Fri Mar 05 20:13:44 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.764903	100.363130	0.000000
-1.897583	92.050135	0.005005
-2.186416	48.003244	0.010010
-4.332993	16.582885	0.015014
-7.711676	-17.230209	0.020019
-13.031449	-16.556711	0.025024
-18.899012	-19.716088	0.030029
-23.100651	-19.654576	0.035034
-27.259659	-11.294136	0.040038
-31.028283	-9.032469	0.045043
-34.326522	-14.631164	0.050048
-38.176234	-12.399129	0.055053
-41.905003	-15.852312	0.060058
-45.601652	-13.613143	0.065062
-49.270221	-15.576251	0.070067
-53.172933	-14.917405	0.075072
-57.114678	-5.446716	0.080077
-60.608649	-18.969789	0.085082
-64.523461	0.525927	0.090086
-68.482370	-22.608504	0.095091
-71.995771	-18.553516	0.100096
-75.834594	-17.624131	0.105101
-79.440246	-21.287703	0.110106
-83.203265	-15.431441	0.115110
-86.801448	-15.332051	0.120115
-90.321835	-17.200465	0.125120
-94.285535	-17.131059	0.130125
-98.273978	-18.797057	0.135130
-102.124378	-17.648167	0.140134
-105.809838	-16.284315	0.145139
-109.362481	-17.769091	0.150144
-113.575820	-15.355924	0.155149
-117.143467	-17.186797	0.160154
-120.816008	-2.755348	0.165158
-124.693279	-10.380933	0.170163
-128.263666	-18.686244	0.175168
-132.126979	-18.814140	0.180173
-135.968684	-28.123228	0.185178
-139.710806	-14.574783	0.190182
-143.216644	-24.055721	0.195187
-147.146154	-22.930407	0.200192
-151.278969	-20.080598	0.205197
-155.224354	-29.004107	0.210202
-159.130145	-12.814964	0.215206
-162.909206	-26.005375	0.220211
-166.638224	-21.318192	0.225216
-170.061773	-22.713091	0.230221
-173.320063	-24.538050	0.235226
-177.000901	-19.798617	0.240230
-180.981788	-20.533715	0.245235
-184.570086	-19.092210	0.250240
-188.668189	-15.388449	0.255245
-192.293123	-22.108020	0.260250
-196.096692	-16.415428	0.265254
-199.981593	-18.984015	0.270259
-203.818091	-17.203257	0.275264
-208.005331	-17.801303	0.280269
-210.866558	-21.883089	0.285274
-215.005669	-13.867714	0.290278
-218.840377	-20.290419	0.295283
-222.697551	-17.109170	0.300288
-226.618348	-13.312217	0.305293
-229.543970	-22.549733	0.310298
-234.056585	-7.435292	0.315302
-237.458671	-11.646769	0.320307
-240.665964	-14.422782	0.325312
-244.815843	-16.969507	0.330317
-248.601844	-24.540056	0.335322
-252.776583	-17.332632	0.340326
-256.585394	-17.054294	0.345331
-260.040278	-19.100067	0.350336
-264.220347	-8.187557	0.355341
-267.550773	-22.641558	0.360346
-271.622013	-17.622056	0.365350
-275.078328	-14.443205	0.370355
-278.833605	-18.062089	0.375360
-282.925179	-9.989536	0.380365
-286.016361	-17.328736	0.385370
-290.078619	-15.220074	0.390374
-294.122151	-21.620359	0.395379
-297.633051	-27.058573	0.400384
-301.584525	-18.904280	0.405389
-305.101759	-23.049966	0.410394
-309.349138	-12.494067	0.415398
-312.675163	-17.132307	0.420403
-316.485768	-15.204119	0.425408
-320.452181	-14.293404	0.430413
-323.996132	-17.761449	0.435418
-327.979166	-19.596658	0.440422
-331.974743	-13.307090	0.445427
-335.211605	-20.652927	0.450432
-338.987780	-8.447037	0.455437
-342.645302	-14.842631	0.460442
-346.871208	-21.469172	0.465446
-350.506356	-18.416206	0.470451
-353.948168	-21.788549	0.475456
-357.643289	-22.201550	0.480461
-361.517115	-24.513023	0.485466
-365.542744	-20.304883	0.490470
-369.800324	-19.604642	0.495475
-373.209343	-15.371930	0.500480
-376.686555	-14.588110	0.505485
-380.047533	-25.123117	0.510490
-384.511835	-21.360565	0.515494
-388.126409	-18.414905	0.520499
-391.587985	-28.437098	0.525504
-395.849138	-17.360050	0.530509
-399.175641	-22.870129	0.535514
-403.059317	-13.315149	0.540518
-406.733015	-19.525132	0.545523
-410.498494	-21.645670	0.550528
-414.593505	-18.142297	0.555533
-417.647434	-33.009204	0.560538
-421.932196	-19.274377	0.565542
-425.939946	-18.468850	0.570547
-429.474915	-18.951467	0.575552
-433.178732	-16.478760	0.580557
-436.971964	-26.984081	0.585562
-440.850587	-16.023232	0.590566
-444.645744	-25.731884	0.595571
-447.954534	-15.675712	0.600576
-451.866500	-26.160470	0.605581
-455.614260	-28.602303	0.610586
-459.751383	-18.101612	0.615590
-463.117452	-25.060783	0.620595
-467.002260	-23.204087	0.625600
-470.964648	-10.454192	0.630605
-474.423210	-18.038813	0.635610
-478.414688	-13.671940	0.640614
-482.070933	-14.880998	0.645619
-485.680390	-18.071836	0.650624
-489.915890	-15.452633	0.655629
-493.356324	-23.962619	0.660634
-496.948926	-11.705397	0.665638
-500.902551	-17.000061	0.670643
-504.516665	-22.167591	0.675648
-508.385283	-18.427409	0.680653
-512.198351	-18.893873	0.685658
-516.064430	-18.656438	0.690662
-519.745754	-12.184951	0.695667
-523.387564	-13.874060	0.700672
-527.398731	-9.322616	0.705677
-531.050201	-12.006788	0.710682
-535.029910	-13.034793	0.715686
-538.709071	-9.029936	0.720691
-542.378924	-9.154956	0.725696
-546.088513	-7.821273	0.730701
-549.448347	-22.080909	0.735706
-553.329229	-5.105126	0.740710
-557.184178	-7.616411	0.745715
-560.680748	-13.048633	0.750720
-565.266115	-14.076037	0.755725
-568.616604	-19.657731	0.760730
-572.420666	-18.832457	0.765734
-575.788310	-12.865149	0.770739
-579.796309	-15.580601	0.775744
-583.995772	-8.956866	0.780749
-587.728043	-11.948159	0.785754
-591.597341	-12.030204	0.790758
-594.924235	-16.757783	0.795763
-598.380820	-17.448208	0.800768
-602.699786	-11.625354	0.805773
-606.049667	-17.893054	0.810778
-609.849655	-20.357837	0.815782
-613.825955	-16.770593	0.820787
-617.447558	-19.334823	0.825792
-621.375869	-16.971043	0.830797
-624.855311	-19.983742	0.835802
-628.880641	-11.318826	0.840806
-632.369293	-13.563658	0.845811
-636.334335	-14.953375	0.850816
-640.310986	-7.155639	0.855821
-643.768763	-17.700014	0.860826
-647.699755	-10.068832	0.865830
-651.311957	-13.184860	0.870835
-655.094249	-11.027277	0.875840
-659.198411	-12.697497	0.880845
-662.737043	-18.903417	0.885850
-666.080344	-11.949567	0.890854
-670.043371	-14.832896	0.895859
-673.906144	-11.279461	0.900864
-677.968182	-15.802728	0.905869
-681.237259	-21.416187	0.910874
-685.240973	-22.019063	0.915878
-689.119295	-17.512236	0.920883
-692.702789	-13.344242	0.925888
-696.590933	-7.102791	0.930893
-700.379031	-14.986064	0.935898
-704.053630	-10.812956	0.940902
-707.652515	-8.440174	0.945907
-711.334715	-18.177464	0.950912
-715.219557	-12.414321	0.955917
-719.022473	-22.756768	0.960922
-722.600752	-15.434141	0.965926
-726.690573	-14.761649	0.970931
-730.507971	-5.100063	0.975936
-734.388407	-2.691709	0.980941
-737.860768	-17.965954	0.985946
-741.490184	-15.698628	0.990950
-745.200212	-16.119682	0.995955
-748.861015	-19.896404	1.000960
-753.441049	-6.686254	1.005965
-756.903558	-10.381118	1.010970
-760.209646	-8.351511	1.015974
-763.963742	-9.796801	1.020979
-767.701676	-19.638628	1.025984
-771.856129	-10.757308	1.030989
-775.311036	-15.421588	1.035994
-779.407446	-18.165143	1.040998
-783.326086	-8.321722	1.046003
-786.929838	-12.381888	1.051008
-790.858087	-8.456686	1.056013
-794.003599	-20.586653	1.061018
-798.065458	-15.990395	1.066022
-801.675948	-16.566038	1.071027
-805.104202	-10.188192	1.076032
-809.339272	-7.158496	1.081037
-813.031001	-25.004201	1.086042
-816.777732	-7.112791	1.091046
-820.559354	-12.119012	1.096051
-824.468306	-15.062759	1.101056
-828.347959	-8.339920	1.106061
-831.941504	-13.715223	1.111066
-835.898098	-12.519800	1.116070
-839.527140	-12.767574	1.121075
-842.994606	-21.365738	1.126080
-846.900344	-4.885440	1.131085
-850.683421	-17.364410	1.136090
-854.650805	-12.415736	1.141094
-858.359961	-19.023012	1.146099
-861.674124	-21.632853	1.151104
-866.149750	-16.107761	1.156109
-869.648473	-17.879127	1.161114
-873.165615	-8.736827	1.166118
-876.959627	-10.818938	1.171123
-880.490904	-20.349841	1.176128
-884.544881	-12.550395	1.181133
-888.365262	-13.336773	1.186138
-892.267380	-14.947422	1.191142
-896.164721	-13.824449	1.196147
-899.371111	-20.373266	1.201152
-903.487492	-11.354314	1.206157
-906.965667	-17.020749	1.211162
-910.718737	-18.436004	1.216166
-914.773401	-11.823819	1.221171
-918.552483	-23.652035	1.226176
-922.579036	-15.207222	1.231181
-925.867953	-15.625935	1.236186
-929.661076	-15.472028	1.241190
-933.347076	-19.621311	1.246195
-936.898870	-26.300922	1.251200
-941.276660	-10.889858	1.256205
-944.724402	-18.294135	1.261210
-948.771716	-11.403953	1.266214
-952.396911	-8.982443	1.271219
-955.893095	-17.156379	1.276224
-959.700160	-14.104971	1.281229
-963.250654	-20.422059	1.286234
-967.261590	-18.837690	1.291238
-971.001885	-19.810199	1.296243
-974.597486	-28.250470	1.301248
-978.809202	-17.902580	1.306253
-982.203963	-20.879396	1.311258
-986.004799	-18.743556	1.316262
-989.951073	-22.327588	1.321267
-993.622198	-23.148699	1.326272
-997.843096	-12.616383	1.331277
-1001.068603	-16.914889	1.336282
-1005.197323	-19.723837	1.341286
-1009.140624	-13.463612	1.346291
-1012.575465	-33.972448	1.351296
-1016.476615	-17.869531	1.356301
-1019.351380	-19.784609	1.361306
-1023.445288	-16.977380	1.366310
-1027.876132	-14.519948	1.371315
-1031.366406	-16.293998	1.376320
-1035.298907	-8.059577	1.381325
-1038.547645	-17.291645	1.386330
-1042.407138	-9.318044	1.391334
-1046.462804	-14.437750	1.396339
-1050.339280	-15.818850	1.401344
-1054.056372	-11.595839	1.406349
-1057.372916	-10.264300	1.411354
-1061.139319	-16.578240	1.416358
-1064.808957	-21.441115	1.421363
-1068.762641	-13.775677	1.426368
-1072.836400	1.233764	1.431373
-1076.561998	-8.771940	1.436378
-1080.351884	-10.420725	1.441382
-1083.915633	-13.569053	1.446387
-1087.308949	-19.389126	1.451392
-1091.448017	-12.067727	1.456397
-1095.432849	-8.501976	1.461402
-1099.076706	-16.716717	1.466406
-1102.958076	-4.593804	1.471411
-1106.214081	-20.971196	1.476416
-1110.521233	-12.187884	1.481421
-1114.245185	-16.904801	1.486426
-1117.744453	-14.908450	1.491430
-1121.580141	-14.941384	1.496435
-1124.803442	-20.282407	1.501440
-1128.947666	-21.628427	1.506445
-1132.650858	-16.667946	1.511450
-1136.491173	-20.003754	1.516454
-1140.862185	-19.184637	1.521459
-1144.220416	-20.894485	1.526464
-1147.849369	-9.261309	1.531469
-1151.449145	-25.802819	1.536474
-1154.900283	-19.452367	1.541478
-1159.338904	-12.945503	1.546483
-1163.103227	-15.393005	1.551488
-1166.998895	-7.963764	1.556493
-1170.336779	-17.471525	1.561498
-1174.106317	-13.965319	1.566502
-1177.899459	-18.489715	1.571507
-1181.677343	-25.198993	1.576512
-1185.716658	-12.952921	1.581517
-1189.380371	-20.126722	1.586522
-1193.045408	-20.248342	1.591526
-1196.913462	-14.195389	1.596531
-1200.423699	-20.212619	1.601536
-1204.132817	-11.666752	1.606541
-1207.830132	-17.176233	1.611546
-1211.794550	-13.378595	1.616550
-1215.512758	-12.531330	1.621555
-1218.799223	-18.658452	1.626560
-1223.187742	-16.317811	1.631565
-1227.148950	-22.759565	1.636570
-1230.593010	-15.473450	1.641574
-1234.892313	-15.862509	1.646579
-1238.086546	-13.279294	1.651584
-1241.949821	-13.605652	1.656589
-1245.642992	-27.381912	1.661594
-1249.199360	-12.716767	1.666598
-1253.418680	-13.730434	1.671603
-1256.696286	-12.259769	1.676608
-1260.741714	-7.882972	1.681613
-1264.424169	-15.096229	1.686618
-1268.323954	-10.140345	1.691622
-1272.008630	-7.552713	1.696627
-1275.788441	-14.408180	1.701632
-1279.630496	-12.195886	1.706637
-1283.210734	-12.387703	1.711642
-1286.943048	-13.830900	1.716646
-1291.243956	-13.767023	1.721651
-1294.170292	-13.532054	1.726656
-1298.368935	-2.119712	1.731661
-1301.980451	-7.794156	1.736666
-1305.746277	-6.420322	1.741670
-1309.435396	-14.964929	1.746675
-1313.281009	-19.231546	1.751680
-1317.297255	-9.972471	1.756685
-1320.606736	-13.807658	1.761690
-1324.347775	-14.993937	1.766694
-1328.840916	-10.810287	1.771699
-1332.322818	-13.957133	1.776704
-1336.183338	-12.874015	1.781709
-1339.637607	-14.894626	1.786714
-1343.172803	-6.357461	1.791718
-1346.969081	-4.543458	1.796723
-1350.897246	-7.604653	1.801728
-1354.764394	-12.689326	1.806733
-1358.656968	-9.555783	1.811738
-1362.430170	-17.610612	1.816742
-1366.027983	-20.535429	1.821747
-1369.711795	-14.934304	1.826752
-1373.502801	-5.264924	1.831757
-1377.205211	-12.610414	1.836762
-1380.966457	-9.893662	1.841766
-1384.944020	-12.092203	1.846771
-1388.635081	-21.491048	1.851776
-1392.701782	-15.051176	1.856781
-1396.085185	-14.815447	1.861786
-1399.768497	-13.517747	1.866790
-1403.664501	-6.734606	1.871795
-1407.146818	-15.868805	1.876800
-1411.226142	-17.431282	1.881805
-1415.105051	-27.479652	1.886810
-1418.738455	-21.730411	1.891814
-1422.237811	-9.286557	1.896819
-1425.924630	-22.232491	1.901824
-1429.977871	-18.516460	1.906829
-1433.538065	-8.480253	1.911834
-1437.385557	-16.338561	1.916838
-1441.603313	-12.616669	1.921843
-1445.002399	-24.399144	1.926848
-1449.060459	-14.885587	1.931853
-1452.836005	-22.581923	1.936858
-1456.312097	-19.581134	1.941862
-1460.137210	-15.204582	1.946867
-1463.420759	-12.425416	1.951872
-1467.769098	-10.557515	1.956877
-1471.311335	-13.923137	1.961882
-1475.260090	-21.320473	1.966886
-1479.332872	-7.510578	1.971891
-1482.298532	-19.035979	1.976896
-1486.252740	-17.645881	1.981901
-1489.975731	-20.435341	1.986906
-1493.712967	-16.093306	1.991910
-1497.741677	-20.647245	1.996915
-1501.855131	-10.767323	2.006912
-1502.483401	-15.946625	2.016909
-1499.735102	-14.773021	2.026906
-1497.143652	-13.687979	2.036902
-1495.154873	-17.800578	2.046899
-1493.413694	-16.277804	2.056896
-1491.361714	-17.263188	2.066893
-1489.281939	-15.180426	2.076890
-1487.487696	-15.871908	2.086886
-1485.531187	-11.108908	2.096883
-1483.408728	-12.563460	2.106880
-1481.778901	-14.071759	2.116877
-1479.763850	-10.046014	2.126874
-1478.016129	-13.232642	2.136870
-1476.184387	-16.822718	2.146867
-1474.151049	-9.872561	2.156864
-1472.121804	-16.187912	2.166861
-1470.544934	-15.309856	2.176858
-1468.343266	-20.500192	2.186854
-1466.589344	-9.662175	2.196851
-1464.764527	-15.925840	2.206848
-1462.926452	-20.277963	2.216845
-1460.823098	-20.265768	2.226842
-1458.948954	-18.178475	2.236838
-1457.155851	-15.265055	2.246835
-1455.607726	-16.910252	2.256832
-1453.725762	-15.572618	2.266829
-1451.264887	-23.842299	2.276826
-1449.329986	-17.206357	2.286822
-1448.053731	-15.525426	2.296819
-1446.020576	-17.366694	2.306816
-1443.771168	-18.587328	2.316813
-1441.885784	-16.062877	2.326810
-1440.302983	-18.713078	2.336806
-1438.351388	-16.369749	2.346803
-1436.460574	-19.508204	2.356800
-1434.804695	-22.956408	2.366797
-1432.693769	-23.940125	2.376794
-1430.908736	-26.534277	2.386790
-1429.063606	-18.859220	2.396787
-1427.045968	-17.469075	2.406784
-1425.192818	-19.418873	2.416781
-1423.200332	-15.217362	2.426778
-1421.225127	-17.734586	2.436774
-1419.479289	-13.171481	2.446771
-1417.637194	-16.508962	2.456768
-1416.028931	-17.001668	2.466765
-1413.730761	-20.503739	2.476762
-1411.922228	-19.241156	2.486758
-1410.343758	-20.861182	2.496755
-1408.333889	-18.228738	2.506752
-1406.324794	-20.476642	2.516749
-1404.275770	-24.589335	2.526746
-1402.809980	-21.334529	2.536742
-1400.730567	-25.021037	2.546739
-1398.756918	-22.204368	2.556736
-1396.975716	-20.705295	2.566733
-1395.127338	-23.298509	2.576730
-1393.377562	-18.049180	2.586726
-1391.404998	-23.179086	2.596723
-1389.104721	-18.205773	2.606720
-1387.571468	-22.903774	2.616717
-1385.873450	-20.864013	2.626714
-1383.943687	-13.458248	2.636710
-1381.638946	-22.366020	2.646707
-1380.069340	-25.850901	2.656704
-1378.522257	-23.258032	2.666701
-1376.175388	-18.934789	2.676698
-1374.601162	-20.768845	2.686694
-1372.666909	-18.683207	2.696691
-1370.411306	-22.418419	2.706688
-1368.899343	-23.816194	2.716685
-1366.798545	-22.428256	2.726682
-1364.952376	-19.782201	2.736678
-1363.269949	-22.959872	2.746675
-1361.465383	-17.027715	2.756672
-1359.377124	-15.988285	2.766669
-1357.371472	-25.268154	2.776666
-1355.833578	-15.657029	2.786662
-1353.821112	-24.186414	2.796659
-1351.836829	-25.375574	2.806656
-1350.165297	-20.328421	2.816653
-1348.034417	-13.981120	2.826650
-1346.147770	-20.960377	2.836646
-1344.252424	-21.540038	2.846643
-1342.579484	-19.693597	2.856640
-1340.629820	-14.566217	2.866637
-1338.648839	-17.766397	2.876634
-1337.011672	-15.337914	2.886630
-1335.068386	-21.178346	2.896627
-1333.194198	-22.420920	2.906624
-1331.193752	-20.740574	2.916621
-1329.212854	-15.041873	2.926618
-1327.410555	-20.810786	2.936614
-1325.674385	-22.830202	2.946611
-1324.012053	-16.750513	2.956608
-1322.018865	-22.172609	2.966605
-1319.977657	-22.137708	2.976602
-1318.011894	-22.551778	2.986598
-1315.889667	-20.589333	2.996595
-1314.271543	-16.954641	3.006592
-1312.789697	-19.335971	3.016589
-1310.762237	-15.345216	3.026586
-1308.690130	-22.761492	3.036582
-1306.892491	-17.363439	3.046579
-1304.914184	-16.930039	3.056576
-1303.175490	-14.975672	3.066573
-1301.307230	-13.848874	3.076570
-1299.443867	-19.918063	3.086566
-1297.574106	-17.316780	3.096563
-1295.319595	-17.363362	3.106560
-1293.587152	-16.732711	3.116557
-1291.965205	-13.569136	3.126554
-1289.963058	-14.696366	3.136550
-1288.220179	-11.440037	3.146547
-1286.201500	-15.536725	3.156544
-1283.846205	-16.485207	3.166541
-1282.593272	-16.017805	3.176538
-1280.576359	-16.080032	3.186534
-1278.753135	-17.072831	3.196531
-1276.650276	-18.975634	3.206528
-1274.682638	-19.986803	3.216525
-1273.258017	-16.823214	3.226522
-1271.372128	-18.520765	3.236518
-1269.379027	-15.223940	3.246515
-1267.578289	-23.446221	3.256512
-1265.388079	-21.786711	3.266509
-1263.886505	-14.089683	3.276506
-1261.949557	-13.512261	3.286502
-1259.771264	-18.087623	3.296499
-1257.731957	-23.423891	3.306496
-1256.077594	-18.574441	3.316493
-1254.332518	-21.605748	3.326490
-1252.462826	-16.664437	3.336486
-1250.656432	-14.761915	3.346483
-1248.860480	-21.440800	3.356480
-1246.797163	-21.338320	3.366477
-1244.844129	-23.960797	3.376474
-1243.018224	-18.458267	3.386470
-1241.065393	-19.463881	3.396467
-1239.198317	-15.150555	3.406464
-1237.450662	-14.403876	3.416461
-1235.613359	-17.453086	3.426458
-1233.724793	-15.023704	3.436454
-1231.691754	-13.894795	3.446451
-1229.880788	-24.581823	3.456448
-1228.249649	-20.660206	3.466445
-1226.053711	-18.092109	3.476442
-1224.373000	-14.644205	3.486438
-1222.429360	-20.846182	3.496435
-1220.309707	-21.106373	3.506432
-1218.687275	-23.364879	3.516429
-1216.696716	-16.178688	3.526426
-1214.890733	-21.436535	3.536422
-1213.005490	-20.838167	3.546419
-1211.224234	-24.001546	3.556416
-1209.008487	-17.992949	3.566413
-1207.613034	-23.301944	3.576410
-1205.327912	-18.401802	3.586406
-1203.361304	-21.062732	3.596403
-1201.840215	-18.588737	3.606400
-1199.909310	-26.977058	3.616397
-1197.753825	-19.831450	3.626394
-1196.205848	-23.762749	3.636390
-1194.361571	-20.580993	3.646387
-1192.350702	-15.468010	3.656384
-1190.437470	-24.980856	3.666381
-1188.700221	-23.341957	3.676378
-1186.806260	-20.690770	3.686374
-1184.967319	-20.220760	3.696371
-1182.839779	-16.811158	3.706368
-1181.078400	-19.785021	3.716365
-1179.221452	-24.462053	3.726362
-1177.258394	-22.355593	3.736358
-1175.487972	-15.680454	3.746355
-1173.462195	-19.252399	3.756352
-1171.990320	-18.703124	3.766349
-1169.889247	-20.106604	3.776346
-1167.810002	-17.732937	3.786342
-1165.781062	-17.350150	3.796339
-1164.464801	-15.680194	3.806336
-1162.390822	-18.645635	3.816333
-1160.461167	-15.671717	3.826330
-1158.551434	-16.712999	3.836326
-1156.859767	-17.501499	3.846323
-1154.882055	-17.506820	3.856320
-1152.766538	-18.352074	3.866317
-1151.011434	-19.747556	3.876314
-1149.393644	-17.298468	3.886310
-1146.963604	-17.570355	3.896307
-1145.506792	-12.079745	3.906304
-1143.604842	-18.110783	3.916301
-1141.570194	-22.121485	3.926298
-1139.698616	-17.515114	3.936294
-1137.977142	-15.384181	3.946291
-1136.493161	-16.654175	3.956288
-1133.993474	-20.556109	3.966285
-1132.399844	-17.867883	3.976282
-1130.535394	-21.827664	3.986278
-1128.450229	-18.884912	3.996275
-1126.434463	-17.161046	4.006272
-1124.702554	-14.667039	4.016269
-1123.050572	-21.925959	4.026266
-1121.087435	-14.953183	4.036262
-1119.201376	-18.373260	4.046259
-1117.327968	-14.817153	4.056256
-1115.353531	-22.383437	4.066253
-1113.599792	-14.811900	4.076250
-1111.843271	-10.196571	4.086246
-1109.871281	-13.927227	4.096243
-1107.685698	-9.691580	4.106240
-1106.027594	-12.434135	4.116237
-1104.435886	-14.867649	4.126234
-1101.862450	-10.878772	4.136230
-1100.509702	-12.102489	4.146227
-1098.470587	-15.720716	4.156224
-1096.681922	-20.337818	4.166221
-1094.804908	-9.506532	4.176218
-1092.938068	-17.478746	4.186214
-1090.948961	-13.664809	4.196211
-1088.941827	-11.421638	4.206208
-1087.436887	-22.781196	4.216205
-1085.606300	-18.487167	4.226202
-1083.689640	-16.084259	4.236198
-1081.655144	-26.982203	4.246195
-1079.639195	-21.966246	4.256192
-1077.592816	-21.401436	4.266189
-1076.087664	-21.866363	4.276186
-1074.221452	-19.905374	4.286182
-1072.226513	-20.813374	4.296179
-1070.539432	-19.035308	4.306176
-1068.289208	-22.379382	4.316173
-1066.730088	-18.780859	4.326170
-1064.824502	-18.750883	4.336166
-1062.825792	-20.254737	4.346163
-1060.960271	-20.624136	4.356160
-1059.176608	-19.314664	4.366157
-1057.265294	-22.896625	4.376154
-1055.451556	-26.685606	4.386150
-1053.454248	-23.395579	4.396147
-1051.549261	-22.157610	4.406144
-1049.691795	-19.865205	4.416141
-1048.108164	-20.011089	4.426138
-1045.985799	-17.528944	4.436134
-1044.018199	-20.410955	4.446131
-1042.091721	-27.039517	4.456128
-1040.172745	-21.033811	4.466125
-1038.712672	-19.854148	4.476122
-1036.570489	-25.127741	4.486118
-1035.072565	-16.356286	4.496115
-1032.918922	-10.746518	4.506112
-1030.956936	-14.611300	4.516109
-1028.915163	-16.902007	4.526106
-1027.382796	-24.678574	4.536102
-1025.170863	-20.271801	4.546099
-1023.504256	-20.808305	4.556096
-1021.823985	-22.426985	4.566093
-1019.675446	-25.884224	4.576090
-1017.752138	-23.482324	4.586086
-1015.846591	-27.181749	4.596083
-1014.136225	-28.947341	4.606080
-1012.011836	-26.227070	4.616077
-1010.381490	-32.779827	4.626074
-1008.842976	-22.598543	4.636070
-1006.694658	-24.167327	4.646067
-1004.632183	-18.056642	4.656064
-1002.671917	-27.229509	4.666061
-1001.177751	-23.180031	4.676058
-998.703211	-18.022599	4.686054
-997.227879	-24.550562	4.696051
-995.385062	-19.680524	4.706048
-993.414343	-21.211422	4.716045
-991.587557	-20.133002	4.726042
-989.890257	-23.652266	4.736038
-987.748434	-22.245277	4.746035
-986.059575	-20.244802	4.756032
-984.092091	-24.003055	4.766029
-981.902902	-21.962587	4.776026
-980.550267	-12.517334	4.786022
-978.453297	-20.068373	4.796019
-976.506249	-23.303882	4.806016
-974.511682	-25.010682	4.816013
-972.715585	-24.789440	4.826010
-971.176278	-20.020847	4.836006
-969.087133	-17.932789	4.846003
-967.111614	-15.098669	4.856000
-965.293689	-20.847719	4.865997
-963.563901	-20.396394	4.875994
-961.546208	-21.318991	4.885990
-959.454695	-17.680786	4.895987
-958.163009	-22.090429	4.905984
-956.023980	-24.219783	4.915981
-954.143950	-18.488823	4.925978
-952.320249	-21.687222	4.935974
-950.235748	-23.121015	4.945971
-948.339558	-19.696304	4.955968
-946.492902	-28.149915	4.965965
-944.701113	-25.706398	4.975962
-942.811152	-22.520686	4.985958
-941.077961	-18.190438	4.995955
-938.786214	-24.646802	5.005952
-937.014441	-22.339025	5.015949
-935.283259	-16.071093	5.025946
-933.480671	-26.076062	5.035942
-931.656545	-20.898247	5.045939
-929.746360	-22.335730	5.055936
-927.753690	-18.841165	5.065933
-925.833781	-21.447035	5.075930
-923.985867	-23.967183	5.085926
-922.334558	-12.805970	5.095923
-920.237749	-21.122721	5.105920
-918.263828	-20.854079	5.115917
-916.444840	-14.914379	5.125914
-914.668485	-16.630452	5.135910
-912.853304	-23.223757	5.145907
-910.957893	-20.231519	5.155904
-908.818991	-18.525569	5.165901
-906.922756	-17.917657	5.175898
-905.519357	-18.014104	5.185894
-903.478556	-18.253508	5.195891
-901.620713	-21.852063	5.205888
-899.672365	-22.839309	5.215885
-897.667950	-18.051865	5.225882
-895.628917	-22.776745	5.235878
-893.871509	-19.858745	5.245875
-892.205427	-17.011406	5.255872
-890.522440	-22.588829	5.265869
-888.501487	-18.130861	5.275866
-886.423234	-19.557284	5.285862
-884.480703	-19.962539	5.295859
-882.529284	-15.406607	5.305856
-880.994106	-11.316231	5.315853
-879.234862	-14.553220	5.325850
-877.211211	-13.915127	5.335846
-875.038479	-12.362974	5.345843
-873.406205	-13.075461	5.355840
-871.177526	-14.074342	5.365837
-869.640983	-17.975192	5.375834
-867.877207	-13.135040	5.385830
-866.073543	-17.214379	5.395827
-863.957087	-18.365839	5.405824
-862.001715	-18.100500	5.415821
-860.182658	-14.732856	5.425818
-858.442294	-13.449464	5.435814
-856.275893	-12.857856	5.445811
-854.415606	-21.577269	5.455808
-853.193407	-15.947904	5.465805
-850.690745	-15.970567	5.475802
-848.963361	-21.795060	5.485798
-847.522615	-13.772216	5.495795
-844.992044	-16.682480	5.505792
-843.263685	-20.192399	5.515789
-841.393869	-12.416558	5.525786
-839.896000	-20.934345	5.535782
-837.621131	-13.801140	5.545779
-835.933421	-16.870348	5.555776
-833.942051	-21.461244	5.565773
-832.027850	-20.654039	5.575770
-829.933718	-23.916100	5.585766
-828.191075	-25.465668	5.595763
-826.702820	-21.636177	5.605760
-824.970179	-25.130977	5.615757
-822.552326	-22.116384	5.625754
-820.734933	-25.192099	5.635750
-819.022046	-24.385862	5.645747
-817.018446	-25.039243	5.655744
-815.008029	-23.712142	5.665741
-813.192203	-14.443444	5.675738
-811.593721	-20.402045	5.685734
-809.468994	-16.787956	5.695731
-807.753344	-22.392651	5.705728
-806.027970	-14.491062	5.715725
-803.864656	-18.923102	5.725722
-802.071431	-18.093378	5.735718
-800.186405	-15.285701	5.745715
-798.457719	-20.834054	5.755712
-796.478082	-20.261488	5.765709
-794.400030	-24.040420	5.775706
-792.836243	-15.099314	5.785702
-790.990158	-20.540110	5.795699
-788.561556	-23.034545	5.805696
-787.128267	-11.271534	5.815693
-784.943558	-15.752768	5.825690
-783.395203	-12.690742	5.835686
-781.797708	-15.369707	5.845683
-779.366381	-15.598788	5.855680
-777.396310	-19.714132	5.865677
-775.638935	-16.751823	5.875674
-774.073349	-22.455670	5.885670
-772.277239	-20.462705	5.895667
-770.141916	-20.881310	5.905664
-768.276913	-22.603548	5.915661
-766.289613	-23.126386	5.925658
-764.525928	-19.681923	5.935654
-762.757052	-16.705653	5.945651
-760.741494	-18.207211	5.955648
-759.028191	-16.823103	5.965645
-757.220168	-15.389396	5.975642
-755.094009	-16.267574	5.985638
-753.194019	-10.556995	5.995635
-751.425515	-16.596416	6.005632
-749.499733	-20.439398	6.015629
-747.933331	-14.632874	6.025626
-745.864071	-16.176159	6.035622
-743.804844	-17.192051	6.045619
-742.225176	-11.750799	6.055616
-740.104562	-13.668600	6.065613
-738.031149	-15.180964	6.075610
-736.294409	-15.723737	6.085606
-734.402332	-12.328186	6.095603
-732.631497	-15.375871	6.105600
-730.963504	-17.170808	6.115597
-728.807338	-12.551143	6.125594
-727.079984	-9.729260	6.135590
-725.061034	-10.618701	6.145587
-723.338972	-18.108045	6.155584
-721.324454	-19.557298	6.165581
-719.689602	-12.640642	6.175578
-717.616988	-13.672862	6.185574
-715.732452	-16.846071	6.195571
-714.025370	-21.085129	6.205568
-711.835203	-13.559312	6.215565
-709.980763	-12.728246	6.225562
-708.226855	-23.986867	6.235558
-706.316082	-17.614818	6.245555
-704.738033	-18.844313	6.255552
-702.453778	-18.634552	6.265549
-700.575010	-17.643156	6.275546
-698.951630	-13.809905	6.285542
-696.887017	-16.945559	6.295539
-695.450808	-24.014997	6.305536
-693.085851	-23.094967	6.315533
-691.497563	-19.955577	6.325530
-689.389455	-23.761329	6.335526
-687.566649	-8.882071	6.345523
-685.691119	-19.841167	6.355520
-683.569845	-17.675878	6.365517
-682.170420	-19.115238	6.375514
-680.278367	-15.711744	6.385510
-678.232691	-15.482786	6.395507
-676.404363	-16.096992	6.405504
-674.683495	-18.345600	6.415501
-672.367466	-17.600888	6.425498
-670.562725	-17.952374	6.435494
-668.750800	-13.190807	6.445491
-667.101158	-17.853288	6.455488
-665.413981	-26.567014	6.465485
-663.358818	-23.170622	6.475482
-660.822809	-23.949989	6.485478
-659.488864	-26.476238	6.495475
-657.639938	-22.295313	6.505472
-655.680069	-24.111568	6.515469
-654.059149	-21.836310	6.525466
-651.851007	-15.450144	6.535462
-650.039812	-16.554222	6.545459
-648.002329	-19.150239	6.555456
-646.297007	-21.830553	6.565453
-644.504352	-25.421657	6.575450
-642.524294	-18.234835	6.585446
-640.958503	-21.816535	6.595443
-638.986294	-18.618445	6.605440
-636.896853	-18.634864	6.615437
-635.111880	-15.301066	6.625434
-633.167470	-22.649032	6.635430
-631.460910	-21.999541	6.645427
-629.437166	-19.302307	6.655424
-627.480280	-20.865432	6.665421
-625.586687	-27.182115	6.675418
-623.782601	-21.871370	6.685414
-622.062235	-24.759332	6.695411
-620.126409	-20.034891	6.705408
-618.113408	-19.214873	6.715405
-616.191546	-19.032398	6.725402
-614.472916	-20.366398	6.735398
-612.815401	-22.405894	6.745395
-610.711056	-25.945716	6.755392
-608.705693	-19.471851	6.765389
-606.708038	-22.153049	6.775386
-605.114055	-22.353974	6.785382
-603.346044	-14.766924	6.795379
-601.129902	-13.052502	6.805376
-599.523065	-17.886522	6.815373
-597.556164	-13.061234	6.825370
-595.579115	-17.425445	6.835366
-593.916850	-16.470430	6.845363
-591.997547	-13.098057	6.855360
-589.909292	-16.316346	6.865357
-588.135236	-21.259175	6.875354
-586.361022	-14.121522	6.885350
-584.553735	-14.064402	6.895347
-582.469491	-18.395200	6.905344
-580.590333	-25.189545	6.915341
-578.750014	-14.865083	6.925338
-577.077630	-14.175357	6.935334
-575.108813	-14.196137	6.945331
-572.970913	-11.141297	6.955328
-571.221421	-12.915986	6.965325
-569.504909	-13.828037	6.975322
-567.217890	-16.659636	6.985318
-565.714769	-12.372869	6.995315
-563.741339	-19.122263	7.005312
-562.016701	-13.767194	7.015309
-560.198688	-18.391763	7.025306
-558.084763	-15.500449	7.035302
-556.090689	-16.494721	7.045299
-554.615381	-16.562972	7.055296
-552.759478	-12.090966	7.065293
-550.504314	-17.817985	7.075290
-548.718952	-15.734706	7.085286
-546.996706	-17.512920	7.095283
-544.795703	-18.440761	7.105280
-543.056176	-18.061734	7.115277
-541.341676	-20.277653	7.125274
-539.290887	-22.026232	7.135270
-537.573455	-17.551046	7.145267
-535.629438	-13.500468	7.155264
-533.958247	-16.307885	7.165261
-531.946348	-17.944457	7.175258
-529.987363	-20.467838	7.185254
-528.183786	-18.521664	7.195251
-526.416407	-16.992864	7.205248
-524.146809	-19.322693	7.215245
-522.384217	-14.145760	7.225242
-520.745467	-17.933250	7.235238
-518.713838	-7.367706	7.245235
-516.834269	-14.626286	7.255232
-515.015332	-17.240973	7.265229
-512.950966	-21.726432	7.275226
-511.233688	-12.804888	7.285222
-509.187142	-9.866450	7.295219
-507.804909	-18.062435	7.305216
-505.633424	-16.285527	7.315213
-503.820486	-13.260829	7.325210
-501.780542	-11.207120	7.335206
-499.966487	-12.251543	7.345203
-498.144483	-15.469864	7.355200
-496.156466	-19.420486	7.365197
-494.425342	-10.245348	7.375194
-492.326650	-15.847853	7.385190
-490.579217	-16.554787	7.395187
-488.673638	-17.125923	7.405184
-486.777612	-20.392372	7.415181
-485.051728	-28.903747	7.425178
-482.985723	-24.094189	7.435174
-481.348217	-16.644092	7.445171
-479.578384	-24.020907	7.455168
-477.573878	-19.334152	7.465165
-475.495185	-16.356609	7.475162
-473.592392	-13.603605	7.485158
-471.695393	-15.554936	7.495155
-469.902977	-13.917986	7.505152
-468.022191	-13.354620	7.515149
-466.320023	-17.526413	7.525146
-464.285443	-16.294446	7.535142
-462.507619	-16.985687	7.545139
-460.489917	-12.223653	7.555136
-458.678009	-21.445069	7.565133
-456.683133	-20.124650	7.575130
-454.821700	-23.150288	7.585126
-453.076463	-13.622109	7.595123
-451.204452	-11.691539	7.605120
-449.263997	-16.280319	7.615117
-447.535722	-10.452056	7.625114
-445.512454	-10.083529	7.635110
-444.129883	-10.397430	7.645107
-441.604680	-11.703788	7.655104
-439.757265	-21.450336	7.665101
-438.242017	-7.486468	7.675098
-435.954218	-15.399126	7.685094
-434.617830	-9.536697	7.695091
-432.431336	-12.671067	7.705088
-430.232628	-9.658961	7.715085
-428.386355	-16.203214	7.725082
-426.880764	-12.005168	7.735078
-425.101694	-11.356052	7.745075
-422.989847	-8.151649	7.755072
-421.315812	-4.481019	7.765069
-419.149495	-11.147423	7.775066
-417.503883	-11.076993	7.785062
-415.530470	-8.267321	7.795059
-413.556532	-8.667733	7.805056
-411.798147	-10.844781	7.815053
-409.866474	-13.545286	7.825050
-407.977074	-9.965877	7.835046
-406.212964	-9.633307	7.845043
-404.227767	-10.889721	7.855040
-402.640266	-7.366315	7.865037
-400.234887	-15.352978	7.875034
-398.600055	-15.811340	7.885030
-397.081063	-10.486465	7.895027
-395.180376	-5.276213	7.905024
-392.993891	-6.171598	7.915021
-390.866051	-6.730774	7.925018
-389.026279	-6.277640	7.935014
-387.612641	-6.010678	7.945011
-385.749633	-12.398101	7.955008
-383.834025	-7.401802	7.965005
-381.560488	-11.955289	7.975002
-379.529218	-16.016936	7.984998
-378.213623	-10.995890	7.994995
-376.298181	-11.732723	8.004992
-374.224120	-4.222762	8.014989
-372.487107	-10.132165	8.024986
-370.551588	-3.020081	8.034982
-368.620978	-1.960906	8.044979
-366.747704	-8.730483	8.054976
-364.782016	-11.515331	8.064973
-362.906585	-9.165235	8.074970
-361.042019	-7.539719	8.084966
-359.325649	-7.750546	8.094963
-357.620778	-5.270584	8.104960
-355.319246	-3.563244	8.114957
-353.425318	-5.654521	8.124954
-351.571722	-9.354624	8.134950
-350.074139	-10.144728	8.144947
-347.902441	-7.189810	8.154944
-346.212162	-9.449097	8.164941
-344.423761	-8.976674	8.174938
-342.190836	-12.498905	8.184934
-340.356120	-2.122802	8.194931
-338.941673	-5.980159	8.204928
-336.847485	-5.918126	8.214925
-334.749911	-8.474531	8.224922
-333.020435	-5.869005	8.234918
-330.997871	-6.681323	8.244915
-329.213723	-3.143467	8.254912
-327.363958	-2.983985	8.264909
-325.340569	-9.839075	8.274906
-323.553458	-14.366966	8.284902
-321.792431	-8.876990	8.294899
-319.829960	-15.619716	8.304896
-318.262674	-10.692496	8.314893
-315.962770	-14.092763	8.324890
-314.090544	-10.755272	8.334886
-312.490194	-10.276492	8.344883
-310.398536	-6.974025	8.354880
-308.660420	-8.358289	8.364877
-306.604902	-12.987434	8.374874
-304.864639	-7.699393	8.384870
-302.989978	-10.275452	8.394867
-301.194541	-8.493591	8.404864
-299.093138	-7.373200	8.414861
-297.176324	-4.751760	8.424858
-295.371624	-8.265596	8.434854
-293.673354	-11.764020	8.444851
-291.919046	-2.875043	8.454848
-290.006070	-10.284062	8.464845
-287.967979	-4.075649	8.474842
-286.008746	-14.998897	8.484838
-284.237899	-3.927287	8.494835
-282.247324	-10.543421	8.504832
-280.550945	-8.458364	8.514829
-278.564850	-9.435345	8.524826
-276.428131	-10.794788	8.534822
-275.027045	-4.453109	8.544819
-272.943653	-12.351948	8.554816
-270.965737	-13.074985	8.564813
-269.083066	-13.512818	8.574810
-267.207372	-10.725317	8.584807
-265.516803	-9.395639	8.594803
-263.864795	-21.029308	8.604800
-261.995291	-22.297140	8.614797
-259.499109	-23.592361	8.624794
-258.009427	-19.446927	8.634791
-256.114208	-18.914119	8.644787
-254.144321	-21.868496	8.654784
-252.345811	-24.966046	8.664781
-250.322933	-29.307299	8.674778
-248.434917	-18.923845	8.684775
-246.675190	-16.100452	8.694771
-244.857132	-24.031127	8.704768
-242.989769	-20.416488	8.714765
-241.114837	-20.838853	8.724762
-238.743653	-26.745164	8.734759
-236.886158	-19.132623	8.744755
-235.277295	-21.513050	8.754752
-233.676685	-24.905845	8.764749
-231.614908	-22.471701	8.774746
-229.903555	-22.381635	8.784743
-228.020153	-18.112699	8.794739
-225.976537	-17.590919	8.804736
-224.125359	-21.074224	8.814733
-222.232922	-25.443587	8.824730
-220.333045	-18.872007	8.834727
-218.506631	-15.511339	8.844723
-216.940227	-24.666573	8.854720
-214.707704	-19.387552	8.864717
-212.834917	-25.807987	8.874714
-210.792243	-19.808663	8.884711
-209.332417	-20.101600	8.894707
-207.608552	-16.358242	8.904704
-205.509521	-19.243190	8.914701
-203.515805	-27.593448	8.924698
-201.591004	-27.576897	8.934695
-199.935915	-21.730450	8.944691
-197.681365	-24.749157	8.954688
-195.796580	-29.272015	8.964685
-194.257115	-30.471338	8.974682
-192.234728	-25.332448	8.984679
-190.323181	-21.003237	8.994675
-188.756989	-25.637883	9.004672
-186.505243	-24.119805	9.014669
-184.646936	-26.481584	9.024666
-183.012026	-27.936131	9.034663
-181.261590	-26.964896	9.044659
-179.120404	-27.783386	9.054656
-177.386993	-26.815747	9.064653
-175.285954	-22.159918	9.074650
-173.434867	-23.200533	9.084647
-171.785924	-25.991526	9.094643
-169.794330	-22.966654	9.104640
-168.014929	-20.023183	9.114637
-165.884358	-24.149450	9.124634
-164.333215	-24.032193	9.134631
-161.886450	-24.067320	9.144627
-160.271074	-25.076630	9.154624
-158.623592	-26.637378	9.164621
-156.507603	-21.999707	9.174618
-154.941066	-21.624374	9.184615
-153.035260	-23.801076	9.194611
-151.083206	-22.063039	9.204608
-149.166548	-20.879881	9.214605
-147.215078	-25.566504	9.224602
-145.267480	-23.109329	9.234599
-143.183283	-22.976059	9.244595
-141.537367	-19.378109	9.254592
-139.747026	-18.877423	9.264589
-138.166007	-19.189654	9.274586
-135.843718	-20.948058	9.284583
-133.882781	-19.959847	9.294579
-132.275572	-20.404149	9.304576
-130.476226	-25.961753	9.314573
-128.517986	-23.231525	9.324570
-126.720704	-28.049846	9.334567
-124.601590	-17.513678	9.344563
-122.869316	-19.905829	9.354560
-120.929493	-24.851101	9.364557
-119.207864	-20.905214	9.374554
-117.411239	-24.537632	9.384551
-115.291892	-19.060455	9.394547
-113.299996	-16.439793	9.404544
-111.703376	-21.420303	9.414541
-109.920539	-16.337854	9.424538
-107.663219	-17.537968	9.434535
-105.929468	-15.670328	9.444531
-104.033194	-15.903360	9.454528
-102.140918	-21.133140	9.464525
-100.109453	-20.219312	9.474522
-98.563952	-23.950600	9.484519
-97.123874	-17.111346	9.494515
-94.721390	-23.390417	9.504512
-92.892543	-18.624770	9.514509
-90.678386	-21.805885	9.524506
-88.869542	-18.707576	9.534503
-87.080592	-19.956109	9.544499
-85.308932	-22.097148	9.554496
-83.340400	-17.922201	9.564493
-81.516576	-25.038946	9.574490
-80.012021	-18.195757	9.584487
-77.902834	-11.216915	9.594483
-76.012872	-23.475809	9.604480
-73.934333	-15.592073	9.614477
-72.227315	-23.114918	9.624474
-70.128377	-17.683389	9.634471
-68.551154	-17.156546	9.644467
-66.726107	-14.720806	9.654464
-64.565951	-21.752248	9.664461
-62.841458	-25.971544	9.674458
-60.853898	-22.990145	9.684455
-59.277415	-21.174752	9.694451
-57.353501	-20.346363	9.704448
-55.346462	-12.220674	9.714445
-53.404365	-12.955189	9.724442
-51.535390	-16.325945	9.734439
-49.678769	-15.739448	9.744435
-47.842267	-15.467109	9.754432
-45.743460	-21.588745	9.764429
-43.385051	-22.591768	9.774426
-42.037438	-19.063004	9.784423
-41.093565	-16.826159	9.794419
-38.864998	-14.633187	9.804416
-36.347397	-18.581084	9.814413
-34.591067	-19.911217	9.824410
-32.652856	-22.934579	9.834407
-30.979695	-20.300900	9.844403
-29.012321	-16.853620	9.854400
-27.116227	-17.620250	9.864397
-25.217589	-20.967296	9.874394
-23.653943	-21.268787	9.884391
-21.512329	-25.057220	9.894387
-19.398763	-22.073780	9.904384
-17.391345	-28.458709	9.914381
-16.134130	-22.038658	9.924378
-14.042542	-23.870676	9.934375
-12.174430	-17.696483	9.944371
-10.409588	-17.870583	9.954368
-8.577359	-17.706482	9.964365
-6.358445	-23.506189	9.974362
-5.277548	-12.581668	9.984359
-3.803162	21.538154	9.994355
-2.205304	74.656987	10.004352
-1.192267	129.227210	10.014349
0.000000	183.393710	10.019354
0.602968	228.665124	10.024359
0.985183	254.748665	10.029363
2.081770	284.105641	10.034368
2.152154	316.855994	10.039373
2.589103	332.721631	10.044378
2.667078	350.275134	10.049383
2.904061	369.670439	10.054387
3.263327	382.474991	10.059392
3.391999	390.992252	10.064397
3.578077	393.862656	10.069402
3.412741	405.445161	10.074407
3.638339	402.658937	10.079411
3.725038	413.155710	10.084416
4.123071	435.004433	10.089421
3.968489	421.665737	10.094426
3.765834	435.569231	10.099431
3.878166	442.964738	10.104435
4.251903	447.404285	10.109440
4.146465	458.190362	10.114445
4.505146	452.169002	10.119450
4.309098	454.829124	10.124455
4.061883	458.610761	10.129459
4.052647	465.352296	10.134464
4.175915	469.735603	10.139469
4.281227	465.587110	10.144474
4.511018	477.399970	10.149479
4.240048	469.111970	10.154483
4.371476	474.687757	10.159488
4.144931	482.887982	10.164493
4.751686	476.857008	10.169498
5.103926	484.294699	10.174503
4.567227	480.584500	10.179507
4.694983	481.865155	10.184512
4.145890	493.237696	10.189517
4.898144	498.432191	10.194522
4.907774	517.256813	10.199527
4.898778	522.402419	10.204531
5.286839	523.628944	10.209536
5.080491	529.569294	10.214541
5.309320	525.588747	10.219546
4.863007	535.271735	10.224551
4.972597	538.198523	10.229555
5.142707	531.994312	10.234560
5.011326	537.722431	10.239565
5.661362	532.666999	10.244570
5.138933	536.907302	10.249575
5.141553	538.009219	10.254579
5.138654	535.149025	10.259584
5.073804	537.428681	10.264589
5.118114	543.141396	10.269594
5.510049	552.053590	10.274599
5.439479	562.998191	10.279603
5.750584	568.684133	10.284608
5.373831	576.486521	10.289613
5.560477	564.945456	10.294618
5.512164	565.582399	10.299623
5.714118	580.141397	10.304627
5.930066	577.194248	10.309632
5.573920	573.491499	10.314637
5.634288	584.451503	10.319642
5.541308	597.309453	10.324647
5.870182	614.274460	10.329651
6.083352	606.910560	10.334656
5.909896	622.165797	10.339661
5.977464	616.053602	10.344666
6.105037	622.543147	10.349671
6.120270	619.323642	10.354675
6.285343	621.984545	10.359680
6.441053	622.812885	10.364685
6.193134	620.261422	10.369690
6.125475	625.561505	10.374695
6.121179	633.445660	10.379699
6.786089	631.742117	10.384704
6.640793	658.550786	10.389709
6.509853	653.750769	10.394714
6.785024	658.430037	10.399719
6.584688	663.883764	10.404723
6.776492	666.712307	10.409728
6.672063	677.198753	10.414733
6.698990	672.280506	10.419738
6.587351	671.509822	10.424743
6.831895	670.835298	10.429747
6.740468	670.247477	10.434752
6.732724	668.567634	10.439757
6.988282	668.459077	10.444762
6.714631	672.852134	10.449767
7.051242	675.633926	10.454771
7.642540	677.023600	10.459776
6.798569	679.194147	10.464781
7.119790	692.971750	10.469786
6.950637	707.865255	10.474791
7.057006	725.534536	10.479795
7.482584	720.451760	10.484800
7.262429	725.124894	10.489805
7.182240	727.227246	10.494810
7.405572	726.652301	10.499815
7.448186	741.098885	10.504819
7.299340	728.921255	10.509824
7.327224	725.018437	10.514829
7.740323	738.844510	10.519834
7.843454	756.490690	10.524839
7.697151	755.247693	10.529843
7.897469	764.897086	10.534848
7.778758	762.515809	10.539853
7.824225	767.709588	10.544858
8.031679	765.314137	10.549863
7.725673	765.736713	10.554867
7.939941	778.895917	10.559872
8.216703	776.240241	10.564877
8.336854	781.653934	10.569882
8.050604	776.788757	10.574887
7.716110	780.937650	10.579891
8.163271	765.340564	10.584896
8.201212	774.544333	10.589901
8.179388	767.085363	10.594906
8.231977	771.347564	10.599911
8.462010	796.360323	10.604915
8.269807	799.347915	10.609920
8.301090	818.639427	10.614925
8.451175	800.881849	10.619930
8.837266	813.734547	10.624935
8.741150	814.087375	10.629939
8.904523	808.238953	10.634944
8.676203	814.187654	10.639949
8.603238	818.900423	10.644954
8.567329	817.994644	10.649959
9.036093	827.590224	10.654963
8.806105	812.649896	10.659968
8.512966	824.382434	10.664973
8.768465	821.903614	10.669978
8.840229	830.387631	10.674983
8.993113	839.199352	10.679987
9.084033	848.235438	10.684992
9.372050	849.481103	10.689997
9.109816	848.892131	10.695002
9.175943	852.360528	10.700007
9.109647	864.220928	10.705011
9.390243	850.829776	10.710016
9.294081	866.041400	10.715021
9.509645	861.220743	10.720026
9.593596	859.866892	10.725031
9.178416	866.722247	10.730035
9.507257	857.871554	10.735040
9.198258	870.216969	10.740045
9.585833	864.804298	10.745050
9.275567	875.371028	10.750055
9.553061	891.328946	10.755059
10.091313	899.164559	10.760064
9.903680	902.618245	10.765069
9.879781	893.372760	10.770074
10.097641	902.328706	10.775079
9.387630	904.845367	10.780083
10.051043	896.808658	10.785088
9.889870	903.303379	10.790093
10.163244	904.554539	10.795098
9.891588	915.774341	10.800103
9.641755	909.950780	10.805107
9.798267	900.943034	10.810112
10.002391	922.083789	10.815117
10.258073	932.888318	10.820122
10.209542	931.386847	10.825127
9.950508	944.432446	10.830131
10.078525	941.628567	10.835136
9.986173	949.832883	10.840141
10.515903	938.543537	10.845146
10.233331	951.512467	10.850151
10.530584	972.040742	10.855155
10.763564	967.949020	10.860160
10.835058	976.843196	10.865165
11.070558	975.094558	10.870170
11.007187	973.895088	10.875175
10.945348	979.001972	10.880179
10.862036	977.206405	10.885184
10.715992	984.192364	10.890189
10.426795	978.854475	10.895194
10.577966	985.334110	10.900199
10.712715	978.493493	10.905203
11.059257	979.800803	10.910208
10.936396	997.259379	10.915213
11.428296	1011.251351	10.920218
11.782859	1013.965688	10.925223
11.475097	1014.568333	10.930227
11.581241	1003.007432	10.935232
11.639569	1003.505953	10.940237
11.340018	1002.760490	10.945242
11.321397	1005.236284	10.950247
11.423317	1011.165512	10.955251
11.482958	1005.978568	10.960256
11.363744	1010.515838	10.965261
11.820198	1017.828367	10.970266
11.953653	1016.646389	10.975271
11.520849	1016.918873	10.980275
11.767503	1019.223042	10.985280
11.889659	1031.463554	10.990285
12.071191	1031.382573	10.995290
12.116134	1037.372941	11.000295
11.746923	1031.256115	11.005299
12.328082	1029.554848	11.010304
11.798622	1033.315412	11.015309
12.347986	1044.047951	11.020314
12.382575	1041.079170	11.025319
12.184984	1034.966511	11.030323
12.264188	1027.251582	11.035328
12.075238	1031.462492	11.040333
12.185426	1047.048272	11.045338
12.230009	1046.191145	11.050343
12.229023	1047.826720	11.055347
12.565340	1044.915477	11.060352
12.171495	1061.330762	11.065357
12.497547	1053.021326	11.070362
12.613709	1048.465636	11.075367
12.392403	1061.030629	11.080371
12.472077	1057.532649	11.085376
12.542693	1060.364828	11.090381
12.387920	1048.531672	11.095386
12.665033	1051.520160	11.100391
12.438641	1063.163390	11.105395
13.050175	1056.114220	11.110400
12.711521	1069.011770	11.115405
13.106941	1067.750157	11.120410
13.071229	1067.774792	11.125415
12.836548	1073.491209	11.130419
12.917592	1069.150861	11.135424
12.768400	1074.741673	11.140429
13.120008	1069.613802	11.145434
12.974880	1072.743761	11.150439
12.888736	1076.469902	11.155443
13.114743	1080.483747	11.160448
13.371556	1098.209916	11.165453
13.266266	1114.923037	11.170458
13.915239	1118.935669	11.175463
13.676096	1130.178837	11.180467
13.500447	1117.931032	11.185472
13.525331	1127.201767	11.190477
13.632059	1127.080673	11.195482
13.778115	1128.994023	11.200487
13.942606	1126.389309	11.205491
14.064098	1119.921350	11.210496
13.614665	1117.032906	11.215501
13.765441	1120.420053	11.220506
13.902605	1125.946287	11.225511
13.885843	1137.929906	11.230515
14.196941	1114.079312	11.235520
13.835764	1117.962878	11.240525
13.716786	1103.654293	11.245530
13.871428	1107.346769	11.250535
13.855020	1111.397710	11.255539
13.956314	1103.489970	11.260544
13.805598	1099.063568	11.265549
14.215759	1102.584393	11.270554
13.974825	1107.913864	11.275559
13.977094	1141.590055	11.280563
14.625781	1144.809479	11.285568
14.215594	1147.771979	11.290573
14.213646	1141.006709	11.295578
14.603755	1142.868519	11.300583
14.521297	1147.169718	11.305587
14.500936	1144.887817	11.310592
14.444047	1143.723571	11.315597
14.529854	1146.957072	11.320602
14.416454	1142.680833	11.325607
14.517542	1148.641791	11.330611
14.806638	1161.827258	11.335616
14.844563	1182.149592	11.340621
14.853087	1176.772030	11.345626
15.379568	1175.363340	11.350631
15.180490	1173.961554	11.355635
15.122946	1178.719292	11.360640
14.953364	1180.692453	11.365645
14.938593	1182.264005	11.370650
15.494326	1193.227468	11.375655
15.419171	1198.787594	11.380659
15.686264	1197.248372	11.385664
15.740586	1202.587561	11.390669
15.778039	1186.653221	11.395674
15.459233	1179.326567	11.400679
15.416284	1176.759661	11.405683
15.661610	1169.995942	11.410688
15.161668	1168.449740	11.415693
15.634114	1172.503159	11.420698
15.595083	1182.485917	11.425703
15.425657	1181.757540	11.430707
15.806700	1171.480550	11.435712
15.463357	1190.239329	11.440717
15.511594	1185.079373	11.445722
15.603467	1184.052259	11.450727
15.235872	1186.563241	11.455731
15.692742	1195.732002	11.460736
15.825072	1204.887871	11.465741
15.875040	1210.661451	11.470746
16.152709	1210.353809	11.475751
16.025443	1219.691450	11.480755
16.722948	1219.208030	11.485760
16.220798	1221.000832	11.490765
16.156715	1219.643748	11.495770
16.537439	1220.945629	11.500775
16.410191	1224.091693	11.505779
16.587855	1212.626460	11.510784
16.578944	1227.502823	11.515789
16.559596	1216.289798	11.520794
16.480107	1223.486046	11.525799
16.741372	1232.012619	11.530803
17.102571	1230.855807	11.535808
16.489150	1226.233483	11.540813
16.785052	1224.183424	11.545818
16.805964	1225.916459	11.550823
16.247838	1215.158401	11.555827
16.651936	1220.482814	11.560832
16.686187	1222.958098	11.565837
16.430334	1229.931723	11.570842
16.877627	1231.432739	11.575847
16.690049	1242.182030	11.580851
17.258586	1232.524848	11.585856
17.084432	1243.885481	11.590861
17.045767	1239.756578	11.595866
17.278106	1236.652131	11.600871
17.121590	1236.077822	11.605875
17.369027	1231.050095	11.610880
17.489482	1231.087673	11.615885
17.190132	1232.482251	11.620890
17.278703	1233.994745	11.625895
17.143527	1246.688097	11.630899
17.432897	1255.768484	11.635904
17.396140	1266.003268	11.640909
17.510202	1274.494992	11.645914
17.837498	1266.784526	11.650919
17.700458	1269.976320	11.655923
17.877971	1266.137808	11.660928
17.811210	1277.463991	11.665933
17.725333	1270.920220	11.670938
17.747544	1270.686439	11.675943
17.658471	1271.449772	11.680947
18.028830	1267.511111	11.685952
17.603048	1270.670103	11.690957
17.712292	1275.369729	11.695962
18.075166	1271.679862	11.700967
17.772163	1269.980804	11.705971
18.162088	1265.975941	11.710976
17.976175	1285.291673	11.715981
18.206808	1292.168813	11.720986
18.228525	1298.845868	11.725991
18.186010	1305.479551	11.730995
18.422007	1299.300780	11.736000
18.543941	1309.423545	11.741005
18.543738	1312.338037	11.746010
18.706385	1306.375982	11.751015
18.640663	1298.873274	11.756019
18.690079	1301.787734	11.761024
18.734366	1306.311635	11.766029
18.781280	1306.854569	11.771034
18.857019	1304.394876	11.776039
18.838331	1304.506690	11.781043
18.947300	1293.601173	11.786048
18.776620	1305.858658	11.791053
18.457805	1296.070125	11.796058
18.556459	1284.771990	11.801063
18.349049	1282.430007	11.806067
18.461157	1281.558943	11.811072
18.341595	1291.543579	11.816077
18.882744	1297.511690	11.821082
19.015435	1306.125050	11.826087
18.563909	1312.544826	11.831091
18.977733	1303.144105	11.836096
18.804102	1316.173259	11.841101
18.809119	1309.947738	11.846106
19.438648	1332.369646	11.851111
19.514108	1345.124114	11.856115
19.620368	1337.092443	11.861120
19.220801	1336.265134	11.866125
19.128406	1342.061472	11.871130
19.349157	1345.428049	11.876135
19.078781	1352.214798	11.881139
19.469270	1344.896369	11.886144
19.356030	1352.695779	11.891149
19.403515	1363.467598	11.896154
20.071896	1364.001309	11.901159
19.774219	1375.176723	11.906163
20.194197	1376.177443	11.911168
19.877094	1373.649496	11.916173
20.214361	1373.026392	11.921178
20.347708	1373.252741	11.926183
20.116730	1374.571767	11.931187
20.449358	1360.025309	11.936192
20.440955	1359.342209	11.941197
19.953627	1350.980967	11.946202
20.176617	1359.584688	11.951207
20.029452	1373.183732	11.956211
20.380309	1365.526232	11.961216
20.250391	1369.016557	11.966221
20.757929	1372.925654	11.971226
20.444642	1370.775599	11.976231
20.288298	1387.189643	11.981235
20.430708	1376.150986	11.986240
20.520216	1381.177097	11.991245
20.790243	1372.743941	11.996250
20.763297	1374.273297	12.001255
20.580727	1378.659922	12.006259
20.423082	1369.930670	12.011264
20.670114	1382.779242	12.016269
20.873350	1372.016341	12.021274
20.740674	1372.288273	12.026279
20.484062	1381.634031	12.031283
20.695813	1376.455814	12.036288
20.819877	1383.354725	12.041293
21.103303	1396.525540	12.046298
21.181040	1391.040657	12.051303
20.887495	1389.789546	12.056307
20.898532	1378.137851	12.061312
20.839540	1373.994804	12.066317
21.015004	1374.498313	12.071322
20.680649	1375.922143	12.076327
20.723149	1384.387494	12.081331
20.693925	1373.346249	12.086336
20.770960	1382.482662	12.091341
20.906358	1391.928344	12.096346
20.960219	1386.876239	12.101351
20.630965	1384.269796	12.106355
21.178811	1382.569074	12.111360
20.728480	1390.863851	12.116365
21.049986	1393.171914	12.121370
21.130119	1384.056193	12.126375
20.734609	1389.399380	12.131379
20.766316	1389.567818	12.136384
21.037280	1385.878388	12.141389
20.814025	1386.585850	12.146394
21.048653	1391.115692	12.151399
20.918683	1397.148300	12.156403
21.339073	1393.832463	12.161408
21.315308	1391.775013	12.166413
21.174385	1389.752020	12.171418
21.146969	1389.529307	12.176423
20.918751	1394.058846	12.181427
21.367298	1386.289553	12.186432
21.153354	1382.748431	12.191437
20.887212	1379.415925	12.196442
21.151501	1373.514909	12.201447
20.670368	1366.855924	12.206451
20.820340	1355.451770	12.211456
20.904505	1359.947248	12.216461
20.616919	1366.922846	12.221466
21.181429	1348.601722	12.226471
20.843680	1367.492311	12.231475
21.183111	1356.198300	12.236480
21.250180	1354.552181	12.241485
21.013394	1360.970848	12.246490
21.270172	1349.196398	12.251495
20.885631	1368.731593	12.256499
21.270113	1353.268469	12.261504
21.036284	1362.601118	12.266509
20.708233	1366.798036	12.271514
20.928570	1359.703873	12.276519
21.072198	1362.843038	12.281523
20.881502	1374.610144	12.286528
20.917112	1355.307255	12.291533
20.620161	1365.380163	12.296538
20.962041	1365.164789	12.301543
20.579331	1372.067243	12.306547
20.974555	1363.743446	12.311552
20.840192	1367.803808	12.316557
20.552764	1369.611270	12.321562
21.140246	1360.853077	12.326567
21.001331	1361.950820	12.331571
20.810343	1364.301189	12.336576
20.813186	1371.227313	12.341581
20.839737	1361.952981	12.346586
21.227110	1360.596427	12.351591
20.693309	1369.647312	12.356595
20.957942	1358.294260	12.361600
20.952054	1369.823712	12.366605
20.879128	1370.768994	12.371610
21.206862	1373.500296	12.376615
20.584153	1359.503632	12.381619
20.455238	1354.076955	12.386624
20.841611	1366.557908	12.391629
20.770653	1371.917140	12.396634
21.124120	1378.795233	12.401639
21.013525	1372.726908	12.406643
21.096438	1363.096626	12.411648
21.038391	1366.148098	12.416653
20.904531	1350.958475	12.421658
20.943774	1347.104145	12.426663
20.769178	1350.499081	12.431667
20.779499	1339.934143	12.436672
20.633534	1344.319651	12.441677
20.603031	1374.656614	12.446682
21.158274	1374.072868	12.451687
21.121468	1379.450312	12.456691
20.882398	1358.517938	12.461696
21.141730	1357.662816	12.466701
21.084042	1355.240167	12.471706
20.818919	1352.830100	12.476711
20.809663	1349.742082	12.481715
20.808947	1354.667447	12.486720
20.839236	1349.589150	12.491725
20.708224	1348.572338	12.496730
20.900244	1341.246138	12.501735
20.708469	1348.487167	12.506739
20.726100	1347.796761	12.511744
20.900289	1351.465680	12.516749
20.690407	1355.328331	12.521754
20.860743	1368.531351	12.526759
21.069180	1383.165033	12.531763
20.979900	1364.520771	12.536768
20.758204	1365.330494	12.541773
20.612067	1362.581299	12.546778
