Fri Mar 05 20:10:33 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.290222	94.495204	0.000000
0.126317	84.280676	0.005005
-1.067865	63.220283	0.010010
-2.425051	14.449135	0.015014
-6.554220	-6.537190	0.020019
-11.867708	-9.125687	0.025024
-16.719991	-15.496697	0.030029
-21.527221	-8.570285	0.035034
-25.525414	-12.798859	0.040038
-29.587510	-9.928909	0.045043
-33.316657	-16.250405	0.050048
-36.242391	-6.933877	0.055053
-39.862115	-1.426885	0.060058
-43.674046	-14.880252	0.065062
-47.945463	-4.341359	0.070067
-51.775916	-10.312355	0.075072
-55.274934	-15.893103	0.080077
-59.085781	-11.847374	0.085082
-62.897977	-4.362128	0.090086
-66.670773	2.692645	0.095091
-70.195519	-13.791636	0.100096
-73.762989	-9.724791	0.105101
-78.032336	-14.402016	0.110106
-81.547643	-17.646262	0.115110
-85.174359	-16.913048	0.120115
-88.934189	-15.004274	0.125120
-92.405506	-15.524275	0.130125
-96.665254	-1.831718	0.135130
-100.634156	-22.397138	0.140134
-104.491162	-12.911441	0.145139
-108.075282	-17.917141	0.150144
-111.973685	-16.771532	0.155149
-115.986319	-2.380372	0.160154
-119.376606	-2.755572	0.165158
-123.157069	-9.961282	0.170163
-127.148727	-7.149719	0.175168
-130.843125	-2.895382	0.180173
-134.298311	-0.350761	0.185178
-137.682230	-17.048208	0.190182
-141.647165	-8.530814	0.195187
-145.406344	-11.337086	0.200192
-149.531352	-6.034729	0.205197
-153.452736	1.015499	0.210202
-156.711209	-11.830571	0.215206
-160.536998	-6.574370	0.220211
-164.384125	-9.421770	0.225216
-168.382744	-7.714459	0.230221
-172.221059	-0.191764	0.235226
-175.725472	-7.543945	0.240230
-179.741816	-4.296277	0.245235
-183.009515	-2.180474	0.250240
-186.817717	-10.118080	0.255245
-190.599845	0.420232	0.260250
-194.269672	-10.191848	0.265254
-198.587158	-4.929653	0.270259
-202.436002	-4.728507	0.275264
-205.654428	-12.459016	0.280269
-209.631671	1.797332	0.285274
-212.827768	-14.901592	0.290278
-216.790707	5.067286	0.295283
-220.712477	0.962459	0.300288
-224.883649	-1.401043	0.305293
-228.976916	5.061735	0.310298
-232.654087	-6.331271	0.315302
-236.190930	-1.466422	0.320307
-239.454020	-7.907711	0.325312
-243.049437	1.139059	0.330317
-247.135841	-5.631266	0.335322
-251.008147	-9.542088	0.340326
-254.660879	5.673344	0.345331
-258.862442	-8.029694	0.350336
-262.205857	-2.566490	0.355341
-265.792352	-3.640281	0.360346
-269.753776	1.681895	0.365350
-273.655346	1.320722	0.370355
-277.599889	-11.199607	0.375360
-280.776315	0.117340	0.380365
-285.005490	3.700351	0.385370
-288.600968	-13.552860	0.390374
-292.259526	-2.685628	0.395379
-296.046593	-7.133524	0.400384
-299.589155	-7.006349	0.405389
-303.601725	-1.310107	0.410394
-307.270425	-0.254472	0.415398
-311.471702	-0.782198	0.420403
-314.995136	-1.970060	0.425408
-318.587440	-5.581703	0.430413
-322.547710	1.626381	0.435418
-325.825242	-10.409004	0.440422
-330.044798	-0.775195	0.445427
-334.260410	-3.055716	0.450432
-337.443254	-5.748699	0.455437
-341.373936	-6.879385	0.460442
-344.864803	-4.590541	0.465446
-348.914817	0.955636	0.470451
-352.490538	3.111386	0.475456
-356.322865	2.297751	0.480461
-360.101032	0.675972	0.485466
-363.941053	-7.798722	0.490470
-367.591052	-4.271779	0.495475
-371.274083	-2.136715	0.500480
-375.097780	-10.279686	0.505485
-379.057186	5.568346	0.510490
-382.666801	0.133480	0.515494
-386.580221	-5.445253	0.520499
-390.016490	-4.224759	0.525504
-393.645999	-12.220513	0.530509
-397.943237	2.963988	0.535514
-401.429575	-3.015650	0.540518
-405.186460	1.930309	0.545523
-409.322415	-4.401314	0.550528
-412.883990	-3.991819	0.555533
-416.537460	-1.738406	0.560538
-420.121709	-4.745638	0.565542
-424.162513	2.645776	0.570547
-427.988197	-8.742110	0.575552
-431.505641	-3.213041	0.580557
-435.479410	7.506046	0.585562
-438.681069	-4.700561	0.590566
-442.509852	-2.152611	0.595571
-446.562976	-11.881479	0.600576
-450.341195	-3.341382	0.605581
-454.318719	-6.937023	0.610586
-457.929604	-6.073315	0.615590
-462.120138	-15.565745	0.620595
-465.643051	-10.180834	0.625600
-469.011496	-12.832954	0.630605
-473.344141	-2.860731	0.635610
-476.430446	-6.776869	0.640614
-480.304064	-14.403916	0.645619
-484.440880	-2.327793	0.650624
-487.859464	-8.053195	0.655629
-491.977713	-1.655383	0.660634
-495.592607	-11.547198	0.665638
-499.002135	-1.097912	0.670643
-502.920077	4.225576	0.675648
-506.482003	-13.059432	0.680653
-510.625605	-2.943879	0.685658
-514.324897	-16.701419	0.690662
-518.474345	3.876414	0.695667
-522.151913	-5.647388	0.700672
-525.441704	-9.926764	0.705677
-529.191378	-6.828351	0.710682
-533.019952	-16.528275	0.715686
-537.249811	-6.944519	0.720691
-541.197808	-4.642293	0.725696
-544.608745	1.156924	0.730701
-548.159184	2.548844	0.735706
-551.694872	-5.994647	0.740710
-555.367855	-2.641944	0.745715
-559.502226	-6.614465	0.750720
-563.195655	-3.840370	0.755725
-567.321620	3.132802	0.760730
-570.953630	-8.317315	0.765734
-574.565552	-0.989446	0.770739
-578.343221	-8.524426	0.775744
-581.798951	-9.421513	0.780749
-585.876915	-12.961458	0.785754
-589.651429	-2.702896	0.790758
-593.204069	-4.697794	0.795763
-597.168217	-12.143024	0.800768
-600.888147	-12.966334	0.805773
-604.490369	-10.493749	0.810778
-608.061704	-4.392858	0.815782
-612.331272	-4.522794	0.820787
-616.049108	-1.730526	0.825792
-619.673203	-3.488467	0.830797
-623.376826	-3.522731	0.835802
-626.869005	-6.227393	0.840806
-630.829199	-9.521153	0.845811
-634.891630	-4.839833	0.850816
-638.266876	-8.939816	0.855821
-642.598689	-11.322638	0.860826
-646.137681	-1.153664	0.865830
-649.876787	-0.217139	0.870835
-653.504006	-5.614070	0.875840
-656.619762	-9.910029	0.880845
-661.111405	2.823890	0.885850
-664.676073	-6.172100	0.890854
-668.542421	-2.830904	0.895859
-672.555352	-12.532669	0.900864
-675.887163	-16.000881	0.905869
-679.967528	-11.420699	0.910874
-683.365489	-5.058828	0.915878
-687.311658	-8.603888	0.920883
-691.468261	6.648508	0.925888
-695.037051	-14.440201	0.930893
-698.801113	0.717930	0.935898
-702.335454	-13.444113	0.940902
-706.241837	2.025352	0.945907
-710.118015	7.438689	0.950912
-713.476037	-3.859443	0.955917
-717.345168	5.906665	0.960922
-720.873222	-7.207703	0.965926
-725.204034	-5.692378	0.970931
-728.858832	-0.402703	0.975936
-732.568528	-12.229631	0.980941
-736.440834	-1.688722	0.985946
-739.769904	2.984371	0.990950
-744.064066	-1.074243	0.995955
-747.690427	-2.541469	1.000960
-751.535116	-13.559903	1.005965
-755.452635	3.882568	1.010970
-758.919334	2.266839	1.015974
-762.643418	0.078832	1.020979
-766.260408	-2.548901	1.025984
-769.810682	-5.684023	1.030989
-773.978185	-4.194712	1.035994
-777.500815	1.315179	1.040998
-781.507860	-9.721408	1.046003
-785.402187	3.346174	1.051008
-788.862869	-4.940853	1.056013
-792.691598	-0.320280	1.061018
-796.231898	-3.996263	1.066022
-800.189210	-3.794159	1.071027
-803.981784	-5.693611	1.076032
-807.468550	-7.982558	1.081037
-811.569051	1.569948	1.086042
-815.455079	-2.684661	1.091046
-818.884691	-2.956383	1.096051
-822.704944	2.415075	1.101056
-826.333079	-2.804819	1.106061
-830.591650	-1.332389	1.111066
-834.041831	-2.878107	1.116070
-837.959071	-12.668986	1.121075
-841.728296	1.925639	1.126080
-845.173567	-11.502948	1.131085
-849.181589	-0.725707	1.136090
-852.897310	0.612668	1.141094
-856.886220	-2.518424	1.146099
-860.461478	-3.172068	1.151104
-863.947345	-9.397067	1.156109
-868.245523	-4.764396	1.161114
-871.819397	-0.917713	1.166118
-875.595543	-3.704328	1.171123
-879.088850	0.742907	1.176128
-882.529630	-3.283162	1.181133
-886.657523	-2.441793	1.186138
-890.615526	0.576954	1.191142
-894.399993	-2.222492	1.196147
-898.282702	6.975221	1.201152
-901.099092	-8.852984	1.206157
-905.393548	-3.082306	1.211162
-909.282388	0.002682	1.216166
-913.090571	-11.289384	1.221171
-916.808450	1.013759	1.226176
-920.562513	-7.536801	1.231181
-924.631161	-6.534532	1.236186
-928.151433	-5.687753	1.241190
-931.630259	-12.451501	1.246195
-935.429116	-14.849615	1.251200
-939.069264	-11.711311	1.256205
-943.153943	-3.875234	1.261210
-947.114442	-7.884323	1.266214
-950.738282	-8.161061	1.271219
-954.742789	-11.172793	1.276224
-958.120784	-5.748851	1.281229
-962.133846	5.775262	1.286234
-965.770754	-8.297407	1.291238
-969.745514	-3.087087	1.296243
-973.643832	-9.580259	1.301248
-976.870137	-11.926373	1.306253
-980.767656	-4.627933	1.311258
-984.238569	5.688319	1.316262
-988.154636	-5.029713	1.321267
-992.203672	2.521634	1.326272
-995.884512	-13.368447	1.331277
-999.814126	-4.240350	1.336282
-1003.202271	-3.638514	1.341286
-1007.420126	-3.616734	1.346291
-1011.168658	-1.842364	1.351296
-1014.613755	-3.722933	1.356301
-1018.594712	3.398109	1.361306
-1021.855125	-16.438388	1.366310
-1025.515733	-18.907350	1.371315
-1029.906961	-0.739020	1.376320
-1033.412465	-1.988593	1.381325
-1037.426191	1.898731	1.386330
-1040.832194	1.741827	1.391334
-1044.394101	-8.912905	1.396339
-1048.555162	-12.225853	1.401344
-1052.161417	-10.346447	1.406349
-1056.127970	6.052511	1.411354
-1060.055558	-5.852545	1.416358
-1063.434233	-6.177787	1.421363
-1067.227962	-15.291014	1.426368
-1070.659403	-5.020387	1.431373
-1074.957434	-5.977540	1.436378
-1078.799404	-8.671290	1.441382
-1082.197246	-14.629335	1.446387
-1086.509460	-16.717999	1.451392
-1089.420923	-12.898119	1.456397
-1093.329934	-17.186418	1.461402
-1097.632842	-3.485314	1.466406
-1101.285248	-4.086823	1.471411
-1105.043031	-6.098577	1.476416
-1108.485987	-9.816454	1.481421
-1112.513696	-4.365622	1.486426
-1116.399641	-13.211705	1.491430
-1119.617251	-15.928006	1.496435
-1123.648352	1.304526	1.501440
-1127.299819	-6.912021	1.506445
-1131.427185	-3.435279	1.511450
-1134.967018	-19.259362	1.516454
-1138.721863	-10.780315	1.521459
-1142.547812	-10.403112	1.526464
-1145.967993	-10.455094	1.531469
-1150.286824	6.867676	1.536474
-1153.624862	-2.554859	1.541478
-1157.409606	-6.544396	1.546483
-1161.397592	3.337605	1.551488
-1164.967613	-16.755041	1.556493
-1168.983319	-4.799686	1.561498
-1172.778860	-6.384251	1.566502
-1176.499733	-7.398876	1.571507
-1180.035604	-1.679709	1.576512
-1183.262574	-10.959120	1.581517
-1187.614211	-3.043648	1.586522
-1191.480755	-17.044481	1.591526
-1195.159314	-6.882372	1.596531
-1199.240806	-10.977312	1.601536
-1202.981036	-8.335085	1.606541
-1206.526837	-8.420491	1.611546
-1210.051994	-22.546876	1.616550
-1213.868427	-12.578717	1.621555
-1217.874406	-6.915149	1.626560
-1221.324244	-0.443309	1.631565
-1225.242632	-7.546251	1.636570
-1228.959693	-3.456930	1.641574
-1232.951056	-13.113815	1.646579
-1236.719013	-1.117576	1.651584
-1240.117666	-7.970940	1.656589
-1244.222948	-4.325653	1.661594
-1247.697399	-2.175312	1.666598
-1251.504301	-14.690669	1.671603
-1255.810092	-5.583959	1.676608
-1259.013287	-13.793182	1.681613
-1262.971251	-12.836425	1.686618
-1266.505262	3.482584	1.691622
-1269.937392	-14.865805	1.696627
-1274.245611	-2.349389	1.701632
-1277.579844	-16.231843	1.706637
-1281.828329	-9.663629	1.711642
-1286.009119	1.887844	1.716646
-1289.337279	-10.967420	1.721651
-1292.914675	-2.194847	1.726656
-1296.501502	-8.251624	1.731661
-1300.609828	-8.191652	1.736666
-1304.246478	-4.282237	1.741670
-1307.975652	-10.024481	1.746675
-1311.929118	-3.799895	1.751680
-1315.444579	-3.757529	1.756685
-1319.202064	2.192854	1.761690
-1322.986808	-4.035622	1.766694
-1326.858734	-3.587679	1.771699
-1330.636543	-2.905643	1.776704
-1334.024072	-0.829012	1.781709
-1338.183131	-0.076471	1.786714
-1342.149901	-6.394042	1.791718
-1345.639791	-10.901960	1.796723
-1349.360001	-11.298261	1.801728
-1352.968014	-8.415196	1.806733
-1357.036143	-1.859950	1.811738
-1360.775595	-5.504745	1.816742
-1364.408230	-14.797783	1.821747
-1368.094538	-13.305611	1.826752
-1371.631299	-11.521993	1.831757
-1375.750528	-2.197364	1.836762
-1379.076504	-18.411650	1.841766
-1382.870315	-9.388265	1.846771
-1387.186617	-9.250687	1.851776
-1390.572175	-11.507640	1.856781
-1394.713519	-5.513029	1.861786
-1398.546039	-12.678292	1.866790
-1402.247733	-15.603682	1.871795
-1405.907911	-10.588085	1.876800
-1409.412605	-13.130279	1.881805
-1413.371975	-6.535585	1.886810
-1417.168549	-11.252899	1.891814
-1420.529046	-13.701472	1.896819
-1424.888309	-11.081195	1.901824
-1428.181801	-7.526151	1.906829
-1432.195694	-11.232534	1.911834
-1436.027219	-9.641309	1.916838
-1439.235364	-16.788210	1.921843
-1443.523315	-9.156861	1.926848
-1446.955621	-12.585772	1.931853
-1451.278970	-5.737195	1.936858
-1454.792865	-2.159434	1.941862
-1458.631882	-8.875711	1.946867
-1462.409419	-2.598627	1.951872
-1465.462037	-8.079951	1.956877
-1469.539226	-2.981706	1.961882
-1473.302323	-5.905032	1.966886
-1477.049134	-4.104962	1.971891
-1481.427070	-4.310564	1.976896
-1484.916012	-5.596791	1.981901
-1488.615944	-4.885969	1.986906
-1492.311216	2.324135	1.991910
-1495.749946	-7.606850	1.996915
-1500.159472	3.886894	2.006912
-1500.892469	-2.012983	2.016909
-1498.527970	-1.076390	2.026906
-1495.777007	-2.827446	2.036902
-1493.227040	-3.545269	2.046899
-1491.681302	-3.072800	2.056896
-1489.669632	1.103429	2.066893
-1487.891062	1.249670	2.076890
-1485.603153	-8.206599	2.086886
-1483.760125	-1.991803	2.096883
-1481.982981	-1.996908	2.106880
-1480.224621	-2.767940	2.116877
-1478.445247	-2.416561	2.126874
-1476.377740	-8.134936	2.136870
-1474.319156	-6.378811	2.146867
-1472.541176	-9.886105	2.156864
-1470.774982	-5.253713	2.166861
-1468.820350	-5.609331	2.176858
-1466.929445	-9.363650	2.186854
-1464.951357	-3.704145	2.196851
-1462.900192	-6.276244	2.206848
-1461.165639	-2.279821	2.216845
-1459.769047	-3.289745	2.226842
-1457.485670	-6.322178	2.236838
-1455.305244	-5.758691	2.246835
-1453.402897	-9.465885	2.256832
-1452.057657	-3.280295	2.266829
-1449.876382	-1.420637	2.276826
-1448.105736	-7.926705	2.286822
-1446.225835	-5.513528	2.296819
-1444.001520	-2.846029	2.306816
-1442.473597	4.805564	2.316813
-1440.652344	-0.153360	2.326810
-1438.610320	-7.789180	2.336806
-1436.595247	-8.696023	2.346803
-1434.770174	-2.236733	2.356800
-1433.148612	-13.086236	2.366797
-1431.191630	-12.453790	2.376794
-1429.067131	-9.411877	2.386790
-1427.314233	-9.319900	2.396787
-1425.431972	-5.129208	2.406784
-1423.758148	-4.705623	2.416781
-1421.426340	-10.586270	2.426778
-1419.802021	-11.934209	2.436774
-1417.761965	-6.314583	2.446771
-1415.954793	-10.135980	2.456768
-1414.499670	-6.345828	2.466765
-1412.508124	0.922081	2.476762
-1410.457545	-3.123022	2.486758
-1408.249520	-1.652866	2.496755
-1406.657119	-8.065630	2.506752
-1404.831166	-5.937460	2.516749
-1402.936700	-5.084982	2.526746
-1400.980928	-4.344948	2.536742
-1398.774494	-12.412843	2.546739
-1397.259572	-8.629098	2.556736
-1395.564249	-9.705759	2.566733
-1393.336484	-8.462958	2.576730
-1391.716183	-10.492332	2.586726
-1389.658644	-11.145409	2.596723
-1388.028748	-6.896912	2.606720
-1386.059087	-9.763786	2.616717
-1383.872910	-8.708526	2.626714
-1382.301110	-12.729053	2.636710
-1380.243647	-11.812653	2.646707
-1378.485242	-6.828416	2.656704
-1376.535921	-1.838426	2.666701
-1374.680615	-4.467512	2.676698
-1372.722257	-4.536281	2.686694
-1370.852022	-8.951945	2.696691
-1369.045263	-9.904325	2.706688
-1367.326310	-9.592133	2.716685
-1365.536099	-3.703512	2.726682
-1363.430531	-8.128426	2.736678
-1361.362215	-12.203167	2.746675
-1359.662793	-6.551057	2.756672
-1357.817287	-14.703238	2.766669
-1356.034101	-8.950853	2.776666
-1354.269877	-4.944885	2.786662
-1351.914456	-3.147748	2.796659
-1350.206691	-5.060045	2.806656
-1348.428168	-10.387842	2.816653
-1346.527837	-7.366805	2.826650
-1344.764093	-12.196449	2.836646
-1342.702123	-3.750816	2.846643
-1341.033911	-7.800962	2.856640
-1338.980479	-9.519115	2.866637
-1337.199686	-11.943614	2.876634
-1335.378515	-4.702044	2.886630
-1333.152357	-4.289444	2.896627
-1331.434641	-8.683820	2.906624
-1329.806707	-5.199167	2.916621
-1327.397112	-2.992260	2.926618
-1325.842462	-8.039470	2.936614
-1324.207686	-12.370039	2.946611
-1322.145040	-6.878674	2.956608
-1320.657074	-6.024213	2.966605
-1318.187291	-5.614281	2.976602
-1316.544709	-4.528781	2.986598
-1314.429363	-13.980955	2.996595
-1312.610162	-15.464224	3.006592
-1311.102921	-9.456054	3.016589
-1308.999853	-9.934771	3.026586
-1307.295996	-11.150102	3.036582
-1305.125221	-9.105468	3.046579
-1303.215208	-8.771706	3.056576
-1301.514894	-4.499678	3.066573
-1299.644313	-5.395905	3.076570
-1297.608319	-2.871799	3.086566
-1296.011571	-6.425744	3.096563
-1293.858552	-8.935054	3.106560
-1292.165573	-12.897553	3.116557
-1290.242901	-9.464785	3.126554
-1288.264590	-10.907188	3.136550
-1286.437077	-10.978624	3.146547
-1284.591376	-10.476660	3.156544
-1282.884248	-12.483541	3.166541
-1280.772622	-14.225168	3.176538
-1278.791563	-12.278037	3.186534
-1277.271042	-14.783988	3.196531
-1275.077103	-12.855138	3.206528
-1273.288431	-14.856117	3.216525
-1271.532429	-13.733476	3.226522
-1269.824775	-8.941552	3.236518
-1267.695671	-14.846450	3.246515
-1265.665189	-9.297779	3.256512
-1263.838648	-12.285329	3.266509
-1262.328304	-10.093899	3.276506
-1260.071853	-13.312883	3.286502
-1258.238084	-13.693190	3.296499
-1256.322796	-12.946553	3.306496
-1254.620124	-8.845392	3.316493
-1252.609129	-5.211991	3.326490
-1250.768141	-9.037100	3.336486
-1248.859094	-12.101000	3.346483
-1247.051827	-7.508156	3.356480
-1245.434388	-13.345357	3.366477
-1243.280541	-4.806963	3.376474
-1241.330696	-10.872623	3.386470
-1239.329191	-8.423471	3.396467
-1237.915375	-13.471770	3.406464
-1235.884097	-3.514817	3.416461
-1233.586020	-7.998849	3.426458
-1232.063695	-2.640396	3.436454
-1230.493534	-6.197938	3.446451
-1228.117290	-12.895506	3.456448
-1226.385683	-9.291580	3.466445
-1224.449751	3.672725	3.476442
-1222.398272	-12.983303	3.486438
-1220.645365	-8.542789	3.496435
-1219.219048	-8.998384	3.506432
-1217.180932	-5.279292	3.516429
-1215.189361	-6.750599	3.526426
-1213.173911	2.081555	3.536422
-1211.227498	-4.191954	3.546419
-1209.305325	-1.799552	3.556416
-1207.901234	-1.381590	3.566413
-1205.835118	-10.480014	3.576410
-1204.108967	-6.703094	3.586406
-1201.663779	-10.787482	3.596403
-1200.190600	-8.596378	3.606400
-1198.085281	0.088777	3.616397
-1196.572632	-6.129518	3.626394
-1194.750786	-13.936748	3.636390
-1192.373539	-10.137694	3.646387
-1190.701583	-5.854726	3.656384
-1188.912574	-10.225675	3.666381
-1187.172155	-0.826861	3.676378
-1185.138170	-9.621709	3.686374
-1182.883209	-7.276221	3.696371
-1181.271240	-7.251504	3.706368
-1179.785290	-6.938203	3.716365
-1177.600011	0.898922	3.726362
-1175.523528	-9.715335	3.736358
-1173.740188	-10.060664	3.746355
-1171.980277	-4.208085	3.756352
-1170.365071	-7.655955	3.766349
-1168.540811	-2.659977	3.776346
-1166.277681	-4.908899	3.786342
-1164.403268	-7.354566	3.796339
-1162.658222	-9.343745	3.806336
-1160.374255	-8.776019	3.816333
-1159.032080	-5.411303	3.826330
-1157.127127	-17.292821	3.836326
-1154.978483	-7.146152	3.846323
-1153.009719	1.747214	3.856320
-1151.472879	-12.191178	3.866317
-1149.521827	-6.943896	3.876314
-1147.429044	-4.881895	3.886310
-1145.402326	-6.594027	3.896307
-1143.909553	-7.423364	3.906304
-1142.486044	-8.429511	3.916301
-1139.887865	-5.317849	3.926298
-1138.130849	-12.705723	3.936294
-1136.458244	-13.211725	3.946291
-1134.338515	-7.631421	3.956288
-1132.532403	-6.142482	3.966285
-1130.603076	-9.111641	3.976282
-1129.073943	-7.295754	3.986278
-1126.916955	-11.515535	3.996275
-1124.943059	-12.181838	4.006272
-1123.262344	-11.260193	4.016269
-1121.359626	-9.161443	4.026266
-1119.561965	-14.155826	4.036262
-1117.639075	-8.296121	4.046259
-1115.636818	-6.467500	4.056256
-1113.751322	-3.783361	4.066253
-1112.125781	-5.870225	4.076250
-1110.039615	-9.969714	4.086246
-1108.058621	-9.986618	4.096243
-1106.073504	-7.642092	4.106240
-1104.551858	-3.819743	4.116237
-1102.509022	-2.008654	4.126234
-1100.748181	-4.625574	4.136230
-1098.749949	-12.195696	4.146227
-1096.816143	-11.388731	4.156224
-1095.099688	-7.791751	4.166221
-1093.316259	-13.898567	4.176218
-1091.544314	-7.462063	4.186214
-1089.317331	-11.576167	4.196211
-1087.187771	-13.582594	4.206208
-1085.662187	-6.820885	4.216205
-1083.875467	-6.705637	4.226202
-1081.826805	-7.102814	4.236198
-1080.077360	-15.261536	4.246195
-1078.262556	-7.425047	4.256192
-1076.284375	-1.206255	4.266189
-1074.058225	-8.547558	4.276186
-1072.442490	-7.242852	4.286182
-1070.620324	-7.947994	4.296179
-1068.913344	-10.256277	4.306176
-1067.069214	-0.120797	4.316173
-1065.057103	-4.674189	4.326170
-1063.104676	-4.389644	4.336166
-1061.127624	-3.442726	4.346163
-1059.496844	-5.108817	4.356160
-1057.505460	-2.547357	4.366157
-1055.510580	-5.234840	4.376154
-1053.683619	-5.497056	4.386150
-1051.912994	0.107597	4.396147
-1049.963525	-4.607867	4.406144
-1048.274361	-0.303856	4.416141
-1046.158074	-3.182856	4.426138
-1044.329681	-2.965296	4.436134
-1042.426472	-2.267075	4.446131
-1040.829947	-9.180795	4.456128
-1038.854440	-4.145745	4.466125
-1036.670035	-7.207735	4.476122
-1034.754058	-1.207901	4.486118
-1033.125050	-5.796303	4.496115
-1031.142129	-3.247677	4.506112
-1029.559752	-1.972340	4.516109
-1027.581441	-3.368737	4.526106
-1025.602241	3.726251	4.536102
-1023.543332	-7.104553	4.546099
-1021.787972	-5.883722	4.556096
-1019.990952	-7.778480	4.566093
-1017.980276	-4.136920	4.576090
-1016.279449	-8.293117	4.586086
-1014.654835	-10.763448	4.596083
-1012.530072	-3.611208	4.606080
-1010.732423	3.530200	4.616077
-1008.893067	-10.868610	4.626074
-1006.660813	-6.094068	4.636070
-1005.073550	-11.762082	4.646067
-1003.028876	-7.868581	4.656064
-1001.133123	-12.076469	4.666061
-999.370294	-10.687870	4.676058
-997.578624	-13.791220	4.686054
-995.568194	-14.137997	4.696051
-993.548745	-9.741510	4.706048
-991.803662	-7.012707	4.716045
-990.194194	-9.321127	4.726042
-988.043436	-9.107713	4.736038
-986.161298	-8.263971	4.746035
-984.249740	-9.108080	4.756032
-982.662023	-7.697777	4.766029
-980.727189	-9.450337	4.776026
-978.535674	-13.209722	4.786022
-976.839095	-8.910002	4.796019
-975.174151	-0.719455	4.806016
-972.992368	1.841630	4.816013
-970.979111	-2.203452	4.826010
-969.268441	-0.737013	4.836006
-967.161979	-7.560138	4.846003
-965.521437	-2.608819	4.856000
-964.136961	-6.344916	4.865997
-961.953099	-0.526804	4.875994
-959.853694	-3.823026	4.885990
-957.744292	-3.846127	4.895987
-956.349121	-6.518147	4.905984
-954.426661	-2.388741	4.915981
-952.424472	-3.913630	4.925978
-950.521130	-9.913209	4.935974
-948.573835	-6.544082	4.945971
-946.725010	-0.877639	4.955968
-945.095030	-8.914541	4.965965
-942.976367	-5.457550	4.975962
-941.228947	-2.773291	4.985958
-939.088308	-11.697107	4.995955
-937.489595	-4.053305	5.005952
-935.732104	-9.167450	5.015949
-933.701477	1.772008	5.025946
-931.832715	-7.747799	5.035942
-929.713780	-4.369787	5.045939
-928.017186	-8.907349	5.055936
-926.410786	-9.026828	5.065933
-924.168131	-9.252784	5.075930
-922.430132	-9.052254	5.085926
-920.534462	-7.651678	5.095923
-918.556215	-10.067968	5.105920
-916.853354	-11.630225	5.115917
-914.821527	-9.403527	5.125914
-913.117707	-7.444902	5.135910
-911.295327	-6.253651	5.145907
-909.499648	2.359729	5.155904
-907.480545	-5.355691	5.165901
-905.354553	-2.259834	5.175898
-903.824711	-8.445971	5.185894
-901.503441	-3.464504	5.195891
-899.963717	-7.405389	5.205888
-898.040045	-6.277691	5.215885
-896.252407	-2.349308	5.225882
-894.097659	-5.788532	5.235878
-892.239653	-5.490325	5.245875
-890.433125	-1.882324	5.255872
-888.581145	-2.173675	5.265869
-886.955834	-3.243514	5.275866
-885.012839	-5.369932	5.285862
-883.045693	-2.389182	5.295859
-880.994991	-4.670185	5.305856
-879.212238	-1.555739	5.315853
-877.409884	-2.372828	5.325850
-875.540755	-3.857431	5.335846
-873.449119	-6.714969	5.345843
-871.624498	-5.615623	5.355840
-870.212002	-1.260925	5.365837
-867.823798	-3.647983	5.375834
-866.131132	-7.123829	5.385830
-864.288989	-3.006766	5.395827
-862.149205	-1.342015	5.405824
-860.551059	-1.182235	5.415821
-858.994716	-2.601028	5.425818
-856.559855	1.833382	5.435814
-854.763656	-3.880578	5.445811
-852.977709	-1.377672	5.455808
-851.249831	0.915047	5.465805
-849.151263	0.407463	5.475802
-847.218508	1.181648	5.485798
-845.534000	3.126044	5.495795
-843.424872	1.465728	5.505792
-841.850023	1.735034	5.515789
-839.887378	3.958651	5.525786
-837.925837	-4.353826	5.535782
-835.799179	-5.421676	5.545779
-834.338855	-12.880336	5.555776
-832.750930	-11.419437	5.565773
-830.742382	-11.123143	5.575770
-828.331654	-9.757464	5.585766
-826.355783	-15.002758	5.595763
-824.768347	-10.199160	5.605760
-823.008764	-10.019375	5.615757
-821.257089	-8.851486	5.625754
-819.135110	-9.768574	5.635750
-817.317461	-12.871209	5.645747
-815.498355	-5.884649	5.655744
-813.526336	-13.575096	5.665741
-811.663578	-10.129179	5.675738
-809.553205	-11.608084	5.685734
-807.920849	-18.161074	5.695731
-806.410931	-14.472435	5.705728
-804.469911	-14.214272	5.715725
-802.540486	-15.957928	5.725722
-800.272028	-10.320550	5.735718
-798.496486	-20.325880	5.745715
-796.860484	-16.254760	5.755712
-794.656575	-8.290753	5.765709
-792.943883	-7.547662	5.775706
-790.991636	-8.053910	5.785702
-789.161890	-11.718982	5.795699
-787.283332	-8.382938	5.805696
-785.543109	-13.648954	5.815693
-783.443992	-9.686587	5.825690
-781.542167	-10.824239	5.835686
-779.975564	-12.852511	5.845683
-777.991096	-14.061791	5.855680
-775.980330	-12.152128	5.865677
-774.293808	-3.263820	5.875674
-772.089543	-12.418722	5.885670
-770.478025	-11.206287	5.895667
-768.515655	-8.140992	5.905664
-766.671256	-12.679965	5.915661
-764.823788	-8.337884	5.925658
-762.960884	-7.724570	5.935654
-761.022153	-11.590199	5.945651
-759.080881	-10.676778	5.955648
-757.376306	-11.636041	5.965645
-755.456331	-11.483420	5.975642
-753.695849	-14.910027	5.985638
-751.600919	-16.081677	5.995635
-749.746474	-10.946493	6.005632
-748.088592	-15.784059	6.015629
-746.191187	-9.435217	6.025626
-744.002861	-14.564404	6.035622
-742.076514	-12.728061	6.045619
-740.343441	-9.918197	6.055616
-738.471835	-6.007845	6.065613
-736.639576	-1.314362	6.075610
-734.974641	-7.998833	6.085606
-732.910394	-10.056087	6.095603
-730.988616	-10.858994	6.105600
-728.955161	-9.098178	6.115597
-727.534520	-7.346787	6.125594
-725.664433	-14.346668	6.135590
-723.374042	-10.447973	6.145587
-721.603964	-13.031358	6.155584
-719.808174	-5.466255	6.165581
-717.711708	-8.133379	6.175578
-715.794093	-9.644554	6.185574
-714.135368	-15.101178	6.195571
-712.311743	-12.751027	6.205568
-710.492953	-14.075877	6.215565
-708.655671	-9.029493	6.225562
-706.389679	-9.416866	6.235558
-704.879880	-12.332852	6.245555
-702.828768	-17.072180	6.255552
-701.089400	-7.052265	6.265549
-699.123912	-5.885296	6.275546
-697.251316	-9.929779	6.285542
-695.352474	-8.305316	6.295539
-693.607717	-6.297806	6.305536
-691.581251	-6.552150	6.315533
-689.582184	-9.416842	6.325530
-687.893390	-7.163544	6.335526
-686.281667	-13.256849	6.345523
-684.166631	-6.424837	6.355520
-681.870973	-13.072697	6.365517
-680.553377	-10.248498	6.375514
-678.379603	-7.600590	6.385510
-676.355406	-4.057201	6.395507
-674.971895	-6.528252	6.405504
-673.071155	-4.829863	6.415501
-671.032998	-2.676590	6.425498
-668.958637	-6.241717	6.435494
-667.281557	-11.601773	6.445491
-665.266881	-9.323166	6.455488
-663.350387	-7.958864	6.465485
-661.857706	-11.178403	6.475482
-659.925395	-9.158208	6.485478
-657.628699	-10.590964	6.495475
-655.789679	-13.175844	6.505472
-654.086502	-12.407446	6.515469
-652.040518	-13.069085	6.525466
-650.312219	-1.196833	6.535462
-648.571981	-4.921711	6.545459
-646.888356	-8.754383	6.555456
-644.619594	-6.791093	6.565453
-642.765279	-7.720517	6.575450
-640.985247	-12.670692	6.585446
-639.160920	-12.275325	6.595443
-637.128159	-14.640096	6.605440
-635.487035	-11.543882	6.615437
-633.317517	-3.757369	6.625434
-631.487424	-0.887133	6.635430
-629.577178	-7.713366	6.645427
-627.774850	-11.797095	6.655424
-626.091303	-7.736602	6.665421
-624.043980	-9.757901	6.675418
-622.149088	-6.659592	6.685414
-620.223495	-11.977219	6.695411
-618.849646	-7.497764	6.705408
-616.414875	-9.554120	6.715405
-614.597582	-17.620746	6.725402
-612.767156	-9.944247	6.735398
-610.845619	-10.134389	6.745395
-608.966440	-6.263033	6.755392
-607.298143	-4.508504	6.765389
-605.477018	-9.594694	6.775386
-603.458709	-3.997671	6.785382
-601.456570	-11.915404	6.795379
-599.533421	-10.610534	6.805376
-598.007480	-5.402209	6.815373
-596.013494	-9.436011	6.825370
-594.204512	-5.706586	6.835366
-592.404370	-10.647308	6.845363
-590.285195	-7.761647	6.855360
-588.424906	-1.833048	6.865357
-586.329787	-5.379318	6.875354
-584.620796	-7.125479	6.885350
-582.713871	-12.790621	6.895347
-580.783315	-7.552190	6.905344
-579.005407	-7.997253	6.915341
-577.519941	-8.640332	6.925338
-575.025561	-10.191433	6.935334
-573.525997	-11.248866	6.945331
-571.312760	-15.320832	6.955328
-569.622282	-13.282453	6.965325
-568.112639	-11.093604	6.975322
-565.996279	-8.254839	6.985318
-563.988575	-11.450808	6.995315
-561.874317	-2.869081	7.005312
-560.262754	-7.582287	7.015309
-558.612480	-10.735362	7.025306
-556.617436	-10.544046	7.035302
-554.827337	-6.851046	7.045299
-552.662075	-6.536919	7.055296
-550.459387	-7.600872	7.065293
-547.759702	-3.753171	7.075290
-547.074798	-3.259396	7.085286
-546.377176	-6.062912	7.095283
-543.638465	-10.853534	7.105280
-541.256315	-8.436152	7.115277
-539.267075	-7.647052	7.125274
-538.395233	-4.104194	7.135270
-536.302993	-3.296808	7.145267
-533.985442	-5.991198	7.155264
-532.183892	-5.663163	7.165261
-530.028298	-2.415368	7.175258
-528.250824	-8.524003	7.185254
-526.591952	-4.432649	7.195251
-524.831529	-6.749088	7.205248
-522.993122	-6.788512	7.215245
-520.708719	-6.815492	7.225242
-519.004062	-11.748805	7.235238
-516.883048	-9.836000	7.245235
-515.131042	-2.887413	7.255232
-513.598944	-4.275268	7.265229
-511.794374	-5.638750	7.275226
-509.483586	-9.712035	7.285222
-507.525266	-8.030602	7.295219
-505.992604	-13.825379	7.305216
-503.708758	-7.642261	7.315213
-501.969556	-3.142142	7.325210
-500.634420	-8.149052	7.335206
-498.539187	-8.501058	7.345203
-496.259313	-8.388343	7.355200
-494.512566	-18.856249	7.365197
-492.774908	-10.602726	7.375194
-490.880984	-8.052047	7.385190
-488.856041	-9.807553	7.395187
-487.149128	-13.842784	7.405184
-485.508633	-14.297409	7.415181
-483.247728	-5.991660	7.425178
-481.512779	-15.526097	7.435174
-479.528329	-11.013029	7.445171
-477.765608	-8.476120	7.455168
-475.879766	-11.785186	7.465165
-473.809080	-11.212724	7.475162
-471.989773	-9.491691	7.485158
-470.194920	-11.238853	7.495155
-468.459345	-14.084966	7.505152
-466.610895	-8.470165	7.515149
-464.470120	-9.396256	7.525146
-462.628484	-11.809305	7.535142
-461.040839	-10.386000	7.545139
-459.039105	-8.236198	7.555136
-456.981775	-5.460536	7.565133
-455.065765	-4.855459	7.575130
-453.374264	-4.539788	7.585126
-451.506872	-5.174311	7.595123
-449.581797	-5.890677	7.605120
-447.241772	-10.802257	7.615117
-445.888003	-3.857908	7.625114
-444.205983	-9.894399	7.635110
-442.162016	-11.105009	7.645107
-439.692296	-2.103088	7.655104
-438.154034	-5.343986	7.665101
-436.928262	-4.710767	7.675098
-434.874209	-3.819824	7.685094
-432.453131	-8.198020	7.695091
-430.778159	-6.982851	7.705088
-428.877749	-9.207893	7.715085
-427.141471	-12.289353	7.725082
-425.080810	-10.112616	7.735078
-423.287046	-9.233781	7.745075
-421.225614	-8.132426	7.755072
-419.752102	-11.301392	7.765069
-417.814388	-8.328173	7.775066
-415.465727	-4.561629	7.785062
-413.803876	-6.499090	7.795059
-412.416405	-7.056944	7.805056
-410.140579	-8.370869	7.815053
-408.272521	-5.392833	7.825050
-406.526955	-3.688393	7.835046
-404.682334	-5.700824	7.845043
-402.571850	-5.924128	7.855040
-400.671902	-9.289075	7.865037
-399.011090	-10.597938	7.875034
-396.726242	-3.094868	7.885030
-394.899306	-6.386573	7.895027
-393.539550	-1.541566	7.905024
-391.585842	-0.077193	7.915021
-389.664026	-4.358257	7.925018
-387.504645	-5.740409	7.935014
-385.971206	-4.436292	7.945011
-383.849845	-8.384477	7.955008
-381.805149	-6.813046	7.965005
-380.296453	-4.814974	7.975002
-378.747086	-5.376555	7.984998
-376.449174	-9.750819	7.994995
-374.281214	-6.582221	8.004992
-372.515157	-8.179451	8.014989
-370.722259	-8.588859	8.024986
-368.915288	0.466863	8.034982
-367.196527	-9.311239	8.044979
-365.061806	-10.902591	8.054976
-362.757916	-6.749898	8.064973
-361.339845	-4.879448	8.074970
-359.895272	-1.315859	8.084966
-357.865222	0.870564	8.094963
-355.604096	-2.570966	8.104960
-353.793087	-1.776937	8.114957
-352.121350	-6.438042	8.124954
-350.243199	-1.505252	8.134950
-348.376463	-3.840120	8.144947
-346.413350	-0.842473	8.154944
-344.280532	-2.728767	8.164941
-342.877638	-2.164832	8.174938
-340.565220	-5.421905	8.184934
-338.821521	-5.675013	8.194931
-336.998601	2.029768	8.204928
-335.079519	-3.052925	8.214925
-333.129771	4.502139	8.224922
-331.544466	-0.453052	8.234918
-329.453587	-6.100011	8.244915
-327.236822	-0.648105	8.254912
-325.868496	-5.262331	8.264909
-324.115720	0.715236	8.274906
-322.209464	-6.796981	8.284902
-319.945007	-10.663746	8.294899
-318.214290	-15.441612	8.304896
-316.304762	-10.554859	8.314893
-314.384680	-6.850841	8.324890
-312.421961	-9.868900	8.334886
-310.869728	-4.947204	8.344883
-309.005850	-3.335790	8.354880
-306.845103	-1.086504	8.364877
-304.941561	-2.876161	8.374874
-303.289465	-2.681987	8.384870
-301.291970	-7.684013	8.394867
-299.366992	-7.373927	8.404864
-297.514573	-5.383306	8.414861
-295.872140	-2.713369	8.424858
-294.044123	-4.288855	8.434854
-292.249588	-4.324255	8.444851
-289.985158	-3.678351	8.454848
-288.162835	-1.425548	8.464845
-286.324008	0.474094	8.474842
-284.477916	1.253103	8.484838
-282.407101	-3.634299	8.494835
-280.709438	-0.662115	8.504832
-278.979477	-3.513518	8.514829
-276.995344	2.439787	8.524826
-274.991434	4.322560	8.534822
-272.944633	-0.879949	8.544819
-271.606476	-0.782481	8.554816
-269.657972	1.469142	8.564813
-267.452529	3.449224	8.574810
-265.510360	0.619218	8.584807
-264.093131	-0.797514	8.594803
-261.780441	2.553352	8.604800
-259.898983	-4.184336	8.614797
-258.299344	2.484047	8.624794
-256.584655	2.289314	8.634791
-254.387777	-0.889237	8.644787
-252.348357	-0.581591	8.654784
-250.698954	-6.386964	8.664781
-248.801886	4.091327	8.674778
-246.908410	1.586477	8.684775
-244.931640	-0.268508	8.694771
-243.275697	2.625101	8.704768
-241.393638	3.995246	8.714765
-239.427739	10.117288	8.724762
-237.580206	1.089232	8.734759
-235.428438	-0.979993	8.744755
-233.696070	3.270374	8.754752
-231.901459	4.363958	8.764749
-230.387829	3.958177	8.774746
-228.253828	8.051285	8.784743
-226.399477	3.706900	8.794739
-224.385869	-3.012382	8.804736
-222.601574	-2.105041	8.814733
-220.556598	4.075447	8.824730
-218.572846	-0.373270	8.834727
-216.842553	1.199539	8.844723
-215.252290	0.701010	8.854720
-213.324688	5.098654	8.864717
-211.128729	-1.755513	8.874714
-209.305104	1.409778	8.884711
-207.544578	1.694081	8.894707
-205.613282	-1.798882	8.904704
-203.664885	-5.296150	8.914701
-202.138101	0.720742	8.924698
-200.213335	2.314630	8.934695
-197.866667	3.915395	8.944691
-196.237582	2.828048	8.954688
-194.312313	0.095531	8.964685
-192.662474	2.115411	8.974682
-190.503801	-4.382259	8.984679
-188.410791	-11.104709	8.994675
-186.796422	-9.426535	9.004672
-184.907453	-9.915875	9.014669
-183.380978	-10.492625	9.024666
-181.166325	-7.964458	9.034663
-179.306217	-11.411301	9.044659
-177.602098	-10.050603	9.054656
-175.530489	-11.139085	9.064653
-173.923410	-14.190277	9.074650
-171.855360	-6.104481	9.084647
-170.016770	-8.777354	9.094643
-168.001696	-13.955765	9.104640
-166.351313	-11.031217	9.114637
-164.631458	-7.389857	9.124634
-162.337233	-6.682271	9.134631
-160.917945	-10.774016	9.144627
-158.993510	-13.929529	9.154624
-157.044146	-14.156905	9.164621
-155.095381	-6.041004	9.174618
-152.872207	-7.081023	9.184615
-151.108338	-10.724066	9.194611
-149.285921	-11.865917	9.204608
-147.346565	-0.410600	9.214605
-145.629761	-9.019830	9.224602
-143.924623	-11.011386	9.234599
-141.583345	-10.819711	9.244595
-140.052102	-11.703511	9.254592
-138.096588	-10.970272	9.264589
-136.228406	-12.179417	9.274586
-134.750511	-12.232067	9.284583
-132.539515	-9.090637	9.294579
-130.456345	-9.377240	9.304576
-128.563340	-7.369277	9.314573
-126.995391	-9.419456	9.324570
-124.983540	-1.330960	9.334567
-122.957063	-11.658544	9.344563
-121.352599	-3.621881	9.354560
-119.447872	-4.390001	9.364557
-117.539731	-1.662863	9.374554
-115.474192	-5.687179	9.384551
-113.417648	-9.591636	9.394547
-112.029610	-8.677824	9.404544
-109.948043	-1.116756	9.414541
-108.017843	-3.257885	9.424538
-106.305929	-3.690491	9.434535
-104.518038	-4.585221	9.444531
-102.497213	-10.806609	9.454528
-100.558069	-12.778631	9.464525
-98.989339	-8.116789	9.474522
-96.770843	-9.271274	9.484519
-95.011792	-15.577202	9.494515
-93.039260	-11.271893	9.504512
-91.233965	-11.147808	9.514509
-89.374687	-4.031255	9.524506
-87.314334	-1.999434	9.534503
-85.631327	-6.303744	9.544499
-83.736405	1.165551	9.554496
-81.780719	-5.730696	9.564493
-80.216011	1.663394	9.574490
-78.196114	-6.291521	9.584487
-75.837839	-5.440913	9.594483
-74.103106	-6.533982	9.604480
-72.631781	-5.445541	9.614477
-70.950149	-4.919602	9.624474
-68.427323	-7.862625	9.634471
-66.799342	-9.797607	9.644467
-64.935410	-7.979166	9.654464
-63.071832	-3.119601	9.664461
-61.116060	2.642630	9.674458
-59.232374	-3.155793	9.684455
-57.427591	-5.259505	9.694451
-55.690830	-2.896554	9.704448
-53.818677	0.264276	9.714445
-51.729822	-9.230048	9.724442
-49.876971	-5.096659	9.734439
-48.107040	-1.055829	9.744435
-46.076374	-9.794019	9.754432
-44.352333	-7.662716	9.764429
-42.462808	-2.221482	9.774426
-40.690158	-2.150571	9.784423
-38.524769	-2.750213	9.794419
-36.722847	-1.326068	9.804416
-35.269857	3.505867	9.814413
-33.247501	2.722205	9.824410
-31.031783	1.272957	9.834407
-29.116319	0.997407	9.844403
-27.411486	-1.965079	9.854400
-25.340415	-3.618615	9.864397
-23.794654	-3.503601	9.874394
-21.980318	0.378586	9.884391
-19.928571	-2.699238	9.894387
-17.959731	-5.909098	9.904384
-16.173301	0.909666	9.914381
-14.489162	-3.746887	9.924378
-12.365077	2.146432	9.934375
-10.314754	-4.717493	9.944371
-8.627966	-2.174428	9.954368
-6.955265	-1.689652	9.964365
-5.437076	3.521904	9.974362
-3.799484	30.126660	9.984359
-2.217824	67.502597	9.994355
-0.991084	109.815838	10.004352
0.000000	159.479766	10.009357
0.972698	175.180894	10.014362
1.345031	219.732078	10.019367
2.054645	232.461666	10.024371
2.652115	261.125452	10.029376
2.792216	283.051332	10.034381
3.061012	278.758542	10.039386
2.885013	286.862281	10.044391
3.005994	304.498738	10.049395
3.317760	322.565258	10.054400
3.384328	332.716662	10.059405
3.615549	329.920090	10.064410
3.546950	347.763462	10.069415
3.779255	338.398620	10.074419
3.950284	345.496119	10.079424
3.852194	342.731576	10.084429
4.060380	345.272002	10.089434
3.760843	347.142781	10.094439
4.057667	337.343441	10.099443
3.600921	350.737014	10.104448
3.809128	348.317853	10.109453
4.133429	343.699219	10.114458
3.894241	362.539660	10.119463
4.125025	353.015777	10.124467
4.093115	355.924093	10.129472
3.874355	358.595706	10.134477
4.014274	370.946356	10.139482
4.099321	365.418117	10.144487
4.125429	367.885089	10.149491
4.044795	374.398265	10.154496
3.814367	375.039020	10.159501
4.232025	389.119479	10.164506
4.390974	394.810688	10.169511
4.455895	395.139397	10.174515
4.666304	405.400373	10.179520
4.726261	412.018874	10.184525
4.849852	402.296011	10.189530
4.624049	413.173789	10.194535
4.697194	413.360835	10.199539
4.476320	413.075956	10.204544
4.411126	420.832505	10.209549
5.107822	407.578820	10.214554
4.589461	423.161675	10.219559
4.549406	416.234089	10.224563
4.794586	428.017630	10.229568
5.235659	438.656581	10.234573
5.038324	431.038126	10.239578
5.158214	444.171063	10.244583
5.325554	445.774986	10.249587
5.143732	445.450760	10.254592
4.945533	460.083701	10.259597
5.480976	462.020000	10.264602
5.255259	461.677544	10.269607
5.258820	463.813807	10.274611
5.496404	464.933431	10.279616
5.381229	465.877510	10.284621
5.675968	462.938314	10.289626
5.386896	474.818155	10.294631
5.471981	464.306591	10.299635
5.334614	465.613763	10.304640
5.224288	472.764091	10.309645
5.349170	467.245229	10.314650
5.623242	478.372906	10.319655
5.793672	495.006627	10.324659
5.848174	507.426213	10.329664
6.111904	504.657540	10.334669
6.430528	509.881765	10.339674
6.115598	493.181219	10.344679
5.815570	485.932362	10.349683
6.017216	505.778174	10.354688
5.978647	505.222932	10.359693
5.901363	518.977184	10.364698
6.005052	517.237006	10.369703
6.298698	507.332401	10.374707
6.322283	517.318898	10.379712
6.179149	522.433856	10.384717
6.419527	518.090335	10.389722
6.467342	524.627244	10.394727
6.452242	514.383944	10.399731
6.629275	524.710254	10.404736
6.245981	527.818163	10.409741
6.415491	521.208767	10.414746
6.377797	526.718502	10.419751
6.625107	536.511625	10.424755
6.738760	544.313829	10.429760
6.667358	561.475071	10.434765
6.968385	562.564082	10.439770
7.120857	564.523638	10.444775
7.113636	559.588802	10.449779
7.077089	560.897247	10.454784
7.015618	553.154550	10.459789
7.182809	556.218808	10.464794
6.824816	551.789374	10.469799
6.945240	562.883277	10.474803
7.192345	565.597312	10.479808
7.159378	571.336551	10.484813
7.304893	564.125396	10.489818
7.157882	575.115308	10.494823
7.137007	566.229112	10.499827
7.098131	569.834038	10.504832
6.947313	577.967039	10.509837
7.347252	578.256504	10.514842
7.257142	584.339976	10.519847
7.454395	593.598635	10.524851
7.821484	604.241625	10.529856
7.606402	603.794963	10.534861
7.774068	604.909982	10.539866
7.922638	612.782349	10.544871
7.782755	608.042129	10.549875
7.851593	612.293802	10.554880
7.699745	625.683145	10.559885
7.774012	616.780165	10.564890
7.947474	626.361195	10.569895
7.799544	619.029659	10.574899
7.997032	619.308841	10.579904
8.120954	621.410158	10.584909
8.475782	612.440348	10.589914
8.144420	620.628982	10.594919
8.296713	624.094613	10.599923
7.924787	617.361800	10.604928
8.043267	620.315567	10.609933
8.142746	617.565189	10.614938
7.893493	627.005485	10.619943
8.196184	635.433618	10.624947
8.102611	651.691724	10.629952
8.219466	657.107467	10.634957
8.388505	653.678911	10.639962
8.310489	664.843972	10.644967
8.630667	660.329979	10.649971
8.525789	650.597662	10.654976
8.540097	670.945109	10.659981
9.039984	678.728354	10.664986
8.960857	676.793383	10.669991
9.115352	665.835347	10.674995
8.911701	665.314318	10.680000
8.548010	673.205352	10.685005
8.887387	690.113555	10.690010
9.268114	686.256971	10.695015
9.067811	695.446643	10.700019
9.418425	692.865933	10.705024
9.214720	698.586725	10.710029
9.255647	689.690595	10.715034
8.957657	697.821907	10.720039
9.092213	701.058565	10.725043
9.390595	706.164661	10.730048
9.059331	699.417439	10.735053
9.406403	697.275702	10.740058
9.027375	703.764082	10.745063
9.295741	708.764575	10.750067
9.108710	720.021188	10.755072
9.333029	732.625198	10.760077
9.688883	736.891050	10.765082
9.730802	740.043142	10.770087
9.723282	739.257425	10.775091
9.811565	739.919897	10.780096
9.717622	743.185129	10.785101
10.211670	740.111580	10.790106
9.870152	748.896440	10.795111
9.677888	744.672331	10.800115
9.960481	750.295069	10.805120
9.679956	755.370520	10.810125
9.871292	748.959398	10.815130
9.829405	763.285423	10.820135
10.075706	774.618039	10.825139
10.454771	780.678005	10.830144
10.102933	784.156280	10.835149
10.279074	783.521044	10.840154
10.235677	786.584250	10.845159
10.266091	792.384432	10.850163
10.221387	791.267160	10.855168
10.106260	789.669092	10.860173
10.549647	786.974214	10.865178
10.270450	793.730572	10.870183
10.301751	801.883534	10.875187
10.996881	805.835078	10.880192
10.671286	821.291408	10.885197
11.179470	814.052242	10.890202
10.581681	829.209786	10.895207
10.844980	818.486604	10.900211
10.941400	819.139897	10.905216
10.781631	822.349412	10.910221
10.839803	821.821306	10.915226
10.869431	823.885652	10.920231
10.783222	832.678724	10.925235
10.978684	828.643489	10.930240
10.570381	840.056921	10.935245
10.857764	827.338105	10.940250
10.874014	843.511095	10.945255
11.038129	851.243911	10.950259
11.439406	864.310264	10.955264
11.364869	856.649918	10.960269
11.446149	854.372353	10.965274
11.452596	879.239535	10.970279
11.340630	865.458387	10.975283
11.459755	867.440651	10.980288
11.295470	870.098936	10.985293
11.336155	865.266747	10.990298
11.365095	879.460157	10.995303
11.418880	886.811602	11.000307
11.457809	901.886579	11.005312
11.708407	905.481684	11.010317
12.110665	908.439131	11.015322
11.924008	921.586704	11.020327
12.271774	912.245657	11.025331
12.119496	912.725726	11.030336
12.017800	908.023473	11.035341
11.895405	908.811027	11.040346
12.078425	907.614842	11.045351
12.058182	915.017536	11.050355
12.136302	895.352082	11.055360
11.832001	920.429760	11.060365
12.425863	909.046623	11.065370
12.228479	919.964401	11.070375
12.084023	915.986518	11.075379
12.338208	925.236308	11.080384
12.446306	936.534323	11.085389
12.282053	950.230312	11.090394
12.734169	942.944830	11.095399
12.787555	945.973706	11.100403
12.855629	952.617968	11.105408
12.860973	947.125879	11.110413
12.551737	927.932201	11.115418
12.596886	953.296410	11.120423
12.641816	946.960598	11.125427
13.035392	937.205351	11.130432
12.852580	956.845010	11.135437
13.145178	944.855430	11.140442
12.965921	955.410778	11.145447
13.479674	948.372519	11.150451
13.017267	944.421690	11.155456
12.755722	955.225143	11.160461
13.348444	943.111992	11.165466
12.908343	955.877378	11.170471
12.920323	956.345439	11.175475
13.049176	949.750221	11.180480
12.962093	964.793321	11.185485
13.583991	971.306669	11.190490
13.444198	992.292616	11.195495
13.450885	988.460924	11.200499
13.579427	994.657142	11.205504
13.350315	990.814175	11.210509
13.682217	999.356139	11.215514
13.747282	990.848659	11.220519
13.696002	997.228113	11.225523
13.867139	980.775917	11.230528
13.539945	993.715725	11.235533
13.908815	980.742489	11.240538
13.765088	997.832199	11.245543
13.781450	989.196863	11.250547
13.905042	984.414491	11.255552
13.613520	988.890924	11.260557
13.860752	987.734954	11.265562
13.761572	991.538849	11.270567
14.018520	999.070844	11.275571
14.025675	1019.169169	11.280576
13.920559	1018.414775	11.285581
14.039470	1019.491869	11.290586
14.100292	1026.037968	11.295591
14.200693	1028.056359	11.300595
14.418054	1020.417178	11.305600
14.358079	1035.042841	11.310605
14.321359	1020.595068	11.315610
14.377798	1037.477842	11.320615
14.552504	1050.115275	11.325619
14.929113	1048.828270	11.330624
14.664468	1055.699129	11.335629
14.892477	1056.568001	11.340634
14.926464	1045.868614	11.345639
15.006731	1038.970426	11.350643
15.008211	1019.618247	11.355648
14.576386	1033.388536	11.360653
14.806349	1038.688602	11.365658
14.964637	1060.186950	11.370663
15.033382	1063.353759	11.375667
14.934152	1059.838583	11.380672
14.947691	1067.800550	11.385677
15.057563	1065.327569	11.390682
15.263689	1071.016249	11.395687
14.947187	1068.983464	11.400691
14.936311	1069.586071	11.405696
15.050410	1071.796260	11.410701
15.489089	1070.098781	11.415706
15.148169	1075.494656	11.420711
15.218669	1080.930567	11.425715
15.546792	1087.812549	11.430720
15.559816	1102.715236	11.435725
15.690808	1094.115173	11.440730
15.767970	1086.991939	11.445735
16.044193	1101.054651	11.450739
16.231868	1087.886282	11.455744
15.595568	1088.669083	11.460749
15.520283	1073.514580	11.465754
15.673218	1073.554858	11.470759
15.783614	1092.465066	11.475763
16.047074	1086.439709	11.480768
16.027662	1085.190639	11.485773
16.356762	1101.684621	11.490778
16.028416	1104.041090	11.495783
16.034117	1101.702998	11.500787
16.289522	1099.258839	11.505792
16.004025	1104.455060	11.510797
16.014429	1093.759400	11.515802
16.213068	1107.098008	11.520807
15.973178	1103.562679	11.525811
16.213409	1098.236505	11.530816
16.013960	1099.955784	11.535821
16.395261	1111.279747	11.540826
16.583364	1125.799692	11.545831
16.525195	1131.527401	11.550835
16.540839	1126.445214	11.555840
16.309449	1138.365280	11.560845
16.627177	1141.288949	11.565850
16.483742	1138.219228	11.570855
16.806534	1142.096210	11.575859
16.748384	1134.242280	11.580864
16.481692	1138.049277	11.585869
16.978139	1141.236193	11.590874
16.815032	1137.171332	11.595879
16.660478	1133.699659	11.600883
17.296068	1134.281155	11.605888
17.015567	1150.383543	11.610893
16.947339	1144.247057	11.615898
17.481732	1158.937317	11.620903
17.314664	1159.642119	11.625907
17.268324	1163.462862	11.630912
17.141929	1167.838886	11.635917
17.467165	1160.622425	11.640922
17.447778	1175.352149	11.645927
17.236414	1175.409535	11.650931
17.774885	1167.905149	11.655936
17.501966	1171.287341	11.660941
17.670158	1167.928192	11.665946
17.709514	1178.663310	11.670951
17.602944	1178.875881	11.675955
17.865957	1174.765116	11.680960
17.775963	1175.735186	11.685965
17.938758	1168.232374	11.690970
17.941645	1173.854160	11.695975
17.727600	1175.507962	11.700979
17.851954	1173.272366	11.705984
17.408855	1170.843415	11.710989
17.459332	1174.585636	11.715994
17.715289	1176.238589	11.720999
17.580085	1184.106066	11.726003
18.134881	1188.830787	11.731008
17.767751	1208.053876	11.736013
17.951856	1205.226806	11.741018
18.209031	1207.499355	11.746023
18.442554	1206.183118	11.751027
18.732315	1199.743483	11.756032
18.619813	1210.173241	11.761037
18.571710	1203.112513	11.766042
18.506424	1201.142145	11.771047
18.237884	1210.207398	11.776051
18.294862	1209.028139	11.781056
18.125632	1208.077366	11.786061
18.632912	1204.716163	11.791066
18.544579	1210.560687	11.796071
18.322220	1212.488652	11.801075
18.725024	1218.347883	11.806080
18.467469	1241.568755	11.811085
18.579476	1234.632293	11.816090
18.874845	1236.944491	11.821095
18.683963	1240.461857	11.826099
19.190102	1236.369068	11.831104
18.808941	1243.581900	11.836109
18.765391	1229.622324	11.841114
18.820908	1249.137621	11.846119
19.025083	1251.633114	11.851123
19.363489	1260.197851	11.856128
19.600250	1269.996308	11.861133
19.604572	1269.748033	11.866138
19.496647	1264.617694	11.871143
19.772405	1259.684794	11.876147
19.599423	1242.238441	11.881152
19.152805	1245.134232	11.886157
19.608403	1251.089142	11.891162
19.768922	1261.823920	11.896167
19.688165	1268.507838	11.901171
20.032831	1263.895131	11.906176
19.696853	1248.231631	11.911181
19.692995	1238.200510	11.916186
19.842885	1242.862094	11.921191
19.579027	1270.703260	11.926195
19.616108	1266.406141	11.931200
19.887021	1270.045410	11.936205
19.868712	1269.589416	11.941210
19.848973	1270.067279	11.946215
19.566449	1270.746344	11.951219
19.717952	1275.428182	11.956224
19.973992	1278.194549	11.961229
20.073715	1281.247645	11.966234
20.344774	1293.291134	11.971239
20.215825	1302.766296	11.976243
20.365874	1303.491488	11.981248
20.147102	1315.997937	11.986253
20.597096	1299.647570	11.991258
20.621009	1306.677537	11.996263
20.680121	1304.731471	12.001267
20.671032	1305.089355	12.006272
20.884145	1301.439136	12.011277
20.894130	1295.074051	12.016282
20.581438	1281.087965	12.021287
20.341801	1280.851794	12.026291
20.744744	1277.884139	12.031296
20.596843	1287.736081	12.036301
20.596269	1286.280546	12.041306
20.774776	1289.475630	12.046311
20.731067	1279.452415	12.051315
20.718505	1283.840280	12.056320
20.410393	1282.627782	12.061325
20.440191	1274.581537	12.066330
20.522229	1285.950219	12.071335
20.649146	1308.171509	12.076339
21.081536	1298.783599	12.081344
20.655374	1291.622270	12.086349
20.670490	1279.947935	12.091354
20.849706	1280.837220	12.096359
20.764156	1282.462652	12.101363
20.975753	1281.108903	12.106368
20.804397	1283.374121	12.111373
20.754935	1282.066744	12.116378
20.936117	1287.369952	12.121383
20.689608	1290.153400	12.126387
20.827658	1278.259168	12.131392
20.661196	1292.823221	12.136397
20.692914	1285.563625	12.141402
20.662205	1284.180712	12.146407
20.225096	1288.680457	12.151411
20.799378	1283.611615	12.156416
20.496833	1296.140872	12.161421
20.901220	1282.362126	12.166426
20.751151	1293.032920	12.171431
20.515507	1290.443113	12.176435
20.794438	1289.330954	12.181440
20.459299	1278.553071	12.186445
20.714003	1285.809586	12.191450
20.529440	1283.445040	12.196455
20.569675	1284.225598	12.201459
20.745833	1278.658824	12.206464
20.335005	1283.996534	12.211469
20.793097	1284.947000	12.216474
20.752724	1292.047143	12.221479
20.437414	1286.956185	12.226483
20.490672	1272.933813	12.231488
20.517583	1292.671368	12.236493
20.752641	1292.731667	12.241498
21.035994	1297.239504	12.246503
20.397231	1279.540950	12.251507
20.622623	1268.374018	12.256512
20.556087	1271.991415	12.261517
20.623887	1274.130168	12.266522
20.680811	1271.802803	12.271527
20.378536	1269.140043	12.276531
20.865672	1265.510783	12.281536
20.674446	1265.848830	12.286541
20.732315	1262.089333	12.291546
20.822619	1265.861497	12.296551
20.752207	1267.959212	12.301555
21.046510	1275.591058	12.306560
20.870323	1274.087837	12.311565
21.136757	1264.803697	12.316570
21.313480	1268.238777	12.321575
21.197938	1264.790813	12.326579
21.414654	1234.736692	12.331584
20.639607	1246.108007	12.336589
20.623365	1246.214699	12.341594
20.882862	1236.352898	12.346599
20.415889	1249.137019	12.351603
20.838260	1246.303476	12.356608
20.553531	1252.784940	12.361613
20.418947	1247.387602	12.366618
20.306517	1244.153629	12.371623
20.320832	1250.940655	12.376627
20.360799	1250.896445	12.381632
20.267388	1253.343205	12.386637
20.132398	1246.097604	12.391642
20.577104	1258.704768	12.396647
20.727514	1272.437605	12.401651
20.629717	1271.672567	12.406656
20.573134	1273.763346	12.411661
20.783466	1273.094250	12.416666
20.657692	1255.578844	12.421671
20.314169	1257.505641	12.426675
20.993363	1256.113579	12.431680
20.484213	1249.020706	12.436685
20.506836	1246.918030	12.441690
20.507276	1248.854619	12.446695
20.751058	1266.499466	12.451699
20.840331	1259.512999	12.456704
20.477444	1252.582889	12.461709
20.435855	1251.668527	12.466714
20.649046	1252.826802	12.471719
20.510694	1275.315877	12.476723
20.551020	1275.959214	12.481728
20.384771	1269.256370	12.486733
20.437245	1278.598490	12.491738
21.003799	1281.544003	12.496743
20.835185	1284.584705	12.501747
20.600342	1274.620369	12.506752
20.415750	1262.443274	12.511757
20.482533	1262.426328	12.516762
20.818402	1277.306084	12.521767
20.568278	1280.637352	12.526771
21.080958	1275.269232	12.531776
20.460716	1271.400263	12.536781
20.329973	1263.877988	12.541786
20.679592	1256.692286	12.546791
20.484524	1260.386957	12.551795
20.528089	1256.123503	12.556800
20.528311	1279.336435	12.561805
20.701550	1275.728856	12.566810
20.669829	1280.807381	12.571815
20.781439	1294.188432	12.576819
20.864234	1277.303681	12.581824
20.498628	1267.101567	12.586829
20.398381	1262.657608	12.591834
20.591522	1262.160001	12.596839
20.536730	1268.929671	12.601843
20.766195	1265.144378	12.606848
20.426993	1265.450831	12.611853
20.605088	1279.127215	12.616858
20.574116	1289.231764	12.621863
20.464331	1298.006798	12.626867
20.854419	1275.091180	12.631872
20.684786	1287.066177	12.636877
20.673196	1282.589145	12.641882
20.702938	1263.539663	12.646887
20.259718	1267.441088	12.651891
20.844383	1267.585980	12.656896
20.447791	1269.833504	12.661901
20.786348	1269.550839	12.666906
20.618601	1266.349341	12.671911
20.407938	1269.032443	12.676915
20.714885	1269.825654	12.681920
20.474083	1265.194363	12.686925
20.648007	1275.332456	12.691930
20.960124	1268.293090	12.696935
20.745744	1271.678584	12.701939
20.911186	1258.939417	12.706944
20.617544	1259.211792	12.711949
20.576914	1264.236535	12.716954
20.720324	1256.541213	12.721959
20.437589	1264.930622	12.726963
20.611195	1264.462941	12.731968
20.764075	1271.988023	12.736973
20.786396	1271.574438	12.741978
20.634041	1267.228683	12.746983
20.297537	1277.000307	12.751987
20.530229	1259.700551	12.756992
20.634536	1274.289210	12.761997
20.480742	1272.124777	12.767002
20.639236	1263.752057	12.772007
20.233818	1273.212948	12.777011
20.255291	1271.619847	12.782016
20.436757	1282.652520	12.787021
20.756936	1292.966007	12.792026
20.749786	1294.082155	12.797031
20.533094	1299.739015	12.802035
20.619769	1300.386000	12.807040
20.920014	1296.548405	12.812045
20.657041	1284.850609	12.817050
20.668180	1279.201339	12.822055
20.638931	1276.838830	12.827059
20.773837	1268.476178	12.832064
20.670316	1276.384387	12.837069
20.870819	1274.590826	12.842074
20.502084	1272.824983	12.847079
20.260363	1278.211416	12.852083
20.761488	1269.403964	12.857088
20.508137	1275.161286	12.862093
20.159550	1283.529669	12.867098
20.455061	1284.398827	12.872103
20.399989	1300.217820	12.877107
20.901328	1302.175450	12.882112
20.622718	1308.009359	12.887117
20.515285	1304.596366	12.892122
20.841703	1305.457441	12.897127
20.539670	1301.193903	12.902131
20.832515	1281.463713	12.907136
20.825632	1280.942813	12.912141
20.654103	1278.543070	12.917146
20.548007	1280.496657	12.922151
20.715028	1281.381579	12.927155
20.631315	1274.063125	12.932160
20.507008	1275.272082	12.937165
20.328703	1270.818493	12.942170
20.546712	1268.372386	12.947175
20.333341	1278.854556	12.952179
20.856143	1291.414595	12.957184
20.600115	1290.140167	12.962189
20.522407	1284.812597	12.967194
20.774460	1268.979577	12.972199
20.914516	1281.151194	12.977203
20.785166	1278.911893	12.982208
20.690575	1283.145672	12.987213
20.585853	1283.017301	12.992218
20.666971	1277.298517	12.997223
20.638746	1280.777331	13.002227
20.917129	1278.029833	13.007232
20.839777	1278.322906	13.012237
20.821186	1291.846158	13.017242
20.996562	1282.535528	13.022247
20.648329	1286.669408	13.027251
20.780489	1280.002545	13.032256
20.795067	1285.158848	13.037261
20.772282	1281.628271	13.042266
20.955658	1278.678291	13.047271
20.405793	1271.670756	13.052275
20.587543	1262.559411	13.057280
20.611225	1263.779457	13.062285
20.634159	1272.293590	13.067290
20.767434	1266.402476	13.072295
20.690235	1262.765456	13.077299
20.415446	1251.722481	13.082304
20.359930	1259.589904	13.087309
20.575739	1277.726543	13.092314
20.965766	1278.312522	13.097319
20.676154	1277.407757	13.102323
20.469116	1265.972311	13.107328
20.521568	1258.100671	13.112333
20.421575	1265.591964	13.117338
20.832284	1271.803220	13.122343
20.759372	1271.529415	13.127347
20.686369	1261.536118	13.132352
20.624000	1267.464838	13.137357
20.383414	1261.273788	13.142362
20.555883	1257.600099	13.147367
20.451843	1265.063650	13.152371
20.759027	1283.978989	13.157376
20.885332	1278.790780	13.162381
20.746795	1267.060533	13.167386
20.493130	1254.814033	13.172391
20.427439	1267.007417	13.177395
20.670993	1259.124218	13.182400
20.603904	1257.419079	13.187405
20.592980	1263.022600	13.192410
20.655077	1261.481371	13.197415
20.237016	1269.152722	13.202419
20.401006	1270.933905	13.207424
20.861216	1285.924733	13.212429
20.638205	1297.460363	13.217434
20.819580	1296.310145	13.222439
20.585149	1280.792850	13.227443
20.607156	1261.142162	13.232448
20.434034	1274.708973	13.237453
20.457635	1273.587077	13.242458
20.663541	1285.784466	13.247463
20.688226	1295.340781	13.252467
20.886830	1296.424109	13.257472
20.701185	1274.753172	13.262477
20.174330	1273.542448	13.267482
20.989118	1274.926486	13.272487
21.057234	1280.282422	13.277491
20.804505	1276.473109	13.282496
20.836084	1270.656566	13.287501
20.707676	1271.916644	13.292506
20.702746	1262.276792	13.297511
20.567273	1268.083123	13.302515
20.689956	1264.687053	13.307520
20.787962	1267.877626	13.312525
20.835554	1272.296897	13.317530
20.948727	1269.757117	13.322535
20.757165	1270.604613	13.327539
20.688051	1260.878798	13.332544
20.604193	1261.172908	13.337549
20.575837	1258.688824	13.342554
20.986430	1249.059977	13.347559
20.611852	1258.612141	13.352563
20.509456	1241.406861	13.357568
20.694726	1250.371363	13.362573
20.641985	1252.800596	13.367578
20.533997	1250.228284	13.372583
20.359392	1254.954249	13.377587
20.559643	1251.077419	13.382592
20.630724	1254.404757	13.387597
20.822957	1267.605754	13.392602
20.937200	1257.282947	13.397607
20.600825	1249.610539	13.402611
20.693064	1235.665570	13.407616
20.716783	1235.597141	13.412621
20.454109	1234.536683	13.417626
20.454638	1237.570898	13.422631
20.485874	1237.201626	13.427635
20.716519	1234.092717	13.432640
20.685177	1236.133729	13.437645
20.528811	1241.561731	13.442650
20.931814	1239.735874	13.447655
20.702467	1244.853796	13.452659
20.674067	1239.972574	13.457664
20.920715	1236.025263	13.462669
20.778436	1233.661866	13.467674
20.867646	1237.860006	13.472679
20.627262	1243.683061	13.477683
20.281736	1240.021035	13.482688
20.662800	1240.632098	13.487693
20.343921	1244.646158	13.492698
20.582562	1239.277605	13.497703
20.316058	1247.714882	13.502707
20.520855	1243.110298	13.507712
20.391802	1247.814801	13.512717
20.455641	1246.098241	13.517722
20.615126	1242.384046	13.522727
20.520378	1259.177645	13.527731
20.665349	1247.884775	13.532736
20.521813	1254.818416	13.537741
20.575564	1268.386882	13.542746
20.960471	1260.712964	13.547751
20.492053	1255.972893	13.552755
20.309073	1245.050907	13.557760
20.482101	1266.403696	13.562765
20.607725	1263.478703	13.567770
20.809387	1272.249777	13.572775
20.579472	1274.532220	13.577779
20.874643	1262.365337	13.582784
20.794755	1250.483812	13.587789
20.421793	1256.354830	13.592794
20.503978	1242.859347	13.597799
20.641609	1242.687586	13.602803
20.270852	1246.451282	13.607808
20.558328	1252.103402	13.612813
20.898977	1274.525531	13.617818
20.784514	1253.425211	13.622823
20.347524	1249.118555	13.627827
20.437570	1265.601966	13.632832
20.728619	1275.697720	13.637837
20.619862	1269.362627	13.642842
20.903900	1271.600938	13.647847
20.752530	1258.369793	13.652851
20.517516	1257.289151	13.657856
20.493807	1251.460933	13.662861
20.379140	1251.616444	13.667866
20.534414	1255.513869	13.672871
20.245697	1269.271015	13.677875
20.643453	1276.626141	13.682880
20.605824	1278.336976	13.687885
20.529941	1273.939594	13.692890
20.888407	1279.222405	13.697895
20.587451	1288.113089	13.702899
20.736238	1273.501423	13.707904
20.431992	1286.146069	13.712909
20.686930	1273.334262	13.717914
20.819552	1269.663772	13.722919
20.516659	1276.559760	13.727923
21.037782	1270.720327	13.732928
21.036774	1255.137439	13.737933
