	39.562829
2888.161656	401107.152285	39.567847
2891.252451	401656.990169	39.572864
2893.919073	402219.460878	39.577882
2896.695483	402781.549373	39.582900
2899.714174	403347.975502	39.587917
2902.830070	403909.863515	39.592935
2905.460441	404470.474752	39.597952
2908.535639	405040.841665	39.602970
2911.702283	405602.843443	39.607988
2914.548128	406162.148064	39.613005
2917.414050	406746.433900	39.618023
2920.834267	407296.602703	39.623040
2923.632458	407871.879027	39.628058
2926.663903	408439.477871	39.633076
2929.571448	409001.357209	39.638093
2932.478698	409570.703555	39.643111
2935.428613	410138.359538	39.648128
2938.497732	410703.375289	39.653146
2941.349210	411270.189014	39.658164
2944.449892	411834.747493	39.663181
2947.123835	412415.583333	39.668199
2949.977811	412976.408096	39.673216
2952.734791	413547.273609	39.678234
2955.467566	414088.911176	39.683252
2958.454687	414626.190182	39.688269
2961.081220	415174.362804	39.693287
2963.941601	415722.842829	39.698304
2966.272539	416277.148686	39.703322
2969.148907	416829.254248	39.708340
2972.293682	417382.776420	39.713357
2974.666843	417955.085378	39.718375
2977.414064	418520.228614	39.723392
2980.244189	419104.452855	39.728410
2982.772230	419695.706133	39.733428
2985.904999	420289.334341	39.738445
2988.825623	420900.212753	39.743463
2991.907803	421500.309481	39.748480
2995.072876	422100.050724	39.753498
2998.087987	422705.807167	39.758516
3001.305822	423311.366163	39.763533
3004.101035	423930.481837	39.768551
3007.135778	424538.905361	39.773568
3010.316451	425160.262741	39.778586
3013.266457	425780.350372	39.783604
3016.691874	426402.780356	39.788621
3019.757192	427032.649638	39.793639
3023.217745	427644.253978	39.798656
3026.351546	428266.205354	39.803674
3029.634597	428899.871450	39.808692
3032.683642	429500.808892	39.813709
3035.500767	430136.899844	39.818727
3038.700048	430753.209798	39.823744
3041.699049	431380.630183	39.828762
3044.565995	432004.459903	39.833780
3048.010069	432625.118790	39.838797
3050.586959	433270.364238	39.843815
3053.778807	433904.834417	39.848832
3056.664502	434540.958004	39.853850
3059.281053	435196.227472	39.858868
3062.427757	435846.610081	39.863885
3065.442135	436503.226093	39.868903
3068.329291	437167.137643	39.873920
3071.458713	437841.552000	39.878938
3073.999208	438515.053779	39.883956
3077.329559	439178.436438	39.888973
3080.322565	439860.463912	39.893991
3083.252920	440533.722338	39.899008
3086.229781	441217.790707	39.904026
3089.330628	441897.212640	39.909044
3092.687477	442579.612964	39.914061
3095.314699	443275.323984	39.919079
3098.670421	443964.722922	39.924096
3102.177351	444646.028348	39.929114
3105.133320	445339.197354	39.934132
3108.533372	446027.922189	39.939149
3111.812439	446722.012173	39.944167
3114.709549	447417.255830	39.949184
3117.687775	448081.587835	39.954202
3120.846991	448749.972454	39.959220
3123.879547	449386.975257	39.964237
3127.045366	450041.199505	39.969255
3130.193035	450680.881779	39.974272
3133.534845	451320.464968	39.979290
3136.349073	451982.231062	39.984308
3139.395321	452615.447800	39.989325
3142.609883	453281.414764	39.994343
3145.904837	453935.861636	39.999360
3148.917755	454590.992058	40.004378
3151.813027	455255.787457	40.009396
3154.905572	455930.247689	40.014413
3157.830709	456598.490111	40.019431
3160.854244	457278.284252	40.024448
3163.678931	457962.339268	40.029466
3166.630382	458666.591679	40.034484
3170.138231	459361.474693	40.039501
3172.696789	460074.497059	40.044519
3175.782682	460771.830532	40.049536
3179.044155	461494.763016	40.054554
3182.058987	462223.831588	40.059572
3185.231790	462936.561690	40.064589
3188.259045	463679.793874	40.069607
3191.585116	464433.828371	40.074624
3195.035590	465175.828787	40.079642
3198.314725	465921.927340	40.084660
3201.617038	466670.828283	40.089677
3204.942240	467413.528745	40.094695
3208.061325	468163.872236	40.099712
3211.226238	468914.181566	40.104730
3214.467702	469667.030866	40.109748
3217.699863	470420.258877	40.114765
3220.951175	471192.469519	40.119783
3224.183885	471952.063492	40.124800
3227.608601	472714.379929	40.129818
3230.737319	473464.276695	40.134836
3233.788358	474245.707071	40.139853
3237.031781	475026.773551	40.144871
3240.152158	475786.545486	40.149888
3243.675141	476574.534936	40.154906
3246.702497	477358.982619	40.159924
3250.677649	478129.904524	40.164941
3253.898305	478911.530796	40.169959
3257.027439	479676.359590	40.174976
3260.772068	480456.881489	40.179994
3263.958991	481232.709665	40.185012
3267.461470	482002.442980	40.190029
3271.064274	482756.412868	40.195047
3274.111705	483531.059794	40.200064
3278.187563	484286.866209	40.205082
3280.875968	485060.750536	40.210100
3284.700095	485810.169929	40.215117
3287.982236	486579.452442	40.220135
3291.039390	487336.259696	40.225152
3294.153653	488076.607629	40.230170
3297.330123	488808.530184	40.235188
3300.653151	489525.851509	40.240205
3304.118750	490244.082737	40.245223
3307.069869	490961.155388	40.250240
3309.912211	491662.912000	40.255258
3312.838643	492401.856092	40.260276
3316.025327	493122.849092	40.265293
3319.545484	493867.499909	40.270311
3322.328768	494609.408789	40.275328
3325.619263	495358.176979	40.280346
3328.706219	496111.037311	40.285364
3331.895357	496869.304321	40.290381
3335.369160	497625.020270	40.295399
3338.700504	498400.066861	40.300416
3342.044067	499171.240715	40.305434
3345.268923	499946.540477	40.310452
3348.690520	500728.995430	40.315469
3351.952662	501519.317149	40.320487
3354.729591	502319.322911	40.325504
3358.011074	503114.013120	40.330522
3361.588454	503934.617739	40.335540
3364.893488	504750.027947	40.340557
3368.220946	505569.434629	40.345575
3371.459578	506393.056558	40.350592
3375.094477	507200.274973	40.355610
3378.009726	508044.410970	40.360628
3381.674277	508865.021819	40.365645
3385.489970	509687.588118	40.370663
3388.956621	510539.134347	40.375680
3392.536044	511346.721915	40.380698
3396.214183	512194.720817	40.385716
3399.267369	513027.438390	40.390733
3402.826304	513860.236746	40.395751
3405.988024	514707.888353	40.400768
3409.507439	515549.790671	40.405786
3412.883065	516402.215820	40.410804
3416.784908	517250.932862	40.415821
3420.060047	518090.677185	40.420839
3423.349619	518945.910539	40.425856
3427.332872	519790.701589	40.430874
3430.851437	520642.431461	40.435892
3434.202332	521475.233241	40.440909
3438.000039	522326.982316	40.445927
3441.130085	523176.775339	40.450944
3444.667631	524015.518299	40.455962
3447.714088	524866.697732	40.460980
3451.461794	525716.007126	40.465997
3455.020401	526561.167595	40.471015
3458.416829	527403.637239	40.476032
3462.402349	528259.074652	40.481050
3465.916571	529094.379034	40.486068
3469.422551	529949.901534	40.491085
3473.154862	530781.301942	40.496103
3476.299056	531630.036741	40.501120
3480.061326	532456.971221	40.506125
3483.213520	533239.584946	40.511130
3486.306097	533979.482314	40.516135
3489.872864	534644.457947	40.521140
3492.610955	535255.184817	40.526144
3495.669062	535802.193854	40.531149
3498.156145	536308.462617	40.536154
3500.841302	536728.871542	40.541159
3503.397952	537096.358844	40.546164
3505.761458	537407.605203	40.551168
3507.794894	537664.100315	40.556173
3509.288476	537878.051465	40.561178
3510.673957	538036.564436	40.566183
3513.155572	538143.743367	40.571188
3514.619003	538225.023226	40.576192
3515.743269	538238.683207	40.581197
3516.828769	538239.269191	40.586202
3517.860931	538192.542803	40.591207
3518.817240	538115.526615	40.596212
3519.476015	538031.183617	40.601216
3520.632023	537895.551087	40.606221
3521.125574	537748.002100	40.611226
3521.572014	537586.721905	40.616231
3522.017015	537396.298779	40.621236
3522.293728	537189.384472	40.626240
3522.638640	536968.365259	40.631245
3522.992057	536752.493255	40.636250
3522.988453	536508.036568	40.641255
3523.435679	536246.533731	40.646260
3523.659589	535984.203068	40.651264
3523.941594	535714.534694	40.656269
3524.091519	535423.819117	40.661274
3523.868278	535139.420591	40.666279
3523.973630	534840.619037	40.671284
3523.854227	534554.879969	40.676288
3523.722248	534253.073684	40.681293
3523.698004	533944.020625	40.686298
3523.339596	533648.957039	40.691303
3523.400988	533339.878398	40.696308
3523.216960	533033.408885	40.701312
3523.198856	532728.978445	40.706317
3522.564577	532428.883233	40.711322
3522.112508	532121.023512	40.716327
3522.306979	531823.564403	40.721332
3522.126914	531532.929085	40.726336
3522.130614	531245.139263	40.731341
3521.758099	530942.043641	40.736346
3521.362195	530655.720880	40.741351
3521.274313	530350.396171	40.746356
3520.669592	530066.925250	40.751360
3521.077198	529770.201961	40.756365
3521.026951	529484.106412	40.761370
3520.457623	529202.382916	40.766375
3520.381621	528914.815691	40.771380
3519.999708	528640.531397	40.776384
3520.001423	528357.338177	40.781389
3520.019447	528095.311649	40.786394
3519.467208	527818.715414	40.791399
3519.398855	527548.355023	40.796404
3518.780995	527287.982317	40.801408
3519.007895	527020.800721	40.806413
3518.798802	526762.780681	40.811418
3518.588038	526508.244018	40.816423
3518.461603	526252.173731	40.821428
3517.941361	525994.190442	40.826432
3517.801334	525738.467869	40.831437
3517.362440	525499.922732	40.836442
3517.217383	525261.630870	40.841447
3517.223915	525022.401700	40.846452
3516.813926	524801.128015	40.851456
3516.718055	524555.387668	40.856461
3516.463726	524334.285144	40.861466
3516.030578	524107.293735	40.866471
3516.191469	523882.227189	40.871476
3515.923132	523661.471491	40.876480
3515.849952	523450.640288	40.881485
3515.224452	523239.539774	40.886490
3515.043156	523029.276223	40.891495
3515.148888	522827.356206	40.896500
3514.695500	522630.728959	40.901504
3514.604348	522430.048374	40.906509
3514.374371	522239.447458	40.911514
3514.371248	522040.163649	40.916519
3514.047519	521855.892354	40.921524
3513.815093	521674.385098	40.926528
3513.597037	521485.340683	40.931533
3513.277014	521308.747142	40.936538
3513.544783	521140.350174	40.941543
3513.267801	520958.336414	40.946548
3512.754005	520801.687763	40.951552
3512.823387	520620.677223	40.956557
3512.657873	520462.756866	40.961562
3512.353663	520294.795504	40.966567
3512.399491	520142.197995	40.971572
3512.027671	519989.361709	40.976576
3512.205450	519826.021516	40.981581
3512.101113	519671.269224	40.986586
3511.790668	519521.300897	40.991591
3511.917693	519373.486818	40.996596
3511.304324	519225.990681	41.001600
3511.329488	519064.841258	41.006605
3511.150523	518941.544431	41.011610
3510.878394	518807.238368	41.016615
3510.725197	518669.575136	41.021620
3510.826626	518545.674818	41.026624
3510.684637	518403.052199	41.031629
3510.708941	518284.016408	41.036634
3510.113176	518159.212061	41.041639
3510.404086	518022.181169	41.046644
3510.019218	517921.714880	41.051648
3509.783900	517787.950946	41.056653
3509.976622	517670.300010	41.061658
3509.778258	517563.430514	41.066663
3509.673418	517429.693633	41.071668
3509.456590	517324.544848	41.076672
3509.908980	517224.397120	41.081677
3509.366186	517106.656157	41.086682
3509.147140	517004.236450	41.091687
3509.404732	516890.160194	41.096692
3509.226148	516790.969274	41.101696
3509.092770	516679.279609	41.106701
3509.010104	516572.688873	41.111706
3508.761888	516488.526802	41.116711
3508.860876	516374.016931	41.121716
3508.557430	516296.032378	41.126720
3508.549778	516188.719319	41.131725
3508.494876	516107.761403	41.136730
3508.506021	516004.237134	41.141735
3508.685243	515916.211643	41.146740
3508.289504	515820.842257	41.151744
3508.400189	515738.592041	41.156749
3508.659185	515648.327285	41.161754
3508.260334	515557.356826	41.166759
3508.394917	515461.041804	41.171764
3508.211724	515379.594888	41.176768
3508.094328	515291.461263	41.181773
3508.196440	515197.526886	41.186778
3508.020262	515127.912274	41.191783
3508.299256	515024.744209	41.196788
3507.738614	514947.350343	41.201792
3507.636070	514872.463110	41.206797
3507.561258	514786.241998	41.211802
3507.354568	514726.796442	41.216807
3507.609148	514637.841934	41.221812
3507.173415	514566.698124	41.226816
3507.468710	514491.341692	41.231821
3507.398792	514417.003623	41.236826
3507.245034	514342.526741	41.241831
3507.498037	514275.571968	41.246836
3507.490873	514205.168140	41.251840
3507.439607	514131.989165	41.256845
3507.282354	514065.654762	41.261850
3507.197769	513988.231807	41.266855
3507.302361	513921.855453	41.271860
3507.116209	513852.490023	41.276864
3507.353999	513775.369193	41.281869
3507.199619	513705.947558	41.286874
3507.015054	513637.339689	41.291879
3507.292642	513575.840897	41.296884
3507.231694	513512.271008	41.301888
3506.977438	513441.700720	41.306893
3506.897893	513366.449079	41.311898
3507.005731	513307.808671	41.316903
3507.243764	513229.370198	41.321908
3506.560323	513185.573584	41.326912
3506.702079	513106.542781	41.331917
3506.602274	513053.447709	41.336922
3506.707650	513000.117714	41.341927
3506.823827	512927.261118	41.346932
3506.450654	512855.290870	41.351936
3506.531717	512799.890206	41.356941
3506.573288	512760.985576	41.361946
3506.654876	512701.942553	41.366951
3506.694764	512628.894398	41.371956
3506.576815	512587.788925	41.376960
3506.455039	512518.003170	41.381965
3506.357444	512472.948692	41.386970
3506.230463	512418.641918	41.391975
3506.112434	512362.158446	41.396980
3506.140557	512317.690692	41.401984
3506.256184	512267.492979	41.406989
3506.145591	512213.031203	41.411994
3506.361985	512157.252958	41.416999
3506.490191	512107.609213	41.422004
3505.947875	512060.044109	41.427008
3506.088932	512000.736320	41.432013
3506.240886	511959.080813	41.437018
3506.115278	511910.285969	41.442023
3506.332834	511856.226450	41.447028
3506.092784	511805.577733	41.452032
3506.095418	511740.574743	41.457037
3506.072279	511701.020294	41.462042
3505.727770	511652.056963	41.467047
3506.080344	511590.185008	41.472052
3505.884891	511550.100994	41.477056
3506.044070	511506.672716	41.482061
3506.058715	511464.278903	41.487066
3505.813878	511406.648803	41.492071
3506.166483	511357.068573	41.497076
3505.990527	511324.771328	41.502080
3505.989396	511284.453626	41.507085
3506.054785	511229.707948	41.512090
3506.031984	511176.038368	41.517095
3505.836869	511120.574701	41.522100
3505.681637	511092.624272	41.527104
3505.590282	511039.066271	41.532109
3505.798313	510996.590141	41.537114
3505.452360	510964.369668	41.542119
3505.471798	510915.346693	41.547124
3505.676151	510865.788466	41.552128
3505.622055	510835.494567	41.557133
3505.360071	510793.092217	41.562138
3505.746820	510748.715445	41.567143
3505.581306	510715.150675	41.572148
3505.335365	510667.737186	41.577152
3505.425245	510620.169308	41.582157
3505.686302	510597.312358	41.587162
3505.562599	510563.032433	41.592167
3505.737747	510519.447349	41.597172
3505.459018	510476.793912	41.602176
3505.478182	510429.135501	41.607181
3505.435036	510400.913275	41.612186
3505.261544	510358.242910	41.617191
3505.524794	510324.154295	41.622196
3505.441959	510292.801586	41.627200
3505.786269	510244.079467	41.632205
3505.666133	510209.140595	41.637210
3505.289465	510157.344993	41.642215
3505.314413	510122.433604	41.647220
3505.530240	510091.235682	41.652224
3505.562449	510039.628053	41.657229
3505.353364	510007.232367	41.662234
3505.328282	509967.775388	41.667239
3505.401930	509930.882861	41.672244
3505.305221	509893.663041	41.677248
3505.447511	509868.547285	41.682253
3505.266821	509827.293289	41.687258
3505.104835	509800.404233	41.692263
3505.189974	509757.489125	41.697268
3505.240629	509718.424334	41.702272
3505.223537	509697.229082	41.707277
3505.066937	509662.497225	41.712282
3504.844696	509651.300946	41.717287
3504.962965	509597.098192	41.722292
3504.835902	509575.818987	41.727296
3504.790158	509537.932641	41.732301
3504.912475	509505.433034	41.737306
3505.164642	509474.531802	41.742311
3505.080465	509448.692338	41.747316
3505.102578	509425.669223	41.752320
3505.136445	509387.365220	41.757325
3505.554126	509357.803622	41.762330
3504.788796	509322.964918	41.767335
3505.073190	509279.612379	41.772340
3505.128519	509258.455732	41.777344
3505.003401	509233.280125	41.782349
3505.401591	509187.379709	41.787354
3505.069709	509155.355975	41.792359
3504.989467	509130.830839	41.797364
3504.776241	509097.118657	41.802368
3505.174186	509071.202424	41.807373
3505.081437	509032.411706	41.812378
3504.598722	509016.348583	41.817383
3504.763863	508992.037435	41.822388
3504.904460	508949.870453	41.827392
3504.633977	508928.258955	41.832397
3505.285173	508908.980868	41.837402
3505.008957	508873.912162	41.842407
3505.130212	508833.215184	41.847412
3504.897215	508821.868279	41.852416
3504.988286	508780.720599	41.857421
3504.974703	508760.535527	41.862426
3505.006142	508724.962540	41.867431
3505.357348	508693.943064	41.872436
3505.063924	508648.251713	41.877440
3504.904732	508629.151994	41.882445
3505.166085	508591.923355	41.887450
3504.981842	508557.952559	41.892455
3505.184114	508522.301558	41.897460
3505.033650	508501.682460	41.902464
3505.141409	508463.718891	41.907469
3505.171154	508432.294393	41.912474
3505.009021	508408.793082	41.917479
3505.091266	508374.375041	41.922484
3505.003574	508344.689199	41.927488
3504.820246	508324.834021	41.932493
3505.034125	508283.615147	41.937498
3504.950720	508266.729270	41.942503
3505.226179	508226.158275	41.947508
3505.027164	508201.599992	41.952512
3505.083176	508166.123161	41.957517
3504.964932	508134.013162	41.962522
3504.780349	508104.038642	41.967527
3504.808506	508069.324962	41.972532
3504.542730	508060.512566	41.977536
3504.390109	508023.550518	41.982541
3504.678718	508006.706782	41.987546
3504.465974	507980.177079	41.992551
3504.925120	507956.425165	41.997556
3504.702095	507934.400143	42.002560
3504.669593	507902.073773	42.007565
3504.893708	507881.091146	42.012570
3504.771992	507855.508210	42.017575
3505.035542	507822.224148	42.022580
3504.768551	507797.220658	42.027584
3504.741755	507768.586746	42.032589
3504.709807	507748.706978	42.037594
3504.644057	507723.418585	42.042599
3504.739834	507695.068764	42.047604
3504.712807	507684.498118	42.052608
3504.522295	507654.017777	42.057613
3504.872374	507631.345211	42.062618
3504.642659	507606.487346	42.067623
3504.685759	507573.490639	42.072628
3504.605079	507559.437131	42.077632
3504.658586	507530.284151	42.082637
3504.756336	507509.068056	42.087642
3504.803372	507484.975846	42.092647
3504.635871	507461.069307	42.097652
3504.494228	507439.739168	42.102656
3504.532652	507410.031788	42.107661
3504.491991	507377.098544	42.112666
3504.778104	507368.147966	42.117671
3504.826902	507338.540021	42.122676
3504.886342	507322.541422	42.127680
3504.640289	507284.479388	42.132685
3504.788601	507263.204401	42.137690
3504.520544	507244.879341	42.142695
3504.924232	507216.581269	42.147700
3504.529502	507200.704939	42.152704
3504.596556	507166.843487	42.157709
3504.684100	507147.804329	42.162714
3504.758035	507108.578149	42.167719
3504.657776	507082.434085	42.172724
3504.624025	507064.021201	42.177728
3504.598834	507039.281994	42.182733
3504.559711	507015.405148	42.187738
3504.104490	507000.398390	42.192743
3504.457925	506982.126621	42.197748
3504.333141	506978.907962	42.202752
3504.585258	506951.240612	42.207757
3504.748844	506917.262215	42.212762
3504.671002	506897.641724	42.217767
3504.830782	506875.757250	42.222772
3504.921196	506840.980667	42.227776
3504.745053	506822.893634	42.232781
3504.814812	506778.607344	42.237786
3504.255266	506758.759228	42.242791
3504.754527	506743.500187	42.247796
3504.858589	506712.718628	42.252800
3504.714008	506694.575872	42.257805
3504.940868	506655.830505	42.262810
3504.686050	506641.803775	42.267815
3504.715621	506605.265311	42.272820
3504.899655	506587.121105	42.277824
3504.724839	506557.850776	42.282829
3504.688865	506526.989820	42.287834
3504.536141	506510.113186	42.292839
3504.739241	506480.479389	42.297844
3504.717835	506464.239771	42.302848
3504.554113	506453.588777	42.307853
3504.343692	506415.316799	42.312858
3504.753634	506385.447742	42.317863
3504.566459	506363.516259	42.322868
3504.429962	506335.656344	42.327872
3504.479238	506319.557224	42.332877
3504.507850	506289.849478	42.337882
3504.462306	506271.589423	42.342887
3504.598993	506254.008973	42.347892
3504.921202	506239.081087	42.352896
3504.429488	506198.069983	42.357901
3504.644701	506188.674588	42.362906
3504.554776	506175.026236	42.367911
3504.447945	506140.178224	42.372916
3504.473209	506121.552605	42.377920
3504.281383	506105.086576	42.382925
3504.678388	506075.522648	42.387930
3504.021982	506074.007123	42.392935
3504.361485	506045.211268	42.397940
3504.431482	506028.400169	42.402944
3504.306722	506013.441529	42.407949
3504.566414	505985.366627	42.412954
3504.453430	505972.177184	42.417959
3504.556325	505954.551171	42.422964
3504.536689	505929.303479	42.427968
3504.546075	505900.255945	42.432973
3504.698737	505868.908581	42.437978
3504.521712	505864.179880	42.442983
3504.706421	505830.145421	42.447988
3504.450920	505813.992799	42.452992
3504.688999	505795.889831	42.457997
3504.736269	505761.320324	42.463002
3504.648040	505746.052062	42.468007
3504.643912	505706.480836	42.473012
3504.601828	505698.795759	42.478016
3504.538919	505661.612087	42.483021
3504.596046	505641.209792	42.488026
3504.608758	505626.735130	42.493031
3504.524261	505595.374155	42.498036
3504.689945	505570.552088	42.503040
3504.273128	505553.665663	42.508045
3504.415619	505534.565453	42.513050
3504.403468	505523.282685	42.518055
3504.064534	505510.179210	42.523060
3503.933200	505477.661533	42.528064
3504.060552	505481.183699	42.533069
3504.346528	505462.313753	42.538074
3504.169760	505439.164959	42.543079
3504.357085	505429.318126	42.548084
3504.412642	505411.294212	42.553088
3504.424760	505386.647969	42.558093
3504.278887	505372.046347	42.563098
3504.335363	505349.467823	42.568103
3504.689891	505327.955461	42.573108
3504.575587	505303.480896	42.578112
3504.371577	505293.139187	42.583117
3504.883996	505254.143155	42.588122
3504.422138	505236.858704	42.593127
3504.349477	505211.921985	42.598132
3504.715498	505194.506641	42.603136
3504.447954	505171.928496	42.608141
3504.385760	505165.612699	42.613146
3504.355751	505132.673525	42.618151
3504.865881	505095.246261	42.623156
3504.642713	505091.789775	42.628160
3504.683252	505059.193549	42.633165
3504.685072	505029.589104	42.638170
3504.512648	505007.451160	42.643175
3504.481496	504988.580222	42.648180
3504.657913	504970.587358	42.653184
3504.787158	504943.088062	42.658189
3504.607209	504913.056698	42.663194
3504.357405	504893.967188	42.668199
3504.611611	504873.887090	42.673204
3504.562477	504845.251899	42.678208
3504.571540	504828.398671	42.683213
3504.700642	504795.737351	42.688218
3504.474258	504787.979792	42.693223
3504.382881	504756.922038	42.698228
3504.681694	504741.692936	42.703232
3504.006991	504715.079444	42.708237
3504.257730	504691.710272	42.713242
3504.554255	504684.376083	42.718247
3504.400723	504651.961592	42.723252
3504.339540	504650.756710	42.728256
3504.175660	504622.948996	42.733261
3504.538289	504599.916264	42.738266
3504.304113	504585.935222	42.743271
3504.499948	504560.347857	42.748276
3504.520962	504549.109826	42.753280
3504.254196	504511.753503	42.758285
3504.388011	504502.319464	42.763290
3504.340690	504480.110473	42.768295
3504.497655	504457.110060	42.773300
3504.375769	504437.797406	42.778304
3504.159183	504426.900494	42.783309
3504.348753	504408.904975	42.788314
3504.258354	504391.864619	42.793319
3504.159295	504372.447071	42.798324
3504.333916	504356.225117	42.803329
3504.056519	504335.924782	42.808333
3504.258126	504330.376709	42.813338
3504.102849	504304.085353	42.818343
3504.107686	504287.940780	42.823348
3504.247329	504263.981308	42.828353
3503.720341	504258.396546	42.833357
3504.695190	504231.420384	42.838362
3504.462385	504225.485468	42.843367
3504.147180	504205.848860	42.848372
3504.405411	504186.627673	42.853377
3504.387831	504166.488508	42.858381
3504.343384	504136.130749	42.863386
3504.133012	504134.797587	42.868391
3504.088648	504112.537056	42.873396
3504.327603	504101.011251	42.878401
3504.379386	504076.053247	42.883405
3504.573943	504060.941251	42.888410
3504.646964	504045.241152	42.893415
3504.484764	504022.796699	42.898420
3504.380352	504009.908072	42.903425
3504.815608	503980.587609	42.908429
3504.738672	503953.271177	42.913434
3504.262970	503937.354059	42.918439
3504.670222	503903.331293	42.923444
3504.435412	503881.454832	42.928449
3504.374053	503872.607999	42.933453
3504.504994	503843.487233	42.938458
3504.387844	503824.274373	42.943463
3504.494857	503799.459074	42.948468
3504.371945	503782.018394	42.953473
3504.642437	503760.669225	42.958477
3504.720060	503740.210870	42.963482
3504.609926	503724.286388	42.968487
3504.602920	503701.412122	42.973492
3504.505756	503666.152783	42.978497
3504.173223	503645.253051	42.983501
3504.589528	503625.348346	42.988506
3504.479503	503598.188421	42.993511
3504.550127	503569.987708	42.998516
3504.480366	503555.524372	43.003521
3504.519246	503544.738363	43.008525
3504.392350	503514.038293	43.013530
3504.510989	503505.770145	43.018535
3504.380326	503470.971198	43.023540
3504.626356	503464.859123	43.028545
3504.210279	503431.674118	43.033549
3504.541813	503404.191053	43.038554
3504.466065	503395.953577	43.043559
3504.293518	503374.319694	43.048564
3504.380228	503361.602825	43.053569
3504.037740	503335.542052	43.058573
3504.110611	503327.028002	43.063578
3503.933782	503322.956516	43.068583
3503.832184	503292.201451	43.073588
3503.921817	503274.423011	43.078593
3503.608812	503270.119984	43.083597
3504.314213	503268.642012	43.088602
3504.132914	503245.086154	43.093607
3504.138921	503227.169053	43.098612
3504.465436	503214.566007	43.103617
3504.085081	503200.961242	43.108621
3504.480999	503188.853315	43.113626
3504.211639	503168.398529	43.118631
3504.203490	503148.206098	43.123636
3504.245501	503122.236070	43.128641
3504.081466	503115.227079	43.133645
3504.192355	503080.743461	43.138650
3504.106359	503089.613990	43.143655
3503.959595	503071.619655	43.148660
3504.315583	503048.839002	43.153665
3504.310641	503046.562286	43.158669
3504.405711	503021.494725	43.163674
3504.350825	502998.728337	43.168679
3504.414100	502985.458177	43.173684
3504.075538	502960.408455	43.178689
3504.020962	502956.469396	43.183693
3504.029408	502942.448698	43.188698
3504.321780	502904.393250	43.193703
3504.178507	502910.843566	43.198708
3504.006505	502878.580562	43.203713
3504.024656	502861.875849	43.208717
3504.045161	502861.214661	43.213722
3503.910391	502854.150329	43.218727
3503.983062	502820.633866	43.223732
3504.097851	502802.699140	43.228737
3503.660664	502807.829429	43.233741
3504.010254	502792.843680	43.238746
3504.162918	502790.592632	43.243751
3504.236674	502773.777824	43.248756
3504.379692	502747.234549	43.253761
3503.930821	502732.425562	43.258765
3504.205796	502712.187884	43.263770
3503.933348	502699.577917	43.268775
3504.044846	502677.139103	43.273780
3504.210088	502671.646870	43.278785
3503.839097	502665.682655	43.283789
3504.026504	502639.891387	43.288794
3503.842926	502643.513881	43.293799
3503.920633	502637.478738	43.298804
3504.218384	502614.048771	43.303809
3503.778558	502605.463571	43.308813
3504.168871	502598.366756	43.313818
3504.163177	502585.208422	43.318823
3504.162561	502574.478675	43.323828
3504.165345	502543.098458	43.328833
3504.029907	502537.046357	43.333837
3504.249719	502520.360061	43.338842
3504.200880	502507.410938	43.343847
3504.211782	502492.832757	43.348852
3504.013497	502465.280136	43.353857
3503.991376	502449.492431	43.358861
3504.152801	502439.344345	43.363866
3504.113375	502435.858291	43.368871
3504.358200	502416.384234	43.373876
3504.732729	502399.673372	43.378881
3504.226189	502373.232202	43.383885
3504.504238	502352.133205	43.388890
3504.408121	502335.850962	43.393895
3504.309606	502319.720923	43.398900
3504.578268	502290.069697	43.403905
3504.112351	502276.730808	43.408909
3504.247176	502258.488684	43.413914
3504.138063	502241.651661	43.418919
3504.408295	502228.601291	43.423924
3504.482995	502214.468318	43.428929
3504.138739	502184.761950	43.433933
3504.252417	502173.254692	43.438938
3504.462843	502149.281164	43.443943
3504.369139	502129.657844	43.448948
3504.458831	502111.473317	43.453953
3504.235767	502096.476264	43.458957
3504.191213	502081.147301	43.463962
3504.206583	502063.278155	43.468967
3504.001726	502034.612396	43.473972
3504.410270	502036.268705	43.478977
3504.095062	502012.529913	43.483981
3504.427898	502007.112215	43.488986
3504.337101	501967.900579	43.493991
3504.206182	501945.195468	43.498996
3504.382373	501927.857524	43.504001
3504.005521	501913.694453	43.509005
3504.180426	501897.672658	43.514010
3504.099708	501904.872669	43.519015
3504.059773	501874.004163	43.524020
3504.254396	501870.177318	43.529025
3504.275704	501856.912946	43.534029
3504.493429	501830.103418	43.539034
3504.267851	501819.864303	43.544039
3504.129466	501796.451577	43.549044
3504.383144	501774.950829	43.554049
3504.173602	501770.782924	43.559053
3504.360868	501734.766171	43.564058
3504.206965	501722.845380	43.569063
3504.029987	501700.653385	43.574068
3504.459753	501694.511662	43.579073
3503.880038	501679.621242	43.584077
3504.314138	501659.002908	43.589082
3503.938063	501641.448283	43.594087
3504.131007	501632.256444	43.599092
3504.687328	501601.698145	43.604097
3504.125233	501603.760987	43.609101
3504.116317	501578.404130	43.614106
3504.326099	501552.557131	43.619111
3504.207290	501545.034214	43.624116
3504.159355	501525.656070	43.629121
3504.036754	501514.388192	43.634125
3503.994948	501502.803844	43.639130
3503.924003	501497.095502	43.644135
3504.072300	501473.940732	43.649140
3504.241867	501461.260020	43.654145
3504.271426	501455.738242	43.659149
3504.636535	501420.401363	43.664154
3504.525801	501416.774532	43.669159
3503.971895	501379.861890	43.674164
3504.352862	501353.076458	43.679169
3504.229501	501352.134257	43.684173
3504.099794	501332.971291	43.689178
3503.924854	501315.283320	43.694183
3503.985949	501313.856417	43.699188
3504.290690	501281.413922	43.704193
3504.118765	501272.127718	43.709197
3504.051771	501256.953439	43.714202
3504.092706	501237.358469	43.719207
3503.957161	501222.296228	43.724212
3504.035452	501221.069065	43.729217
3503.749459	501224.556184	43.734221
3504.044094	501190.343548	43.739226
3504.046252	501180.473000	43.744231
3504.171981	501170.633533	43.749236
3504.427012	501155.307036	43.754241
3504.164354	501145.579558	43.759245
3503.963657	501136.550914	43.764250
3503.984874	501107.291143	43.769255
3503.741058	501098.117444	43.774260
3503.860281	501089.594995	43.779265
3503.875308	501088.377822	43.784269
3504.205913	501066.408510	43.789274
3504.105129	501048.657937	43.794279
3503.870098	501046.417331	43.799284
3504.198205	501036.140867	43.804289
3503.518383	501008.763329	43.809293
3503.873600	500987.144348	43.814298
3504.144656	500986.443489	43.819303
3504.357761	500976.438253	43.824308
3504.060301	500967.880370	43.829313
3503.670223	500949.719869	43.834317
3504.464338	500933.700572	43.839322
3503.926777	500911.564585	43.844327
3504.097313	500907.538872	43.849332
3503.977519	500894.549171	43.854337
3503.966874	500879.719985	43.859341
3504.164561	500870.931943	43.864346
3503.950194	500851.933693	43.869351
3504.117189	500839.354180	43.874356
3504.210014	500816.106089	43.879361
3503.953787	500814.982388	43.884365
3503.803043	500792.582644	43.889370
3504.092892	500769.100881	43.894375
3503.919029	500764.015982	43.899380
3504.097391	500750.979051	43.904385
3503.495807	500742.975306	43.909389
3503.524682	500720.142139	43.914394
3503.900343	500710.566622	43.919399
3504.008049	500704.627317	43.924404
3503.798583	500708.254294	43.929409
3503.830831	500704.351629	43.934413
3503.690988	500669.548635	43.939418
3504.006382	500671.574124	43.944423
3503.629115	500667.533705	43.949428
3503.806733	500650.244912	43.954433
3503.969726	500650.371008	43.959437
3504.122968	500620.988336	43.964442
3504.019693	500624.092366	43.969447
3504.045995	500616.546121	43.974452
3503.992942	500585.626837	43.979457
3503.637624	500574.901328	43.984461
3504.314504	500565.379360	43.989466
3504.324236	500563.960516	43.994471
3503.984336	500540.628606	43.999476
3503.976263	500526.962942	44.004481
3503.984258	500523.114688	44.009485
3503.895377	500491.441629	44.014490