21.034216	1375.086518	12.551783
20.697341	1390.188835	12.556787
21.184326	1378.406032	12.561792
21.084642	1364.433187	12.566797
20.763759	1361.465838	12.571802
20.772408	1353.433956	12.576807
21.155744	1361.890669	12.581811
20.935528	1359.225836	12.586816
21.004960	1353.999357	12.591821
21.019491	1356.775878	12.596826
21.078426	1350.197936	12.601831
20.891612	1356.083461	12.606835
21.039585	1347.709213	12.611840
21.045960	1356.680246	12.616845
20.721756	1361.210891	12.621850
21.086996	1358.878496	12.626855
20.848221	1367.078012	12.631859
20.733448	1347.620908	12.636864
20.699600	1359.607434	12.641869
20.747198	1355.419005	12.646874
20.998463	1355.692785	12.651879
21.009205	1358.047252	12.656883
21.021031	1356.293240	12.661888
21.117209	1368.470365	12.666893
21.149911	1360.967697	12.671898
21.181567	1352.586765	12.676903
21.048485	1359.635496	12.681907
21.292257	1352.777316	12.686912
21.002499	1345.788171	12.691917
21.011459	1338.516402	12.696922
21.229049	1325.726271	12.701927
20.907838	1333.115679	12.706931
20.982874	1334.188760	12.711936
20.929340	1331.634554	12.716941
20.601154	1329.873266	12.721946
20.863522	1334.277232	12.726951
20.785920	1328.750910	12.731955
20.860550	1327.972560	12.736960
20.792506	1330.148762	12.741965
20.936460	1334.025942	12.746970
21.002421	1326.663079	12.751975
21.044242	1331.226808	12.756979
20.877027	1325.904030	12.761984
20.796084	1334.067316	12.766989
20.918749	1336.922789	12.771994
20.795878	1339.593477	12.776999
20.796069	1334.516832	12.782003
20.587848	1333.398786	12.787008
20.923741	1332.394248	12.792013
20.889182	1341.761339	12.797018
20.836880	1332.411286	12.802023
20.733201	1341.745243	12.807027
20.799089	1334.494361	12.812032
21.054222	1327.675385	12.817037
20.910504	1344.677196	12.822042
20.825830	1326.448598	12.827047
20.719167	1341.536227	12.832051
20.510121	1341.668939	12.837056
20.916584	1336.035446	12.842061
21.001714	1347.695456	12.847066
20.924862	1337.335249	12.852071
20.394159	1340.462100	12.857075
20.698926	1359.502537	12.862080
20.899330	1366.587977	12.867085
20.801820	1365.341875	12.872090
21.021369	1372.999902	12.877095
20.816149	1382.122979	12.882099
20.677783	1384.854499	12.887104
20.717717	1381.184570	12.892109
20.213521	1381.124639	12.897114
20.844951	1380.957709	12.902119
20.679217	1377.088751	12.907123
20.526461	1376.974345	12.912128
20.918504	1375.935616	12.917133
20.861489	1381.120725	12.922138
20.971733	1383.076094	12.927143
20.697305	1383.671859	12.932147
20.982602	1380.450117	12.937152
20.945447	1382.659249	12.942157
20.788273	1386.772144	12.947162
21.141559	1381.599740	12.952167
20.793320	1384.339499	12.957171
20.979625	1385.672405	12.962176
21.121110	1384.664174	12.967181
21.045865	1380.495330	12.972186
21.404912	1375.222652	12.977191
21.035676	1381.429044	12.982195
21.222589	1378.142562	12.987200
21.409590	1359.935254	12.992205
20.890539	1356.496421	12.997210
21.206462	1345.078425	13.002215
20.736682	1348.331189	13.007219
20.872831	1346.779718	13.012224
20.927868	1347.341860	13.017229
20.927522	1350.472442	13.022234
20.975994	1348.657388	13.027239
20.835664	1356.828581	13.032243
20.848755	1353.158208	13.037248
20.983092	1346.957781	13.042253
20.637674	1360.213086	13.047258
20.837806	1351.688580	13.052263
20.807606	1354.451732	13.057267
20.965833	1350.259854	13.062272
21.271549	1343.215166	13.067277
20.996600	1351.994501	13.072282
21.155794	1346.338935	13.077287
20.966313	1351.335409	13.082291
21.229317	1348.614011	13.087296
21.288232	1354.392530	13.092301
20.894305	1349.941756	13.097306
20.833420	1328.946310	13.102311
20.521816	1331.640790	13.107315
20.852181	1340.244723	13.112320
21.052679	1354.583151	13.117325
20.786170	1354.272404	13.122330
20.973605	1353.893989	13.127335
20.726977	1355.505693	13.132339
21.125890	1363.776981	13.137344
20.859855	1336.867054	13.142349
20.971780	1338.741718	13.147354
20.784091	1328.697263	13.152359
20.833180	1328.411883	13.157363
20.755674	1332.598796	13.162368
20.672837	1341.167698	13.167373
20.679833	1351.662091	13.172378
21.014713	1349.727234	13.177383
20.985269	1361.205238	13.182387
21.013272	1355.892318	13.187392
20.805924	1344.824306	13.192397
20.573074	1357.605878	13.197402
20.815612	1347.685198	13.202407
21.028557	1365.347722	13.207411
20.934516	1350.219563	13.212416
21.131155	1363.009918	13.217421
20.779832	1349.469915	13.222426
20.683762	1354.670707	13.227431
20.581683	1360.348738	13.232435
20.840145	1371.902268	13.237440
21.083762	1365.277516	13.242445
20.793890	1362.158551	13.247450
21.050557	1362.876209	13.252455
21.027487	1379.486626	13.257459
20.747166	1350.804727	13.262464
21.137677	1352.087713	13.267469
20.930015	1348.887825	13.272474
20.991097	1330.430955	13.277479
20.761587	1330.756181	13.282483
20.713862	1336.655788	13.287488
20.906678	1340.447900	13.292493
20.788388	1338.643673	13.297498
20.901243	1344.038239	13.302503
20.834791	1340.104567	13.307507
20.888235	1348.009864	13.312512
20.525310	1348.353214	13.317517
20.706156	1359.188923	13.322522
21.135939	1361.359853	13.327527
21.201731	1367.810696	13.332531
20.888775	1354.065857	13.337536
20.700640	1339.769647	13.342541
20.645083	1358.766617	13.347546
21.066908	1359.439008	13.352551
20.952441	1358.003207	13.357555
20.708725	1363.829996	13.362560
21.174569	1355.733080	13.367565
20.730268	1354.892402	13.372570
20.846550	1342.769749	13.377575
21.044018	1341.978116	13.382579
20.667971	1341.251142	13.387584
20.836178	1346.586414	13.392589
20.792456	1358.746417	13.397594
20.961234	1363.217361	13.402599
20.877744	1367.843669	13.407603
20.937298	1362.793819	13.412608
20.823697	1350.187386	13.417613
20.556141	1350.231651	13.422618
21.060338	1346.880378	13.427623
20.889580	1361.714877	13.432627
21.004984	1360.783354	13.437632
21.171025	1352.147579	13.442637
20.624318	1348.710005	13.447642
20.961644	1341.835332	13.452647
20.649624	1345.160714	13.457651
20.782671	1344.611186	13.462656
21.182753	1353.577777	13.467661
20.809555	1358.392225	13.472666
20.937037	1344.089830	13.477671
20.767702	1355.536520	13.482675
20.702379	1344.963140	13.487680
20.801724	1346.177436	13.492685
20.913927	1358.722612	13.497690
21.185731	1350.062085	13.502695
21.256303	1352.968451	13.507699
21.023699	1353.051300	13.512704
21.197787	1351.943246	13.517709
20.621847	1344.730064	13.522714
20.896895	1352.106393	13.527719
20.794348	1348.632675	13.532723
20.734164	1349.992273	13.537728
20.716290	1342.707434	13.542733
20.691832	1350.327088	13.547738
20.782063	1348.096909	13.552743
20.733536	1345.351075	13.557747
21.068064	1342.717627	13.562752
20.890581	1345.557889	13.567757
20.813436	1341.804132	13.572762
20.958714	1346.140036	13.577767
20.786723	1346.820395	13.582771
20.898781	1339.866524	13.587776
20.894720	1339.999661	13.592781
20.754268	1343.425423	13.597786
20.979945	1343.029870	13.602791
20.971933	1350.381951	13.607795
20.989463	1352.311099	13.612800
20.961428	1344.398622	13.617805
20.574786	1351.098250	13.622810
21.007479	1347.625907	13.627815
21.182630	1341.209221	13.632819
21.099537	1350.164554	13.637824
20.916355	1351.780332	13.642829
20.632860	1357.487296	13.647834
20.639138	1344.420165	13.652839
21.036476	1358.776092	13.657843
21.053704	1354.999395	13.662848
21.353357	1344.817274	13.667853
21.172012	1348.577593	13.672858
21.192943	1345.353864	13.677863
21.065601	1346.170616	13.682867
21.084758	1349.332783	13.687872
21.157811	1346.014002	13.692877
21.075494	1337.771113	13.697882
21.085590	1320.151934	13.702887
20.978904	1315.554426	13.707891
20.920008	1322.357899	13.712896
20.923745	1316.837534	13.717901
20.721782	1322.260224	13.722906
20.725924	1319.822987	13.727911
20.607893	1322.555984	13.732915
20.612259	1316.084539	13.737920
20.917917	1322.683201	13.742925
20.629547	1327.149768	13.747930
20.811620	1334.894183	13.752935
21.080530	1349.104990	13.757939
20.966462	1344.600121	13.762944
20.622680	1333.194303	13.767949
20.764107	1335.969506	13.772954
20.816112	1353.449509	13.777959
20.955394	1350.847199	13.782963
20.953803	1353.400768	13.787968
20.970865	1351.109712	13.792973
20.851822	1350.444259	13.797978
20.613883	1346.287179	13.802983
20.854910	1357.143252	13.807987
20.876874	1360.981544	13.812992
20.959724	1353.912466	13.817997
20.937198	1358.604748	13.823002
20.897166	1355.313463	13.828007
20.790871	1352.587880	13.833011
20.877048	1350.337845	13.838016
21.010875	1353.536923	13.843021
20.493747	1343.489803	13.848026
20.931826	1342.949977	13.853031
20.631991	1359.856847	13.858035
20.779097	1357.724836	13.863040
20.859854	1366.150957	13.868045
20.743788	1359.744436	13.873050
20.819817	1364.242790	13.878055
20.810615	1373.397682	13.883059
20.898618	1362.217891	13.888064
20.699917	1356.534239	13.893069
20.685013	1359.539401	13.898074
21.231718	1355.870662	13.903079
20.840535	1360.820454	13.908083
20.639387	1363.774890	13.913088
21.321056	1352.812684	13.918093
20.768958	1364.937069	13.923098
21.104766	1361.596879	13.928103
20.811064	1363.048920	13.933107
20.986450	1362.439018	13.938112
20.953139	1362.520046	13.943117
20.967508	1369.239310	13.948122
20.995148	1360.780159	13.953127
20.980653	1363.163885	13.958131
20.751062	1353.752199	13.963136
21.064439	1343.727176	13.968141
21.170521	1348.291701	13.973146
21.228727	1342.819414	13.978151
21.204617	1341.285618	13.983155
20.956593	1340.082449	13.988160
21.607989	1326.923482	13.993165
20.907865	1345.177922	13.998170
20.916361	1336.146202	14.003175
21.081897	1340.598732	14.008179
21.176988	1348.260825	14.013184
21.173044	1332.194144	14.018189
20.854843	1316.593072	14.023207
20.835625	1310.203247	14.028224
20.703053	1315.748983	14.033242
20.795503	1322.106711	14.038259
21.142724	1322.312475	14.043277
21.004234	1318.384629	14.048295
20.981254	1311.548656	14.053312
20.717011	1312.525211	14.058330
20.912401	1331.331435	14.063347
20.897505	1340.522067	14.068365
20.744681	1337.412921	14.073383
20.970563	1340.754270	14.078400
20.958055	1340.178966	14.083418
21.022197	1341.483830	14.088435
21.234441	1337.213743	14.093453
20.945765	1346.935693	14.098471
21.115811	1345.134175	14.103488
21.290622	1343.490776	14.108506
20.959005	1348.201514	14.113523
21.328326	1349.346018	14.118541
21.111139	1349.097521	14.123559
21.164092	1342.768532	14.128576
21.124383	1344.067936	14.133594
20.879277	1345.552686	14.138611
21.242881	1346.753158	14.143629
21.051823	1345.024963	14.148647
21.128468	1345.826027	14.153664
21.235823	1349.269654	14.158682
21.013633	1365.207189	14.163699
21.439874	1371.080683	14.168717
21.327420	1379.335196	14.173735
21.394888	1378.059707	14.178752
21.443615	1383.051149	14.183770
21.222924	1383.193330	14.188787
21.735819	1373.333377	14.193805
21.452831	1383.038713	14.198823
21.232353	1381.629819	14.203840
21.262798	1384.816726	14.208858
21.020345	1388.427841	14.213875
21.091938	1379.673343	14.218893
21.034477	1398.035477	14.223911
21.288753	1407.529295	14.228928
21.311640	1407.417119	14.233946
21.332498	1421.442429	14.238963
21.380202	1414.461423	14.243981
21.296228	1409.068196	14.248999
21.327013	1416.658074	14.254016
21.648213	1415.724369	14.259034
21.671601	1427.145853	14.264051
21.979226	1434.488661	14.269069
21.502485	1430.424391	14.274087
21.659274	1445.022664	14.279104
22.032129	1449.421298	14.284122
21.823288	1445.130247	14.289139
22.107958	1441.767253	14.294157
21.700102	1434.136855	14.299175
21.374159	1440.083150	14.304192
21.943382	1443.225041	14.309210
22.195619	1448.435739	14.314227
22.480697	1443.225893	14.319245
22.114467	1426.616065	14.324263
22.088792	1414.027759	14.329280
22.062051	1419.035970	14.334298
21.877219	1420.165039	14.339315
22.065193	1413.331553	14.344333
21.704250	1423.132721	14.349351
21.691598	1419.088821	14.354368
22.026929	1427.479589	14.359386
21.973227	1441.373661	14.364403
22.102135	1440.439162	14.369421
21.838216	1448.297861	14.374439
21.877566	1445.368833	14.379456
22.257332	1449.130843	14.384474
21.995975	1455.567081	14.389491
22.435439	1441.410148	14.394509
22.043556	1452.603719	14.399527
22.194776	1453.513235	14.404544
22.369408	1449.684069	14.409562
21.918717	1445.486648	14.414579
22.519963	1444.368274	14.419597
22.309536	1446.166836	14.424615
22.465239	1451.348886	14.429632
22.571718	1445.058508	14.434650
22.260769	1454.099795	14.439667
22.319901	1449.474986	14.444685
22.220040	1448.482589	14.449703
21.827683	1455.477710	14.454720
22.263662	1451.517196	14.459738
22.128945	1475.062437	14.464755
22.350275	1476.699330	14.469773
22.430120	1483.716684	14.474791
22.418347	1477.110088	14.479808
22.653762	1475.847131	14.484826
22.611833	1490.344219	14.489843
22.629468	1480.978474	14.494861
22.675705	1481.137861	14.499879
22.381666	1484.228673	14.504896
22.403518	1483.225513	14.509914
22.380643	1482.375783	14.514931
22.770294	1483.457279	14.519949
22.521036	1488.769212	14.524967
22.580579	1484.749960	14.529984
22.840063	1476.523879	14.535002
22.789120	1483.779177	14.540019
23.043566	1479.498385	14.545037
23.070927	1473.835686	14.550055
22.929038	1483.660162	14.555072
23.000377	1472.832335	14.560090
22.755857	1474.652856	14.565107
23.176103	1468.719065	14.570125
22.952709	1481.557964	14.575143
22.878411	1481.172627	14.580160
23.291377	1471.518888	14.585178
23.142761	1484.157094	14.590195
22.919634	1478.151299	14.595213
23.117015	1482.883106	14.600231
23.107402	1480.380318	14.605248
23.419438	1474.897953	14.610266
23.460437	1476.847547	14.615283
23.235025	1471.844168	14.620301
22.916805	1455.019791	14.625319
23.052419	1462.365664	14.630336
23.462644	1464.240639	14.635354
22.651182	1468.202081	14.640371
22.975522	1473.579833	14.645389
23.003684	1472.850955	14.650407
23.058985	1483.864687	14.655424
23.336923	1468.578066	14.660442
23.005381	1474.397062	14.665459
23.042030	1475.560813	14.670477
23.211842	1481.495699	14.675495
23.089985	1472.031868	14.680512
23.299302	1463.596711	14.685530
23.173788	1473.195978	14.690547
23.513623	1478.457213	14.695565
23.266726	1470.355158	14.700583
23.134563	1480.193810	14.705600
23.453608	1471.468220	14.710618
23.606851	1470.544783	14.715635
23.635525	1469.039512	14.720653
23.547581	1474.578190	14.725671
23.594556	1482.225296	14.730688
23.556433	1472.516081	14.735706
23.524416	1476.912440	14.740723
23.349432	1472.951832	14.745741
23.538396	1483.061751	14.750759
23.945219	1502.386624	14.755776
24.159540	1485.142998	14.760794
23.937323	1469.150394	14.765811
23.826260	1471.606388	14.770829
23.983287	1473.554780	14.775847
23.647342	1478.665810	14.780864
23.838785	1467.808607	14.785882
23.729208	1480.306872	14.790899
23.414848	1474.842610	14.795917
23.510887	1459.784789	14.800935
23.377293	1465.645359	14.805952
24.154624	1478.038351	14.810970
24.076662	1479.515333	14.815987
23.485055	1471.220496	14.821005
23.709413	1480.564973	14.826023
23.855393	1496.793942	14.831040
24.165993	1503.324603	14.836058
23.939509	1517.155065	14.841075
23.785448	1504.850647	14.846093
24.274846	1498.642326	14.851111
23.906431	1509.921076	14.856128
24.289577	1498.735964	14.861146
24.316254	1503.946476	14.866163
24.154569	1504.421392	14.871181
24.276425	1498.192249	14.876199
23.830924	1500.873838	14.881216
24.280211	1492.742537	14.886234
24.021547	1503.696242	14.891251
24.058728	1505.283855	14.896269
24.310584	1501.243365	14.901287
24.180960	1514.610050	14.906304
24.158871	1505.193994	14.911322
24.131982	1510.425636	14.916339
23.992036	1512.385218	14.921357
24.075635	1508.800225	14.926375
23.908383	1510.334710	14.931392
24.086038	1508.075766	14.936410
24.125251	1510.273410	14.941427
24.147535	1514.762584	14.946445
24.370483	1531.164153	14.951463
24.398921	1532.476301	14.956480
24.686762	1532.923569	14.961498
24.745796	1541.970399	14.966515
24.724374	1534.001453	14.971533
24.468172	1508.030671	14.976551
24.438452	1500.341502	14.981568
24.956516	1498.648847	14.986586
24.422357	1496.737033	14.991603
24.393692	1502.201771	14.996621
25.098787	1513.407630	15.001639
24.895677	1509.032272	15.006656
24.640373	1501.370429	15.011674
24.526460	1501.996606	15.016691
24.627360	1504.162388	15.021709
24.907874	1509.564447	15.026727
24.748052	1514.591556	15.031744
25.035896	1501.511923	15.036762
24.730543	1504.525890	15.041779
24.793209	1500.692545	15.046797
25.003558	1500.533952	15.051815
24.898940	1509.204154	15.056832
24.629199	1508.665151	15.061850
24.627665	1519.737527	15.066867
25.133595	1530.283794	15.071885
24.938361	1526.268197	15.076903
24.761308	1537.733534	15.081920
25.247072	1532.120403	15.086938
24.985382	1536.591951	15.091955
24.743879	1538.753357	15.096973
25.230317	1530.889039	15.101991
24.889471	1532.356041	15.107008
25.053318	1531.349895	15.112026
24.907755	1543.048536	15.117043
25.059765	1534.160779	15.122061
25.344630	1530.513793	15.127079
25.236721	1536.795027	15.132096
25.148971	1528.513395	15.137114
25.241347	1527.613033	15.142131
24.883633	1532.509682	15.147149
25.178932	1533.951521	15.152167
24.904876	1535.031119	15.157184
25.091965	1536.920454	15.162202
25.172459	1538.040250	15.167219
25.205838	1556.453378	15.172237
25.600980	1563.980502	15.177255
25.183592	1574.464053	15.182272
25.351506	1555.003404	15.187290
25.546627	1564.393498	15.192307
25.437712	1563.592880	15.197325
25.496911	1561.326865	15.202343
25.661919	1558.562610	15.207360
25.677848	1559.157857	15.212378
25.664640	1553.496878	15.217395
25.593941	1558.719794	15.222413
25.871446	1553.932703	15.227431
25.460369	1557.310408	15.232448
25.869624	1552.060269	15.237466
25.728320	1551.157847	15.242483
25.712069	1563.629501	15.247501
25.895348	1551.624400	15.252519
25.983854	1554.128019	15.257536
25.890829	1563.674184	15.262554
25.902820	1556.712964	15.267571
25.836978	1559.496040	15.272589
26.068600	1550.465010	15.277607
25.857387	1555.904611	15.282624
25.850091	1551.119684	15.287642
26.095423	1554.510680	15.292659
25.805142	1558.041371	15.297677
26.255475	1555.711402	15.302695
26.247877	1548.924775	15.307712
25.981984	1526.569663	15.312730
26.031450	1525.526702	15.317747
25.736782	1535.704353	15.322765
26.192924	1539.325214	15.327783
26.056620	1556.664247	15.332800
26.191228	1554.475085	15.337818
26.422085	1561.355916	15.342835
26.098726	1554.765158	15.347853
25.992098	1546.810581	15.352871
26.087468	1562.273739	15.357888
26.060969	1550.931329	15.362906
26.313225	1557.354124	15.367923
26.164069	1554.825600	15.372941
26.254639	1546.826202	15.377959
26.091548	1560.493219	15.382976
26.283567	1556.145281	15.387994
26.480307	1559.396944	15.393011
26.225934	1562.614371	15.398029
26.440087	1559.153268	15.403047
26.296661	1551.630077	15.408064
26.190227	1559.362254	15.413082
26.601483	1562.148680	15.418099
26.514236	1561.710348	15.423117
26.328431	1567.993007	15.428135
26.268743	1562.679224	15.433152
26.259924	1563.891134	15.438170
26.457579	1575.591693	15.443187
26.633285	1591.042855	15.448205
26.523687	1593.735385	15.453223
26.710033	1599.212274	15.458240
26.747809	1598.671414	15.463258
26.845286	1590.043228	15.468275
26.882199	1596.955795	15.473293
26.886576	1592.925648	15.478311
26.782979	1602.507346	15.483328
26.586519	1607.720449	15.488346
27.272938	1594.378956	15.493363
26.985021	1588.177374	15.498381
26.963129	1580.919513	15.503399
26.865507	1576.530457	15.508416
26.947554	1585.133180	15.513434
26.984377	1588.495301	15.518451
26.835062	1593.581324	15.523469
27.322778	1587.480204	15.528487
27.371172	1588.062408	15.533504
26.910363	1570.893321	15.538522
27.067021	1561.112867	15.543539
26.816491	1567.110896	15.548557
27.220132	1585.126795	15.553575
27.569942	1585.123718	15.558592
27.316701	1568.181875	15.563610
27.344125	1555.049343	15.568627
27.357601	1554.443931	15.573645
27.070734	1550.339905	15.578663
27.293330	1554.987487	15.583680
26.743611	1552.050137	15.588698
27.022027	1568.015023	15.593715
27.080016	1584.794546	15.598733
27.213866	1597.277684	15.603751
27.235927	1586.123351	15.608768
27.260588	1591.930416	15.613786
27.467507	1585.908688	15.618803
27.221114	1588.096836	15.623821
27.322114	1586.425069	15.628839
27.476662	1584.760493	15.633856
27.538038	1582.885039	15.638874
27.401682	1584.317859	15.643891
27.655502	1593.292755	15.648909
27.453533	1599.475755	15.653927
27.554283	1595.723617	15.658944
27.663475	1609.917499	15.663962
27.716627	1609.437110	15.668979
27.968982	1612.027870	15.673997
27.832099	1603.194011	15.679015
27.580307	1591.431306	15.684032
27.424015	1599.712598	15.689050
27.692332	1602.703521	15.694067
27.911648	1614.782131	15.699085
27.786567	1620.031046	15.704103
27.850040	1616.208554	15.709120
27.780398	1611.223543	15.714138
28.241416	1602.548381	15.719155
28.261175	1609.636730	15.724173
28.181179	1609.273535	15.729191
28.229856	1606.969076	15.734208
27.813032	1607.979423	15.739226
27.920067	1603.310743	15.744243
27.994788	1610.722248	15.749261
28.023976	1610.898513	15.754279
28.109491	1613.020359	15.759296
27.737702	1622.018754	15.764314
28.310526	1600.075626	15.769331
28.311166	1617.690992	15.774349
28.307879	1611.749184	15.779367
28.586762	1608.569554	15.784384
28.253527	1623.080985	15.789402
28.400924	1607.664021	15.794419
28.142856	1621.391076	15.799437
28.103944	1607.956818	15.804455
28.319591	1609.613511	15.809472
28.235733	1615.102825	15.814490
28.167687	1608.928304	15.819507
28.026654	1627.282032	15.824525
28.259801	1615.946140	15.829543
28.315188	1612.080892	15.834560
28.193054	1628.845933	15.839578
28.177186	1633.361679	15.844595
28.503158	1639.975684	15.849613
28.764160	1645.448549	15.854631
28.608914	1645.995591	15.859648
28.165108	1653.461500	15.864666
28.733702	1640.390453	15.869683
28.820107	1653.457744	15.874701
28.509555	1652.039592	15.879719
28.380500	1648.556123	15.884736
28.642458	1651.351434	15.889754
28.604034	1648.241278	15.894771
28.567276	1645.066361	15.899789
29.118539	1649.650544	15.904807
28.860886	1641.846636	15.909824
28.836245	1654.736576	15.914842
28.947179	1644.162654	15.919859
28.905413	1653.493055	15.924877
28.977321	1655.331560	15.929895
29.204278	1658.294483	15.934912
28.988179	1657.606126	15.939930
28.864059	1646.644955	15.944947
29.212569	1654.766328	15.949965
29.499899	1663.379617	15.954983
28.897193	1649.735564	15.960000
28.987075	1659.993549	15.965018
29.285971	1663.376813	15.970035
29.305310	1673.557965	15.975053
29.100817	1672.497292	15.980071
29.331875	1666.788660	15.985088
29.112325	1673.788572	15.990106
29.423027	1671.577600	15.995123
29.272930	1674.156262	16.000141
29.206495	1664.311428	16.005159
29.641104	1671.070149	16.010176
29.417640	1674.163903	16.015194
29.423946	1665.981241	16.020211
29.507506	1667.378209	16.025229
29.417070	1675.455551	16.030247
29.765832	1672.132622	16.035264
29.572685	1662.485758	16.040282
29.871639	1667.011868	16.045299
29.539550	1656.422074	16.050317
29.646856	1658.722143	16.055335
29.938553	1666.868315	16.060352
29.643161	1674.441918	16.065370
29.713251	1667.970836	16.070387
29.789604	1666.763908	16.075405
29.366340	1662.770483	16.080423
29.687890	1671.172243	16.085440
29.614218	1666.143810	16.090458
29.919438	1668.553108	16.095475
29.814581	1671.434454	16.100493
29.706252	1674.656929	16.105511
29.904197	1667.485879	16.110528
29.829528	1670.115434	16.115546
29.697054	1665.663479	16.120563
29.910516	1668.174718	16.125581
29.819011	1682.790021	16.130599
29.685515	1668.821781	16.135616
29.933387	1699.110006	16.140634
30.159596	1703.209621	16.145651
30.147771	1700.368145	16.150669
30.410632	1701.800231	16.155687
30.521247	1704.005394	16.160704
30.250272	1696.711692	16.165722
30.237176	1687.191046	16.170739
30.393228	1689.399972	16.175757
30.427425	1690.594020	16.180775
30.337696	1661.947315	16.185792
30.342340	1680.870933	16.190810
30.456656	1690.992903	16.195827
30.515324	1691.992704	16.200845
30.062576	1688.409833	16.205863
30.447763	1671.700332	16.210880
30.353829	1686.306587	16.215898
30.524529	1683.533536	16.220915
30.639428	1681.706951	16.225933
30.262146	1690.412881	16.230951
30.859152	1683.483360	16.235968
30.291426	1695.511372	16.240986
30.625639	1687.189095	16.246003
30.760315	1687.362695	16.251021
30.516892	1688.729227	16.256039
30.733608	1688.770974	16.261056
30.685329	1698.133118	16.266074
30.821689	1694.526294	16.271091
30.738447	1689.244537	16.276109
30.492303	1693.503644	16.281127
30.924765	1687.540289	16.286144
30.656602	1695.655425	16.291162
30.817191	1690.989975	16.296179
30.496261	1692.995748	16.301197
30.720924	1705.586411	16.306215
31.133961	1711.842841	16.311232
30.878517	1717.899133	16.316250
31.160409	1720.003833	16.321267
31.248465	1717.048892	16.326285
31.149074	1723.939211	16.331303
31.060054	1721.264993	16.336320
31.176357	1727.147950	16.341338
31.341288	1725.739691	16.346355
31.648055	1725.811123	16.351373
31.509035	1721.439637	16.356391
31.390359	1721.895901	16.361408
30.970893	1710.911782	16.366426
31.177429	1720.232514	16.371443
31.546143	1712.504859	16.376461
31.456611	1716.753153	16.381479
31.561937	1714.678754	16.386496
31.322598	1719.690299	16.391514
31.231870	1728.208971	16.396531
31.470943	1723.884941	16.401549
31.246257	1720.220070	16.406567
31.305953	1719.662338	16.411584
31.222399	1732.066215	16.416602
31.273336	1725.108928	16.421619
31.632958	1721.321765	16.426637
31.262325	1734.701132	16.431655
31.803323	1747.478919	16.436672
31.952337	1748.059240	16.441690
31.597380	1756.128474	16.446707
31.758715	1754.023114	16.451725
31.979453	1762.728097	16.456743
32.083489	1749.085284	16.461760
32.088462	1762.593546	16.466778
31.889606	1761.590172	16.471795
32.266838	1761.860376	16.476813
31.705148	1752.440552	16.481831
31.922700	1761.054016	16.486848
31.879377	1761.678384	16.491866
31.644649	1757.243496	16.496883
31.968096	1750.484994	16.501901
31.770073	1748.219858	16.506919
31.499881	1754.489313	16.511936
31.979717	1754.206724	16.516954
31.459338	1754.732561	16.521971
32.255130	1766.274956	16.526989
31.889942	1776.320081	16.532007
31.850909	1788.883655	16.537024
31.907839	1780.224069	16.542042
32.021860	1767.435417	16.547059
32.246299	1776.680967	16.552077
32.214172	1780.010868	16.557095
32.387167	1786.058636	16.562112
32.711229	1793.125285	16.567130
32.804373	1792.297147	16.572147
33.127808	1773.266818	16.577165
33.100693	1777.609001	16.582183
33.128306	1774.026580	16.587200
33.185524	1768.619354	16.592218
33.029618	1766.470200	16.597235
33.037770	1738.278880	16.602253
32.757419	1742.723577	16.607271
32.860273	1734.561660	16.612288
32.766698	1733.867916	16.617306
32.626529	1739.841334	16.622323
32.743512	1722.564972	16.627341
32.610174	1732.941984	16.632359
32.831411	1744.580713	16.637376
33.150752	1750.195333	16.642394
32.847391	1755.079453	16.647411
33.125373	1758.197076	16.652429
32.922938	1761.385026	16.657447
33.108775	1757.813556	16.662464
33.031393	1763.321556	16.667482
32.801433	1770.102153	16.672499
33.300830	1756.169751	16.677517
33.208184	1770.053043	16.682535
33.080956	1769.941208	16.687552
33.111698	1759.159758	16.692570
32.864393	1765.170724	16.697587
33.223647	1771.783414	16.702605
32.735500	1762.808055	16.707623
33.164259	1760.007205	16.712640
33.186867	1761.549190	16.717658
33.073478	1763.828629	16.722675
33.592243	1757.437755	16.727693
33.322902	1764.871176	16.732711
33.113676	1778.348330	16.737728
33.828968	1788.929041	16.742746
33.935632	1798.355419	16.747763
34.036358	1777.435118	16.752781
33.820135	1772.004643	16.757799
33.899945	1761.875283	16.762816
33.975870	1761.318895	16.767834
33.713889	1761.288329	16.772851
34.023587	1758.155665	16.777869
33.838537	1768.196438	16.782887
33.479819	1768.432998	16.787904
33.909610	1764.071461	16.792922
33.700084	1766.936483	16.797939
33.521750	1760.654425	16.802957
33.510850	1765.018401	16.807975
33.823407	1753.864803	16.812992
33.795513	1764.305248	16.818010
33.543158	1780.425808	16.823027
34.319724	1785.464126	16.828045
34.287126	1793.195664	16.833063
34.100230	1783.902458	16.838080
34.303943	1790.130955	16.843098
33.979301	1775.618912	16.848115
34.412490	1782.093967	16.853133
34.363029	1772.344672	16.858151
34.294271	1763.556483	16.863168
34.292976	1759.513036	16.868186
34.078780	1763.306148	16.873203
34.218622	1769.182222	16.878221
34.543639	1779.724491	16.883239
34.626119	1785.221949	16.888256
34.601516	1766.085893	16.893274
34.051062	1764.215966	16.898291
34.580554	1773.543431	16.903309
34.174542	1788.877570	16.908327
34.127189	1794.376860	16.913344
34.283807	1789.586950	16.918362
33.993538	1790.614092	16.923379
34.161642	1790.552689	16.928397
34.520853	1800.923557	16.933415
34.590729	1816.910964	16.938432
34.827465	1814.908407	16.943450
34.948135	1821.555238	16.948467
34.988330	1813.663621	16.953485
35.031248	1812.712138	16.958503
34.906293	1810.383426	16.963520
35.053575	1801.299622	16.968538
34.623925	1805.727248	16.973555
34.952072	1810.299874	16.978573
35.097535	1815.037711	16.983591
34.992425	1824.442822	16.988608
35.149448	1814.123350	16.993626
35.123025	1826.023452	16.998643
35.262631	1812.586490	17.003661
35.183399	1818.436958	17.008679
35.377568	1823.145793	17.013696
35.533081	1810.197894	17.018714
34.974620	1813.076887	17.023731
35.362625	1814.248341	17.028749
35.310348	1813.684081	17.033767
35.432100	1819.921730	17.038784
35.533668	1819.857566	17.043802
35.130362	1818.793981	17.048819
35.130341	1815.280455	17.053837
35.536791	1818.013426	17.058855
35.258522	1826.672970	17.063872
35.693516	1818.126109	17.068890
35.371665	1823.967293	17.073907
35.352743	1818.355102	17.078925
35.449638	1824.142088	17.083943
35.324430	1825.883843	17.088960
35.362196	1816.756145	17.093978
35.514163	1823.933630	17.098995
35.598321	1826.887900	17.104013
35.949382	1843.466816	17.109031
35.661322	1848.517637	17.114048
35.811623	1844.696182	17.119066
35.764915	1852.906655	17.124083
35.868974	1842.920458	17.129101
35.970178	1844.638691	17.134119
35.664755	1847.719595	17.139136
35.859051	1847.318941	17.144154
35.707888	1858.878721	17.149171
35.884274	1856.107877	17.154189
35.796366	1857.890881	17.159207
35.866423	1857.621732	17.164224
36.238602	1855.728924	17.169242
35.997896	1878.782817	17.174259
36.148632	1882.908679	17.179277
36.445557	1883.155512	17.184295
36.412429	1883.083728	17.189312
36.425639	1873.045928	17.194330
36.721545	1887.132434	17.199347
36.845781	1867.479334	17.204365
36.568401	1855.116417	17.209383
36.363834	1855.378732	17.214400
36.328753	1845.971607	17.219418
36.520873	1858.705241	17.224435
36.570271	1871.296470	17.229453
36.794839	1882.816796	17.234471
36.951012	1879.935907	17.239488
36.643018	1859.860939	17.244506
36.505953	1867.271742	17.249523
36.769750	1873.452152	17.254541
37.115665	1878.160400	17.259559
36.899288	1876.644616	17.264576
36.827664	1851.294266	17.269594
36.846576	1859.666534	17.274611
36.806323	1877.767749	17.279629
37.035062	1879.280019	17.284647
36.851468	1877.272913	17.289664
36.809796	1881.539578	17.294682
36.827353	1883.360038	17.299699
36.819572	1876.850157	17.304717
36.618221	1879.616364	17.309735
36.584093	1888.436793	17.314752
36.796567	1891.232177	17.319770
37.043506	1906.973568	17.324787
37.290383	1909.283667	17.329805
37.344854	1911.729065	17.334823
37.268668	1912.963546	17.339840
37.621248	1908.803842	17.344858
37.396352	1911.588755	17.349875
37.655127	1910.627223	17.354893
37.738587	1904.805177	17.359911
37.116057	1913.761936	17.364928
37.719088	1906.356268	17.369946
37.775549	1908.246036	17.374963
37.674254	1909.409798	17.379981
37.865846	1906.962943	17.384999
37.587313	1900.031374	17.390016
37.954852	1892.881933	17.395034
37.597720	1882.090674	17.400051
37.706763	1896.522401	17.405069
37.934030	1897.809952	17.410087
37.832358	1900.773423	17.415104
38.085450	1905.963701	17.420122
38.213305	1899.270147	17.425139
37.699859	1879.419051	17.430157
37.971999	1884.026589	17.435175
37.646898	1903.391646	17.440192
37.971374	1895.095188	17.445210
37.950100	1901.653002	17.450227
37.723319	1901.144885	17.455245
38.141556	1894.637057	17.460263
38.102318	1900.133520	17.465280
38.135463	1891.860716	17.470298
38.431931	1898.953055	17.475315
38.028752	1901.371545	17.480333
38.359822	1895.381017	17.485351
38.316461	1908.353609	17.490368
38.301528	1900.384214	17.495386
38.290597	1902.335856	17.500403
38.129086	1902.521301	17.505421
38.570218	1909.279096	17.510439
38.454061	1934.187588	17.515456
38.239173	1935.330926	17.520474
38.507771	1934.241190	17.525491
38.652502	1931.487179	17.530509
38.911403	1929.109815	17.535527
38.815472	1939.355944	17.540544
38.620658	1933.443764	17.545562
38.819440	1928.711582	17.550579
38.470398	1926.560957	17.555597
38.476989	1920.405864	17.560615
38.552718	1932.447073	17.565632
38.604157	1937.028475	17.570650
38.708857	1942.058377	17.575667
38.976030	1949.278116	17.580685
39.017058	1954.879783	17.585703
39.112443	1966.647308	17.590720
39.249599	1963.075687	17.595738
39.533757	1963.004427	17.600755
39.208515	1965.364090	17.605773
39.359283	1963.300501	17.610791
39.352466	1968.853957	17.615808
39.337302	1953.857409	17.620826
39.362269	1937.072912	17.625843
39.261685	1951.911743	17.630861
39.410295	1949.429261	17.635879
39.202335	1962.203982	17.640896
39.203336	1966.976706	17.645914
39.719764	1961.703039	17.650931
39.234825	1960.126250	17.655949
39.766346	1951.657518	17.660967
39.662362	1956.892177	17.665984
39.708316	1951.341952	17.671002
39.527576	1949.922730	17.676019
39.602220	1959.919858	17.681037
39.948280	1953.353511	17.686055
39.795657	1960.972136	17.691072
39.710005	1948.267083	17.696090
39.923563	1959.265375	17.701107
39.793893	1962.843698	17.706125
39.941458	1947.191953	17.711143
40.003116	1957.191937	17.716160
39.914914	1959.416262	17.721178
40.049272	1953.938459	17.726195
39.846168	1956.895308	17.731213
39.848757	1951.884502	17.736231
39.652299	1955.837653	17.741248
40.012595	1975.654316	17.746266
40.337211	1974.531260	17.751283
40.234684	1996.001971	17.756301
40.509431	1983.142663	17.761319
40.235845	1988.379998	17.766336
40.331751	1985.835125	17.771354
40.708321	1983.455504	17.776371
40.390494	1984.412329	17.781389
40.520418	1978.276083	17.786407
40.077961	1977.491667	17.791424
40.267440	1980.710761	17.796442
40.446509	1981.259556	17.801459
40.469219	1982.650529	17.806477
40.442479	1986.422454	17.811495
40.696883	1983.484978	17.816512
40.616351	1992.529963	17.821530
40.994473	2002.555018	17.826547
40.753905	2009.403488	17.831565
40.554027	2013.617553	17.836583
40.327803	2017.177465	17.841600
40.842286	2022.234856	17.846618
40.958653	2019.426360	17.851635
40.899647	2019.217907	17.856653
40.983252	2008.261876	17.861671
41.039119	2019.659768	17.866688
40.863841	2022.257451	17.871706
41.195126	2009.804410	17.876723
41.306250	2007.563866	17.881741
41.004710	2004.742579	17.886759
41.170896	2011.287850	17.891776
41.428295	2024.718342	17.896794
41.716682	2018.246113	17.901811
41.672446	2014.100898	17.906829
41.180109	2007.736668	17.911847
41.605810	2009.610036	17.916864
41.193191	2017.709846	17.921882
41.758767	2010.524833	17.926899
41.808394	2009.246629	17.931917
41.726186	2013.452939	17.936935
41.474387	2007.807811	17.941952
41.622422	2007.428689	17.946970
42.012448	2012.947190	17.951987
41.881105	2019.057750	17.957005
42.020782	2001.834071	17.962023
42.055064	2002.904641	17.967040
41.548631	2009.290536	17.972058
42.048725	2002.959168	17.977075
41.985369	2020.405890	17.982093
41.797320	2020.218803	17.987111
42.162202	2026.948699	17.992128
42.070117	2025.217221	17.997146
42.070848	2024.252788	18.002163
41.987140	2019.665524	18.007181
42.116262	2020.894801	18.012199
42.331764	2024.035031	18.017216
42.019712	2028.530490	18.022234
42.279115	2022.943051	18.027251
42.184090	2019.517777	18.032269
42.420103	2019.860851	18.037287
42.607309	2025.299223	18.042304
42.325947	2023.869297	18.047322
42.347345	2013.722335	18.052339
42.191511	2020.054680	18.057357
42.549186	2021.721021	18.062375
42.208761	2026.170664	18.067392
42.420640	2050.785562	18.072410
42.716940	2050.770572	18.077427
42.833778	2054.628950	18.082445
43.046788	2056.628274	18.087463
42.864412	2051.532880	18.092480
43.018263	2054.641262	18.097498
42.961223	2046.532987	18.102515
42.800118	2049.784412	18.107533
42.684481	2054.228104	18.112551
43.089982	2048.599263	18.117568
43.090034	2049.893175	18.122586
43.271538	2051.676497	18.127603
43.032729	2052.166088	18.132621
43.365592	2052.083915	18.137639
43.714796	2046.917117	18.142656
43.260497	2051.764054	18.147674
43.274303	2044.513641	18.152691
43.213052	2046.474113	18.157709
43.350225	2047.801216	18.162727
43.505990	2048.010787	18.167744
42.913826	2053.950231	18.172762
43.091478	2046.816842	18.177779
43.240893	2059.104399	18.182797
43.709760	2077.965510	18.187815
43.963473	2067.477845	18.192832
43.847319	2073.933670	18.197850
43.920942	2055.971647	18.202867
43.514559	2054.612783	18.207885
43.355729	2061.792759	18.212903
43.989577	2071.674038	18.217920
43.583694	2075.704668	18.222938
43.981790	2061.626101	18.227955
44.380047	2059.601685	18.232973
44.698139	2053.626534	18.237991
44.706134	2044.114876	18.243008
44.375973	2034.233980	18.248026
44.352446	2028.219720	18.253043
44.021848	2026.380765	18.258061
44.215808	2027.738138	18.263079
44.377819	2022.172524	18.268096
44.480485	2021.685012	18.273114
44.392144	2021.656641	18.278131
44.049422	2024.662513	18.283149
44.152165	2021.598196	18.288167
44.383835	2026.066720	18.293184
44.023127	2031.733272	18.298202
44.679948	2040.010988	18.303219
44.542826	2052.413455	18.308237
44.649948	2057.470541	18.313255
44.591883	2050.915114	18.318272
44.512099	2058.822643	18.323290
44.849668	2049.156954	18.328307
44.804426	2048.993499	18.333325
44.657984	2048.468630	18.338343
44.717223	2051.071392	18.343360
44.395945	2053.553141	18.348378
45.085970	2050.871031	18.353395
44.720532	2048.945601	18.358413
44.626681	2056.035768	18.363431
45.076872	2066.312875	18.368448
44.962785	2075.784077	18.373466
45.179199	2081.237477	18.378483
45.319425	2093.926894	18.383501
45.147369	2085.486916	18.388519
45.551873	2081.379450	18.393536
45.015469	2090.120431	18.398554
44.952073	2085.492937	18.403571
45.231071	2088.339890	18.408589
45.361500	2092.512312	18.413607
45.555911	2082.122977	18.418624
45.038581	2076.719170	18.423642
45.202368	2085.678054	18.428659
45.489999	2101.266078	18.433677
45.629466	2108.959330	18.438695
45.876148	2105.441785	18.443712
45.592670	2118.271946	18.448730
45.618113	2119.211790	18.453747
45.900973	2118.668794	18.458765
45.633717	2121.676022	18.463783
45.599859	2116.557706	18.468800
45.868209	2115.867575	18.473818
45.917464	2115.155753	18.478835
45.862559	2122.255472	18.483853
46.034341	2117.872841	18.488871
45.931450	2110.378291	18.493888
45.841038	2117.173761	18.498906
46.200697	2129.375148	18.503923
46.331713	2138.806515	18.508941
46.242331	2146.501674	18.513959
46.720298	2149.131277	18.518976
46.621403	2151.564991	18.523994
46.589097	2136.718864	18.529011
46.318312	2125.396874	18.534029
46.680664	2128.601018	18.539047
46.687001	2127.749737	18.544064
46.737196	2134.221534	18.549082
46.767981	2130.755719	18.554099
46.705728	2126.855609	18.559117
46.508810	2140.095947	18.564135
46.752824	2135.705724	18.569152
46.615645	2139.585758	18.574170
46.334970	2137.100916	18.579187
46.631079	2144.766059	18.584205
46.480963	2138.738905	18.589223
47.122601	2136.840059	18.594240
47.036405	2138.476521	18.599258
46.782900	2134.171149	18.604275
47.159468	2139.200237	18.609293
47.301584	2158.865528	18.614311
47.450826	2162.817089	18.619328
47.165247	2160.381792	18.624346
47.453928	2168.238484	18.629363
47.047017	2172.580787	18.634381
47.012379	2174.792669	18.639399
47.505189	2161.085897	18.644416
47.412703	2168.563681	18.649434
47.452960	2164.272017	18.654451
47.327438	2165.243806	18.659469
47.485444	2168.211539	18.664487
47.912796	2170.072868	18.669504
47.830145	2166.338035	18.674522
47.763017	2161.215570	18.679539
48.187103	2166.797131	18.684557
47.775584	2165.822923	18.689575
47.840764	2158.196929	18.694592
47.911373	2163.248863	18.699610
47.829792	2166.499429	18.704627
47.927046	2157.001780	18.709645
48.277654	2165.711465	18.714663
48.633939	2153.524111	18.719680
48.325836	2154.473889	18.724698
48.141082	2155.429166	18.729715
48.257697	2152.254849	18.734733
48.239686	2158.784728	18.739751
48.276795	2149.426460	18.744768
48.320853	2154.130240	18.749786
48.212564	2152.352563	18.754803
48.450102	2159.007655	18.759821
48.156477	2155.235679	18.764839
48.339601	2177.939285	18.769856
48.375608	2185.005658	18.774874
48.639838	2190.566314	18.779891
48.871848	2183.465091	18.784909
48.536312	2186.631884	18.789927
48.672997	2191.166734	18.794944
48.761174	2184.356672	18.799962
48.493638	2192.697729	18.804979
48.883499	2189.888059	18.809997
48.508532	2195.007917	18.815015
48.944176	2184.311029	18.820032
48.879880	2201.949256	18.825050
48.892155	2216.691699	18.830067
49.401308	2211.431690	18.835085
49.453517	2217.313270	18.840103
49.742915	2208.106654	18.845120
49.710436	2187.372189	18.850138
49.283710	2183.608847	18.855155
49.508987	2169.497171	18.860173
49.253848	2182.415685	18.865191
49.263509	2170.379558	18.870208
49.548436	2181.472039	18.875226
49.560141	2205.685721	18.880243
49.789169	2201.877575	18.885261
49.616182	2209.592393	18.890279
49.794134	2209.394915	18.895296
49.806991	2197.434554	18.900314
49.736972	2212.677008	18.905331
50.209425	2205.235384	18.910349
49.999869	2215.484881	18.915367
49.965253	2206.595803	18.920384
49.938397	2215.460892	18.925402
49.861568	2215.197858	18.930419
50.005092	2199.535475	18.935437
49.555487	2209.533004	18.940455
49.991317	2205.937290	18.945472
49.952295	2209.872480	18.950490
49.878938	2216.645611	18.955507
50.407516	2220.077331	18.960525
50.282250	2235.411997	18.965543
50.417345	2243.588977	18.970560
50.560690	2234.346643	18.975578
50.191747	2238.938549	18.980595
50.552849	2234.215779	18.985613
50.567143	2243.442441	18.990631
50.845070	2233.174971	18.995648
50.601724	2231.908861	19.000666
50.638468	2240.318619	19.005683
50.718749	2225.801327	19.010701
50.639413	2229.336291	19.015719
50.568479	2228.749033	19.020736
50.760625	2230.409547	19.025754
50.778155	2233.501952	19.030771
50.996684	2224.699917	19.035789
51.032217	2230.027264	19.040807
51.185358	2242.832738	19.045824
51.325594	2246.909252	19.050842
51.033698	2258.951940	19.055859
51.236746	2252.702448	19.060877
51.356592	2256.934026	19.065895
51.636127	2257.758632	19.070912
51.557401	2252.991945	19.075930
51.329789	2253.706291	19.080947
51.482955	2250.489154	19.085965
51.393740	2255.465926	19.090983
51.551869	2253.336623	19.096000
51.773804	2246.753759	19.101018
51.637293	2261.910906	19.106035
51.793000	2258.532900	19.111053
51.655739	2267.447877	19.116071
51.492183	2258.411002	19.121088
51.496050	2258.843019	19.126106
51.553146	2264.697881	19.131123
51.670512	2262.850381	19.136141
51.658646	2296.956859	19.141159
52.033317	2296.273363	19.146176
51.892015	2287.947923	19.151194
51.813542	2297.552815	19.156211
51.965121	2297.970715	19.161229
51.934845	2302.178266	19.166247
52.242456	2309.650523	19.171264
52.410581	2316.969621	19.176282
52.511344	2320.605671	19.181299
52.713650	2311.794372	19.186317
52.008159	2324.610997	19.191335
52.566774	2318.204091	19.196352
52.623865	2319.149913	19.201370
52.325569	2324.899440	19.206387
52.742837	2312.552778	19.211405
52.809264	2315.338501	19.216423
52.765897	2313.559102	19.221440
52.702859	2309.612660	19.226458
52.891782	2316.162310	19.231475
53.078901	2303.311190	19.236493
52.872281	2309.105871	19.241511
53.056586	2311.584905	19.246528
53.406373	2316.641138	19.251546
53.394546	2311.340686	19.256563
53.309082	2303.254106	19.261581
53.088604	2300.533099	19.266599
53.305691	2308.678161	19.271616
53.584609	2325.199129	19.276634
53.588140	2319.992188	19.281651
53.588954	2295.538801	19.286669
53.400695	2309.171989	19.291687
53.403015	2325.473563	19.296704
53.780474	2330.410547	19.301722
53.775574	2329.370693	19.306739
53.551410	2329.773792	19.311757
53.743862	2330.978051	19.316775
53.755306	2324.848757	19.321792
53.835250	2330.517514	19.326810
53.705287	2333.289725	19.331827
54.032452	2328.356814	19.336845
54.262875	2324.904737	19.341863
53.862439	2331.700980	19.346880
54.227586	2323.323856	19.351898
54.170964	2326.870953	19.356915
54.121862	2315.335692	19.361933
53.940144	2326.435057	19.366951
53.498419	2336.768859	19.371968
54.247687	2343.998439	19.376986
54.067767	2356.061104	19.382003
54.261161	2359.528221	19.387021
54.400214	2356.794702	19.392039
54.371065	2361.754065	19.397056
54.815982	2355.480903	19.402074
54.848156	2357.291225	19.407091
54.676547	2354.302841	19.412109
54.966264	2358.154968	19.417127
54.556771	2357.766428	19.422144
54.632912	2350.754482	19.427162
54.667832	2371.766485	19.432179
54.948268	2377.385982	19.437197
55.431519	2388.042688	19.442215
55.071127	2388.265360	19.447232
55.291077	2389.617837	19.452250
55.228393	2393.742484	19.457267
55.532903	2385.020246	19.462285
55.477642	2391.423236	19.467303
55.488331	2391.357047	19.472320
55.431411	2389.206172	19.477338
55.522922	2392.107470	19.482355
55.555212	2386.364186	19.487373
55.595512	2389.387706	19.492391
55.628302	2389.036393	19.497408
55.931928	2376.736905	19.502426
55.741381	2383.994462	19.507443
55.835562	2388.997093	19.512461
55.827655	2387.595098	19.517479
56.076157	2389.956146	19.522496
56.123268	2377.741613	19.527514
55.825108	2382.045395	19.532531
56.304469	2380.155882	19.537549
56.216271	2381.128025	19.542567
56.014971	2383.772396	19.547584
56.019991	2378.769708	19.552602
56.347945	2383.716178	19.557619
56.172336	2380.635609	19.562637
56.112986	2377.247824	19.567655
56.060780	2381.481705	19.572672
56.293244	2384.779774	19.577690
56.074675	2388.996927	19.582707
56.258549	2397.053732	19.587725
56.712517	2389.374268	19.592743
56.627923	2399.641722	19.597760
56.919799	2396.540085	19.602778
56.868240	2401.023217	19.607795
56.763592	2402.324418	19.612813
56.780751	2405.981688	19.617831
56.814087	2401.113703	19.622848
57.078151	2398.343722	19.627866
56.885853	2405.792710	19.632883
56.720076	2400.110897	19.637901
57.185862	2404.038787	19.642919
56.867374	2428.070306	19.647936
57.308210	2431.682041	19.652954
57.087445	2425.698285	19.657971
57.254264	2427.627943	19.662989
57.260205	2418.769237	19.668007
57.315722	2429.480028	19.673024
57.421055	2420.047779	19.678042
57.464945	2426.241472	19.683059
57.231802	2424.254775	19.688077
57.405598	2446.355401	19.693095
57.415994	2457.799431	19.698112
58.051977	2452.253245	19.703130
58.130228	2446.965122	19.708147
58.015472	2443.906298	19.713165
58.237245	2448.651839	19.718183
57.863046	2453.797621	19.723200
58.004515	2442.490656	19.728218
58.225985	2450.155280	19.733235
58.232526	2452.684712	19.738253
58.782804	2442.962819	19.743271
58.270674	2450.505310	19.748288
58.795071	2449.255971	19.753306
58.631392	2452.689596	19.758323
58.599770	2452.785899	19.763341
58.686922	2447.538832	19.768359
58.753494	2451.338472	19.773376
58.859268	2447.388669	19.778394
58.545930	2445.166982	19.783411
58.758061	2443.618196	19.788429
58.806290	2440.778797	19.793447
58.343243	2442.815198	19.798464
58.326646	2439.822527	19.803482
58.637203	2447.771846	19.808499
58.467541	2476.256194	19.813517
58.746707	2470.285510	19.818535
58.888595	2471.871477	19.823552
59.059236	2469.243809	19.828570
58.970331	2471.285047	19.833587
59.031856	2475.353726	19.838605
59.345165	2492.663071	19.843623
59.329494	2505.483112	19.848640
59.601289	2502.074738	19.853658
59.660968	2508.940845	19.858675
59.557707	2505.678808	19.863693
59.537645	2500.558157	19.868711
59.537397	2520.750846	19.873728
59.503518	2503.362326	19.878746
59.704596	2497.658154	19.883763
59.555010	2503.100862	19.888781
59.889186	2502.323132	19.893799
59.932769	2501.605904	19.898816
59.901046	2508.002832	19.903834
59.759011	2515.531171	19.908851
60.029473	2537.507970	19.913869
60.477557	2527.696128	19.918887
60.301761	2532.268333	19.923904
60.511353	2534.571110	19.928922
60.508817	2534.867289	19.933939
60.409259	2543.209286	19.938957
60.697184	2533.811560	19.943975
60.495083	2541.347918	19.948992
60.411364	2533.071363	19.954010
60.904062	2539.282416	19.959027
60.795033	2537.380527	19.964045
60.942762	2528.890867	19.969063
60.586426	2536.472271	19.974080
60.859838	2536.766919	19.979098
60.986529	2530.640398	19.984115
60.482002	2532.798267	19.989133
60.737033	2535.118182	19.994151
60.992350	2551.761947	19.999168
60.756422	2563.822703	20.004186
61.267501	2564.320936	20.009203
61.156225	2560.905205	20.014221
61.171804	2558.347872	20.019239
60.969816	2565.713533	20.024256
61.556697	2570.643947	20.029274
61.546226	2580.504049	20.034291
61.506727	2594.993981	20.039309
61.636042	2593.500863	20.044327
61.871748	2594.361584	20.049344
61.719358	2596.669394	20.054362
61.963597	2588.290951	20.059379
61.682191	2596.702882	20.064397
61.759446	2584.318184	20.069415
61.660635	2593.986295	20.074432
61.864573	2595.021987	20.079450
62.029256	2582.980463	20.084467
61.843769	2607.152318	20.089485
62.347712	2602.484526	20.094503
62.221187	2618.480536	20.099520
62.224411	2618.658595	20.104538
62.791789	2612.567166	20.109555
62.679512	2609.434758	20.114573
62.678501	2611.109603	20.119591
62.550542	2612.062143	20.124608
62.602284	2613.740375	20.129626
62.625302	2614.668839	20.134643
62.740628	2614.697658	20.139661
62.742894	2605.258129	20.144679
62.878367	2612.882277	20.149696
62.949785	2614.261610	20.154714
62.883007	2611.056658	20.159731
62.787108	2607.703752	20.164749
62.838781	2600.878079	20.169767
62.941233	2615.492488	20.174784
63.158249	2620.080737	20.179802
63.307877	2634.541334	20.184819
63.329487	2649.902567	20.189837
63.358244	2640.906366	20.194855
63.408592	2632.399925	20.199872
63.383121	2637.931440	20.204890
63.555181	2636.852332	20.209907
63.490303	2633.227028	20.214925
63.520910	2636.184498	20.219943
63.834999	2642.492513	20.224960
63.737697	2647.411713	20.229978
63.867686	2654.737850	20.234995
63.841114	2664.399206	20.240013
63.905592	2666.456127	20.245031
64.249972	2661.301686	20.250048
64.164182	2659.847584	20.255066
64.497972	2665.820522	20.260083
64.382326	2659.183545	20.265101
64.380575	2659.519718	20.270119
64.122600	2668.083700	20.275136
64.253607	2667.719865	20.280154
64.467978	2661.561214	20.285171
64.286185	2669.062935	20.290189
64.664265	2679.256801	20.295207
64.635286	2690.103968	20.300224
64.662756	2691.666515	20.305242
64.808886	2689.295217	20.310259
64.547226	2696.063202	20.315277
64.960580	2693.394429	20.320295
65.091393	2689.635645	20.325312
65.033361	2680.555721	20.330330
65.260323	2683.605384	20.335347
65.225637	2682.193472	20.340365
65.106475	2680.882346	20.345383
65.254390	2689.334416	20.350400
65.490257	2694.879338	20.355418
65.650046	2691.491144	20.360435
65.188337	2708.678919	20.365453
65.341355	2706.941309	20.370471
65.533528	2713.512645	20.375488
65.185903	2722.633712	20.380506
65.358289	2713.685356	20.385523
65.494015	2704.943435	20.390541
65.442003	2719.944419	20.395559
65.983868	2735.314022	20.400576
66.015305	2745.622997	20.405594
66.066117	2746.253633	20.410611
66.230946	2751.216018	20.415629
66.205505	2746.863079	20.420647
66.437661	2751.885522	20.425664
65.927433	2750.352788	20.430682
66.270095	2752.727985	20.435699
66.268925	2758.333544	20.440717
66.430010	2756.670942	20.445735
66.571747	2762.188425	20.450752
66.422980	2745.471608	20.455770
67.402400	2737.365210	20.460787
67.353090	2733.514789	20.465805
67.462723	2722.499010	20.470823
67.404141	2724.087870	20.475840
67.270326	2727.759071	20.480858
67.543207	2722.729282	20.485875
67.755539	2722.128294	20.490893
67.734099	2716.631789	20.495911
67.494837	2696.833384	20.500928
67.181825	2695.316402	20.505946
67.604249	2683.836231	20.510963
67.159421	2688.964252	20.515981
67.456975	2696.973205	20.520999
67.872628	2708.049962	20.526016
67.788487	2712.701212	20.531034
67.808839	2702.914989	20.536051
67.558598	2696.061905	20.541069
67.665193	2704.405729	20.546087
67.595637	2704.176136	20.551104
67.733005	2712.624395	20.556122
67.795131	2708.411678	20.561139
67.634150	2717.577705	20.566157
67.863468	2709.686908	20.571175
67.910681	2725.608133	20.576192
67.779160	2747.938038	20.581210
68.364402	2745.560420	20.586227
68.268153	2750.110568	20.591245
68.261229	2743.527009	20.596263
68.432389	2742.590413	20.601280
68.229827	2750.808939	20.606298
68.496621	2761.154333	20.611315
68.568443	2770.535768	20.616333
68.731384	2782.051692	20.621351
68.659517	2775.484767	20.626368
68.461394	2785.585743	20.631386
68.692511	2773.741133	20.636403
68.995652	2786.816570	20.641421
68.895195	2787.903966	20.646439
69.213099	2800.747371	20.651456
69.260394	2807.938890	20.656474
69.148980	2804.720562	20.661491
68.929706	2807.512610	20.666509
69.178143	2801.402745	20.671527
69.348383	2805.550146	20.676544
69.364414	2807.230161	20.681562
69.367220	2799.431287	20.686579
69.910070	2813.333791	20.691597
69.835155	2813.842890	20.696615
70.107812	2805.470805	20.701632
69.800765	2809.663642	20.706650
70.163711	2815.755491	20.711667
69.944589	2834.303320	20.716685
70.230372	2833.099870	20.721703
70.508503	2818.896548	20.726720
70.022515	2833.493315	20.731738
70.156441	2825.025351	20.736755
70.341721	2832.212969	20.741773
70.324950	2823.332468	20.746791
70.286674	2824.898435	20.751808
70.478529	2825.814934	20.756826
70.669312	2827.124908	20.761843
70.548075	2833.868990	20.766861
70.580721	2827.591367	20.771879
71.101207	2826.193168	20.776896
70.754928	2855.390769	20.781914
70.750078	2857.962205	20.786931
70.954808	2857.818660	20.791949
70.973453	2860.456358	20.796967
71.406934	2853.147270	20.801984
71.199435	2867.610774	20.807002
71.396084	2855.115560	20.812019
71.273361	2855.501707	20.817037
71.081024	2859.288465	20.822055
71.515771	2852.521938	20.827072
70.898018	2857.690966	20.832090
71.312712	2877.616606	20.837107
71.492137	2876.461578	20.842125
71.317539	2892.725923	20.847143
71.712661	2879.587839	20.852160
71.656705	2901.791869	20.857178
72.203731	2905.691999	20.862195
71.985983	2919.693872	20.867213
72.175305	2913.382575	20.872231
71.951724	2906.706060	20.877248
71.914949	2913.376140	20.882266
71.979127	2903.596953	20.887283
72.128448	2916.080330	20.892301
72.607900	2930.129928	20.897319
72.693988	2926.508795	20.902336
72.537549	2943.542756	20.907354
73.052231	2928.813903	20.912371
73.215297	2934.000818	20.917389
73.293067	2933.143605	20.922407
73.211570	2916.566895	20.927424
72.926415	2908.485078	20.932442
72.849702	2898.187958	20.937459
73.299651	2908.980939	20.942477
73.200550	2922.766454	20.947495
73.317875	2927.157526	20.952512
73.490651	2927.472953	20.957530
73.247221	2921.351015	20.962547
73.606506	2924.396146	20.967565
73.530363	2931.682139	20.972583
73.802282	2924.441258	20.977600
73.620830	2924.028131	20.982618
73.765901	2924.506873	20.987635
73.988484	2926.835959	20.992653
73.806211	2927.668176	20.997671
73.770614	2925.172429	21.002688
73.666712	2924.094831	21.007706
74.023071	2926.655875	21.012723
73.952934	2930.991102	21.017741
73.699527	2951.053274	21.022759
73.957184	2948.203192	21.027776
74.359474	2954.962957	21.032794
74.608921	2957.176065	21.037811
74.749357	2951.149437	21.042829
74.233463	2948.314158	21.047847
74.267818	2946.826709	21.052864
74.413215	2959.110948	21.057882
74.596618	2965.461971	21.062899
75.055551	2972.491961	21.067917
74.629752	2977.036521	21.072935
75.131162	2978.739055	21.077952
75.101236	2978.720244	21.082970
74.928089	2986.629789	21.087987
75.272134	2977.107198	21.093005
75.112200	2978.525032	21.098023
75.313850	2983.058425	21.103040