20.474978	1251.423168	13.742938
20.518908	1245.374412	13.747943
20.460192	1256.856994	13.752947
20.380452	1244.749928	13.757952
20.617525	1250.381700	13.762957
20.683783	1252.392952	13.767962
20.790624	1255.750860	13.772967
20.323174	1258.170546	13.777971
20.490984	1254.163261	13.782976
20.715509	1283.735452	13.787981
20.526195	1275.016050	13.792986
20.858472	1269.465381	13.797991
20.507501	1260.497364	13.802995
20.456791	1256.154323	13.808000
20.653177	1266.757218	13.813005
20.441224	1280.019544	13.818010
20.886844	1270.298356	13.823015
20.413577	1272.905067	13.828019
20.707001	1281.866529	13.833024
20.794384	1280.207716	13.838029
20.544165	1263.970657	13.843034
20.459935	1261.132759	13.848039
20.594230	1269.711135	13.853043
20.734073	1278.509422	13.858048
20.579342	1256.817809	13.863053
20.430050	1256.456832	13.868058
20.698509	1272.441824	13.873063
20.731979	1279.776207	13.878067
20.652462	1269.796559	13.883072
20.364894	1259.634047	13.888077
20.597244	1271.190068	13.893082
21.121668	1273.902584	13.898087
20.835352	1269.234394	13.903091
20.616652	1259.452010	13.908096
20.498773	1257.081563	13.913101
20.394493	1269.836234	13.918106
20.522166	1257.647184	13.923111
20.298741	1262.418788	13.928115
20.402475	1275.411541	13.933120
20.858247	1290.966098	13.938125
20.524377	1281.962221	13.943130
20.747244	1286.941787	13.948135
20.395007	1278.659988	13.953139
20.761443	1292.812584	13.958144
20.646261	1280.195438	13.963149
20.528436	1275.278002	13.968154
20.748370	1269.917154	13.973159
20.353533	1275.667081	13.978163
20.467634	1280.343848	13.983168
20.754710	1289.066612	13.988173
20.610566	1295.689686	13.993178
20.991864	1284.860601	13.998183
20.756556	1279.296377	14.003187
20.592064	1262.539405	14.008192
20.655558	1262.747561	14.013210
20.658251	1268.638221	14.018227
20.705804	1256.946033	14.023245
20.656069	1268.537924	14.028263
20.306897	1263.141442	14.033280
20.781063	1274.833816	14.038298
20.741022	1279.111054	14.043315
20.713148	1271.097670	14.048333
20.600148	1279.001418	14.053351
20.678849	1279.105285	14.058368
20.745687	1293.494364	14.063386
20.545084	1301.405805	14.068403
20.856876	1293.670143	14.073421
20.739264	1301.189240	14.078439
20.685620	1305.185506	14.083456
20.941707	1306.886043	14.088474
20.701388	1311.067819	14.093491
20.815884	1303.635762	14.098509
20.997621	1311.070934	14.103527
20.968355	1313.770262	14.108544
21.033282	1301.560877	14.113562
20.937352	1310.638563	14.118579
21.209894	1296.011314	14.123597
21.103156	1304.258575	14.128615
20.880394	1302.730507	14.133632
21.188497	1301.814623	14.138650
21.060880	1301.141277	14.143667
20.970874	1300.013611	14.148685
21.131632	1297.452219	14.153703
20.926830	1296.978379	14.158720
21.123575	1302.565961	14.163738
20.591328	1307.876564	14.168755
20.971041	1295.544611	14.173773
21.043538	1311.192822	14.178791
21.080332	1301.054920	14.183808
21.018772	1302.298029	14.188826
20.832313	1312.127920	14.193843
21.212130	1326.676324	14.198861
21.093946	1338.747960	14.203879
21.176979	1332.286765	14.208896
21.610741	1338.838591	14.213914
21.510658	1340.688757	14.218931
21.526413	1335.392917	14.223949
21.973137	1346.885229	14.228967
21.399462	1330.162329	14.233984
21.295895	1315.171902	14.239002
21.479950	1325.241581	14.244019
21.577217	1330.395147	14.249037
21.162266	1330.031906	14.254055
21.646210	1334.286928	14.259072
21.572759	1337.570620	14.264090
21.262002	1347.701939	14.269107
21.496475	1340.368704	14.274125
21.620248	1342.231927	14.279143
21.385940	1348.364922	14.284160
21.677495	1343.028231	14.289178
21.414790	1341.800692	14.294195
21.514784	1339.135726	14.299213
21.857929	1335.514882	14.304231
21.717168	1333.865189	14.309248
21.745538	1336.490831	14.314266
21.471644	1347.300550	14.319283
21.721771	1338.371310	14.324301
21.701140	1337.817753	14.329319
21.821723	1340.826672	14.334336
21.736248	1346.350746	14.339354
21.656187	1344.902160	14.344371
21.831393	1343.799828	14.349389
21.655421	1352.487605	14.354407
21.674676	1340.658288	14.359424
21.901911	1328.317596	14.364442
21.834993	1335.219851	14.369459
21.999088	1336.206740	14.374477
22.113350	1334.046023	14.379495
21.837533	1335.477471	14.384512
21.858061	1335.238253	14.389530
21.762551	1341.220113	14.394547
21.805063	1333.478619	14.399565
21.994283	1336.953225	14.404583
21.721173	1344.116467	14.409600
21.750793	1338.703581	14.414618
21.890040	1365.049015	14.419635
22.401525	1365.676893	14.424653
22.411444	1355.703693	14.429671
22.195259	1360.183661	14.434688
22.339238	1358.468096	14.439706
22.064320	1353.622891	14.444723
22.089150	1355.467291	14.449741
22.141784	1355.740488	14.454759
21.977460	1361.525689	14.459776
22.324302	1352.304155	14.464794
22.287492	1360.288604	14.469811
22.455422	1364.068640	14.474829
22.422063	1366.823687	14.479847
21.977863	1372.675559	14.484864
22.346204	1361.603815	14.489882
22.267611	1367.760744	14.494899
22.341133	1365.880234	14.499917
22.591698	1367.350420	14.504935
22.489101	1370.550677	14.509952
22.580192	1364.173128	14.514970
22.263312	1367.601051	14.519987
22.534747	1370.631532	14.525005
22.600739	1361.726930	14.530023
22.586998	1361.793632	14.535040
22.763327	1355.306534	14.540058
22.612151	1365.747472	14.545075
22.758301	1363.202557	14.550093
22.832147	1360.831201	14.555111
22.450568	1365.200696	14.560128
22.572036	1360.724853	14.565146
22.770722	1369.521196	14.570163
22.590622	1369.713537	14.575181
22.782697	1363.947531	14.580199
22.560404	1366.619455	14.585216
22.790981	1365.193677	14.590234
22.666710	1368.051317	14.595251
22.659028	1368.771447	14.600269
22.996890	1355.953751	14.605287
22.610196	1365.614265	14.610304
22.983021	1356.355550	14.615322
22.736875	1359.528364	14.620339
22.722782	1363.817218	14.625357
22.708946	1362.798523	14.630375
22.706150	1356.115049	14.635392
22.846303	1362.655517	14.640410
22.634463	1361.780093	14.645427
22.651639	1365.390690	14.650445
23.142680	1372.419472	14.655463
22.814290	1380.996295	14.660480
23.182704	1385.795163	14.665498
23.117026	1396.961826	14.670515
22.997813	1394.613394	14.675533
23.388456	1393.997378	14.680551
23.081363	1387.511869	14.685568
23.446760	1362.470221	14.690586
23.096993	1378.857557	14.695603
23.318781	1362.482799	14.700621
23.228305	1362.064654	14.705639
23.286331	1366.458411	14.710656
23.277966	1363.296334	14.715674
23.291782	1358.479005	14.720691
23.134122	1355.394228	14.725709
23.466665	1365.385192	14.730727
23.466509	1364.532633	14.735744
23.516287	1355.614890	14.740762
23.460395	1361.787073	14.745779
22.971843	1368.470301	14.750797
22.950633	1361.420092	14.755815
23.017067	1386.256030	14.760832
23.240577	1388.164699	14.765850
23.383950	1397.201122	14.770867
23.260521	1401.240006	14.775885
23.733600	1394.932076	14.780903
23.089430	1402.668928	14.785920
23.168961	1391.684129	14.790938
23.242135	1397.705175	14.795955
23.112520	1397.598446	14.800973
23.582651	1415.420240	14.805991
23.540885	1434.599468	14.811008
24.010255	1426.538145	14.816026
24.020958	1428.896055	14.821043
23.457231	1420.437939	14.826061
23.939708	1425.699985	14.831079
23.572912	1427.330003	14.836096
23.944399	1433.619666	14.841114
23.795473	1429.589638	14.846131
23.811623	1433.526040	14.851149
24.135157	1426.444405	14.856167
23.680961	1415.481801	14.861184
23.753342	1421.474668	14.866202
23.857387	1422.507322	14.871219
23.939656	1430.726079	14.876237
23.994105	1438.080944	14.881255
23.844042	1441.918016	14.886272
24.116986	1434.064204	14.891290
24.322138	1419.549831	14.896307
24.086082	1420.949775	14.901325
24.053484	1404.116886	14.906343
23.667118	1404.674045	14.911360
23.943231	1416.597906	14.916378
24.126186	1419.736894	14.921395
23.916609	1428.947616	14.926413
24.072045	1441.829869	14.931431
24.317386	1437.700768	14.936448
24.453341	1435.857483	14.941466
24.324856	1435.266068	14.946483
24.230661	1420.818319	14.951501
24.150993	1413.854489	14.956519
23.961120	1427.622389	14.961536
24.031070	1427.468096	14.966554
24.269724	1427.327794	14.971571
24.362967	1436.123693	14.976589
24.236287	1435.255130	14.981607
24.352715	1439.647459	14.986624
24.121224	1436.590172	14.991642
24.249699	1437.475782	14.996659
24.483801	1441.773834	15.001677
24.358627	1430.020967	15.006695
24.270146	1435.182176	15.011712
24.488831	1439.488979	15.016730
24.645221	1430.033500	15.021747
24.143455	1429.695115	15.026765
24.232830	1429.603793	15.031783
24.576380	1438.899330	15.036800
24.205127	1444.821394	15.041818
24.674081	1453.371751	15.046835
24.650393	1472.197350	15.051853
24.713518	1465.179257	15.056871
24.734110	1469.759134	15.061888
24.498108	1468.618562	15.066906
25.055329	1460.185333	15.071923
24.781757	1470.495641	15.076941
24.754133	1470.705348	15.081959
24.605442	1462.630904	15.086976
24.726544	1459.942099	15.091994
25.342000	1457.904345	15.097011
24.866657	1470.372057	15.102029
25.243866	1463.082850	15.107047
24.947949	1454.404238	15.112064
24.861539	1451.509428	15.117082
25.105087	1452.559160	15.122099
24.686800	1453.546142	15.127117
25.053401	1454.955355	15.132135
25.032841	1464.124151	15.137152
25.098638	1462.890607	15.142170
25.256158	1456.639278	15.147187
24.874852	1466.730021	15.152205
25.239443	1458.894612	15.157223
25.260846	1462.246575	15.162240
24.970833	1454.454235	15.167258
25.033634	1454.071414	15.172275
25.054529	1459.421258	15.177293
24.875335	1464.381436	15.182311
24.998678	1475.503064	15.187328
25.340663	1463.820375	15.192346
25.302725	1462.452363	15.197363
25.191768	1469.713288	15.202381
25.376263	1463.146972	15.207399
25.414953	1468.573420	15.212416
25.317112	1462.105624	15.217434
25.392687	1463.262376	15.222451
25.226098	1465.099570	15.227469
25.287197	1470.982568	15.232487
25.410875	1463.161989	15.237504
25.273753	1467.053634	15.242522
25.466352	1459.269255	15.247539
25.502429	1482.172961	15.252557
25.636469	1463.568883	15.257575
25.467751	1466.173289	15.262592
25.343437	1475.237515	15.267610
25.727787	1468.190205	15.272627
25.434073	1463.546169	15.277645
25.825442	1472.902528	15.282663
25.774714	1472.476467	15.287680
25.653019	1461.596074	15.292698
25.484400	1471.424013	15.297715
25.448221	1474.762353	15.302733
25.523355	1477.816304	15.307751
25.494847	1476.907697	15.312768
25.632053	1480.543222	15.317786
26.126675	1478.476761	15.322803
25.756446	1481.612763	15.327821
26.133548	1485.549021	15.332839
25.993965	1489.481178	15.337856
25.892264	1486.403177	15.342874
26.393823	1481.201259	15.347891
26.250292	1492.342659	15.352909
26.170414	1484.468019	15.357927
26.233945	1482.980783	15.362944
26.042730	1482.799720	15.367962
26.011734	1481.972522	15.372979
26.120385	1482.173863	15.377997
26.201363	1478.831551	15.383015
26.434039	1480.379323	15.388032
26.047268	1482.768394	15.393050
26.072169	1482.050262	15.398067
25.760751	1489.480816	15.403085
26.164147	1481.843705	15.408103
26.390828	1477.728581	15.413120
25.796880	1490.463775	15.418138
26.210586	1489.328108	15.423155
26.102520	1490.979786	15.428173
26.103451	1488.479249	15.433191
26.180424	1477.686709	15.438208
26.066904	1482.685183	15.443226
26.267333	1470.413929	15.448243
25.702571	1486.859276	15.453261
26.038021	1499.829273	15.458279
26.413953	1511.684592	15.463296
26.573264	1511.326489	15.468314
26.257173	1513.546197	15.473331
26.777567	1524.050806	15.478349
26.858321	1514.904648	15.483367
26.802476	1518.545021	15.488384
26.618864	1519.132766	15.493402
26.976424	1514.584609	15.498419
26.810423	1511.840127	15.503437
27.055646	1512.813302	15.508455
27.126382	1505.326772	15.513472
26.773554	1509.130135	15.518490
26.831850	1509.429960	15.523507
26.971425	1514.395939	15.528525
26.913336	1503.001199	15.533543
26.677840	1490.027082	15.538560
27.023123	1501.622219	15.543578
27.178730	1488.440996	15.548595
26.715290	1484.093808	15.553613
26.824759	1490.430010	15.558631
26.896314	1497.678354	15.563648
26.764065	1507.701869	15.568666
27.245314	1501.324949	15.573683
27.110386	1506.803488	15.578701
27.208014	1508.959562	15.583719
27.189376	1505.386160	15.588736
27.239737	1510.334907	15.593754
27.255450	1506.331294	15.598771
27.230815	1493.407700	15.603789
27.014418	1496.968281	15.608807
27.319359	1491.033207	15.613824
27.215839	1495.625810	15.618842
27.365391	1497.764949	15.623859
27.197249	1503.180356	15.628877
27.232814	1510.883560	15.633895
27.459580	1501.725132	15.638912
27.375227	1511.689098	15.643930
27.401103	1505.806397	15.648947
27.583435	1503.751206	15.653965
27.423849	1503.576109	15.658983
27.330490	1505.064201	15.664000
27.335448	1518.585597	15.669018
27.648871	1509.631213	15.674035
27.638986	1507.542972	15.679053
27.546773	1506.064845	15.684071
27.794088	1501.413938	15.689088
27.418830	1512.161293	15.694106
27.568485	1505.541525	15.699123
27.632425	1505.893934	15.704141
27.439227	1517.318565	15.709159
27.631802	1510.805209	15.714176
27.439785	1516.752984	15.719194
27.549080	1508.605901	15.724211
27.678006	1513.730100	15.729229
27.410676	1513.346452	15.734247
27.502880	1511.431482	15.739264
27.510119	1514.121091	15.744282
27.447279	1509.924721	15.749299
27.653919	1522.658873	15.754317
27.490141	1541.123863	15.759335
27.779418	1529.428293	15.764352
27.581646	1540.407702	15.769370
27.909795	1538.639144	15.774387
28.066192	1541.470139	15.779405
28.065680	1538.697682	15.784423
28.325477	1534.799851	15.789440
28.027649	1541.296214	15.794458
28.184686	1541.927154	15.799475
28.307734	1535.065430	15.804493
28.067308	1540.619013	15.809511
28.372754	1535.151046	15.814528
28.227973	1538.350989	15.819546
28.271295	1544.133816	15.824563
28.387766	1542.321941	15.829581
28.272115	1548.087654	15.834599
28.399291	1538.658788	15.839616
28.227525	1544.646603	15.844634
28.391905	1537.839634	15.849651
28.521319	1538.539477	15.854669
28.440226	1539.875387	15.859687
28.369144	1535.876959	15.864704
28.362154	1538.004106	15.869722
28.564123	1536.924234	15.874739
28.377357	1531.227243	15.879757
28.247401	1543.918360	15.884775
28.408973	1537.679721	15.889792
28.209401	1547.698272	15.894810
28.690513	1567.345636	15.899827
28.959163	1564.783506	15.904845
28.359235	1571.814939	15.909863
28.731210	1566.324550	15.914880
28.895014	1571.452645	15.919898
28.816658	1569.871624	15.924915
28.770264	1562.877246	15.929933
28.975032	1569.847965	15.934951
29.111051	1570.372143	15.939968
29.004567	1567.164322	15.944986
28.814850	1554.875002	15.950003
28.922273	1552.024762	15.955021
28.625721	1559.043192	15.960039
28.792351	1561.117479	15.965056
28.899257	1573.798370	15.970074
28.812070	1579.452585	15.975091
28.847686	1567.414400	15.980109
28.600233	1571.323671	15.985127
28.996489	1568.373871	15.990144
28.897309	1573.763360	15.995162
29.076590	1567.731104	16.000179
29.049750	1563.065703	16.005197
28.687920	1564.523477	16.010215
29.030395	1566.862310	16.015232
29.359266	1587.355134	16.020250
29.238350	1593.724197	16.025267
29.587059	1589.077539	16.030285
29.364840	1596.536392	16.035303
29.271210	1587.370812	16.040320
29.405511	1594.186822	16.045338
29.591386	1594.141457	16.050355
29.655775	1583.983226	16.055373
29.396503	1575.072173	16.060391
29.354364	1559.172678	16.065408
29.319002	1569.876870	16.070426
29.393681	1588.369953	16.075443
29.691612	1585.691460	16.080461
29.695474	1597.185397	16.085479
29.861574	1592.692139	16.090496
29.573773	1593.821130	16.095514
29.775749	1596.420702	16.100531
29.842119	1588.176598	16.105549
29.983110	1597.145883	16.110567
29.694178	1581.553940	16.115584
29.720899	1576.849316	16.120602
29.492040	1575.933333	16.125619
29.885806	1579.219636	16.130637
29.560610	1591.534508	16.135655
29.739073	1589.201486	16.140672
29.962036	1595.644691	16.145690
29.978256	1594.560621	16.150707
29.939253	1588.657560	16.155725
29.715035	1594.229029	16.160743
29.843014	1592.187214	16.165760
29.957442	1592.243698	16.170778
30.163667	1589.635677	16.175795
30.185066	1583.162178	16.180813
29.694068	1595.972280	16.185831
29.900216	1582.417955	16.190848
30.003807	1591.519836	16.195866
29.996199	1594.583076	16.200883
30.364767	1609.010859	16.205901
30.240179	1625.858076	16.210919
30.354327	1628.795719	16.215936
30.380486	1633.546226	16.220954
30.198312	1624.574079	16.225971
30.585154	1629.749991	16.230989
30.161932	1629.585483	16.236007
30.546140	1622.774872	16.241024
30.563656	1633.247298	16.246042
30.252512	1631.643625	16.251059
30.724748	1625.420679	16.256077
30.330549	1624.297462	16.261095
30.591175	1622.836978	16.266112
30.529962	1619.860247	16.271130
30.787301	1614.778252	16.276147
30.533840	1609.349068	16.281165
30.562420	1623.949079	16.286183
30.529754	1614.590493	16.291200
30.755721	1621.399759	16.296218
30.660386	1623.419883	16.301235
30.663282	1610.568875	16.306253
30.610314	1618.451432	16.311271
30.740719	1623.796453	16.316288
30.903860	1636.078302	16.321306
30.515147	1632.786491	16.326323
30.772295	1627.993183	16.331341
30.628211	1643.653488	16.336359
30.938191	1643.615857	16.341376
31.400638	1644.854066	16.346394
31.071800	1636.872756	16.351411
31.238915	1635.759109	16.356429
31.141444	1644.701963	16.361447
31.009078	1638.920744	16.366464
31.123302	1646.661026	16.371482
31.088726	1642.653599	16.376499
31.415549	1639.219337	16.381517
31.260891	1648.776956	16.386535
31.268191	1637.856978	16.391552
31.570056	1632.910239	16.396570
31.322530	1635.692420	16.401587
31.522027	1633.448061	16.406605
31.660619	1634.993554	16.411623
31.539597	1641.519963	16.416640
31.665877	1634.682060	16.421658
31.672638	1628.265148	16.426675
31.667556	1620.126808	16.431693
31.325703	1613.429655	16.436711
31.375865	1607.620906	16.441728
31.538976	1606.430032	16.446746
31.294940	1610.069770	16.451763
31.539931	1601.576149	16.456781
31.253513	1603.062797	16.461799
31.584755	1623.659906	16.466816
31.610263	1628.168259	16.471834
31.574267	1634.915494	16.476851
31.650363	1642.662642	16.481869
31.218302	1639.907088	16.486887
31.476158	1641.417828	16.491904
31.654882	1641.151011	16.496922
31.412577	1649.542006	16.501939
31.816119	1640.481928	16.506957
31.952013	1659.636261	16.511975
32.103491	1669.926103	16.516992
32.197476	1657.943816	16.522010
31.930248	1651.245753	16.527027
32.099111	1649.943842	16.532045
31.831158	1649.261402	16.537063
31.924707	1676.038638	16.542080
32.257060	1669.146611	16.547098
32.015601	1683.627726	16.552115
32.103496	1668.580438	16.557133
32.287143	1674.377115	16.562151
32.046422	1676.678424	16.567168
32.163327	1668.068335	16.572186
32.002695	1680.530073	16.577203
32.133550	1670.448487	16.582221
32.238872	1673.242822	16.587239
31.988157	1675.939785	16.592256
32.431708	1664.027582	16.597274
32.407350	1669.117295	16.602291
32.663628	1680.397209	16.607309
32.572345	1675.045956	16.612327
32.583087	1676.117895	16.617344
32.587092	1668.960477	16.622362
32.331818	1676.105305	16.627379
32.796603	1691.016494	16.632397
32.726978	1692.179121	16.637415
32.556248	1699.046981	16.642432
32.612832	1699.487090	16.647450
32.566868	1701.672390	16.652467
32.929550	1704.135444	16.657485
32.873618	1699.300812	16.662503
32.862337	1705.472316	16.667520
33.159870	1693.573941	16.672538
32.770891	1698.050112	16.677555
33.213068	1689.452624	16.682573
33.336988	1684.962920	16.687591
33.452969	1701.107219	16.692608
33.384710	1673.160269	16.697626
33.176400	1663.223239	16.702643
32.773670	1677.472871	16.707661
32.915160	1668.484464	16.712679
33.041639	1679.783508	16.717696
32.988779	1686.271536	16.722714
33.010090	1703.283555	16.727731
33.181225	1691.166234	16.732749
33.218050	1685.902300	16.737767
33.181744	1702.951825	16.742784
33.440895	1695.130750	16.747802
33.464112	1703.111318	16.752819
33.184157	1705.860143	16.757837
33.573439	1690.145746	16.762855
33.462245	1690.381370	16.767872
33.573095	1694.635448	16.772890
33.387654	1701.667685	16.777907
33.709558	1689.718234	16.782925
33.612594	1690.514757	16.787943
33.630564	1694.154411	16.792960
33.803586	1684.096765	16.797978
33.711405	1687.478695	16.802995
33.659400	1684.067881	16.808013
33.701237	1687.187751	16.813031
33.379758	1696.315025	16.818048
33.603251	1690.902546	16.823066
33.757925	1688.979948	16.828083
33.485463	1690.208751	16.833101
33.824377	1701.648541	16.838119
33.920287	1711.330622	16.843136
33.868517	1712.479391	16.848154
33.765911	1727.971928	16.853171
33.719041	1727.840986	16.858189
34.155654	1725.221362	16.863207
34.095017	1726.284240	16.868224
34.307034	1729.659345	16.873242
34.162805	1725.868383	16.878259
34.098401	1727.722344	16.883277
34.147579	1724.635957	16.888295
33.920342	1731.084176	16.893312
34.430955	1717.126428	16.898330
33.981563	1725.867477	16.903347
34.008736	1721.708600	16.908365
34.199205	1727.004751	16.913383
34.439666	1731.526830	16.918400
34.360511	1725.005597	16.923418
34.351838	1719.850373	16.928435
34.109198	1720.138427	16.933453
34.366007	1725.702435	16.938471
34.438020	1749.470754	16.943488
34.864024	1750.636918	16.948506
34.952658	1754.138681	16.953523
34.376212	1742.756430	16.958541
34.637443	1741.619898	16.963559
34.612130	1754.303158	16.968576
34.850896	1749.105310	16.973594
34.833492	1752.262173	16.978611
34.979137	1762.792910	16.983629
35.066480	1754.730206	16.988647
34.723518	1758.303172	16.993664
35.164036	1747.311652	16.998682
35.095417	1745.721193	17.003699
34.622093	1726.808584	17.008717
35.081783	1728.556926	17.013735
35.072345	1740.539972	17.018752
35.040083	1746.543372	17.023770
34.846138	1751.709717	17.028787
35.108276	1745.513941	17.033805
35.139174	1743.084876	17.038823
34.988002	1753.500134	17.043840
35.159943	1741.395227	17.048858
35.166725	1754.611370	17.053875
35.087114	1754.925332	17.058893
35.486051	1746.713827	17.063911
35.267809	1750.591743	17.068928
35.555543	1749.861563	17.073946
35.381136	1753.690800	17.078963
35.104764	1754.693704	17.083981
35.479679	1733.716375	17.088999
34.998845	1739.700869	17.094016
35.319416	1750.670907	17.099034
35.537573	1748.430634	17.104051
35.386224	1745.594103	17.109069
35.860138	1763.897094	17.114087
35.618928	1786.594598	17.119104
35.790341	1771.603886	17.124122
35.774160	1779.052777	17.129139
35.528737	1784.782651	17.134157
35.912382	1780.077662	17.139175
35.679099	1785.848860	17.144192
35.993618	1772.805637	17.149210
36.126231	1777.273356	17.154227
35.838893	1782.597761	17.159245
35.967694	1787.923434	17.164263
35.957827	1779.660707	17.169280
36.193547	1774.165232	17.174298
36.059600	1789.206633	17.179315
35.889555	1786.426561	17.184333
36.098456	1778.548959	17.189351
35.935923	1793.884375	17.194368
36.000193	1772.847996	17.199386
36.142992	1781.547319	17.204403
36.243236	1782.208567	17.209421
36.517788	1779.330838	17.214439
36.227506	1784.197939	17.219456
35.970050	1779.888593	17.224474
36.044789	1776.176741	17.229491
35.862666	1779.405503	17.234509
36.402320	1785.368821	17.239527
36.428212	1796.671416	17.244544
36.238682	1809.892965	17.249562
36.797043	1809.640315	17.254579
36.655706	1800.233659	17.259597
36.734658	1793.825609	17.264615
36.762689	1804.344461	17.269632
36.762505	1798.618390	17.274650
36.599767	1804.430256	17.279667
36.547499	1805.104032	17.284685
36.739015	1803.901533	17.289703
36.646517	1808.991152	17.294720
36.511540	1804.698444	17.299738
36.858962	1797.113360	17.304755
36.780051	1791.450188	17.309773
37.152065	1800.686360	17.314791
36.869437	1806.245202	17.319808
36.651452	1799.896311	17.324826
36.731409	1806.714010	17.329843
36.861918	1827.889296	17.334861
36.908114	1820.719568	17.339879
37.166156	1836.714722	17.344896
37.324990	1823.577516	17.349914
37.549402	1833.990343	17.354931
37.685689	1827.976636	17.359949
37.608084	1832.624203	17.364967
37.530747	1823.344184	17.369984
37.638599	1819.854354	17.375002
37.287994	1795.665532	17.380019
37.087156	1814.957155	17.385037
37.568938	1802.912107	17.390055
37.713313	1825.203658	17.395072
37.474912	1823.975344	17.400090
37.720278	1829.680438	17.405107
37.401809	1826.858748	17.410125
37.641408	1826.551544	17.415143
37.871655	1835.498088	17.420160
37.877347	1833.158763	17.425178
37.817345	1828.342042	17.430195
37.355652	1842.184363	17.435213
37.826161	1832.472443	17.440231
37.687670	1833.501339	17.445248
37.830739	1831.962054	17.450266
37.876308	1828.199783	17.455283
37.686693	1831.714484	17.460301
38.029185	1830.376211	17.465319
37.749529	1830.199810	17.470336
37.580292	1836.025309	17.475354
37.879831	1822.333163	17.480371
37.702080	1848.432719	17.485389
38.244986	1844.563586	17.490407
38.466643	1867.756854	17.495424
38.079445	1855.989590	17.500442
38.453516	1864.573418	17.505459
38.148454	1857.414079	17.510477
38.224064	1860.986376	17.515495
38.233435	1862.906456	17.520512
38.377035	1860.562434	17.525530
38.684944	1855.085304	17.530547
38.544574	1857.730877	17.535565
38.639963	1853.460402	17.540583
38.447455	1853.982721	17.545600
38.284833	1852.241281	17.550618
38.597376	1856.950901	17.555635
38.553806	1856.735270	17.560653
38.723665	1849.020383	17.565671
38.316310	1853.044113	17.570688
38.416061	1858.142412	17.575706
38.939699	1861.348288	17.580723
38.763130	1873.363607	17.585741
39.143433	1884.798514	17.590759
39.433857	1878.776719	17.595776
39.082119	1868.587917	17.600794
38.763113	1855.513529	17.605811
38.825437	1852.177253	17.610829
38.991879	1857.014789	17.615847
39.235729	1879.768783	17.620864
39.489240	1866.992412	17.625882
39.111268	1852.304763	17.630899
38.711542	1864.433539	17.635917
39.240038	1867.655945	17.640935
39.581202	1867.106012	17.645952
39.483256	1876.759345	17.650970
39.477917	1873.927029	17.655987
39.498748	1886.751704	17.661005
39.796990	1867.657637	17.666023
39.265249	1849.963124	17.671040
39.316530	1854.753743	17.676058
40.004814	1854.325418	17.681075
39.495166	1852.319201	17.686093
39.329794	1847.368262	17.691111
39.409212	1850.089681	17.696128
39.424550	1868.779786	17.701146
39.658356	1871.110047	17.706163
39.337048	1867.665848	17.711181
39.722860	1867.069465	17.716199
39.623845	1877.112316	17.721216
39.481841	1878.546066	17.726234
39.750761	1869.463274	17.731251
39.654783	1879.821838	17.736269
39.629198	1884.312465	17.741287
39.998924	1884.736454	17.746304
39.841720	1896.907589	17.751322
40.087535	1895.792382	17.756339
40.187307	1909.464195	17.761357
39.959798	1904.017389	17.766375
40.281766	1899.368607	17.771392
40.321433	1899.634445	17.776410
40.603242	1900.523156	17.781427
40.474852	1902.222168	17.786445
40.166231	1900.448163	17.791463
39.963541	1897.956438	17.796480
40.014993	1902.489841	17.801498
40.219128	1895.696816	17.806515
39.884423	1906.403382	17.811533
40.150939	1928.004672	17.816551
40.428477	1929.219703	17.821568
40.302428	1935.975148	17.826586
40.874525	1927.227018	17.831603
40.652411	1932.041606	17.836621
40.718346	1934.297187	17.841639
40.864365	1931.979512	17.846656
40.802085	1930.610619	17.851674
41.043270	1930.368444	17.856691
41.037871	1926.397973	17.861709
40.611810	1930.483700	17.866727
40.850858	1932.249958	17.871744
40.959303	1934.011090	17.876762
41.168404	1929.528175	17.881779
40.701752	1932.429524	17.886797
40.735539	1931.771304	17.891815
41.273436	1940.428154	17.896832
41.082406	1952.225607	17.901850
41.354901	1953.709662	17.906867
41.223658	1951.125516	17.911885
41.211961	1956.697832	17.916903
41.702598	1955.840105	17.921920
41.477429	1948.073336	17.926938
41.301841	1931.557604	17.931955
41.683983	1946.362682	17.936973
41.217669	1943.832769	17.941991
41.428921	1941.007580	17.947008
41.749743	1947.934014	17.952026
41.813808	1954.253278	17.957043
41.741382	1947.362760	17.962061
41.702093	1951.720304	17.967079
41.880241	1940.057077	17.972096
41.665232	1943.936101	17.977114
41.866615	1946.233005	17.982131
41.968229	1944.824597	17.987149
41.746817	1946.113708	17.992167
42.318038	1941.159298	17.997184
42.094587	1934.476144	18.002202
42.007729	1919.952005	18.007219
41.792473	1919.288674	18.012237
42.068579	1939.885588	18.017255
42.066689	1933.056190	18.022272
41.823243	1940.690074	18.027290
42.200155	1942.527158	18.032307
42.070322	1946.409114	18.037325
41.864286	1942.837965	18.042343
42.265019	1939.311617	18.047360
41.932135	1948.480981	18.052378
42.493618	1941.074051	18.057395
42.392941	1948.717416	18.062413
42.284468	1954.652041	18.067431
42.453551	1946.891606	18.072448
41.888767	1964.495308	18.077466
42.515002	1981.893329	18.082483
42.407930	1974.643359	18.087501
42.551608	1980.792623	18.092519
42.551980	1980.368620	18.097536
42.833430	1983.038175	18.102554
42.204158	1974.207128	18.107571
42.275405	1979.477555	18.112589
42.683254	1993.440890	18.117607
43.108913	1996.399712	18.122624
43.363582	2005.233133	18.127642
43.289489	1997.178741	18.132659
43.332162	1974.454401	18.137677
43.224496	1984.081827	18.142695
43.361798	1977.767429	18.147712
43.298753	1970.181655	18.152730
43.319185	1968.864064	18.157747
43.452348	1974.967809	18.162765
43.375680	1972.044597	18.167783
43.624924	1969.432008	18.172800
43.137459	1968.209585	18.177818
43.426333	1967.007276	18.182835
43.387517	1968.189394	18.187853
43.091993	1983.434529	18.192871
43.269533	1975.153597	18.197888
43.019786	1983.726879	18.202906
43.080505	1982.823672	18.207923
43.258328	2001.155314	18.212941
43.149327	1999.284959	18.217959
43.229396	1994.876091	18.222976
43.244939	2015.716034	18.227994
43.585820	2022.986180	18.233011
43.791278	2031.404294	18.238029
43.772396	2038.027854	18.243047
44.329847	2035.514754	18.248064
44.140524	2043.490081	18.253082
44.208276	2030.703868	18.258099
44.072997	2026.855553	18.263117
44.118447	2029.422750	18.268135
44.282632	2022.941227	18.273152
44.093278	2014.984652	18.278170
44.055171	2023.695671	18.283187
44.289620	2031.210902	18.288205
44.058689	2033.396652	18.293223
44.085028	2032.961427	18.298240
43.901222	2030.119790	18.303258
44.255944	2031.170712	18.308275
44.559105	2035.366686	18.313293
44.446565	2032.711897	18.318311
44.651120	2028.980062	18.323328
44.499049	2032.135654	18.328346
44.587624	2030.819773	18.333363
44.634249	2024.232723	18.338381
44.539306	2024.413846	18.343399
44.640997	2019.204731	18.348416
44.665813	2027.223764	18.353434
44.763020	2037.412404	18.358451
44.984543	2041.160473	18.363469
44.993306	2058.751463	18.368487
45.134234	2043.258785	18.373504
45.057881	2042.316086	18.378522
45.035252	2050.930265	18.383539
45.283419	2043.807655	18.388557
45.178189	2046.053587	18.393575
45.405167	2030.474833	18.398592
45.068169	2027.427954	18.403610
45.246913	2024.700749	18.408627
45.298146	2029.569304	18.413645
45.048647	2043.906543	18.418663
45.515816	2036.836315	18.423680
45.596851	2039.571670	18.428698
45.086242	2046.364120	18.433715
45.243995	2044.713138	18.438733
45.189967	2045.588567	18.443751
45.574407	2049.554489	18.448768
45.621487	2043.506943	18.453786
45.457014	2045.786707	18.458803
45.805763	2049.747309	18.463821
45.495196	2044.756535	18.468839
45.337394	2043.074868	18.473856
45.965795	2051.070005	18.478874
45.368966	2054.517567	18.483891
45.583400	2061.633284	18.488909
45.563937	2077.741399	18.493927
45.650199	2075.013991	18.498944
45.741468	2080.680051	18.503962
45.797678	2082.924621	18.508979
46.026202	2080.983115	18.513997
46.229394	2084.237794	18.519015
46.087248	2083.416492	18.524032
46.462733	2096.038482	18.529050
46.419612	2098.824328	18.534067
46.758632	2108.926468	18.539085
46.247319	2095.882535	18.544103
46.551434	2085.120175	18.549120
46.453977	2086.650667	18.554138
46.383380	2089.276500	18.559155
46.730876	2100.056879	18.564173
46.593056	2107.430165	18.569191
46.771999	2108.092247	18.574208
46.884320	2112.591624	18.579226
46.679474	2104.747591	18.584243
46.919628	2104.854816	18.589261
46.565476	2114.271512	18.594279
46.630626	2110.345585	18.599296
46.762200	2116.404022	18.604314
46.893327	2114.534679	18.609331
46.564730	2109.815765	18.614349
46.368895	2112.902844	18.619367
46.910526	2115.937583	18.624384
47.011430	2137.736287	18.629402
46.831329	2140.337120	18.634419
47.192837	2140.952780	18.639437
47.200111	2138.676080	18.644455
47.313720	2136.307696	18.649472
47.257845	2131.376162	18.654490
47.445604	2139.578495	18.659507
47.352304	2124.975735	18.664525
46.823301	2137.502123	18.669543
47.218966	2134.301392	18.674560
47.481853	2147.904151	18.679578
47.576674	2164.170325	18.684595
47.747483	2166.096158	18.689613
47.661696	2162.235193	18.694631
47.788698	2155.555033	18.699648
47.960145	2163.889766	18.704666
47.855868	2162.230224	18.709683
47.924907	2157.330672	18.714701
48.023838	2166.140264	18.719719
48.233146	2161.361494	18.724736
48.394658	2150.333159	18.729754
47.998556	2155.698643	18.734771
48.323150	2158.163920	18.739789
48.381696	2150.725411	18.744807
48.235318	2142.791802	18.749824
48.209478	2132.915801	18.754842
48.281987	2149.799831	18.759859
48.602279	2144.033520	18.764877
48.280543	2154.726399	18.769895
48.172520	2153.826499	18.774912
48.191770	2149.382451	18.779930
48.084902	2157.796181	18.784947
48.172222	2149.781245	18.789965
48.556933	2152.121306	18.794983
48.606166	2155.104806	18.800000
48.687678	2149.743908	18.805018
48.153043	2154.816858	18.810035
48.601758	2157.285935	18.815053
48.954102	2182.856337	18.820071
48.952187	2192.043855	18.825088
49.122884	2186.766254	18.830106
48.965782	2185.245706	18.835123
48.852630	2181.054020	18.840141
49.122504	2185.304115	18.845159
48.983190	2192.479466	18.850176
49.319521	2179.623540	18.855194
48.791668	2184.249431	18.860211
49.128527	2184.113912	18.865229
49.104157	2178.155577	18.870247
48.956456	2186.976204	18.875264
49.270852	2187.688263	18.880282
49.419543	2204.690777	18.885299
49.483722	2209.613961	18.890317
49.594997	2214.473001	18.895335
49.394374	2208.828293	18.900352
49.667622	2209.197678	18.905370
49.243204	2216.897539	18.910387
49.436990	2201.222429	18.915405
49.494878	2211.988517	18.920423
49.219902	2215.748178	18.925440
49.914558	2230.327508	18.930458
50.020483	2243.293093	18.935475
49.953629	2240.243983	18.940493
49.941983	2246.966379	18.945511
50.004248	2233.893762	18.950528
50.117230	2242.313377	18.955546
49.777432	2248.407723	18.960563
50.459717	2242.399577	18.965581
50.088070	2242.663380	18.970599
50.109525	2243.485093	18.975616
50.539716	2235.925911	18.980634
50.221568	2239.946528	18.985651
50.353033	2238.799195	18.990669
50.320007	2241.039932	18.995687
50.338375	2236.703759	19.000704
50.618823	2239.688154	19.005722
50.515146	2240.805127	19.010739
50.331658	2244.842810	19.015757
50.555336	2262.548431	19.020775
50.503230	2267.884258	19.025792
50.654052	2264.451968	19.030810
50.664190	2267.670622	19.035827
50.989810	2269.820336	19.040845
51.138003	2262.995949	19.045863
51.015672	2269.021009	19.050880
51.223137	2270.729420	19.055898
50.938597	2266.847428	19.060915
50.958265	2258.083387	19.065933
51.343738	2265.427561	19.070951
51.210143	2262.704509	19.075968
51.397970	2262.208911	19.080986
51.083937	2263.677216	19.086003
51.391707	2268.290984	19.091021
51.113488	2264.665195	19.096039
51.158907	2283.262937	19.101056
51.766125	2292.666420	19.106074
51.757188	2305.117866	19.111091
52.085089	2291.523801	19.116109
51.981831	2278.482265	19.121127
51.498483	2261.142142	19.126144
51.850324	2265.358737	19.131162
51.876672	2277.205944	19.136179
52.020670	2282.885697	19.141197
52.271941	2285.830707	19.146215
51.920686	2266.252926	19.151232
52.138979	2261.391673	19.156250
52.110094	2285.629244	19.161267
52.233334	2280.966419	19.166285
52.458079	2288.456588	19.171303
51.868635	2275.752958	19.176320
52.492202	2271.453965	19.181338
52.300123	2279.898661	19.186355
52.144241	2288.817403	19.191373
52.287158	2285.073310	19.196391
52.249488	2284.514569	19.201408
52.260668	2273.860933	19.206426
51.992917	2291.249321	19.211443
52.130050	2282.746553	19.216461
52.630388	2286.920591	19.221479
52.495453	2299.747663	19.226496
52.666498	2296.408890	19.231514
52.801825	2301.706968	19.236531
52.816583	2297.925107	19.241549
53.078927	2296.387201	19.246567
53.077342	2298.929699	19.251584
53.157654	2292.932596	19.256602
53.061066	2302.972205	19.261619
53.019838	2301.658912	19.266637
53.382634	2292.972268	19.271655
53.122275	2297.927580	19.276672
53.309647	2300.583884	19.281690
53.090412	2297.316012	19.286707
53.113684	2295.385192	19.291725
53.220739	2295.578935	19.296743
52.996789	2300.685758	19.301760
53.581117	2311.593702	19.306778
53.677862	2328.640042	19.311795
53.731756	2336.856759	19.316813
53.632888	2329.454279	19.321831
53.503097	2339.402459	19.326848
53.633304	2343.855793	19.331866
53.653303	2334.591386	19.336883
53.731174	2329.834313	19.341901
53.775654	2337.564063	19.346919
53.678948	2335.490337	19.351936
53.730745	2328.446893	19.356954
53.696011	2325.897628	19.361971
53.873464	2344.812619	19.366989
54.137141	2358.467364	19.372007
54.089086	2367.497169	19.377024
54.159824	2361.257724	19.382042
54.101916	2361.860059	19.387059
54.233871	2362.436045	19.392077
54.549624	2357.423137	19.397095
54.485075	2355.794992	19.402112
54.475143	2358.691221	19.407130
54.596360	2369.390691	19.412147
54.472030	2364.917564	19.417165
54.924674	2359.008926	19.422183
54.734745	2359.275209	19.427200
54.895131	2351.192661	19.432218
54.824779	2355.899017	19.437235
55.103898	2352.307019	19.442253
55.055779	2355.287209	19.447271
54.731594	2367.208491	19.452288
55.232509	2368.065433	19.457306
55.464127	2379.899649	19.462323
55.227270	2363.990216	19.467341
55.289121	2369.985941	19.472359
55.408608	2382.078738	19.477376
55.260922	2373.655954	19.482394
55.364183	2373.456225	19.487411
55.246396	2393.487339	19.492429
55.839697	2380.981972	19.497447
55.496346	2396.125042	19.502464
55.541879	2383.820308	19.507482
55.521725	2387.453631	19.512499
55.588421	2389.796473	19.517517
55.678355	2386.432861	19.522535
55.500452	2395.520362	19.527552
55.969104	2389.948964	19.532570
55.740100	2391.642055	19.537587
55.720810	2391.505920	19.542605
55.749567	2388.641322	19.547623
55.402745	2393.062993	19.552640
55.869108	2411.855692	19.557658
56.039269	2418.468151	19.562675
55.763090	2414.193850	19.567693
55.740635	2417.626181	19.572711
56.086505	2413.697874	19.577728
56.099643	2416.058702	19.582746
56.434127	2424.468264	19.587763
56.254449	2438.701148	19.592781
56.526007	2444.111270	19.597799
56.478802	2439.559745	19.602816
56.808680	2443.885299	19.607834
57.118635	2441.519372	19.612851
56.406992	2447.983025	19.617869
57.075403	2433.546356	19.622887
56.929214	2438.833538	19.627904
56.810828	2433.955134	19.632922
57.116033	2441.244555	19.637939
57.026653	2444.048070	19.642957
57.326150	2430.485151	19.647975
57.030977	2435.318635	19.652992
56.941826	2425.481638	19.658010
57.184287	2431.955144	19.663027
57.044558	2440.975231	19.668045
57.440582	2428.672765	19.673063
57.108758	2437.407280	19.678080
57.482182	2433.532781	19.683098
57.322369	2433.645597	19.688115
57.291851	2454.210340	19.693133
57.610879	2450.393281	19.698151
57.906513	2464.811528	19.703168
57.783184	2461.275040	19.708186
57.892309	2464.485814	19.713203
57.488084	2472.283270	19.718221
57.623537	2462.647189	19.723239
57.885704	2461.391681	19.728256
57.905429	2461.148640	19.733274
58.022133	2459.022766	19.738291
57.985833	2463.761482	19.743309
58.193933	2455.919829	19.748327
58.029058	2462.471689	19.753344
58.127472	2483.141764	19.758362
58.460540	2485.097609	19.763379
58.072232	2506.882861	19.768397
58.695356	2498.382687	19.773415
58.599851	2498.170609	19.778432
58.690321	2491.539385	19.783450
58.638289	2486.924114	19.788467
58.616215	2492.237142	19.793485
58.641872	2494.068969	19.798503
58.889010	2495.920533	19.803520
58.794257	2487.193482	19.808538
58.749743	2479.791696	19.813555
58.847551	2494.003973	19.818573
58.977554	2495.086054	19.823591
58.800081	2492.450976	19.828608
58.786881	2490.464593	19.833626
58.790317	2494.002935	19.838643
58.972888	2506.403556	19.843661
59.074688	2512.109008	19.848679
59.201344	2513.345797	19.853696
59.360503	2512.047719	19.858714
59.352025	2516.428048	19.863731
59.270209	2518.831568	19.868749
59.330668	2512.187816	19.873767
59.345090	2515.063673	19.878784
59.434970	2533.912645	19.883802
59.754690	2538.888001	19.888819
59.458184	2549.421396	19.893837
60.064136	2543.591277	19.898855
60.288415	2543.203127	19.903872
60.212212	2544.476993	19.908890
60.243972	2534.604119	19.913907
60.044748	2548.940911	19.918925
60.287953	2534.628597	19.923943
60.208589	2539.461518	19.928960
60.241334	2544.077551	19.933978
60.377673	2542.937283	19.938995
60.094025	2540.132708	19.944013
60.159698	2546.487369	19.949031
60.583048	2539.510417	19.954048
60.287187	2545.373698	19.959066
60.729419	2540.519899	19.964083
60.097984	2537.293332	19.969101
60.253872	2554.475236	19.974119
60.628648	2565.775484	19.979136
60.721683	2565.094414	19.984154
61.063277	2573.812847	19.989171
60.817642	2568.728155	19.994189
61.325949	2574.401045	19.999207
61.385880	2573.477477	20.004224
60.758080	2578.259442	20.009242
61.383191	2563.079928	20.014259
61.251901	2566.683825	20.019277
61.328160	2565.605053	20.024295
61.400644	2560.412990	20.029312
61.210515	2569.573343	20.034330
61.078139	2560.070373	20.039347
61.197457	2567.510641	20.044365
61.632373	2582.350430	20.049383
61.788320	2583.465350	20.054400
61.829527	2590.013502	20.059418
62.291117	2584.110428	20.064435
62.007402	2586.318047	20.069453
61.680315	2570.648533	20.074471
61.958685	2580.506607	20.079488
61.977143	2584.641961	20.084506
62.269618	2594.027409	20.089523
62.067239	2595.931804	20.094541
62.293011	2589.597527	20.099559
62.595318	2596.380920	20.104576
62.133135	2599.771731	20.109594
62.401897	2587.309300	20.114611
62.224545	2590.631082	20.119629
62.164932	2583.977344	20.124647
62.415953	2587.331487	20.129664
62.170660	2597.705721	20.134682
62.302889	2590.502229	20.139699
61.957026	2592.216340	20.144717
62.292118	2604.644634	20.149735
62.297889	2613.250682	20.154752
62.167600	2620.254110	20.159770
62.700446	2620.717398	20.164787
62.524491	2639.132226	20.169805
62.886497	2643.975018	20.174823
63.135221	2650.811033	20.179840
63.195455	2654.345074	20.184858
63.154480	2645.267181	20.189875
63.242949	2653.966253	20.194893
63.449510	2648.468025	20.199911
63.483816	2640.885253	20.204928
63.246447	2652.774040	20.209946
63.469120	2640.074283	20.214963
63.747407	2643.917288	20.219981
63.751953	2645.775312	20.224999
63.967065	2645.762256	20.230016
63.946954	2654.245814	20.235034
64.020200	2639.295828	20.240051
63.763773	2653.012566	20.245069
63.786780	2647.798473	20.250087
64.253658	2658.481567	20.255104
63.972222	2668.293691	20.260122
64.120029	2670.681064	20.265139
63.962600	2661.023917	20.270157
64.106606	2676.547347	20.275175
64.364659	2675.399455	20.280192
64.356924	2678.654088	20.285210
64.455497	2669.585386	20.290227
64.014392	2684.057640	20.295245
64.105792	2679.709688	20.300263
64.660082	2683.345856	20.305280
64.816207	2689.113507	20.310298
65.301854	2694.721626	20.315315
65.179870	2701.430365	20.320333
65.037345	2688.858033	20.325351
65.182362	2684.411855	20.330368
64.861666	2691.009121	20.335386
65.040357	2690.862646	20.340403
65.310774	2695.569822	20.345421
65.368589	2694.166756	20.350439
65.432735	2697.922793	20.355456
65.324444	2699.864896	20.360474
65.497355	2696.181990	20.365491
65.167920	2692.661800	20.370509
65.471360	2694.051327	20.375527
65.814837	2687.641600	20.380544
65.400442	2688.682308	20.385562
65.693811	2684.431931	20.390579
65.730081	2686.168484	20.395597
65.569885	2691.763979	20.400615
65.583545	2689.646642	20.405632
65.489046	2690.362591	20.410650
65.897392	2698.766825	20.415667
65.929477	2704.385146	20.420685
65.792155	2710.974413	20.425703
65.901655	2717.315865	20.430720
65.640478	2714.867149	20.435738
65.990342	2708.615288	20.440755
66.438231	2722.264594	20.445773
66.353772	2739.730471	20.450791
66.870736	2722.485899	20.455808
66.855657	2731.949594	20.460826
67.106284	2723.619613	20.465843
67.311874	2719.601903	20.470861
66.931997	2703.987073	20.475879
66.816088	2701.489232	20.480896
66.773640	2700.788074	20.485914
66.924653	2682.342565	20.490931
67.371292	2717.560702	20.495949
66.835905	2712.593753	20.500967
67.236908	2718.606323	20.505984
67.148276	2725.183897	20.511002
67.209308	2736.117417	20.516019
67.435736	2737.408321	20.521037
67.437849	2740.493063	20.526055
67.603860	2730.059034	20.531072
67.473095	2737.774471	20.536090
67.330208	2728.206993	20.541107
67.648865	2737.281583	20.546125
67.565624	2729.542886	20.551143
67.726041	2731.271443	20.556160
67.614753	2737.752738	20.561178
67.776154	2747.825445	20.566195
67.991762	2755.677579	20.571213
67.772428	2757.439176	20.576231
68.008154	2753.249102	20.581248
67.904159	2768.350447	20.586266
67.625821	2766.079872	20.591283
67.969679	2778.771217	20.596301
67.998576	2792.909037	20.601319
68.299089	2787.678165	20.606336
68.375598	2793.604077	20.611354
68.516007	2808.438366	20.616371
68.722986	2799.860443	20.621389
68.753664	2799.006028	20.626407
68.940407	2806.336553	20.631424
68.789528	2807.645950	20.636442
68.828572	2797.803201	20.641459
68.863614	2801.401078	20.646477
68.759526	2827.706163	20.651495
69.092137	2823.020786	20.656512
69.106622	2819.654163	20.661530
69.095504	2823.116245	20.666547
69.220693	2825.360155	20.671565
68.944210	2828.881867	20.676583
69.161360	2822.106005	20.681600
69.266807	2821.068970	20.686618
69.568081	2838.048674	20.691635
69.846762	2837.625095	20.696653
69.731530	2853.768218	20.701671
69.948529	2847.222846	20.706688
70.171302	2841.763651	20.711706
70.038065	2851.993548	20.716723
70.292880	2844.703518	20.721741
69.890120	2856.371066	20.726759
70.176743	2843.915795	20.731776
70.070150	2855.573863	20.736794
69.927278	2854.584296	20.741811
70.010118	2853.377810	20.746829
70.119613	2857.272964	20.751847
70.254176	2849.003115	20.756864
70.075085	2851.255442	20.761882
69.998540	2867.792008	20.766899
70.490085	2875.557720	20.771917
70.951966	2876.636456	20.776935
70.538817	2880.683409	20.781952
70.638799	2880.551059	20.786970
70.775037	2875.893052	20.791987
70.990152	2883.269433	20.797005
70.657607	2901.651357	20.802023
70.810527	2899.992399	20.807040
70.767024	2909.493780	20.812058
70.873688	2911.531419	20.817075
71.231124	2911.040215	20.822093
71.281193	2918.918052	20.827111
71.517979	2929.114160	20.832128
71.449978	2937.620465	20.837146
71.569800	2940.623546	20.842163
71.846948	2935.154071	20.847181
71.692635	2941.660409	20.852199
72.044352	2932.625113	20.857216
72.069361	2931.755862	20.862234
71.761634	2935.889063	20.867251
72.419452	2930.244031	20.872269
72.095747	2933.996698	20.877287
72.360719	2930.995993	20.882304
72.229201	2933.697768	20.887322
72.187200	2936.006118	20.892339
72.363392	2928.594861	20.897357
72.262680	2935.028145	20.902375
72.200739	2931.894724	20.907392
72.521580	2952.430875	20.912410
72.239028	2954.073572	20.917427
72.633293	2960.485346	20.922445
72.816132	2962.676032	20.927463
72.737533	2956.503416	20.932480
72.681973	2955.996271	20.937498
72.497600	2955.180866	20.942515
72.895686	2955.806466	20.947533
72.847322	2975.131147	20.952551
73.359412	2981.290514	20.957568
73.422631	2981.538456	20.962586
73.407389	2988.790374	20.967603
73.573439	2973.389460	20.972621
73.410777	2979.019281	20.977639
73.747202	2983.325862	20.982656
73.616773	2983.147664	20.987674
73.622532	2980.709032	20.992691
73.754944	2972.015469	20.997709
73.790015	2985.407564	21.002727
73.483520	2991.356098	21.007744
73.564465	2983.189119	21.012762
73.734583	3000.967109	21.017779
73.866178	3000.888713	21.022797
73.854123	3015.605150	21.027815
74.170154	3016.388578	21.032832
74.265240	3008.926501	21.037850
74.305402	3014.604222	21.042867
74.541441	3011.187274	21.047885
74.219024	3012.981860	21.052903
74.602496	3029.609644	21.057920
74.826465	3032.186305	21.062938
74.509598	3034.176663	21.067955
75.021147	3037.477561	21.072973
74.784961	3041.395646	21.077991
74.760849	3033.810188	21.083008
74.922554	3043.437038	21.088026
74.968131	3042.139725	21.093043
75.203683	3035.773806	21.098061
75.296715	3056.012909	21.103079
75.318054	3060.705653	21.108096
75.625100	3062.813616	21.113114
75.457499	3073.464484	21.118131
75.713977	3064.900538	21.123149
75.890062	3073.640951	21.128167
75.895569	3061.748715	21.133184
75.896524	3062.900979	21.138202
75.747209	3075.351085	21.143219
76.238684	3054.978645	21.148237
75.769900	3058.463431	21.153255
76.004513	3076.882551	21.158272
76.458606	3067.661721	21.163290
76.110528	3065.297599	21.168307
76.003986	3058.429303	21.173325
75.992877	3066.796030	21.178343
76.277224	3077.481015	21.183360
76.511937	3080.995985	21.188378
76.394732	3098.889143	21.193395
76.426154	3095.680226	21.198413
76.374703	3101.239653	21.203431
76.473159	3092.361859	21.208448
76.582710	3097.408686	21.213466
76.812838	3107.872647	21.218483
77.194862	3118.100001	21.223501
77.043028	3123.299439	21.228519
77.285114	3124.251992	21.233536
77.541041	3115.299512	21.238554
77.029165	3132.430486	21.243571
77.494663	3115.769473	21.248589
77.474262	3128.378414	21.253607
77.230892	3114.896726	21.258624
77.673623	3117.978924	21.263642
77.439590	3124.776523	21.268659
77.535826	3115.574979	21.273677
77.760206	3117.536449	21.278695
77.600579	3140.691080	21.283712
77.619229	3128.556773	21.288730
77.431926	3148.153202	21.293747
77.760497	3134.868184	21.298765
77.810874	3154.578533	21.303783
77.710091	3168.489610	21.308800
78.088739	3162.936213	21.313818
78.017363	3171.634343	21.318835
78.239363	3174.743890	21.323853
78.571275	3188.366507	21.328871
78.804931	3197.178049	21.333888
78.983637	3188.429777	21.338906
78.877669	3202.819984	21.343923
79.133017	3188.601066	21.348941
79.078118	3192.005715	21.353959
79.184382	3194.660174	21.358976
79.328303	3186.979401	21.363994
79.541452	3177.685229	21.369011
79.451937	3185.587045	21.374029
79.397627	3183.180772	21.379047
79.524765	3186.174871	21.384064
79.478050	3175.949872	21.389082
79.521362	3187.922546	21.394099
79.584527	3185.799601	21.399117
79.627775	3176.968319	21.404135
79.556851	3187.440233	21.409152
80.160618	3199.815175	21.414170
80.258436	3211.579371	21.419187
80.150570	3217.777931	21.424205
80.375973	3218.197456	21.429223
80.436137	3216.932413	21.434240
80.511818	3209.370280	21.439258
80.152404	3225.396216	21.444275
79.997949	3225.954987	21.449293
80.294278	3211.122232	21.454311
80.010912	3216.429997	21.459328
80.247791	3214.214840	21.464346
80.307732	3231.729856	21.469363
80.545870	3242.361762	21.474381
80.547585	3252.199124	21.479399
80.480861	3247.700018	21.484416
80.852729	3251.200235	21.489434
80.831947	3274.222018	21.494451
81.286949	3278.402007	21.499469
81.232942	3281.683032	21.504487
81.001960	3281.387926	21.509504
81.484015	3285.153767	21.514522
81.479832	3273.188962	21.519539
81.377787	3275.484915	21.524557
81.503099	3270.182700	21.529575
81.727147	3289.871040	21.534592
82.346959	3297.623604	21.539610
82.137059	3301.038838	21.544627
81.888327	3300.586875	21.549645
82.250913	3297.255875	21.554663
81.940770	3303.785652	21.559680
82.187073	3298.362655	21.564698
82.062485	3301.615609	21.569715
82.073062	3299.254819	21.574733
82.138839	3305.470560	21.579751
82.039330	3316.217727	21.584768
82.611649	3327.078799	21.589786
82.571863	3342.007659	21.594803
82.535481	3330.879417	21.599821
83.070577	3331.747495	21.604839
82.740305	3333.116227	21.609856
82.844890	3326.023766	21.614874
82.809523	3350.242108	21.619891
83.262363	3346.643405	21.624909
83.294494	3349.740007	21.629927
83.544243	3355.082366	21.634944
83.904742	3343.854633	21.639962
83.840847	3351.049985	21.644979
83.753220	3349.939869	21.649997
84.144588	3339.893465	21.655015
84.043456	3349.409042	21.660032
84.181383	3342.211353	21.665050
83.943542	3342.466411	21.670067
84.213642	3350.172514	21.675085
84.124018	3338.564256	21.680103
84.163449	3340.436472	21.685120
84.362607	3341.285757	21.690138
84.074681	3335.046462	21.695155
84.214067	3333.015177	21.700173
84.365199	3340.237588	21.705191
84.179258	3343.003968	21.710208
84.544443	3341.891647	21.715226
84.721730	3363.584816	21.720243
84.835567	3369.526249	21.725261
84.860582	3373.569531	21.730279
84.479989	3377.402965	21.735296
84.780795	3368.097053	21.740314
84.861595	3382.290882	21.745331
84.913086	3400.317976	21.750349
85.255530	3401.697422	21.755367
85.555255	3396.490061	21.760384
85.599684	3403.086049	21.765402
85.481728	3402.435445	21.770419
85.599097	3390.731202	21.775437
85.908573	3392.882878	21.780455
85.616141	3403.302956	21.785472
85.701744	3397.924431	21.790490
85.711874	3407.307451	21.795507
85.639719	3429.475512	21.800525
86.161182	3427.658603	21.805543
86.240330	3438.209025	21.810560
86.122889	3439.234672	21.815578
86.460869	3430.169011	21.820595
85.922426	3435.861298	21.825613
86.234398	3440.379590	21.830631
86.162537	3459.642579	21.835648
86.422826	3463.779733	21.840666
86.817167	3463.994541	21.845683
86.563601	3461.016644	21.850701
86.904580	3459.703648	21.855719
86.600302	3462.248211	21.860736
86.639256	3469.763902	21.865754
87.289754	3488.846433	21.870771
87.426109	3488.952925	21.875789
87.654402	3477.635257	21.880807
87.259396	3492.229173	21.885824
87.413797	3485.896457	21.890842
87.160095	3497.877421	21.895859
87.455310	3514.264962	21.900877
88.053495	3517.939186	21.905895
87.834532	3516.630529	21.910912
87.831662	3516.199919	21.915930
88.166832	3518.776239	21.920947
87.911803	3514.322029	21.925965
88.244859	3521.330653	21.930983
88.019980	3532.673798	21.936000
88.130687	3548.281343	21.941018
88.428618	3549.490907	21.946035
88.090354	3548.193407	21.951053
88.487124	3550.883413	21.956071
88.426034	3556.285646	21.961088
88.774446	3576.916610	21.966106
88.829047	3573.020294	21.971123
88.875360	3584.140872	21.976141
88.978987	3572.359224	21.981159
88.895255	3583.786882	21.986176
88.960531	3583.390241	21.991194
89.420986	3600.253408	21.996211
89.249201	3609.840993	22.001229
89.358975	3598.583041	22.006247
89.520696	3616.820950	22.011264
89.715766	3607.892037	22.016282
89.895193	3614.059105	22.021299
89.671540	3602.636423	22.026317
90.133923	3605.516571	22.031335
89.993704	3605.391844	22.036352
90.116293	3627.591292	22.041370
90.488822	3621.524230	22.046387
90.173149	3637.633316	22.051405
90.878632	3618.926712	22.056423
90.738065	3632.854013	22.061440
90.660850	3614.730860	22.066458
90.641148	3623.820635	22.071475
90.359615	3618.939533	22.076493
90.725801	3627.404525	22.081511
90.646855	3629.119447	22.086528
90.489203	3633.273744	22.091546
91.096345	3649.219936	22.096563
90.895364	3664.922153	22.101581
91.061419	3655.694190	22.106599
91.313163	3662.954994	22.111616
91.110624	3658.885695	22.116634
91.360903	3664.678050	22.121651
91.601922	3688.190507	22.126669
91.819478	3685.773832	22.131687
91.749366	3690.087249	22.136704
91.964911	3687.028196	22.141722
91.880952	3681.582212	22.146739
91.513187	3693.000973	22.151757
92.014416	3688.676256	22.156775
91.786387	3698.634730	22.161792
92.349360	3708.965014	22.166810
92.190962	3721.626365	22.171827
92.294962	3722.809446	22.176845
92.212315	3716.604114	22.181863
92.406944	3741.549479	22.186880
92.236594	3739.118353	22.191898
92.849852	3731.055650	22.196915
93.050049	3745.106496	22.201933
93.108311	3739.355397	22.206951
93.601938	3736.721621	22.211968
93.395355	3735.084506	22.216986
93.498402	3736.483285	22.222003
93.407555	3737.783188	22.227021
93.665949	3739.895078	22.232039
93.825530	3756.464214	22.237056
93.904008	3766.808874	22.242074
94.331483	3752.513976	22.247091
94.298608	3766.806545	22.252109
94.050940	3749.950972	22.257127
94.387597	3751.527254	22.262144
94.331476	3761.692779	22.267162
94.657110	3766.445779	22.272179
94.497945	3761.820445	22.277197
94.639485	3756.542214	22.282215
94.856473	3761.141835	22.287232
94.947555	3762.227074	22.292250
94.534939	3735.839910	22.297267
94.464803	3745.105361	22.302285
95.186900	3745.528290	22.307303
94.976899	3751.525458	22.312320
95.078213	3759.241390	22.317338
94.986194	3752.478223	22.322355
94.758018	3756.502990	22.327373
94.893002	3753.780876	22.332391
95.022936	3771.006896	22.337408
94.939725	3789.016618	22.342426
95.459815	3775.809039	22.347443
95.563187	3776.717681	22.352461
95.473005	3788.074940	22.357479
95.498102	3803.063934	22.362496
95.689460	3810.838693	22.367514
95.828905	3811.195640	22.372531
95.763229	3819.851550	22.377549
96.142607	3831.714515	22.382567
96.327947	3832.625034	22.387584
96.193772	3855.303160	22.392602
96.572446	3842.411501	22.397619
96.267362	3851.062344	22.402637
96.238625	3845.556358	22.407655
96.691865	3863.556138	22.412672
96.685909	3880.098320	22.417690
96.639244	3872.245412	22.422707
96.518509	3884.396643	22.427725
97.161559	3895.165836	22.432743
97.393838	3895.048567	22.437760
97.276132	3900.150008	22.442778
97.438567	3906.254616	22.447795
97.577121	3896.898728	22.452813
97.324698	3894.615972	22.457831
97.573112	3899.563838	22.462848
97.685867	3929.296076	22.467866
97.803211	3932.402025	22.472883
97.827728	3935.973540	22.477901
98.210551	3938.937245	22.482919
98.410988	3936.650700	22.487936
98.132465	3945.629337	22.492954
98.577373	3955.358730	22.497971
98.426673	3968.640535	22.502989
98.812473	3963.408237	22.508007
99.037590	3956.931093	22.513024
98.954706	3964.604135	22.518042
99.150255	3959.889915	22.523059
99.125828	3957.690362	22.528077
99.129128	3958.979203	22.533095
99.299907	3956.134130	22.538112
98.811702	3960.637023	22.543130
99.624364	3961.600120	22.548147
99.667878	3981.887732	22.553165
99.408970	3988.194877	22.558183
99.599485	3988.649098	22.563200
99.854039	3986.759052	22.568218
100.255112	3975.606183	22.573235
99.950256	3993.736463	22.578253
99.904450	3993.188393	22.583271
100.189512	3977.046071	22.588288
100.140907	3988.116799	22.593306
100.112606	3986.868158	22.598323
100.196317	4000.358050	22.603341
100.473371	4007.418321	22.608359
100.423719	4000.399694	22.613376
100.462488	4002.052618	22.618394
100.501029	4000.362221	22.623411
100.678298	4022.118515	22.628429
100.846371	4029.525007	22.633447
101.165295	4030.943667	22.638464
101.468441	4040.282722	22.643482
101.071891	4037.479336	22.648499
101.352531	4044.027714	22.653517
101.102017	4046.220023	22.658535
101.173268	4057.683906	22.663552
101.172870	4070.723924	22.668570
101.668432	4070.124128	22.673587
101.911348	4087.103578	22.678605
101.750639	4099.559513	22.683623
102.104453	4099.765066	22.688640
101.968920	4096.209672	22.693658
102.351884	4096.517564	22.698675
102.344271	4102.044417	22.703693
102.421166	4100.038727	22.708711
102.549957	4114.089515	22.713728
102.432892	4131.740036	22.718746
102.691166	4129.141367	22.723763
102.826461	4130.879607	22.728781
103.149847	4128.004657	22.733799
103.392692	4120.501932	22.738816
102.984288	4149.175470	22.743834
103.484805	4153.375206	22.748851
103.620977	4157.474924	22.753869
103.650213	4152.668377	22.758887
103.730068	4152.327611	22.763904
103.790965	4164.725446	22.768922
104.103017	4153.202741	22.773939
104.038305	4155.473209	22.778957
104.275732	4157.412289	22.783975
104.351134	4153.980577	22.788992
104.115022	4165.086061	22.794010
104.122062	4168.086142	22.799027
104.191730	4177.032991	22.804045
104.349444	4191.533942	22.809063
104.153493	4186.058429	22.814080
104.383106	4203.526306	22.819098
104.682378	4219.977712	22.824115
104.670813	4224.113597	22.829133
104.716189	4225.595569	22.834151
105.149171	4223.916191	22.839168
105.220455	4229.184277	22.844186
105.434641	4242.975337	22.849203
105.730981	4247.884999	22.854221
105.753357	4255.933175	22.859239
105.993140	4240.780358	22.864256
105.835483	4252.294272	22.869274
105.868689	4240.243261	22.874291
106.089333	4238.102918	22.879309
106.194406	4241.365867	22.884327
106.461693	4228.811818	22.889344
106.443178	4234.869112	22.894362
106.440410	4240.433792	22.899379
106.624655	4241.794497	22.904397
106.576008	4240.628535	22.909415
106.572868	4235.687881	22.914432
106.104273	4258.397932	22.919450
106.602078	4258.115594	22.924467
106.812459	4265.378574	22.929485
106.765361	4277.851942	22.934503
107.133678	4285.616826	22.939520
107.255581	4292.895504	22.944538
107.061009	4300.080691	22.949555
107.250104	4300.244075	22.954573
107.081938	4310.462462	22.959591
107.609640	4318.996502	22.964608
107.480424	4330.457166	22.969626
107.532824	4332.366775	22.974643
107.891328	4336.557745	22.979661
107.965075	4351.623715	22.984679
108.265862	4354.724100	22.989696
108.389014	4352.733814	22.994714
108.464046	4349.866174	22.999731
108.696441	4352.062543	23.004749
108.694760	4351.060582	23.009767
108.735283	4357.438921	23.014784
108.893182	4380.277389	23.019802
109.070550	4382.225290	23.024819
109.342930	4390.247832	23.029837
109.159520	4390.354978	23.034855
109.271287	4384.709166	23.039872
109.540857	4389.612131	23.044890
109.348759	4386.895648	23.049907
109.583278	4400.633266	23.054925
109.642839	4413.830018	23.059943
109.499751	4414.330375	23.064960
109.591574	4424.147072	23.069978
109.697454	4433.571332	23.074995
110.197831	4449.089371	23.080013
110.021927	4462.418121	23.085031
110.335854	4457.914581	23.090048
110.421037	4451.966170	23.095066
110.964580	4461.116112	23.100083
110.834496	4473.886090	23.105101
110.898378	4475.617666	23.110119
111.298098	4482.552401	23.115136
111.057138	4477.619698	23.120154
111.033188	4474.694656	23.125171
111.334414	4474.681248	23.130189
111.201174	4482.393270	23.135207
111.294294	4482.868548	23.140224
111.443231	4478.706779	23.145242
111.260048	4488.304618	23.150259
111.712187	4501.903781	23.155277
111.516581	4511.875725	23.160295
111.444647	4509.096001	23.165312
111.492462	4521.644122	23.170330
112.027566	4530.059101	23.175347
112.488685	4525.137930	23.180365
112.126917	4539.681161	23.185383
112.422810	4551.440806	23.190400
112.641233	4563.749346	23.195418
112.436985	4568.367623	23.200435
113.251489	4562.977851	23.205453
113.474026	4570.285461	23.210471
113.614078	4558.683665	23.215488
113.151394	4560.102727	23.220506
113.433449	4559.628222	23.225523
113.759621	4552.571425	23.230541
113.616320	4559.537726	23.235559
113.459744	4565.710003	23.240576
113.774319	4570.074828	23.245594
113.838170	4580.464876	23.250611
114.029281	4582.506591	23.255629
113.772589	4592.794358	23.260647
113.722813	4585.954053	23.265664
114.409242	4597.538170	23.270682
114.225763	4617.416009	23.275699
114.634736	4615.266035	23.280717
114.446083	4620.846342	23.285735
114.694513	4625.820414	23.290752
114.612686	4634.337771	23.295770
114.721836	4642.503701	23.300787
114.961785	4646.798632	23.305805
115.232715	4658.267328	23.310823
115.222799	4656.214044	23.315840