3504.008720	500480.439515	44.019495
3503.969839	500465.057645	44.024500
3504.232711	500453.981262	44.029505
3503.870227	500435.765256	44.034509
3504.362704	500424.753803	44.039514
3503.938282	500420.670162	44.044519
3503.826197	500415.929729	44.049524
3504.006981	500397.324106	44.054529
3504.332315	500392.514531	44.059533
3503.929302	500367.066384	44.064538
3503.717867	500350.901787	44.069543
3504.094613	500345.375410	44.074548
3504.340122	500336.883261	44.079553
3504.045027	500326.957986	44.084557
3503.810366	500310.240216	44.089562
3503.998957	500304.794184	44.094567
3503.915795	500287.546258	44.099572
3504.141228	500260.125725	44.104577
3503.810029	500259.671886	44.109581
3503.883026	500241.791805	44.114586
3503.922902	500216.526537	44.119591
3504.092469	500210.172338	44.124596
3503.954469	500201.993836	44.129601
3503.550902	500212.181475	44.134605
3503.884338	500181.807836	44.139610
3503.662573	500162.000110	44.144615
3503.765617	500168.817441	44.149620
3503.933162	500163.627790	44.154625
3503.984376	500164.834564	44.159629
3503.854013	500131.800701	44.164634
3503.903198	500132.602843	44.169639
3503.977673	500119.126297	44.174644
3504.236286	500108.809667	44.179649
3503.960134	500085.365847	44.184653
3503.916626	500072.565969	44.189658
3504.242877	500073.324321	44.194663
3503.647066	500060.054913	44.199668
3504.128126	500032.492389	44.204673
3503.784056	500036.039537	44.209677
3504.124383	500009.460996	44.214682
3503.815024	500002.170024	44.219687
3503.827123	499969.012103	44.224692
3504.124302	499971.749232	44.229697
3503.915888	499974.414412	44.234701
3504.194873	499939.240078	44.239706
3504.105831	499927.105352	44.244711
3503.792022	499917.385288	44.249716
3503.958072	499913.511922	44.254721
3503.701564	499894.468692	44.259725
3503.638505	499878.077736	44.264730
3503.732053	499878.721017	44.269735
3503.790926	499878.762336	44.274740
3504.101260	499866.311345	44.279745
3503.721532	499852.400186	44.284749
3503.900435	499843.918331	44.289754
3503.786146	499834.925990	44.294759
3503.765545	499832.651337	44.299764
3503.944051	499803.263330	44.304769
3504.027446	499788.924580	44.309773
3504.270949	499784.735222	44.314778
3504.220926	499778.010614	44.319783
3504.236081	499750.976881	44.324788
3504.246557	499743.685872	44.329793
3504.092249	499720.677901	44.334797
3504.093731	499708.984306	44.339802
3504.326997	499693.103171	44.344807
3503.999674	499679.183595	44.349812
3503.751752	499664.846491	44.354817
3503.530861	499673.132593	44.359821
3503.907398	499653.685326	44.364826
3503.894396	499658.243257	44.369831
3503.995457	499634.536742	44.374836
3503.859965	499606.109217	44.379841
3503.610110	499621.588092	44.384845
3503.970712	499609.837671	44.389850
3504.162404	499589.255269	44.394855
3504.120826	499568.152882	44.399860
3504.290490	499579.363938	44.404865
3504.020195	499552.425644	44.409869
3504.059403	499530.702991	44.414874
3504.238705	499539.330870	44.419879
3504.126224	499503.559481	44.424884
3504.232444	499487.850110	44.429889
3504.012364	499485.100729	44.434893
3503.979039	499454.024508	44.439898
3503.858922	499441.843745	44.444903
3503.889433	499436.776786	44.449908
3504.082919	499425.811979	44.454913
3503.958977	499407.405358	44.459917
3504.144004	499389.962314	44.464922
3503.865062	499384.033063	44.469927
3503.912144	499375.369336	44.474932
3504.022465	499355.660095	44.479937
3503.877243	499341.660852	44.484941
3503.661147	499339.518279	44.489946
3504.106934	499342.940720	44.494951
3503.923028	499319.228208	44.499956
3504.026417	499301.797982	44.504961
3504.006852	499301.750457	44.509965
3504.210044	499279.242255	44.514970
3504.203910	499262.639251	44.519975
3503.971663	499252.703445	44.524980
3504.472140	499232.729915	44.529985
3504.117343	499209.196135	44.534989
3503.949036	499203.603692	44.539994
3504.011822	499169.879441	44.544999
3504.023492	499162.992984	44.550004
3504.374966	499150.838730	44.555009
3504.038733	499144.412232	44.560013
3504.058023	499114.592664	44.565018
3504.055097	499098.191491	44.570023
3504.138940	499102.784878	44.575028
3504.302331	499064.032914	44.580033
3504.414036	499065.635181	44.585037
3504.267681	499030.576919	44.590042
3504.255216	499021.669321	44.595047
3503.979005	499016.346987	44.600052
3504.220382	498986.593350	44.605057
3504.003169	498972.858311	44.610061
3504.079647	498971.530037	44.615066
3504.200044	498937.188771	44.620071
3503.734687	498926.175927	44.625076
3503.941887	498911.513172	44.630081
3503.723303	498909.978415	44.635085
3503.938472	498878.811301	44.640090
3503.953217	498868.532505	44.645095
3503.949069	498859.674135	44.650100
3504.039163	498840.878742	44.655105
3503.853869	498837.617532	44.660109
3504.209094	498815.034096	44.665114
3504.256143	498803.889565	44.670119
3503.953341	498799.634456	44.675124
3503.993911	498774.265803	44.680129
3503.974177	498779.533747	44.685133
3504.100837	498747.722293	44.690138
3504.146048	498736.831127	44.695143
3504.019783	498732.699970	44.700148
3504.241765	498717.781604	44.705153
3504.086907	498693.709312	44.710157
3504.129847	498681.198519	44.715162
3504.190527	498660.787633	44.720167
3504.206676	498647.116709	44.725172
3504.135348	498640.091300	44.730177
3504.160417	498619.230383	44.735181
3503.999262	498593.943983	44.740186
3504.227638	498597.805922	44.745191
3503.847086	498580.400864	44.750196
3504.051747	498564.523257	44.755201
3504.060547	498545.537909	44.760205
3504.108346	498537.683649	44.765210
3503.970626	498514.215895	44.770215
3503.758391	498506.858337	44.775220
3503.961849	498487.740914	44.780225
3503.764996	498489.341379	44.785229
3503.987746	498474.523939	44.790234
3504.052099	498461.199622	44.795239
3503.938580	498452.307715	44.800244
3503.874886	498443.205431	44.805249
3503.816590	498421.496850	44.810253
3504.005583	498405.317833	44.815258
3503.813843	498391.578324	44.820263
3503.654306	498389.781068	44.825268
3503.715950	498391.948176	44.830273
3504.120914	498386.366118	44.835277
3503.832515	498359.023901	44.840282
3503.826815	498350.621146	44.845287
3503.563466	498354.915229	44.850292
3503.921076	498347.062543	44.855297
3503.598035	498321.598850	44.860301
3503.737872	498299.555059	44.865306
3503.830984	498305.919046	44.870311
3504.020075	498306.041038	44.875316
3503.761022	498293.071461	44.880321
3503.921170	498269.353810	44.885325
3503.712125	498261.590650	44.890330
3503.883241	498267.436075	44.895335
3503.705648	498260.731062	44.900340
3504.072665	498239.258787	44.905345
3503.859429	498224.560678	44.910349
3503.587464	498215.339323	44.915354
3504.109434	498200.119990	44.920359
3504.091788	498205.387771	44.925364
3503.689625	498177.708886	44.930369
3503.934372	498170.683962	44.935373
3503.953656	498177.565913	44.940378
3503.763055	498155.776675	44.945383
3503.647749	498143.898021	44.950388
3504.034192	498117.663776	44.955393
3503.582246	498128.720861	44.960397
3503.622830	498120.411934	44.965402
3503.876881	498110.044258	44.970407
3503.894065	498094.803371	44.975412
3503.953959	498080.011348	44.980417
3503.782278	498082.063497	44.985421
3503.923401	498061.234217	44.990426
3504.102905	498051.840170	44.995431
3503.843667	498046.109863	45.000436
3504.180050	498024.237172	45.005441
3503.987508	498014.243780	45.010445
3503.898844	498001.854568	45.015450
3503.925934	497984.890758	45.020455
3503.927733	497975.879138	45.025460
3503.888008	497971.582251	45.030465
3503.683124	497956.882603	45.035469
3503.807978	497932.866335	45.040474
3504.016396	497923.315775	45.045479
3503.593382	497924.698907	45.050484
3504.059580	497912.373811	45.055489
3503.528901	497898.484994	45.060493
3503.719112	497888.684164	45.065498
3503.912931	497878.477753	45.070503
3503.966340	497884.898790	45.075508
3503.838243	497860.770530	45.080513
3503.914840	497845.975676	45.085517
3503.927479	497838.886058	45.090522
3504.224339	497835.143450	45.095527
3504.045277	497825.603456	45.100532
3503.793109	497797.140890	45.105537
3503.620476	497798.737587	45.110541
3503.245353	497792.721759	45.115546
3503.531054	497790.702191	45.120551
3503.460759	497801.091640	45.125556
3503.545624	497785.789170	45.130561
3503.560840	497758.347428	45.135565
3503.491118	497745.094402	45.140570
3503.683631	497745.722118	45.145575
3503.623527	497745.731622	45.150580
3503.958803	497747.045541	45.155585
3503.916605	497743.964018	45.160589
3503.700362	497732.556683	45.165594
3504.087458	497700.904728	45.170599
3503.650797	497705.884498	45.175604
3503.779473	497699.485253	45.180609
3503.867544	497693.244302	45.185613
3503.648447	497675.407839	45.190618
3504.302773	497658.293958	45.195623
3503.873446	497656.589895	45.200628
3503.720591	497650.994527	45.205633
3504.147640	497622.069946	45.210637
3503.794645	497627.441526	45.215642
3504.060539	497611.148391	45.220647
3503.497656	497606.832854	45.225652
3503.782356	497594.941242	45.230657
3503.955247	497580.384084	45.235661
3503.878479	497556.297931	45.240666
3504.094109	497559.858349	45.245671
3503.579712	497566.217365	45.250676
3503.646125	497530.160650	45.255681
3504.113959	497517.885655	45.260685
3503.885823	497513.112171	45.265690
3503.625899	497515.380837	45.270695
3503.774586	497506.497647	45.275700
3504.197175	497476.105360	45.280705
3503.514830	497478.187663	45.285709
3503.614961	497467.590813	45.290714
3503.876311	497455.652174	45.295719
3503.533490	497455.098840	45.300724
3503.798015	497437.084449	45.305729
3504.081681	497424.230975	45.310733
3504.002919	497422.775243	45.315738
3504.119736	497416.630908	45.320743
3503.939208	497394.130380	45.325748
3503.991452	497379.541502	45.330753
3503.896286	497389.023830	45.335757
3503.664177	497373.821738	45.340762
3503.809277	497344.435007	45.345767
3503.825074	497335.724619	45.350772
3504.084434	497332.494109	45.355777
3503.768372	497331.885914	45.360781
3503.889952	497312.830819	45.365786
3503.846272	497292.384256	45.370791
3503.977051	497290.389120	45.375796
3504.077315	497283.386689	45.380801
3503.829822	497271.882748	45.385805
3503.424335	497257.467375	45.390810
3503.721866	497233.726653	45.395815
3503.701212	497244.817362	45.400820
3503.536480	497245.197796	45.405825
3503.763388	497231.036840	45.410829
3503.508074	497236.443724	45.415834
3503.426513	497211.395946	45.420839
3503.470757	497193.112364	45.425844
3503.520445	497184.295291	45.430849
3503.403549	497190.642237	45.435853
3503.626796	497190.252562	45.440858
3503.824805	497190.778175	45.445863
3503.605701	497203.317851	45.450868
3503.978730	497184.121623	45.455873
3503.600886	497171.473782	45.460877
3503.112570	497155.400703	45.465882
3503.476791	497152.710493	45.470887
3503.369067	497152.119990	45.475892
3503.677336	497136.781661	45.480897
3503.825867	497147.744432	45.485901
3503.309321	497139.016835	45.490906
3503.877103	497135.990681	45.495911
3503.531809	497140.449886	45.500916
3503.720604	497115.713639	45.505921
3503.784923	497106.236053	45.510925
3503.802806	497107.650814	45.515930
3503.842872	497098.227685	45.520935
3503.760271	497091.203455	45.525940
3503.919382	497075.382370	45.530945
3503.777299	497075.607344	45.535949
3503.819922	497062.943598	45.540954
3503.956650	497051.935696	45.545959
3503.907188	497044.045533	45.550964
3504.134432	497025.580973	45.555969
3503.960587	496995.484666	45.560973
3503.957156	496996.295264	45.565978
3504.436867	496979.309601	45.570983
3503.922659	496967.037569	45.575988
3503.943938	496944.960241	45.580993
3504.097434	496938.911204	45.585997
3503.919075	496928.307428	45.591002
3504.105613	496908.887243	45.596007
3503.880083	496903.961300	45.601012
3504.009766	496877.057046	45.606017
3503.892505	496876.366784	45.611021
3503.871770	496874.294293	45.616026
3503.841867	496869.033649	45.621031
3503.481132	496840.586739	45.626036
3503.723727	496815.942839	45.631041
3503.933078	496810.036817	45.636045
3503.575844	496807.916247	45.641050
3503.840798	496809.494494	45.646055
3503.504558	496815.420581	45.651060
3503.540972	496784.328744	45.656065
3503.852097	496769.090912	45.661069
3503.714724	496772.302248	45.666074
3503.552565	496772.581028	45.671079
3503.823632	496776.284725	45.676084
3503.886579	496775.211573	45.681089
3503.716908	496757.771426	45.686093
3503.608220	496737.131997	45.691098
3503.886575	496718.405902	45.696103
3503.580868	496724.884112	45.701108
3503.796466	496718.369524	45.706113
3503.853768	496719.524939	45.711117
3503.725354	496696.509018	45.716122
3503.797140	496687.738841	45.721127
3503.675819	496691.302058	45.726132
3503.901205	496685.140316	45.731137
3504.098114	496673.413866	45.736141
3503.592961	496660.076982	45.741146
3503.913859	496635.724236	45.746151
3503.402256	496637.222722	45.751156
3503.495703	496635.486562	45.756161
3503.627866	496642.148738	45.761165
3503.875869	496634.616414	45.766170
3503.952823	496597.138561	45.771175
3503.646733	496599.769043	45.776180
3503.713858	496592.366549	45.781185
3503.821954	496593.108909	45.786189
3503.460426	496596.861999	45.791194
3503.657957	496569.642790	45.796199
3503.567907	496561.252538	45.801204
3503.559804	496543.837277	45.806209
3503.546051	496543.839455	45.811213
3503.763053	496535.198141	45.816218
3504.199329	496539.736476	45.821223
3503.557977	496535.382452	45.826228
3503.414966	496512.976159	45.831233
3503.583027	496503.836269	45.836237
3503.584259	496496.950448	45.841242
3503.812399	496499.901542	45.846247
3503.499695	496499.900342	45.851252
3503.456562	496500.767868	45.856257
3503.608919	496504.034717	45.861261
3503.462928	496507.652499	45.866266
3503.424294	496483.356377	45.871271
3503.826366	496470.129108	45.876276
3504.056213	496460.371874	45.881281
3504.070673	496454.952209	45.886285
3504.148488	496450.332605	45.891290
3504.073523	496432.370878	45.896295
3503.820969	496422.841760	45.901300
3504.130862	496394.288154	45.906305
3503.694442	496378.661851	45.911309
3503.769619	496370.447915	45.916314
3503.828944	496361.578291	45.921319
3503.613368	496364.346389	45.926324
3503.992906	496358.058912	45.931329
3503.698798	496339.372280	45.936333
3503.411619	496332.329461	45.941338
3503.796037	496314.851941	45.946343
3503.871925	496328.965758	45.951348
3503.970288	496312.191640	45.956353
3503.698325	496305.500817	45.961357
3503.615394	496282.527813	45.966362
3503.714641	496270.107716	45.971367
3503.491948	496276.066660	45.976372
3503.924434	496273.061752	45.981377
3503.891275	496260.713207	45.986381
3504.060973	496259.218110	45.991386
3503.804350	496224.222468	45.996391
3503.697229	496218.923210	46.001396
3503.530810	496221.227887	46.006401
3503.661937	496229.459922	46.011405
3503.580074	496213.726806	46.016410
3503.912148	496181.929013	46.021415
3503.924552	496182.787776	46.026420
3503.953862	496174.479740	46.031425
3504.223510	496173.373883	46.036429
3504.025479	496149.558185	46.041434
3504.163341	496143.156940	46.046439
3504.084282	496134.562231	46.051444
3504.197796	496113.178145	46.056449
3504.026856	496092.598455	46.061453
3504.111603	496085.699278	46.066458
3503.943485	496070.334088	46.071463
3503.841158	496063.464471	46.076468
3503.766442	496053.350111	46.081473
3503.966843	496036.964659	46.086477
3503.989756	496027.594318	46.091482
3504.243492	496001.884307	46.096487
3503.948261	495999.450054	46.101492
3503.798848	495993.701736	46.106497
3503.768229	495978.770415	46.111501
3503.568140	495968.827718	46.116506
3503.951988	495961.071121	46.121511
3503.895322	495971.054413	46.126516
3503.862602	495944.123819	46.131521
3503.940439	495917.327605	46.136525
3503.943459	495909.631179	46.141530
3503.855162	495904.278223	46.146535
3503.819328	495902.309270	46.151540
3503.796578	495883.680543	46.156545
3503.743762	495865.056548	46.161549
3503.791040	495871.276741	46.166554
3504.065002	495853.512450	46.171559
3503.858398	495845.849130	46.176564
3503.694688	495837.723343	46.181569
3503.959982	495814.745342	46.186573
3503.643572	495812.770095	46.191578
3503.762108	495807.181893	46.196583
3503.753350	495806.575703	46.201588
3503.679072	495783.145017	46.206593
3503.753129	495774.728464	46.211597
3503.579516	495760.730935	46.216602
3504.103715	495766.166940	46.221607
3503.835813	495752.690625	46.226612
3503.733776	495724.504870	46.231617
3503.978638	495717.934670	46.236621
3503.789103	495717.306418	46.241626
3504.062028	495703.643322	46.246631
3503.794144	495686.977149	46.251636
3503.893457	495673.189575	46.256641
3504.074349	495658.528353	46.261645
3503.674719	495675.097538	46.266650
3504.152361	495642.263160	46.271655
3503.635785	495629.788067	46.276660
3503.777472	495623.284772	46.281665
3504.000854	495615.097704	46.286669
3503.982645	495600.974226	46.291674
3503.826185	495593.252242	46.296679
3503.795748	495586.269818	46.301684
3503.899220	495573.139729	46.306689
3504.200689	495562.408684	46.311693
3503.633555	495546.194739	46.316698
3504.080608	495532.503993	46.321703
3503.951520	495535.815502	46.326708
3503.924626	495523.465468	46.331713
3504.098690	495491.944611	46.336717
3504.018628	495488.666161	46.341722
3504.051348	495471.395322	46.346727
3503.624151	495454.450321	46.351732
3503.839268	495436.644294	46.356737
3503.984009	495440.064437	46.361741
3504.066130	495444.102068	46.366746
3503.911779	495418.000044	46.371751
3503.815437	495395.736900	46.376756
3503.904191	495394.153262	46.381761
3504.008899	495381.681066	46.386765
3504.079083	495369.011787	46.391770
3504.148602	495344.697054	46.396775
3503.763808	495346.378129	46.401780
3503.813931	495336.901867	46.406785
3504.000537	495312.315421	46.411789
3503.677544	495319.050022	46.416794
3503.910132	495301.342368	46.421799
3503.921448	495309.543123	46.426804
3503.818089	495290.318935	46.431809
3503.976519	495262.243198	46.436813
3503.878850	495265.397890	46.441818
3503.716011	495252.157764	46.446823
3503.797633	495249.360047	46.451828
3503.676669	495231.505674	46.456833
3503.973396	495212.775134	46.461837
3503.760907	495227.948047	46.466842
3503.835318	495210.771638	46.471847
3503.409787	495215.345256	46.476852
3503.146366	495193.817139	46.481857
3503.376130	495175.957911	46.486861
3502.969723	495185.085511	46.491866
3503.379203	495189.729689	46.496871
3503.429618	495207.645895	46.501876
3503.252114	495192.585248	46.506881
3503.598244	495187.568483	46.511885
3503.656471	495165.179361	46.516890
3503.303299	495162.602253	46.521895
3503.408720	495167.395762	46.526900
3503.296487	495168.578072	46.531905
3503.913357	495155.062738	46.536909
3503.713268	495151.448765	46.541914
3503.990464	495150.291022	46.546919
3503.637929	495137.890931	46.551924
3503.651358	495120.116475	46.556929
3503.800661	495112.194058	46.561933
3503.598431	495116.884307	46.566938
3503.712706	495118.385253	46.571943
3503.847493	495116.642415	46.576948
3503.779901	495080.551399	46.581953
3503.636925	495056.826840	46.586957
3503.581111	495069.949774	46.591962
3503.865876	495059.221076	46.596967
3503.533200	495052.792556	46.601972
3503.418444	495054.633509	46.606977
3503.828417	495033.859541	46.611981
3503.655103	495029.532440	46.616986
3503.799580	495020.699340	46.621991
3503.572297	495019.064354	46.626996
3503.747658	495009.618762	46.632001
3503.608583	495011.615466	46.637005
3503.460357	495004.702071	46.642010
3503.947849	494983.510723	46.647015
3503.403912	494985.925857	46.652020
3503.449106	494978.222373	46.657025
3503.648889	494959.608165	46.662029
3503.514403	494974.262620	46.667034
3503.488359	494968.848916	46.672039
3503.690810	494962.639586	46.677044
3503.967772	494964.368001	46.682049
3504.091457	494943.386011	46.687053
3503.676553	494933.122265	46.692058
3503.683687	494910.335835	46.697063
3503.949675	494909.078581	46.702068
3503.854330	494904.283420	46.707073
3503.982526	494881.528454	46.712077
3503.613149	494888.321178	46.717082
3503.612597	494870.852495	46.722087
3503.505426	494868.793438	46.727092
3503.763848	494865.714547	46.732097
3503.803200	494847.885095	46.737101
3503.390801	494841.418467	46.742106
3503.868854	494825.038680	46.747111
3503.462966	494826.419329	46.752116
3503.689835	494828.763286	46.757121
3503.672827	494822.943037	46.762125
3503.526817	494833.548682	46.767130
3503.659157	494804.514316	46.772135
3503.736943	494786.020483	46.777140
3503.305853	494783.202464	46.782145
3503.735148	494770.476012	46.787149
3503.368128	494775.597469	46.792154
3503.458550	494779.076956	46.797159
3503.431169	494773.157061	46.802164
3503.205504	494784.889282	46.807169
3503.674701	494775.599664	46.812173
3503.435791	494783.992107	46.817178
3503.604954	494774.446105	46.822183
3503.376710	494752.760006	46.827188
3503.386862	494745.011328	46.832193
3503.467400	494735.631218	46.837197
3503.362881	494742.837844	46.842202
3503.551824	494726.098589	46.847207
3503.794547	494717.705526	46.852212
3503.538333	494721.948696	46.857217
3503.758018	494727.585048	46.862221
3503.471559	494723.883372	46.867226
3503.440886	494724.850281	46.872231
3503.635969	494725.376431	46.877236
3503.523311	494698.102196	46.882241
3503.865299	494689.237718	46.887245
3503.685035	494689.114311	46.892250
3503.849705	494683.214667	46.897255
3503.794232	494671.780000	46.902260
3503.663760	494670.230950	46.907265
3503.599408	494639.353928	46.912269
3503.831134	494650.153149	46.917274
3503.965594	494626.131007	46.922279
3503.571259	494647.966303	46.927284
3503.569036	494631.763525	46.932289
3504.192523	494613.284536	46.937293
3503.628429	494602.588470	46.942298
3503.663670	494589.721636	46.947303
3504.142420	494588.734542	46.952308
3503.541714	494577.841708	46.957313
3503.768525	494549.905978	46.962317
3503.534879	494550.955612	46.967322
3503.831822	494536.325786	46.972327
3503.823526	494550.201107	46.977332
3503.645304	494539.393380	46.982337
3503.842411	494531.159347	46.987341
3503.488810	494514.049936	46.992346
3503.579606	494497.984243	46.997351
3503.919839	494496.208875	47.002356
3503.700444	494485.154447	47.007361
3503.608841	494478.485079	47.012365
3503.401564	494493.353964	47.017370
3503.654909	494486.579443	47.022375
3503.785223	494473.900042	47.027380
3503.646337	494459.794758	47.032385
3503.907651	494449.170682	47.037389
3503.567941	494451.502969	47.042394
3503.764846	494447.370390	47.047399
3503.613747	494444.811875	47.052404
3503.654886	494426.171566	47.057409
3503.824871	494407.156425	47.062413
3503.353273	494417.003605	47.067418
3503.948777	494408.655913	47.072423
3503.669851	494404.294721	47.077428
3503.821125	494395.915965	47.082433
3503.782256	494382.098626	47.087437
3503.605906	494367.189024	47.092442
3503.909289	494373.166706	47.097447
3503.941204	494368.503196	47.102452
3503.770679	494363.112150	47.107457
3503.649235	494339.028809	47.112461
3503.575906	494329.976625	47.117466
3503.578392	494320.558004	47.122471
3503.773545	494310.855747	47.127476
3503.534938	494311.197279	47.132481
3503.703584	494303.068915	47.137485
3503.663677	494294.619059	47.142490
3503.495045	494278.138457	47.147495
3503.575364	494274.783804	47.152500
3503.874539	494274.483343	47.157505
3503.688618	494262.056323	47.162509
3503.559376	494277.621949	47.167514
3503.835624	494260.817836	47.172519
3503.410686	494246.149970	47.177524
3503.544190	494234.330710	47.182529
3503.555410	494228.758990	47.187533
3503.275366	494221.663591	47.192538
3503.576947	494218.982859	47.197543
3503.621536	494223.583686	47.202548
3503.553499	494224.860343	47.207553
3503.760009	494218.194398	47.212557
3503.448192	494222.547743	47.217562
3503.737134	494208.020193	47.222567
3503.675002	494182.003104	47.227572
3503.385264	494194.657277	47.232577
3503.764737	494172.013624	47.237581
3503.834097	494176.408004	47.242586
3503.410020	494181.943732	47.247591
3503.582004	494177.612488	47.252596
3503.514238	494168.356800	47.257601
3503.825693	494157.673995	47.262605
3503.374182	494140.883528	47.267610
3503.573342	494133.965534	47.272615
3503.784425	494140.616150	47.277620
3503.515488	494133.772142	47.282625
3504.099352	494120.919539	47.287629
3503.882959	494123.029830	47.292634
3503.810473	494093.722900	47.297639
3503.889742	494083.735022	47.302644
3503.783103	494088.461059	47.307649
3503.856625	494080.853994	47.312653
3503.768202	494056.714428	47.317658
3504.026510	494045.584230	47.322663
3504.181958	494043.534208	47.327668
3503.915933	494020.891123	47.332673
3503.983244	494007.512448	47.337677
3503.851154	494001.456945	47.342682
3503.833014	493984.699111	47.347687
3503.543026	493997.100275	47.352692
3503.802359	493964.803772	47.357697
3503.971256	493953.130647	47.362701
3503.654383	493946.800513	47.367706
3503.641787	493933.029320	47.372711
3503.709892	493942.487628	47.377716
3503.671286	493939.658078	47.382721
3503.667546	493920.062252	47.387725
3503.741034	493915.037600	47.392730
3503.622610	493899.662732	47.397735
3503.863826	493901.143715	47.402740
3503.636412	493895.913433	47.407745
3503.805477	493882.721132	47.412749
3503.403592	493860.960151	47.417754
3503.812993	493847.375379	47.422759
3503.627549	493855.101513	47.427764
3503.294773	493853.888191	47.432769
3503.796921	493853.505005	47.437773
3503.658951	493848.766942	47.442778
3503.846451	493849.395591	47.447783
3503.660634	493824.157101	47.452788
3503.654872	493805.726125	47.457793
3503.534862	493790.857788	47.462797
3503.613104	493802.036228	47.467802
3503.423907	493797.103700	47.472807
3503.710522	493795.589926	47.477812
3503.527986	493797.644266	47.482817
3503.657585	493776.558736	47.487821
3503.829254	493765.745887	47.492826
3503.388095	493761.106360	47.497831
3503.793465	493763.118418	47.502836
3503.660088	493759.645536	47.507841
3503.849045	493749.842689	47.512845
3503.524880	493769.743718	47.517850
3503.851409	493736.220901	47.522855
3503.784662	493726.053359	47.527860
3503.587144	493728.667085	47.532865
3503.941308	493720.964878	47.537869
3503.753193	493723.880942	47.542874
3503.677850	493697.004422	47.547879
3503.611056	493677.418304	47.552884
3503.761274	493681.394923	47.557889
3503.941114	493663.896581	47.562893
3503.691297	493671.734241	47.567898
3503.784380	493660.427376	47.572903
3503.961514	493641.967329	47.577908
3503.607764	493625.717951	47.582913
3503.825762	493628.215378	47.587917
3503.630434	493626.879041	47.592922
3504.081880	493604.628418	47.597927
3503.952965	493595.027644	47.602932
3503.592654	493571.639344	47.607937
3503.558356	493572.404335	47.612941
3503.669841	493574.969242	47.617946
3503.507925	493554.638463	47.622951
3503.714110	493568.075522	47.627956
3503.429161	493549.435229	47.632961
3503.933273	493521.403473	47.637965
3503.619348	493536.543174	47.642970
3503.437755	493519.456287	47.647975
3503.732519	493523.308817	47.652980
3503.495534	493520.561196	47.657985
3503.623854	493524.186845	47.662989
3503.687577	493501.693553	47.667994
3503.452418	493486.691257	47.672999
3503.419412	493473.479965	47.678004
3503.433117	493478.693516	47.683009
3503.483986	493481.369293	47.688013
3503.188664	493467.693078	47.693018
3503.505623	493476.504635	47.698023
3503.707707	493468.319980	47.703028
3503.635792	493476.737260	47.708033
3503.990937	493479.567496	47.713037
3503.676179	493443.461695	47.718042
3503.596185	493437.549686	47.723047
3503.598927	493415.724223	47.728052
3503.402743	493423.907978	47.733057
3503.646251	493413.691226	47.738061
3503.465964	493431.949456	47.743066
3503.528376	493432.952358	47.748071
3503.573871	493424.792433	47.753076
3503.459407	493407.846747	47.758081
3503.368232	493378.389718	47.763085
3503.061327	493384.160353	47.768090
3503.458783	493375.387756	47.773095
3503.664721	493378.444145	47.778100
3503.476957	493381.461484	47.783105
3503.375415	493381.629452	47.788109
3503.542589	493375.728995	47.793114
3503.880718	493365.750452	47.798119
3503.801520	493376.346375	47.803124
3503.456138	493363.235016	47.808129
3503.762132	493351.337289	47.813133
3503.784079	493337.104447	47.818138
3503.670896	493331.501480	47.823143
3503.351013	493336.058860	47.828148
3503.771986	493332.143810	47.833153
3503.785244	493326.014472	47.838157
3503.799100	493329.101229	47.843162
3503.779377	493303.987689	47.848167
3503.940510	493284.466406	47.853172
3503.601733	493298.040436	47.858177
3503.615161	493284.062092	47.863181
3503.642965	493281.829606	47.868186
3503.727900	493263.890139	47.873191
3503.788248	493246.511566	47.878196
3503.750476	493247.479674	47.883201
3503.811989	493240.988211	47.888205
3503.646624	493243.596923	47.893210
3503.728335	493224.847709	47.898215
3503.708325	493208.393298	47.903220
3503.417994	493199.172301	47.908225
3503.742857	493199.171597	47.913229
3503.707593	493195.075436	47.918234
3503.815974	493188.424631	47.923239
3503.828798	493182.953619	47.928244
3503.456708	493170.454009	47.933249
3503.649208	493154.016599	47.938253
3503.449023	493144.224299	47.943258
3503.846275	493144.617265	47.948263
3504.052566	493142.711024	47.953268
3503.906848	493134.530555	47.958273
3503.890918	493105.567587	47.963277
3503.689546	493098.206123	47.968282
3503.772700	493107.004173	47.973287
3503.676622	493098.258814	47.978292
3503.638002	493092.289516	47.983297
3503.711968	493059.970090	47.988301
3503.853854	493054.428002	47.993306
3503.814962	493058.991676	47.998311
3503.763078	493056.670481	48.003316
3503.668153	493046.810853	48.008321
3503.569558	493028.596331	48.013325
3503.662441	493016.326960	48.018330
3503.684771	493004.676403	48.023335
3503.759293	493001.879467	48.028340
3503.627803	492999.975961	48.033345
3503.752819	492997.221684	48.038349
3503.739031	493001.072454	48.043354
3503.473633	492962.932339	48.048359
3503.625042	492951.818380	48.053364
3503.539896	492965.099368	48.058369
3503.830606	492954.216590	48.063373
3503.800634	492956.652024	48.068378
3503.626166	492959.768608	48.073383
3503.736440	492939.495409	48.078388
3503.610350	492923.715823	48.083393
3503.782166	492923.435473	48.088397
3503.547386	492921.143169	48.093402
3503.362819	492909.829091	48.098407
3503.373822	492903.953168	48.103412
3503.400133	492919.799189	48.108417
3503.571969	492909.998604	48.113421
3503.557898	492913.646880	48.118426
3503.461806	492899.229799	48.123431
3503.433615	492876.193239	48.128436
3503.493543	492863.878335	48.133441
3503.467901	492856.590279	48.138445
3503.490056	492865.448725	48.143450
3503.693655	492869.518361	48.148455
3504.067693	492864.597838	48.153460
3503.188654	492862.964393	48.158465
3503.551294	492872.781813	48.163469
3503.490445	492859.371924	48.168474
3503.487055	492841.142169	48.173479
3503.710118	492831.536005	48.178484
3503.448015	492823.829552	48.183489
3503.503036	492803.767496	48.188493
3503.458961	492819.979207	48.193498
3503.331893	492830.988126	48.198503
3503.639629	492803.796559	48.203508
3503.174335	492802.198992	48.208513
3503.570816	492808.820787	48.213517
3503.293156	492818.992639	48.218522
3503.223219	492810.496210	48.223527
3503.728254	492810.163191	48.228532
3503.553320	492807.658854	48.233537
3503.789610	492802.051129	48.238541
3503.935374	492789.368130	48.243546
3503.269717	492781.370965	48.248551
3503.773953	492772.125448	48.253556
3503.860835	492772.111720	48.258561
3503.677132	492772.140760	48.263565
3503.629119	492738.017014	48.268570
3503.717975	492728.685209	48.273575
3503.894805	492719.542055	48.278580
3503.713836	492730.610194	48.283585
3503.959669	492711.176199	48.288589
3503.799189	492694.996733	48.293594
3503.305553	492687.630659	48.298599
3503.848625	492675.846948	48.303604
3503.629749	492667.171434	48.308609
3503.721069	492676.879922	48.313613
3503.929010	492683.227721	48.318618
3504.185471	492651.486420	48.323623
3503.742130	492635.604812	48.328628
3503.501308	492623.489205	48.333633
3503.745380	492622.539106	48.338637
3503.921573	492618.156193	48.343642
3503.649517	492606.551916	48.348647
3503.616979	492592.630955	48.353652
3503.511928	492595.584707	48.358657
3503.655421	492582.547443	48.363661
3503.738475	492586.433633	48.368666
3503.845821	492578.820605	48.373671
3503.699186	492567.601603	48.378676
3503.881293	492559.318423	48.383681
3504.226994	492535.969141	48.388685
3504.075194	492533.207907	48.393690
3503.794236	492520.541531	48.398695
3504.108018	492494.310726	48.403700
3503.829629	492490.404759	48.408705
3503.934388	492475.955603	48.413709
3503.626303	492468.965239	48.418714
3503.763453	492444.028301	48.423719
3504.042366	492443.427171	48.428724
3503.422439	492439.524535	48.433729
3503.814765	492436.626642	48.438733
3503.859524	492432.112537	48.443738
3503.706779	492412.437383	48.448743
3503.671799	492408.543566	48.453748
3503.614073	492396.095025	48.458753
3503.703108	492399.777746	48.463757