75.314768	3000.258507	21.108058
75.518862	2999.858625	21.113075
75.825390	3009.057261	21.118093
75.809799	3013.144681	21.123111
75.885015	3002.632111	21.128128
75.587409	3017.095971	21.133146
75.593102	3001.233671	21.138163
75.647817	2998.415943	21.143181
75.870025	3005.007793	21.148199
75.935864	3018.540549	21.153216
75.998869	3041.286681	21.158234
76.390250	3039.987714	21.163251
76.745830	3037.590827	21.168269
76.196899	3035.604844	21.173287
76.821712	3033.590585	21.178304
76.623213	3045.472710	21.183322
76.298720	3042.869622	21.188339
76.361082	3034.615111	21.193357
76.461652	3034.881485	21.198375
76.520735	3037.743247	21.203392
76.557954	3055.284506	21.208410
76.704074	3057.868087	21.213427
76.475414	3065.025076	21.218445
76.287820	3072.682892	21.223463
76.760150	3075.411899	21.228480
76.951622	3100.289838	21.233498
77.122194	3100.261079	21.238515
77.221258	3106.498967	21.243533
77.279081	3101.432548	21.248551
77.333698	3106.142817	21.253568
77.617416	3119.161867	21.258586
77.994435	3115.033331	21.263603
78.581056	3104.485547	21.268621
78.040808	3100.400241	21.273639
78.623400	3092.268047	21.278656
78.512290	3086.117072	21.283674
78.321123	3083.196158	21.288691
78.373347	3078.004780	21.293709
78.427371	3086.073235	21.298727
78.395352	3064.627916	21.303744
78.732269	3079.447681	21.308762
78.440141	3081.913149	21.313779
78.607736	3063.029500	21.318797
78.398117	3078.228255	21.323815
78.602492	3071.260805	21.328832
78.930250	3087.659218	21.333850
78.683378	3096.576446	21.338867
78.874664	3102.063344	21.343885
78.706595	3109.651203	21.348903
78.865654	3112.310606	21.353920
78.920856	3113.676053	21.358938
78.895956	3109.729605	21.363955
79.159726	3118.541030	21.368973
79.014916	3137.623310	21.373991
79.196108	3139.955099	21.379008
79.643773	3138.254622	21.384026
79.386167	3143.755695	21.389043
79.630567	3135.181833	21.394061
79.571120	3147.912663	21.399079
79.770849	3156.597450	21.404096
80.057535	3160.207996	21.409114
80.131802	3167.124004	21.414131
80.347188	3153.317386	21.419149
80.293274	3166.273111	21.424167
80.442813	3158.762152	21.429184
80.679310	3153.556308	21.434202
80.490099	3163.656909	21.439219
80.771885	3152.555144	21.444237
80.609125	3152.095764	21.449255
80.682274	3148.406630	21.454272
80.482182	3155.314466	21.459290
80.585925	3153.238546	21.464307
80.753688	3146.404333	21.469325
80.455618	3154.175777	21.474343
80.418095	3153.366829	21.479360
80.844910	3173.422309	21.484378
80.753755	3196.069764	21.489395
81.240404	3200.493273	21.494413
80.852360	3201.919972	21.499431
81.134166	3190.790643	21.504448
81.320880	3195.829927	21.509466
81.088504	3214.754786	21.514483
81.452295	3208.545335	21.519501
81.531850	3216.059935	21.524519
81.649326	3221.464253	21.529536
81.934116	3215.655207	21.534554
81.779453	3212.763057	21.539571
81.788052	3212.176447	21.544589
82.062186	3240.962015	21.549607
82.246389	3244.887844	21.554624
82.265238	3247.219580	21.559642
81.929891	3247.512207	21.564659
82.238312	3237.875562	21.569677
82.123272	3242.594837	21.574695
82.272158	3245.915873	21.579712
82.894660	3259.746320	21.584730
82.817467	3269.844863	21.589747
82.625419	3276.860029	21.594765
82.843060	3279.320542	21.599783
83.072540	3267.533221	21.604800
83.272847	3270.430719	21.609818
82.970709	3272.058476	21.614835
83.510251	3270.151395	21.619853
83.081658	3267.819735	21.624871
83.190234	3271.951144	21.629888
83.501111	3275.817451	21.634906
83.307975	3279.560393	21.639923
83.683194	3285.562381	21.644941
83.593041	3298.077979	21.649959
83.475904	3301.052850	21.654976
83.759355	3300.968333	21.659994
83.724571	3296.006291	21.665011
83.556021	3298.164180	21.670029
83.825660	3306.707327	21.675047
83.755285	3318.774553	21.680064
84.260364	3324.810914	21.685082
84.142310	3321.794123	21.690099
84.169882	3321.977747	21.695117
84.296883	3337.553381	21.700135
84.459486	3348.383857	21.705152
84.642914	3349.799677	21.710170
84.468061	3360.275709	21.715187
84.849557	3345.702982	21.720205
84.829582	3358.891816	21.725223
84.641384	3362.528582	21.730240
85.130821	3356.601889	21.735258
85.037208	3363.289890	21.740275
85.243828	3383.685201	21.745293
85.189277	3390.223816	21.750311
85.293194	3375.589913	21.755328
85.383748	3384.893239	21.760346
85.311071	3386.917856	21.765363
85.331939	3383.730223	21.770381
85.720173	3383.551907	21.775399
85.688457	3382.551653	21.780416
86.002751	3391.090089	21.785434
85.785174	3407.258806	21.790451
85.922755	3404.346762	21.795469
86.454900	3416.123688	21.800487
86.242654	3408.225054	21.805504
86.542569	3407.803589	21.810522
86.359546	3417.124601	21.815539
86.460948	3413.681047	21.820557
86.678183	3408.157236	21.825575
86.482607	3404.519543	21.830592
86.562137	3419.456214	21.835610
86.523202	3415.865124	21.840627
86.533655	3424.768261	21.845645
86.703929	3441.200052	21.850663
87.045013	3443.589777	21.855680
87.108694	3437.032406	21.860698
86.972474	3444.317220	21.865715
87.397668	3444.723778	21.870733
87.305904	3447.377615	21.875751
87.411615	3457.086051	21.880768
88.355451	3452.701842	21.885786
88.372434	3435.723384	21.890803
88.582310	3416.753874	21.895821
87.968418	3418.411693	21.900839
88.337255	3414.424402	21.905856
88.569447	3407.152648	21.910874
88.295470	3412.832639	21.915891
88.419829	3401.667688	21.920909
88.788605	3403.926342	21.925927
88.246888	3409.383141	21.930944
88.539770	3413.473401	21.935962
88.513115	3413.413162	21.940979
88.577869	3411.381969	21.945997
88.686818	3411.266280	21.951015
88.694775	3421.492158	21.956032
88.967941	3408.718388	21.961050
88.717963	3416.164497	21.966067
88.575991	3433.391021	21.971085
89.283070	3440.887482	21.976103
88.799591	3447.890202	21.981120
89.026413	3443.835086	21.986138
89.172738	3449.819364	21.991155
89.261098	3462.450593	21.996173
89.316901	3472.750688	22.001191
89.203160	3482.872512	22.006208
89.670059	3469.300030	22.011226
89.423084	3477.113841	22.016243
89.364059	3483.049854	22.021261
89.862781	3499.979987	22.026279
89.660138	3511.962267	22.031296
89.798774	3511.148021	22.036314
89.692376	3517.521899	22.041331
89.954454	3521.551023	22.046349
90.245167	3535.083797	22.051367
90.529511	3536.127978	22.056384
90.781111	3520.364353	22.061402
90.650459	3537.656845	22.066419
90.990674	3526.618641	22.071437
91.055125	3532.427214	22.076455
90.866335	3533.257355	22.081472
91.099199	3527.434441	22.086490
90.804578	3537.325552	22.091507
91.110291	3528.134392	22.096525
91.326058	3521.156261	22.101543
90.882932	3537.114080	22.106560
91.575264	3541.145400	22.111578
91.685239	3555.469276	22.116595
91.624192	3550.936913	22.121613
91.595473	3556.464572	22.126631
91.716687	3556.218703	22.131648
91.906973	3554.640249	22.136666
91.725303	3554.519770	22.141683
92.020181	3569.128835	22.146701
92.247949	3575.948974	22.151719
91.979689	3590.175081	22.156736
92.265798	3588.551450	22.161754
92.298640	3579.522556	22.166771
92.166196	3588.458805	22.171789
92.245313	3583.116643	22.176807
92.228043	3603.276568	22.181824
92.755564	3612.259417	22.186842
92.755138	3617.967451	22.191859
92.920839	3617.970937	22.196877
92.612558	3607.962759	22.201895
92.782419	3627.491874	22.206912
93.216417	3637.957548	22.211930
93.086353	3640.825203	22.216947
92.977690	3645.707214	22.221965
93.426800	3640.657667	22.226983
93.212720	3653.971331	22.232000
93.522261	3654.978464	22.237018
93.942079	3661.102508	22.242035
94.262026	3664.795983	22.247053
94.159835	3654.950000	22.252071
94.086744	3673.585732	22.257088
94.346615	3657.601952	22.262106
94.360552	3657.538386	22.267123
94.507856	3660.818076	22.272141
94.715383	3660.181634	22.277159
94.634111	3667.842471	22.282176
94.646803	3659.824446	22.287194
94.563415	3665.770711	22.292211
94.778512	3661.044815	22.297229
95.086117	3668.682188	22.302247
94.963825	3683.140772	22.307264
95.024735	3685.708160	22.312282
95.721641	3675.461770	22.317299
95.318823	3689.367234	22.322317
95.659329	3685.286844	22.327335
95.746949	3692.896376	22.332352
95.530318	3676.857973	22.337370
95.638965	3677.208818	22.342387
95.329297	3684.052561	22.347405
95.509292	3678.392203	22.352423
95.289137	3688.605082	22.357440
95.340861	3689.099523	22.362458
95.734821	3704.891002	22.367475
95.891090	3715.500924	22.372493
96.084541	3717.745106	22.377511
96.125859	3718.017010	22.382528
96.208338	3719.886346	22.387546
96.413677	3736.100479	22.392563
96.136614	3746.431818	22.397581
96.509180	3739.289342	22.402599
96.870941	3754.671441	22.407616
96.675616	3746.938269	22.412634
97.024028	3753.024966	22.417651
96.897866	3767.195546	22.422669
97.454399	3769.152135	22.427687
97.440235	3766.154084	22.432704
97.669330	3758.678120	22.437722
97.909481	3762.742275	22.442739
97.748273	3764.818033	22.447757
98.053420	3754.047996	22.452775
97.856714	3757.016767	22.457792
98.086962	3762.555129	22.462810
98.242793	3760.301686	22.467827
98.093694	3760.021825	22.472845
98.425537	3761.696431	22.477863
98.291577	3758.158956	22.482880
98.213443	3761.060834	22.487898
98.309122	3758.922395	22.492915
98.107316	3763.466874	22.497933
98.828079	3771.220925	22.502951
98.589636	3789.453655	22.507968
98.574653	3790.156975	22.512986
99.054435	3786.634906	22.518003
98.878986	3800.446005	22.523021
98.957851	3796.723544	22.528039
98.899134	3803.416407	22.533056
99.146629	3812.347274	22.538074
99.437098	3821.361761	22.543091
99.321409	3827.041842	22.548109
100.122270	3811.850334	22.553127
99.562247	3821.601449	22.558144
99.592804	3812.347789	22.563162
100.018192	3810.062370	22.568179
99.477137	3815.677329	22.573197
99.868262	3828.401408	22.578215
99.943264	3837.913608	22.583232
99.706438	3843.852158	22.588250
100.332745	3840.973017	22.593267
100.279829	3849.947090	22.598285
100.627366	3857.374449	22.603303
100.729092	3865.758260	22.608320
100.530550	3877.652076	22.613338
100.933313	3873.980215	22.618355
100.315427	3874.220356	22.623373
100.482367	3880.970884	22.628391
100.363993	3879.646148	22.633408
100.482643	3899.289992	22.638426
101.198319	3896.319497	22.643443
100.748641	3908.626264	22.648461
101.218133	3915.787192	22.653479
101.375205	3933.801271	22.658496
101.492396	3939.664529	22.663514
101.430168	3928.305517	22.668531
101.738719	3954.212510	22.673549
102.060520	3957.587163	22.678567
102.044103	3969.072049	22.683584
102.054019	3961.571145	22.688602
102.378538	3955.907303	22.693619
102.315557	3964.139646	22.698637
102.626772	3955.262014	22.703655
102.800829	3957.383459	22.708672
102.261334	3974.148506	22.713690
103.004382	3977.693568	22.718707
103.239148	3983.781965	22.723725
103.357876	3988.549950	22.728743
103.113907	3991.770171	22.733760
103.311522	3988.953068	22.738778
103.345736	3993.841518	22.743795
103.116808	3995.184701	22.748813
103.412701	3995.993434	22.753831
103.497382	3995.762824	22.758848
103.516483	4022.320257	22.763866
103.770448	4022.691993	22.768883
103.628706	4024.786710	22.773901
103.669604	4028.158185	22.778919
103.995339	4030.498537	22.783936
103.991748	4052.074484	22.788954
104.065112	4048.079074	22.793971
104.074141	4055.453524	22.798989
104.281351	4057.782887	22.804007
104.267712	4065.059474	22.809024
104.252225	4073.904993	22.814042
104.692793	4075.706262	22.819059
104.811646	4081.517392	22.824077
104.966437	4074.701339	22.829095
104.972981	4085.841237	22.834112
105.099524	4107.063749	22.839130
105.528067	4102.484615	22.844147
105.434749	4122.236504	22.849165
105.490315	4114.455265	22.854183
105.833514	4114.945724	22.859200
105.298109	4115.652589	22.864218
105.873758	4105.920061	22.869235
105.798436	4123.006961	22.874253
105.872517	4136.379739	22.879271
106.119589	4132.441569	22.884288
105.958017	4137.513903	22.889306
106.449352	4134.981129	22.894323
105.956298	4141.634840	22.899341
106.232223	4144.414255	22.904359
106.822240	4162.125936	22.909376
106.515361	4172.083932	22.914394
106.913205	4168.511906	22.919411
106.777760	4164.750364	22.924429
106.917229	4166.391186	22.929447
107.107449	4174.785450	22.934464
107.274065	4186.961922	22.939482
107.665383	4196.970661	22.944499
107.516297	4202.804109	22.949517
107.928843	4188.032078	22.954535
107.891346	4192.091851	22.959552
107.714968	4198.681719	22.964570
107.916734	4192.046139	22.969587
107.879998	4192.492555	22.974605
108.012050	4196.762086	22.979623
108.053712	4200.208213	22.984640
107.973664	4224.454022	22.989658
108.402240	4221.069821	22.994675
108.289316	4223.778306	22.999693
108.231666	4231.309799	23.004711
108.656871	4237.954802	23.009728
108.904424	4251.748436	23.014746
108.841726	4244.785259	23.019763
109.170362	4257.511023	23.024781
109.424044	4231.265281	23.029799
109.963131	4228.981338	23.034816
109.909325	4219.615792	23.039834
110.397432	4220.765992	23.044851
110.591233	4224.972977	23.049869
110.505304	4210.151391	23.054887
110.484045	4192.066572	23.059904
110.238158	4185.872116	23.064922
110.505467	4182.037695	23.069939
110.845149	4174.344857	23.074957
110.634896	4174.435826	23.079975
110.910914	4169.710282	23.084992
110.448996	4185.749677	23.090010
110.886681	4177.188446	23.095027
110.319776	4182.534684	23.100045
110.286858	4187.038202	23.105063
110.322829	4191.727407	23.110080
110.428173	4204.481650	23.115098
110.767020	4216.505601	23.120115
110.833893	4245.724255	23.125133
111.017714	4250.292355	23.130151
111.321717	4242.531223	23.135168
110.980141	4255.838224	23.140186
111.480860	4268.640401	23.145203
111.562689	4277.660118	23.150221
111.362673	4280.693241	23.155239
111.809436	4282.983657	23.160256
111.366628	4298.360095	23.165274
111.477869	4312.022903	23.170291
111.988384	4317.365743	23.175309
111.765280	4318.473591	23.180327
112.390340	4336.025705	23.185344
112.230336	4343.631791	23.190362
112.352525	4340.708644	23.195379
112.643355	4347.990318	23.200397
112.632112	4367.628753	23.205415
113.022657	4364.071219	23.210432
113.020680	4370.899256	23.215450
113.254119	4367.954432	23.220467
113.763152	4366.941836	23.225485
113.361855	4371.080121	23.230503
113.678420	4371.358497	23.235520
113.380773	4391.911141	23.240538
113.823669	4387.770181	23.245555
114.099814	4395.162783	23.250573
113.776589	4397.878871	23.255591
114.047295	4388.909102	23.260608
114.159360	4406.247301	23.265626
114.796598	4421.358822	23.270643
114.568524	4426.297892	23.275661
114.182869	4432.566433	23.280679
114.725105	4424.310935	23.285696
114.507653	4432.840368	23.290714
114.689774	4436.300342	23.295731
114.972700	4458.027086	23.300749
115.021553	4457.962669	23.305767
115.165975	4449.651798	23.310784
115.315563	4450.737205	23.315802
115.709762	4453.957252	23.320819
115.774496	4472.890633	23.325837
115.626708	4482.894273	23.330855
116.107636	4482.653183	23.335872
116.187698	4491.894376	23.340890
116.242125	4478.464625	23.345907
116.074312	4486.824114	23.350925
116.154926	4486.616173	23.355943
116.406062	4490.081677	23.360960
116.494455	4494.082125	23.365978
116.433108	4503.518946	23.370995
116.699802	4501.866061	23.376013
116.693499	4502.948007	23.381031
116.956285	4502.294855	23.386048
116.721178	4516.655813	23.391066
117.277449	4526.518112	23.396083
117.501961	4533.417889	23.401101
117.077277	4542.218798	23.406119
117.418694	4538.071950	23.411136
117.587819	4546.467432	23.416154
117.905298	4536.763989	23.421171
117.701731	4539.011029	23.426189
117.793940	4560.605488	23.431207
118.054939	4565.125192	23.436224
117.999012	4562.657582	23.441242
117.829709	4565.889622	23.446259
118.662379	4582.639533	23.451277
118.667708	4593.161660	23.456295
118.785591	4595.541542	23.461312
118.652452	4596.878943	23.466330
118.876212	4597.541874	23.471347
118.783191	4600.837282	23.476365
118.472597	4605.311252	23.481383
118.943048	4617.268133	23.486400
119.163814	4621.237282	23.491418
119.276709	4618.873338	23.496435
119.693833	4630.435153	23.501453
119.877694	4647.263416	23.506471
119.961867	4646.589962	23.511488
120.243649	4643.001716	23.516506
120.087685	4653.083872	23.521523
120.432768	4645.856448	23.526541
120.438093	4653.923303	23.531559
120.753786	4645.707740	23.536576
120.863757	4649.005407	23.541594
120.337550	4649.215985	23.546611
120.628373	4650.384306	23.551629
120.472740	4669.807007	23.556647
120.523832	4682.347675	23.561664
120.731636	4681.354771	23.566682
120.904861	4703.229176	23.571699
121.104741	4705.630617	23.576717
121.098973	4718.203984	23.581735
121.579809	4720.592098	23.586752
121.538504	4743.949107	23.591770
121.225105	4741.590965	23.596787
121.695754	4739.730884	23.601805
121.779111	4766.129937	23.606823
121.701475	4769.486653	23.611840
122.123547	4776.025411	23.616858
122.430610	4779.661437	23.621875
122.841483	4789.637571	23.626893
122.746040	4806.441320	23.631911
123.209418	4804.532041	23.636928
122.942331	4797.204687	23.641946
122.916785	4807.756278	23.646963
123.295430	4803.820554	23.651981
123.185539	4806.836267	23.656999
123.651736	4815.422910	23.662016
123.773485	4825.484504	23.667034
123.752755	4831.200180	23.672051
124.045308	4819.916865	23.677069
123.444798	4835.494441	23.682087
124.105048	4821.959914	23.687104
124.135705	4821.173831	23.692122
123.843220	4830.179619	23.697139
124.482429	4831.302633	23.702157
124.397925	4852.445798	23.707175
124.588524	4850.462786	23.712192
124.664224	4857.709786	23.717210
124.916151	4860.002254	23.722227
124.958861	4852.027570	23.727245
124.768569	4868.592402	23.732263
125.027132	4871.903403	23.737280
125.196860	4891.702493	23.742298
125.305905	4886.566716	23.747315
125.287878	4890.647179	23.752333
125.375820	4896.570554	23.757351
125.612165	4911.399560	23.762368
125.820165	4921.196503	23.767386
125.891140	4919.607823	23.772403
126.080211	4926.095687	23.777421
126.182671	4944.472165	23.782439
126.490128	4949.986081	23.787456
126.839247	4941.588799	23.792474
126.632373	4942.673649	23.797491
126.613004	4948.787235	23.802509
126.773891	4952.457626	23.807527
126.897396	4958.633402	23.812544
127.173290	4968.910467	23.817562
126.868643	4971.725969	23.822579
127.340707	4976.363986	23.827597
127.132219	5000.809350	23.832615
127.370866	5010.927171	23.837632
127.600094	5003.326257	23.842650
127.280400	5015.405516	23.847667
127.567357	5024.916158	23.852685
127.874088	5042.607990	23.857703
128.198398	5050.889330	23.862720
128.864424	5047.094963	23.867738
128.984109	5049.218159	23.872755
129.393290	5050.717736	23.877773
128.963112	5055.480755	23.882791
129.275886	5054.178427	23.887808
129.435648	5049.715815	23.892826
129.389092	5057.649552	23.897843
129.487245	5051.796384	23.902861
129.270622	5050.421120	23.907879
129.459063	5045.567653	23.912896
129.944218	5063.605545	23.917914
129.850144	5073.405910	23.922931
130.042241	5074.088074	23.927949
129.836042	5074.142995	23.932967
130.296637	5065.416324	23.937984
130.307478	5073.740577	23.943002
130.109468	5100.757045	23.948019
130.672891	5098.640604	23.953037
130.691751	5113.270044	23.958055
130.761437	5102.566469	23.963072
130.925658	5102.423864	23.968090
130.700199	5121.814234	23.973107
130.759158	5123.672553	23.978125
131.188953	5139.470883	23.983143
131.063167	5146.872881	23.988160
131.528095	5162.347005	23.993178
131.376209	5169.923111	23.998195
131.334943	5172.301714	24.003213
131.599545	5178.786301	24.008231
132.414833	5183.864517	24.013248
132.244971	5185.455647	24.018266
132.363923	5197.306980	24.023283
132.414595	5189.576307	24.028301
132.730139	5186.549786	24.033319
132.875461	5181.825094	24.038336
132.987713	5197.676476	24.043354
132.776445	5218.939506	24.048371
133.581261	5221.439691	24.053389
133.950611	5204.565079	24.058407
133.885747	5204.555768	24.063424
134.319862	5206.440822	24.068442
134.382325	5204.223293	24.073459
134.702743	5199.971042	24.078477
134.478678	5197.554522	24.083495
134.365221	5175.199414	24.088512
134.686344	5183.412892	24.093530
134.569311	5189.852910	24.098547
134.988007	5185.573980	24.103565
135.208560	5186.216996	24.108583
134.908476	5194.394208	24.113600
135.097583	5188.544579	24.118618
134.805020	5190.248109	24.123635
135.013845	5177.900043	24.128653
135.035764	5182.974946	24.133671
135.260384	5195.911648	24.138688
135.347528	5205.514058	24.143706
135.244522	5223.920498	24.148723
135.505025	5224.324272	24.153741
135.903663	5235.676308	24.158759
135.846101	5260.282920	24.163776
135.718725	5260.245026	24.168794
135.912469	5273.208747	24.173811
136.194454	5280.438012	24.178829
136.119151	5286.400161	24.183847
136.161479	5295.004319	24.188864
136.506133	5306.944846	24.193882
136.760954	5315.961220	24.198899
136.752789	5323.553039	24.203917
137.128680	5347.228414	24.208935
137.271756	5348.375507	24.213952
137.332487	5342.632041	24.218970
137.422739	5363.523064	24.223987
138.135317	5374.165072	24.229005
138.072569	5382.020530	24.234023
138.237688	5375.608982	24.239040
138.681030	5372.149006	24.244058
138.295563	5380.488628	24.249075
138.307120	5372.963143	24.254093
138.515024	5375.553022	24.259111
138.582201	5388.343485	24.264128
138.926442	5393.537793	24.269146
138.990964	5402.969281	24.274163
139.077192	5394.277719	24.279181
139.095211	5383.114851	24.284199
138.902355	5410.917810	24.289216
139.197745	5415.073538	24.294234
139.349693	5424.928533	24.299251
139.510719	5439.486851	24.304269
139.818971	5445.073996	24.309287
139.870362	5452.251996	24.314304
139.951520	5459.857180	24.319322
139.875194	5482.130502	24.324339
140.488537	5494.263581	24.329357
140.439853	5498.034398	24.334375
140.323789	5500.536698	24.339392
140.714305	5510.682575	24.344410
140.547161	5522.903928	24.349427
140.737839	5524.528872	24.354445
141.279018	5536.496472	24.359463
141.469029	5547.746691	24.364480
141.787701	5541.244502	24.369498
141.953224	5547.763145	24.374515
142.262294	5545.967284	24.379533
142.099927	5546.026231	24.384551
142.126695	5570.826831	24.389568
142.575779	5568.530295	24.394586
142.467593	5580.012185	24.399603
142.454041	5587.154186	24.404621
142.644244	5578.427843	24.409639
142.662856	5599.590253	24.414656
143.003622	5602.682970	24.419674
142.975271	5610.097987	24.424691
143.395436	5606.096430	24.429709
143.463304	5617.842953	24.434727
143.589878	5624.315914	24.439744
144.146821	5621.030526	24.444762
144.397538	5628.903798	24.449779
144.078364	5632.751606	24.454797
144.296597	5629.548543	24.459815
144.460765	5620.899495	24.464832
144.616105	5624.393919	24.469850
144.465816	5639.372634	24.474867
144.977713	5656.352733	24.479885
145.046048	5656.320610	24.484903
144.859949	5661.569674	24.489920
144.883256	5657.160107	24.494938
145.064477	5676.815229	24.499955
145.037416	5679.813977	24.504973
145.096061	5688.311123	24.509991
145.205691	5703.231153	24.515008
145.991028	5720.595729	24.520026
146.074937	5725.268338	24.525043
145.962776	5729.233437	24.530061
146.133713	5717.713134	24.535079
145.822916	5748.238067	24.540096
146.389616	5748.640244	24.545114
146.360125	5755.321462	24.550131
146.041380	5772.047041	24.555149
146.557835	5789.515937	24.560167
146.829305	5799.175889	24.565184
146.822352	5801.239921	24.570202
146.942327	5825.100059	24.575219
147.061029	5833.660882	24.580237
147.394749	5848.677508	24.585255
147.605212	5853.565225	24.590272
147.604455	5865.929487	24.595290
148.048932	5858.337091	24.600307
148.136455	5879.685607	24.605325
148.447539	5874.860310	24.610343
148.437433	5881.701356	24.615360
148.782425	5884.566870	24.620378
149.150136	5905.924252	24.625395
148.872384	5908.520848	24.630413
149.373208	5909.082235	24.635431
149.227357	5905.022930	24.640448
149.438237	5906.820934	24.645466
149.616562	5916.107934	24.650483
149.692233	5939.418283	24.655501
150.023716	5935.685694	24.660519
149.503639	5938.736349	24.665536
150.092899	5951.743036	24.670554
150.286936	5961.835579	24.675571
150.535353	5965.829011	24.680589
150.901608	5962.328478	24.685607
150.553833	5970.109314	24.690624
150.663503	5976.363254	24.695642
151.606783	5980.893422	24.700659
151.307445	5987.885273	24.705677
151.852270	5993.164258	24.710695
151.360448	5989.079838	24.715712
151.738190	5997.711179	24.720730
151.955585	6005.643466	24.725747
152.120321	6018.296182	24.730765
152.504831	6012.984706	24.735783
152.135098	6026.956315	24.740800
152.347550	6020.227738	24.745818
152.677244	6035.212937	24.750835
152.773439	6045.889195	24.755853
152.986078	6053.644453	24.760871
152.786200	6052.681843	24.765888
153.130706	6056.301206	24.770906
153.349336	6074.670797	24.775923
153.387421	6081.098272	24.780941
153.998295	6078.611429	24.785959
153.844063	6079.859483	24.790976
153.686125	6083.029455	24.795994
153.996492	6091.616519	24.801011
154.078933	6109.597165	24.806029
154.187542	6105.155769	24.811047
153.864105	6115.426909	24.816064
154.118850	6130.763260	24.821082
154.446013	6150.821395	24.826099
154.463185	6150.787987	24.831117
154.822934	6164.545072	24.836135
154.659941	6167.989670	24.841152
154.907281	6183.472025	24.846170
155.272194	6204.174101	24.851187
155.561149	6215.675777	24.856205
155.918439	6211.011379	24.861223
155.883472	6219.833751	24.866240
156.204565	6226.943163	24.871258
156.753974	6231.463037	24.876275
156.449853	6229.684608	24.881293
156.823565	6233.370958	24.886311
157.037982	6243.366030	24.891328
157.158356	6253.099152	24.896346
157.648762	6263.339776	24.901363
157.312703	6266.878866	24.906381
157.306503	6266.570660	24.911399
157.141407	6274.428745	24.916416
157.705620	6288.518419	24.921434
158.010872	6296.255893	24.926451
157.882287	6302.938994	24.931469
158.152386	6293.793508	24.936487
158.131878	6315.164596	24.941504
158.344170	6323.459794	24.946522
158.507023	6330.365527	24.951539
158.275070	6347.221111	24.956557
158.769397	6352.758480	24.961575
158.955372	6357.858771	24.966592
159.016676	6369.719449	24.971610
159.438870	6384.872007	24.976627
159.303573	6395.569688	24.981645
159.705094	6396.512792	24.986663
159.582633	6407.452343	24.991680
159.659865	6422.255522	24.996698
160.170171	6425.740752	25.001715
160.315359	6437.263161	25.006733
160.332690	6440.682219	25.011751
160.634459	6438.938562	25.016768
160.680247	6459.543956	25.021786
161.128875	6471.571924	25.026803
161.236572	6480.828839	25.031821
161.526880	6477.994132	25.036839
161.724586	6483.784985	25.041856
161.792747	6497.565264	25.046874
162.066135	6504.370842	25.051891
161.946563	6509.697717	25.056909
162.269396	6504.349481	25.061927
162.265576	6510.281053	25.066944
162.241451	6513.749225	25.071962
162.496241	6526.581573	25.076979
162.629784	6536.060216	25.081997
162.710542	6539.371620	25.087015
162.854053	6543.593587	25.092032
163.027650	6566.225242	25.097050
163.367235	6572.419174	25.102067
163.219385	6582.439973	25.107085
163.721217	6577.866506	25.112103
163.887390	6601.903855	25.117120
163.571466	6594.601485	25.122138
164.161179	6593.481480	25.127155
164.149211	6621.603275	25.132173
164.413622	6629.710156	25.137191
164.727303	6630.852969	25.142208
164.616957	6639.428746	25.147226
164.620817	6654.644342	25.152243
164.844262	6668.210400	25.157261
164.855124	6664.202222	25.162279
165.044789	6689.569619	25.167296
165.355831	6699.636932	25.172314
165.540873	6702.472246	25.177331
165.743565	6720.409282	25.182349
166.465938	6711.524259	25.187367
166.707330	6710.209571	25.192384
166.697635	6718.888157	25.197402
167.077038	6731.224790	25.202419
167.309974	6741.494208	25.207437
167.721914	6738.994916	25.212455
167.859523	6737.399355	25.217472
167.728520	6737.886839	25.222490
168.056095	6724.143987	25.227507
168.086974	6735.344947	25.232525
167.818753	6733.284558	25.237543
168.601311	6727.993561	25.242560
168.175189	6726.417062	25.247578
168.419683	6727.791223	25.252595
168.651990	6743.939063	25.257613
168.876642	6760.610590	25.262631
168.901786	6755.885677	25.267648
168.820316	6766.241430	25.272666
169.075414	6767.550172	25.277683
168.984203	6791.433732	25.282701
169.142928	6793.538368	25.287719
169.607013	6794.499066	25.292736
169.275967	6810.088451	25.297754
169.695978	6813.830513	25.302771
169.416009	6838.181715	25.307789
169.801890	6849.330884	25.312807
170.262747	6863.801101	25.317824
169.869633	6892.202123	25.322842
170.287807	6893.807477	25.327859
170.213303	6908.375678	25.332877
170.500168	6931.709780	25.337895
171.155874	6938.953456	25.342912
171.128714	6950.709890	25.347930
171.543293	6950.384943	25.352947
171.558622	6966.685642	25.357965
171.827719	6978.792217	25.362983
172.095988	6983.539694	25.368000
172.061476	6985.512291	25.373018
172.337384	6993.453878	25.378035
172.447889	7002.163035	25.383053
172.930410	7004.747979	25.388071
173.299071	6997.695850	25.393088
173.311392	7009.940168	25.398106
173.348975	7031.907312	25.403123
173.450502	7043.145237	25.408141
173.825165	7030.692875	25.413159
173.884994	7043.571704	25.418176
173.670918	7056.686986	25.423194
174.052729	7058.021190	25.428211
174.299918	7068.868460	25.433229
174.084533	7070.426915	25.438247
174.449324	7087.705936	25.443264
174.477122	7104.808160	25.448282
174.829604	7107.506701	25.453299
174.914877	7127.373393	25.458317
175.335045	7132.136043	25.463335
175.261759	7141.162567	25.468352
175.075670	7163.562918	25.473370
175.467973	7172.393273	25.478387
175.931133	7188.328934	25.483405
175.535546	7205.681319	25.488423
175.966605	7208.716710	25.493440
175.969767	7234.837881	25.498458
176.593649	7244.802185	25.503475
176.909292	7262.710067	25.508493
177.149600	7271.683527	25.513511
177.399477	7272.312526	25.518528
177.052454	7293.618259	25.523546
177.767052	7292.915000	25.528563
177.880833	7301.590763	25.533581
178.093288	7308.459145	25.538599
178.221620	7317.243543	25.543616
178.334065	7320.561087	25.548634
178.516249	7317.907914	25.553651
178.313495	7336.012623	25.558669
178.721302	7355.828199	25.563687
178.904283	7351.969437	25.568704
178.816713	7377.712685	25.573722
179.174383	7388.569328	25.578739
179.777305	7386.005652	25.583757
179.621073	7419.777166	25.588775
179.738988	7419.730843	25.593792
179.925212	7431.884835	25.598810
180.332007	7445.856718	25.603827
180.671608	7452.095870	25.608845
180.681862	7445.318630	25.613863
181.156925	7435.863586	25.618880
181.194031	7456.096415	25.623898
181.131561	7452.423113	25.628915
181.671650	7460.146579	25.633933
181.633040	7469.554906	25.638951
181.992524	7466.597255	25.643968
182.334836	7466.273592	25.648986
182.204052	7461.484399	25.654003
182.463007	7468.066895	25.659021
182.251722	7469.548411	25.664039
182.983846	7486.644226	25.669056
182.274988	7496.124802	25.674074
182.665373	7501.738194	25.679092
183.292827	7510.032395	25.684109
183.062668	7535.184896	25.689127
183.363455	7525.161926	25.694144
183.552039	7537.439952	25.699162
183.961536	7549.796865	25.704180
184.096206	7563.757949	25.709197
183.945563	7570.592277	25.714215
184.270100	7572.591118	25.719232
184.212050	7599.143657	25.724250
184.120278	7598.015776	25.729268
184.499893	7617.495485	25.734285
184.432357	7638.728038	25.739303
184.915964	7656.966856	25.744320
184.939340	7669.695450	25.749338
185.201336	7688.911517	25.754356
185.956482	7685.922222	25.759373
185.827873	7691.370562	25.764391
186.288613	7708.568914	25.769408
186.633843	7718.611799	25.774426
186.451928	7722.356418	25.779444
187.090421	7731.184844	25.784461
187.324818	7749.142461	25.789479
187.774943	7746.735280	25.794496
187.594312	7753.456440	25.799514
187.914128	7749.080819	25.804532
187.789693	7748.202064	25.809549
187.888292	7765.125367	25.814567
188.210611	7766.806692	25.819584
188.631478	7781.654800	25.824602
188.427723	7786.481722	25.829620
188.417275	7781.529243	25.834637
188.612226	7797.712512	25.839655
189.033318	7807.297205	25.844672
188.957220	7821.805176	25.849690
189.060733	7834.976737	25.854708
189.356980	7836.776324	25.859725
189.171899	7861.313144	25.864743
189.883637	7872.430022	25.869760
189.908223	7887.019577	25.874778
190.006048	7907.580123	25.879796
190.297917	7901.245647	25.884813
190.183252	7924.949055	25.889831
190.697469	7933.770660	25.894848
190.630788	7950.009967	25.899866
190.703437	7968.095929	25.904884
190.850274	7978.405109	25.909901
190.871970	7998.605720	25.914919
191.532723	8002.050825	25.919936
191.710433	8011.129139	25.924954
192.119314	8026.922093	25.929972
192.911098	8025.104863	25.934989
193.109909	8026.832662	25.940007
193.378865	8019.527624	25.945024
193.593939	8020.004042	25.950042
193.635943	8009.436561	25.955060
193.637300	8009.984819	25.960077
193.437699	8035.586928	25.965095
194.073941	8042.954258	25.970112
194.268024	8049.387616	25.975130
194.050304	8053.204517	25.980148
194.446375	8046.563794	25.985165
194.644370	8065.534419	25.990183
194.728527	8076.036218	25.995200
194.570654	8079.034270	26.000218
194.661393	8090.640216	26.005236
194.945708	8106.845378	26.010253
195.052919	8118.113897	26.015271
195.405535	8128.080341	26.020288
195.871217	8147.690632	26.025306
195.639277	8154.584612	26.030324
196.467330	8155.702995	26.035341
196.181565	8173.981295	26.040359
196.617565	8177.017678	26.045376
196.584082	8197.117975	26.050394
196.748252	8214.411405	26.055412
197.213648	8208.612162	26.060429
197.039849	8238.198890	26.065447
197.179949	8248.877993	26.070464
197.660845	8256.525543	26.075482
197.503794	8277.968425	26.080500
197.838344	8285.773879	26.085517
198.220735	8297.417691	26.090535
198.717180	8306.131793	26.095552
198.468823	8315.733830	26.100570
198.774889	8328.538317	26.105588
198.873394	8333.307785	26.110605
198.885094	8361.270131	26.115623
199.202316	8374.408886	26.120640
199.301130	8387.326727	26.125658
199.790920	8407.362381	26.130676
200.117145	8414.249336	26.135693
200.042281	8437.958622	26.140711
200.301689	8448.833281	26.145728
200.197599	8452.810797	26.150746
200.862671	8465.788341	26.155764
201.232428	8470.735733	26.160781
201.381595	8484.918458	26.165799
201.766311	8491.823274	26.170816
202.366724	8488.295068	26.175834
203.753461	8429.628276	26.180852
204.560295	8417.425752	26.185869
204.643063	8404.188599	26.190887
204.380269	8377.787710	26.195904
204.419453	8365.342085	26.200922
203.997026	8345.678999	26.205940
204.071567	8327.672229	26.210957
204.037754	8334.728678	26.215975
203.970574	8330.788362	26.220992
204.104772	8319.645690	26.226010
204.206376	8332.035421	26.231028
204.317751	8327.158557	26.236045
204.283292	8349.966161	26.241063
204.625444	8348.743080	26.246080
204.557588	8361.829505	26.251098
204.477709	8372.206577	26.256116
204.909622	8386.402761	26.261133
204.989964	8406.387618	26.266151
205.198989	8420.982523	26.271168
205.500424	8423.593840	26.276186
205.181574	8448.884378	26.281204
205.663023	8465.587702	26.286221
205.438314	8492.276202	26.291239
205.619282	8518.605773	26.296256
205.967082	8535.912403	26.301274
206.032729	8560.928975	26.306292
206.298214	8576.157154	26.311309
206.350564	8612.703072	26.316327
206.671665	8633.533954	26.321344
207.183733	8654.327340	26.326362
207.109794	8681.554789	26.331380
207.511661	8692.045327	26.336397
207.899545	8711.412227	26.341415
207.914530	8745.480896	26.346432
208.575011	8745.776954	26.351450
208.461080	8768.348408	26.356468
209.073334	8766.621886	26.361485
209.156003	8791.703411	26.366503
209.311552	8807.312124	26.371520
209.665943	8815.878803	26.376538
209.605705	8835.887430	26.381556
210.071215	8844.757086	26.386573
210.081450	8857.708340	26.391591
210.239542	8874.388910	26.396608
210.550377	8892.323128	26.401626
210.809748	8909.442833	26.406644
211.227812	8911.415148	26.411661
211.264182	8932.781702	26.416679
211.254515	8953.726746	26.421696
211.840927	8956.703510	26.426714
212.040677	8986.600057	26.431732
212.376178	8988.097250	26.436749
212.688336	8999.109879	26.441767
213.111386	9010.773737	26.446784
213.388502	9008.400239	26.451802
213.110614	9015.921649	26.456820
213.623628	9008.235697	26.461837
213.686329	9010.638864	26.466855
213.706109	9038.675552	26.471872
214.427803	9038.604591	26.476890
214.260425	9044.888248	26.481908
214.370313	9048.434406	26.486925
214.489811	9058.348925	26.491943
214.729758	9079.056044	26.496960
214.771193	9074.282946	26.501978
215.060977	9101.969017	26.506996
215.427487	9099.585583	26.512013
215.196353	9113.822840	26.517031
215.179058	9141.402513	26.522048
215.515243	9143.106580	26.527066
215.859864	9170.196974	26.532084
216.333545	9192.575059	26.537101
216.160635	9203.543186	26.542119
216.566824	9221.071091	26.547136
216.697534	9232.468912	26.552154
216.918433	9251.264656	26.557172
217.087215	9267.766896	26.562189
217.602885	9285.629979	26.567207
217.476887	9306.774665	26.572224
217.842134	9307.547480	26.577242
218.111567	9340.222983	26.582260
218.304422	9347.341751	26.587277
218.906957	9356.717130	26.592295
219.006150	9374.010848	26.597312
219.871861	9378.625693	26.602330
219.942548	9396.018809	26.607348
220.216252	9385.294987	26.612365
220.103135	9393.077165	26.617383
220.124744	9406.033768	26.622400
220.920092	9415.079405	26.627418
220.897106	9421.730928	26.632436
220.815580	9427.200720	26.637453
221.432262	9434.859109	26.642471
221.193097	9440.319409	26.647488
221.785242	9451.914949	26.652506
221.602029	9468.634061	26.657524
221.847806	9481.760393	26.662541
221.875667	9491.401384	26.667559
221.978761	9511.406515	26.672576
222.661152	9519.243345	26.677594
222.524100	9537.431128	26.682612
223.064530	9552.285554	26.687629
223.577988	9564.918356	26.692647
223.323901	9583.131540	26.697664
223.708982	9583.426274	26.702682
223.681659	9595.418147	26.707700
224.047592	9606.257389	26.712717
224.345283	9612.146064	26.717735
224.468396	9641.223125	26.722752
224.903793	9641.623951	26.727770
224.866162	9648.302304	26.732788
224.982174	9656.127184	26.737805
225.228854	9671.588485	26.742823
225.493399	9687.071744	26.747840
225.376299	9702.111404	26.752858
225.623274	9720.821734	26.757876
226.079703	9742.306633	26.762893
226.476458	9755.708583	26.767911
226.464936	9777.003307	26.772928
226.373301	9785.471262	26.777946
226.628655	9801.340150	26.782964
226.694486	9816.246489	26.787981
226.983637	9840.010137	26.792999
227.530050	9865.528317	26.798016
227.622904	9870.273993	26.803034
227.660770	9894.308763	26.808052
228.037726	9910.628212	26.813069
228.587018	9920.710493	26.818087
228.652281	9936.479578	26.823104
228.980060	9960.824353	26.828122
229.332251	9967.883390	26.833140
229.767071	9995.041168	26.838157
229.793168	9996.276139	26.843175
229.809253	10010.217880	26.848192
230.355823	10026.898406	26.853210
230.366686	10045.058107	26.858228
230.710484	10063.609017	26.863245
231.020237	10074.639350	26.868263
231.269422	10088.786795	26.873280
232.022608	10097.790778	26.878298
232.050923	10103.053641	26.883316
232.081744	10113.139211	26.888333
232.435414	10126.588891	26.893351
232.438750	10132.759218	26.898368
232.709976	10147.991623	26.903386
232.759926	10162.339313	26.908404
233.193239	10168.404520	26.913421
233.557882	10187.396521	26.918439
233.569405	10205.789657	26.923456
233.773367	10215.815036	26.928474
233.965993	10239.323187	26.933492
233.737598	10244.437745	26.938509
234.147335	10266.526205	26.943527
234.021411	10285.076317	26.948544
234.737498	10302.291656	26.953562
235.242439	10315.584783	26.958580
235.153062	10336.632208	26.963597
235.127868	10351.552012	26.968615
235.335081	10370.200625	26.973632
235.741533	10396.043048	26.978650
236.024693	10407.983321	26.983668
236.555813	10430.874315	26.988685
236.879442	10443.067486	26.993703
236.950958	10466.608478	26.998720
237.149488	10465.172224	27.003738
237.523039	10482.999381	27.008756
237.641747	10513.846071	27.013773
237.899251	10505.557891	27.018791
237.956168	10526.592885	27.023808
238.111549	10531.428361	27.028826
238.526334	10548.354381	27.033844
238.717366	10569.362548	27.038861
238.995405	10580.451433	27.043879
239.089314	10603.314002	27.048896
239.457917	10611.407629	27.053914
239.619822	10629.757240	27.058932
239.748350	10651.887156	27.063949
240.294155	10666.097260	27.068967
240.399198	10675.785733	27.073984
241.035518	10703.088572	27.079002
241.228543	10706.307453	27.084020
241.082939	10711.565983	27.089037
241.572042	10720.572301	27.094055
241.541254	10740.272608	27.099072
242.018896	10753.100225	27.104090
242.780935	10758.636729	27.109108
242.873790	10767.092747	27.114125
243.333663	10774.834672	27.119143
243.409475	10789.411404	27.124160
243.570314	10799.533375	27.129178
243.887617	10796.709706	27.134196
244.203955	10803.969250	27.139213
244.289016	10816.847299	27.144231
244.146295	10831.278675	27.149248
244.372516	10834.696528	27.154266
244.688506	10843.715955	27.159284
244.868185	10849.924971	27.164301
245.667931	10858.695331	27.169319
245.753080	10876.366855	27.174336
245.593874	10886.218394	27.179354
245.931331	10911.975502	27.184372
246.157450	10919.247516	27.189389
246.308771	10932.712464	27.194407
246.446272	10952.339787	27.199424
246.427237	10961.621253	27.204442
246.859442	10984.210498	27.209460
246.694815	11015.819978	27.214477
247.050235	11022.984463	27.219495
247.289950	11050.297237	27.224512
247.591989	11079.236003	27.229530
247.888057	11091.360505	27.234548
248.265401	11118.266206	27.239565
248.827747	11125.942789	27.244583
248.706712	11157.999743	27.249600
249.074817	11175.509637	27.254618
249.611043	11178.432685	27.259636
249.661671	11204.080174	27.264653
249.993241	11215.376254	27.269671
250.176032	11227.963213	27.274688
250.288916	11251.645817	27.279706
250.364720	11262.546277	27.284724
250.619661	11292.660950	27.289741
251.081833	11296.962551	27.294759
251.310853	11325.713121	27.299776
251.147338	11333.463402	27.304794
251.734902	11352.209228	27.309812
251.804570	11373.639851	27.314829
252.076054	11383.620418	27.319847
252.737061	11409.321294	27.324864
252.667879	11426.846676	27.329882
253.254238	11440.040655	27.334900
253.395718	11459.809675	27.339917
253.832401	11464.567557	27.344935
254.041067	11485.988973	27.349952
254.114816	11497.544377	27.354970
254.553604	11504.042144	27.359988
254.597517	11539.866891	27.365005
254.770037	11552.017556	27.370023
255.289793	11570.078692	27.375040
255.758152	11579.808416	27.380058
255.996899	11601.225594	27.385076
256.203813	11619.149723	27.390093
256.511291	11625.100993	27.395111
256.362232	11635.568860	27.400128
256.484578	11656.009018	27.405146
256.985945	11666.226837	27.410164
256.979542	11692.082586	27.415181
257.372346	11704.226400	27.420199
257.408764	11725.546923	27.425216
257.511464	11742.503565	27.430234
258.178870	11767.172561	27.435252
258.239636	11791.013270	27.440269
258.910324	11803.326369	27.445287
258.952833	11828.967945	27.450304
259.153766	11847.339181	27.455322
259.739036	11859.765507	27.460340
260.075644	11879.478589	27.465357
260.363518	11890.514923	27.470375
260.671231	11909.673226	27.475392
260.651906	11926.780968	27.480410
261.162505	11916.878287	27.485428
260.957241	11934.907055	27.490445
261.516280	11946.445859	27.495463
261.589165	11964.243984	27.500480
261.930392	11985.586733	27.505498
262.575692	12000.678348	27.510516
262.517353	12006.696734	27.515533
262.760551	12034.936354	27.520551
262.871885	12044.975156	27.525568
262.879142	12067.376965	27.530586
263.112931	12081.546050	27.535604
263.514557	12108.680656	27.540621
264.068827	12122.535414	27.545639
264.146106	12126.288208	27.550656
264.549252	12146.197449	27.555674
265.426607	12157.033763	27.560692
265.354876	12177.182058	27.565709
265.702840	12171.089924	27.570727
265.951503	12181.206496	27.575744
265.947508	12205.876374	27.580762
266.168677	12207.154816	27.585780
266.460543	12218.322593	27.590797
267.037419	12231.198428	27.595815
266.955083	12236.622529	27.600832
267.206838	12253.142951	27.605850
267.427286	12266.601610	27.610868
267.556378	12279.299541	27.615885
267.806666	12299.277032	27.620903
268.354154	12313.582487	27.625920
268.600516	12330.888012	27.630938
268.318299	12352.181686	27.635956
268.751509	12374.594767	27.640973
269.131279	12383.141342	27.645991
269.621299	12402.004576	27.651008
269.411601	12429.196460	27.656026
270.345400	12437.083708	27.661044
270.716053	12448.364840	27.666061
270.780632	12466.440762	27.671079
271.077503	12472.503861	27.676096
271.209627	12490.468097	27.681114
271.544443	12498.162761	27.686132
271.533674	12524.475577	27.691149
271.782913	12536.199795	27.696167
272.141072	12557.796466	27.701184
272.140031	12582.919670	27.706202
272.421780	12598.351424	27.711220
272.816460	12621.274771	27.716237
272.958784	12636.104791	27.721255
273.515110	12656.759902	27.726272
273.873081	12678.648997	27.731290
274.031192	12694.195600	27.736308
274.127204	12706.525667	27.741325
275.047977	12725.579813	27.746343
275.343326	12737.659311	27.751360
275.670721	12760.309635	27.756378
276.001041	12762.515682	27.761396
275.997137	12778.427055	27.766413
276.172640	12794.725851	27.771431
276.387222	12810.935589	27.776448
276.323477	12833.757972	27.781466
277.010820	12848.077852	27.786484
277.001864	12874.107219	27.791501
277.156943	12891.791198	27.796519
277.428346	12906.903564	27.801536
277.635833	12940.025717	27.806554
278.010187	12953.123559	27.811572
278.596325	12976.681080	27.816589
278.391464	12982.973221	27.821607
278.705847	13010.570346	27.826624
279.050766	13032.549601	27.831642
279.346915	13043.431866	27.836660
279.526555	13064.553641	27.841677
280.012262	13083.854788	27.846695
280.085882	13101.789811	27.851712
280.467908	13124.213634	27.856730
280.631275	13141.663978	27.861748
280.938469	13164.148196	27.866765
280.754484	13179.452766	27.871783
281.486247	13200.414313	27.876800
281.289954	13228.208444	27.881818
282.022510	13255.362314	27.886836
282.260277	13280.805878	27.891853
282.467153	13312.403027	27.896871
282.903643	13327.457423	27.901888
283.275848	13349.993863	27.906906
283.325199	13372.675047	27.911924
283.767580	13391.126760	27.916941
283.628125	13412.864469	27.921959
284.358129	13432.821012	27.926976
284.217790	13471.912080	27.931994
284.809452	13489.607559	27.937012
285.171457	13514.056898	27.942029
285.465968	13536.065381	27.947047
286.021778	13553.890727	27.952064
285.968960	13581.092324	27.957082
286.369159	13588.327252	27.962100
286.597452	13614.586527	27.967117
286.837391	13645.375781	27.972135
287.616728	13666.986111	27.977152
287.468107	13691.520561	27.982170
288.168906	13697.862987	27.987188
288.208187	13721.023030	27.992205
288.626164	13741.983479	27.997223
288.767188	13758.812771	28.002240
289.549413	13782.224475	28.007258
289.522823	13800.482310	28.012276
289.918454	13808.495222	28.017293
290.013459	13835.922266	28.022311
289.984990	13852.097755	28.027328
290.372436	13882.371099	28.032346
290.786829	13893.990339	28.037364
291.431304	13914.249456	28.042381
291.848230	13935.585930	28.047399
292.709093	13942.126808	28.052416
292.500210	13955.712558	28.057434
292.578572	13964.009915	28.062452
293.238071	13984.925418	28.067469
293.444259	13986.797883	28.072487
293.852003	13999.882352	28.077504
293.729627	14019.135871	28.082522
294.419451	14022.447208	28.087540
294.466934	14040.575737	28.092557
294.432012	14057.905818	28.097575
294.833805	14061.532980	28.102592
294.780677	14084.272389	28.107610
295.182368	14099.144659	28.112628
295.562558	14098.549177	28.117645
295.602600	14123.025025	28.122663
295.880436	14139.538123	28.127680
295.907402	14169.043710	28.132698
296.386138	14189.147148	28.137716
297.086545	14207.242861	28.142733
296.581267	14225.172768	28.147751
297.428301	14241.626750	28.152768
297.557305	14274.217883	28.157786
297.585525	14295.663847	28.162804
297.906202	14321.190002	28.167821
297.838691	14349.706311	28.172839
298.737163	14379.401282	28.177856
299.007358	14411.197846	28.182874
299.139725	14430.073269	28.187892
299.491478	14456.567406	28.192909
299.666910	14480.415298	28.197927
300.189296	14510.786268	28.202944
300.321038	14541.697499	28.207962
300.169137	14573.646790	28.212980
301.024231	14600.099726	28.217997
301.457142	14631.762080	28.223015
301.665107	14656.834321	28.228032
301.768388	14675.431967	28.233050
302.191649	14702.007632	28.238068
302.583999	14727.371597	28.243085
302.600029	14756.202541	28.248103
303.498778	14776.904070	28.253120
303.480297	14813.672826	28.258138
303.775661	14828.295289	28.263156
303.955913	14851.009954	28.268173
304.306727	14878.947590	28.273191
305.007863	14907.094353	28.278208
305.018841	14930.028988	28.283226
305.394641	14965.698764	28.288244
306.198058	14989.189541	28.293261
306.166937	15009.381146	28.298279
306.537051	15026.566682	28.303296
307.140946	15035.742097	28.308314
307.701428	15054.025455	28.313332
308.353789	15060.000956	28.318349
308.322937	15078.552074	28.323367
308.754132	15086.980486	28.328384
308.793554	15098.851807	28.333402
308.948804	15121.265304	28.338420
309.501081	15127.351548	28.343437
309.585009	15155.569480	28.348455
309.988011	15163.597975	28.353472
310.279258	15180.785231	28.358490
310.705808	15196.259617	28.363508
311.084275	15216.826395	28.368525
311.247089	15217.928508	28.373543
311.676954	15227.152735	28.378560
311.929974	15243.125704	28.383578
311.666376	15250.858091	28.388596
312.543853	15253.371532	28.393613
312.522978	15286.375541	28.398631
312.873929	15293.196963	28.403648
312.956030	15310.634391	28.408666
313.396247	15328.825453	28.413684
313.594117	15347.045122	28.418701
313.644554	15366.871798	28.423719
313.920892	15386.948474	28.428736
314.563738	15411.085761	28.433754
315.211789	15424.876240	28.438772
315.856414	15435.238516	28.443789
315.741459	15458.005260	28.448807
316.134562	15467.507396	28.453824
316.390829	15484.734421	28.458842
316.459705	15503.731600	28.463860
317.128879	15512.640644	28.468877
316.997373	15539.536057	28.473895
317.648917	15564.071644	28.478912
317.550377	15581.678106	28.483930
317.767425	15607.815248	28.488948
318.367880	15619.817901	28.493965
318.458522	15651.428753	28.498983
318.857922	15671.117052	28.504000
319.327399	15697.988214	28.509018
319.240032	15735.628291	28.514036
320.072913	15744.181115	28.519053
320.101473	15770.053338	28.524071
320.087636	15794.856530	28.529088
320.474438	15818.854680	28.534106
320.561329	15851.223323	28.539124
321.344696	15874.433265	28.544141
321.410993	15905.968412	28.549159
321.450453	15925.181792	28.554176
321.756824	15960.156868	28.559194
322.449807	15998.337704	28.564212
322.908685	16028.967734	28.569229
323.156891	16049.803698	28.574247
323.579397	16071.471845	28.579264
323.823004	16104.209105	28.584282
323.820492	16136.497330	28.589300
324.892796	16153.226204	28.594317
325.091600	16183.613967	28.599335
325.276320	16204.537020	28.604352
325.614931	16230.107876	28.609370
325.519941	16258.348173	28.614388
326.275408	16275.820903	28.619405
326.383804	16317.507320	28.624423
326.865252	16338.606274	28.629440
326.992926	16362.174963	28.634458
327.472613	16374.855260	28.639476
328.167519	16399.080973	28.644493
328.197002	16428.487841	28.649511
328.625884	16439.287897	28.654528
329.556497	16446.491427	28.659546
329.550711	16467.724499	28.664564
329.990804	16466.474183	28.669581
330.301766	16493.292476	28.674599
330.728668	16509.569333	28.679616
330.833126	16527.655890	28.684634
330.847709	16543.902240	28.689652
331.146045	16559.048565	28.694669
331.081392	16583.214133	28.699687
331.347218	16609.419011	28.704704
331.912725	16631.339149	28.709722
332.191070	16659.527375	28.714740
332.797301	16688.758386	28.719757
333.002177	16709.967076	28.724775
333.336745	16734.301327	28.729792
333.346479	16761.594629	28.734810
333.428788	16791.061873	28.739828
333.904682	16829.241768	28.744845
334.314065	16849.900187	28.749863
334.573902	16882.724495	28.754880
335.633808	16902.354188	28.759898
335.719565	16930.297633	28.764916
336.169830	16948.172498	28.769933
336.878429	16978.834892	28.774951
337.091972	17001.708830	28.779968
337.418978	17015.335975	28.784986
337.339109	17042.836952	28.790004
338.019522	17065.689142	28.795021
338.143775	17088.298320	28.800039
338.424400	17120.447026	28.805056
338.526820	17136.701062	28.810074
338.994535	17172.516706	28.815092
339.372636	17188.837095	28.820109
339.531553	17221.777019	28.825127
339.863421	17250.231006	28.830144
340.473781	17274.494010	28.835162
340.885553	17301.423618	28.840180
341.013038	17330.231962	28.845197
341.296576	17361.674041	28.850215
341.571453	17387.754391	28.855232
342.291930	17407.859277	28.860250
342.490869	17446.713940	28.865268
342.576520	17466.199225	28.870285
342.776812	17503.004672	28.875303
342.781926	17534.834767	28.880320
343.684022	17563.218539	28.885338
343.615108	17607.389761	28.890356
343.921232	17637.895360	28.895373
344.599270	17669.329527	28.900391
344.637446	17707.755747	28.905408
344.955921	17741.734713	28.910426
345.445115	17768.458311	28.915444
345.917831	17802.898651	28.920461
346.738967	17828.276953	28.925479
347.010997	17848.830249	28.930496
347.691193	17867.160674	28.935514
347.851422	17891.968421	28.940532
348.254938	17914.189027	28.945549
348.537583	17926.059685	28.950567
348.945747	17948.635504	28.955584
349.240650	17961.655019	28.960602
349.350864	17988.299624	28.965620
349.746292	18012.923234	28.970637
349.992209	18041.007722	28.975655
350.437280	18056.970718	28.980672
350.839648	18072.316910	28.985690
351.042705	18096.326815	28.990708
351.400268	18120.404658	28.995725
351.744671	18150.865795	29.000743
352.194540	18178.054638	29.005760
352.384251	18201.338084	29.010778
352.575514	18235.826204	29.015796
352.734439	18252.760997	29.020813
353.288711	18298.012845	29.025831
353.346591	18339.867471	29.030848
353.901086	18365.065911	29.035866
354.101668	18398.997382	29.040884
354.235983	18427.338941	29.045901
354.934156	18455.466681	29.050919
355.424353	18485.659959	29.055936
356.181163	18513.691056	29.060954
356.646464	18543.405721	29.065972
356.754555	18580.672521	29.070989
357.215851	18601.668718	29.076007
357.187610	18619.950715	29.081024
358.299344	18635.289156	29.086042
358.784806	18660.351432	29.091060
359.258271	18672.780074	29.096077
359.849326	18686.995186	29.101095
359.761123	18698.757806	29.106112
360.388380	18718.519395	29.111130
360.503178	18733.306132	29.116148
360.910886	18759.097921	29.121165
361.054125	18777.628381	29.126183
361.494489	18800.780259	29.131200
361.951734	18813.150179	29.136218
361.628355	18849.680821	29.141236
362.073554	18866.742721	29.146253
362.589827	18885.818233	29.151271
363.356725	18901.095347	29.156288
363.701722	18925.777655	29.161306
363.591616	18947.304373	29.166324
364.325011	18972.677274	29.171341
364.591978	18997.261886	29.176359
364.807396	19024.765177	29.181376
365.616986	19043.170480	29.186394
365.660074	19069.239401	29.191412
365.191669	19094.999686	29.196429
366.172994	19126.840480	29.201447
366.439586	19156.931312	29.206464
367.272097	19165.274888	29.211482
367.670467	19181.829205	29.216500
367.677659	19198.191914	29.221517
367.996727	19219.036793	29.226535
368.298061	19250.729482	29.231552
368.837219	19265.983399	29.236570
369.151737	19304.821133	29.241588
369.119419	19320.649670	29.246605
369.596027	19335.154503	29.251623
369.710424	19379.527142	29.256640
369.937876	19417.777401	29.261658
370.351748	19449.684472	29.266676
370.893053	19477.724876	29.271693
371.284244	19511.952442	29.276711
371.524599	19550.381302	29.281728
372.044929	19577.543644	29.286746
372.324823	19613.383815	29.291764
372.463850	19637.701603	29.296781
373.367744	19672.308503	29.301799
373.465021	19713.659690	29.306816
373.889127	19747.336798	29.311834
373.990522	19775.669511	29.316852
374.141920	19808.981497	29.321869
374.719149	19840.551489	29.326887
375.188736	19889.146642	29.331904
375.749550	19907.382744	29.336922
376.216488	19940.273819	29.341940
376.846374	19967.269758	29.346957
377.506786	19997.944419	29.351975
378.030111	20024.304203	29.356992
378.382594	20036.473653	29.362010
378.650093	20064.613471	29.367028