115.406106	4668.853970	23.320858
115.349841	4685.373610	23.325875
115.678407	4684.535306	23.330893
115.530936	4692.897169	23.335911
115.280423	4687.667755	23.340928
115.417074	4711.967111	23.345946
115.814096	4711.943934	23.350963
116.094294	4724.130258	23.355981
116.286796	4744.976541	23.360999
116.775116	4746.827701	23.366016
116.993060	4735.277069	23.371034
117.443101	4729.948509	23.376051
117.922319	4720.999573	23.381069
118.030686	4708.218714	23.386087
118.046751	4691.397097	23.391104
118.185280	4683.339573	23.396122
118.195708	4673.828190	23.401139
118.086077	4662.978888	23.406157
117.877605	4655.535278	23.411175
118.179628	4644.498403	23.416192
118.126652	4637.586993	23.421210
117.947943	4645.310285	23.426227
118.286691	4645.043082	23.431245
117.963556	4641.611876	23.436263
118.149887	4644.756539	23.441280
118.129041	4662.953273	23.446298
118.129334	4673.718555	23.451315
118.076297	4673.048099	23.456333
118.113748	4681.625919	23.461351
117.879526	4694.750980	23.466368
118.142443	4708.529987	23.471386
117.969774	4729.239379	23.476403
118.734941	4735.932654	23.481421
118.838695	4752.279737	23.486439
118.754731	4772.640690	23.491456
119.157475	4775.030239	23.496474
119.228538	4784.335190	23.501491
119.435705	4786.660737	23.506509
119.204439	4807.601437	23.511527
119.568332	4807.364837	23.516544
119.879514	4818.123130	23.521562
119.950910	4842.913006	23.526579
120.422715	4839.060751	23.531597
120.189934	4837.697531	23.536615
120.413326	4846.187578	23.541632
120.517313	4848.653891	23.546650
120.514686	4872.453343	23.551667
120.459658	4869.877761	23.556685
120.484018	4889.681912	23.561703
120.931050	4901.230497	23.566720
121.197829	4904.248312	23.571738
121.263943	4912.444856	23.576755
121.429360	4906.698243	23.581773
121.494713	4913.588953	23.586791
121.630872	4925.116327	23.591808
121.728056	4926.823764	23.596826
122.041222	4935.813276	23.601843
122.061015	4931.792344	23.606861
121.882559	4935.435019	23.611879
122.250185	4948.002522	23.616896
122.404072	4960.958145	23.621914
122.089389	4975.452597	23.626931
122.297078	4964.694081	23.631949
122.373764	4975.322311	23.636967
122.575941	4990.134797	23.641984
123.149011	4992.750547	23.647002
123.021465	4988.129222	23.652019
123.563146	4979.271659	23.657037
123.605815	5000.854971	23.662055
123.767244	5014.685852	23.667072
123.977289	5001.591142	23.672090
123.701767	5018.241314	23.677107
124.131116	5009.861095	23.682125
124.224193	5009.184630	23.687143
124.493869	5006.593433	23.692160
124.645840	5006.466939	23.697178
124.438281	5008.694232	23.702195
124.725262	4993.412749	23.707213
124.776886	5006.348531	23.712231
124.521060	5001.763393	23.717248
124.798953	4995.331666	23.722266
124.734241	5007.427684	23.727283
124.826570	5018.953467	23.732301
124.931293	5016.621445	23.737319
125.086840	5039.365330	23.742336
125.325584	5033.217545	23.747354
125.086448	5045.158887	23.752371
125.417201	5060.722721	23.757389
125.804982	5068.595848	23.762407
125.590512	5071.452063	23.767424
125.955656	5076.727877	23.772442
126.056710	5094.713742	23.777459
126.193684	5097.635074	23.782477
126.132644	5099.245034	23.787495
126.283413	5110.783597	23.792512
126.340497	5117.907020	23.797530
126.129100	5129.633163	23.802547
126.706965	5132.388213	23.807565
126.588894	5157.683232	23.812583
126.554178	5162.455606	23.817600
126.969717	5166.404062	23.822618
126.944585	5180.024895	23.827635
127.367786	5190.815162	23.832653
127.291611	5193.219002	23.837671
127.325940	5215.140680	23.842688
127.915033	5216.881425	23.847706
128.229709	5221.146515	23.852723
128.311387	5220.525356	23.857741
128.641823	5215.673579	23.862759
128.678715	5217.724242	23.867776
128.769568	5222.881781	23.872794
128.923934	5248.653545	23.877811
129.120708	5244.609025	23.882829
129.131240	5250.930382	23.887847
129.206749	5248.589607	23.892864
129.344142	5255.800207	23.897882
129.252231	5252.523947	23.902899
129.104651	5247.498991	23.907917
129.464561	5259.490525	23.912935
129.490960	5271.289789	23.917952
129.907787	5268.381629	23.922970
130.010608	5277.546507	23.927987
129.805635	5281.992823	23.933005
130.118828	5292.201211	23.938023
130.280971	5302.502141	23.943040
130.734498	5299.341085	23.948058
130.678298	5308.374779	23.953075
130.428133	5307.493412	23.958093
130.778096	5296.431887	23.963111
130.968365	5312.086836	23.968128
131.280676	5316.257921	23.973146
131.289377	5330.273162	23.978163
131.224998	5328.330747	23.983181
131.554640	5325.921112	23.988199
131.671899	5331.662963	23.993216
131.742634	5323.026631	23.998234
131.802792	5327.956226	24.003251
131.936603	5345.517839	24.008269
132.300626	5351.289580	24.013287
131.919752	5361.489898	24.018304
132.467980	5355.069193	24.023322
132.382768	5365.009945	24.028339
132.552329	5364.075016	24.033357
133.029424	5362.117057	24.038375
133.217986	5376.673264	24.043392
133.100747	5377.330025	24.048410
132.985022	5378.152548	24.053427
133.076476	5373.794355	24.058445
133.615383	5365.513692	24.063463
133.203670	5390.454694	24.068480
133.646595	5395.992796	24.073498
134.166612	5400.344779	24.078515
133.819866	5395.729957	24.083533
133.786508	5404.591704	24.088551
134.161663	5409.494698	24.093568
134.712539	5407.684677	24.098586
134.428995	5416.775146	24.103603
134.989270	5419.177448	24.108621
135.095959	5415.107124	24.113639
135.037637	5417.513660	24.118656
135.148882	5401.621728	24.123674
135.305269	5407.124492	24.128691
135.241251	5430.460224	24.133709
135.555071	5432.359759	24.138727
135.679761	5442.837484	24.143744
135.856765	5450.312504	24.148762
135.656687	5449.788192	24.153779
135.467616	5455.956579	24.158797
135.853001	5458.895017	24.163815
135.972436	5471.185486	24.168832
135.972471	5473.732995	24.173850
136.463449	5481.508068	24.178867
136.397297	5501.926978	24.183885
136.668095	5505.053637	24.188903
136.882659	5518.353328	24.193920
136.727272	5515.303489	24.198938
137.195044	5528.724096	24.203955
136.983118	5546.146751	24.208973
137.607363	5538.973511	24.213991
137.354646	5548.088254	24.219008
137.041098	5555.890167	24.224026
137.340712	5567.020629	24.229043
137.378871	5584.375914	24.234061
137.779793	5577.313008	24.239079
137.766580	5598.703122	24.244096
137.858416	5599.921342	24.249114
138.074718	5610.590707	24.254131
138.279066	5625.842498	24.259149
138.834349	5624.761862	24.264167
138.789177	5626.923227	24.269184
139.102461	5619.806615	24.274202
139.323171	5638.561608	24.279219
139.207550	5656.437944	24.284237
139.422293	5665.783480	24.289255
139.064218	5666.010535	24.294272
139.716406	5671.865481	24.299290
139.555216	5680.064081	24.304307
139.469092	5695.070374	24.309325
139.950778	5698.493886	24.314343
140.091466	5714.260234	24.319360
140.231035	5728.031542	24.324378
140.255975	5732.206087	24.329395
140.496794	5735.255753	24.334413
140.741643	5739.581696	24.339431
140.792804	5759.379592	24.344448
140.993802	5767.412698	24.349466
141.418138	5761.792836	24.354483
140.814070	5766.940217	24.359501
141.079278	5774.860808	24.364519
141.492274	5783.963165	24.369536
141.373485	5789.417900	24.374554
141.820609	5798.475485	24.379571
142.279311	5818.284790	24.384589
142.824817	5820.974327	24.389607
142.941067	5822.109208	24.394624
143.192914	5817.068357	24.399642
143.156234	5813.740680	24.404659
142.476088	5822.207002	24.409677
142.947989	5815.872230	24.414695
143.313091	5811.444309	24.419712
143.290352	5811.595076	24.424730
143.592084	5817.077176	24.429747
143.553494	5835.094865	24.434765
143.800914	5839.222949	24.439783
143.737140	5843.733460	24.444800
143.500986	5836.347166	24.449818
144.012465	5848.775273	24.454835
144.164512	5864.559640	24.459853
144.367090	5855.446434	24.464871
144.346237	5874.881465	24.469888
144.076199	5877.009487	24.474906
144.799833	5884.129272	24.479923
144.705034	5892.593560	24.484941
144.746321	5897.832409	24.489959
144.889015	5903.188055	24.494976
144.957042	5926.957481	24.499994
145.137790	5934.930179	24.505011
145.019589	5939.487951	24.510029
145.441727	5954.439422	24.515047
145.952713	5961.477498	24.520064
145.798671	5968.674336	24.525082
146.385945	5964.685370	24.530099
146.254640	5973.104384	24.535117
146.326476	5986.183355	24.540135
146.252939	5996.874828	24.545152
146.357024	6001.685134	24.550170
146.482756	6001.990040	24.555187
146.239553	6031.107432	24.560205
146.701990	6035.442040	24.565223
146.803471	6035.587949	24.570240
146.831475	6058.493788	24.575258
147.535550	6060.829211	24.580275
147.388696	6086.655975	24.585293
147.932136	6086.356902	24.590311
147.771092	6099.238645	24.595328
148.023212	6097.488775	24.600346
148.303112	6109.003595	24.605363
148.203607	6125.825209	24.610381
148.628646	6120.404945	24.615399
148.873615	6120.881242	24.620416
148.846696	6129.824221	24.625434
149.198384	6137.135621	24.630451
149.094989	6147.547146	24.635469
149.399342	6149.079284	24.640487
149.318147	6147.997826	24.645504
149.269901	6170.801913	24.650522
149.830796	6168.670774	24.655539
149.742389	6179.747128	24.660557
149.784984	6174.395697	24.665575
150.020824	6196.087639	24.670592
150.046901	6204.694121	24.675610
150.745149	6209.733122	24.680627
150.641449	6220.606593	24.685645
150.904280	6226.008503	24.690663
151.053322	6226.676341	24.695680
151.230892	6235.788195	24.700698
151.522729	6229.227042	24.705715
151.710354	6240.327090	24.710733
151.438009	6238.545176	24.715751
151.908727	6252.504140	24.720768
151.963727	6259.113097	24.725786
152.139858	6261.793954	24.730803
152.273815	6269.327395	24.735821
152.337565	6267.599675	24.740839
152.295682	6288.143258	24.745856
152.427674	6301.114565	24.750874
152.753140	6290.352046	24.755891
152.925686	6305.848796	24.760909
152.873045	6318.087941	24.765927
153.319279	6317.484140	24.770944
152.985139	6320.753070	24.775962
153.359560	6325.621872	24.780979
153.130700	6348.982973	24.785997
153.364752	6348.790668	24.791015
153.841121	6359.117762	24.796032
153.851826	6367.641816	24.801050
154.166939	6379.952980	24.806067
154.052863	6391.779471	24.811085
154.050617	6399.014469	24.816103
154.734617	6410.911991	24.821120
154.605645	6425.626869	24.826138
154.603816	6418.696242	24.831155
154.622166	6430.398577	24.836173
155.013951	6450.792980	24.841191
155.456850	6452.792450	24.846208
155.291668	6468.240151	24.851226
155.634503	6480.378602	24.856243
155.734277	6489.272483	24.861261
155.673837	6487.492941	24.866279
156.225980	6498.664095	24.871296
156.361667	6513.424981	24.876314
156.575416	6513.249288	24.881331
156.403112	6512.420732	24.886349
156.903694	6536.517138	24.891367
157.602922	6536.437917	24.896384
157.225178	6549.168917	24.901402
157.502003	6549.381290	24.906419
157.693189	6541.565355	24.911437
157.591721	6547.818575	24.916455
157.749184	6552.962811	24.921472
157.729552	6571.776194	24.926490
158.404701	6574.970005	24.931507
158.130523	6575.945321	24.936525
158.243232	6576.316048	24.941543
158.446988	6598.665173	24.946560
158.293704	6607.152568	24.951578
158.395790	6607.624915	24.956595
158.617435	6633.627552	24.961613
158.992905	6635.700746	24.966631
159.160895	6650.732789	24.971648
159.080966	6662.485597	24.976666
159.301610	6667.861351	24.981683
159.368674	6680.801642	24.986701
159.806149	6693.502700	24.991719
160.412282	6695.481685	24.996736
160.439646	6697.220133	25.001754
160.736187	6708.169407	25.006771
160.954763	6727.754638	25.011789
160.674066	6731.216560	25.016807
161.001080	6721.830415	25.021824
160.927573	6727.542643	25.026842
161.328885	6743.373963	25.031859
161.287247	6753.699744	25.036877
161.535495	6761.548036	25.041895
161.777363	6759.377991	25.046912
161.766374	6776.168129	25.051930
162.007647	6782.281820	25.056947
162.384059	6791.554294	25.061965
162.175260	6791.877940	25.066983
162.723099	6789.928195	25.072000
162.267922	6789.550727	25.077018
162.753546	6804.359965	25.082035
162.954572	6808.712883	25.087053
162.988625	6808.928565	25.092071
163.393180	6817.394797	25.097088
163.250011	6840.074992	25.102106
163.311274	6848.274957	25.107123
163.483413	6843.495108	25.112141
163.609104	6854.959564	25.117159
163.790869	6857.740345	25.122176
163.828488	6872.239477	25.127194
164.236695	6887.478946	25.132211
164.569048	6895.851302	25.137229
164.391974	6905.925754	25.142247
164.994142	6911.484679	25.147264
164.997252	6933.979606	25.152282
165.373479	6930.013028	25.157299
165.546845	6929.529039	25.162317
165.435472	6938.478889	25.167335
165.843378	6939.417856	25.172352
165.972971	6958.507715	25.177370
166.475687	6953.592503	25.182387
166.548820	6958.573291	25.187405
166.603654	6954.370760	25.192423
166.850127	6947.699290	25.197440
166.784804	6966.843058	25.202458
166.899789	6974.849622	25.207475
167.340583	6976.408091	25.212493
167.536766	6978.266792	25.217511
167.658470	6977.324448	25.222528
167.860873	6982.062745	25.227546
167.939789	6981.974641	25.232563
167.889538	6993.044729	25.237581
167.982668	7009.559661	25.242599
168.298560	7012.130246	25.247616
167.990374	7017.850105	25.252634
168.480943	7033.810708	25.257651
168.849535	7043.887946	25.262669
168.426564	7051.276898	25.267687
168.902065	7050.700668	25.272704
168.957371	7076.543338	25.277722
169.040441	7080.003988	25.282739
169.302180	7098.190126	25.287757
169.628453	7113.335884	25.292775
169.815212	7119.636232	25.297792
169.902274	7130.582239	25.302810
169.973956	7135.305234	25.307827
170.424371	7137.065979	25.312845
170.330295	7155.482026	25.317863
170.554127	7156.056152	25.322880
170.703100	7176.548498	25.327898
170.465033	7179.366383	25.332915
170.724837	7201.720463	25.337933
171.342634	7193.486807	25.342951
171.832654	7191.843660	25.347968
171.960504	7197.589269	25.352986
172.167755	7206.066727	25.358003
172.241532	7219.919942	25.363021
172.359492	7224.655258	25.368039
172.472544	7223.294104	25.373056
172.747222	7216.966590	25.378074
172.854350	7209.817576	25.383091
172.949339	7212.447811	25.388109
173.257685	7243.695381	25.393127
173.579113	7244.050156	25.398144
173.581427	7257.909294	25.403162
173.643696	7258.441516	25.408179
174.109677	7248.940824	25.413197
173.628875	7256.568856	25.418215
173.880857	7274.789814	25.423232
174.086644	7280.568666	25.428250
174.101702	7284.961606	25.433267
174.343575	7303.735791	25.438285
174.539988	7307.722135	25.443303
174.812427	7314.636023	25.448320
174.774057	7344.614034	25.453338
174.728912	7350.406958	25.458355
174.828325	7353.717925	25.463373
175.041899	7377.230410	25.468391
175.591055	7385.669979	25.473408
175.800410	7405.733621	25.478426
175.925469	7403.409002	25.483443
176.245754	7417.809302	25.488461
176.251131	7435.640942	25.493479
176.557536	7434.160025	25.498496
176.666209	7452.973735	25.503514
176.909358	7463.670059	25.508531
177.199094	7472.683744	25.513549
177.215239	7477.891751	25.518567
177.769543	7493.310774	25.523584
177.833688	7493.463440	25.528602
178.206512	7493.477974	25.533619
178.411232	7489.810851	25.538637
178.049986	7502.062405	25.543655
178.643296	7513.755750	25.548672
178.519840	7517.618469	25.553690
178.538642	7537.256293	25.558707
179.033633	7545.348930	25.563725
178.930301	7558.092898	25.568743
179.222010	7555.511921	25.573760
179.536228	7575.426093	25.578778
179.593863	7590.365735	25.583795
179.938448	7595.031200	25.588813
179.597796	7605.603536	25.593831
180.053644	7617.640708	25.598848
180.170014	7622.335488	25.603866
179.967004	7631.071385	25.608883
180.524703	7649.978991	25.613901
180.601275	7665.757636	25.618919
180.827646	7667.433780	25.623936
181.205785	7693.861048	25.628954
181.207991	7695.580806	25.633971
181.727792	7695.628561	25.638989
181.715105	7716.221392	25.644007
181.814655	7715.642922	25.649024
182.076642	7727.342839	25.654042
182.094329	7722.832841	25.659059
182.376503	7744.551920	25.664077
182.317957	7759.570846	25.669095
182.521272	7758.041026	25.674112
183.021443	7777.995851	25.679130
183.241020	7780.129477	25.684148
183.293847	7786.360974	25.689165
183.043379	7811.624173	25.694183
183.308650	7823.274856	25.699200
183.888890	7833.890159	25.704218
183.726238	7842.991937	25.709236
184.414058	7840.728603	25.714253
184.041281	7863.044080	25.719271
184.674765	7863.129580	25.724288
184.779082	7871.327178	25.729306
185.091443	7883.001087	25.734324
185.447964	7895.444614	25.739341
185.690456	7901.009333	25.744359
185.634353	7890.176672	25.749376
186.067364	7897.471260	25.754394
185.890537	7916.972383	25.759412
186.098829	7923.907801	25.764429
186.191769	7928.426217	25.769447
186.427633	7946.497127	25.774464
186.520045	7957.969313	25.779482
186.711452	7965.878455	25.784500
187.179905	7965.009027	25.789517
187.278674	7984.076789	25.794535
187.388485	7993.798559	25.799552
187.390098	7998.877656	25.804570
187.606497	8016.912410	25.809588
188.232436	8018.610658	25.814605
188.022159	8024.802368	25.819623
188.488140	8042.451916	25.824640
188.819267	8054.008082	25.829658
188.709752	8055.190939	25.834676
188.640878	8057.553549	25.839693
188.815865	8081.732316	25.844711
189.146989	8084.681517	25.849728
189.134483	8102.538444	25.854746
188.909868	8118.148802	25.859764
189.519284	8130.125316	25.864781
189.673613	8148.691441	25.869799
189.884325	8159.350552	25.874816
190.349461	8177.059412	25.879834
190.722443	8197.808990	25.884852
190.962134	8190.405059	25.889869
191.085270	8202.091684	25.894887
191.163645	8215.149146	25.899904
191.472119	8221.661905	25.904922
191.342263	8224.127904	25.909940
191.857652	8216.156323	25.914957
192.012390	8245.181536	25.919975
191.709560	8250.084206	25.924992
192.028316	8254.555701	25.930010
191.789409	8286.890499	25.935028
192.124921	8293.047234	25.940045
192.327670	8307.164179	25.945063
192.383966	8320.451881	25.950080
192.919375	8332.605608	25.955098
193.121405	8357.659086	25.960116
193.242972	8364.342957	25.965133
193.654587	8377.023224	25.970151
193.782548	8380.173669	25.975168
194.467654	8384.563579	25.980186
194.297650	8404.785052	25.985204
195.028610	8400.002172	25.990221
194.832938	8402.507416	25.995239
194.755414	8414.278136	26.000256
195.302559	8424.662676	26.005274
195.293631	8440.791389	26.010292
195.648808	8439.317160	26.015309
195.837798	8460.753509	26.020327
195.937323	8467.612486	26.025344
196.251872	8472.321578	26.030362
196.202923	8478.945734	26.035380
196.309604	8498.342998	26.040397
196.644486	8511.625011	26.045415
196.399740	8525.721442	26.050432
197.306175	8527.046889	26.055450
197.477737	8531.822077	26.060468
197.367851	8547.093921	26.065485
197.617840	8554.870098	26.070503
197.556086	8559.972866	26.075520
198.067920	8577.114868	26.080538
198.064870	8592.951255	26.085556
198.449341	8593.866533	26.090573
198.842499	8614.847583	26.095591
198.986152	8636.069894	26.100608
199.333748	8630.098046	26.105626
199.348798	8633.278745	26.110644
199.633637	8652.250804	26.115661
199.743549	8658.144237	26.120679
199.622486	8665.733719	26.125696
199.979873	8684.310629	26.130714
199.994619	8687.951736	26.135732
200.236551	8694.406456	26.140749
200.417746	8707.974405	26.145767
200.473777	8724.130838	26.150784
201.076699	8733.723714	26.155802
201.413364	8748.015670	26.160820
201.223951	8753.329292	26.165837
201.311201	8759.104406	26.170855
201.329777	8777.862146	26.175872
201.773640	8781.101595	26.180890
201.726758	8800.589443	26.185908
201.843334	8805.002844	26.190925
202.322778	8818.327003	26.195943
202.414399	8840.862626	26.200960
203.097044	8839.205521	26.205978
202.982385	8859.239756	26.210996
203.199672	8878.430622	26.216013
203.441832	8887.011677	26.221031
203.872060	8902.306365	26.226048
203.982707	8912.014829	26.231066
204.102027	8920.888161	26.236084
204.168704	8930.762214	26.241101
204.481544	8947.935976	26.246119
204.123784	8958.490740	26.251136
204.718575	8977.969372	26.256154
204.774565	8989.268341	26.261172
204.993574	9010.778205	26.266189
205.178320	9027.590816	26.271207
205.152478	9052.117159	26.276224
205.590073	9058.721445	26.281242
205.943606	9086.855681	26.286260
206.082065	9091.347520	26.291277
206.601895	9107.501245	26.296295
206.531606	9120.607200	26.301312
207.273785	9124.773794	26.306330
207.436232	9151.995467	26.311348
207.508748	9157.948966	26.316365
207.721740	9155.353122	26.321383
207.478687	9173.008849	26.326400
208.061067	9179.317035	26.331418
207.810275	9196.388929	26.336436
208.234715	9219.245858	26.341453
208.613203	9220.657124	26.346471
208.481246	9253.356259	26.351488
208.796886	9253.997680	26.356506
209.126168	9281.968529	26.361524
209.323243	9281.340614	26.366541
209.756712	9290.525290	26.371559
209.988438	9311.241096	26.376576
210.512847	9308.175737	26.381594
210.520723	9320.996332	26.386612
210.648560	9326.820674	26.391629
211.576525	9328.905331	26.396647
211.726714	9336.556569	26.401664
211.750487	9321.598692	26.406682
211.855847	9327.020156	26.411700
211.914402	9341.822503	26.416717
212.167788	9346.956744	26.421735
212.544703	9356.922088	26.426752
212.528268	9349.965280	26.431770
212.654411	9357.128516	26.436788
212.658419	9367.195422	26.441805
213.342932	9372.634348	26.446823
213.037508	9382.624291	26.451840
213.091429	9383.525038	26.456858
213.328391	9402.471843	26.461876
213.146041	9415.519586	26.466893
213.566903	9417.978641	26.471911
213.723048	9447.378191	26.476928
214.303627	9455.226471	26.481946
214.444714	9474.211081	26.486964
214.285364	9486.870395	26.491981
214.875646	9489.868277	26.496999
214.664736	9520.339310	26.502016
214.951002	9527.355906	26.507034
215.650340	9541.120982	26.512052
215.564769	9558.914562	26.517069
215.806614	9571.700430	26.522087
215.887000	9595.273446	26.527104
216.404834	9599.743121	26.532122
216.523393	9617.172912	26.537140
216.561057	9629.169786	26.542157
216.937033	9647.962133	26.547175
217.102654	9666.703836	26.552192
217.355040	9663.522414	26.557210
217.783633	9683.828028	26.562228
218.042152	9700.895237	26.567245
218.143702	9696.097015	26.572263
218.159080	9723.399440	26.577280
218.360446	9732.292832	26.582298
218.392256	9749.468641	26.587316
218.318863	9769.731241	26.592333
218.779510	9791.937951	26.597351
218.811269	9817.805240	26.602368
219.379865	9840.154175	26.607386
219.612202	9851.356031	26.612404
219.772671	9869.292937	26.617421
220.023567	9875.762087	26.622439
220.236846	9905.995496	26.627456
220.495963	9909.855283	26.632474
220.456858	9936.013847	26.637492
220.790346	9942.889715	26.642509
221.228498	9958.576535	26.647527
221.179628	9981.067406	26.652544
221.424845	9994.914744	26.657562
222.015256	10003.919410	26.662580
222.432522	10029.104274	26.667597
223.022421	10026.583950	26.672615
222.918030	10043.345422	26.677632
222.968629	10060.363552	26.682650
223.293566	10066.666337	26.687668
223.594481	10081.056558	26.692685
224.081178	10097.056090	26.697703
224.040249	10097.667829	26.702720
223.856589	10106.524451	26.707738
224.238309	10122.801636	26.712756
224.474914	10134.936007	26.717773
224.448042	10137.634588	26.722791
224.991510	10152.550485	26.727808
225.017762	10167.072721	26.732826
225.066063	10166.650680	26.737844
225.075804	10190.187490	26.742861
225.860203	10195.782757	26.747879
225.816642	10228.691456	26.752896
225.919440	10230.628027	26.757914
226.385232	10248.774059	26.762932
226.309300	10269.184117	26.767949
226.618035	10276.662209	26.772967
226.722084	10295.166604	26.777984
227.148637	10316.149830	26.783002
227.648226	10327.407810	26.788020
227.808680	10336.767301	26.793037
228.232571	10332.247639	26.798055
228.240948	10357.853181	26.803072
228.466296	10357.512697	26.808090
229.152542	10369.070708	26.813108
229.354119	10377.670107	26.818125
229.703206	10378.178755	26.823143
229.577371	10386.805173	26.828160
230.114585	10397.690462	26.833178
230.393925	10404.175375	26.838196
230.068700	10418.257283	26.843213
230.649133	10421.514677	26.848231
230.630773	10445.780809	26.853248
230.774549	10458.258424	26.858266
230.957278	10453.569402	26.863284
231.041291	10464.279081	26.868301
231.561934	10473.200714	26.873319
231.560777	10503.404777	26.878336
231.753243	10514.736652	26.883354
232.252449	10532.756108	26.888372
232.205919	10545.543133	26.893389
232.424140	10557.243194	26.898407
232.588525	10576.658341	26.903424
233.012139	10602.123726	26.908442
233.120510	10606.703060	26.913460
233.296692	10629.171610	26.918477
233.567020	10641.936141	26.923495
233.703350	10662.008312	26.928512
234.154137	10674.620933	26.933530
234.654694	10683.222819	26.938548
234.858588	10706.788115	26.943565
234.867058	10712.559619	26.948583
235.192424	10731.798192	26.953600
235.495005	10742.475979	26.958618
235.993556	10743.045812	26.963636
235.870150	10765.216820	26.968653
236.232594	10770.131900	26.973671
236.539563	10786.475633	26.978688
236.622131	10800.612513	26.983706
237.335276	10801.022606	26.988724
236.801384	10809.958297	26.993741
237.256576	10824.530445	26.998759
237.251386	10850.997638	27.003776
236.977055	10859.338301	27.008794
237.662999	10872.653411	27.013812
237.732654	10891.585085	27.018829
238.022040	10905.031916	27.023847
237.972196	10919.143974	27.028864
238.035631	10936.420376	27.033882
238.920022	10962.969466	27.038900
238.678392	10990.693329	27.043917
239.146711	11007.544800	27.048935
239.326318	11026.067166	27.053952
239.350851	11045.662226	27.058970
239.911007	11061.241420	27.063988
239.983617	11074.466385	27.069005
240.782872	11099.543348	27.074023
241.257642	11114.018209	27.079040
241.221316	11138.421327	27.084058
241.513248	11144.330009	27.089076
241.446116	11164.937421	27.094093
241.440285	11181.298786	27.099111
242.188004	11198.303479	27.104128
242.186406	11215.636215	27.109146
242.514386	11224.788136	27.114164
242.691566	11242.071152	27.119181
243.196173	11270.439216	27.124199
243.353999	11280.117683	27.129216
243.352834	11310.336148	27.134234
243.689147	11316.715172	27.139252
243.848711	11333.609146	27.144269
244.342102	11353.125137	27.149287
244.854623	11369.511898	27.154304
244.988887	11384.116860	27.159322
245.227156	11380.247869	27.164340
245.523842	11402.356380	27.169357
245.508251	11408.884417	27.174375
245.813386	11430.504037	27.179392
246.470172	11443.751502	27.184410
246.868053	11440.570525	27.189428
246.926513	11469.085841	27.194445
246.964903	11475.075409	27.199463
247.340294	11478.887553	27.204480
247.433315	11496.895982	27.209498
247.781428	11502.646502	27.214516
247.751227	11521.461868	27.219533
247.920404	11532.417084	27.224551
248.407687	11541.514090	27.229568
248.104505	11578.760972	27.234586
248.627775	11580.113778	27.239604
248.852319	11610.592208	27.244621
248.705064	11635.641305	27.249639
249.546140	11650.373315	27.254656
249.705723	11670.943501	27.259674
249.769194	11693.100438	27.264692
250.132188	11698.474997	27.269709
250.415694	11718.410982	27.274727
250.723932	11724.267706	27.279744
250.465794	11751.119962	27.284762
251.091077	11754.273302	27.289780
251.510604	11774.947013	27.294797
251.412356	11786.064287	27.299815
251.988259	11795.100489	27.304832
252.081213	11811.983577	27.309850
252.124506	11820.395931	27.314868
252.414152	11845.809999	27.319885
252.682151	11878.169274	27.324903
253.261318	11884.731392	27.329920
253.015798	11912.156494	27.334938
253.617423	11926.550915	27.339956
253.833919	11943.384940	27.344973
253.793181	11953.541378	27.349991
254.299077	11973.867671	27.355008
254.418301	11996.503176	27.360026
254.493268	12014.789203	27.365044
254.994320	12026.453778	27.370061
255.414526	12047.350699	27.375079
255.415685	12056.813983	27.380096
255.443598	12092.224009	27.385114
255.963542	12106.050548	27.390132
256.554314	12115.980292	27.395149
256.956356	12138.551837	27.400167
257.613921	12145.781824	27.405184
257.758074	12162.662060	27.410202
258.163822	12178.392570	27.415220
258.373158	12186.386483	27.420237
258.217488	12188.467227	27.425255
258.553952	12202.063360	27.430272
258.425339	12221.012361	27.435290
258.732934	12232.796879	27.440308
259.463110	12248.218163	27.445325
259.183654	12261.790729	27.450343
259.811312	12273.722018	27.455360
260.005272	12290.244390	27.460378
260.072336	12314.353887	27.465396
260.333271	12318.044584	27.470413
260.602005	12346.855073	27.475431
261.032665	12349.477374	27.480448
260.923313	12379.870471	27.485466
261.111415	12394.189973	27.490484
261.451154	12410.222085	27.495501
261.631543	12437.459416	27.500519
262.372063	12443.389783	27.505536
263.312767	12446.433171	27.510554
263.575427	12459.833502	27.515572
263.866163	12470.091917	27.520589
263.817640	12473.572037	27.525607
264.200091	12466.762534	27.530624
264.456718	12475.762673	27.535642
264.400046	12468.195318	27.540660
264.796684	12490.373117	27.545677
264.510774	12508.783384	27.550695
264.924510	12507.519449	27.555712
265.383752	12538.269898	27.560730
265.268136	12544.906067	27.565748
265.444185	12561.489837	27.570765
265.730648	12581.924736	27.575783
265.920488	12592.390589	27.580800
265.694969	12617.794996	27.585818
265.955451	12641.889528	27.590836
266.122763	12666.788834	27.595853
266.263969	12693.073951	27.600871
266.586153	12719.719499	27.605888
267.159270	12751.550077	27.610906
267.202466	12771.198898	27.615924
267.526489	12799.987659	27.620941
267.443045	12828.056259	27.625959
268.136736	12853.275367	27.630976
268.292881	12882.786285	27.635994
268.799904	12908.881417	27.641012
268.868300	12924.824694	27.646029
269.276750	12954.985855	27.651047
269.529150	12976.560790	27.656064
270.241175	13010.958095	27.661082
270.085250	13019.560003	27.666100
272.005981	13003.048674	27.671117
272.570816	13008.062994	27.676135
272.594994	12994.963812	27.681152
272.856006	12999.807635	27.686170
272.991333	13004.230104	27.691188
273.457889	13001.779945	27.696205
273.411732	12997.976354	27.701223
273.646605	13003.025068	27.706240
273.668514	13026.609895	27.711258
273.880690	13038.960172	27.716276
274.213414	13042.278008	27.721293
274.063612	13053.908789	27.726311
274.358195	13071.920310	27.731328
274.416559	13085.830280	27.736346
274.718350	13102.773413	27.741364
274.699141	13120.935571	27.746381
274.801297	13139.912490	27.751399
275.302684	13165.966064	27.756416
275.392418	13192.681277	27.761434
275.612348	13209.294378	27.766452
275.871366	13240.565021	27.771469
276.045504	13269.919439	27.776487
276.367136	13292.514769	27.781504
276.470186	13322.451212	27.786522
276.968248	13343.702753	27.791540
277.413930	13366.745625	27.796557
277.732256	13388.198760	27.801575
277.926712	13405.243860	27.806592
278.140157	13434.152401	27.811610
278.501840	13462.566050	27.816628
278.836134	13469.681232	27.821645
279.234871	13488.748178	27.826663
279.870493	13491.224757	27.831680
280.191052	13508.073152	27.836698
280.225163	13519.330484	27.841716
280.968584	13519.794404	27.846733
281.038634	13545.556269	27.851751
281.151927	13551.361833	27.856768
281.160057	13568.737025	27.861786
281.691180	13581.791605	27.866804
281.770304	13592.574233	27.871821
281.925182	13620.338070	27.876839
281.948376	13633.361585	27.881856
282.124809	13658.020672	27.886874
282.144793	13689.452055	27.891892
282.623436	13703.218057	27.896909
282.908708	13747.682165	27.901927
283.082693	13762.506838	27.906944
283.472257	13799.187913	27.911962
283.569559	13823.067677	27.916980
284.047981	13847.027828	27.921997
284.015088	13883.460194	27.927015
284.384023	13909.533201	27.932032
284.995339	13943.950245	27.937050
284.899335	13970.102190	27.942068
285.473265	13990.975905	27.947085
285.715537	14020.559721	27.952103
286.334536	14047.039345	27.957120
286.902727	14074.156088	27.962138
287.056840	14092.006312	27.967156
287.752922	14101.452393	27.972173
287.694147	14108.138135	27.977191
288.024896	14130.512443	27.982208
288.637286	14152.245878	27.987226
288.663218	14168.509841	27.992244
289.195331	14188.733448	27.997261
289.270521	14205.484555	28.002279
289.477807	14212.969064	28.007296
289.974961	14236.905194	28.012314
289.961655	14254.743328	28.017332
290.557918	14277.526895	28.022349
290.754701	14300.928469	28.027367
290.596362	14320.540065	28.032384
290.912803	14337.512346	28.037402
290.913087	14365.547098	28.042420
291.510135	14385.916017	28.047437
291.636036	14412.039445	28.052455
291.793271	14447.337099	28.057472
292.028883	14467.327225	28.062490
292.508473	14496.955217	28.067508
293.114382	14518.689027	28.072525
293.146293	14545.601997	28.077543
293.454928	14571.947596	28.082560
293.674140	14599.549937	28.087578
293.851879	14624.720004	28.092596
294.505086	14642.533629	28.097613
294.380740	14658.664029	28.102631
295.145494	14678.654223	28.107648
295.383554	14702.334021	28.112666
295.307273	14733.075362	28.117684
295.819146	14753.219816	28.122701
295.975385	14772.793359	28.127719
296.166012	14799.377307	28.132736
296.640304	14823.511464	28.137754
296.584103	14845.995730	28.142772
297.226249	14879.357328	28.147789
297.529156	14895.925086	28.152807
297.749938	14927.318635	28.157824
298.342639	14949.397319	28.162842
298.659845	14972.630359	28.167860
299.055745	14986.238992	28.172877
299.196344	15017.200317	28.177895
299.441045	15033.294427	28.182912
300.333551	15040.806709	28.187930
300.635852	15055.841273	28.192948
301.496466	15061.193218	28.197965
301.962166	15061.427409	28.202983
302.539456	15079.791733	28.208000
302.778678	15089.416845	28.213018
302.602876	15097.287591	28.218036
303.100643	15089.584608	28.223053
303.243690	15095.906390	28.228071
302.860863	15100.930465	28.233088
303.417356	15123.714943	28.238106
303.219631	15145.095939	28.243124
303.753761	15152.501652	28.248141
303.869975	15176.081744	28.253159
304.060958	15213.229572	28.258176
304.448459	15226.042167	28.263194
304.446184	15240.714018	28.268212
304.935601	15264.146881	28.273229
305.287226	15295.605155	28.278247
305.268741	15322.520826	28.283264
305.488046	15340.161065	28.288282
305.708664	15373.056276	28.293300
306.377742	15402.632888	28.298317
306.848533	15419.813323	28.303335
306.976746	15444.922956	28.308352
307.428358	15467.763534	28.313370
307.344599	15497.512384	28.318388
307.935156	15515.517695	28.323405
308.077300	15552.776867	28.328423
308.501877	15574.709657	28.333440
308.906126	15600.349471	28.338458
308.987950	15632.934538	28.343476
309.377989	15654.240761	28.348493
309.418346	15678.219283	28.353511
309.934623	15722.568744	28.358528
310.580128	15726.311365	28.363546
310.932075	15744.988545	28.368564
311.810974	15759.691971	28.373581
312.059236	15777.816313	28.378599
312.459513	15786.089710	28.383616
312.494982	15792.841170	28.388634
312.362239	15809.353683	28.393652
312.764051	15823.923597	28.398669
313.047883	15839.889105	28.403687
313.371076	15865.191936	28.408704
313.442029	15882.230250	28.413722
313.862761	15905.089588	28.418740
314.355822	15916.899359	28.423757
315.151948	15921.560414	28.428775
315.278166	15946.012807	28.433792
315.660210	15948.668888	28.438810
315.791832	15968.627945	28.443828
315.962689	15989.495025	28.448845
316.232489	16005.793608	28.453863
316.585933	16025.921885	28.458880
317.329881	16025.902917	28.463898
317.996709	16045.433112	28.468916
318.683676	16048.003214	28.473933
318.877709	16049.774239	28.478951
318.589688	16057.660506	28.483968
318.998932	16070.853857	28.488986
319.214059	16085.007572	28.494004
319.600785	16101.526959	28.499021
320.109771	16116.340077	28.504039
319.917008	16133.862578	28.509056
320.397671	16152.173521	28.514074
320.324428	16173.368108	28.519092
320.613312	16186.631721	28.524109
321.071281	16206.074756	28.529127
321.387065	16229.086328	28.534144
321.499428	16251.135785	28.539162
322.047090	16277.571495	28.544180
322.180287	16296.387154	28.549197
322.305606	16327.139202	28.554215
322.390388	16347.866566	28.559232
322.674693	16369.307550	28.564250
322.702777	16411.889564	28.569268
323.571148	16431.579251	28.574285
323.989852	16453.866756	28.579303
323.805568	16496.719442	28.584320
324.558823	16519.617632	28.589338
324.973410	16544.453513	28.594356
325.212579	16580.091587	28.599373
325.483288	16597.505115	28.604391
325.683376	16629.535690	28.609408
326.481222	16642.783531	28.614426
326.545634	16668.511767	28.619444
326.775246	16700.157501	28.624461
327.278629	16723.503069	28.629479
327.592069	16750.089706	28.634496
328.441444	16767.815888	28.639514
328.151915	16796.432607	28.644532
328.543146	16804.937114	28.649549
329.147990	16824.850396	28.654567
329.256314	16848.105193	28.659584
329.639182	16861.894525	28.664602
329.786263	16888.018778	28.669620
329.830370	16902.633343	28.674637
330.305188	16922.466695	28.679655
330.379936	16964.566054	28.684672
330.987437	16981.699580	28.689690
331.061306	17015.276756	28.694708
331.167200	17039.752228	28.699725
331.729168	17076.604682	28.704743
331.942373	17110.949770	28.709760
332.472986	17136.186591	28.714778
332.565274	17164.031362	28.719796
333.179372	17184.735914	28.724813
333.615835	17215.889916	28.729831
333.861503	17246.634648	28.734848
334.676588	17273.262109	28.739866
335.405568	17276.370982	28.744884
335.843673	17295.193981	28.749901
336.446221	17311.246431	28.754919
336.545641	17315.972511	28.759936
336.824183	17330.178282	28.764954
336.951042	17347.535664	28.769972
337.249951	17362.914152	28.774989
337.838146	17368.693402	28.780007
337.675257	17401.279074	28.785024
338.059940	17414.822362	28.790042
338.529964	17433.342423	28.795060
338.545267	17447.254441	28.800077
339.063704	17472.500445	28.805095
339.091903	17509.991543	28.810112
339.716893	17532.719958	28.815130
339.640253	17563.975336	28.820148
339.892086	17589.095128	28.825165
340.245987	17612.327089	28.830183
340.699422	17652.300297	28.835200
340.928377	17677.591198	28.840218
341.224003	17707.813933	28.845236
341.261756	17739.454574	28.850253
341.745420	17774.285970	28.855271
342.007387	17813.624371	28.860288
342.404541	17847.713824	28.865306
342.612345	17873.024949	28.870324
343.252778	17905.645455	28.875341
344.198187	17924.628918	28.880359
344.875131	17954.917346	28.885376
345.246110	17974.472340	28.890394
345.507109	17994.345280	28.895412
345.975003	18017.366767	28.900429
346.224066	18025.758585	28.905447
346.297233	18045.631999	28.910464
346.978456	18055.901417	28.915482
347.269014	18088.897757	28.920500
347.019589	18099.813561	28.925517
347.835558	18116.604494	28.930535
347.633975	18142.503748	28.935552
348.066169	18159.258646	28.940570
348.460254	18182.011430	28.945588
348.411736	18195.295306	28.950605
348.956328	18221.631288	28.955623
349.204302	18253.858377	28.960640
349.428447	18282.766045	28.965658
349.908307	18303.695857	28.970676
350.177543	18336.976441	28.975693
350.935886	18361.026974	28.980711
351.217032	18393.512850	28.985728
351.386676	18410.133875	28.990746
351.944226	18430.410122	28.995764
351.992763	18464.199786	29.000781
352.206997	18494.578367	29.005799
352.342675	18526.935732	29.010816
353.058301	18555.355721	29.015834
353.689328	18572.738062	29.020852
353.663091	18606.469870	29.025869
354.323853	18628.087459	29.030887
354.719696	18672.849036	29.035904
354.983586	18689.603377	29.040922
355.403313	18721.590272	29.045940
355.430228	18747.484035	29.050957
355.825253	18773.776678	29.055975
356.147771	18805.201256	29.060992
356.525961	18842.220469	29.066010
356.878041	18875.677988	29.071028
356.916601	18908.569366	29.076045
357.414098	18934.856580	29.081063
358.487606	18955.819048	29.086080
359.092064	18966.676541	29.091098
359.731650	18993.314461	29.096116
360.031219	19015.168903	29.101133
360.482232	19031.815439	29.106151
361.141041	19047.819782	29.111168
361.544838	19063.312776	29.116186
362.191589	19070.488555	29.121204
362.274088	19082.399852	29.126221
362.551285	19092.570957	29.131239
362.717455	19108.317235	29.136256
363.001054	19114.950474	29.141274
363.238002	19136.820580	29.146292
363.413891	19151.396766	29.151309
363.948388	19164.787779	29.156327
364.029752	19188.278932	29.161344
364.380001	19208.524269	29.166362
364.646466	19237.426176	29.171380
364.637974	19259.058381	29.176397
365.385340	19278.922780	29.181415
365.435049	19297.393934	29.186432
365.978145	19332.270535	29.191450
366.137664	19360.566039	29.196468
366.223128	19392.634751	29.201485
366.736861	19419.020205	29.206503
366.916561	19447.546135	29.211520
367.114719	19478.910780	29.216538
367.612296	19497.745088	29.221556
367.884436	19546.400120	29.226573
368.262973	19573.090084	29.231591
368.690525	19606.843473	29.236608
368.804621	19641.125284	29.241626
369.089105	19672.315519	29.246644
369.805491	19709.585681	29.251661
370.110122	19731.200924	29.256679
370.380697	19764.985971	29.261696
370.554073	19806.798518	29.266714
370.957468	19836.501851	29.271732
371.160834	19876.005993	29.276749
371.720265	19914.513218	29.281767
372.485614	19944.163799	29.286784
372.520229	19980.578965	29.291802
373.636636	20003.278361	29.296820
373.808354	20040.217949	29.301837
374.197818	20065.167417	29.306855
374.351004	20088.288584	29.311872
374.629856	20131.727926	29.316890
375.265118	20156.411173	29.321908
375.591195	20194.844056	29.326925
375.950971	20221.653881	29.331943
376.516259	20261.178099	29.336960
377.055163	20283.995137	29.341978
377.523517	20307.730278	29.346996
377.810215	20342.990595	29.352013
377.979999	20371.778882	29.357031
378.121732	20403.635150	29.362048
378.465985	20435.490710	29.367066
379.622174	20437.428061	29.372084
380.009720	20467.775769	29.377101
380.174745	20487.758927	29.382119
380.699431	20517.353264	29.387136
381.091264	20548.605314	29.392154
381.650404	20565.437865	29.397172
381.623191	20596.951310	29.402189
382.318768	20616.565785	29.407207
382.582461	20637.405209	29.412224
382.883461	20670.731377	29.417242
383.110808	20701.044424	29.422260
383.533488	20718.843143	29.427277
383.952870	20751.500111	29.432295
384.166916	20776.089229	29.437312
384.486725	20801.874344	29.442330
385.040843	20833.733496	29.447348
385.155234	20870.058074	29.452365
385.412766	20889.149677	29.457383
386.219755	20912.525415	29.462400
386.198241	20951.424278	29.467418
386.758157	20970.813527	29.472436
386.926914	21007.339246	29.477453
387.196545	21043.844250	29.482471
387.647957	21061.264691	29.487488
387.846408	21099.633496	29.492506
388.501340	21126.658120	29.497524
388.774435	21161.616081	29.502541
389.164509	21190.642471	29.507559
389.856679	21216.713880	29.512576
389.649280	21250.101816	29.517594
390.148328	21281.631212	29.522612
390.346776	21310.151239	29.527629
390.901969	21352.746600	29.532647
391.786155	21381.221272	29.537664
392.301879	21419.539509	29.542682
392.880340	21440.449548	29.547700
393.126872	21458.978117	29.552717
393.973339	21486.700559	29.557735
394.457360	21502.816795	29.562752
394.429447	21526.762026	29.567770
395.269122	21548.766271	29.572788
395.044847	21581.829176	29.577805
395.104986	21604.238888	29.582823
395.487756	21636.965748	29.587840
396.047078	21683.199193	29.592858
396.662468	21698.715820	29.597876
396.723740	21739.128200	29.602893
396.682774	21771.758257	29.607911
397.424613	21805.213475	29.612928
397.451743	21852.988480	29.617946
398.053606	21884.079761	29.622964
398.558421	21916.780665	29.627981
398.647120	21961.243792	29.632999
399.105876	21998.412380	29.638016
399.437932	22042.675498	29.643034
400.215952	22065.706301	29.648052
400.423733	22112.157692	29.653069
401.262485	22140.551195	29.658087
402.036681	22168.161914	29.663104
401.909587	22210.498140	29.668122
402.101648	22243.796161	29.673140
402.627181	22278.411564	29.678157
402.949755	22314.870116	29.683175
403.391353	22348.478296	29.688192
403.787308	22390.850585	29.693210
404.468656	22417.417186	29.698228
404.893208	22464.536053	29.703245
404.830636	22495.388649	29.708263
405.676289	22531.858864	29.713280
405.920880	22570.623215	29.718298
406.338857	22595.665490	29.723316
407.064270	22622.048197	29.728333
407.913933	22654.931181	29.733351
408.700284	22662.953965	29.738368
409.085280	22682.512611	29.743386
409.392485	22694.211256	29.748404
409.367583	22716.058756	29.753421
409.766103	22724.990083	29.758439
410.430047	22750.857447	29.763456
410.775217	22770.368989	29.768474
411.115869	22788.097269	29.773492
411.393939	22809.433488	29.778509
411.625494	22832.836832	29.783527
412.116387	22856.517882	29.788544
412.078607	22888.629886	29.793562
412.480926	22907.226698	29.798580
413.148883	22941.827949	29.803597
413.219437	22972.509032	29.808615
413.889717	22992.501493	29.813632
414.009590	23034.127121	29.818650
414.502631	23060.729538	29.823668
414.931892	23098.301602	29.828685
415.226226	23145.548002	29.833703
415.501362	23176.890807	29.838720
415.975841	23217.452206	29.843738
416.435272	23243.217487	29.848756
416.815083	23282.379493	29.853773
417.105111	23325.063384	29.858791
417.378361	23362.968911	29.863808
417.503464	23412.083852	29.868826
418.201703	23450.769404	29.873844
418.509079	23486.280775	29.878861
418.783402	23536.742089	29.883879
419.599049	23575.057144	29.888896
419.895599	23631.907238	29.893914
420.433503	23668.848947	29.898932
421.336377	23695.825866	29.903949
421.347711	23737.964508	29.908967
421.782823	23770.406234	29.913984
421.974026	23812.450247	29.919002
422.596540	23848.180813	29.924020
423.303417	23898.475888	29.929037
423.838768	23931.295818	29.934055
424.143379	23959.306661	29.939072
424.349053	24005.318877	29.944090
424.784341	24043.673614	29.949108
425.157568	24085.455395	29.954125
425.143931	24132.761675	29.959143
426.077113	24164.412754	29.964160
426.374717	24215.377429	29.969178
426.599349	24266.572091	29.974196
427.249831	24301.261013	29.979213
427.623529	24349.120633	29.984231
428.224984	24381.051076	29.989248
429.015661	24414.761616	29.994266
429.961720	24439.890442	29.999284
430.301794	24467.820119	30.004301
430.730046	24485.431571	30.009319
431.417250	24511.360334	30.014336
431.873507	24545.103956	30.019354
432.214494	24562.411944	30.024372
432.369694	24591.843560	30.029389
432.645334	24605.839364	30.034407
433.105038	24638.066253	30.039424
433.272809	24668.178183	30.044442
433.583657	24709.582397	30.049460
434.041246	24723.444545	30.054477
434.030550	24771.228038	30.059495
434.153518	24798.952628	30.064512
434.505420	24855.211395	30.069530
435.149852	24891.116477	30.074548
435.426257	24930.469163	30.079565
436.047201	24969.914358	30.084583
436.492792	25019.228955	30.089600
436.684809	25074.254354	30.094618
437.068993	25108.120146	30.099636
438.055597	25152.045784	30.104653
438.070100	25214.664783	30.109671
438.905500	25242.968279	30.114688
439.201220	25290.056167	30.119706
439.347970	25351.415475	30.124724
439.733604	25385.562856	30.129741
440.916608	25421.062694	30.134759
441.599561	25455.982921	30.139776
442.037182	25483.498643	30.144794
442.490792	25521.929638	30.149812
443.464237	25550.718225	30.154829
443.408658	25586.368514	30.159847
444.069461	25616.649457	30.164864
444.588193	25645.193190	30.169882
444.858365	25680.461704	30.174900
445.239674	25707.009144	30.179917
445.284181	25752.529762	30.184935
445.667673	25783.785582	30.189952
445.643528	25821.741965	30.194970
446.115082	25868.762572	30.199988
447.008912	25912.185926	30.205005
447.056215	25969.501574	30.210023
447.332895	26015.260883	30.215040
447.517796	26064.454005	30.220058
448.184188	26121.439939	30.225076
449.227424	26160.452878	30.230093
449.791641	26198.409366	30.235111
450.121151	26241.197955	30.240128
450.825274	26294.055878	30.245146
451.260317	26338.473652	30.250164
451.753715	26357.362503	30.255181
452.004278	26408.185659	30.260199
452.750832	26443.626533	30.265216
452.952942	26465.525703	30.270234
453.462478	26518.541419	30.275252
453.770326	26557.174589	30.280269
453.935459	26599.343514	30.285287
454.371743	26638.815148	30.290304
455.077654	26682.836980	30.295322
455.010088	26728.012656	30.300340
455.904854	26763.334504	30.305357
455.939056	26813.380364	30.310375
456.642327	26848.468197	30.315392
457.343472	26880.617795	30.320410
457.758262	26930.479689	30.325428
458.491898	26958.417179	30.330445
459.207282	26995.519500	30.335463
459.342742	27027.170999	30.340480
459.669171	27062.951983	30.345498
460.163430	27102.164980	30.350516
460.591861	27135.689222	30.355533
460.768406	27181.545795	30.360551
461.307741	27227.072098	30.365568
461.880295	27259.264213	30.370586
462.485761	27286.601074	30.375604
463.060567	27331.419247	30.380621
463.685646	27369.742250	30.385639
464.455957	27400.120988	30.390656
464.786303	27428.138519	30.395674
465.108076	27467.914061	30.400692
465.849000	27485.490028	30.405709
466.079346	27538.013887	30.410727
466.839313	27564.357519	30.415744
467.076842	27605.383785	30.420762
467.284205	27646.489021	30.425780
467.469330	27672.579325	30.430797
467.815460	27708.757269	30.435815
468.339410	27756.060249	30.440832
468.501645	27797.103724	30.445850
468.873145	27846.022786	30.450868
469.651971	27892.529184	30.455885
470.064050	27953.963274	30.460903
470.548034	28003.874972	30.465920
471.325842	28050.088888	30.470938
471.761591	28085.534832	30.475956
472.430110	28125.315050	30.480973
472.653829	28173.718145	30.485991
473.013820	28214.198545	30.491008
473.449182	28258.871318	30.496026
473.800567	28312.393228	30.501044
474.548684	28347.514210	30.506061
474.803906	28405.536548	30.511079
475.109267	28456.653668	30.516096
475.783572	28496.946024	30.521114
475.962766	28544.375568	30.526132
476.432635	28597.827539	30.531149
476.505011	28662.813669	30.536167
477.276945	28713.051998	30.541184
478.060244	28759.029107	30.546202
478.226490	28822.998671	30.551220
479.096222	28862.586326	30.556237
479.766906	28916.413927	30.561255
480.268051	28968.133391	30.566272
481.077330	29004.374387	30.571290
481.328336	29042.907505	30.576308
481.889847	29074.088541	30.581325
482.601067	29113.386883	30.586343
483.384123	29132.032701	30.591360
483.817729	29164.006479	30.596378
484.160761	29193.232183	30.601396
485.109511	29218.607621	30.606413
485.308017	29251.599243	30.611431
485.794795	29282.570382	30.616448
486.059387	29315.951889	30.621466
486.026846	29346.895572	30.626484
486.766157	29381.902004	30.631501
487.043298	29427.107492	30.636519
487.328669	29466.009633	30.641536
487.870326	29503.262003	30.646554
488.029591	29551.933192	30.651572
488.279991	29596.341255	30.656589
489.013420	29652.613469	30.661607
489.167985	29705.941229	30.666624
490.271453	29752.265707	30.671642
490.743738	29806.458812	30.676660
491.262056	29848.260778	30.681677
491.688276	29904.417327	30.686695
492.139770	29950.652392	30.691712
493.005299	29989.970821	30.696730
493.281101	30036.610780	30.701748
493.586457	30077.941369	30.706765
494.378332	30127.730158	30.711783
494.643127	30182.419333	30.716800
495.254925	30228.155268	30.721818
495.745227	30276.665556	30.726836
496.452411	30328.365967	30.731853
496.632314	30374.155356	30.736871
497.198622	30420.991261	30.741888
498.059777	30461.439958	30.746906
498.079414	30510.768233	30.751924
498.631103	30556.328690	30.756941
499.493521	30599.195171	30.761959
499.728879	30652.246792	30.766976
500.023342	30696.540498	30.771994
500.665044	30748.199082	30.777012
501.364616	30798.524718	30.782029
501.708866	30853.116790	30.787047
501.961524	30906.484842	30.792064
502.895501	30948.278565	30.797082
502.902401	31001.490644	30.802100
503.407395	31056.158653	30.807117
503.984755	31112.816952	30.812135
504.444607	31164.343480	30.817152
505.008749	31210.200078	30.822170
505.446334	31278.200782	30.827188
506.149102	31321.258503	30.832205
506.705093	31372.691564	30.837223
507.064463	31427.836354	30.842240
507.412052	31479.246207	30.847258
507.875895	31535.848396	30.852276
508.587272	31590.556231	30.857293
509.099757	31634.526148	30.862311
509.328308	31681.885999	30.867328
509.872075	31723.490102	30.872346
510.393179	31788.951467	30.877364
511.057218	31831.520206	30.882381
511.837496	31884.864122	30.887399
511.932280	31928.283509	30.892416
512.711535	31961.597874	30.897434
513.145983	32016.508859	30.902452
513.554103	32073.687622	30.907469
514.465313	32115.568334	30.912487
515.265596	32157.756843	30.917504
515.711649	32196.330929	30.922522
516.077864	32246.082050	30.927540
516.680524	32284.237344	30.932557
517.056183	32340.656169	30.937575
517.258151	32391.308689	30.942592
517.921645	32437.843264	30.947610
518.139990	32496.992475	30.952628
518.705165	32546.930327	30.957645
519.027466	32597.848032	30.962663
519.385499	32658.777204	30.967680
519.790535	32715.110662	30.972698
520.137835	32772.567919	30.977716
520.754902	32838.889828	30.982733
521.604405	32904.642198	30.987751
521.872047	32967.450050	30.992768
522.510286	33022.680271	30.997786
523.028387	33087.223564	31.002804
523.334247	33149.497963	31.007821
524.160192	33199.156649	31.012839
524.642157	33270.347329	31.017856
525.181677	33335.763023	31.022874
525.545746	33391.894084	31.027892
526.266936	33455.947755	31.032909
526.964095	33509.535575	31.037927
527.704079	33572.267321	31.042944
528.765491	33617.441359	31.047962
529.083792	33678.161499	31.052980
529.865988	33741.728926	31.057997
530.687631	33776.381675	31.063015
531.178028	33815.095921	31.068032
531.817080	33850.660667	31.073050
532.167479	33900.392481	31.078068
532.608371	33944.413054	31.083085
533.152070	33992.446559	31.088103
533.335781	34036.259278	31.093120
533.848498	34091.142607	31.098138
534.362302	34149.932218	31.103156
534.570284	34201.391686	31.108173
535.388087	34244.992023	31.113191
535.647522	34314.734514	31.118208
536.136466	34360.616565	31.123226
536.718630	34408.383463	31.128244
537.240402	34460.055428	31.133261
538.139773	34496.078237	31.138279
538.211361	34553.087427	31.143296
539.024546	34594.466665	31.148314
539.595369	34641.548718	31.153332
539.729949	34694.422845	31.158349
540.824343	34739.749179	31.163367
541.301702	34796.429723	31.168384
541.648939	34841.123386	31.173402
542.289424	34897.426741	31.178420
542.742484	34944.044436	31.183437
543.479697	34991.378430	31.188455
543.749854	35050.455957	31.193472
544.248623	35091.988987	31.198490
545.139223	35127.803315	31.203508
546.349373	35167.478061	31.208525
547.569350	35195.981970	31.213543
547.921440	35227.797634	31.218560
548.538373	35264.306937	31.223578
549.058954	35288.244976	31.228596
549.776760	35320.617393	31.233613
550.276388	35351.629429	31.238631
550.433665	35381.858935	31.243648
550.916995	35419.677859	31.248666
551.411319	35464.904693	31.253684
551.640943	35505.215690	31.258701
552.374290	35538.741637	31.263719
552.451917	35595.874814	31.268736
553.279822	35642.855683	31.273754
553.622170	35690.691256	31.278772
553.685789	35743.751846	31.283789
553.974522	35787.060552	31.288807
554.749980	35851.206234	31.293824
554.933970	35913.776810	31.298842
555.646240	35966.310691	31.303860
555.716944	36038.873055	31.308877
556.269883	36105.147247	31.313895
557.088756	36174.491496	31.318912
557.495463	36235.276222	31.323930
558.089720	36306.216029	31.328948
559.364102	36345.013074	31.333965
561.428269	36371.275059	31.338983
562.102542	36412.329356	31.344000
562.561484	36443.975806	31.349018
563.523726	36471.397267	31.354036
563.648219	36510.601733	31.359053
564.566197	36542.780670	31.364071
564.676138	36578.735074	31.369088
565.216442	36605.594895	31.374106
565.685141	36647.158648	31.379124
566.013657	36689.471655	31.384141
566.294638	36724.208778	31.389159
566.843664	36781.674518	31.394176
567.008708	36813.745293	31.399194
567.722477	36860.411937	31.404212
567.860385	36897.191877	31.409229
568.664410	36943.486479	31.414247
569.051565	36989.525971	31.419264
569.350674	37038.151135	31.424282
569.686355	37085.050480	31.429300
570.085529	37143.121532	31.434317
570.745719	37196.328182	31.439335
571.053852	37263.992413	31.444352
571.465967	37323.443191	31.449370
572.153652	37386.837725	31.454388
572.530954	37457.697117	31.459405
572.977861	37519.363027	31.464423
573.464471	37591.222539	31.469440
573.864925	37660.951751	31.474458
574.448706	37739.863239	31.479476
575.185801	37817.282744	31.484493
575.703436	37890.901367	31.489511
576.202642	37964.059685	31.494528
576.630301	38043.185087	31.499546
577.597154	38105.131393	31.504564
577.851811	38179.795974	31.509581
578.820716	38252.841309	31.514599
579.599105	38323.892727	31.519616
580.270171	38390.321076	31.524634
581.021460	38453.077190	31.529652
581.398428	38518.316685	31.534669
582.455507	38580.617755	31.539687
583.245133	38648.874664	31.544704
583.739083	38716.467800	31.549722
584.389969	38775.243888	31.554740
585.030770	38835.111369	31.559757
586.262613	38867.801382	31.564775
587.014026	38913.144752	31.569792
587.720118	38961.125617	31.574810
588.410185	39008.707078	31.579828
588.596949	39062.226799	31.584845
588.930031	39108.827836	31.589863
589.800385	39163.454747	31.594880
589.667943	39221.079892	31.599898
590.399398	39281.264071	31.604916
590.796464	39345.722996	31.609933
591.060276	39403.476447	31.614951
591.744793	39474.926087	31.619968
592.326991	39531.066573	31.624986
593.076120	39592.887423	31.630004
593.193266	39661.175085	31.635021
593.952984	39722.390767	31.640039
594.755739	39793.703069	31.645056
595.181767	39866.764547	31.650074
595.911555	39926.438775	31.655092
596.120055	39998.890503	31.660109
596.896716	40067.174095	31.665127
597.437228	40145.160643	31.670144
597.852011	40219.844942	31.675162
598.467320	40271.537176	31.680180
599.115034	40342.028061	31.685197
599.491671	40415.883503	31.690215
600.024150	40488.159547	31.695232
600.562697	40562.355691	31.700250
601.390570	40616.664441	31.705268
602.376473	40692.013640	31.710285
602.644177	40755.022423	31.715303
603.335306	40810.381770	31.720320
603.801510	40883.726632	31.725338
604.726515	40947.060382	31.730356
604.927290	41018.281274	31.735373
605.934603	41074.196694	31.740391
606.455583	41141.102818	31.745408
606.904868	41214.792430	31.750426
608.610852	41257.163954	31.755444
609.331558	41314.056261	31.760461
609.911791	41369.599091	31.765479
610.596606	41430.266659	31.770496
610.879075	41485.131838	31.775514
611.531944	41542.975638	31.780532
611.881161	41600.413796	31.785549
612.590782	41648.821161	31.790567
613.588917	41709.477666	31.795584
613.992548	41767.812964	31.800602
615.109698	41837.052420	31.805620
615.319911	41885.360199	31.810637
615.603861	41941.702766	31.815655
616.279673	42003.714334	31.820672
616.820162	42069.523297	31.825690
617.259052	42134.333025	31.830708
618.067856	42202.269887	31.835725
618.391709	42268.536782	31.840743
619.343307	42315.819265	31.845760
619.642852	42393.613106	31.850778
620.418423	42455.134114	31.855796
620.830724	42515.801596	31.860813
621.255410	42579.930773	31.865831
622.020682	42652.749784	31.870848
622.711009	42728.628145	31.875866
623.640876	42789.132149	31.880884
624.041139	42855.710875	31.885901
624.864783	42925.925687	31.890919
625.566432	42992.081568	31.895936
625.762396	43065.097078	31.900954
626.561707	43127.130871	31.905972
627.432922	43190.733810	31.910989
627.664897	43256.110645	31.916007
628.486708	43334.696175	31.921024
629.279930	43405.365713	31.926042
629.491524	43469.525816	31.931060
629.838206	43548.790491	31.936077
630.270464	43622.486790	31.941095
631.330049	43687.799697	31.946112
631.630341	43760.189540	31.951130
632.704451	43834.999024	31.956148
632.885356	43903.686100	31.961165
633.146191	43974.127284	31.966183
633.853266	44050.040314	31.971200
634.176783	44136.024340	31.976218
635.034122	44205.917204	31.981236
635.748909	44286.833276	31.986253
637.385931	44326.239079	31.991271
638.807214	44380.143424	31.996288
639.047228	44445.725354	32.001306
639.757217	44505.544799	32.006324
640.362653	44561.403036	32.011341
641.060714	44625.723382	32.016359
641.395681	44678.337868	32.021376
641.808966	44737.009723	32.026394
642.764843	44802.778695	32.031412
643.375995	44865.435449	32.036429
644.018296	44925.973781	32.041447
644.781214	44979.732452	32.046464
645.154161	45040.885090	32.051482
645.650182	45092.150172	32.056500
646.455237	45167.289015	32.061517
647.121099	45239.696196	32.066535
647.779754	45309.445309	32.071552
647.999486	45375.532424	32.076570
648.774407	45443.869121	32.081588
649.304827	45511.576190	32.086605
649.477726	45591.202781	32.091623
650.319044	45663.921351	32.096640
650.740360	45749.374041	32.101658
651.595055	45828.388353	32.106676
652.349275	45917.010018	32.111693
652.969584	45989.948123	32.116711
653.576181	46059.585472	32.121728
653.660859	46153.101026	32.126746
654.466884	46239.201554	32.131764
655.148028	46315.693312	32.136781
656.189647	46403.612273	32.141799
656.927719	46480.313380	32.146816
657.244455	46565.559534	32.151834
658.228274	46647.838229	32.156852
658.718640	46730.602894	32.161869
659.392091	46809.524284	32.166887
660.238077	46891.330718	32.171904
660.574216	46975.600839	32.176922
661.785687	47042.747871	32.181940
662.710204	47113.660775	32.186957
663.689709	47182.164131	32.191975
665.015589	47236.568928	32.196992
665.629895	47306.351973	32.202010
666.556168	47355.501135	32.207028
667.652271	47409.801076	32.212045
667.776874	47476.813629	32.217063
668.677215	47510.317502	32.222080
668.796221	47572.226164	32.227098
669.524921	47628.043000	32.232116
670.299205	47668.527709	32.237133
671.262781	47697.645542	32.242151
672.387813	47728.555144	32.247168
672.930333	47780.559006	32.252186
673.320966	47819.372912	32.257204
674.063981	47867.126501	32.262221
674.319129	47917.923880	32.267239
674.845680	47960.168343	32.272256
675.459873	48016.610460	32.277274
676.202378	48073.802223	32.282292
676.754596	48125.960168	32.287309
676.813652	48192.253834	32.292327
677.476921	48247.846398	32.297344
678.199562	48321.566706	32.302362
678.503310	48390.147651	32.307380
679.490667	48449.412587	32.312397
679.964709	48523.693960	32.317415
681.133702	48581.990109	32.322432
681.616917	48655.352349	32.327450
682.041880	48723.101181	32.332468
682.649850	48787.791902	32.337485
683.229024	48868.324695	32.342503
683.938797	48939.361169	32.347520
684.474305	49005.771333	32.352538
685.424054	49094.914268	32.357556
685.970185	49166.858093	32.362573
686.494508	49237.259473	32.367591
687.605313	49324.519310	32.372608
687.948761	49391.662028	32.377626
688.806669	49468.675738	32.382644
689.792219	49542.539122	32.387661
690.438307	49621.799285	32.392679
691.034973	49688.858625	32.397696
691.825338	49765.710817	32.402714
692.367691	49840.952435	32.407732
693.288822	49911.782423	32.412749
693.801578	49997.288420	32.417767
694.427501	50070.693728	32.422784
694.947304	50152.942693	32.427802
695.395021	50227.674009	32.432820
696.436229	50302.528882	32.437837
696.648660	50390.328292	32.442855
697.411372	50464.044787	32.447872
698.181511	50554.927725	32.452890