3503.646211	492402.521353	48.468762
3503.655514	492389.100036	48.473767
3503.837816	492353.318668	48.478772
3503.400427	492367.010247	48.483777
3503.766987	492345.581788	48.488781
3503.836212	492351.445215	48.493786
3503.409031	492355.361460	48.498791
3503.615957	492349.960805	48.503796
3503.453066	492350.087837	48.508801
3503.575724	492311.682481	48.513805
3503.374870	492306.700754	48.518810
3503.219097	492299.838176	48.523815
3503.720226	492291.504454	48.528820
3503.448227	492303.853266	48.533825
3503.524988	492300.194970	48.538829
3503.563583	492298.061944	48.543834
3503.626762	492300.432099	48.548839
3503.635773	492305.798646	48.553844
3503.592025	492299.374133	48.558849
3503.762512	492279.597107	48.563853
3503.266343	492262.153648	48.568858
3503.570180	492251.622874	48.573863
3503.780597	492244.094700	48.578868
3503.589092	492248.986543	48.583873
3503.737608	492245.418178	48.588877
3503.652536	492243.405975	48.593882
3503.456304	492248.501131	48.598887
3503.571137	492230.809145	48.603892
3503.391145	492223.950367	48.608897
3503.759438	492213.814514	48.613901
3503.549542	492220.633647	48.618906
3503.643994	492211.047490	48.623911
3504.132657	492219.072888	48.628916
3503.505068	492204.637991	48.633921
3503.607276	492180.769693	48.638925
3503.787247	492168.131505	48.643930
3504.005780	492164.754624	48.648935
3503.893032	492162.291012	48.653940
3503.877825	492163.863309	48.658945
3504.158037	492134.092391	48.663949
3504.089001	492128.026306	48.668954
3503.711050	492117.451293	48.673959
3503.769741	492107.009826	48.678964
3503.799292	492084.418931	48.683969
3503.859572	492069.672639	48.688973
3503.907036	492066.120212	48.693978
3503.754581	492075.107918	48.698983
3503.742443	492047.358100	48.703988
3503.241961	492038.980011	48.708993
3503.447455	492023.096607	48.713997
3503.507926	492030.835272	48.719002
3503.744814	492030.645909	48.724007
3504.004424	492017.539253	48.729012
3503.559818	492033.308538	48.734017
3503.711532	492010.343751	48.739021
3503.531195	491993.255255	48.744026
3503.406671	491991.553112	48.749031
3503.520515	491979.786162	48.754036
3503.575940	491991.374440	48.759041
3503.527653	491975.379181	48.764045
3503.313132	491980.983722	48.769050
3503.373058	491974.998488	48.774055
3503.651588	491969.282552	48.779060
3503.507983	491981.307431	48.784065
3503.662851	491965.583906	48.789069
3503.795240	491944.698419	48.794074
3503.700818	491934.078487	48.799079
3503.790824	491931.228301	48.804084
3503.542479	491938.104256	48.809089
3503.728894	491932.149658	48.814093
3503.835586	491928.689128	48.819098
3503.444862	491910.266469	48.824103
3503.665559	491883.998875	48.829108
3503.335489	491888.811429	48.834113
3503.549641	491897.133568	48.839117
3503.708048	491886.169793	48.844122
3503.547999	491880.725720	48.849127
3503.593944	491876.312578	48.854132
3503.554349	491883.206201	48.859137
3503.868763	491864.874613	48.864141
3503.414066	491849.753761	48.869146
3503.446419	491834.302701	48.874151
3503.958113	491843.489400	48.879156
3503.656491	491838.726044	48.884161
3503.769798	491834.099674	48.889165
3503.459403	491841.998322	48.894170
3503.830224	491816.010758	48.899175
3503.833414	491802.995123	48.904180
3503.413738	491798.706200	48.909185
3503.574197	491791.590880	48.914189
3503.606579	491788.749781	48.919194
3503.396652	491791.821521	48.924199
3503.655944	491778.562821	48.929204
3503.740499	491789.032482	48.934209
3503.666561	491763.824139	48.939213
3503.620060	491752.082390	48.944218
3503.708448	491743.459162	48.949223
3504.026067	491729.127710	48.954228
3503.466431	491742.687140	48.959233
3504.104974	491730.482601	48.964237
3503.852584	491704.897243	48.969242
3503.108742	491703.394246	48.974247
3503.534191	491692.692007	48.979252
3503.629512	491679.256580	48.984257
3503.690689	491678.335343	48.989261
3503.661399	491685.429982	48.994266
3503.194218	491688.593044	48.999271
3503.215979	491681.600890	49.004276
3502.958564	491692.732372	49.009281
3503.329514	491674.138447	49.014285
3503.661938	491681.023987	49.019290
3503.436173	491692.910109	49.024295
3503.632019	491662.544058	49.029300
3503.618138	491651.354161	49.034305
3503.652206	491649.120490	49.039309
3503.551756	491635.614689	49.044314
3503.680989	491651.141668	49.049319
3503.895370	491630.648014	49.054324
3503.633763	491638.640322	49.059329
3503.397041	491613.356218	49.064333
3503.553061	491600.316286	49.069338
3503.513052	491599.613611	49.074343
3503.646369	491593.768583	49.079348
3503.795752	491592.681471	49.084353
3503.693460	491588.291690	49.089357
3503.660752	491583.485764	49.094362
3503.398467	491577.956476	49.099367
3503.566999	491557.976420	49.104372
3503.473245	491548.875459	49.109377
3503.925229	491550.475251	49.114381
3503.762760	491541.739650	49.119386
3503.565726	491549.316644	49.124391
3503.879397	491546.025901	49.129396
3503.791193	491527.251186	49.134401
3503.445367	491505.326639	49.139405
3503.608230	491503.427097	49.144410
3503.060392	491506.704224	49.149415
3503.555809	491493.104139	49.154420
3503.205683	491490.981817	49.159425
3503.164423	491486.481078	49.164429
3503.453801	491498.488475	49.169434
3503.305620	491512.388186	49.174439
3503.317081	491491.268087	49.179444
3503.160703	491496.711653	49.184449
3503.311076	491483.368671	49.189453
3503.778710	491485.928220	49.194458
3503.582544	491493.454456	49.199463
3503.854228	491482.928330	49.204468
3503.556130	491482.317086	49.209473
3503.580888	491457.497877	49.214477
3503.947974	491455.515407	49.219482
3503.753464	491458.635409	49.224487
3503.579554	491447.622614	49.229492
3503.681749	491452.873393	49.234497
3503.830002	491439.581358	49.239501
3503.894442	491422.960084	49.244506
3504.017791	491410.077114	49.249511
3504.022114	491402.935681	49.254516
3503.729530	491396.499542	49.259521
3503.883036	491365.126825	49.264525
3504.060466	491356.337414	49.269530
3503.557974	491362.392806	49.274535
3503.661461	491354.931819	49.279540
3503.843158	491327.656729	49.284545
3503.761601	491311.463583	49.289549
3503.713089	491314.155381	49.294554
3503.680480	491311.729632	49.299559
3503.685322	491300.637854	49.304564
3503.352828	491313.553966	49.309569
3503.653210	491296.236916	49.314573
3503.766775	491274.138198	49.319578
3503.569063	491265.661258	49.324583
3503.656778	491269.445700	49.329588
3503.490229	491270.687485	49.334593
3503.762845	491266.339658	49.339597
3503.896476	491268.243014	49.344602
3503.539381	491238.723330	49.349607
3503.842805	491216.797112	49.354612
3503.557778	491231.174458	49.359617
3503.291490	491213.997543	49.364621
3503.673137	491216.520077	49.369626
3503.447999	491211.643182	49.374631
3503.557646	491210.663617	49.379636
3503.615228	491215.820225	49.384641
3503.583608	491206.202834	49.389645
3503.377488	491177.570785	49.394650
3503.431452	491168.598223	49.399655
3503.517549	491166.609492	49.404660
3503.847001	491167.874175	49.409665
3503.599698	491163.051415	49.414669
3503.843831	491169.596590	49.419674
3503.307739	491167.098470	49.424679
3503.509935	491164.433012	49.429684
3503.338048	491153.521012	49.434689
3503.366099	491123.079315	49.439693
3503.498544	491124.881584	49.444698
3503.366838	491123.940162	49.449703
3503.676304	491111.837879	49.454708
3503.886784	491113.070727	49.459713
3503.657781	491119.741347	49.464717
3504.024295	491126.216550	49.469722
3503.621229	491108.149557	49.474727
3503.746114	491095.468704	49.479732
3503.645044	491087.330919	49.484737
3503.628524	491075.077559	49.489741
3503.626348	491073.355993	49.494746
3503.488021	491086.241572	49.499751
3503.886575	491082.127020	49.504756
3503.974405	491052.840584	49.509761
3503.994615	491041.239777	49.514765
3504.019438	491020.117033	49.519770
3503.953350	491032.991230	49.524775
3503.972933	491004.627110	49.529780
3503.897400	490998.916197	49.534785
3504.098181	490988.907448	49.539789
3504.218110	490967.921547	49.544794
3503.615347	490950.037899	49.549799
3503.905322	490936.469882	49.554804
3503.776902	490943.833696	49.559809
3503.723569	490934.219596	49.564813
3503.726144	490915.176692	49.569818
3503.429558	490897.092664	49.574823
3503.602310	490890.329574	49.579828
3503.610703	490894.734370	49.584833
3503.326651	490897.514102	49.589837
3503.744969	490881.798669	49.594842
3503.552236	490906.898428	49.599847
3504.096082	490876.222868	49.604852
3503.814844	490860.820568	49.609857
3503.753034	490834.950666	49.614861
3503.883620	490846.527776	49.619866
3504.006286	490828.985157	49.624871
3503.912686	490812.692191	49.629876
3503.961424	490799.618012	49.634881
3503.603782	490798.762929	49.639885
3503.873650	490777.702471	49.644890
3503.717256	490778.740101	49.649895
3503.595931	490761.438566	49.654900
3503.907669	490747.157936	49.659905
3503.597976	490753.993377	49.664909
3503.624051	490736.668520	49.669914
3503.775580	490753.205632	49.674919
3503.798636	490725.904094	49.679924
3503.679493	490719.845470	49.684929
3503.732703	490717.709952	49.689933
3504.041036	490699.732703	49.694938
3503.850161	490715.057829	49.699943
3504.088620	490677.694359	49.704948
3504.152455	490669.580972	49.709953
3504.198417	490663.243006	49.714957
3503.835456	490641.978544	49.719962
3503.699132	490623.362463	49.724967
3503.987700	490616.986135	49.729972
3503.787647	490617.119051	49.734977
3503.694928	490610.245882	49.739981
3503.532087	490576.136323	49.744986
3503.330612	490581.587282	49.749991
3503.741245	490569.924472	49.754996
3503.743465	490559.643002	49.760001
3503.782338	490567.841503	49.765005
3503.512890	490559.882039	49.770010
3503.642676	490567.610357	49.775015
3503.719746	490545.769776	49.780020
3503.577923	490534.852662	49.785025
3503.776200	490521.045609	49.790029
3503.775221	490530.162053	49.795034
3503.504867	490528.634763	49.800039
3503.526127	490521.135794	49.805044
3503.448773	490516.286004	49.810049
3503.593908	490525.430002	49.815053
3503.619927	490486.681639	49.820058
3503.579063	490492.968222	49.825063
3503.803678	490482.904790	49.830068
3503.561417	490483.095024	49.835073
3503.518569	490484.165370	49.840077
3503.596601	490476.049656	49.845082
3503.247530	490470.432462	49.850087
3503.509842	490462.085031	49.855092
3503.176880	490475.710840	49.860097
3503.221739	490472.310460	49.865101
3503.412881	490462.353600	49.870106
3503.357444	490452.131831	49.875111
3503.373590	490451.116359	49.880116
3503.470919	490432.108632	49.885121
3503.432263	490432.519917	49.890125
3503.599159	490412.488249	49.895130
3503.379811	490418.448544	49.900135
3503.217421	490421.614287	49.905140
3503.445288	490421.173104	49.910145
3503.490643	490427.142204	49.915149
3503.582724	490416.086758	49.920154
3503.312049	490423.270675	49.925159
3503.329396	490424.230218	49.930164
3503.445779	490413.677392	49.935169
3503.016579	490423.823853	49.940173
3503.709190	490398.644445	49.945178
3503.406374	490416.570474	49.950183
3503.581097	490409.351082	49.955188
3503.666097	490395.106023	49.960193
3503.331023	490389.790471	49.965197
3503.589283	490367.971691	49.970202
3503.410601	490385.067786	49.975207
3503.667072	490366.591950	49.980212
3503.449667	490363.283650	49.985217
3503.129154	490366.271809	49.990221
3503.692726	490363.903645	49.995226
3503.421954	490364.908730	50.000231
3503.605593	490364.423891	50.005236
3503.437975	490367.286590	50.010241
3503.627278	490362.647845	50.015245
3503.623227	490335.299375	50.020250
3503.460646	490318.510416	50.025255
3503.370679	490319.486925	50.030260
3503.739330	490323.986854	50.035265
3503.455306	490304.583455	50.040269
3503.667048	490319.085568	50.045274
3503.756835	490319.729787	50.050279
3503.756199	490309.347338	50.055284
3503.629227	490294.274714	50.060289
3503.774606	490282.805592	50.065293
3503.761927	490272.323733	50.070298
3503.558246	490281.117810	50.075303
3503.816996	490281.330150	50.080308
3503.782656	490266.344156	50.085313
3503.539854	490247.744530	50.090317
3503.856079	490245.010273	50.095322
3503.605472	490235.072467	50.100327
3503.759620	490222.335752	50.105332
3503.497879	490234.329779	50.110337
3503.306193	490236.335307	50.115341
3503.743187	490213.829689	50.120346
3503.720650	490213.225493	50.125351
3503.523334	490183.273710	50.130356
3503.768971	490187.539880	50.135361
3503.413255	490178.074480	50.140365
3503.679687	490179.298547	50.145370
3503.561909	490183.824747	50.150375
3503.449762	490182.981478	50.155380
3503.758884	490189.111551	50.160385
3503.743213	490151.533965	50.165389
3503.711696	490136.699361	50.170394
3503.697174	490139.132720	50.175399
3503.697857	490131.181024	50.180404
3503.718024	490137.356786	50.185409
3503.580309	490130.338612	50.190413
3503.624397	490097.107120	50.195418
3503.387335	490090.053986	50.200423
3503.812866	490078.591106	50.205428
3503.754828	490091.920503	50.210433
3503.801359	490084.721249	50.215437
3504.053017	490073.539084	50.220442
3503.850848	490061.061167	50.225447
3503.501933	490045.719539	50.230452
3503.833245	490034.676703	50.235457
3503.685182	490043.968574	50.240461
3503.830381	490025.813875	50.245466
3503.620026	490018.148724	50.250471
3503.470464	489987.328074	50.255476
3503.574188	490005.443475	50.260481
3503.642518	489993.682470	50.265485
3504.162149	489988.940775	50.270490
3503.767170	490001.006658	50.275495
3503.781492	489972.388568	50.280500
3503.737095	489963.785508	50.285505
3503.342890	489968.355451	50.290509
3503.550185	489956.065983	50.295514
3503.625508	489954.585302	50.300519
3503.579958	489947.096663	50.305524
3503.684742	489949.055361	50.310529
3503.355403	489934.419614	50.315533
3503.618922	489915.385096	50.320538
3503.256456	489912.352883	50.325543
3503.371517	489904.433660	50.330548
3503.795428	489892.261855	50.335553
3503.643121	489905.454341	50.340557
3503.771975	489907.004058	50.345562
3503.600966	489909.310238	50.350567
3503.738031	489890.194386	50.355572
3503.722651	489872.419454	50.360577
3503.417730	489858.742096	50.365581
3503.492538	489851.082451	50.370586
3503.557785	489857.909602	50.375591
3503.877032	489857.555260	50.380596
3503.621644	489857.393039	50.385601
3503.448617	489855.799661	50.390605
3503.825279	489838.671800	50.395610
3503.627336	489828.016384	50.400615
3503.571771	489807.867289	50.405620
3503.400318	489797.562204	50.410625
3503.555489	489809.845142	50.415629
3503.652947	489800.763754	50.420634
3503.595176	489813.688123	50.425639
3503.521402	489800.885851	50.430644
3503.818172	489789.037963	50.435649
3503.605629	489784.057407	50.440653
3503.796525	489766.249770	50.445658
3503.644614	489757.967498	50.450663
3503.850584	489755.909022	50.455668
3503.946421	489748.651198	50.460673
3503.675672	489737.602052	50.465677
3503.675593	489716.886960	50.470682
3503.678258	489719.216361	50.475687
3503.474317	489713.221462	50.480692
3503.347685	489721.041307	50.485697
3503.062970	489717.237049	50.490701
3503.274053	489711.227200	50.495706
3503.128633	489715.251399	50.500711
3503.529493	489702.576632	50.505716
3503.251237	489708.597111	50.510721
3503.073196	489714.601747	50.515725
3503.268027	489708.543817	50.520730
3503.383844	489693.786872	50.525735
3503.199577	489658.615416	50.530740
3503.244327	489639.564549	50.535745
3503.149643	489590.754375	50.540749
3503.247741	489539.583763	50.545754
3503.181172	489481.702744	50.550759
3502.863725	489408.565194	50.555764
3502.817717	489320.797469	50.560769
3502.337295	489235.225277	50.565773
3502.714905	489128.092222	50.570778
3502.377730	489031.708053	50.575783
3501.749099	488910.702736	50.580788
3501.837722	488777.731004	50.585793
3501.484158	488637.230560	50.590797
3501.544453	488509.225223	50.595802
3501.119993	488365.441618	50.600807
3501.122252	488203.911834	50.605812
3501.289068	488032.173464	50.610817
3500.708498	487859.234685	50.615821
3500.795619	487677.932244	50.620826
3500.160903	487483.926655	50.625831
3499.853932	487294.983405	50.630836
3499.373958	487089.197429	50.635841
3499.087963	486884.290369	50.640845
3499.176404	486661.136284	50.645850
3498.389527	486454.784083	50.650855
3497.916115	486223.253970	50.655860
3497.743512	485978.755667	50.660865
3497.206121	485751.181287	50.665869
3497.312911	485503.390585	50.670874
3496.800005	485260.861963	50.675879
3496.434935	485008.782687	50.680884
3496.173411	484744.676973	50.685889
3495.732872	484474.111173	50.690893
3495.489358	484189.679458	50.695898
3494.767099	483916.465225	50.700903
3494.193559	483636.789246	50.705908
3493.968695	483354.470189	50.710913
3493.046489	483067.950644	50.715917
3492.531370	482768.087864	50.720922
3492.173322	482477.569100	50.725927
3491.950927	482181.400389	50.730932
3491.584665	481877.396230	50.735937
3491.076737	481574.879150	50.740941
3490.614150	481240.985137	50.745946
3489.860437	480937.686321	50.750951
3489.341316	480605.969290	50.755956
3489.345266	480281.866285	50.760961
3488.573286	479961.985178	50.765965
3488.157868	479621.164513	50.770970
3487.645993	479283.545776	50.775975
3487.337595	478933.017269	50.780980
3486.893760	478589.092033	50.785985
3485.872430	478247.938067	50.790989
3485.470179	477901.105675	50.795994
3484.671075	477562.286738	50.800999
3484.237877	477183.923740	50.806004
3483.738487	476840.078426	50.811009
3482.844172	476487.420147	50.816013
3482.588250	476120.666057	50.821018
3482.003687	475773.065311	50.826023
3481.395235	475411.067664	50.831028
3481.015330	475039.903837	50.836033
3479.989422	474676.691839	50.841037
3479.642571	474285.183302	50.846042
3478.898970	473930.023414	50.851047
3478.249690	473549.598730	50.856052
3477.810095	473177.193670	50.861057
3476.894498	472806.276427	50.866061
3476.397240	472423.221404	50.871066
3475.950532	472043.902569	50.876071
3475.429316	471671.229516	50.881076
3474.897737	471286.435063	50.886081
3473.938856	470906.517148	50.891085
3473.344043	470510.666328	50.896090
3472.819603	470127.724947	50.901095
3471.779456	469748.913969	50.906100
3471.455329	469350.868816	50.911105
3470.697895	468972.505995	50.916109
3469.675708	468588.651600	50.921114
3469.166362	468205.013299	50.926119
3468.489040	467815.969168	50.931124
3468.330760	467427.849873	50.936129
3467.459226	467044.703942	50.941133
3467.137889	466650.054988	50.946138
3466.297022	466262.833432	50.951143
3465.450755	465877.481865	50.956148
3464.998315	465465.844052	50.961153
3464.099899	465076.682937	50.966157
3463.289424	464695.310403	50.971162
3463.017548	464297.212165	50.976167
3461.915879	463903.649766	50.981172
3461.353582	463508.625574	50.986177
3460.394066	463120.402055	50.991181
3459.932513	462727.680484	50.996186
3459.311665	462339.186471	51.001191
3458.878796	461956.133314	51.006196
3458.208824	461551.656687	51.011201
3457.169010	461153.621706	51.016205
3456.555894	460772.097729	51.021210
3456.120901	460372.684825	51.026215
3455.252353	459993.419362	51.031220
3454.612615	459591.234788	51.036225
3453.505098	459213.008056	51.041229
3452.987131	458815.405944	51.046234
3452.269284	458417.777524	51.051239
3451.529498	458036.327403	51.056244
3451.217222	457647.041714	51.061249
3450.202784	457272.013583	51.066253
3449.558478	456869.222087	51.071258
3448.913402	456490.368362	51.076263
3448.201380	456100.408553	51.081268
3447.776209	455709.584872	51.086273
3446.763090	455330.718940	51.091277
3446.216956	454939.190686	51.096282
3445.540058	454552.952749	51.101287
3444.493221	454173.362360	51.106292
3444.206292	453779.236186	51.111297
3443.097631	453399.135208	51.116301
3442.692121	453007.652730	51.121306
3441.944606	452631.084249	51.126311
3441.221806	452255.013043	51.131316
3440.353829	451858.662134	51.136321
3439.504662	451501.474222	51.141325
3438.662191	451108.861217	51.146330
3437.849514	450738.766991	51.151335
3437.114084	450385.045064	51.156340
3436.707677	449999.397691	51.161345
3435.836021	449637.769601	51.166349
3435.816722	449254.839672	51.171354
3434.496153	448880.482532	51.176359
3434.128573	448516.321412	51.181364
3433.642280	448131.619903	51.186369
3432.619144	447769.428509	51.191373
3432.248437	447387.893770	51.196378
3431.351202	447015.774403	51.201383
3430.374873	446638.332640	51.206388
3429.876284	446270.401700	51.211393
3429.104176	445902.812805	51.216397
3428.608008	445526.800018	51.221402
3427.507286	445158.337953	51.226407
3427.107235	444792.855560	51.231412
3426.550358	444421.606032	51.236417
3425.524482	444059.256795	51.241421
3424.694671	443690.018637	51.246426
3424.318953	443324.357706	51.251431
3423.560073	442951.340779	51.256436
3422.835696	442581.053736	51.261441
3421.971958	442225.960878	51.266445
3421.643828	441857.122974	51.271450
3420.616949	441500.167066	51.276455
3420.028196	441138.720169	51.281460
3419.555635	440769.380978	51.286465
3418.300696	440415.389620	51.291469
3417.716843	440054.128977	51.296474
3417.021338	439688.210091	51.301479
3416.203641	439334.870151	51.306484
3415.477102	438979.327684	51.311489
3414.688248	438625.922270	51.316493
3414.077991	438281.317577	51.321498
3413.661239	437936.195185	51.326503
3412.760754	437585.077291	51.331508
3412.193651	437231.997785	51.336513
3411.344437	436881.598087	51.341517
3410.551870	436526.919543	51.346522
3409.848207	436175.344556	51.351527
3408.843784	435837.648412	51.356532
3408.737192	435497.952479	51.361537
3407.685364	435152.460586	51.366541
3407.210914	434796.209492	51.371546
3406.433557	434458.992201	51.376551
3405.442765	434110.810637	51.381556
3404.725892	433772.990743	51.386561
3403.790873	433438.298443	51.391565
3403.183373	433094.688781	51.396570
3402.587517	432766.941800	51.401575
3402.137381	432428.884280	51.406580
3401.179873	432087.855593	51.411585
3400.503120	431766.405706	51.416589
3400.047197	431422.597430	51.421594
3399.272547	431092.115132	51.426599
3398.504983	430761.018090	51.431604
3397.736199	430416.611159	51.436609
3397.000879	430101.777485	51.441613
3396.376212	429765.922089	51.446618
3395.820246	429437.847439	51.451623
3394.985535	429104.251444	51.456628
3394.703409	428777.141022	51.461633
3393.858310	428451.715430	51.466637
3393.113043	428108.391889	51.471642
3392.431102	427784.151259	51.476647
3391.519786	427464.285607	51.481652
3391.109483	427111.474397	51.486657
3390.309570	426795.367116	51.491661
3389.531142	426473.259083	51.496666
3388.757861	426140.835186	51.501671
3388.127619	425824.892802	51.506676
3387.417391	425493.009664	51.511681
3386.555354	425170.594468	51.516685
3385.807096	424845.795401	51.521690
3385.188944	424525.467404	51.526695
3384.417644	424210.950770	51.531700
3384.150881	423890.331138	51.536705
3383.125923	423578.463414	51.541709
3382.496656	423252.254936	51.546714
3381.837864	422925.920241	51.551719
3381.018865	422602.197827	51.556724
3380.272302	422283.743473	51.561729
3379.221659	421979.888223	51.566733
3378.767901	421653.836240	51.571738
3378.484484	421347.109398	51.576743
3377.493238	421050.600974	51.581748
3376.510297	420728.254231	51.586753
3376.032284	420413.698635	51.591757
3375.347880	420104.125635	51.596762
3374.651152	419794.906799	51.601767
3373.912676	419489.552432	51.606772
3373.228369	419182.382538	51.611777
3372.298688	418879.871565	51.616781
3371.725870	418579.460258	51.621786
3371.332965	418276.273654	51.626791
3370.447551	417969.274795	51.631796
3369.988230	417659.309096	51.636801
3369.069884	417352.308781	51.641805
3368.566951	417046.509743	51.646810
3367.772345	416753.608786	51.651815
3367.190023	416444.894229	51.656820
3366.529143	416137.687738	51.661825
3365.810558	415832.621229	51.666829
3365.136165	415519.998721	51.671834
3364.491010	415225.635804	51.676839
3363.624292	414934.633273	51.681844
3362.894721	414616.547191	51.686849
3362.501971	414322.668763	51.691853
3361.610865	414018.728388	51.696858
3360.877298	413719.358834	51.701863
3360.116723	413426.799970	51.706868
3359.826262	413116.326897	51.711873
3358.642531	412824.896119	51.716877
3358.333781	412528.242244	51.721882
3357.628686	412225.575184	51.726887
3356.393128	411928.045460	51.731892
3356.009568	411634.189533	51.736897
3355.293512	411347.523573	51.741901
3354.385929	411056.641581	51.746906
3353.952494	410761.920981	51.751911
3353.109504	410474.275688	51.756916
3352.832552	410178.126995	51.761921
3352.081778	409892.926444	51.766925
3351.320184	409594.434547	51.771930
3350.550365	409298.304317	51.776935
3349.712246	409021.012480	51.781940
3348.985817	408719.177379	51.786945
3348.293502	408431.997047	51.791949
3347.778916	408146.564812	51.796954
3347.013792	407858.526549	51.801959
3346.123678	407574.139464	51.806964
3345.489623	407290.954521	51.811969
3344.800976	407013.417492	51.816973
3344.028570	406726.970836	51.821978
3343.689818	406451.228648	51.826983
3343.069580	406167.980371	51.831988
3341.978935	405876.671137	51.836993
3341.122681	405597.902576	51.841997
3340.438084	405318.697728	51.847002
3339.788736	405035.367488	51.852007
3339.302672	404771.858575	51.857012
3338.728632	404486.249450	51.862017
3337.945074	404210.456104	51.867021
3337.411506	403925.445471	51.872026
3336.710471	403645.287913	51.877031
3336.014174	403375.014293	51.882036
3335.481493	403089.309721	51.887041
3334.521749	402816.455035	51.892045
3333.754460	402528.062861	51.897050
3333.228692	402253.380909	51.902055
3332.448648	401984.328767	51.907060
3332.167622	401710.264315	51.912065
3331.217050	401434.930808	51.917069
3330.611642	401157.761053	51.922074
3329.911219	400886.856983	51.927079
3328.910876	400610.532965	51.932084
3328.534835	400333.904507	51.937089
3327.662815	400055.826952	51.942093
3326.941655	399776.579274	51.947098
3326.191156	399520.948972	51.952103
3325.664893	399243.292782	51.957108
3325.127056	398966.754563	51.962113
3324.176536	398706.599285	51.967117
3323.278187	398438.782044	51.972122
3322.586507	398166.710058	51.977127
3321.795986	397907.972164	51.982132
3321.652240	397645.774340	51.987137
3320.903794	397381.407552	51.992141
3320.088683	397108.787119	51.997146
3319.771255	396843.839460	52.002151
3319.042151	396580.505556	52.007156
3318.048452	396293.009290	52.012161
3317.228502	396044.176308	52.017165
3316.766014	395774.184027	52.022170
3316.385798	395510.913669	52.027175
3315.566503	395261.108722	52.032180
3314.999695	394981.186123	52.037185
3313.882239	394718.941433	52.042189
3313.331928	394444.986348	52.047194
3312.687856	394182.993170	52.052199
3311.708365	393932.797004	52.057204
3311.297697	393665.805230	52.062209
3310.435854	393418.002011	52.067213
3309.893994	393143.272424	52.072218
3309.240599	392884.703140	52.077223
3308.405258	392620.770560	52.082228
3307.699248	392362.358237	52.087233
3306.889205	392109.376079	52.092237
3306.530377	391857.973391	52.097242
3306.318769	391599.502629	52.102247
3304.955369	391341.847761	52.107252
3304.604631	391073.148390	52.112257
3303.477771	390820.893502	52.117261
3302.616434	390570.527235	52.122266
3302.613373	390303.648564	52.127271
3301.709396	390056.641732	52.132276
3300.922715	389801.172792	52.137281
3300.351369	389560.466691	52.142285
3299.710341	389298.410830	52.147290
3299.158508	389043.306137	52.152295
3298.274541	388792.549467	52.157300
3297.758760	388539.037429	52.162305
3297.048960	388280.799193	52.167309
3296.223160	388032.240263	52.172314
3295.538707	387768.450932	52.177319
3295.124672	387521.832223	52.182324
3294.539788	387268.220448	52.187329
3293.361354	387022.278666	52.192333
3292.711428	386764.299837	52.197338
3292.217074	386515.627213	52.202343
3291.035738	386264.645723	52.207348
3290.868330	386015.053372	52.212353
3289.919532	385762.226138	52.217357
3289.253104	385524.864940	52.222362
3288.875395	385280.081738	52.227367
3287.940748	385040.572828	52.232372
3287.442188	384788.837512	52.237377
3286.442263	384546.589212	52.242381
3285.925829	384301.109412	52.247386
3285.677487	384051.033403	52.252391
3285.224074	383814.263340	52.257396
3284.042225	383563.543337	52.262401
3283.769987	383316.848596	52.267405
3282.659910	383066.012189	52.272410
3282.300743	382807.069678	52.277415
3281.379837	382577.766492	52.282420
3280.941346	382320.944070	52.287425
3280.051578	382073.525036	52.292429
3279.472208	381820.536394	52.297434
3278.814878	381584.649309	52.302439
3277.882503	381337.410261	52.307444
3277.316345	381089.679330	52.312449
3276.795315	380849.976609	52.317453
3276.202977	380598.355342	52.322458
3275.484468	380349.753565	52.327463
3274.402164	380112.525799	52.332468
3274.196719	379866.332285	52.337473
3273.646031	379621.082012	52.342477
3272.945027	379376.922210	52.347482
3272.130877	379128.047957	52.352487
3271.214389	378888.395654	52.357492
3270.749622	378639.259554	52.362497
3269.865600	378400.311309	52.367501
3268.823676	378168.279508	52.372506
3268.330613	377920.364219	52.377511
3267.924078	377684.668139	52.382516
3267.288565	377440.460516	52.387521
3266.318271	377210.421183	52.392525
3265.643908	376963.851253	52.397530
3265.219793	376723.243129	52.402535
3264.226980	376493.890001	52.407540
3263.660467	376257.549447	52.412545
3263.073627	376023.601750	52.417549
3262.300043	375780.932025	52.422554
3261.879154	375553.136457	52.427559
3261.009224	375313.150026	52.432564
3260.382173	375070.707237	52.437569
3259.451351	374847.872287	52.442573
3258.890220	374615.413191	52.447578
3258.487507	374379.671713	52.452583
3257.360802	374153.786021	52.457588
3256.799072	373917.202155	52.462593
3256.110947	373685.266630	52.467597
3255.447996	373449.917114	52.472602
3254.745242	373222.483848	52.477607
3253.789181	372984.303525	52.482612
3253.373415	372765.217025	52.487617
3252.727186	372546.852668	52.492621
3252.354223	372308.372740	52.497626
3251.719726	372071.611790	52.502631
3250.558559	371850.069062	52.507636
3250.497831	371611.968250	52.512641
3249.514981	371380.346351	52.517645
3249.052841	371150.752297	52.522650
3248.487322	370923.768192	52.527655
3247.326083	370700.489549	52.532660
3247.001157	370450.492746	52.537665
3246.260232	370234.268351	52.542669
3245.252886	370003.838504	52.547674
3244.789695	369772.710778	52.552679
3243.963139	369549.907432	52.557684
3243.598518	369315.886889	52.562689
3242.967416	369089.844735	52.567693
3242.158302	368855.154225	52.572698
3241.779664	368636.702030	52.577703
3240.814430	368409.437133	52.582708
3240.168739	368168.916494	52.587713
3239.335755	367943.281933	52.592717
3238.545496	367723.618208	52.597722
3238.086787	367490.798490	52.602727
3237.295036	367271.514367	52.607732
3236.709659	367045.683381	52.612737
3235.977973	366825.039120	52.617741
3234.990047	366604.459735	52.622746
3234.360120	366379.243015	52.627751
3233.485248	366168.540636	52.632756
3233.071634	365934.967787	52.637761
3232.734173	365729.292281	52.642765
3231.673026	365507.981226	52.647770
3231.340826	365284.874542	52.652775
3230.233018	365059.803114	52.657780
3229.634981	364845.641375	52.662785
3229.078542	364628.418849	52.667789
3228.563165	364408.313686	52.672794
3227.887135	364184.212793	52.677799
3227.030189	363972.937576	52.682804
3226.334980	363750.771310	52.687809
3225.754917	363533.394649	52.692813
3224.781272	363322.872771	52.697818
3224.370163	363094.399168	52.702823
3223.594279	362896.667904	52.707828
3223.027799	362669.463549	52.712833
3221.975743	362455.973139	52.717837
3221.487342	362254.376992	52.722842
3220.775354	362030.551223	52.727847
3219.981071	361829.179741	52.732852
3219.596623	361615.249100	52.737857
3218.914929	361397.293298	52.742861
3218.078366	361190.582307	52.747866
3217.724794	360972.165513	52.752871
3216.780830	360762.848779	52.757876
3216.190187	360541.388610	52.762881
3215.924289	360338.451351	52.767885
3215.052139	360126.372330	52.772890
3214.656184	359906.557837	52.777895
3213.647316	359703.480956	52.782900
3213.119084	359487.197012	52.787905
3212.508219	359269.271167	52.792909
3211.425485	359055.083252	52.797914
3210.992586	358836.363916	52.802919
3210.060482	358633.143162	52.807924
3209.635186	358414.904211	52.812929
3209.068955	358211.420248	52.817933
3208.095185	357994.996566	52.822938
3207.659768	357783.270797	52.827943
3206.748750	357584.113866	52.832948
3206.443424	357361.448909	52.837953
3205.779016	357160.342718	52.842957
3204.653825	356944.320089	52.847962
3203.952969	356728.407525	52.852967
3203.558545	356522.751835	52.857972
3202.695864	356320.452131	52.862977
3202.124198	356113.270485	52.867981
3201.471211	355903.734193	52.872986
3200.667730	355697.579976	52.877991
3200.139425	355490.974215	52.882996
3199.739545	355277.832545	52.888001
3198.884418	355077.384378	52.893005
3198.178308	354867.597716	52.898010
3197.830222	354663.072300	52.903015
3197.086887	354459.219361	52.908020
3196.297327	354236.439048	52.913025