378.973550	20093.644543	29.372045
379.662048	20110.133141	29.377063
379.656091	20143.339397	29.382080
380.051506	20167.512810	29.387098
380.511899	20191.854277	29.392116
380.439097	20214.779349	29.397133
381.151096	20243.748002	29.402151
381.339394	20282.801608	29.407168
381.484864	20306.618546	29.412186
381.888788	20333.933448	29.417204
382.292642	20377.998972	29.422221
382.590246	20401.219679	29.427239
383.020343	20441.893675	29.432256
383.675402	20472.713056	29.437274
383.770372	20503.398872	29.442292
383.880669	20535.516395	29.447309
384.289787	20567.302072	29.452327
384.808199	20596.834595	29.457344
385.310857	20629.282770	29.462362
385.734495	20666.811393	29.467380
386.082984	20706.022447	29.472397
386.831783	20738.457618	29.477415
386.670437	20772.873633	29.482432
387.287361	20793.082888	29.487450
387.839831	20822.808871	29.492468
387.954399	20850.928001	29.497485
388.319472	20876.732046	29.502503
388.469979	20911.421568	29.507520
388.859772	20944.772795	29.512538
389.237770	20983.667182	29.517556
389.091270	21019.624183	29.522573
389.569230	21047.604644	29.527591
389.975804	21086.971204	29.532608
390.270033	21128.279768	29.537626
391.093261	21166.950093	29.542644
391.199118	21211.971523	29.547661
391.540579	21257.539915	29.552679
391.957868	21298.558395	29.557696
392.422362	21340.177464	29.562714
393.009624	21382.564652	29.567732
393.302605	21430.088931	29.572749
394.072197	21452.661059	29.577767
394.108878	21498.321238	29.582784
394.655864	21535.787388	29.587802
397.845747	21494.995333	29.592820
398.866798	21495.384753	29.597837
399.599600	21501.004720	29.602855
399.498921	21486.631749	29.607872
399.592081	21480.627404	29.612890
400.042804	21477.193442	29.617908
399.737573	21484.244429	29.622925
400.152647	21486.741083	29.627943
400.465284	21489.099695	29.632960
400.863512	21485.067662	29.637978
401.428517	21482.328248	29.642996
400.845874	21505.912936	29.648013
401.099512	21514.442958	29.653031
401.526555	21540.731245	29.658048
401.747697	21550.414755	29.663066
401.655815	21565.862827	29.668084
401.535720	21601.864989	29.673101
402.057061	21645.562116	29.678119
401.777243	21681.296139	29.683136
402.279393	21730.028445	29.688154
402.651050	21772.428986	29.693172
403.005509	21824.860803	29.698189
403.275903	21872.739707	29.703207
403.787512	21916.398967	29.708224
404.110020	21962.996296	29.713242
404.961243	22008.088688	29.718260
405.137889	22054.991489	29.723277
405.653664	22094.199035	29.728295
406.120434	22134.297396	29.733312
406.455793	22179.312584	29.738330
406.893185	22215.224166	29.743348
407.031463	22266.015062	29.748365
407.906849	22299.804526	29.753383
408.270213	22340.001009	29.758400
408.638550	22376.979370	29.763418
409.373869	22401.683327	29.768436
409.535463	22443.660741	29.773453
409.708839	22484.433683	29.778471
410.228696	22519.950820	29.783488
410.580596	22555.334120	29.788506
411.243944	22584.911081	29.793524
411.310531	22638.908438	29.798541
411.834427	22666.467011	29.803559
412.727492	22701.265055	29.808576
413.031001	22734.145479	29.813594
413.491054	22764.119055	29.818612
413.640410	22806.152150	29.823629
414.344469	22828.324761	29.828647
414.855472	22863.107633	29.833664
415.704947	22884.448243	29.838682
416.856704	22897.252254	29.843700
416.886770	22923.974711	29.848717
417.374614	22956.870337	29.853735
417.496171	22982.459065	29.858752
418.013188	22993.968567	29.863770
418.497233	23020.295132	29.868788
418.497906	23054.561116	29.873805
419.044025	23071.922250	29.878823
419.224749	23105.900520	29.883840
419.385153	23139.838780	29.888858
419.837103	23165.476772	29.893876
420.204349	23204.778473	29.898893
420.721433	23243.330961	29.903911
421.085325	23286.485863	29.908928
421.470164	23309.001445	29.913946
421.655639	23345.651237	29.918964
422.072210	23383.597822	29.923981
422.875274	23409.358282	29.928999
423.269722	23446.918645	29.934016
423.421401	23486.070283	29.939034
424.050443	23522.101590	29.944052
424.217057	23570.687436	29.949069
424.451284	23616.715294	29.954087
424.580621	23649.641904	29.959104
424.990559	23695.187501	29.964122
425.794617	23734.884867	29.969140
426.273716	23781.700473	29.974157
426.811391	23823.622403	29.979175
427.091029	23860.661677	29.984192
427.254637	23902.711154	29.989210
427.896774	23945.445419	29.994228
428.026607	23991.809222	29.999245
428.620721	24030.853113	30.004263
429.063023	24077.327285	30.009280
429.424036	24126.731424	30.014298
430.077181	24167.602392	30.019316
430.280942	24217.263451	30.024333
430.864934	24255.628923	30.029351
431.344523	24284.467162	30.034368
431.617868	24329.824438	30.039386
432.037365	24355.990203	30.044404
432.625241	24398.349922	30.049421
432.984249	24444.025506	30.054439
433.847176	24470.451657	30.059456
434.100940	24498.623611	30.064474
435.011377	24523.987518	30.069492
435.286065	24561.157607	30.074509
435.780323	24593.076451	30.079527
436.489730	24611.031626	30.084544
436.301234	24658.138131	30.089562
436.955269	24682.298520	30.094580
437.302330	24723.897131	30.099597
437.424382	24762.953429	30.104615
437.953241	24793.023852	30.109632
438.112952	24844.701829	30.114650
438.707898	24877.009311	30.119668
439.046352	24927.339607	30.124685
439.338872	24965.872173	30.129703
439.836285	25015.852870	30.134720
439.903806	25065.386232	30.139738
440.712475	25111.193750	30.144756
440.835719	25164.481650	30.149773
441.336506	25213.059427	30.154791
441.817666	25251.912395	30.159808
442.094453	25309.359335	30.164826
443.008957	25348.998227	30.169844
443.244327	25401.987032	30.174861
443.506243	25455.453112	30.179879
444.203505	25501.744283	30.184896
444.336915	25553.818683	30.189914
444.976132	25599.262281	30.194932
445.573109	25650.743997	30.199949
446.275479	25692.396444	30.204967
446.830330	25736.177467	30.209984
446.790854	25785.648955	30.215002
447.364713	25826.536798	30.220020
447.845743	25881.039208	30.225037
448.593722	25918.975259	30.230055
449.098186	25954.630132	30.235072
449.482219	25998.234255	30.240090
450.711863	26022.380602	30.245108
451.333230	26059.767579	30.250125
451.769302	26083.739502	30.255143
452.568808	26109.010163	30.260160
453.079582	26129.578756	30.265178
453.658488	26156.694226	30.270196
453.957215	26178.476798	30.275213
454.159750	26210.325596	30.280231
454.624992	26228.968286	30.285248
454.652316	26261.101135	30.290266
454.995141	26288.843721	30.295284
455.414302	26324.272723	30.300301
455.541078	26360.518867	30.305319
456.091079	26385.193156	30.310336
456.248511	26422.479990	30.315354
456.780629	26452.668822	30.320372
456.905175	26500.930707	30.325389
457.071541	26537.634182	30.330407
457.462433	26585.069213	30.335424
457.868300	26637.570111	30.340442
458.214139	26685.430164	30.345460
458.852378	26731.846947	30.350477
458.724792	26790.853395	30.355495
459.416378	26834.771620	30.360512
459.893236	26891.352501	30.365530
460.547383	26938.350348	30.370548
460.960545	26984.747779	30.375565
461.238790	27040.673820	30.380583
462.071707	27086.958192	30.385600
462.309619	27142.322181	30.390618
463.032717	27189.101782	30.395636
464.065339	27232.568895	30.400653
464.397858	27282.135405	30.405671
465.109530	27320.340544	30.410688
465.495450	27361.162958	30.415706
466.109704	27400.187429	30.420724
466.443129	27436.670944	30.425741
466.741323	27493.230396	30.430759
467.388869	27521.911403	30.435776
467.634840	27575.569058	30.440794
468.121222	27617.767505	30.445812
468.592218	27663.545491	30.450829
468.957807	27709.283671	30.455847
469.372324	27752.439377	30.460864
470.029701	27804.487999	30.465882
470.390127	27846.954506	30.470900
470.720888	27896.743787	30.475917
470.914950	27949.495419	30.480935
471.623758	27997.647423	30.485952
471.805614	28047.922597	30.490970
471.920026	28106.015200	30.495988
472.740439	28156.551423	30.501005
473.770021	28211.531370	30.506023
474.640262	28247.036133	30.511040
474.742973	28293.873637	30.516058
475.181213	28338.123897	30.521076
475.836582	28375.992244	30.526093
475.894664	28432.468732	30.531111
476.751539	28474.060425	30.536128
477.889456	28506.201249	30.541146
477.840261	28553.125155	30.546164
478.407453	28585.210498	30.551181
478.815174	28643.029800	30.556199
479.550037	28675.213103	30.561216
479.417662	28722.948134	30.566234
479.917334	28768.522962	30.571252
480.715475	28818.957640	30.576269
480.669188	28862.090424	30.581287
481.580524	28900.172937	30.586304
482.134482	28935.064572	30.591322
482.274937	28978.390116	30.596340
482.702216	29011.532371	30.601357
482.781290	29061.500843	30.606375
483.272118	29110.626957	30.611392
483.386495	29163.858538	30.616410
484.148303	29212.008856	30.621428
485.001169	29257.911739	30.626445
485.260338	29318.771832	30.631463
485.775739	29369.543226	30.636480
486.251711	29421.457306	30.641498
486.516205	29469.318837	30.646516
487.289191	29519.685627	30.651533
487.538480	29580.718471	30.656551
488.166793	29626.368190	30.661568
488.537976	29677.912095	30.666586
489.947062	29706.500878	30.671604
490.737954	29747.042572	30.676621
490.974297	29793.155491	30.681639
491.531669	29830.957739	30.686656
492.243730	29862.023360	30.691674
492.845922	29904.102135	30.696692
493.463920	29933.959919	30.701709
494.302350	29975.303088	30.706727
494.435833	30002.689810	30.711744
495.085771	30036.602438	30.716762
495.353007	30068.617137	30.721780
495.943392	30096.530114	30.726797
496.697090	30119.452729	30.731815
497.029538	30153.225477	30.736832
497.490264	30185.121328	30.741850
497.741124	30224.683279	30.746868
498.561580	30255.053125	30.751885
498.693286	30293.776872	30.756903
499.117168	30321.663173	30.761920
499.564130	30375.658950	30.766938
500.026802	30412.024536	30.771956
500.831715	30440.055228	30.776973
500.933400	30486.018187	30.781991
501.178285	30520.454967	30.787008
502.041085	30563.819379	30.792026
502.319052	30603.661615	30.797044
503.261905	30637.413783	30.802061
503.394272	30693.036766	30.807079
504.077545	30717.230708	30.812096
504.315507	30761.549395	30.817114
504.755421	30808.360889	30.822132
505.482375	30841.652985	30.827149
505.922585	30891.723979	30.832167
506.352120	30934.527958	30.837184
506.757266	30976.651914	30.842202
507.105175	31027.760901	30.847220
507.812318	31070.730636	30.852237
508.509401	31098.098764	30.857255
509.417999	31129.527943	30.862272
510.045205	31156.045175	30.867290
510.308651	31183.364310	30.872308
510.602621	31211.944240	30.877325
511.256314	31255.718907	30.882343
511.467909	31293.117814	30.887360
512.162907	31320.590671	30.892378
512.169485	31360.126498	30.897396
512.573313	31396.256193	30.902413
512.775944	31458.346857	30.907431
513.366283	31493.239743	30.912448
513.751123	31559.377638	30.917466
514.094163	31607.407857	30.922484
514.673830	31657.862465	30.927501
515.012597	31716.688711	30.932519
515.492965	31777.541617	30.937536
516.467655	31824.289740	30.942554
516.512833	31885.554389	30.947572
516.973754	31948.116436	30.952589
517.358429	31997.863919	30.957607
518.295755	32051.268538	30.962624
519.064757	32101.183664	30.967642
519.191142	32172.071684	30.972660
520.012538	32217.272299	30.977677
520.457232	32278.525210	30.982695
521.069457	32340.782505	30.987712
521.630692	32390.830903	30.992730
521.857765	32453.555059	30.997748
522.550654	32497.268466	31.002765
523.275783	32565.569217	31.007783
523.353666	32619.246547	31.012800
524.181074	32664.018694	31.017818
524.481003	32727.432134	31.022836
525.354592	32796.038051	31.027853
525.666706	32845.930476	31.032871
525.876219	32898.249501	31.037888
526.990193	32962.401128	31.042906
527.209573	33019.520285	31.047924
528.011052	33067.210612	31.052941
528.162224	33144.372445	31.057959
528.748552	33194.092987	31.062976
529.578906	33249.884539	31.067994
529.771868	33314.950311	31.073012
530.850148	33365.973855	31.078029
531.249169	33410.097459	31.083047
531.674576	33478.422919	31.088064
532.259091	33525.362541	31.093082
532.670293	33581.891910	31.098100
533.102008	33640.667634	31.103117
533.642125	33717.243683	31.108135
533.886688	33762.762667	31.113152
534.544457	33823.999967	31.118170
534.975428	33890.701018	31.123188
535.991502	33930.518848	31.128205
538.005891	33941.919858	31.133223
538.484640	33983.150696	31.138240
539.432002	34007.395698	31.143258
539.612535	34038.864427	31.148276
540.117823	34056.555997	31.153293
540.675987	34099.048184	31.158311
540.933876	34121.929255	31.163328
541.808876	34143.523478	31.168346
542.034244	34188.528056	31.173364
542.317780	34212.051485	31.178381
542.696406	34251.339484	31.183399
542.870539	34288.193086	31.188416
543.403404	34332.624138	31.193434
544.032399	34378.906462	31.198452
544.377670	34415.665303	31.203469
544.770863	34471.155407	31.208487
544.980284	34530.456794	31.213504
545.534271	34576.843047	31.218522
545.825657	34632.302610	31.223540
546.488125	34685.899815	31.228557
547.173466	34746.196568	31.233575
547.365692	34809.340315	31.238592
547.974329	34864.898308	31.243610
548.350597	34932.472987	31.248628
548.969639	34992.022912	31.253645
549.377477	35058.673996	31.258663
549.708568	35131.755400	31.263680
550.715764	35184.586736	31.268698
550.802236	35257.381317	31.273716
551.865524	35321.520184	31.278733
552.636822	35385.556035	31.283751
553.166200	35443.357747	31.288768
554.114143	35495.281979	31.293786
555.459575	35531.920248	31.298804
557.421985	35542.916054	31.303821
557.986012	35569.236029	31.308839
558.790093	35595.383810	31.313856
559.503285	35606.178180	31.318874
559.713012	35625.556499	31.323892
560.393209	35648.083904	31.328909
560.747641	35665.478027	31.333927
560.831121	35694.677798	31.338944
560.964100	35727.267161	31.343962
561.220572	35764.087258	31.348980
561.853132	35794.610753	31.353997
562.024027	35837.648319	31.359015
562.217774	35884.948491	31.364032
562.950978	35932.114007	31.369050
562.801658	35990.609027	31.374068
563.580245	36049.875605	31.379085
564.170697	36095.456223	31.384103
564.281115	36162.234745	31.389120
564.666352	36223.707145	31.394138
565.075741	36283.771187	31.399156
565.821979	36351.335239	31.404173
565.977912	36408.411462	31.409191
566.727697	36471.225150	31.414208
567.595660	36523.502707	31.419226
568.024023	36588.783385	31.424244
567.996730	36652.500354	31.429261
569.222558	36705.766784	31.434279
569.280632	36776.557550	31.439296
570.193213	36831.011015	31.444314
570.463438	36901.960871	31.449332
571.134944	36958.114922	31.454349
571.696474	37028.437134	31.459367
572.290315	37096.720603	31.464384
573.086388	37144.399812	31.469402
573.788730	37219.286913	31.474420
574.186986	37276.515110	31.479437
574.744869	37345.593652	31.484455
575.298753	37408.390007	31.489472
575.746784	37472.926781	31.494490
576.465338	37544.880093	31.499508
577.055698	37612.917088	31.504525
577.640637	37684.851281	31.509543
577.944551	37749.850391	31.514560
578.678007	37810.357049	31.519578
579.171387	37887.071553	31.524596
579.770628	37957.724322	31.529613
580.510587	38028.148423	31.534631
580.809951	38104.374483	31.539648
581.506019	38174.639047	31.544666
581.928467	38244.021916	31.549684
582.336176	38325.860776	31.554701
582.928763	38402.298493	31.559719
583.615909	38473.134934	31.564736
584.804431	38538.712056	31.569754
585.141547	38607.761531	31.574772
585.735885	38682.801612	31.579789
586.670050	38752.890321	31.584807
586.907415	38826.155626	31.589824
587.767888	38888.145465	31.594842
588.347279	38956.219562	31.599860
588.985059	39027.200210	31.604877
589.945616	39087.590116	31.609895
589.932553	39160.619218	31.614912
590.758995	39221.726350	31.619930
591.120600	39296.913432	31.624948
591.623510	39362.356933	31.629965
592.730103	39429.943715	31.634983
593.201178	39505.970531	31.640000
593.892069	39569.371212	31.645018
594.108108	39644.102056	31.650036
594.475402	39710.069944	31.655053
595.056421	39789.310011	31.660071
595.287579	39868.919968	31.665088
596.416087	39939.780543	31.670106
596.797189	40019.411477	31.675124
597.537247	40098.488884	31.680141
598.113105	40166.432764	31.685159
599.099103	40235.308234	31.690176
599.637658	40289.397150	31.695194
600.077077	40364.655392	31.700212
600.519421	40421.283187	31.705229
601.439852	40473.457359	31.710247
602.286129	40536.735964	31.715264
603.184207	40580.193332	31.720282
603.784127	40641.357398	31.725300
604.241908	40704.253780	31.730317
605.088931	40749.760340	31.735335
605.273287	40815.110324	31.740352
605.684265	40869.896350	31.745370
606.590894	40945.508539	31.750388
606.842422	41008.495655	31.755405
607.329430	41062.320821	31.760423
607.615009	41137.316784	31.765440
608.245432	41200.458744	31.770458
608.801538	41279.266533	31.775476
609.438777	41353.702786	31.780493
610.486137	41418.659004	31.785511
611.149875	41503.591755	31.790528
611.643215	41563.287331	31.795546
612.178162	41639.598905	31.800564
612.744520	41717.104402	31.805581
613.497625	41775.945574	31.810599
614.037298	41855.607099	31.815616
614.611202	41930.954885	31.820634
615.380229	41997.799677	31.825652
615.428086	42072.395979	31.830669
616.321937	42150.807013	31.835687
616.679384	42226.244181	31.840704
618.052952	42288.574708	31.845722
618.787130	42368.116156	31.850740
618.924437	42443.037325	31.855757
619.665837	42496.823318	31.860775
620.369105	42576.282327	31.865792
621.552883	42639.085953	31.870810
622.754552	42694.559396	31.875828
623.268902	42757.075755	31.880845
624.491967	42794.976315	31.885863
625.163055	42845.424651	31.890880
625.582252	42892.184757	31.895898
626.201097	42950.161784	31.900916
626.798075	42987.550510	31.905933
627.690180	43036.002169	31.910951
628.245344	43096.614302	31.915968
628.557889	43141.950494	31.920986
629.113827	43184.103068	31.926004
629.195623	43251.137857	31.931021
630.288335	43299.507841	31.936039
630.468251	43358.682274	31.941056
630.749284	43426.452552	31.946074
631.311204	43492.288823	31.951092
632.023272	43568.397761	31.956109
632.552368	43626.542761	31.961127
632.773080	43699.872518	31.966144
632.910560	43769.004515	31.971162
633.525604	43829.092328	31.976180
634.116529	43901.026451	31.981197
634.625830	43969.415497	31.986215
635.237800	44051.466802	31.991232
635.602193	44134.381271	31.996250
636.444308	44213.589089	32.001268
636.413857	44303.718781	32.006285
637.495311	44386.536046	32.011303
638.150993	44475.875969	32.016320
638.491176	44568.310865	32.021338
639.278216	44642.062320	32.026356
640.032414	44743.347424	32.031373
640.717027	44833.340755	32.036391
641.201219	44925.612650	32.041408
641.970147	45012.628009	32.046426
643.016330	45096.463794	32.051444
643.664203	45182.858855	32.056461
644.351658	45247.580753	32.061479
644.974684	45333.958433	32.066496
645.085660	45425.361718	32.071514
646.353903	45508.164036	32.076532
647.239446	45591.481986	32.081549
648.063169	45665.944930	32.086567
649.011498	45742.473743	32.091584
649.630640	45813.773973	32.096602
650.652407	45884.054441	32.101620
650.947045	45960.937532	32.106637
651.434129	46029.745177	32.111655
652.437060	46100.793014	32.116672
653.097959	46177.413664	32.121690
654.073482	46237.506012	32.126708
654.480572	46321.294835	32.131725
655.420254	46384.441133	32.136743
655.573091	46445.179452	32.141760
656.236225	46510.408386	32.146778
658.106013	46552.287353	32.151796
658.666911	46623.574909	32.156813
659.491065	46675.880929	32.161831
660.211133	46733.945927	32.166848
660.754278	46809.909744	32.171866
661.168904	46848.342271	32.176884
661.559079	46925.059770	32.181901
661.973559	46984.101854	32.186919
662.666748	47048.939922	32.191936
663.177119	47125.777983	32.196954
663.815230	47202.422507	32.201972
664.214807	47262.436532	32.206989
664.958554	47337.174871	32.212007
665.680884	47408.540869	32.217024
665.867490	47490.410980	32.222042
666.358907	47558.924172	32.227060
666.687456	47653.058906	32.232077
667.274949	47726.738368	32.237095
667.744308	47808.296734	32.242112
668.544379	47893.478733	32.247130
669.510679	47967.114661	32.252148
670.159241	48056.391909	32.257165
670.584802	48130.815094	32.262183
671.500601	48208.095010	32.267200
671.748460	48305.284659	32.272218
672.285069	48378.258667	32.277236
673.057027	48458.516010	32.282253
674.191802	48544.436700	32.287271
674.829058	48628.644740	32.292288
675.569811	48699.369308	32.297306
677.002501	48757.125555	32.302324
678.675937	48820.198468	32.307341
680.364892	48845.580291	32.312359
681.821583	48870.756160	32.317376
682.430707	48917.950195	32.322394
683.269323	48952.290260	32.327412
683.376304	48984.336086	32.332429
683.664976	49024.670915	32.337447
684.340623	49063.760914	32.342464
684.463537	49114.295665	32.347482
685.331967	49153.528721	32.352500
685.709318	49213.966274	32.357517
685.952849	49267.101342	32.362535
686.481768	49317.224921	32.367552
686.615894	49393.406951	32.372570
687.285417	49455.392363	32.377588
687.845707	49530.898106	32.382605
688.197160	49595.370753	32.387623
688.629135	49687.978819	32.392640
689.121416	49773.244094	32.397658
690.057486	49852.146778	32.402676
690.476656	49941.924438	32.407693
691.203329	50026.711815	32.412711
692.148336	50113.724303	32.417728
692.602530	50203.582905	32.422746
693.225667	50293.266743	32.427764
694.169521	50384.522016	32.432781
694.868427	50458.895643	32.437799
696.596045	50510.053008	32.442816
697.673862	50592.388794	32.447834
698.425365	50657.540035	32.452852
699.190761	50717.712619	32.457869
699.670496	50784.980945	32.462887
700.480747	50842.082523	32.467904
700.784758	50921.649138	32.472922
701.463690	50980.618223	32.477940
702.246222	51052.547855	32.482957
702.869902	51128.511010	32.487975
703.675190	51200.579626	32.492992
704.010712	51273.815258	32.498010
704.758560	51333.440424	32.503028
705.288369	51408.911610	32.508045
705.755305	51491.901069	32.513063
706.815614	51558.249856	32.518080
706.993334	51642.576832	32.523098
707.660313	51704.261161	32.528116
708.196850	51791.185874	32.533133
708.762836	51877.367816	32.538151
709.569725	51950.777328	32.543168
709.742402	52040.282819	32.548186
710.620746	52115.433218	32.553204
710.936539	52207.469986	32.558221
711.514214	52312.421192	32.563239
712.350503	52403.110511	32.568256
712.841145	52510.787802	32.573274
713.813103	52598.006880	32.578292
714.358605	52696.110347	32.583309
716.259436	52762.083585	32.588327
718.278336	52815.445199	32.593344
718.826449	52893.555078	32.598362
719.687880	52957.968080	32.603380
720.437982	53022.358003	32.608397
720.733607	53104.826662	32.613415
721.197446	53169.120650	32.618432
721.428493	53233.253083	32.623450
721.988715	53307.253407	32.628468
723.065445	53397.754785	32.633485
723.656074	53476.990352	32.638503
724.432315	53558.052613	32.643520
724.687658	53651.510893	32.648538
725.393808	53736.189605	32.653556
726.347258	53821.937217	32.658573
726.515829	53923.888620	32.663591
727.122803	54006.816826	32.668608
727.742118	54113.694062	32.673626
728.170429	54212.701860	32.678644
729.109904	54315.331301	32.683661
730.119426	54410.109586	32.688679
731.077375	54492.188709	32.693696
731.970028	54593.482525	32.698714
732.590286	54692.171976	32.703732
733.420801	54776.999870	32.708749
734.155661	54868.939227	32.713767
735.621129	54946.031226	32.718784
736.445739	55019.440878	32.723802
737.231094	55106.597550	32.728820
738.054804	55190.039564	32.733837
738.939827	55272.686209	32.738855
739.528188	55340.026770	32.743872
740.423199	55434.134154	32.748890
740.798224	55508.258130	32.753908
741.803200	55582.256873	32.758925
742.137156	55667.309994	32.763943
742.686629	55754.036958	32.768960
743.139117	55850.496036	32.773978
744.021297	55935.652533	32.778996
744.654667	56026.935172	32.784013
745.355573	56114.795092	32.789031
745.954112	56192.106112	32.794048
746.631404	56278.051273	32.799066
747.492355	56358.942023	32.804084
748.447302	56447.631207	32.809101
748.228063	56539.500376	32.814119
749.390677	56615.820541	32.819136
750.371696	56702.735833	32.824154
750.847462	56793.024550	32.829172
751.909813	56884.066374	32.834189
752.451832	56984.011787	32.839207
753.373675	57069.138808	32.844224
753.757850	57172.115725	32.849242
754.351551	57274.131727	32.854260
755.286409	57361.196377	32.859277
755.860836	57463.989945	32.864295
757.007629	57563.154007	32.869312
757.290274	57663.586358	32.874330
758.238812	57761.485517	32.879348
759.089123	57866.043213	32.884365
759.446640	57973.587580	32.889383
760.283083	58071.970310	32.894400
760.959557	58177.207787	32.899418
761.930632	58287.987031	32.904436
762.852460	58387.465985	32.909453
763.402295	58493.577835	32.914471
764.269892	58603.529322	32.919488
765.330623	58704.623269	32.924506
766.042768	58812.116042	32.929524
766.636994	58910.958520	32.934541
767.138925	59026.003293	32.939559
768.318993	59119.427391	32.944576
769.033728	59226.113888	32.949594
770.919246	59296.144981	32.954612
772.434270	59381.658639	32.959629
773.104763	59478.133497	32.964647
774.255460	59551.228279	32.969664
774.680080	59631.369248	32.974682
774.808188	59710.680017	32.979700
775.841472	59796.619567	32.984717
776.572796	59881.331999	32.989735
777.422102	59970.916823	32.994752
778.196513	60054.660180	32.999770
778.414748	60153.228085	33.004788
779.127859	60238.974353	33.009805
779.805397	60335.964018	33.014823
780.513248	60435.257464	33.019840
781.453704	60522.803330	33.024858
781.693868	60622.162734	33.029876
782.580393	60718.476985	33.034893
783.580017	60814.091702	33.039911
785.074394	60894.023596	33.044928
786.176128	60990.772307	33.049946
786.461549	61083.407671	33.054964
787.307136	61163.895514	33.059981
787.799467	61250.960367	33.064999
788.743049	61335.093003	33.070016
789.191843	61430.628020	33.075034
789.777978	61512.847983	33.080052
790.678301	61606.897402	33.085069
791.130019	61702.960662	33.090087
791.772716	61791.011375	33.095104
792.778214	61877.839561	33.100122
793.150685	61988.868620	33.105140
793.791777	62085.551018	33.110157
794.643758	62185.490723	33.115175
795.415395	62289.684633	33.120192
796.285662	62390.999303	33.125210
796.959600	62491.120536	33.130228
798.069911	62612.140795	33.135245
798.763341	62714.900050	33.140263
799.710093	62818.475323	33.145280
800.224102	62924.103185	33.150298
801.592503	63022.683018	33.155316
802.305362	63125.719302	33.160333
802.973862	63227.329504	33.165351
803.548958	63328.854062	33.170368
804.898551	63427.540046	33.175386
805.997588	63515.661937	33.180404
807.306513	63610.455246	33.185421
807.960867	63715.607260	33.190439
808.381068	63809.437705	33.195456
809.558322	63908.965231	33.200474
809.818663	64006.302248	33.205492
811.026927	64089.170195	33.210509
812.259929	64184.666907	33.215527
812.972859	64272.850597	33.220544
814.671896	64344.414501	33.225562
815.197612	64424.982900	33.230580
816.593396	64505.207886	33.235597
817.097718	64586.045653	33.240615
817.989839	64654.486250	33.245632
818.650172	64727.167514	33.250650
819.468481	64815.308513	33.255668
820.465537	64885.587095	33.260685
821.055165	64967.079276	33.265703
821.852971	65051.674793	33.270720
822.427092	65123.275376	33.275738
823.223488	65218.679358	33.280756
823.840542	65292.655066	33.285773
824.729570	65386.267035	33.290791
825.402886	65473.350845	33.295808
826.268500	65558.541041	33.300826
826.542516	65664.291735	33.305844
827.490391	65751.652101	33.310861
828.069192	65850.220611	33.315879
828.553334	65953.668591	33.320896
829.309760	66062.070373	33.325914
830.044023	66171.278529	33.330932
830.835622	66274.647716	33.335949
831.461142	66398.946500	33.340967
832.025889	66497.192074	33.345984
832.795023	66603.693480	33.351002
833.189974	66721.695117	33.356020
834.047323	66830.628415	33.361037
834.877875	66943.059935	33.366055
835.885255	67056.032507	33.371072
837.026741	67162.528268	33.376090
837.722252	67278.565052	33.381108
838.845634	67380.352272	33.386125
840.028919	67485.415466	33.391143
840.926863	67598.484425	33.396160
842.120291	67683.262266	33.401178
842.694928	67793.818984	33.406196
843.609147	67895.869621	33.411213
844.560072	67996.133441	33.416231
844.988824	68101.958109	33.421248
845.991768	68205.695648	33.426266
846.812685	68314.295613	33.431284
847.689319	68420.758299	33.436301
848.329007	68536.103906	33.441319
849.185648	68649.987883	33.446336
850.252398	68744.330137	33.451354
851.004619	68862.407947	33.456372
851.498248	68985.038488	33.461389
852.702424	69103.178501	33.466407
853.226123	69223.562939	33.471424
854.263584	69334.496981	33.476442
854.840025	69456.643458	33.481460
855.964150	69566.825831	33.486477
856.713897	69684.997446	33.491495
857.228792	69806.997949	33.496512
858.524119	69918.892508	33.501530
859.372709	70046.325454	33.506548
860.068260	70163.124911	33.511565
861.114191	70288.537816	33.516583
861.989065	70412.677192	33.521600
863.209031	70529.325870	33.526618
863.886084	70647.584339	33.531636
865.102968	70755.938957	33.536653
865.717574	70880.356475	33.541671
866.008926	70997.124102	33.546688
867.650753	71100.781617	33.551706
868.569659	71216.439729	33.556724
869.679927	71328.011595	33.561741
870.792164	71447.134419	33.566759
871.399475	71543.673620	33.571776
872.498142	71652.443722	33.576794
873.256148	71763.214769	33.581812
874.351701	71865.592084	33.586829
875.339266	71969.490963	33.591847
876.010510	72068.815412	33.596864
876.952214	72177.872443	33.601882
877.571092	72286.633910	33.606900
878.442152	72390.749415	33.611917
879.077668	72495.351585	33.616935
879.969765	72607.831056	33.621952
880.722638	72702.937297	33.626970
881.339941	72816.592762	33.631988
882.224854	72915.849526	33.637005
883.362893	73031.325370	33.642023
884.032178	73133.069312	33.647040
885.124938	73239.207671	33.652058
885.883582	73350.372917	33.657076
886.802236	73458.581227	33.662093
887.484998	73575.206921	33.667111
888.319050	73684.763269	33.672128
889.878058	73791.209524	33.677146
891.622384	73869.379580	33.682164
892.884278	73958.224215	33.687181
894.059602	74028.497811	33.692199
894.998510	74118.487799	33.697216
896.042782	74203.557568	33.702234
896.657884	74281.681424	33.707252
897.298568	74373.034448	33.712269
898.149012	74464.664166	33.717287
898.823566	74573.403942	33.722304
899.487821	74661.860189	33.727322
899.947807	74769.573482	33.732340
900.921351	74868.421373	33.737357
901.626513	74982.176258	33.742375
902.021109	75101.100144	33.747392
902.986002	75210.606080	33.752410
903.636296	75328.915528	33.757428
904.188562	75444.751269	33.762445
905.176198	75564.386134	33.767463
906.240848	75687.409541	33.772480
907.386195	75808.246810	33.777498
908.154327	75936.197879	33.782516
909.070604	76053.837251	33.787533
909.954909	76180.937143	33.792551
910.600547	76305.124339	33.797568
911.659649	76426.724787	33.802586
912.668961	76556.935592	33.807604
914.104616	76674.969938	33.812621
915.453415	76772.990051	33.817639
916.648420	76884.945952	33.822656
917.652172	76990.220769	33.827674
918.314513	77104.019664	33.832692
919.548771	77215.345427	33.837709
920.586361	77310.857913	33.842727
920.965130	77429.109041	33.847744
921.988818	77536.418681	33.852762
922.996520	77648.155762	33.857780
923.299457	77767.425869	33.862797
924.167749	77883.048248	33.867815
924.524755	78016.962242	33.872832
925.498981	78131.172318	33.877850
926.044702	78273.179963	33.882868
927.033545	78407.356255	33.887885
928.379603	78524.600190	33.892903
928.634371	78656.214909	33.897920
929.212068	78787.557860	33.902938
930.531463	78921.716524	33.907956
931.163880	79039.494121	33.912973
932.206915	79162.813735	33.917991
933.137164	79295.469158	33.923008
934.111439	79430.760618	33.928026
934.664344	79573.711609	33.933044
935.415707	79710.013810	33.938061
936.719283	79829.244127	33.943079
937.260151	79978.072174	33.948096
938.253865	80117.391638	33.953114
939.226463	80261.481643	33.958132
940.202388	80411.065349	33.963149
941.322619	80551.258910	33.968167
941.913578	80696.038468	33.973184
943.249860	80828.348338	33.978202
943.990191	80984.547970	33.983220
945.093594	81132.959761	33.988237
946.322801	81272.786847	33.993255
947.201423	81423.784074	33.998272
948.013938	81557.945651	34.003290
949.284022	81707.080973	34.008308
949.897616	81850.442569	34.013325
951.226652	81992.629260	34.018343
952.005621	82151.657331	34.023360
952.982259	82291.657865	34.028378
954.056427	82435.582385	34.033396
954.763759	82595.453395	34.038413
955.858549	82736.019723	34.043431
956.697362	82889.246571	34.048448
957.933101	83028.028572	34.053466
958.926039	83169.410592	34.058484
959.971030	83321.096791	34.063501
961.119562	83451.512223	34.068519
962.105181	83612.073748	34.073536
963.237691	83756.889478	34.078554
964.186474	83888.464768	34.083572
965.190142	84039.056292	34.088589
966.443606	84165.975797	34.093607
967.289574	84313.433137	34.098624
968.091107	84450.207155	34.103642
969.001775	84590.676049	34.108660
969.916795	84730.753178	34.113677
970.938452	84877.693329	34.118695
972.074742	85028.675441	34.123712
972.618583	85168.315013	34.128730
973.791929	85325.717259	34.133748
974.129384	85466.605599	34.138765
975.621398	85617.389874	34.143783
976.171584	85769.115414	34.148800
977.443121	85915.890200	34.153818
978.700084	86064.331269	34.158836
979.451960	86210.824017	34.163853
980.463114	86347.798189	34.168871
981.455462	86489.746221	34.173888
982.429154	86630.250152	34.178906
983.621312	86748.772338	34.183924
984.624286	86875.899614	34.188941
985.939877	87000.031256	34.193959
987.168094	87137.045499	34.198976
988.059639	87263.984130	34.203994
988.835524	87387.198451	34.209012
989.816810	87518.765692	34.214029
991.250864	87642.471178	34.219047
992.138256	87774.510209	34.224064
992.998585	87900.496384	34.229082
993.983534	88036.473725	34.234100
994.966175	88176.581625	34.239117
995.811442	88296.312103	34.244135
996.543228	88439.971256	34.249152
997.368145	88580.024652	34.254170
998.136313	88719.980476	34.259188
999.291703	88872.769918	34.264205
1000.092499	89015.953945	34.269223
1001.309646	89160.052894	34.274240
1002.411954	89307.845294	34.279258
1003.246076	89454.454501	34.284276
1004.088304	89591.267448	34.289293
1005.895749	89725.505587	34.294311
1007.074250	89870.646220	34.299328
1007.743611	90018.569231	34.304346
1008.808364	90162.035017	34.309364
1009.518845	90306.513062	34.314381
1010.748631	90453.907174	34.319399
1011.721407	90591.831351	34.324416
1012.796624	90732.503857	34.329434
1014.031740	90879.925287	34.334452
1014.660807	91030.119362	34.339469
1017.857964	91104.947993	34.344487
1020.638728	91204.350612	34.349504
1021.543830	91292.547694	34.354522
1022.641685	91389.758604	34.359540
1023.721795	91479.800673	34.364557
1024.728124	91573.858334	34.369575
1025.285434	91669.942138	34.374592
1025.876033	91758.336582	34.379610
1026.793932	91851.979420	34.384628
1027.572659	91966.320346	34.389645
1028.517403	92065.152429	34.394663
1028.916706	92181.989859	34.399680
1029.721096	92302.691192	34.404698
1030.461278	92419.709676	34.409716
1031.192536	92543.440916	34.414733
1032.094186	92667.961662	34.419751
1032.593979	92801.686615	34.424768
1033.238328	92941.271642	34.429786
1034.585887	93079.714710	34.434804
1035.588670	93226.366529	34.439821
1036.379434	93357.872715	34.444839
1038.160135	93475.110770	34.449856
1039.182349	93601.040736	34.454874
1040.370049	93717.868379	34.459892
1041.086845	93850.597363	34.464909
1042.067461	93966.485155	34.469927
1043.449511	94081.316622	34.474944
1044.088099	94210.517997	34.479962
1045.169663	94326.524436	34.484980
1046.002788	94473.869293	34.489997
1047.241140	94595.836068	34.495015
1048.335698	94721.318065	34.500032
1049.108057	94857.295504	34.505050
1050.440942	94989.737165	34.510068
1051.056614	95128.935597	34.515085
1052.178829	95260.273749	34.520103
1053.180454	95409.527281	34.525120
1054.007153	95549.966223	34.530138
1055.065585	95691.862070	34.535156
1055.886860	95841.779732	34.540173
1056.583381	95989.263792	34.545191
1057.770832	96142.047761	34.550208
1059.175349	96289.408523	34.555226
1060.332935	96436.050400	34.560244
1061.462714	96587.043641	34.565261
1062.361219	96742.085410	34.570279
1062.887444	96905.373462	34.575296
1063.942145	97071.634176	34.580314
1065.053351	97218.598475	34.585332
1066.086608	97375.862620	34.590349
1067.165903	97538.985016	34.595367
1068.757130	97698.585624	34.600384
1069.902268	97866.090378	34.605402
1070.894912	98021.745884	34.610420
1072.031282	98192.651728	34.615437
1072.893319	98341.105334	34.620455
1073.843631	98502.066147	34.625472
1074.678749	98678.312546	34.630490
1076.051816	98835.203712	34.635508
1077.135326	99008.192868	34.640525
1077.744248	99171.477637	34.645543
1079.222505	99333.271368	34.650560
1080.119242	99518.473163	34.655578
1081.137464	99680.747420	34.660596
1082.454444	99858.280181	34.665613
1083.606943	100032.189791	34.670631
1084.599933	100202.994194	34.675648
1085.585194	100378.704579	34.680666
1087.075569	100530.343479	34.685684
1088.007523	100699.465581	34.690701
1089.254630	100868.943736	34.695719
1090.531330	101037.608533	34.700736
1091.475766	101195.298891	34.705754
1093.047281	101360.464434	34.710772
1093.600886	101530.222213	34.715789
1094.549878	101690.965011	34.720807
1095.624906	101837.401408	34.725824
1096.553372	102005.717310	34.730842
1097.631960	102157.944841	34.735860
1098.815915	102312.934428	34.740877
1099.502368	102476.078249	34.745895
1101.134596	102631.852890	34.750912
1101.811790	102796.651942	34.755930
1103.240593	102961.927432	34.760948
1104.869561	103109.701116	34.765965
1105.922420	103258.257086	34.770983
1107.347597	103415.461985	34.776000
1108.185317	103568.926619	34.781018
1109.679487	103718.959333	34.786036
1110.779479	103864.353961	34.791053
1111.692571	104018.954907	34.796071
1113.175428	104174.415472	34.801088
1114.352628	104323.755718	34.806106
1114.807405	104474.806494	34.811124
1115.830592	104645.518261	34.816141
1116.893078	104798.233702	34.821159
1118.318903	104964.574176	34.826176
1119.124569	105140.690509	34.831194
1120.276640	105299.678996	34.836212
1121.300965	105457.581379	34.841229
1122.342432	105623.000335	34.846247
1123.775526	105788.345502	34.851264
1124.962313	105953.699340	34.856282
1126.638540	106101.604410	34.861300
1128.062354	106265.587371	34.866317
1129.441373	106420.591812	34.871335
1130.632489	106568.311103	34.876352
1131.313772	106735.244303	34.881370
1132.370317	106871.753259	34.886388
1133.822176	107028.686663	34.891405
1134.553620	107188.469739	34.896423
1135.782205	107352.035480	34.901440
1136.565195	107516.818735	34.906458
1138.066365	107680.957272	34.911476
1139.021147	107846.500257	34.916493
1139.638901	108008.705557	34.921511
1141.166475	108178.779992	34.926528
1142.031078	108348.929397	34.931546
1143.738928	108509.420375	34.936564
1145.745361	108645.383231	34.941581
1146.993831	108788.916994	34.946599
1148.304169	108932.979761	34.951616
1149.731588	109081.968027	34.956634
1150.749271	109216.838083	34.961652
1151.751583	109357.028086	34.966669
1152.931006	109508.539547	34.971687
1153.832678	109658.001031	34.976704
1154.784121	109808.335326	34.981722
1155.982798	109955.523384	34.986740
1157.087001	110110.069762	34.991757
1157.846110	110266.608878	34.996775
1159.254740	110400.828302	35.001792
1159.933859	110530.999463	35.006810
1161.194996	110669.206245	35.011828
1161.691741	110820.847022	35.016845
1163.370835	110978.193859	35.021863
1164.291591	111112.507399	35.026880
1165.024047	111282.837464	35.031898
1166.028663	111437.085177	35.036916
1167.250056	111585.374459	35.041933
1167.976990	111780.845457	35.046951
1169.199863	111936.846667	35.051968
1170.119293	112109.209976	35.056986
1171.222915	112277.240640	35.062004
1172.342492	112458.943282	35.067021
1172.977856	112648.706769	35.072039
1174.144317	112835.684187	35.077056
1175.262327	113027.247598	35.082074
1176.502854	113222.357047	35.087092
1178.326291	113408.778502	35.092109
1179.553236	113592.884245	35.097127
1180.699559	113764.577188	35.102144
1182.299924	113955.399961	35.107162
1183.503077	114132.201546	35.112180
1184.868323	114299.735727	35.117197
1186.052254	114499.498200	35.122215
1187.368459	114661.990623	35.127232
1188.600279	114851.258091	35.132250
1189.201446	115035.296614	35.137268
1190.534011	115213.990809	35.142285
1192.248746	115388.655960	35.147303
1194.180785	115566.579913	35.152320
1195.619750	115727.432580	35.157338
1196.907472	115892.919375	35.162356
1198.325078	116046.483994	35.167373
1199.259485	116233.105649	35.172391
1200.928391	116378.762617	35.177408
1201.839699	116545.206203	35.182426
1202.741997	116711.044497	35.187444
1203.990765	116868.053495	35.192461
1205.024915	117053.120424	35.197479
1206.106399	117222.314518	35.202496
1206.909903	117395.213531	35.207514
1207.874326	117569.962260	35.212532
1209.256008	117753.339111	35.217549
1210.089588	117949.562659	35.222567
1211.788798	118119.012681	35.227584
1212.827241	118305.126328	35.232602
1213.888413	118482.873432	35.237620
1215.202902	118677.588741	35.242637
1216.434404	118853.513073	35.247655
1217.745648	119045.743242	35.252672
1218.959483	119221.799519	35.257690
1219.914763	119408.694144	35.262708
1221.193755	119598.976944	35.267725
1222.247980	119786.124492	35.272743
1223.042044	119959.852631	35.277760
1223.882829	120155.863750	35.282778
1225.026739	120340.556788	35.287796
1226.623487	120515.427450	35.292813
1228.078303	120690.701783	35.297831
1229.509275	120863.663438	35.302848
1231.234601	121036.769408	35.307866
1232.119316	121222.155762	35.312884
1233.683022	121380.839081	35.317901
1234.858824	121571.956834	35.322919
1236.212123	121737.388219	35.327936
1237.477319	121922.161738	35.332954
1238.523416	122105.096916	35.337972
1239.569304	122285.259672	35.342989
1240.727818	122467.292900	35.348007
1241.534078	122653.145044	35.353024
1242.739360	122846.255792	35.358042
1244.093710	123048.704222	35.363060
1245.240772	123236.368120	35.368077
1246.202489	123430.598415	35.373095
1247.616360	123634.764392	35.378112
1248.665173	123834.202170	35.383130
1249.971153	124037.438410	35.388148
1251.500928	124241.679249	35.393165
1252.722247	124447.883302	35.398183
1254.149969	124651.662156	35.403200
1255.460370	124854.498540	35.408218
1256.521923	125054.602003	35.413236
1257.880727	125252.405008	35.418253
1259.055359	125474.837806	35.423271
1260.362585	125663.949871	35.428288
1261.743527	125866.757295	35.433306
1263.000009	126073.221491	35.438324
1264.298323	126262.871162	35.443341
1265.733256	126485.726876	35.448359
1266.805866	126687.842055	35.453376
1268.484145	126904.493460	35.458394
1269.373723	127108.401630	35.463412
1271.177983	127308.631620	35.468429
1272.225063	127529.644662	35.473447
1273.609105	127703.139207	35.478464
1275.076244	127912.130044	35.483482
1276.185639	128114.503241	35.488500
1277.492024	128313.869584	35.493517
1279.180213	128520.080891	35.498535
1280.553888	128710.647610	35.503552
1281.735942	128912.875749	35.508570
1283.273848	129107.903731	35.513588
1284.690062	129298.024324	35.518605
1285.880752	129485.369608	35.523623
1287.142461	129686.171813	35.528640
1288.078548	129881.908983	35.533658
1288.917452	130088.342936	35.538676
1290.638966	130278.447021	35.543693
1291.355116	130493.366422	35.548711
1292.413380	130685.922495	35.553728
1293.585480	130887.279666	35.558746
1294.714508	131076.938554	35.563764
1296.228364	131275.760971	35.568781
1297.138421	131476.910617	35.573799
1298.248264	131690.104179	35.578816
1299.708593	131880.704045	35.583834
1300.488803	132108.536101	35.588852
1302.385509	132306.608066	35.593869
1303.730653	132514.740439	35.598887
1305.229691	132728.741509	35.603904
1306.572340	132934.495353	35.608922
1307.773392	133142.490501	35.613940
1308.839892	133356.945141	35.618957
1310.039644	133571.291514	35.623975
1311.536416	133782.019156	35.628992
1313.451018	133998.561159	35.634010
1314.664732	134204.864120	35.639028
1316.117900	134416.553657	35.644045
1317.568735	134626.217755	35.649063
1318.616634	134833.603262	35.654080
1319.971313	135037.507600	35.659098
1320.851494	135260.001547	35.664116
1322.676684	135468.813955	35.669133
1323.858696	135689.147095	35.674151
1324.891635	135906.248999	35.679168
1326.429895	136122.081067	35.684186
1328.182798	136348.651618	35.689204
1329.414974	136560.125794	35.694221
1330.602144	136782.683938	35.699239
1332.052813	136995.355706	35.704256
1333.993524	137206.367112	35.709274
1335.164243	137429.705770	35.714292
1336.759971	137626.974959	35.719309
1337.966359	137844.747941	35.724327
1339.500639	138060.658245	35.729344
1340.884078	138256.127859	35.734362
1342.157931	138467.380987	35.739380
1343.489560	138680.540021	35.744397
1344.980106	138892.027855	35.749415
1345.838305	139100.310047	35.754432
1347.691532	139312.554292	35.759450
1348.587673	139538.525073	35.764468
1350.203099	139743.485098	35.769485
1351.422936	139958.483288	35.774503
1352.418367	140175.660484	35.779520
1354.041288	140395.426303	35.784538
1355.303840	140619.053073	35.789556
1356.918097	140832.131798	35.794573
1358.100662	141053.404516	35.799591
1359.287428	141260.255331	35.804608
1361.278007	141478.361014	35.809626
1362.691591	141690.653861	35.814644
1364.102413	141894.735797	35.819661
1365.075414	142106.936799	35.824679
1366.168547	142312.288739	35.829696
1367.865961	142512.641041	35.834714
1369.032671	142707.172697	35.839732
1369.879810	142904.544770	35.844749
1371.321130	143122.800185	35.849767
1372.714527	143318.655873	35.854784
1374.049160	143522.203067	35.859802
1374.948113	143736.163540	35.864820
1376.204985	143943.895905	35.869837
1377.748205	144171.864243	35.874855
1378.591893	144407.487137	35.879872
1380.416952	144619.075703	35.884890
1381.449597	144851.693252	35.889908
1383.161306	145086.625630	35.894925
1384.625441	145315.286707	35.899943
1385.815567	145534.232777	35.904960
1387.335273	145754.535004	35.909978
1388.572710	145996.267693	35.914996
1390.028431	146225.355040	35.920013
1391.670972	146448.482007	35.925031
1392.811904	146692.377609	35.930048
1394.529742	146922.619913	35.935066
1396.091234	147164.893155	35.940084
1397.476325	147384.961949	35.945101
1398.872991	147616.718104	35.950119
1400.230413	147848.317386	35.955136
1402.091760	148077.493097	35.960154
1403.050431	148331.165871	35.965172
1404.617182	148551.353282	35.970189
1406.425106	148787.641578	35.975207
1407.401376	149026.510424	35.980224
1409.025137	149242.421358	35.985242
1409.956298	149475.735456	35.990260
1411.516629	149722.566649	35.995277
1413.314643	149965.330551	36.000295
1414.516057	150206.149996	36.005312
1416.176465	150438.759300	36.010330
1417.428872	150674.439697	36.015348
1418.915033	150908.905621	36.020365
1420.352940	151150.645288	36.025383
1421.437111	151397.716959	36.030400
1423.375433	151632.559940	36.035418
1424.958448	151869.527585	36.040436
1426.289916	152111.709607	36.045453
1427.993681	152332.940432	36.050471
1429.318074	152573.466104	36.055488
1431.195959	152797.537679	36.060506
1433.148437	153030.435861	36.065524
1434.639661	153239.509742	36.070541
1436.166657	153450.962846	36.075559
1437.573017	153680.541772	36.080576
1439.176364	153888.232588	36.085594
1440.743668	154103.334927	36.090612
1441.985587	154316.778675	36.095629
1443.551608	154517.721391	36.100647
1445.066687	154711.978791	36.105664
1446.672982	154906.032628	36.110682
1448.026707	155098.707624	36.115700
1449.101716	155291.072977	36.120717
1450.586109	155482.207865	36.125735
1451.518251	155684.729046	36.130752
1453.075142	155892.236697	36.135770
1454.147688	156103.322164	36.140788
1455.078059	156314.165247	36.145805
1456.365334	156528.731521	36.150823
1457.256482	156751.794234	36.155840
1458.951530	156990.631424	36.160858
1459.843063	157238.004852	36.165876
1461.042150	157473.766838	36.170893
1462.794589	157710.266735	36.175911
1463.715984	157958.439429	36.180928
1465.280876	158205.040724	36.185946
1466.729022	158462.592963	36.190964
1468.077039	158723.320497	36.195981
1469.348630	158987.359115	36.200999
1470.484615	159259.207311	36.206016
1472.171229	159529.144072	36.211034
1473.509899	159810.969605	36.216052
1475.187734	160073.759820	36.221069
1476.741070	160339.348961	36.226087
1477.995765	160621.676182	36.231104
1479.670852	160901.161621	36.236122
1481.383140	161167.834988	36.241140
1482.940920	161444.845062	36.246157
1484.775715	161708.751088	36.251175
1486.446629	161981.029732	36.256192
1488.619494	162221.449813	36.261210
1490.308504	162483.799453	36.266228
1491.744492	162742.221700	36.271245
1493.736043	162987.051010	36.276263
1495.253280	163254.240069	36.281280
1496.775396	163502.254586	36.286298
1498.645470	163737.279423	36.291316
1500.029932	163983.771824	36.296333
1501.355078	164234.980556	36.301351
1502.927876	164484.667789	36.306368
1504.193422	164725.502216	36.311386
1506.010249	164975.471081	36.316404
1507.145615	165223.951844	36.321421
1509.270206	165465.326823	36.326439
1510.658459	165718.704429	36.331456
1512.085991	165959.229435	36.336474
1514.015645	166205.079307	36.341492
1515.801784	166441.453755	36.346509
1517.249158	166674.395564	36.351527
1518.429949	166925.112735	36.356544
1520.147131	167157.240982	36.361562
1521.662627	167408.314077	36.366580
1522.728212	167647.715136	36.371597
1524.217724	167885.972238	36.376615
1525.509406	168119.277478	36.381632
1526.763939	168351.055285	36.386650
1528.599109	168586.813857	36.391668
1529.816291	168812.423251	36.396685
1531.324041	169047.437573	36.401703
1532.333650	169294.049822	36.406720
1534.377684	169525.062424	36.411738
1535.871961	169763.787108	36.416756
1537.159306	170011.945390	36.421773
1538.856257	170250.881893	36.426791
1540.134165	170494.731990	36.431808
1541.664616	170739.088945	36.436826
1542.985045	170995.683639	36.441844
1544.423317	171257.233801	36.446861
1546.037433	171508.013548	36.451879
1546.909652	171782.621236	36.456896
1548.500279	172045.408270	36.461914
1550.536193	172318.376044	36.466932
1551.543108	172587.995295	36.471949
1553.732772	172848.282285	36.476967
1555.271204	173118.759433	36.481984
1556.770901	173385.134421	36.487002
1558.599143	173645.154191	36.492020
1560.013696	173933.606823	36.497037
1561.517756	174197.817237	36.502055
1563.019721	174475.185076	36.507072
1564.855166	174744.344706	36.512090
1566.622665	175006.387300	36.517108
1568.062987	175292.650824	36.522125
1570.016787	175551.191304	36.527143
1571.785874	175809.077694	36.532160
1573.339557	176074.852849	36.537178
1575.327952	176337.097245	36.542196
1577.338212	176588.036044	36.547213
1579.459831	176832.057110	36.552231
1581.112758	177088.840845	36.557248
1582.299095	177319.717577	36.562266
1584.441143	177573.978059	36.567284
1585.791772	177817.911690	36.572301
1587.438896	178064.958737	36.577319
1589.187739	178310.354439	36.582336
1590.298717	178564.074211	36.587354
1591.973532	178806.591873	36.592372
1593.054718	179068.781842	36.597389
1594.387262	179312.891938	36.602407
1596.063040	179588.261764	36.607424
1597.486439	179839.744601	36.612442
1599.035795	180105.749009	36.617460
1600.109821	180385.736362	36.622477
1601.612592	180643.352191	36.627495
1603.417319	180929.469454	36.632512
1604.628327	181207.943210	36.637530
1606.192134	181476.466006	36.642548
1607.632857	181778.430674	36.647565
1609.322038	182043.117906	36.652583
1610.844175	182324.467684	36.657600
1612.451547	182584.984029	36.662618
1614.631687	182838.356150	36.667636
1616.175225	183106.676451	36.672653
1617.667881	183350.060589	36.677671
1619.356914	183613.945209	36.682688
1620.791344	183872.174561	36.687706
1622.547204	184138.183387	36.692724
1623.994668	184397.263856	36.697741
1626.240875	184669.720077	36.702759
1627.595676	184919.897899	36.707776
1629.016351	185187.298516	36.712794
1631.177486	185437.554175	36.717812
1632.641703	185723.693031	36.722829
1634.110807	185993.742768	36.727847
1635.678719	186272.204208	36.732864
1637.370141	186555.266716	36.737882
1639.066414	186824.790378	36.742900
1640.425541	187099.140477	36.747917
1642.084337	187370.741694	36.752935
1643.830566	187652.444414	36.757952
1645.411703	187946.547721	36.762970
1646.837571	188220.107056	36.767988
1648.546866	188517.416855	36.773005
1649.873382	188805.868141	36.778023
1651.768403	189085.157402	36.783040
1653.280779	189387.123188	36.788058
1655.088930	189671.746934	36.793076
1656.521210	189980.594698	36.798093
1658.553024	190262.572212	36.803111
1660.030498	190552.190323	36.808128
1661.865173	190837.248258	36.813146
1663.984834	191126.336355	36.818164
1665.719108	191422.289661	36.823181
1667.498291	191695.064027	36.828199
1669.607917	191996.392926	36.833216
1671.051351	192276.787678	36.838234
1672.811795	192566.867790	36.843252
1674.308885	192848.209108	36.848269
1676.129952	193134.297883	36.853287
1678.168195	193407.040592	36.858304
1679.917835	193693.727726	36.863322
1681.803495	193962.398367	36.868340
1683.422104	194254.059192	36.873357
1685.271463	194519.286467	36.878375
1686.983821	194795.997491	36.883392
1688.604116	195077.115993	36.888410
1690.867548	195343.982530	36.893428
1692.343075	195614.757754	36.898445
1694.331203	195876.048268	36.903463
1697.142134	196104.362498	36.908480
1699.401384	196354.138804	36.913498
1701.402580	196583.345251	36.918516
1703.091897	196819.963704	36.923533
1704.559894	197060.654512	36.928551
1705.900467	197265.891651	36.933568
1707.720504	197483.898134	36.938586
1709.502216	197687.772263	36.943604
1710.816529	197906.723881	36.948621
1712.400157	198121.203960	36.953639
1713.786763	198345.260999	36.958656
1715.029578	198574.837718	36.963674
1716.507073	198808.833295	36.968692
1717.683561	199046.152414	36.973709
1719.072894	199296.690063	36.978727
1720.878807	199548.228938	36.983744
1721.982635	199799.169653	36.988762
1723.678932	200059.283333	36.993780
1725.058162	200342.676851	36.998797
1726.591970	200614.242716	37.003815
1728.421990	200884.861684	37.008832
1729.501071	201182.130056	37.013850
1731.418158	201457.307580	37.018868
1732.980637	201751.582810	37.023885
1734.582368	202049.953343	37.028903
1736.341732	202347.462673	37.033920
1738.295275	202640.449234	37.038938
1740.109977	202941.405575	37.043956
1741.523520	203247.860111	37.048973
1743.613161	203550.299283	37.053991
1745.427113	203844.418595	37.059008
1747.204689	204156.316650	37.064026
1749.376252	204448.160853	37.069044
1751.390010	204748.041518	37.074061
1752.866986	205038.336052	37.079079
1755.120496	205330.768315	37.084096
1757.179115	205633.223335	37.089114
1759.039344	205922.953652	37.094132
1760.663530	206212.138925	37.099149
1762.454790	206508.014431	37.104167
1764.204900	206802.108021	37.109184
1765.444351	207107.379152	37.114202
1767.440027	207400.801973	37.119220
1769.047928	207706.741248	37.124237
1770.968986	208004.279225	37.129255
1772.495684	208299.367695	37.134272
1774.389292	208619.890606	37.139290
1776.020868	208931.227582	37.144308
1777.618459	209244.869317	37.149325
1779.277900	209552.688490	37.154343
1781.474752	209864.422835	37.159360
1783.252855	210175.730096	37.164378
1784.836504	210486.968207	37.169396
1786.978502	210794.729574	37.174413
1788.657812	211106.920391	37.179431
1790.371758	211415.273221	37.184448
1792.418757	211733.769139	37.189466
1794.492845	212031.213123	37.194484
1796.592495	212334.227788	37.199501
1798.066812	212633.788345	37.204519
1800.364204	212912.119348	37.209536
1802.196242	213186.386582	37.214554
1803.987794	213454.732440	37.219572
1806.223416	213715.886516	37.224589
1807.755700	213991.372690	37.229607
1809.609997	214260.130808	37.234624
1811.365973	214540.789085	37.239642
1812.977474	214807.289950	37.244660
1814.641927	215083.343641	37.249677
1816.384942	215368.171737	37.254695
1818.503732	215640.270539	37.259712