698.771988	50645.012918	32.457908
699.486255	50730.998417	32.462925
700.207669	50835.192195	32.467943
701.027798	50909.043392	32.472960
701.904740	51002.452032	32.477978
702.246030	51075.401848	32.482996
703.052386	51159.023628	32.488013
703.511132	51251.067386	32.493031
704.250286	51335.833652	32.498048
705.711261	51405.494817	32.503066
706.712760	51477.637379	32.508084
707.516901	51547.981215	32.513101
708.088591	51612.858368	32.518119
708.922341	51675.418586	32.523136
709.199950	51749.754119	32.528154
709.909235	51823.614106	32.533172
710.634025	51883.254177	32.538189
711.351587	51958.176968	32.543207
712.155922	52028.273327	32.548224
712.947904	52088.676606	32.553242
713.646498	52162.088372	32.558260
714.498761	52231.868602	32.563277
715.329949	52302.700271	32.568295
715.951918	52371.147974	32.573312
716.586969	52437.693889	32.578330
717.124030	52517.419752	32.583348
717.781929	52591.366814	32.588365
718.556382	52671.588944	32.593383
718.856422	52753.367197	32.598400
719.553897	52822.966052	32.603418
719.977702	52901.329243	32.608436
720.869121	52997.106744	32.613453
721.144638	53088.248508	32.618471
722.070845	53166.545482	32.623488
722.860607	53265.007588	32.628506
723.167024	53361.236809	32.633524
724.157422	53451.651112	32.638541
724.582240	53548.275944	32.643559
725.404046	53648.874991	32.648576
726.408578	53735.819687	32.653594
726.853888	53819.943698	32.658612
728.057971	53905.443400	32.663629
728.854209	53996.626759	32.668647
729.822277	54088.199860	32.673664
730.688471	54172.261649	32.678682
731.539481	54263.892148	32.683700
732.603342	54332.074895	32.688717
733.277443	54431.032043	32.693735
734.011141	54494.069315	32.698752
734.674482	54566.091816	32.703770
734.802583	54656.359005	32.708788
735.649219	54740.451783	32.713805
736.169657	54831.285514	32.718823
737.016297	54913.532533	32.723840
737.947270	55014.450025	32.728858
738.383748	55104.610357	32.733876
739.517633	55178.624747	32.738893
740.378308	55270.536543	32.743911
740.861865	55356.729114	32.748928
741.774683	55440.710412	32.753946
742.278233	55524.425808	32.758964
743.175312	55606.936232	32.763981
744.032416	55709.242456	32.768999
744.432493	55790.945813	32.774016
744.963127	55881.839954	32.779034
745.520251	55971.530782	32.784052
746.390265	56053.684504	32.789069
747.221070	56134.698945	32.794087
747.463413	56222.449216	32.799104
748.310254	56314.400017	32.804122
749.004173	56402.006647	32.809140
749.848665	56495.060439	32.814157
750.840684	56579.643604	32.819175
752.123700	56654.047443	32.824192
753.390393	56740.226007	32.829210
753.769966	56820.911235	32.834228
754.701514	56891.492225	32.839245
755.204223	56970.387506	32.844263
755.991204	57049.297849	32.849280
756.947973	57124.948835	32.854298
757.635958	57204.936323	32.859316
758.956409	57283.289203	32.864333
759.396035	57362.003629	32.869351
759.844529	57436.556115	32.874368
761.269615	57509.668546	32.879386
761.355764	57596.196904	32.884404
762.419684	57676.423342	32.889421
762.995470	57757.741237	32.894439
763.714046	57839.017815	32.899456
764.568711	57918.050534	32.904474
764.777870	58007.317319	32.909492
765.715865	58086.798421	32.914509
766.604506	58181.119669	32.919527
767.149081	58265.260875	32.924544
768.190828	58360.616288	32.929562
768.682509	58456.927970	32.934580
769.222634	58538.554893	32.939597
769.939176	58635.949333	32.944615
770.536381	58734.313589	32.949632
771.629115	58827.863698	32.954650
772.398751	58922.709651	32.959668
773.221479	59019.940809	32.964685
774.015395	59116.334079	32.969703
774.654537	59215.467725	32.974720
775.797643	59303.212331	32.979738
776.627934	59403.854140	32.984756
777.416581	59493.430464	32.989773
778.025574	59579.556455	32.994791
778.413250	59679.613489	32.999808
779.561211	59763.763290	33.004826
780.727602	59857.092144	33.009844
781.850855	59946.570016	33.014861
782.315262	60043.500451	33.019879
782.872129	60135.705815	33.024896
784.352288	60206.748849	33.029914
784.666578	60304.298126	33.034932
785.304063	60385.014602	33.039949
786.136915	60471.367976	33.044967
786.860240	60571.003761	33.049984
787.542574	60658.578643	33.055002
788.259807	60745.823155	33.060020
789.229955	60821.367071	33.065037
790.026516	60902.170963	33.070055
790.840109	60986.227928	33.075072
791.675464	61073.174136	33.080090
792.234911	61159.684714	33.085108
792.681112	61234.811643	33.090125
793.419672	61321.316555	33.095143
794.137658	61427.254001	33.100160
795.231961	61512.566418	33.105178
795.749875	61602.688510	33.110196
796.856406	61696.696000	33.115213
797.203762	61782.526408	33.120231
798.081809	61870.382072	33.125248
799.063111	61969.943150	33.130266
799.412841	62067.025420	33.135284
800.297196	62170.692252	33.140301
801.207037	62266.663277	33.145319
801.699209	62369.247357	33.150336
802.637422	62471.085222	33.155354
803.444793	62572.736047	33.160372
804.182896	62676.725767	33.165389
805.228618	62783.853364	33.170407
805.684215	62886.240804	33.175424
806.970243	62992.800808	33.180442
807.355412	63104.847984	33.185460
807.996442	63208.818177	33.190477
808.878426	63317.411705	33.195495
809.666667	63436.985210	33.200512
810.991006	63531.930325	33.205530
811.882453	63650.948734	33.210548
812.904957	63747.607235	33.215565
814.028881	63847.648123	33.220583
814.545909	63942.332196	33.225600
816.018994	64030.229476	33.230618
816.520997	64126.053754	33.235636
817.406401	64228.942138	33.240653
817.997578	64320.736107	33.245671
819.002861	64423.780156	33.250688
819.904406	64517.698457	33.255706
820.788836	64618.391030	33.260724
821.277496	64706.021769	33.265741
822.066680	64813.163721	33.270759
822.453308	64921.845230	33.275776
823.425767	65028.308623	33.280794
824.211931	65139.429083	33.285812
824.553184	65238.967029	33.290829
825.699092	65349.762995	33.295847
826.432524	65464.134120	33.300864
827.181792	65572.448919	33.305882
827.861449	65686.694120	33.310900
828.959791	65803.447413	33.315917
829.688042	65909.003896	33.320935
830.227213	66025.279031	33.325952
831.298025	66131.837112	33.330970
832.472327	66234.336530	33.335988
833.074707	66335.244078	33.341005
833.891971	66436.443272	33.346023
834.758200	66541.993893	33.351040
835.852655	66645.563136	33.356058
836.263686	66738.370141	33.361076
837.256600	66836.890333	33.366093
837.928305	66938.538567	33.371111
838.473104	67050.055903	33.376128
839.629675	67154.173890	33.381146
840.624246	67260.118618	33.386164
841.185573	67386.190039	33.391181
842.283297	67476.238050	33.396199
843.452811	67584.298253	33.401216
844.330288	67674.148501	33.406234
845.122168	67774.967060	33.411252
846.322530	67878.380743	33.416269
847.419623	67968.835456	33.421287
848.054888	68067.652574	33.426304
848.907527	68166.738834	33.431322
849.656826	68265.949444	33.436340
850.186469	68365.265013	33.441357
851.723446	68464.610288	33.446375
852.216622	68574.047153	33.451392
852.769483	68682.110523	33.456410
853.369158	68779.237467	33.461428
854.126259	68896.973461	33.466445
855.000390	69004.380980	33.471463
855.849459	69127.505395	33.476480
856.442124	69243.317450	33.481498
857.419748	69357.217789	33.486516
858.099959	69481.407433	33.491533
858.972959	69599.230291	33.496551
859.696911	69715.915072	33.501568
860.928537	69838.357588	33.506586
861.819350	69960.147490	33.511604
862.411798	70081.903497	33.516621
863.274110	70199.889613	33.521639
863.780319	70328.004269	33.526656
864.953700	70445.367396	33.531674
865.731958	70568.891213	33.536692
866.875252	70700.944259	33.541709
867.593740	70813.611671	33.546727
868.676338	70931.889347	33.551744
869.744565	71059.584436	33.556762
870.743593	71178.951021	33.561780
871.518184	71296.338453	33.566797
872.991437	71401.717629	33.571815
873.725933	71521.115744	33.576832
874.226038	71633.809951	33.581850
875.139584	71744.815114	33.586868
876.127075	71860.699770	33.591885
877.054682	71979.494915	33.596903
878.013688	72094.646185	33.601920
878.867024	72189.291592	33.606938
879.388851	72303.749080	33.611956
880.164829	72419.740169	33.616973
881.311129	72516.520508	33.621991
882.085318	72627.818178	33.627008
883.010089	72730.568264	33.632026
883.890246	72835.973626	33.637044
884.582288	72954.850002	33.642061
885.563264	73060.929281	33.647079
886.125831	73179.277842	33.652096
887.174087	73287.363403	33.657114
888.117744	73403.004935	33.662132
888.675679	73507.978553	33.667149
889.987169	73626.166340	33.672167
890.918643	73734.317139	33.677184
891.924467	73854.791937	33.682202
892.879342	73966.485386	33.687220
893.598397	74083.487334	33.692237
894.643996	74183.325076	33.697255
895.396436	74309.151219	33.702272
896.267999	74415.962871	33.707290
896.941927	74541.979911	33.712308
897.949948	74664.152846	33.717325
899.030771	74778.112124	33.722343
899.898700	74903.462277	33.727360
900.338241	75013.442467	33.732378
901.498461	75141.389200	33.737396
902.562185	75258.412648	33.742413
903.340140	75380.304233	33.747431
904.092738	75509.689560	33.752448
905.359235	75630.101911	33.757466
906.266139	75747.823055	33.762484
907.474082	75875.318134	33.767501
908.310690	75988.823841	33.772519
909.190482	76105.584428	33.777536
910.032416	76235.168736	33.782554
911.660107	76342.369543	33.787572
912.720944	76456.480514	33.792589
913.214306	76554.907373	33.797607
914.183887	76664.995473	33.802624
915.129330	76773.925094	33.807642
916.168214	76897.832032	33.812660
916.756558	77016.338059	33.817677
917.863917	77118.809721	33.822695
918.857189	77235.754676	33.827712
919.365844	77360.551489	33.832730
920.445164	77471.511343	33.837748
921.129204	77586.756763	33.842765
922.208746	77706.067177	33.847783
922.991997	77836.840310	33.852800
923.950557	77955.084298	33.857818
924.809751	78069.198467	33.862836
925.390166	78194.835912	33.867853
926.598973	78314.508544	33.872871
927.356190	78438.362200	33.877888
927.993432	78572.595412	33.882906
929.323918	78684.925088	33.887924
930.150660	78811.140227	33.892941
930.898581	78906.415413	33.897959
931.930289	79029.027989	33.902976
932.583711	79143.117663	33.907994
933.575581	79259.897414	33.913012
934.372782	79392.549244	33.918029
935.284183	79505.032262	33.923047
936.362619	79627.451334	33.928064
937.145013	79749.766532	33.933082
938.080209	79875.737053	33.938100
938.702266	80005.841662	33.943117
939.542276	80135.571060	33.948135
940.302701	80265.832279	33.953152
941.516838	80401.173994	33.958170
942.504207	80536.028004	33.963188
942.873006	80685.994644	33.968205
943.914595	80821.025199	33.973223
945.273415	80964.957379	33.978240
946.302580	81101.515213	33.983258
947.138632	81229.899275	33.988276
947.944626	81375.983096	33.993293
949.115549	81520.600145	33.998311
950.249008	81648.345227	34.003328
951.687402	81785.082652	34.008346
953.240921	81897.191992	34.013364
953.808129	82028.828888	34.018381
954.854492	82148.107022	34.023399
955.836924	82284.420843	34.028416
956.749807	82407.906787	34.033434
957.532121	82536.124095	34.038452
958.713222	82666.080506	34.043469
959.701102	82792.951701	34.048487
960.505179	82928.457258	34.053504
961.275380	83056.496333	34.058522
962.715202	83176.413149	34.063540
963.508270	83320.584340	34.068557
964.486534	83430.517429	34.073575
965.710379	83566.997156	34.078592
966.696776	83692.489438	34.083610
967.585135	83810.550341	34.088628
968.591626	83948.951183	34.093645
969.363294	84070.515742	34.098663
970.361427	84203.653006	34.103680
971.167645	84331.694095	34.108698
972.315148	84453.333828	34.113716
973.325087	84585.333559	34.118733
974.233889	84724.494760	34.123751
975.483783	84847.037244	34.128768
976.039444	84983.961211	34.133786
977.021860	85111.903106	34.138804
978.342090	85251.729417	34.143821
979.090111	85373.317855	34.148839
979.928323	85503.118662	34.153856
980.553980	85642.975858	34.158874
981.695477	85744.757434	34.163892
982.578070	85876.677956	34.168909
983.609484	86005.989510	34.173927
985.384936	86107.469619	34.178944
986.116642	86238.986422	34.183962
987.349508	86341.085107	34.188980
988.266117	86466.105361	34.193997
988.912165	86571.422139	34.199015
990.142002	86693.010990	34.204032
990.692463	86815.018460	34.209050
991.786880	86944.319340	34.214068
992.861361	87066.693822	34.219085
993.417520	87206.091719	34.224103
994.460650	87318.412173	34.229120
995.352999	87457.985856	34.234138
996.171412	87587.005698	34.239156
997.199333	87731.694240	34.244173
998.241382	87876.659741	34.249191
999.094749	88003.520185	34.254208
1000.178270	88142.637883	34.259226
1001.066280	88290.090559	34.264244
1001.971821	88428.947527	34.269261
1002.198763	88579.327720	34.274279
1003.570520	88744.286570	34.279296
1004.553426	88885.454991	34.284314
1005.604361	89031.299507	34.289332
1006.663331	89186.035169	34.294349
1007.706836	89336.973684	34.299367
1008.875283	89493.667198	34.304384
1010.058295	89650.599839	34.309402
1011.140089	89788.153674	34.314420
1011.875211	89948.182635	34.319437
1012.873465	90100.879109	34.324455
1014.466299	90259.249765	34.329472
1015.271131	90410.290601	34.334490
1016.379405	90552.999335	34.339508
1017.768936	90693.754297	34.344525
1018.603556	90853.571674	34.349543
1020.148563	90976.152660	34.354560
1020.592269	91146.811224	34.359578
1021.803143	91272.236124	34.364596
1022.894216	91420.044487	34.369613
1023.945400	91565.140605	34.374631
1024.895447	91707.432970	34.379648
1025.938207	91856.649701	34.384666
1027.006247	92001.638492	34.389684
1028.582242	92142.455293	34.394701
1029.748147	92269.252856	34.399719
1031.705285	92390.625049	34.404736
1032.457725	92517.806057	34.409754
1033.635055	92647.785396	34.414772
1034.769137	92765.894099	34.419789
1035.373356	92894.726366	34.424807
1036.442595	93023.162829	34.429824
1037.156244	93152.187908	34.434842
1038.295496	93256.320000	34.439860
1039.160034	93384.658291	34.444877
1040.176813	93501.587795	34.449895
1041.527326	93610.210436	34.454912
1042.043524	93731.249932	34.459930
1043.220491	93848.294931	34.464948
1043.916444	93970.129414	34.469965
1044.398959	94111.252850	34.474983
1045.403872	94246.228033	34.480000
1046.321247	94384.399644	34.485018
1047.331479	94518.154817	34.490036
1048.077992	94669.335209	34.495053
1049.384430	94818.238913	34.500071
1050.390188	94953.237203	34.505088
1051.144823	95116.918670	34.510106
1052.170231	95262.428887	34.515124
1053.332271	95408.437019	34.520141
1054.399977	95567.934956	34.525159
1055.556970	95710.473013	34.530176
1056.429260	95865.044717	34.535194
1057.525408	96026.091202	34.540212
1058.576127	96185.368476	34.545229
1059.549637	96343.330701	34.550247
1060.712380	96503.870246	34.555264
1061.555998	96664.777996	34.560282
1062.449900	96828.177700	34.565300
1063.789500	96982.208245	34.570317
1064.658937	97157.304936	34.575335
1065.892561	97320.173351	34.580352
1067.334184	97481.984989	34.585370
1068.336828	97639.281015	34.590388
1069.392660	97800.251616	34.595405
1070.544455	97965.136796	34.600423
1072.006052	98117.833402	34.605440
1072.945685	98283.931354	34.610458
1073.916375	98437.676140	34.615476
1075.304825	98592.848585	34.620493
1075.915117	98759.274414	34.625511
1076.990704	98913.961034	34.630528
1078.481377	99082.817807	34.635546
1079.289910	99241.946191	34.640564
1080.673927	99392.158231	34.645581
1081.414082	99563.839466	34.650599
1083.011494	99696.823150	34.655616
1084.184451	99852.772302	34.660634
1085.692591	100001.494397	34.665652
1087.288646	100150.247757	34.670669
1088.362846	100293.561556	34.675687
1089.201929	100433.769072	34.680704
1090.591799	100580.242277	34.685722
1091.362429	100733.110447	34.690740
1092.354059	100866.513580	34.695757
1093.461356	101014.894678	34.700775
1094.471733	101165.772441	34.705792
1095.428677	101309.016256	34.710810
1096.025594	101457.462374	34.715828
1097.390166	101600.870936	34.720845
1098.066787	101751.875183	34.725863
1099.153572	101882.465942	34.730880
1099.698995	102028.411868	34.735898
1100.918609	102174.023679	34.740916
1102.138030	102329.861850	34.745933
1103.347129	102484.626998	34.750951
1105.260063	102615.881411	34.755968
1106.469663	102753.822936	34.760986
1107.579246	102887.168239	34.766004
1109.015532	103018.785471	34.771021
1109.838000	103168.282291	34.776039
1111.009543	103302.607241	34.781056
1112.014824	103457.094824	34.786074
1112.735949	103605.250033	34.791092
1113.647274	103749.053900	34.796109
1114.556829	103914.760259	34.801127
1115.360428	104074.934902	34.806144
1116.259612	104222.293632	34.811162
1117.571805	104391.495696	34.816180
1119.088936	104552.635874	34.821197
1119.957599	104728.928872	34.826215
1120.894658	104885.885670	34.831232
1122.183224	105055.020282	34.836250
1123.255283	105219.412599	34.841268
1124.206617	105386.388265	34.846285
1125.234766	105570.857452	34.851303
1126.600384	105733.637163	34.856320
1127.884528	105905.227649	34.861338
1128.390717	106079.847928	34.866356
1129.817449	106254.209158	34.871373
1130.653465	106433.608326	34.876391
1132.105697	106605.942872	34.881408
1133.333067	106771.916004	34.886426
1134.146893	106963.284084	34.891444
1135.733803	107142.980499	34.896461
1136.249769	107341.892367	34.901479
1137.491275	107506.349364	34.906496
1139.131724	107683.091981	34.911514
1140.105585	107869.441856	34.916532
1141.584864	108044.978579	34.921549
1142.244577	108222.007687	34.926567
1143.784608	108392.935957	34.931584
1145.169911	108567.124294	34.936602
1146.290170	108743.729523	34.941620
1147.867531	108912.725075	34.946637
1149.060042	109082.175427	34.951655
1150.100129	109244.555892	34.956672
1151.336666	109417.381494	34.961690
1152.205362	109592.760652	34.966708
1153.795247	109770.792401	34.971725
1154.664578	109938.420202	34.976743
1155.522421	110103.006408	34.981760
1156.749328	110276.871343	34.986778
1157.841182	110451.429940	34.991796
1159.020866	110598.934926	34.996813
1159.821901	110759.135355	35.001831
1160.634306	110930.633842	35.006848
1161.990228	111096.324840	35.011866
1163.214391	111265.152246	35.016884
1164.530747	111422.021427	35.021901
1165.683446	111593.153898	35.026919
1167.196542	111755.754251	35.031936
1168.633186	111916.424481	35.036954
1169.570043	112072.427604	35.041972
1170.800159	112231.733752	35.046989
1172.287849	112389.525012	35.052007
1173.784924	112534.984383	35.057024
1175.365640	112688.280906	35.062042
1176.262480	112861.596123	35.067060
1177.695467	112993.869551	35.072077
1178.780145	113149.836926	35.077095
1179.955222	113307.113969	35.082112
1181.203165	113449.491033	35.087130
1181.824964	113632.243485	35.092148
1183.090286	113774.360079	35.097165
1184.303598	113935.775199	35.102183
1185.527746	114099.392710	35.107200
1186.943835	114256.814642	35.112218
1187.743661	114422.242674	35.117236
1189.169255	114570.263876	35.122253
1190.171092	114735.953060	35.127271
1191.580415	114899.369057	35.132288
1192.746121	115073.517779	35.137306
1194.099693	115231.538179	35.142324
1195.116996	115389.980235	35.147341
1196.002289	115562.423219	35.152359
1196.921225	115749.012012	35.157376
1198.460555	115914.623436	35.162394
1199.347049	116087.145761	35.167412
1200.589875	116265.487966	35.172429
1201.929689	116433.945555	35.177447
1203.107583	116609.628697	35.182464
1204.424445	116784.999708	35.187482
1205.405830	116959.551532	35.192500
1206.711263	117133.673134	35.197517
1207.880594	117318.682378	35.202535
1208.936224	117494.897551	35.207552
1210.366003	117671.687596	35.212570
1211.010463	117859.430785	35.217588
1212.245369	118044.998340	35.222605
1213.199424	118239.976480	35.227623
1214.363842	118421.366357	35.232640
1216.411827	118596.836088	35.237658
1217.330578	118789.538206	35.242676
1218.706534	118971.746772	35.247693
1219.674998	119160.479980	35.252711
1220.978139	119348.857409	35.257728
1222.322769	119522.773599	35.262746
1223.097782	119705.089188	35.267764
1224.216313	119879.246333	35.272781
1225.442454	120045.434352	35.277799
1226.480745	120220.252408	35.282816
1227.634352	120406.438650	35.287834
1228.783082	120595.071251	35.292852
1230.248915	120772.801187	35.297869
1231.326342	120973.365276	35.302887
1232.140785	121151.859912	35.307904
1234.316396	121337.864933	35.312922
1235.144062	121536.054021	35.317940
1236.210090	121719.223881	35.322957
1237.476623	121914.344400	35.327975
1238.318799	122115.397855	35.332992
1239.564285	122295.300855	35.338010
1240.526292	122501.530989	35.343028
1241.817921	122698.401123	35.348045
1243.191440	122913.890885	35.353063
1244.452535	123117.367786	35.358080
1245.811848	123319.070068	35.363098
1246.747847	123530.669961	35.368116
1248.189638	123742.064450	35.373133
1249.540742	123949.447187	35.378151
1250.707902	124158.254061	35.383168
1252.537760	124363.030626	35.388186
1253.719169	124581.933611	35.393204
1254.876931	124769.061757	35.398221
1256.108256	124981.234114	35.403239
1257.756423	125182.866472	35.408256
1259.158055	125377.142100	35.413274
1260.551841	125588.292712	35.418292
1261.579352	125790.471612	35.423309
1263.186262	125993.307262	35.428327
1264.400467	126186.263100	35.433344
1265.462894	126391.430377	35.438362
1266.565003	126605.358727	35.443380
1268.076020	126805.922872	35.448397
1269.635074	127000.121726	35.453415
1270.598866	127220.169982	35.458432
1272.534390	127407.395317	35.463450
1273.689330	127613.975842	35.468468
1275.015652	127822.126834	35.473485
1276.157874	128007.062794	35.478503
1277.432274	128213.882187	35.483520
1278.960636	128398.924072	35.488538
1280.190800	128595.251397	35.493556
1281.415842	128795.634818	35.498573
1282.828206	128985.247023	35.503591
1284.351221	129185.940611	35.508608
1285.684166	129369.968556	35.513626
1287.062368	129573.563752	35.518644
1288.260046	129760.288888	35.523661
1289.793254	129949.369031	35.528679
1290.914759	130150.399444	35.533696
1292.146741	130329.268137	35.538714
1293.380968	130510.342053	35.543732
1294.414528	130675.878514	35.548749
1295.443753	130865.995159	35.553767
1296.138386	131056.685724	35.558784
1297.988554	131245.394813	35.563802
1298.974152	131438.981038	35.568820
1300.145746	131619.489245	35.573837
1301.398256	131818.293555	35.578855
1302.706303	131998.136329	35.583872
1304.008516	132193.045724	35.588890
1305.349527	132386.290516	35.593908
1306.726459	132585.954660	35.598925
1308.056990	132775.884196	35.603943
1309.134572	132987.876167	35.608960
1310.507232	133187.253784	35.613978
1312.007501	133383.229493	35.618996
1312.959570	133602.974961	35.624013
1314.615014	133800.360629	35.629031
1315.928279	133999.829368	35.634048
1317.284748	134209.581335	35.639066
1318.133901	134414.017660	35.644084
1319.369566	134626.845558	35.649101
1320.739017	134834.990790	35.654119
1321.875914	135064.677514	35.659136
1323.080210	135277.920665	35.664154
1324.660403	135506.361990	35.669172
1326.280788	135719.871701	35.674189
1328.105457	135928.674693	35.679207
1329.267002	136132.921414	35.684224
1330.936131	136343.437432	35.689242
1332.281407	136559.860841	35.694260
1333.288592	136764.022457	35.699277
1334.979199	136971.257542	35.704295
1336.081894	137186.558305	35.709312
1337.257193	137402.368662	35.714330
1338.722766	137614.801642	35.719348
1340.003742	137840.634878	35.724365
1341.073577	138042.476345	35.729383
1342.698177	138272.909064	35.734400
1344.717181	138478.188972	35.739418
1345.677065	138687.757294	35.744436
1346.759457	138912.869890	35.749453
1348.610918	139123.769618	35.754471
1349.837854	139337.900345	35.759488
1351.059809	139554.631389	35.764506
1352.304408	139764.390128	35.769524
1353.747984	139993.673633	35.774541
1354.932425	140214.534235	35.779559
1355.960519	140427.056795	35.784576
1357.716744	140640.909910	35.789594
1359.191673	140866.874598	35.794612
1360.415635	141087.545202	35.799629
1361.795599	141302.223226	35.804647
1362.793730	141532.298949	35.809664
1364.194606	141746.381112	35.814682
1365.704477	141948.090170	35.819700
1367.176718	142156.549231	35.824717
1368.535763	142362.682958	35.829735
1369.599229	142568.991798	35.834752
1371.443843	142774.658219	35.839770
1373.019767	142968.948946	35.844788
1373.988916	143172.298311	35.849805
1375.359011	143369.260606	35.854823
1376.757143	143580.897131	35.859840
1377.926111	143799.479348	35.864858
1379.897406	143991.001253	35.869876
1380.667907	144216.595634	35.874893
1382.264791	144434.581969	35.879911
1383.239734	144646.039526	35.884928
1384.786041	144859.359712	35.889946
1386.154722	145084.117466	35.894964
1387.602181	145300.080187	35.899981
1389.082134	145519.005325	35.904999
1390.058929	145737.061283	35.910016
1391.232021	145970.095676	35.915034
1392.827360	146194.369040	35.920052
1393.967524	146434.485239	35.925069
1395.275860	146662.648364	35.930087
1396.817412	146898.939511	35.935104
1398.109497	147135.005866	35.940122
1399.692172	147376.744824	35.945140
1400.881595	147626.800480	35.950157
1402.527340	147858.125713	35.955175
1403.749991	148098.875213	35.960192
1405.441666	148339.551986	35.965210
1406.842143	148572.404540	35.970228
1408.032765	148826.969655	35.975245
1409.556210	149065.485498	35.980263
1410.595638	149315.628870	35.985280
1412.141539	149558.062011	35.990298
1414.226021	149801.932654	35.995316
1415.372032	150059.607830	36.000333
1417.198284	150285.470534	36.005351
1418.492147	150529.751190	36.010368
1419.899124	150782.192803	36.015386
1421.720948	151006.172229	36.020404
1422.948300	151252.535333	36.025421
1424.686261	151496.803347	36.030439
1426.130053	151730.229482	36.035456
1427.481150	151952.553278	36.040474
1429.211843	152197.372805	36.045492
1430.272611	152432.234020	36.050509
1431.890050	152666.070236	36.055527
1433.563003	152889.135239	36.060544
1435.044340	153121.132550	36.065562
1436.770670	153350.987886	36.070580
1438.247802	153570.158183	36.075597
1439.566174	153801.894511	36.080615
1440.766931	154025.473227	36.085632
1442.638371	154241.859293	36.090650
1444.464375	154443.254622	36.095668
1445.446443	154643.491989	36.100685
1446.878131	154848.426486	36.105703
1448.349055	155054.826792	36.110720
1449.719066	155271.248427	36.115738
1451.074621	155482.259607	36.120756
1452.470082	155694.343518	36.125773
1453.555014	155904.728307	36.130791
1454.737493	156125.153897	36.135808
1455.948467	156353.995759	36.140826
1457.481490	156571.490211	36.145844
1458.760735	156803.811194	36.150861
1460.026131	157031.038571	36.155879
1461.835098	157261.756869	36.160896
1463.847262	157479.180929	36.165914
1465.761301	157696.812154	36.170932
1467.356615	157920.784855	36.175949
1468.912120	158135.508602	36.180967
1470.238436	158364.434239	36.185984
1471.456184	158589.473004	36.191002
1472.755403	158801.084107	36.196020
1474.326506	159034.540292	36.201037
1475.544805	159260.052473	36.206055
1477.272532	159491.166217	36.211072
1478.407707	159730.808510	36.216090
1479.756168	159957.420410	36.221108
1481.078651	160203.528876	36.226125
1482.565964	160431.732265	36.231143
1484.369482	160684.273132	36.236160
1485.688373	160927.204168	36.241178
1487.506576	161151.352268	36.246196
1488.813520	161393.172404	36.251213
1490.618057	161641.205236	36.256231
1492.477584	161873.087135	36.261248
1493.759662	162106.672878	36.266266
1495.228665	162336.134168	36.271284
1496.664968	162586.578192	36.276301
1498.087302	162816.569914	36.281319
1499.544360	163058.618349	36.286336
1501.406867	163293.654088	36.291354
1503.468204	163515.267185	36.296372
1504.680299	163765.564732	36.301389
1506.400775	163988.414328	36.306407
1508.102929	164220.412349	36.311424
1509.216133	164458.998943	36.316442
1510.731634	164682.950672	36.321460
1512.154583	164924.078353	36.326477
1513.770206	165156.768217	36.331495
1515.642661	165378.308431	36.336512
1516.921198	165626.971973	36.341530
1518.402889	165827.700603	36.346548
1520.272798	166076.831259	36.351565
1521.318128	166304.050975	36.356583
1523.522324	166514.878588	36.361600
1524.893401	166735.986516	36.366618
1526.451056	166950.457984	36.371636
1527.882069	167162.249188	36.376653
1528.961059	167366.550721	36.381671
1530.281820	167577.575385	36.386688
1531.402543	167798.260021	36.391706
1533.002399	168018.552725	36.396724
1534.591238	168245.000181	36.401741
1536.097800	168461.847553	36.406759
1537.438122	168689.986060	36.411776
1538.571912	168920.822418	36.416794
1540.256550	169159.538376	36.421812
1541.557062	169407.030991	36.426829
1542.941085	169647.395963	36.431847
1544.610386	169877.112865	36.436864
1545.934232	170132.851357	36.441882
1547.304835	170373.108810	36.446900
1548.725073	170640.784293	36.451917
1550.349243	170894.856440	36.456935
1551.851182	171148.239303	36.461952
1553.052539	171423.045788	36.466970
1554.816072	171690.534385	36.471988
1556.306744	171957.966665	36.477005
1558.185053	172227.609842	36.482023
1559.829599	172497.025599	36.487040
1561.347733	172763.989608	36.492058
1563.504773	173006.320122	36.497076
1564.754920	173285.749321	36.502093
1566.183743	173545.096015	36.507111
1568.211266	173804.070195	36.512128
1569.367470	174073.548796	36.517146
1571.495586	174336.912419	36.522164
1572.533301	174600.641263	36.527181
1574.001163	174883.700544	36.532199
1575.510427	175156.301798	36.537216
1577.189851	175434.815023	36.542234
1578.806636	175705.652163	36.547252
1580.365600	175981.409933	36.552269
1581.948565	176259.398572	36.557287
1583.633025	176526.690834	36.562304
1585.177399	176807.860953	36.567322
1587.362560	177073.542126	36.572340
1589.050875	177346.307071	36.577357
1591.221188	177610.332056	36.582375
1593.142309	177863.842692	36.587392
1594.231985	178125.035758	36.592410
1596.150605	178377.433433	36.597428
1597.583241	178642.165705	36.602445
1599.198115	178911.349320	36.607463
1600.917183	179157.059070	36.612480
1602.316168	179432.433680	36.617498
1604.010399	179694.694976	36.622516
1605.525241	179958.191705	36.627533
1606.948056	180221.184477	36.632551
1608.501049	180489.766192	36.637568
1609.583810	180752.955796	36.642586
1611.194733	181014.071103	36.647604
1612.886364	181260.558552	36.652621
1614.122213	181517.067269	36.657639
1616.003966	181772.307595	36.662656
1617.348037	182022.293061	36.667674
1619.544523	182267.970106	36.672692
1620.837171	182529.982481	36.677709
1622.273153	182785.134564	36.682727
1623.877234	183045.057693	36.687744
1625.072809	183325.437851	36.692762
1626.786624	183592.744234	36.697780
1628.149623	183864.637837	36.702797
1629.980371	184155.187562	36.707815
1631.459707	184424.464875	36.712832
1632.638735	184702.661120	36.717850
1634.475146	184987.226112	36.722868
1636.296809	185275.513168	36.727885
1637.665166	185570.573982	36.732903
1639.649197	185846.885595	36.737920
1641.221353	186141.232511	36.742938
1643.086887	186426.677454	36.747956
1645.359653	186703.722444	36.752973
1647.159061	186990.513795	36.757991
1649.073068	187273.596014	36.763008
1650.609020	187562.628074	36.768026
1652.224800	187828.439453	36.773044
1654.215734	188115.194641	36.778061
1655.558224	188396.877036	36.783079
1657.332528	188660.954811	36.788096
1658.700932	188959.438159	36.793114
1660.443733	189235.224502	36.798132
1662.365028	189515.057698	36.803149
1663.607481	189807.183144	36.808167
1665.156248	190090.784482	36.813184
1666.781377	190371.989545	36.818202
1668.574119	190663.779006	36.823220
1670.526204	190962.512130	36.828237
1672.020461	191257.893291	36.833255
1674.139106	191530.904615	36.838272
1675.993284	191816.295060	36.843290
1677.950368	192089.588986	36.848308
1680.104541	192365.569028	36.853325
1681.570758	192646.977461	36.858343
1683.369060	192915.123197	36.863360
1684.870236	193202.760628	36.868378
1686.569159	193477.143915	36.873396
1687.997558	193751.863574	36.878413
1689.829219	194035.595126	36.883431
1691.820047	194307.905969	36.888448
1693.055327	194588.981274	36.893466
1695.027458	194864.179089	36.898484
1696.935195	195141.749294	36.903501
1698.964795	195413.387257	36.908519
1701.164323	195651.721483	36.913536
1703.237446	195908.569093	36.918554
1704.690943	196151.174382	36.923572
1706.588893	196384.660774	36.928589
1707.802257	196612.647000	36.933607
1709.565561	196850.370664	36.938624
1711.180002	197088.931357	36.943642
1712.727746	197325.231807	36.948660
1714.240245	197565.156246	36.953677
1715.547737	197805.050872	36.958695
1716.839261	198062.312456	36.963712
1718.638283	198328.303340	36.968730
1720.067799	198593.833834	36.973748
1721.972684	198849.554878	36.978765
1723.236444	199125.331948	36.983783
1725.595885	199384.169250	36.988800
1727.433464	199645.489616	36.993818
1729.132040	199903.266605	36.998836
1731.150401	200169.714129	37.003853
1732.645519	200441.310572	37.008871
1734.169847	200712.269072	37.013888
1735.765885	200980.463105	37.018906
1737.245730	201255.366235	37.023924
1739.177938	201530.503546	37.028941
1740.386779	201832.489326	37.033959
1742.141201	202111.173810	37.038976
1743.978037	202405.142272	37.043994
1745.666157	202697.181078	37.049012
1747.084137	202993.148545	37.054029
1748.992410	203292.340077	37.059047
1750.761267	203581.108348	37.064064
1752.588359	203875.098695	37.069082
1754.334161	204179.575929	37.074100
1756.180844	204481.956947	37.079117
1757.478880	204792.944359	37.084135
1759.245799	205083.599202	37.089152
1761.098407	205398.297337	37.094170
1763.166891	205711.693467	37.099188
1765.018546	206029.175178	37.104205
1766.397495	206341.668594	37.109223
1768.050464	206656.316287	37.114240
1769.581410	206972.140215	37.119258
1771.719973	207284.225996	37.124276
1773.704715	207599.587648	37.129293
1775.341208	207927.523216	37.134311
1777.128367	208229.653552	37.139328
1779.142345	208560.033467	37.144346
1780.863631	208871.114598	37.149364
1782.791871	209175.144128	37.154381
1784.804431	209495.982679	37.159399
1786.883730	209809.195234	37.164416
1788.832812	210116.057066	37.169434
1790.634686	210417.383264	37.174452
1792.762862	210727.088763	37.179469
1794.424528	211035.359095	37.184487
1796.240225	211330.200122	37.189504
1798.501958	211620.236293	37.194522
1800.317168	211897.217502	37.199540
1801.813971	212175.710440	37.204557
1803.762042	212442.732268	37.209575
1805.656990	212716.771636	37.214592
1807.167583	212980.703897	37.219610
1808.616501	213263.347886	37.224628
1810.566231	213537.991383	37.229645
1812.042146	213825.902260	37.234663
1814.029521	214114.621904	37.239680
1816.189247	214389.616459	37.244698
1817.569638	214678.434891	37.249716
1819.380955	214959.885892	37.254733
1821.265746	215259.037531	37.259751
1823.256541	215537.199521	37.264768
1824.957650	215830.606049	37.269786
1826.629537	216131.560077	37.274804
1828.753423	216408.231690	37.279821
1830.646437	216710.727480	37.284839
1832.408359	217005.627505	37.289856
1834.481789	217302.193351	37.294874
1835.971249	217603.690542	37.299892
1837.785777	217892.542350	37.304909
1839.828705	218203.679848	37.309927
1841.800231	218504.025103	37.314944
1843.778312	218797.603179	37.319962
1845.620710	219094.263923	37.324980
1847.701399	219385.161750	37.329997
1849.560713	219680.590593	37.335015
1851.820527	219968.186487	37.340032
1853.913687	220252.813452	37.345050
1856.005160	220542.546006	37.350068
1858.425978	220811.378703	37.355085
1860.176279	221107.681231	37.360103
1862.084014	221421.037718	37.365120
1864.633379	221681.028528	37.370138
1866.473894	221954.223685	37.375156
1868.562543	222221.133321	37.380173
1870.034231	222483.519951	37.385191
1871.879755	222756.729854	37.390208
1874.176099	223013.286220	37.395226
1875.580349	223295.049980	37.400244
1877.791449	223548.713888	37.405261
1879.765769	223813.971038	37.410279
1881.902145	224074.365537	37.415296
1883.761697	224330.335230	37.420314
1885.209292	224594.599268	37.425332
1887.060908	224858.304830	37.430349
1888.593296	225129.439361	37.435367
1890.315394	225403.058861	37.440384
1892.267173	225670.357348	37.445402
1893.737847	225952.805544	37.450420
1895.225050	226235.175888	37.455437
1897.334104	226516.178684	37.460455
1898.990778	226799.336708	37.465472
1901.230908	227085.095084	37.470490
1902.725168	227363.150724	37.475508
1904.328933	227608.123735	37.480525
1905.969155	227890.170554	37.485543
1907.812300	228155.348149	37.490560
1909.725760	228433.747056	37.495578
1911.494639	228708.030127	37.500596
1913.402338	228982.774562	37.505613
1915.103768	229285.133628	37.510631
1916.941929	229564.309962	37.515648
1918.790153	229853.847574	37.520666
1920.256635	230161.859638	37.525684
1921.849956	230456.061914	37.530701
1923.694306	230762.187436	37.535719
1925.338885	231082.314256	37.540736
1927.679927	231396.134661	37.545754
1929.253578	231723.411640	37.550772
1931.045245	232042.807277	37.555789
1933.233752	232368.388859	37.560807
1934.933159	232704.182912	37.565824
1937.493029	233017.262820	37.570842
1939.029372	233353.872344	37.575860
1941.212793	233666.175947	37.580877
1943.534207	234007.082393	37.585895
1945.347849	234334.050745	37.590912
1947.473289	234654.544902	37.595930
1949.693166	234989.806978	37.600948
1951.524829	235310.197439	37.605965
1953.578082	235634.820700	37.610983
1955.563941	235975.533035	37.616000
1957.921749	236284.794598	37.621018
1959.740855	236630.640675	37.626036
1961.708437	236948.677908	37.631053
1963.896316	237274.808802	37.636071
1965.556773	237604.173862	37.641088
1967.922716	237925.732028	37.646106
1969.970485	238252.853256	37.651124
1972.102443	238577.853949	37.656141
1974.147326	238901.345443	37.661159
1976.160637	239229.059182	37.666176
1978.368326	239542.417700	37.671194
1980.264837	239871.904382	37.676212
1982.412270	240191.827317	37.681229
1984.973504	240504.344950	37.686247
1986.773491	240826.763120	37.691264
1989.179819	241128.308876	37.696282
1991.204278	241436.392960	37.701300
1993.117824	241741.625230	37.706317
1995.415272	242057.338361	37.711335
1997.039982	242357.309383	37.716352
1999.492523	242657.149771	37.721370
2001.650297	242955.056430	37.726388
2003.911843	243246.165449	37.731405
2005.882635	243537.346664	37.736423
2007.758990	243838.754478	37.741440
2010.163725	244127.734531	37.746458
2011.914891	244401.146809	37.751476
2013.772266	244665.932011	37.756493
2015.355881	244933.072627	37.761511
2017.240856	245207.913154	37.766528
2019.036158	245487.619997	37.771546
2020.534270	245775.833012	37.776564
2022.626261	246051.658406	37.781581
2024.581008	246345.769334	37.786599
2026.204232	246648.595183	37.791616
2027.812464	246947.334494	37.796634
2029.531081	247266.707935	37.801652
2031.529171	247571.457512	37.806669
2033.819057	247884.747001	37.811687
2035.415535	248200.204655	37.816704
2037.736472	248516.487869	37.821722
2039.190351	248848.988313	37.826740
2041.081812	249183.223537	37.831757
2043.599089	249518.630250	37.836775
2045.499400	249854.541977	37.841792
2047.410405	250187.404524	37.846810
2049.620267	250536.883750	37.851828
2051.445154	250879.236134	37.856845
2053.665634	251220.230967	37.861863
2055.283395	251579.382715	37.866880
2057.679471	251917.226659	37.871898
2059.298936	252285.117788	37.876916
2061.674365	252644.380117	37.881933
2064.012714	252995.596634	37.886951
2065.988276	253360.944058	37.891968
2067.885073	253721.452904	37.896986
2070.025401	254078.850146	37.902004
2072.204316	254444.014967	37.907021
2074.301442	254796.441560	37.912039
2076.347540	255169.427237	37.917056
2079.040490	255517.594601	37.922074
2081.087360	255883.291003	37.927092
2083.168066	256240.853924	37.932109
2085.620726	256597.443943	37.937127
2087.596420	256966.887612	37.942144
2089.740853	257318.599615	37.947162
2092.148604	257678.500789	37.952180
2094.166755	258036.228898	37.957197
2096.273272	258385.001824	37.962215
2098.763571	258735.543353	37.967232
2101.185786	259073.801305	37.972250
2103.375005	259424.213736	37.977268
2105.699325	259764.190102	37.982285
2108.223313	260092.704004	37.987303
2110.125179	260437.193710	37.992320
2112.293505	260769.549849	37.997338
2114.558180	261112.103023	38.002356
2116.659349	261439.542440	38.007373
2118.963662	261771.497107	38.012391
2120.689751	262121.529104	38.017408
2123.084386	262435.408693	38.022426
2125.000665	262754.673682	38.027444
2126.876446	263069.144241	38.032461
2129.028930	263363.502835	38.037479
2130.928828	263678.376573	38.042496
2132.923305	263984.903390	38.047514
2135.120652	264292.643034	38.052532
2137.039764	264608.530644	38.057549
2139.139392	264923.907218	38.062567
2140.836320	265246.740222	38.067584
2143.174231	265560.961756	38.072602
2145.363460	265898.146155	38.077620
2147.118506	266229.252109	38.082637
2149.815738	266554.543946	38.087655
2151.703016	266892.158013	38.092672
2153.838445	267226.760772	38.097690
2155.974283	267562.049570	38.102708
2158.079756	267911.543812	38.107725
2160.109694	268242.480457	38.112743
2162.621153	268584.797795	38.117760
2165.034355	268921.135726	38.122778
2167.339884	269261.377612	38.127796
2169.445900	269594.106520	38.132813
2172.155255	269923.005596	38.137831
2174.410476	270264.703912	38.142848
2176.375336	270596.566512	38.147866
2178.340157	270933.535316	38.152884
2180.497956	271279.314002	38.157901
2182.768879	271624.947842	38.162919
2184.824763	271977.805046	38.167936
2186.730518	272317.628810	38.172954
2188.880861	272671.182504	38.177972
2191.261172	273036.893434	38.182989
2193.420071	273383.231342	38.188007
2195.367998	273741.847202	38.193024
2197.584016	274110.480339	38.198042
2199.939854	274464.789211	38.203060
2201.831356	274824.074601	38.208077
2204.554306	275179.697065	38.213095
2206.190873	275552.283472	38.218112
2208.482678	275917.627590	38.223130
2211.027692	276285.598883	38.228148
2213.250981	276649.277175	38.233165
2215.863175	276999.353728	38.238183
2218.188188	277370.281150	38.243200
2220.452100	277729.481817	38.248218
2222.519005	278085.995479	38.253236
2224.759128	278450.737677	38.258253
2227.144654	278806.489317	38.263271
2229.466047	279171.980499	38.268288
2231.742079	279520.636319	38.273306
2234.596005	279867.574552	38.278324
2236.807936	280227.239905	38.283341
2239.292544	280563.236768	38.288359
2241.133213	280916.101775	38.293376
2243.402822	281265.443738	38.298394
2245.347031	281590.297545	38.303412
2247.513861	281911.076763	38.308429
2249.533964	282232.310931	38.313447
2251.874722	282554.103749	38.318464
2254.081182	282870.024126	38.323482
2257.000234	283187.203093	38.328500
2258.882837	283522.582473	38.333517
2261.191176	283837.495364	38.338535
2263.091407	284168.146502	38.343552
2264.788280	284509.371944	38.348570
2267.296430	284851.814842	38.353588
2269.476750	285190.880023	38.358605
2272.034269	285543.069306	38.363623
2273.829269	285888.367934	38.368640
2275.677790	286245.775003	38.373658
2278.128882	286591.222978	38.378676
2280.233220	286951.916576	38.383693
2282.498323	287316.064509	38.388711
2284.807163	287684.040950	38.393728
2286.780178	288053.797615	38.398746
2289.071746	288423.681158	38.403764
2291.522254	288806.062646	38.408781
2294.198319	289182.565237	38.413799
2296.169583	289556.460991	38.418816
2298.264041	289947.610568	38.423834
2300.871045	290313.910703	38.428852
2302.822483	290709.882964	38.433869
2305.358634	291089.250220	38.438887
2307.767896	291486.469637	38.443904
2310.044008	291866.613625	38.448922
2312.815075	292253.638830	38.453940
2314.950712	292646.632113	38.458957
2317.612285	293027.729229	38.463975
2319.530059	293421.339984	38.468992
2322.044312	293809.393976	38.474010
2324.955769	294196.774651	38.479028
2327.465825	294581.347809	38.484045
2329.701102	294962.001084	38.489063
2332.213553	295338.088130	38.494080
2334.439242	295725.269843	38.499098
2337.043661	296110.409397	38.504116
2339.406278	296495.434109	38.509133
2341.965490	296859.775105	38.514151
2344.750226	297230.303102	38.519168
2347.024746	297605.153345	38.524186
2349.849156	297973.920819	38.529204
2352.035209	298341.569446	38.534221
2354.730388	298687.976998	38.539239
2356.985941	299053.682577	38.544256
2359.038411	299426.227182	38.549274
2361.348815	299790.906406	38.554292
2363.756165	300162.046826	38.559309
2366.159753	300513.932740	38.564327
2368.827470	300877.384424	38.569344
2370.968358	301231.393306	38.574362
2373.359269	301557.649017	38.579380
2375.455125	301904.297146	38.584397
2378.062653	302225.970287	38.589415
2380.454382	302558.701007	38.594432
2382.565687	302887.131862	38.599450
2385.415262	303209.602738	38.604468
2387.429956	303551.255903	38.609485
2389.864823	303890.860386	38.614503
2392.474885	304212.274739	38.619520
2394.835612	304550.466941	38.624538
2397.619647	304871.902996	38.629556
2399.835113	305210.675417	38.634573
2401.873970	305547.366742	38.639591
2404.215238	305886.523930	38.644608
2406.293195	306232.300686	38.649626
2408.719217	306582.110811	38.654644
2410.952012	306937.487871	38.659661
2413.187811	307295.886091	38.664679
2415.269322	307659.667173	38.669696
2417.104566	308038.624648	38.674714
2420.055022	308408.463418	38.679732
2422.087076	308789.774980	38.684749
2424.195816	309172.622572	38.689767
2426.510390	309561.633843	38.694784
2428.922788	309962.108959	38.699802
2431.492782	310357.985808	38.704820
2433.598530	310760.640337	38.709837
2435.662135	311167.110029	38.714855
2438.415202	311577.532865	38.719872
2440.846325	311988.183015	38.724890
2443.478389	312384.296921	38.729908
2446.128887	312803.900525	38.734925
2448.697285	313217.140395	38.739943
2451.573558	313627.891592	38.744960
2453.629645	314036.205916	38.749978
2456.133046	314447.368591	38.754996
2458.720801	314869.793190	38.760013
2461.244588	315292.175389	38.765031
2464.049067	315697.570701	38.770048
2466.350435	316118.384601	38.775066
2469.008448	316523.596587	38.780084
2471.578014	316937.049859	38.785101
2474.223663	317345.511342	38.790119
2477.217976	317752.391976	38.795136
2479.671383	318164.893282	38.800154
2482.647180	318562.452457	38.805172
2484.819294	318966.105702	38.810189
2487.155605	319363.381848	38.815207
2489.978391	319765.099887	38.820224
2492.102885	320172.844336	38.825242
2494.791241	320565.487986	38.830260
2497.217762	320974.171426	38.835277
2499.617067	321373.435111	38.840295
2502.082887	321777.207044	38.845312
2504.216027	322178.439386	38.850330
2507.090546	322548.086265	38.855348
2509.338110	322936.420979	38.860365
2511.501151	323309.453432	38.865383
2514.118145	323678.704481	38.870400
2516.500119	324075.291777	38.875418
2519.001550	324450.678147	38.880436
2520.957521	324843.316735	38.885453
2523.498435	325224.788282	38.890471
2525.912619	325622.962934	38.895488
2528.243258	326027.523085	38.900506
2531.163751	326418.553667	38.905524
2533.189159	326839.715730	38.910541
2535.830717	327239.471563	38.915559
2538.611421	327642.733181	38.920576
2541.011026	328069.086051	38.925594
2543.748105	328469.709221	38.930612
2546.424962	328884.611480	38.935629
2549.173856	329306.356501	38.940647
2551.575758	329715.761812	38.945664
2554.202286	330138.257967	38.950682
2556.604694	330552.686594	38.955700
2559.320792	330973.716324	38.960717
2561.644388	331408.086629	38.965735
2564.546665	331813.490369	38.970752
2567.044190	332249.529405	38.975770
2569.869706	332677.438809	38.980788
2572.660952	333102.227728	38.985805
2575.311901	333524.750958	38.990823
2578.125541	333947.753704	38.995840
2580.764746	334378.221493	39.000858
2583.153110	334793.414773	39.005876
2586.392332	335216.088366	39.010893
2588.609836	335635.264752	39.015911
2591.772458	336048.245535	39.020928
2594.171894	336465.788222	39.025946
2596.931717	336882.611009	39.030964
2599.872694	337298.310634	39.035981
2602.452589	337719.066890	39.040999
2605.256821	338129.679257	39.046016
2608.132169	338539.185942	39.051034
2610.918090	338944.514718	39.056052
2613.670859	339351.902806	39.061069
2615.973882	339758.216959	39.066087
2619.343754	340142.803187	39.071104
2622.261296	340535.253461	39.076122
2624.771043	340922.586324	39.081140
2627.638877	341317.197672	39.086157
2629.837189	341718.945465	39.091175
2632.451248	342100.795627	39.096192
2635.118619	342499.747302	39.101210
2637.602110	342902.178389	39.106228
2639.836478	343297.842016	39.111245
2641.980073	343710.730968	39.116263
2644.859870	344115.401476	39.121280
2647.284587	344515.647553	39.126298
2649.377850	344901.548286	39.131316
2652.407056	345277.599969	39.136333
2654.418250	345665.717396	39.141351
2656.462106	346043.900442	39.146368
2658.935798	346446.156469	39.151386
2661.488899	346853.576105	39.156404
2663.933283	347269.667065	39.161421
2665.911220	347689.027604	39.166439
2669.062637	348098.729854	39.171456
2671.378708	348530.749310	39.176474
2673.645851	348969.246685	39.181492
2676.421776	349395.703081	39.186509
2678.620847	349855.960139	39.191527
2681.338996	350300.518834	39.196544
2683.999152	350743.356848	39.201562
2686.832704	351215.179220	39.206580
2689.379763	351672.141739	39.211597
2691.717236	352149.466842	39.216615
2694.955452	352612.404161	39.221632
2697.363528	353094.557995	39.226650
2700.109548	353575.917710	39.231668
2703.031575	354049.731424	39.236685
2705.476286	354538.719714	39.241703
2708.042003	355015.677779	39.246720
2710.780277	355512.276077	39.251738
2713.851720	355999.704238	39.256756
2716.739777	356492.867845	39.261773
2719.083417	356993.651421	39.266791
2721.996674	357487.714970	39.271808
2724.897138	357989.973992	39.276826
2727.829662	358485.166678	39.281844
2731.281244	358969.408861	39.286861
2733.963061	359469.529868	39.291879
2736.753553	359956.278093	39.296896
2739.523109	360449.750584	39.301914
2742.541204	360938.787792	39.306932
2745.432238	361427.840081	39.311949
2748.192849	361920.105822	39.316967
2751.117413	362405.614823	39.321984
2753.776384	362898.977681	39.327002
2756.653711	363395.396961	39.332020
2759.756775	363874.923596	39.337037
2762.601860	364362.048888	39.342055
2765.660666	364838.577754	39.347072
2768.685102	365327.136248	39.352090
2771.396769	365792.695967	39.357108
2774.204694	366258.717786	39.362125
2776.822747	366739.534363	39.367143
2779.889269	367214.945555	39.372160
2782.844641	367685.040128	39.377178
2785.257616	368168.715818	39.382196
2788.105556	368642.369836	39.387213
2790.801166	369120.356715	39.392231
2793.429252	369599.693915	39.397248
2796.210414	370058.701299	39.402266
2799.146720	370510.574190	39.407284
2801.794850	370954.164999	39.412301
2804.133804	371401.809303	39.417319
2807.058477	371838.952681	39.422336
2809.356998	372294.028565	39.427354
2811.805407	372744.280142	39.432372
2814.738097	373209.724969	39.437389
2817.158502	373680.599417	39.442407
2819.682245	374145.007430	39.447424
2822.657753	374616.798190	39.452442
2825.201614	375114.303190	39.457460
2828.254274	375588.049531	39.462477
2830.963057	376070.648736	39.467495
2833.994145	376552.810558	39.472512
2836.964801	377040.633889	39.477530
2839.917269	377530.382310	39.482548
2843.281477	378021.733947	39.487565
2845.989278	378517.623166	39.492583
2848.405437	379006.550256	39.497600
2851.102607	379514.326979	39.502618
2853.536265	380023.990749	39.507636
2856.860283	380519.655505	39.512653
2859.823412	381043.580732	39.517671
2862.577169	381549.520616	39.522688
2865.534586	382054.051697	39.527706
2867.969541	382581.032858	39.532724
2871.447639	383101.931008	39.537741
2874.141523	383617.974232	39.542759
2877.065222	384147.012272	39.547776
2880.080808	384665.678935	39.552794
2882.999416	385195.108733	39.557812
2886.508979	385698.488707	39.562829
2889.932654	386215.952923	39.567847
2893.259907	386710.698424	39.572864
2896.554556	387214.776406	39.577882
2898.966354	387718.124770	39.582900
2902.048026	388221.639070	39.587917
2905.282926	388740.593588	39.592935
2907.748986	389245.535212	39.597952
2910.744722	389755.838752	39.602970
2913.791559	390270.489133	39.607988
2916.510215	390769.890855	39.613005
2919.078064	391286.174644	39.618023
2922.100661	391800.172425	39.623040
2925.109710	392310.309957	39.628058
2927.720597	392835.795216	39.633076
2930.244827	393352.562417	39.638093
2933.077645	393893.161587	39.643111
2935.907897	394422.670726	39.648128
2938.942683	394954.015796	39.653146
2941.364960	395505.609286	39.658164
2944.628190	396035.354359	39.663181
2947.187687	396585.310902	39.668199
2949.920129	397124.023238	39.673216
2952.714702	397677.398485	39.678234
2955.080714	398206.591840	39.683252
2957.961190	398729.280271	39.688269
2961.450313	399237.918598	39.693287
2964.667004	399745.349744	39.698304
2967.823847	400259.374653	39.703322
2970.393924	400782.738568	39.708340
2973.499598	401291.557589	39.713357
2976.526576	401814.147900	39.718375
2979.029335	402343.632603	39.723392
2982.183362	402864.994049	39.728410
2985.186383	403407.235622	39.733428
2988.082089	403942.487833	39.738445
2991.020782	404474.935517	39.743463
2994.144798	405018.347084	39.748480
2997.667397	405543.788768	39.753498
3001.049092	406085.493187	39.758516
3004.290954	406612.279423	39.763533
3007.230662	407150.689009	39.768551
3009.871353	407697.197346	39.773568
3012.894237	408234.256628	39.778586
3015.659691	408776.112562	39.783604
3018.810831	409330.292594	39.788621
3021.735693	409892.355780	39.793639
3024.668636	410441.024352	39.798656
3027.963353	410997.432153	39.803674
3030.389049	411578.653488	39.808692
3033.541586	412141.981700	39.813709
3036.387290	412723.291569	39.818727
3039.065115	413301.904754	39.823744
3042.402078	413874.117077	39.828762
3045.313416	414460.678935	39.833780
3048.383350	415053.539467	39.838797
3051.550778	415642.799253	39.843815
3054.652051	416238.722245	39.848832
3057.723505	416822.093917	39.853850
3060.451917	417432.317980	39.858868
3063.784666	418025.633123	39.863885
3066.600601	418633.638353	39.868903
3069.684787	419242.829651	39.873920
3072.972559	419844.298110	39.878938
3075.773418	420464.783182	39.883956
3078.782339	421085.221537	39.888973
3081.891518	421704.819410	39.893991
3085.274486	422322.941280	39.899008
3088.413607	422932.017840	39.904026
3091.354696	423562.621367	39.909044
3094.222066	424196.211426	39.914061
3097.337810	424821.564705	39.919079
3099.783951	425467.706488	39.924096
3103.205115	426099.796416	39.929114
3106.109754	426747.810839	39.934132
3109.039746	427382.684042	39.939149
3111.942457	428038.241427	39.944167
3114.993859	428690.694164	39.949184
3118.669081	429311.573164	39.954202
3121.414918	429944.083747	39.959220
3124.834973	430551.726882	39.964237
3128.185472	431149.134564	39.969255
3131.421062	431743.355496	39.974272
3134.468759	432341.138188	39.979290
3137.700575	432944.474869	39.984308
3140.731282	433547.474635	39.989325
3143.837691	434152.930010	39.994343
3146.692528	434776.593357	39.999360
3149.806494	435388.450381	40.004378
3152.643763	436013.149636	40.009396
3155.724446	436640.428373	40.014413
3158.725003	437270.919913	40.019431
3161.543678	437920.338903	40.024448
3165.174191	438551.280776	40.029466
3168.133863	439201.909945	40.034484
3171.374709	439849.565827	40.039501
3174.878367	440490.631002	40.044519
3177.373500	441149.358590	40.049536
3180.865733	441805.480247	40.054554
3183.915382	442463.882005	40.059572
3187.247794	443135.840769	40.064589
3190.956648	443796.532174	40.069607
3194.183582	444476.267072	40.074624
3197.278454	445145.979500	40.079642
3200.550168	445809.114488	40.084660
3204.003031	446478.682094	40.089677
3207.441007	447149.549247	40.094695
3210.453821	447820.717623	40.099712
3214.005134	448492.642122	40.104730
3217.354818	449168.021176	40.109748
3220.636014	449835.242216	40.114765
3224.210867	450507.205991	40.119783
3227.074938	451188.423635	40.124800
3230.193952	451850.550696	40.129818
3233.613961	452540.952812	40.134836
3236.260681	453221.891262	40.139853
3239.326014	453921.012322	40.144871
3242.350927	454613.488818	40.149888
3245.850537	455295.899924	40.154906
3249.134473	456004.232937	40.159924
3251.994102	456716.405690	40.164941
3255.133236	457423.350323	40.169959
3258.345099	458129.805537	40.174976
3262.158809	458833.916739	40.179994
3265.470283	459557.260156	40.185012
3268.832836	460266.962149	40.190029
3271.821768	460984.238247	40.195047
3274.842810	461705.886895	40.200064
3278.681823	462411.497555	40.205082
3281.572373	463152.240750	40.210100
3284.792602	463874.190055	40.215117
3288.197777	464581.872019	40.220135
3291.333413	465323.917624	40.225152
3294.507951	466032.346542	40.230170
3297.597924	466722.253712	40.235188
3300.548114	467418.077797	40.240205
3303.675384	468107.781912	40.245223
3306.750397	468801.820804	40.250240
3310.204796	469479.341039	40.255258
3313.825870	470179.164441	40.260276
3316.858432	470891.294589	40.265293
3320.195314	471572.152921	40.270311
3323.502772	472285.758897	40.275328
3326.553941	472992.756864	40.280346
3330.276106	473714.691267	40.285364
3333.318716	474412.237033	40.290381
3336.734121	475139.275681	40.295399
3339.442892	475874.690914	40.300416
3342.820691	476592.178684	40.305434
3346.156236	477349.886400	40.310452
3349.198474	478094.620492	40.315469
3352.928261	478838.207009	40.320487
3356.197013	479601.753508	40.325504
3359.382423	480356.842825	40.330522
3362.886927	481106.950117	40.335540
3366.172715	481874.095182	40.340557
3369.567896	482642.658373	40.345575
3373.181405	483420.303624	40.350592
3376.571636	484187.846174	40.355610
3379.641054	484964.454084	40.360628
3382.971639	485750.792070	40.365645
3386.751208	486540.311049	40.370663
3389.967057	487330.593812	40.375680
3393.672345	488129.607897	40.380698
3396.979369	488910.008850	40.385716
3400.366499	489709.764185	40.390733
3403.737583	490511.912804	40.395751
3407.002848	491303.688209	40.400768
3410.379543	492108.343596	40.405786
3413.633623	492931.217757	40.410804
3416.729414	493744.382753	40.415821
3420.630283	494562.334154	40.420839
3423.900456	495383.328514	40.425856
3427.162987	496207.216290	40.430874
3430.777660	497026.112702	40.435892
3434.530183	497855.756671	40.440909
3438.678060	498664.193332	40.445927
3441.979165	499483.229937	40.450944
3445.738106	500285.394091	40.455962
3449.644560	501101.988882	40.460980
3452.783930	501916.799516	40.465997
3456.415261	502723.619594	40.471015
3460.103060	503535.240060	40.476032
3463.391302	504329.269296	40.481050
3466.940597	505130.944183	40.486068
3470.281833	505944.627964	40.491085
3474.541189	506747.176294	40.496103
3477.747589	507547.229554	40.501120
3481.195133	508321.262951	40.506125
3484.616701	509068.716505	40.511130
3487.591171	509763.896458	40.516135
3490.642758	510383.454890	40.521140
3493.804561	510968.320576	40.526144
3496.297718	511472.839293	40.531149
3499.488522	511925.433492	40.536154
3501.721751	512319.843576	40.541159
3504.116152	512656.706094	40.546164
3506.092591	512944.411501	40.551168
3507.976287	513161.413731	40.556173
3509.637047	513354.422437	40.561178
3510.955677	513505.400027	40.566183
3512.519966	513613.748921	40.571188
3513.885359	513673.672922	40.576192
3514.924424	513702.389893	40.581197
3516.021874	513698.321784	40.586202
3516.953238	513661.251155	40.591207
3517.732529	513599.673061	40.596212
3518.347268	513509.087538	40.601216
3518.707250	513405.340196	40.606221
3519.595323	513272.576289	40.611226
3519.987463	513128.964085	40.616231
3520.470071	512958.983055	40.621236
3520.905027	512777.070326	40.626240
3520.526626	512591.439871	40.631245
3521.180726	512390.620771	40.636250
3521.047542	512188.962626	40.641255
3521.494315	511961.310824	40.646260
3520.945716	511737.506067	40.651264
3521.095663	511504.128268	40.656269
3521.397832	511266.575055	40.661274
3521.550455	511030.408042	40.666279
3521.459226	510777.834983	40.671284
3520.853165	510532.927976	40.676288
3520.980218	510269.082034	40.681293
3520.960918	510020.128899	40.686298
3520.697391	509781.278487	40.691303
3521.002492	509514.610239	40.696308
3520.567123	509255.896836	40.701312
3520.228946	509001.110500	40.706317
3520.686341	508731.420985	40.711322
3520.051599	508483.807722	40.716327
3519.768047	508223.435743	40.721332
3519.648926	507971.382345	40.726336
3519.478652	507716.499885	40.731341
3519.228381	507471.493010	40.736346
3518.881964	507229.837407	40.741351
3518.874237	506965.253759	40.746356
3518.576796	506744.278998	40.751360
3518.285853	506490.055383	40.756365
3518.346829	506253.584331	40.761370
3517.673451	506024.057500	40.766375
3517.753554	505776.950397	40.771380
3517.463827	505541.132352	40.776384
3517.143241	505315.386338	40.781389
3517.369619	505092.081221	40.786394
3517.343361	504877.719840	40.791399
3516.832873	504650.628905	40.796404
3516.796232	504425.433813	40.801408
3516.852350	504207.711142	40.806413
3516.385261	503976.859643	40.811418
3516.187144	503769.242826	40.816423
3516.072969	503541.973697	40.821428
3515.566541	503350.494589	40.826432
3515.232035	503143.954779	40.831437
3515.365522	502936.781852	40.836442
3515.000172	502753.574259	40.841447
3515.001141	502546.670768	40.846452
3514.406280	502356.358951	40.851456
3514.155956	502167.762111	40.856461
3514.070402	501982.528377	40.861466
3513.722048	501807.102902	40.866471
3514.028024	501623.220747	40.871476
3513.814713	501451.920874	40.876480
3513.458299	501269.101457	40.881485
3513.863494	501097.447327	40.886490
3513.340892	500936.820909	40.891495
3513.364903	500755.100283	40.896500
3513.159679	500598.115743	40.901504
3512.443933	500418.938298	40.906509
3512.941294	500270.191909	40.911514
3512.225049	500104.425456	40.916519
3512.199759	499955.657827	40.921524
3511.700569	499803.217957	40.926528
3511.870607	499651.987150	40.931533
3511.882195	499497.945320	40.936538
3511.634508	499367.988468	40.941543
3511.392921	499224.361752	40.946548
3511.256061	499085.880827	40.951552
3510.992227	498959.517769	40.956557
3511.373706	498819.991032	40.961562
3510.639804	498686.056245	40.966567
3511.096398	498550.362941	40.971572
3511.053860	498423.303029	40.976576
3510.648232	498298.628350	40.981581
3510.914717	498156.229047	40.986586
3510.316202	498042.973732	40.991591
3510.553410	497910.145318	40.996596
3510.231801	497792.895854	41.001600
3510.104695	497680.120638	41.006605
3510.043209	497550.779396	41.011610
3509.869275	497445.705391	41.016615
3509.858924	497319.847685	41.021620
3509.655018	497208.954890	41.026624
3509.599404	497104.872762	41.031629
3509.387170	496983.196130	41.036634
3509.256123	496883.984981	41.041639
3509.155959	496772.769351	41.046644
3509.296964	496681.969131	41.051648
3509.162135	496563.821499	41.056653
3508.899608	496479.767153	41.061658
3508.793262	496379.182342	41.066663
3508.676077	496286.800800	41.071668
3508.656703	496189.795947	41.076672
3508.652419	496107.876179	41.081677
3508.459326	495997.683118	41.086682
3508.471307	495920.215473	41.091687
3508.150909	495822.648674	41.096692