3195.472119	354035.498537	52.918029
3194.987726	353829.286289	52.923034
3194.896221	353602.626359	52.928039
3193.552759	353395.046789	52.933044
3192.916936	353180.406787	52.938049
3192.281404	352983.631322	52.943053
3191.491115	352776.521661	52.948058
3191.016631	352556.585531	52.953063
3190.261874	352351.809934	52.958068
3189.520226	352145.479029	52.963073
3188.916331	351931.083363	52.968077
3187.817896	351726.512410	52.973082
3187.573280	351509.131450	52.978087
3186.722822	351314.368864	52.983092
3186.421844	351104.782928	52.988097
3185.511722	350901.375180	52.993101
3184.590354	350696.721367	52.998106
3184.070992	350489.941680	53.003111
3183.344713	350293.196049	53.008116
3182.759754	350093.067844	53.013121
3182.153733	349885.739642	53.018125
3181.134131	349680.435803	53.023130
3181.068924	349476.430911	53.028135
3180.158243	349283.401202	53.033140
3179.291750	349074.533158	53.038145
3178.985599	348869.037052	53.043149
3178.297517	348669.988912	53.048154
3177.774142	348463.660315	53.053159
3176.665486	348257.703514	53.058164
3176.176417	348048.619175	53.063169
3175.507932	347845.772675	53.068173
3174.679556	347646.081318	53.073178
3174.395853	347436.249546	53.078183
3173.401085	347233.172480	53.083188
3172.593427	347031.134070	53.088193
3172.203705	346831.166808	53.093197
3171.392204	346624.240721	53.098202
3170.843570	346423.431785	53.103207
3170.274662	346223.694355	53.108212
3169.660874	346016.887501	53.113217
3169.133210	345829.741217	53.118221
3167.742546	345621.579592	53.123226
3167.504303	345421.761607	53.128231
3166.621210	345216.114411	53.133236
3165.878361	345015.000397	53.138241
3165.393875	344816.084688	53.143245
3164.632201	344620.164731	53.148250
3163.881609	344421.340686	53.153255
3163.020867	344218.460850	53.158260
3162.594060	344024.903999	53.163265
3161.700621	343833.100277	53.168269
3161.271567	343634.757232	53.173274
3160.575949	343429.634095	53.178279
3159.617965	343247.332938	53.183284
3159.017109	343056.982196	53.188289
3158.058142	342854.113237	53.193293
3157.345776	342677.549539	53.198298
3156.994966	342483.059312	53.203303
3156.157688	342296.434418	53.208308
3155.681111	342103.897391	53.213313
3154.837369	341910.679666	53.218317
3154.025974	341726.492547	53.223322
3153.778890	341534.451953	53.228327
3152.891489	341359.464843	53.233332
3152.503614	341175.743606	53.238337
3151.917052	340966.318480	53.243341
3151.166855	340775.856950	53.248346
3150.444787	340586.306762	53.253351
3149.667597	340405.852156	53.258356
3149.425415	340203.879196	53.263361
3148.815399	340007.309368	53.268365
3147.959828	339830.200127	53.273370
3146.978101	339629.156892	53.278375
3146.397389	339436.144386	53.283380
3145.646609	339232.746907	53.288385
3144.988366	339051.251373	53.293389
3144.336716	338862.295778	53.298394
3143.715578	338664.959867	53.303399
3142.944100	338492.950185	53.308404
3142.272251	338303.079726	53.313409
3141.967819	338114.092444	53.318413
3141.123706	337929.161134	53.323418
3140.586858	337730.918063	53.328423
3139.836349	337534.108282	53.333428
3139.161835	337345.151858	53.338433
3138.751566	337151.290924	53.343437
3137.653307	336958.531071	53.348442
3137.071475	336767.292699	53.353447
3136.277158	336590.852178	53.358452
3135.729412	336392.759524	53.363457
3135.462881	336196.836514	53.368461
3134.504247	336010.161408	53.373466
3133.799437	335819.856207	53.378471
3133.217659	335643.074063	53.383476
3132.170912	335444.242929	53.388481
3131.699324	335256.928610	53.393485
3130.938091	335068.259462	53.398490
3130.646443	334884.556008	53.403495
3129.447580	334704.330501	53.408500
3129.288259	334508.080133	53.413505
3128.619918	334320.590710	53.418509
3127.559487	334136.879602	53.423514
3127.005304	333946.087085	53.428519
3126.575987	333769.810565	53.433524
3125.740371	333582.269231	53.438529
3125.133319	333390.872568	53.443533
3124.459632	333197.016517	53.448538
3123.691778	333015.929218	53.453543
3122.968204	332837.762106	53.458548
3122.401412	332646.560705	53.463553
3121.748479	332465.428348	53.468557
3120.721715	332278.728436	53.473562
3120.658745	332095.439678	53.478567
3119.629769	331904.538534	53.483572
3118.998150	331715.101506	53.488577
3118.421842	331540.242883	53.493581
3117.884069	331353.666851	53.498586
3117.021359	331164.392234	53.503591
3116.027569	330986.441474	53.508596
3115.989816	330800.268613	53.513601
3115.359644	330606.780533	53.518605
3114.308675	330426.571630	53.523610
3113.865573	330235.318801	53.528615
3113.190800	330057.086175	53.533620
3112.260840	329874.540017	53.538625
3111.631172	329678.427147	53.543629
3110.897852	329501.271731	53.548634
3110.265503	329331.304858	53.553639
3109.513671	329152.573079	53.558644
3108.709669	328965.243896	53.563649
3108.616601	328779.660285	53.568653
3107.493170	328602.768157	53.573658
3107.395929	328416.573293	53.578663
3106.668913	328234.322015	53.583668
3105.778627	328047.233359	53.588673
3105.478171	327865.015544	53.593677
3104.422079	327677.570330	53.598682
3104.045728	327487.394747	53.603687
3103.075004	327308.082255	53.608692
3102.496831	327129.241893	53.613697
3101.790967	326940.211889	53.618701
3101.197067	326766.923455	53.623706
3100.387074	326576.152313	53.628711
3099.781866	326394.157507	53.633716
3099.223847	326203.090992	53.638721
3098.557156	326022.836357	53.643725
3097.638296	325839.413221	53.648730
3097.115046	325656.843636	53.653735
3096.382975	325479.831591	53.658740
3095.725214	325301.203389	53.663745
3095.278528	325111.720669	53.668749
3094.204491	324937.103919	53.673754
3093.586932	324758.111713	53.678759
3092.950885	324581.286201	53.683764
3092.321043	324403.262672	53.688769
3091.883678	324219.225012	53.693773
3090.933415	324040.589424	53.698778
3090.428819	323859.438681	53.703783
3089.539004	323690.111469	53.708788
3088.789571	323510.475449	53.713793
3088.646343	323318.980099	53.718797
3087.726502	323148.510799	53.723802
3087.217434	322966.595004	53.728807
3086.322476	322790.595970	53.733812
3085.821876	322607.837847	53.738817
3085.108833	322421.650209	53.743821
3084.183033	322255.839493	53.748826
3083.893077	322065.383003	53.753831
3083.181097	321892.103008	53.758836
3082.199087	321707.458623	53.763841
3081.447630	321529.702920	53.768845
3080.327081	321365.856406	53.773850
3080.109793	321188.881179	53.778855
3079.410135	321026.596978	53.783860
3078.755103	320843.986899	53.788865
3078.303341	320672.394723	53.793869
3077.408438	320498.937239	53.798874
3076.761729	320318.234408	53.803879
3075.854940	320149.564977	53.808884
3075.453168	319981.681022	53.813889
3075.315780	319805.963515	53.818893
3074.257682	319638.361022	53.823898
3073.865944	319461.588229	53.828903
3072.871012	319282.771722	53.833908
3072.028693	319115.439672	53.838913
3071.507608	318932.931854	53.843917
3070.668343	318768.552326	53.848922
3070.517889	318586.799972	53.853927
3069.582447	318406.775626	53.858932
3068.874629	318250.649693	53.863937
3068.427443	318078.491760	53.868941
3067.371507	317900.140582	53.873946
3066.963801	317723.647110	53.878951
3066.307736	317555.951790	53.883956
3065.459102	317381.870035	53.888961
3065.171203	317207.928392	53.893965
3064.046849	317044.405799	53.898970
3063.401378	316862.575712	53.903975
3062.611472	316700.400072	53.908980
3061.932272	316536.908030	53.913985
3061.324427	316370.578029	53.918989
3060.949234	316196.546543	53.923994
3060.269893	316025.720311	53.928999
3059.427113	315854.181218	53.934004
3058.701909	315681.630158	53.939009
3058.490934	315515.974351	53.944013
3057.355734	315353.851152	53.949018
3056.855903	315175.177830	53.954023
3056.225149	315004.520413	53.959028
3055.500021	314833.775792	53.964033
3054.916574	314660.156556	53.969037
3054.346613	314498.884691	53.974042
3053.680202	314319.243160	53.979047
3052.864331	314155.539712	53.984052
3052.213175	313975.487754	53.989057
3051.980592	313803.517619	53.994061
3050.899448	313645.304578	53.999066
3050.403108	313464.539723	54.004071
3049.920151	313283.670586	54.009076
3048.915215	313122.210802	54.014081
3048.420718	312948.752898	54.019085
3047.771258	312773.103878	54.024090
3047.086303	312605.863296	54.029095
3046.520078	312439.622224	54.034100
3045.641208	312268.082931	54.039105
3045.227712	312092.930211	54.044109
3044.212312	311929.738747	54.049114
3043.713442	311746.552328	54.054119
3043.213881	311575.130173	54.059124
3042.406020	311409.486000	54.064129
3041.895289	311232.310170	54.069133
3040.934998	311063.812147	54.074138
3040.372954	310884.352102	54.079143
3039.442645	310725.907250	54.084148
3038.975129	310555.751692	54.089153
3038.590714	310383.214534	54.094157
3037.672509	310215.905427	54.099162
3036.832333	310041.300871	54.104167
3036.355026	309879.065335	54.109172
3035.307016	309714.347971	54.114177
3034.865929	309538.839170	54.119181
3033.812352	309382.576485	54.124186
3033.797108	309206.566894	54.129191
3033.145732	309054.747378	54.134196
3032.040897	308889.834143	54.139201
3031.742315	308707.655253	54.144205
3030.898166	308546.698268	54.149210
3030.189333	308370.415251	54.154215
3029.498789	308211.801748	54.159220
3028.736662	308046.960453	54.164225
3028.367090	307882.871688	54.169229
3027.665979	307718.860643	54.174234
3027.100875	307544.769156	54.179239
3026.088289	307382.589520	54.184244
3025.458173	307218.159141	54.189249
3024.882644	307052.319324	54.194253
3023.866530	306890.470662	54.199258
3023.682875	306723.880835	54.204263
3023.023829	306561.083961	54.209268
3022.413097	306391.887445	54.214273
3021.894657	306230.315701	54.219277
3021.102340	306064.661714	54.224282
3020.376348	305893.674753	54.229287
3019.707241	305718.425842	54.234292
3019.345850	305555.224088	54.239297
3018.572769	305384.396716	54.244301
3017.738641	305229.825792	54.249306
3017.090569	305053.604989	54.254311
3016.571119	304885.410724	54.259316
3015.946651	304720.696197	54.264321
3015.271235	304547.484009	54.269325
3014.328648	304387.148593	54.274330
3013.393580	304222.991944	54.279335
3013.104357	304053.817994	54.284340
3012.018540	303886.832647	54.289345
3011.866053	303715.904976	54.294349
3011.106015	303560.047166	54.299354
3010.485297	303391.587002	54.304359
3010.015159	303223.077340	54.309364
3009.142556	303052.542977	54.314369
3008.773255	302879.331227	54.319373
3007.869902	302706.254730	54.324378
3007.241434	302545.154477	54.329383
3006.472360	302374.679337	54.334388
3005.595970	302216.852153	54.339393
3004.917623	302046.285879	54.344397
3004.491156	301883.472177	54.349402
3003.963947	301715.784745	54.354407
3003.217053	301555.211496	54.359412
3002.473804	301385.342338	54.364417
3002.190284	301214.508910	54.369421
3001.332066	301046.211018	54.374426
3000.732966	300867.761816	54.379431
2999.795918	300712.438381	54.384436
2999.198414	300554.896412	54.389441
2998.809463	300375.598470	54.394445
2998.029871	300204.766067	54.399450
2997.329456	300022.970391	54.404455
2996.852936	299867.369514	54.409460
2996.104904	299695.360125	54.414465
2995.360543	299527.246348	54.419469
2994.504908	299360.779872	54.424474
2993.781683	299192.789745	54.429479
2993.191511	299023.555995	54.434484
2992.310535	298865.267810	54.439489
2992.071598	298696.232805	54.444493
2991.081374	298531.493080	54.449498
2990.500132	298369.540731	54.454503
2990.051815	298200.232782	54.459508
2989.111927	298030.442210	54.464513
2988.745186	297868.582779	54.469517
2987.716363	297704.408656	54.474522
2987.364645	297538.064396	54.479527
2986.778592	297365.161169	54.484532
2985.901576	297209.137414	54.489537
2985.340685	297040.330058	54.494541
2984.507065	296883.458751	54.499546
2984.238029	296714.070096	54.504551
2983.373860	296545.539497	54.509556
2982.490428	296370.925196	54.514561
2981.995285	296202.692417	54.519565
2980.863528	296050.935537	54.524570
2980.400725	295882.850163	54.529575
2979.793641	295723.599075	54.534580
2979.096706	295558.122652	54.539585
2978.760024	295389.201945	54.544589
2978.020075	295232.212596	54.549594
2976.952075	295068.322528	54.554599
2976.780065	294905.665727	54.559604
2975.937610	294738.963773	54.564609
2975.453380	294569.989337	54.569613
2974.711734	294416.233962	54.574618
2974.001829	294247.778863	54.579623
2973.446341	294083.475814	54.584628
2972.161442	293928.914723	54.589633
2972.010698	293756.728907	54.594637
2971.216510	293599.466775	54.599642
2970.753155	293428.501679	54.604647
2970.024037	293275.965935	54.609652
2969.171238	293109.264349	54.614657
2968.752517	292933.045531	54.619661
2967.705245	292785.118476	54.624666
2967.322587	292613.477833	54.629671
2966.636235	292434.601450	54.634676
2965.758790	292290.161700	54.639681
2965.234022	292119.689223	54.644685
2964.306953	291964.790002	54.649690
2963.871930	291794.404955	54.654695
2963.362765	291641.247566	54.659700
2962.725324	291482.150984	54.664705
2962.373209	291319.061663	54.669709
2961.306323	291151.806830	54.674714
2961.061029	290986.230029	54.679719
2960.332383	290813.547770	54.684724
2959.626372	290650.666844	54.689729
2958.669004	290473.716536	54.694733
2958.057193	290318.027830	54.699738
2957.560587	290156.590573	54.704743
2956.733617	289993.091696	54.709748
2955.889162	289822.082519	54.714753
2955.725375	289657.739897	54.719757
2954.605176	289498.922266	54.724762
2954.319513	289330.294698	54.729767
2953.830614	289167.913334	54.734772
2952.924952	288994.570307	54.739777
2952.499901	288831.822097	54.744781
2951.565861	288663.704261	54.749786
2951.204709	288495.470174	54.754791
2950.535171	288332.836797	54.759796
2949.530660	288161.928375	54.764801
2948.957570	287991.104371	54.769805
2948.653866	287827.164890	54.774810
2947.961287	287654.118446	54.779815
2947.174805	287479.762442	54.784820
2946.122226	287319.379416	54.789825
2945.925361	287144.726153	54.794829
2945.136052	286981.601686	54.799834
2944.635228	286804.602378	54.804839
2943.946970	286640.162886	54.809844
2943.171401	286468.835318	54.814849
2942.976433	286295.098169	54.819853
2941.882498	286121.859797	54.824858
2941.294023	285947.955563	54.829863
2940.799943	285781.549369	54.834868
2939.802612	285611.224288	54.839873
2939.381644	285431.664862	54.844877
2938.673413	285262.898348	54.849882
2938.057173	285081.968931	54.854887
2937.449462	284917.719673	54.859892
2936.346741	284750.314265	54.864897
2936.136759	284574.159246	54.869901
2935.194325	284403.213727	54.874906
2934.296676	284227.396640	54.879911
2934.106543	284050.143135	54.884916
2933.103658	283890.209218	54.889921
2932.599690	283716.800016	54.894925
2932.011425	283557.768135	54.899930
2931.345915	283375.979889	54.904935
2930.849363	283208.350600	54.909940
2929.976405	283027.919410	54.914945
2929.219322	282858.955966	54.919949
2928.834850	282703.508029	54.924954
2927.968065	282526.972320	54.929959
2927.615021	282350.991928	54.934964
2926.599271	282175.371075	54.939969
2926.280707	281995.641283	54.944973
2925.188177	281831.213033	54.949978
2924.720654	281660.573412	54.954983
2924.148320	281486.282907	54.959988
2923.334548	281322.039603	54.964993
2923.011843	281137.267494	54.969997
2922.123705	280969.852340	54.975002
2921.179538	280792.258701	54.980007
2920.900455	280627.039187	54.985012
2920.387209	280455.184012	54.990017
2919.724850	280275.024270	54.995021
2918.708262	280105.184291	55.000026
2917.920925	279932.430064	55.005031
2917.678873	279758.341525	55.010036
2916.702425	279587.527288	55.015041
2916.243493	279415.892506	55.020045
2915.755119	279235.348436	55.025050
2915.034901	279062.303258	55.030055
2914.548120	278887.540183	55.035060
2913.493661	278712.816013	55.040065
2912.964748	278537.677525	55.045069
2912.335385	278361.739924	55.050074
2911.316837	278186.780772	55.055079
2910.941423	277995.674710	55.060084
2910.268239	277823.818909	55.065089
2909.715077	277638.853345	55.070093
2908.766082	277469.358788	55.075098
2908.248761	277289.914144	55.080103
2907.248500	277117.524274	55.085108
2906.597209	276955.342895	55.090113
2905.978875	276781.007868	55.095117
2905.582606	276616.493934	55.100122
2904.589543	276442.676639	55.105127
2904.080701	276272.450119	55.110132
2902.985315	276115.177985	55.115137
2903.026625	275936.154158	55.120141
2902.331168	275766.008094	55.125146
2901.260737	275596.761847	55.130151
2900.719780	275415.410688	55.135156
2900.167146	275262.458629	55.140161
2899.744460	275081.343422	55.145165
2899.061757	274908.903165	55.150170
2898.312400	274732.322112	55.155175
2897.806546	274560.134010	55.160180
2896.846116	274392.372974	55.165185
2896.525788	274204.135886	55.170189
2895.833057	274030.551152	55.175194
2895.085533	273860.668015	55.180199
2894.363026	273682.478231	55.185204
2893.503534	273519.209150	55.190209
2893.056025	273336.085917	55.195213
2892.364495	273167.008941	55.200218
2891.487907	272991.263093	55.205223
2891.251312	272803.980630	55.210228
2890.288045	272640.600699	55.215233
2889.735660	272463.428276	55.220237
2889.092731	272292.509958	55.225242
2888.419823	272123.582938	55.230247
2887.889544	271934.335069	55.235252
2887.422596	271762.446621	55.240257
2886.684404	271587.952431	55.245261
2885.716692	271414.997239	55.250266
2885.211993	271243.038435	55.255271
2884.665598	271057.460694	55.260276
2883.822024	270886.548865	55.265281
2883.049697	270701.490858	55.270285
2882.433042	270540.552217	55.275290
2881.663039	270361.428029	55.280295
2881.331216	270179.356579	55.285300
2880.335672	270011.499702	55.290305
2879.562476	269830.313196	55.295309
2878.976641	269668.656725	55.300314
2878.258099	269494.057934	55.305319
2878.004858	269319.461916	55.310324
2876.796501	269151.180491	55.315329
2876.402807	268975.384316	55.320333
2875.989848	268797.935799	55.325338
2875.169564	268630.229763	55.330343
2874.522908	268451.239308	55.335348
2873.712541	268281.112309	55.340353
2873.150827	268096.174403	55.345357
2872.350683	267926.937273	55.350362
2871.442598	267763.269357	55.355367
2871.386988	267584.465728	55.360372
2870.445995	267413.391871	55.365377
2869.929341	267249.585725	55.370381
2869.339206	267069.975510	55.375386
2868.708976	266890.066087	55.380391
2868.039303	266722.718787	55.385396
2867.467105	266548.046743	55.390401
2866.530985	266365.231634	55.395405
2866.024393	266191.873676	55.400410
2865.138431	266018.677722	55.405415
2864.755555	265829.077101	55.410420
2863.828020	265674.199451	55.415425
2863.215777	265491.002323	55.420429
2862.456630	265317.659222	55.425434
2862.026829	265144.416851	55.430439
2861.221336	264967.668506	55.435444
2860.517188	264796.609040	55.440449
2860.080725	264617.739501	55.445453
2859.613338	264445.445697	55.450458
2858.609932	264275.936454	55.455463
2857.971054	264089.713475	55.460468
2857.148461	263921.296353	55.465473
2856.556319	263752.384394	55.470477
2856.024246	263581.833050	55.475482
2855.211455	263402.361506	55.480487
2854.987783	263222.083667	55.485492
2854.043645	263051.572356	55.490497
2853.595760	262866.134742	55.495501
2853.099666	262703.396787	55.500506
2852.225993	262522.432733	55.505511
2851.686748	262345.159606	55.510516
2851.105889	262160.456542	55.515521
2850.284713	261976.122719	55.520525
2849.719820	261810.034345	55.525530
2849.152978	261621.101711	55.530535
2848.620589	261446.680400	55.535540
2847.591662	261271.930328	55.540545
2847.245047	261070.916890	55.545549
2846.473058	260893.910657	55.550554
2845.618701	260718.369237	55.555559
2845.003850	260526.694381	55.560564
2844.374733	260349.716796	55.565569
2843.619360	260166.443320	55.570573
2842.808138	259995.428772	55.575578
2841.989422	259814.381251	55.580583
2841.917765	259633.521168	55.585588
2841.145555	259461.940492	55.590593
2840.518623	259276.024113	55.595597
2839.699996	259094.238506	55.600602
2838.876028	258909.856178	55.605607
2838.760601	258730.506238	55.610612
2837.665052	258551.744574	55.615617
2837.108771	258369.561398	55.620621
2836.264152	258187.551352	55.625626
2835.887121	258006.256891	55.630631
2835.190370	257822.975796	55.635636
2834.219252	257655.833725	55.640641
2833.777842	257467.011497	55.645645
2833.131297	257287.593918	55.650650
2832.100692	257117.481962	55.655655
2832.095715	256930.628454	55.660660
2831.101364	256752.794411	55.665665
2830.306916	256565.938880	55.670669
2829.521158	256386.060177	55.675674
2828.892544	256198.389209	55.680679
2828.600391	256042.066284	55.685684
2827.809118	255868.046357	55.690689
2827.160962	255677.908610	55.695693
2826.504642	255495.743565	55.700698
2825.784023	255312.850311	55.705703
2825.310757	255127.676937	55.710708
2824.443886	254953.720672	55.715713
2824.054002	254762.396838	55.720717
2823.644117	254586.280216	55.725722
2822.489027	254391.614380	55.730727
2821.807253	254213.452840	55.735732
2821.270665	254038.681052	55.740737
2820.241830	253857.238611	55.745741
2819.859540	253678.342523	55.750746
2819.094476	253506.230495	55.755751
2818.620839	253323.554625	55.760756
2817.708990	253137.917761	55.765761
2817.243314	252953.254570	55.770765
2816.436414	252782.270371	55.775770
2816.048932	252593.647790	55.780775
2815.223254	252414.008181	55.785780
2814.572647	252245.317214	55.790785
2813.845324	252056.341538	55.795789
2813.846346	251881.817699	55.800794
2812.717056	251694.765134	55.805799
2812.257031	251504.092380	55.810804
2811.601960	251322.058454	55.815809
2811.034100	251133.720649	55.820813
2810.465577	250952.055407	55.825818
2809.451635	250770.842893	55.830823
2809.302282	250573.144130	55.835828
2808.357655	250380.664844	55.840833
2807.606011	250201.550595	55.845837
2807.050174	250012.015214	55.850842
2806.125309	249822.334760	55.855847
2805.672934	249632.070374	55.860852
2804.760672	249452.880516	55.865857
2804.362097	249265.409345	55.870861
2803.410815	249083.704911	55.875866
2802.578864	248904.273755	55.880871
2802.247291	248698.966242	55.885876
2801.502913	248524.003714	55.890881
2800.653100	248351.528303	55.895885
2800.274489	248164.029822	55.900890
2799.353795	247978.807505	55.905895
2798.893788	247786.942203	55.910900
2797.895525	247607.920889	55.915905
2797.485564	247427.049465	55.920909
2796.648089	247247.875790	55.925914
2795.684339	247065.029762	55.930919
2795.552384	246878.130479	55.935924
2795.097842	246711.349664	55.940929
2794.116914	246511.775943	55.945933
2793.308366	246332.216824	55.950938
2792.559742	246151.196889	55.955943
2792.014015	245963.447550	55.960948
2791.271095	245788.895485	55.965953
2790.688450	245601.738188	55.970957
2790.348060	245422.437139	55.975962
2789.431802	245246.970973	55.980967
2788.915081	245051.782297	55.985972
2788.362314	244876.615557	55.990977
2787.825812	244684.359081	55.995981
2787.031231	244508.237957	56.000986
2786.131043	244328.594086	56.005991
2785.540020	244135.302945	56.010996
2784.492400	243962.049279	56.016001
2784.129363	243769.919440	56.021005
2783.612451	243595.818247	56.026010
2782.865331	243425.828194	56.031015
2782.590919	243227.115068	56.036020
2781.778372	243034.242615	56.041025
2781.120635	242852.754342	56.046029
2780.292739	242661.769307	56.051034
2779.571358	242490.554091	56.056039
2779.117340	242301.700388	56.061044
2778.343377	242119.594949	56.066049
2777.527337	241927.030320	56.071053
2777.149184	241742.749151	56.076058
2776.288468	241564.427083	56.081063
2775.902769	241381.522757	56.086068
2775.112527	241196.441867	56.091073
2774.733632	241000.091594	56.096077
2774.074623	240812.418562	56.101082
2773.303428	240633.090561	56.106087
2772.941426	240443.232032	56.111092
2772.014678	240253.055814	56.116097
2771.330824	240061.542740	56.121101
2770.469629	239863.259024	56.126106
2769.958171	239681.624987	56.131111
2769.156235	239491.684887	56.136116
2768.622216	239305.878837	56.141121
2767.702030	239119.650424	56.146125
2767.321880	238934.049788	56.151130
2766.706420	238740.210817	56.156135
2765.880509	238552.669723	56.161140
2765.174058	238369.668121	56.166145
2764.735636	238181.811635	56.171149
2763.992675	237988.732619	56.176154
2763.141830	237805.041818	56.181159
2762.810276	237611.872839	56.186164
2762.116004	237426.171677	56.191169
2761.058094	237230.470154	56.196173
2760.624743	237041.876359	56.201178
2759.678029	236854.433683	56.206183
2759.054807	236666.761853	56.211188
2758.458395	236484.382577	56.216193
2757.963707	236307.614992	56.221197
2757.376824	236115.838714	56.226202
2756.390060	235931.892537	56.231207
2756.195277	235742.830378	56.236212
2755.479890	235555.226048	56.241217
2754.745615	235367.319487	56.246221
2754.034801	235184.120296	56.251226
2753.411094	234988.430552	56.256231
2752.955079	234787.061750	56.261236
2752.087247	234611.629323	56.266241
2751.391208	234422.419810	56.271245
2751.242603	234223.778937	56.276250
2750.091111	234039.225666	56.281255
2749.679008	233838.004582	56.286260
2748.691343	233652.382091	56.291265
2748.302422	233465.722982	56.296269
2747.534644	233277.087193	56.301274
2746.849936	233073.899265	56.306279
2746.034822	232884.686081	56.311284
2745.459224	232699.178369	56.316289
2744.625332	232511.394807	56.321293
2744.384972	232317.864874	56.326298
2743.262387	232126.715781	56.331303
2742.640814	231931.031754	56.336308
2742.152853	231752.361444	56.341313
2741.394296	231576.229660	56.346317
2740.365032	231382.062708	56.351322
2739.653875	231198.896474	56.356327
2739.420199	231003.433021	56.361332
2738.599869	230825.351830	56.366337
2737.902915	230646.462108	56.371341
2737.528195	230459.730247	56.376346
2736.652747	230275.267824	56.381351
2736.198303	230077.295080	56.386356
2735.672857	229893.847401	56.391361
2734.489520	229703.705934	56.396365
2734.153791	229517.020752	56.401370
2733.265817	229334.599185	56.406375
2732.986080	229132.246849	56.411380
2731.959523	228959.243430	56.416385
2731.467596	228775.970957	56.421389
2730.692462	228582.940961	56.426394
2730.084135	228406.282277	56.431399
2729.334768	228211.950469	56.436404
2728.872382	228024.804717	56.441409
2728.428716	227834.448254	56.446413
2727.766428	227642.115382	56.451418
2726.750668	227469.800654	56.456423
2726.336659	227269.103414	56.461428
2725.657862	227093.629785	56.466433
2724.900855	226895.202883	56.471437
2724.804029	226708.103934	56.476442
2723.819065	226519.974865	56.481447
2723.016901	226317.686380	56.486452
2722.424911	226116.969133	56.491457
2721.950193	225935.354946	56.496461
2721.358923	225744.873772	56.501466
2720.314191	225555.559678	56.506471
2719.979413	225354.307041	56.511476
2719.088151	225158.808046	56.516481
2718.395307	224970.738052	56.521485
2718.359377	224769.974183	56.526490
2717.345273	224584.591135	56.531495
2716.625144	224388.213951	56.536500
2715.979875	224193.467581	56.541505
2715.042358	224002.090548	56.546509
2714.440488	223798.809051	56.551514
2713.898539	223617.274321	56.556519
2713.459521	223406.775520	56.561524
2712.879516	223221.301402	56.566529
2711.890094	223026.255955	56.571533
2711.294749	222823.803374	56.576538
2710.585636	222637.829153	56.581543
2709.918809	222441.855695	56.586548
2709.051808	222248.065788	56.591553
2708.623005	222052.297476	56.596557
2708.060836	221862.470151	56.601562
2706.939135	221673.037440	56.606567
2706.571671	221471.723431	56.611572
2705.963865	221279.397016	56.616577
2705.032498	221084.487296	56.621581
2704.814593	220894.824245	56.626586
2703.639027	220709.106796	56.631591
2703.122881	220516.220426	56.636596
2702.784867	220326.883341	56.641601
2701.731633	220135.623305	56.646605
2701.410203	219938.137680	56.651610
2700.392821	219754.179676	56.656615
2700.037552	219557.056851	56.661620
2699.440086	219364.835546	56.666625
2698.728011	219168.381293	56.671629
2697.992415	218973.000556	56.676634
2697.191653	218786.477524	56.681639
2696.448725	218592.791964	56.686644
2695.779958	218405.548892	56.691649
2695.281347	218203.755341	56.696653
2694.861368	218011.051247	56.701658
2693.808971	217820.522699	56.706663
2693.335036	217625.982464	56.711668
2692.419064	217428.648747	56.716673
2692.094529	217245.974822	56.721677
2691.732161	217047.714352	56.726682
2690.683942	216860.955496	56.731687
2689.946749	216666.192293	56.736692
2689.656209	216475.393932	56.741697
2688.900487	216275.403181	56.746701
2688.219018	216081.078291	56.751706
2687.112373	215890.499915	56.756711
2686.636900	215692.681255	56.761716
2686.173906	215494.186565	56.766721
2685.206917	215306.362538	56.771725
2684.813289	215113.394931	56.776730
2684.392268	214924.225330	56.781735
2684.031701	214722.025362	56.786740
2683.267687	214530.887350	56.791745
2682.497255	214323.713004	56.796749
2681.744491	214111.776058	56.801754
2680.835259	213916.946088	56.806759
2680.572102	213718.641318	56.811764
2679.709229	213531.518519	56.816769
2678.866309	213338.054394	56.821773
2678.224974	213134.554489	56.826778
2677.431599	212930.773820	56.831783
2676.682009	212739.218624	56.836788
2675.992113	212558.409813	56.841793
2675.211485	212366.135121	56.846797
2675.271275	212161.203437	56.851802
2674.301551	211972.638274	56.856807
2673.476930	211777.279379	56.861812
2672.612509	211573.730578	56.866817
2671.879669	211387.013334	56.871821
2671.614723	211185.178157	56.876826
2670.616371	211004.842569	56.881831
2670.207824	210802.522236	56.886836
2669.476176	210620.936342	56.891841
2668.891080	210422.807163	56.896845
2668.583336	210223.616451	56.901850
2667.517687	210035.314023	56.906855
2667.058599	209840.463170	56.911860
2666.253734	209644.789499	56.916865
2665.537938	209459.335261	56.921869
2665.255124	209243.127009	56.926874
2664.493649	209044.571936	56.931879
2664.013895	208853.405672	56.936884
2663.218057	208659.171870	56.941889
2662.424716	208467.445568	56.946893
2661.913528	208250.398781	56.951898
2661.152167	208061.761410	56.956903
2660.039597	207860.453062	56.961908
2659.534015	207661.951010	56.966913
2658.961901	207480.056308	56.971917
2658.366967	207276.186103	56.976922
2657.559133	207082.595578	56.981927
2657.185079	206885.907930	56.986932
2656.357937	206690.794488	56.991937
2655.642123	206501.696600	56.996941
2654.914654	206298.219795	57.001946
2654.259296	206111.162596	57.006951
2653.626053	205919.508112	57.011956
2653.054531	205721.684726	57.016961
2652.316892	205531.129814	57.021965
2651.684469	205326.941324	57.026970
2650.821015	205141.040115	57.031975
2650.524140	204941.814095	57.036980
2650.062812	204754.246860	57.041985
2648.946353	204567.165817	57.046989
2648.742106	204359.553083	57.051994
2647.882209	204166.413077	57.056999
2647.480252	203965.565350	57.062004
2646.825160	203757.440796	57.067009
2645.857811	203561.252805	57.072013
2645.036997	203371.761721	57.077018
2644.513679	203174.486612	57.082023
2643.982820	202966.650685	57.087028
2643.105715	202778.277670	57.092033
2642.323003	202588.261393	57.097037
2642.072160	202384.048346	57.102042
2641.037051	202191.948151	57.107047
2640.217910	201993.693229	57.112052
2639.863675	201798.495919	57.117057
2639.100340	201604.916657	57.122061
2638.714794	201401.250295	57.127066
2637.448803	201215.349321	57.132071
2637.112686	201017.848522	57.137076
2636.591123	200829.285764	57.142081
2635.574369	200642.749126	57.147085
2635.512112	200450.628080	57.152090
2634.729018	200253.735312	57.157095
2633.866107	200057.161312	57.162100
2633.433042	199845.109427	57.167105
2632.435728	199661.830767	57.172109
2632.021377	199462.897279	57.177114
2630.825603	199278.149773	57.182119
2631.002076	199073.003247	57.187124
2629.973843	198871.267846	57.192129
2628.839670	198679.284728	57.197133
2628.818440	198479.045526	57.202138
2628.153617	198287.727508	57.207143
2627.048705	198091.644400	57.212148
2626.743209	197893.666588	57.217153
2626.251737	197695.400859	57.222157
2625.516630	197488.725165	57.227162
2624.628861	197300.398204	57.232167
2624.213732	197095.785675	57.237172
2623.568531	196893.628094	57.242177
2622.601721	196703.839732	57.247181
2621.981012	196498.511356	57.252186
2621.247494	196317.111142	57.257191
2620.947512	196115.207274	57.262196
2619.944022	195913.186617	57.267201
2619.226261	195717.356450	57.272205
2618.513841	195514.069694	57.277210
2617.691325	195336.262578	57.282215
2617.318983	195127.172071	57.287220
2616.701617	194931.901587	57.292225
2615.950578	194746.323415	57.297229
2615.521871	194554.803569	57.302234
2614.690725	194354.301379	57.307239
2614.051789	194162.841772	57.312244
2613.752457	193970.667433	57.317249
2612.758862	193760.663068	57.322253
2612.553302	193558.957935	57.327258
2611.464021	193375.855930	57.332263
2610.771014	193172.130154	57.337268
2610.351051	192965.511828	57.342273
2609.054687	192768.944977	57.347277
2608.764249	192568.974990	57.352282
2608.034282	192384.216524	57.357287
2607.125820	192186.000077	57.362292