1819.946005	215923.358514	37.264730
1821.644771	216208.654189	37.269748
1823.706052	216501.333579	37.274765
1825.007171	216794.566537	37.279783
1827.100132	217081.720384	37.284800
1828.660544	217380.450304	37.289818
1830.271915	217674.932734	37.294836
1832.229653	217978.858502	37.299853
1833.943606	218278.189961	37.304871
1836.252447	218581.338847	37.309888
1837.518551	218892.932832	37.314906
1839.694777	219194.518235	37.319924
1841.444893	219492.211080	37.324941
1843.070869	219798.495288	37.329959
1845.595900	220096.651647	37.334976
1847.549363	220406.187619	37.339994
1849.308791	220707.400965	37.345012
1851.719154	221013.032401	37.350029
1853.171768	221320.353450	37.355047
1855.386727	221616.673183	37.360064
1856.882100	221960.278849	37.365082
1858.716273	222294.347332	37.370100
1860.592481	222601.555502	37.375117
1862.518453	222912.591630	37.380135
1864.351812	223216.228332	37.385152
1866.315801	223528.365554	37.390170
1868.426606	223833.217660	37.395188
1870.497969	224132.414026	37.400205
1872.190125	224441.918763	37.405223
1874.113993	224745.204096	37.410240
1876.021331	225057.991163	37.415258
1877.892128	225360.093617	37.420276
1880.150450	225664.357819	37.425293
1881.733875	225973.568178	37.430311
1883.847979	226268.841932	37.435328
1885.608329	226576.337613	37.440346
1887.407170	226883.548951	37.445364
1889.731684	227181.332140	37.450381
1891.513387	227486.542072	37.455399
1893.723703	227774.745619	37.460416
1895.700627	228079.240970	37.465434
1897.415653	228368.363183	37.470452
1899.791216	228660.810089	37.475469
1901.428747	228950.810011	37.480487
1903.648174	229214.254974	37.485504
1904.919161	229493.394174	37.490522
1906.890970	229764.753121	37.495540
1908.477923	230036.732696	37.500557
1910.534302	230322.251496	37.505575
1912.572420	230584.967330	37.510592
1914.133100	230869.423624	37.515610
1915.511646	231157.922493	37.520628
1917.583512	231428.889542	37.525645
1919.345900	231723.450051	37.530663
1921.269571	232008.842728	37.535680
1923.089946	232311.065964	37.540698
1924.593955	232608.616363	37.545716
1926.819286	232911.158201	37.550733
1928.730554	233222.386138	37.555751
1930.666174	233519.845452	37.560768
1932.679380	233833.294186	37.565786
1934.486031	234143.474921	37.570804
1936.505547	234443.717507	37.575821
1938.089220	234759.319972	37.580839
1940.322031	235077.106279	37.585856
1942.037874	235392.791333	37.590874
1943.940193	235722.315410	37.595892
1946.028134	236033.295433	37.600909
1947.763965	236371.229551	37.605927
1949.595008	236688.474977	37.610944
1951.890905	237026.423914	37.615962
1953.513736	237355.387868	37.620980
1955.904183	237677.474867	37.625997
1957.667368	238012.869908	37.631015
1959.771313	238343.640040	37.636032
1961.929671	238661.906062	37.641050
1964.198102	238994.404578	37.646068
1966.497033	239311.329366	37.651085
1968.156545	239645.551969	37.656103
1970.418581	239957.963284	37.661120
1972.699617	240280.964086	37.666138
1974.553779	240600.579143	37.671156
1976.744888	240928.904535	37.676173
1978.148032	241253.647468	37.681191
1980.284720	241589.019065	37.686208
1982.326678	241910.716008	37.691226
1984.132744	242244.770257	37.696244
1986.551106	242557.925539	37.701261
1988.315235	242891.962772	37.706279
1990.273870	243213.422289	37.711296
1992.126331	243539.776324	37.716314
1993.901765	243878.030789	37.721332
1996.227541	244211.931536	37.726349
1997.914319	244541.057605	37.731367
2000.190466	244875.374301	37.736384
2002.122089	245206.850810	37.741402
2003.868893	245541.278527	37.746420
2006.147651	245877.426113	37.751437
2007.904049	246208.018395	37.756455
2010.143238	246523.091111	37.761472
2012.266430	246829.216390	37.766490
2013.820440	247143.256126	37.771508
2016.132097	247447.320729	37.776525
2017.780455	247753.320067	37.781543
2019.731803	248077.814811	37.786560
2021.885897	248388.561432	37.791578
2023.824768	248714.583587	37.796596
2025.677160	249013.745554	37.801613
2028.161365	249342.629065	37.806631
2030.369238	249659.516823	37.811648
2032.625917	249971.190164	37.816666
2034.592114	250289.158958	37.821684
2036.807671	250593.956200	37.826701
2038.861125	250908.432326	37.831719
2041.086324	251218.715922	37.836736
2043.105455	251535.357795	37.841754
2044.900191	251858.640299	37.846772
2046.939757	252168.142186	37.851789
2048.746626	252509.967265	37.856807
2050.593894	252828.086618	37.861824
2053.037502	253156.806137	37.866842
2054.925545	253498.162944	37.871860
2057.063034	253818.778149	37.876877
2059.253283	254146.929933	37.881895
2060.966922	254478.561756	37.886912
2063.694806	254822.099267	37.891930
2064.987180	255173.282514	37.896948
2067.680393	255508.291549	37.901965
2069.451167	255853.455941	37.906983
2071.092271	256195.923414	37.912000
2073.446234	256536.195360	37.917018
2075.600127	256888.032255	37.922036
2077.483472	257230.183484	37.927053
2079.508894	257568.197488	37.932071
2081.615168	257911.787709	37.937088
2083.590650	258259.997032	37.942106
2085.532023	258618.093869	37.947124
2088.473744	258961.984904	37.952141
2090.514454	259315.215081	37.957159
2092.211300	259662.987898	37.962176
2094.514447	260006.549764	37.967194
2096.689736	260366.517119	37.972212
2098.856262	260715.461523	37.977229
2101.053638	261063.944212	37.982247
2103.286631	261416.613138	37.987264
2105.411726	261755.429626	37.992282
2107.365091	262114.011779	37.997300
2109.414923	262460.157007	38.002317
2112.025873	262805.095879	38.007335
2113.659475	263157.963434	38.012352
2116.164520	263506.704865	38.017370
2118.126284	263855.329583	38.022388
2120.812295	264182.399591	38.027405
2122.855880	264517.116488	38.032423
2125.015537	264842.822570	38.037440
2127.359893	265146.754559	38.042458
2129.449229	265455.426799	38.047476
2131.758034	265749.000388	38.052493
2133.883919	266057.387829	38.057511
2136.242460	266353.824489	38.062528
2138.039875	266660.181367	38.067546
2139.729780	266983.270806	38.072564
2141.913638	267293.377271	38.077581
2143.583799	267612.100879	38.082599
2145.867823	267933.623290	38.087616
2147.820854	268250.600383	38.092634
2149.662526	268590.763102	38.097652
2152.170270	268915.908635	38.102669
2154.457216	269250.742603	38.107687
2156.311395	269583.359064	38.112704
2158.468978	269920.601771	38.117722
2160.532777	270265.023238	38.122740
2162.501732	270605.725592	38.127757
2164.627339	270950.340752	38.132775
2166.287865	271296.020518	38.137792
2169.295734	271636.329841	38.142810
2171.414904	271990.879076	38.147828
2173.690195	272337.045931	38.152845
2176.563825	272667.901345	38.157863
2178.591695	273023.481440	38.162880
2181.320570	273354.461549	38.167898
2183.741795	273699.792612	38.172916
2185.727334	274030.941490	38.177933
2188.189902	274379.390686	38.182951
2189.914295	274723.181118	38.187968
2192.302304	275049.719020	38.192986
2194.187902	275413.120739	38.198004
2196.509901	275747.290125	38.203021
2198.869987	276084.451056	38.208039
2200.910649	276436.218764	38.213056
2203.208652	276785.684721	38.218074
2205.291680	277138.385544	38.223092
2207.592531	277477.410140	38.228109
2210.092722	277824.532145	38.233127
2212.115741	278180.189060	38.238144
2214.521625	278530.933124	38.243162
2216.355126	278876.280715	38.248180
2218.298590	279230.730565	38.253197
2221.129083	279569.111736	38.258215
2223.352905	279917.140633	38.263232
2225.638161	280269.681438	38.268250
2227.934047	280619.934100	38.273268
2229.887399	280962.188060	38.278285
2231.971290	281314.277630	38.283303
2234.081555	281675.228572	38.288320
2236.308403	282020.283779	38.293338
2238.347383	282390.568592	38.298356
2240.532303	282751.125986	38.303373
2243.149640	283104.349255	38.308391
2244.947596	283442.942937	38.313408
2247.111597	283774.721102	38.318426
2249.053445	284111.741903	38.323444
2250.919823	284453.728029	38.328461
2253.301584	284797.156359	38.333479
2255.298377	285152.381676	38.338496
2257.670109	285496.750928	38.343514
2259.442961	285864.331604	38.348532
2261.328028	286219.522857	38.353549
2263.937003	286581.711834	38.358567
2265.926693	286956.725514	38.363584
2268.218165	287326.076888	38.368602
2270.369561	287708.227726	38.373620
2272.434626	288088.029331	38.378637
2274.933520	288467.888710	38.383655
2277.099712	288862.203760	38.388672
2279.453742	289240.916597	38.393690
2281.527158	289632.069967	38.398708
2283.993335	290026.132642	38.403725
2286.557097	290416.902331	38.408743
2288.608428	290821.063667	38.413760
2291.384990	291202.932929	38.418778
2293.553509	291611.062646	38.423796
2295.851566	292007.511397	38.428813
2298.480079	292394.381179	38.433831
2300.655746	292799.383246	38.438848
2303.018296	293193.406544	38.443866
2305.534307	293588.319309	38.448884
2307.917843	293989.475930	38.453901
2310.504690	294385.442918	38.458919
2312.459039	294792.660996	38.463936
2315.369239	295188.702214	38.468954
2317.730966	295580.028608	38.473972
2320.505849	295969.815419	38.478989
2323.134590	296355.890525	38.484007
2325.075775	296743.953589	38.489024
2327.550434	297139.018415	38.494042
2329.767961	297527.696492	38.499060
2331.707065	297920.329746	38.504077
2334.351160	298310.411819	38.509095
2336.309062	298712.845401	38.514112
2339.046666	299104.688988	38.519130
2341.497690	299508.465022	38.524148
2343.831717	299901.234380	38.529165
2346.304206	300297.664058	38.534183
2348.645239	300701.861017	38.539200
2351.087488	301086.685116	38.544218
2353.869751	301485.831475	38.549236
2356.042812	301874.404875	38.554253
2358.289507	302257.859988	38.559271
2360.440350	302666.450943	38.564288
2362.551550	303050.052498	38.569306
2365.204333	303452.389270	38.574324
2367.420422	303840.544267	38.579341
2370.171734	304220.180315	38.584359
2372.236522	304600.508364	38.589376
2374.666429	304959.059960	38.594394
2376.727144	305318.761355	38.599412
2378.663589	305695.931624	38.604429
2381.736073	306060.017354	38.609447
2383.672230	306430.860871	38.614464
2386.195982	306807.807866	38.619482
2388.410476	307173.296481	38.624500
2390.682766	307560.822192	38.629517
2393.000718	307926.800232	38.634535
2395.150779	308324.375962	38.639552
2397.915867	308692.211263	38.644570
2400.629011	309076.868355	38.649588
2402.883152	309469.699471	38.654605
2406.061651	309838.075332	38.659623
2408.347406	310221.348670	38.664640
2410.810033	310601.519373	38.669658
2413.271351	310976.863141	38.674676
2415.398758	311350.455236	38.679693
2418.396464	311722.765199	38.684711
2420.651940	312114.698083	38.689728
2423.402412	312489.254375	38.694746
2425.518836	312874.120244	38.699764
2427.748025	313264.757811	38.704781
2430.537203	313649.158702	38.709799
2432.641470	314043.242038	38.714816
2435.141307	314434.772141	38.719834
2437.689099	314818.216447	38.724852
2439.976331	315214.552197	38.729869
2442.598974	315612.484137	38.734887
2444.913603	316010.031545	38.739904
2447.386356	316409.787340	38.744922
2449.737054	316798.538132	38.749940
2452.148993	317212.929532	38.754957
2454.618174	317616.439842	38.759975
2457.072770	318023.963595	38.764992
2459.355743	318433.569997	38.770010
2461.671800	318831.943703	38.775028
2464.042693	319246.256541	38.780045
2466.592628	319665.567796	38.785063
2468.927332	320093.520851	38.790080
2471.289338	320506.483341	38.795098
2474.124280	320926.378523	38.800116
2476.161529	321351.756835	38.805133
2478.429379	321783.572690	38.810151
2480.895408	322220.231130	38.815168
2483.532284	322641.774859	38.820186
2485.761674	323079.456896	38.825204
2488.263076	323524.763198	38.830221
2490.719791	323947.649589	38.835239
2493.116422	324402.135773	38.840256
2495.581834	324837.053877	38.845274
2498.192289	325283.450879	38.850292
2500.744518	325721.677328	38.855309
2503.849891	326143.840116	38.860327
2506.138766	326550.232679	38.865344
2508.527109	326948.201643	38.870362
2511.133161	327353.447828	38.875380
2513.512081	327756.442365	38.880397
2516.468417	328149.896515	38.885415
2518.900446	328547.139319	38.890432
2521.356391	328947.068066	38.895450
2524.634714	329337.290778	38.900468
2526.615102	329745.492974	38.905485
2529.240813	330135.941891	38.910503
2531.781275	330542.222609	38.915520
2533.652316	330943.960097	38.920538
2536.739456	331347.991269	38.925556
2538.927487	331768.998459	38.930573
2541.587574	332189.852216	38.935591
2544.330258	332605.967289	38.940608
2546.650668	333027.149230	38.945626
2549.186635	333439.533985	38.950644
2551.575624	333869.130408	38.955661
2554.571191	334287.861660	38.960679
2557.062904	334711.139237	38.965696
2559.570168	335139.134673	38.970714
2561.815112	335561.658902	38.975732
2564.265739	336002.912472	38.980749
2566.725849	336442.409603	38.985767
2569.192433	336879.693739	38.990784
2571.675001	337331.699420	38.995802
2574.545254	337774.931395	39.000820
2577.143323	338230.746613	39.005837
2579.914196	338679.320249	39.010855
2582.397319	339127.682423	39.015872
2585.108149	339582.784614	39.020890
2587.676153	340031.837880	39.025908
2590.095998	340496.704030	39.030925
2593.111505	340944.308788	39.035943
2596.061275	341390.067273	39.040960
2598.463915	341848.654733	39.045978
2601.443316	342279.803074	39.050996
2604.457872	342734.910140	39.056013
2607.130566	343172.041759	39.061031
2609.939523	343617.856950	39.066048
2611.887005	344060.504742	39.071066
2614.439572	344501.200018	39.076084
2617.002632	344957.427901	39.081101
2619.533120	345413.555822	39.086119
2622.111120	345870.510422	39.091136
2624.682016	346330.788295	39.096154
2627.298719	346786.333153	39.101172
2630.219703	347246.218145	39.106189
2632.763405	347702.808069	39.111207
2635.614606	348147.591496	39.116224
2638.057044	348602.260722	39.121242
2641.217725	349054.933863	39.126260
2643.635135	349515.082993	39.131277
2646.232198	349950.829299	39.136295
2648.781226	350372.262164	39.141312
2651.020798	350801.051798	39.146330
2654.272360	351205.587035	39.151348
2656.880129	351636.114038	39.156365
2659.674532	352043.609235	39.161383
2662.080513	352465.809816	39.166400
2664.405318	352887.512177	39.171418
2667.532731	353298.143372	39.176436
2670.073940	353727.699203	39.181453
2672.356575	354157.698568	39.186471
2675.197601	354575.370955	39.191488
2677.720676	355015.706997	39.196506
2680.515578	355438.837082	39.201524
2683.318701	355878.461330	39.206541
2685.945817	356318.871103	39.211559
2688.443851	356754.195543	39.216576
2691.113613	357204.185396	39.221594
2693.680944	357641.953182	39.226612
2695.949498	358114.664562	39.231629
2698.859703	358571.380834	39.236647
2701.788124	359016.287568	39.241664
2705.263083	359458.260972	39.246682
2708.291355	359907.077791	39.251700
2710.729743	360360.679269	39.256717
2713.581408	360806.850642	39.261735
2716.103368	361263.247525	39.266752
2719.012484	361718.563488	39.271770
2721.563573	362168.018249	39.276788
2724.205561	362631.057723	39.281805
2726.868581	363096.830217	39.286823
2729.403442	363559.826624	39.291840
2731.585386	364035.512880	39.296858
2734.227350	364503.939234	39.301876
2737.391379	364985.982341	39.306893
2739.945712	365458.092569	39.311911
2743.343048	365938.312109	39.316928
2745.621317	366417.181060	39.321946
2748.207154	366905.208066	39.326964
2751.122266	367395.892883	39.331981
2753.511987	367891.273969	39.336999
2757.003266	368365.920241	39.342016
2759.200567	368855.509705	39.347034
2762.422061	369337.445636	39.352052
2765.421906	369832.073629	39.357069
2768.005157	370317.753712	39.362087
2770.743663	370808.072667	39.367104
2773.155791	371301.482593	39.372122
2776.337076	371792.785785	39.377140
2779.258186	372275.395789	39.382157
2781.922334	372768.900850	39.387175
2785.384905	373245.552592	39.392192
2787.694923	373744.075326	39.397210
2790.443558	374229.760082	39.402228
2793.704161	374713.937172	39.407245
2796.241500	375187.845814	39.412263
2798.565428	375648.031153	39.417280
2800.971825	376113.297895	39.422298
2804.066675	376558.330807	39.427316
2806.369953	377024.288353	39.432333
2808.759272	377497.457494	39.437351
2811.218038	377963.430174	39.442368
2813.664834	378457.661572	39.447386
2816.428654	378932.530156	39.452404
2819.387848	379434.862575	39.457421
2822.448350	379925.096764	39.462439
2825.138960	380435.830596	39.467456
2827.699465	380938.434985	39.472474
2830.340905	381426.509398	39.477492
2832.964389	381962.601725	39.482509
2835.724414	382478.421651	39.487527
2838.516910	382999.150632	39.492544
2841.080845	383532.160749	39.497562
2844.239307	384054.415284	39.502580
2847.541057	384593.330682	39.507597
2850.472071	385128.821853	39.512615
2853.323422	385651.964971	39.517632
2856.318446	386188.039390	39.522650
2859.162039	386718.118527	39.527668
2862.473935	387256.714280	39.532685
2864.990433	387793.906112	39.537703
2868.368041	388329.913732	39.542720
2871.388190	388868.683781	39.547738
2874.201786	389405.170400	39.552756
2877.254623	389939.861056	39.557773
2879.843328	390488.109641	39.562791
2883.314321	391010.772430	39.567808
2885.911564	391547.539726	39.572826
2888.984301	392093.987388	39.577844
2892.246853	392627.513353	39.582861
2895.134052	393176.357192	39.587879
2897.907111	393708.498404	39.592896
2901.025068	394242.808365	39.597914
2903.988736	394781.039626	39.602932
2906.935562	395332.958530	39.607949
2909.901872	395868.661616	39.612967
2912.704256	396402.125298	39.617984
2915.451005	396951.488210	39.623002
2918.574949	397483.058028	39.628020
2921.694038	398022.734122	39.633037
2924.268767	398589.212660	39.638055
2927.340545	399125.379086	39.643072
2930.068370	399669.983691	39.648090
2932.697183	400223.925368	39.653108
2936.014069	400773.666670	39.658125
2939.018534	401335.592507	39.663143
2941.714333	401893.298032	39.668160
2944.481058	402447.965633	39.673178
2947.627152	402999.267734	39.678196
2950.320073	403551.570008	39.683213
2952.911797	404109.582745	39.688231
2956.180534	404631.277093	39.693248
2958.841982	405159.269785	39.698266
2961.723402	405680.931876	39.703284
2964.711069	406211.440837	39.708301
2967.443279	406729.940181	39.713319
2970.627645	407267.523063	39.718336
2973.011274	407807.682064	39.723354
2975.906361	408346.863407	39.728372
2978.414771	408889.239505	39.733389
2981.143026	409445.005104	39.738407
2984.127215	410010.427754	39.743424
2986.847976	410585.918554	39.748442
2989.425912	411164.766536	39.753460
2992.575842	411738.418384	39.758477
2995.323685	412332.271821	39.763495
2998.443795	412923.672072	39.768512
3001.481068	413525.008273	39.773530
3004.510136	414120.656574	39.778548
3008.006176	414703.724906	39.783565
3010.842843	415303.763738	39.788583
3014.223543	415915.969371	39.793600
3016.982242	416521.798455	39.798618
3020.216477	417125.385557	39.803636
3023.441769	417726.300623	39.808653
3026.596518	418334.233183	39.813671
3030.242942	418923.096057	39.818688
3033.359508	419527.512222	39.823706
3036.815538	420124.640387	39.828724
3040.628857	420707.637073	39.833741
3042.740951	421310.374705	39.838759
3046.127001	421897.569266	39.843776
3049.061487	422497.946670	39.848794
3052.299209	423098.795033	39.853812
3055.410093	423706.389278	39.858829
3058.338351	424318.432336	39.863847
3061.475353	424914.367201	39.868864
3064.460893	425519.736731	39.873882
3067.613945	426112.982662	39.878900
3070.973553	426712.971706	39.883917
3073.951964	427325.723836	39.888935
3077.056184	427931.045439	39.893952
3080.406912	428534.186508	39.898970
3083.177667	429132.871601	39.903988
3086.228103	429740.135959	39.909005
3089.031470	430363.230154	39.914023
3092.349136	430959.076888	39.919040
3095.149806	431582.699555	39.924058
3098.238629	432210.288522	39.929076
3101.280917	432831.107590	39.934093
3104.015242	433449.858386	39.939111
3106.586434	434081.788814	39.944128
3110.092536	434723.229417	39.949146
3112.831889	435369.282657	39.954164
3115.862305	435998.585712	39.959181
3118.683134	436635.933278	39.964199
3122.006924	437240.723055	39.969216
3124.627992	437851.179932	39.974234
3127.628403	438467.866548	39.979252
3130.520827	439087.162820	39.984269
3133.377138	439702.119745	39.989287
3136.283388	440333.408993	39.994304
3139.404565	440959.533827	39.999322
3142.273292	441604.467707	40.004340
3145.337809	442244.290261	40.009357
3148.504160	442898.003379	40.014375
3151.821914	443547.168784	40.019392
3154.708711	444209.244441	40.024410
3157.664823	444883.491926	40.029428
3160.978761	445541.969823	40.034445
3163.697704	446215.710822	40.039463
3166.683961	446901.286677	40.044480
3170.200426	447590.099712	40.049498
3173.013621	448284.420071	40.054516
3176.415868	448982.878553	40.059533
3179.511884	449683.338559	40.064551
3182.724443	450384.265112	40.069568
3185.680470	451092.448696	40.074586
3188.951451	451817.819329	40.079604
3192.480006	452532.751116	40.084621
3195.744556	453246.740672	40.089639
3198.724564	453970.722395	40.094656
3202.139872	454688.286397	40.099674
3205.706778	455421.895602	40.104692
3209.393750	456145.037755	40.109709
3212.657484	456850.260204	40.114727
3216.177451	457569.182711	40.119744
3219.625002	458282.730020	40.124762
3222.971976	458998.293997	40.129780
3226.650434	459704.270560	40.134797
3229.881107	460427.547211	40.139815
3233.178667	461126.455123	40.144832
3236.603986	461838.524123	40.149850
3240.273613	462547.799331	40.154868
3243.880100	463244.566479	40.159885
3247.123479	463952.446387	40.164903
3250.408898	464650.938456	40.169920
3253.515203	465345.035423	40.174938
3256.586991	466060.054956	40.179956
3260.130621	466748.220202	40.184973
3263.492163	467458.543998	40.189991
3266.440496	468153.736866	40.195008
3269.952244	468854.734515	40.200026
3273.043306	469567.659236	40.205044
3276.326794	470260.705998	40.210061
3279.632380	470961.361715	40.215079
3282.906946	471670.089017	40.220096
3286.485155	472367.518671	40.225114
3289.518446	473074.111904	40.230132
3292.332958	473778.338908	40.235149
3295.527397	474477.931151	40.240167
3298.239188	475152.752093	40.245184
3301.248144	475839.333398	40.250202
3304.097549	476514.440838	40.255220
3307.148870	477198.188511	40.260237
3310.492422	477890.510614	40.265255
3313.706883	478588.237699	40.270272
3316.887047	479278.818595	40.275290
3319.488174	479999.793718	40.280308
3322.999907	480704.424758	40.285325
3326.257787	481424.485624	40.290343
3329.431186	482155.449767	40.295360
3332.536756	482885.942365	40.300378
3336.097152	483624.572800	40.305396
3339.175642	484365.474676	40.310413
3342.243800	485115.849588	40.315431
3345.542399	485884.703004	40.320448
3348.896222	486638.105947	40.325466
3352.023912	487405.207209	40.330484
3355.270201	488186.910459	40.335501
3358.805172	488960.048206	40.340519
3362.047455	489749.366593	40.345536
3365.098953	490539.136604	40.350554
3368.396175	491342.574423	40.355572
3372.014796	492147.189591	40.360589
3375.485858	492949.823295	40.365607
3378.791662	493757.095027	40.370624
3382.529135	494564.970213	40.375642
3385.778873	495380.563490	40.380660
3389.450069	496186.407974	40.385677
3393.131266	497005.647994	40.390695
3396.310529	497815.588437	40.395712
3400.196911	498621.290730	40.400730
3403.611782	499445.360233	40.405748
3407.155285	500249.377483	40.410765
3411.316184	501072.951191	40.415783
3414.765509	501883.775984	40.420800
3418.457244	502676.250491	40.425818
3422.026109	503496.120003	40.430836
3425.299348	504293.535133	40.435853
3429.267150	505088.936611	40.440871
3432.707536	505900.536927	40.445888
3436.271004	506685.077672	40.450906
3439.908399	507478.251999	40.455924
3443.561702	508263.262250	40.460941
3447.003508	509063.560988	40.465959
3450.249259	509854.467434	40.470976
3453.971726	510639.257243	40.475994
3457.168531	511445.942211	40.481012
3460.413702	512233.105516	40.486029
3463.762541	513042.516060	40.491047
3466.830852	513839.874467	40.496064
3470.358138	514639.140467	40.501082
3473.676039	515459.891315	40.506100
3476.581127	516262.658872	40.511117
3479.769014	517076.199147	40.516122
3483.265941	517842.873058	40.521127
3486.499318	518550.037882	40.526132
3489.633185	519213.248723	40.531136
3492.592336	519806.938660	40.536141
3495.510715	520345.149617	40.541146
3498.067171	520828.241126	40.546151
3500.295882	521253.432013	40.551156
3502.417882	521635.049688	40.556160
3504.825595	521950.487775	40.561165
3506.484612	522224.128932	40.566170
3508.153647	522452.569402	40.571175
3510.123857	522620.498180	40.576180
3511.542297	522757.928343	40.581184
3512.604102	522858.662497	40.586189
3514.100314	522914.993550	40.591194
3514.761989	522945.270563	40.596199
3515.575634	522932.908485	40.601204
3516.835041	522920.324294	40.606208
3517.612252	522854.029133	40.611213
3518.082294	522766.853647	40.616218
3518.485569	522680.547638	40.621223
3518.910643	522543.179374	40.626228
3519.471931	522413.624187	40.631232
3519.742418	522259.898681	40.636237
3520.670526	522101.669570	40.641242
3520.674403	521912.746552	40.646247
3520.665676	521715.077237	40.651252
3520.909806	521515.545542	40.656256
3520.952651	521309.976410	40.661261
3520.977712	521083.577849	40.666266
3521.253339	520862.900177	40.671271
3521.335703	520629.408130	40.676276
3521.065707	520386.867715	40.681280
3520.955697	520148.393809	40.686285
3521.138830	519914.723967	40.691290
3520.814138	519676.277124	40.696295
3520.719945	519410.992239	40.701300
3520.759657	519180.115557	40.706304
3520.521751	518919.648974	40.711309
3520.352183	518674.286372	40.716314
3520.077287	518424.942082	40.721319
3520.385224	518173.024162	40.726324
3520.264660	517929.665407	40.731328
3519.748057	517680.803194	40.736333
3519.673738	517428.125262	40.741338
3519.571228	517186.522637	40.746343
3519.487501	516935.760330	40.751348
3518.951679	516703.372355	40.756352
3519.151343	516446.236517	40.761357
3519.295934	516199.776193	40.766362
3518.714992	515972.796396	40.771367
3518.824613	515714.146305	40.776372
3518.273908	515470.465511	40.781376
3518.298519	515248.235323	40.786381
3518.009406	515006.529438	40.791386
3517.367385	514774.030228	40.796391
3517.386899	514549.717936	40.801396
3516.969299	514322.993404	40.806400
3516.988001	514103.075567	40.811405
3516.594796	513887.165146	40.816410
3516.458560	513683.704607	40.821415
3516.255685	513463.206470	40.826420
3515.926711	513253.752103	40.831424
3515.695308	513053.384457	40.836429
3515.981439	512851.263421	40.841434
3515.583183	512659.465914	40.846439
3515.295843	512451.158430	40.851444
3515.003485	512259.946664	40.856448
3514.798160	512069.427173	40.861453
3514.778787	511871.136588	40.866458
3514.553869	511697.966813	40.871463
3514.481861	511502.867162	40.876468
3514.238747	511336.070475	40.881472
3514.033240	511147.412396	40.886477
3513.941842	510971.887100	40.891482
3513.233828	510802.730436	40.896487
3513.319115	510632.839648	40.901492
3513.009516	510471.559219	40.906496
3513.121755	510310.817678	40.911501
3512.990659	510149.253046	40.916506
3512.313180	510005.024764	40.921511
3512.648460	509848.645044	40.926516
3512.483525	509695.327874	40.931520
3512.036682	509530.670612	40.936525
3512.164596	509395.214158	40.941530
3511.661086	509262.639053	40.946535
3511.731002	509109.077155	40.951540
3511.449460	508974.896346	40.956544
3511.260552	508847.783061	40.961549
3511.367692	508697.297861	40.966554
3511.021775	508578.403757	40.971559
3510.984522	508453.085015	40.976564
3510.808517	508331.733770	40.981568
3510.657235	508204.559197	40.986573
3510.817761	508088.971625	40.991578
3510.524996	507965.157022	40.996583
3510.570930	507837.493204	41.001588
3510.391106	507727.623905	41.006592
3510.119412	507615.542117	41.011597
3510.143932	507488.688675	41.016602
3510.186850	507383.943021	41.021607
3509.968380	507264.614940	41.026612
3510.219969	507148.348906	41.031616
3509.833274	507040.633115	41.036621
3509.633140	506923.576773	41.041626
3509.562335	506830.433143	41.046631
3509.657333	506719.856215	41.051636
3509.200626	506631.225358	41.056640
3508.811883	506525.986137	41.061645
3509.104995	506418.614455	41.066650
3509.023201	506328.202349	41.071655
3508.896839	506236.987185	41.076660
3508.789939	506152.346758	41.081664
3508.726019	506055.099105	41.086669
3508.468893	505968.406824	41.091674
3508.400174	505883.809662	41.096679
3508.746753	505784.319690	41.101684
3508.596423	505704.744284	41.106688
3508.304679	505624.634224	41.111693
3508.646867	505533.695553	41.116698
3508.310431	505460.878784	41.121703
3508.025167	505364.623745	41.126708
3508.324125	505288.568354	41.131712
3508.124684	505198.624429	41.136717
3507.826906	505127.976177	41.141722
3507.733268	505052.032412	41.146727
3508.089089	504979.660888	41.151732
3507.962150	504902.608414	41.156736
3507.763340	504824.048777	41.161741
3508.104387	504758.561102	41.166746
3507.890408	504676.410155	41.171751
3507.852199	504606.326052	41.176756
3507.550748	504532.386540	41.181760
3507.587326	504459.709077	41.186765
3507.324774	504395.479408	41.191770
3507.604255	504327.418880	41.196775
3507.576187	504253.991671	41.201780
3507.488934	504186.089773	41.206784
3506.902138	504119.329335	41.211789
3507.677053	504038.638570	41.216794
3507.408991	503989.084700	41.221799
3507.110760	503918.178602	41.226804
3507.271573	503854.031867	41.231808
3507.012640	503789.698192	41.236813
3506.985092	503730.034373	41.241818
3506.534987	503685.518732	41.246823
3507.028854	503614.030734	41.251828
3507.079101	503563.666214	41.256832
3506.405029	503503.243443	41.261837
3506.853953	503432.470351	41.266842
3506.871926	503377.859152	41.271847
3506.564094	503328.461538	41.276852
3506.460058	503273.970522	41.281856
3506.500557	503214.648477	41.286861
3506.737092	503160.406948	41.291866
3506.302893	503118.367292	41.296871
3506.556750	503061.288505	41.301876
3506.753137	503004.927175	41.306880
3506.213983	502956.779751	41.311885
3506.555807	502908.138678	41.316890
3506.079096	502866.611257	41.321895
3506.167922	502810.620589	41.326900
3506.257401	502774.520160	41.331904
3506.361044	502729.610914	41.336909
3506.399908	502666.440766	41.341914
3506.156375	502624.015512	41.346919
3506.386721	502575.036855	41.351924
3506.361699	502519.771837	41.356928
3506.169992	502472.529821	41.361933
3506.188845	502428.291178	41.366938
3505.955060	502382.169057	41.371943
3506.212334	502330.351134	41.376948
3506.002537	502297.232600	41.381952
3506.010273	502244.846506	41.386957
3505.973884	502205.221865	41.391962
3505.788635	502162.431997	41.396967
3505.880327	502114.435643	41.401972
3506.030251	502078.172400	41.406976
3505.792224	502046.070137	41.411981
3505.888460	501996.250638	41.416986
3505.806711	501966.198713	41.421991
3505.920003	501911.416080	41.426996
3505.767194	501878.945745	41.432000
3505.813217	501840.673857	41.437005
3506.315210	501779.958085	41.442010
3506.201665	501757.907972	41.447015
3506.199154	501706.179902	41.452020
3506.100709	501648.595482	41.457024
3505.846013	501611.382932	41.462029
3506.134007	501568.061298	41.467034
3505.783236	501528.687296	41.472039
3505.809966	501492.442328	41.477044
3505.769895	501446.692083	41.482048
3505.755031	501422.854406	41.487053
3505.873226	501365.386676	41.492058
3505.663357	501329.533083	41.497063
3505.572255	501285.815134	41.502068
3505.442642	501250.151161	41.507072
3505.647581	501226.379713	41.512077
3505.968833	501176.319889	41.517082
3505.499163	501145.011856	41.522087
3505.591483	501094.481818	41.527092
3505.407957	501064.900006	41.532096
3505.332641	501033.326982	41.537101
3506.138592	500997.008467	41.542106
3505.350923	500958.461510	41.547111
3505.655153	500909.517204	41.552116
3505.747916	500877.613636	41.557120
3505.404872	500855.952998	41.562125
3505.605085	500810.871788	41.567130
3505.506442	500782.693383	41.572135
3505.578283	500735.354476	41.577140
3505.495660	500706.312917	41.582144
3505.386419	500662.241980	41.587149
3505.768481	500639.302262	41.592154
3505.551097	500598.386579	41.597159
3505.477352	500560.637051	41.602164
3505.743689	500525.769560	41.607168
3505.469242	500499.187663	41.612173
3505.608001	500447.889179	41.617178
3505.494634	500417.029738	41.622183
3505.629066	500380.512395	41.627188
3505.672702	500343.958709	41.632192
3505.312029	500317.693883	41.637197
3505.218016	500264.153807	41.642202
3505.098718	500254.301946	41.647207
3505.109773	500208.591064	41.652212
3505.286991	500185.379425	41.657216
3505.123779	500166.777307	41.662221
3505.431992	500134.888981	41.667226
3505.302832	500100.437506	41.672231
3505.469669	500074.291428	41.677236
3505.690177	500037.051104	41.682240
3505.264961	500003.557390	41.687245
3505.677100	499960.667816	41.692250
3505.164337	499932.654762	41.697255
3505.112100	499908.820970	41.702260
3505.257214	499872.250282	41.707264
3505.271684	499844.457483	41.712269
3505.369893	499811.893089	41.717274
3504.985478	499782.695246	41.722279
3505.441347	499743.139191	41.727284
3505.376047	499717.586109	41.732288
3505.014750	499692.585980	41.737293
3505.334315	499644.445724	41.742298
3505.326836	499624.603528	41.747303
3505.274507	499588.569677	41.752308
3505.690746	499555.600206	41.757312
3505.293795	499519.772547	41.762317
3505.518897	499487.592479	41.767322
3504.965352	499474.872784	41.772327
3505.388732	499435.827402	41.777332
3505.131201	499407.975673	41.782336
3504.935393	499378.342389	41.787341
3505.147891	499348.492659	41.792346
3504.930209	499323.216207	41.797351
3505.137512	499291.747306	41.802356
3505.025867	499267.770186	41.807360
3504.870391	499240.610775	41.812365
3505.177343	499204.620613	41.817370
3504.672927	499181.363542	41.822375
3505.078590	499156.190824	41.827380
3505.468962	499125.401410	41.832384
3505.318088	499094.748109	41.837389
3505.151954	499069.817511	41.842394
3504.970137	499035.119199	41.847399
3505.082619	499007.815840	41.852404
3505.487047	498984.516117	41.857408
3505.151535	498954.296741	41.862413
3505.368987	498913.460351	41.867418
3504.906275	498881.742269	41.872423
3504.888299	498850.915679	41.877428
3504.775961	498830.836064	41.882432
3504.895299	498813.706580	41.887437
3504.937431	498792.083812	41.892442
3504.835642	498773.419917	41.897447
3504.868397	498738.484627	41.902452
3504.959597	498720.650774	41.907456
3504.805039	498704.121333	41.912461
3505.094744	498667.373471	41.917466
3504.688800	498648.656272	41.922471
3504.762771	498620.548434	41.927476
3504.908762	498594.352875	41.932480
3504.716170	498572.817565	41.937485
3504.804104	498558.983355	41.942490
3504.678748	498523.515775	41.947495
3504.723845	498505.942116	41.952500
3504.710836	498492.579426	41.957504
3504.507086	498479.095000	41.962509
3504.939385	498434.123011	41.967514
3504.561737	498424.412225	41.972519
3504.718066	498400.897839	41.977524
3504.766906	498380.184755	41.982528
3504.493551	498358.915077	41.987533
3504.759123	498348.292597	41.992538
3504.683770	498316.461671	41.997543
3504.575841	498302.354473	42.002548
3504.710180	498278.944653	42.007552
3504.610696	498261.849230	42.012557
3504.866851	498226.270142	42.017562
3504.730500	498218.849851	42.022567
3504.804574	498177.933208	42.027572
3504.769610	498155.764987	42.032576
3504.589740	498124.760243	42.037581
3505.286500	498114.676978	42.042586
3505.329416	498106.418305	42.047591
3505.127007	498063.064465	42.052596
3504.871633	498043.968461	42.057600
3504.760885	498010.725080	42.062605
3505.026728	497976.915862	42.067610
3504.832130	497969.808428	42.072615
3504.933171	497938.961469	42.077620
3505.008446	497915.206134	42.082624
3504.754769	497890.692746	42.087629
3505.124318	497858.233811	42.092634
3504.756453	497835.915310	42.097639
3504.604011	497811.436439	42.102644
3505.075402	497792.326556	42.107648
3504.618130	497764.706358	42.112653
3504.908759	497743.954330	42.117658
3505.024274	497716.800418	42.122663
3504.749299	497698.618420	42.127668
3504.997419	497666.988357	42.132672
3505.082205	497647.483787	42.137677
3504.999646	497610.438228	42.142682
3504.628826	497586.904847	42.147687
3504.801341	497567.335698	42.152692
3504.881929	497532.998037	42.157696
3504.840615	497529.308825	42.162701
3505.109784	497486.030949	42.167706
3504.806481	497461.423568	42.172711
3504.878257	497430.630995	42.177716
3505.272458	497417.760049	42.182720
3504.725150	497402.557168	42.187725
3504.794530	497370.651075	42.192730
3504.807697	497356.220235	42.197735
3505.049045	497318.717868	42.202740
3505.154380	497288.324769	42.207744
3504.583696	497272.163551	42.212749
3504.949359	497247.804542	42.217754
3504.800417	497226.564494	42.222759
3504.852925	497196.179590	42.227764
3504.620755	497180.521692	42.232768
3504.568572	497148.381282	42.237773
3504.727768	497122.738413	42.242778
3504.473138	497111.691149	42.247783
3504.669070	497100.927062	42.252788
3504.742343	497063.754500	42.257792
3504.913405	497048.285898	42.262797
3504.687098	497029.437369	42.267802
3504.693593	497014.045376	42.272807
3504.689844	496979.061829	42.277812
3504.793413	496966.844039	42.282816
3504.518802	496933.877721	42.287821
3504.828997	496921.120958	42.292826
3504.936619	496898.017349	42.297831
3504.862869	496877.676322	42.302836
3504.821436	496844.116072	42.307840
3504.435305	496838.405440	42.312845
3504.622504	496812.403306	42.317850
3504.667445	496786.524876	42.322855
3504.442268	496765.650740	42.327860
3504.603960	496742.234613	42.332864
3504.649029	496738.936618	42.337869
3504.419067	496713.607824	42.342874
3504.470795	496701.803082	42.347879
3504.595128	496681.531786	42.352884
3504.516912	496656.887738	42.357888
3504.253949	496641.386129	42.362893
3504.575648	496612.780358	42.367898
3504.537049	496607.824795	42.372903
3504.441459	496589.258925	42.377908
3504.476776	496577.962991	42.382912
3504.260918	496563.213313	42.387917
3504.617177	496536.019585	42.392922
3504.565062	496540.787017	42.397927
3504.804715	496499.840417	42.402932
3504.577064	496482.712942	42.407936
3504.389094	496463.351469	42.412941
3504.363061	496436.825572	42.417946
3504.373514	496427.457409	42.422951
3504.469156	496415.544281	42.427956
3504.574090	496388.288796	42.432960
3504.413680	496375.251621	42.437965
3504.658906	496358.758111	42.442970
3504.679852	496333.490390	42.447975
3504.736726	496318.950559	42.452980
3504.747176	496285.229188	42.457984
3504.545716	496272.704730	42.462989
3504.567957	496248.955597	42.467994
3504.481931	496230.134698	42.472999
3504.324427	496219.020908	42.478004
3504.495340	496194.286227	42.483008
3504.320065	496178.466581	42.488013
3504.452833	496158.699677	42.493018
3504.574241	496147.288607	42.498023
3504.578758	496128.250770	42.503028
3505.018211	496100.587568	42.508032
3504.613223	496088.652090	42.513037
3504.970585	496062.318207	42.518042
3504.889804	496040.610321	42.523047
3504.641826	496024.548877	42.528052
3504.577529	496012.660764	42.533056
3504.850068	495988.314791	42.538061
3504.677019	495955.836959	42.543066
3504.483301	495946.450187	42.548071
3504.184426	495934.750993	42.553076
3504.557776	495891.149070	42.558080
3504.181000	495892.778208	42.563085
3504.293548	495872.963558	42.568090
3504.142161	495855.114599	42.573095
3504.082020	495857.807587	42.578100
3504.233320	495845.075186	42.583104
3504.298791	495815.293507	42.588109
3504.567627	495803.200711	42.593114
3504.536695	495796.117187	42.598119
3504.550652	495768.470101	42.603124
3504.767524	495752.233684	42.608128
3504.123166	495734.462521	42.613133
3504.518877	495712.020721	42.618138
3504.655744	495704.708113	42.623143
3504.531869	495679.968695	42.628148
3504.808015	495656.482453	42.633152
3504.594222	495638.288721	42.638157
3504.315995	495620.611475	42.643162
3504.280448	495601.224995	42.648167
3504.481869	495582.459260	42.653172
3504.580360	495566.545182	42.658176
3504.205969	495550.958990	42.663181
3504.338286	495535.039538	42.668186
3504.406901	495526.117411	42.673191
3504.160589	495499.624967	42.678196
3504.358587	495503.441754	42.683200
3504.247181	495482.902592	42.688205
3504.616210	495454.388792	42.693210
3504.287904	495439.200282	42.698215
3504.010654	495421.623954	42.703220
3504.276835	495404.062985	42.708224
3504.026832	495408.153131	42.713229
3503.967748	495393.428359	42.718234
3504.381323	495371.439013	42.723239
3504.287986	495367.808217	42.728244
3504.209158	495357.694123	42.733248
3504.220681	495344.173341	42.738253
3504.460444	495330.262044	42.743258
3504.351290	495319.595760	42.748263
3504.407474	495292.498244	42.753268
3504.906146	495277.280160	42.758272
3504.322121	495266.790165	42.763277
3504.032704	495247.089002	42.768282
3504.384004	495238.476488	42.773287
3504.371135	495210.984699	42.778292
3503.943090	495204.571309	42.783296
3503.989981	495200.411984	42.788301
3504.255299	495187.002873	42.793306
3504.389428	495173.715753	42.798311
3504.253679	495171.711888	42.803316
3504.418523	495138.774133	42.808321
3504.612041	495126.287727	42.813325
3504.462963	495096.083085	42.818330
3504.472613	495090.461247	42.823335
3504.331206	495072.356777	42.828340
3504.386455	495047.942629	42.833345
3504.292529	495027.805263	42.838349
3504.732490	494999.684615	42.843354
3504.557057	494985.686778	42.848359
3504.509389	494978.656216	42.853364
3504.947705	494948.915466	42.858369
3504.512310	494940.984125	42.863373
3504.404371	494918.671591	42.868378
3504.245620	494893.632818	42.873383
3504.175060	494885.542521	42.878388
3504.460543	494864.990571	42.883393
3504.019455	494852.401743	42.888397
3504.130633	494835.928048	42.893402
3504.359832	494816.195087	42.898407
3504.358259	494804.802619	42.903412
3504.462051	494796.988533	42.908417
3504.296429	494766.228983	42.913421
3504.275462	494757.016834	42.918426
3504.291053	494743.343061	42.923431
3504.204768	494730.292995	42.928436
3504.259665	494707.043045	42.933441
3504.640972	494703.894080	42.938445
3504.588974	494679.698931	42.943450
3504.573371	494662.991945	42.948455
3504.190403	494654.393941	42.953460
3504.337902	494641.408132	42.958465
3504.265840	494628.001301	42.963469
3504.273284	494600.100307	42.968474
3504.670592	494598.012129	42.973479
3504.514867	494592.112466	42.978484
3504.425977	494551.061528	42.983489
3504.151467	494562.548453	42.988493
3504.424374	494533.845876	42.993498
3504.389950	494507.065330	42.998503
3504.348093	494505.147823	43.003508
3504.388478	494471.620918	43.008513
3504.595419	494456.195089	43.013517
3504.386961	494448.582113	43.018522
3504.188348	494422.890737	43.023527
3504.171399	494415.500657	43.028532
3504.198363	494381.114905	43.033537
3503.881033	494368.911268	43.038541
3503.786668	494370.951621	43.043546
3504.428619	494357.533013	43.048551
3504.069326	494358.298713	43.053556
3503.813405	494328.970500	43.058561
3504.188019	494328.050499	43.063565
3504.234900	494327.384841	43.068570
3504.141877	494310.942950	43.073575
3504.562849	494293.558998	43.078580
3504.668656	494281.744148	43.083585
3504.464183	494247.850449	43.088589
3504.252634	494246.820545	43.093594
3504.490863	494220.047124	43.098599
3504.448405	494193.419299	43.103604
3504.498877	494193.006248	43.108609
3504.435587	494172.002287	43.113613
3504.211383	494152.188367	43.118618
3504.466335	494144.046296	43.123623
3504.389872	494106.942024	43.128628
3504.326997	494094.799260	43.133633
3503.999895	494086.647886	43.138637
3503.978014	494064.270075	43.143642
3504.385675	494069.269300	43.148647
3504.245110	494061.594796	43.153652
3504.339374	494025.830560	43.158657
3504.320313	494013.731455	43.163661
3504.305583	494009.936055	43.168666
3504.300880	493993.479921	43.173671
3504.057776	493974.782802	43.178676
3504.604749	493966.088132	43.183681
3504.335625	493958.028810	43.188685
3504.421916	493940.039146	43.193690
3504.483789	493913.495700	43.198695
3504.352790	493895.439061	43.203700
3504.268046	493895.553743	43.208705
3504.245437	493879.657343	43.213709
3504.292116	493857.470993	43.218714
3504.349500	493843.739310	43.223719
3504.136671	493826.303180	43.228724
3504.608290	493804.302789	43.233729
3504.265132	493805.926792	43.238733
3504.176248	493775.305366	43.243738
3504.193425	493764.922035	43.248743
3504.288586	493769.869458	43.253748
3504.666954	493734.161028	43.258753
3504.401012	493725.392179	43.263757
3504.314863	493705.809144	43.268762
3504.530824	493688.102564	43.273767
3504.140886	493673.935079	43.278772
3504.588936	493650.317830	43.283777
3504.549061	493644.450190	43.288781
3504.649969	493621.394146	43.293786
3504.363770	493600.931141	43.298791
3503.971315	493596.587705	43.303796
3504.069133	493571.253390	43.308801
3504.486630	493554.071843	43.313805
3504.333425	493537.081756	43.318810
3504.235823	493526.311328	43.323815
3504.010062	493519.612184	43.328820
3504.112054	493500.606850	43.333825
3504.124329	493489.110103	43.338829
3504.094488	493472.151097	43.343834
3504.045362	493457.524475	43.348839
3504.122470	493449.967227	43.353844
3504.481953	493441.605773	43.358849
3504.068095	493428.252090	43.363853
3503.955471	493412.723982	43.368858
3504.284072	493417.938434	43.373863
3504.245949	493392.017700	43.378868
3504.644557	493366.129181	43.383873
3504.036225	493361.161509	43.388877
3504.297755	493338.940578	43.393882
3504.513474	493318.752400	43.398887
3504.192661	493312.777141	43.403892
3504.426113	493286.914615	43.408897
3504.340327	493281.965609	43.413901
3504.563495	493265.675365	43.418906
3504.672786	493248.896718	43.423911
3504.365094	493242.970002	43.428916
3504.273664	493208.296943	43.433921
3504.205264	493213.067812	43.438925
3504.312802	493194.517037	43.443930
3504.318974	493177.400151	43.448935
3504.669188	493163.469763	43.453940
3504.529650	493134.627642	43.458945
3504.311690	493126.863702	43.463949
3504.232474	493107.532132	43.468954
3504.320023	493075.615684	43.473959
3503.846137	493076.348906	43.478964
3504.417312	493067.042322	43.483969
3504.434032	493050.075569	43.488973
3504.055415	493026.031149	43.493978
3504.343086	493024.618437	43.498983
3504.146661	493007.634694	43.503988
3504.184045	492985.296847	43.508993
3504.221357	492979.518075	43.513997
3504.144333	492974.263765	43.519002
3504.379976	492940.652577	43.524007
3504.315325	492943.853099	43.529012
3504.403365	492918.468795	43.534017
3504.306172	492909.926084	43.539021
3504.082870	492896.339338	43.544026
3504.381244	492881.556058	43.549031
3504.405559	492855.928543	43.554036
3504.050490	492845.552889	43.559041
3504.212627	492839.804984	43.564045
3504.093305	492824.935757	43.569050
3504.302224	492806.824328	43.574055
3504.268139	492796.296635	43.579060
3504.424905	492768.318628	43.584065
3504.461234	492757.070824	43.589069
3504.186711	492741.061339	43.594074
3504.354467	492717.942964	43.599079
3504.377103	492716.369558	43.604084
3504.319412	492691.311817	43.609089
3504.277920	492674.607121	43.614093
3504.233926	492672.132718	43.619098
3504.396848	492645.267639	43.624103
3504.010383	492639.758300	43.629108
3503.872497	492620.435494	43.634113
3504.083596	492624.959778	43.639117
3503.822972	492608.137735	43.644122
3504.040596	492583.795941	43.649127
3503.891988	492582.300229	43.654132
3503.916780	492576.827153	43.659137
3504.051805	492577.362872	43.664141
3503.990614	492555.394571	43.669146
3504.394516	492530.972625	43.674151
3504.273485	492530.080238	43.679156
3504.399387	492515.020082	43.684161
3504.171776	492479.810135	43.689165
3504.067898	492482.662451	43.694170
3504.059262	492467.420957	43.699175
3503.736695	492445.443195	43.704180
3503.762828	492429.082076	43.709185
3503.618699	492441.359965	43.714189
3504.194031	492431.444717	43.719194
3504.433160	492412.163388	43.724199
3504.227918	492410.119562	43.729204
3504.355744	492388.982085	43.734209
3504.251585	492382.769717	43.739213
3504.036581	492358.192159	43.744218
3504.354731	492346.342511	43.749223
3503.851929	492336.800178	43.754228
3504.184952	492326.771249	43.759233
3504.051180	492316.714809	43.764237
3503.881064	492298.460227	43.769242
3504.465479	492298.823645	43.774247
3503.920849	492273.892943	43.779252
3504.083824	492260.548526	43.784257
3503.817632	492257.855979	43.789261
3503.833319	492257.954798	43.794266
3504.128774	492252.337564	43.799271
3504.387759	492223.532319	43.804276
3504.483900	492217.186955	43.809281
3504.457139	492205.999429	43.814285
3504.006145	492191.030190	43.819290
3504.756930	492164.223427	43.824295
3504.245586	492147.693801	43.829300
3504.119065	492132.977082	43.834305
3504.445966	492124.316337	43.839309
3504.067708	492105.739970	43.844314
3504.128070	492079.903117	43.849319
3504.096650	492088.112077	43.854324
3503.984314	492065.189083	43.859329
3504.046442	492051.860456	43.864333
3503.937764	492029.088766	43.869338
3504.182644	492034.620695	43.874343
3503.960994	492029.287692	43.879348
3503.815972	492021.410476	43.884353
3503.879417	491992.483852	43.889357
3503.555292	491986.154191	43.894362
3503.970386	491998.546554	43.899367
3503.590764	491991.212824	43.904372
3503.924260	491987.108761	43.909377
3504.201686	491974.961462	43.914381
3504.070489	491957.206813	43.919386
3504.159952	491945.798193	43.924391
3504.150423	491950.256229	43.929396
3503.928250	491934.642910	43.934401
3504.291753	491914.176636	43.939405
3504.315151	491906.070182	43.944410
3504.552517	491889.776487	43.949415
3504.361669	491878.260202	43.954420
3504.492269	491855.450481	43.959425
3504.125985	491843.404834	43.964429
3503.846674	491839.397595	43.969434
3504.333780	491823.975936	43.974439
3504.027777	491819.922268	43.979444
3503.768908	491783.044734	43.984449
3503.933652	491772.079893	43.989453
3503.814718	491771.490993	43.994458
3504.100193	491763.596269	43.999463
3504.090022	491766.180670	44.004468
3504.155078	491740.190676	44.009473
3504.209181	491722.254588	44.014477
3503.522475	491736.087339	44.019482
3504.081431	491738.328578	44.024487
3503.843178	491711.019126	44.029492
3503.908609	491688.574001	44.034497
3503.958363	491686.084649	44.039501
3504.056776	491680.093243	44.044506
3504.086313	491672.492147	44.049511
3503.677948	491657.465096	44.054516
3503.892094	491642.187715	44.059521
3503.972212	491646.834226	44.064525
3503.734817	491647.327549	44.069530
3504.095759	491637.698981	44.074535
3504.186864	491612.413695	44.079540
3504.219417	491601.824148	44.084545
3504.059542	491601.900075	44.089549
3504.152838	491589.427124	44.094554
3504.496539	491567.646876	44.099559
3503.890299	491566.476627	44.104564
3504.239136	491545.455191	44.109569
3503.908363	491518.514583	44.114573
3504.168320	491520.499246	44.119578
3504.474514	491516.956473	44.124583
3503.904898	491493.193468	44.129588
3504.042682	491463.292047	44.134593
3504.173201	491473.501423	44.139597
3503.877370	491469.851218	44.144602
3503.856775	491456.282022	44.149607
3503.937123	491429.580168	44.154612
3504.425061	491420.488497	44.159617
3504.177352	491419.210928	44.164621
3504.182719	491410.904534	44.169626
3504.309126	491387.487178	44.174631
3504.035667	491370.817973	44.179636
3504.255680	491367.845875	44.184641
3504.087046	491343.867371	44.189645
3504.290440	491337.606044	44.194650
3504.348676	491323.213990	44.199655
3504.012382	491319.823370	44.204660
3504.218515	491293.911744	44.209665
3504.205168	491280.746427	44.214669
3504.158344	491276.550387	44.219674
3504.216569	491250.155638	44.224679
3504.072222	491246.633379	44.229684
3504.038022	491231.850711	44.234689
3504.175587	491207.975569	44.239693
3504.050751	491201.462208	44.244698
3504.213490	491192.269892	44.249703
3503.906623	491179.404116	44.254708
3504.037993	491168.393550	44.259713
3504.541546	491147.347213	44.264717
3504.038542	491146.970929	44.269722
3503.729882	491128.281295	44.274727
3504.156704	491112.463422	44.279732
3504.348010	491112.179978	44.284737
3504.016197	491117.499462	44.289741
3503.712379	491086.097255	44.294746
3503.980400	491073.646988	44.299751
3503.893450	491079.636806	44.304756
3503.792878	491068.308329	44.309761
3503.838608	491063.692457	44.314765
3503.557652	491063.129142	44.319770
3503.695835	491055.713201	44.324775
3503.868996	491030.414157	44.329780
3503.882053	491027.221491	44.334785
3503.889786	491033.044425	44.339789
3503.893311	491036.386432	44.344794
3504.480934	491008.793486	44.349799
3503.932817	491002.752114	44.354804
3504.053198	490989.413521	44.359809
3503.669448	490990.233860	44.364813
3503.734046	490982.019203	44.369818
3504.131489	490978.765776	44.374823
3503.795943	490965.701806	44.379828
3503.912905	490941.728290	44.384833
3503.892194	490943.200282	44.389837
3503.875355	490951.458082	44.394842
3503.876581	490943.101490	44.399847
3504.052138	490918.916104	44.404852
3503.661040	490898.922499	44.409857
3504.188354	490890.584024	44.414861
3503.941093	490898.118590	44.419866
3503.905845	490892.198702	44.424871
3503.626770	490868.540913	44.429876
3504.069119	490849.124559	44.434881
3503.946862	490846.611636	44.439885
3503.919613	490844.387569	44.444890
3504.199242	490835.227248	44.449895
3503.901823	490820.384566	44.454900
3503.986809	490806.899500	44.459905
3504.195471	490804.992659	44.464909
3503.793624	490804.448443	44.469914
3504.049582	490779.591781	44.474919
3503.837270	490775.928239	44.479924
3503.885189	490767.361606	44.484929
3504.377315	490766.473513	44.489933
3504.037527	490750.979081	44.494938
3504.133361	490722.956987	44.499943
3504.070889	490711.470335	44.504948
3504.070350	490708.634283	44.509953
3504.277137	490696.598609	44.514957
3504.152354	490684.311459	44.519962
3504.324120	490675.674565	44.524967
3504.167076	490660.708277	44.529972
3504.054385	490632.313840	44.534977
3503.867092	490632.495394	44.539981
3503.827979	490625.157951	44.544986
3504.136298	490610.168717	44.549991
3503.987766	490608.875416	44.554996
3504.024380	490577.266608	44.560001
3504.206301	490588.987723	44.565005
3504.170937	490581.345795	44.570010
3504.062973	490555.280206	44.575015
3504.045669	490538.620416	44.580020
3503.910206	490541.883188	44.585025
3504.044131	490533.961253	44.590029
3503.926162	490524.002639	44.595034
3504.015107	490493.448986	44.600039
3504.053143	490491.315851	44.605044
3504.201879	490493.216912	44.610049
3504.144088	490474.638910	44.615053
3504.215182	490450.570723	44.620058
3504.228164	490449.707700	44.625063
3503.875512	490442.318448	44.630068
3504.090251	490425.824468	44.635073
3504.343413	490418.491396	44.640077
3503.893885	490421.550594	44.645082
3503.869815	490408.183771	44.650087
3503.842035	490382.409146	44.655092
3504.064004	490372.042198	44.660097
3503.946674	490371.554292	44.665101
3503.989651	490377.118627	44.670106
3504.198815	490352.623320	44.675111
3503.751141	490340.538917	44.680116
3503.875347	490327.097955	44.685121
3503.915104	490322.989310	44.690125
3503.780382	490331.772481	44.695130
3503.986637	490312.950000	44.700135
3503.906729	490298.781578	44.705140
3504.223326	490279.789684	44.710145
3504.031299	490279.870695	44.715149
3503.815559	490284.564308	44.720154
3504.055540	490260.823711	44.725159
3503.763276	490242.282538	44.730164
3504.158340	490234.724379	44.735169
3504.202782	490235.223838	44.740173
3504.056726	490226.383735	44.745178
3503.960074	490191.401998	44.750183
3503.914400	490192.422171	44.755188
3504.097033	490182.821040	44.760193
3503.952309	490183.350399	44.765197
3503.821355	490170.608064	44.770202
3504.148170	490142.143418	44.775207
3504.026209	490151.836304	44.780212
3504.100035	490143.873057	44.785217
3504.284599	490128.497822	44.790221
3503.769651	490119.969209	44.795226
3504.264114	490098.771191	44.800231
3504.245976	490100.141548	44.805236
3504.028663	490076.219758	44.810241
3504.126336	490062.175032	44.815245
3504.350530	490063.304501	44.820250
3504.281383	490039.156656	44.825255
3504.136013	490028.644988	44.830260
3504.038691	490016.505001	44.835265
3504.327810	489999.289827	44.840269
3504.185091	489981.281882	44.845274
3504.019319	489967.835846	44.850279
3503.946213	489963.289133	44.855284