3508.184954	495736.417493	41.101696
3508.031812	495657.405246	41.106701
3508.503586	495570.800301	41.111706
3507.633254	495486.128596	41.116711
3507.931535	495401.170512	41.121716
3507.826758	495317.187138	41.126720
3507.608056	495238.841675	41.131725
3507.616698	495163.903013	41.136730
3507.373863	495091.130407	41.141735
3507.780000	495020.482818	41.146740
3507.795356	494946.757419	41.151744
3507.480198	494871.615574	41.156749
3507.522991	494798.695390	41.161754
3507.549019	494722.081237	41.166759
3507.556078	494643.849448	41.171764
3507.204114	494573.876956	41.176768
3507.230093	494496.704885	41.181773
3507.503223	494419.493423	41.186778
3507.121998	494359.702467	41.191783
3507.134813	494294.886722	41.196788
3507.207219	494214.414799	41.201792
3507.037645	494148.918465	41.206797
3507.287241	494081.431456	41.211802
3507.095239	494017.659837	41.216807
3506.960388	493944.460525	41.221812
3506.940652	493889.117572	41.226816
3506.362668	493821.962974	41.231821
3506.883576	493753.874872	41.236826
3506.550630	493699.998704	41.241831
3506.490635	493640.509096	41.246836
3506.524174	493579.080276	41.251840
3506.567221	493537.398541	41.256845
3506.466802	493470.217811	41.261850
3506.469727	493417.857508	41.266855
3506.566871	493360.620880	41.271860
3506.750051	493300.787908	41.276864
3506.801459	493238.848746	41.281869
3506.726486	493179.917048	41.286874
3506.626211	493127.065845	41.291879
3506.536532	493058.160193	41.296884
3506.730761	493009.414517	41.301888
3506.551440	492943.510328	41.306893
3506.709435	492890.212508	41.311898
3506.157264	492838.343425	41.316903
3506.405624	492773.991503	41.321908
3506.156711	492721.820957	41.326912
3505.832930	492681.258719	41.331917
3506.211124	492618.151739	41.336922
3506.221793	492578.093454	41.341927
3505.840662	492517.536902	41.346932
3506.352322	492472.942817	41.351936
3505.923844	492422.774804	41.356941
3506.056991	492369.175568	41.361946
3505.845951	492320.340218	41.366951
3505.924222	492271.459007	41.371956
3506.044134	492235.383381	41.376960
3505.724867	492189.248790	41.381965
3506.112105	492137.735668	41.386970
3505.606124	492096.846459	41.391975
3505.591431	492049.042837	41.396980
3505.847311	492005.551543	41.401984
3505.618171	491955.046903	41.406989
3505.824889	491911.411233	41.411994
3505.744326	491881.190477	41.416999
3505.824468	491833.270025	41.422004
3505.860755	491789.812937	41.427008
3505.765025	491738.932124	41.432013
3505.856457	491687.819015	41.437018
3505.443787	491654.814382	41.442023
3505.760474	491600.778774	41.447028
3505.963330	491564.891310	41.452032
3505.678917	491515.913513	41.457037
3505.516592	491466.004706	41.462042
3505.288110	491437.275273	41.467047
3505.684154	491404.041074	41.472052
3505.941690	491354.875902	41.477056
3505.250600	491320.597944	41.482061
3505.377682	491274.289241	41.487066
3505.221857	491247.421862	41.492071
3505.192653	491203.264740	41.497076
3505.192516	491167.560531	41.502080
3504.927602	491133.316152	41.507085
3505.478344	491098.436333	41.512090
3505.287876	491058.913015	41.517095
3505.477928	491016.493358	41.522100
3505.564771	490988.776931	41.527104
3505.391556	490945.249701	41.532109
3505.482126	490912.518720	41.537114
3505.456848	490865.574701	41.542119
3505.374421	490829.325755	41.547124
3505.234967	490791.566393	41.552128
3505.134084	490761.144451	41.557133
3505.321593	490726.372002	41.562138
3505.470488	490700.772453	41.567143
3504.854968	490662.682916	41.572148
3505.380450	490618.639317	41.577152
3504.849941	490585.195603	41.582157
3504.992421	490564.256308	41.587162
3505.099839	490533.193317	41.592167
3505.193060	490482.532441	41.597172
3505.227132	490460.141425	41.602176
3504.982483	490438.199611	41.607181
3505.510433	490400.536548	41.612186
3504.863462	490375.315589	41.617191
3504.858295	490321.934919	41.622196
3505.165459	490300.665418	41.627200
3505.097861	490263.450745	41.632205
3504.948449	490236.986073	41.637210
3504.791977	490206.673311	41.642215
3504.813614	490175.927170	41.647220
3504.942465	490157.927104	41.652224
3505.103775	490121.739556	41.657229
3504.794671	490097.528406	41.662234
3504.761202	490068.056980	41.667239
3505.000374	490035.959393	41.672244
3504.960450	490020.062418	41.677248
3505.144654	489982.706090	41.682253
3505.116301	489942.952199	41.687258
3504.964953	489916.892563	41.692263
3504.903489	489872.281570	41.697268
3504.807015	489844.035301	41.702272
3504.794931	489823.271555	41.707277
3504.895793	489782.534587	41.712282
3504.544554	489768.408644	41.717287
3504.981802	489743.572580	41.722292
3505.167325	489707.380406	41.727296
3504.822554	489682.819820	41.732301
3504.854869	489641.586898	41.737306
3504.965772	489619.790517	41.742311
3504.788111	489588.061945	41.747316
3504.789421	489564.712716	41.752320
3504.701881	489536.211327	41.757325
3504.682206	489504.812183	41.762330
3504.545018	489481.332796	41.767335
3504.820772	489456.420583	41.772340
3504.864834	489429.012508	41.777344
3504.739066	489408.468871	41.782349
3504.798082	489392.555725	41.787354
3504.883561	489358.050116	41.792359
3504.913464	489329.327253	41.797364
3504.813399	489302.093723	41.802368
3504.733259	489270.602447	41.807373
3504.811171	489240.605622	41.812378
3504.720132	489225.627748	41.817383
3504.891604	489198.705693	41.822388
3505.297204	489157.311406	41.827392
3505.068043	489127.717489	41.832397
3504.920779	489087.879287	41.837402
3504.873097	489062.865730	41.842407
3505.116396	489028.942371	41.847412
3504.909586	488988.252318	41.852416
3504.722760	488979.266118	41.857421
3505.192467	488934.974143	41.862426
3504.911186	488911.618123	41.867431
3504.873886	488892.376850	41.872436
3504.967470	488851.284464	41.877440
3504.673431	488828.284912	41.882445
3504.732267	488783.551022	41.887450
3504.698074	488764.663683	41.892455
3504.458721	488745.454199	41.897460
3504.440773	488705.746700	41.902464
3504.374191	488701.147997	41.907469
3504.739352	488650.185944	41.912474
3504.633832	488640.072404	41.917479
3504.447822	488610.876064	41.922484
3504.872555	488595.512253	41.927488
3504.892633	488575.349864	41.932493
3504.912890	488538.472451	41.937498
3504.704637	488510.089895	41.942503
3504.849762	488478.814947	41.947508
3504.877531	488445.735036	41.952512
3504.367255	488434.773635	41.957517
3504.712618	488396.730218	41.962522
3504.810779	488377.163096	41.967527
3504.698755	488355.400493	41.972532
3504.745812	488321.557538	41.977536
3504.931938	488306.585774	41.982541
3504.900484	488262.675356	41.987546
3504.516495	488234.927992	41.992551
3504.641949	488204.364832	41.997556
3504.829235	488178.147957	42.002560
3504.632039	488170.328015	42.007565
3504.696367	488129.289337	42.012570
3504.294474	488105.900732	42.017575
3504.523970	488085.299497	42.022580
3504.831277	488070.764266	42.027584
3504.598734	488035.546720	42.032589
3504.751664	488017.743417	42.037594
3504.764311	487999.354439	42.042599
3504.408136	487957.925983	42.047604
3504.817321	487942.716060	42.052608
3504.475559	487921.191885	42.057613
3504.339674	487899.533835	42.062618
3504.107529	487868.773394	42.067623
3504.251243	487848.489380	42.072628
3504.508582	487841.357253	42.077632
3504.503684	487816.031364	42.082637
3504.833308	487790.449948	42.087642
3504.430522	487779.167253	42.092647
3504.645772	487738.407793	42.097652
3504.826834	487707.075238	42.102656
3504.128656	487687.987858	42.107661
3504.603827	487681.581045	42.112666
3504.622386	487639.687428	42.117671
3504.896261	487626.474142	42.122676
3504.462296	487596.656931	42.127680
3504.409118	487576.808983	42.132685
3504.531465	487548.423380	42.137690
3504.529360	487516.967502	42.142695
3504.065610	487505.086429	42.147700
3504.271118	487472.128686	42.152704
3504.241379	487461.040105	42.157709
3504.502767	487442.712577	42.162714
3504.801499	487417.135542	42.167719
3504.207454	487398.385991	42.172724
3504.381244	487376.171848	42.177728
3504.167473	487361.211897	42.182733
3504.416881	487330.678391	42.187738
3504.243149	487320.828201	42.192743
3504.410441	487302.768685	42.197748
3504.784610	487285.588238	42.202752
3504.586659	487261.203911	42.207757
3504.572758	487240.032375	42.212762
3504.350093	487216.411720	42.217767
3504.303113	487192.864576	42.222772
3504.638169	487160.949573	42.227776
3504.209802	487150.481028	42.232781
3504.560704	487119.221967	42.237786
3504.494388	487116.750357	42.242791
3504.274309	487075.298460	42.247796
3504.434768	487060.633705	42.252800
3504.367160	487044.941224	42.257805
3504.269520	487017.197467	42.262810
3504.266319	487000.684281	42.267815
3504.126812	486978.823131	42.272820
3504.465088	486971.120673	42.277824
3504.260825	486948.712513	42.282829
3504.575090	486917.306945	42.287834
3504.558583	486897.553802	42.292839
3504.164836	486882.064708	42.297844
3504.664334	486855.239443	42.302848
3504.118046	486841.294106	42.307853
3503.992737	486814.364923	42.312858
3504.144278	486801.828933	42.317863
3503.850878	486780.397130	42.322868
3504.034605	486756.407728	42.327872
3503.894744	486761.647440	42.332877
3504.177668	486748.634741	42.337882
3504.353383	486720.340780	42.342887
3504.392073	486710.558008	42.347892
3504.546053	486674.719620	42.352896
3504.420731	486664.253560	42.357901
3504.477330	486645.045821	42.362906
3504.428277	486624.639004	42.367911
3504.650556	486608.647059	42.372916
3504.347071	486584.785112	42.377920
3504.339350	486561.838862	42.382925
3504.161853	486542.516053	42.387930
3504.592979	486525.680516	42.392935
3504.162263	486510.551561	42.397940
3504.522950	486479.644504	42.402944
3504.167372	486470.835757	42.407949
3504.160447	486454.272029	42.412954
3504.260614	486431.663167	42.417959
3504.368455	486418.931205	42.422964
3504.575622	486380.297716	42.427968
3504.319666	486372.334348	42.432973
3504.135462	486346.730903	42.437978
3504.224297	486337.497244	42.442983
3503.837992	486311.368466	42.447988
3504.258067	486288.506237	42.452992
3504.208513	486290.996300	42.457997
3504.352104	486258.248877	42.463002
3504.700837	486246.086612	42.468007
3504.508898	486223.979596	42.473012
3504.693045	486197.456545	42.478016
3504.324986	486177.200992	42.483021
3504.601057	486152.436369	42.488026
3504.398709	486117.007864	42.493031
3504.198993	486109.846024	42.498036
3504.470157	486081.130765	42.503040
3504.517448	486070.333146	42.508045
3504.378352	486037.731346	42.513050
3504.279033	486023.917388	42.518055
3504.446665	485997.751278	42.523060
3504.357122	485974.817256	42.528064
3504.163544	485956.458903	42.533069
3504.164019	485936.904715	42.538074
3503.980450	485932.475808	42.543079
3503.925017	485915.412697	42.548084
3504.241760	485896.061766	42.553088
3504.048070	485893.052888	42.558093
3504.192817	485855.390716	42.563098
3504.261254	485857.456916	42.568103
3504.163140	485840.552460	42.573108
3504.485783	485815.425430	42.578112
3504.197838	485802.806279	42.583117
3504.400714	485763.716294	42.588122
3504.410230	485757.027836	42.593127
3504.241695	485743.731205	42.598132
3504.341565	485717.778059	42.603136
3504.144101	485694.556807	42.608141
3504.183402	485673.729737	42.613146
3504.245158	485677.063489	42.618151
3503.905320	485638.717605	42.623156
3504.374063	485624.965542	42.628160
3504.027591	485611.848925	42.633165
3503.918046	485587.600460	42.638170
3503.998823	485589.310123	42.643175
3503.822464	485568.263731	42.648180
3503.891422	485546.773264	42.653184
3504.023707	485555.820402	42.658189
3503.940262	485530.605211	42.663194
3504.093269	485520.905080	42.668199
3504.353635	485504.754214	42.673204
3504.136033	485481.687866	42.678208
3503.674376	485469.805188	42.683213
3503.759992	485455.961587	42.688218
3503.915687	485446.615611	42.693223
3503.994508	485431.050637	42.698228
3504.225709	485406.596103	42.703232
3503.983237	485411.092506	42.708237
3504.069639	485375.819625	42.713242
3504.151949	485381.531193	42.718247
3504.191633	485362.020881	42.723252
3504.368558	485325.568421	42.728256
3504.011995	485339.758934	42.733261
3504.222051	485301.173471	42.738266
3504.322698	485284.794368	42.743271
3504.203091	485270.729773	42.748276
3504.250648	485241.187381	42.753280
3504.213045	485229.997426	42.758285
3504.354573	485208.596429	42.763290
3504.095607	485208.992001	42.768295
3503.760572	485179.813954	42.773300
3504.166179	485164.957014	42.778304
3504.048703	485159.048328	42.783309
3503.958017	485146.701525	42.788314
3504.586009	485116.813890	42.793319
3504.070096	485108.080517	42.798324
3503.915964	485066.005910	42.803329
3504.208085	485075.737258	42.808333
3504.369298	485058.031211	42.813338
3504.115545	485034.716735	42.818343
3504.017322	485029.362234	42.823348
3504.156398	484986.379871	42.828353
3503.853771	484980.196431	42.833357
3504.197416	484978.267671	42.838362
3504.243270	484948.775760	42.843367
3504.013065	484942.276894	42.848372
3504.312792	484922.775691	42.853377
3504.204847	484901.160481	42.858381
3504.344150	484886.294761	42.863386
3504.283492	484867.661048	42.868391
3504.512882	484853.540981	42.873396
3504.335157	484829.504981	42.878401
3503.867061	484810.935617	42.883405
3504.241026	484794.056939	42.888410
3504.301505	484767.703445	42.893415
3504.035567	484759.690321	42.898420
3504.253607	484738.732661	42.903425
3504.425346	484713.932015	42.908429
3504.390900	484701.120082	42.913434
3504.478249	484672.634421	42.918439
3504.155165	484668.987200	42.923444
3504.382625	484625.534105	42.928449
3503.896755	484634.527405	42.933453
3503.956357	484600.017265	42.938458
3504.168780	484586.304980	42.943463
3504.038094	484582.070048	42.948468
3504.092061	484556.730534	42.953473
3504.040850	484544.022470	42.958477
3503.962687	484532.939845	42.963482
3504.141872	484509.505635	42.968487
3503.792353	484508.598318	42.973492
3503.928174	484483.195107	42.978497
3503.831784	484482.653073	42.983501
3503.753800	484457.384949	42.988506
3503.892563	484448.395801	42.993511
3503.745775	484450.850810	42.998516
3503.941664	484421.081063	43.003521
3503.961346	484417.328949	43.008525
3504.132237	484407.726756	43.013530
3503.965163	484387.792176	43.018535
3504.018832	484377.448560	43.023540
3504.161052	484367.648228	43.028545
3503.882870	484345.299366	43.033549
3503.977884	484335.557143	43.038554
3504.046700	484323.133937	43.043559
3504.019993	484303.025093	43.048564
3504.116149	484285.227294	43.053569
3503.955420	484285.404703	43.058573
3503.797184	484261.567565	43.063578
3503.855962	484252.337656	43.068583
3503.490694	484236.081971	43.073588
3503.953651	484228.561361	43.078593
3503.862397	484217.075321	43.083597
3504.379298	484201.186790	43.088602
3504.104469	484183.244888	43.093607
3504.055466	484185.532483	43.098612
3504.298525	484159.554602	43.103617
3504.008494	484148.201268	43.108621
3504.057652	484122.557965	43.113626
3504.039042	484103.460897	43.118631
3503.760527	484099.958511	43.123636
3504.243563	484066.444412	43.128641
3504.017279	484063.491060	43.133645
3503.796494	484055.369177	43.138650
3504.137984	484033.935268	43.143655
3504.000583	484033.551695	43.148660
3504.202595	484010.315925	43.153665
3504.285157	483994.141237	43.158669
3503.893936	483983.057118	43.163674
3504.581310	483966.280168	43.168679
3504.004818	483939.924904	43.173684
3503.895952	483922.868470	43.178689
3503.915202	483898.901500	43.183693
3504.023957	483890.474138	43.188698
3504.341816	483872.590250	43.193703
3504.212820	483866.429668	43.198708
3504.486058	483833.302975	43.203713
3503.997998	483827.908433	43.208717
3504.052895	483827.089147	43.213722
3504.342308	483800.444825	43.218727
3503.901027	483788.051242	43.223732
3503.884666	483756.692773	43.228737
3503.685651	483753.532406	43.233741
3503.684280	483746.895634	43.238746
3504.030362	483725.460658	43.243751
3503.741319	483713.245619	43.248756
3504.170712	483705.983435	43.253761
3503.751298	483683.858788	43.258765
3503.978378	483673.234062	43.263770
3504.130705	483658.871983	43.268775
3504.010888	483657.776321	43.273780
3504.357981	483625.954873	43.278785
3504.157982	483622.389324	43.283789
3503.893468	483591.981774	43.288794
3503.932676	483582.045335	43.293799
3503.706055	483584.665066	43.298804
3503.970082	483562.330917	43.303809
3503.979276	483542.215607	43.308813
3503.716429	483533.948160	43.313818
3503.922714	483530.166377	43.318823
3503.844928	483509.659465	43.323828
3504.076103	483494.727488	43.328833
3504.181746	483493.545512	43.333837
3503.791923	483469.592009	43.338842
3503.691274	483452.736521	43.343847
3503.745497	483457.997116	43.348852
3504.127615	483435.086840	43.353857
3503.884438	483427.373552	43.358861
3504.097396	483411.583086	43.363866
3504.342376	483402.931319	43.368871
3503.842648	483376.005834	43.373876
3504.100032	483369.429361	43.378881
3503.869487	483352.695649	43.383885
3503.980739	483316.452436	43.388890
3504.143420	483318.656008	43.393895
3503.653763	483309.360346	43.398900
3504.367582	483277.176365	43.403905
3503.982141	483281.999852	43.408909
3503.720906	483264.966923	43.413914
3504.220170	483232.158133	43.418919
3504.171860	483226.440581	43.423924
3504.179777	483214.583610	43.428929
3504.137145	483189.510902	43.433933
3504.059887	483175.792744	43.438938
3504.234185	483164.821424	43.443943
3503.984256	483145.202653	43.448948
3504.212594	483129.510857	43.453953
3504.161495	483123.591053	43.458957
3503.960519	483110.753723	43.463962
3503.934692	483096.267391	43.468967
3503.657601	483071.636919	43.473972
3503.670594	483060.944368	43.478977
3503.929491	483061.562115	43.483981
3503.846541	483045.716794	43.488986
3504.271928	483017.327259	43.493991
3503.980080	483005.568211	43.498996
3504.203830	483003.151551	43.504001
3504.183132	482968.245864	43.509005
3504.068223	482968.568040	43.514010
3504.358008	482955.906362	43.519015
3504.231513	482935.203877	43.524020
3504.225666	482911.948981	43.529025
3504.042023	482899.412769	43.534029
3504.354506	482879.552828	43.539034
3504.205513	482865.744457	43.544039
3503.852263	482839.504402	43.549044
3504.188102	482825.366030	43.554049
3504.105346	482798.475163	43.559053
3503.867185	482802.768821	43.564058
3504.254599	482776.259602	43.569063
3504.080562	482758.655111	43.574068
3504.348731	482736.370026	43.579073
3504.283392	482726.095007	43.584077
3504.110629	482704.031584	43.589082
3504.100917	482688.529063	43.594087
3504.219406	482664.088878	43.599092
3504.333878	482648.262692	43.604097
3504.141529	482624.884933	43.609101
3503.933526	482610.680371	43.614106
3504.319357	482597.952612	43.619111
3503.425027	482583.907187	43.624116
3503.940876	482563.913444	43.629121
3503.463298	482567.940995	43.634125
3503.802259	482553.497930	43.639130
3503.989001	482536.950888	43.644135
3503.739208	482517.128791	43.649140
3503.719950	482514.193142	43.654145
3504.048110	482514.850627	43.659149
3503.734967	482491.086462	43.664154
3503.838217	482477.085939	43.669159
3503.380295	482479.793047	43.674164
3504.059382	482461.648091	43.679169
3503.900347	482456.099818	43.684173
3503.987264	482425.736223	43.689178
3504.003935	482429.077664	43.694183
3503.718023	482410.223852	43.699188
3504.011845	482399.030536	43.704193
3503.853477	482393.735478	43.709197
3503.911739	482383.390072	43.714202
3503.800032	482353.564439	43.719207
3504.063931	482343.439845	43.724212
3504.089323	482341.155794	43.729217
3503.695689	482324.244303	43.734221
3504.000673	482306.259675	43.739226
3503.974321	482299.525021	43.744231
3503.986641	482294.912306	43.749236
3503.851865	482257.033967	43.754241
3503.865521	482251.661009	43.759245
3503.781812	482245.188744	43.764250
3504.041835	482218.800240	43.769255
3503.831662	482204.089043	43.774260
3504.003979	482203.707142	43.779265
3503.905359	482196.426526	43.784269
3503.587737	482178.185519	43.789274
3504.184609	482154.327763	43.794279
3503.666104	482159.020554	43.799284
3503.639044	482159.683534	43.804289
3503.709570	482123.799214	43.809293
3503.661978	482117.625208	43.814298
3503.779880	482113.046428	43.819303
3503.648599	482122.998202	43.824308
3503.778147	482091.917990	43.829313
3503.773470	482085.230505	43.834317
3503.909730	482073.707230	43.839322
3504.043348	482064.920468	43.844327
3503.966018	482040.561123	43.849332
3504.265139	482024.502569	43.854337
3503.917077	482023.290886	43.859341
3503.847158	482001.615759	43.864346
3504.097153	481985.362264	43.869351
3503.687496	481979.448121	43.874356
3503.954923	481963.343858	43.879361
3504.025346	481948.486775	43.884365
3503.698129	481940.988855	43.889370
3503.948137	481927.876779	43.894375
3503.879778	481916.487094	43.899380
3503.832400	481897.341734	43.904385
3503.927530	481888.054287	43.909389
3503.418580	481872.579363	43.914394
3503.877229	481860.194297	43.919399
3503.775747	481843.337544	43.924404
3504.079475	481844.961629	43.929409
3503.821080	481828.687027	43.934413
3503.811000	481815.007959	43.939418
3504.473187	481799.702537	43.944423
3504.011718	481790.705703	43.949428
3504.105946	481764.444132	43.954433
3503.681693	481761.673727	43.959437
3503.780062	481752.537711	43.964442
3503.801131	481731.506603	43.969447
3503.350132	481724.990884	43.974452
3503.716977	481710.036094	43.979457
3503.739858	481714.086048	43.984461
3503.607009	481705.543924	43.989466
3504.076918	481688.748725	43.994471
3503.566354	481684.573206	43.999476
3503.644628	481682.483397	44.004481
3503.891292	481674.438633	44.009485
3503.787774	481655.605927	44.014490
3504.122314	481635.842574	44.019495
3503.769656	481639.698558	44.024500
3503.843763	481612.933268	44.029505
3503.752328	481601.091019	44.034509
3503.525906	481590.131487	44.039514
3503.810955	481585.272814	44.044519
3503.649169	481592.746860	44.049524
3503.815783	481566.220232	44.054529
3503.783746	481551.024354	44.059533
3503.654807	481540.353404	44.064538
3503.809036	481542.710524	44.069543
3503.705164	481527.576653	44.074548
3503.731181	481501.578861	44.079553
3503.539301	481495.832826	44.084557
3503.765584	481497.165162	44.089562
3503.927752	481491.920530	44.094567
3503.764147	481481.913738	44.099572
3503.924079	481457.921521	44.104577
3503.929449	481457.515326	44.109581
3503.646394	481438.761462	44.114586
3503.675730	481415.955252	44.119591
3503.877307	481409.184261	44.124596
3503.639253	481408.259171	44.129601
3503.519383	481411.673040	44.134605
3503.777806	481399.724696	44.139610
3503.952002	481371.828509	44.144615
3503.640681	481366.810700	44.149620
3503.855435	481358.416158	44.154625
3503.559599	481347.011428	44.159629
3503.595769	481319.542348	44.164634
3503.438415	481320.935339	44.169639
3503.366349	481310.103261	44.174644
3503.349766	481320.189324	44.179649
3503.663218	481315.934141	44.184653
3503.749946	481325.699847	44.189658
3503.999373	481291.964550	44.194663
3503.856765	481290.619002	44.199668
3503.714923	481274.832221	44.204673
3503.630730	481268.461048	44.209677
3503.566405	481247.797613	44.214682
3504.092419	481230.739801	44.219687
3503.462091	481233.474329	44.224692
3503.714284	481222.742959	44.229697
3503.771200	481222.024587	44.234701
3503.415196	481199.329706	44.239706
3503.960461	481182.826188	44.244711
3503.686476	481179.423896	44.249716
3503.686326	481187.379254	44.254721
3503.816007	481175.704478	44.259725
3503.667867	481162.502815	44.264730
3503.681336	481143.499111	44.269735
3503.504665	481141.905582	44.274740
3503.957119	481129.419694	44.279745
3503.897579	481116.051980	44.284749
3503.775145	481111.966997	44.289754
3504.076135	481095.603361	44.294759
3503.810596	481094.581258	44.299764
3503.616269	481065.982823	44.304769
3503.626386	481059.647346	44.309773
3503.744018	481056.740511	44.314778
3503.666728	481044.338306	44.319783
3503.699199	481042.711710	44.324788
3503.820595	481016.394170	44.329793
3503.996753	481013.984789	44.334797
3503.485705	481028.253535	44.339802
3503.959395	481003.197742	44.344807
3503.772151	480987.265891	44.349812
3503.739319	480982.761346	44.354817
3503.928946	480987.139792	44.359821
3503.708346	480964.828607	44.364826
3503.825782	480941.349190	44.369831
3503.532442	480940.078116	44.374836
3503.664238	480933.419335	44.379841
3503.626253	480939.252573	44.384845
3503.706899	480919.021917	44.389850
3503.918658	480899.986634	44.394855
3503.578854	480891.324852	44.399860
3503.686304	480884.872590	44.404865
3503.769272	480881.363149	44.409869
3503.726790	480876.302717	44.414874
3503.865564	480854.644002	44.419879
3503.369603	480843.523971	44.424884
3503.692012	480847.830787	44.429889
3503.798865	480837.223525	44.434893
3503.568220	480825.706842	44.439898
3503.847766	480812.741368	44.444903
3503.937051	480803.454330	44.449908
3503.689866	480800.554453	44.454913
3503.591184	480772.497860	44.459917
3503.350386	480761.185432	44.464922
3503.657761	480754.752197	44.469927
3503.238332	480756.693373	44.474932
3503.387726	480751.197203	44.479937
3503.562625	480755.121982	44.484941
3503.380329	480751.299746	44.489946
3503.740398	480749.773357	44.494951
3503.486518	480729.190010	44.499956
3503.545825	480708.405119	44.504961
3503.630674	480710.266587	44.509965
3503.756156	480705.584937	44.514970
3504.088070	480690.432205	44.519975
3503.576162	480680.074683	44.524980
3503.632631	480675.606624	44.529985
3503.879306	480671.969924	44.534989
3503.813133	480662.960754	44.539994
3503.820370	480631.897560	44.544999
3503.924102	480620.327901	44.550004
3503.709169	480625.479790	44.555009
3503.951740	480617.941964	44.560013
3503.887758	480604.979983	44.565018
3504.035282	480566.901728	44.570023
3503.888837	480579.592993	44.575028
3503.591520	480547.665703	44.580033
3503.753128	480534.414654	44.585037
3503.684654	480522.568123	44.590042
3503.861246	480520.766685	44.595047
3503.883924	480510.577932	44.600052
3503.975795	480487.254031	44.605057
3503.891664	480485.848511	44.610061
3503.650840	480484.062379	44.615066
3504.194729	480457.626633	44.620071
3504.021137	480448.837036	44.625076
3504.008494	480443.467740	44.630081
3503.825284	480419.528496	44.635085
3503.538376	480398.392622	44.640090
3503.946192	480389.663112	44.645095
3503.584249	480379.129706	44.650100
3503.800294	480381.426523	44.655105
3503.590492	480349.079694	44.660109
3503.672704	480349.877481	44.665114
3504.183622	480332.922625	44.670119
3503.899926	480338.541516	44.675124
3503.484500	480311.649140	44.680129
3503.910487	480298.153447	44.685133
3503.713542	480299.451421	44.690138
3503.821596	480290.819926	44.695143
3503.559852	480285.946020	44.700148
3503.800927	480271.820789	44.705153
3503.881746	480263.345606	44.710157
3503.580749	480271.146198	44.715162
3503.829246	480249.570818	44.720167
3503.549964	480233.956944	44.725172
3503.398863	480227.139950	44.730177
3503.550193	480222.504773	44.735181
3503.529537	480215.363115	44.740186
3503.453537	480214.919083	44.745191
3503.487543	480214.761703	44.750196
3503.640976	480194.924183	44.755201
3503.828805	480177.361511	44.760205
3503.593504	480163.412851	44.765210
3503.601442	480165.438549	44.770215
3503.710384	480169.373872	44.775220
3503.539804	480138.946088	44.780225
3503.579161	480131.946934	44.785229
3503.628865	480129.506762	44.790234
3503.849635	480115.790017	44.795239
3503.340075	480129.704462	44.800244
3503.623654	480123.274782	44.805249
3503.984311	480101.884206	44.810253
3503.477506	480098.974589	44.815258
3503.771281	480083.422031	44.820263
3503.853758	480102.158255	44.825268
3503.893973	480072.355804	44.830273
3503.670132	480053.692601	44.835277
3503.567127	480041.040459	44.840282
3503.899976	480041.545270	44.845287
3503.738386	480036.706145	44.850292
3503.674795	480018.727011	44.855297
3503.783978	479998.896289	44.860301
3503.524244	480005.524964	44.865306
3503.941736	479987.824472	44.870311
3503.805941	479970.464793	44.875316
3503.739593	479953.499513	44.880321
3503.719388	479946.307013	44.885325
3503.505890	479953.080419	44.890330
3503.978138	479932.736174	44.895335
3503.898698	479932.444701	44.900340
3504.019289	479909.875688	44.905345
3504.165504	479894.650351	44.910349
3503.929498	479884.299469	44.915354
3503.787471	479854.880216	44.920359
3503.790419	479854.981113	44.925364
3503.704518	479837.917476	44.930369
3503.866105	479829.125294	44.935373
3503.688341	479819.069216	44.940378
3504.038062	479811.716842	44.945383
3503.709601	479800.417718	44.950388
3503.818124	479789.809627	44.955393
3503.807263	479772.886095	44.960397
3503.781367	479779.376534	44.965402
3503.831489	479759.858954	44.970407
3503.629710	479737.492725	44.975412
3503.884481	479736.134929	44.980417
3503.670380	479728.010182	44.985421
3503.708819	479720.504281	44.990426
3504.032150	479704.440007	44.995431
3503.949188	479686.717005	45.000436
3503.875400	479679.127479	45.005441
3504.159921	479650.400616	45.010445
3503.693621	479653.160103	45.015450
3504.005589	479644.192043	45.020455
3504.063388	479613.676673	45.025460
3503.810620	479600.895896	45.030465
3503.787412	479591.930120	45.035469
3503.848974	479602.511460	45.040474
3504.146204	479572.870327	45.045479
3503.915304	479566.167068	45.050484
3503.841528	479562.986220	45.055489
3503.644937	479530.230558	45.060493
3503.723984	479523.174239	45.065498
3504.069289	479506.700930	45.070503
3503.873965	479507.441272	45.075508
3503.669840	479477.879248	45.080513
3503.648512	479474.284693	45.085517
3503.962409	479473.779012	45.090522
3504.114269	479457.589616	45.095527
3503.895851	479442.725622	45.100532
3503.600774	479427.012253	45.105537
3503.775090	479412.846285	45.110541
3503.671708	479426.697017	45.115546
3503.871780	479389.317637	45.120551
3503.739414	479399.017583	45.125556
3503.926701	479372.788783	45.130561
3503.812478	479373.972389	45.135565
3503.574037	479346.442611	45.140570
3503.831021	479335.405405	45.145575
3503.795699	479332.775872	45.150580
3503.567705	479326.730855	45.155585
3503.856030	479316.904899	45.160589
3503.708595	479286.826871	45.165594
3503.968243	479283.137190	45.170599
3503.826498	479288.075155	45.175604
3503.767945	479258.033709	45.180609
3503.890714	479245.446719	45.185613
3503.812880	479242.722543	45.190618
3503.750807	479225.603935	45.195623
3503.451318	479229.857387	45.200628
3503.462362	479200.615666	45.205633
3503.751698	479197.478712	45.210637
3503.382236	479194.547248	45.215642
3503.608055	479190.254787	45.220647
3503.828759	479189.915858	45.225652
3503.851387	479180.435890	45.230657
3503.709645	479151.218247	45.235661
3503.466509	479157.996610	45.240666
3503.715984	479141.892878	45.245671
3503.736307	479149.187034	45.250676
3503.510713	479131.283375	45.255681
3503.967122	479102.680575	45.260685
3503.663128	479103.640814	45.265690
3503.866360	479093.726846	45.270695
3503.691146	479089.295051	45.275700
3503.440830	479065.212741	45.280705
3503.654830	479057.324103	45.285709
3503.372537	479064.615450	45.290714
3503.930643	479044.459427	45.295719
3503.838034	479055.268136	45.300724
3503.794843	479025.984054	45.305729
3503.911597	479016.185069	45.310733
3503.794944	479009.666267	45.315738
3503.749498	478997.713827	45.320743
3504.055773	478972.073804	45.325748
3503.871685	478974.129979	45.330753
3504.085222	478947.339024	45.335757
3503.858423	478947.070830	45.340762
3503.860576	478924.975503	45.345767
3503.750975	478929.908476	45.350772
3503.538316	478918.337156	45.355777
3503.671464	478895.714324	45.360781
3503.597157	478889.543525	45.365786
3503.605546	478875.707463	45.370791
3503.731691	478890.890559	45.375796
3504.112747	478874.005661	45.380801
3504.092855	478854.954347	45.385805
3504.119790	478846.537751	45.390810
3504.017869	478820.860704	45.395815
3503.976253	478802.471573	45.400820
3503.854756	478798.233929	45.405825
3504.167752	478780.751586	45.410829
3503.915087	478766.551297	45.415834
3504.007661	478742.161007	45.420839
3503.808631	478742.192482	45.425844
3503.952795	478724.382038	45.430849
3503.528170	478700.681578	45.435853
3503.369012	478703.544674	45.440858
3503.652749	478704.462704	45.445863
3503.584857	478696.162389	45.450868
3503.396426	478685.195229	45.455873
3503.656931	478659.967457	45.460877
3503.410528	478661.577418	45.465882
3503.809438	478655.585129	45.470887
3503.164375	478657.258108	45.475892
3503.223993	478658.769018	45.480897
3503.635784	478645.274446	45.485901
3503.461519	478659.643692	45.490906
3503.724679	478619.009539	45.495911
3503.579244	478609.302476	45.500916
3503.245390	478615.031137	45.505921
3503.570842	478612.192448	45.510925
3503.635772	478611.979489	45.515930
3503.552361	478610.117623	45.520935
3503.542804	478608.294761	45.525940
3503.717590	478576.340331	45.530945
3503.699943	478565.903561	45.535949
3503.785335	478575.164068	45.540954
3503.504085	478560.005276	45.545959
3503.998064	478545.940192	45.550964
3503.498870	478534.667329	45.555969
3503.933732	478512.148400	45.560973
3503.597717	478524.313494	45.565978
3503.778905	478501.631941	45.570983
3503.612080	478490.813292	45.575988
3503.440131	478479.539347	45.580993
3503.898125	478466.240062	45.585997
3503.348127	478479.452564	45.591002
3503.378711	478477.521988	45.596007
3503.475995	478468.131234	45.601012
3503.698551	478469.413691	45.606017
3503.663985	478432.120274	45.611021
3503.475753	478437.927322	45.616026
3503.405931	478423.697885	45.621031
3503.462749	478420.597565	45.626036
3503.552031	478429.654813	45.631041
3503.723054	478418.580008	45.636045
3503.331364	478405.060249	45.641050
3503.687522	478387.317347	45.646055
3503.932677	478382.818944	45.651060
3503.800086	478369.460916	45.656065
3503.901316	478369.901031	45.661069
3503.317793	478349.164595	45.666074
3503.561618	478337.824846	45.671079
3503.412236	478334.098292	45.676084
3503.360440	478341.252111	45.681089
3503.529621	478335.498753	45.686093
3503.575949	478335.643479	45.691098
3503.648430	478331.577785	45.696103
3503.583092	478309.289729	45.701108
3503.650532	478304.008549	45.706113
3503.674296	478294.071873	45.711117
3503.733044	478296.900583	45.716122
3503.925174	478285.467620	45.721127
3504.020867	478264.573050	45.726132
3503.528968	478255.528721	45.731137
3503.591925	478242.494445	45.736141
3503.409993	478244.448996	45.741146
3503.400823	478240.142798	45.746151
3503.467532	478230.908800	45.751156
3503.415201	478208.517218	45.756161
3503.349758	478205.993654	45.761165
3503.464137	478214.337534	45.766170
3503.388778	478209.129580	45.771175
3503.360464	478196.515129	45.776180
3503.203482	478210.628575	45.781185
3503.868585	478206.063750	45.786189
3503.528767	478199.326564	45.791194
3503.665799	478182.834402	45.796199
3503.920760	478158.417726	45.801204
3503.760407	478155.503730	45.806209
3503.537471	478151.281982	45.811213
3503.765916	478156.921889	45.816218
3503.656960	478137.478536	45.821223
3503.708561	478141.017899	45.826228
3503.453643	478127.070901	45.831233
3504.190290	478114.031406	45.836237
3503.883646	478110.785776	45.841242
3503.721490	478092.263006	45.846247
3503.707150	478081.876139	45.851252
3503.673938	478089.331183	45.856257
3503.791977	478064.936037	45.861261
3503.452135	478050.647657	45.866266
3503.902537	478031.774607	45.871271
3503.881257	478031.271196	45.876276
3503.589167	478035.067622	45.881281
3503.745071	478000.733343	45.886285
3503.732215	477992.525391	45.891290
3503.504567	477991.649169	45.896295
3503.633879	477980.530035	45.901300
3503.875186	477981.860239	45.906305
3503.665664	477957.314023	45.911309
3503.290413	477952.406802	45.916314
3503.376561	477941.547865	45.921319
3503.914988	477942.983143	45.926324
3503.357777	477955.741019	45.931329
3503.498559	477945.582955	45.936333
3503.672079	477926.297461	45.941338
3503.563963	477917.597744	45.946343
3503.639010	477903.953185	45.951348
3503.764369	477903.882704	45.956353
3503.773674	477893.086567	45.961357
3503.251313	477875.178005	45.966362
3503.597001	477857.486966	45.971367
3503.766273	477844.638342	45.976372
3503.916315	477855.865460	45.981377
3503.936760	477842.736284	45.986381
3503.390385	477827.061368	45.991386
3503.605463	477809.948407	45.996391
3503.934673	477805.842023	46.001396
3503.593830	477806.352032	46.006401
3503.812254	477798.715595	46.011405
3503.560589	477788.062012	46.016410
3503.607830	477777.969329	46.021415
3503.470798	477765.017033	46.026420
3503.002900	477767.675669	46.031425
3503.547913	477761.660019	46.036429
3503.283414	477760.333494	46.041434
3503.577539	477758.158472	46.046439
3503.411468	477761.377553	46.051444
3503.568014	477750.101947	46.056449
3503.736405	477718.349869	46.061453
3503.328131	477723.634430	46.066458
3503.699510	477713.186399	46.071463
3503.463179	477712.818333	46.076468
3503.227029	477715.338983	46.081473
3503.241789	477708.292182	46.086477
3503.339514	477707.719272	46.091482
3503.525066	477709.413067	46.096487
3503.273661	477705.955920	46.101492
3503.370098	477676.343698	46.106497
3503.411544	477668.076349	46.111501
3503.377647	477675.937095	46.116506
3503.229547	477675.960521	46.121511
3503.682972	477670.212720	46.126516
3503.232847	477667.445817	46.131521
3503.639213	477665.962560	46.136525
3503.473919	477676.226029	46.141530
3503.367866	477659.974579	46.146535
3503.379907	477635.544983	46.151540
3503.241344	477633.134264	46.156545
3503.605911	477621.622983	46.161549
3503.606958	477618.277954	46.166554
3503.568228	477618.284091	46.171559
3503.755890	477615.517723	46.176564
3503.618525	477616.350331	46.181569
3503.862417	477590.363631	46.186573
3504.124083	477588.041681	46.191578
3504.108153	477580.695606	46.196583
3504.129068	477565.589650	46.201588
3503.754855	477542.031877	46.206593
3504.027268	477530.383071	46.211597
3503.741242	477517.403485	46.216602
3503.640242	477505.509609	46.221607
3503.838348	477495.139534	46.226612
3503.627279	477496.338560	46.231617
3503.826021	477485.005454	46.236621
3503.807860	477457.640956	46.241626
3503.790777	477451.409984	46.246631
3503.665837	477451.125666	46.251636
3503.396227	477451.218979	46.256641
3503.544892	477439.234917	46.261645
3503.177997	477429.258203	46.266650
3503.198199	477424.085617	46.271655
3503.325451	477417.983861	46.276660
3503.640451	477413.271478	46.281665
3503.829113	477411.518533	46.286669
3503.293903	477416.873921	46.291674
3503.615867	477411.096147	46.296679
3503.827878	477404.322141	46.301684
3503.513594	477381.666955	46.306689
3503.514596	477359.418029	46.311693
3503.339071	477365.578144	46.316698
3503.420955	477360.547834	46.321703
3503.417427	477357.811653	46.326708
3503.020950	477356.607324	46.331713
3503.064171	477357.664800	46.336717
3502.793770	477364.650803	46.341722
3502.921266	477349.325113	46.346727
3503.299708	477352.204783	46.351732
3503.123825	477364.598673	46.356737
3503.103846	477365.919542	46.361741
3503.210324	477360.936025	46.366746
3503.568610	477365.896785	46.371751
3503.849408	477366.207177	46.376756
3503.618530	477357.577302	46.381761
3503.472781	477330.638243	46.386765
3503.318978	477324.124758	46.391770
3503.399158	477319.145388	46.396775
3503.399973	477314.888092	46.401780
3503.323717	477320.525722	46.406785
3503.522103	477312.892267	46.411789
3503.378852	477321.378608	46.416794
3503.556147	477315.978440	46.421799
3503.616018	477315.208779	46.426804
3503.489715	477294.855093	46.431809
3503.577237	477279.383626	46.436813
3503.495839	477283.957782	46.441818
3503.647381	477267.614612	46.446823
3503.763117	477257.460158	46.451828
3503.602457	477260.070294	46.456833
3503.851578	477231.852342	46.461837
3503.582806	477229.411476	46.466842
3503.347955	477235.023518	46.471847
3503.438488	477229.535680	46.476852
3503.156535	477233.786782	46.481857
3503.703302	477225.743458	46.486861
3503.442029	477222.693234	46.491866
3503.193892	477194.047022	46.496871
3503.279333	477188.053167	46.501876
3502.968245	477190.281642	46.506881
3503.393448	477171.006314	46.511885
3503.437692	477183.162796	46.516890
3503.367322	477181.146691	46.521895
3503.427371	477185.799872	46.526900
3503.404311	477178.505457	46.531905
3503.423010	477174.346667	46.536909
3503.574980	477178.225103	46.541914
3503.597055	477170.214015	46.546919
3503.903898	477158.255463	46.551924
3503.559958	477152.076065	46.556929
3503.590535	477141.935013	46.561933
3503.571291	477142.140795	46.566938
3503.266458	477134.890905	46.571943
3503.703182	477131.679651	46.576948
3503.679802	477112.221770	46.581953
3503.912403	477089.429122	46.586957
3503.314352	477087.547102	46.591962
3503.417256	477084.185883	46.596967
3503.597497	477086.336703	46.601972
3503.571801	477092.523899	46.606977
3503.335245	477070.362885	46.611981
3503.477195	477060.964407	46.616986
3503.588533	477055.574595	46.621991
3503.843593	477046.817090	46.626996
3503.323379	477052.220885	46.632001
3503.235009	477049.650116	46.637005
3503.431253	477046.527544	46.642010
3503.568759	477053.347812	46.647015
3503.482073	477039.373458	46.652020
3503.205524	477018.992559	46.657025
3503.565156	476999.778114	46.662029
3503.094367	476991.642138	46.667034
3503.294973	476998.351087	46.672039
3503.282295	476995.565621	46.677044
3503.444502	476998.479525	46.682049
3503.726148	476986.119401	46.687053
3503.449274	477002.279915	46.692058
3503.574492	476992.934732	46.697063
3503.898008	476973.421881	46.702068
3503.383772	476964.076403	46.707073
3503.486056	476962.286392	46.712077
3503.213214	476957.160009	46.717082
3503.321138	476943.661641	46.722087
3503.516798	476954.071150	46.727092
3503.417904	476956.063382	46.732097
3503.425621	476947.040841	46.737101
3503.317596	476961.603566	46.742106
3503.421104	476925.704590	46.747111
3503.595487	476911.435470	46.752116
3503.344292	476914.617461	46.757121
3503.732690	476899.250185	46.762125
3503.127168	476918.807715	46.767130
3503.263281	476917.620533	46.772135
3503.491788	476911.147845	46.777140
3503.579896	476923.246869	46.782145
3503.770686	476900.561978	46.787149
3503.315178	476888.875819	46.792154
3503.438901	476872.942179	46.797159
3503.563543	476857.515201	46.802164
3503.310374	476863.687743	46.807169
3503.463052	476861.433620	46.812173
3503.337529	476874.681445	46.817178
3503.607555	476860.954670	46.822183
3503.508416	476858.892399	46.827188
3503.307830	476848.635694	46.832193
3503.626026	476822.636251	46.837197
3503.498631	476822.909813	46.842202
3503.419389	476826.115319	46.847207
3503.447993	476818.964652	46.852212
3503.416246	476815.979447	46.857217
3503.734875	476819.679562	46.862221
3503.587109	476805.917429	46.867226
3503.569329	476781.136727	46.872231
3503.726797	476781.111850	46.877236
3503.400480	476783.646869	46.882241
3503.667309	476776.661259	46.887245
3503.885029	476771.355918	46.892250
3503.570308	476751.893058	46.897255
3503.480470	476734.472602	46.902260
3503.353859	476735.455593	46.907265
3503.461846	476725.656869	46.912269
3503.351158	476732.871256	46.917274
3503.398137	476732.661116	46.922279
3503.629401	476725.174287	46.927284
3503.223986	476729.292965	46.932289
3503.297364	476699.834989	46.937293
3503.297675	476698.871991	46.942298
3503.507362	476708.265764	46.947303
3503.397247	476696.271483	46.952308
3503.384078	476698.655647	46.957313
3503.621945	476698.871473	46.962317
3503.756465	476703.259582	46.967322
3503.719129	476696.727483	46.972327
3503.649149	476675.147887	46.977332
3503.528641	476654.235126	46.982337
3503.922024	476645.861040	46.987341
3503.741923	476652.630286	46.992346
3503.429427	476644.975970	46.997351
3503.708243	476625.520529	47.002356
3503.874665	476622.047828	47.007361
3503.636201	476604.042562	47.012365
3503.858143	476600.561081	47.017370
3503.843281	476594.126760	47.022375
3503.862826	476565.285286	47.027380
3503.486249	476568.081690	47.032385
3503.530798	476561.435237	47.037389
3503.489841	476566.712720	47.042394
3503.328453	476564.102749	47.047399
3503.576638	476536.036014	47.052404
3503.407562	476525.470066	47.057409
3503.747357	476535.046085	47.062413
3503.836187	476529.609007	47.067418
3503.797097	476523.837369	47.072423
3504.003653	476512.046334	47.077428
3503.737019	476495.616589	47.082433
3503.487156	476472.747457	47.087437
3503.817116	476482.679836	47.092442
3503.410520	476468.350190	47.097447
3503.761147	476438.746639	47.102452
3503.721277	476428.464313	47.107457
3503.928338	476427.924767	47.112461
3503.954546	476427.565858	47.117466
3503.852408	476404.115783	47.122471
3503.836235	476376.901542	47.127476
3503.548085	476383.586592	47.132481
3503.797193	476380.050095	47.137485
3503.933373	476364.215449	47.142490
3503.525740	476351.457060	47.147495
3503.701270	476341.140641	47.152500
3503.384892	476340.633151	47.157505
3503.887203	476337.968920	47.162509
3503.452525	476320.653298	47.167514
3503.498192	476314.209319	47.172519
3503.328645	476292.340950	47.177524
3503.544659	476288.353519	47.182529
3503.394605	476289.441603	47.187533
3503.274044	476286.318308	47.192538
3503.408702	476286.702504	47.197543
3503.627740	476281.295460	47.202548
3503.590965	476280.236937	47.207553
3503.634102	476252.962469	47.212557
3503.777553	476245.083875	47.217562
3503.434475	476245.188805	47.222567
3503.919570	476242.679333	47.227572
3503.753934	476231.960636	47.232577
3503.423761	476205.556050	47.237581
3503.578302	476180.240532	47.242586
3503.545280	476182.982681	47.247591
3503.442651	476180.515422	47.252596
3503.569926	476197.778420	47.257601
3503.495639	476189.680806	47.262605
3503.651474	476172.525128	47.267610
3503.658020	476165.276348	47.272615
3503.863468	476144.412898	47.277620
3503.641990	476151.898424	47.282625
3503.544746	476142.537328	47.287629
3503.631355	476122.756998	47.292634
3503.665751	476103.035586	47.297639
3503.693628	476102.676407	47.302644
3503.515895	476098.903231	47.307649
3503.879667	476094.284199	47.312653
3503.844769	476073.306616	47.317658
3503.684611	476061.877388	47.322663
3503.834179	476048.523888	47.327668
3503.363501	476060.458343	47.332673
3503.463316	476056.083763	47.337677
3503.841881	476038.537976	47.342682
3503.909741	476017.442723	47.347687
3503.762033	476011.181267	47.352692
3503.683201	476020.722339	47.357697
3503.517488	476004.428291	47.362701
3503.394008	475984.224878	47.367706
3503.238053	475976.545560	47.372711
3503.618307	475970.352686	47.377716
3503.759256	475974.486519	47.382721
3503.807921	475974.884314	47.387725
3504.011753	475965.323491	47.392730
3503.706551	475946.618606	47.397735
3503.569216	475936.655540	47.402740
3503.553884	475933.464872	47.407745
3503.697544	475932.225756	47.412749
3503.763602	475923.345586	47.417754
3503.467901	475904.791213	47.422759
3503.684371	475882.405220	47.427764
3503.758680	475885.687971	47.432769
3503.677503	475886.765189	47.437773
3503.958598	475860.060785	47.442778
3503.909728	475850.134377	47.447783
3504.014396	475837.142626	47.452788
3503.891019	475843.345648	47.457793
3504.082888	475811.434784	47.462797
3504.041171	475810.275649	47.467802
3503.665325	475802.478970	47.472807
3503.647694	475766.090224	47.477812
3503.772457	475760.596574	47.482817
3503.892794	475756.117316	47.487821
3503.855890	475751.460173	47.492826
3503.644472	475738.011475	47.497831
3503.839205	475713.145179	47.502836
3503.509457	475709.497328	47.507841
3503.600077	475700.714547	47.512845
3503.611453	475703.855222	47.517850
3503.268812	475688.754636	47.522855
3503.819045	475656.482770	47.527860
3503.687823	475659.392568	47.532865
3503.349427	475654.935115	47.537869
3503.673044	475647.281233	47.542874
3503.517742	475652.526346	47.547879
3503.763094	475634.443732	47.552884
3503.510269	475619.227526	47.557889
3503.427272	475606.620086	47.562893
3503.511021	475605.086310	47.567898
3503.390850	475611.491637	47.572903
3503.806020	475603.620526	47.577908
3503.526580	475601.535940	47.582913
3503.673143	475574.396259	47.587917
3503.410759	475566.074700	47.592922
3503.369759	475565.726400	47.597927
3503.545167	475558.754819	47.602932
3503.245029	475551.351556	47.607937
3503.706305	475554.573192	47.612941
3503.726652	475553.606972	47.617946
3503.682623	475530.653544	47.622951
3503.621200	475518.245380	47.627956
3503.244330	475516.429612	47.632961
3503.481384	475510.918144	47.637965
3503.455058	475513.000417	47.642970
3503.225419	475503.761321	47.647975
3503.422402	475495.721917	47.652980
3503.522493	475512.432263	47.657985
3503.305104	475494.118557	47.662989
3503.551058	475475.123369	47.667994
3503.488634	475474.981195	47.672999
3503.659693	475461.319796	47.678004
3503.356254	475463.344508	47.683009
3503.534825	475464.228633	47.688013
3503.487181	475462.563560	47.693018
3503.095973	475456.543163	47.698023
3503.437378	475458.617999	47.703028
3503.290514	475444.753417	47.708033
3503.586232	475421.188620	47.713037
3503.507205	475425.965565	47.718042
3503.157827	475417.911124	47.723047
3503.319768	475418.696508	47.728052
3503.659381	475425.384013	47.733057
3503.635483	475421.890505	47.738061
3503.445818	475426.076712	47.743066
3503.328738	475430.961042	47.748071
3503.705940	475393.343444	47.753076
3503.629234	475384.485604	47.758081
3503.434992	475377.268280	47.763085
3503.756563	475376.507863	47.768090
3503.652147	475374.851758	47.773095
3503.790088	475366.466836	47.778100
3503.680686	475345.804386	47.783105
3503.545238	475336.144838	47.788109
3503.549201	475339.134684	47.793114
3503.370333	475335.817715	47.798119
3503.813708	475325.052951	47.803124
3503.627454	475312.056163	47.808129
3503.425760	475295.260370	47.813133
3503.397173	475289.385346	47.818138
3503.215206	475293.925164	47.823143
3503.470718	475282.581844	47.828148
3503.476852	475284.811067	47.833153
3503.507688	475281.866427	47.838157
3503.642643	475284.328716	47.843162
3503.282828	475277.543016	47.848167
3503.426459	475258.006253	47.853172
3503.707975	475255.326098	47.858177
3503.507525	475259.412673	47.863181
3503.581132	475249.213179	47.868186
3503.723893	475245.541238	47.873191
3503.566428	475243.944193	47.878196
3503.834564	475232.446791	47.883201
3503.529253	475208.216462	47.888205
3503.888652	475201.367732	47.893210
3503.579222	475200.453624	47.898215
3503.664381	475192.989323	47.903220
3503.633909	475185.543298	47.908225
3503.265920	475172.169658	47.913229
3503.537597	475159.100384	47.918234
3503.510916	475164.882840	47.923239
3503.300529	475156.198089	47.928244
3503.294902	475163.599175	47.933249
3503.378075	475154.715961	47.938253
3503.750798	475147.915794	47.943258
3503.409211	475131.851585	47.948263
3503.539235	475110.796243	47.953268
3503.749062	475113.652208	47.958273
3503.650655	475114.276014	47.963277
3503.906794	475109.572400	47.968282
3503.546153	475093.916663	47.973287
3503.599468	475073.988508	47.978292
3503.425039	475072.799622	47.983297
3503.072153	475066.266186	47.988301
3503.563346	475058.940398	47.993306
3503.062896	475072.350047	47.998311
3503.397085	475061.957208	48.003316
3503.219628	475065.989501	48.008321
3503.082430	475067.835913	48.013325
3503.369666	475057.754613	48.018330
3503.493795	475065.236596	48.023335
3503.644253	475061.918210	48.028340
3503.672008	475038.344638	48.033345
3503.283752	475021.527421	48.038349
3503.313471	475017.113009	48.043354
3503.447349	475012.986252	48.048359
3503.431340	475017.145093	48.053364
3503.321032	475013.665173	48.058369
3503.209799	475016.014352	48.063373
3503.478448	475021.446045	48.068378
3503.323707	475018.885507	48.073383
3503.595210	475011.138250	48.078388
3503.249696	474997.862315	48.083393
3503.139890	474980.342122	48.088397
3503.649765	474974.432576	48.093402
3503.247923	474980.730567	48.098407
3503.758098	474975.631960	48.103412
3503.557931	474979.921293	48.108417
3503.287457	474965.518368	48.113421
3503.421761	474968.335606	48.118426
3503.347594	474972.706396	48.123431
3503.706541	474965.908346	48.128436
3503.433044	474938.378030	48.133441
3503.339658	474928.863699	48.138445
3503.637159	474921.568479	48.143450
3503.260370	474936.073780	48.148455
3503.496559	474928.078640	48.153460
3503.503633	474926.354186	48.158465
3503.365196	474931.343386	48.163469
3503.457566	474925.601196	48.168474
3503.408841	474906.601368	48.173479
3503.579771	474888.073668	48.178484
3503.480166	474885.453711	48.183489
3503.454366	474881.048046	48.188493
3503.807842	474883.171721	48.193498
3503.378790	474883.898487	48.198503
3503.527612	474865.982504	48.203508
3503.813390	474846.726996	48.208513
3503.550533	474842.916352	48.213517
3503.430846	474835.940483	48.218522
3503.560129	474834.348765	48.223527
3503.614909	474831.805770	48.228532
3503.343148	474832.000804	48.233537
3503.246678	474818.938818	48.238541
3503.658930	474792.719142	48.243546
3503.288949	474797.542227	48.248551
3503.214592	474793.346967	48.253556
3503.213431	474794.614343	48.258561
3503.173954	474791.325937	48.263565
3503.572038	474785.940878	48.268570
3503.507152	474792.692534	48.273575
3503.740264	474788.093861	48.278580
3503.595471	474788.167451	48.283585
3503.545776	474770.637574	48.288589
3503.720993	474743.086749	48.293594
3503.451603	474743.484158	48.298599
3503.533463	474742.913673	48.303604
3503.473763	474741.808006	48.308609
3503.479706	474736.738358	48.313613
3503.678038	474731.080738	48.318618
3503.479462	474717.781391	48.323623
3503.642307	474702.650847	48.328628
3503.433670	474697.006861	48.333633
3503.344387	474705.941958	48.338637
3503.574589	474691.206258	48.343642
3503.170209	474697.555425	48.348647
3503.574499	474696.680534	48.353652
3503.662788	474682.575508	48.358657
3503.655113	474658.297470	48.363661
3503.612449	474652.880673	48.368666
3503.544926	474658.568354	48.373671
3503.501251	474647.728159	48.378676
3503.620842	474651.967016	48.383681
3503.677186	474640.097258	48.388685
3503.747695	474609.927054	48.393690
3503.546308	474615.433158	48.398695
3503.383559	474607.298204	48.403700
3503.421682	474612.918510	48.408705
3503.331728	474609.587366	48.413709
3503.303374	474604.624482	48.418714
3503.463899	474601.861992	48.423719
3503.794260	474582.092310	48.428724
3503.542034	474569.764411	48.433729
3503.582356	474565.094787	48.438733
3503.643356	474555.657251	48.443738
3503.453654	474563.695906	48.448743
3503.383968	474549.260945	48.453748
3503.736114	474547.076411	48.458753
3503.532097	474531.902356	48.463757
3503.641018	474523.217546	48.468762
3503.563631	474525.510743	48.473767
3503.579726	474520.236685	48.478772
3503.442290	474526.239582	48.483777
3503.355872	474513.125122	48.488781
3503.584791	474482.625562	48.493786
3503.395502	474481.185550	48.498791
3503.476330	474478.384954	48.503796
3503.701220	474478.653547	48.508801
3503.443705	474476.869504	48.513805
3503.487036	474470.171867	48.518810
3503.116122	474473.880042	48.523815
3503.604859	474465.844799	48.528820
3503.430377	474440.072230	48.533825
3503.609668	474439.232896	48.538829
3503.945331	474425.342027	48.543834
3503.437914	474429.071788	48.548839
3503.660091	474422.700680	48.553844
3503.417397	474426.287220	48.558849
3503.507310	474409.089778	48.563853
3503.491754	474397.383307	48.568858
3503.418087	474388.980742	48.573863
3503.648513	474382.760383	48.578868
3503.917139	474379.372518	48.583873
3503.708728	474379.709606	48.588877
3503.609470	474353.164713	48.593882
3503.331228	474342.310746	48.598887
3503.625633	474340.338070	48.603892
3503.584166	474339.432251	48.608897
3503.407481	474339.764324	48.613901
3503.665327	474331.207956	48.618906
3503.561293	474317.589271	48.623911
3503.683596	474303.174475	48.628916
3503.624173	474294.059983	48.633921
3503.487825	474297.781800	48.638925
3503.788678	474280.348151	48.643930
3503.625834	474281.843870	48.648935
3503.443779	474263.117955	48.653940
3503.496366	474251.248563	48.658945
3503.492359	474244.811777	48.663949
3503.483113	474234.929000	48.668954
3503.166777	474243.849503	48.673959
3503.278884	474237.292983	48.678964
3503.657874	474238.703055	48.683969
3503.821568	474238.727882	48.688973
3503.879083	474211.803203	48.693978
3503.286777	474201.860511	48.698983
3503.508788	474194.475587	48.703988
3503.265694	474197.403278	48.708993
3503.464590	474194.685357	48.713997
3503.767843	474194.485369	48.719002
3503.316168	474180.161217	48.724007
3503.689612	474157.089549	48.729012
3503.650213	474158.109565	48.734017
3503.433359	474154.798406	48.739021
3503.072959	474149.533077	48.744026
3503.366032	474157.799710	48.749031
3503.266197	474151.732863	48.754036
3503.625034	474165.970363	48.759041
3503.354140	474154.101359	48.764045
3503.582767	474144.282314	48.769050
3503.397891	474125.404652	48.774055
3503.236910	474106.371129	48.779060
3503.167081	474099.741946	48.784065
3503.202749	474104.653138	48.789069
3503.228329	474098.921272	48.794074
3503.523213	474100.648782	48.799079
3503.473093	474102.734961	48.804084
3503.457100	474107.502252	48.809089
3503.204595	474105.717384	48.814093
3503.452579	474091.231882	48.819098
3503.158106	474108.766091	48.824103
3503.358474	474103.817618	48.829108
3503.275612	474091.006455	48.834113
3503.148807	474088.492072	48.839117
3503.297142	474086.491773	48.844122
3503.444444	474068.980838	48.849127
3503.484304	474059.951924	48.854132
3503.576715	474061.103176	48.859137
3503.423111	474058.086136	48.864141
3503.795798	474052.603522	48.869146
3503.590782	474062.976487	48.874151
3503.430154	474041.509778	48.879156
3503.579263	474021.261312	48.884161
3503.489324	474019.805562	48.889165
3503.704795	474008.417170	48.894170
3503.136958	474020.216114	48.899175
3503.467097	474002.676220	48.904180
3503.303811	474011.167119	48.909185
3503.474555	474008.098800	48.914189
3503.580863	474005.902381	48.919194
3503.557806	473984.059042	48.924199
3503.515705	473982.849173	48.929204
3503.802795	473968.560158	48.934209
3503.638817	473969.245052	48.939213
3503.535055	473965.966674	48.944218
3503.224550	473971.743645	48.949223
3503.232795	473954.964242	48.954228
3503.612283	473931.587228	48.959233
3503.343480	473930.463881	48.964237
3503.774299	473931.764403	48.969242
3503.549060	473931.039684	48.974247
3503.265217	473926.775980	48.979252
3503.463509	473912.957166	48.984257
3503.135450	473923.197584	48.989261
3503.347381	473924.127194	48.994266
3503.238639	473911.320009	48.999271
3503.377015	473914.288818	49.004276
3503.351282	473896.500952	49.009281
3503.115489	473883.308318	49.014285
3503.569198	473872.693221	49.019290
3503.670458	473874.349979	49.024295
3503.462605	473870.682524	49.029300
3503.499834	473882.081766	49.034305
3503.314856	473879.171037	49.039309
3503.676928	473869.533522	49.044314
3503.202965	473880.760124	49.049319
3503.510462	473863.375757	49.054324
3503.555593	473845.728712	49.059329
3503.204291	473842.489443	49.064333
3503.592591	473835.483619	49.069338
3503.463603	473842.600550	49.074343
3503.559755	473843.142950	49.079348
3503.851396	473835.239994	49.084353
3503.557535	473816.429962	49.089357
3503.614216	473802.785527	49.094362
3503.692953	473802.519647	49.099367
3503.773782	473799.718959	49.104372
3503.727863	473806.822771	49.109377
3503.777721	473774.424250	49.114381
3503.783897	473756.986045	49.119386
3503.497664	473754.446131	49.124391
3503.214594	473746.481919	49.129396
3503.457097	473748.521878	49.134401
3503.305362	473746.467600	49.139405
3503.607602	473740.843970	49.144410
3503.599598	473725.283498	49.149415
3503.219430	473706.334938	49.154420
3503.401003	473708.992810	49.159425
3503.166046	473709.080655	49.164429
3503.524582	473695.946021	49.169434
3503.450182	473699.404705	49.174439
3503.385352	473701.645319	49.179444
3503.550425	473706.536152	49.184449
3503.391952	473698.248087	49.189453
3503.664532	473683.809097	49.194458
3503.675411	473670.628022	49.199463
3503.429046	473658.906921	49.204468
3503.599185	473646.004795	49.209473
3503.509176	473660.465671	49.214477
3503.669801	473644.270202	49.219482
3503.437931	473645.371359	49.224487
3503.103528	473628.544470	49.229492
3503.476490	473616.319924	49.234497
3503.012376	473617.052274	49.239501
3503.412387	473604.316544	49.244506
3503.286218	473614.119683	49.249511
3503.457094	473612.115775	49.254516
3503.677911	473610.965703	49.259521
3503.314818	473610.414833	49.264525
3503.591664	473602.159295	49.269530
3503.750672	473610.548725	49.274535
3503.668485	473579.640778	49.279540
3503.487392	473567.047573	49.284545
3503.519219	473572.719854	49.289549
3503.625323	473560.081246	49.294554
3503.443999	473558.589218	49.299559
3503.361749	473563.823322	49.304564
3503.716389	473555.960990	49.309569
3503.448272	473541.151158	49.314573
3503.521562	473530.798779	49.319578
3503.366525	473524.892541	49.324583
3503.215549	473517.262191	49.329588
3503.020626	473509.182571	49.334593
3503.312892	473519.933417	49.339597
3503.294246	473523.028485	49.344602
3503.249867	473514.519549	49.349607
3502.850064	473521.527330	49.354612
3503.289321	473516.997165	49.359617
3503.075818	473518.095425	49.364621
3503.380920	473506.236372	49.369626
3503.357526	473527.276552	49.374631
3503.393065	473515.308045	49.379636
3503.390999	473519.211538	49.384641
3503.024952	473530.725414	49.389645
3503.546610	473513.915179	49.394650
3503.441500	473520.268094	49.399655
3503.462697	473494.615463	49.404660
3503.582547	473478.223547	49.409665
3503.400352	473479.316860	49.414669
3503.874045	473470.675321	49.419674
3503.487758	473483.763825	49.424679
3503.516662	473464.142090	49.429684
3503.576715	473450.446196	49.434689
3503.174748	473438.597492	49.439693
3503.665592	473427.368009	49.444698
3502.949476	473445.020130	49.449703
3503.084711	473436.938983	49.454708
3503.302471	473435.992146	49.459713
3503.198992	473447.464565	49.464717
3503.369001	473430.963301	49.469722
3503.208713	473445.029915	49.474727
3503.435947	473427.201650	49.479732
3503.439692	473429.887669	49.484737
3502.839774	473447.926944	49.489741
3503.625406	473426.411388	49.494746
3503.542130	473437.627165	49.499751
3503.170138	473423.999548	49.504756
3503.248187	473426.673822	49.509761
3503.312399	473412.368959	49.514765
3503.593360	473397.877751	49.519770
3503.710073	473379.914843	49.524775
3503.617923	473384.339508	49.529780
3503.549371	473385.262790	49.534785
3503.202823	473386.838303	49.539789
3503.343068	473377.489075	49.544794
3503.019458	473395.535410	49.549799
3503.270259	473385.002825	49.554804
3503.493584	473368.036867	49.559809
3503.392323	473367.292529	49.564813
3503.544323	473345.826358	49.569818
3503.446415	473348.224312	49.574823
3503.457450	473330.379448	49.579828
3503.481860	473338.435431	49.584833
3503.267433	473344.096011	49.589837
3503.669879	473333.995645	49.594842
3503.778296	473340.619007	49.599847
3503.303028	473315.247392	49.604852
3503.765330	473295.404913	49.609857
3503.819197	473288.553149	49.614861