2606.912634	191985.193181	57.367297
2605.934927	191792.663964	57.372301
2605.531879	191591.227142	57.377306
2604.704718	191409.299607	57.382311
2604.062954	191203.372698	57.387316
2603.789031	191009.182813	57.392321
2602.692343	190817.961339	57.397325
2602.245882	190607.578340	57.402330
2601.678476	190418.399342	57.407335
2600.855482	190218.268887	57.412340
2600.275133	190024.843993	57.417345
2599.211894	189833.239433	57.422349
2599.147167	189626.731615	57.427354
2598.066448	189436.505483	57.432359
2597.789595	189235.478334	57.437364
2597.198599	189039.998022	57.442369
2596.335130	188844.090950	57.447373
2596.075186	188636.295202	57.452378
2595.125425	188441.764787	57.457383
2594.485214	188241.740897	57.462388
2593.927572	188036.577628	57.467393
2593.087686	187837.006939	57.472397
2592.637527	187629.156720	57.477402
2591.723110	187438.899567	57.482407
2590.942749	187235.836110	57.487412
2590.842638	187025.808501	57.492417
2589.696098	186834.318386	57.497421
2589.213278	186633.271402	57.502426
2588.068558	186425.231295	57.507431
2587.692502	186234.512121	57.512436
2587.329080	186027.164217	57.517441
2586.479107	185841.699579	57.522445
2585.827305	185630.429951	57.527450
2584.845183	185446.756183	57.532455
2584.057659	185243.944361	57.537460
2583.577598	185048.806746	57.542465
2582.756369	184845.582229	57.547469
2581.711732	184643.628012	57.552474
2581.106224	184457.087122	57.557479
2580.845248	184269.767290	57.562484
2580.261147	184079.688022	57.567489
2579.508676	183887.244635	57.572493
2579.252176	183680.590189	57.577498
2578.689737	183486.591865	57.582503
2577.487688	183296.499353	57.587508
2576.834337	183088.918286	57.592513
2576.351242	182897.174308	57.597517
2575.832733	182702.574556	57.602522
2574.741482	182501.642365	57.607527
2574.523149	182313.166398	57.612532
2573.924942	182114.371270	57.617537
2573.220503	181917.667355	57.622541
2572.615769	181718.099092	57.627546
2571.978617	181517.417463	57.632551
2571.193007	181311.850148	57.637556
2570.883987	181111.970664	57.642561
2569.946199	180919.722235	57.647565
2569.283593	180710.538389	57.652570
2568.562755	180507.330610	57.657575
2568.161518	180312.811958	57.662580
2567.460765	180112.464914	57.667585
2566.829873	179909.881709	57.672589
2566.377989	179707.970698	57.677594
2565.562190	179501.742620	57.682599
2564.414377	179292.477201	57.687604
2564.304633	179091.468882	57.692609
2563.289649	178898.224144	57.697613
2562.982307	178677.635108	57.702618
2561.954154	178482.384629	57.707623
2561.357824	178277.717677	57.712628
2560.713954	178076.646177	57.717633
2559.918296	177883.918264	57.722637
2559.557474	177677.194506	57.727642
2558.563474	177476.079609	57.732647
2557.935579	177278.456362	57.737652
2557.363806	177075.546652	57.742657
2556.500068	176878.013553	57.747661
2555.866091	176674.556010	57.752666
2555.274272	176485.083798	57.757671
2554.588791	176276.167156	57.762676
2554.313886	176080.566874	57.767681
2553.262752	175887.608875	57.772685
2552.525899	175676.185067	57.777690
2551.994834	175473.798236	57.782695
2551.447295	175276.286289	57.787700
2550.777085	175079.430670	57.792705
2549.704818	174887.778034	57.797709
2549.149937	174677.551537	57.802714
2548.921174	174491.172479	57.807719
2548.242674	174291.205956	57.812724
2547.493759	174083.671435	57.817729
2546.345798	173896.257976	57.822733
2546.378719	173684.442722	57.827738
2545.526725	173486.199205	57.832743
2544.835462	173287.397035	57.837748
2544.243554	173079.321368	57.842753
2543.251147	172884.791311	57.847757
2542.749285	172670.878665	57.852762
2542.169528	172484.589962	57.857767
2541.359265	172284.692470	57.862772
2541.084574	172080.043705	57.867777
2540.149700	171885.649312	57.872781
2539.565945	171685.350136	57.877786
2538.766489	171483.547338	57.882791
2538.219566	171278.933146	57.887796
2537.576337	171077.107673	57.892801
2537.011435	170869.611612	57.897805
2536.460040	170670.533341	57.902810
2535.561051	170468.281000	57.907815
2534.780981	170274.187982	57.912820
2534.359163	170062.731219	57.917825
2533.501014	169870.191357	57.922829
2532.953504	169667.137177	57.927834
2532.406944	169457.000613	57.932839
2531.467957	169262.670789	57.937844
2530.936543	169058.472744	57.942849
2530.012817	168869.915884	57.947853
2529.718114	168662.376091	57.952858
2528.960224	168464.244770	57.957863
2528.164860	168251.966976	57.962868
2527.509610	168045.225225	57.967873
2526.890886	167855.963773	57.972877
2526.249458	167654.028732	57.977882
2525.893531	167456.411177	57.982887
2525.037986	167251.867239	57.987892
2524.208256	167049.647357	57.992897
2523.665677	166855.521293	57.997901
2522.880340	166648.197409	58.002906
2522.298756	166447.899683	58.007911
2521.747257	166247.216783	58.012916
2521.394862	166043.019291	58.017921
2520.444007	165844.220192	58.022925
2519.924630	165633.172230	58.027930
2519.042509	165430.676921	58.032935
2518.570493	165234.500876	58.037940
2517.967242	165020.621419	58.042945
2517.242141	164825.034411	58.047949
2516.750579	164617.687967	58.052954
2516.087313	164410.649635	58.057959
2515.263082	164202.086733	58.062964
2514.743362	164009.802854	58.067969
2514.101176	163733.811424	58.072973
2513.684069	163520.381625	58.077978
2512.864543	163305.974238	58.082983
2512.032815	163103.788887	58.087988
2511.463260	162887.869434	58.092993
2510.975334	162679.452636	58.097997
2510.388102	162464.593809	58.103002
2509.781910	162260.266803	58.108007
2508.849212	162047.919088	58.113012
2508.234978	161826.291587	58.118017
2507.210371	161630.832738	58.123021
2506.721783	161420.312752	58.128026
2506.156714	161215.845299	58.133031
2505.253363	161003.638957	58.138036
2504.888912	160786.428184	58.143041
2504.014625	160596.100290	58.148045
2503.323188	160380.405906	58.153050
2502.602949	160169.446885	58.158055
2501.907140	159974.199267	58.163060
2501.388027	159756.625174	58.168065
2500.205381	159564.114109	58.173069
2499.851558	159359.700129	58.178074
2499.353131	159159.124248	58.183079
2498.586543	158958.185189	58.188084
2498.034081	158743.470405	58.193089
2496.955808	158549.766027	58.198093
2496.676799	158343.095888	58.203098
2495.922523	158136.082771	58.208103
2494.957061	157939.668754	58.213108
2494.426491	157724.448249	58.218113
2493.355483	157528.574509	58.223117
2492.947694	157331.287354	58.228122
2492.436561	157140.602821	58.233127
2491.777867	156940.052393	58.238132
2491.478574	156732.136517	58.243137
2490.641873	156542.129801	58.248141
2490.125710	156328.962391	58.253146
2489.432381	156125.689057	58.258151
2488.587778	155926.343531	58.263156
2488.048127	155717.404076	58.268161
2487.169573	155522.451947	58.273165
2486.602025	155313.748201	58.278170
2486.350649	155112.953227	58.283175
2485.459544	154905.663435	58.288180
2484.685178	154695.953901	58.293185
2484.160530	154493.807620	58.298189
2483.661133	154289.802664	58.303194
2482.900076	154083.793872	58.308199
2481.777290	153886.220467	58.313204
2481.484967	153672.818146	58.318209
2480.654568	153470.243441	58.323213
2479.898038	153273.721465	58.328218
2479.443860	153072.767403	58.333223
2478.403369	152863.505523	58.338228
2477.983499	152661.404511	58.343233
2477.035602	152461.206069	58.348237
2476.520564	152257.737114	58.353242
2476.226226	152063.729299	58.358247
2475.052244	151871.044133	58.363252
2474.660456	151660.301558	58.368257
2473.697192	151467.115060	58.373261
2473.152796	151263.606033	58.378266
2472.806556	151063.549474	58.383271
2472.146750	150872.402855	58.388276
2471.663663	150655.071874	58.393281
2470.685085	150462.541929	58.398285
2470.124097	150254.707660	58.403290
2469.471828	150046.520596	58.408295
2468.565726	149848.987794	58.413300
2467.999810	149651.148075	58.418305
2467.207732	149444.626580	58.423309
2466.446227	149242.613457	58.428314
2466.103663	149045.809632	58.433319
2465.422625	148847.370303	58.438324
2464.584942	148635.942652	58.443329
2463.733739	148451.284247	58.448333
2463.453438	148239.211643	58.453338
2462.674232	148045.863781	58.458343
2461.842220	147854.736827	58.463348
2461.348465	147656.783523	58.468353
2460.704915	147449.272696	58.473357
2460.054904	147247.165479	58.478362
2459.465946	147042.902093	58.483367
2458.773422	146852.521555	58.488372
2458.271204	146659.887994	58.493377
2457.178370	146464.362730	58.498381
2456.475535	146259.512430	58.503386
2456.166244	146052.504203	58.508391
2455.498954	145860.308341	58.513396
2454.621264	145656.290292	58.518401
2454.192343	145462.419722	58.523405
2453.350231	145263.481813	58.528410
2452.942684	145062.328644	58.533415
2452.333040	144858.730774	58.538420
2451.854994	144656.498513	58.543425
2450.658256	144452.881981	58.548429
2450.448415	144253.939224	58.553434
2449.876659	144046.909596	58.558439
2448.831549	143849.461532	58.563444
2448.195770	143644.096704	58.568449
2447.511257	143446.708411	58.573453
2446.953895	143234.205102	58.578458
2445.963173	143037.198350	58.583463
2445.098122	142848.648512	58.588468
2445.151734	142643.879938	58.593473
2444.237119	142453.281857	58.598477
2443.658156	142242.796495	58.603482
2443.189786	142042.905120	58.608487
2442.581381	141848.183419	58.613492
2442.026650	141642.399784	58.618497
2441.001352	141436.374472	58.623501
2440.513032	141229.719058	58.628506
2439.744749	141016.311584	58.633511
2439.129566	140818.090618	58.638516
2438.402179	140612.989332	58.643521
2437.688486	140416.628990	58.648525
2436.889482	140217.183204	58.653530
2436.457191	140014.110266	58.658535
2435.741859	139807.081255	58.663540
2435.202076	139600.661123	58.668545
2434.712454	139404.805490	58.673549
2433.858757	139193.546275	58.678554
2433.281663	138987.847781	58.683559
2432.433691	138777.340214	58.688564
2431.859826	138570.526013	58.693569
2431.369907	138378.907982	58.698573
2430.420937	138177.187208	58.703578
2430.023754	137964.873329	58.708583
2429.230600	137758.531504	58.713588
2428.619801	137556.901091	58.718593
2427.539591	137356.489889	58.723597
2427.037324	137152.253272	58.728602
2426.399020	136949.665813	58.733607
2425.327799	136753.856319	58.738612
2424.974078	136535.307940	58.743617
2424.170108	136352.938062	58.748621
2423.548536	136155.130230	58.753626
2423.191725	135946.292722	58.758631
2422.026052	135756.285224	58.763636
2421.686943	135546.977715	58.768641
2421.105043	135358.074433	58.773645
2420.631492	135150.518804	58.778650
2420.079389	134955.363172	58.783655
2418.993705	134755.847190	58.788660
2418.690980	134545.994861	58.793665
2417.626948	134343.797852	58.798669
2416.899258	134143.772015	58.803674
2416.091271	133950.645436	58.808679
2415.499318	133750.054572	58.813684
2415.132399	133551.563541	58.818689
2414.002281	133357.983886	58.823693
2413.669692	133166.438590	58.828698
2413.074821	132966.526911	58.833703
2412.094808	132777.589302	58.838708
2411.807423	132569.616249	58.843713
2410.927839	132375.279475	58.848717
2410.645179	132180.849394	58.853722
2409.835818	131975.453103	58.858727
2409.381137	131778.271231	58.863732
2408.768898	131567.714928	58.868737
2408.222249	131380.699425	58.873741
2407.180663	131169.731468	58.878746
2406.715545	130961.417303	58.883751
2405.982367	130756.652867	58.888756
2405.748683	130551.378873	58.893761
2404.584712	130349.035512	58.898765
2403.953249	130143.192479	58.903770
2403.381714	129938.738612	58.908775
2402.902574	129739.783967	58.913780
2402.260444	129529.425458	58.918785
2401.273740	129332.586376	58.923789
2400.846994	129124.495680	58.928794
2400.203333	128925.255394	58.933799
2399.549033	128724.583022	58.938804
2399.148306	128504.045988	58.943809
2398.066033	128302.809477	58.948813
2397.475501	128105.243142	58.953818
2396.555969	127884.450375	58.958823
2396.044443	127697.619041	58.963828
2395.728400	127489.256354	58.968833
2394.677853	127288.911223	58.973837
2394.299548	127086.479755	58.978842
2393.542126	126882.839882	58.983847
2393.056179	126679.221979	58.988852
2392.336138	126461.596687	58.993857
2391.653700	126262.877068	58.998861
2391.112861	126053.405246	59.003866
2390.397623	125849.842571	59.008871
2389.620526	125647.840558	59.013876
2389.124130	125431.242082	59.018881
2388.257060	125222.615734	59.023885
2387.523575	125010.363252	59.028890
2387.261545	124804.857079	59.033895
2386.238716	124607.155960	59.038900
2385.496690	124394.071536	59.043905
2384.846283	124180.745692	59.048909
2384.025381	123981.848856	59.053914
2383.658600	123776.443315	59.058919
2382.922265	123578.590037	59.063924
2382.311582	123376.578622	59.068929
2381.584823	123168.618940	59.073933
2380.880493	122962.422366	59.078938
2380.702543	122749.934562	59.083943
2379.646110	122552.457076	59.088948
2379.058602	122339.186713	59.093953
2378.131598	122131.838265	59.098957
2377.743348	121922.006153	59.103962
2376.844057	121728.484252	59.108967
2376.047882	121521.056347	59.113972
2375.924293	121313.371061	59.118977
2374.922631	121122.002990	59.123981
2374.400229	120907.933891	59.128986
2373.858677	120697.805668	59.133991
2372.996437	120495.843354	59.138996
2372.532732	120287.521738	59.144001
2371.848887	120093.012714	59.149005
2371.103336	119880.409405	59.154010
2370.473978	119664.170867	59.159015
2369.499550	119464.214960	59.164020
2369.035822	119254.073273	59.169025
2368.616978	119049.906120	59.174029
2367.789065	118844.897649	59.179034
2367.469376	118634.693683	59.184039
2366.403536	118427.840855	59.189044
2365.823635	118223.223285	59.194049
2364.956265	118012.831886	59.199053
2364.334401	117798.461260	59.204058
2363.847987	117603.298411	59.209063
2363.247364	117399.382557	59.214068
2362.840441	117187.223684	59.219073
2361.796430	116991.246161	59.224077
2360.895550	116780.273457	59.229082
2360.617399	116571.114362	59.234087
2359.982035	116360.940884	59.239092
2359.361799	116151.046021	59.244097
2358.524505	115945.941492	59.249101
2357.665127	115741.711698	59.254106
2357.083249	115518.226311	59.259111
2356.256940	115321.579646	59.264116
2356.100162	115124.752177	59.269121
2355.121791	114924.698869	59.274125
2354.676200	114702.855645	59.279130
2354.100027	114495.201628	59.284135
2353.203498	114284.629727	59.289140
2352.701421	114088.836144	59.294145
2352.113341	113872.912742	59.299149
2351.099004	113664.725734	59.304154
2350.881513	113448.956652	59.309159
2350.017832	113253.220556	59.314164
2349.428182	113027.790939	59.319169
2348.386496	112834.751931	59.324173
2347.959867	112624.969871	59.329178
2347.586039	112410.408630	59.334183
2346.748865	112207.771518	59.339188
2346.034916	111985.169797	59.344193
2344.969090	111791.774596	59.349197
2344.693305	111580.365434	59.354202
2344.180149	111366.323945	59.359207
2343.023697	111169.241764	59.364212
2342.645981	110949.318527	59.369217
2341.933557	110762.056451	59.374221
2341.450568	110549.965484	59.379226
2341.019769	110327.746242	59.384231
2340.282415	110134.400755	59.389236
2339.812678	109908.510837	59.394241
2338.903581	109710.271531	59.399245
2338.313549	109486.149670	59.404250
2337.803623	109270.399816	59.409255
2336.860000	109067.462679	59.414260
2336.276841	108849.240660	59.419265
2335.294937	108636.636157	59.424269
2334.820344	108435.063994	59.429274
2334.398169	108218.630552	59.434279
2333.473066	108017.761478	59.439284
2333.250923	107799.091862	59.444289
2332.408318	107591.068418	59.449293
2331.715533	107376.036935	59.454298
2331.417242	107158.685937	59.459303
2330.270262	106953.723836	59.464308
2329.850613	106726.599152	59.469313
2329.376517	106522.435011	59.474317
2328.229491	106310.054770	59.479322
2327.860549	106077.560365	59.484327
2326.856681	105882.685711	59.489332
2326.566608	105663.564012	59.494337
2325.682532	105449.519094	59.499341
2325.133708	105230.137847	59.504346
2324.989480	105022.552474	59.509351
2323.840191	104806.150781	59.514356
2323.023870	104587.871048	59.519361
2322.493848	104383.892625	59.524365
2321.587972	104158.436476	59.529370
2320.820712	103952.329612	59.534375
2320.110039	103725.666584	59.539380
2319.707210	103515.115525	59.544385
2319.163298	103309.651321	59.549389
2318.121200	103104.515322	59.554394
2318.030964	102887.214611	59.559399
2317.011946	102668.432790	59.564404
2316.649992	102457.383516	59.569409
2315.896517	102249.246605	59.574413
2315.079502	102034.619242	59.579418
2314.584975	101820.164736	59.584423
2314.119798	101606.988960	59.589428
2313.570985	101395.211295	59.594433
2312.649529	101175.305124	59.599437
2312.062539	100951.827354	59.604442
2311.443095	100729.904670	59.609447
2310.503360	100523.937714	59.614452
2310.038923	100295.885929	59.619457
2309.459905	100082.285440	59.624461
2308.847919	99876.031218	59.629466
2308.287396	99651.337530	59.634471
2307.499341	99430.519665	59.639476
2306.719417	99214.935605	59.644481
2306.053086	98993.925012	59.649485
2305.399426	98778.788045	59.654490
2304.905929	98549.064558	59.659495
2303.855728	98347.644278	59.664500
2303.309166	98115.624775	59.669505
2302.605600	97912.218826	59.674509
2301.725220	97692.878422	59.679514
2301.332118	97466.460698	59.684519
2300.999426	97260.046122	59.689524
2300.363182	97034.235725	59.694529
2299.709322	96818.203914	59.699533
2298.984378	96604.620866	59.704538
2298.375929	96371.176532	59.709543
2297.453912	96149.815401	59.714548
2296.971073	95937.842857	59.719553
2296.550140	95710.394248	59.724557
2295.494764	95501.275377	59.729562
2295.303534	95282.305586	59.734567
2294.051973	95058.438933	59.739572
2293.434112	94831.157255	59.744577
2293.152402	94609.570169	59.749581
2292.279992	94388.928728	59.754586
2291.626991	94167.290740	59.759591
2290.767436	93955.383916	59.764596
2289.992956	93733.623631	59.769601
2289.687868	93511.137940	59.774605
2288.871691	93303.073322	59.779610
2288.449273	93080.439317	59.784615
2287.376995	92853.820504	59.789620
2286.982604	92635.092706	59.794625
2286.332094	92420.383551	59.799629
2285.597976	92207.687163	59.804634
2285.223761	91979.076946	59.809639
2284.259257	91757.112868	59.814644
2283.686482	91543.680751	59.819649
2283.059780	91318.617557	59.824653
2282.145677	91100.507290	59.829658
2281.720274	90876.805304	59.834663
2280.897023	90661.386104	59.839668
2280.513227	90439.178353	59.844673
2279.749056	90224.470551	59.849677
2278.777011	90007.115827	59.854682
2278.685523	89770.526490	59.859687
2277.659667	89563.931588	59.864692
2276.793599	89332.624486	59.869697
2276.540351	89117.491476	59.874701
2275.583675	88909.471610	59.879706
2275.475634	88672.288158	59.884711
2274.291644	88449.124397	59.889716
2273.894309	88233.693302	59.894721
2273.336990	88006.960443	59.899725
2272.241685	87789.152911	59.904730
2271.916913	87561.512950	59.909735
2270.864339	87349.142540	59.914740
2269.938191	87133.780910	59.919745
2269.631791	86909.638018	59.924750
2269.036477	86689.771688	59.929754
2268.571063	86479.180533	59.934759
2267.584492	86265.200152	59.939764
2266.989158	86047.261217	59.944769
2266.990643	85832.703720	59.949774
2265.858700	85594.714903	59.954778
2265.181100	85375.534373	59.959783
2264.533528	85148.446614	59.964788
2263.941917	84932.413814	59.969793
2263.315743	84706.740949	59.974798
2262.532644	84488.961803	59.979802
2261.928214	84259.797562	59.984807
2260.813637	84048.192379	59.989812
2260.674378	83819.523259	59.994817
2260.020789	83594.082088	59.999822
2259.165222	83380.287408	60.004826
2258.632661	83146.236873	60.009831
2257.945354	82941.838794	60.014836
2257.437005	82715.585343	60.019841
2256.816714	82495.468433	60.024846
2255.753699	82269.707057	60.029850
2255.043482	82041.800597	60.034855
2254.284173	81830.034582	60.039860
2253.687308	81612.661231	60.044865
2253.186542	81387.479331	60.049870
2252.138629	81178.972638	60.054874
2251.968176	80951.252299	60.059879
2251.136985	80741.961413	60.064884
2250.568123	80516.007512	60.069889
2249.856088	80299.680124	60.074894
2249.112651	80075.824731	60.079898
2248.702163	79850.429659	60.084903
2247.361242	79640.020282	60.089908
2247.107792	79430.974182	60.094913
2246.419858	79205.725191	60.099918
2245.776007	78993.228297	60.104922
2245.322500	78767.275172	60.109927
2244.629021	78555.456051	60.114932
2243.456620	78339.044756	60.119937
2243.021179	78121.435250	60.124942
2242.499031	77909.323125	60.129946
2241.981949	77678.265583	60.134951
2241.126557	77471.945573	60.139956
2240.653282	77250.929508	60.144961
2240.190160	77022.050600	60.149966
2238.996296	76821.949932	60.154970
2238.720763	76597.557587	60.159975
2237.872051	76378.650831	60.164980
2237.318590	76160.168481	60.169985
2236.616005	75939.684554	60.174990
2235.860703	75725.813612	60.179994
2235.548208	75501.705336	60.184999
2234.617028	75290.059160	60.190004
2233.904176	75070.758466	60.195009
2233.417953	74841.236174	60.200014
2232.913527	74623.643292	60.205018
2232.117178	74396.234375	60.210023
2231.541229	74188.078725	60.215028
2230.861781	73963.285443	60.220033
2230.304617	73735.446913	60.225038
2229.644062	73518.359570	60.230042
2228.972682	73287.623610	60.235047
2227.950007	73071.922628	60.240052
2227.501501	72839.154535	60.245057
2226.665434	72624.398068	60.250062
2225.710096	72410.023929	60.255066
2225.319899	72193.497242	60.260071
2224.710600	71978.325327	60.265076
2224.384688	71755.825693	60.270081
2223.569272	71531.733807	60.275086
2222.893894	71304.613246	60.280090
2222.340255	71081.523814	60.285095
2221.309449	70866.342121	60.290100
2220.535326	70655.486532	60.295105
2220.038933	70426.453632	60.300110
2219.262388	70210.516623	60.305114
2218.680608	69993.778298	60.310119
2217.805994	69781.180720	60.315124
2217.169118	69569.041794	60.320129
2216.675730	69345.500030	60.325134
2215.589659	69131.486179	60.330138
2215.253973	68911.952775	60.335143
2214.631332	68698.307184	60.340148
2213.972833	68488.906934	60.345153
2213.518633	68268.626814	60.350158
2212.874111	68058.722256	60.355162
2212.202725	67831.299132	60.360167
2211.606146	67620.143969	60.365172
2210.932972	67399.199044	60.370177
2210.330955	67178.137673	60.375182
2209.344596	66965.284431	60.380186
2208.649567	66731.145602	60.385191
2208.053885	66525.550111	60.390196
2207.475412	66315.799554	60.395201
2206.980406	66095.414360	60.400206
2206.139732	65876.619087	60.405210
2205.478628	65656.851043	60.410215
2204.865512	65448.901268	60.415220
2204.283158	65228.780472	60.420225
2203.531997	65013.381486	60.425230
2202.975463	64796.098586	60.430234
2202.256905	64573.261715	60.435239
2201.621362	64359.254382	60.440244
2200.687767	64136.070422	60.445249
2200.339987	63922.430760	60.450254
2198.900636	63710.549702	60.455258
2198.773756	63484.009605	60.460263
2198.156363	63280.725504	60.465268
2197.212186	63067.360980	60.470273
2196.584701	62846.201453	60.475278
2195.813878	62645.652218	60.480282
2195.262782	62423.953605	60.485287
2194.339513	62220.893977	60.490292
2193.750518	62004.670579	60.495297
2193.102226	61799.419075	60.500302
2192.347519	61586.386215	60.505306
2191.890838	61381.295631	60.510311
2190.943614	61170.754608	60.515316
2190.404453	60963.566957	60.520321
2189.961420	60760.348698	60.525326
2188.926208	60561.705894	60.530330
2188.397741	60353.355152	60.535335
2187.626123	60140.331819	60.540340
2187.058720	59931.517101	60.545345
2186.489039	59724.908228	60.550350
2185.841669	59528.345187	60.555354
2185.239714	59310.553063	60.560359
2184.281720	59116.420832	60.565364
2183.562720	58908.850734	60.570369
2183.115258	58704.253220	60.575374
2182.235404	58504.426941	60.580378
2181.649212	58304.723977	60.585383
2181.062834	58104.681345	60.590388
2180.390918	57895.912292	60.595393
2179.972973	57691.058522	60.600398
2179.091390	57493.892578	60.605402
2178.731948	57283.656555	60.610407
2177.651367	57081.934085	60.615412
2176.787210	56870.285773	60.620417
2176.503143	56668.542733	60.625422
2175.391681	56482.346244	60.630426
2174.471962	56284.806792	60.635431
2173.777758	56084.211260	60.640436
2173.566753	55887.576384	60.645441
2172.925253	55689.128863	60.650446
2171.661142	55502.687998	60.655450
2171.190084	55298.878739	60.660455
2170.642819	55120.407526	60.665460
2170.094194	54932.735489	60.670465
2169.391370	54730.222515	60.675470
2168.527218	54555.595109	60.680474
2167.530098	54355.873489	60.685479
2166.893705	54170.400401	60.690484
2165.731367	53988.205591	60.695489
2164.918569	53807.159640	60.700494
2164.344900	53636.200516	60.705498
2163.488076	53463.670916	60.710503
2162.432364	53299.594859	60.715508
2161.875939	53130.691417	60.720513
2161.078333	52969.229104	60.725518
2159.893237	52824.106723	60.730522
2159.459162	52658.849328	60.735527
2158.565732	52501.785697	60.740532
2157.863964	52352.233291	60.745537
2157.089845	52199.662328	60.750542
2156.180291	52062.048881	60.755546
2155.594068	51915.187100	60.760551
2154.691282	51780.479384	60.765556
2153.936137	51647.378747	60.770561
2153.768455	51497.830948	60.775566
2152.815185	51367.041923	60.780570
2151.872375	51222.919113	60.785575
2151.194130	51074.085466	60.790580
2150.547334	50944.570267	60.795585
2149.841113	50813.730252	60.800590
2148.990640	50688.064906	60.805594
2148.574450	50557.731262	60.810599
2147.886973	50427.296067	60.815604
2146.875022	50306.638919	60.820609
2146.360701	50174.188044	60.825614
2145.712855	50052.560501	60.830618
2144.958177	49919.466265	60.835623
2144.584592	49800.948030	60.840628
2143.563761	49682.523777	60.845633
2143.540962	49556.912224	60.850638
2142.678317	49424.727800	60.855642
2142.126607	49300.771146	60.860647
2141.497208	49180.016621	60.865652
2140.631745	49059.006150	60.870657
2140.289221	48922.858012	60.875662
2139.286393	48800.365225	60.880666
2138.496513	48671.237180	60.885671
2138.033560	48547.366592	60.890676
2137.341043	48421.533957	60.895681
2136.505833	48294.778973	60.900686
2135.754734	48185.135335	60.905690
2135.193259	48066.639463	60.910695
2134.982345	47943.232924	60.915700
2133.936327	47826.175804	60.920705
2133.432842	47696.167951	60.925710
2132.618221	47572.673135	60.930714
2132.295116	47445.311534	60.935719
2131.403574	47327.625846	60.940724
2130.855247	47201.130522	60.945729
2130.123374	47078.679401	60.950734
2129.331439	46964.020225	60.955738
2128.850350	46837.026539	60.960743
2128.115456	46726.680809	60.965748
2127.263654	46615.152313	60.970753
2126.913556	46483.038190	60.975758
2125.982930	46371.447827	60.980762
2125.729068	46245.570568	60.985767
2125.278841	46126.899248	60.990772
2124.282425	45994.255558	60.995777
2123.929079	45870.206041	61.000782
2123.062448	45760.545187	61.005786
2122.244668	45631.934051	61.010791
2121.692216	45511.755377	61.015796
2120.961436	45391.488791	61.020801
2120.679529	45264.952460	61.025806
2119.869326	45144.908922	61.030810
2119.254675	45017.007029	61.035815
2118.871220	44892.305000	61.040820
2117.949624	44770.880554	61.045825
2117.213120	44651.815516	61.050830
2116.416397	44535.781319	61.055834
2115.825983	44401.216065	61.060839
2115.067118	44274.133186	61.065844
2114.296581	44158.486364	61.070849
2113.892226	44035.447880	61.075854
2112.914257	43925.670720	61.080858
2112.562660	43802.157434	61.085863
2111.853383	43670.668656	61.090868
2111.346566	43553.367899	61.095873
2110.689387	43423.656443	61.100878
2109.803468	43313.334066	61.105882
2109.459389	43185.952967	61.110887
2109.111032	43061.302747	61.115892
2108.264382	42943.424361	61.120897
2107.396911	42810.183544	61.125902
2106.622502	42699.227534	61.130906
2106.059824	42561.500164	61.135911
2105.239706	42451.625063	61.140916
2104.682264	42333.502548	61.145921
2103.954526	42203.156806	61.150926
2103.074565	42090.763594	61.155930
2102.891464	41960.355402	61.160935
2102.530757	41846.942174	61.165940
2101.734906	41719.728929	61.170945
2100.757273	41593.952676	61.175950
2100.080362	41466.080492	61.180954
2099.678091	41349.973411	61.185959
2098.857833	41225.363875	61.190964
2098.437545	41107.161590	61.195969
2097.690866	40971.793981	61.200974
2096.743945	40852.080127	61.205978
2096.263616	40733.532618	61.210983
2095.597108	40604.950551	61.215988
2094.470460	40489.846442	61.220993
2094.027800	40364.282052	61.225998
2093.629251	40253.203112	61.231002
2092.732882	40119.497584	61.236007
2092.174253	40005.141369	61.241012
2091.504920	39888.381429	61.246017
2091.044870	39759.157952	61.251022
2090.110849	39643.747560	61.256026
2089.262467	39517.437989	61.261031
2088.898074	39388.412404	61.266036
2087.987756	39278.396435	61.271041
2087.410604	39168.370996	61.276046
2086.462079	39048.707962	61.281050
2086.020352	38928.032628	61.286055
2085.676299	38810.738372	61.291060
2084.569373	38688.409193	61.296065
2083.851407	38571.593266	61.301070
2083.384783	38461.135933	61.306074
2082.711593	38335.910756	61.311079
2082.234973	38212.459028	61.316084
2081.639884	38100.883069	61.321089
2081.242516	37989.959375	61.326094
2080.495988	37865.163478	61.331098
2080.057849	37743.466892	61.336103
2079.223033	37619.229023	61.341108
2078.464715	37494.176904	61.346113
2077.861599	37364.771430	61.351118
2077.106102	37244.840730	61.356122
2076.466739	37117.202255	61.361127
2076.123454	36987.532395	61.366132
2075.341026	36872.774359	61.371137
2074.473093	36750.604616	61.376142
2073.709474	36633.006319	61.381146
2072.803462	36507.257835	61.386151
2072.337119	36373.303339	61.391156
2071.443215	36264.873923	61.396161
2071.341203	36148.670886	61.401166
2070.324246	36022.184930	61.406170
2069.547626	35911.817151	61.411175
2069.234289	35786.215518	61.416180
2068.297564	35670.154565	61.421185
2067.838254	35547.460864	61.426190
2067.103481	35429.999170	61.431194
2066.436181	35299.745695	61.436199
2065.657837	35182.646691	61.441204
2064.698855	35061.575280	61.446209
2064.425454	34941.777321	61.451214
2063.843218	34834.004703	61.456218
2063.181996	34710.204888	61.461223
2062.397494	34593.713150	61.466228
2061.430759	34473.797816	61.471233
2061.009949	34359.103893	61.476238
2060.393148	34246.194577	61.481242
2059.644790	34126.247086	61.486247
2058.896284	34008.408770	61.491252
2058.676251	33894.699231	61.496257
2057.734231	33768.024035	61.501262
2057.117613	33657.364431	61.506266
2056.365203	33546.090218	61.511271
2055.739968	33426.610244	61.516276
2055.189137	33308.216092	61.521281
2054.530976	33181.727888	61.526286
2053.736465	33066.104971	61.531290
2053.207379	32954.173469	61.536295
2052.437608	32836.098724	61.541300
2051.410614	32724.437425	61.546305
2051.154260	32602.626044	61.551310
2050.401528	32503.778393	61.556314
2049.755721	32379.873366	61.561319
2049.120552	32267.994938	61.566324
2048.480493	32139.144586	61.571329
2047.771389	32027.369593	61.576334
2046.949679	31915.507351	61.581338
2046.437430	31799.998605	61.586343
2045.756251	31689.077947	61.591348
2044.810200	31578.667805	61.596353
2044.388817	31463.687419	61.601358
2043.698585	31351.493680	61.606362
2042.993630	31252.859259	61.611367
2042.668420	31130.361740	61.616372
2042.035770	31010.347336	61.621377
2041.216851	30886.188669	61.626382
2040.254342	30779.509282	61.631386
2039.438206	30663.031235	61.636391
2038.775171	30555.316633	61.641396
2037.648826	30445.547887	61.646401
2037.337120	30333.252040	61.651406
2036.592239	30245.146988	61.656410
2036.090955	30128.099769	61.661415
2035.716785	30026.669338	61.666420
2034.706293	29912.099822	61.671425
2034.009615	29804.755736	61.676430
2033.275168	29694.620145	61.681434
2032.810264	29586.250041	61.686439
2032.067647	29488.504365	61.691444
2031.103807	29389.577793	61.696449
2030.634738	29285.029170	61.701454
2029.987228	29184.503684	61.706458
2029.162847	29088.749912	61.711463
2028.428956	28979.066183	61.716468
2027.683284	28878.487064	61.721473
2027.494063	28768.841544	61.726478
2026.597535	28681.143433	61.731482
2026.077531	28577.522198	61.736487
2025.698956	28469.062075	61.741492
2024.530742	28374.144380	61.746497
2024.280892	28269.467944	61.751502
2023.419091	28168.575127	61.756506
2022.681552	28069.473732	61.761511
2022.034221	27965.615925	61.766516
2021.225807	27863.880790	61.771521
2020.826751	27750.842442	61.776526
2019.705885	27660.526599	61.781530
2019.234782	27565.381354	61.786535
2018.694818	27457.667667	61.791540
2018.134110	27370.135034	61.796545
2017.504748	27268.471585	61.801550
2016.444713	27167.302083	61.806554
2015.635823	27075.721989	61.811559
2015.399986	26975.476581	61.816564
2014.562181	26887.707759	61.821569
2013.545843	26789.135525	61.826574
2012.935181	26690.430790	61.831578
2012.132482	26595.132192	61.836583
2011.864238	26502.115731	61.841588
2010.786056	26413.510902	61.846593
2010.154506	26323.346032	61.851598
2009.494500	26233.792778	61.856602
2008.710375	26149.142479	61.861607
2008.062282	26057.804076	61.866612
2007.243450	25979.495406	61.871617
2007.026620	25886.737345	61.876622