3503.809246	489950.800836	44.860289
3504.211714	489935.188413	44.865293
3503.814890	489928.616301	44.870298
3504.207329	489925.667371	44.875303
3504.046784	489916.322935	44.880308
3503.863709	489901.258859	44.885313
3504.299843	489882.399614	44.890317
3503.982073	489881.943375	44.895322
3504.250724	489863.161229	44.900327
3504.312254	489843.145603	44.905332
3503.848045	489828.277846	44.910337
3504.048637	489827.840973	44.915341
3503.754863	489826.773164	44.920346
3503.837167	489799.005068	44.925351
3503.811385	489804.681737	44.930356
3503.600273	489791.293389	44.935361
3504.068196	489783.419645	44.940365
3503.745244	489792.080874	44.945370
3503.954699	489788.654364	44.950375
3504.080232	489759.917065	44.955380
3503.893169	489753.109145	44.960385
3504.011975	489748.481399	44.965389
3504.125341	489751.147849	44.970394
3504.111850	489728.712846	44.975399
3503.966777	489708.577786	44.980404
3503.618939	489715.723535	44.985409
3503.881816	489699.677145	44.990413
3503.998754	489708.319535	44.995418
3503.737207	489693.217046	45.000423
3503.730764	489670.223728	45.005428
3503.869715	489665.440833	45.010433
3503.980372	489656.711832	45.015437
3503.667410	489664.155979	45.020442
3503.955503	489660.514423	45.025447
3503.877481	489650.447734	45.030452
3503.617499	489630.128157	45.035457
3504.056298	489609.444872	45.040461
3503.711564	489620.743347	45.045466
3503.712583	489607.321339	45.050471
3503.590402	489623.041710	45.055476
3503.580199	489605.113756	45.060481
3503.593514	489621.775035	45.065485
3503.689717	489624.190973	45.070490
3503.721734	489583.413835	45.075495
3503.503349	489585.474311	45.080500
3503.711034	489579.667558	45.085505
3503.834053	489567.391158	45.090509
3503.891150	489577.815770	45.095514
3503.781826	489567.095550	45.100519
3503.572756	489580.347905	45.105524
3503.466108	489563.042938	45.110529
3503.856919	489573.313511	45.115533
3503.512186	489551.082595	45.120538
3503.980699	489530.293229	45.125543
3503.676587	489543.307388	45.130548
3503.479722	489533.006175	45.135553
3503.770472	489525.970707	45.140557
3503.660293	489523.506346	45.145562
3503.829472	489527.328928	45.150567
3504.073152	489522.022956	45.155572
3504.106652	489489.754375	45.160577
3504.002521	489483.186494	45.165581
3503.858332	489482.905405	45.170586
3503.647205	489467.642819	45.175591
3503.664050	489471.995979	45.180596
3503.727352	489466.060064	45.185601
3503.679315	489450.417145	45.190605
3504.127564	489436.924330	45.195610
3503.758490	489423.104844	45.200615
3503.795507	489437.382034	45.205620
3503.785215	489431.609688	45.210625
3503.752687	489432.323930	45.215629
3504.075278	489417.534087	45.220634
3503.736385	489407.964341	45.225639
3504.031817	489391.304753	45.230644
3503.920270	489384.586062	45.235649
3504.182913	489386.925076	45.240653
3504.050484	489369.775954	45.245658
3504.140339	489340.689108	45.250663
3503.737493	489355.896919	45.255668
3503.964204	489347.200082	45.260673
3503.914800	489326.036506	45.265677
3503.852747	489315.815165	45.270682
3504.139256	489306.349118	45.275687
3503.956834	489306.428614	45.280692
3503.855239	489304.874556	45.285697
3503.813961	489268.869361	45.290701
3503.839442	489272.157564	45.295706
3504.115984	489254.386553	45.300711
3503.548996	489268.404790	45.305716
3503.623418	489270.925515	45.310721
3504.240122	489250.821512	45.315725
3504.046563	489241.836504	45.320730
3504.054037	489214.839116	45.325735
3503.968413	489209.331856	45.330740
3503.867382	489217.046580	45.335745
3504.267445	489196.217016	45.340749
3503.868792	489177.235757	45.345754
3504.060276	489170.671694	45.350759
3503.996547	489169.314239	45.355764
3503.691878	489161.663647	45.360769
3503.791256	489129.535985	45.365773
3503.914651	489133.771083	45.370778
3503.627322	489122.622896	45.375783
3503.876929	489120.354866	45.380788
3503.804171	489139.005521	45.385793
3503.933219	489129.614922	45.390797
3503.948074	489106.617549	45.395802
3503.918127	489090.768872	45.400807
3503.756398	489094.289294	45.405812
3503.615053	489087.170007	45.410817
3503.954646	489075.720106	45.415821
3503.962200	489086.558019	45.420826
3503.837980	489071.838526	45.425831
3503.785887	489050.320515	45.430836
3503.643889	489047.354620	45.435841
3503.765554	489037.762542	45.440845
3503.737101	489039.894357	45.445850
3503.938204	489035.202779	45.450855
3503.977879	489046.086290	45.455860
3503.730599	489012.848268	45.460865
3504.175755	489003.407644	45.465869
3503.833044	489012.274954	45.470874
3504.208627	489012.722109	45.475879
3503.999893	488988.139125	45.480884
3503.747140	488975.212628	45.485889
3503.778979	488958.746272	45.490893
3503.783301	488954.237726	45.495898
3503.998680	488960.180436	45.500903
3504.165229	488945.212285	45.505908
3503.928208	488937.550909	45.510913
3504.280181	488920.628719	45.515917
3503.756330	488918.634863	45.520922
3503.933884	488907.868926	45.525927
3504.123908	488880.740907	45.530932
3504.186910	488872.728182	45.535937
3504.377020	488874.572219	45.540941
3503.957085	488860.000599	45.545946
3504.024218	488842.566202	45.550951
3504.014276	488838.161185	45.555956
3503.951499	488838.525676	45.560961
3504.211657	488815.843732	45.565965
3504.093500	488800.160705	45.570970
3504.215835	488788.289112	45.575975
3504.001376	488787.563261	45.580980
3504.066155	488769.268106	45.585985
3504.105779	488749.862590	45.590989
3503.524851	488751.473947	45.595994
3503.914793	488728.264877	45.600999
3503.808889	488728.180329	45.606004
3503.923413	488735.101417	45.611009
3503.982286	488702.979431	45.616013
3504.059983	488701.802193	45.621018
3504.076800	488696.075987	45.626023
3504.293152	488694.218371	45.631028
3504.286423	488677.352657	45.636033
3504.358052	488655.004224	45.641037
3503.843872	488652.907508	45.646042
3503.914949	488632.028018	45.651047
3504.073013	488618.529833	45.656052
3503.795406	488605.303103	45.661057
3504.028851	488592.096893	45.666061
3504.106626	488602.822684	45.671066
3503.767541	488578.361071	45.676071
3503.805090	488565.894923	45.681076
3503.822573	488564.220680	45.686081
3504.213847	488550.381679	45.691085
3503.821882	488552.267095	45.696090
3504.064153	488525.687473	45.701095
3504.040398	488520.068930	45.706100
3503.577288	488505.757117	45.711105
3503.874762	488510.673962	45.716109
3504.080756	488511.857055	45.721114
3504.095274	488494.430653	45.726119
3504.185692	488475.877904	45.731124
3504.025152	488474.434396	45.736129
3504.017047	488471.042035	45.741133
3503.983613	488448.456705	45.746138
3503.821582	488425.233201	45.751143
3503.695432	488426.722054	45.756148
3503.891320	488428.666525	45.761153
3504.116773	488430.099807	45.766157
3503.812798	488406.848063	45.771162
3504.212892	488389.765837	45.776167
3503.992677	488378.150735	45.781172
3503.867965	488377.461335	45.786177
3504.025361	488362.443518	45.791181
3503.713165	488346.588174	45.796186
3503.819475	488344.444005	45.801191
3504.002160	488329.067601	45.806196
3503.803622	488325.097488	45.811201
3504.052545	488321.968388	45.816205
3504.052411	488310.926284	45.821210
3504.013859	488301.156547	45.826215
3504.109299	488294.607361	45.831220
3504.029763	488304.547751	45.836225
3504.236007	488276.251303	45.841229
3503.900538	488268.453259	45.846234
3503.687243	488250.150899	45.851239
3503.581205	488250.268978	45.856244
3503.810848	488253.575742	45.861249
3504.044673	488248.017711	45.866253
3503.944729	488222.454143	45.871258
3503.980489	488213.331095	45.876263
3504.195705	488209.396867	45.881268
3503.916326	488202.653629	45.886273
3504.173501	488167.409599	45.891277
3503.783389	488172.181946	45.896282
3503.915210	488162.385210	45.901287
3504.187587	488154.085827	45.906292
3503.768172	488140.627922	45.911297
3503.821760	488120.307808	45.916301
3504.007916	488111.059635	45.921306
3504.046862	488109.128697	45.926311
3503.970503	488114.256690	45.931316
3503.939585	488104.941518	45.936321
3504.218202	488077.697039	45.941325
3503.655697	488083.661667	45.946330
3503.741708	488061.664828	45.951335
3503.971854	488061.679120	45.956340
3503.886714	488057.336459	45.961345
3503.751040	488035.931809	45.966349
3503.865222	488027.556068	45.971354
3504.106476	488026.555549	45.976359
3503.957845	488027.946681	45.981364
3503.805995	488018.397316	45.986369
3503.999669	488006.615263	45.991373
3503.913113	487994.928147	45.996378
3503.661756	487998.868161	46.001383
3503.752343	487976.262665	46.006388
3503.561333	487984.296031	46.011393
3503.677461	487987.519477	46.016397
3503.577808	487981.760811	46.021402
3503.839723	487981.719430	46.026407
3503.953159	487961.187074	46.031412
3503.693790	487955.757562	46.036417
3504.106178	487936.494907	46.041421
3503.944009	487953.337354	46.046426
3503.921226	487941.184248	46.051431
3504.126816	487915.774587	46.056436
3503.766012	487903.978802	46.061441
3504.108792	487895.921444	46.066445
3504.171558	487893.328228	46.071450
3504.110859	487881.687609	46.076455
3503.940890	487867.328979	46.081460
3503.760078	487857.378884	46.086465
3504.035978	487850.699716	46.091469
3503.831054	487856.405284	46.096474
3503.461158	487826.122442	46.101479
3503.976115	487815.302558	46.106484
3503.790756	487812.242014	46.111489
3504.005652	487811.954797	46.116493
3503.853979	487816.689547	46.121498
3504.047318	487805.413956	46.126503
3504.164733	487778.853020	46.131508
3503.871652	487780.216347	46.136513
3504.154445	487754.237081	46.141517
3503.729676	487759.015008	46.146522
3503.920492	487748.398278	46.151527
3503.821596	487730.735831	46.156532
3503.826440	487719.743249	46.161537
3503.928793	487716.637216	46.166541
3503.680294	487716.879121	46.171546
3503.991115	487718.653540	46.176551
3503.805039	487713.516295	46.181556
3503.514560	487693.857949	46.186561
3503.957346	487677.882717	46.191565
3503.681669	487681.978601	46.196570
3503.785421	487685.609285	46.201575
3503.703802	487687.952270	46.206580
3503.513653	487677.598327	46.211585
3503.796237	487665.852664	46.216589
3503.817822	487675.676094	46.221594
3503.854010	487648.823893	46.226599
3503.753024	487636.227068	46.231604
3503.387823	487634.258650	46.236609
3503.918027	487627.539210	46.241613
3503.532834	487621.065757	46.246618
3503.739051	487638.356797	46.251623
3503.838914	487635.858990	46.256628
3503.714838	487634.207039	46.261633
3503.964423	487611.727940	46.266637
3504.030313	487606.297573	46.271642
3504.079215	487604.466318	46.276647
3503.960656	487593.189243	46.281652
3503.774016	487581.315075	46.286657
3503.950675	487559.252673	46.291661
3504.054881	487556.500899	46.296666
3503.780045	487550.465865	46.301671
3503.827789	487558.613637	46.306676
3503.790539	487550.666853	46.311681
3503.623242	487537.320632	46.316685
3503.551655	487521.933108	46.321690
3503.687733	487515.174613	46.326695
3503.845255	487512.617023	46.331700
3503.336957	487513.001301	46.336705
3503.767371	487515.769921	46.341709
3503.828282	487514.088721	46.346714
3503.545377	487512.056629	46.351719
3503.921026	487507.337088	46.356724
3504.079319	487501.081619	46.361729
3503.623549	487476.282442	46.366733
3504.000766	487475.513677	46.371738
3504.068081	487462.231630	46.376743
3503.876607	487462.109945	46.381748
3503.763873	487460.354878	46.386753
3504.175028	487436.634333	46.391757
3504.069467	487419.580502	46.396762
3503.948327	487424.867721	46.401767
3503.760644	487427.227502	46.406772
3503.837896	487415.970029	46.411777
3503.942954	487382.825416	46.416781
3504.006403	487383.625875	46.421786
3503.727660	487375.919804	46.426791
3504.426683	487369.629483	46.431796
3503.825556	487355.034683	46.436801
3503.979027	487339.003585	46.441805
3503.510351	487336.291671	46.446810
3503.654912	487331.861883	46.451815
3503.869409	487329.649847	46.456820
3503.858027	487329.955588	46.461825
3503.879499	487304.523556	46.466829
3503.753392	487292.031782	46.471834
3503.455308	487283.264981	46.476839
3503.943617	487281.820138	46.481844
3503.895240	487279.345715	46.486849
3503.921966	487266.829769	46.491853
3504.187516	487277.729251	46.496858
3503.692456	487261.851245	46.501863
3504.058228	487237.935006	46.506868
3504.001762	487243.921223	46.511873
3504.140875	487245.216277	46.516877
3503.893160	487220.231918	46.521882
3504.140444	487191.116887	46.526887
3504.056870	487194.523998	46.531892
3503.661319	487192.357710	46.536897
3503.719207	487189.562549	46.541901
3503.287632	487183.146931	46.546906
3503.555639	487189.689741	46.551911
3503.816860	487175.515711	46.556916
3503.663055	487169.562737	46.561921
3503.727229	487158.509798	46.566925
3503.595444	487144.499171	46.571930
3503.758707	487149.690861	46.576935
3504.062767	487144.627960	46.581940
3503.692103	487143.977387	46.586945
3503.904040	487147.540420	46.591949
3503.931393	487119.523799	46.596954
3503.719012	487110.591406	46.601959
3503.999204	487104.367196	46.606964
3503.654914	487103.611143	46.611969
3504.161396	487102.467346	46.616973
3503.833703	487084.789805	46.621978
3503.857476	487065.992934	46.626983
3504.342235	487052.847245	46.631988
3503.854643	487062.346226	46.636993
3503.707088	487051.985209	46.641997
3503.776932	487027.912858	46.647002
3503.628913	487010.662749	46.652007
3503.791982	487006.027339	46.657012
3503.784585	487018.641742	46.662017
3503.512158	487008.958959	46.667021
3503.838999	487006.070607	46.672026
3503.496228	487008.708229	46.677031
3503.762855	487004.056451	46.682036
3503.691320	487015.161328	46.687041
3504.041001	486999.808110	46.692045
3503.878237	486977.697370	46.697050
3503.727172	486971.389311	46.702055
3504.074241	486967.585955	46.707060
3503.870722	486971.164030	46.712065
3504.110799	486954.865642	46.717069
3503.959426	486933.208951	46.722074
3503.857501	486927.095733	46.727079
3503.796703	486915.606504	46.732084
3503.830347	486926.137596	46.737089
3503.612535	486922.271545	46.742093
3503.954684	486906.311574	46.747098
3503.861300	486891.686822	46.752103
3503.908785	486883.777022	46.757108
3503.672894	486890.855481	46.762113
3503.880231	486877.348272	46.767117
3504.111722	486889.874348	46.772122
3503.844648	486864.487333	46.777127
3503.791390	486840.940761	46.782132
3503.379454	486841.461787	46.787137
3503.580743	486828.259435	46.792141
3503.840987	486828.218318	46.797146
3503.783890	486828.835229	46.802151
3504.074086	486823.267874	46.807156
3503.806331	486820.422816	46.812161
3503.675942	486791.012275	46.817165
3504.182330	486778.622820	46.822170
3503.846705	486785.615769	46.827175
3503.911456	486785.706862	46.832180
3503.637765	486767.817866	46.837185
3503.815341	486747.527344	46.842189
3503.427045	486738.166674	46.847194
3503.586674	486731.150898	46.852199
3503.911888	486738.951228	46.857204
3503.402172	486739.589024	46.862209
3503.674966	486728.756144	46.867213
3503.827584	486741.852002	46.872218
3503.722780	486746.427641	46.877223
3503.793554	486731.067633	46.882228
3503.591618	486714.534964	46.887233
3503.678127	486698.108661	46.892237
3503.646017	486698.822939	46.897242
3503.488317	486699.405099	46.902247
3503.696799	486697.447222	46.907252
3503.433870	486699.312422	46.912257
3503.783629	486692.063955	46.917261
3503.701088	486700.232687	46.922266
3503.707608	486707.576837	46.927271
3503.485663	486690.996655	46.932276
3503.821169	486692.058081	46.937281
3504.017366	486678.349867	46.942285
3503.626720	486659.263501	46.947290
3503.358966	486657.684829	46.952295
3503.758934	486651.542854	46.957300
3503.729699	486647.900224	46.962305
3503.514287	486654.316999	46.967309
3503.972466	486646.646128	46.972314
3503.691414	486647.501068	46.977319
3504.092633	486645.158127	46.982324
3503.822453	486621.949509	46.987329
3503.766998	486612.485514	46.992333
3503.709315	486614.622221	46.997338
3503.673636	486606.826764	47.002343
3503.728501	486604.183965	47.007348
3503.624454	486600.654463	47.012353
3503.829629	486597.380027	47.017357
3503.671497	486567.618930	47.022362
3503.490513	486568.052804	47.027367
3503.676918	486559.057122	47.032372
3503.661759	486565.087680	47.037377
3504.098440	486560.256946	47.042381
3503.940040	486558.103759	47.047386
3503.542337	486553.506214	47.052391
3504.215955	486542.052653	47.057396
3503.650862	486524.108172	47.062401
3503.731196	486527.793435	47.067405
3504.104725	486519.325384	47.072410
3503.579436	486528.374676	47.077415
3503.769003	486511.425355	47.082420
3503.602961	486524.014503	47.087425
3503.636707	486503.391857	47.092429
3503.612831	486478.979027	47.097434
3503.628545	486473.657581	47.102439
3503.750194	486462.189899	47.107444
3503.655559	486472.234947	47.112449
3503.912496	486470.877272	47.117453
3503.908412	486475.943626	47.122458
3503.793629	486464.006744	47.127463
3503.629005	486452.938902	47.132468
3503.490877	486433.356485	47.137473
3503.764589	486423.029857	47.142477
3503.668388	486427.857497	47.147482
3503.557455	486430.965126	47.152487
3503.736224	486426.580379	47.157492
3503.920500	486429.033464	47.162497
3503.610169	486429.335813	47.167501
3503.991963	486424.159121	47.172506
3504.136713	486412.485130	47.177511
3503.913630	486397.627213	47.182516
3504.018257	486388.543062	47.187521
3504.118452	486389.337756	47.192525
3504.185951	486376.409523	47.197530
3503.426621	486356.064038	47.202535
3503.912371	486330.658640	47.207540
3503.807395	486343.086283	47.212545
3503.960180	486328.726135	47.217549
3504.020467	486337.480335	47.222554
3504.001251	486311.698808	47.227559
3503.743072	486302.570645	47.232564
3503.853645	486294.599972	47.237569
3503.926740	486280.151068	47.242573
3504.088869	486281.999783	47.247578
3503.335374	486280.649825	47.252583
3504.103517	486261.987799	47.257588
3503.800964	486243.545640	47.262593
3503.646828	486261.502777	47.267597
3504.144329	486248.658468	47.272602
3503.896766	486251.281145	47.277607
3503.963167	486229.893179	47.282612
3503.940704	486216.624454	47.287617
3503.608900	486203.911189	47.292621
3503.687661	486211.244113	47.297626
3503.790365	486205.706213	47.302631
3503.995881	486191.793547	47.307636
3503.700089	486180.189043	47.312641
3503.666000	486166.820806	47.317645
3503.779707	486168.018635	47.322650
3503.438504	486175.873868	47.327655
3503.613102	486163.891062	47.332660
3503.667788	486179.231726	47.337665
3503.757687	486164.628106	47.342669
3503.732236	486173.598563	47.347674
3503.503918	486171.101777	47.352679
3504.061328	486165.542656	47.357684
3503.671119	486144.530710	47.362689
3503.581377	486130.715323	47.367693
3503.938103	486119.868833	47.372698
3503.901386	486116.176627	47.377703
3504.060643	486116.050155	47.382708
3503.651494	486120.572730	47.387713
3503.693828	486097.060789	47.392717
3503.791573	486088.281531	47.397722
3503.492973	486079.666229	47.402727
3503.872549	486068.360177	47.407732
3503.701935	486073.959537	47.412737
3503.827104	486070.444367	47.417741
3503.982347	486077.663938	47.422746
3503.844247	486066.895627	47.427751
3503.758935	486047.000518	47.432756
3503.689832	486041.135119	47.437761
3503.478322	486032.151423	47.442765
3503.864494	486022.870626	47.447770
3503.524811	486031.586866	47.452775
3503.481417	486020.296979	47.457780
3503.884318	486023.627409	47.462785
3503.653810	486025.082284	47.467789
3503.680298	486020.518881	47.472794
3503.603010	486015.667930	47.477799
3504.100257	485980.432568	47.482804
3503.686841	485997.113820	47.487809
3503.510263	485978.854127	47.492813
3503.946455	485979.190466	47.497818
3503.557395	485991.865871	47.502823
3503.860786	485984.016568	47.507828
3503.948815	485968.450587	47.512833
3503.713725	485950.909331	47.517837
3503.274121	485939.580702	47.522842
3503.330706	485936.228323	47.527847
3503.670556	485935.769356	47.532852
3503.860613	485934.523531	47.537857
3503.780486	485928.913132	47.542861
3504.046931	485922.640053	47.547866
3504.024108	485921.934458	47.552871
3504.216564	485907.567724	47.557876
3503.832690	485904.791539	47.562881
3503.950098	485890.892580	47.567885
3503.755610	485879.525174	47.572890
3504.122880	485889.396205	47.577895
3504.338010	485860.284229	47.582900
3503.466492	485859.358160	47.587905
3503.874821	485838.017031	47.592909
3503.952833	485839.524474	47.597914
3503.516944	485842.176972	47.602919
3503.487775	485815.028566	47.607924
3503.554091	485798.199411	47.612929
3503.467322	485809.611349	47.617933
3503.600714	485796.165723	47.622938
3503.474191	485810.876760	47.627943
3504.061282	485802.729250	47.632948
3503.792801	485815.537690	47.637953
3503.726859	485802.984772	47.642957
3503.986955	485798.739004	47.647962
3503.879033	485794.754037	47.652967
3503.886889	485776.667636	47.657972
3503.649712	485757.860063	47.662977
3503.695598	485769.453693	47.667981
3503.717898	485757.950633	47.672986
3503.442990	485765.947532	47.677991
3503.665879	485748.485681	47.682996
3503.640912	485758.621410	47.688001
3503.422498	485758.200017	47.693005
3503.706099	485745.541155	47.698010
3503.528393	485741.009959	47.703015
3503.737163	485706.984844	47.708020
3503.655548	485702.995700	47.713025
3503.904082	485703.615000	47.718029
3503.667997	485702.132560	47.723034
3503.484977	485700.591073	47.728039
3503.669143	485692.456542	47.733044
3503.808654	485696.943157	47.738049
3503.805375	485695.727875	47.743053
3503.688607	485682.372367	47.748058
3503.688256	485672.291288	47.753063
3503.698613	485660.536762	47.758068
3503.743772	485660.580298	47.763073
3504.141453	485650.942889	47.768077
3504.186337	485662.790038	47.773082
3503.649111	485640.584956	47.778087
3503.741603	485617.621749	47.783092
3503.561621	485620.335148	47.788097
3503.442103	485623.798877	47.793101
3503.852086	485626.520348	47.798106
3504.053091	485614.381047	47.803111
3503.944228	485619.413528	47.808116
3503.738480	485611.188612	47.813121
3503.500352	485593.191575	47.818125
3503.831503	485586.300249	47.823130
3503.254398	485579.603132	47.828135
3503.484128	485572.018600	47.833140
3503.642075	485582.733424	47.838145
3503.666975	485579.943242	47.843149
3503.750476	485565.542813	47.848154
3503.578935	485584.567182	47.853159
3503.678254	485569.607004	47.858164
3503.708598	485567.423872	47.863169
3503.925178	485570.277238	47.868173
3504.029160	485551.415540	47.873178
3503.569493	485543.281387	47.878183
3503.830240	485538.680844	47.883188
3503.608706	485533.497953	47.888193
3503.928212	485530.965157	47.893197
3503.807853	485517.356805	47.898202
3503.681642	485512.614777	47.903207
3503.764496	485492.236577	47.908212
3503.510152	485496.278894	47.913217
3503.395154	485484.037478	47.918221
3503.831885	485474.697766	47.923226
3503.497830	485485.642385	47.928231
3503.861918	485480.721537	47.933236
3504.217893	485469.114906	47.938241
3503.847274	485480.419924	47.943245
3503.861064	485453.973450	47.948250
3503.674055	485448.987719	47.953255
3503.732860	485449.231737	47.958260
3503.974729	485449.193524	47.963265
3504.197744	485445.460136	47.968269
3503.759688	485415.336211	47.973274
3503.442543	485417.108782	47.978279
3503.581344	485406.853591	47.983284
3503.674114	485395.491155	47.988289
3503.675496	485391.640808	47.993293
3503.733346	485396.495019	47.998298
3503.669710	485408.916734	48.003303
3503.555550	485392.875645	48.008308
3503.620146	485400.160459	48.013313
3503.623358	485407.454972	48.018317
3503.817713	485399.065407	48.023322
3503.638154	485394.179803	48.028327
3503.491667	485362.591237	48.033332
3503.866668	485348.093913	48.038337
3503.579252	485350.368391	48.043341
3503.645611	485344.228068	48.048346
3503.502691	485349.620623	48.053351
3503.449738	485347.754590	48.058356
3503.509292	485351.291386	48.063361
3503.396353	485357.439098	48.068365
3503.643840	485348.889134	48.073370
3503.472196	485345.927343	48.078375
3504.023169	485346.954793	48.083380
3503.516804	485362.131489	48.088385
3503.504950	485344.807693	48.093389
3503.853069	485314.103411	48.098394
3503.451671	485319.536827	48.103399
3503.679402	485306.126608	48.108404
3503.652121	485303.952554	48.113409
3503.811272	485311.577076	48.118413
3503.843480	485294.550231	48.123418
3503.681665	485306.430270	48.128423
3503.779394	485297.042732	48.133428
3504.142794	485296.326730	48.138433
3503.558548	485277.674861	48.143437
3503.616744	485264.291407	48.148442
3503.161446	485269.784017	48.153447
3503.883762	485262.982731	48.158452
3503.781598	485267.355664	48.163457
3503.350226	485261.901905	48.168461
3503.541535	485260.655839	48.173466
3503.176854	485262.334617	48.178471
3503.593651	485263.585920	48.183476
3503.947835	485256.589515	48.188481
3503.656706	485267.020872	48.193485
3503.788978	485255.905410	48.198490
3503.489268	485235.688724	48.203495
3503.985573	485209.469611	48.208500
3503.697604	485215.746354	48.213505
3503.572809	485217.083259	48.218509
3503.580323	485212.168041	48.223514
3503.561009	485211.208564	48.228519
3503.782064	485213.605333	48.233524
3503.893233	485212.321270	48.238529
3503.520857	485204.781099	48.243533
3503.866685	485179.446954	48.248538
3503.619447	485172.089632	48.253543
3503.877791	485162.271360	48.258548
3503.436101	485175.614206	48.263553
3503.633494	485168.946513	48.268557
3503.923821	485165.709037	48.273562
3503.655695	485172.286619	48.278567
3503.925029	485163.530479	48.283572
3503.615230	485143.416610	48.288577
3503.561016	485128.277713	48.293581
3503.931180	485129.333753	48.298586
3504.049116	485124.755683	48.303591
3504.148810	485123.777391	48.308596
3504.195957	485123.972597	48.313601
3503.685422	485103.079844	48.318605
3503.880515	485089.775954	48.323610
3503.502921	485091.406127	48.328615
3503.433633	485088.985385	48.333620
3503.660701	485092.394431	48.338625
3503.694587	485088.640206	48.343629
3503.696735	485089.957057	48.348634
3503.819593	485093.737198	48.353639
3503.760560	485066.288489	48.358644
3503.954685	485051.920851	48.363649
3503.593461	485051.522012	48.368653
3503.907941	485047.115503	48.373658
3503.515519	485043.377988	48.378663
3503.726503	485043.952585	48.383668
3503.749958	485053.473104	48.388673
3503.780677	485041.866963	48.393677
3503.725868	485017.507820	48.398682
3503.310425	485020.815787	48.403687
3503.662849	484996.240270	48.408692
3503.731309	484995.773517	48.413697
3503.745172	485010.969586	48.418701
3504.057120	484996.481963	48.423706
3503.670721	485001.963759	48.428711
3503.639372	485014.177983	48.433716
3504.243388	484998.732305	48.438721
3503.961793	484963.719500	48.443725
3503.917127	484958.153872	48.448730
3503.694753	484960.570098	48.453735
3503.600550	484949.084967	48.458740
3503.971764	484952.977865	48.463745
3503.790736	484946.521889	48.468749
3503.842343	484919.714076	48.473754
3503.772201	484920.485093	48.478759
3503.613836	484918.281052	48.483764
3503.648035	484921.011358	48.488769
3503.724776	484925.710719	48.493773
3503.796582	484915.111228	48.498778
3503.675533	484910.773524	48.503783
3504.030462	484888.730527	48.508788
3503.690822	484883.464805	48.513793
3503.820369	484875.845173	48.518797
3503.960119	484871.111612	48.523802
3503.973311	484866.448713	48.528807
3504.214824	484850.502939	48.533812
3503.988270	484834.580471	48.538817
3503.668458	484826.474568	48.543821
3503.852257	484817.630467	48.548826
3503.721379	484824.389120	48.553831
3503.730124	484825.198333	48.558836
3503.909114	484788.845880	48.563841
3503.710509	484791.309032	48.568845
3503.680234	484770.897286	48.573850
3503.707048	484777.225740	48.578855
3503.923933	484772.024011	48.583860
3503.879477	484776.894549	48.588865
3503.764389	484775.544895	48.593869
3504.161225	484753.900412	48.598874
3503.498314	484753.853218	48.603879
3503.547800	484751.768291	48.608884
3503.902971	484741.377225	48.613889
3503.509661	484742.148665	48.618893
3503.942008	484744.512098	48.623898
3503.846649	484737.941188	48.628903
3504.125689	484703.092606	48.633908
3504.008064	484697.994388	48.638913
3503.593521	484703.734024	48.643917
3504.143784	484691.285631	48.648922
3503.684708	484702.503763	48.653927
3503.944947	484681.590051	48.658932
3503.741612	484663.383995	48.663937
3503.473728	484659.474736	48.668941
3503.666195	484649.514630	48.673946
3503.691202	484661.112230	48.678951
3503.771075	484652.841758	48.683956
3503.855188	484648.268921	48.688961
3503.345569	484658.887125	48.693965
3503.937660	484639.998048	48.698970
3503.609717	484628.397684	48.703975
3503.723987	484610.394688	48.708980
3503.870988	484603.532118	48.713985
3503.643650	484611.572638	48.718989
3503.591783	484608.693125	48.723994
3503.405774	484608.519892	48.728999
3503.521392	484597.963963	48.734004
3503.547275	484598.111873	48.739009
3503.369448	484601.990297	48.744013
3503.740131	484597.828112	48.749018
3503.581406	484610.721329	48.754023
3503.772384	484604.915707	48.759028
3503.955625	484581.734272	48.764033
3503.851552	484568.122672	48.769037
3503.737133	484564.493110	48.774042
3503.600873	484553.470348	48.779047
3503.869942	484564.725458	48.784052
3503.770692	484558.357750	48.789057
3503.702471	484558.115238	48.794061
3504.044861	484529.133118	48.799066
3503.772604	484519.195734	48.804071
3503.893091	484521.507162	48.809076
3503.716502	484520.977804	48.814081
3503.561022	484526.423236	48.819085
3503.832149	484507.990057	48.824090
3503.805149	484511.084728	48.829095
3503.761354	484478.262587	48.834100
3503.815070	484470.401469	48.839105
3503.471350	484472.583623	48.844109
3503.721141	484464.336877	48.849114
3503.570441	484465.069982	48.854119
3503.488619	484472.783587	48.859124
3504.189236	484466.593400	48.864129
3503.884042	484455.951918	48.869133
3503.817005	484434.937679	48.874138
3503.889509	484430.873249	48.879143
3503.843179	484416.441818	48.884148
3503.813909	484416.649109	48.889153
3503.703625	484424.468557	48.894157
3503.626572	484419.262528	48.899162
3503.493906	484403.426187	48.904167
3503.352499	484395.139917	48.909172
3503.788046	484381.898859	48.914177
3503.423783	484382.311084	48.919181
3503.792179	484377.186626	48.924186
3503.928679	484386.233646	48.929191
3503.814779	484381.185418	48.934196
3503.738451	484391.329986	48.939201
3503.729077	484387.329150	48.944205
3504.063711	484366.302013	48.949210
3503.940270	484342.814126	48.954215
3503.881437	484340.999588	48.959220
3503.623207	484337.646025	48.964225
3503.619150	484325.588985	48.969229
3504.011257	484331.353225	48.974234
3503.533499	484331.023450	48.979239
3503.645530	484315.148362	48.984244
3503.858164	484295.508321	48.989249
3503.623687	484290.327139	48.994253
3503.959661	484286.879651	48.999258
3503.802415	484286.144579	49.004263
3503.687002	484296.042060	49.009268
3503.549774	484282.688812	49.014273
3503.309763	484285.259898	49.019277
3503.606417	484284.453085	49.024282
3503.662348	484285.254863	49.029287
3503.411363	484263.965535	49.034292
3503.904474	484240.684052	49.039297
3503.655838	484252.527799	49.044301
3503.671435	484248.016359	49.049306
3503.798400	484254.430482	49.054311
3503.655975	484244.523099	49.059316
3503.744017	484233.363376	49.064321
3503.539718	484233.699658	49.069325
3503.486831	484234.265323	49.074330
3503.301203	484239.208972	49.079335
3503.128692	484236.297809	49.084340
3503.508629	484229.499615	49.089345
3503.582960	484240.380392	49.094349
3503.879662	484241.397431	49.099354
3503.871747	484229.492930	49.104359
3503.806185	484201.182751	49.109364
3503.984090	484212.655128	49.114369
3503.803316	484202.652459	49.119373
3503.857471	484187.799671	49.124378
3503.831338	484192.110168	49.129383
3503.556240	484161.806531	49.134388
3503.890498	484152.735693	49.139393
3503.685048	484150.387016	49.144397
3503.511468	484147.830650	49.149402
3503.575252	484145.591408	49.154407
3503.965511	484140.868738	49.159412
3503.847750	484139.772777	49.164417
3503.851829	484149.550121	49.169421
3503.817189	484114.243423	49.174426
3503.686933	484116.898509	49.179431
3503.711604	484105.596739	49.184436
3504.236407	484098.826266	49.189441
3503.752889	484095.204289	49.194445
3503.885238	484092.194256	49.199450
3503.924396	484073.493347	49.204455
3504.087531	484067.489311	49.209460
3503.667656	484057.271041	49.214465
3503.501876	484054.916082	49.219469
3504.031717	484055.693630	49.224474
3504.023903	484042.370424	49.229479
3503.788661	484032.021632	49.234484
3503.957791	484027.688528	49.239489
3503.806316	484013.780048	49.244493
3503.835917	484024.110719	49.249498
3503.891499	484022.278067	49.254503
3503.930360	483998.966763	49.259508
3504.112364	483976.392758	49.264513
3503.888973	483978.454622	49.269517
3504.099815	483967.224673	49.274522
3504.212814	483952.413068	49.279527
3503.859062	483946.389364	49.284532
3503.881655	483922.421911	49.289537
3503.930549	483930.723037	49.294541
3503.929362	483923.174355	49.299546
3503.542873	483917.409135	49.304551
3503.623488	483897.890884	49.309556
3504.060356	483882.014762	49.314561
3503.334908	483889.425018	49.319565
3503.717895	483867.883059	49.324570
3503.845171	483882.048817	49.329575
3503.689455	483868.242231	49.334580
3503.894858	483870.945626	49.339585
3503.722778	483872.442089	49.344589
3503.889691	483861.978979	49.349594
3503.520113	483844.507717	49.354599
3503.705032	483833.332452	49.359604
3503.725374	483827.958878	49.364609
3503.571008	483839.939970	49.369613
3504.031850	483839.613827	49.374618
3503.666156	483833.338656	49.379623
3503.678903	483844.533373	49.384628
3503.667391	483817.835333	49.389633
3503.444400	483798.415632	49.394637
3503.394995	483786.112103	49.399642
3503.476594	483792.938862	49.404647
3503.565294	483795.964697	49.409652
3503.709035	483792.142193	49.414657
3503.632736	483785.162634	49.419661
3503.842663	483790.499854	49.424666
3503.719943	483788.695361	49.429671
3503.385555	483800.147627	49.434676
3503.786561	483784.834397	49.439681
3503.592465	483789.323523	49.444685
3503.656499	483786.070920	49.449690
3503.969177	483776.800661	49.454695
3503.522718	483757.517567	49.459700
3503.722921	483744.059950	49.464705
3503.460898	483743.290752	49.469709
3503.510154	483736.493988	49.474714
3503.438083	483748.411465	49.479719
3503.449236	483745.572526	49.484724
3503.540583	483738.262468	49.489729
3503.511711	483742.928147	49.494733
3503.508605	483732.593167	49.499738
3503.652132	483748.073723	49.504743
3503.579764	483731.973980	49.509748
3503.517546	483746.676429	49.514753
3503.560868	483745.706979	49.519757
3503.862682	483745.304642	49.524762
3503.904785	483719.611274	49.529767
3503.641635	483706.632179	49.534772
3503.842903	483699.152740	49.539777
3503.857565	483694.793312	49.544781
3503.885677	483684.605366	49.549786
3503.955362	483698.729696	49.554791
3503.706930	483681.796447	49.559796
3504.193756	483665.506937	49.564801
3503.494792	483658.727076	49.569805
3503.822095	483657.662072	49.574810
3503.733170	483647.036625	49.579815
3503.798798	483657.817777	49.584820
3504.015060	483635.845933	49.589825
3503.455534	483624.028243	49.594829
3503.711574	483611.372340	49.599834
3503.742437	483609.036911	49.604839
3503.786966	483601.176892	49.609844
3504.028863	483606.154459	49.614849
3503.571145	483612.154562	49.619853
3503.971767	483596.790580	49.624858
3503.993672	483578.294577	49.629863
3503.652851	483569.127507	49.634868
3503.917188	483563.512637	49.639873
3503.867689	483565.901712	49.644877
3503.769419	483567.538526	49.649882
3503.744514	483560.500097	49.654887
3503.505802	483546.554405	49.659892
3504.147346	483529.277699	49.664897
3503.661634	483535.940891	49.669901
3503.624792	483521.051310	49.674906
3503.423135	483518.651291	49.679911
3503.444025	483516.874739	49.684916
3503.725795	483516.475566	49.689921
3503.581332	483509.658675	49.694925
3503.335962	483509.596142	49.699930
3503.475635	483517.629773	49.704935
3503.432095	483525.540364	49.709940
3503.849804	483510.224278	49.714945
3503.434687	483504.818111	49.719949
3503.393192	483479.897609	49.724954
3503.522506	483493.506017	49.729959
3503.429498	483494.128710	49.734964
3503.731791	483477.817544	49.739969
3503.584014	483479.816844	49.744973
3503.808354	483464.581949	49.749978
3503.726983	483472.245217	49.754983
3503.317518	483481.682943	49.759988
3503.716033	483468.244455	49.764993
3503.246424	483473.283848	49.769997
3503.632720	483472.665494	49.775002
3503.704323	483467.435713	49.780007
3503.490349	483474.207971	49.785012
3503.864956	483469.791602	49.790017
3503.801972	483458.452643	49.795021
3503.543939	483437.720831	49.800026
3503.570778	483433.258090	49.805031
3503.517310	483427.744076	49.810036
3503.647504	483424.835610	49.815041
3503.464320	483422.280665	49.820045
3503.645906	483423.113284	49.825050
3503.739955	483420.565185	49.830055
3503.798504	483428.155691	49.835060
3503.642010	483426.913816	49.840065
3503.748942	483416.865266	49.845069
3503.913933	483407.415514	49.850074
3503.765170	483386.869037	49.855079
3503.572688	483377.526436	49.860084
3504.070728	483374.610489	49.865089
3503.891660	483385.430468	49.870093
3504.052529	483370.205531	49.875098
3504.222921	483353.205797	49.880103
3503.897268	483342.566933	49.885108
3503.850570	483329.958695	49.890113
3503.744897	483335.852576	49.895117
3503.817368	483330.571955	49.900122
3503.724251	483320.605639	49.905127
3503.364973	483314.734606	49.910132
3503.837515	483300.473658	49.915137
3503.872315	483303.558755	49.920141
3503.592907	483300.664345	49.925146
3503.655662	483288.596099	49.930151
3504.050235	483299.477456	49.935156
3503.712651	483295.528268	49.940161
3503.609528	483287.438133	49.945165
3503.672563	483257.231629	49.950170
3503.873757	483259.986441	49.955175
3503.609590	483245.385904	49.960180
3503.548117	483246.307613	49.965185
3503.452719	483249.919951	49.970189
3503.485722	483243.074917	49.975194
3503.760707	483247.895351	49.980199
3503.584050	483251.267205	49.985204
3503.515175	483255.179342	49.990209
3503.409182	483243.847055	49.995213
3503.749462	483242.729313	50.000218
3503.520803	483253.405208	50.005223
3503.163928	483251.485677	50.010228
3503.865214	483237.948511	50.015233
3503.648911	483231.801527	50.020237
3503.337393	483216.195143	50.025242
3503.631114	483203.381022	50.030247
3503.371361	483206.766017	50.035252
3503.931607	483195.632393	50.040257
3503.301296	483208.195756	50.045261
3503.548627	483204.306098	50.050266
3503.816504	483199.653210	50.055271
3503.380985	483205.548597	50.060276
3503.638140	483198.161464	50.065281
3503.560429	483202.176340	50.070285
3503.386770	483195.313287	50.075290
3503.740720	483207.011765	50.080295
3503.605659	483201.763911	50.085300
3503.668942	483199.017984	50.090305
3503.674886	483192.683864	50.095309
3503.569339	483165.493131	50.100314
3503.559789	483151.004277	50.105319
3503.335855	483165.276736	50.110324
3503.329358	483156.917945	50.115329
3503.397019	483151.334042	50.120333
3503.382227	483155.541646	50.125338
3503.806093	483147.976147	50.130343
3503.565997	483153.840663	50.135348
3503.598853	483164.931263	50.140353
3503.567449	483160.781659	50.145357
3503.501806	483154.104181	50.150362
3503.794095	483158.009921	50.155367
3503.415238	483156.499180	50.160372
3503.678167	483155.545656	50.165377
3503.797302	483155.476175	50.170381
3503.772195	483151.274908	50.175386
3503.881226	483126.026166	50.180391
3503.574612	483119.437429	50.185396
3503.762322	483104.664033	50.190401
3503.564195	483117.159145	50.195405
3503.762595	483102.637387	50.200410
3503.525962	483101.357492	50.205415
3503.541633	483110.018881	50.210420
3503.743115	483106.643109	50.215425
3503.727138	483110.749578	50.220429
3503.633796	483089.738035	50.225434
3503.609632	483073.984786	50.230439
3503.451190	483064.940649	50.235444
3503.550499	483063.911650	50.240449
3503.663698	483072.202980	50.245453
3503.070436	483060.896935	50.250458
3503.905269	483057.573048	50.255463
3503.724432	483066.012186	50.260468
3503.682325	483057.202988	50.265473
3503.970554	483064.098677	50.270477
3503.449706	483063.269028	50.275482
3503.549612	483067.661185	50.280487
3503.484117	483063.922275	50.285492
3503.786457	483050.701364	50.290497
3503.326860	483025.390367	50.295501
3503.585529	483026.464151	50.300506
3503.703704	483013.930981	50.305511
3503.650501	483011.811431	50.310516
3503.707984	483013.423673	50.315521
3503.559338	483016.740475	50.320525
3503.552621	483011.877612	50.325530
3503.656875	483009.682509	50.330535
3503.517045	483016.088545	50.335540
3503.943517	483007.103931	50.340545
3503.467661	483014.019073	50.345549
3503.662233	483003.399131	50.350554
3503.325375	482991.393860	50.355559
3503.625179	482974.424007	50.360564
3503.604284	482965.104752	50.365569
3503.894296	482977.522802	50.370573
3503.738966	482961.232866	50.375578
3503.629636	482966.975438	50.380583
3503.564604	482968.860379	50.385588
3503.946625	482967.128031	50.390593
3503.667597	482969.350792	50.395597
3503.346671	482961.041613	50.400602
3503.438595	482963.611074	50.405607
3503.565461	482965.111022	50.410612
3503.535520	482947.990598	50.415617
3503.875794	482932.331633	50.420621
3503.670146	482929.020179	50.425626
3503.709402	482936.107264	50.430631
3503.293486	482929.383738	50.435636
3503.839985	482919.468121	50.440641
3503.494343	482926.464045	50.445645
3503.618155	482925.633831	50.450650
3503.665768	482926.386314	50.455655
3503.769569	482926.775253	50.460660
3503.315994	482934.092231	50.465665
3503.308088	482934.194828	50.470669
3503.528107	482933.096077	50.475674
3503.819251	482927.983450	50.480679
3503.543498	482906.899207	50.485684
3503.751034	482891.818518	50.490689
3503.672494	482889.500294	50.495693
3503.152704	482882.641171	50.500698
3503.508006	482870.779759	50.505703
3503.859820	482880.654782	50.510708
3503.701458	482875.917186	50.515713
3503.507007	482886.638541	50.520717
3503.805506	482872.911453	50.525722
3503.742929	482876.772005	50.530727
3503.305382	482848.417308	50.535732
3503.643879	482818.369249	50.540737
3503.953195	482791.416421	50.545741
3503.309126	482752.707566	50.550746
3503.249923	482690.092774	50.555751
3503.082645	482638.134939	50.560756
3503.075650	482560.311366	50.565761
3502.741020	482476.611177	50.570765
3502.903632	482387.258594	50.575770
3502.921259	482284.146842	50.580775
3502.692870	482186.241584	50.585780
3502.658843	482055.117254	50.590785
3502.285929	481934.534058	50.595789
3501.817560	481796.636344	50.600794
3501.933986	481650.740773	50.605799
3501.793479	481503.820652	50.610804
3501.699124	481335.053203	50.615809
3500.953649	481180.524370	50.620813
3500.912208	480992.946731	50.625818
3501.126582	480804.921491	50.630823
3500.256649	480630.848680	50.635828
3500.022856	480420.949513	50.640833
3499.646333	480225.512550	50.645837
3499.049563	480010.801742	50.650842
3498.834598	479804.642887	50.655847
3498.418513	479594.510349	50.660852
3498.142376	479367.174476	50.665857
3497.786810	479137.466767	50.670861
3497.251101	478908.697044	50.675866
3497.341986	478654.740394	50.680871
3496.738363	478420.705331	50.685876
3496.440687	478167.817423	50.690881
3495.875038	477914.208466	50.695885
3495.261254	477650.670635	50.700890
3494.974540	477388.141914	50.705895
3494.661363	477119.532179	50.710900
3494.487368	476845.625919	50.715905
3493.503407	476562.923794	50.720909
3492.858482	476287.766590	50.725914
3492.889732	476005.250922	50.730919
3491.913601	475715.135745	50.735924
3491.914870	475410.365844	50.740929
3491.118129	475129.945499	50.745933
3490.804543	474825.926142	50.750938
3490.283925	474519.958116	50.755943
3489.700776	474222.713773	50.760948
3489.718826	473892.523395	50.765953
3488.933444	473581.007227	50.770957
3487.975172	473268.956016	50.775962
3487.836546	472944.655164	50.780967
3487.061013	472629.625169	50.785972
3486.565015	472288.287020	50.790977
3485.830351	471970.807143	50.795981
3485.627741	471640.361753	50.800986
3484.877460	471295.954899	50.805991
3484.408961	470968.633188	50.810996
3483.948268	470628.225125	50.816001
3483.061549	470292.593727	50.821005
3483.076933	469947.485670	50.826010
3482.531738	469597.238388	50.831015
3481.453701	469237.791182	50.836020
3481.186832	468890.884961	50.841025
3480.550232	468541.901906	50.846029
3479.955976	468178.100950	50.851034
3479.508599	467813.763410	50.856039
3478.253440	467466.584141	50.861044
3477.698638	467103.113231	50.866049
3476.824665	466750.791289	50.871053
3476.328890	466390.239745	50.876058
3476.029011	466032.034385	50.881063
3475.554951	465676.538094	50.886068
3474.517889	465312.047704	50.891073
3473.927723	464947.176153	50.896077
3473.162913	464585.723659	50.901082
3472.776197	464221.872483	50.906087
3472.188285	463862.459010	50.911092
3471.481322	463494.335419	50.916097
3470.931447	463114.617558	50.921101
3470.447765	462749.083106	50.926106
3469.974746	462371.825093	50.931111
3468.793031	462008.417115	50.936116
3468.520643	461625.687530	50.941121
3467.674748	461256.888362	50.946125
3467.109414	460877.235073	50.951130
3466.226996	460504.979916	50.956135
3465.166950	460142.586634	50.961140
3464.781848	459758.016020	50.966145
3464.102265	459395.296601	50.971149
3463.241616	459031.838932	50.976154
3462.720518	458661.727223	50.981159
3461.853870	458294.098801	50.986164
3461.418490	457925.026440	50.991169
3460.889387	457553.781419	50.996173
3460.080995	457183.284540	51.001178
3459.640638	456809.121468	51.006183
3458.705180	456444.618517	51.011188
3458.255089	456061.820180	51.016193
3457.462181	455691.296048	51.021197
3456.405031	455316.444479	51.026202
3456.005565	454945.490695	51.031207
3455.039003	454575.685879	51.036212
3454.491916	454208.041068	51.041217
3453.856107	453849.942815	51.046221
3452.916670	453474.483900	51.051226
3452.330751	453098.354025	51.056231
3451.420452	452748.958057	51.061236
3450.787862	452377.796094	51.066241
3450.218663	452011.134013	51.071245
3449.672870	451648.217241	51.076250
3448.661820	451276.995762	51.081255
3448.108494	450916.656478	51.086260
3447.503639	450548.403623	51.091265
3446.934187	450179.631843	51.096269
3446.282264	449814.419420	51.101274
3445.367757	449446.197958	51.106279
3444.116454	449095.734706	51.111284
3444.057066	448730.614553	51.116289
3443.574485	448368.093029	51.121293
3442.582067	448011.736434	51.126298
3441.891242	447651.774209	51.131303
3441.356994	447284.727292	51.136308
3440.458933	446918.848703	51.141313
3439.982476	446560.358442	51.146317
3439.134833	446201.566144	51.151322
3438.487816	445844.817616	51.156327
3437.805554	445487.104947	51.161332
3437.332134	445127.831204	51.166337
3436.573625	444767.429710	51.171341
3435.546717	444401.481892	51.176346
3434.922679	444038.408759	51.181351
3434.183978	443679.002896	51.186356
3433.556470	443322.467379	51.191361
3433.093277	442964.174752	51.196365
3432.042414	442615.614329	51.201370
3431.605707	442245.022648	51.206375
3430.753527	441907.131376	51.211380
3429.967082	441545.518520	51.216385
3429.258135	441195.462260	51.221389
3428.203544	440845.658678	51.226394
3427.950204	440494.403514	51.231399
3426.986666	440152.698119	51.236404
3426.379892	439795.802999	51.241409
3425.385908	439449.675909	51.246413
3424.976765	439110.711386	51.251418
3424.362508	438765.809267	51.256423
3423.523176	438421.826397	51.261428
3422.792559	438066.118959	51.266433
3422.046504	437726.858764	51.271437
3421.418134	437385.036748	51.276442
3420.668695	437050.921247	51.281447
3419.919262	436711.114673	51.286452
3419.208360	436371.728981	51.291457
3418.730336	436036.668512	51.296461
3417.770852	435695.282005	51.301466
3417.032195	435358.781245	51.306471
3416.492249	435025.900515	51.311476
3415.943838	434690.680992	51.316481
3415.263843	434351.923384	51.321485
3414.289496	434013.512476	51.326490
3413.589070	433682.340614	51.331495
3413.143401	433345.716110	51.336500
3412.341261	433016.963770	51.341505
3411.554691	432673.478159	51.346509
3410.809743	432352.274699	51.351514
3410.202717	432015.531326	51.356519
3409.232786	431686.940881	51.361524
3408.349345	431365.747050	51.366529
3407.902837	431030.438221	51.371533
3407.086919	430709.352558	51.376538
3406.389042	430397.157194	51.381543
3405.816957	430066.934404	51.386548
3404.767111	429745.086675	51.391553
3404.265887	429430.766416	51.396557
3403.738301	429105.196948	51.401562
3403.165439	428781.865327	51.406567
3402.060927	428472.098434	51.411572
3401.236177	428148.037035	51.416577
3400.849089	427825.781736	51.421581
3399.962873	427514.597781	51.426586
3399.329260	427200.551293	51.431591
3398.725488	426882.382188	51.436596
3398.128708	426566.265313	51.441601
3397.274231	426250.007671	51.446605
3396.443556	425934.987001	51.451610
3395.900963	425619.586925	51.456615
3395.090928	425332.721753	51.461620
3394.252697	425008.319664	51.466625
3393.973405	424695.330777	51.471629
3393.150330	424390.958201	51.476634
3392.381616	424064.273346	51.481639
3391.816830	423761.681615	51.486644
3391.082097	423453.677902	51.491649
3390.485496	423142.423103	51.496653
3389.511984	422832.824568	51.501658
3389.160576	422519.796731	51.506663
3388.378697	422218.162095	51.511668
3387.569283	421915.283867	51.516673
3387.036906	421604.712747	51.521677
3386.331782	421294.876699	51.526682
3385.592554	420997.540267	51.531687
3384.997317	420689.331208	51.536692
3384.154530	420383.342482	51.541697
3383.723748	420083.813735	51.546701
3382.810497	419772.748943	51.551706
3382.345965	419464.962973	51.556711
3381.270356	419162.300135	51.561716
3380.578346	418856.042275	51.566721
3379.913929	418553.485713	51.571725
3379.514900	418258.962511	51.576730
3378.894798	417954.995314	51.581735
3377.943446	417649.908618	51.586740
3377.584440	417356.055658	51.591745
3376.721221	417044.470251	51.596749
3375.470489	416755.731555	51.601754
3375.363242	416454.538114	51.606759
3374.431950	416160.814181	51.611764
3373.522882	415865.025817	51.616769
3373.079302	415566.645558	51.621773
3372.609681	415278.657763	51.626778
3371.974842	414976.236551	51.631783
3371.107501	414669.707538	51.636788
3370.528575	414374.842640	51.641793
3369.766400	414075.176222	51.646797
3368.792918	413781.002907	51.651802
3368.492649	413489.210219	51.656807
3367.643494	413198.771852	51.661812
3366.763659	412891.641771	51.666817
3366.372842	412606.257699	51.671821
3365.541698	412315.096313	51.676826
3364.693687	412021.698672	51.681831
3363.916177	411745.337073	51.686836
3363.298838	411447.450537	51.691841
3362.831408	411166.333637	51.696845
3361.692309	410893.832876	51.701850
3361.150701	410594.324974	51.706855
3360.252221	410306.686715	51.711860
3359.172791	410039.225570	51.716865
3359.213811	409754.177901	51.721869
3358.212830	409469.597244	51.726874
3357.898051	409191.639618	51.731879
3357.061824	408915.235811	51.736884
3356.282566	408632.136965	51.741889
3355.880337	408349.585775	51.746893
3355.090522	408073.649822	51.751898
3354.557656	407790.021344	51.756903
3353.976333	407516.004215	51.761908
3352.789801	407227.696148	51.766913
3352.159308	406951.114960	51.771917
3351.537663	406669.980745	51.776922
3350.869278	406390.172911	51.781927
3350.147314	406116.368883	51.786932
3349.432780	405842.688337	51.791937
3349.205841	405558.050601	51.796941
3348.097383	405289.256348	51.801946
3347.349306	405015.878820	51.806951
3346.812348	404746.099977	51.811956
3345.891363	404471.270917	51.816961
3345.226711	404197.237652	51.821965
3344.258276	403925.461270	51.826970
3343.877877	403653.513309	51.831975
3343.300684	403396.081755	51.836980
3342.647123	403115.378119	51.841985
3342.076225	402841.470774	51.846989
3341.133264	402574.101377	51.851994
3340.533137	402296.483003	51.856999
3339.784291	402038.254230	51.862004
3339.070696	401762.631764	51.867009
3338.425943	401500.213611	51.872013
3337.460143	401231.489432	51.877018
3337.174345	400967.866338	51.882023
3336.269230	400705.762490	51.887028
3335.596988	400437.010693	51.892033
3335.228617	400166.480094	51.897037
3334.267462	399917.927297	51.902042
3333.967724	399641.331602	51.907047
3333.199052	399376.577206	51.912052
3332.465183	399110.900033	51.917057
3331.824376	398843.833283	51.922061
3330.891543	398578.945878	51.927066
3330.655027	398308.912892	51.932071
3329.403877	398050.681005	51.937076
3328.691882	397782.854277	51.942081
3328.296919	397525.499748	51.947085
3327.616850	397263.637826	51.952090
3326.937933	396998.773878	51.957095
3326.254328	396739.755648	51.962100
3325.749219	396483.808701	51.967105
3325.002553	396216.127387	51.972109
3324.247605	395956.580506	51.977114
3323.442710	395686.183950	51.982119
3322.421366	395432.344456	51.987124
3321.557053	395177.461291	51.992129
3321.564713	394917.760397	51.997133
3320.690911	394673.476524	52.002138
3320.158065	394407.806376	52.007143
3319.513744	394156.923150	52.012148
3318.776463	393892.145731	52.017153
3318.229077	393641.573908	52.022157
3317.320916	393382.438366	52.027162
3316.765503	393123.829856	52.032167
3315.989114	392869.703722	52.037172
3315.219069	392615.447587	52.042177
3314.862629	392358.556213	52.047181
3313.790718	392109.454596	52.052186
3313.363366	391852.011325	52.057191
3312.812648	391594.534807	52.062196
3312.030011	391336.025170	52.067201
3311.294595	391088.083490	52.072205
3310.287800	390837.640326	52.077210
3309.922802	390576.694378	52.082215
3309.229514	390335.682201	52.087220
3308.422201	390072.285211	52.092225
3307.758609	389807.770159	52.097229
3306.876935	389568.638731	52.102234
3306.123744	389319.263495	52.107239
3305.381537	389080.411858	52.112244
3304.649106	388838.124307	52.117249
3304.426017	388595.246002	52.122253
3303.527270	388351.710056	52.127258
3303.160743	388087.440403	52.132263
3302.216910	387857.919306	52.137268
3301.303225	387611.151275	52.142273
3300.983171	387353.531232	52.147277
3300.014885	387115.617730	52.152282
3299.368334	386874.625701	52.157287
3298.827381	386630.894423	52.162292
3298.069804	386394.570366	52.167297
3297.561741	386143.328890	52.172301
3296.646120	385907.764145	52.177306
3296.262434	385653.117454	52.182311
3295.487860	385408.474070	52.187316
3294.251436	385170.844622	52.192321
3293.800217	384932.021379	52.197325
3293.190340	384696.146228	52.202330
3292.562142	384460.882818	52.207335
3291.943516	384226.277615	52.212340
3291.340499	383995.813763	52.217345
3290.990695	383747.964203	52.222349
3289.864174	383513.129665	52.227354
3289.175708	383271.332369	52.232359
3289.067142	383029.925011	52.237364
3288.170473	382796.066919	52.242369
3287.451933	382553.125325	52.247373
3286.576931	382312.979049	52.252378
3286.250296	382072.363038	52.257383
3285.448037	381834.414865	52.262388
3284.596145	381594.641886	52.267393
3284.017273	381345.973519	52.272397
3283.111808	381102.772465	52.277402
3282.430419	380878.736627	52.282407
3281.925389	380651.441535	52.287412
3281.283716	380413.967811	52.292417
3280.931801	380166.222398	52.297421
3279.874812	379925.326920	52.302426
3279.659657	379700.218582	52.307431
3278.964126	379461.653870	52.312436
3278.362849	379225.514499	52.317441
3277.832551	378974.025403	52.322445
3276.814227	378743.417521	52.327450
3276.207329	378489.928087	52.332455
3275.815530	378249.603812	52.337460
3274.691151	378011.759413	52.342465
3274.239110	377764.853987	52.347469
3273.472837	377537.556658	52.352474
3273.096363	377296.130439	52.357479
3272.100803	377049.408269	52.362484
3271.611105	376812.855277	52.367489
3270.763185	376571.651854	52.372493
3269.639944	376337.841616	52.377498
3269.373589	376101.961321	52.382503
3268.452244	375863.436086	52.387508
3267.237827	375633.324485	52.392513
3266.887017	375411.138480	52.397517
3266.433522	375175.333248	52.402522
3265.656665	374950.897338	52.407527
3264.832979	374714.715555	52.412532
3263.919884	374492.791529	52.417537
3263.714104	374259.231193	52.422541
3262.600824	374040.109076	52.427546
3262.244532	373815.524107	52.432551
3261.684289	373595.650767	52.437556
3260.989763	373365.215222	52.442561