3503.563334	473288.694991	49.619866
3503.569799	473292.952014	49.624871
3503.475240	473274.464812	49.629876
3503.304167	473261.869834	49.634881
3503.277781	473258.984637	49.639885
3503.489745	473246.582557	49.644890
3503.482081	473253.274988	49.649895
3503.063979	473246.903344	49.654900
3503.557862	473248.143253	49.659905
3503.339508	473243.311451	49.664909
3503.506045	473239.027099	49.669914
3503.174912	473238.116329	49.674919
3503.413307	473240.055608	49.679924
3503.420520	473234.326402	49.684929
3503.003372	473225.876269	49.689933
3503.235797	473221.682881	49.694938
3503.208306	473220.470656	49.699943
3503.065142	473201.636233	49.704948
3503.375199	473206.301505	49.709953
3502.778261	473205.280677	49.714957
3503.378144	473214.766472	49.719962
3503.114510	473220.992466	49.724967
3503.239732	473207.843708	49.729972
3503.361077	473198.041166	49.734977
3503.369516	473212.588180	49.739981
3503.858706	473201.967127	49.744986
3503.594615	473198.764660	49.749991
3503.444126	473201.779236	49.754996
3503.826907	473188.589752	49.760001
3503.670442	473177.259691	49.765005
3503.635864	473156.431108	49.770010
3503.721911	473159.002770	49.775015
3503.369566	473149.123009	49.780020
3503.681875	473142.787947	49.785025
3503.351521	473146.388566	49.790029
3503.357918	473125.452092	49.795034
3503.578429	473115.278996	49.800039
3503.256529	473101.643244	49.805044
3503.542539	473108.593448	49.810049
3503.272546	473112.437989	49.815053
3503.216122	473108.898532	49.820058
3503.404875	473110.794978	49.825063
3503.159763	473113.621760	49.830068
3503.392735	473099.746222	49.835073
3503.348986	473107.356849	49.840077
3503.239655	473111.885671	49.845082
3503.454108	473098.874812	49.850087
3503.049266	473103.399657	49.855092
3503.199131	473105.403634	49.860097
3502.873526	473104.339910	49.865101
3503.066264	473110.950018	49.870106
3503.214373	473101.700803	49.875111
3503.202621	473106.366276	49.880116
3503.462664	473102.067114	49.885121
3503.116326	473109.015894	49.890125
3503.027548	473101.375555	49.895130
3503.211047	473099.217527	49.900135
3503.026590	473106.901088	49.905140
3503.149775	473107.591308	49.910145
3503.455455	473100.547602	49.915149
3503.530013	473090.803096	49.920154
3503.383036	473076.480689	49.925159
3503.635502	473069.749532	49.930164
3503.910226	473062.812089	49.935169
3503.499298	473072.761884	49.940173
3503.749038	473056.247714	49.945178
3503.557701	473037.674211	49.950183
3503.528422	473025.259440	49.955188
3503.659551	473015.810104	49.960193
3503.130485	473029.580458	49.965197
3503.401347	473012.049084	49.970202
3503.495184	473021.158740	49.975207
3503.299204	473016.576805	49.980212
3503.652675	473021.235257	49.985217
3503.397684	473005.510512	49.990221
3503.123747	472986.240338	49.995226
3503.182841	472978.424503	50.000231
3503.426352	472975.141761	50.005236
3503.480510	472975.437364	50.010241
3503.586678	472977.245495	50.015245
3503.417876	472977.018734	50.020250
3503.587028	472978.259301	50.025255
3503.221683	472976.694935	50.030260
3503.631154	472970.496536	50.035265
3503.587927	472962.139261	50.040269
3503.512606	472929.049500	50.045274
3503.468216	472929.411374	50.050279
3503.471085	472925.203520	50.055284
3503.451582	472932.759687	50.060289
3503.397712	472929.777405	50.065293
3503.369004	472927.247370	50.070298
3503.491785	472929.813255	50.075303
3503.102845	472917.201812	50.080308
3503.299022	472898.364160	50.085313
3502.923296	472893.557152	50.090317
3503.284876	472901.103783	50.095322
3503.240291	472884.686692	50.100327
3503.310356	472889.339281	50.105332
3503.393199	472877.160154	50.110337
3503.100649	472893.681265	50.115341
3503.144951	472884.245594	50.120346
3503.344443	472884.416842	50.125351
3502.980682	472884.879892	50.130356
3503.280900	472879.154962	50.135361
3503.170646	472886.978951	50.140365
3503.487487	472887.689258	50.145370
3503.347064	472892.527195	50.150375
3503.350757	472883.909012	50.155380
3503.742950	472887.446153	50.160385
3503.455946	472888.606756	50.165389
3503.274559	472884.681479	50.170394
3503.511135	472872.934275	50.175399
3502.836252	472860.367997	50.180404
3503.276756	472858.372087	50.185409
3503.236436	472849.406003	50.190413
3503.206258	472834.558044	50.195418
3503.388520	472846.289783	50.200423
3503.103282	472837.818637	50.205428
3503.431774	472841.112396	50.210433
3503.131413	472854.289103	50.215437
3503.633241	472844.122095	50.220442
3503.574860	472830.900734	50.225447
3503.097454	472846.082421	50.230452
3503.456417	472837.357367	50.235457
3503.504816	472836.893504	50.240461
3503.437573	472845.319013	50.245466
3503.548955	472831.006286	50.250471
3503.523500	472805.208087	50.255476
3503.777690	472795.232276	50.260481
3503.198802	472794.056497	50.265485
3503.349024	472791.092624	50.270490
3503.664665	472789.826134	50.275495
3503.243874	472796.381251	50.280500
3503.530627	472783.865684	50.285505
3503.314985	472786.941312	50.290509
3503.387284	472767.971045	50.295514
3503.137961	472760.102496	50.300519
3503.567008	472748.274104	50.305524
3503.674467	472746.229444	50.310529
3503.228490	472744.779190	50.315533
3503.286491	472743.046501	50.320538
3503.115499	472745.506771	50.325543
3503.100122	472751.237434	50.330548
3503.255044	472741.784211	50.335553
3503.392267	472745.868603	50.340557
3503.526019	472747.621701	50.345562
3503.470747	472757.515428	50.350567
3503.621967	472744.818493	50.355572
3503.219344	472725.112184	50.360577
3503.408166	472725.639965	50.365581
3503.140540	472706.926145	50.370586
3503.242043	472713.905650	50.375591
3503.124634	472715.495684	50.380596
3503.303157	472713.287711	50.385601
3503.098870	472715.601170	50.390605
3503.567840	472703.360904	50.395610
3503.523523	472711.833536	50.400615
3503.526903	472700.528635	50.405620
3503.395237	472699.687693	50.410625
3503.190733	472714.978415	50.415629
3503.098140	472701.103378	50.420634
3503.280952	472700.618264	50.425639
3503.161363	472709.305566	50.430644
3503.445633	472692.329413	50.435649
3503.628017	472674.152735	50.440653
3503.442496	472665.108139	50.445658
3503.204284	472664.436115	50.450663
3502.846215	472667.027351	50.455668
3503.348270	472661.574609	50.460673
3503.150404	472669.970147	50.465677
3503.250555	472663.820550	50.470682
3503.440621	472657.403277	50.475687
3503.267826	472660.066611	50.480692
3503.103626	472665.516669	50.485697
3503.151868	472656.435117	50.490701
3503.251757	472658.903270	50.495706
3503.538310	472658.705910	50.500711
3503.178927	472656.329498	50.505716
3503.897165	472650.284964	50.510721
3503.397736	472638.755354	50.515725
3503.334425	472628.576189	50.520730
3503.741651	472601.746181	50.525735
3503.348431	472579.807773	50.530740
3503.273835	472542.459092	50.535745
3503.148354	472510.745286	50.540749
3503.093035	472441.659670	50.545754
3503.182479	472386.592926	50.550759
3503.044064	472312.501393	50.555764
3503.188315	472227.516507	50.560769
3502.696496	472133.000013	50.565773
3502.727684	472027.703981	50.570778
3502.795072	471909.930902	50.575783
3502.537642	471784.705697	50.580788
3502.209817	471659.896416	50.585793
3501.857647	471524.545622	50.590797
3501.658991	471365.292052	50.595802
3501.767729	471219.017527	50.600807
3501.485563	471054.755856	50.605812
3500.795565	470884.879304	50.610817
3500.503497	470700.844622	50.615821
3500.383510	470527.376913	50.620826
3500.434653	470341.256868	50.625831
3499.597586	470146.960986	50.630836
3499.502440	469944.079253	50.635841
3499.130483	469728.057395	50.640845
3498.386211	469512.700546	50.645850
3498.431507	469298.129263	50.650855
3497.746019	469079.716596	50.655860
3497.690183	468845.738068	50.660865
3497.360110	468622.549161	50.665869
3497.053055	468372.076075	50.670874
3496.667775	468125.668637	50.675879
3496.219966	467871.561156	50.680884
3495.690651	467617.007136	50.685889
3495.309153	467350.967248	50.690893
3494.588640	467077.523795	50.695898
3494.439663	466820.263289	50.700903
3493.760374	466542.547014	50.705908
3493.356711	466262.045282	50.710913
3492.868485	465983.835088	50.715917
3492.284239	465700.616191	50.720922
3491.935453	465420.449602	50.725927
3491.202301	465127.307426	50.730932
3490.880810	464823.497444	50.735937
3490.619824	464521.600629	50.740941
3490.383740	464227.505390	50.745946
3489.622735	463906.712310	50.750951
3488.426403	463612.557559	50.755956
3488.738048	463290.368542	50.760961
3487.985630	462980.616136	50.765965
3487.439954	462661.139726	50.770970
3487.079196	462332.753818	50.775975
3486.327991	462000.316474	50.780980
3485.950607	461668.677147	50.785985
3485.017595	461347.416672	50.790989
3484.653610	461007.497817	50.795994
3484.294720	460669.348088	50.800999
3483.191969	460330.245544	50.806004
3482.886822	459997.301267	50.811009
3482.329982	459654.957130	50.816013
3481.842691	459315.995183	50.821018
3481.417036	458962.054338	50.826023
3480.471745	458621.530877	50.831028
3480.300201	458259.422413	50.836033
3479.522837	457909.172590	50.841037
3478.786892	457554.345119	50.846042
3478.453503	457201.629686	50.851047
3477.618208	456850.662090	50.856052
3476.923122	456487.694319	50.861057
3476.517129	456130.559810	50.866061
3475.717840	455761.103048	50.871066
3475.165451	455401.341953	50.876071
3474.415105	455034.249939	50.881076
3473.835792	454673.568232	50.886081
3472.930972	454315.468999	50.891085
3472.344178	453948.434909	50.896090
3472.033373	453572.928826	50.901095
3471.138575	453218.007095	50.906100
3470.470495	452835.695639	50.911105
3469.780250	452473.068345	50.916109
3469.176856	452106.565267	50.921114
3468.584462	451736.045996	50.926119
3467.833194	451368.539648	50.931124
3466.905867	450987.100888	50.936129
3466.299874	450634.681296	50.941133
3465.522649	450266.704758	50.946138
3465.006523	449900.152704	50.951143
3463.868412	449539.731994	50.956148
3463.788225	449170.156192	50.961153
3462.859572	448813.547884	50.966157
3462.134402	448447.665684	50.971162
3461.619885	448081.236954	50.976167
3460.972095	447701.171723	50.981172
3460.073095	447336.974404	50.986177
3459.543972	446974.996802	50.991181
3458.885624	446610.953208	50.996186
3458.352008	446242.519484	51.001191
3457.344975	445879.585574	51.006196
3457.056559	445504.402042	51.011201
3456.184688	445149.099606	51.016205
3455.418872	444782.304115	51.021210
3454.984477	444411.491514	51.026215
3454.346241	444045.476660	51.031220
3454.005797	443672.658200	51.036225
3452.868253	443310.314959	51.041229
3452.100677	442932.324303	51.046234
3451.524114	442558.866044	51.051239
3450.377844	442204.730908	51.056244
3449.624479	441836.213372	51.061249
3449.126893	441479.020845	51.066253
3448.380864	441113.943127	51.071258
3448.052629	440754.276520	51.076263
3446.833225	440391.547275	51.081268
3446.496521	440020.702752	51.086273
3445.626763	439656.028990	51.091277
3444.971411	439300.251108	51.096282
3444.250877	438933.258497	51.101287
3443.223693	438581.489018	51.106292
3442.585550	438228.739172	51.111297
3442.321342	437879.555320	51.116301
3441.474397	437518.933532	51.121306
3440.851813	437160.327343	51.126311
3439.756819	436805.801780	51.131316
3439.425996	436446.326864	51.136321
3438.778264	436096.772568	51.141325
3437.651233	435747.213035	51.146330
3437.344318	435390.715008	51.151335
3436.540825	435031.954741	51.156340
3435.708215	434675.605926	51.161345
3434.878913	434327.528425	51.166349
3434.304772	433979.024981	51.171354
3433.828855	433631.491446	51.176359
3432.838499	433289.823469	51.181364
3432.269279	432931.986810	51.186369
3431.532342	432581.788924	51.191373
3430.582159	432242.487396	51.196378
3429.989388	431895.710586	51.201383
3429.314208	431554.985405	51.206388
3428.578166	431207.891940	51.211393
3427.753215	430871.015670	51.216397
3427.068304	430522.940063	51.221402
3426.614938	430181.120703	51.226407
3425.545336	429847.139318	51.231412
3425.175302	429503.571178	51.236417
3424.414899	429162.472710	51.241421
3423.618750	428826.251209	51.246426
3422.931098	428490.592348	51.251431
3422.213425	428147.975713	51.256436
3421.553811	427810.297578	51.261441
3420.522772	427478.006984	51.266445
3420.143274	427139.336394	51.271450
3419.393419	426812.021456	51.276455
3418.555457	426490.557679	51.281460
3418.094542	426155.823990	51.286465
3417.389336	425820.286644	51.291469
3416.224209	425494.062572	51.296474
3416.007284	425163.138397	51.301479
3414.874921	424839.745807	51.306484
3414.514428	424506.448868	51.311489
3413.565751	424182.181240	51.316493
3412.821787	423846.650947	51.321498
3412.627683	423519.716205	51.326503
3411.625130	423194.327772	51.331508
3410.912009	422868.330907	51.336513
3410.193682	422560.339856	51.341517
3409.482277	422224.174933	51.346522
3408.835123	421905.674829	51.351527
3407.815689	421584.435781	51.356532
3407.270712	421258.367895	51.361537
3406.312129	420946.688222	51.366541
3405.564182	420635.606803	51.371546
3405.251483	420316.527538	51.376551
3404.214176	420016.738243	51.381556
3403.694556	419691.460909	51.386561
3403.344636	419382.665097	51.391565
3402.438692	419070.270302	51.396570
3402.016531	418745.830343	51.401575
3401.057733	418439.610054	51.406580
3400.469509	418115.316142	51.411585
3399.765321	417813.824859	51.416589
3398.700619	417487.388914	51.421594
3398.432230	417173.881610	51.426599
3397.363252	416874.165625	51.431604
3397.075277	416563.805014	51.436609
3396.335739	416248.939359	51.441613
3395.309169	415951.976294	51.446618
3394.620440	415633.437362	51.451623
3393.884459	415339.115138	51.456628
3393.313916	415016.536437	51.461633
3392.279808	414720.298719	51.466637
3391.649407	414422.088570	51.471642
3391.037365	414108.703932	51.476647
3390.030834	413824.419878	51.481652
3389.247074	413521.041507	51.486657
3388.684863	413221.893627	51.491661
3388.185000	412921.157488	51.496666
3387.517450	412634.419865	51.501671
3386.920719	412342.103586	51.506676
3386.319599	412033.700760	51.511681
3385.443352	411744.776869	51.516685
3384.833172	411454.537584	51.521690
3384.299655	411156.812668	51.526695
3383.400103	410865.952738	51.531700
3382.814551	410560.530658	51.536705
3382.270348	410261.324682	51.541709
3381.411565	409980.741263	51.546714
3380.825958	409677.317719	51.551719
3379.630643	409387.989538	51.556724
3379.120067	409100.405400	51.561729
3378.551634	408803.831671	51.566733
3377.884480	408521.018932	51.571738
3377.552468	408230.120078	51.576743
3376.418259	407941.759559	51.581748
3376.035639	407658.690524	51.586753
3375.453677	407361.799955	51.591757
3374.690630	407070.805763	51.596762
3373.765532	406772.667657	51.601767
3372.778905	406481.855743	51.606772
3372.196423	406197.152936	51.611777
3371.644158	405919.736797	51.616781
3370.858661	405634.374727	51.621786
3370.432273	405341.226995	51.626791
3369.832525	405071.969123	51.631796
3369.056963	404775.999345	51.636801
3368.497167	404494.861018	51.641805
3367.728167	404218.023184	51.646810
3366.972142	403921.533935	51.651815
3366.336038	403642.331709	51.656820
3366.085277	403351.577628	51.661825
3365.262609	403068.282297	51.666829
3364.034956	402783.370934	51.671834
3363.603677	402495.789318	51.676839
3363.018284	402230.114236	51.681844
3362.169546	401942.771581	51.686849
3361.583081	401655.994910	51.691853
3360.539841	401375.972979	51.696858
3359.956202	401098.824499	51.701863
3359.303379	400821.023686	51.706868
3358.730359	400535.378764	51.711873
3358.149064	400264.170840	51.716877
3357.250838	399996.289897	51.721882
3356.495438	399707.819541	51.726887
3355.880120	399437.652319	51.731892
3355.208019	399160.679221	51.736897
3354.516688	398890.112775	51.741901
3353.551586	398608.020994	51.746906
3352.956031	398347.730303	51.751911
3352.525378	398070.023465	51.756916
3351.771658	397794.221140	51.761921
3351.199201	397521.057109	51.766925
3350.530389	397261.888005	51.771930
3350.060202	396975.255234	51.776935
3349.057518	396709.118179	51.781940
3348.391678	396437.256555	51.786945
3347.588886	396166.380439	51.791949
3347.131562	395883.651351	51.796954
3346.447924	395613.514617	51.801959
3345.670692	395351.932699	51.806964
3344.821840	395088.351638	51.811969
3344.294763	394810.912652	51.816973
3343.470012	394549.357474	51.821978
3342.812098	394276.282276	51.826983
3341.964443	394020.396199	51.831988
3341.779399	393750.826818	51.836993
3340.590356	393484.871836	51.841997
3340.029270	393225.527611	51.847002
3339.448635	392949.073547	51.852007
3338.729852	392689.953629	51.857012
3338.109878	392425.120871	51.862017
3337.201721	392163.077621	51.867021
3336.347584	391907.609106	51.872026
3335.998803	391652.491032	51.877031
3334.953708	391383.242613	51.882036
3334.157273	391122.470595	51.887041
3333.827447	390874.641185	51.892045
3332.966974	390611.765102	51.897050
3332.351181	390350.755371	51.902055
3331.611162	390101.154656	51.907060
3331.161223	389845.251213	51.912065
3330.461364	389580.282445	51.917069
3329.898055	389328.817570	51.922074
3329.249728	389063.455388	51.927079
3328.326531	388811.687792	51.932084
3327.461142	388560.748408	51.937089
3326.829127	388298.480196	51.942093
3326.154200	388044.404826	51.947098
3325.872793	387791.460570	51.952103
3325.117633	387540.878064	51.957108
3324.127848	387275.760106	51.962113
3323.524206	387031.787084	51.967117
3322.694226	386777.142459	51.972122
3322.303779	386522.095953	51.977127
3321.478577	386275.381083	51.982132
3321.146394	386015.413891	51.987137
3320.521101	385764.493459	51.992141
3319.682401	385524.362055	51.997146
3319.055565	385255.586366	52.002151
3318.181173	385010.828926	52.007156
3317.555225	384758.401345	52.012161
3316.981244	384503.013837	52.017165
3316.137915	384257.941342	52.022170
3315.710813	384003.544421	52.027175
3314.445124	383750.600833	52.032180
3314.171440	383510.010993	52.037185
3313.516125	383256.026559	52.042189
3312.716886	383011.752745	52.047194
3312.456257	382754.548941	52.052199
3311.411057	382499.069711	52.057204
3310.741173	382257.084896	52.062209
3309.954141	382010.132274	52.067213
3309.080907	381771.940559	52.072218
3308.802286	381516.130010	52.077223
3308.126870	381281.922356	52.082228
3307.595564	381027.623628	52.087233
3306.453976	380784.406986	52.092237
3305.875146	380532.045436	52.097242
3305.129313	380292.807038	52.102247
3304.329826	380050.269236	52.107252
3303.877783	379816.068207	52.112257
3303.258208	379572.430731	52.117261
3302.141187	379333.728377	52.122266
3302.088058	379098.061043	52.127271
3301.248695	378844.636051	52.132276
3300.558477	378608.939366	52.137281
3300.099636	378364.861987	52.142285
3298.934019	378124.710160	52.147290
3298.488374	377866.333038	52.152295
3297.710106	377636.545466	52.157300
3296.822479	377390.011774	52.162305
3296.364551	377151.522607	52.167309
3295.387980	376918.557340	52.172314
3294.815802	376686.518758	52.177319
3294.071238	376456.210325	52.182324
3293.644684	376223.866233	52.187329
3292.949080	375987.569820	52.192333
3291.999362	375758.154682	52.197338
3291.685713	375522.049496	52.202343
3290.699757	375281.903046	52.207348
3289.856993	375047.023449	52.212353
3289.717594	374815.210902	52.217357
3288.500064	374588.858551	52.222362
3287.901934	374360.219344	52.227367
3287.636337	374121.402060	52.232372
3286.818449	373887.376748	52.237377
3286.327625	373660.929769	52.242381
3285.466574	373438.661083	52.247386
3284.704279	373193.023255	52.252391
3283.999167	372959.229230	52.257396
3283.555332	372738.620611	52.262401
3282.834283	372500.578292	52.267405
3281.965854	372276.905432	52.272410
3281.542159	372040.314350	52.277415
3280.916072	371809.910214	52.282420
3280.276793	371585.612323	52.287425
3279.580671	371347.712157	52.292429
3278.473671	371118.804919	52.297434
3278.181433	370880.634725	52.302439
3277.449103	370654.693040	52.307444
3276.742307	370422.894928	52.312449
3276.150040	370191.789765	52.317453
3275.372538	369967.403430	52.322458
3274.904301	369744.060938	52.327463
3274.319688	369511.475356	52.332468
3273.580425	369275.249532	52.337473
3272.893197	369039.090508	52.342477
3271.882991	368821.425936	52.347482
3271.258274	368584.618526	52.352487
3270.625303	368362.846861	52.357492
3269.964085	368138.432643	52.362497
3269.147296	367906.104157	52.367501
3268.304150	367693.521257	52.372506
3267.691803	367460.725568	52.377511
3266.936962	367247.541385	52.382516
3266.639381	367015.634903	52.387521
3265.924136	366784.124021	52.392525
3264.922802	366575.835029	52.397530
3264.389712	366341.010981	52.402535
3263.976985	366127.054913	52.407540
3263.077324	365911.800947	52.412545
3262.708306	365676.438602	52.417549
3261.548162	365465.192759	52.422554
3261.081827	365231.497264	52.427559
3260.311719	365016.269403	52.432564
3259.490326	364797.970004	52.437569
3259.445736	364575.348527	52.442573
3258.221692	364363.776885	52.447578
3257.877216	364137.333300	52.452583
3257.345636	363922.367853	52.457588
3256.441248	363704.890545	52.462593
3255.902083	363469.874451	52.467597
3255.021295	363247.582343	52.472602
3254.501720	363034.646371	52.477607
3253.637426	362815.148433	52.482612
3252.774675	362601.526872	52.487617
3252.438154	362372.528920	52.492621
3251.379461	362165.501046	52.497626
3251.161409	361941.291277	52.502631
3250.226626	361735.234243	52.507636
3249.543086	361522.749867	52.512641
3249.160642	361300.242413	52.517645
3248.407752	361093.135992	52.522650
3247.898312	360871.206403	52.527655
3246.872462	360659.917338	52.532660
3246.251218	360430.700529	52.537665
3245.885194	360216.149863	52.542669
3244.724522	359992.079975	52.547674
3244.276258	359781.611703	52.552679
3243.704050	359562.052431	52.557684
3242.835153	359349.027864	52.562689
3242.220464	359126.954162	52.567693
3241.653388	358909.732171	52.572698
3240.806122	358702.452222	52.577703
3240.081654	358485.813058	52.582708
3239.351723	358279.352486	52.587713
3238.706090	358062.546293	52.592717
3237.944279	357856.445238	52.597722
3237.411835	357645.472095	52.602727
3237.030167	357435.746555	52.607732
3235.885366	357231.306644	52.612737
3235.539655	357006.865077	52.617741
3234.498678	356809.201452	52.622746
3234.126303	356587.306958	52.627751
3233.496618	356379.830137	52.632756
3232.460845	356166.105641	52.637761
3231.983069	355966.364658	52.642765
3231.143703	355767.418076	52.647770
3230.864610	355544.918914	52.652775
3230.404681	355330.768953	52.657780
3229.391960	355130.116809	52.662785
3228.766691	354915.991255	52.667789
3228.126167	354704.793798	52.672794
3227.250366	354493.581792	52.677799
3226.650989	354290.723272	52.682804
3225.968071	354084.467021	52.687809
3225.451277	353879.532459	52.692813
3224.514956	353684.334091	52.697818
3224.074279	353471.343971	52.702823
3223.446182	353272.277918	52.707828
3222.299312	353061.713721	52.712833
3221.717901	352848.081633	52.717837
3221.432850	352652.954512	52.722842
3220.674108	352437.338288	52.727847
3220.173143	352237.484698	52.732852
3219.244938	352035.102056	52.737857
3218.902535	351820.257290	52.742861
3217.937564	351626.277386	52.747866
3217.018823	351408.951679	52.752871
3216.440023	351205.288991	52.757876
3215.380722	351008.522236	52.762881
3215.135893	350813.051129	52.767885
3214.123782	350612.941451	52.772890
3213.658798	350413.507991	52.777895
3213.236417	350218.928140	52.782900
3212.535582	350019.759598	52.787905
3212.154996	349811.071925	52.792909
3211.203747	349610.898015	52.797914
3210.435531	349414.792040	52.802919
3209.831444	349209.751483	52.807924
3209.259189	348999.385807	52.812929
3208.557171	348799.525824	52.817933
3207.791705	348603.696485	52.822938
3207.192469	348395.114379	52.827943
3206.473163	348197.494694	52.832948
3205.826649	348006.302081	52.837953
3205.135848	347797.681319	52.842957
3204.289660	347604.330063	52.847962
3203.548095	347402.613331	52.852967
3203.224223	347201.415191	52.857972
3202.054860	347015.774125	52.862977
3201.516719	346819.393535	52.867981
3200.810348	346624.311499	52.872986
3200.230632	346417.755154	52.877991
3199.873279	346222.514715	52.882996
3199.169549	346036.694975	52.888001
3198.624902	345830.640015	52.893005
3198.012229	345628.616623	52.898010
3197.120226	345430.327385	52.903015
3196.430367	345227.933010	52.908020
3195.958366	345034.208409	52.913025
3195.456669	344829.339382	52.918029
3194.501271	344635.664483	52.923034
3193.724801	344431.422959	52.928039
3193.187883	344239.564087	52.933044
3192.214065	344043.548435	52.938049
3191.644924	343849.428031	52.943053
3190.957223	343652.016773	52.948058
3190.570578	343448.855587	52.953063
3189.596173	343251.870167	52.958068
3188.944399	343059.338395	52.963073
3188.407022	342865.057033	52.968077
3187.462581	342688.300941	52.973082
3186.958166	342486.351465	52.978087
3186.640316	342295.673477	52.983092
3185.554813	342101.807284	52.988097
3184.887241	341901.078023	52.993101
3184.129959	341712.020447	52.998106
3183.271125	341520.407443	53.003111
3182.926731	341328.966993	53.008116
3181.981009	341137.188357	53.013121
3181.693043	340948.563270	53.018125
3180.841324	340756.921308	53.023130
3180.259835	340570.250624	53.028135
3179.724483	340379.906555	53.033140
3178.988847	340186.488071	53.038145
3178.625264	339993.239219	53.043149
3177.810504	339799.246588	53.048154
3177.314992	339593.340656	53.053159
3176.428732	339405.518320	53.058164
3175.760708	339207.453241	53.063169
3175.494375	339011.309523	53.068173
3174.351655	338819.147669	53.073178
3173.790134	338627.504215	53.078183
3173.095170	338431.808373	53.083188
3172.321003	338243.226659	53.088193
3171.807468	338048.901019	53.093197
3171.075149	337856.213143	53.098202
3170.570777	337665.041450	53.103207
3169.708593	337464.787037	53.108212
3168.856652	337284.971772	53.113217
3168.252938	337078.463951	53.118221
3167.621141	336893.699705	53.123226
3167.026303	336699.612019	53.128231
3166.342504	336510.400042	53.133236
3165.670467	336329.229960	53.138241
3165.074376	336129.489430	53.143245
3164.616790	335941.894729	53.148250
3164.238625	335750.010183	53.153255
3163.460750	335549.482065	53.158260
3162.530672	335357.581898	53.163265
3162.274712	335158.395628	53.168269
3161.275881	334962.839401	53.173274
3160.223137	334768.258517	53.178279
3159.947988	334571.670201	53.183284
3159.026829	334388.370452	53.188289
3158.751283	334194.912373	53.193293
3157.949708	334005.126492	53.198298
3157.214053	333810.696380	53.203303
3156.790183	333613.059641	53.208308
3155.722961	333427.234689	53.213313
3155.202015	333223.451437	53.218317
3154.440882	333027.292040	53.223322
3153.737494	332842.655401	53.228327
3153.535240	332649.792425	53.233332
3152.471127	332456.148805	53.238337
3151.546637	332261.591529	53.243341
3150.993146	332071.837534	53.248346
3150.055108	331883.951421	53.253351
3149.702032	331691.975296	53.258356
3148.595529	331507.118937	53.263361
3148.517032	331319.095340	53.268365
3147.531239	331132.971458	53.273370
3146.987198	330945.326059	53.278375
3146.208590	330758.073714	53.283380
3145.579876	330576.398093	53.288385
3145.147468	330384.838405	53.293389
3144.126807	330209.970478	53.298394
3143.385789	330015.607271	53.303399
3142.849968	329826.888440	53.308404
3142.030689	329647.073733	53.313409
3141.992747	329453.106986	53.318413
3141.186757	329276.497133	53.323418
3140.215358	329099.556610	53.328423
3139.785351	328900.609545	53.333428
3138.887076	328721.976252	53.338433
3138.332366	328522.818793	53.343437
3137.484348	328349.395855	53.348442
3136.706741	328167.661568	53.353447
3136.588871	327978.159113	53.358452
3135.506198	327797.108713	53.363457
3134.709979	327598.827240	53.368461
3133.959656	327431.267972	53.373466
3133.598977	327243.966222	53.378471
3132.942712	327058.747589	53.383476
3132.298996	326882.895802	53.388481
3131.345656	326702.662570	53.393485
3130.724766	326522.503621	53.398490
3130.101335	326328.545263	53.403495
3129.618234	326154.626871	53.408500
3128.592995	325973.028507	53.413505
3128.131352	325786.783149	53.418509
3127.417663	325627.463401	53.423514
3126.474434	325437.016097	53.428519
3125.823715	325258.590329	53.433524
3124.915819	325084.609539	53.438529
3124.705320	324903.720040	53.443533
3123.831418	324736.251041	53.448538
3123.391631	324561.685849	53.453543
3122.802322	324375.355615	53.458548
3121.976914	324206.935816	53.463553
3121.601320	324022.124077	53.468557
3120.738641	323842.099277	53.473562
3119.717321	323674.855144	53.478567
3119.220262	323491.894642	53.483572
3118.523134	323320.804807	53.488577
3118.211325	323135.828252	53.493581
3117.574553	322968.496402	53.498586
3116.640072	322792.656356	53.503591
3116.180787	322608.593134	53.508596
3115.143595	322444.022518	53.513601
3114.606959	322256.126117	53.518605
3113.885001	322091.810479	53.523610
3113.185841	321923.849927	53.528615
3112.665622	321741.984188	53.533620
3111.849240	321563.780484	53.538625
3111.467115	321378.836743	53.543629
3110.530391	321210.250410	53.548634
3110.062063	321036.777360	53.553639
3109.559974	320864.658788	53.558644
3108.793698	320694.414944	53.563649
3107.998422	320510.120392	53.568653
3107.747565	320317.947946	53.573658
3106.569669	320151.714813	53.578663
3106.015455	319979.169935	53.583668
3105.428826	319803.421632	53.588673
3104.859023	319622.985289	53.593677
3104.082479	319455.108714	53.598682
3103.139082	319277.811739	53.603687
3102.811288	319105.152991	53.608692
3102.094293	318937.215123	53.613697
3101.793290	318750.445332	53.618701
3100.991126	318584.226285	53.623706
3099.661710	318408.134547	53.628711
3099.223512	318226.274219	53.633716
3098.610445	318062.901591	53.638721
3098.509049	317874.392476	53.643725
3097.707931	317712.296673	53.648730
3096.633202	317531.095925	53.653735
3096.342908	317356.492867	53.658740
3095.596642	317191.994002	53.663745
3095.499366	317000.401515	53.668749
3094.547427	316824.807301	53.673754
3093.597621	316639.689286	53.678759
3092.963108	316470.409941	53.683764
3092.202254	316287.705808	53.688769
3091.507521	316105.678375	53.693773
3090.694660	315934.974940	53.698778
3090.036322	315757.066139	53.703783
3089.806521	315583.494342	53.708788
3088.857815	315411.894836	53.713793
3088.236277	315232.451485	53.718797
3087.618840	315054.993310	53.723802
3087.063527	314888.041382	53.728807
3086.188214	314714.315619	53.733812
3085.101613	314532.983951	53.738817
3084.851646	314360.991997	53.743821
3084.044693	314200.317343	53.748826
3083.611207	314026.545964	53.753831
3083.032575	313845.794759	53.758836
3082.060966	313683.770331	53.763841
3081.385608	313495.802140	53.768845
3080.750243	313332.960048	53.773850
3079.911366	313162.714476	53.778855
3079.498799	312986.264372	53.783860
3078.634366	312827.022703	53.788865
3078.099435	312642.493877	53.793869
3077.117878	312471.022058	53.798874
3076.704265	312303.738041	53.803879
3075.977634	312134.262470	53.808884
3075.415572	311978.256569	53.813889
3074.779397	311807.238331	53.818893
3074.293070	311625.984974	53.823898
3073.345352	311453.080218	53.828903
3072.453804	311287.092585	53.833908
3072.020772	311125.310143	53.838913
3071.561115	310949.042473	53.843917
3070.970840	310787.921043	53.848922
3069.837158	310611.963240	53.853927
3069.643219	310438.963101	53.858932
3069.035904	310267.123098	53.863937
3068.362271	310094.936832	53.868941
3067.583669	309919.838498	53.873946
3066.928701	309749.635004	53.878951
3066.048420	309571.063590	53.883956
3065.492780	309405.402048	53.888961
3065.146801	309230.870835	53.893965
3064.313983	309065.481870	53.898970
3063.692001	308889.440490	53.903975
3063.172481	308703.731466	53.908980
3062.331337	308536.484159	53.913985
3061.362951	308354.079677	53.918989
3061.121185	308190.556768	53.923994
3060.252125	308020.257379	53.928999
3059.824345	307849.964309	53.934004
3058.743815	307683.746863	53.939009
3058.218404	307509.521698	53.944013
3057.615754	307341.420141	53.949018
3056.906705	307188.970799	53.954023
3056.171311	306986.333577	53.959028
3055.688496	306823.203542	53.964033
3054.768799	306662.892693	53.969037
3054.308239	306491.889953	53.974042
3053.532000	306324.069185	53.979047
3053.006481	306147.524834	53.984052
3052.144822	305979.335161	53.989057
3051.532436	305799.569987	53.994061
3050.765685	305641.347304	53.999066
3050.199963	305480.367810	54.004071
3049.734146	305312.318364	54.009076
3048.873593	305141.861026	54.014081
3047.975634	304973.268381	54.019085
3047.531622	304807.481291	54.024090
3046.668783	304632.949181	54.029095
3046.573450	304453.660620	54.034100
3045.650432	304295.970414	54.039105
3045.010147	304116.945930	54.044109
3044.466449	303953.516442	54.049114
3043.435213	303790.953369	54.054119
3043.219300	303615.426289	54.059124
3042.227156	303457.287700	54.064129
3041.470735	303279.095444	54.069133
3041.049358	303111.189099	54.074138
3040.174481	302948.040071	54.079143
3039.878808	302779.960652	54.084148
3038.750825	302617.869955	54.089153
3038.376710	302434.446559	54.094157
3037.547709	302269.863420	54.099162
3036.768315	302115.815207	54.104167
3036.550522	301938.121794	54.109172
3035.388578	301779.651751	54.114177
3034.646622	301611.743518	54.119181
3034.234692	301440.905185	54.124186
3033.631830	301270.173281	54.129191
3033.264222	301101.492185	54.134196
3032.216739	300942.901300	54.139201
3031.772024	300761.269707	54.144205
3030.841242	300593.466661	54.149210
3030.335670	300430.969538	54.154215
3029.927456	300271.538272	54.159220
3028.830460	300106.740592	54.164225
3028.341614	299932.143773	54.169229
3027.713169	299768.723174	54.174234
3027.055529	299606.071029	54.179239
3026.489437	299418.115983	54.184244
3025.730949	299265.895273	54.189249
3024.985249	299095.565672	54.194253
3024.504451	298928.963026	54.199258
3023.543186	298763.964264	54.204263
3022.969693	298583.471180	54.209268
3022.539017	298422.208102	54.214273
3021.985268	298249.606211	54.219277
3021.491402	298079.515877	54.224282
3020.543077	297915.736664	54.229287
3019.677971	297731.086847	54.234292
3018.859230	297576.989650	54.239297
3018.398466	297410.942657	54.244301
3018.005696	297245.190352	54.249306
3017.332655	297069.422851	54.254311
3016.642757	296895.262264	54.259316
3015.851945	296727.229546	54.264321
3015.226610	296559.832624	54.269325
3014.895674	296384.825268	54.274330
3013.730971	296208.803714	54.279335
3013.660883	296036.072244	54.284340
3012.640139	295872.506425	54.289345
3011.504847	295694.162248	54.294349
3011.266777	295538.468912	54.299354
3010.089396	295363.441817	54.304359
3009.836213	295193.489034	54.309364
3008.819127	295027.578965	54.314369
3008.529930	294866.214030	54.319373
3007.991383	294704.073489	54.324378
3007.188280	294535.225892	54.329383
3007.024958	294351.964313	54.334388
3006.030966	294188.265562	54.339393
3005.046243	294015.575277	54.344397
3004.710832	293850.549590	54.349402
3003.790293	293685.820137	54.354407
3003.346614	293509.733057	54.359412
3002.690658	293346.005626	54.364417
3002.136942	293164.689418	54.369421
3001.551400	293001.994749	54.374426
3000.457540	292840.399123	54.379431
3000.223940	292666.009906	54.384436
2999.531653	292499.409796	54.389441
2998.736418	292310.541847	54.394445
2998.423687	292144.569023	54.399450
2997.485996	291973.779787	54.404455
2996.829054	291792.071364	54.409460
2995.939555	291623.235248	54.414465
2995.268784	291453.676769	54.419469
2994.411503	291283.281800	54.424474
2993.949200	291122.247192	54.429479
2993.554430	290945.182679	54.434484
2992.798062	290790.077423	54.439489
2991.796308	290612.497542	54.444493
2991.328241	290438.169318	54.449498
2990.569076	290278.505493	54.454503
2990.383744	290106.602657	54.459508
2989.425885	289930.568897	54.464513
2988.791819	289765.918766	54.469517
2988.200008	289594.563838	54.474522
2987.386811	289422.327011	54.479527
2986.795136	289253.926110	54.484532
2986.535680	289084.759421	54.489537
2985.500543	288906.827169	54.494541
2985.148320	288742.182763	54.499546
2984.262015	288567.384752	54.504551
2983.776863	288384.984660	54.509556
2982.976130	288222.881347	54.514561
2982.457465	288044.663082	54.519565
2981.549192	287866.022501	54.524570
2980.687963	287694.836462	54.529575
2980.315747	287519.574459	54.534580
2979.499222	287348.686773	54.539585
2978.614571	287183.412726	54.544589
2978.171736	287016.285900	54.549594
2977.374985	286846.948371	54.554599
2976.986153	286667.282596	54.559604
2975.956016	286506.462676	54.564609
2975.678834	286330.191761	54.569613
2975.142756	286150.701840	54.574618
2973.916096	285988.537526	54.579623
2973.459239	285825.054281	54.584628
2972.803346	285663.385235	54.589633
2972.014999	285488.926664	54.594637
2971.581084	285317.773689	54.599642
2970.992309	285151.407682	54.604647
2970.386739	284969.559675	54.609652
2969.579844	284805.596586	54.614657
2969.226623	284630.584863	54.619661
2968.568363	284454.908251	54.624666
2967.656325	284290.324904	54.629671
2967.053408	284105.114312	54.634676
2967.023085	283938.353801	54.639681
2965.848576	283767.826799	54.644685
2965.308700	283591.647210	54.649690
2964.566542	283419.701824	54.654695
2964.247218	283236.177824	54.659700
2963.298791	283061.921894	54.664705
2962.375915	282886.745004	54.669709
2961.698966	282705.442222	54.674714
2960.702899	282544.207909	54.679719
2960.499882	282356.386522	54.684724
2959.951162	282186.091002	54.689729
2959.300240	282012.602613	54.694733
2958.782334	281842.225708	54.699738
2957.935228	281666.272387	54.704743
2957.651602	281485.365371	54.709748
2956.832529	281319.212791	54.714753
2955.982698	281133.556342	54.719757
2955.504466	280948.426783	54.724762
2954.633367	280789.973725	54.729767
2954.550889	280602.769425	54.734772
2953.716116	280420.141126	54.739777
2952.789005	280234.496673	54.744781
2952.388964	280057.478894	54.749786
2951.479842	279879.854025	54.754791
2950.977882	279691.671712	54.759796
2950.005993	279521.646264	54.764801
2949.420640	279342.085371	54.769805
2948.771744	279159.325493	54.774810
2947.801981	278989.885383	54.779815
2947.357025	278806.023481	54.784820
2946.848928	278620.872658	54.789825
2945.981746	278454.064930	54.794829
2945.238027	278272.083960	54.799834
2944.596736	278107.430700	54.804839
2944.078564	277928.750327	54.809844
2943.075764	277760.945243	54.814849
2942.585566	277581.445409	54.819853
2942.169138	277400.354836	54.824858
2940.848227	277232.294437	54.829863
2940.435208	277054.234024	54.834868
2940.012645	276888.119775	54.839873
2939.642005	276709.441380	54.844877
2938.563047	276532.428684	54.849882
2938.064719	276362.760818	54.854887
2937.451930	276170.724352	54.859892
2936.962081	276012.770582	54.864897
2935.965589	275834.242154	54.869901
2935.349019	275660.543500	54.874906
2934.485434	275490.933423	54.879911
2933.957758	275307.211608	54.884916
2933.002831	275141.920144	54.889921
2932.581745	274966.687892	54.894925
2931.976571	274796.527526	54.899930
2931.191320	274624.103516	54.904935
2930.654789	274448.787670	54.909940
2929.828557	274285.589711	54.914945
2929.062479	274111.838320	54.919949
2928.667043	273936.169061	54.924954
2927.801887	273767.756262	54.929959
2927.122844	273594.984380	54.934964
2926.484769	273418.691384	54.939969
2926.003792	273236.668609	54.944973
2925.488767	273062.801120	54.949978
2924.596186	272884.358177	54.954983
2924.265640	272697.268891	54.959988
2923.146695	272534.473934	54.964993
2922.561686	272372.867876	54.969997
2922.267662	272190.255295	54.975002
2921.491232	272020.937197	54.980007
2920.983919	271845.489571	54.985012
2920.081999	271673.695485	54.990017
2919.430287	271497.353908	54.995021
2919.144759	271320.139393	55.000026
2918.327534	271137.125900	55.005031
2917.794117	270954.042035	55.010036
2916.822741	270788.065863	55.015041
2915.925919	270612.374479	55.020045
2915.676605	270438.847289	55.025050
2914.826090	270270.432580	55.030055
2914.438032	270078.004463	55.035060
2913.693046	269904.555858	55.040065
2913.035089	269728.291998	55.045069
2912.424518	269551.995206	55.050074
2911.703240	269379.154203	55.055079
2911.123525	269191.366409	55.060084
2910.657360	269011.557727	55.065089
2909.954937	268839.121362	55.070093
2909.293292	268654.632093	55.075098
2908.524044	268478.971933	55.080103
2908.011950	268291.351962	55.085108
2907.118189	268111.127334	55.090113
2906.614511	267927.759339	55.095117
2906.126081	267754.652686	55.100122
2905.372969	267575.348278	55.105127
2904.843544	267393.869180	55.110132
2904.254723	267199.792785	55.115137
2903.276807	267019.352619	55.120141
2902.747538	266833.875181	55.125146
2901.888027	266650.283810	55.130151
2901.408982	266458.584324	55.135156
2900.663961	266277.139759	55.140161
2899.898951	266098.296181	55.145165
2899.691896	265917.454216	55.150170
2898.626413	265747.648604	55.155175
2898.008914	265546.726486	55.160180
2897.736386	265368.798477	55.165185
2896.936605	265184.765277	55.170189
2896.133853	264990.137906	55.175194
2895.384319	264821.250422	55.180199
2894.807732	264626.969434	55.185204
2893.970207	264442.254909	55.190209
2893.676505	264259.924762	55.195213
2892.837145	264068.563548	55.200218
2891.909046	263893.974435	55.205223
2891.286105	263705.762641	55.210228
2890.440202	263520.566002	55.215233
2889.681938	263344.192970	55.220237
2889.112527	263163.002146	55.225242
2888.214570	262998.799625	55.230247
2887.905002	262818.510152	55.235252
2887.289581	262642.853431	55.240257
2886.702102	262453.185028	55.245261
2886.339320	262270.459358	55.250266
2885.594201	262097.497595	55.255271
2884.780134	261906.923079	55.260276
2884.544674	261716.944693	55.265281
2883.598741	261527.944828	55.270285
2883.274259	261344.475066	55.275290
2882.198023	261164.129651	55.280295
2881.673412	260974.273919	55.285300
2881.189682	260790.447697	55.290305
2880.403918	260607.382516	55.295309
2879.699179	260408.540092	55.300314
2878.578462	260232.710092	55.305319
2878.189675	260043.495632	55.310324
2877.480087	259863.347661	55.315329
2876.572643	259682.823656	55.320333
2876.200883	259494.880266	55.325338
2875.353120	259317.708789	55.330343
2874.795037	259135.830988	55.335348
2874.113645	258958.302332	55.340353
2873.531149	258778.185914	55.345357
2873.179950	258586.165114	55.350362
2872.150672	258408.437255	55.355367
2871.461655	258224.237829	55.360372
2870.856295	258033.480145	55.365377
2870.189508	257854.625654	55.370381
2869.575119	257670.007352	55.375386
2868.799007	257488.801973	55.380391
2868.148489	257313.001408	55.385396
2867.712411	257130.061614	55.390401
2866.909480	256940.431199	55.395405
2866.522228	256749.589087	55.400410
2865.311830	256562.595716	55.405415
2864.793964	256387.819023	55.410420
2864.167066	256202.694542	55.415425
2863.465127	256026.826723	55.420429
2863.038451	255837.850755	55.425434
2862.429190	255661.255477	55.430439
2861.923061	255474.380726	55.435444
2860.851033	255288.588973	55.440449
2860.257046	255108.375399	55.445453
2860.013002	254917.665037	55.450458
2858.995043	254736.805847	55.455463
2858.433468	254553.429707	55.460468
2857.764539	254364.722648	55.465473
2856.696849	254190.034859	55.470477
2856.534089	254004.533239	55.475482
2855.643401	253820.267615	55.480487
2854.945226	253635.003935	55.485492
2854.239141	253454.809611	55.490497
2853.564291	253274.483177	55.495501
2853.072447	253082.387690	55.500506
2852.070385	252911.510710	55.505511
2851.557893	252722.398490	55.510516
2851.296497	252552.983497	55.515521
2850.394220	252356.140528	55.520525
2850.063400	252162.314225	55.525530
2848.808432	251980.196385	55.530535
2848.604707	251801.426666	55.535540
2847.841752	251621.268618	55.540545
2846.690747	251438.319939	55.545549
2846.731542	251248.306724	55.550554
2845.810407	251069.396696	55.555559
2845.225202	250881.036484	55.560564
2844.533981	250694.144864	55.565569
2843.611681	250511.364691	55.570573
2843.185405	250326.316047	55.575578
2842.520879	250144.921579	55.580583
2841.901578	249949.742797	55.585588
2841.347276	249769.324480	55.590593
2840.365118	249593.609004	55.595597
2840.091977	249398.630730	55.600602
2839.052867	249217.373017	55.605607
2838.631355	249018.216758	55.610612
2838.115054	248838.124535	55.615617
2837.438065	248648.609989	55.620621
2836.866624	248453.934784	55.625626
2835.884383	248270.224405	55.630631
2835.376321	248072.636501	55.635636
2834.890958	247892.871541	55.640641
2833.707991	247711.994898	55.645645
2833.215316	247516.900960	55.650650
2832.491497	247338.625991	55.655655
2831.963679	247154.641281	55.660660
2831.261345	246980.310572	55.665665
2830.587693	246792.096597	55.670669
2829.908978	246593.315320	55.675674
2829.232697	246423.565015	55.680679
2828.474528	246230.068257	55.685684
2828.202955	246049.125737	55.690689
2827.147959	245867.569009	55.695693
2826.786704	245672.176621	55.700698
2825.868917	245490.955172	55.705703
2825.149399	245295.543653	55.710708
2824.625012	245106.416983	55.715713
2824.141451	244935.950388	55.720717
2823.512011	244750.635221	55.725722
2822.951519	244552.067316	55.730727
2821.988771	244358.503714	55.735732
2821.700888	244169.595552	55.740737
2820.850361	243993.458542	55.745741
2820.140740	243806.374803	55.750746
2819.494442	243615.818015	55.755751
2818.955763	243425.117136	55.760756
2818.157422	243229.695654	55.765761
2817.320215	243050.400115	55.770765
2816.897559	242860.038210	55.775770
2815.937024	242670.118286	55.780775
2815.434724	242486.594215	55.785780
2814.912496	242294.899276	55.790785
2814.128375	242115.087353	55.795789
2813.524666	241925.468554	55.800794
2812.465063	241740.404082	55.805799
2812.084741	241551.972797	55.810804
2811.194758	241359.624532	55.815809
2810.429924	241190.251509	55.820813
2809.973908	241003.310022	55.825818
2809.325867	240826.177711	55.830823
2808.816918	240638.939597	55.835828
2808.414991	240448.043376	55.840833
2807.283062	240259.427573	55.845837
2806.930128	240074.813965	55.850842
2805.905250	239898.863164	55.855847
2805.525149	239704.476047	55.860852
2804.903834	239517.079264	55.865857
2803.805120	239327.874026	55.870861
2803.685108	239150.737011	55.875866
2803.003827	238967.424928	55.880871
2802.511897	238771.427382	55.885876
2801.706535	238581.794959	55.890881
2800.861157	238390.539481	55.895885
2800.534325	238194.083902	55.900890
2799.742813	238014.304891	55.905895
2798.948200	237824.137306	55.910900
2798.356578	237634.574502	55.915905
2797.695726	237446.143407	55.920909
2797.302461	237244.709094	55.925914
2796.192457	237066.433529	55.930919
2795.371738	236867.435765	55.935924
2795.214139	236676.838266	55.940929
2793.962873	236490.004719	55.945933
2793.200894	236310.198393	55.950938
2792.407927	236129.556979	55.955943
2792.240041	235947.008952	55.960948
2791.537820	235762.203220	55.965953
2790.998643	235578.135899	55.970957
2790.390192	235390.871471	55.975962
2789.371614	235211.260458	55.980967
2788.959806	235021.622916	55.985972
2788.571458	234825.998112	55.990977
2787.696843	234638.318874	55.995981
2787.109112	234457.418708	56.000986
2786.765634	234269.910661	56.005991
2785.930198	234071.939119	56.010996
2785.234420	233871.144903	56.016001
2784.248113	233689.239800	56.021005
2784.049141	233490.939439	56.026010
2783.394688	233309.924606	56.031015
2782.333924	233123.270760	56.036020
2782.333410	232917.937810	56.041025
2781.167781	232731.097621	56.046029
2780.717186	232533.628404	56.051034
2780.009752	232349.288125	56.056039
2779.219166	232148.206914	56.061044
2778.674963	231958.647143	56.066049
2777.942766	231770.976296	56.071053
2777.646686	231578.984500	56.076058
2776.594051	231387.011074	56.081063
2775.971670	231187.025614	56.086068
2775.814336	230994.834799	56.091073
2774.537211	230801.599553	56.096077
2774.012945	230608.907485	56.101082
2773.247031	230420.811833	56.106087
2772.909376	230212.610005	56.111092
2772.374866	230027.279348	56.116097
2771.040439	229836.041258	56.121101
2770.882349	229633.694050	56.126106
2769.662116	229461.229631	56.131111
2769.179227	229266.242276	56.136116
2768.691907	229067.283999	56.141121
2767.671531	228880.632259	56.146125
2767.044756	228688.011446	56.151130
2766.719915	228511.358627	56.156135
2766.108714	228319.041693	56.161140
2765.521914	228129.369319	56.166145
2764.741755	227934.024604	56.171149
2764.454444	227731.956823	56.176154
2763.535322	227548.500028	56.181159
2762.698029	227350.466771	56.186164
2762.254923	227160.009921	56.191169
2761.660286	226969.042811	56.196173
2760.899805	226767.816083	56.201178
2760.196714	226580.864428	56.206183
2759.755792	226378.314953	56.211188
2758.885972	226183.714080	56.216193
2757.948165	225991.543217	56.221197
2757.845153	225786.892042	56.226202
2757.015790	225599.542473	56.231207
2755.888396	225402.310840	56.236212
2755.189992	225210.192980	56.241217
2754.665497	225024.285879	56.246221
2754.076107	224818.517497	56.251226
2753.480922	224634.735708	56.256231
2752.857261	224452.613775	56.261236
2752.300396	224254.161554	56.266241
2751.373453	224063.215591	56.271245
2750.713611	223861.750869	56.276250
2750.565891	223672.681039	56.281255
2749.548523	223479.204772	56.286260
2748.692750	223281.044184	56.291265
2747.969493	223097.107988	56.296269
2747.309081	222899.681214	56.301274
2746.411505	222710.821571	56.306279
2745.784015	222519.475457	56.311284
2745.685757	222333.430725	56.316289
2744.683765	222151.297631	56.321293
2743.863902	221960.390723	56.326298
2743.465969	221770.766811	56.331303
2742.668725	221580.175508	56.336308
2742.366389	221388.411528	56.341313
2741.487142	221201.385756	56.346317
2740.823067	221003.913489	56.351322
2740.103604	220820.593139	56.356327
2739.580855	220629.642498	56.361332
2738.943098	220430.028990	56.366337
2738.150272	220244.735851	56.371341
2737.657058	220048.652007	56.376346
2737.211293	219854.852468	56.381351
2736.100517	219656.627097	56.386356
2735.407387	219472.427555	56.391361
2734.577399	219279.365048	56.396365
2734.337653	219079.552104	56.401370
2733.464102	218890.278138	56.406375
2732.598370	218703.625657	56.411380
2732.323469	218518.114799	56.416385
2731.365599	218335.309363	56.421389
2731.092364	218135.338841	56.426394
2730.535479	217955.322186	56.431399
2729.368913	217758.129160	56.436404
2728.776600	217564.549872	56.441409
2728.273848	217381.101968	56.446413
2727.721905	217182.934869	56.451418
2727.075065	216999.077994	56.456423
2726.271145	216802.441169	56.461428
2726.007750	216613.356611	56.466433
2725.239855	216425.001654	56.471437
2724.524515	216216.107273	56.476442
2724.017465	216024.746260	56.481447
2723.364054	215833.281673	56.486452
2722.726351	215626.820691	56.491457
2721.903187	215434.251247	56.496461
2721.575820	215238.408911	56.501466
2720.767897	215034.700607	56.506471
2719.755194	214842.735641	56.511476
2719.396785	214629.830952	56.516481
2718.267079	214444.211733	56.521485
2717.998716	214248.235617	56.526490
2717.118184	214055.908281	56.531495
2716.571420	213858.157241	56.536500
2716.093328	213663.832562	56.541505
2715.130642	213477.222208	56.546509
2714.438682	213273.857259	56.551514
2713.804199	213076.427917	56.556519
2712.916434	212890.711053	56.561524
2712.774208	212690.926535	56.566529
2711.889603	212507.348587	56.571533
2711.279771	212310.299486	56.576538
2710.567661	212113.623569	56.581543
2709.891365	211913.595105	56.586548
2709.385525	211709.200016	56.591553
2708.613348	211509.913485	56.596557
2708.280224	211315.954645	56.601562
2707.567001	211121.623858	56.606567
2706.813758	210925.721752	56.611572
2706.319838	210722.142498	56.616577
2705.306952	210530.024710	56.621581
2704.865649	210325.916553	56.626586
2704.007233	210133.546399	56.631591
2703.288813	209927.650649	56.636596
2702.611468	209731.167475	56.641601
2701.742871	209536.026152	56.646605
2701.519356	209335.017688	56.651610
2700.731668	209149.894026	56.656615
2700.030001	208955.097176	56.661620
2699.606605	208750.914959	56.666625
2698.755200	208554.895810	56.671629
2698.127538	208353.560012	56.676634
2697.687857	208151.444186	56.681639
2696.809352	207961.947581	56.686644
2696.330026	207766.495644	56.691649
2695.316761	207563.149013	56.696653
2695.024816	207359.026981	56.701658
2693.839876	207158.177964	56.706663
2693.159991	206967.520297	56.711668
2692.824232	206778.895939	56.716673
2692.000754	206580.231538	56.721677
2691.049086	206386.666132	56.726682
2690.606585	206190.755312	56.731687
2689.930022	205998.865709	56.736692
2689.513008	205793.877955	56.741697
2688.413896	205610.736202	56.746701
2688.059482	205410.817822	56.751706
2687.446895	205220.040565	56.756711
2686.324212	205026.773972	56.761716
2685.959545	204831.720751	56.766721
2685.386199	204654.391086	56.771725
2684.887386	204447.079329	56.776730
2684.213146	204251.097165	56.781735
2683.509375	204052.740512	56.786740
2682.801539	203853.010744	56.791745
2681.427921	203659.890283	56.796749
2680.945654	203474.659519	56.801754
2680.622249	203283.091989	56.806759
2679.938362	203101.139562	56.811764
2679.783202	202895.929686	56.816769
2678.870879	202704.482862	56.821773
2678.113481	202509.525209	56.826778
2677.641130	202317.462774	56.831783
2676.819347	202122.058529	56.836788
2676.508724	201919.943788	56.841793
2675.620998	201730.850675	56.846797
2674.856645	201526.989446	56.851802
2674.354936	201327.286854	56.856807
2673.479234	201134.452492	56.861812
2672.980851	200933.490947	56.866817
2672.095185	200743.204665	56.871821
2671.660309	200547.808290	56.876826
2671.060259	200343.836318	56.881831
2670.299876	200149.714586	56.886836
2669.708139	199953.263520	56.891841
2668.625474	199770.621649	56.896845
2668.319861	199567.242205	56.901850
2667.870449	199361.226717	56.906855
2667.058025	199172.486805	56.911860
2666.514855	198970.954229	56.916865
2665.747740	198775.146040	56.921869
2664.974969	198572.836927	56.926874
2664.476732	198378.629129	56.931879
2663.731826	198170.552669	56.936884
2663.045698	197964.516431	56.941889
2662.659279	197777.431823	56.946893
2661.774856	197578.478116	56.951898
2661.275648	197381.996368	56.956903
2660.602590	197173.772474	56.961908
2660.334036	196983.389017	56.966913
2659.430367	196787.240797	56.971917
2658.719969	196570.906867	56.976922
2658.117106	196363.145891	56.981927
2657.473929	196166.844216	56.986932
2656.986749	195955.312807	56.991937
2655.892069	195765.306466	56.996941
2655.174670	195559.615499	57.001946
2654.893253	195346.030812	57.006951
2653.999022	195138.791732	57.011956
2653.158502	194937.499923	57.016961
2652.235105	194741.807956	57.021965
2651.549247	194544.272279	57.026970
2650.995288	194338.483990	57.031975
2650.218279	194147.784409	57.036980
2649.998454	193947.059833	57.041985
2649.050591	193750.790272	57.046989
2648.324883	193553.990047	57.051994
2647.537953	193360.762969	57.056999
2646.916989	193161.682848	57.062004
2646.617158	192964.104934	57.067009
2645.860992	192782.072111	57.072013
2645.124645	192573.787950	57.077018
2644.699324	192375.405225	57.082023
2643.874479	192184.389908	57.087028
2643.478256	191969.565400	57.092033
2642.235861	191784.356085	57.097037
2641.803994	191589.629188	57.102042
2641.487527	191383.993611	57.107047
2640.667443	191184.545869	57.112052
2639.952188	190981.418046	57.117057
2639.061521	190793.459439	57.122061
2638.648535	190590.247189	57.127066
2637.924166	190389.642468	57.132071
2637.402296	190194.388330	57.137076
2636.806340	189987.657888	57.142081
2635.838667	189800.847695	57.147085
2635.535702	189601.795299	57.152090
2635.031319	189391.999432	57.157095
2634.242217	189190.277655	57.162100
2633.367730	188982.272530	57.167105
2632.420038	188797.893136	57.172109
2632.130420	188579.262759	57.177114
2631.630476	188391.658802	57.182119
2630.646300	188183.445567	57.187124
2630.001994	187975.293903	57.192129
2629.146837	187788.295702	57.197133
2628.776492	187590.254791	57.202138
2628.280587	187390.275386	57.207143
2627.332225	187185.623150	57.212148
2626.790886	186985.410963	57.217153
2625.696017	186789.854582	57.222157
2625.250501	186590.799350	57.227162
2624.689885	186392.806417	57.232167
2623.889187	186198.719845	57.237172
2623.430928	185987.583402	57.242177
2622.483447	185801.129453	57.247181
2622.009292	185609.690658	57.252186
2621.782814	185398.443876	57.257191
2620.682222	185192.794171	57.262196
2619.897331	184985.479730	57.267201
2619.124102	184803.836461	57.272205
2618.656668	184603.495759	57.277210
2618.292093	184409.334985	57.282215
2617.348095	184214.529022	57.287220
2616.701630	184003.495236	57.292225
2616.305991	183814.964775	57.297229
2615.561105	183610.512609	57.302234
2615.036427	183405.873832	57.307239
2614.079330	183210.234722	57.312244
2613.677864	183007.944374	57.317249
2612.819325	182811.820725	57.322253
2612.031657	182607.545325	57.327258
2611.556947	182406.350610	57.332263
2610.811787	182209.270328	57.337268
2610.295045	181998.925156	57.342273
2609.382502	181813.080153	57.347277
2608.706066	181610.483612	57.352282
2608.006386	181414.226539	57.357287
2607.318634	181210.577840	57.362292
2606.897182	181012.866510	57.367297
2606.044396	180817.526824	57.372301
2605.455830	180619.970971	57.377306
2604.742178	180427.333152	57.382311
2603.887730	180233.281118	57.387316
2603.461270	180031.250194	57.392321
2602.579101	179838.400032	57.397325
2602.060442	179638.560705	57.402330
2601.658864	179436.515919	57.407335
2600.837866	179249.586236	57.412340
2600.321725	179045.946023	57.417345
2599.573720	178846.388429	57.422349
2598.720557	178646.683081	57.427354
2598.289313	178438.122506	57.432359
2597.517961	178254.496462	57.437364
2596.810923	178048.779836	57.442369
2596.284680	177856.709045	57.447373
2595.276827	177666.012838	57.452378
2594.500143	177464.125951	57.457383
2593.951524	177268.932429	57.462388
2593.340876	177073.546141	57.467393
2592.794219	176886.061984	57.472397
2592.429757	176693.767394	57.477402
2591.783545	176485.097983	57.482407
2591.046959	176294.072533	57.487412
2590.550465	176094.017599	57.492417
2590.061406	175885.211842	57.497421
2589.423758	175681.798047	57.502426
2588.754049	175479.878438	57.507431
2587.623414	175275.667185	57.512436
2587.341209	175061.109416	57.517441
2586.156562	174870.950149	57.522445
2585.889354	174675.113818	57.527450
2585.483575	174467.612109	57.532455
2584.584063	174269.868415	57.537460
2583.929133	174058.160338	57.542465
2583.409734	173855.194786	57.547469
2582.573925	173660.152977	57.552474
2581.842450	173455.200852	57.557479
2581.096907	173248.344290	57.562484
2580.601324	173041.334722	57.567489
2579.923589	172841.617045	57.572493
2579.335129	172645.383642	57.577498
2578.647135	172440.506135	57.582503
2578.045014	172242.381927	57.587508
2577.228405	172030.239637	57.592513
2576.505810	171825.701448	57.597517
2575.934560	171621.000439	57.602522
2575.094905	171421.201116	57.607527
2574.548992	171215.162863	57.612532
2574.194755	171013.762589	57.617537
2573.209181	170814.727084	57.622541
2572.345327	170610.192169	57.627546
2572.152175	170407.052661	57.632551
2570.976703	170206.371685	57.637556
2570.454320	170001.124561	57.642561
2569.768864	169803.788892	57.647565
2568.892158	169604.958508	57.652570
2568.317743	169413.278975	57.657575
2567.677368	169210.432793	57.662580
2567.240631	169000.993581	57.667585
2566.617835	168812.325850	57.672589
2565.724325	168605.097583	57.677594
2565.679584	168403.102292	57.682599
2564.834987	168210.912049	57.687604
2563.858821	168004.653870	57.692609
2563.223293	167802.666370	57.697613
2562.677873	167593.468267	57.702618
2562.095486	167396.344828	57.707623
2561.194768	167200.722502	57.712628
2561.023643	166990.616428	57.717633
2559.976217	166782.532366	57.722637
2559.429918	166587.874326	57.727642
2558.878084	166379.637654	57.732647
2557.955943	166171.320951	57.737652
2557.428187	165968.041899	57.742657
2556.605010	165766.718115	57.747661
2555.870775	165560.574841	57.752666
2555.238834	165371.429824	57.757671
2554.341441	165171.481579	57.762676
2553.928201	164969.842831	57.767681
2553.312752	164770.793000	57.772685
2552.399226	164569.579033	57.777690
2552.236363	164372.722927	57.782695
2550.978822	164179.334572	57.787700
2550.495924	163982.836434	57.792705
2549.691180	163798.227976	57.797709
2549.224377	163525.885120	57.802714
2548.655043	163326.047481	57.807719
2547.756397	163143.771302	57.812724
2547.663342	162920.872183	57.817729
2546.783160	162726.325535	57.822733
2545.892409	162527.089952	57.827738
2545.371701	162321.388740	57.832743
2544.602133	162136.261845	57.837748
2543.945537	161928.092392	57.842753
2543.081764	161728.183081	57.847757
2542.551719	161531.629384	57.852762
2542.080880	161332.613560	57.857767
2541.146550	161141.097287	57.862772
2540.612086	160938.076109	57.867777
2540.275504	160743.390453	57.872781
2539.380072	160543.797906	57.877786
2538.826568	160340.770432	57.882791
2538.280326	160142.434309	57.887796
2537.535211	159935.396577	57.892801
2536.802995	159742.711573	57.897805
2536.290375	159532.359263	57.902810
2535.540955	159329.355926	57.907815
2534.804713	159130.241941	57.912820
2534.323931	158928.774786	57.917825
2533.523156	158730.804771	57.922829
2532.856155	158516.541928	57.927834
2532.392544	158322.334707	57.932839
2531.258726	158113.144539	57.937844
2530.969073	157913.928552	57.942849
2530.174926	157718.505799	57.947853
2529.730971	157508.968381	57.952858
2529.126094	157302.279939	57.957863
2528.180228	157108.956829	57.962868
2527.853816	156893.912677	57.967873
2526.957357	156699.795854	57.972877
2526.390175	156492.496090	57.977882
2525.967885	156290.323077	57.982887
2525.310216	156090.235225	57.987892
2524.780727	155879.805990	57.992897
2523.816312	155668.836809	57.997901
2523.553378	155459.295893	58.002906
2522.936307	155251.058160	58.007911
2521.684514	155054.477331	58.012916
2520.913511	154838.525040	58.017921
2520.272736	154627.320348	58.022925
2519.506712	154420.153680	58.027930
2518.822020	154220.284497	58.032935
2518.089380	154037.851450	58.037940
2517.579775	153830.609628	58.042945
2516.952451	153640.471684	58.047949
2516.096733	153433.706643	58.052954
2515.872637	153215.555298	58.057959
2515.031059	153036.322742	58.062964
2514.345873	152829.089524	58.067969
2513.685044	152623.862052	58.072973
2512.749509	152419.480170	58.077978
2512.084399	152215.107525	58.082983
2511.797358	152026.462841	58.087988
2511.146483	151825.001086	58.092993
2510.484165	151619.551275	58.097997
2509.897445	151413.760290	58.103002
2509.204738	151209.817678	58.108007
2508.375029	151008.287576	58.113012
2507.556371	150808.218631	58.118017
2507.036304	150611.891191	58.123021
2506.372093	150412.486528	58.128026