2006.059796	25799.500411	61.881626
2005.383417	25713.534472	61.886631
2005.051234	25622.404302	61.891636
2004.434155	25535.988397	61.896641
2003.649036	25442.264753	61.901646
2003.093788	25349.690656	61.906650
2002.465486	25260.917314	61.911655
2001.785788	25173.758257	61.916660
2001.041524	25086.918726	61.921665
2000.338185	24994.337011	61.926670
1999.985156	24916.062268	61.931674
1999.104209	24823.806681	61.936679
1998.354998	24733.236611	61.941684
1997.629783	24648.194729	61.946689
1997.162859	24557.478181	61.951694
1996.263885	24471.314932	61.956698
1995.733401	24378.774890	61.961703
1995.184557	24285.302452	61.966708
1994.395340	24212.253452	61.971713
1993.639887	24117.433534	61.976718
1993.015972	24032.085859	61.981722
1992.048817	23948.639499	61.986727
1991.637879	23873.135982	61.991732
1990.847761	23791.484236	61.996737
1990.314511	23704.421290	62.001742
1989.605132	23620.458746	62.006746
1988.854605	23534.468103	62.011751
1988.279153	23448.232969	62.016756
1987.627351	23368.928171	62.021761
1987.128614	23288.346229	62.026766
1986.247141	23197.024859	62.031770
1985.505474	23119.516316	62.036775
1985.090369	23037.235603	62.041780
1984.123391	22947.361720	62.046785
1983.249102	22872.688260	62.051790
1982.840139	22802.988073	62.056794
1982.305130	22716.143231	62.061799
1981.654795	22635.288587	62.066804
1980.646612	22562.261384	62.071809
1980.192663	22476.361263	62.076814
1979.593385	22396.913210	62.081818
1979.067687	22317.856595	62.086823
1978.383705	22236.134398	62.091828
1977.459505	22156.519602	62.096833
1976.893631	22073.351834	62.101838
1976.157335	21999.038821	62.106842
1975.562025	21908.608840	62.111847
1975.369212	21832.057829	62.116852
1974.252987	21761.564834	62.121857
1973.995444	21682.473565	62.126862
1973.187112	21601.089440	62.131866
1972.162342	21518.297479	62.136871
1971.817719	21426.163608	62.141876
1971.218443	21351.772669	62.146881
1970.348650	21273.545745	62.151886
1969.780975	21193.782088	62.156890
1969.191949	21109.501058	62.161895
1968.669617	21027.287279	62.166900
1967.542178	20950.749918	62.171905
1967.298753	20865.913951	62.176910
1966.542356	20787.771714	62.181914
1965.597472	20710.880451	62.186919
1965.027251	20641.880982	62.191924
1964.443225	20558.183223	62.196929
1964.024696	20478.075796	62.201934
1963.241942	20402.403064	62.206938
1962.518031	20327.568540	62.211943
1961.923411	20245.566123	62.216948
1960.942460	20162.132439	62.221953
1960.336815	20074.975402	62.226958
1959.819837	20002.204213	62.231962
1959.060383	19938.133350	62.236967
1958.365155	19854.869909	62.241972
1957.439827	19774.059360	62.246977
1956.748501	19697.395722	62.251982
1956.092799	19628.622703	62.256986
1955.531167	19565.422795	62.261991
1954.903605	19485.893236	62.266996
1954.203600	19418.024655	62.272001
1953.783931	19334.076402	62.277006
1952.981084	19263.322628	62.282010
1952.125150	19190.529271	62.287015
1951.976325	19112.379856	62.292020
1951.003223	19037.165908	62.297025
1950.551707	18964.620069	62.302030
1949.697893	18894.264083	62.307034
1948.860214	18817.588511	62.312039
1948.413913	18735.904000	62.317044
1947.448224	18676.991912	62.322049
1946.633201	18589.130729	62.327054
1946.316555	18535.328947	62.332058
1945.788568	18458.706240	62.337063
1944.979574	18389.218946	62.342068
1944.112194	18315.729666	62.347073
1943.933457	18239.806120	62.352078
1943.000609	18171.799133	62.357082
1942.534511	18106.396114	62.362087
1941.975794	18026.999229	62.367092
1941.137132	17960.638386	62.372097
1940.243164	17883.110739	62.377102
1940.041361	17809.031123	62.382106
1939.114083	17731.377687	62.387111
1938.902431	17655.354062	62.392116
1937.901642	17581.627735	62.397121
1937.241585	17505.231980	62.402126
1936.357331	17440.518609	62.407130
1935.583646	17364.483395	62.412135
1935.355525	17285.932199	62.417140
1934.248755	17230.374095	62.422145
1933.693267	17139.893852	62.427150
1933.248460	17076.648384	62.432154
1932.417677	17005.932982	62.437159
1931.990312	16931.885456	62.442164
1931.182891	16868.895346	62.447169
1930.438516	16786.607082	62.452174
1929.744272	16713.339444	62.457178
1928.897110	16648.106460	62.462183
1928.592762	16575.116417	62.467188
1927.723863	16512.842411	62.472193
1927.485911	16442.339178	62.477198
1926.655693	16368.325537	62.482202
1926.038602	16295.016255	62.487207
1925.359317	16224.108101	62.492212
1924.407870	16157.620736	62.497217
1923.712684	16086.452889	62.502222
1923.493516	16018.738694	62.507226
1922.696687	15944.777627	62.512231
1922.026865	15866.431414	62.517236
1921.053503	15801.324059	62.522241
1920.989736	15729.307180	62.527246
1920.195881	15663.982868	62.532250
1919.320936	15587.841236	62.537255
1918.447449	15508.874045	62.542260
1918.109776	15445.810433	62.547265
1917.331651	15376.046223	62.552270
1916.418925	15307.826635	62.557274
1915.854621	15239.570784	62.562279
1915.522748	15168.356011	62.567284
1914.547255	15105.926329	62.572289
1914.073878	15024.853470	62.577294
1913.342515	14957.987485	62.582298
1912.745673	14884.080859	62.587303
1912.169705	14815.409244	62.592308
1911.212668	14741.919600	62.597313
1910.829293	14675.046563	62.602318
1910.258767	14596.892701	62.607322
1909.332483	14529.926335	62.612327
1908.884089	14452.259138	62.617332
1908.332311	14393.187074	62.622337
1907.288009	14318.908871	62.627342
1906.664143	14255.384833	62.632346
1905.943195	14182.796523	62.637351
1905.347194	14112.042328	62.642356
1904.474103	14050.734415	62.647361
1903.964838	13980.996603	62.652366
1903.214698	13902.065445	62.657370
1902.276845	13847.708067	62.662375
1902.032033	13775.185989	62.667380
1901.363815	13706.444900	62.672385
1900.834212	13643.180418	62.677390
1900.395895	13569.030235	62.682394
1899.673037	13491.895157	62.687399
1899.164440	13423.673067	62.692404
1898.289837	13369.091974	62.697409
1897.912343	13288.997878	62.702414
1896.980391	13210.140685	62.707418
1895.969823	13141.728656	62.712423
1895.453957	13074.551070	62.717428
1894.792930	13011.829245	62.722433
1894.364505	12937.089959	62.727438
1893.646582	12862.523561	62.732442
1892.839788	12795.198788	62.737447
1892.166305	12719.515879	62.742452
1891.766412	12658.398559	62.747457
1890.988749	12583.178937	62.752462
1890.438328	12517.797630	62.757466
1889.412916	12441.973895	62.762471
1888.908265	12370.335142	62.767476
1888.350587	12314.087804	62.772481
1887.468149	12244.632795	62.777486
1886.680855	12182.171272	62.782490
1886.136722	12109.787774	62.787495
1885.685872	12041.592289	62.792500
1884.706748	11980.008388	62.797505
1884.200376	11900.388588	62.802510
1883.716223	11830.199915	62.807514
1882.800671	11767.246945	62.812519
1882.488493	11690.687764	62.817524
1881.591789	11630.416710	62.822529
1881.368196	11560.788816	62.827534
1880.282236	11490.628605	62.832538
1879.356286	11422.856357	62.837543
1878.920210	11344.179563	62.842548
1878.154231	11278.855564	62.847553
1877.730872	11207.147051	62.852558
1877.083688	11129.836458	62.857562
1876.111685	11070.674036	62.862567
1875.687920	11000.840613	62.867572
1874.478171	10936.579617	62.872577
1873.910772	10868.929677	62.877582
1873.454711	10815.565255	62.882586
1872.628585	10752.118812	62.887591
1872.192105	10682.209972	62.892596
1871.332272	10619.263386	62.897601
1870.762429	10557.834123	62.902606
1870.429549	10488.959555	62.907610
1869.498018	10423.506542	62.912615
1869.530522	10356.188943	62.917620
1868.433461	10299.875330	62.922625
1867.857272	10218.107190	62.927630
1867.338906	10161.762379	62.932634
1866.295055	10097.293595	62.937639
1865.728233	10018.831447	62.942644
1864.741561	9952.050666	62.947649
1864.305499	9893.414523	62.952654
1864.227146	9822.337534	62.957658
1863.051256	9753.144512	62.962663
1862.565128	9680.455115	62.967668
1861.850652	9622.168785	62.972673
1861.129784	9547.970466	62.977678
1860.548935	9475.811519	62.982682
1859.494065	9415.631623	62.987687
1859.313819	9350.329093	62.992692
1858.562944	9287.898995	62.997697
1857.674126	9212.182596	63.002702
1857.259013	9139.327135	63.007706
1856.376162	9075.191025	63.012711
1855.840243	9015.539423	63.017716
1855.176430	8951.106735	63.022721
1854.584943	8879.496723	63.027726
1853.816771	8810.846074	63.032730
1852.972526	8748.193992	63.037735
1852.479658	8679.532186	63.042740
1851.995036	8621.483066	63.047745
1851.078449	8547.949156	63.052750
1850.651732	8471.479113	63.057754
1850.058145	8409.953119	63.062759
1849.733554	8339.846856	63.067764
1848.574295	8284.990874	63.072769
1848.221387	8209.715928	63.077774
1847.277390	8140.914812	63.082778
1846.727958	8071.202098	63.087783
1846.366413	8002.779728	63.092788
1845.058699	7930.644215	63.097793
1844.255153	7865.729535	63.102798
1843.825030	7792.583607	63.107802
1843.031840	7739.460342	63.112807
1842.851822	7667.609343	63.117812
1842.141947	7603.766448	63.122817
1841.353252	7540.726807	63.127822
1840.877780	7474.497147	63.132826
1839.798715	7406.264404	63.137831
1839.449333	7339.423662	63.142836
1838.542242	7272.865045	63.147841
1837.762146	7198.702357	63.152846
1837.230339	7140.431787	63.157850
1836.477184	7081.027493	63.162855
1835.786605	7010.477150	63.167860
1835.254665	6954.917851	63.172865
1834.567184	6882.180910	63.177870
1834.229409	6817.754949	63.182874
1833.169214	6749.734420	63.187879
1832.433506	6678.289586	63.192884
1831.975410	6631.358394	63.197889
1831.161170	6557.796738	63.202894
1830.780300	6495.626804	63.207898
1829.767974	6441.272154	63.212903
1829.341552	6377.580404	63.217908
1828.664973	6318.338961	63.222913
1828.184499	6241.034180	63.227918
1827.678038	6181.879071	63.232922
1826.555630	6117.055772	63.237927
1826.208254	6037.244578	63.242932
1825.648562	5970.731285	63.247937
1824.809372	5915.056643	63.252942
1823.954610	5839.910808	63.257946
1823.305380	5779.228405	63.262951
1822.844078	5710.985813	63.267956
1821.764736	5649.642605	63.272961
1821.099502	5588.255193	63.277966
1820.915918	5529.354310	63.282970
1819.955029	5473.338602	63.287975
1819.439449	5402.456539	63.292980
1818.862426	5336.654009	63.297985
1817.838008	5279.536166	63.302990
1817.711605	5215.156550	63.307994
1816.311651	5151.499233	63.312999
1816.127357	5085.570780	63.318004
1815.438197	5036.134423	63.323009
1814.745286	4974.907758	63.328014
1814.304023	4898.823948	63.333018
1813.389279	4841.007330	63.338023
1812.866581	4770.963915	63.343028
1812.185334	4709.563763	63.348033
1811.486663	4652.098480	63.353038
1810.838107	4575.508965	63.358042
1810.002680	4517.399444	63.363047
1809.798272	4447.631976	63.368052
1808.788822	4396.030730	63.373057
1808.129006	4325.289521	63.378062
1807.716923	4258.085345	63.383066
1806.522156	4207.031586	63.388071
1806.144849	4140.201006	63.393076
1805.629913	4076.545037	63.398081
1804.888606	4016.320649	63.403086
1804.370105	3946.213442	63.408090
1803.318939	3888.599682	63.413095
1803.081524	3820.798748	63.418100
1802.391304	3756.845476	63.423105
1801.620667	3691.779800	63.428110
1800.901330	3623.269983	63.433114
1800.172609	3568.360350	63.438119
1799.329043	3498.343963	63.443124
1798.501075	3440.278523	63.448129
1798.237663	3384.419475	63.453134
1797.615647	3328.889673	63.458138
1796.392393	3264.337839	63.463143
1796.211265	3201.152378	63.468148
1795.285575	3147.629722	63.473153
1794.768579	3093.401978	63.478158
1794.076098	3024.204564	63.483162
1793.334400	2973.412020	63.488167
1792.724434	2906.523832	63.493172
1792.260262	2847.796501	63.498177
1791.304280	2787.786319	63.503182
1790.926012	2724.356614	63.508186
1789.873883	2665.243105	63.513191
1789.770376	2605.544661	63.518196
1788.863431	2545.533995	63.523201
1788.100769	2497.215610	63.528206
1787.668943	2435.063763	63.533210
1786.528872	2385.664552	63.538215
1785.985676	2328.125312	63.543220
1785.093670	2263.617560	63.548225
1784.831480	2207.823519	63.553230
1784.239104	2144.927144	63.558234
1783.433743	2097.689360	63.563239
1782.983192	2034.601389	63.568244
1782.245579	1970.226555	63.573249
1781.400095	1912.654941	63.578254
1781.022032	1850.208417	63.583258
1780.053202	1791.690850	63.588263
1779.426697	1740.598830	63.593268
1778.667580	1688.866433	63.598273
1778.235964	1629.567104	63.603278
1777.480618	1579.619037	63.608282
1776.602970	1510.294167	63.613287
1776.042529	1456.481559	63.618292
1775.066092	1411.418061	63.623297
1774.476933	1357.444781	63.628302
1774.125917	1292.742646	63.633306
1773.430486	1240.040480	63.638311
1772.673941	1191.327232	63.643316
1771.969694	1152.617241	63.648321
1771.179467	1093.795760	63.653326
1770.736976	1033.539346	63.658330
1769.886541	984.206138	63.663335
1769.055280	928.293665	63.668340
1768.688859	880.714924	63.673345
1767.581086	836.289913	63.678350
1767.249919	786.471186	63.683354
1766.587234	749.107207	63.688359
1765.906719	693.832481	63.693364
1764.883862	643.710904	63.698369
1764.539724	594.836386	63.703374
1763.811341	543.466689	63.708378
1762.910548	508.724319	63.713383
1761.979498	459.934001	63.718388
1761.455605	421.976365	63.723393
1760.961017	382.675292	63.728398
1760.594014	337.262083	63.733402
1759.679207	298.203022	63.738407
1758.855834	249.780312	63.743412
1758.004324	210.925907	63.748417
1757.449833	174.427767	63.753422
1756.559273	129.237133	63.758426
1755.615899	99.809063	63.763431
1755.193115	62.189557	63.768436
1754.402446	31.642953	63.773441
1753.571416	11.092936	63.778446
1752.843824	-27.033024	63.783450
1751.545711	-39.931457	63.788455
1747.947820	18.793846	63.793460
1746.510752	44.299393	63.798465
1746.297693	38.350192	63.803470
1747.163192	42.880587	63.808474
1747.651775	36.379978	63.813479
1747.061476	26.122475	63.818484
1746.585537	27.278293	63.823489
1745.312778	35.322723	63.828494
1744.753253	42.716136	63.833498
1743.671870	45.947214	63.838503
1743.322749	50.252614	63.843508
1742.923788	45.223926	63.848513
1741.729111	38.579057	63.853518
1741.659074	38.049282	63.858522
1741.047699	47.286530	63.863527
1740.193679	35.484469	63.868532
1739.413865	49.761673	63.873537
1738.456612	54.638327	63.878542
1738.764993	54.102069	63.883546
1737.898194	54.820065	63.888551
1737.336772	51.406770	63.893556
1736.666856	48.925353	63.898561
1735.502848	57.029798	63.903566
1734.935610	48.093281	63.908570
1733.808943	58.284444	63.913575
1733.129872	52.853959	63.918580
1732.921325	54.449868	63.923585
1732.199312	49.207556	63.928590
1731.584368	52.683109	63.933594
1730.903563	58.630783	63.938599
1730.930255	52.540997	63.943604
1730.566098	53.474059	63.948609
1728.971973	61.426045	63.953614
1728.635674	56.340095	63.958618
1727.977809	63.733369	63.963623
1727.308069	50.446484	63.968628
1726.254816	47.436164	63.973633
1725.196348	58.578453	63.978638
1724.844000	46.630479	63.983642
1724.551879	55.720835	63.988647
1724.114255	53.831740	63.993652
1723.832524	50.924392	63.998657
1722.898639	51.741358	64.003662
1722.333940	49.639055	64.008666
1721.632294	59.158737	64.013671
1721.154190	50.621233	64.018676
1720.132227	55.164390	64.023681
1719.141542	54.747722	64.028686
1718.831332	52.586076	64.033690
1717.870301	50.918888	64.038695
1716.910218	47.824388	64.043700
1716.370528	49.658975	64.048705
1715.601341	48.650456	64.053710
1715.640608	49.703951	64.058714
1715.455798	52.798949	64.063719
1714.157164	49.313513	64.068724
1712.997395	49.398373	64.073729
1712.411941	54.474606	64.078734
1712.700570	46.354654	64.083738
1712.062082	48.201780	64.088743
1711.053976	51.184687	64.093748
1710.047505	44.841104	64.098753
1709.409253	55.080856	64.103758
1709.433848	52.164280	64.108762
1708.202719	48.775360	64.113767
1707.589804	51.203483	64.118772
1707.141979	61.105483	64.123777
1706.098886	66.005248	64.128782
1705.788613	53.378798	64.133786
1705.081236	51.117808	64.138791
1704.214814	56.563528	64.143796
1703.928265	52.283401	64.148801
1702.947871	55.777581	64.153806
1702.411134	47.604217	64.158810
1701.470353	52.844124	64.163815
1700.945698	46.332552	64.168820
1700.820702	48.020849	64.173825
1699.797186	55.759211	64.178830
1698.529485	48.033115	64.183834
1698.204942	53.935246	64.188839
1697.483518	51.184473	64.193844
1697.008971	49.854767	64.198849
1696.428332	62.080248	64.203854
1696.202376	52.709481	64.208858
1695.009337	59.765135	64.213863
1694.518929	58.155669	64.218868
1694.106930	59.367575	64.223873
1693.291631	55.434789	64.228878
1692.714841	51.870980	64.233882
1691.943650	45.983626	64.238887
1690.590335	59.560298	64.243892
1690.611682	53.452439	64.248897
1689.898290	51.687580	64.253902
1689.452066	44.278870	64.258906
1688.634175	44.938650	64.263911
1687.416640	48.666046	64.268916
1687.425439	47.224875	64.273921
1686.709319	53.983999	64.278926
1685.546989	56.414239	64.283930
1685.059573	62.793260	64.288935
1684.965946	49.403845	64.293940
1684.140187	53.291366	64.298945
1682.848878	53.480713	64.303950
1682.697525	47.106971	64.308954
1682.134691	48.030596	64.313959
1681.029873	48.816379	64.318964
1680.525899	48.500615	64.323969
1680.093208	55.556924	64.328974
1679.492661	51.897543	64.333978
1678.660421	51.933546	64.338983
1677.826780	47.238848	64.343988
1677.373753	52.065391	64.348993
1676.458956	54.353813	64.353998
1675.908914	49.653492	64.359002
1675.495850	49.441561	64.364007
1675.160896	38.766616	64.369012
1674.477790	42.368124	64.374017
1673.778581	53.533784	64.379022
1673.353059	44.768746	64.384026
1672.316208	45.568968	64.389031
1671.046781	50.181411	64.394036
1671.151566	47.354603	64.399041
1669.892136	48.683775	64.404046
1669.510961	47.574212	64.409050
1668.514177	51.938342	64.414055
1668.137741	46.147567	64.419060
1667.722458	47.460924	64.424065
1666.724520	47.980574	64.429070
1666.139786	42.896255	64.434074
1665.672504	56.283304	64.439079
1664.905650	51.529115	64.444084
1664.517293	48.225545	64.449089
1663.749266	57.728971	64.454094
1663.248913	47.654315	64.459098
1662.875618	53.338684	64.464103
1661.425297	47.819421	64.469108
1660.760593	42.342525	64.474113
1659.808571	48.814268	64.479118
1659.262903	37.584589	64.484122
1659.004323	54.664872	64.489127
1658.159264	48.114319	64.494132
1657.686131	41.099406	64.499137
1656.869327	55.349386	64.504142
1656.357471	49.023451	64.509146
1655.880427	42.330863	64.514151
1655.207057	56.882916	64.519156
1655.106145	46.457803	64.524161
1653.811487	52.116642	64.529166
1653.035523	39.439613	64.534170
1652.260177	57.007269	64.539175
1651.456089	55.155901	64.544180
1651.073201	52.351366	64.549185
1650.363632	56.315059	64.554190
1650.056906	49.724725	64.559194
1649.335009	51.801161	64.564199
1648.995809	54.513827	64.569204
1648.169765	52.910379	64.574209
1646.561441	56.949034	64.579214
1645.929499	54.310220	64.584218
1646.042414	50.985372	64.589223
1645.254667	54.354350	64.594228
1644.426076	55.397471	64.599233
1643.487446	60.446243	64.604238
1643.196167	46.060049	64.609242
1642.693031	45.923933	64.614247
1641.737692	50.745119	64.619252
1641.602160	48.524196	64.624257
1640.590284	49.862943	64.629262
1640.176129	46.470435	64.634266
1638.823181	52.744098	64.639271
1638.141689	55.407061	64.644276
1638.067830	52.641746	64.649281
1637.204585	53.882766	64.654286
1636.646535	49.076493	64.659290
1636.052756	47.909245	64.664295
1635.403076	52.890037	64.669300
1635.411453	42.110096	64.674305
1634.040661	54.915267	64.679310
1632.852456	50.439339	64.684314
1632.285768	58.745403	64.689319
1631.590954	51.716822	64.694324
1631.610916	46.449717	64.699329
1630.877012	62.493750	64.704334
1630.085741	47.638199	64.709338
1629.525033	43.160363	64.714343
1628.968159	47.839403	64.719348
1628.586663	44.263511	64.724353
1627.045734	56.862323	64.729358
1626.258535	53.948553	64.734362
1625.677475	48.537227	64.739367
1625.215626	51.393960	64.744372
1624.712344	40.977583	64.749377
1623.858632	53.456181	64.754382
1623.567590	51.865522	64.759386
1622.900357	50.487593	64.764391
1622.254476	52.298067	64.769396
1622.284229	43.414984	64.774401
1620.527567	58.205371	64.779406
1620.021879	40.861730	64.784410
1619.333799	37.435473	64.789415
1618.641666	47.010424	64.794420
1618.572726	40.547906	64.799425
1617.991486	47.299806	64.804430
1617.058352	49.893939	64.809434
1616.025638	48.782234	64.814439
1614.739027	52.134277	64.819444
1614.505269	42.318489	64.824449
1613.889473	50.961940	64.829454
1613.425490	44.019702	64.834458
1612.726743	43.712816	64.839463
1612.503807	46.802834	64.844468
1612.239094	51.482772	64.849473
1611.828243	51.935983	64.854478
1610.354570	38.325860	64.859482
1609.609916	37.162088	64.864487
1608.548280	39.437588	64.869492
1608.575476	30.062905	64.874497
1607.764091	37.146258	64.879502
1607.000109	35.368962	64.884506
1606.046940	45.986761	64.889511
1605.024213	41.708491	64.894516
1604.601205	32.563028	64.899521
1603.843648	42.268222	64.904526
1603.501628	45.053880	64.909530
1603.399387	34.830846	64.914535
1602.666189	36.932742	64.919540
1602.583973	30.652115	64.924545
1600.904494	34.199040	64.929550
1600.095292	36.171084	64.934554
1599.259988	32.198938	64.939559
1598.437521	44.309866	64.944564
1597.984508	37.651324	64.949569
1597.625204	42.336825	64.954574
1597.151223	38.781942	64.959578
1596.806750	40.945086	64.964583
1596.111162	40.960983	64.969588
1595.643399	41.079457	64.974593
1594.055979	37.398693	64.979598
1593.590284	36.887628	64.984602
1592.737029	42.720793	64.989607
1592.261082	44.661972	64.994612
1591.996369	30.076042	64.999617
1591.539072	41.782019	65.004622
1590.670636	36.979343	65.009626
1589.853159	37.241691	65.014631
1588.733883	41.689961	65.019636
1588.485688	46.960216	65.024641
1587.936502	40.230221	65.029646
1587.478127	33.022173	65.034650
1586.998497	31.221783	65.039655
1585.358351	41.511909	65.044660
1585.030804	36.145478	65.049665
1584.025965	36.152163	65.054670
1583.922073	42.164320	65.059674
1583.609910	42.161880	65.064679
1582.851711	41.788754	65.069684
1582.220550	43.380852	65.074689
1580.847384	47.462606	65.079694
1580.114067	31.847249	65.084698
1579.724826	42.075831	65.089703
1579.108260	44.632295	65.094708
1578.621123	34.307990	65.099713
1578.437752	54.806229	65.104718
1577.973805	44.246417	65.109722
1576.775492	41.459487	65.114727
1575.867486	42.531016	65.119732
1575.575541	44.949171	65.124737
1574.712673	43.074053	65.129742
1573.971067	40.689230	65.134746
1572.867718	42.381584	65.139751
1572.156069	46.968527	65.144756
1571.888566	32.928676	65.149761
1570.811465	36.004594	65.154766
1570.505720	44.392203	65.159770
1570.266120	43.540863	65.164775
1569.882620	30.777868	65.169780
1569.583241	32.016052	65.174785
1567.975004	44.111481	65.179790
1567.370974	35.852660	65.184794
1566.811571	36.627528	65.189799
1566.225302	50.692653	65.194804
1565.849121	38.696475	65.199809
1564.585866	47.844931	65.204814
1563.714433	44.093003	65.209818
1563.071972	31.155110	65.214823
1562.646654	43.149325	65.219828
1562.527918	36.156980	65.224833
1561.848563	41.117265	65.229838
1560.664730	47.127546	65.234842
1559.754652	45.885991	65.239847
1558.934677	42.100658	65.244852
1558.720534	36.979568	65.249857
1558.213007	37.091751	65.254862
1557.741818	35.113406	65.259866
1557.473563	41.572729	65.264871
1556.305363	41.398797	65.269876
1555.492858	35.672605	65.274881
1554.843024	42.684573	65.279886
1554.276884	35.671852	65.284890
1553.763769	37.420243	65.289895
1552.542234	48.318821	65.294900
1551.698144	40.011413	65.299905
1550.764208	43.851502	65.304910
1550.660982	43.905755	65.309914
1550.282614	43.387130	65.314919
1549.561544	43.724059	65.319924
1549.534693	38.342972	65.324929
1548.865011	53.037951	65.329934
1547.633080	42.991265	65.334938
1546.692774	37.208111	65.339943
1546.078525	47.062437	65.344948
1545.805906	32.129263	65.349953
1545.168855	44.138199	65.354958
1544.041978	38.826242	65.359962
1543.175044	42.155786	65.364967
1542.372464	40.818309	65.369972
1542.621625	34.671115	65.374977
1541.883478	35.397117	65.379982
1540.987451	34.230610	65.384986
1540.863087	41.401938	65.389991
1539.782582	43.134831	65.394996
1538.962409	36.086784	65.400001
1538.394307	42.732526	65.405006
1537.935462	40.842110	65.410010
1537.681232	38.565940	65.415015
1536.201511	42.139514	65.420020
1535.449160	30.794488	65.425025
1534.630673	34.311879	65.430030
1534.193733	34.138459	65.435034
1534.144490	42.128914	65.440039
1533.208862	32.508253	65.445044
1532.726261	32.372051	65.450049
1531.562468	38.287691	65.455054
1530.988487	30.213347	65.460058
1530.348548	28.630833	65.465063
1529.498730	34.185919	65.470068
1529.344412	31.311973	65.475073
1528.490438	34.451801	65.480078
1527.559593	28.231912	65.485082
1527.034936	32.040087	65.490087
1526.337472	36.036573	65.495092
1526.079043	28.318949	65.500097
1525.540557	38.760482	65.505102
1524.465878	27.482451	65.510106
1523.595553	35.505601	65.515111
1522.520366	36.856028	65.520116
1522.135136	23.173954	65.525121
1521.784840	26.957577	65.530126
1521.115617	29.317412	65.535130
1521.000956	29.909653	65.540135
1520.245175	33.852328	65.545140
1519.378701	32.966564	65.550145
1518.714649	46.818542	65.555150
1518.001556	40.918868	65.560154
1517.635727	35.859735	65.565159
1516.397530	46.929708	65.570164
1515.496775	38.219731	65.575169
1514.567719	45.613548	65.580174
1514.280563	31.620990	65.585178
1513.977983	35.393879	65.590183
1513.436978	40.376346	65.595188
1513.075123	46.133024	65.600193
1512.092347	38.394880	65.605198
1511.008265	47.746700	65.610202
1510.516496	40.436740	65.615207
1509.885256	46.991595	65.620212
1509.875623	41.073181	65.625217
1508.849989	43.491234	65.630222
1507.672956	47.338427	65.635226
1507.373802	38.466622	65.640231
1506.349779	45.322016	65.645236
1506.296066	41.411782	65.650241
1505.806533	50.670704	65.655246
1504.672289	51.388697	65.660250
1504.362692	49.006208	65.665255
1503.279633	45.062426	65.670260
1502.937069	39.690510	65.675265
1502.232125	45.232047	65.680270
1501.060839	44.191297	65.685274
1500.876752	41.000380	65.690279
1499.868195	49.408213	65.695284
1499.495678	42.719555	65.700289
1499.312662	46.005087	65.705294
1498.098503	52.035983	65.710298
1497.358458	46.022324	65.715303
1496.351640	49.340997	65.720308
1496.140828	33.712030	65.725313
1495.428590	36.652725	65.730318
1494.785969	35.639932	65.735322
1493.939607	41.262290	65.740327
1493.186611	40.579277	65.745332
1492.592634	33.764966	65.750337
1492.130577	40.701371	65.755342
1491.721267	39.965320	65.760346
1491.397043	35.498828	65.765351
1490.140223	43.988692	65.770356
1489.515031	35.288554	65.775361
1488.976361	43.102892	65.780366
1488.285358	48.799915	65.785370
1487.860444	46.189747	65.790375
1486.633516	43.689686	65.795380
1486.127233	38.569299	65.800385
1485.343202	46.982455	65.805390
1484.713142	43.821411	65.810394
1484.521167	43.273175	65.815399
1483.229528	51.052634	65.820404
1482.416552	43.558756	65.825409
1481.882892	41.953056	65.830414
1481.247765	40.265709	65.835418
1481.135697	43.205649	65.840423
1480.431576	49.532393	65.845428
1480.410841	38.641979	65.850433
1479.284792	44.685686	65.855438
1478.136089	50.816575	65.860442
1477.803985	38.408135	65.865447
1477.268387	45.993327	65.870452
1476.227674	42.344030	65.875457
1475.362301	44.555275	65.880462
1474.843398	48.652711	65.885466
1474.356110	36.612715	65.890471
1473.797519	42.936830	65.895476
1473.464312	37.818903	65.900481
1471.837007	40.588057	65.905486
1471.248970	41.100987	65.910490
1471.160377	30.279713	65.915495
1470.370428	35.951458	65.920500
1469.810974	34.887607	65.925505
1469.417376	36.598096	65.930510
1468.386689	42.754386	65.935514
1467.915767	34.594294	65.940519
1467.113647	45.035156	65.945524
1466.748840	33.645913	65.950529
1465.571585	38.978663	65.955534
1464.591150	39.400989	65.960538
1464.253846	44.261204	65.965543
1463.472756	50.890347	65.970548
1463.380138	34.345307	65.975553
1462.739214	37.829770	65.980558
1461.867551	37.241320	65.985562
1461.009393	39.236954	65.990567
1460.491963	44.296109	65.995572
1459.903439	44.995201	66.000577
1459.523576	45.861408	66.005582
1458.280985	44.425151	66.010586
1457.873925	39.183344	66.015591
1456.902360	36.210626	66.020596
1456.395196	31.341127	66.025601
1455.648256	37.349820	66.030606
1455.287793	41.839973	66.035610
1455.138579	46.299709	66.040615
1453.871205	48.847666	66.045620
1453.168572	41.292110	66.050625
1452.643689	42.121440	66.055630
1451.831204	42.867167	66.060634
1451.152380	37.233310	66.065639
1450.264111	43.234505	66.070644
1449.560828	38.558602	66.075649
1449.238223	40.502242	66.080654
1448.638759	39.791688	66.085658
1448.616995	41.055150	66.090663
1447.532365	42.003404	66.095668
1446.900658	39.725736	66.100673
1446.480323	40.327137	66.105678
1445.273496	37.797095	66.110682
1444.229546	41.276228	66.115687
1443.600957	43.635933	66.120692
1443.124849	47.818037	66.125697
1442.810281	35.116660	66.130702
1442.080607	39.976157	66.135706
1440.919295	40.761557	66.140711
1440.435965	35.355257	66.145716
1440.028746	34.789194	66.150721
1439.599373	42.267619	66.155726
1438.902487	41.676631	66.160730
1438.411359	42.492714	66.165735
1437.196078	38.557362	66.170740
1436.927279	35.594385	66.175745
1436.324288	35.948848	66.180750
1435.443323	42.850913	66.185754
1434.601861	37.223987	66.190759
1433.743652	47.639079	66.195764
1433.480082	43.612392	66.200769
1432.982447	42.488261	66.205774
1432.224742	34.487301	66.210778
1431.191365	33.921411	66.215783
1430.380247	48.968462	66.220788
1430.039668	45.838695	66.225793
1429.485603	39.341336	66.230798
1428.830009	42.872293	66.235802
1428.791900	31.554141	66.240807
1427.212938	40.908943	66.245812
1426.795183	43.293490	66.250817
1426.111909	42.093209	66.255822
1425.572418	38.438388	66.260826
1425.061093	35.064524	66.265831
1423.872688	46.607591	66.270836
1423.488373	43.782824	66.275841
1423.087788	36.974066	66.280846
1422.286042	29.175657	66.285850
1421.730090	36.166415	66.290855
1420.747939	40.892579	66.295860
1420.206827	38.479092	66.300865
1419.823941	33.503115	66.305870
1418.607762	39.886023	66.310874
1417.674030	29.173855	66.315879
1416.978063	42.915795	66.320884
1416.478330	40.699161	66.325889
1416.225304	37.552327	66.330894
1415.901197	38.151054	66.335898
1415.624721	31.942323	66.340903
1414.147095	36.129068	66.345908
1413.573619	33.615071	66.350913
1412.980951	32.796212	66.355918
1412.355127	43.623806	66.360922
1411.951995	35.121791	66.365927
1410.620009	45.271565	66.370932
1410.076951	38.397145	66.375937
1409.557478	30.024013	66.380942
1408.883261	38.258875	66.385946
1408.862528	42.326024	66.390951
1407.802236	46.072701	66.395956
1406.876570	41.299692	66.400961
1406.379089	38.215370	66.405966
1405.697075	47.082264	66.410970
1405.129824	28.964752	66.415975
1403.897196	33.071560	66.420980
1403.371564	37.177958	66.425985
1403.075537	40.713270	66.430990
1402.282472	42.340605	66.435994
1402.354932	40.895627	66.440999
1401.395501	34.429595	66.446004
1400.433752	38.330921	66.451009
1399.676483	39.272893	66.456014
1399.395186	40.416757	66.461018
1398.544623	32.722310	66.466023
1397.441135	40.416698	66.471028
1396.711123	34.937655	66.476033
1396.516925	31.090763	66.481038
1395.761638	40.264194	66.486042
1395.618032	31.962210	66.491047
1394.521451	36.695531	66.496052
1394.059976	38.870987	66.501057
1393.767955	30.762906	66.506062
1392.162493	36.671532	66.511066
1391.784274	34.076041	66.516071
1390.917903	36.708520	66.521076
1390.624489	30.721684	66.526081
1389.969534	32.312876	66.531086
1388.981660	34.840089	66.536090
1388.333299	25.205378	66.541095
1387.584714	39.225343	66.546100
1386.962551	33.472114	66.551105
1386.740989	30.654602	66.556110
1385.963764	33.936816	66.561114
1385.334159	25.155419	66.566119
1384.112442	37.884936	66.571124
1383.926245	30.655755	66.576129
1383.841690	29.986372	66.581134
1382.667419	39.926580	66.586138
1382.013805	32.073100	66.591143
1380.935238	33.941366	66.596148
1380.984475	33.438376	66.601153
1380.273354	28.091957	66.606158
1379.063085	42.210544	66.611162
1378.420568	31.882615	66.616167
1377.855830	43.730263	66.621172
1377.423368	39.990631	66.626177
1376.586675	37.617832	66.631182
1375.567566	47.162795	66.636186
1375.141196	32.957435	66.641191
1374.891212	39.626749	66.646196
1374.336902	35.073849	66.651201
1373.754687	31.112019	66.656206
1372.374767	41.001341	66.661210
1372.056743	30.667566	66.666215
1371.456249	39.480502	66.671220
1370.692181	39.133603	66.676225
1369.778601	31.349837	66.681230
1368.986180	38.507504	66.686234
1368.389698	33.792574	66.691239
1368.019336	36.190095	66.696244
1367.722938	34.797444	66.701249
1367.304333	36.243837	66.706254
1365.969540	34.480082	66.711258
1365.221453	29.254662	66.716263
1364.560928	36.350361	66.721268
1364.247771	35.471312	66.726273
1363.457798	37.721068	66.731278
1362.260556	36.052146	66.736282