3260.503024	373138.154262	52.447565
3259.496843	372908.961073	52.452570
3259.357383	372673.422521	52.457575
3258.588300	372449.912985	52.462580
3257.259707	372226.287238	52.467585
3257.239494	371992.532146	52.472589
3256.484974	371763.394624	52.477594
3255.650082	371531.673760	52.482599
3254.992291	371308.140541	52.487604
3254.252843	371082.075102	52.492609
3253.521890	370855.142164	52.497613
3252.825031	370620.748753	52.502618
3252.315548	370402.326149	52.507623
3251.742418	370183.123852	52.512628
3250.853255	369956.669076	52.517633
3250.077812	369725.844816	52.522637
3249.432905	369507.464510	52.527642
3248.898022	369282.730980	52.532647
3248.190978	369056.242660	52.537652
3247.505465	368838.170681	52.542657
3246.736281	368611.155605	52.547661
3246.375475	368396.032088	52.552666
3245.808303	368169.745993	52.557671
3244.909099	367945.953619	52.562676
3244.009099	367729.690919	52.567681
3243.839408	367494.561141	52.572685
3242.795872	367277.377578	52.577690
3242.131660	367047.284782	52.582695
3241.785118	366823.831800	52.587700
3240.880943	366605.096371	52.592705
3240.116402	366367.332380	52.597709
3239.502747	366149.668222	52.602714
3238.645961	365933.644341	52.607719
3238.351886	365716.563590	52.612724
3237.143019	365494.945011	52.617729
3236.494636	365273.745544	52.622733
3235.882779	365064.751879	52.627738
3235.391819	364839.225509	52.632743
3234.539099	364630.344267	52.637748
3234.265857	364410.124418	52.642753
3233.251740	364198.366172	52.647757
3232.671664	363977.225913	52.652762
3232.065833	363745.249609	52.657767
3231.228622	363536.895231	52.662772
3230.517109	363331.242536	52.667777
3229.937958	363105.568900	52.672781
3229.233847	362901.337991	52.677786
3228.314244	362681.517428	52.682791
3228.043831	362467.140034	52.687796
3226.867801	362247.688760	52.692801
3226.454515	362029.515264	52.697805
3225.293036	361829.066926	52.702810
3224.949860	361618.284871	52.707815
3224.209151	361415.274605	52.712820
3223.408570	361203.265346	52.717825
3223.070574	360994.744303	52.722829
3222.320183	360788.119644	52.727834
3221.577053	360593.223313	52.732839
3221.122474	360377.058904	52.737844
3220.389064	360166.815584	52.742849
3219.616362	359951.106700	52.747853
3218.790307	359758.179409	52.752858
3217.795986	359546.931359	52.757863
3217.184691	359337.250348	52.762868
3216.752599	359133.748971	52.767873
3216.371077	358928.101244	52.772877
3215.413415	358724.452268	52.777882
3214.842374	358525.118095	52.782887
3214.373145	358313.527142	52.787892
3213.522434	358115.100723	52.792897
3212.733665	357904.245611	52.797901
3212.038532	357699.202150	52.802906
3211.351182	357494.996359	52.807911
3210.768929	357296.905880	52.812916
3210.231722	357104.405895	52.817921
3209.852240	356890.657058	52.822925
3209.140095	356686.808124	52.827930
3208.329556	356474.907017	52.832935
3207.486115	356269.321260	52.837940
3206.715574	356076.981458	52.842945
3206.685789	355861.620586	52.847949
3205.542084	355661.678391	52.852954
3205.054593	355453.844462	52.857959
3204.218460	355239.117454	52.862964
3203.340732	355052.083945	52.867969
3202.904719	354831.896868	52.872973
3202.046886	354637.453184	52.877978
3201.457990	354433.728350	52.882983
3200.882468	354228.677255	52.887988
3200.040023	354029.240870	52.892993
3199.621004	353821.822102	52.897997
3198.838029	353629.475028	52.903002
3198.461374	353424.134788	52.908007
3197.714167	353215.467601	52.913012
3196.999107	353009.212184	52.918017
3196.616748	352800.536520	52.923021
3196.035801	352603.114701	52.928026
3195.441206	352391.671532	52.933031
3194.245221	352177.090528	52.938036
3193.674496	351986.917967	52.943041
3193.093096	351775.063043	52.948045
3192.409102	351579.206144	52.953050
3191.575222	351368.153039	52.958055
3191.035955	351155.576379	52.963060
3190.288226	350955.349827	52.968065
3189.639894	350752.180001	52.973069
3188.996071	350563.006495	52.978074
3188.195731	350347.235717	52.983079
3187.581057	350151.769850	52.988084
3186.905606	349942.391287	52.993089
3186.190132	349734.977971	52.998093
3185.271184	349534.264224	53.003098
3184.858339	349344.719071	53.008103
3184.056128	349141.923877	53.013108
3183.670132	348951.456875	53.018113
3182.968682	348743.019535	53.023117
3182.443529	348548.246418	53.028122
3181.551757	348343.629952	53.033127
3180.759880	348141.618451	53.038132
3179.808490	347947.852371	53.043137
3179.360443	347745.428718	53.048141
3178.644295	347552.362156	53.053146
3178.011332	347364.499435	53.058151
3177.629205	347166.313754	53.063156
3176.599421	346965.811877	53.068161
3176.347127	346765.873503	53.073165
3175.568059	346577.318616	53.078170
3174.638474	346368.246779	53.083175
3174.077047	346171.714949	53.088180
3173.200126	345969.301890	53.093185
3172.660734	345769.049108	53.098189
3171.892724	345585.859734	53.103194
3171.290631	345399.232841	53.108199
3170.685595	345197.512194	53.113204
3169.803883	345004.921363	53.118209
3169.423303	344810.748879	53.123213
3168.858362	344622.739145	53.128218
3167.755641	344430.664996	53.133223
3167.347244	344243.952854	53.138228
3166.594961	344040.775212	53.143233
3166.201105	343852.226878	53.148237
3165.406335	343661.705078	53.153242
3164.774634	343463.215302	53.158247
3164.250733	343268.576790	53.163252
3163.204272	343079.645628	53.168257
3162.777317	342876.921617	53.173261
3161.955401	342696.022635	53.178266
3161.121403	342496.848946	53.183271
3160.829631	342301.279678	53.188276
3159.796706	342113.336057	53.193281
3159.604211	341923.171632	53.198285
3158.750571	341734.231208	53.203290
3157.928580	341542.765192	53.208295
3157.427826	341344.018641	53.213300
3156.480068	341148.829462	53.218305
3155.851029	340960.894764	53.223309
3155.045064	340778.613012	53.228314
3154.703521	340582.155210	53.233319
3154.218865	340379.228397	53.238324
3152.920461	340201.248394	53.243329
3152.558007	339999.268306	53.248333
3152.130048	339826.520567	53.253338
3151.307204	339633.266925	53.258343
3150.713287	339440.103749	53.263348
3150.003139	339247.060194	53.268353
3148.955536	339063.207987	53.273357
3148.860377	338877.626312	53.278362
3148.009728	338681.752240	53.283367
3147.370153	338499.132093	53.288372
3146.660693	338312.016798	53.293377
3146.016546	338112.366305	53.298381
3145.317925	337924.611772	53.303386
3144.566236	337739.054314	53.308391
3143.724684	337548.368399	53.313396
3143.402606	337363.480128	53.318401
3142.584263	337175.487812	53.323405
3141.923456	336981.564153	53.328410
3140.979436	336794.150669	53.333415
3140.733226	336609.120987	53.338420
3139.766981	336436.474785	53.343425
3139.171211	336241.800423	53.348429
3138.957428	336051.800008	53.353434
3137.848172	335858.071296	53.358439
3137.145581	335675.147770	53.363444
3136.380514	335494.804782	53.368449
3136.006417	335311.191869	53.373453
3135.141171	335128.750820	53.378458
3134.505569	334930.133110	53.383463
3133.717644	334749.129866	53.388468
3132.863861	334582.774503	53.393473
3132.402060	334395.201656	53.398477
3131.811301	334213.809397	53.403482
3131.089230	334028.924302	53.408487
3130.621523	333850.311941	53.413492
3129.980784	333660.779718	53.418497
3129.502330	333475.752770	53.423501
3128.664499	333287.167190	53.428506
3128.141621	333100.084197	53.433511
3127.370815	332904.562451	53.438516
3126.680736	332729.902925	53.443521
3125.884065	332537.006422	53.448525
3125.262654	332356.072431	53.453530
3124.426430	332163.206628	53.458535
3124.081109	331987.777898	53.463540
3123.199972	331799.908033	53.468545
3122.765614	331611.814236	53.473549
3121.787797	331429.177664	53.478554
3121.594448	331244.863541	53.483559
3121.276009	331050.792654	53.488564
3119.862557	330869.827489	53.493569
3119.139271	330679.332959	53.498573
3119.038944	330497.242591	53.503578
3118.107136	330308.638580	53.508583
3117.329306	330125.126959	53.513588
3116.574067	329945.862952	53.518593
3116.263787	329752.067390	53.523597
3115.365065	329564.449151	53.528602
3114.688846	329379.621198	53.533607
3114.166525	329189.905732	53.538612
3113.112803	329013.920035	53.543617
3112.627277	328831.530111	53.548621
3112.171802	328649.644181	53.553626
3111.232140	328453.475297	53.558631
3110.674323	328272.164766	53.563636
3109.810419	328088.610876	53.568641
3109.301676	327899.170093	53.573645
3108.625025	327720.728542	53.578650
3107.860659	327544.031721	53.583655
3107.168363	327355.255143	53.588660
3106.182280	327182.818911	53.593665
3105.909036	326994.127912	53.598669
3105.257856	326825.049531	53.603674
3104.465516	326644.739784	53.608679
3104.091875	326463.141288	53.613684
3103.392459	326285.820311	53.618689
3102.816219	326091.497481	53.623693
3102.009153	325910.195445	53.628698
3101.035429	325736.124645	53.633703
3100.652796	325551.775782	53.638708
3099.826426	325366.325529	53.643713
3099.488696	325187.722791	53.648717
3098.831377	325000.259032	53.653722
3097.773268	324827.345355	53.658727
3096.997640	324648.276052	53.663732
3096.106157	324475.768098	53.668737
3095.646510	324292.116011	53.673741
3094.762517	324118.995067	53.678746
3094.259408	323957.067208	53.683751
3094.011200	323783.463049	53.688756
3093.199950	323605.441026	53.693761
3092.098105	323433.295188	53.698765
3091.709971	323253.550499	53.703770
3090.852023	323081.365350	53.708775
3090.311643	322911.624797	53.713780
3089.735323	322739.598080	53.718785
3089.357224	322559.162880	53.723789
3088.444089	322382.351092	53.728794
3087.563095	322207.290692	53.733799
3087.265662	322026.332381	53.738804
3086.696979	321860.413449	53.743809
3085.895228	321678.795832	53.748813
3085.290496	321499.412746	53.753818
3084.446283	321321.620349	53.758823
3084.165071	321152.039027	53.763828
3083.176699	320970.755017	53.768833
3082.488513	320792.376707	53.773837
3082.154792	320609.053268	53.778842
3081.016940	320430.465308	53.783847
3080.668615	320254.145483	53.788852
3079.526878	320081.464624	53.793857
3078.775940	319914.348713	53.798861
3078.594917	319739.885605	53.803866
3078.028003	319567.571125	53.808871
3077.287783	319386.753900	53.813876
3076.365585	319218.772638	53.818881
3076.242025	319029.123570	53.823885
3075.451754	318860.484222	53.828890
3074.193266	318683.210514	53.833895
3073.965269	318500.502671	53.838900
3072.983296	318337.392605	53.843905
3072.077168	318168.439329	53.848909
3071.682016	317993.141092	53.853914
3070.926693	317825.181843	53.858919
3070.517634	317654.570309	53.863924
3069.731833	317480.478766	53.868929
3069.038255	317305.353803	53.873933
3068.525012	317134.375888	53.878938
3067.703878	316964.668612	53.883943
3067.481217	316783.357092	53.888948
3066.376617	316620.161655	53.893953
3065.656110	316445.523199	53.898957
3065.358252	316272.880057	53.903962
3064.521569	316102.180687	53.908967
3064.101941	315928.079353	53.913972
3062.993005	315763.304470	53.918977
3062.674315	315596.392666	53.923981
3062.294313	315403.237651	53.928986
3060.973780	315242.645913	53.933991
3060.671492	315049.630704	53.938996
3059.632382	314888.790164	53.944001
3058.989160	314714.365631	53.949005
3058.733430	314549.784780	53.954010
3057.690520	314384.640721	53.959015
3057.453683	314202.155461	53.964020
3056.574318	314031.917708	53.969025
3055.862808	313858.240983	53.974029
3055.497936	313679.390911	53.979034
3054.528895	313522.764139	53.984039
3054.032884	313341.540655	53.989044
3053.070236	313160.747203	53.994049
3052.601085	312996.197687	53.999053
3052.057499	312823.409392	54.004058
3051.201227	312657.952993	54.009063
3050.715664	312474.791131	54.014068
3049.559557	312312.972078	54.019073
3049.402248	312139.866924	54.024077
3048.719761	311968.296063	54.029082
3047.715533	311795.731822	54.034087
3047.218876	311619.318286	54.039092
3046.232543	311458.107715	54.044097
3045.709901	311286.408647	54.049101
3045.447151	311114.871901	54.054106
3044.423386	310956.824108	54.059111
3044.013221	310776.703232	54.064116
3043.290056	310611.350038	54.069121
3042.817362	310440.889540	54.074125
3041.956328	310266.364999	54.079130
3041.015206	310097.225885	54.084135
3040.294661	309926.039916	54.089140
3039.920237	309759.229761	54.094145
3039.010711	309595.814455	54.099149
3038.526707	309417.307421	54.104154
3037.658558	309266.846632	54.109159
3037.422609	309097.594479	54.114164
3036.313654	308926.290276	54.119169
3035.719728	308754.267700	54.124173
3035.369287	308579.507071	54.129178
3034.578803	308424.220077	54.134183
3033.988909	308245.473411	54.139188
3033.265297	308084.674979	54.144193
3032.817626	307911.660399	54.149197
3032.493420	307744.432065	54.154202
3031.152183	307581.668057	54.159207
3030.975248	307401.174122	54.164212
3029.733457	307242.162770	54.169217
3029.280865	307058.350573	54.174221
3028.577920	306889.602201	54.179226
3028.058402	306719.602245	54.184231
3027.710270	306554.617063	54.189236
3026.984146	306387.603338	54.194241
3026.021626	306206.951926	54.199245
3025.311610	306031.302445	54.204250
3024.741494	305863.626724	54.209255
3024.182861	305691.161472	54.214260
3023.343734	305526.507355	54.219265
3022.784516	305358.090773	54.224269
3022.366505	305185.577145	54.229274
3021.451755	305013.269242	54.234279
3020.776578	304842.221949	54.239284
3019.794820	304680.085001	54.244289
3019.310044	304501.622117	54.249293
3018.729990	304329.515038	54.254298
3017.831586	304170.292854	54.259303
3017.582317	303993.574644	54.264308
3016.860477	303830.249609	54.269313
3016.139074	303661.856619	54.274317
3015.206009	303489.014940	54.279322
3014.318073	303328.465927	54.284327
3014.078696	303151.897900	54.289332
3013.289178	302986.545339	54.294337
3012.519193	302821.851615	54.299341
3012.061662	302651.938657	54.304346
3011.346314	302490.801152	54.309351
3010.751602	302308.201967	54.314356
3009.945944	302149.064737	54.319361
3009.300952	301985.318010	54.324365
3008.597702	301814.067818	54.329370
3008.022163	301654.740849	54.334375
3007.331886	301482.749712	54.339380
3006.522460	301318.646301	54.344385
3006.085193	301147.684327	54.349389
3005.173377	300986.245260	54.354394
3004.378887	300827.257687	54.359399
3003.928592	300660.295452	54.364404
3003.169708	300494.629733	54.369409
3002.576881	300335.074956	54.374413
3002.197894	300165.936275	54.379418
3001.350158	300001.964894	54.384423
3000.662179	299833.485967	54.389428
2999.851081	299672.615363	54.394433
2999.213799	299504.204474	54.399437
2999.147206	299333.054569	54.404442
2998.244899	299178.080691	54.409447
2997.622646	299007.705999	54.414452
2997.098694	298844.649958	54.419457
2996.461496	298659.124652	54.424461
2995.730069	298492.255653	54.429466
2995.026866	298329.252961	54.434471
2994.032933	298152.493179	54.439476
2993.399284	297988.078493	54.444481
2992.598170	297822.238555	54.449485
2992.435765	297651.993484	54.454490
2991.440259	297487.100807	54.459495
2991.113300	297315.429855	54.464500
2990.116946	297144.908834	54.469505
2989.687276	296982.702028	54.474509
2989.047505	296812.480796	54.479514
2988.172238	296638.705847	54.484519
2987.764069	296466.614025	54.489524
2987.064968	296311.962031	54.494529
2986.511428	296139.001577	54.499533
2986.030465	295961.292618	54.504538
2984.905603	295794.025027	54.509543
2984.511248	295618.033804	54.514548
2983.829590	295452.733136	54.519553
2983.065812	295278.302641	54.524557
2982.470771	295098.955600	54.529562
2981.540917	294936.775313	54.534567
2981.185669	294757.619220	54.539572
2980.298830	294601.467576	54.544577
2979.956611	294436.596231	54.549581
2979.477292	294246.992315	54.554586
2978.526567	294080.561637	54.559591
2977.868330	293901.249031	54.564596
2977.133689	293735.649769	54.569601
2976.220886	293569.747506	54.574605
2975.629351	293393.963879	54.579610
2975.209913	293225.793074	54.584615
2974.498187	293056.369573	54.589620
2973.568526	292885.172255	54.594625
2972.891404	292732.627908	54.599629
2972.376233	292553.928253	54.604634
2971.750290	292392.512918	54.609639
2971.002817	292224.367831	54.614644
2970.198153	292049.024383	54.619649
2969.582096	291878.948190	54.624653
2969.426495	291720.514047	54.629658
2968.711442	291549.256320	54.634663
2968.172467	291366.968622	54.639668
2967.372246	291191.853060	54.644673
2966.546483	291017.021563	54.649677
2965.939899	290841.442159	54.654682
2965.340196	290669.299674	54.659687
2964.735291	290501.894877	54.664692
2963.913177	290333.531117	54.669697
2963.229512	290159.491514	54.674701
2962.623909	289991.271540	54.679706
2961.378872	289827.533122	54.684711
2961.045614	289656.111837	54.689716
2960.458216	289488.041479	54.694721
2959.956547	289325.509418	54.699725
2959.719950	289142.433760	54.704730
2958.428619	288984.636165	54.709735
2957.950414	288811.760183	54.714740
2957.340785	288633.938681	54.719745
2956.782265	288470.014410	54.724749
2956.382078	288290.427740	54.729754
2955.371967	288120.411549	54.734759
2955.032926	287948.964710	54.739764
2954.164007	287782.338678	54.744769
2953.417358	287596.745096	54.749773
2953.031676	287421.026750	54.754778
2952.119295	287245.951977	54.759783
2951.281974	287070.534147	54.764788
2950.953144	286898.754054	54.769793
2950.154953	286722.005516	54.774797
2949.826139	286543.909189	54.779802
2948.892986	286375.153313	54.784807
2948.196048	286193.651437	54.789812
2947.646641	286024.809184	54.794817
2946.792736	285840.555967	54.799821
2946.504658	285655.550922	54.804826
2945.532419	285489.373099	54.809831
2944.918673	285313.486064	54.814836
2944.292920	285145.088461	54.819841
2943.323960	284969.563119	54.824845
2942.933841	284791.806753	54.829850
2941.842868	284621.674343	54.834855
2941.456691	284442.363651	54.839860
2941.081624	284274.562713	54.844865
2940.148401	284102.240335	54.849869
2939.519876	283925.489138	54.854874
2938.678985	283757.507063	54.859879
2938.196719	283579.586513	54.864884
2937.875643	283415.647870	54.869889
2936.942775	283241.567812	54.874893
2936.301114	283062.704512	54.879898
2935.708553	282886.915028	54.884903
2935.403363	282700.179601	54.889908
2934.864091	282529.933627	54.894913
2933.867560	282349.700038	54.899917
2933.019172	282159.765012	54.904922
2932.414094	281985.963735	54.909927
2931.557617	281817.117574	54.914932
2931.179426	281635.843549	54.919937
2930.200322	281473.332829	54.924941
2929.861714	281284.361021	54.929946
2929.294634	281119.136286	54.934951
2928.441650	280928.030063	54.939956
2927.792344	280748.861636	54.944961
2926.729375	280576.813365	54.949965
2926.613746	280398.248011	54.954970
2925.812344	280227.253387	54.959975
2925.333840	280050.018810	54.964980
2924.489982	279874.726687	54.969985
2923.809402	279698.899312	54.974989
2923.329902	279511.222766	54.979994
2922.446374	279345.054474	54.984999
2921.799294	279148.082973	54.990004
2920.998987	278979.889444	54.995009
2919.898258	278812.252813	55.000013
2919.959753	278633.582650	55.005018
2918.932901	278463.591181	55.010023
2918.486501	278290.655341	55.015028
2917.739291	278105.644159	55.020033
2917.097325	277924.894973	55.025037
2916.483928	277755.016233	55.030042
2915.314811	277592.203781	55.035047
2914.915598	277418.318030	55.040052
2914.444693	277240.979910	55.045057
2913.417763	277076.846011	55.050061
2913.096338	276901.598069	55.055066
2912.668431	276733.421711	55.060071
2911.851383	276553.540553	55.065076
2911.176833	276377.508017	55.070081
2910.331077	276203.361767	55.075085
2909.901953	276016.899255	55.080090
2908.968580	275849.592384	55.085095
2908.547257	275674.614864	55.090100
2908.106811	275498.392414	55.095105
2907.009321	275331.697283	55.100109
2906.648754	275135.826051	55.105114
2905.746083	274972.410963	55.110119
2905.435516	274788.934919	55.115124
2904.591502	274609.694675	55.120129
2903.852133	274426.795888	55.125133
2903.140079	274244.071058	55.130138
2902.725301	274073.065567	55.135143
2902.025118	273900.067794	55.140148
2901.600867	273722.645782	55.145153
2900.547248	273541.197539	55.150157
2900.045765	273358.031920	55.155162
2899.399374	273182.886326	55.160167
2898.555518	273004.104560	55.165172
2897.728416	272830.795858	55.170177
2897.088940	272664.079245	55.175181
2896.857228	272471.345819	55.180186
2895.614004	272297.084313	55.185191
2895.049983	272131.272668	55.190196
2894.593088	271961.802106	55.195201
2893.916369	271785.438973	55.200205
2893.493592	271606.463355	55.205210
2892.704508	271431.009453	55.210215
2892.281390	271249.410701	55.215220
2891.594465	271072.794605	55.220225
2890.656843	270881.930488	55.225229
2890.079955	270704.176426	55.230234
2889.325078	270538.624438	55.235239
2888.656133	270349.271458	55.240244
2888.186368	270179.828679	55.245249
2887.438390	270006.991757	55.250253
2886.738225	269826.557745	55.255258
2886.098361	269649.195891	55.260263
2885.398202	269466.877306	55.265268
2884.870644	269281.780862	55.270273
2884.294790	269118.874990	55.275277
2883.791467	268929.801748	55.280282
2883.065680	268756.121148	55.285287
2882.145043	268574.881899	55.290292
2881.472674	268395.819134	55.295297
2881.054294	268220.332699	55.300301
2880.434116	268039.631805	55.305306
2879.653381	267862.369130	55.310311
2879.017157	267672.629665	55.315316
2878.293551	267495.689146	55.320321
2877.475853	267320.317142	55.325325
2877.105549	267125.518526	55.330330
2876.365654	266950.618222	55.335335
2875.850990	266763.050097	55.340340
2875.180659	266579.072233	55.345345
2874.400442	266414.926070	55.350349
2873.943080	266226.788778	55.355354
2873.142633	266037.916368	55.360359
2872.726631	265851.326236	55.365364
2871.957824	265670.547836	55.370369
2871.119340	265489.602265	55.375373
2870.735607	265298.193784	55.380378
2869.925920	265118.950173	55.385383
2869.088557	264947.657063	55.390388
2868.668167	264750.116828	55.395393
2867.627471	264571.572203	55.400397
2867.011094	264388.376227	55.405402
2866.831525	264207.403302	55.410407
2865.992793	264022.485411	55.415412
2865.140779	263830.005716	55.420417
2864.269864	263652.326021	55.425421
2863.694994	263467.952395	55.430426
2862.859980	263293.170543	55.435431
2862.383234	263114.970282	55.440436
2861.721783	262927.732769	55.445441
2860.671019	262748.171911	55.450445
2860.384572	262572.437660	55.455450
2859.463186	262402.050422	55.460455
2859.071659	262218.743562	55.465460
2858.338882	262038.903533	55.470465
2857.755884	261856.824187	55.475469
2857.334772	261673.038437	55.480474
2856.537268	261499.397653	55.485479
2856.067608	261317.428019	55.490484
2855.456430	261136.525082	55.495489
2854.573072	260941.938214	55.500493
2854.205829	260764.664243	55.505498
2853.581137	260587.889563	55.510503
2852.892329	260393.093987	55.515508
2852.029655	260208.105679	55.520513
2851.427949	260027.991440	55.525517
2850.895239	259839.003640	55.530522
2850.097313	259645.932204	55.535527
2849.234185	259457.888357	55.540532
2848.852906	259276.109790	55.545537
2848.087285	259088.865732	55.550541
2847.684011	258898.253650	55.555546
2846.600682	258724.175976	55.560551
2846.282413	258532.532005	55.565556
2845.909235	258342.272123	55.570561
2844.968001	258159.971797	55.575565
2844.303511	257964.282817	55.580570
2843.679712	257778.061456	55.585575
2842.720571	257584.533243	55.590580
2842.383950	257395.541692	55.595585
2841.472410	257216.751892	55.600589
2840.811598	257023.075037	55.605594
2840.118308	256840.227124	55.610599
2839.280691	256658.955720	55.615604
2839.124335	256466.192693	55.620609
2838.432270	256289.686401	55.625613
2837.702728	256086.903942	55.630618
2836.964357	255905.057163	55.635623
2836.302270	255716.500573	55.640628
2835.634853	255525.958552	55.645633
2835.026145	255328.276590	55.650637
2834.651569	255145.863515	55.655642
2833.412428	254957.602718	55.660647
2832.977133	254770.921108	55.665652
2832.173690	254575.078872	55.670657
2831.453452	254399.164376	55.675661
2830.972460	254197.414022	55.680666
2830.391233	254028.608620	55.685671
2829.477599	253840.552004	55.690676
2828.857968	253652.550883	55.695681
2828.137256	253465.431830	55.700685
2827.757633	253268.683382	55.705690
2826.859405	253086.889933	55.710695
2825.849668	252901.650822	55.715700
2825.639573	252716.107007	55.720705
2824.945525	252533.925233	55.725709
2824.503278	252342.102781	55.730714
2823.599638	252156.592955	55.735719
2822.825558	251981.173108	55.740724
2822.411447	251787.003852	55.745729
2821.711743	251593.287501	55.750733
2820.975024	251404.696026	55.755738
2820.620501	251235.398887	55.760743
2819.565909	251035.780158	55.765748
2818.795488	250844.164106	55.770753
2818.230035	250660.996178	55.775757
2817.645420	250472.890976	55.780762
2816.984229	250295.112046	55.785767
2816.324042	250101.976862	55.790772
2815.672034	249923.509283	55.795777
2814.878332	249727.568906	55.800781
2814.590970	249539.595964	55.805786
2813.875355	249362.514260	55.810791
2813.041927	249171.419459	55.815796
2812.294537	248980.209398	55.820801
2811.489650	248798.736790	55.825805
2811.100057	248608.387310	55.830810
2810.837788	248422.678216	55.835815
2809.914575	248232.388233	55.840820
2809.281089	248041.645149	55.845825
2808.332476	247855.255979	55.850829
2807.897252	247657.937190	55.855834
2807.209592	247469.393490	55.860839
2806.067225	247292.228947	55.865844
2805.559357	247107.477139	55.870849
2804.768947	246922.388316	55.875853
2804.613380	246731.061909	55.880858
2803.973704	246543.454038	55.885863
2803.059717	246361.288612	55.890868
2802.411710	246173.733476	55.895873
2801.778362	245994.172523	55.900877
2801.184077	245790.031159	55.905882
2800.359342	245609.813429	55.910887
2799.841123	245422.544329	55.915892
2799.640387	245235.505328	55.920897
2798.634717	245048.874172	55.925901
2797.963872	244858.217616	55.930906
2797.497191	244668.369360	55.935911
2796.856280	244473.888773	55.940916
2795.855106	244276.078612	55.945921
2795.129275	244095.159655	55.950925
2794.716490	243904.820103	55.955930
2793.958346	243713.109458	55.960935
2793.186550	243528.251428	55.965940
2792.626218	243333.759758	55.970945
2791.777020	243148.558013	55.975949
2791.275828	242957.571750	55.980954
2790.626883	242773.433838	55.985959
2789.840320	242589.598103	55.990964
2789.098356	242397.326623	55.995969
2788.502871	242217.128147	56.000973
2787.932911	242027.198248	56.005978
2787.170177	241835.593013	56.010983
2786.559453	241643.276449	56.015988
2785.864151	241454.564133	56.020993
2785.203632	241280.463435	56.025997
2784.745865	241089.778736	56.031002
2784.254711	240893.701090	56.036007
2783.224016	240708.709981	56.041012
2782.424781	240522.765773	56.046017
2781.753941	240341.690741	56.051021
2781.559731	240153.639588	56.056026
2780.820924	239967.992260	56.061031
2779.888122	239781.280973	56.066036
2779.518831	239586.153850	56.071041
2778.537452	239411.419171	56.076045
2778.206782	239209.360234	56.081050
2777.473456	239017.958603	56.086055
2776.423589	238835.061585	56.091060
2776.071947	238637.743351	56.096065
2775.405723	238469.861033	56.101069
2774.697564	238275.579214	56.106074
2774.242883	238084.695253	56.111079
2773.239470	237896.241223	56.116084
2772.508039	237698.246338	56.121089
2771.915727	237522.816381	56.126093
2771.492705	237332.412527	56.131098
2771.051028	237145.118563	56.136103
2770.099685	236952.660075	56.141108
2769.542632	236755.275890	56.146113
2768.545855	236576.957715	56.151117
2768.121345	236383.169088	56.156122
2767.471029	236198.176099	56.161127
2766.968499	236016.317525	56.166132
2766.492209	235815.459238	56.171137
2765.557169	235626.030750	56.176141
2764.544453	235432.922696	56.181146
2764.062227	235257.428116	56.186151
2763.453548	235059.698805	56.191156
2763.090762	234866.132393	56.196161
2762.229952	234685.656997	56.201165
2761.617022	234483.065977	56.206170
2761.084671	234298.006784	56.211175
2759.998735	234110.871233	56.216180
2759.612192	233909.926084	56.221185
2758.950738	233730.566672	56.226189
2758.200306	233530.061869	56.231194
2757.643897	233353.181884	56.236199
2756.957740	233162.216282	56.241204
2756.253410	232962.316448	56.246209
2755.387345	232782.965708	56.251213
2755.115001	232588.880148	56.256218
2754.496483	232400.477075	56.261223
2753.667107	232208.950390	56.266228
2752.880511	232012.986810	56.271233
2752.421570	231818.015707	56.276237
2751.817807	231634.322393	56.281242
2751.128650	231449.217061	56.286247
2750.538752	231255.846535	56.291252
2750.302845	231043.680015	56.296257
2749.080422	230863.523619	56.301261
2748.594219	230666.496778	56.306266
2747.849359	230467.092410	56.311271
2747.125344	230277.615427	56.316276
2746.553816	230079.712181	56.321281
2745.696344	229893.745445	56.326285
2745.257574	229696.560406	56.331290
2744.461817	229505.135820	56.336295
2743.597369	229317.185342	56.341300
2743.116331	229116.774605	56.346305
2742.202293	228936.063953	56.351309
2741.636599	228734.394394	56.356314
2741.463095	228548.449432	56.361319
2740.506308	228360.846606	56.366324
2739.914303	228155.668832	56.371329
2738.935531	227968.070330	56.376333
2738.367917	227780.025190	56.381338
2737.637862	227587.219439	56.386343
2736.900419	227401.213473	56.391348
2736.701038	227205.447391	56.396353
2736.109187	227020.819562	56.401357
2734.998643	226825.427818	56.406362
2734.465652	226634.629896	56.411367
2733.822800	226439.266810	56.416372
2733.396905	226252.208299	56.421377
2732.395585	226065.534145	56.426381
2731.718911	225866.103997	56.431386
2731.083024	225682.848233	56.436391
2730.185113	225491.054090	56.441396
2730.221341	225294.835032	56.446401
2729.368623	225104.371319	56.451405
2728.889656	224905.956061	56.456410
2728.106221	224710.504742	56.461415
2727.410133	224510.979110	56.466420
2726.853385	224314.741755	56.471425
2725.805716	224121.676068	56.476429
2724.985159	223917.741516	56.481434
2724.778185	223740.443545	56.486439
2724.013813	223547.588973	56.491444
2723.488033	223345.951528	56.496449
2722.526683	223153.549206	56.501453
2721.782374	222967.414323	56.506458
2721.323138	222776.881080	56.511463
2720.655216	222576.872094	56.516468
2719.987687	222388.218631	56.521473
2719.288038	222192.912990	56.526477
2718.509369	221997.887685	56.531482
2717.978407	221814.204085	56.536487
2717.055120	221633.358156	56.541492
2716.736067	221436.670252	56.546497
2715.798223	221242.690458	56.551501
2715.372424	221049.317457	56.556506
2714.815005	220852.936140	56.561511
2714.447399	220667.587304	56.566516
2713.290918	220473.593195	56.571521
2712.857115	220279.790629	56.576525
2712.567302	220083.458042	56.581530
2711.665371	219877.866761	56.586535
2710.578606	219688.929985	56.591540
2710.361169	219479.132507	56.596545
2709.666542	219297.059422	56.601549
2708.848469	219089.547648	56.606554
2708.223394	218896.402741	56.611559
2707.733288	218707.475818	56.616564
2706.893970	218502.629499	56.621569
2705.994524	218312.202748	56.626573
2705.311437	218110.171409	56.631578
2704.899100	217921.616096	56.636583
2703.988297	217734.591355	56.641588
2703.312713	217540.070609	56.646593
2702.850534	217353.497697	56.651597
2702.025774	217161.852921	56.656602
2701.479513	216966.905933	56.661607
2700.763923	216777.077881	56.666612
2700.139131	216584.206481	56.671617
2699.901411	216393.870988	56.676621
2699.116915	216188.398945	56.681626
2698.359298	215985.583569	56.686631
2697.466621	215793.176844	56.691636
2696.742090	215590.535588	56.696641
2696.220824	215406.790281	56.701645
2695.474469	215207.055753	56.706650
2694.725157	215012.439178	56.711655
2694.267672	214829.499950	56.716660
2693.714931	214635.006060	56.721665
2692.819218	214444.742005	56.726669
2692.172645	214236.542799	56.731674
2691.726918	214042.721001	56.736679
2690.839807	213874.019159	56.741684
2689.870642	213673.140716	56.746689
2689.722626	213473.902041	56.751693
2688.964809	213287.832505	56.756698
2688.347017	213092.004201	56.761703
2687.675747	212900.525269	56.766708
2686.869325	212699.496719	56.771713
2686.128520	212497.109209	56.776717
2685.638291	212300.359360	56.781722
2684.979703	212105.405974	56.786727
2684.115598	211917.638875	56.791732
2683.650605	211726.665285	56.796737
2683.174561	211534.841239	56.801741
2682.226325	211335.035800	56.806746
2681.542545	211132.401689	56.811751
2680.914671	210950.658451	56.816756
2680.643133	210749.423952	56.821761
2679.601360	210560.645288	56.826765
2678.890874	210375.874847	56.831770
2678.187441	210167.226717	56.836775
2677.664062	209979.284063	56.841780
2677.016271	209789.414357	56.846785
2676.397897	209593.316792	56.851789
2675.627754	209399.038465	56.856794
2675.161417	209203.248957	56.861799
2674.293735	209007.192731	56.866804
2673.860219	208810.075612	56.871809
2672.954673	208633.066753	56.876813
2672.413829	208428.891445	56.881818
2671.902454	208234.117602	56.886823
2671.101857	208033.866577	56.891828
2670.557246	207834.784740	56.896833
2669.870229	207647.855087	56.901837
2669.252081	207442.053524	56.906842
2668.472158	207248.216276	56.911847
2667.907288	207056.598267	56.916852
2667.565683	206857.894750	56.921857
2666.690704	206656.018289	56.926861
2665.942894	206459.429481	56.931866
2665.490178	206254.382121	56.936871
2665.036873	206054.629915	56.941876
2664.421753	205848.057015	56.946881
2663.380855	205650.639169	56.951885
2662.863434	205452.528177	56.956890
2662.272118	205243.840995	56.961895
2661.309517	205049.734418	56.966900
2660.909125	204845.879970	56.971905
2660.097278	204647.716533	56.976909
2659.203054	204449.325020	56.981914
2658.905872	204244.947270	56.986919
2657.960383	204046.323460	56.991924
2657.461350	203850.556663	56.996929
2656.389393	203657.566544	57.001933
2655.777658	203455.366722	57.006938
2655.239999	203255.930193	57.011943
2654.581736	203061.400312	57.016948
2654.277664	202861.202771	57.021953
2653.373081	202669.780249	57.026957
2652.904497	202478.811071	57.031962
2652.564717	202266.747912	57.036967
2651.478714	202071.232949	57.041972
2650.687211	201864.345974	57.046977
2649.923610	201670.486606	57.051981
2649.369084	201477.803741	57.056986
2648.647478	201271.226040	57.061991
2648.122379	201076.694672	57.066996
2647.611900	200878.865726	57.072001
2646.654992	200692.663075	57.077005
2645.913479	200486.116919	57.082010
2645.305389	200281.001112	57.087015
2644.609260	200091.157869	57.092020
2643.920401	199900.359727	57.097025
2643.574724	199708.591658	57.102029
2642.800932	199503.861341	57.107034
2642.410204	199293.650136	57.112039
2641.247326	199102.293639	57.117044
2641.094437	198901.806547	57.122049
2640.166165	198704.344379	57.127053
2639.334614	198504.857051	57.132058
2638.798020	198300.170091	57.137063
2638.012635	198109.915318	57.142068
2637.586023	197905.097928	57.147073
2636.860118	197714.580650	57.152077
2636.143832	197523.948012	57.157082
2635.643655	197314.372741	57.162087
2634.441056	197121.731735	57.167092
2634.149575	196925.180571	57.172097
2633.416989	196734.769701	57.177101
2632.561178	196536.935139	57.182106
2632.142632	196335.011086	57.187111
2631.276067	196147.830183	57.192116
2630.698751	195946.479952	57.197121
2630.246461	195752.974399	57.202125
2629.183379	195562.009424	57.207130
2628.840262	195363.932705	57.212135
2628.125903	195166.691749	57.217140
2627.737405	194965.760794	57.222145
2627.257901	194768.904065	57.227149
2626.066984	194563.724703	57.232154
2625.729167	194367.686873	57.237159
2624.976289	194169.158029	57.242164
2624.183768	193967.251664	57.247169
2623.585759	193777.212177	57.252173
2622.900202	193582.873878	57.257178
2622.426867	193373.564918	57.262183
2621.470379	193185.798416	57.267188
2621.020431	192973.102898	57.272193
2620.519216	192776.524599	57.277197
2619.664359	192583.680239	57.282202
2619.392266	192372.905829	57.287207
2618.553481	192172.057394	57.292212
2617.827064	191966.178921	57.297217
2616.968370	191777.295324	57.302221
2616.389595	191571.369668	57.307226
2615.837846	191379.779785	57.312231
2615.257036	191168.779540	57.317236
2614.518407	190961.965706	57.322241
2613.976624	190764.714831	57.327245
2613.137038	190573.937117	57.332250
2612.607626	190373.657774	57.337255
2612.054374	190162.390358	57.342260
2611.228982	189952.642851	57.347265
2610.435341	189762.637171	57.352269
2609.616672	189558.424786	57.357274
2609.046907	189355.242552	57.362279
2608.362743	189163.962351	57.367284
2607.700315	188959.855004	57.372289
2607.039917	188761.473398	57.377293
2606.398049	188563.916656	57.382298
2605.864205	188364.753309	57.387303
2605.078010	188176.088662	57.392308
2604.277530	187965.735303	57.397313
2603.472559	187776.642675	57.402317
2602.889996	187585.365500	57.407322
2602.533152	187381.229302	57.412327
2601.510131	187189.005760	57.417332
2601.065081	186987.874983	57.422337
2600.177371	186796.674843	57.427341
2599.441910	186595.897112	57.432346
2599.219944	186401.603442	57.437351
2597.954850	186208.137410	57.442356
2597.730365	186005.105841	57.447361
2597.098513	185812.558893	57.452365
2596.217372	185626.527639	57.457370
2595.992356	185419.911207	57.462375
2595.154765	185227.577429	57.467380
2594.678149	185025.328020	57.472385
2594.050990	184830.723577	57.477389
2593.003748	184631.352362	57.482394
2592.787150	184437.117092	57.487399
2591.782401	184239.954406	57.492404
2591.218088	184042.481094	57.497409
2590.326839	183836.664410	57.502413
2589.905553	183643.571754	57.507418
2589.800960	183439.171523	57.512423
2588.662563	183240.431551	57.517428
2588.266643	183036.550009	57.522433
2587.478141	182830.848901	57.527437
2586.587842	182631.805205	57.532442
2585.947920	182427.723431	57.537447
2585.195615	182231.890775	57.542452
2584.622919	182025.192448	57.547457
2583.783418	181829.604376	57.552461
2583.342313	181630.786611	57.557466
2583.111261	181432.114555	57.562471
2581.876650	181232.928232	57.567476
2581.475391	181032.783945	57.572481
2580.691814	180835.397886	57.577485
2580.010578	180629.283071	57.582490
2579.775259	180430.183782	57.587495
2578.702203	180226.168223	57.592500
2578.200466	180009.978944	57.597505
2577.309605	179821.951125	57.602509
2576.400974	179625.061070	57.607514
2576.044820	179414.384949	57.612519
2575.343128	179219.842609	57.617524
2574.795843	179020.570339	57.622529
2573.999720	178819.659418	57.627533
2573.456956	178621.711163	57.632538
2572.825552	178417.405314	57.637543
2572.442147	178219.153858	57.642548
2571.513740	178010.216220	57.647553
2571.118228	177813.991001	57.652557
2570.208596	177607.392781	57.657562
2569.882563	177394.445168	57.662567
2568.716036	177207.235814	57.667572
2567.683456	176992.290803	57.672577
2567.396266	176791.461568	57.677581
2566.606973	176588.448860	57.682586
2566.152907	176395.572005	57.687591
2565.375127	176199.618467	57.692596
2564.964215	175996.625019	57.697601
2564.461328	175792.960326	57.702605
2563.342018	175600.853985	57.707610
2563.039332	175392.758837	57.712615
2562.598189	175198.537353	57.717620
2561.612570	174988.504768	57.722625
2560.839045	174776.735368	57.727629
2560.215072	174580.752479	57.732634
2559.463096	174371.512759	57.737639
2558.818219	174175.191744	57.742644
2558.412040	173968.837256	57.747649
2557.620198	173767.276127	57.752653
2556.512082	173577.148909	57.757658
2556.299418	173367.689031	57.762663
2555.536907	173173.197514	57.767668
2554.576774	172978.013332	57.772673
2554.079024	172779.831705	57.777677
2553.284893	172586.810616	57.782682
2552.741129	172383.640123	57.787687
2551.716327	172187.274588	57.792692
2551.528218	171985.207090	57.797697
2550.898156	171786.606263	57.802701
2550.179224	171593.323741	57.807706
2549.718551	171398.017311	57.812711
2549.063334	171200.504410	57.817716
2548.504391	170993.998782	57.822721
2547.534967	170790.382530	57.827725
2546.940696	170594.096605	57.832730
2546.282241	170382.052542	57.837735
2545.593568	170200.103095	57.842740
2544.920231	169990.530643	57.847745
2544.469969	169784.510158	57.852749
2543.632250	169587.949964	57.857754
2543.219150	169389.670290	57.862759
2542.642715	169187.742368	57.867764
2542.096883	168982.771360	57.872769
2541.140235	168776.836499	57.877773
2540.862496	168581.286332	57.882778
2540.332287	168360.191555	57.887783
2539.421567	168154.379928	57.892788
2538.636524	167942.102297	57.897793
2538.054233	167733.392431	57.902797
2536.935831	167529.638985	57.907802
2536.570827	167325.703661	57.912807
2535.834784	167125.223431	57.917812
2535.443728	166916.195289	57.922817
2534.653973	166708.592096	57.927821
2533.863012	166516.007698	57.932826
2533.253990	166304.525181	57.937831
2532.282900	166102.383728	57.942836
2531.809500	165893.844805	57.947841
2531.055042	165691.811115	57.952845
2530.423505	165493.751718	57.957850
2530.284896	165289.588125	57.962855
2529.286338	165090.813395	57.967860
2528.616039	164881.192393	57.972865
2527.863226	164676.074141	57.977869
2527.049985	164470.241839	57.982874
2526.474153	164265.657289	57.987879
2525.711428	164066.164084	57.992884
2525.008758	163883.026628	57.997889
2524.776783	163610.683996	58.002893
2523.913211	163398.915106	58.007898
2523.328297	163186.149677	58.012903
2522.593015	162992.188892	58.017908
2521.955842	162786.427153	58.022913
2521.400897	162586.019081	58.027917
2520.634875	162389.065759	58.032922
2520.168854	162169.434349	58.037927
2519.168951	161974.719940	58.042932
2518.179316	161775.758396	58.047937
2518.017028	161564.829936	58.052941
2517.116542	161376.434669	58.057946
2516.276214	161170.968620	58.062951
2515.650640	160970.288307	58.067956
2515.399245	160771.355194	58.072961
2514.713695	160571.169757	58.077965
2514.272110	160371.048492	58.082970
2513.478057	160146.345114	58.087975
2512.559743	159955.519156	58.092980
2511.985694	159757.774359	58.097985
2511.892814	159547.151960	58.102989
2510.709442	159338.674216	58.107994
2510.231158	159131.420859	58.112999
2509.285086	158937.502761	58.118004
2508.920022	158734.454595	58.123009
2507.989319	158527.937587	58.128013
2507.209025	158328.275700	58.133018
2506.814607	158108.836035	58.138023
2506.116700	157913.651130	58.143028
2505.140696	157723.087999	58.148033
2504.597790	157507.718326	58.153037
2503.801777	157306.806235	58.158042
2503.378023	157104.221816	58.163047
2502.593521	156900.945721	58.168052
2501.842108	156718.463099	58.173057
2501.509907	156507.719010	58.178061
2500.745941	156297.197189	58.183066
2500.051910	156092.436911	58.188071
2499.379980	155899.382214	58.193076
2498.471738	155700.378687	58.198081
2498.148494	155490.516565	58.203085
2497.289754	155290.579609	58.208090
2496.761090	155088.214405	58.213095
2496.000327	154888.582081	58.218100
2495.506950	154686.734860	58.223105
2494.827845	154485.769954	58.228109
2493.774365	154292.250971	58.233114
2493.627285	154082.217103	58.238119
2492.780692	153892.798842	58.243124
2492.270382	153683.371620	58.248129
2491.658988	153478.372515	58.253133
2490.713087	153270.631233	58.258138
2490.522719	153057.165920	58.263143
2489.499133	152858.578758	58.268148
2489.131370	152657.232258	58.273153
2488.209121	152443.810604	58.278157
2487.309905	152248.842665	58.283162
2486.628988	152051.960094	58.288167
2485.898864	151846.176368	58.293172
2485.372769	151656.325990	58.298177
2484.845700	151445.364819	58.303181
2483.959594	151246.892633	58.308186
2483.561351	151051.598151	58.313191
2482.893335	150847.755490	58.318196
2482.232085	150652.492358	58.323201
2481.724243	150438.153714	58.328205
2480.727127	150237.862274	58.333210
2480.448675	150043.063218	58.338215
2479.290744	149836.076205	58.343220
2478.861345	149634.681707	58.348225
2478.261319	149430.150799	58.353229
2477.426272	149230.322844	58.358234
2477.128162	149024.539234	58.363239
2476.345039	148821.350271	58.368244
2475.644449	148622.381714	58.373249
2475.103412	148414.467201	58.378253
2474.284893	148212.850925	58.383258
2473.612996	148002.430695	58.388263
2472.802007	147803.853269	58.393268
2472.020776	147613.533166	58.398273
2471.292400	147400.863653	58.403277
2470.660783	147198.461614	58.408282
2470.437026	146991.116079	58.413287
2469.394283	146797.995550	58.418292
2468.525705	146598.252864	58.423297
2468.200583	146398.933636	58.428301
2467.414633	146212.676661	58.433306
2466.649787	146003.237509	58.438311
2465.988807	145801.446334	58.443316
2465.528483	145611.862576	58.448321
2465.190365	145411.547700	58.453325
2464.350031	145212.355759	58.458330
2463.600516	145006.072394	58.463335
2462.984068	144807.737091	58.468340
2462.127362	144607.026661	58.473345
2461.542562	144411.573510	58.478349
2460.663080	144227.821135	58.483354
2460.350218	144010.597460	58.488359
2459.672514	143810.994754	58.493364
2459.301016	143608.587309	58.498369
2458.296812	143404.286440	58.503373
2457.729395	143205.114911	58.508378
2456.960797	142999.584901	58.513383
2456.249015	142804.594052	58.518388
2455.747071	142605.365192	58.523393
2455.278547	142398.165150	58.528397
2454.204627	142202.307927	58.533402
2453.559013	141999.941794	58.538407
2452.897390	141797.998853	58.543412
2452.432268	141603.230678	58.548417
2452.070164	141392.907485	58.553421
2451.122572	141198.917222	58.558426
2450.560322	140992.605599	58.563431
2449.723687	140792.374292	58.568436
2448.983068	140582.180239	58.573441
2448.609598	140383.453770	58.578445
2447.341523	140183.256764	58.583450
2446.963598	139986.896906	58.588455
2446.618106	139786.569000	58.593460
2445.720260	139585.656582	58.598465
2444.963471	139373.656612	58.603469
2444.193162	139179.015950	58.608474
2443.754129	138983.676067	58.613479
2442.833835	138784.818146	58.618484
2441.713464	138578.598828	58.623489
2441.687806	138386.767489	58.628493
2441.060382	138201.499645	58.633498
2440.572173	137998.512863	58.638503
2439.790116	137796.628553	58.643508
2439.054116	137601.497269	58.648513
2438.624535	137393.753740	58.653517
2437.651699	137196.159846	58.658522
2437.214958	136998.647454	58.663527
2436.398791	136800.180175	58.668532
2435.807118	136599.684063	58.673537
2435.479909	136391.791619	58.678541
2434.943375	136198.086296	58.683546
2434.082607	135986.304894	58.688551
2433.452703	135784.791382	58.693556
2432.503979	135582.097519	58.698561
2431.960507	135375.720231	58.703565
2431.207669	135170.432005	58.708570
2430.725491	134976.573727	58.713575
2429.500825	134780.535094	58.718580
2429.069043	134574.310939	58.723585
2428.884260	134377.093915	58.728589
2427.913853	134174.070327	58.733594
2427.288559	133966.255159	58.738599
2426.552165	133779.381157	58.743604
2425.616651	133567.426009	58.748609
2425.217016	133368.344486	58.753613
2424.185378	133173.467555	58.758618
2423.795526	132973.370992	58.763623
2423.150178	132784.062806	58.768628
2422.274593	132587.348643	58.773633
2421.880646	132381.553401	58.778637
2421.087539	132194.736835	58.783642
2420.594635	131994.625360	58.788647
2419.914641	131802.648990	58.793652
2419.285679	131600.465987	58.798657
2418.792654	131404.944169	58.803661
2417.913872	131196.820971	58.808666
2417.378097	130988.937075	58.813671
2416.718820	130795.706762	58.818676
2415.920972	130599.197296	58.823681
2415.321554	130393.055316	58.828685
2414.881736	130192.833863	58.833690
2413.864644	129986.100603	58.838695
2413.144913	129786.663107	58.843700
2412.607415	129593.345553	58.848705
2411.904759	129386.236645	58.853709
2411.218381	129197.746473	58.858714
2410.859300	128984.349852	58.863719
2410.105511	128789.509936	58.868724
2409.362774	128592.358088	58.873729
2409.063965	128388.621798	58.878733
2408.406017	128182.797535	58.883738
2407.900839	127975.667830	58.888743
2406.970224	127772.214044	58.893748
2406.117599	127567.250754	58.898753
2405.997656	127368.459457	58.903757
2404.664319	127163.143575	58.908762
2404.310680	126950.320585	58.913767
2403.681454	126753.074980	58.918772
2403.014374	126550.477451	58.923777
2402.513897	126336.895110	58.928781
2401.727940	126137.583325	58.933786
2401.262580	125921.598425	58.938791
2400.589777	125715.782304	58.943796
2400.103085	125510.179522	58.948801
2399.317249	125293.780533	58.953805
2398.305457	125090.524646	58.958810
2397.620764	124885.821529	58.963815
2397.283155	124680.734761	58.968820
2396.400737	124470.237298	58.973825
2395.785073	124265.058080	58.978829
2395.082085	124051.729004	58.983834
2394.267237	123846.736935	58.988839
2393.729462	123642.705686	58.993844
2392.913799	123445.234326	58.998849
2392.705234	123229.636571	59.003853
2391.974542	123030.097675	59.008858
2391.500289	122819.510347	59.013863
2390.784657	122605.318618	59.018868
2389.884890	122394.852895	59.023873
2389.392385	122188.108218	59.028877
2388.748917	121977.465489	59.033882
2388.011421	121769.467744	59.038887
2387.248287	121547.025931	59.043892
2386.468887	121342.339535	59.048897
2385.952708	121131.988087	59.053901
2384.984976	120930.509069	59.058906
2384.424170	120728.217948	59.063911
2383.840936	120516.650421	59.068916
2383.168422	120309.314124	59.073921
2382.659901	120107.451185	59.078925
2381.720985	119894.332568	59.083930
2381.236749	119683.898764	59.088935
2380.545092	119480.514358	59.093940
2379.732041	119279.239342	59.098945
2379.415896	119063.679930	59.103949
2378.684972	118858.992530	59.108954
2377.674485	118650.288310	59.113959
2377.393979	118450.338194	59.118964
2376.540028	118244.608677	59.123969
2375.834969	118027.094529	59.128973
2375.148322	117829.340143	59.133978
2374.804483	117611.880133	59.138983
2373.655135	117408.609920	59.143988
2372.838174	117208.322814	59.148993
2372.489406	117000.225255	59.153997
2371.630745	116809.215435	59.159002
2371.131040	116598.472722	59.164007
2370.701029	116383.702728	59.169012
2369.823396	116188.860307	59.174017
2369.368909	115980.464067	59.179021
2368.765867	115776.472748	59.184026
2368.069221	115566.982105	59.189031
2367.314744	115357.350020	59.194036
2366.512993	115152.900117	59.199041
2366.175705	114939.358941	59.204045
2365.613367	114741.430985	59.209050
2365.021192	114537.936610	59.214055
2364.376282	114317.175751	59.219060
2363.519966	114105.786666	59.224065
2362.751610	113900.307038	59.229069
2362.281233	113683.440075	59.234074
2361.441752	113475.404731	59.239079
2361.240448	113258.346448	59.244084
2360.253190	113039.770872	59.249089
2359.783756	112831.523529	59.254093
2358.713966	112615.147978	59.259098
2358.156250	112409.653508	59.264103
2357.647807	112200.973348	59.269108
2357.225121	111982.723677	59.274113
2356.610580	111772.445600	59.279117
2355.375289	111563.651213	59.284122
2354.967820	111349.942274	59.289127
2354.867970	111130.893695	59.294132
2353.802491	110922.477593	59.299137
2353.363649	110710.556058	59.304141
2352.339369	110497.409195	59.309146
2351.683591	110269.419680	59.314151
2351.173759	110045.971832	59.319156
2350.335929	109842.465870	59.324161
2349.684654	109630.866521	59.329165
2348.984428	109428.249623	59.334170
2348.687861	109201.380679	59.339175
2348.238391	108981.778429	59.344180
2347.312287	108772.901575	59.349185
2346.927959	108547.378838	59.354189
2346.159087	108329.705021	59.359194
2345.484317	108110.495337	59.364199
2344.883110	107893.287437	59.369204
2343.888787	107669.976204	59.374209
2343.679171	107460.571883	59.379213
2342.351373	107241.727403	59.384218
2341.796848	107021.512310	59.389223
2341.402504	106795.531560	59.394228
2340.401990	106588.544416	59.399233
2339.932339	106372.001891	59.404237
2339.281633	106164.030228	59.409242
2338.673413	105948.103566	59.414247
2337.963321	105722.944336	59.419252
2337.273687	105507.535787	59.424257
2336.986036	105282.891079	59.429261
2336.133428	105071.864724	59.434266
2335.524832	104844.001225	59.439271
2334.972528	104621.733146	59.444276
2333.849211	104407.234421	59.449281
2333.353482	104185.754496	59.454285
2332.594260	103970.535827	59.459290
2331.942111	103763.568677	59.464295
2331.145965	103536.622963	59.469300
2330.361826	103332.858944	59.474305
2329.739475	103103.954869	59.479309
2329.025143	102904.116804	59.484314
2328.243191	102677.633867	59.489319
2327.952051	102469.605789	59.494324
2326.950202	102261.070550	59.499329
2326.400676	102051.589999	59.504333
2325.948669	101842.888823	59.509338
2325.247126	101624.967323	59.514343
2324.649075	101401.284138	59.519348
2323.642891	101206.258177	59.524353
2323.410956	100978.740232	59.529357
2322.609715	100770.268948	59.534362
2321.911801	100546.882564	59.539367
2321.674321	100333.416034	59.544372
2320.509485	100129.391385	59.549377
2320.090435	99904.641224	59.554381
2319.214638	99690.102000	59.559386
2318.666303	99476.375501	59.564391
2318.235210	99258.604572	59.569396
2317.189843	99052.223572	59.574401
2316.715452	98827.372153	59.579405
2315.893251	98617.521814	59.584410
2315.686191	98401.233065	59.589415
2315.025173	98182.176798	59.594420
2314.097706	97968.911329	59.599425
2313.537816	97748.923484	59.604429
2313.043964	97528.521361	59.609434
2312.119025	97312.705570	59.614439
2311.477945	97093.555094	59.619444
2311.083536	96879.783985	59.624449
2310.397400	96651.835369	59.629453
2309.604957	96436.450838	59.634458
2308.644575	96216.731566	59.639463
2308.301026	95997.982086	59.644468
2307.346086	95783.193981	59.649473
2306.884485	95557.840032	59.654477
2306.198687	95345.087244	59.659482
2305.606874	95125.288427	59.664487
2305.107717	94903.587203	59.669492
2304.315986	94690.946178	59.674497
2303.867178	94465.030375	59.679501
2303.386642	94253.980294	59.684506
2302.628590	94024.167140	59.689511
2301.780219	93794.611645	59.694516
2301.027839	93583.167093	59.699521
2300.484990	93358.152490	59.704525
2299.821430	93136.209468	59.709530
2299.000164	92909.480663	59.714535
2298.414341	92693.205142	59.719540
2297.697218	92470.357787	59.724545
2297.173737	92246.727376	59.729549
2296.549664	92025.765707	59.734554
2295.891710	91814.792235	59.739559
2295.156335	91585.793293	59.744564
2294.245323	91372.296128	59.749569
2293.852847	91135.036151	59.754573
2293.324509	90924.437422	59.759578
2292.483025	90704.614055	59.764583
2292.032921	90483.881189	59.769588
2291.238852	90255.514086	59.774593
2290.748196	90036.085615	59.779597
2289.899365	89818.028596	59.784602
2289.143148	89593.732902	59.789607
2288.547382	89367.550042	59.794612
2287.549506	89161.075108	59.799617
2287.218599	88931.443763	59.804621
2286.346722	88700.106402	59.809626
2285.949921	88488.876268	59.814631
2285.436608	88262.469920	59.819636
2284.220196	88051.348664	59.824641
2283.728558	87819.681440	59.829645
2283.286168	87599.230164	59.834650
2282.517974	87384.386331	59.839655
2282.059935	87157.583385	59.844660
2281.260736	86943.370142	59.849665
2280.458552	86718.027434	59.854669
2280.086982	86501.810901	59.859674
2279.299767	86275.728751	59.864679
2278.663661	86053.124286	59.869684
2277.917819	85840.175099	59.874689
2277.594818	85606.140449	59.879693
2277.079209	85380.151466	59.884698
2276.010670	85154.360326	59.889703
2275.519298	84929.874608	59.894708
2274.801430	84707.151344	59.899713
2274.100922	84475.046261	59.904718
2273.466996	84249.816997	59.909722
2273.051757	84039.045596	59.914727
2272.381556	83799.254317	59.919732
2271.168714	83574.802268	59.924737
2270.870948	83343.292239	59.929742
2270.137395	83123.712960	59.934746
2269.585940	82901.356262	59.939751
2269.262873	82678.122704	59.944756
2268.234791	82455.047690	59.949761
2267.509094	82220.461456	59.954766
2266.887482	82002.948683	59.959770
2266.288128	81774.894591	59.964775
2266.073226	81541.889151	59.969780
2264.720150	81313.287808	59.974785
2264.052629	81084.554894	59.979790
2263.549882	80860.488247	59.984794
2262.715498	80643.428982	59.989799
2262.069057	80417.228764	59.994804
2261.466349	80202.444229	59.999809
2260.875200	79971.404590	60.004814
2260.070807	79744.641032	60.009818
2259.209973	79525.734467	60.014823
2258.686007	79295.021255	60.019828
2257.781865	79083.496423	60.024833
2257.432806	78857.747693	60.029838
2256.896065	78639.515212	60.034842
2256.044435	78422.988927	60.039847
2255.444396	78194.194844	60.044852