2505.963806	150203.662573	58.133031
2504.982897	150007.272002	58.138036
2504.327310	149809.877816	58.143041
2503.673527	149604.108839	58.148045
2502.722703	149403.573781	58.153050
2502.469689	149193.536993	58.158055
2501.736856	149000.900638	58.163060
2501.302266	148802.473509	58.168065
2500.752752	148602.502569	58.173069
2499.589796	148397.800595	58.178074
2498.914799	148190.340947	58.183079
2498.182861	147995.130509	58.188084
2498.048955	147787.219136	58.193089
2497.115983	147594.216247	58.198093
2496.329552	147400.657524	58.203098
2496.010427	147180.401045	58.208103
2495.153760	146996.031638	58.213108
2494.363656	146783.592150	58.218113
2493.740034	146584.293718	58.223117
2493.225140	146387.139739	58.228122
2492.907943	146175.900206	58.233127
2492.000171	145964.857365	58.238132
2491.321109	145769.906375	58.243137
2490.561169	145558.232831	58.248141
2489.554285	145360.629516	58.253146
2489.472280	145143.742676	58.258151
2488.299164	144959.003263	58.263156
2487.911384	144744.950676	58.268161
2487.460823	144556.388435	58.273165
2486.502374	144341.272675	58.278170
2485.580989	144141.528635	58.283175
2484.957948	143933.275426	58.288180
2484.366449	143751.259326	58.293185
2483.825166	143557.151697	58.298189
2482.863888	143353.899133	58.303194
2482.393346	143145.461853	58.308199
2481.595261	142952.161159	58.313204
2481.117089	142765.329638	58.318209
2480.061758	142554.066456	58.323213
2479.526403	142359.164895	58.328218
2479.152206	142171.634335	58.333223
2478.275346	141961.604909	58.338228
2477.774701	141773.093012	58.343233
2477.210519	141580.488158	58.348237
2476.397952	141380.960792	58.353242
2476.112967	141177.462970	58.358247
2475.155650	140980.858212	58.363252
2474.499055	140776.494430	58.368257
2473.795750	140588.339653	58.373261
2473.064476	140382.351287	58.378266
2472.801779	140170.191220	58.383271
2471.954076	139986.942138	58.388276
2471.626772	139786.115891	58.393281
2471.059552	139585.621245	58.398285
2470.321335	139383.909901	58.403290
2469.829975	139171.983703	58.408295
2468.896207	138961.107450	58.413300
2468.315486	138756.631004	58.418305
2467.631951	138553.010800	58.423309
2466.686085	138351.085238	58.428314
2466.330141	138136.603899	58.433319
2465.356611	137940.860149	58.438324
2464.692223	137732.719569	58.443329
2464.177385	137525.674762	58.448333
2463.505812	137342.858660	58.453338
2462.918308	137125.499270	58.458343
2461.990878	136925.181283	58.463348
2461.132086	136730.011773	58.468353
2460.957768	136524.495358	58.473357
2460.300045	136320.098762	58.478362
2459.689906	136110.093516	58.483367
2458.933915	135912.855071	58.488372
2458.394208	135697.124796	58.493377
2457.793937	135497.272861	58.498381
2457.054560	135296.834567	58.503386
2456.473918	135081.051821	58.508391
2455.390681	134881.699901	58.513396
2454.980539	134679.790865	58.518401
2454.119681	134472.784388	58.523405
2453.065280	134274.931079	58.528410
2452.734708	134074.144252	58.533415
2451.971797	133878.686475	58.538420
2451.499995	133677.403970	58.543425
2450.952392	133468.055785	58.548429
2450.085868	133276.581859	58.553434
2449.811606	133073.277913	58.558439
2449.079464	132866.351504	58.563444
2448.624207	132661.974034	58.568449
2447.566535	132449.716332	58.573453
2447.065550	132251.293842	58.578458
2446.558393	132039.650555	58.583463
2445.940398	131839.166302	58.588468
2445.064594	131624.815453	58.593473
2444.462388	131411.083358	58.598477
2443.609654	131225.133736	58.603482
2443.301197	131014.724094	58.608487
2442.211055	130800.946949	58.613492
2441.701050	130602.435821	58.618497
2440.808872	130390.370543	58.623501
2440.289758	130196.893562	58.628506
2440.006635	129990.132900	58.633511
2439.192417	129789.148162	58.638516
2438.219923	129579.032358	58.643521
2437.435431	129370.653789	58.648525
2436.727922	129180.465199	58.653530
2436.174400	128963.276619	58.658535
2435.805470	128769.912716	58.663540
2434.958131	128577.146736	58.668545
2434.406302	128364.306240	58.673549
2433.504264	128170.408698	58.678554
2433.238484	127958.097500	58.683559
2432.241837	127762.084135	58.688564
2431.702265	127557.033267	58.693569
2430.804415	127354.314067	58.698573
2429.987553	127161.832535	58.703578
2429.762118	126955.504430	58.708583
2429.231920	126755.080872	58.713588
2428.499815	126551.452324	58.718593
2428.214164	126339.804458	58.723597
2427.062149	126134.099332	58.728602
2426.616032	125922.302345	58.733607
2425.369040	125731.359520	58.738612
2424.884722	125522.276690	58.743617
2424.387923	125318.315258	58.748621
2423.643580	125119.486982	58.753626
2422.722207	124917.399165	58.758631
2422.353718	124720.939753	58.763636
2421.752799	124523.020147	58.768641
2421.114373	124321.742751	58.773645
2420.341308	124128.221728	58.778650
2419.576101	123917.786272	58.783655
2418.963518	123727.531633	58.788660
2418.081263	123526.425831	58.793665
2417.463920	123317.063706	58.798669
2416.611743	123126.203706	58.803674
2416.010414	122928.956216	58.808679
2415.312208	122735.547660	58.813684
2415.055243	122536.305668	58.818689
2414.543300	122342.197442	58.823693
2413.537602	122145.108749	58.828698
2413.163957	121946.486468	58.833703
2412.504746	121745.434918	58.838708
2411.812724	121542.066453	58.843713
2411.325581	121341.130363	58.848717
2410.292207	121135.863744	58.853722
2409.868839	120932.977960	58.858727
2409.071608	120739.206054	58.863732
2408.337123	120530.620905	58.868737
2407.998391	120331.167230	58.873741
2407.109654	120138.137987	58.878746
2406.775423	119923.095006	58.883751
2405.952993	119729.296459	58.888756
2405.144060	119525.714534	58.893761
2404.882324	119314.315315	58.898765
2403.845858	119116.333694	58.903770
2403.462809	118916.974006	58.908775
2403.189669	118710.323536	58.913780
2402.728087	118495.801312	58.918785
2401.897751	118287.699984	58.923789
2400.878449	118085.070448	58.928794
2400.390334	117867.510635	58.933799
2399.623079	117660.400966	58.938804
2398.938123	117454.606591	58.943809
2398.569450	117243.526855	58.948813
2397.993068	117031.840670	58.953818
2397.349770	116808.081011	58.958823
2396.599487	116601.618280	58.963828
2395.524005	116382.634391	58.968833
2394.910660	116177.454603	58.973837
2394.256070	115972.714625	58.978842
2393.988648	115759.326953	58.983847
2393.312993	115547.021359	58.988852
2392.559173	115334.679152	58.993857
2391.949810	115122.868019	58.998861
2391.322009	114917.059609	59.003866
2390.397975	114701.246076	59.008871
2389.842929	114489.272947	59.013876
2389.475503	114280.121633	59.018881
2388.903761	114064.619451	59.023885
2387.631165	113849.173117	59.028890
2386.846386	113624.251664	59.033895
2386.348553	113416.511796	59.038900
2385.628692	113210.458993	59.043905
2385.017311	112996.755668	59.048909
2384.129505	112798.843890	59.053914
2383.508860	112580.385645	59.058919
2382.892224	112380.930048	59.063924
2382.439112	112170.648485	59.068929
2381.715332	111959.294651	59.073933
2381.054853	111749.189147	59.078938
2380.309392	111542.494151	59.083943
2379.879081	111331.530668	59.088948
2379.075251	111129.297069	59.093953
2378.332891	110929.206710	59.098957
2378.022200	110704.991602	59.103962
2377.383864	110488.953364	59.108967
2376.532021	110286.163139	59.113972
2375.866657	110067.841990	59.118977
2375.608235	109854.699915	59.123981
2374.414205	109642.038024	59.128986
2373.688230	109423.440307	59.133991
2373.161991	109216.850612	59.138996
2372.569276	109002.556926	59.144001
2372.122571	108785.151678	59.149005
2371.123263	108580.856973	59.154010
2370.412485	108363.084902	59.159015
2369.718043	108162.558982	59.164020
2368.880867	107950.800704	59.169025
2368.514961	107736.970779	59.174029
2367.830447	107548.999338	59.179034
2367.163895	107326.299302	59.184039
2366.853844	107111.831518	59.189044
2365.896064	106905.482172	59.194049
2365.563451	106691.364334	59.199053
2364.757005	106484.486993	59.204058
2364.250085	106256.219680	59.209063
2363.299884	106045.942661	59.214068
2362.738935	105833.118604	59.219073
2362.379597	105603.736444	59.224077
2361.194871	105399.130065	59.229082
2360.802089	105180.321151	59.234087
2360.077172	104964.028597	59.239092
2359.713448	104756.975425	59.244097
2358.856273	104542.427031	59.249101
2358.488445	104326.559474	59.254106
2357.803281	104105.833688	59.259111
2356.991859	103884.654156	59.264116
2356.329776	103674.092252	59.269121
2355.777316	103446.588632	59.274125
2354.620255	103233.387502	59.279130
2354.266257	103009.751894	59.284135
2353.673494	102795.703953	59.289140
2352.636931	102582.318319	59.294145
2352.391746	102362.395484	59.299149
2351.494250	102146.993435	59.304154
2351.245951	101923.021520	59.309159
2350.370358	101710.791879	59.314164
2349.753708	101494.748643	59.319169
2349.168271	101275.283273	59.324173
2348.264440	101060.748614	59.329178
2347.813487	100833.038551	59.334183
2347.338176	100617.799330	59.339188
2346.535745	100381.243311	59.344193
2345.977435	100167.074421	59.349197
2345.097283	99953.047351	59.354202
2344.547644	99723.873161	59.359207
2343.824381	99519.035473	59.364212
2343.144165	99296.603558	59.369217
2342.415430	99067.489655	59.374221
2341.727090	98845.475674	59.379226
2341.081828	98630.884471	59.384231
2340.643570	98420.962449	59.389236
2339.699713	98198.887409	59.394241
2339.169277	97972.619887	59.399245
2338.293859	97754.014086	59.404250
2337.837813	97534.722302	59.409255
2337.410009	97317.755835	59.414260
2336.741494	97099.592832	59.419265
2336.038918	96869.133150	59.424269
2335.112818	96652.797480	59.429274
2334.298194	96428.594510	59.434279
2333.743497	96209.058424	59.439284
2332.803219	95991.678509	59.444289
2332.495368	95761.541664	59.449293
2331.563736	95551.128179	59.454298
2330.957182	95332.496703	59.459303
2330.111093	95124.065000	59.464308
2329.331623	94913.696753	59.469313
2329.161190	94697.786328	59.474317
2328.517824	94481.071484	59.479322
2327.867649	94273.428335	59.484327
2327.220078	94053.699674	59.489332
2326.644358	93834.126654	59.494337
2326.045660	93606.144346	59.499341
2325.027640	93394.515514	59.504346
2324.773623	93164.301624	59.509351
2324.060892	92943.091334	59.514356
2323.283467	92745.983678	59.519361
2322.893096	92503.103189	59.524365
2321.923997	92278.794975	59.529370
2320.961334	92065.419887	59.534375
2320.655849	91847.427889	59.539380
2319.830301	91630.554078	59.544385
2319.295301	91401.347832	59.549389
2318.828294	91188.156243	59.554394
2318.032606	90963.649998	59.559399
2317.531957	90738.167183	59.564404
2316.539526	90519.840730	59.569409
2315.649169	90300.352634	59.574413
2315.028328	90080.963482	59.579418
2314.349263	89863.976078	59.584423
2314.000863	89653.411834	59.589428
2313.350781	89442.637514	59.594433
2312.779151	89210.727319	59.599437
2311.925857	89000.281152	59.604442
2311.130817	88782.390902	59.609447
2310.782222	88562.117939	59.614452
2310.283603	88344.267491	59.619457
2309.630354	88111.392940	59.624461
2308.722427	87898.569652	59.629466
2307.717976	87677.908846	59.634471
2307.107632	87457.726662	59.639476
2306.751785	87237.189381	59.644481
2306.227999	87013.029420	59.649485
2305.336229	86802.705814	59.654490
2304.822152	86580.133690	59.659495
2304.083204	86368.167214	59.664500
2303.348239	86137.019553	59.669505
2303.023134	85913.150183	59.674509
2302.105863	85695.779602	59.679514
2301.213485	85475.155337	59.684519
2300.606622	85263.540180	59.689524
2299.971827	85048.527536	59.694529
2299.841733	84818.591352	59.699533
2298.832788	84605.493476	59.704538
2298.342677	84383.618682	59.709543
2297.718432	84151.391054	59.714548
2297.003560	83920.562161	59.719553
2296.577368	83699.565454	59.724557
2295.849618	83476.362383	59.729562
2295.078662	83255.367953	59.734567
2294.381530	83031.511873	59.739572
2293.789895	82806.285047	59.744577
2293.261906	82579.206117	59.749581
2292.252602	82375.517677	59.754586
2291.775105	82153.372759	59.759591
2291.194595	81921.333878	59.764596
2290.148849	81711.509797	59.769601
2289.683874	81496.088087	59.774605
2289.261699	81273.443035	59.779610
2288.523001	81043.733269	59.784615
2287.806656	80817.115274	59.789620
2286.838812	80598.911616	59.794625
2286.529388	80370.795302	59.799629
2285.649882	80157.176987	59.804634
2285.180774	79926.131281	59.809639
2284.518467	79699.092302	59.814644
2283.605266	79471.417518	59.819649
2282.778288	79242.755637	59.824653
2281.931948	79031.539137	59.829658
2281.314538	78809.781636	59.834663
2280.719707	78585.760632	59.839668
2279.945066	78384.925724	59.844673
2279.460965	78159.732137	59.849677
2278.719818	77948.871263	59.854682
2278.083223	77726.152622	59.859687
2277.635316	77499.991014	59.864692
2276.731864	77286.444272	59.869697
2276.168267	77075.887390	59.874701
2275.539223	76849.894768	59.879706
2274.799913	76630.657720	59.884711
2274.587852	76401.632160	59.889716
2273.566321	76201.706911	59.894721
2272.994638	75972.743218	59.899725
2272.350101	75748.336656	59.904730
2271.568714	75527.762245	59.909735
2271.115651	75304.451705	59.914740
2270.376493	75092.549290	59.919745
2269.557195	74869.320651	59.924750
2269.115146	74648.125446	59.929754
2268.494606	74420.587263	59.934759
2267.755550	74207.933836	59.939764
2266.973402	73982.301585	59.944769
2266.623502	73755.513602	59.949774
2265.940289	73537.169143	59.954778
2264.905082	73313.003686	59.959783
2264.524536	73094.463993	59.964788
2263.852700	72877.689730	59.969793
2262.959704	72642.219886	59.974798
2262.416510	72434.058492	59.979802
2262.024285	72212.565481	59.984807
2261.139068	71986.623652	59.989812
2260.370578	71777.947375	59.994817
2259.959830	71543.833029	59.999822
2259.129648	71302.781779	60.004826
2258.126371	71065.403330	60.009831
2257.796729	70854.937793	60.014836
2257.026480	70630.804853	60.019841
2256.495747	70401.936321	60.024846
2255.464491	70190.708659	60.029850
2254.641633	69970.550533	60.034855
2254.217136	69762.943104	60.039860
2253.432805	69550.169267	60.044865
2253.192350	69326.068472	60.049870
2252.381183	69103.251553	60.054874
2251.725076	68890.945903	60.059879
2251.211929	68666.781881	60.064884
2250.230996	68454.519820	60.069889
2249.918399	68234.553580	60.074894
2248.975574	68023.423894	60.079898
2248.327325	67799.246917	60.084903
2247.797014	67584.212068	60.089908
2246.918256	67373.085600	60.094913
2246.637021	67150.073900	60.099918
2245.821066	66928.954569	60.104922
2244.871125	66706.123707	60.109927
2244.263902	66482.433566	60.114932
2243.724863	66272.519150	60.119937
2242.937611	66046.763183	60.124942
2242.278737	65839.994647	60.129946
2241.772108	65618.556239	60.134951
2240.991575	65407.058822	60.139956
2240.234006	65200.844751	60.144961
2239.572986	64976.696137	60.149966
2239.078587	64769.928829	60.154970
2238.448832	64547.879513	60.159975
2237.839006	64333.203741	60.164980
2237.103507	64112.993648	60.169985
2236.681604	63896.570554	60.174990
2235.714347	63682.573011	60.179994
2235.049115	63464.850971	60.184999
2234.626451	63244.588596	60.190004
2233.439197	63037.785279	60.195009
2233.217790	62811.214627	60.200014
2232.548300	62601.848628	60.205018
2232.039333	62379.023389	60.210023
2231.270079	62166.825537	60.215028
2230.466383	61946.724118	60.220033
2229.804924	61731.478013	60.225038
2229.096737	61521.933798	60.230042
2228.217550	61307.312725	60.235047
2227.981309	61081.331762	60.240052
2226.911220	60879.281949	60.245057
2226.240149	60656.097519	60.250062
2225.674304	60441.879778	60.255066
2224.879310	60228.064865	60.260071
2224.397645	60020.274118	60.265076
2223.765530	59810.705221	60.270081
2222.937205	59589.824880	60.275086
2222.215077	59395.215753	60.280090
2221.393109	59179.119004	60.285095
2221.108019	58961.458214	60.290100
2220.202973	58759.829211	60.295105
2219.720153	58548.816894	60.300110
2219.081413	58336.812499	60.305114
2218.478567	58123.010165	60.310119
2218.066456	57906.280757	60.315124
2217.095631	57699.197977	60.320129
2216.570252	57472.572144	60.325134
2215.668319	57272.544477	60.330138
2214.985282	57059.469754	60.335143
2214.277279	56841.039994	60.340148
2213.642626	56631.032547	60.345153
2213.127669	56419.941931	60.350158
2212.358402	56214.862993	60.355162
2211.681265	56007.904477	60.360167
2211.179316	55798.401325	60.365172
2210.463808	55579.490828	60.370177
2209.847647	55364.035701	60.375182
2208.961049	55164.645591	60.380186
2208.478486	54947.696254	60.385191
2208.021761	54734.166322	60.390196
2207.156870	54530.073912	60.395201
2206.464887	54321.253857	60.400206
2205.573516	54107.857152	60.405210
2205.003668	53897.383362	60.410215
2204.216985	53686.864125	60.415220
2203.566255	53485.040470	60.420225
2202.876032	53267.330792	60.425230
2202.269288	53070.849339	60.430234
2201.428802	52864.275074	60.435239
2201.013003	52653.250149	60.440244
2200.218470	52453.419436	60.445249
2199.538714	52248.048079	60.450254
2198.758220	52055.126922	60.455258
2198.020530	51841.169256	60.460263
2197.774797	51627.212015	60.465268
2196.645286	51434.912894	60.470273
2196.194282	51221.562555	60.475278
2195.895191	51024.624221	60.480282
2194.817840	50820.914164	60.485287
2194.222085	50609.109569	60.490292
2193.289797	50414.682924	60.495297
2192.782457	50204.106145	60.500302
2192.230226	50019.621135	60.505306
2191.244875	49818.005460	60.510311
2190.778803	49610.627657	60.515316
2189.808093	49422.519987	60.520321
2189.116333	49218.545525	60.525326
2188.495232	49027.045758	60.530330
2187.489025	48833.926126	60.535335
2187.706551	48633.395260	60.540340
2186.684479	48445.552806	60.545345
2186.171420	48247.448387	60.550350
2185.384955	48049.955807	60.555354
2184.289153	47861.843354	60.560359
2183.675820	47662.372644	60.565364
2183.041494	47479.072107	60.570369
2182.625800	47279.903335	60.575374
2181.829533	47093.548274	60.580378
2180.849663	46903.795373	60.585383
2180.331713	46715.024570	60.590388
2179.464591	46532.801983	60.595393
2178.636614	46339.459851	60.600398
2177.899514	46147.977973	60.605402
2177.402430	45963.282810	60.610407
2176.283187	45783.271516	60.615412
2175.451904	45613.122873	60.620417
2175.050392	45441.949317	60.625422
2174.212792	45277.004847	60.630426
2173.387507	45103.422091	60.635431
2172.665031	44931.760422	60.640436
2172.045778	44768.895732	60.645441
2170.970481	44601.218372	60.650446
2170.032108	44447.595274	60.655450
2169.081064	44289.405360	60.660455
2168.495699	44137.171204	60.665460
2167.634760	43994.520801	60.670465
2167.114834	43838.252758	60.675470
2166.203719	43696.561560	60.680474
2165.347971	43547.949245	60.685479
2164.613342	43408.544268	60.690484
2163.832176	43264.574721	60.695489
2163.095977	43130.064722	60.700494
2162.319183	42997.630494	60.705498
2161.372665	42866.463906	60.710503
2161.053724	42728.560712	60.715508
2159.999518	42608.538736	60.720513
2159.326215	42476.996530	60.725518
2158.797677	42353.230835	60.730522
2157.957029	42233.126984	60.735527
2157.467930	42099.041173	60.740532
2156.791134	41974.691378	60.745537
2156.128849	41854.011619	60.750542
2155.296835	41737.745728	60.755546
2154.559283	41619.131880	60.760551
2154.269255	41491.258361	60.765556
2153.358144	41373.483277	60.770561
2152.799225	41249.496316	60.775566
2152.111039	41134.938237	60.780570
2151.541674	41018.654503	60.785575
2150.974502	40884.663259	60.790580
2150.294992	40771.364755	60.795585
2149.371957	40651.057341	60.800590
2148.852563	40532.277246	60.805594
2148.216873	40428.925080	60.810599
2147.617377	40298.892937	60.815604
2147.145818	40181.467353	60.820609
2146.311623	40062.345214	60.825614
2145.744081	39949.598791	60.830618
2145.147907	39827.689615	60.835623
2144.551633	39706.562316	60.840628
2143.758030	39587.897101	60.845633
2143.319366	39470.075945	60.850638
2142.582633	39359.092970	60.855642
2141.881552	39233.510059	60.860647
2141.511504	39106.824247	60.865652
2140.651552	38991.129999	60.870657
2139.993364	38868.135636	60.875662
2139.574647	38735.128888	60.880666
2138.610017	38622.294576	60.885671
2137.928718	38499.927819	60.890676
2137.126983	38393.650240	60.895681
2136.803906	38268.385968	60.900686
2136.235452	38153.338828	60.905690
2135.214642	38033.711942	60.910695
2134.810388	37911.972561	60.915700
2134.145540	37799.119868	60.920705
2133.353296	37678.499689	60.925710
2132.508793	37559.504197	60.930714
2131.982183	37439.888451	60.935719
2131.169558	37317.018357	60.940724
2130.744639	37203.469237	60.945729
2130.103663	37088.883438	60.950734
2129.137713	36975.661966	60.955738
2128.549923	36867.450532	60.960743
2128.301809	36738.735025	60.965748
2127.408475	36630.602045	60.970753
2126.770820	36504.758988	60.975758
2126.047319	36385.140858	60.980762
2125.276506	36274.039657	60.985767
2124.809721	36155.153778	60.990772
2124.159732	36042.389502	60.995777
2123.763262	35927.058366	61.000782
2122.834665	35819.239673	61.005786
2122.321208	35702.281664	61.010791
2121.737782	35575.000207	61.015796
2120.826288	35463.183822	61.020801
2120.042935	35341.736521	61.025806
2119.698247	35221.775744	61.030810
2118.589974	35109.160002	61.035815
2117.604828	34986.381723	61.040820
2117.173083	34888.882076	61.045825
2116.862655	34778.945777	61.050830
2116.112382	34660.580138	61.055834
2115.266943	34551.316591	61.060839
2114.707496	34436.543130	61.065844
2113.901568	34325.594757	61.070849
2113.137655	34219.792702	61.075854
2112.759801	34108.212049	61.080858
2111.530393	34004.734182	61.085863
2111.029731	33879.723563	61.090868
2110.594294	33787.229779	61.095873
2110.128086	33681.946523	61.100878
2109.314016	33573.373461	61.105882
2108.586818	33468.901034	61.110887
2108.102347	33350.023672	61.115892
2107.430352	33240.096416	61.120897
2106.841719	33141.457682	61.125902
2106.401316	33024.617456	61.130906
2105.716932	32909.085766	61.135911
2104.810356	32801.254638	61.140916
2103.921150	32698.386757	61.145921
2103.332993	32587.170482	61.150926
2103.031057	32476.310925	61.155930
2101.861285	32377.053091	61.160935
2101.667744	32258.935417	61.165940
2100.520495	32154.964595	61.170945
2099.838315	32039.271118	61.175950
2099.120654	31934.193720	61.180954
2098.525723	31832.653004	61.185959
2097.779773	31732.925672	61.190964
2097.014939	31633.051821	61.195969
2096.588032	31528.338560	61.200974
2096.015377	31434.338999	61.205978
2095.127728	31336.711326	61.210983
2094.694602	31229.550106	61.215988
2093.804428	31123.882666	61.220993
2093.043637	31019.796054	61.225998
2092.530039	30923.263397	61.231002
2091.704616	30827.068372	61.236007
2091.254139	30731.209439	61.241012
2090.049689	30628.380795	61.246017
2089.408185	30528.061132	61.251022
2088.795966	30442.782987	61.256026
2087.914959	30357.682247	61.261031
2087.588698	30246.849439	61.266036
2087.064893	30167.694087	61.271041
2086.470936	30059.766509	61.276046
2085.785786	29968.079517	61.281050
2085.206048	29878.635752	61.286055
2084.430848	29778.954942	61.291060
2083.463079	29679.663962	61.296065
2083.155319	29580.213545	61.301070
2082.421546	29484.689677	61.306074
2081.635573	29396.979767	61.311079
2080.988568	29301.312063	61.316084
2080.228328	29211.519820	61.321089
2079.233301	29119.186842	61.326094
2078.899147	29022.229281	61.331098
2078.082417	28938.636158	61.336103
2077.822398	28841.906474	61.341108
2076.973678	28756.774190	61.346113
2076.242055	28666.801875	61.351118
2075.793375	28571.435602	61.356122
2074.836848	28483.348480	61.361127
2074.524591	28383.245674	61.366132
2073.573381	28295.245621	61.371137
2072.885999	28210.799956	61.376142
2072.384492	28123.590494	61.381146
2071.782839	28029.310181	61.386151
2071.039861	27942.207948	61.391156
2070.083498	27848.300948	61.396161
2069.908033	27759.788889	61.401166
2069.122818	27666.048521	61.406170
2067.937142	27579.484538	61.411175
2067.482776	27485.278801	61.416180
2066.814313	27415.360520	61.421185
2066.311164	27322.548947	61.426190
2065.739827	27229.897227	61.431194
2064.448086	27147.783651	61.436199
2064.401206	27061.400318	61.441204
2063.658482	26988.361431	61.446209
2062.564051	26893.039574	61.451214
2062.392860	26811.825675	61.456218
2061.353456	26726.926250	61.461223
2060.746975	26643.169418	61.466228
2060.165466	26569.094245	61.471233
2059.661967	26483.107939	61.476238
2058.834068	26397.871008	61.481242
2057.985515	26310.803003	61.486247
2057.429797	26215.800103	61.491252
2056.908914	26143.668160	61.496257
2056.073567	26060.990885	61.501262
2056.057969	25973.484475	61.506266
2055.193634	25887.226098	61.511271
2054.333001	25797.242821	61.516276
2053.408917	25724.011770	61.521281
2052.961563	25634.270263	61.526286
2052.456279	25546.032759	61.531290
2051.462627	25471.326701	61.536295
2050.900298	25377.009030	61.541300
2050.165090	25308.956232	61.546305
2049.413502	25226.967341	61.551310
2048.914840	25139.347055	61.556314
2048.369011	25065.682251	61.561319
2047.776354	24971.077189	61.566324
2047.046244	24900.327443	61.571329
2046.000404	24815.991975	61.576334
2045.588410	24737.728362	61.581338
2044.731963	24670.258251	61.586343
2044.304253	24578.307410	61.591348
2043.884475	24502.470735	61.596353
2042.996414	24420.405754	61.601358
2042.634567	24334.939172	61.606362
2041.887220	24246.594028	61.611367
2041.287112	24168.953777	61.616372
2040.616965	24083.670145	61.621377
2040.106336	23998.608045	61.626382
2039.291801	23909.570991	61.631386
2038.365429	23840.596056	61.636391
2037.929588	23752.248432	61.641396
2037.114646	23666.975003	61.646401
2036.274171	23583.516092	61.651406
2035.740374	23509.206620	61.656410
2035.004115	23424.127327	61.661415
2034.059768	23338.678769	61.666420
2033.579825	23262.795935	61.671425
2032.713695	23181.990247	61.676430
2032.559121	23108.178399	61.681434
2031.441724	23031.807156	61.686439
2031.121362	22944.794454	61.691444
2030.182914	22882.330152	61.696449
2029.531338	22812.126027	61.701454
2029.300272	22734.836134	61.706458
2028.386891	22656.286429	61.711463
2027.681082	22572.013107	61.716468
2027.013965	22504.124138	61.721473
2026.172221	22420.189059	61.726478
2025.769075	22337.998628	61.731482
2024.739965	22262.328550	61.736487
2024.133704	22191.636719	61.741492
2023.530441	22118.905890	61.746497
2023.105861	22046.078337	61.751502
2022.724526	21963.982718	61.756506
2021.936782	21892.025251	61.761511
2021.016992	21807.016130	61.766516
2020.552667	21741.921920	61.771521
2019.889269	21661.582156	61.776526
2019.360446	21569.843986	61.781530
2018.241512	21504.099790	61.786535
2018.105616	21422.020930	61.791540
2017.017788	21346.036086	61.796545
2016.319453	21262.409703	61.801550
2015.718049	21186.294731	61.806554
2014.916832	21112.941434	61.811559
2014.433966	21037.226056	61.816564
2013.749458	20965.169575	61.821569
2013.076933	20893.712386	61.826574
2012.406719	20811.260397	61.831578
2011.503878	20753.171498	61.836583
2010.981483	20669.873269	61.841588
2010.600422	20599.920273	61.846593
2009.780848	20521.307868	61.851598
2009.385194	20445.347784	61.856602
2008.410567	20376.068737	61.861607
2008.128479	20296.157032	61.866612
2007.163567	20229.046758	61.871617
2006.431998	20149.612965	61.876622
2005.906359	20072.512326	61.881626
2005.208682	20001.106215	61.886631
2004.533612	19919.200106	61.891636
2003.727156	19848.267118	61.896641
2002.796527	19769.880588	61.901646
2002.544717	19698.483246	61.906650
2001.859660	19639.228977	61.911655
2001.295317	19557.059277	61.916660
2000.524031	19483.486985	61.921665
1999.592669	19415.620104	61.926670
1999.223604	19341.295404	61.931674
1998.222430	19279.858794	61.936679
1997.662425	19204.889638	61.941684
1996.985200	19137.557978	61.946689
1996.378498	19067.111962	61.951694
1996.137382	18990.780305	61.956698
1995.250094	18925.545808	61.961703
1994.757223	18846.359419	61.966708
1994.052670	18762.344312	61.971713
1993.144499	18691.904023	61.976718
1992.763785	18615.888061	61.981722
1992.093725	18550.237370	61.986727
1991.390548	18471.033372	61.991732
1990.415948	18408.792313	61.996737
1989.677945	18331.129242	62.001742
1989.247777	18254.451862	62.006746
1988.585576	18185.670142	62.011751
1988.141521	18113.168627	62.016756
1987.422878	18036.184839	62.021761
1986.832927	17965.421811	62.026766
1986.041329	17887.141867	62.031770
1985.255071	17823.896737	62.036775
1984.683089	17741.545182	62.041780
1984.370374	17670.637258	62.046785
1983.698166	17598.310529	62.051790
1982.875909	17531.522732	62.056794
1981.754961	17455.558094	62.061799
1981.303235	17380.970086	62.066804
1980.461163	17302.365606	62.071809
1979.889276	17238.645981	62.076814
1979.361212	17162.268175	62.081818
1978.488027	17097.708108	62.086823
1978.080989	17024.783076	62.091828
1977.021838	16959.590816	62.096833
1976.410700	16895.387051	62.101838
1975.995052	16823.646811	62.106842
1975.087113	16756.172036	62.111847
1974.517530	16678.378400	62.116852
1974.099403	16621.649982	62.121857
1973.064622	16554.570573	62.126862
1972.955613	16480.582722	62.131866
1972.240102	16413.356353	62.136871
1971.476051	16338.459442	62.141876
1970.719752	16266.193323	62.146881
1969.870701	16198.267039	62.151886
1969.404223	16121.106699	62.156890
1969.005078	16056.886772	62.161895
1968.196718	15979.180336	62.166900
1967.618134	15912.572777	62.171905
1966.685109	15840.712616	62.176910
1966.104616	15765.762902	62.181914
1965.356450	15702.464547	62.186919
1964.789890	15633.278592	62.191924
1964.168285	15571.902576	62.196929
1963.388009	15496.047601	62.201934
1962.878481	15421.677902	62.206938
1961.893662	15360.874611	62.211943
1961.487988	15285.966568	62.216948
1960.724342	15216.802127	62.221953
1959.694114	15149.857650	62.226958
1959.056222	15086.333189	62.231962
1958.356664	15013.794591	62.236967
1958.013264	14953.249916	62.241972
1957.236885	14889.040178	62.246977
1956.712543	14821.535864	62.251982
1956.421918	14751.629028	62.256986
1955.387328	14691.971049	62.261991
1954.971026	14625.078007	62.266996
1954.543215	14553.761151	62.272001
1953.568468	14493.410558	62.277006
1953.092528	14412.564023	62.282010
1952.623523	14344.327310	62.287015
1951.744779	14267.848033	62.292020
1951.139116	14191.160639	62.297025
1950.246945	14125.046750	62.302030
1950.015986	14048.467113	62.307034
1949.058664	13985.504600	62.312039
1948.553655	13909.999417	62.317044
1947.680921	13843.196644	62.322049
1946.943134	13770.581994	62.327054
1946.444419	13685.552487	62.332058
1945.694019	13623.314973	62.337063
1945.273535	13554.062513	62.342068
1944.255530	13493.771166	62.347073
1943.606510	13424.112539	62.352078
1943.463580	13344.730276	62.357082
1942.461332	13279.325002	62.362087
1941.841472	13202.977750	62.367092
1941.087629	13121.634749	62.372097
1940.357408	13065.098000	62.377102
1940.070964	12987.668428	62.382106
1939.144497	12924.289104	62.387111
1938.439452	12843.989528	62.392116
1937.551846	12779.212454	62.397121
1936.784960	12706.427259	62.402126
1936.435319	12636.694216	62.407130
1935.420531	12579.128066	62.412135
1934.992556	12513.160239	62.417140
1934.396513	12438.883654	62.422145
1933.628156	12378.973658	62.427150
1933.173706	12309.407702	62.432154
1932.192177	12240.836991	62.437159
1931.969349	12170.107623	62.442164
1931.091020	12107.580660	62.447169
1930.275145	12031.007520	62.452174
1929.934410	11957.177869	62.457178
1929.048841	11896.897372	62.462183
1928.184530	11823.778837	62.467188
1927.591290	11755.296634	62.472193
1926.613733	11692.638584	62.477198
1926.250478	11629.836711	62.482202
1925.302597	11577.815461	62.487207
1925.052156	11505.851131	62.492212
1924.319524	11439.364629	62.497217
1923.665502	11386.184175	62.502222
1923.266466	11313.904642	62.507226
1922.279574	11247.951538	62.512231
1921.879929	11176.601308	62.517236
1921.271661	11114.696615	62.522241
1920.457440	11048.828226	62.527246
1919.907318	10973.153089	62.532250
1919.326389	10907.936342	62.537255
1918.617211	10830.945364	62.542260
1917.688383	10758.258049	62.547265
1917.064427	10702.041896	62.552270
1916.750426	10635.851678	62.557274
1915.930464	10579.973249	62.562279
1915.091393	10507.465813	62.567284
1914.507491	10443.041375	62.572289
1913.872599	10379.685773	62.577294
1912.861060	10303.098977	62.582298
1912.300519	10250.129987	62.587303
1912.154356	10168.845299	62.592308
1911.392105	10112.375167	62.597313
1910.547010	10041.545232	62.602318
1910.389514	9966.193897	62.607322
1909.319580	9898.189500	62.612327
1908.513615	9821.799352	62.617332
1908.175469	9765.999329	62.622337
1907.240731	9691.140443	62.627342
1906.832346	9618.744455	62.632346
1905.847508	9549.869299	62.637351
1905.154235	9483.863485	62.642356
1904.377053	9417.606972	62.647361
1903.531454	9355.104548	62.652366
1903.611446	9280.878342	62.657370
1902.448330	9219.885714	62.662375
1901.967248	9158.997283	62.667380
1901.316858	9090.493628	62.672385
1900.607040	9021.494389	62.677390
1900.209251	8954.308666	62.682394
1899.176984	8895.551436	62.687399
1898.957271	8820.203481	62.692404
1897.998125	8752.455321	62.697409
1897.065307	8696.030609	62.702414
1897.019072	8619.480190	62.707418
1896.029110	8559.731381	62.712423
1895.427109	8482.898306	62.717428
1894.915165	8416.984366	62.722433
1893.974726	8358.402431	62.727438
1893.163785	8282.205119	62.732442
1892.449686	8222.882083	62.737447
1892.035403	8159.498049	62.742452
1891.293661	8085.870913	62.747457
1890.659376	8027.391165	62.752462
1890.491318	7953.103607	62.757466
1889.123728	7893.642256	62.762471
1888.452921	7828.700450	62.767476
1888.042520	7758.830350	62.772481
1887.146919	7699.822606	62.777486
1886.721011	7634.098044	62.782490
1886.083156	7579.813973	62.787495
1885.293032	7508.366022	62.792500
1884.689967	7449.457187	62.797505
1883.578183	7387.738902	62.802510
1883.539805	7317.406313	62.807514
1883.017604	7262.736628	62.812519
1882.268919	7195.338404	62.817524
1881.363408	7124.556695	62.822529
1880.504944	7054.303491	62.827534
1880.051561	6995.903586	62.832538
1879.380832	6937.160557	62.837543
1878.737867	6864.450273	62.842548
1878.224273	6803.636540	62.847553
1877.025351	6749.786150	62.852558
1876.428352	6682.369318	62.857562
1875.736222	6622.989599	62.862567
1875.255726	6567.612199	62.867572
1874.863305	6506.154895	62.872577
1873.965353	6455.215121	62.877582
1873.598463	6385.671908	62.882586
1872.818434	6321.520752	62.887591
1872.162103	6254.753437	62.892596
1871.568214	6179.539334	62.897601
1871.194128	6131.523668	62.902606
1870.196732	6050.869160	62.907610
1869.713531	5989.632706	62.912615
1868.770179	5923.878740	62.917620
1868.340939	5856.432707	62.922625
1867.746724	5802.964597	62.927630
1866.852168	5726.353091	62.932634
1866.379712	5675.075514	62.937639
1865.478250	5606.445115	62.942644
1864.839591	5538.554987	62.947649
1864.056103	5487.840153	62.952654
1863.580905	5417.635589	62.957658
1862.835263	5357.035789	62.962663
1861.957756	5285.856916	62.967668
1861.597772	5223.384627	62.972673
1860.814653	5167.146327	62.977678
1860.114057	5105.115115	62.982682
1859.230396	5042.040523	62.987687
1858.639628	4987.782901	62.992692
1858.402343	4914.211257	62.997697
1857.444963	4860.472156	63.002702
1857.008035	4797.867174	63.007706
1856.544039	4740.070964	63.012711
1855.738400	4676.174723	63.017716
1854.905629	4607.827519	63.022721
1854.224408	4551.445244	63.027726
1853.633416	4482.581470	63.032730
1852.665105	4433.596943	63.037735
1851.925225	4363.113671	63.042740
1851.568433	4292.729226	63.047745
1850.965344	4240.963913	63.052750
1850.415894	4186.584369	63.057754
1849.353131	4124.066635	63.062759
1848.898980	4068.249570	63.067764
1848.499672	4010.486959	63.072769
1847.596183	3951.358163	63.077774
1846.883323	3884.298202	63.082778
1846.322366	3818.665616	63.087783
1845.481999	3763.791998	63.092788
1845.213586	3703.094033	63.097793
1844.082243	3638.435360	63.102798
1843.689635	3582.405307	63.107802
1843.083261	3522.565413	63.112807
1842.205811	3457.121137	63.117812
1841.736760	3393.334751	63.122817
1840.934643	3341.095520	63.127822
1840.434186	3279.336751	63.132826
1839.469498	3218.767910	63.137831
1838.343185	3171.530381	63.142836
1837.929897	3111.905983	63.147841
1837.496444	3060.992504	63.152846
1836.697908	3004.615073	63.157850
1836.367402	2937.538939	63.162855
1835.610320	2886.395123	63.167860
1835.064523	2830.949830	63.172865
1834.106403	2779.837521	63.177870
1833.144632	2715.543213	63.182874
1832.657673	2665.834379	63.187879
1831.840467	2614.696328	63.192884
1831.626391	2557.847689	63.197889
1830.860403	2512.749807	63.202894
1830.356352	2447.759405	63.207898
1829.435124	2388.235170	63.212903
1828.828363	2332.205256	63.217908
1828.205538	2269.312494	63.222913
1827.496185	2220.817088	63.227918
1827.078141	2166.583459	63.232922
1826.391545	2104.837118	63.237927
1825.546512	2050.984796	63.242932
1824.933749	2000.331383	63.247937
1824.296817	1945.112897	63.252942
1823.595335	1880.978863	63.257946
1822.918082	1837.558915	63.262951
1822.390021	1780.286852	63.267956
1821.615281	1716.077644	63.272961
1820.794638	1669.003835	63.277966
1820.101846	1612.328730	63.282970
1819.557684	1557.626110	63.287975
1818.551846	1507.839590	63.292980
1818.026133	1453.900915	63.297985
1816.842240	1403.067431	63.302990
1816.613112	1355.961420	63.307994
1815.857634	1313.792703	63.312999
1814.935815	1265.303463	63.318004
1814.730716	1203.635876	63.323009
1813.963286	1165.241909	63.328014
1813.280998	1113.922890	63.333018
1812.827214	1060.866091	63.338023
1812.302511	1009.178612	63.343028
1811.695572	960.404612	63.348033
1810.934015	911.264216	63.353038
1810.290792	866.304911	63.358042
1809.504163	813.980007	63.363047
1808.683087	756.443879	63.368052
1808.106407	704.281584	63.373057
1807.135736	669.985248	63.378062
1806.563283	622.662514	63.383066
1805.561186	581.083899	63.388071
1804.835608	536.141850	63.393076
1804.430856	494.329843	63.398081
1803.679469	452.309643	63.403086
1802.991035	404.767909	63.408090
1802.126369	369.034565	63.413095
1801.633509	325.947043	63.418100
1801.328008	277.913602	63.423105
1800.303231	244.550989	63.428110
1799.530783	200.781246	63.433114
1799.244277	171.397002	63.438119
1798.209656	136.749382	63.443124
1797.742419	90.430407	63.448129
1796.398241	64.332036	63.453134
1795.434231	26.934261	63.458138
1794.954441	5.888535	63.463143
1793.939884	-6.072481	63.468148
1790.505653	36.701028	63.473153
1788.325314	74.658143	63.478158
1788.892898	68.373656	63.483162
1789.480182	70.305239	63.488167
1789.347799	74.481609	63.493172
1788.900493	59.781134	63.498177
1788.841029	67.033638	63.503182
1788.335468	61.359561	63.508186
1787.616010	65.310615	63.513191
1785.813698	74.005297	63.518196
1785.351722	72.813945	63.523201
1784.375899	75.266589	63.528206
1784.045415	80.745466	63.533210
1783.668413	73.726307	63.538215
1782.958674	74.840419	63.543220
1782.633871	72.963376	63.548225
1781.437465	78.988211	63.553230
1781.475417	84.015908	63.558234
1781.092424	77.973848	63.563239
1779.793602	85.088872	63.568244
1779.305990	80.966838	63.573249
1778.113585	79.724333	63.578254
1777.441875	80.658940	63.583258
1776.719384	73.689921	63.588263
1776.533584	90.190967	63.593268
1776.351507	70.482459	63.598273
1775.671769	82.968115	63.603278
1774.705197	78.367055	63.608282
1774.043786	76.822597	63.613287
1772.910492	90.269707	63.618292
1772.545276	77.913762	63.623297
1771.509289	78.075158	63.628302
1771.345985	81.089479	63.633306
1771.211388	78.040497	63.638311
1770.674612	81.077863	63.643316
1769.463175	67.604206	63.648321
1768.776184	74.909068	63.653326
1768.285507	72.992138	63.658330
1767.378552	74.834600	63.663335
1766.558471	74.816625	63.668340
1766.104325	69.340969	63.673345
1765.254059	72.024416	63.678350
1764.520456	76.370393	63.683354
1763.839985	62.602677	63.688359
1763.168481	68.939969	63.693364
1763.338586	68.364180	63.698369
1763.058074	71.188954	63.703374
1761.287350	71.788750	63.708378
1760.691139	71.361478	63.713383
1760.089230	67.718083	63.718388
1759.908726	71.235035	63.723393
1759.304136	67.916922	63.728398
1758.643120	72.743386	63.733402
1757.587990	73.989633	63.738407
1756.908517	80.593129	63.743412
1756.580998	68.574991	63.748417
1756.025769	78.443592	63.753422
1754.597761	71.417901	63.758426
1753.971271	75.116076	63.763431
1753.448698	74.820616	63.768436
1752.787174	73.594731	63.773441
1752.442830	73.983755	63.778446
1751.852024	74.154878	63.783450
1751.189317	66.624435	63.788455
1750.146005	76.870183	63.793460
1749.620279	64.530288	63.798465
1748.768249	73.777390	63.803470
1747.952542	78.521193	63.808474
1748.122161	63.683317	63.813479
1747.415247	75.753811	63.818484
1746.747810	71.054791	63.823489
1745.808935	77.177509	63.828494
1744.650989	75.292448	63.833498
1744.946083	63.698983	63.838503
1743.876788	77.203735	63.843508
1743.274545	62.945778	63.848513
1742.523193	74.394117	63.853518
1741.792619	76.197534	63.858522
1741.013970	75.375037	63.863527
1740.301586	70.836124	63.868532
1740.481795	72.375029	63.873537
1739.284214	75.096303	63.878542
1738.386036	73.895395	63.883546
1738.033115	69.867099	63.888551
1736.910023	82.005280	63.893556
1736.956297	74.404807	63.898561
1736.541718	80.225054	63.903566
1735.363078	77.375021	63.908570
1734.844821	72.513535	63.913575
1734.001818	77.569187	63.918580
1733.500895	72.023695	63.923585
1732.756433	81.840355	63.928590
1731.979236	77.646056	63.933594
1731.652886	77.664790	63.938599
1730.700420	80.206785	63.943604
1730.378089	74.763815	63.948609
1730.171001	80.571607	63.953614
1728.515286	74.052037	63.958618
1727.569521	77.698428	63.963623
1727.298739	77.112240	63.968628
1727.116134	72.648457	63.973633
1726.230751	76.499725	63.978638
1724.931567	83.040810	63.983642
1725.044587	77.210141	63.988647
1724.052066	86.247756	63.993652
1723.364844	76.142856	63.998657
1722.848423	82.909697	64.003662
1722.087977	80.232945	64.008666
1721.258112	76.721962	64.013671
1720.670391	84.886291	64.018676
1720.927201	76.344038	64.023681
1719.705498	81.560774	64.028686
1719.042131	82.740079	64.033690
1718.475420	79.665120	64.038695
1717.811032	78.658898	64.043700
1717.330093	75.347963	64.048705
1716.661303	77.901674	64.053710
1715.086752	80.227092	64.058714
1714.802251	82.377559	64.063719
1714.201839	79.252760	64.068724
1713.761045	80.615912	64.073729
1712.718552	81.923249	64.078734
1711.826931	81.017779	64.083738
1712.005329	76.514000	64.088743
1711.036159	80.864292	64.093748
1710.059499	72.253038	64.098753
1709.601169	74.013218	64.103758
1708.771066	72.844086	64.108762
1708.595725	69.882009	64.113767
1707.871343	79.402165	64.118772
1707.588549	68.386199	64.123777
1706.883681	73.913508	64.128782
1706.326625	76.238159	64.133786
1705.044235	67.584009	64.138791
1704.041858	76.173752	64.143796
1703.549742	73.656237	64.148801
1702.989812	72.248646	64.153806
1702.067148	76.690901	64.158810
1701.613321	70.418836	64.163815
1701.176282	79.869695	64.168820
1700.655525	64.018682	64.173825
1700.067379	66.717282	64.178830
1699.318934	69.736240	64.183834
1699.329451	69.529578	64.188839
1697.636024	71.430758	64.193844
1696.894928	68.944910	64.198849
1696.207482	68.107940	64.203854
1695.848491	71.564936	64.208858
1695.432185	67.709146	64.213863
1694.555071	71.798810	64.218868
1694.149932	66.618165	64.223873
1693.348751	68.527427	64.228878
1692.838491	69.862191	64.233882
1692.416752	68.640811	64.238887
1691.450095	73.124751	64.243892
1690.213189	62.474824	64.248897
1689.394662	66.381713	64.253902
1688.818973	70.852433	64.258906
1688.978164	63.609352	64.263911
1688.110047	67.219764	64.268916
1687.391921	58.064406	64.273921
1686.860568	69.567691	64.278926
1686.010904	71.424732	64.283930
1685.883461	67.012118	64.288935
1684.643248	75.161824	64.293940
1683.560740	73.823057	64.298945
1683.112012	69.267512	64.303950
1682.912497	65.572832	64.308954
1682.189292	56.670600	64.313959
1680.832364	70.254169	64.318964
1680.668890	64.328655	64.323969
1680.009754	69.968553	64.328974
1679.351087	69.917080	64.333978
1679.240006	62.543466	64.338983
1678.651620	68.856532	64.343988
1677.940072	59.157653	64.348993
1676.700459	72.113878	64.353998
1675.736402	64.713336	64.359002
1675.110454	62.499368	64.364007
1674.307471	71.662999	64.369012
1674.122586	65.147944	64.374017
1673.798170	66.177218	64.379022
1673.557381	70.175264	64.384026
1672.714757	69.590036	64.389031
1671.237487	71.758096	64.394036
1670.746769	70.410482	64.399041
1669.966315	67.296951	64.404046
1669.468682	68.328511	64.409050
1669.155150	60.988638	64.414055
1668.624207	73.218846	64.419060
1667.741180	67.811344	64.424065
1666.696749	68.198054	64.429070
1665.569913	79.368586	64.434074
1665.278300	66.259811	64.439079
1664.637487	70.428640	64.444084
1664.042335	66.511381	64.449089
1663.694697	70.343472	64.454094
1663.178521	77.061394	64.459098
1662.868107	71.252263	64.464103
1662.113182	76.278172	64.469108
1661.363093	72.111132	64.474113
1660.353954	66.472930	64.479118
1659.141943	73.369202	64.484122
1659.165426	65.980520	64.489127
1658.483075	76.399187	64.494132
1658.136256	67.167502	64.499137
1656.827592	67.809083	64.504142
1655.664590	68.440140	64.509146
1655.617608	69.325993	64.514151
1654.921622	73.000534	64.519156
1654.316374	67.611988	64.524161
1653.812257	67.953867	64.529166
1653.063144	67.361675	64.534170
1652.743546	60.540016	64.539175
1652.440696	62.004264	64.544180
1651.226115	61.052352	64.549185
1650.506900	62.554361	64.554190
1649.726385	69.675402	64.559194
1649.372047	62.517058	64.564199
1648.585038	65.772393	64.569204
1647.963912	62.042195	64.574209
1646.688392	65.589607	64.579214
1645.854487	75.720113	64.584218
1645.325527	68.868633	64.589223
1644.783422	70.717827	64.594228
1644.627450	72.188705	64.599233
1644.353204	65.867626	64.604238
1643.783439	70.985548	64.609242
1643.267651	68.498616	64.614247
1642.007232	68.550637	64.619252
1641.122433	69.195851	64.624257
1640.578523	66.323875	64.629262
1639.744432	76.165826	64.634266
1639.361115	63.713458	64.639271
1638.012780	72.367642	64.644276
1637.431694	67.875714	64.649281
1637.212419	69.910166	64.654286
1636.547986	67.673936	64.659290
1636.185525	66.640270	64.664295
1635.334638	65.819821	64.669300
1635.010461	67.243305	64.674305
1634.678570	69.136375	64.679310
1633.054755	68.938624	64.684314
1632.647230	63.275819	64.689319
1631.768486	71.661433	64.694324
1631.192282	78.508745	64.699329
1631.307335	67.618828	64.704334
1629.946265	62.028669	64.709338
1628.976618	57.969067	64.714343
1628.082337	60.637469	64.719348
1627.694977	71.810373	64.724353
1627.082087	64.462873	64.729358
1626.471024	69.934293	64.734362
1626.175640	63.286988	64.739367
1625.692563	71.163458	64.744372
1625.300529	65.121297	64.749377
1624.272962	65.355531	64.754382
1623.047044	73.840461	64.759386
1622.474443	64.685658	64.764391
1622.271135	67.491868	64.769396
1621.554322	63.083011	64.774401
1621.247759	67.779069	64.779406
1619.927508	68.416202	64.784410
1619.383557	66.976129	64.789415
1618.259094	66.386811	64.794420
1617.690790	67.577843	64.799425
1617.860293	62.667045	64.804430
1617.123167	80.345343	64.809434
1616.798943	65.699482	64.814439
1615.233019	65.339578	64.819444
1614.349323	70.173064	64.824449
1614.057412	68.273474	64.829454
1613.373577	71.916132	64.834458
1613.095201	65.713987	64.839463
1612.614814	67.711078	64.844468
1611.458413	70.725489	64.849473
1610.480163	67.428936	64.854478
1609.393315	69.153372	64.859482
1609.508769	66.356418	64.864487
1608.686262	78.860043	64.869492
1608.431230	75.939022	64.874497
1608.005458	65.627051	64.879502
1607.155925	74.848557	64.884506
1606.299869	71.527860	64.889511
1605.589890	71.219627	64.894516
1604.842915	82.104319	64.899521
1604.405733	72.271980	64.904526
1603.852741	74.025140	64.909530
1602.831602	71.607470	64.914535
1601.750224	67.625554	64.919540
1601.021316	67.990543	64.924545
1600.814329	62.084569	64.929550
1600.152419	67.497838	64.934554
1599.808019	68.527142	64.939559
1599.343789	74.151859	64.944564
1599.094040	71.351428	64.949569
1598.123618	63.176063	64.954574
1597.367768	72.611346	64.959578
1596.446111	64.716819	64.964583
1594.959342	73.746259	64.969588
1594.731390	73.448174	64.974593
1594.000012	64.525192	64.979598
1593.362320	75.662180	64.984602
1593.004338	61.155736	64.989607
1592.535244	67.330011	64.994612
1591.952202	61.721912	64.999617
1591.817568	58.363869	65.004622
1590.562825	72.312865	65.009626
1590.095623	68.779000	65.014631
1589.361909	69.662003	65.019636
1588.731696	58.906280	65.024641
1587.400447	65.447780	65.029646
1586.937045	68.632790	65.034650
1586.318839	63.377213	65.039655
1585.602111	65.345628	65.044660
1585.102314	71.969489	65.049665
1584.939004	67.210919	65.054670
1584.046859	63.321949	65.059674
1583.372766	66.751751	65.064679
1582.427584	66.602323	65.069684
1582.095723	68.634167	65.074689
1581.765794	66.494614	65.079694
1580.118710	69.441922	65.084698
1579.712508	62.629306	65.089703
1578.906009	67.958320	65.094708
1578.212999	65.821266	65.099713
1577.948978	56.041856	65.104718
1577.262618	61.902142	65.109722
1576.787638	60.250845	65.114727
1575.488657	61.058087	65.119732
1574.972013	65.847453	65.124737
1574.189532	60.370399	65.129742
1573.868900	54.763190	65.134746
1573.947517	61.634189	65.139751
1573.183541	67.375922	65.144756
1572.141251	58.089188	65.149761
1571.314757	54.528842	65.154766
1570.753378	70.430346	65.159770
1569.987839	60.500388	65.164775
1568.917723	67.244834	65.169780
1568.154283	59.132791	65.174785
1567.804225	54.522174	65.179790
1566.864462	63.138270	65.184794
1566.769651	63.646942	65.189799
1566.515510	68.211670	65.194804
1565.695492	68.594300	65.199809
1564.760293	57.857086	65.204814
1563.719296	66.017757	65.209818
1563.334217	61.534130	65.214823
1562.908723	59.106988	65.219828
1562.458210	65.309852	65.224833
1561.253375	60.716785	65.229838
1560.279360	66.476126	65.234842
1560.115856	64.548255	65.239847
1559.325296	60.845005	65.244852
1558.669764	59.999848	65.249857
1558.382869	55.656742	65.254862
1557.313316	65.416269	65.259866
1556.299223	64.041456	65.264871
1555.618948	65.822734	65.269876
1555.315442	65.478311	65.274881
1554.973549	54.150080	65.279886
1553.952551	66.377736	65.284890
1554.076229	60.395571	65.289895
1553.039565	64.600514	65.294900
1552.102498	66.786879	65.299905
1551.860390	64.370022	65.304910
1551.102463	64.862639	65.309914
1549.854188	57.092579	65.314919
1549.204714	69.559249	65.319924
1548.031493	64.577960	65.324929
1548.060862	72.541744	65.329934
1547.409809	63.120309	65.334938
1547.537329	58.160988	65.339943
1546.624285	60.753549	65.344948
1545.800506	62.649097	65.349953
1545.374651	51.504526	65.354958
1544.151892	66.192779	65.359962
1543.469265	58.545727	65.364967
1542.382915	57.797420	65.369972
1541.886826	59.030609	65.374977
1541.347226	55.809465	65.379982
1540.723711	58.277170	65.384986
1540.378492	60.140827	65.389991
1539.938446	57.443187	65.394996
1539.309873	61.354624	65.400001
1538.396458	58.361618	65.405006
1537.445997	69.154067	65.410010
1537.166305	54.584743	65.415015
1536.511340	58.017822	65.420020
1535.754234	60.505180	65.425025
1534.981003	65.007316	65.430030
1534.040605	66.815744	65.435034
1533.615162	62.575082	65.440039
1533.301763	64.834235	65.445044
1532.112430	59.549584	65.450049
1531.365270	63.196014	65.455054
1530.520831	64.140783	65.460058
1530.068560	58.213875	65.465063
1529.850258	48.435100	65.470068
1529.181701	58.810581	65.475073
1528.849971	60.831371	65.480078
1527.320295	64.313568	65.485082
1526.678912	65.919937	65.490087
1526.356403	63.943219	65.495092
1525.696892	62.507339	65.500097
1525.700993	59.546729	65.505102
1524.681606	64.665157	65.510106
1523.933292	63.891524	65.515111
1523.282972	65.983444	65.520116
1522.925598	68.266934	65.525121
1522.130082	58.685539	65.530126
1520.796060	72.237144	65.535130
1520.071757	64.382252	65.540135
1519.857254	61.949973	65.545140
1519.396927	63.297333	65.550145
1518.509344	58.724837	65.555150
1517.228825	59.764142	65.560154
1516.847858	66.058462	65.565159
1516.146897	55.873835	65.570164
1515.620449	67.125613	65.575169
1516.107712	60.100062	65.580174
1514.693016	60.831105	65.585178
1513.714324	56.720949	65.590183
1513.211543	57.658737	65.595188
1512.369299	60.422985	65.600193
1512.107577	56.068002	65.605198
1511.377431	63.985320	65.610202
1510.452036	65.092773	65.615207
1509.817088	53.951477	65.620212
1509.187673	69.926875	65.625217
1508.636884	62.050721	65.630222
1507.986761	66.441836	65.635226
1507.521189	62.095592	65.640231
1506.318990	66.046159	65.645236
1505.795426	62.396691	65.650241
1505.442226	52.194652	65.655246
1505.004439	60.560675	65.660250
1504.065245	57.108151	65.665255
1503.226321	59.906568	65.670260
1502.320813	62.097395	65.675265
1502.333448	55.546248	65.680270
1501.041625	57.121950	65.685274
1500.108522	57.555688	65.690279
1499.669656	56.996238	65.695284
1498.837086	60.791869	65.700289
1498.607532	60.662783	65.705294
1498.085898	61.603570	65.710298
1497.817818	66.299827	65.715303
1497.337061	61.350443	65.720308
1496.347872	65.853794	65.725313
1495.800919	54.110309	65.730318
1494.924262	65.586480	65.735322
1493.701217	68.904847	65.740327
1492.906910	62.723218	65.745332
1492.299980	61.551806	65.750337
1492.186194	56.640299	65.755342
1491.511105	62.858360	65.760346
1491.021925	61.986783	65.765351
1490.028148	60.432147	65.770356
1488.980469	62.106251	65.775361
1488.661129	61.062601	65.780366
1488.166891	63.509772	65.785370
1487.981363	61.456096	65.790375
1487.123016	71.410742	65.795380
1486.044728	62.213349	65.800385
1485.596972	54.019630	65.805390
1484.852443	56.539696	65.810394
1483.974163	57.499320	65.815399
1483.229869	57.808439	65.820404
1482.422545	64.588419	65.825409
1482.460318	59.796328	65.830414
1481.764223	63.666469	65.835418
1481.076111	56.070774	65.840423
1479.890802	62.786247	65.845428
1478.957882	55.683629	65.850433
1478.836050	48.658689	65.855438
1478.215127	63.800094	65.860442
1477.656056	63.676072	65.865447
1477.577394	55.371654	65.870452
1476.008821	64.456724	65.875457
1475.595568	56.954544	65.880462
1474.758367	64.243904	65.885466
1474.602180	59.471601	65.890471
1473.806397	62.537564	65.895476
1472.556345	61.603991	65.900481
1472.250981	49.401070	65.905486
1471.352477	56.219194	65.910490
1471.225386	47.835745	65.915495
1470.783876	58.887939	65.920500
1469.639768	64.939272	65.925505
1469.186250	61.198255	65.930510
1468.705334	60.372678	65.935514
1467.754031	65.671118	65.940519
1466.958772	59.284645	65.945524
1466.130136	64.878982	65.950529
1465.925221	60.492897	65.955534
1464.468657	68.145633	65.960538
1464.450225	53.880161	65.965543
1463.345238	66.100689	65.970548
1462.557282	59.891255	65.975553
1462.413933	56.854734	65.980558
1461.763064	62.695209	65.985562
1461.467870	63.754556	65.990567
1460.796923	59.559239	65.995572
1459.746267	63.580357	66.000577
1459.227605	52.764377	66.005582
1458.391220	68.299582	66.010586
1457.454270	57.557967	66.015591
1456.589292	65.387916	66.020596
1456.068782	66.725929	66.025601
1455.992268	57.053938	66.030606
1455.288665	63.159843	66.035610
1454.956994	54.146581	66.040615
1453.899276	65.198949	66.045620
1453.378670	64.829120	66.050625
1452.788409	59.201709	66.055630
1451.026439	54.227317	66.060634
1450.261812	58.215590	66.065639
1450.541459	49.210825	66.070644
1449.707563	59.185239	66.075649
1449.328291	56.955779	66.080654
1448.830490	63.765418	66.085658
1448.238601	56.274291	66.090663
1447.072200	57.164603	66.095668
1446.273331	62.025653	66.100673
1446.189240	53.882953	66.105678
1445.601762	62.134002	66.110682
1444.382973	61.515599	66.115687
1443.724946	52.804952	66.120692
1443.032332	54.801108	66.125697
1442.557370	56.915636	66.130702
1442.145383	66.316789	66.135706
1441.098765	65.672598	66.140711
1440.438360	56.855093	66.145716
1439.589243	59.481683	66.150721
1439.348433	52.901439	66.155726
1438.673876	61.803424	66.160730
1438.279748	46.028597	66.165735
1437.189104	57.363744	66.170740
1436.497409	61.127538	66.175745
1436.186043	51.292609	66.180750
1435.464141	65.978555	66.185754
1434.407996	51.835456	66.190759
1433.744598	60.671013	66.195764
1433.084693	64.839767	66.200769
1433.217428	53.073424	66.205774
1432.509284	63.117744	66.210778
1431.226689	66.609607	66.215783
1430.505226	61.373644	66.220788
1429.622697	60.567757	66.225793
1429.433445	61.783734	66.230798
1429.074141	63.613373	66.235802
1428.268467	67.735913	66.240807
1427.519696	61.578611	66.245812
1426.476511	70.834091	66.250817
1426.185680	57.925536	66.255822
1424.999884	62.337157	66.260826
1424.257301	56.164682	66.265831
1423.727615	63.495061	66.270836
1423.229583	57.097631	66.275841
1423.182350	51.008597	66.280846
1422.791240	61.223298	66.285850
1421.567721	56.243765	66.290855
1420.954912	48.885286	66.295860
1419.938053	66.868250	66.300865
1419.842551	55.502465	66.305870
1418.485078	59.977648	66.310874
1417.854305	66.166602	66.315879
1417.588313	57.969239	66.320884
1416.909201	62.104779	66.325889
1416.595969	57.653917	66.330894
1415.118539	69.060023	66.335898
1414.496899	61.433283	66.340903
1414.477852	59.939782	66.345908
1413.442135	69.225617	66.350913
1413.299687	60.543409	66.355918
1412.090289	63.541093	66.360922
1411.432138	67.693805	66.365927
1411.154497	51.651303	66.370932
1410.046238	64.474766	66.375937
1409.148401	60.921087	66.380942
1408.050690	64.009830	66.385946
1407.870170	62.616115	66.390951
1407.548571	55.938329	66.395956
1407.065932	64.885509	66.400961
1406.987802	65.170759	66.405966
1405.882887	64.266188	66.410970
1404.955039	65.153292	66.415975
1404.386711	57.713626	66.420980
1403.555721	68.671623	66.425985
1402.745741	52.158651	66.430990
1401.717651	64.329124	66.435994
1401.416771	65.482422	66.440999
1401.060613	65.141657	66.446004
1400.381127	69.963243	66.451009
1400.127653	57.162299	66.456014
1398.930991	58.454839	66.461018
1398.108501	65.915346	66.466023
1397.596555	46.513311	66.471028
1397.307844	59.108723	66.476033
1396.460009	53.962249	66.481038
1395.529330	62.966458	66.486042
1395.081987	68.273119	66.491047
1394.562836	66.028055	66.496052
1393.637857	59.570768	66.501057
1393.126359	51.959647	66.506062
1392.329267	60.810154	66.511066
1391.741904	66.112265	66.516071
1391.571564	65.503840	66.521076
1390.013027	67.664472	66.526081
1389.677935	57.226188	66.531086
1388.919038	61.122102	66.536090
1388.487560	62.955335	66.541095
1388.232129	56.885205	66.546100
1386.966461	66.447300	66.551105
1386.274496	48.590927	66.556110
1385.536249	61.046489	66.561114
1384.945801	59.864600	66.566119
1384.810736	61.196546	66.571124
1383.570628	55.718194	66.576129
1383.083295	50.746232	66.581134
1382.461344	67.449007	66.586138
1381.834423	54.355773	66.591143
1381.324220	54.802750	66.596148
1380.297962	66.299575	66.601153
1379.644578	57.853140	66.606158
1379.155322	53.949090	66.611162
1378.716580	59.990826	66.616167
1377.931324	59.740356	66.621172
1376.914916	63.191505	66.626177
1376.291680	58.241147	66.631182
1375.838680	62.257171	66.636186
1375.559031	58.698272	66.641191
1374.953150	49.235033	66.646196
1373.798207	54.207899	66.651201
1373.344968	49.266790	66.656206
1372.885549	61.778954	66.661210
1371.732016	57.174678	66.666215
1371.112576	54.593900	66.671220
1369.962942	59.657390	66.676225
1369.706136	58.832475	66.681230
1369.411727	53.394603	66.686234
1368.847895	54.912984	66.691239
1368.233198	55.740856	66.696244
1367.043249	68.422779	66.701249
1367.086620	61.948754	66.706254
1366.438606	61.012566	66.711258
1365.282256	52.669753	66.716263
1364.884263	61.109886	66.721268
1363.874097	62.711842	66.726273
1363.307831	55.509984	66.731278
1361.923744	48.876542	66.736282
1361.495541	57.069162	66.741287
1361.098256	55.121704	66.746292
1360.516063	53.407070	66.751297
1360.559916	47.443913	66.756302
1360.244648	54.355428	66.761306
1358.640994	63.190666	66.766311
1358.371988	54.755672	66.771316
1357.433274	66.981337	66.776321
1356.460821	65.018084	66.781326
1355.627292	65.939097	66.786330
1355.002600	57.737270	66.791335
1354.764744	56.234403	66.796340
1354.376266	54.034808	66.801345
1353.828582	54.815759	66.806350
1352.549231	66.911074	66.811354
1351.929645	58.459275	66.816359
1351.819836	61.381521	66.821364
1350.911640	68.485079	66.826369
1349.993988	59.446726	66.831374
1349.443431	60.874692	66.836378
1348.757422	59.780544	66.841383
1348.432455	54.057371	66.846388
1347.149452	63.674276	66.851393
1346.554952	50.837681	66.856398
1345.878296	59.230654	66.861402
1345.128792	57.957366	66.866407
1345.020156	53.511837	66.871412
1344.556533	63.823228	66.876417
1343.919096	55.725935	66.881422
1343.017933	62.202319	66.886426
1342.421020	56.158102	66.891431
1341.454927	47.827636	66.896436
1340.352418	58.357292	66.901441
1339.675767	63.678337	66.906446
1339.442754	57.986277	66.911450
1338.819923	56.404267	66.916455
1338.880637	56.604366	66.921460
1337.564014	60.070142	66.926465
1336.753209	51.607752	66.931470
1336.188570	58.279794	66.936474
1335.768442	59.330631	66.941479
1335.504814	53.387972	66.946484
1334.155392	61.194045	66.951489
1333.580762	53.164042	66.956494
1333.416398	52.937874	66.961498
1332.098872	62.823626	66.966503
1331.240345	52.705126	66.971508
1330.386809	61.151456	66.976513
1330.200533	49.350687	66.981518
1329.969783	52.071384	66.986522
1329.250212	62.169577	66.991527
1328.456423	59.094554	66.996532
1327.702818	61.687068	67.001537
1327.029510	53.325824	67.006542
1326.529818	56.805224	67.011546
1325.759338	55.751322	67.016551
1324.888436	49.515708	67.021556
1324.090236	60.623043	67.026561
1323.899595	44.256080	67.031566
1323.394490	54.708103	67.036570
1322.089719	57.227399	67.041575
1321.602178	54.136805	67.046580
1320.977755	63.171189	67.051585
1320.835217	55.395768	67.056590
1319.646288	61.536286	67.061594
1318.837740	62.869657	67.066599
1318.485986	51.819027	67.071604
1317.951436	63.384345	67.076609
1317.407334	53.354631	67.081614
1316.564864	60.086620	67.086618
1315.599329	58.641106	67.091623
1315.330415	57.655695	67.096628
1314.566026	59.281670	67.101633
1313.430511	62.305498	67.106638
1312.992090	54.485659	67.111642
1312.111547	53.647958	67.116647
1311.981196	56.647586	67.121652
1311.189084	58.642249	67.126657
1310.584232	56.126978	67.131662
1309.611764	52.810712	67.136666
1308.705971	62.902247	67.141671
1308.625230	50.438146	67.146676
1308.102418	57.330624	67.151681
1307.418301	51.809645	67.156686
1306.183124	51.086681	67.161690
1305.724973	56.406105	67.166695
1305.475058	54.023637	67.171700
1304.706130	58.876808	67.176705
1303.702731	62.691770	67.181710
1303.113692	63.004641	67.186714
1302.301621	60.493934	67.191719
1302.397138	51.466403	67.196724