1361.854415	31.083032	66.741287
1361.274921	32.408343	66.746292
1360.572924	30.189182	66.751297
1360.213092	37.197659	66.756302
1359.612969	35.567859	66.761306
1359.040330	36.475762	66.766311
1357.982529	33.280249	66.771316
1357.427977	23.594368	66.776321
1357.029323	31.569386	66.781326
1356.168102	43.520937	66.786330
1355.551669	25.562657	66.791335
1354.825490	31.404066	66.796340
1354.438827	38.020989	66.801345
1353.838909	23.672921	66.806350
1352.274494	30.292561	66.811354
1351.760660	34.855988	66.816359
1351.175772	29.484780	66.821364
1350.452700	33.762923	66.826369
1350.745674	29.794437	66.831374
1349.725725	33.424331	66.836378
1349.131640	35.780147	66.841383
1348.407963	29.169430	66.846388
1347.696642	24.374993	66.851393
1347.146703	30.782902	66.856398
1346.093557	30.622315	66.861402
1345.365369	32.737674	66.866407
1344.651657	27.856884	66.871412
1344.461598	29.669074	66.876417
1344.354607	29.433772	66.881422
1342.881720	36.895162	66.886426
1342.550504	30.477525	66.891431
1341.929899	40.706625	66.896436
1340.554906	34.267258	66.901441
1340.077400	34.245401	66.906446
1339.326161	34.626608	66.911450
1338.896861	33.117892	66.916455
1338.215255	35.632705	66.921460
1337.951107	36.486840	66.926465
1337.355329	32.771605	66.931470
1336.076407	35.124330	66.936474
1335.813198	25.851036	66.941479
1335.278279	35.077753	66.946484
1334.455189	31.136880	66.951489
1333.507495	35.583201	66.956494
1332.586849	42.605143	66.961498
1332.204637	32.614320	66.966503
1332.140283	39.334550	66.971508
1331.482500	35.042541	66.976513
1330.351362	36.272629	66.981518
1329.436960	33.864892	66.986522
1328.887054	32.864212	66.991527
1328.741744	39.693507	66.996532
1327.935988	40.651092	67.001537
1326.831341	24.804730	67.006542
1326.087802	30.421821	67.011546
1325.970333	36.128619	67.016551
1325.256757	40.521955	67.021556
1324.623340	42.906107	67.026561
1324.100471	38.293028	67.031566
1322.745906	54.041514	67.036570
1322.637932	45.987759	67.041575
1322.195500	50.145603	67.046580
1320.970291	41.616604	67.051585
1320.525607	38.618525	67.056590
1319.765712	44.807508	67.061594
1319.576139	40.336986	67.066599
1318.395826	45.927328	67.071604
1317.687241	39.705305	67.076609
1317.547609	45.412476	67.081614
1316.656012	43.412705	67.086618
1316.038741	30.100318	67.091623
1314.994792	41.858574	67.096628
1314.059495	39.537743	67.101633
1313.755348	36.372243	67.106638
1313.116051	45.256015	67.111642
1313.128165	32.540585	67.116647
1311.757527	34.234538	67.121652
1311.077482	40.180589	67.126657
1310.914660	36.249870	67.131662
1310.038800	36.592550	67.136666
1309.455692	32.518914	67.141671
1308.372966	30.330337	67.146676
1307.757371	34.438436	67.151681
1307.411458	32.375570	67.156686
1306.681467	38.767959	67.161690
1305.875422	27.914119	67.166695
1305.074074	33.586139	67.171700
1304.458939	30.176768	67.176705
1303.914718	28.795141	67.181710
1303.583142	37.368210	67.186714
1302.670231	31.098256	67.191719
1301.608453	34.567659	67.196724
1301.202962	37.587367	67.201729
1300.790644	33.537042	67.206734
1300.405898	36.227019	67.211738
1299.883898	34.788242	67.216743
1298.708042	34.495796	67.221748
1298.014180	38.460223	67.226753
1297.743581	31.786949	67.231758
1296.429680	34.813888	67.236762
1295.871287	31.941128	67.241767
1294.975310	35.540294	67.246772
1294.387570	33.604187	67.251777
1294.415825	32.505285	67.256782
1293.527954	39.384829	67.261786
1293.164748	38.076927	67.266791
1291.975839	38.368459	67.271796
1291.693260	44.267092	67.276801
1291.368868	28.314040	67.281806
1290.032897	42.482604	67.286810
1289.431405	39.646659	67.291815
1288.869715	41.811256	67.296820
1287.985870	40.778522	67.301825
1287.175723	43.143473	67.306830
1286.424369	41.637084	67.311834
1285.899950	42.075285	67.316839
1285.623056	38.757221	67.321844
1285.042674	41.900932	67.326849
1284.942145	34.429483	67.331854
1283.358962	39.542992	67.336858
1283.379106	27.097532	67.341863
1282.452685	42.118776	67.346868
1280.934346	38.575468	67.351873
1280.576454	41.082982	67.356878
1279.720761	42.248797	67.361882
1279.695173	33.797176	67.366887
1279.404295	31.783912	67.371892
1278.279841	32.847377	67.376897
1277.424892	26.066745	67.381902
1276.612244	38.532561	67.386906
1276.770035	31.452131	67.391911
1275.859054	38.690172	67.396916
1274.394447	41.525039	67.401921
1273.885015	37.357695	67.406926
1273.514537	37.818731	67.411930
1273.058590	29.727278	67.416935
1273.078252	30.447983	67.421940
1271.819561	38.474599	67.426945
1271.289442	35.816548	67.431950
1270.295159	39.358812	67.436954
1269.387008	27.447309	67.441959
1268.067576	31.172158	67.446964
1267.745247	27.102803	67.451969
1268.127143	29.923201	67.456974
1267.033329	41.284118	67.461978
1267.004994	40.107480	67.466983
1266.264871	33.562483	67.471988
1265.107838	38.753324	67.476993
1264.483955	28.966529	67.481998
1263.444688	39.178627	67.487002
1262.532489	37.199499	67.492007
1261.954414	33.262272	67.497012
1261.109250	30.460350	67.502017
1261.156498	33.529501	67.507022
1260.569716	42.169961	67.512026
1260.467377	33.117107	67.517031
1259.613146	40.957992	67.522036
1258.274123	34.087175	67.527041
1258.060790	25.949267	67.532046
1256.960274	26.441228	67.537050
1256.129062	39.231700	67.542055
1255.647380	31.046571	67.547060
1255.081477	42.284128	67.552065
1254.605728	34.443410	67.557070
1253.906131	45.558724	67.562074
1252.898833	32.320992	67.567079
1252.354224	31.209099	67.572084
1251.487679	36.019438	67.577089
1251.530976	32.013373	67.582094
1250.599330	37.854361	67.587098
1249.752132	33.264487	67.592103
1249.079895	34.670802	67.597108
1248.737970	28.027804	67.602113
1248.476554	28.104069	67.607118
1246.943821	36.357196	67.612122
1246.228092	34.666959	67.617127
1245.912708	33.830858	67.622132
1245.174667	37.977364	67.627137
1244.921340	28.915406	67.632142
1244.032292	30.588011	67.637146
1243.524272	33.152515	67.642151
1242.902402	29.165487	67.647156
1241.681506	30.690584	67.652161
1241.317145	30.715410	67.657166
1240.221719	36.128277	67.662170
1240.029495	43.297771	67.667175
1239.547359	31.534583	67.672180
1238.485644	36.869550	67.677185
1238.051884	25.177524	67.682190
1237.052124	45.455426	67.687194
1236.514590	33.093914	67.692199
1236.479465	32.889767	67.697204
1235.224895	29.569479	67.702209
1234.510621	36.956025	67.707214
1233.985956	34.951556	67.712218
1233.599802	36.320268	67.717223
1232.526692	35.364959	67.722228
1231.512843	41.613266	67.727233
1231.131719	33.505194	67.732238
1230.716375	33.730518	67.737242
1229.884490	32.230645	67.742247
1229.971658	31.369959	67.747252
1228.806187	35.497703	67.752257
1227.988825	31.902889	67.757262
1227.287653	33.791631	67.762266
1226.559109	32.399907	67.767271
1225.860918	35.997605	67.772276
1224.844747	32.782915	67.777281
1224.625447	31.898422	67.782286
1224.027372	27.418756	67.787290
1223.957403	27.174419	67.792295
1223.338853	33.206901	67.797300
1222.063383	33.758237	67.802305
1221.500432	22.698623	67.807310
1221.053487	34.171152	67.812314
1220.553474	35.919097	67.817319
1219.479149	30.117974	67.822324
1218.630165	32.869167	67.827329
1218.352715	21.270565	67.832334
1216.983784	36.691770	67.837338
1216.423395	25.510322	67.842343
1215.790434	31.049929	67.847348
1215.111881	40.406737	67.852353
1215.034441	24.759797	67.857358
1214.584152	40.086963	67.862362
1213.756287	33.262622	67.867367
1212.938248	33.312287	67.872372
1212.310673	28.851509	67.877377
1212.077924	32.212766	67.882382
1210.775840	34.706430	67.887386
1210.057328	26.945334	67.892391
1209.685691	27.551643	67.897396
1209.061725	35.046836	67.902401
1208.149995	33.513936	67.907406
1207.428393	44.129703	67.912410
1206.785406	38.195334	67.917415
1206.476345	38.477878	67.922420
1205.563636	41.560911	67.927425
1204.858730	32.493500	67.932430
1203.837204	39.485787	67.937434
1203.589858	33.909554	67.942439
1203.319341	28.012153	67.947444
1202.226904	29.343374	67.952449
1201.320356	29.970095	67.957454
1200.478971	37.532981	67.962458
1200.198421	30.687842	67.967463
1200.048768	37.454746	67.972468
1199.362983	36.750094	67.977473
1198.529035	24.984525	67.982478
1197.686152	34.842131	67.987482
1197.093774	29.363348	67.992487
1196.738093	36.919958	67.997492
1195.475704	45.363515	68.002497
1195.126407	37.039075	68.007502
1194.753506	35.269102	68.012506
1193.622585	40.317046	68.017511
1192.792650	30.602468	68.022516
1192.132522	40.175547	68.027521
1191.815638	32.472010	68.032526
1191.359203	41.684689	68.037530
1190.589272	33.676305	68.042535
1189.872563	30.798787	68.047540
1189.012075	39.443359	68.052545
1188.743299	30.951575	68.057550
1187.586169	29.173857	68.062554
1186.386214	24.556530	68.067559
1186.175539	24.367687	68.072564
1185.723499	36.271540	68.077569
1185.619395	31.221314	68.082574
1184.648090	39.394652	68.087578
1183.754076	30.522905	68.092583
1182.978075	32.396750	68.097588
1182.498198	38.019254	68.102593
1182.399713	28.188357	68.107598
1180.790169	30.242072	68.112602
1180.314016	25.883380	68.117607
1180.130998	42.219877	68.122612
1179.302403	47.374291	68.127617
1178.352500	31.885027	68.132622
1177.421239	34.767590	68.137626
1176.730941	32.989750	68.142631
1176.447995	38.547820	68.147636
1175.847665	40.903089	68.152641
1175.988961	39.385660	68.157646
1174.701443	41.441783	68.162650
1173.786027	35.266898	68.167655
1173.280547	39.338590	68.172660
1172.706650	50.755629	68.177665
1171.620929	37.919919	68.182670
1171.044776	36.609632	68.187674
1170.440235	41.652719	68.192679
1170.426459	29.632139	68.197684
1169.580704	42.230976	68.202689
1168.938317	25.708791	68.207694
1168.018039	38.764181	68.212698
1167.253991	41.921356	68.217703
1166.444173	35.518367	68.222708
1165.285587	50.516641	68.227713
1164.909998	26.841488	68.232718
1164.570939	37.918392	68.237722
1163.978109	32.715659	68.242727
1164.053045	35.412969	68.247732
1162.914409	45.068466	68.252737
1162.265159	32.778365	68.257742
1161.308741	31.064932	68.262746
1160.705578	39.674893	68.267751
1159.816566	28.429032	68.272756
1159.228093	45.858195	68.277761
1158.840722	40.059807	68.282766
1158.366077	40.365537	68.287770
1157.223206	38.487792	68.292775
1156.736832	33.581945	68.297780
1155.738259	36.148790	68.302785
1155.711358	26.000582	68.307790
1154.836707	40.885882	68.312794
1153.589489	37.473001	68.317799
1153.396329	38.159744	68.322804
1152.749164	43.903478	68.327809
1152.428046	28.460884	68.332814
1151.636851	31.250216	68.337818
1150.710683	34.139863	68.342823
1150.200415	33.164458	68.347828
1149.447396	38.396744	68.352833
1148.933208	30.940641	68.357838
1147.628725	31.741058	68.362842
1147.099237	35.051743	68.367847
1147.088708	33.649925	68.372852
1146.183864	26.020991	68.377857
1145.856196	30.468106	68.382862
1144.725172	44.343929	68.387866
1144.076744	36.529128	68.392871
1143.976871	31.951322	68.397876
1143.077920	39.032943	68.402881
1142.025882	30.806096	68.407886
1141.379736	38.812611	68.412890
1140.887270	34.522752	68.417895
1140.545031	29.381096	68.422900
1139.261638	32.515222	68.427905
1138.735146	31.955564	68.432910
1138.362736	32.774897	68.437914
1137.867307	33.612219	68.442919
1136.915586	29.384369	68.447924
1135.664496	37.671606	68.452929
1135.703019	27.180255	68.457934
1135.106654	35.595169	68.462938
1134.430318	26.646248	68.467943
1133.445522	27.837374	68.472948
1132.676193	23.750830	68.477953
1132.264387	12.843834	68.482958
1131.840971	27.606891	68.487962
1131.156441	28.611487	68.492967
1130.466556	21.583889	68.497972
1129.303766	33.458863	68.502977
1129.407351	16.948943	68.507982
1128.579779	26.595965	68.512986
1127.378271	33.795098	68.517991
1127.062779	24.208464	68.522996
1125.998317	41.200819	68.528001
1125.883936	28.186991	68.533006
1125.290835	32.961758	68.538010
1124.172512	39.024865	68.543015
1123.734805	27.024415	68.548020
1123.058456	29.360245	68.553025
1122.444549	19.087793	68.558030
1121.258970	28.321826	68.563034
1120.798277	28.798809	68.568039
1120.316387	26.610944	68.573044
1119.809141	28.055702	68.578049
1119.513444	25.773566	68.583054
1118.321806	32.422350	68.588058
1117.464174	26.219378	68.593063
1117.100980	21.856928	68.598068
1116.266479	35.900053	68.603073
1116.258942	21.894676	68.608078
1115.406268	19.999179	68.613082
1114.677649	32.024296	68.618087
1114.198489	25.731164	68.623092
1113.032113	31.440792	68.628097
1112.180966	34.094590	68.633102
1111.500654	30.097972	68.638106
1110.915059	31.044259	68.643111
1111.020252	27.607099	68.648116
1109.537213	37.364700	68.653121
1109.012473	21.897744	68.658126
1108.232394	24.363617	68.663130
1107.934127	22.906643	68.668135
1107.597697	27.099686	68.673140
1106.278078	32.161907	68.678145
1105.952290	24.582812	68.683150
1105.344720	31.532936	68.688154
1104.815896	30.350756	68.693159
1104.099676	18.703704	68.698164
1103.120448	29.794122	68.703169
1102.648141	27.462809	68.708174
1102.227525	33.146859	68.713178
1101.069534	30.028900	68.718183
1100.580729	20.408341	68.723188
1099.982287	27.226124	68.728193
1099.597690	21.824710	68.733198
1098.537723	29.835550	68.738202
1097.634098	20.837644	68.743207
1097.198424	18.304963	68.748212
1096.509499	18.152777	68.753217
1096.133834	16.621384	68.758222
1094.999974	21.113160	68.763226
1094.270784	25.468028	68.768231
1093.921220	21.661658	68.773236
1093.152072	33.157059	68.778241
1093.208409	25.469873	68.783246
1092.073643	20.192520	68.788250
1091.230637	23.125727	68.793255
1090.875237	20.099305	68.798260
1090.321367	34.592960	68.803265
1089.608794	24.985918	68.808270
1088.654794	30.297495	68.813274
1088.151740	26.807278	68.818279
1087.653422	32.912122	68.823284
1086.245606	28.433568	68.828289
1085.732833	30.368071	68.833294
1084.968714	27.479204	68.838298
1084.464444	29.577935	68.843303
1084.410662	19.195895	68.848308
1083.558297	34.516051	68.853313
1082.526520	20.492258	68.858318
1081.836580	28.817982	68.863322
1081.402818	25.947530	68.868327
1081.395354	26.740356	68.873332
1080.511260	34.893541	68.878337
1079.435319	23.234331	68.883342
1078.847020	20.408963	68.888346
1078.304629	26.896134	68.893351
1077.302357	30.945939	68.898356
1076.340559	35.779365	68.903361
1075.861901	32.031379	68.908366
1075.911278	31.775945	68.913370
1075.234868	35.795993	68.918375
1074.307726	29.126276	68.923380
1073.516986	29.409764	68.928385
1072.787996	20.589094	68.933390
1072.053108	26.301060	68.938394
1070.797438	33.087782	68.943399
1070.568337	26.928348	68.948404
1069.909091	34.785568	68.953409
1069.488111	33.097382	68.958414
1069.455414	31.762170	68.963418
1068.611569	26.858019	68.968423
1067.804404	24.133703	68.973428
1067.220996	34.462573	68.978433
1066.506498	34.782821	68.983438
1065.526167	26.826884	68.988442
1064.705233	30.089328	68.993447
1064.411208	20.483526	68.998452
1063.545769	35.925616	69.003457
1063.020720	32.369517	69.008462
1061.695352	39.947929	69.013466
1061.095381	28.842216	69.018471
1061.341258	27.027447	69.023476
1060.729526	36.226990	69.028481
1059.899319	29.366816	69.033486
1059.116746	34.783597	69.038490
1058.322356	35.759957	69.043495
1057.839204	28.360446	69.048500
1056.744147	35.996838	69.053505
1056.090939	32.942102	69.058510
1055.575097	30.379603	69.063514
1055.003042	27.308804	69.068519
1054.829426	22.804242	69.073524
1053.567264	29.106299	69.078529
1052.932981	27.822635	69.083534
1052.642336	22.445708	69.088538
1051.636064	29.730505	69.093543
1050.717414	30.920601	69.098548
1050.382724	30.820884	69.103553
1049.825593	28.143530	69.108558
1049.563395	30.586958	69.113562
1048.377620	33.596787	69.118567
1047.686064	17.927737	69.123572
1046.764751	27.539228	69.128577
1046.231198	28.270667	69.133582
1046.097602	20.263618	69.138586
1045.056565	31.247189	69.143591
1044.572163	14.013960	69.148596
1043.865715	29.008127	69.153601
1043.548906	25.433098	69.158606
1042.480229	28.657690	69.163610
1041.344764	26.925480	69.168615
1040.989302	26.050051	69.173620
1040.244555	28.327396	69.178625
1040.197385	31.547174	69.183630
1039.101795	25.922990	69.188634
1038.234774	29.096578	69.193639
1038.094973	21.191442	69.198644
1037.299931	32.648394	69.203649
1036.720422	36.019096	69.208654
1035.918209	30.417624	69.213658
1035.012171	27.554506	69.218663
1034.715236	26.179331	69.223668
1033.675306	32.509121	69.228673
1032.828596	31.653498	69.233678
1032.338659	39.635180	69.238682
1031.885043	34.799846	69.243687
1031.686646	30.638273	69.248692
1030.721595	35.287727	69.253697
1029.805092	27.227035	69.258702
1029.452609	35.538509	69.263706
1028.546464	35.386206	69.268711
1028.322089	21.550959	69.273716
1026.797634	29.583681	69.278721
1026.547037	27.551427	69.283726
1026.157305	26.512717	69.288730
1025.239999	27.163288	69.293735
1024.755509	28.172356	69.298740
1023.537959	19.434164	69.303745
1023.343791	23.781199	69.308750
1022.800448	30.792082	69.313754
1022.052838	33.208660	69.318759
1021.023666	30.828764	69.323764
1020.457816	30.986603	69.328769
1020.177154	29.209870	69.333774
1019.468578	31.473581	69.338778
1018.683937	30.434623	69.343783
1017.913147	20.830567	69.348788
1017.219905	30.293817	69.353793
1016.676292	31.542529	69.358798
1016.695052	19.918928	69.363802
1015.351419	22.938114	69.368807
1014.661553	26.063024	69.373812
1013.962173	25.608170	69.378817
1013.565545	29.485945	69.383822
1012.762343	24.343537	69.388826
1011.516000	24.010400	69.393831
1011.334894	12.937423	69.398836
1010.641179	27.511672	69.403841
1010.533639	24.147783	69.408846
1009.645541	24.145582	69.413850
1008.782635	32.535110	69.418855
1008.438916	23.922826	69.423860
1007.282173	31.266271	69.428865
1006.563918	24.088686	69.433870
1005.975408	21.428952	69.438874
1005.384856	30.555743	69.443879
1005.322268	23.638118	69.448884
1004.588981	29.941206	69.453889
1003.409609	26.932354	69.458894
1002.889397	24.460451	69.463898
1002.267563	27.006833	69.468903
1001.641383	23.730194	69.473908
1000.712430	30.479155	69.478913
999.862078	27.998277	69.483918
999.550358	23.690737	69.488922
999.257544	31.702556	69.493927
998.302701	29.913243	69.498932
997.268201	34.632105	69.503937
997.010166	34.018725	69.508942
996.500215	27.828294	69.513946
995.542181	25.317242	69.518951
994.890562	28.978546	69.523956
994.405819	31.772779	69.528961
993.615177	27.628172	69.533966
992.758778	34.994800	69.538970
991.855593	31.338033	69.543975
991.526281	28.889374	69.548980
991.134403	31.252515	69.553985
990.537892	29.022990	69.558990
989.830463	24.811528	69.563994
988.687926	28.240281	69.568999
988.490356	18.576573	69.574004
988.076902	26.336347	69.579009
986.597730	31.583282	69.584014
986.199036	20.712083	69.589018
985.279604	29.946398	69.594023
985.084780	30.403181	69.599028
984.631961	27.696630	69.604033
983.678916	25.197405	69.609038
983.069094	28.292240	69.614042
982.308052	32.144423	69.619047
982.066855	24.678051	69.624052
980.776392	30.174085	69.629057
979.920944	25.049464	69.634062
979.414307	25.723017	69.639066
978.893272	25.255567	69.644071
978.606313	25.080456	69.649076
978.007716	25.472173	69.654081
977.009939	23.178766	69.659086
976.607722	24.513798	69.664090
975.946970	38.423648	69.669095
975.458109	17.770722	69.674100
974.172966	24.606325	69.679105
974.093428	21.676379	69.684110
973.516747	27.363194	69.689114
972.286115	27.957983	69.694119
971.762468	29.004830	69.699124
970.911708	32.374549	69.704129
970.496907	36.048641	69.709134
970.041446	26.249346	69.714138
968.693915	32.752682	69.719143
968.370100	25.782009	69.724148
967.710923	24.333595	69.729153
967.466587	34.072358	69.734158
967.217130	26.750806	69.739162
965.575097	37.103056	69.744167
965.285555	27.852951	69.749172
964.950066	30.514630	69.754177
963.804680	32.363734	69.759182
963.138684	25.147887	69.764186
962.258765	33.067046	69.769191
962.367308	23.148049	69.774196
961.161078	28.490339	69.779201
960.264456	22.646876	69.784206
959.839512	33.049891	69.789210
959.250710	43.542065	69.794215
958.743052	27.261885	69.799220
957.435277	26.432345	69.804225
956.599083	26.477096	69.809230
956.512456	29.960196	69.814234
956.061285	35.447273	69.819239
955.690426	34.653154	69.824244
954.745099	25.723446	69.829249
953.759667	27.935034	69.834254
953.752973	33.155840	69.839258
952.907053	37.423663	69.844263
951.810039	29.415383	69.849268
950.941528	28.843957	69.854273
950.621406	37.434139	69.859278
950.190847	31.573285	69.864282
949.682651	39.116332	69.869287
948.901605	36.327974	69.874292
948.051326	39.180383	69.879297
947.622858	39.467765	69.884302
946.466248	33.102700	69.889306
945.333733	33.672426	69.894311
945.221998	31.778935	69.899316
944.446277	48.258613	69.904321
944.147283	42.231741	69.909326
944.243680	27.118590	69.914330
942.857628	35.288607	69.919335
942.302795	26.679968	69.924340
941.446745	42.678835	69.929345
940.436716	39.494830	69.934350
939.772450	36.031877	69.939354
938.854249	33.937134	69.944359
938.709803	30.123381	69.949364
938.043561	40.213137	69.954369
938.041618	35.753807	69.959374
937.239391	32.899438	69.964378
936.136927	37.679601	69.969383
935.608343	35.246891	69.974388
934.541631	37.365765	69.979393
933.871414	28.073741	69.984398
933.245757	27.574063	69.989402
932.574713	38.776340	69.994407
932.420527	32.360576	69.999412
931.948860	31.178800	70.004417
930.809656	39.580781	70.009422
930.549096	38.018480	70.014426
929.773610	38.755327	70.019431
928.816728	31.475391	70.024436
927.805801	37.234475	70.029441
927.083470	36.237669	70.034446
927.067093	33.177824	70.039450
926.445969	38.882763	70.044455
925.727968	32.577222	70.049460
924.958063	33.582842	70.054465
924.279907	28.947271	70.059470
923.757531	38.266656	70.064474
922.693520	42.014105	70.069479
922.335576	18.065021	70.074484
921.479058	29.995401	70.079489
921.012760	33.141527	70.084494
920.373863	31.079615	70.089498
919.519249	43.865992	70.094503
918.869093	34.062997	70.099508
918.107936	33.657425	70.104513
917.774829	35.982838	70.109518
917.278144	27.503726	70.114522
916.096590	34.505801	70.119527
915.747647	27.338862	70.124532
915.024425	24.684820	70.129537
914.416568	38.901651	70.134542
913.913013	33.407238	70.139546
913.356856	30.702954	70.144551
912.617719	32.332888	70.149556
911.403222	29.764911	70.154561
910.839401	20.701975	70.159566
910.535069	20.390865	70.164570
909.759534	36.878390	70.169575
908.880812	31.708612	70.174580
907.769012	37.329214	70.179585
907.267969	32.405262	70.184590
906.976275	29.704625	70.189594
906.800584	35.450643	70.194599
906.262436	28.451012	70.199604
905.319663	39.113062	70.204609
904.385750	33.259784	70.209614
904.208007	23.512508	70.214618
903.040945	37.875103	70.219623
902.129794	35.389742	70.224628
901.666758	31.830122	70.229633
900.983329	32.875603	70.234638
900.930027	32.431503	70.239642
899.613712	40.402786	70.244647
898.931157	31.458092	70.249652
898.393676	34.658128	70.254657
897.874164	39.164181	70.259662
897.449556	35.699371	70.264666
896.232718	37.499951	70.269671
895.692363	35.767717	70.274676
895.057269	33.702052	70.279681
894.505186	44.166313	70.284686
894.025581	34.120141	70.289690
893.183535	38.029395	70.294695
892.465729	34.169698	70.299700
892.409681	34.170738	70.304705
891.005292	39.896259	70.309710
890.603564	36.525580	70.314714
889.686666	37.289675	70.319719
889.734708	35.236717	70.324724
888.634524	43.954205	70.329729
887.458837	39.333168	70.334734
887.284794	35.796943	70.339738
886.679870	37.689378	70.344743
886.164316	26.962957	70.349748
884.968953	36.063020	70.354753
884.226475	39.883891	70.359758
883.889794	27.905282	70.364762
883.464675	38.921770	70.369767
882.847193	29.481022	70.374772
881.850033	34.730149	70.379777
880.908592	34.323319	70.384782
880.742608	27.269196	70.389786
880.234927	35.032941	70.394791
879.367870	21.154935	70.399796
878.595734	29.651473	70.404801
877.762037	40.274094	70.409806
877.730789	33.092869	70.414810
876.984204	34.514263	70.419815
875.983596	35.750581	70.424820
875.208099	37.586586	70.429825
874.584817	36.990350	70.434830
874.447676	25.932470	70.439834
873.324146	36.099744	70.444839
872.694117	30.857285	70.449844
872.014634	28.000751	70.454849
871.640412	30.162401	70.459854
870.525616	19.690636	70.464858
869.650278	33.954768	70.469863
869.589362	23.982322	70.474868
868.759026	25.254621	70.479873
868.267541	30.246649	70.484878
867.580083	24.005658	70.489882
866.765180	36.634331	70.494887
866.758602	21.220617	70.499892
865.670323	20.234766	70.504897
864.593116	34.108404	70.509902
864.082216	25.756150	70.514906
863.416090	41.168134	70.519911
863.003772	32.264020	70.524916
861.697010	33.124869	70.529921
861.053043	28.619495	70.534926
860.950488	22.842079	70.539930
860.250546	29.991449	70.544935
859.890891	19.429464	70.549940
858.744362	23.082833	70.554945
858.326995	37.969519	70.559950
857.977710	26.584283	70.564954
856.540456	38.611845	70.569959
855.879631	33.025783	70.574964
855.215815	30.737620	70.579969
854.828638	41.437411	70.584974
854.653670	31.304919	70.589978
853.683674	44.062365	70.594983
852.964530	40.060967	70.599988
852.364177	37.114572	70.604993
851.784458	34.526016	70.609998
851.001766	31.348446	70.615002
849.838029	41.345512	70.620007
849.170783	33.757737	70.625012
849.157439	36.658315	70.630017
848.447824	34.994033	70.635022
847.935083	31.383988	70.640026
846.378724	39.284690	70.645031
846.414078	34.735850	70.650036
845.910795	36.023910	70.655041
844.960927	40.074920	70.660046
844.478446	27.211200	70.665050
843.717876	36.454963	70.670055
843.203373	35.540222	70.675060
842.201874	22.377494	70.680065
841.473578	37.912912	70.685070
840.963911	35.262747	70.690074
840.203498	35.618752	70.695079
840.048534	33.022517	70.700084
839.141007	35.592332	70.705089
837.976648	43.583612	70.710094
837.873284	27.899872	70.715098
837.455509	38.538300	70.720103
836.528923	30.337372	70.725108
835.711556	31.476729	70.730113
834.869726	36.833613	70.735118
834.548766	30.975843	70.740122
833.575595	35.737041	70.745127
832.822667	37.211497	70.750132
832.075055	30.636313	70.755137
831.710777	35.251708	70.760142
831.624706	16.310388	70.765146
830.887486	33.053595	70.770151
829.883672	30.972521	70.775156
829.534057	38.794693	70.780161
828.375381	30.857793	70.785166
827.359195	32.673775	70.790170
826.626660	31.194498	70.795175
826.586030	22.131890	70.800180
826.070533	26.539540	70.805185
825.277548	36.698372	70.810190
824.403030	27.833148	70.815194
823.764688	33.045680	70.820199
823.110724	36.518161	70.825204
822.880812	27.257019	70.830209
821.726729	27.322453	70.835214
821.629225	33.152220	70.840218
820.885338	29.083810	70.845223
820.008061	26.921099	70.850228
819.419083	25.551438	70.855233
818.500176	35.031722	70.860238
818.590680	23.152294	70.865242
817.000566	37.448213	70.870247
816.243042	21.849688	70.875252
815.721381	26.975837	70.880257
815.056248	30.692948	70.885262
814.974315	29.673087	70.890266
813.677741	32.519304	70.895271
813.131350	32.984753	70.900276
812.598969	24.001998	70.905281
811.928694	28.714987	70.910286
811.658193	27.059666	70.915290
810.685405	32.724407	70.920295
809.746462	35.461660	70.925300
809.316917	20.675105	70.930305
808.764212	30.112865	70.935310
807.898580	25.297440	70.940314
806.903262	29.811435	70.945319
806.316151	28.176552	70.950324
805.793634	30.937404	70.955329
805.700908	36.982454	70.960334
805.379251	24.846935	70.965338
804.290300	32.428825	70.970343
803.647267	33.732831	70.975348
802.710801	30.311673	70.980353
801.304358	39.904265	70.985358
801.153105	21.214596	70.990362
800.499669	34.585555	70.995367
800.263386	33.796846	71.000372
800.160337	36.894629	71.005377
798.872928	32.882784	71.010382
798.508858	34.834668	71.015386
797.452184	31.397955	71.020391
796.181508	23.141437	71.025396
795.925869	26.282431	71.030401
794.907757	28.898249	71.035406
794.898781	41.300876	71.040410
794.122571	43.043978	71.045415
793.744535	34.571242	71.050420
792.649923	21.122166	71.055425
792.161175	36.627340	71.060430
791.647483	16.183452	71.065434
790.856305	22.662957	71.070439
789.783267	31.713618	71.075444
789.143453	32.580298	71.080449
788.582357	18.290934	71.085454
788.601298	20.617087	71.090458
787.978658	26.456329	71.095463
786.811131	24.404490	71.100468
786.244018	28.541243	71.105473
785.532413	34.719503	71.110478
785.062915	21.714969	71.115482
783.967093	29.414653	71.120487
783.366000	29.903008	71.125492
782.864248	30.457551	71.130497
782.748944	19.301599	71.135502
782.001369	24.238211	71.140506
780.566700	26.103483	71.145511
780.078005	29.198001	71.150516
779.995493	26.607585	71.155521
779.042485	25.567122	71.160526
778.121209	25.407857	71.165530
777.657024	26.699167	71.170535
777.179262	27.497474	71.175540
776.220383	19.889925	71.180545
775.318156	21.880173	71.185550
775.423779	26.709349	71.190554
774.671565	30.058708	71.195559
773.425644	25.508840	71.200564
772.766395	39.207161	71.205569
772.062544	31.883862	71.210574
771.648729	22.568431	71.215578
771.090190	29.917658	71.220583
770.738966	36.681951	71.225588
769.691870	25.251709	71.230593
768.745135	30.303611	71.235598
768.976477	23.088482	71.240602
767.433578	28.667376	71.245607
766.701166	31.199875	71.250612
766.389972	23.799880	71.255617
765.950887	29.253514	71.260622
765.475554	32.626606	71.265626
764.399307	28.869748	71.270631
763.748569	22.922569	71.275636
763.271169	39.353190	71.280641
762.356504	33.055362	71.285646
761.290602	21.714855	71.290650
761.041021	29.404405	71.295655
760.435504	28.073662	71.300660
760.405963	25.787052	71.305665
759.084455	31.251859	71.310670
758.523837	24.481355	71.315674
757.724825	30.723998	71.320679
757.021792	32.190531	71.325684
756.199508	28.481556	71.330689
755.110174	37.848641	71.335694
754.918835	21.742114	71.340698
754.313212	35.480782	71.345703
753.980805	35.483243	71.350708
753.947715	27.423961	71.355713
752.682658	28.609386	71.360718
752.196615	27.835214	71.365722
751.520218	32.973393	71.370727
750.415871	34.786094	71.375732
749.831988	24.907961	71.380737
748.960273	32.967796	71.385742
748.858290	23.976464	71.390746
747.754194	22.963222	71.395751
746.758619	35.954995	71.400756
746.370964	38.538270	71.405761
745.720547	27.896443	71.410766
745.996819	13.880641	71.415770
744.661451	27.544671	71.420775
743.678606	28.716710	71.425780
743.837168	21.442205	71.430785
742.597728	29.797128	71.435790
741.758016	21.650227	71.440794
741.285153	26.363340	71.445799
740.553448	28.656036	71.450804
740.370060	27.172937	71.455809
739.161966	31.444864	71.460814
738.346224	23.559076	71.465818
737.797113	31.075541	71.470823
737.262335	29.884930	71.475828
736.937436	20.432351	71.480833
735.762822	35.967875	71.485838
735.328563	31.157914	71.490842
734.744984	30.828206	71.495847
734.492091	23.166623	71.500852
733.606799	22.210014	71.505857
732.314241	29.420643	71.510862
732.078580	26.007788	71.515866
731.731793	18.146691	71.520871
730.701001	27.682653	71.525876
730.029268	22.815888	71.530881
729.404678	31.388317	71.535886
729.044251	26.240175	71.540890
727.773628	32.488526	71.545895
727.218817	28.262313	71.550900
726.899249	28.731090	71.555905
726.175930	38.254376	71.560910
725.540510	26.096292	71.565914
724.692306	29.117171	71.570919
723.820877	30.788720	71.575924
723.749805	25.783745	71.580929
722.891315	28.919802	71.585934
721.991341	19.971950	71.590938
721.207310	25.515201	71.595943
720.855438	19.824805	71.600948
720.376638	21.254069	71.605953
719.379303	28.539125	71.610958
718.667013	17.694278	71.615962
718.125883	28.718198	71.620967
717.673610	32.087626	71.625972
717.257470	27.784143	71.630977
715.859064	27.133165	71.635982
715.768153	21.844344	71.640986
714.914278	28.592473	71.645991
714.274903	34.893290	71.650996
713.431407	29.647022	71.656001
712.477454	33.211445	71.661006
712.395501	23.024751	71.666010
711.972227	23.979974	71.671015
711.100269	19.763263	71.676020
710.448077	23.214983	71.681025
709.663786	28.632123	71.686030
709.096099	19.252901	71.691034
707.817365	28.159719	71.696039
706.883039	19.387655	71.701044
706.838052	28.754049	71.706049
706.015649	33.112815	71.711054
706.325528	18.224334	71.716058
705.170407	23.815635	71.721063
704.206293	29.237754	71.726068
703.635720	15.596487	71.731073
702.977484	27.019098	71.736078
702.436392	27.551535	71.741082
701.234908	28.504513	71.746087
700.651213	29.188813	71.751092
700.316626	25.876870	71.756097
699.950344	28.477246	71.761102
699.331979	22.248967	71.766106
698.229479	28.088937	71.771111
697.684679	29.312672	71.776116
697.435895	21.103239	71.781121
696.208442	25.550154	71.786126
695.608156	17.964394	71.791130
694.986927	26.012741	71.796135
694.359852	32.395181	71.801140
694.242247	20.509479	71.806145
692.738885	31.232454	71.811150
692.454123	25.531376	71.816154
691.770388	23.033543	71.821159
691.117780	25.395660	71.826164
690.466466	20.847356	71.831169
689.461148	20.119610	71.836174
689.061274	23.501197	71.841178
688.520042	25.566458	71.846183
688.096597	25.034644	71.851188
687.219746	18.552638	71.856193
686.687588	25.457704	71.861198
686.266599	15.020652	71.866202
684.907900	22.800072	71.871207
684.282167	21.026290	71.876212
684.117980	14.094919	71.881217
683.334107	24.678097	71.886222
682.513761	19.940668	71.891226
681.929082	20.377547	71.896231
680.936548	23.285802	71.901236
680.727030	22.503883	71.906241
679.328629	29.838622	71.911246
678.846590	23.389945	71.916250
678.248901	21.272654	71.921255
678.020742	22.116389	71.926260
677.900013	23.036058	71.931265
676.675373	25.960773	71.936270
676.054360	20.188663	71.941274
675.444118	27.202359	71.946279
674.779186	29.779331	71.951284
673.876855	27.978632	71.956289
672.913303	31.642369	71.961294
672.371239	16.489004	71.966298
672.362475	25.474309	71.971303
671.155384	33.462989	71.976308
670.376607	19.719266	71.981313
669.768829	28.609146	71.986318
669.408287	21.396803	71.991322
668.833579	19.195431	71.996327
667.894756	31.261973	72.001332
667.030042	23.305164	72.006337
666.626920	24.895852	72.011342
666.425066	21.203234	72.016346
665.131406	26.701495	72.021351
664.182498	33.654007	72.026356
663.935590	11.551320	72.031361
663.169165	29.303709	72.036366
662.865195	21.844239	72.041370
662.414242	19.151653	72.046375
661.010246	21.623964	72.051380
660.843894	26.065929	72.056385
660.404883	28.816664	72.061390
659.782420	22.877632	72.066394
658.616887	26.881041	72.071399
658.007608	30.076783	72.076404
657.650151	18.856911	72.081409
656.622557	22.526118	72.086414
656.085419	19.820449	72.091418
655.162269	20.032112	72.096423
654.793817	19.292851	72.101428
654.255923	15.265817	72.106433
653.173182	23.906479	72.111438
652.502584	9.849080	72.116442
652.201289	20.038446	72.121447
651.671735	20.725175	72.126452
651.346296	14.259456	72.131457
650.174266	24.500752	72.136462
649.958999	21.977218	72.141466
648.903503	22.198920	72.146471
647.583024	21.532417	72.151476
647.218742	15.124924	72.156481
646.556623	29.741493	72.161486
646.108476	26.594300	72.166490
645.936449	18.612352	72.171495
644.711300	21.502469	72.176500
644.336063	15.609230	72.181505
643.480632	22.907980	72.186510
642.955834	20.153040	72.191514
642.502354	16.437419	72.196519
641.340251	27.847239	72.201524
641.108439	17.603999	72.206529
640.512018	21.243972	72.211534
639.580768	20.269485	72.216538
639.116235	18.462161	72.221543
638.301960	25.971979	72.226548
637.808303	24.967230	72.231553
636.365941	33.953755	72.236558
636.211141	20.317260	72.241562
635.948681	17.526854	72.246567
635.263932	26.895773	72.251572
634.288955	17.948868	72.256577
633.480998	23.976922	72.261582
633.278727	23.466666	72.266586
632.608988	19.399131	72.271591
631.271705	22.147840	72.276596
630.709453	31.025746	72.281601
630.043747	30.770643	72.286606
629.840523	24.903627	72.291610
629.099252	23.397418	72.296615
628.294367	32.244580	72.301620
628.007978	19.310288	72.306625
627.092589	26.618592	72.311630
626.333190	21.653858	72.316634
625.193521	18.466987	72.321639
624.426237	22.988883	72.326644
624.192494	15.715359	72.331649
623.840606	35.188431	72.336654
623.813947	24.248620	72.341658
622.669515	25.214627	72.346663
621.487331	27.071316	72.351668
621.277526	21.911826	72.356673
620.829850	25.603810	72.361678
619.538752	24.774947	72.366682
619.028647	22.178523	72.371687
618.435488	26.590689	72.376692
618.487901	22.728273	72.381697
616.776223	25.397842	72.386702
616.203933	16.153427	72.391706
615.813285	20.732037	72.396711
615.085642	12.926892	72.401716
614.145732	19.147851	72.406721
613.319523	26.396225	72.411726
612.891307	26.018148	72.416730
612.517068	26.172370	72.421735
612.344755	21.784349	72.426740
611.636385	12.657804	72.431745
610.728548	26.017251	72.436750
610.231310	19.448012	72.441754
609.048321	21.449915	72.446759
607.935671	28.291324	72.451764
608.033339	14.647748	72.456769
607.109567	9.485277	72.461774
606.910248	16.319995	72.466778
606.116170	19.510483	72.471783
605.049933	16.094309	72.476788
604.892546	15.718833	72.481793
603.973150	29.950605	72.486798
602.988442	23.708160	72.491802
602.147176	17.359295	72.496807
601.584388	18.566989	72.501812
601.600994	16.963743	72.506817
600.971424	18.484848	72.511822
600.014700	18.766534	72.516826
599.178240	13.208536	72.521831
598.604153	21.031768	72.526836
598.351144	17.646928	72.531841
596.941221	21.427510	72.536846
596.622051	26.084626	72.541850
596.033433	19.430597	72.546855
595.376090	20.990820	72.551860
594.598078	25.311006	72.556865
593.946795	30.077788	72.561870
593.166232	31.468403	72.566874
592.958400	22.766765	72.571879
591.924398	24.502097	72.576884
591.408854	21.021874	72.581889
590.317466	30.517070	72.586894
590.107144	27.450281	72.591898
589.667995	21.471038	72.596903
588.634022	30.006186	72.601908
587.915646	20.756660	72.606913
587.107344	27.101749	72.611918
586.932190	26.448406	72.616922
586.528841	25.027162	72.621927
585.302780	22.057496	72.626932
584.589971	16.156534	72.631937
583.993583	36.204709	72.636942
583.667320	34.328063	72.641946
582.904375	27.058402	72.646951
581.544994	36.178395	72.651956
581.381298	20.031241	72.656961
581.053819	25.575929	72.661966
580.144513	26.616469	72.666970
579.327738	24.828988	72.671975
578.518101	32.655053	72.676980
578.515150	27.267078	72.681985
577.527225	23.084658	72.686990
576.719130	21.164910	72.691994
575.977532	23.064987	72.696999
575.220026	35.462220	72.702004
574.953148	27.168957	72.707009
574.494453	27.984764	72.712014
573.351976	12.383023	72.717018
572.900304	16.796314	72.722023
572.210854	22.005993	72.727028
571.789433	15.240187	72.732033
570.598867	24.273365	72.737038
570.086534	25.331105	72.742042
569.881561	22.250853	72.747047
568.860607	34.797281	72.752052
568.772448	16.211173	72.757057
567.358503	32.116022	72.762062
567.029077	20.243582	72.767066
566.577807	27.791794	72.772071
565.504982	31.113426	72.777076
564.787335	25.894482	72.782081
564.027343	30.396311	72.787086
563.359929	25.795416	72.792090
563.105505	14.753127	72.797095
561.889280	14.522651	72.802100
561.154190	13.490142	72.807105
560.831606	22.825041	72.812110
560.445874	14.624835	72.817114
560.323641	15.505324	72.822119
559.448205	30.395577	72.827124
558.671879	15.765272	72.832129
557.558877	24.376093	72.837134
556.481948	22.887101	72.842138
556.294812	20.652410	72.847143
555.329698	24.838405	72.852148
554.942726	16.684128	72.857153
554.589055	25.508318	72.862158
553.930002	16.970025	72.867162
553.206029	12.767654	72.872167
552.477435	23.614864	72.877172
551.853658	24.743975	72.882177
551.062235	32.436258	72.887182
550.105740	26.093149	72.892186
549.483752	17.722418	72.897191
548.965263	24.514939	72.902196
548.916072	16.811485	72.907201
547.981364	20.784481	72.912206
547.343421	27.323217	72.917210
546.913259	25.876289	72.922215
545.397590	25.515322	72.927220
544.969984	24.534764	72.932225
544.608248	32.625383	72.937230
544.181705	22.615028	72.942234
543.180107	19.731057	72.947239
542.046232	28.610139	72.952244
541.803568	22.700534	72.957249
541.364960	28.508931	72.962254
540.744170	23.332915	72.967258
539.663341	24.861260	72.972263
538.845398	34.491114	72.977268
538.458182	23.686019	72.982273
538.300840	22.738107	72.987278
537.396299	38.639104	72.992282
536.419941	21.711506	72.997287
535.597426	33.967713	73.002292
535.421018	19.850558	73.007297
534.444959	28.471115	73.012302
533.593799	26.003153	73.017306
533.007042	26.221201	73.022311
532.338697	31.921116	73.027316
532.030484	25.769640	73.032321
531.750588	24.959521	73.037326
530.386847	34.647933	73.042330
529.607190	33.360758	73.047335
529.451013	40.559199	73.052340
529.092106	20.921817	73.057345
527.800200	33.143986	73.062350
527.142725	25.504309	73.067354
527.112965	18.062690	73.072359
525.942447	25.758592	73.077364
524.902074	19.977637	73.082369
524.464581	22.322872	73.087374
524.103279	19.942463	73.092378
523.800753	12.624722	73.097383
522.206860	21.080345	73.102388
521.860198	24.358859	73.107393
520.945675	25.859144	73.112398
520.680071	27.549373	73.117402
520.542397	19.099925	73.122407
519.226322	24.768980	73.127412
518.662192	24.813116	73.132417
518.051279	24.621855	73.137422
517.573183	19.251229	73.142426
516.543071	22.758463	73.147431
515.826021	20.737500	73.152436
515.400174	19.706206	73.157441
515.105802	27.893326	73.162446
514.489123	25.329671	73.167450
513.822385	20.072675	73.172455
512.868125	26.819501	73.177460
512.137888	17.595550	73.182465
510.717279	21.597077	73.187470
510.586012	26.336230	73.192474
509.952456	13.504586	73.197479
509.242835	26.873482	73.202484
509.388198	16.934462	73.207489
508.075727	19.162040	73.212494
507.342760	17.824858	73.217498
507.117950	20.826919	73.222503
506.512374	25.613245	73.227508
505.685829	23.218643	73.232513
504.912172	22.329490	73.237518
504.138054	23.381637	73.242522
503.802055	24.177910	73.247527
502.464325	22.705258	73.252532
501.928567	21.300391	73.257537
501.600804	20.758099	73.262542
501.310922	34.555299	73.267546
500.262758	21.075342	73.272551
499.051467	29.675036	73.277556
498.742574	18.485318	73.282561
498.104936	21.198331	73.287566
497.729965	22.939100	73.292570
497.167836	23.178465	73.297575
495.991411	26.608091	73.302580
495.879188	19.211150	73.307585
494.916850	27.255522	73.312590
493.806172	15.815069	73.317594
493.266394	19.315161	73.322599
492.778564	18.314245	73.327604
492.575492	6.347590	73.332609
491.938807	16.317573	73.337614
491.039810	26.133810	73.342618
490.544507	17.916382	73.347623
489.748684	27.244674	73.352628
489.079908	18.457218	73.357633
487.738619	23.215672	73.362638
487.146381	27.708142	73.367642
487.268583	20.057813	73.372647
486.506213	21.393522	73.377652
485.667502	17.830769	73.382657
484.922876	28.158579	73.387662
484.126717	21.349989	73.392666
484.118022	17.871049	73.397671
483.406249	17.388359	73.402676
482.410595	12.976981	73.407681
481.600298	21.429217	73.412686
481.065612	16.051848	73.417690
480.653434	13.023541	73.422695
479.353728	27.243384	73.427700
479.182850	17.848332	73.432705
478.535203	19.790239	73.437710
477.928919	12.237048	73.442714
477.145885	11.573325	73.447719
476.166089	25.866781	73.452724
475.590544	15.654685	73.457729
475.120511	23.026120	73.462734
474.268901	18.710067	73.467738
473.773790	12.768155	73.472743
472.904262	14.590870	73.477748
472.613646	12.897799	73.482753
472.070310	19.441974	73.487758
470.872720	15.699860	73.492762
470.640036	16.501755	73.497767
470.129669	17.620701	73.502772
469.243551	16.795208	73.507777
468.317874	20.891371	73.512782
467.414785	21.684956	73.517786
467.228726	18.004039	73.522791
466.467849	20.339302	73.527796
466.311781	18.825067	73.532801
465.246875	21.849010	73.537806
464.289956	24.482011	73.542810
464.114726	20.474517	73.547815
463.110352	18.362152	73.552820
462.535636	22.433941	73.557825
461.839660	22.297246	73.562830
461.182914	20.220961	73.567834
461.044952	26.520785	73.572839
459.552174	18.884906	73.577844
459.276436	18.801107	73.582849
458.273416	23.964576	73.587854
458.191970	26.240480	73.592858
457.829805	13.688894	73.597863
456.719125	11.984552	73.602868
456.484760	15.987923	73.607873
455.055748	11.342827	73.612878
454.338511	16.277837	73.617882
453.745292	12.586099	73.622887
453.265355	18.385317	73.627892
453.021847	14.614208	73.632897
452.032352	21.609515	73.637902
450.986785	18.991209	73.642906
450.811710	14.775536	73.647911
450.466480	21.102072	73.652916
449.458965	15.246535	73.657921
448.321271	21.814448	73.662926
447.814879	28.163510	73.667930
447.595715	11.012835	73.672935
446.689402	28.645610	73.677940
445.685653	19.599302	73.682945
444.969005	22.479457	73.687950
444.589050	20.865277	73.692954
444.228852	14.042440	73.697959
443.695398	22.475808	73.702964
443.163216	24.038205	73.707969
442.432696	13.961200	73.712974
441.402571	13.401511	73.717978
440.137833	10.434933	73.722983
439.495912	25.616004	73.727988
439.057990	30.260514	73.732993
438.440975	27.491931	73.737998
437.846045	15.371672	73.743002
437.849543	13.822555	73.748007
437.302014	29.401751	73.753012
436.264785	21.120871	73.758017
435.407641	24.941199	73.763022
435.174722	24.954660	73.768026
434.303871	17.412095	73.773031
433.140395	21.822124	73.778036
433.140392	18.160453	73.783041
432.678695	18.065286	73.788046
431.363033	20.064754	73.793050
430.781526	12.376744	73.798055
430.181529	14.784154	73.803060
429.712851	16.629747	73.808065
428.564383	15.664721	73.813070
427.582964	23.671151	73.818074
427.351917	13.451491	73.823079
426.747257	37.162663	73.828084
426.486225	22.932857	73.833089
425.958835	23.518362	73.838094
425.002789	19.684169	73.843098
424.555164	20.559739	73.848103
423.490258	27.168105	73.853108
422.769211	20.822234	73.858113
421.986338	12.362068	73.863118
421.378029	21.859190	73.868122
421.345723	15.843550	73.873127
420.671789	32.072092	73.878132
419.643652	16.389149	73.883137
418.885382	18.884858	73.888142
418.367788	14.561339	73.893146
417.764594	14.479259	73.898151
416.598710	27.077200	73.903156
416.204160	22.357182	73.908161
415.956250	14.852564	73.913166
414.891102	16.985588	73.918170
414.230880	18.666162	73.923175
413.453086	24.832969	73.928180
413.041591	16.756752	73.933185
412.914872	26.486224	73.938190
411.932190	24.834047	73.943194
410.943069	22.441730	73.948199
410.353421	27.840547	73.953204
410.039728	29.797068	73.958209
408.902837	20.196406	73.963214
407.946604	27.951251	73.968218
407.507913	25.263071	73.973223
407.052551	34.858835	73.978228
406.671765	21.069164	73.983233
405.862997	25.411647	73.988238
404.947966	22.681099	73.993242
404.757663	16.293244	73.998247
403.995481	18.043684	74.003252
402.714948	21.616095	74.008257
402.201750	22.467425	74.013262
401.616685	27.157463	74.018266
401.505745	16.086039	74.023271
400.708021	21.661514	74.028276
399.766604	20.032729	74.033281
399.211174	31.126768	74.038286
398.737900	32.063201	74.043290
397.602907	16.023560	74.048295
396.652874	18.830529	74.053300
396.424984	24.301013	74.058305
396.020927	32.839929	74.063310
395.655210	29.633923	74.068314
394.632385	17.933521	74.073319
393.557693	19.331640	74.078324
393.256757	18.083346	74.083329
392.826613	12.405493	74.088334
391.752562	22.123490	74.093338
391.151790	14.224097	74.098343
390.435425	19.583183	74.103348
390.088635	16.763670	74.108353
389.441489	19.203834	74.113358
388.221948	26.962794	74.118362
388.044373	12.448475	74.123367
387.448193	22.951340	74.128372
386.646830	23.042770	74.133377
385.909544	25.535146	74.138382
384.743807	30.289334	74.143386
384.610224	17.092638	74.148391
384.073582	23.291986	74.153396
383.600401	18.606584	74.158401
382.659983	22.440197	74.163406
382.140956	16.790701	74.168410
381.570356	16.378585	74.173415
380.147548	18.355728	74.178420
379.878171	17.528183	74.183425
379.332195	17.509534	74.188430
378.756072	18.687863	74.193434
378.337490	14.712851	74.198439
377.245530	24.553556	74.203444
376.442238	27.660425	74.208449
375.854353	26.907289	74.213454
375.644162	13.645536	74.218458
374.900972	17.140216	74.223463
373.770801	26.225347	74.228468
373.300371	21.752396	74.233473
373.108973	18.326229	74.238478
371.903739	26.253227	74.243482
371.082205	21.214909	74.248487
370.516251	32.367400	74.253492
370.076896	25.926194	74.258497
369.718964	27.093409	74.263502
368.854255	30.036603	74.268506
368.020440	22.010348	74.273511
367.384936	26.123382	74.278516
366.973870	17.610293	74.283521
366.467600	22.377665	74.288526
365.206895	23.625667	74.293530
365.001730	12.040989	74.298535
364.415473	28.047404	74.303540
363.566775	25.315762	74.308545
362.759238	24.474631	74.313550
362.229113	15.986825	74.318554
361.645028	16.365336	74.323559
360.909878	20.767062	74.328564
360.353908	19.327603	74.333569
359.465010	20.708743	74.338574
358.818827	27.472755	74.343578
358.128984	18.847975	74.348583
357.456356	24.917612	74.353588
356.727257	21.421017	74.358593
356.188892	11.865358	74.363598
355.424538	23.497314	74.368602
354.882510	15.791996	74.373607
353.964306	25.803716	74.378612
353.509106	21.214802	74.383617
353.106957	21.493359	74.388622
352.141312	24.335949	74.393626
351.695679	21.320883	74.398631
351.035918	15.354780	74.403636
350.439778	26.658735	74.408641
349.779549	15.234888	74.413646
348.927127	28.167673	74.418650
348.401088	17.279103	74.423655
347.859808	13.424577	74.428660
346.847100	12.270798	74.433665
346.194085	7.238755	74.438670
345.368490	11.678549	74.443674
345.131675	6.092902	74.448679
344.503859	12.308358	74.453684
343.650580	17.941585	74.458689
343.222769	11.438629	74.463694
342.308236	17.242467	74.468698
342.137940	8.471823	74.473703
340.928095	25.653093	74.478708
339.975735	23.321180	74.483713
339.717453	20.627918	74.488718
338.971004	23.799854	74.493722
338.128823	13.906266	74.498727
337.243409	13.935415	74.503732
336.792014	17.255869	74.508737
336.465973	14.707448	74.513742
335.771526	14.468044	74.518746
335.601512	1.578376	74.523751
334.295011	10.885577	74.528756
333.557661	18.845252	74.533761
333.425678	13.805866	74.538766
332.362470	15.214796	74.543770
331.274456	12.223266	74.548775
330.913644	14.203072	74.553780
330.653055	13.796754	74.558785
330.409947	16.551006	74.563790
329.475903	19.931036	74.568794
328.568731	12.250807	74.573799
327.968083	24.356570	74.578804
326.917948	25.785496	74.583809
325.964763	17.442396	74.588814
325.502077	18.162689	74.593818
325.172582	15.949133	74.598823
324.333311	16.598557	74.603828
323.915179	16.523276	74.608833
323.776960	18.475492	74.613838
322.537241	20.642684	74.618842
322.078256	10.833113	74.623847
321.247451	25.859794	74.628852
320.581163	21.362878	74.633857
320.083407	19.666570	74.638862
319.706960	23.148547	74.643866
318.907343	19.350970	74.648871
317.748865	24.476186	74.653876
316.839045	25.868561	74.658881
316.847743	11.494881	74.663886
315.553751	16.944467	74.668890
314.992576	6.381638	74.673895
314.280488	18.216577	74.678900
314.036923	21.707338	74.683905
313.461958	15.991083	74.688910
312.596306	19.670877	74.693914
311.930792	12.832077	74.698919
311.304949	17.523897	74.703924
310.918312	11.780782	74.708929
310.258379	11.319843	74.713934
308.996216	29.154437	74.718938
308.901945	16.415114	74.723943
308.158550	22.626925	74.728948
307.428983	22.713247	74.733953
306.631849	20.202067	74.738958
305.689312	24.348279	74.743962
305.516749	19.085129	74.748967
304.938944	23.903336	74.753972
303.979156	20.859842	74.758977
303.496088	14.291585	74.763982
302.566087	25.410637	74.768986
302.080462	9.139834	74.773991
301.015016	18.017551	74.778996
300.479176	22.264523	74.784001
300.004244	21.912872	74.789006
299.187965	20.071794	74.794010
299.287216	10.518607	74.799015
298.368672	16.671602	74.804020
297.472389	18.744643	74.809025
297.126501	18.008150	74.814030
295.984834	13.998596	74.819034
295.490754	14.279199	74.824039
294.854895	14.503552	74.829044
294.256626	13.349971	74.834049
293.453425	5.329916	74.839054
292.367407	17.077802	74.844058
292.222385	15.803094	74.849063
291.540307	19.395288	74.854068
291.297518	14.362530	74.859073
290.046139	18.592665	74.864078
289.280856	23.547989	74.869082
288.848757	18.865524	74.874087
288.315436	15.664177	74.879092
287.424101	17.750626	74.884097
286.832379	12.899640	74.889102
285.876245	15.628773	74.894106
285.866046	8.896844	74.899111
284.666452	15.004753	74.904116
283.619029	21.477916	74.909121
283.334035	8.795813	74.914126
282.718448	24.078353	74.919130
282.361412	16.829272	74.924135
282.133872	9.707786	74.929140
281.049623	23.852356	74.934145
280.393563	11.568439	74.939150
279.450480	13.114361	74.944154
279.360005	11.942923	74.949159
278.312689	15.847225	74.954164
277.209327	19.482918	74.959169
277.125129	5.100405	74.964174
276.408403	10.678766	74.969178
275.724988	16.417400	74.974183
275.065960	19.783575	74.979188
274.596901	20.547471	74.984193
273.891141	16.939953	74.989198
272.531125	25.503516	74.994202
272.290121	14.113804	74.999207
271.727425	19.713350	75.004212
271.184614	21.115049	75.009217
270.348866	9.526829	75.014222
269.448193	22.237081	75.019226
269.002863	14.238835	75.024231
268.676308	18.892420	75.029236
267.775702	14.231024	75.034241
267.025857	12.037172	75.039246
266.032761	22.828822	75.044250
265.967861	10.084832	75.049255
265.225844	13.328618	75.054260
264.354513	16.201936	75.059265
263.793837	11.382279	75.064270
263.252126	22.278597	75.069274
262.674335	15.001631	75.074279
261.369224	17.092544	75.079284
260.802453	14.118885	75.084289
260.831706	19.221955	75.089294
260.146553	15.365154	75.094298
259.105214	10.439191	75.099303
258.515819	17.066431	75.104308
257.986103	17.228144	75.109313
257.226083	12.012912	75.114318
256.317204	20.003099	75.119322
255.800720	12.475091	75.124327
255.370029	8.292304	75.129332
254.344507	18.961391	75.134337
253.626269	8.496157	75.139342
252.877230	17.544226	75.144346
252.523339	13.057461	75.149351
252.127174	10.897123	75.154356
251.028482	15.188091	75.159361
250.358841	5.189774	75.164366
249.286395	19.114849	75.169370
249.593388	4.610059	75.174375
248.791176	14.015108	75.179380
248.031535	15.711572	75.184385
246.969004	8.470884	75.189390
246.487222	15.079394	75.194394
246.486853	3.334371	75.199399
245.082704	8.818893	75.204404
244.219823	10.195925	75.209409
244.095689	8.212998	75.214414
243.594230	7.616429	75.219418
242.696990	5.517045	75.224423
241.829191	9.430589	75.229428
241.180964	12.730393	75.234433
240.773925	9.814857	75.239438
239.955045	11.224300	75.244442
239.172152	9.959816	75.249447
238.487807	19.860166	75.254452
237.534893	12.056383	75.259457
237.583340	4.115056	75.264462
236.883287	13.139547	75.269466
236.324526	14.233138	75.274471
235.507019	17.306042	75.279476
234.915153	14.255967	75.284481
233.847577	17.283579	75.289486
233.150974	13.704578	75.294490
232.495992	16.191758	75.299495
232.282480	12.633518	75.304500
231.451564	17.545702	75.309505
230.784382	16.311659	75.314510
229.800736	23.061680	75.319514
229.602568	20.948628	75.324519
228.883483	16.904858	75.329524
228.079744	12.762621	75.334529
227.488532	14.941595	75.339534
226.800718	19.078765	75.344538
226.463903	9.806408	75.349543
225.464279	16.126891	75.354548
224.412859	26.882123	75.359553
223.976378	25.452033	75.364558
223.387704	21.344896	75.369562
222.883470	20.133765	75.374567
221.880811	16.281859	75.379572
221.446098	20.826536	75.384577
220.946195	11.829335	75.389582
220.345807	23.022017	75.394586
219.480463	19.730114	75.399591
218.558725	21.668470	75.404596
218.129014	21.118815	75.409601
217.882299	17.299364	75.414606
216.674308	13.593735	75.419610
215.997568	12.143603	75.424615
215.519167	16.263160	75.429620
214.847704	16.699790	75.434625
214.753956	6.978683	75.439630
213.368458	10.619955	75.444634
212.948989	21.728601	75.449639
212.549866	16.821701	75.454644
211.435973	19.949747	75.459649
210.674427	16.212372	75.464654
209.905211	22.868291	75.469658
209.652973	15.099474	75.474663
209.592749	16.298095	75.479668
208.216480	12.206139	75.484673
207.627610	8.501163	75.489678
207.243830	13.692151	75.494682
206.345120	12.953918	75.499687
205.276217	18.334555	75.504692
204.539180	23.178166	75.509697
204.354707	9.008767	75.514702
203.861005	12.927339	75.519706
203.079392	5.105729	75.524711
202.342054	6.721379	75.529716
201.435632	12.779430	75.534721
201.548637	2.030315	75.539726
200.267495	11.891769	75.544730
199.762481	8.290120	75.549735
199.107277	8.891318	75.554740
198.353612	4.425723	75.559745
197.551352	10.659556	75.564750
196.739104	15.992971	75.569754
196.461367	6.173467	75.574759
195.706903	11.579669	75.579764
195.325511	4.566307	75.584769
194.354862	4.353631	75.589774
193.608688	10.791411	75.594778
193.018794	9.967679	75.599783
192.675196	11.104246	75.604788
191.460874	11.163807	75.609793
190.606288	6.662265	75.614798
190.254295	13.123934	75.619802
189.997822	16.763415	75.624807
189.683910	8.717434	75.629812
188.116587	21.710605	75.634817
187.657286	9.379589	75.639822
187.102900	17.726437	75.644826
186.629791	4.112418	75.649831
185.993401	13.320733	75.654836
185.127143	9.283097	75.659841
184.612938	11.057143	75.664846
184.204780	19.968879	75.669850
183.292598	2.857815	75.674855
182.330867	2.837686	75.679860
181.760019	18.885799	75.684865
181.337127	5.714780	75.689870
180.565544	8.807184	75.694874
179.528741	20.151448	75.699879
179.280411	16.420570	75.704884
178.833313	14.025515	75.709889
178.172232	15.048700	75.714894
177.036451	20.922557	75.719898
176.675460	16.394360	75.724903
176.095147	7.335880	75.729908
174.794045	20.660348	75.734913
174.556446	14.254838	75.739918
173.612877	17.656940	75.744922
173.272488	11.539055	75.749927
173.264560	13.721237	75.754932
171.865074	15.761010	75.759937
171.135140	15.052651	75.764942
170.764489	16.546770	75.769946
170.177575	11.360741	75.774951
169.080941	17.244127	75.779956
168.226989	9.530256	75.784961
168.144047	6.930490	75.789966
167.571775	21.524891	75.794970
166.651499	19.317244	75.799975
165.797534	14.113870	75.804980
165.106249	27.686470	75.809985
164.768330	5.521206	75.814990
164.268760	12.381719	75.819994
163.226678	10.939390	75.824999
162.507232	5.515877	75.830004
161.844806	11.164455	75.835009
161.725218	11.046333	75.840014
160.916945	16.850630	75.845018
159.857080	7.849692	75.850023
159.435873	3.334258	75.855028
159.004043	13.683208	75.860033
158.037905	8.267490	75.865038
157.144001	10.614587	75.870042
156.731686	6.209698	75.875047
156.397897	8.661453	75.880052
155.189781	17.085729	75.885057
154.428142	13.972860	75.890062
153.763870	17.544901	75.895066
153.446751	8.319885	75.900071
152.822053	4.984912	75.905076
152.515942	14.858081	75.910081
151.620630	7.057774	75.915086
150.505832	14.785932	75.920090
150.264190	7.171559	75.925095
149.639957	8.087951	75.930100
148.610033	14.302904	75.935105
148.425008	12.195651	75.940110
147.416389	18.216399	75.945114
146.789592	9.469690	75.950119
145.865436	18.291816	75.955124
144.986950	23.304650	75.960129
145.000446	11.532192	75.965134
144.289570	11.773276	75.970138
144.120420	20.161208	75.975143
142.934473	7.498218	75.980148
142.209874	13.746491	75.985153
141.962965	10.434860	75.990158
141.159659	13.827223	75.995162
140.074419	13.905652	76.000167
139.918241	11.281294	76.005172
138.903708	14.024521	76.010177
138.363929	5.475253	76.015182
137.426327	21.189190	76.020186
137.266225	4.779818	76.025191
136.534763	2.971008	76.030196
134.976792	11.361188	76.035201
134.581955	8.948349	76.040206
133.886575	14.163799	76.045210
133.836880	11.793696	76.050215
133.099035	14.751427	76.055220
132.409495	18.530928	76.060225
131.543685	4.470191	76.065230
131.011587	18.864223	76.070234
130.738647	14.321996	76.075239
130.051981	14.999191	76.080244
129.024943	20.767419	76.085249
128.478475	11.314051	76.090254
127.661329	16.063220	76.095258
126.656376	21.698618	76.100263
126.090091	15.149985	76.105268
125.543097	17.612088	76.110273
125.297117	9.239900	76.115278
124.504170	16.820554	76.120282
123.557620	10.469755	76.125287
123.117040	5.881723	76.130292
122.567731	16.802917	76.135297
121.898558	15.704841	76.140302
121.002829	15.013472	76.145306
120.255766	-1.254985	76.150311
120.180205	5.973155	76.155316
119.194503	7.191619	76.160321
118.543569	0.683301	76.165326
117.796351	5.635783	76.170330
117.159183	11.579962	76.175335
116.663406	-3.072771	76.180340
115.464949	-1.345721	76.185345
114.953173	8.251159	76.190350
114.385819	7.097426	76.195354
113.780537	2.985090	76.200359
113.301969	0.506761	76.205364
112.310971	14.759502	76.210369
112.021662	4.246432	76.215374
111.106595	15.689571	76.220378
110.614353	10.512118	76.225383
109.620514	9.368047	76.230388
108.718313	14.906639	76.235393
108.786334	3.144421	76.240398
108.284593	11.139108	76.245402
107.334875	8.529330	76.250407
106.407855	3.602560	76.255412
105.544759	6.651231	76.260417
105.400332	12.180950	76.265422
104.870014	9.233060	76.270426
103.604837	17.258028	76.275431
103.098907	14.364595	76.280436
102.483068	20.160301	76.285441
102.203466	8.537090	76.290446
100.809246	14.816461	76.295450
100.395714	18.685996	76.300455
99.931414	4.526556	76.305460
99.445944	24.913425	76.310465
99.209980	11.304190	76.315470
98.152754	13.844508	76.320474
97.179306	16.470815	76.325479
96.900817	11.809631	76.330484
95.942515	19.862938	76.335489
95.478374	7.952192	76.340494
94.775638	9.822551	76.345498
94.126318	10.914844	76.350503
93.173263	15.980584	76.355508
92.214188	22.778770	76.360513
92.140391	10.092997	76.365518
91.363990	18.793806	76.370522
91.011590	10.232015	76.375527
90.323045	11.597067	76.380532
89.227575	17.934458	76.385537
89.158528	6.687681	76.390542
87.865287	11.836056	76.395546
87.173214	11.173724	76.400551
86.587632	10.689951	76.405556
86.230331	18.204296	76.410561
85.582200	6.460090	76.415566
84.342153	8.740987	76.420570
83.777956	11.633192	76.425575
83.728394	10.322776	76.430580
82.996368	11.045064	76.435585
82.407312	3.523955	76.440590
81.503264	8.438379	76.445594
80.832052	2.111502	76.450599
80.192609	3.135991	76.455604
78.810027	14.320959	76.460609
78.756069	7.345292	76.465614
78.018198	10.799777	76.470618
77.525476	11.466557	76.475623
77.321213	0.436891	76.480628
75.943545	10.386329	76.485633
75.586753	6.075104	76.490638
75.260570	18.264851	76.495642
74.205342	3.269264	76.500647
73.624313	10.768824	76.505652
72.554753	11.343095	76.510657
72.351402	10.038282	76.515662
71.803970	2.398576	76.520666
70.685826	5.101582	76.525671
70.243032	5.366166	76.530676
69.471870	11.251299	76.535681
69.161480	8.164266	76.540686
68.042476	7.271984	76.545690
67.282871	7.993944	76.550695
66.802869	4.241685	76.555700
66.023193	4.564726	76.560705
65.954710	2.345858	76.565710
65.102199	-0.386635	76.570714
64.009508	0.818951	76.575719
63.802624	1.189415	76.580724
62.906344	5.620061	76.585729
62.596154	1.020712	76.590734
61.577172	11.390767	76.595738
60.914621	8.117050	76.600743
60.509759	5.199626	76.605748
58.988553	9.763055	76.610753
58.703885	4.724400	76.615758
58.207212	2.856093	76.620762
57.523657	-0.617697	76.625767
57.466122	2.770867	76.630772
56.535116	11.803839	76.635777
55.620933	5.219255	76.640782
55.058658	2.915136	76.645786
54.594197	5.269472	76.650791
53.658469	5.461287	76.655796
52.375225	7.075735	76.660801
52.217349	13.342453	76.665806
51.895806	0.096970	76.670810
51.465193	12.817451	76.675815
50.772670	6.957602	76.680820
49.710129	10.733532	76.685825
49.625152	5.166293	76.690830
48.322923	18.345908	76.695834
47.499198	16.543955	76.700839
47.084991	5.659737	76.705844
46.367607	12.851469	76.710849
45.972313	1.666196	76.715854
45.087059	-1.799075	76.720858
44.002871	12.654622	76.725863
44.016118	3.719141	76.730868
43.238681	9.477548	76.735873
42.456184	-10.369597	76.740878
41.590151	3.915260	76.745882
40.846937	0.983996	76.750887
40.690058	-2.867098	76.755892
40.170736	18.591171	76.760897
38.902716	14.589284	76.765902
38.482588	13.949825	76.770906
37.976165	14.642453	76.775911
37.775820	6.398622	76.780916
36.310141	11.033632	76.785921
35.660971	3.700320	76.790926
35.465331	5.587587	76.795930
34.462206	5.799621	76.800935
33.684399	2.344024	76.805940
32.800452	8.113114	76.810945
32.363927	2.765949	76.815950
32.147427	7.920811	76.820954
31.575747	8.923466	76.825959
30.591684	8.645187	76.830964
30.037800	12.275342	76.835969
29.570408	6.876330	76.840974
28.466414	4.694889	76.845978
27.609862	14.610122	76.850983
27.259985	14.807855	76.855988
26.290149	9.044283	76.860993
26.414095	6.156063	76.865998
25.828510	2.384384	76.871002
24.694252	11.596438	76.876007
24.291639	2.973291	76.881012
23.130070	20.309376	76.886017
22.493503	7.535183	76.891022
21.505191	8.866065	76.896026
21.268504	23.681341	76.901031
20.970726	6.587485	76.906036
20.605457	9.181470	76.911041
19.588112	7.692682	76.916046
18.516774	20.242554	76.921050
18.092093	11.809002	76.926055
17.390105	11.928858	76.931060
16.239765	12.340998	76.936065
16.039330	-1.877840	76.941070
15.678502	8.797256	76.946074
14.794775	9.483836	76.951079
13.900297	1.820655	76.956084
13.007377	11.524072	76.961089
12.689054	5.869477	76.966094
12.412317	16.077007	76.971098
11.789927	11.475421	76.976103
10.852786	9.333606	76.981108
9.936889	4.589606	76.986113
9.604715	7.610395	76.991118
8.448131	8.958659	76.996122
7.701415	4.219214	77.001127
7.425901	3.963545	77.006132
6.996778	9.708982	77.011137
6.906031	6.765120	77.016142
5.869339	8.871695	77.021147
5.103885	9.130986	77.026151
4.379817	13.234566	77.031156
3.048440	13.325508	77.036161