1301.124970	57.733702	67.201729
1300.362237	55.722935	67.206734
1299.900088	62.154759	67.211738
1298.846227	65.375346	67.216743
1298.781282	51.371192	67.221748
1298.375448	52.695730	67.226753
1297.222435	61.287458	67.231758
1296.806620	59.710389	67.236762
1296.048535	58.775952	67.241767
1295.474644	58.569170	67.246772
1294.372595	58.373828	67.251777
1293.937933	55.520838	67.256782
1293.220009	50.341134	67.261786
1292.734778	64.421757	67.266791
1292.506261	60.119873	67.271796
1291.100689	57.249373	67.276801
1290.501620	54.185982	67.281806
1290.252980	54.886280	67.286810
1289.461739	56.368296	67.291815
1288.872316	57.351441	67.296820
1287.793414	57.603433	67.301825
1287.389247	50.855224	67.306830
1286.906193	56.071376	67.311834
1285.436061	62.816443	67.316839
1285.100185	53.329223	67.321844
1284.422681	57.854046	67.326849
1283.988551	47.401581	67.331854
1283.701145	50.900848	67.336858
1283.169536	60.070289	67.341863
1282.659941	49.566743	67.346868
1281.639660	52.463448	67.351873
1280.832917	46.419503	67.356878
1279.356360	56.778418	67.361882
1278.877696	60.358562	67.366887
1278.340242	53.544814	67.371892
1278.186753	59.941752	67.376897
1277.646468	56.798052	67.381902
1277.611099	47.113242	67.386906
1276.398795	56.892395	67.391911
1275.928312	47.470740	67.396916
1274.953003	50.066980	67.401921
1274.087174	45.325544	67.406926
1273.122802	48.776337	67.411930
1272.599931	53.470539	67.416935
1272.427775	52.723639	67.421940
1271.907604	48.979075	67.426945
1271.070258	55.817492	67.431950
1270.333989	48.772009	67.436954
1269.670197	55.630138	67.441959
1269.181071	52.109297	67.446964
1267.822692	54.551987	67.451969
1267.435076	45.194430	67.456974
1266.973427	47.300560	67.461978
1266.303315	55.055410	67.466983
1265.985914	44.376231	67.471988
1264.832665	56.833143	67.476993
1263.915168	46.549011	67.481998
1263.295375	45.222007	67.487002
1263.201466	52.751189	67.492007
1262.588795	46.233264	67.497012
1261.184985	51.092782	67.502017
1261.045486	49.995334	67.507022
1260.495651	39.665360	67.512026
1259.794802	53.632026	67.517031
1258.853140	54.526109	67.522036
1258.040861	49.609004	67.527041
1257.328836	50.688923	67.532046
1257.185230	52.712941	67.537050
1256.420580	48.996218	67.542055
1255.752314	49.056768	67.547060
1254.934087	52.556868	67.552065
1254.669733	55.405917	67.557070
1254.233574	49.413439	67.562074
1252.823936	58.877049	67.567079
1252.400646	48.312481	67.572084
1251.605973	47.855388	67.577089
1250.923191	55.648526	67.582094
1250.075132	45.340743	67.587098
1249.170410	52.521041	67.592103
1248.613035	49.334336	67.597108
1248.276546	56.451083	67.602113
1247.705517	45.987282	67.607118
1247.777067	46.493163	67.612122
1246.906175	50.299687	67.617127
1246.132108	45.395435	67.622132
1245.322703	52.396572	67.627137
1244.625570	40.334865	67.632142
1243.405789	48.197626	67.637146
1242.648595	45.105778	67.642151
1242.421097	46.222190	67.647156
1242.023913	51.468847	67.652161
1241.374835	46.800188	67.657166
1240.446211	42.421992	67.662170
1239.794345	50.068286	67.667175
1239.402799	44.297378	67.672180
1238.673211	42.298708	67.677185
1237.705723	44.001156	67.682190
1236.999266	48.609438	67.687194
1236.250489	47.735041	67.692199
1236.398266	48.962088	67.697204
1235.282090	55.955242	67.702209
1234.212219	55.576612	67.707214
1233.780587	60.223196	67.712218
1233.405718	63.392600	67.717223
1232.763321	51.770042	67.722228
1231.869383	62.044215	67.727233
1230.760718	56.469348	67.732238
1230.488519	53.871235	67.737242
1230.013454	54.113957	67.742247
1229.802764	52.168388	67.747252
1228.212447	56.709075	67.752257
1227.616179	53.538021	67.757262
1227.253968	44.389325	67.762266
1226.844173	52.649989	67.767271
1226.154815	37.026272	67.772276
1224.859171	56.288357	67.777281
1224.029975	46.851224	67.782286
1223.869289	48.081593	67.787290
1223.413349	54.804172	67.792295
1223.415811	49.349077	67.797300
1222.329452	51.715414	67.802305
1221.505107	57.944646	67.807310
1220.874548	48.354497	67.812314
1219.640053	50.235033	67.817319
1219.264916	52.004136	67.822324
1218.895245	51.085223	67.827329
1218.442751	46.396347	67.832334
1217.489718	52.508847	67.837338
1216.314979	55.866960	67.842343
1216.213741	53.416703	67.847348
1215.852938	49.638923	67.852353
1214.667338	55.802604	67.857358
1213.920813	52.316403	67.862362
1212.936270	60.233235	67.867367
1212.937971	44.745619	67.872372
1212.307828	52.606085	67.877377
1211.399108	51.296659	67.882382
1210.514799	51.536659	67.887386
1209.883710	60.225186	67.892391
1209.565351	53.059644	67.897396
1209.203279	53.714911	67.902401
1208.117247	52.023674	67.907406
1207.373905	44.391134	67.912410
1206.492577	47.609545	67.917415
1206.736280	52.579237	67.922420
1205.659032	42.580741	67.927425
1204.571221	48.597983	67.932430
1204.246539	55.381692	67.937434
1203.807242	50.031548	67.942439
1202.756594	38.909182	67.947444
1201.458563	53.413957	67.952449
1201.225216	54.793079	67.957454
1201.304337	51.869435	67.962458
1200.662425	54.650801	67.967463
1199.935839	41.571923	67.972468
1198.907489	52.010977	67.977473
1198.463054	39.559015	67.982478
1197.308626	47.179586	67.987482
1196.389812	43.291860	67.992487
1195.839494	41.537507	67.997492
1195.406465	39.780269	68.002497
1194.956765	53.342721	68.007502
1194.961136	39.403268	68.012506
1193.755416	55.192782	68.017511
1192.922083	36.147891	68.022516
1192.219413	41.572445	68.027521
1191.765326	48.748895	68.032526
1191.016059	46.497901	68.037530
1190.119568	47.370631	68.042535
1189.662610	43.374760	68.047540
1189.093556	50.165793	68.052545
1188.096219	44.179006	68.057550
1187.438239	44.058164	68.062554
1186.950761	54.630397	68.067559
1186.674364	44.233301	68.072564
1186.008559	49.144214	68.077569
1184.490820	53.195562	68.082574
1184.091246	54.233691	68.087578
1183.558719	60.388136	68.092583
1183.474295	51.138494	68.097588
1182.568355	47.141492	68.102593
1181.565788	51.013133	68.107598
1181.025487	47.216599	68.112602
1180.504550	53.224117	68.117607
1180.062900	45.341752	68.122612
1178.897152	43.626938	68.127617
1178.393149	51.325420	68.132622
1177.834555	46.063644	68.137626
1177.055420	54.389363	68.142631
1176.612402	45.488499	68.147636
1175.670633	48.631376	68.152641
1174.894394	59.419854	68.157646
1174.900869	48.506254	68.162650
1173.802076	54.750762	68.167655
1172.782647	45.747611	68.172660
1171.988468	56.408052	68.177665
1171.823272	52.758440	68.182670
1171.985453	49.452577	68.187674
1170.609978	56.234684	68.192679
1170.003878	47.831270	68.197684
1169.397439	43.051773	68.202689
1168.127970	52.638204	68.207694
1167.582900	47.449974	68.212698
1166.772828	55.521994	68.217703
1166.401074	58.589984	68.222708
1165.865996	53.802288	68.227713
1165.437343	47.417551	68.232718
1164.666709	52.285219	68.237722
1163.760016	55.826225	68.242727
1163.560677	54.848689	68.247732
1163.028879	56.289477	68.252737
1161.478223	53.442131	68.257742
1161.327124	50.815304	68.262746
1160.327529	55.381921	68.267751
1160.012354	57.231381	68.272756
1159.145769	54.712049	68.277761
1158.435490	47.695591	68.282766
1158.041615	42.694629	68.287770
1157.211629	56.796969	68.292775
1156.849088	51.535553	68.297780
1156.247915	50.666088	68.302785
1154.972996	51.917568	68.307790
1154.902904	40.858459	68.312794
1154.126899	48.358930	68.317799
1153.554074	48.658217	68.322804
1152.285525	53.340156	68.327809
1151.616247	45.124996	68.332814
1151.652781	42.708025	68.337818
1150.732200	51.890459	68.342823
1150.017697	38.294018	68.347828
1149.216205	40.353295	68.352833
1148.296659	46.127749	68.357838
1148.528471	47.841319	68.362842
1147.123846	53.174113	68.367847
1146.587236	39.639262	68.372852
1146.023245	43.991512	68.377857
1145.252888	46.736549	68.382862
1145.361842	43.286188	68.387866
1143.777581	52.522151	68.392871
1143.202902	48.240659	68.397876
1142.755411	49.387341	68.402881
1142.289508	49.862012	68.407886
1141.674701	45.522249	68.412890
1140.513702	55.108785	68.417895
1140.026256	53.454830	68.422900
1139.782659	41.328909	68.427905
1138.467749	48.744793	68.432910
1137.661874	51.954378	68.437914
1137.081450	50.826149	68.442919
1136.778582	40.937904	68.447924
1136.358957	49.581761	68.452929
1136.096505	54.232983	68.457934
1135.245260	47.328843	68.462938
1134.263698	44.728462	68.467943
1133.731380	45.883907	68.472948
1132.446460	45.209943	68.477953
1131.876266	54.699349	68.482958
1131.679656	39.717964	68.487962
1130.973982	38.978669	68.492967
1130.441322	45.018018	68.497972
1129.390953	38.659648	68.502977
1128.945230	42.163607	68.507982
1128.848708	37.634174	68.512986
1127.553549	51.299572	68.517991
1126.547459	40.610130	68.522996
1126.182075	35.429604	68.528001
1125.383693	44.781837	68.533006
1125.133445	40.909218	68.538010
1124.129724	45.908588	68.543015
1123.412020	46.685092	68.548020
1122.768945	41.831013	68.553025
1122.024564	43.914330	68.558030
1121.653543	35.494046	68.563034
1121.019847	49.975171	68.568039
1120.404478	43.523952	68.573044
1119.616336	41.756985	68.578049
1118.852644	49.526744	68.583054
1118.447281	42.229986	68.588058
1117.117879	44.582985	68.593063
1116.769776	38.097140	68.598068
1116.493463	47.658068	68.603073
1115.788450	46.032420	68.608078
1115.587259	41.754604	68.613082
1114.199882	45.673288	68.618087
1113.833441	44.627721	68.623092
1113.375612	51.024180	68.628097
1111.876556	45.345898	68.633102
1111.244461	38.838997	68.638106
1110.798531	52.678396	68.643111
1110.395849	50.049017	68.648116
1109.922786	49.116606	68.653121
1109.332903	46.971172	68.658126
1108.529135	45.378582	68.663130
1107.593245	50.241013	68.668135
1106.962217	39.040907	68.673140
1106.800094	45.756179	68.678145
1105.712219	37.506703	68.683150
1105.282495	34.889515	68.688154
1104.326278	40.157301	68.693159
1104.010725	39.043716	68.698164
1103.058141	36.957560	68.703169
1102.138749	41.714862	68.708174
1102.006670	40.794443	68.713178
1101.405546	37.103802	68.718183
1100.523107	40.529003	68.723188
1099.714479	38.926151	68.728193
1098.862835	46.624748	68.733198
1098.546419	43.732490	68.738202
1098.016920	47.651906	68.743207
1096.807012	43.099319	68.748212
1096.278244	35.987781	68.753217
1095.776047	44.499692	68.758222
1095.344540	41.526395	68.763226
1094.656858	49.194180	68.768231
1093.887116	41.501230	68.773236
1093.246454	43.131237	68.778241
1092.771769	53.436512	68.783246
1092.211887	46.303112	68.788250
1091.056867	51.794922	68.793255
1090.276105	47.790658	68.798260
1089.864398	44.024154	68.803265
1089.364030	49.799752	68.808270
1089.097436	43.474410	68.813274
1088.043437	51.159471	68.818279
1087.293536	50.089755	68.823284
1086.872858	46.892384	68.828289
1085.288522	49.170838	68.833294
1084.789069	49.859015	68.838298
1084.472936	43.483207	68.843303
1084.109578	50.922780	68.848308
1083.742047	49.785927	68.853313
1082.915235	51.669480	68.858318
1082.513556	55.092325	68.863322
1081.511315	48.377809	68.868327
1080.548407	49.750000	68.873332
1079.898798	46.404546	68.878337
1079.114004	44.257012	68.883342
1078.759708	44.195119	68.888346
1078.322492	44.985360	68.893351
1077.225722	45.584061	68.898356
1076.594669	48.291185	68.903361
1076.106985	52.923048	68.908366
1075.485471	41.185273	68.913370
1074.131687	42.608612	68.918375
1073.440993	36.994145	68.923380
1073.325207	42.468861	68.928385
1072.809440	47.453699	68.933390
1072.652291	45.449166	68.938394
1071.645599	48.069395	68.943399
1071.140738	37.161470	68.948404
1070.806315	35.576228	68.953409
1069.463218	47.569809	68.958414
1068.437759	39.550119	68.963418
1068.111240	41.518087	68.968423
1067.527116	42.088850	68.973428
1066.870288	35.496014	68.978433
1065.718540	45.658265	68.983438
1065.174339	42.245584	68.988442
1064.667711	43.982008	68.993447
1064.460027	42.826036	68.998452
1063.758097	33.824474	69.003457
1062.627822	46.875454	69.008462
1062.371272	29.134490	69.013466
1061.838849	45.140192	69.018471
1061.029504	39.997192	69.023476
1060.245865	44.330786	69.028481
1059.679612	39.600123	69.033486
1059.275053	36.315039	69.038490
1057.943459	45.944508	69.043495
1057.426759	40.015357	69.048500
1056.783967	32.710661	69.053505
1055.998940	47.873457	69.058510
1055.870143	43.908985	69.063514
1054.375886	36.241434	69.068519
1053.447263	49.263490	69.073524
1053.515653	41.370977	69.078529
1052.739460	46.901879	69.083534
1052.753140	36.245778	69.088538
1051.853237	41.767974	69.093543
1050.597303	42.387277	69.098548
1050.222931	43.060292	69.103553
1049.708324	45.794626	69.108558
1049.301395	36.834444	69.113562
1048.203017	45.179437	69.118567
1047.176159	43.863637	69.123572
1047.175406	42.662128	69.128577
1046.623528	47.886106	69.133582
1045.653600	42.259302	69.138586
1044.704216	42.755719	69.143591
1043.997825	47.493345	69.148596
1043.975109	44.809834	69.153601
1043.196257	51.967008	69.158606
1042.148489	43.906724	69.163610
1041.451665	51.546012	69.168615
1041.057763	40.262471	69.173620
1040.784810	38.749455	69.178625
1039.800443	46.992734	69.183630
1038.988190	35.279017	69.188634
1038.654205	44.939005	69.193639
1037.700142	42.667028	69.198644
1036.989537	45.774750	69.203649
1036.207480	51.639328	69.208654
1035.794074	46.346607	69.213658
1035.338245	43.889703	69.218663
1034.693659	43.804617	69.223668
1033.846886	47.202087	69.228673
1033.030758	46.997637	69.233678
1032.846911	45.173975	69.238682
1031.702237	46.903112	69.243687
1030.877650	44.640499	69.248692
1030.535789	47.024076	69.253697
1029.702036	47.489485	69.258702
1029.628147	38.564628	69.263706
1028.473296	52.031119	69.268711
1027.919639	53.235712	69.273716
1027.456371	42.851039	69.278721
1025.834607	52.592927	69.283726
1025.146135	47.079044	69.288730
1024.717673	54.719793	69.293735
1024.386598	44.506476	69.298740
1024.090124	44.548931	69.303745
1023.856620	49.715949	69.308750
1023.186053	40.050239	69.313754
1022.168429	39.915700	69.318759
1021.142879	51.182262	69.323764
1020.303267	40.751816	69.328769
1019.260302	41.811914	69.333774
1018.658059	43.461058	69.338778
1018.376821	47.741534	69.343783
1018.179741	44.896532	69.348788
1017.768590	48.059114	69.353793
1016.801442	45.973731	69.358798
1016.293765	36.532846	69.363802
1015.628806	35.181554	69.368807
1014.773252	44.612294	69.373812
1013.893526	44.134117	69.378817
1013.356890	51.905619	69.383822
1012.759820	46.996942	69.388826
1011.436495	51.594619	69.393831
1010.720721	43.498872	69.398836
1010.391379	38.779413	69.403841
1009.623024	59.477854	69.408846
1009.519610	45.043062	69.413850
1009.042591	44.418808	69.418855
1008.302289	49.926664	69.423860
1007.521809	37.510887	69.428865
1006.575742	45.785928	69.433870
1006.167536	39.574598	69.438874
1004.973594	45.548875	69.443879
1004.424634	41.018902	69.448884
1004.187272	34.086530	69.453889
1003.430958	41.557090	69.458894
1003.029768	35.898159	69.463898
1002.063244	47.292527	69.468903
1001.266781	42.393505	69.473908
1000.913279	40.808154	69.478913
1000.242090	44.043654	69.483918
999.143352	36.144471	69.488922
998.368286	41.044421	69.493927
997.704563	46.014965	69.498932
997.833873	45.056113	69.503937
997.144019	40.606910	69.508942
996.495806	49.386497	69.513946
995.528222	44.462666	69.518951
994.896880	50.027304	69.523956
994.293940	36.140365	69.528961
992.914168	45.872146	69.533966
992.705637	52.367722	69.538970
992.073601	43.492255	69.543975
991.779413	50.722131	69.548980
991.218584	38.817036	69.553985
989.820398	47.954082	69.558990
989.737194	43.870397	69.563994
989.334185	47.853283	69.568999
988.359544	46.251653	69.574004
987.654613	47.966030	69.579009
987.088747	53.025086	69.584014
986.268901	35.294924	69.589018
985.388550	38.519554	69.594023
984.568822	47.302779	69.599028
984.514035	41.115641	69.604033
983.629195	44.333102	69.609038
983.118668	36.296174	69.614042
982.094979	40.212244	69.619047
981.602379	40.382108	69.624052
980.996068	36.656056	69.629057
979.838726	47.058925	69.634062
979.194000	46.953375	69.639066
978.854531	50.867804	69.644071
978.305220	47.027024	69.649076
978.205331	35.354519	69.654081
976.943940	45.248818	69.659086
976.181566	45.993047	69.664090
975.611231	45.486151	69.669095
974.972837	53.808440	69.674100
974.773748	42.315720	69.679105
973.564794	49.730585	69.684110
972.992893	44.168209	69.689114
972.560184	40.493382	69.694119
971.386460	51.009250	69.699124
970.908980	46.318100	69.704129
970.038346	49.855005	69.709134
969.697032	46.053669	69.714138
969.506511	42.061181	69.719143
968.414480	52.906252	69.724148
967.805835	47.840157	69.729153
967.270509	48.929882	69.734158
966.401032	37.722044	69.739162
965.417719	44.541183	69.744167
964.769450	48.044281	69.749172
964.256029	38.295241	69.754177
963.844635	42.686317	69.759182
963.615451	40.838338	69.764186
962.534117	48.571945	69.769191
961.455412	46.750342	69.774196
961.201620	38.773489	69.779201
960.499421	44.000899	69.784206
960.162879	41.687455	69.789210
958.862382	40.366352	69.794215
958.506296	37.898323	69.799220
958.291280	32.585093	69.804225
956.887919	46.341883	69.809230
955.783360	45.923160	69.814234
955.428081	41.624154	69.819239
954.840880	48.812350	69.824244
955.104479	38.471302	69.829249
954.346352	45.987896	69.834254
953.326890	38.858291	69.839258
952.566501	36.792073	69.844263
951.991170	45.243098	69.849268
951.230201	42.205564	69.854273
950.071798	45.906542	69.859278
949.716004	36.826284	69.864282
949.301527	45.333713	69.869287
948.645024	47.161818	69.874292
948.184699	43.269039	69.879297
947.001993	43.514040	69.884302
946.885200	32.681597	69.889306
946.400748	37.442270	69.894311
944.978487	43.422942	69.899316
944.619405	38.725574	69.904321
944.104341	48.324498	69.909326
943.626115	52.349322	69.914330
942.469868	36.754302	69.919335
941.854296	36.775009	69.924340
941.014563	29.739815	69.929345
940.564201	45.521149	69.934350
940.265125	46.054463	69.939354
939.475142	44.902862	69.944359
938.301148	43.843913	69.949364
938.201610	40.369961	69.954369
937.278913	49.297319	69.959374
936.210093	30.316859	69.964378
935.873699	47.094041	69.969383
935.273318	35.926972	69.974388
935.306688	36.981391	69.979393
934.460223	46.407550	69.984398
933.508494	44.165206	69.989402
932.914809	35.271046	69.994407
931.981161	37.277302	69.999412
930.929500	46.313493	70.004417
930.385441	45.968007	70.009422
929.910662	40.500575	70.014426
929.426672	42.170342	70.019431
928.978850	44.856222	70.024436
928.361924	42.678869	70.029441
927.106652	43.982527	70.034446
926.591525	34.550741	70.039450
926.396086	44.303800	70.044455
925.452996	46.418795	70.049460
924.602651	35.149586	70.054465
923.835522	36.091706	70.059470
923.656304	38.637066	70.064474
923.306772	38.777864	70.069479
922.159596	45.664097	70.074484
921.398879	41.874326	70.079489
920.670442	36.310072	70.084494
920.385633	35.754593	70.089498
919.575788	38.822943	70.094503
918.447749	44.045595	70.099508
918.306238	42.178937	70.104513
917.495749	44.380064	70.109518
917.139967	33.550968	70.114522
916.215136	39.722146	70.119527
915.207134	40.458176	70.124532
915.197965	40.847581	70.129537
914.279510	47.919768	70.134542
913.064215	44.653355	70.139546
912.479442	46.572556	70.144551
911.970498	47.079349	70.149556
911.859079	38.691914	70.154561
911.518177	35.103415	70.159566
910.414248	37.378054	70.164570
909.657930	38.182839	70.169575
908.929763	40.984303	70.174580
908.214344	31.297396	70.179585
907.060359	43.727718	70.184590
906.514621	39.867467	70.189594
906.098054	40.572448	70.194599
905.595471	51.938737	70.199604
905.527208	45.137159	70.204609
904.535879	49.871281	70.209614
904.047309	33.192310	70.214618
903.703424	39.113334	70.219623
902.386475	50.502002	70.224628
901.623296	30.145121	70.229633
901.048268	42.793959	70.234638
900.364070	43.527345	70.239642
899.313573	45.582173	70.244647
898.528266	46.378960	70.249652
898.316023	44.447866	70.254657
897.792249	48.282826	70.259662
897.594492	47.346064	70.264666
896.612653	39.026204	70.269671
895.402411	40.120860	70.274676
895.085649	40.317947	70.279681
894.784717	48.772617	70.284686
893.761242	44.048538	70.289690
892.873586	49.308637	70.294695
892.255341	46.273638	70.299700
891.799783	38.541800	70.304705
891.066600	42.886331	70.309710
889.969520	49.909685	70.314714
889.497101	42.937469	70.319719
888.958204	49.275891	70.324724
889.069154	46.224181	70.329729
888.091944	50.202276	70.334734
887.125545	56.411625	70.339738
886.850168	41.050172	70.344743
885.821561	41.712222	70.349748
884.921113	45.351669	70.354753
883.960563	46.450744	70.359758
883.291947	49.121311	70.364762
883.482678	38.012846	70.369767
882.674725	45.360767	70.374772
882.406522	37.742615	70.379777
881.383578	42.272039	70.384782
880.839338	44.355106	70.389786
879.878045	43.522528	70.394791
878.998949	46.486795	70.399796
878.714854	44.980303	70.404801
877.670619	39.035818	70.409806
877.294453	46.231435	70.414810
876.708812	36.675268	70.419815
875.770507	50.651388	70.424820
875.262259	36.667422	70.429825
875.077172	39.519648	70.434830
873.983640	46.318514	70.439834
873.154435	42.555429	70.444839
872.508072	48.783225	70.449844
872.115466	42.474825	70.454849
870.885618	47.562314	70.459854
869.961051	42.641154	70.464858
869.679535	39.114171	70.469863
869.338323	45.452668	70.474868
869.079782	41.212398	70.479873
868.262365	41.329906	70.484878
867.561325	34.972833	70.489882
866.880892	28.391709	70.494887
866.334307	47.130959	70.499892
865.484175	42.292570	70.504897
864.851640	49.937428	70.509902
864.092107	45.450471	70.514906
863.330896	37.314707	70.519911
862.061543	41.011303	70.524916
861.594820	36.092965	70.529921
860.912066	50.428957	70.534926
860.867100	42.458305	70.539930
860.524232	37.701603	70.544935
859.585416	46.415502	70.549940
858.795697	40.602402	70.554945
858.272454	51.295469	70.559950
857.652445	43.728586	70.564954
856.657254	41.196724	70.569959
855.680745	49.418308	70.574964
855.444607	44.122642	70.579969
854.984321	44.361504	70.584974
854.162381	47.739306	70.589978
853.352763	39.891948	70.594983
852.785284	44.501849	70.599988
852.640805	39.795569	70.604993
851.639515	43.458963	70.609998
850.684819	45.955879	70.615002
850.323739	38.459750	70.620007
849.589648	50.089974	70.625012
849.058010	43.183965	70.630017
848.006615	46.569908	70.635022
847.273073	44.989882	70.640026
847.066779	39.743086	70.645031
846.003218	47.950144	70.650036
844.959799	42.384014	70.655041
844.667896	45.997569	70.660046
844.064741	45.836550	70.665050
844.028885	43.282872	70.670055
843.114599	36.693246	70.675060
842.137384	39.930186	70.680065
841.805321	44.903161	70.685070
841.228715	39.861969	70.690074
840.379259	28.655741	70.695079
839.292895	40.501307	70.700084
838.962355	36.980557	70.705089
838.509213	43.210716	70.710094
837.358049	44.185609	70.715098
836.488918	42.374857	70.720103
835.837082	45.996823	70.725108
835.948608	33.951644	70.730113
835.301372	45.481308	70.735118
834.667649	44.596604	70.740122
833.843437	33.007887	70.745127
832.933330	41.878071	70.750132
832.530983	41.205695	70.755137
831.636514	43.746646	70.760142
830.939352	38.614261	70.765146
830.471913	33.700777	70.770151
829.951408	39.785540	70.775156
829.003183	41.380991	70.780161
827.967828	37.425236	70.785166
827.305351	39.259051	70.790170
827.139404	37.375790	70.795175
826.448176	31.343600	70.800180
825.676646	31.102156	70.805185
824.993729	37.895595	70.810190
824.107286	34.546920	70.815194
824.107153	34.889155	70.820199
823.237945	35.800246	70.825204
822.326414	40.736156	70.830209
822.112802	37.960041	70.835214
821.167285	46.067890	70.840218
820.177282	42.268921	70.845223
819.384332	46.031626	70.850228
819.078171	40.346568	70.855233
818.524786	37.446346	70.860238
818.134242	48.697032	70.865242
817.443615	46.779023	70.870247
816.505413	38.274059	70.875252
815.981994	40.178781	70.880257
814.910546	44.585064	70.885262
814.077435	55.333774	70.890266
813.591954	47.482136	70.895271
813.143336	51.320916	70.900276
813.061818	41.131003	70.905281
812.233485	38.460634	70.910286
810.928931	41.054258	70.915290
810.408564	31.550804	70.920295
810.076266	45.668580	70.925300
809.300013	38.471943	70.930305
808.928952	43.787021	70.935310
808.017397	46.423740	70.940314
807.426144	42.103981	70.945319
805.947801	52.187431	70.950324
805.559046	41.571765	70.955329
805.012190	37.536677	70.960334
804.546911	40.018773	70.965338
804.330019	39.775772	70.970343
803.586957	44.916682	70.975348
802.548289	44.411843	70.980353
802.161246	49.186995	70.985358
801.009781	48.597611	70.990362
800.319583	33.769008	70.995367
799.894517	45.357926	71.000372
799.560810	39.342942	71.005377
799.111872	29.485922	71.010382
797.864773	46.204651	71.015386
797.345915	38.826693	71.020391
796.435070	46.079050	71.025396
796.021596	44.459124	71.030401
795.283878	42.190650	71.035406
794.055518	46.057372	71.040410
793.533756	37.525546	71.045415
792.872890	45.841976	71.050420
792.729209	44.362027	71.055425
792.534515	45.208323	71.060430
791.822078	43.694341	71.065434
790.911084	30.164037	71.070439
790.066757	40.778909	71.075444
789.409038	38.776823	71.080449
788.776549	38.201018	71.085454
787.555195	47.647471	71.090458
787.375280	40.981954	71.095463
787.009168	42.604594	71.100468
786.496429	39.647446	71.105473
785.613575	39.909440	71.110478
784.955700	39.414948	71.115482
784.387047	34.456087	71.120487
782.815832	44.380863	71.125492
782.403664	37.126273	71.130497
781.765783	41.673277	71.135502
781.210748	43.359112	71.140506
781.344723	38.124384	71.145511
780.570083	42.358847	71.150516
779.650313	36.044512	71.155521
779.223560	40.991565	71.160526
777.948768	35.514346	71.165530
777.066160	31.151098	71.170535
776.541453	38.329366	71.175540
776.311741	37.135928	71.180545
775.999002	45.280241	71.185550
774.935020	42.560669	71.190554
774.329658	31.957428	71.195559
773.292731	50.210200	71.200564
773.058329	43.121273	71.205569
772.136156	46.100317	71.210574
771.123804	46.345086	71.215578
770.770875	44.784912	71.220583
770.056552	45.061080	71.225588
769.787977	44.537728	71.230593
769.337011	40.380148	71.235598
768.039767	43.661759	71.240602
767.981903	34.223453	71.245607
767.156730	43.901726	71.250612
765.804023	39.575478	71.255617
765.550820	37.453802	71.260622
764.943570	42.163089	71.265626
764.663263	36.513350	71.270631
763.804867	47.007470	71.275636
762.899208	33.728641	71.280641
762.576166	39.565932	71.285646
762.043107	34.707066	71.290650
760.978577	34.838722	71.295655
759.636198	42.208679	71.300660
759.467589	37.670257	71.305665
759.284314	41.107249	71.310670
758.479147	42.850260	71.315674
757.630151	40.397665	71.320679
756.734356	43.823523	71.325684
756.126120	38.937202	71.330689
756.195338	40.734963	71.335694
755.042306	44.340550	71.340698
754.454128	38.184742	71.345703
753.690407	41.587995	71.350708
753.409608	36.718929	71.355713
752.227777	37.542623	71.360718
751.544466	35.571431	71.365722
751.076437	40.633869	71.370727
750.568712	35.237962	71.375732
750.050290	41.716644	71.380737
749.369591	42.616669	71.385742
748.250899	46.923268	71.390746
748.009931	39.939471	71.395751
746.732978	43.749295	71.400756
745.976374	34.575209	71.405761
745.483443	38.998216	71.410766
744.893418	49.947929	71.415770
744.910586	32.127206	71.420775
744.098111	42.591937	71.425780
743.325431	35.501992	71.430785
742.863903	40.665898	71.435790
741.828826	42.226323	71.440794
741.021990	30.551306	71.445799
740.070076	38.660193	71.450804
739.472598	37.403890	71.455809
739.620681	28.692891	71.460814
738.626951	38.245040	71.465818
738.065631	41.664957	71.470823
736.803522	41.701925	71.475828
736.263345	45.921146	71.480833
736.264943	42.401144	71.485838
735.159834	37.436249	71.490842
734.583596	36.851501	71.495847
733.622649	38.278701	71.500852
733.284139	36.691006	71.505857
733.187233	31.934590	71.510862
731.900226	35.085277	71.515866
731.102639	29.300291	71.520871
730.438469	39.976376	71.525876
730.341709	33.144665	71.530881
729.179895	42.334076	71.535886
728.183483	50.489482	71.540890
727.776964	37.404004	71.545895
727.207205	39.435970	71.550900
727.138974	38.921723	71.555905
726.188225	44.791158	71.560910
725.304233	38.695076	71.565914
724.847461	31.789804	71.570919
723.794508	40.824687	71.575924
722.714491	39.482796	71.580929
722.452555	33.995720	71.585934
721.667359	29.954452	71.590938
721.339150	37.572947	71.595943
721.045006	46.832362	71.600948
720.551703	34.615418	71.605953
719.847330	27.642342	71.610958
718.736497	30.930562	71.615962
718.252831	24.559433	71.620967
717.503758	33.935434	71.625972
716.946223	32.371579	71.630977
716.599141	30.830984	71.635982
715.201648	40.627206	71.640986
714.646131	34.780024	71.645991
714.125300	38.302307	71.650996
713.888752	32.144140	71.656001
712.636714	37.071224	71.661006
711.858651	42.123112	71.666010
711.543616	34.769495	71.671015
710.902477	39.793271	71.676020
709.951673	36.008611	71.681025
709.266958	30.910558	71.686030
708.466017	31.027071	71.691034
708.264643	35.983975	71.696039
707.895427	35.815700	71.701044
706.975430	39.873054	71.706049
706.296092	27.269428	71.711054
705.664895	40.794550	71.716058
705.080892	31.730194	71.721063
704.048105	40.157898	71.726068
703.235202	41.108950	71.731073
703.030112	26.941164	71.736078
702.053926	34.456259	71.741082
701.173280	26.002116	71.746087
700.279317	34.639525	71.751092
700.031112	31.321732	71.756097
699.620690	34.804357	71.761102
699.256263	40.418008	71.766106
698.610567	27.048937	71.771111
697.690264	39.092028	71.776116
697.060921	36.246511	71.781121
696.783165	31.897366	71.786126
695.209512	40.832247	71.791130
694.896633	34.605812	71.796135
694.428981	40.005665	71.801140
693.696561	39.204524	71.806145
692.637553	32.390430	71.811150
691.400368	49.776245	71.816154
691.659519	27.479456	71.821159
690.947779	37.464530	71.826164
690.490263	37.433321	71.831169
690.245155	26.973020	71.836174
688.876263	39.650520	71.841178
688.239293	26.756303	71.846183
687.825240	31.460068	71.851188
687.162330	33.730802	71.856193
686.139052	27.335224	71.861198
685.367022	33.996222	71.866202
685.463797	31.747862	71.871207
684.495784	29.542907	71.876212
683.157961	36.710321	71.881217
682.915131	33.342788	71.886222
682.368539	41.410802	71.891226
682.325208	40.965132	71.896231
680.797394	35.793188	71.901236
680.194053	28.953847	71.906241
679.969376	31.517494	71.911246
679.148727	42.563860	71.916250
678.626697	32.010461	71.921255
677.499804	37.851188	71.926260
677.076042	42.458733	71.931265
676.846017	41.372588	71.936270
675.708095	43.518697	71.941274
675.266739	37.030450	71.946279
674.444012	32.697131	71.951284
673.886658	39.170983	71.956289
673.637036	35.596375	71.961294
672.566743	40.544998	71.966298
671.966036	35.960280	71.971303
671.181165	34.342753	71.976308
669.842552	41.663266	71.981313
669.387628	23.575549	71.986318
668.713839	46.797830	71.991322
668.582131	24.277864	71.996327
668.240690	40.374585	72.001332
667.449868	30.474277	72.006337
666.669012	35.190727	72.011342
666.039162	33.329318	72.016346
665.627471	21.556722	72.021351
664.379279	34.940404	72.026356
663.661648	25.591417	72.031361
663.112667	26.872610	72.036366
662.545175	35.778159	72.041370
662.224987	33.930515	72.046375
661.196115	34.436579	72.051380
660.741275	31.120159	72.056385
659.934075	31.865312	72.061390
659.191042	35.662686	72.066394
658.352347	34.626169	72.071399
657.524418	31.520553	72.076404
657.277226	36.688182	72.081409
657.148258	23.034990	72.086414
656.158865	34.958204	72.091418
655.453261	29.116021	72.096423
654.755442	36.859613	72.101428
653.854319	34.517861	72.106433
653.430125	25.035414	72.111438
652.163759	31.462910	72.116442
651.884670	28.034925	72.121447
651.768509	31.499077	72.126452
650.940642	38.881760	72.131457
650.218937	30.862795	72.136462
649.000147	40.137001	72.141466
648.847719	31.095394	72.146471
648.354896	27.833913	72.151476
647.229944	39.155826	72.156481
646.495368	26.531060	72.161486
645.958971	34.841879	72.166490
646.031279	25.064319	72.171495
644.611965	33.112051	72.176500
643.791662	32.192458	72.181505
643.688556	33.216565	72.186510
643.054618	44.517055	72.191514
642.176290	26.939900	72.196519
641.068844	33.474555	72.201524
640.849145	37.876139	72.206529
640.482673	33.826559	72.211534
639.111880	35.279642	72.216538
638.246905	34.639978	72.221543
638.020279	36.547927	72.226548
637.113972	37.897074	72.231553
637.110959	28.369629	72.236558
636.254872	42.130848	72.241562
635.542195	33.545900	72.246567
634.577858	36.206851	72.251572
634.218505	35.630164	72.256577
633.983806	29.977917	72.261582
632.638157	37.987117	72.266586
632.048090	36.731238	72.271591
631.577373	31.627513	72.276596
631.029506	29.559092	72.281601
630.748684	27.583758	72.286606
629.479764	41.910622	72.291610
628.981888	35.272117	72.296615
628.597475	44.840799	72.301620
627.658612	33.112742	72.306625
627.104822	25.190048	72.311630
626.226337	41.424340	72.316634
625.706307	40.524738	72.321639
624.790275	34.455881	72.326644
623.973905	37.657818	72.331649
623.922719	34.291309	72.336654
623.094559	40.514988	72.341658
622.148440	28.701361	72.346663
621.480775	34.325465	72.351668
620.901618	34.556493	72.356673
620.923500	36.811217	72.361678
619.501829	34.590233	72.366682
618.866319	24.308822	72.371687
618.316595	39.981398	72.376692
617.598927	29.200560	72.381697
616.819009	27.976501	72.386702
615.967665	34.121869	72.391706
615.527695	36.967393	72.396711
615.210742	40.285333	72.401716
614.716791	37.680049	72.406721
613.641594	30.955305	72.411726
612.902149	43.308659	72.416730
612.430040	42.270540	72.421735
611.957920	30.114917	72.426740
610.878869	37.923969	72.431745
610.290309	32.670285	72.436750
609.539431	30.818706	72.441754
609.328919	33.750686	72.446759
608.623054	37.332419	72.451764
607.574276	32.106305	72.456769
607.367477	33.747747	72.461774
606.585899	41.932046	72.466778
605.732142	39.456612	72.471783
605.019538	31.004129	72.476788
604.296104	34.634393	72.481793
604.267577	34.069672	72.486798
603.016769	38.646527	72.491802
602.351735	31.763419	72.496807
602.179556	37.262878	72.501812
601.113763	35.619156	72.506817
599.993153	34.760025	72.511822
599.207584	40.391877	72.516826
598.893764	37.783136	72.521831
598.628413	38.453042	72.526836
598.152922	38.282788	72.531841
598.040742	32.689879	72.536846
596.290307	35.266319	72.541850
596.022277	35.671724	72.546855
595.362333	35.977127	72.551860
594.393954	37.148519	72.556865
593.917845	41.031128	72.561870
593.226783	46.431889	72.566874
592.889621	37.760334	72.571879
592.024760	40.485882	72.576884
590.975950	37.355547	72.581889
590.562355	31.909997	72.586894
589.863650	39.018234	72.591898
589.374693	37.027171	72.596903
588.315465	34.248581	72.601908
587.569588	41.086789	72.606913
587.064442	28.376618	72.611918
586.635733	42.136005	72.616922
586.723914	31.772445	72.621927
585.486097	36.085464	72.626932
584.276277	41.917361	72.631937
584.215184	28.221829	72.636942
583.078703	38.629391	72.641946
582.432080	39.259105	72.646951
581.684400	43.309553	72.651956
581.055189	38.600091	72.656961
581.405710	30.974910	72.661966
579.996712	34.919384	72.666970
579.534611	37.448317	72.671975
578.903795	41.371341	72.676980
578.104735	41.028704	72.681985
577.208684	37.337880	72.686990
576.051188	50.599928	72.691994
575.709779	41.624699	72.696999
575.295428	47.910212	72.702004
574.949078	37.145933	72.707009
574.479125	36.752451	72.712014
573.550457	41.073004	72.717018
573.011693	44.120352	72.722023
572.203692	40.057536	72.727028
571.081954	44.359959	72.732033
570.463606	31.305124	72.737038
569.901076	41.928774	72.742042
569.349288	43.700867	72.747047
569.029062	36.676112	72.752052
567.933702	41.255031	72.757057
567.477051	31.257380	72.762062
566.897045	49.820611	72.767066
566.378384	45.334815	72.772071
565.694802	39.612153	72.777076
564.740909	43.894150	72.782081
564.207736	34.812280	72.787086
563.696777	47.742683	72.792090
562.685318	40.304488	72.797095
562.040187	45.005657	72.802100
561.219670	46.397935	72.807105
561.141950	43.070348	72.812110
560.209560	47.599657	72.817114
559.324211	39.622558	72.822119
558.716904	39.608927	72.827124
558.213608	40.958559	72.832129
558.201425	34.200128	72.837134
556.580690	38.328153	72.842138
555.810594	32.026346	72.847143
555.756375	37.007121	72.852148
555.072295	43.870187	72.857153
554.598346	42.830795	72.862158
553.495016	48.529050	72.867162
553.002214	46.376180	72.872167
552.471475	46.664166	72.877172
551.074152	46.976657	72.882177
550.968778	37.317287	72.887182
549.956521	42.983687	72.892186
549.701635	39.072466	72.897191
549.674248	41.746621	72.902196
548.497045	34.506726	72.907201
547.748909	34.581763	72.912206
547.167016	41.904790	72.917210
546.272708	30.932923	72.922215
545.428080	41.790747	72.927220
544.591269	47.613705	72.932225
544.378563	43.506530	72.937230
543.928860	47.222517	72.942234
543.314932	43.739075	72.947239
542.508245	41.046431	72.952244
541.428704	48.570163	72.957249
541.295110	43.956800	72.962254
540.047505	43.933210	72.967258
539.274026	47.847432	72.972263
538.909506	41.873678	72.977268
538.197728	46.924514	72.982273
538.248113	43.694792	72.987278
537.455201	46.147122	72.992282
536.446141	48.357920	72.997287
536.068475	41.908445	73.002292
534.907727	49.490848	73.007297
534.360707	44.254218	73.012302
533.620273	44.525152	73.017306
533.314716	36.428895	73.022311
532.946618	38.373581	73.027316
531.403491	48.423326	73.032321
530.953960	41.430214	73.037326
530.260181	47.717668	73.042330
530.111208	41.070913	73.047335
529.188490	34.358190	73.052340
527.943527	31.736950	73.057345
527.628950	36.088997	73.062350
527.277934	44.949045	73.067354
527.067280	41.484942	73.072359
526.174934	37.634276	73.077364
525.175474	40.884334	73.082369
524.900073	33.500789	73.087374
523.551463	47.618041	73.092378
522.531078	41.791354	73.097383
522.374246	43.355457	73.102388
521.630828	50.719994	73.107393
521.427218	39.070396	73.112398
520.806728	44.447313	73.117402
520.216569	45.918024	73.122407
519.733210	42.006934	73.127412
518.703932	45.988721	73.132417
518.119794	32.786530	73.137422
517.196171	38.079274	73.142426
516.666593	41.766987	73.147431
516.150894	36.175293	73.152436
514.984613	43.123072	73.157441
514.682231	35.226586	73.162446
514.199752	36.814183	73.167450
513.443787	38.525775	73.172455
512.583832	35.814820	73.177460
511.520743	41.025707	73.182465
511.383869	32.153533	73.187470
510.911631	34.936403	73.192474
510.058116	38.566915	73.197479
509.156861	42.201879	73.202484
508.478327	41.013741	73.207489
508.232483	42.688220	73.212494
507.496614	39.968536	73.217498
506.181277	45.353655	73.222503
505.988984	36.994931	73.227508
505.132131	41.401836	73.232513
504.694441	33.911685	73.237518
504.256338	38.795923	73.242522
503.585128	41.386569	73.247527
502.918248	36.184816	73.252532
502.011850	48.301440	73.257537
501.948632	45.927177	73.262542
500.872579	48.650132	73.267546
500.025359	38.511294	73.272551
499.678925	44.243521	73.277556
498.201424	44.450544	73.282561
497.568111	39.741761	73.287566
497.381458	37.074929	73.292570
497.142691	49.693891	73.297575
496.731504	43.506808	73.302580
495.367914	46.121033	73.307585
494.682170	36.798564	73.312590
494.198338	45.488963	73.317594
493.834178	40.390369	73.322599
492.985234	34.165802	73.327604
491.936833	40.227485	73.332609
491.803177	41.966092	73.337614
490.995579	39.879161	73.342618
489.868447	40.998614	73.347623
489.240202	34.852426	73.352628
488.810953	43.704438	73.357633
488.652030	31.186719	73.362638
487.868865	39.707186	73.367642
486.610399	41.427883	73.372647
486.230528	34.821078	73.377652
485.516686	44.650410	73.382657
484.829749	29.793046	73.387662
483.831987	27.220755	73.392666
483.119033	37.578219	73.397671
483.234798	37.252284	73.402676
482.396692	44.378024	73.407681
481.969148	42.025539	73.412686
480.774828	39.356830	73.417690
480.430094	43.205911	73.422695
479.986641	39.006200	73.427700
478.405652	37.479309	73.432705
478.052635	42.760002	73.437710
477.378950	49.913165	73.442714
477.230627	44.226676	73.447719
476.776089	39.530416	73.452724
475.530107	43.505744	73.457729
475.044622	44.912478	73.462734
474.309379	39.663279	73.467738
473.501147	49.819891	73.472743
473.090983	39.720239	73.477748
472.319624	42.232232	73.482753
471.620624	43.281903	73.487758
471.176280	33.058392	73.492762
470.170696	37.544196	73.497767
470.017180	34.791664	73.502772
469.005676	42.697238	73.507777
468.681201	39.382165	73.512782
467.474595	44.380971	73.517786
466.374625	41.109034	73.522791
466.407181	36.421900	73.527796
465.502069	39.538676	73.532801
465.552492	37.447508	73.537806
464.653489	39.970378	73.542810
463.548361	43.929577	73.547815
463.338365	42.709376	73.552820
462.753571	45.081260	73.557825
461.925241	40.056631	73.562830
461.131974	41.865644	73.567834
460.542855	33.499196	73.572839
459.838117	36.536739	73.577844
458.791389	49.719673	73.582849
458.298670	39.309904	73.587854
457.585555	44.550204	73.592858
457.284573	43.380771	73.597863
457.229605	43.370621	73.602868
455.679908	46.129638	73.607873
455.046884	33.867237	73.612878
454.438180	39.147670	73.617882
453.799234	37.103265	73.622887
452.907619	37.819356	73.627892
452.135511	39.785849	73.632897
451.646612	37.220798	73.637902
451.105025	35.386385	73.642906
451.153076	38.734489	73.647911
450.345813	32.799765	73.652916
449.166423	40.066623	73.657921
449.044547	31.436496	73.662926
447.920319	42.278969	73.667930
447.040133	41.804222	73.672935
446.731058	33.774777	73.677940
446.198802	46.257572	73.682945
445.112875	41.743926	73.687950
444.315845	39.514978	73.692954
444.130427	43.740798	73.697959
443.660753	32.485276	73.702964
442.590961	40.015370	73.707969
442.047275	29.673659	73.712974
441.391720	35.579722	73.717978
440.545289	29.137159	73.722983
439.722779	27.860020	73.727988
438.734633	38.409575	73.732993
438.509316	31.417035	73.737998
438.016844	34.960076	73.743002
437.779126	32.545815	73.748007
437.180441	34.503602	73.753012
435.910919	35.765616	73.758017
435.726856	28.067916	73.763022
434.738864	33.484482	73.768026
433.327506	37.736914	73.773031
433.102542	38.256899	73.778036
431.995810	38.236147	73.783041
431.944469	37.690834	73.788046
432.039620	33.928859	73.793050
431.139984	41.453921	73.798055
430.207938	38.773408	73.803060
429.122599	41.595641	73.808065
429.033872	30.963818	73.813070
428.090037	31.956319	73.818074
427.072187	30.793890	73.823079
426.657715	29.907473	73.828084
426.312382	39.813709	73.833089
425.659806	29.580818	73.838094
424.986963	38.940001	73.843098
424.370184	38.120515	73.848103
424.070563	29.439868	73.853108
422.683276	35.079337	73.858113
422.047948	36.431111	73.863118
421.348302	33.909111	73.868122
420.757965	42.480869	73.873127
419.929634	30.432532	73.878132
419.011985	38.802557	73.883137
418.600399	31.729316	73.888142
417.952392	38.727007	73.893146
417.710646	34.438399	73.898151
417.674896	34.374725	73.903156
416.162513	38.737882	73.908161
415.538655	32.643059	73.913166
415.099925	35.819573	73.918170
414.060692	36.310043	73.923175
413.587012	34.991518	73.928180
413.083925	39.925547	73.933185
412.453709	45.337151	73.938190
411.588194	35.956629	73.943194
410.525063	43.042552	73.948199
410.389639	32.134322	73.953204
409.584568	36.220766	73.958209
409.057639	42.085841	73.963214
408.156227	31.525178	73.968218
407.237639	37.113621	73.973223
407.151544	30.548331	73.978228
406.475143	34.932815	73.983233
405.635828	36.572564	73.988238
405.021646	31.952226	73.993242
404.177000	36.741989	73.998247
403.909731	32.859573	74.003252
402.963582	40.712175	74.008257
402.178679	39.017472	74.013262
401.720807	31.107944	74.018266
401.382913	41.574390	74.023271
400.508861	29.173805	74.028276
399.597946	34.333673	74.033281
398.855415	37.659528	74.038286
398.469648	36.655002	74.043290
397.713693	33.148506	74.048295
397.091209	26.335962	74.053300
395.993304	36.860441	74.058305
395.613768	31.370084	74.063310
395.487378	32.743261	74.068314
394.511966	34.366856	74.073319
393.639242	33.613396	74.078324
393.087394	35.939042	74.083329
392.545483	30.625950	74.088334
391.645935	30.999552	74.093338
390.555596	43.716365	74.098343
390.704156	33.734281	74.103348
390.002583	34.377531	74.108353
388.963912	35.542856	74.113358
387.918629	35.621141	74.118362
387.122113	34.358801	74.123367
387.108895	32.288814	74.128372
386.577455	40.795996	74.133377
386.633134	36.876308	74.138382
385.564961	27.187479	74.143386
384.625970	36.742046	74.148391
384.365264	30.387511	74.153396
382.878471	34.838071	74.158401
382.123087	34.302458	74.163406
381.676537	32.814037	74.168410
381.382335	37.687972	74.173415
380.988435	35.492572	74.178420
379.738524	39.339260	74.183425
379.304591	34.805320	74.188430
378.737816	35.129048	74.193434
377.303560	37.896521	74.198439
376.849143	24.880299	74.203444
376.149731	33.475748	74.208449
375.666968	35.001914	74.213454
375.423947	29.054569	74.218458
375.084806	37.802340	74.223463
374.237617	28.194993	74.228468
373.434717	44.139744	74.233473
372.968537	34.143668	74.238478
372.406246	36.360596	74.243482
371.030848	43.931536	74.248487
370.406755	32.331642	74.253492
369.967262	33.797296	74.258497
369.300151	39.210056	74.263502
368.577534	34.846705	74.268506
367.756400	37.705703	74.273511
367.350212	29.485175	74.278516
366.884346	42.514054	74.283521
366.201610	34.566254	74.288526
365.289600	33.087363	74.293530
364.416591	35.520969	74.298535
364.260742	32.164848	74.303540
363.525030	31.626106	74.308545
362.329646	33.387272	74.313550
361.889119	30.283102	74.318554
361.337781	34.501008	74.323559
361.169164	27.027939	74.328564
359.996343	35.394492	74.333569
359.170561	36.727749	74.338574
358.969448	31.557469	74.343578
358.014518	38.365968	74.348583
357.175237	29.291953	74.353588
356.664757	39.566708	74.358593
356.144296	31.619859	74.363598
356.065459	36.341201	74.368602
355.118434	38.613142	74.373607
354.216476	25.723447	74.378612
353.456006	38.077035	74.383617
352.454052	32.206495	74.388622
351.774718	34.035229	74.393626
350.855471	26.377446	74.398631
350.709249	38.101706	74.403636
350.211082	35.932392	74.408641
349.888750	36.595634	74.413646
349.319204	33.895227	74.418650
348.144011	36.129420	74.423655
347.887631	28.268219	74.428660
346.839059	42.455986	74.433665
345.467072	41.545574	74.438670
345.413630	34.970354	74.443674
344.802888	35.435137	74.448679
344.817696	34.133388	74.453684
343.908852	28.076126	74.458689
342.725088	31.018158	74.463694
342.423181	36.577718	74.468698
341.696308	32.707063	74.473703
340.667815	35.069264	74.478708
339.918398	24.615302	74.483713
339.497378	25.410968	74.488718
339.289967	23.654208	74.493722
337.959717	38.659571	74.498727
337.096298	33.005077	74.503732
336.738006	35.098035	74.508737
336.274212	27.854942	74.513742
336.149908	26.151168	74.518746
335.198436	30.432853	74.523751
334.316927	21.340352	74.528756
333.736662	27.570323	74.533761
333.117573	32.115998	74.538766
332.476115	28.572353	74.543770
331.268299	32.295658	74.548775
330.835628	29.791059	74.553780
330.656152	37.594024	74.558785
330.032052	44.815003	74.563790
329.080753	40.254725	74.568794
328.465526	43.921430	74.573799
327.812860	31.460362	74.578804
326.295127	33.099459	74.583809
326.144148	36.014080	74.588814
325.495922	36.601537	74.593818
324.910253	41.197083	74.598823
324.543171	39.369578	74.603828
324.457266	33.834012	74.608833
323.110825	42.721840	74.613838
322.590485	39.726591	74.618842
321.707492	35.477127	74.623847
320.813866	34.999838	74.628852
320.203573	38.656295	74.633857
319.465144	30.250616	74.638862
319.518991	27.830898	74.643866
318.580700	37.014790	74.648871
317.780245	27.521445	74.653876
317.137438	38.479612	74.658881
316.537670	34.858363	74.663886
316.282452	27.798072	74.668890
314.809207	42.487197	74.673895
314.383007	31.492868	74.678900
313.924923	45.349985	74.683905
313.054495	33.261099	74.688910
312.260448	35.100243	74.693914
311.372553	32.207739	74.698919
311.187778	36.964889	74.703924
310.961960	31.060543	74.708929
310.149388	38.762571	74.713934
309.627863	30.230860	74.718938
308.477954	36.658869	74.723943
308.112423	32.547703	74.728948
306.974340	34.659305	74.733953
305.970920	38.939821	74.738958
306.186143	36.470725	74.743962
305.421558	38.180597	74.748967
305.093674	28.897357	74.753972
303.597171	32.092682	74.758977
302.932650	34.073608	74.763982
302.981885	27.519875	74.768986
301.893106	24.132698	74.773991
300.999620	29.814940	74.778996
300.443163	39.696485	74.784001
300.008535	37.837174	74.789006
299.518671	39.422833	74.794010
298.485833	37.740877	74.799015
298.081756	34.049017	74.804020
297.239841	33.238643	74.809025
296.721243	25.286788	74.814030
296.558972	25.607557	74.819034
295.144982	37.259507	74.824039
294.666728	28.687788	74.829044
294.304821	37.661539	74.834049
293.373138	34.627789	74.839054
292.647196	23.575597	74.844058
291.754177	34.814922	74.849063
291.635262	22.540030	74.854068
290.401998	35.743271	74.859073
289.483614	32.352590	74.864078
289.594670	24.715106	74.869082
288.782641	35.490515	74.874087
288.524740	33.811193	74.879092
287.113198	28.302441	74.884097
286.260771	31.177489	74.889102
286.139352	26.406100	74.894106
285.567791	37.042256	74.899111
285.208660	29.503373	74.904116
284.156076	24.576067	74.909121
283.161505	30.518854	74.914126
283.051801	22.817214	74.919130
282.105898	31.570243	74.924135
281.208271	28.911114	74.929140
280.559482	22.036572	74.934145
280.174324	37.903700	74.939150
279.875783	27.463043	74.944154
279.025948	37.590051	74.949159
278.322330	37.270145	74.954164
277.615736	37.762840	74.959169
277.029462	32.477351	74.964174
275.949759	30.470142	74.969178
275.168623	34.062378	74.974183
274.788949	28.065872	74.979188
274.443122	36.209164	74.984193
273.631479	34.192340	74.989198
272.779606	26.482852	74.994202
272.063562	28.992390	74.999207
271.648780	25.593978	75.004212
271.123789	32.417543	75.009217
270.247601	33.181701	75.014222
269.879274	30.998016	75.019226
269.102242	35.830656	75.024231
268.493294	27.927903	75.029236
267.341862	29.786185	75.034241
266.556765	33.282861	75.039246
266.545629	28.077580	75.044250
265.605509	36.883312	75.049255
264.931208	24.342147	75.054260
264.402569	29.325999	75.059265
263.721182	31.233929	75.064270
263.317660	31.796585	75.069274
261.923000	34.434808	75.074279
261.530450	34.426438	75.079284
261.027951	24.510308	75.084289
260.559562	35.735565	75.089294
259.468973	34.376645	75.094298
258.554016	34.752752	75.099303
257.953386	30.365263	75.104308
257.686485	31.303531	75.109313
257.386112	32.355943	75.114318
256.540437	27.752055	75.119322
255.672491	40.857651	75.124327
255.123317	32.577943	75.129332
254.859270	32.903902	75.134337
253.568596	31.160569	75.139342
253.084346	28.195856	75.144346
252.532308	30.442712	75.149351
251.686037	29.257736	75.154356
250.627289	27.896899	75.159361
250.053015	31.762091	75.164366
250.100772	27.421050	75.169370
249.413617	27.070143	75.174375
248.612172	29.577532	75.179380
247.726778	30.936097	75.184385
246.862198	36.558556	75.189390
246.746032	25.117437	75.194394
245.714086	30.102682	75.199399
244.959006	32.738299	75.204404
244.519692	25.910796	75.209409
243.712727	29.422003	75.214414
243.476285	31.150196	75.219418
242.334972	34.042928	75.224423
241.619155	35.219921	75.229428
241.193204	39.014162	75.234433
240.634780	42.372210	75.239438
239.875512	36.587610	75.244442
238.777601	37.937482	75.249447
238.363620	44.588818	75.254452
238.256516	34.239071	75.259457
237.484027	32.463598	75.264462
236.734867	33.603330	75.269466
236.173873	34.713064	75.274471
235.240572	39.676282	75.279476
234.420639	38.237955	75.284481
233.643311	41.359668	75.289486
233.295474	40.366468	75.294490
232.727764	45.503216	75.299495
232.038510	37.360962	75.304500
231.141854	27.567603	75.309505
230.510390	40.466769	75.314510
230.363431	31.282435	75.319514
229.212744	34.973024	75.324519
228.267582	30.832859	75.329524
227.839537	34.162236	75.334529
227.113017	39.333763	75.339534
227.175982	39.085621	75.344538
226.163949	26.465851	75.349543
225.282823	28.985950	75.354548
225.024640	30.386452	75.359553
223.799685	36.854845	75.364558
223.023070	21.713861	75.369562
222.359015	33.460742	75.374567
221.564930	26.293994	75.379572
221.753281	22.384700	75.384577
221.254281	23.435667	75.389582
220.117350	28.611123	75.394586
219.405111	31.949541	75.399591
218.808002	23.726377	75.404596
218.137290	30.784491	75.409601
216.913926	41.105108	75.414606
216.829712	34.350304	75.419610
215.978553	34.743063	75.424615
215.789883	28.323458	75.429620
214.842927	35.681082	75.434625
213.760592	44.586777	75.439630
213.558180	31.848967	75.444634
212.677741	34.685928	75.449639
212.407592	41.915149	75.454644
211.311793	39.170948	75.459649
210.524225	39.503108	75.464654
210.627726	29.646491	75.469658
209.316989	40.438355	75.474663
208.176926	36.941125	75.479668
207.716208	35.584307	75.484673
207.210774	45.227498	75.489678
206.962771	30.022733	75.494682
206.577853	37.200865	75.499687
205.968073	27.289240	75.504692
205.155374	44.771521	75.509697
204.285901	34.778295	75.514702
203.638996	37.951761	75.519706
202.397104	38.298013	75.524711
202.018431	32.332900	75.529716
201.716974	33.980000	75.534721
200.980789	40.436706	75.539726
200.239826	39.334304	75.544730
199.183077	39.259957	75.549735
198.840552	30.352813	75.554740
198.634274	33.377178	75.559745
198.008346	40.585855	75.564750
197.073023	31.740109	75.569754
196.128544	38.012408	75.574759
195.597826	32.983013	75.579764
194.778827	32.963800	75.584769
193.891293	39.334253	75.589774
193.350640	32.100297	75.594778
192.748083	31.075178	75.599783
192.583127	36.887300	75.604788
192.023257	26.702796	75.609793
190.575425	33.304508	75.614798
190.526720	25.820231	75.619802
189.880106	36.055205	75.624807
188.877717	35.156915	75.629812
188.064439	30.232498	75.634817
187.665967	33.356894	75.639822
187.379144	22.748815	75.644826
186.308623	36.291996	75.649831
185.284629	37.330485	75.654836
184.822617	30.653271	75.659841
183.939018	39.795365	75.664846
183.915365	30.132488	75.669850
183.452876	31.584493	75.674855
182.815118	32.152971	75.679860
181.952524	34.160778	75.684865
181.030107	35.536308	75.689870
180.252915	36.451870	75.694874
179.537226	29.299445	75.699879
179.003421	35.214532	75.704884
178.850083	32.083533	75.709889
177.974053	34.752646	75.714894
177.402554	29.945800	75.719898
176.874486	34.582650	75.724903
175.731405	31.141112	75.729908
175.139661	29.887194	75.734913
174.396092	31.716753	75.739918
174.062134	28.430053	75.744922
172.853257	27.272960	75.749927
172.088334	33.106629	75.754932
171.589161	39.631206	75.759937
171.190973	33.763827	75.764942
170.888907	26.572263	75.769946
170.038878	38.027113	75.774951
169.031592	31.206613	75.779956
168.705630	25.691996	75.784961
168.052560	33.531048	75.789966
167.180775	32.340708	75.794970
166.102081	36.308426	75.799975
165.828811	31.138641	75.804980
165.314913	29.173727	75.809985
164.653533	36.061633	75.814990
163.787495	31.131446	75.819994
162.793216	35.508325	75.824999
162.709927	37.273605	75.830004
162.307052	37.314205	75.835009
160.961993	37.918202	75.840014
160.559605	27.363246	75.845018
159.940137	46.016353	75.850023
159.560967	37.286944	75.855028
158.816903	35.063843	75.860033
157.679200	38.507968	75.865038
157.441768	29.629807	75.870042
156.654379	37.569129	75.875047
155.978607	35.494411	75.880052
155.320991	23.182442	75.885057
154.489354	31.584553	75.890062
154.378521	35.625022	75.895066
153.237634	40.250787	75.900071
152.464217	45.555967	75.905076
151.904696	35.100181	75.910081
151.450930	42.002295	75.915086
151.001178	28.025041	75.920090
149.931393	29.789932	75.925095
149.318735	36.964961	75.930100
148.663591	28.356836	75.935105
148.218083	36.328375	75.940110
147.441727	35.031362	75.945114
146.709599	37.023108	75.950119
145.800743	40.416553	75.955124
145.449001	28.420083	75.960129
145.037270	32.092220	75.965134
143.782831	36.239358	75.970138
143.299922	33.078915	75.975143
142.741865	27.861508	75.980148
142.398490	29.097408	75.985153
141.355204	35.210439	75.990158
140.569079	32.744895	75.995162
140.025733	33.618448	76.000167
139.758933	32.292222	76.005172
139.043684	30.969698	76.010177
137.948967	38.592182	76.015182
137.743818	27.715622	76.020186
137.044275	34.672696	76.025191
136.079678	37.535718	76.030196
135.868893	33.969186	76.035201
134.732338	32.269150	76.040206
134.393363	36.733928	76.045210
133.152266	44.245719	76.050215
132.745987	27.383618	76.055220
132.495110	26.614668	76.060225
131.715370	44.148473	76.065230
130.893946	33.597266	76.070234
130.186037	33.555629	76.075239
129.425432	36.911245	76.080244
129.157408	30.073801	76.085249
127.855106	37.915471	76.090254
127.496333	29.247477	76.095258
126.546677	28.071147	76.100263
126.152890	28.070881	76.105268
126.059303	26.977230	76.110273
125.056642	34.613421	76.115278
123.983342	24.755245	76.120282
123.660809	29.009243	76.125287
123.070106	37.623677	76.130292
122.392521	26.223223	76.135297
121.324460	34.352389	76.140302
120.993914	29.795714	76.145306
120.550743	30.665912	76.150311
119.396209	32.977337	76.155316
118.811695	28.543166	76.160321
118.017543	38.440560	76.165326
117.943331	28.959217	76.170330
117.667952	35.766652	76.175335
116.162326	33.745439	76.180340
116.007893	33.615541	76.185345
115.081100	38.610876	76.190350
114.267572	31.046726	76.195354
113.340105	30.915529	76.200359
112.572607	23.900704	76.205364
112.735638	33.468832	76.210369
111.825959	32.292440	76.215374
110.987005	33.694109	76.220378
110.339141	31.602339	76.225383
109.762247	41.573899	76.230388
109.481804	26.489455	76.235393
108.402688	33.030831	76.240398
107.583548	36.498289	76.245402
107.074551	32.378503	76.250407
106.432221	31.793408	76.255412
105.779183	33.876630	76.260417
104.482498	36.015192	76.265422
104.159645	32.195302	76.270426
103.974366	30.742540	76.275431
103.477439	31.780584	76.280436
102.857750	31.436306	76.285441
101.543765	29.009227	76.290446
101.119122	26.560166	76.295450
100.854188	37.317751	76.300455
99.677464	42.688841	76.305460
98.943940	29.930105	76.310465
98.169658	35.785786	76.315470
98.025466	22.638182	76.320474
97.630206	27.462018	76.325479
96.081651	42.748295	76.330484
96.066382	29.040810	76.335489
95.367165	33.365925	76.340494
94.722905	27.160922	76.345498
93.564645	30.524773	76.350503
92.850943	38.326203	76.355508
92.554456	32.814781	76.360513
92.349184	34.560092	76.365518
91.535114	29.260528	76.370522
90.527689	35.875633	76.375527
89.919868	41.061378	76.380532
89.388620	22.683287	76.385537
88.472701	33.667693	76.390542
87.872059	25.523983	76.395546
87.827171	23.413326	76.400551
86.801032	30.073991	76.405556
85.832498	28.355067	76.410561
85.256831	37.859657	76.415566
84.698868	31.636162	76.420570
84.034059	30.758193	76.425575
82.919492	35.854447	76.430580
82.714224	27.754913	76.435585
81.912105	30.322383	76.440590
81.680598	34.864642	76.445594
80.615651	31.369691	76.450599
79.713320	26.787525	76.455604
79.833318	31.234298	76.460609
78.935634	31.945182	76.465614
77.856734	31.134835	76.470618
77.295366	28.885779	76.475623
76.747752	25.521209	76.480628
76.217081	34.700079	76.485633
75.161280	34.668212	76.490638
74.337142	33.691080	76.495642
73.664837	28.225411	76.500647
73.313097	35.008756	76.505652
73.495890	17.022994	76.510657
72.225001	27.387507	76.515662
71.616203	24.318123	76.520666
71.094452	26.173834	76.525671
69.644811	28.861929	76.530676
69.164522	27.068295	76.535681
68.306552	33.036677	76.540686
68.082092	22.005522	76.545690
67.804737	29.496086	76.550695
67.039857	34.935540	76.555700
66.274454	31.313973	76.560705
65.448996	33.651785	76.565710
65.163604	28.676337	76.570714
64.093602	29.343748	76.575719
62.875326	27.910669	76.580724
62.581071	26.513139	76.585729
62.135191	35.478216	76.590734
61.612785	32.220014	76.595738
61.410667	31.722414	76.600743
60.046177	31.258821	76.605748
59.708706	30.032185	76.610753
58.910686	33.993025	76.615758
58.170030	33.616013	76.620762
57.469174	25.936148	76.625767
56.430224	25.245594	76.630772
56.394794	31.003939	76.635777
55.504758	32.688161	76.640782
54.979307	30.386073	76.645786
53.990168	28.195790	76.650791
53.422135	28.803642	76.655796
53.366574	23.163918	76.660801
52.707911	36.625677	76.665806
51.500447	27.594755	76.670810
50.910509	33.063079	76.675815
50.317133	40.048971	76.680820
49.910984	32.006711	76.685825
48.721789	32.303636	76.690830
48.327954	36.419206	76.695834
47.853457	34.593113	76.700839
46.647167	39.869592	76.705844
46.426303	25.912638	76.710849
45.617024	31.031174	76.715854
45.071988	20.262468	76.720858
44.973066	29.802979	76.725863
43.800712	32.992483	76.730868
43.459564	31.238161	76.735873
42.407486	38.279871	76.740878
41.117536	28.680220	76.745882
40.893271	26.052554	76.750887
40.416659	33.631673	76.755892
40.229696	23.775671	76.760897
38.844066	32.258290	76.765902
37.999600	31.613993	76.770906
37.623249	35.163808	76.775911
37.173806	29.935413	76.780916
36.557082	29.261099	76.785921
35.509195	33.733306	76.790926
34.785605	26.178500	76.795930
34.267015	30.854860	76.800935
33.708327	28.520233	76.805940
33.613639	25.498164	76.810945
32.671955	34.201709	76.815950
31.986600	29.113447	76.820954
31.526171	33.167102	76.825959
30.143985	39.033036	76.830964
29.655163	28.204900	76.835969
29.071197	35.859492	76.840974
28.722760	24.259920	76.845978
28.149020	29.981128	76.850983
26.768335	33.624913	76.855988
26.440849	22.326351	76.860993
25.700467	30.431665	76.865998
25.381563	27.079511	76.871002
24.516989	20.067591	76.876007
23.577305	24.606119	76.881012
23.245318	26.299106	76.886017
22.686030	33.568143	76.891022
22.375274	26.504149	76.896026
21.241756	32.754617	76.901031
20.612718	37.295636	76.906036
20.286173	30.754550	76.911041
19.074690	33.187067	76.916046
18.428007	36.142922	76.921050
17.630912	32.914355	76.926055
17.194198	38.071242	76.931060
17.033880	28.553187	76.936065
15.918864	30.244925	76.941070
15.147824	23.290627	76.946074
14.668731	31.070415	76.951079
13.820852	32.134497	76.956084
12.795737	20.852606	76.961089
12.278584	28.408230	76.966094
11.700641	24.588049	76.971098
11.375385	28.446680	76.976103
10.872956	23.557904	76.981108
10.689178	24.957595	76.986113
9.368543	30.287019	76.991118
8.877379	31.748360	76.996122
8.013025	28.262446	77.001127
6.785662	26.591151	77.006132
6.674799	27.162356	77.011137
6.171149	22.918745	77.016142
5.907249	28.691454	77.021147
4.670092	30.801647	77.026151
3.703197	31.198749	77.031156
3.576208	24.177986	77.036161