2254.556295	77978.452125	60.049857
2253.909835	77751.108797	60.054862
2253.214493	77527.685468	60.059866
2252.632142	77319.093321	60.064871
2252.339440	77091.289332	60.069876
2251.410033	76866.769769	60.074881
2250.828289	76642.869197	60.079886
2250.257075	76422.435384	60.084890
2249.206628	76212.857946	60.089895
2248.748166	75979.434388	60.094900
2247.912576	75768.142033	60.099905
2247.597514	75544.179579	60.104910
2246.817106	75328.834312	60.109914
2245.894628	75102.033186	60.114919
2245.665477	74870.670542	60.119924
2244.647466	74663.372219	60.124929
2244.230042	74441.706415	60.129934
2243.731512	74210.159646	60.134938
2242.924330	73997.221367	60.139943
2242.519987	73764.518049	60.144948
2241.575336	73548.197836	60.149953
2241.035585	73319.005644	60.154958
2240.412261	73098.077868	60.159962
2239.779281	72877.382129	60.164967
2239.090603	72641.505988	60.169972
2238.326608	72422.058741	60.174977
2237.759168	72195.392508	60.179982
2237.213726	71969.846646	60.184986
2236.078352	71751.992401	60.189991
2235.682284	71521.201677	60.194996
2234.811902	71308.302080	60.200001
2234.049859	71086.569756	60.205006
2233.339093	70861.050040	60.210010
2232.541430	70648.842800	60.215015
2232.187385	70423.917608	60.220020
2231.119401	70212.999474	60.225025
2230.466823	69992.655619	60.230030
2229.974849	69775.082148	60.235034
2229.453046	69560.752565	60.240039
2228.946188	69341.317674	60.245044
2228.240907	69124.450312	60.250049
2227.669951	68900.698046	60.255054
2226.852033	68686.057611	60.260058
2226.289634	68465.634242	60.265063
2225.616395	68231.556415	60.270068
2224.943091	68018.249457	60.275073
2224.114142	67802.822432	60.280078
2223.634744	67580.647818	60.285082
2222.714686	67371.782534	60.290087
2222.340581	67144.124104	60.295092
2221.537001	66933.497044	60.300097
2221.270560	66713.667215	60.305102
2220.274514	66492.226650	60.310106
2219.626154	66268.105238	60.315111
2219.297856	66036.811016	60.320116
2218.427753	65819.313145	60.325121
2217.560768	65604.616360	60.330126
2217.124382	65379.939671	60.335130
2216.181351	65164.015463	60.340135
2215.739912	64933.230543	60.345140
2214.700330	64726.489910	60.350145
2214.284077	64506.392356	60.355150
2213.678943	64287.590608	60.360154
2212.571655	64070.761219	60.365159
2212.052570	63844.944120	60.370164
2211.458883	63638.245825	60.375169
2210.726116	63430.026781	60.380174
2210.620591	63221.270438	60.385178
2209.409509	62995.832762	60.390183
2208.994000	62779.028631	60.395188
2208.117643	62557.988070	60.400193
2207.578237	62345.466714	60.405198
2206.897075	62132.352879	60.410202
2206.082281	61921.994744	60.415207
2205.531553	61689.705633	60.420212
2204.926118	61484.590186	60.425217
2204.324535	61263.625611	60.430222
2203.642631	61047.912395	60.435226
2203.124275	60839.849223	60.440231
2202.631291	60618.390637	60.445236
2201.345611	60404.065802	60.450241
2200.636732	60181.047997	60.455246
2199.984048	59976.193881	60.460250
2199.177972	59763.978141	60.465255
2198.823721	59543.330077	60.470260
2197.922984	59338.699540	60.475265
2197.230516	59124.659256	60.480270
2196.779396	58921.202787	60.485274
2196.134095	58708.957687	60.490279
2195.457151	58498.961017	60.495284
2194.825337	58283.822415	60.500289
2194.227530	58072.881095	60.505294
2193.740755	57863.997721	60.510298
2192.657096	57650.492206	60.515303
2191.870881	57433.935152	60.520308
2191.061117	57222.394608	60.525313
2190.428926	57010.999223	60.530318
2189.880117	56820.386819	60.535322
2189.023876	56615.434217	60.540327
2188.961253	56404.341540	60.545332
2187.927752	56196.918275	60.550337
2187.171822	55993.374528	60.555342
2186.674458	55783.687144	60.560346
2185.672588	55587.839348	60.565351
2185.163331	55381.158626	60.570356
2184.183935	55175.067486	60.575361
2184.134776	54973.008430	60.580366
2183.609548	54769.254937	60.585370
2182.837968	54561.928847	60.590375
2182.168143	54359.433875	60.595380
2181.246135	54154.696379	60.600385
2180.505000	53941.954866	60.605390
2180.128503	53739.480365	60.610394
2179.204770	53533.626744	60.615399
2178.714686	53331.124170	60.620404
2177.893458	53120.832020	60.625409
2177.439824	52922.577903	60.630414
2176.779187	52719.985788	60.635418
2175.835098	52519.355255	60.640423
2175.351483	52314.587921	60.645428
2174.314079	52117.030087	60.650433
2173.547089	51912.242650	60.655438
2173.118712	51711.428525	60.660442
2172.048246	51513.297187	60.665447
2171.546446	51320.462960	60.670452
2171.116198	51123.123436	60.675457
2170.141672	50926.122369	60.680462
2169.405245	50737.036587	60.685466
2168.728713	50541.707299	60.690471
2168.424003	50346.957083	60.695476
2167.292906	50160.645064	60.700481
2166.563194	49970.803815	60.705486
2166.485377	49771.521810	60.710490
2165.045607	49587.890624	60.715495
2164.858460	49402.173900	60.720500
2164.170373	49200.612827	60.725505
2163.440285	49020.763002	60.730510
2162.494541	48841.591408	60.735514
2161.676563	48644.090789	60.740519
2161.313605	48458.772424	60.745524
2160.303878	48275.807821	60.750529
2159.607444	48101.959887	60.755534
2159.063700	47923.954857	60.760538
2157.670783	47747.079628	60.765543
2157.081941	47574.836280	60.770548
2156.315453	47411.407318	60.775553
2155.606045	47237.228288	60.780558
2154.945543	47072.817676	60.785562
2154.031244	46918.707206	60.790567
2153.240559	46750.666717	60.795572
2152.367993	46599.680818	60.800577
2151.516610	46452.906162	60.805582
2150.580897	46289.976250	60.810586
2149.771213	46153.262517	60.815591
2149.135062	46005.827989	60.820596
2148.244631	45863.182760	60.825601
2147.733975	45717.112994	60.830606
2147.254172	45585.004141	60.835610
2146.121855	45454.673011	60.840615
2145.502945	45311.185802	60.845620
2144.816499	45181.168686	60.850625
2143.773492	45052.600777	60.855630
2143.449296	44914.412191	60.860634
2142.498986	44799.978949	60.865639
2141.945130	44659.956403	60.870644
2140.861956	44531.585307	60.875649
2140.373812	44405.274606	60.880654
2139.603816	44285.502668	60.885658
2138.829744	44170.036680	60.890663
2138.592790	44040.481757	60.895668
2137.843112	43923.732634	60.900673
2136.854392	43812.496797	60.905678
2136.830674	43680.873959	60.910682
2135.542548	43570.882650	60.915687
2135.415036	43435.084498	60.920692
2134.787148	43329.692756	60.925697
2134.433872	43201.190374	60.930702
2133.634132	43076.485242	60.935706
2132.721096	42952.624397	60.940711
2132.577798	42830.739048	60.945716
2131.467059	42718.606135	60.950721
2130.850333	42580.691205	60.955726
2130.341497	42464.524040	60.960730
2129.403119	42337.800135	60.965735
2128.741889	42217.275723	60.970740
2127.990595	42096.187730	60.975745
2127.719441	41981.573604	60.980750
2127.293890	41849.364330	60.985754
2126.353711	41729.159541	60.990759
2126.028983	41604.373852	60.995764
2125.496962	41478.945235	61.000769
2124.304873	41358.147392	61.005774
2124.022952	41230.454702	61.010778
2122.954766	41104.645873	61.015783
2122.583138	40978.357481	61.020788
2121.938329	40863.044838	61.025793
2121.288905	40737.210206	61.030798
2120.436977	40619.759691	61.035802
2119.882133	40500.795649	61.040807
2119.367496	40365.339177	61.045812
2118.454249	40246.342065	61.050817
2117.749642	40134.073023	61.055822
2117.036747	40006.214341	61.060826
2116.484180	39887.579879	61.065831
2115.783382	39772.060543	61.070836
2115.014896	39658.377149	61.075841
2114.181693	39549.534561	61.080846
2114.095826	39420.137378	61.085850
2113.032525	39313.335845	61.090855
2112.759665	39185.728092	61.095860
2111.933693	39059.072221	61.100865
2111.316569	38945.695226	61.105870
2110.615277	38820.961093	61.110874
2109.778169	38707.446692	61.115879
2109.353209	38570.693916	61.120884
2108.634362	38468.822720	61.125889
2107.678308	38353.498939	61.130894
2107.135031	38228.363102	61.135898
2106.327878	38117.671237	61.140903
2105.929888	37997.629554	61.145908
2105.140715	37876.599563	61.150913
2104.528818	37760.986506	61.155918
2104.078679	37641.771298	61.160922
2103.006688	37521.367279	61.165927
2102.651036	37413.518548	61.170932
2102.003289	37304.074465	61.175937
2101.374762	37188.034840	61.180942
2100.723002	37064.663608	61.185946
2099.804995	36951.214907	61.190951
2099.688903	36826.979553	61.195956
2098.929588	36708.314738	61.200961
2098.106935	36596.168421	61.205966
2097.530922	36466.904713	61.210970
2096.727846	36344.503248	61.215975
2096.336009	36229.581790	61.220980
2095.458057	36119.301508	61.225985
2095.014936	35996.388661	61.230990
2094.457567	35875.807260	61.235994
2093.231767	35760.253161	61.240999
2093.069074	35639.707247	61.246004
2092.761728	35519.393784	61.251009
2091.654292	35392.169918	61.256014
2090.917109	35271.951722	61.261018
2090.185288	35161.131389	61.266023
2089.443697	35038.849808	61.271028
2088.711309	34923.272187	61.276033
2087.864805	34809.213368	61.281038
2087.632478	34687.850841	61.286042
2086.468726	34580.346057	61.291047
2085.969323	34455.817639	61.296052
2085.621004	34344.448762	61.301057
2084.356928	34228.849678	61.306062
2083.847750	34119.771024	61.311066
2083.400568	34009.336723	61.316071
2082.857248	33893.824732	61.321076
2082.244420	33782.928286	61.326081
2081.374940	33672.476303	61.331086
2080.744661	33553.630037	61.336090
2079.958659	33440.557138	61.341095
2079.218099	33328.694676	61.346100
2078.536800	33219.617623	61.351105
2077.886368	33109.438052	61.356110
2077.584776	32995.485345	61.361114
2076.712683	32893.422604	61.366119
2076.272143	32771.715152	61.371124
2075.581083	32658.690986	61.376129
2074.727349	32556.352436	61.381134
2074.408113	32437.874097	61.386138
2073.753555	32335.857707	61.391143
2073.010050	32208.499287	61.396148
2072.316468	32093.696852	61.401153
2071.562548	31979.005924	61.406158
2070.610263	31865.918009	61.411162
2069.916668	31759.911829	61.416167
2069.298405	31641.715773	61.421172
2068.735666	31540.716854	61.426177
2068.134259	31433.266493	61.431182
2067.660511	31314.394076	61.436186
2066.940141	31205.203771	61.441191
2065.935563	31093.850243	61.446196
2065.318388	30984.044575	61.451201
2064.807765	30882.287698	61.456206
2064.365098	30776.383921	61.461210
2063.589280	30664.929053	61.466215
2062.929510	30554.638438	61.471220
2062.204065	30445.673616	61.476225
2061.348737	30338.387626	61.481230
2060.896362	30231.578779	61.486234
2059.758328	30127.386976	61.491239
2059.307329	30017.251712	61.496244
2058.908158	29915.519482	61.501249
2058.052372	29808.960687	61.506254
2057.374120	29702.330174	61.511258
2056.204009	29602.387562	61.516263
2055.850154	29503.303530	61.521268
2055.138397	29399.304681	61.526273
2054.002992	29310.593619	61.531278
2054.110813	29196.774436	61.536282
2052.892305	29101.418149	61.541287
2052.180417	29001.395444	61.546292
2051.720658	28917.710969	61.551297
2051.068887	28816.036726	61.556302
2050.496646	28713.306171	61.561306
2049.462256	28619.811490	61.566311
2048.909545	28513.141967	61.571316
2048.355047	28419.188370	61.576321
2047.007760	28330.187657	61.581326
2046.854948	28229.191503	61.586330
2046.067757	28140.139288	61.591335
2045.155217	28054.049140	61.596340
2044.698937	27958.880349	61.601345
2044.367124	27871.476215	61.606350
2043.665219	27772.036124	61.611354
2042.803229	27689.420248	61.616359
2042.403474	27593.661674	61.621364
2041.912725	27493.832744	61.626369
2040.823884	27409.786659	61.631374
2040.549706	27316.987699	61.636378
2039.588062	27224.694887	61.641383
2038.903966	27128.952587	61.646388
2038.065757	27033.489650	61.651393
2037.197710	26944.477374	61.656398
2036.837859	26852.691490	61.661402
2036.053159	26764.338368	61.666407
2035.614585	26679.286916	61.671412
2034.860741	26584.212125	61.676417
2034.121266	26506.763512	61.681422
2033.792252	26411.413800	61.686426
2032.918817	26325.607042	61.691431
2031.871155	26237.433600	61.696436
2031.198065	26148.213906	61.701441
2030.802459	26062.486738	61.706446
2030.056142	25979.185159	61.711450
2029.325561	25900.183674	61.716455
2028.728171	25805.079173	61.721460
2028.360919	25721.421802	61.726465
2027.359381	25639.697091	61.731470
2026.835025	25544.616502	61.736474
2026.304462	25462.693160	61.741479
2025.540336	25364.525658	61.746484
2024.466612	25286.546776	61.751489
2024.091332	25207.569710	61.756494
2023.855539	25117.945145	61.761498
2022.936860	25035.772821	61.766503
2022.395641	24949.389958	61.771508
2021.462869	24863.579101	61.776513
2020.613594	24783.810596	61.781518
2020.094381	24692.234488	61.786522
2019.379830	24606.538063	61.791527
2018.609300	24520.639327	61.796532
2017.970541	24443.281820	61.801537
2017.395578	24367.422979	61.806542
2016.961536	24278.734090	61.811546
2016.228099	24200.424560	61.816551
2015.524755	24127.164939	61.821556
2015.155636	24040.147626	61.826561
2014.367852	23956.672814	61.831566
2013.629869	23871.521062	61.836570
2012.787449	23790.822186	61.841575
2012.208176	23705.275757	61.846580
2011.690338	23621.673778	61.851585
2011.057351	23539.375363	61.856590
2010.297968	23452.293679	61.861594
2009.423478	23377.084096	61.866599
2008.560019	23292.046170	61.871604
2008.024746	23215.505791	61.876609
2007.561758	23138.845332	61.881614
2007.083148	23044.597565	61.886618
2006.547142	22988.556160	61.891623
2005.719823	22904.427439	61.896628
2005.010650	22813.834339	61.901633
2004.002879	22733.080207	61.906638
2003.674760	22644.007721	61.911642
2002.687400	22572.351226	61.916647
2002.193886	22485.711964	61.921652
2001.775904	22405.905077	61.926657
2000.938332	22329.232957	61.931662
2000.099738	22249.740769	61.936666
1999.690163	22174.085651	61.941671
1999.148583	22095.282253	61.946676
1998.241405	22014.708487	61.951681
1997.709329	21945.892357	61.956686
1996.990335	21855.245490	61.961690
1996.302028	21781.869534	61.966695
1995.473038	21703.499035	61.971700
1995.055005	21612.553907	61.976705
1994.231709	21537.445996	61.981710
1993.927682	21461.918869	61.986714
1993.270832	21377.785415	61.991719
1992.284179	21294.552777	61.996724
1991.714619	21218.188560	62.001729
1990.908507	21136.453591	62.006734
1990.391041	21055.549670	62.011738
1989.576964	20980.271609	62.016743
1988.860645	20910.644381	62.021748
1988.197641	20827.748943	62.026753
1987.429091	20759.141325	62.031758
1986.869537	20681.401115	62.036762
1986.251335	20613.769856	62.041767
1985.778181	20529.511499	62.046772
1985.112898	20446.967411	62.051777
1984.199608	20374.555907	62.056782
1983.634879	20292.802798	62.061786
1983.150155	20221.089839	62.066791
1982.164671	20149.327991	62.071796
1981.653621	20067.511476	62.076801
1980.802781	19990.515701	62.081806
1980.134345	19920.289954	62.086810
1979.444131	19851.816374	62.091815
1978.831544	19776.358932	62.096820
1978.283755	19708.976986	62.101825
1977.354984	19643.217845	62.106830
1977.117452	19564.507137	62.111834
1976.329711	19491.328963	62.116839
1975.670212	19420.097816	62.121844
1975.148348	19341.580992	62.126849
1974.554249	19265.016204	62.131854
1973.736003	19189.331724	62.136858
1972.876394	19107.579882	62.141863
1972.132120	19034.828397	62.146868
1972.021684	18963.556787	62.151873
1970.688341	18889.009075	62.156878
1970.458339	18815.160145	62.161882
1969.841877	18749.389537	62.166887
1969.060461	18679.195184	62.171892
1968.381261	18604.748292	62.176897
1967.598155	18530.252722	62.181902
1966.922195	18457.158356	62.186906
1965.892279	18389.161928	62.191911
1965.470245	18316.311726	62.196916
1965.087011	18246.543998	62.201921
1964.045610	18172.847417	62.206926
1963.327702	18108.346083	62.211930
1962.629603	18045.082856	62.216935
1961.995201	17973.430401	62.221940
1961.646100	17901.957582	62.226945
1961.021046	17834.895962	62.231950
1960.615174	17757.580452	62.236954
1960.083923	17694.008374	62.241959
1959.227701	17609.137383	62.246964
1958.712944	17534.956057	62.251969
1958.179423	17470.460861	62.256974
1957.414144	17388.421643	62.261978
1956.796743	17315.421230	62.266983
1956.129812	17239.357110	62.271988
1955.300003	17161.374958	62.276993
1954.339632	17087.504500	62.281998
1954.093460	17020.710297	62.287002
1953.140300	16949.675984	62.292007
1952.612069	16867.827259	62.297012
1952.234215	16793.094725	62.302017
1951.397215	16730.420142	62.307022
1950.690311	16647.478465	62.312026
1949.984795	16578.063021	62.317031
1948.988046	16503.756320	62.322036
1948.910172	16428.806242	62.327041
1947.806239	16357.572234	62.332046
1947.094034	16290.816273	62.337050
1946.687699	16229.270228	62.342055
1945.682364	16154.890396	62.347060
1945.283069	16071.437668	62.352065
1944.383203	16004.107120	62.357070
1943.828877	15938.735188	62.362074
1943.381902	15863.799272	62.367079
1942.598094	15789.350322	62.372084
1942.194263	15730.280570	62.377089
1941.367877	15664.119668	62.382094
1940.995973	15579.801940	62.387098
1940.364060	15507.666386	62.392103
1939.210425	15430.622069	62.397108
1938.761169	15353.545260	62.402113
1937.838979	15278.246010	62.407118
1937.439258	15208.598754	62.412122
1936.497505	15137.961368	62.417127
1935.529706	15074.932655	62.422132
1935.229504	14995.092319	62.427137
1934.512745	14934.094012	62.432142
1933.975916	14862.894697	62.437146
1933.608698	14802.751158	62.442151
1932.901133	14726.586780	62.447156
1932.220598	14656.332202	62.452161
1931.399942	14585.958911	62.457166
1930.607355	14510.552875	62.462170
1929.949117	14442.145642	62.467175
1928.997702	14373.110252	62.472180
1929.122525	14299.085729	62.477185
1927.969336	14239.011447	62.482190
1927.551020	14159.476646	62.487194
1926.727137	14089.665020	62.492199
1925.847574	14010.512304	62.497204
1925.314891	13941.210054	62.502209
1924.411080	13885.689881	62.507214
1923.924012	13808.508735	62.512218
1923.335662	13744.845186	62.517223
1922.555427	13688.283271	62.522228
1922.219904	13615.779664	62.527233
1921.361062	13560.255484	62.532238
1921.117352	13485.463143	62.537242
1920.199253	13416.026562	62.542247
1919.356404	13344.410936	62.547252
1919.266360	13264.201070	62.552257
1918.081543	13200.327379	62.557262
1917.580392	13121.407642	62.562266
1916.945337	13052.961186	62.567271
1916.293447	12984.415437	62.572276
1915.589445	12910.493378	62.577281
1914.724872	12838.105260	62.582286
1914.102677	12764.564420	62.587290
1913.337787	12706.702480	62.592295
1912.714840	12644.306631	62.597300
1912.275394	12575.003569	62.602305
1911.190451	12500.456029	62.607310
1910.819154	12435.977096	62.612314
1910.184529	12364.432649	62.617319
1909.471191	12292.839481	62.622324
1909.014293	12222.509786	62.627329
1908.125235	12157.926409	62.632334
1907.829392	12087.206406	62.637338
1906.947506	12008.021342	62.642343
1906.396316	11948.767029	62.647348
1905.673136	11871.504238	62.652353
1905.091065	11806.575731	62.657358
1903.972578	11735.468325	62.662362
1903.358500	11671.573684	62.667367
1902.502674	11611.041777	62.672372
1902.145884	11538.364800	62.677377
1901.373995	11481.844479	62.682382
1901.033621	11403.663977	62.687386
1900.264076	11342.978196	62.692391
1899.476782	11269.839396	62.697396
1899.164460	11204.132458	62.702401
1898.435911	11136.941740	62.707406
1897.541148	11061.748891	62.712410
1897.061278	10988.814360	62.717415
1896.223265	10927.590343	62.722420
1895.765478	10855.559189	62.727425
1894.640092	10798.151455	62.732430
1894.162172	10726.651992	62.737434
1893.530708	10661.062381	62.742439
1892.833003	10604.650735	62.747444
1892.393131	10533.601425	62.752449
1891.632526	10474.438989	62.757454
1891.081279	10409.125737	62.762458
1890.554612	10335.929959	62.767463
1889.644445	10269.168814	62.772468
1889.201261	10194.411797	62.777473
1888.480098	10133.604048	62.782478
1887.666087	10057.957973	62.787482
1887.032346	9993.995031	62.792487
1886.361155	9934.937291	62.797492
1885.982805	9851.904986	62.802497
1885.099293	9787.902486	62.807502
1884.185388	9716.245447	62.812506
1883.742504	9647.308212	62.817511
1882.754084	9579.269380	62.822516
1882.633139	9502.218170	62.827521
1881.368118	9446.696226	62.832526
1880.946997	9385.397693	62.837530
1880.277340	9321.566390	62.842535
1879.435902	9255.704186	62.847540
1879.081235	9188.034772	62.852545
1878.773959	9119.135232	62.857550
1878.105519	9051.603426	62.862554
1877.239942	8977.369808	62.867559
1876.528535	8914.372909	62.872564
1876.023332	8841.224773	62.877569
1875.270383	8778.103680	62.882574
1874.651177	8702.827181	62.887578
1874.202212	8626.919306	62.892583
1873.296894	8574.219195	62.897588
1872.522851	8493.120691	62.902593
1871.765541	8431.640768	62.907598
1871.196478	8359.105500	62.912602
1870.637623	8304.830275	62.917607
1869.850799	8239.374501	62.922612
1869.448710	8160.539762	62.927617
1868.341383	8094.221147	62.932622
1867.728574	8025.540807	62.937626
1867.309078	7955.606097	62.942631
1866.582824	7900.823638	62.947636
1865.747397	7827.238233	62.952641
1865.129772	7764.626521	62.957646
1864.701347	7697.616126	62.962650
1863.754009	7631.247739	62.967655
1863.286023	7567.983558	62.972660
1862.849172	7494.392130	62.977665
1861.980181	7438.601378	62.982670
1861.318853	7363.550511	62.987674
1860.996321	7289.734466	62.992679
1859.809992	7237.066729	62.997684
1859.232634	7159.073689	63.002689
1858.410414	7094.898234	63.007694
1857.833076	7026.250778	63.012698
1857.497973	6964.628610	63.017703
1856.107013	6903.589267	63.022708
1856.025265	6832.142080	63.027713
1855.185159	6771.370017	63.032718
1854.652347	6710.212579	63.037722
1854.235379	6643.383377	63.042727
1853.682569	6586.306351	63.047732
1852.871031	6512.870759	63.052737
1852.061365	6447.220985	63.057742
1851.659993	6371.136764	63.062746
1850.846044	6300.747472	63.067751
1850.039773	6243.086469	63.072756
1849.653687	6165.704841	63.077761
1849.018850	6096.820747	63.082766
1847.944735	6034.767592	63.087770
1847.297925	5959.684424	63.092775
1846.701156	5903.696085	63.097780
1846.100363	5830.705264	63.102785
1845.188331	5779.732929	63.107790
1844.923972	5697.764924	63.112794
1844.329756	5639.798100	63.117799
1843.130733	5587.859977	63.122804
1843.014411	5496.387602	63.127809
1841.869443	5448.104482	63.132814
1841.404673	5373.224126	63.137818
1840.584426	5313.101679	63.142823
1839.786480	5242.923105	63.147828
1839.346724	5186.971702	63.152833
1838.539614	5124.445363	63.157838
1837.803506	5064.234848	63.162842
1837.327149	4999.440905	63.167847
1836.475415	4934.620083	63.172852
1836.142547	4870.948397	63.177857
1835.437782	4813.217692	63.182862
1834.813787	4761.727523	63.187866
1834.440282	4682.840410	63.192871
1833.539878	4626.234687	63.197876
1832.555410	4557.156930	63.202881
1831.980253	4499.743661	63.207886
1831.563918	4433.321047	63.212890
1830.998171	4366.650348	63.217895
1830.028113	4309.482714	63.222900
1829.487173	4233.956122	63.227905
1828.780894	4168.583979	63.232910
1827.883979	4106.750559	63.237914
1827.275888	4042.458110	63.242919
1826.580052	3988.750809	63.247924
1825.895734	3918.848365	63.252929
1825.310951	3871.695274	63.257934
1824.743277	3807.988163	63.262938
1824.087946	3747.867995	63.267943
1823.244627	3692.278939	63.272948
1822.724238	3628.110029	63.277953
1822.066474	3560.456753	63.282958
1821.446151	3503.501718	63.287962
1820.687398	3442.164949	63.292967
1820.002330	3379.064317	63.297972
1819.406818	3319.491626	63.302977
1818.757001	3256.677729	63.307982
1818.157886	3189.463231	63.312986
1817.771425	3137.776199	63.317991
1816.654058	3070.478918	63.322996
1816.057115	3008.103277	63.328001
1815.294322	2946.694298	63.333006
1814.567288	2891.038552	63.338010
1813.979224	2835.200859	63.343015
1813.090198	2789.034878	63.348020
1812.662323	2727.084687	63.353025
1812.041830	2672.953051	63.358030
1811.222929	2615.440735	63.363034
1810.780355	2550.178243	63.368039
1810.209780	2508.443536	63.373044
1809.464871	2433.721967	63.378049
1808.541230	2383.868885	63.383054
1807.766856	2330.086283	63.388058
1807.016360	2273.214267	63.393063
1806.486362	2218.712704	63.398068
1806.122324	2157.451123	63.403073
1805.110003	2105.920734	63.408078
1804.236048	2055.736770	63.413082
1803.783036	2002.580962	63.418087
1803.076910	1952.171979	63.423092
1802.756757	1892.469892	63.428097
1802.031462	1848.642706	63.433102
1801.473630	1794.524877	63.438106
1800.747342	1725.996702	63.443111
1800.034831	1684.039277	63.448116
1799.212856	1619.438923	63.453121
1798.635388	1572.620907	63.458126
1798.181496	1517.083948	63.463130
1797.434401	1445.780697	63.468135
1796.420966	1402.279759	63.473140
1795.957662	1346.035241	63.478145
1795.598921	1298.016311	63.483150
1794.426854	1239.606615	63.488154
1793.936241	1182.308041	63.493159
1793.037117	1138.538982	63.498164
1792.371230	1080.927987	63.503169
1791.758977	1040.672367	63.508174
1790.906637	994.072551	63.513178
1790.731780	928.978233	63.518183
1789.936253	888.056651	63.523188
1789.395728	843.369673	63.528193
1788.839059	793.189358	63.533198
1787.908601	738.905160	63.538202
1787.484952	687.533916	63.543207
1786.235637	637.054096	63.548212
1785.820832	583.524427	63.553217
1785.019018	540.939476	63.558222
1784.297104	487.768025	63.563226
1783.722982	437.851917	63.568231
1782.700759	409.072872	63.573236
1782.260629	352.116496	63.578241
1781.692938	314.937286	63.583246
1781.040295	267.928823	63.588250
1780.442952	220.764282	63.593255
1779.274425	195.262233	63.598260
1778.908629	138.033113	63.603265
1778.154251	101.648934	63.608270
1777.139416	72.347408	63.613274
1776.584037	29.029384	63.618279
1775.410631	-0.264160	63.623284
1774.857057	-30.080277	63.628289
1774.142281	-65.274983	63.633294
1772.950060	-77.885841	63.638298
1772.030612	-85.031683	63.643303
1766.680745	33.795486	63.648308
1765.652877	46.208659	63.653313
1766.518887	63.403682	63.658318
1767.236288	58.030559	63.663322
1767.870174	58.134918	63.668327
1767.540574	71.544263	63.673332
1767.725276	53.308759	63.678337
1767.308594	46.395255	63.683342
1765.729809	51.078859	63.688346
1764.720276	45.082682	63.693351
1763.289458	54.008507	63.698356
1763.478947	53.472221	63.703361
1762.424375	57.082242	63.708366
1761.639780	59.752092	63.713370
1761.730683	46.964175	63.718375
1760.998161	55.607219	63.723380
1760.401645	51.004155	63.728385
1759.175952	51.840644	63.733390
1758.343133	57.716258	63.738394
1758.553510	54.849040	63.743399
1757.790707	66.340185	63.748404
1756.937075	58.835314	63.753409
1756.106980	55.611350	63.758414
1755.286774	64.241516	63.763418
1755.525559	65.124564	63.768423
1754.620601	74.879965	63.773428
1753.956909	68.518197	63.778433
1753.384416	63.127559	63.783438
1752.689501	73.507201	63.788442
1751.635146	66.923619	63.793447
1750.868696	75.884306	63.798452
1750.357987	71.119376	63.803457
1749.179401	68.098990	63.808462
1748.852301	67.799285	63.813466
1749.023861	68.817590	63.818471
1748.216157	76.662023	63.823476
1747.521015	64.960879	63.828481
1746.669042	68.761087	63.833486
1745.767101	76.524291	63.838490
1745.656163	58.819866	63.843495
1744.666898	73.489896	63.848500
1743.751791	66.904704	63.853505
1743.208387	68.664189	63.858510
1742.120087	73.686241	63.863514
1741.574865	65.731841	63.868519
1740.917400	73.735343	63.873524
1740.626314	58.830278	63.878529
1740.500621	58.495435	63.883534
1739.637690	70.227996	63.888538
1738.782853	69.080111	63.893543
1738.088555	69.895297	63.898548
1737.645104	79.340865	63.903553
1736.937120	68.457058	63.908558
1735.865391	74.023691	63.913562
1735.818771	64.942997	63.918567
1734.539909	76.156561	63.923572
1734.320185	71.061566	63.928577
1733.888697	62.398393	63.933582
1732.308062	66.697532	63.938586
1732.367927	64.726282	63.943591
1731.538257	72.927447	63.948596
1731.073349	62.506522	63.953601
1730.270870	60.090322	63.958606
1729.449639	62.385949	63.963610
1728.848941	56.208158	63.968615
1728.160004	78.918805	63.973620
1727.407328	63.454678	63.978625
1726.584380	69.623631	63.983630
1726.037608	72.840781	63.988634
1725.391828	73.853272	63.993639
1724.432881	72.116367	63.998644
1723.881043	69.297657	64.003649
1723.799283	71.043754	64.008654
1723.132295	68.645461	64.013658
1722.500429	50.467112	64.018663
1721.436507	61.834194	64.023668
1721.145456	60.661432	64.028673
1720.277204	65.658003	64.033678
1719.404817	71.937314	64.038682
1719.490765	66.621886	64.043687
1718.535977	69.872297	64.048692
1717.746580	66.455797	64.053697
1716.784031	64.640619	64.058702
1716.164612	73.808199	64.063706
1715.920911	65.785418	64.068711
1715.080918	64.818113	64.073716
1714.450718	61.636532	64.078721
1713.714314	70.283364	64.083726
1712.799278	62.643180	64.088730
1712.994665	54.941758	64.093735
1711.887738	71.065527	64.098740
1711.320686	67.042850	64.103745
1710.693929	58.046417	64.108750
1710.314080	68.562105	64.113754
1709.475551	59.812198	64.118759
1708.577907	63.911410	64.123764
1708.317110	64.345512	64.128769
1707.636393	62.897167	64.133774
1705.919981	70.004402	64.138778
1706.030756	65.110815	64.143783
1705.266745	66.998386	64.148788
1704.107207	68.112981	64.153793
1703.951829	69.142207	64.158798
1703.407375	65.234217	64.163802
1702.756574	59.037582	64.168807
1701.514160	61.627196	64.173812
1701.240150	60.893282	64.178817
1700.936749	65.396439	64.183822
1700.011338	61.747656	64.188826
1699.179179	66.516147	64.193831
1698.383512	65.275299	64.198836
1697.711846	58.916397	64.203841
1697.361709	58.770171	64.208846
1696.526718	69.724008	64.213850
1696.337373	62.976257	64.218855
1695.610182	72.149917	64.223860
1694.982947	63.981473	64.228865
1694.494267	64.812899	64.233870
1693.411381	72.792513	64.238874
1693.023579	58.003750	64.243879
1692.446577	63.556472	64.248884
1691.599057	64.222540	64.253889
1690.322230	62.965076	64.258894
1689.700601	71.286173	64.263898
1689.543086	63.725956	64.268903
1688.813609	65.813053	64.273908
1688.081388	67.072675	64.278913
1687.631006	64.173204	64.283918
1686.384670	66.041193	64.288922
1686.374041	58.588538	64.293927
1685.340426	61.860941	64.298932
1684.791544	62.899053	64.303937
1684.348709	64.795541	64.308942
1684.119586	69.695339	64.313946
1683.469115	66.248900	64.318951
1682.437876	67.199621	64.323956
1681.332515	65.713073	64.328961
1680.552360	62.947986	64.333966
1679.614384	71.054400	64.338970
1679.925346	61.549482	64.343975
1679.358105	72.348832	64.348980
1677.991789	63.406795	64.353985
1677.834766	64.475708	64.358990
1677.004572	71.450082	64.363994
1676.667012	64.173934	64.368999
1675.896792	70.091671	64.374004
1675.368231	69.707279	64.379009
1674.276516	64.465367	64.384014
1673.144033	69.245298	64.389018
1672.733761	65.511547	64.394023
1671.909904	65.423223	64.399028
1671.762429	62.013589	64.404033
1671.130075	61.760804	64.409038
1670.533064	67.206321	64.414042
1670.134128	58.157945	64.419047
1669.533983	75.216803	64.424052
1668.877925	68.489569	64.429057
1667.973268	74.867062	64.434062
1666.703606	75.544997	64.439066
1666.354463	69.641080	64.444071
1665.631168	69.399587	64.449076
1664.987642	61.170664	64.454081
1664.595481	63.707242	64.459086
1663.710057	78.400225	64.464090
1663.465355	74.526632	64.469095
1662.678903	70.849481	64.474100
1662.352730	66.326502	64.479105
1661.238110	64.761008	64.484110
1660.037638	77.927060	64.489114
1659.957645	65.202553	64.494119
1659.034050	70.428710	64.499124
1658.533768	68.445508	64.504129
1658.272965	69.027852	64.509134
1657.664096	66.954665	64.514138
1656.734959	73.116850	64.519143
1655.532335	67.151385	64.524148
1654.779225	66.023640	64.529153
1653.883496	70.232954	64.534158
1653.645378	69.502806	64.539162
1653.718673	65.219155	64.544167
1652.929448	68.941613	64.549172
1651.880785	64.200659	64.554177
1651.374774	65.947914	64.559182
1650.763974	68.091864	64.564186
1650.308795	58.921538	64.569191
1649.203845	59.682128	64.574196
1648.180204	61.339716	64.579201
1647.967900	60.794705	64.584206
1647.253030	61.646299	64.589210
1646.767576	55.964321	64.594215
1646.005657	65.758521	64.599220
1645.378195	64.502009	64.604225
1645.140964	61.202831	64.609230
1644.295048	62.978848	64.614234
1643.213880	55.210545	64.619239
1642.221198	66.763457	64.624244
1641.667997	68.360512	64.629249
1641.780106	58.879299	64.634254
1640.681589	64.954848	64.639258
1640.246810	65.451288	64.644263
1639.656649	65.699594	64.649268
1639.083634	69.275745	64.654273
1638.254797	60.814490	64.659278
1636.986414	59.953109	64.664282
1636.359633	56.476114	64.669287
1635.825118	62.838969	64.674292
1635.243106	63.860275	64.679297
1634.926104	52.395588	64.684302
1634.137814	65.458313	64.689306
1634.322563	61.869751	64.694311
1633.471694	62.519022	64.699316
1632.243598	63.649269	64.704321
1631.527856	58.458043	64.709326
1630.877622	61.874571	64.714330
1630.423390	54.482929	64.719335
1629.885172	66.488783	64.724340
1628.509039	55.058301	64.729345
1627.771721	56.403904	64.734350
1626.973386	56.065532	64.739354
1626.922956	57.805074	64.744359
1626.310252	49.276381	64.749364
1625.862689	52.999761	64.754369
1625.322711	57.100527	64.759374
1624.582100	65.953048	64.764378
1623.936939	59.236718	64.769383
1622.918377	66.564305	64.774388
1621.665562	57.905479	64.779393
1621.630234	56.715761	64.784398
1621.369288	72.577428	64.789402
1620.738142	63.349905	64.794407
1620.091012	63.383334	64.799412
1618.560990	62.087280	64.804417
1618.267163	64.190345	64.809422
1617.612542	70.603824	64.814426
1617.151091	61.123838	64.819431
1616.511788	61.168642	64.824436
1615.953184	61.750989	64.829441
1615.036204	61.122381	64.834446
1613.804206	68.403453	64.839450
1613.237697	59.162512	64.844455
1612.889058	51.448169	64.849460
1612.195051	61.472861	64.854465
1612.117925	58.786927	64.859470
1611.341916	64.648825	64.864474
1610.907485	62.882257	64.869479
1609.997077	60.448550	64.874484
1609.120197	63.325493	64.879489
1608.377504	58.004514	64.884494
1607.560205	58.514418	64.889498
1607.235530	63.757407	64.894503
1606.746214	68.498266	64.899508
1605.730082	69.834553	64.904513
1604.872532	59.670011	64.909518
1603.840537	69.478742	64.914522
1603.712630	61.462820	64.919527
1603.098106	64.569326	64.924532
1602.524852	69.351907	64.929537
1602.131107	66.441878	64.934542
1601.676338	69.354270	64.939546
1600.914518	60.660031	64.944551
1599.578425	67.523977	64.949556
1598.983832	62.898572	64.954561
1598.614185	54.033223	64.959566
1597.916070	61.035515	64.964570
1597.430897	62.039868	64.969575
1596.660678	66.729159	64.974580
1595.039336	68.923275	64.979585
1594.992914	60.867601	64.984590
1594.353089	73.070958	64.989594
1593.762654	57.191612	64.994599
1593.474658	62.379888	64.999604
1592.610189	64.680847	65.004609
1592.826347	61.415303	65.009614
1591.354654	57.572650	65.014618
1590.661450	57.187625	65.019623
1590.128145	61.350416	65.024628
1589.449063	62.014988	65.029633
1588.899226	56.953540	65.034638
1587.788942	60.903641	65.039642
1586.843182	67.383879	65.044647
1586.270405	57.830126	65.049652
1585.918441	58.994669	65.054657
1585.596565	58.825044	65.059662
1585.065825	63.492061	65.064666
1584.623885	62.005815	65.069671
1583.404958	61.095603	65.074676
1582.130889	58.368017	65.079681
1581.797811	54.615715	65.084686
1581.221754	67.513844	65.089690
1580.600806	57.441037	65.094695
1580.702879	44.399051	65.099700
1579.903129	57.821571	65.104705
1578.814461	55.302655	65.109710
1578.192548	59.794920	65.114714
1577.567860	60.394082	65.119719
1576.846217	58.952276	65.124724
1576.007354	61.868921	65.129729
1575.362396	57.049673	65.134734
1574.122655	58.506653	65.139738
1573.585392	64.396862	65.144743
1573.386909	63.020174	65.149748
1572.583750	62.351421	65.154753
1572.618515	54.688136	65.159758
1572.035265	58.598664	65.164762
1571.561826	61.898806	65.169767
1570.373689	63.738678	65.174772
1569.205180	67.012055	65.179777
1569.036269	58.229938	65.184782
1568.777966	62.125111	65.189786
1567.469093	58.736004	65.194791
1566.490719	65.603055	65.199796
1565.649844	55.457963	65.204801
1565.402167	61.958182	65.209806
1564.495297	61.458875	65.214810
1564.593341	50.767215	65.219815
1564.147598	50.153644	65.224820
1562.779158	69.782025	65.229825
1561.802618	55.224041	65.234830
1561.222430	59.545675	65.239834
1560.791065	57.103686	65.244839
1560.313608	63.432254	65.249844
1559.812334	66.593316	65.254849
1559.583355	60.354938	65.259854
1558.402276	65.360255	65.264858
1557.661810	62.674059	65.269863
1557.151524	50.216648	65.274868
1556.312697	59.485333	65.279873
1556.056278	52.461256	65.284878
1555.217081	62.923770	65.289882
1554.482802	54.627304	65.294887
1554.027652	57.098209	65.299892
1553.169906	62.659288	65.304897
1551.864207	59.662351	65.309902
1551.078919	58.268512	65.314906
1550.783718	48.331625	65.319911
1550.397766	49.410108	65.324916
1549.642392	58.159327	65.329921
1549.525576	59.584561	65.334926
1549.074241	62.529529	65.339930
1547.799498	60.664672	65.344935
1546.995730	54.903982	65.349940
1546.467110	54.707286	65.354945
1545.831052	46.574998	65.359950
1545.338500	55.911668	65.364954
1544.353511	53.715344	65.369959
1543.416943	51.061890	65.374964
1542.821947	56.125478	65.379969
1542.796978	54.224479	65.384974
1542.087964	52.605633	65.389978
1541.270711	51.749893	65.394983
1540.037359	51.450705	65.399988
1539.122375	59.127714	65.404993
1539.091809	53.247329	65.409998
1538.351964	59.742170	65.415002
1538.179885	52.078637	65.420007
1537.754109	49.996893	65.425012
1536.840005	56.986203	65.430017
1536.020763	52.959492	65.435022
1535.143866	59.040864	65.440026
1534.465218	61.312315	65.445031
1534.144314	58.598887	65.450036
1533.017558	61.361013	65.455041
1532.071641	57.411201	65.460046
1531.427312	66.893422	65.465050
1530.944619	57.628152	65.470055
1530.686603	50.601181	65.475060
1530.130653	62.622472	65.480065
1530.119066	53.531512	65.485070
1529.251082	59.247190	65.490074
1528.047715	61.020114	65.495079
1527.537560	50.396710	65.500084
1526.570260	57.717755	65.505089
1525.717290	56.292100	65.510094
1524.873544	60.209335	65.515098
1524.439098	60.111223	65.520103
1523.777663	51.330105	65.525108
1523.372836	51.214670	65.530113
1523.056242	49.484591	65.535118
1522.458099	66.297119	65.540122
1521.202675	57.324949	65.545127
1520.585384	55.193212	65.550132
1519.747100	55.241270	65.555137
1519.315640	51.887816	65.560142
1518.772743	60.395120	65.565146
1518.341501	58.585486	65.570151
1517.379093	56.098575	65.575156
1516.288325	59.351735	65.580161
1516.323744	56.288375	65.585166
1515.491331	60.560207	65.590170
1514.879311	64.185157	65.595175
1513.832486	55.083651	65.600180
1512.990337	59.178833	65.605185
1512.746003	39.570203	65.610190
1512.143699	55.276347	65.615194
1511.817589	51.805229	65.620199
1511.432736	54.492053	65.625204
1510.139700	55.937030	65.630209
1509.474746	53.836524	65.635214
1508.892586	52.746317	65.640218
1508.235002	55.683061	65.645223
1507.174006	49.439708	65.650228
1506.499760	58.324279	65.655233
1506.092614	44.355533	65.660238
1505.021320	64.327797	65.665242
1504.727011	60.039484	65.670247
1504.581163	55.052638	65.675252
1504.116770	64.294956	65.680257
1503.084382	50.256821	65.685262
1502.094770	57.376413	65.690266
1501.725319	52.338366	65.695271
1501.093474	56.814876	65.700276
1499.978233	55.604373	65.705281
1499.203366	42.592936	65.710286
1498.603221	49.507133	65.715290
1498.270631	62.131607	65.720295
1497.873134	55.379118	65.725300
1497.171385	59.286413	65.730305
1496.322806	55.833663	65.735310
1495.668074	55.158695	65.740314
1494.883205	54.846609	65.745319
1494.664470	48.819510	65.750324
1493.799245	54.416485	65.755329
1492.961509	53.873101	65.760334
1492.007894	62.614411	65.765338
1491.376336	62.359967	65.770343
1491.203806	52.354711	65.775348
1490.538230	50.085575	65.780353
1489.652044	55.092941	65.785358
1488.752404	49.973567	65.790362
1488.098949	54.269008	65.795367
1487.852281	53.835129	65.800372
1487.138426	58.097591	65.805377
1486.669991	56.109367	65.810382
1485.938376	56.149948	65.815386
1485.044491	52.934640	65.820391
1484.557963	49.722411	65.825396
1483.730491	57.998969	65.830401
1482.856639	46.873553	65.835406
1482.282901	59.345532	65.840410
1481.672598	55.601031	65.845415
1481.196450	51.625475	65.850420
1480.157065	54.048881	65.855425
1480.157766	50.637799	65.860430
1479.200951	53.145856	65.865434
1478.166362	57.042968	65.870439
1477.600937	52.588008	65.875444
1476.986143	53.187198	65.880449
1476.881031	50.046823	65.885454
1475.905087	46.696326	65.890458
1475.044456	56.714398	65.895463
1474.726047	53.538532	65.900468
1473.983353	55.511088	65.905473
1473.447683	47.723996	65.910478
1472.202103	53.763047	65.915482
1471.641064	55.154796	65.920487
1471.116220	54.640545	65.925492
1470.374423	62.133933	65.930497
1470.465964	53.731496	65.935502
1469.117571	49.315809	65.940506
1468.426879	52.875996	65.945511
1468.125006	48.954751	65.950516
1467.309666	55.806958	65.955521
1466.553132	57.013731	65.960526
1465.789512	55.261658	65.965530
1464.602406	59.362788	65.970535
1464.265493	59.350111	65.975540
1463.952234	49.654236	65.980545
1463.730918	48.233879	65.985550
1463.027804	51.349758	65.990554
1461.979716	57.196578	65.995559
1461.629697	52.765739	66.000564
1460.562044	57.136471	66.005569
1460.259008	46.284632	66.010574
1458.887910	54.001030	66.015578
1458.068107	49.638542	66.020583
1457.861934	49.573550	66.025588
1456.833046	57.520998	66.030593
1456.570792	53.386875	66.035598
1456.508392	54.672575	66.040602
1455.748220	54.627815	66.045607
1455.334970	53.867172	66.050612
1454.242840	56.790985	66.055617
1453.485387	52.022770	66.060622
1452.385994	56.009038	66.065626
1451.759868	58.999145	66.070631
1451.366672	54.023229	66.075636
1450.452706	53.545591	66.080641
1450.330524	51.391960	66.085646
1449.951692	49.564548	66.090650
1448.923740	49.332109	66.095655
1448.455433	43.606459	66.100660
1447.203965	59.519860	66.105665
1446.454824	53.422517	66.110670
1445.604871	54.379212	66.115674
1445.032124	56.856206	66.120679
1444.488032	48.920648	66.125684
1443.922802	54.958820	66.130689
1443.749596	54.786087	66.135694
1443.501718	53.188602	66.140698
1442.333833	60.825405	66.145703
1441.835008	47.203988	66.150708
1441.150447	59.106950	66.155713
1440.235351	54.213980	66.160718
1439.502964	55.785934	66.165722
1438.483587	63.220941	66.170727
1438.312547	48.568131	66.175732
1437.500468	63.812460	66.180737
1436.837300	55.785437	66.185742
1435.700862	55.704288	66.190746
1435.251346	63.909754	66.195751
1434.758098	52.460513	66.200756
1434.377194	54.459160	66.205761
1433.937066	58.406891	66.210766
1433.111200	50.998671	66.215770
1432.078199	57.354042	66.220775
1431.408888	54.938857	66.225780
1430.808870	59.599559	66.230785
1430.627376	49.595741	66.235790
1429.822174	56.976208	66.240794
1428.601323	57.876737	66.245799
1428.308859	54.769295	66.250804
1427.578257	59.332480	66.255809
1427.343139	57.121104	66.260814
1426.172417	53.694348	66.265818
1425.409762	57.034167	66.270823
1425.063448	62.690619	66.275828
1424.355052	56.667233	66.280833
1424.051932	56.024711	66.285838
1422.669759	59.259565	66.290842
1421.924206	63.486080	66.295847
1421.605700	53.789468	66.300852
1421.085265	60.572741	66.305857
1420.871225	42.004852	66.310862
1419.509157	54.666781	66.315866
1418.536779	50.869457	66.320871
1418.314781	51.835167	66.325876
1417.630545	58.436313	66.330881
1417.429319	53.455125	66.335886
1416.840840	50.060416	66.340890
1415.522858	50.140594	66.345895
1414.897979	48.997275	66.350900
1414.451168	51.334408	66.355905
1414.013661	47.048373	66.360910
1413.107023	50.770627	66.365914
1412.410988	51.631905	66.370919
1411.825235	44.138225	66.375924
1411.168222	56.226047	66.380929
1410.395038	48.875696	66.385934
1409.587461	50.689845	66.390938
1408.387274	57.270494	66.395943
1408.410664	48.740122	66.400948
1407.418673	54.232688	66.405953
1407.452360	48.152867	66.410958
1406.999393	53.006244	66.415962
1406.109255	52.960078	66.420967
1405.419655	48.480721	66.425972
1404.502714	57.313994	66.430977
1404.205860	49.730241	66.435982
1402.948963	47.692311	66.440986
1401.831011	54.247274	66.445991
1401.911369	43.430709	66.450996
1401.213276	51.849147	66.456001
1401.111573	49.231790	66.461006
1399.947112	54.698154	66.466010
1399.097469	49.381634	66.471015
1398.499137	48.582609	66.476020
1398.008075	55.179862	66.481025
1397.554663	48.305398	66.486030
1396.524280	52.329604	66.491034
1395.493040	53.930147	66.496039
1395.154068	47.950560	66.501044
1394.528786	60.001804	66.506049
1394.144210	50.298355	66.511054
1393.270850	49.850554	66.516058
1392.279564	58.791844	66.521063
1391.805172	42.654453	66.526068
1391.552867	46.657490	66.531073
1390.847475	46.917859	66.536078
1390.248036	52.829010	66.541082
1389.293632	56.334936	66.546087
1389.001303	48.789891	66.551092
1388.308777	55.094312	66.556097
1386.842661	52.854676	66.561102
1386.215007	52.372553	66.566106
1385.648976	58.729411	66.571111
1385.439288	43.611247	66.576116
1384.963152	57.534298	66.581121
1384.453450	51.368958	66.586126
1383.650703	53.557665	66.591130
1382.741498	55.239742	66.596135
1382.340091	48.060546	66.601140
1381.463653	47.406656	66.606145
1380.332568	40.510605	66.611150
1379.785300	40.876731	66.616154
1379.161557	44.475181	66.621159
1378.773908	41.982126	66.626164
1378.429329	52.648326	66.631169
1377.673759	48.132154	66.636174
1377.007673	49.931708	66.641178
1376.164292	53.385297	66.646183
1375.655196	43.859347	66.651188
1374.322259	57.844472	66.656193
1373.495527	46.054021	66.661198
1373.257923	50.234497	66.666202
1372.599904	51.668490	66.671207
1372.601307	48.440230	66.676212
1372.184379	59.220437	66.681217
1370.917259	46.965396	66.686222
1370.464651	48.338353	66.691226
1369.802376	54.994363	66.696231
1368.961465	48.547358	66.701236
1367.655679	48.870053	66.706241
1367.096139	46.125199	66.711246
1366.839150	47.957499	66.716250
1366.421841	59.341746	66.721255
1365.979129	45.120074	66.726260
1364.878175	58.719818	66.731265
1364.080924	55.859783	66.736270
1363.744377	55.031769	66.741274
1363.301891	51.060352	66.746279
1362.051466	47.233133	66.751284
1361.074899	51.002789	66.756289
1360.725003	46.765918	66.761294
1360.456561	46.056391	66.766298
1359.639037	55.283883	66.771303
1359.328542	43.622694	66.776308
1358.197316	49.653075	66.781313
1357.474769	50.023414	66.786318
1357.217715	45.136268	66.791322
1356.266482	47.906832	66.796327
1355.431978	41.829404	66.801332
1354.399350	46.607770	66.806337
1354.124016	45.158165	66.811342
1353.550197	43.596733	66.816346
1353.113292	49.884180	66.821351
1352.954495	51.691410	66.826356
1351.732785	49.917574	66.831361
1351.257226	55.047365	66.836366
1350.863611	53.621293	66.841370
1349.704714	56.879038	66.846375
1348.698395	52.347541	66.851380
1348.114841	49.392041	66.856385
1347.455424	54.363400	66.861390
1347.559308	48.302386	66.866394
1346.522696	52.359139	66.871399
1345.330966	46.310113	66.876404
1344.605852	51.291916	66.881409
1344.111377	48.408990	66.886414
1344.116541	40.105455	66.891418
1343.358830	49.066394	66.896423
1342.378908	45.047951	66.901428
1341.535095	53.200980	66.906433
1341.085053	47.718457	66.911438
1340.598354	51.115356	66.916442
1340.072728	47.543518	66.921447
1339.305705	42.026231	66.926452
1338.531369	43.863502	66.931457
1338.295264	48.972574	66.936462
1337.355440	44.603980	66.941466
1336.222678	45.760209	66.946471
1335.747440	48.615964	66.951476
1334.970420	43.970753	66.956481
1334.614953	49.518274	66.961486
1334.274375	50.548572	66.966490
1333.033585	52.420572	66.971495
1332.854903	54.527435	66.976500
1331.865959	50.603470	66.981505
1330.988315	46.029450	66.986510
1330.374772	49.429167	66.991514
1329.738978	49.218015	66.996519
1329.544083	44.168026	67.001524
1328.899072	51.705976	67.006529
1327.861909	49.339837	67.011534
1327.344764	44.189688	67.016538
1326.579639	43.988058	67.021543
1326.367974	42.580374	67.026548
1324.968737	48.850494	67.031553
1324.081702	44.262200	67.036558
1323.750140	39.136168	67.041562
1322.947680	43.898454	67.046567
1322.999565	43.812950	67.051572
1322.182669	47.437386	67.056577
1321.510129	40.747593	67.061582
1320.785788	40.388092	67.066586
1320.222426	49.314985	67.071591
1319.271130	42.604850	67.076596
1318.100236	47.635447	67.081601
1317.645433	40.149366	67.086606
1317.202825	37.204586	67.091610
1316.820233	49.702954	67.096615
1316.485769	43.400967	67.101620
1315.587345	53.661625	67.106625
1314.603321	48.065301	67.111630
1314.438297	44.442451	67.116634
1313.282052	44.134268	67.121639
1313.058920	37.115989	67.126644
1311.906435	47.300338	67.131649
1310.975683	41.272923	67.136654
1310.706302	42.129477	67.141658
1309.811503	53.794638	67.146663
1309.933913	49.481112	67.151668
1308.448514	55.917906	67.156673
1307.732450	53.070215	67.161678
1307.410588	50.101508	67.166682
1306.532589	55.005123	67.171687
1306.340506	47.609739	67.176692
1305.577825	45.744027	67.181697
1304.841575	53.600842	67.186702
1304.772870	52.097891	67.191706
1303.626964	51.794376	67.196711
1302.878260	46.813511	67.201716
1302.057628	53.786448	67.206721
1301.390650	46.280483	67.211726
1301.288379	46.500185	67.216730
1299.680245	48.704993	67.221735
1298.953551	53.324355	67.226740
1298.660719	55.537678	67.231745
1298.150988	50.512513	67.236750
1297.707949	48.313708	67.241754
1297.305462	55.581295	67.246759
1295.980398	46.308096	67.251764
1295.464798	53.300349	67.256769
1295.284497	47.979958	67.261774
1294.941710	45.659560	67.266778
1293.608033	54.447150	67.271783
1292.862854	50.424523	67.276788
1292.716124	50.222359	67.281793
1291.199761	56.578929	67.286798
1290.559213	50.153716	67.291802
1289.938046	59.772636	67.296807
1289.503621	41.451138	67.301812
1289.095334	54.431415	67.306817
1288.584083	52.383807	67.311822
1287.865845	49.873940	67.316826
1286.728603	53.443661	67.321831
1286.118033	47.653934	67.326836
1285.789775	53.205018	67.331841
1285.294398	52.624620	67.336846
1284.218348	49.958751	67.341850
1283.244761	64.329910	67.346855
1283.007618	50.004614	67.351860
1282.553274	51.324244	67.356865
1281.461465	50.179501	67.361870
1280.995252	44.612832	67.366874
1280.134545	51.551143	67.371879
1279.675010	50.176564	67.376884
1279.362820	50.685111	67.381889
1278.318630	57.031273	67.386894
1277.718654	51.413328	67.391898
1276.936055	49.487713	67.396903
1276.774016	54.471472	67.401908
1276.133483	53.721764	67.406913
1274.889791	58.897998	67.411918
1274.476372	46.756447	67.416922
1273.888935	49.527547	67.421927
1273.454275	49.052617	67.426932
1271.925398	56.026202	67.431937
1271.548243	50.517914	67.436942
1271.194850	50.052140	67.441946
1270.834425	54.023490	67.446951
1270.124338	44.275637	67.451956
1268.917154	52.049636	67.456961
1268.445793	57.456318	67.461966
1267.981961	49.591631	67.466970
1267.094846	55.619506	67.471975
1265.741600	50.924007	67.476980
1265.549798	50.030416	67.481985
1265.042468	54.608601	67.486990
1264.529257	54.418975	67.491994
1264.136262	54.285931	67.496999
1263.700129	58.575251	67.502004
1262.674420	48.287795	67.507009
1262.279924	49.192633	67.512014
1261.482824	48.228123	67.517018
1260.200276	56.507701	67.522023
1259.343784	52.275700	67.527028
1258.918800	55.240173	67.532033
1258.572899	56.528373	67.537038
1258.202825	48.429584	67.542042
1257.102832	45.668186	67.547047
1256.359276	53.781640	67.552052
1255.928465	46.935159	67.557057
1255.232558	54.369251	67.562062
1255.132784	50.855880	67.567066
1253.862844	61.883688	67.572071
1253.079616	48.676564	67.577076
1252.675438	59.317553	67.582081
1252.193971	60.843354	67.587086
1251.548910	55.309856	67.592090
1250.444498	56.214031	67.597095
1249.674561	57.096564	67.602100
1249.329688	54.374377	67.607105
1248.989267	49.882127	67.612110
1248.194336	50.718172	67.617114
1247.073939	59.716302	67.622119
1246.413220	48.098209	67.627124
1246.409178	48.769077	67.632129
1245.473791	47.310893	67.637134
1244.847325	45.358886	67.642138
1244.036697	55.714414	67.647143
1243.348090	52.176398	67.652148
1243.087892	59.831377	67.657153
1242.211025	53.054244	67.662158
1241.792663	47.929410	67.667162
1240.879947	52.581518	67.672167
1239.715442	52.023943	67.677172
1238.917884	50.703120	67.682177
1237.921969	49.014864	67.687182
1237.897696	47.388157	67.692186
1237.662484	53.260343	67.697191
1237.681199	49.294468	67.702196
1236.867374	53.364723	67.707201
1235.307578	51.830784	67.712206
1235.035519	46.394104	67.717210
1233.529687	45.192211	67.722215
1233.198319	46.935422	67.727220
1232.397688	49.082835	67.732225
1232.049512	58.268843	67.737230
1231.808735	50.207848	67.742234
1231.309289	53.592599	67.747239
1230.430341	50.701446	67.752244
1229.525725	58.733285	67.757249
1228.810212	53.796051	67.762254
1228.482376	54.557829	67.767258
1227.051387	63.154344	67.772263
1226.644543	46.862764	67.777268
1226.030834	52.441895	67.782273
1225.645062	60.799668	67.787278
1225.212669	56.493935	67.792282
1224.016945	51.836491	67.797287
1223.223619	52.940372	67.802292
1222.858698	55.204588	67.807297
1222.352418	54.072420	67.812302
1221.997487	50.528662	67.817306
1221.167456	56.910175	67.822311
1220.205448	57.501558	67.827316
1220.004802	50.208474	67.832321
1218.732414	53.610477	67.837326
1217.998699	45.875454	67.842330
1217.243365	49.144775	67.847335
1216.726657	50.788149	67.852340
1216.823537	57.684598	67.857345
1215.796018	55.011042	67.862350
1214.916566	51.165911	67.867354
1214.275696	58.812036	67.872359
1213.460241	44.421026	67.877364
1213.532481	47.000507	67.882369
1211.868794	53.460968	67.887374
1211.776939	47.322273	67.892378
1210.658815	57.042302	67.897383
1210.399231	58.884490	67.902388
1210.338895	54.096971	67.907393
1209.060975	55.445072	67.912398
1208.306075	46.319384	67.917402
1207.587309	53.933740	67.922407
1207.322764	40.301963	67.927412
1206.380929	50.252579	67.932417
1205.617382	57.978138	67.937422
1205.173537	54.956303	67.942426
1204.584303	58.401068	67.947431
1203.886840	49.305671	67.952436
1202.552234	51.476503	67.957441
1201.656568	54.299787	67.962446
1201.450594	42.068504	67.967450
1201.090376	54.695784	67.972455
1200.946744	56.781310	67.977460
1200.396077	53.407453	67.982465
1199.352542	51.562781	67.987470
1199.068258	46.730452	67.992474
1197.396629	51.810764	67.997479
1196.455249	45.632120	68.002484
1195.978780	50.441951	68.007489
1195.537037	57.332586	68.012494
1195.884461	49.436683	68.017498
1194.997435	48.555882	68.022503
1194.048767	44.120945	68.027508
1193.317704	51.210551	68.032513
1192.429474	54.663441	68.037518
1192.352394	47.289211	68.042522
1190.939966	52.558545	68.047527
1190.213702	52.399661	68.052532
1190.142349	45.051331	68.057537
1189.524312	48.726183	68.062542
1188.664539	44.524695	68.067546
1187.837411	52.399138	68.072551
1187.370421	52.834541	68.077556
1187.233691	46.348168	68.082561
1185.376998	56.097346	68.087566
1184.785366	49.006796	68.092570
1184.207883	53.419528	68.097575
1183.892921	50.369318	68.102580
1183.816408	48.358255	68.107585
1182.686652	56.151517	68.112590
1182.050669	47.913682	68.117594
1181.659709	58.096829	68.122599
1180.649895	46.387620	68.127604
1179.645313	49.758091	68.132609
1178.783026	51.943710	68.137614
1178.510350	55.066900	68.142618
1177.725007	56.893352	68.147623
1177.668256	51.047123	68.152628
1177.201535	46.153923	68.157633
1175.835039	52.904614	68.162638
1175.342871	48.047000	68.167642
1174.816194	60.057356	68.172647
1174.091297	51.739043	68.177652
1173.106482	53.193515	68.182657
1172.590728	59.851495	68.187662
1172.363517	51.278993	68.192666
1171.467614	53.509385	68.197671
1171.015684	56.686314	68.202676
1170.148999	58.159849	68.207681
1169.246827	56.237514	68.212686
1169.094777	55.591500	68.217690
1168.133662	46.667358	68.222695
1167.004360	58.311499	68.227700
1166.635459	50.048540	68.232705
1166.009174	51.463343	68.237710
1165.548939	57.308241	68.242714
1165.265745	52.794289	68.247719
1164.126019	57.275942	68.252724
1163.591831	57.736228	68.257729
1162.972378	61.868634	68.262734
1162.172192	49.033258	68.267738
1161.464095	42.700835	68.272743
1160.607083	48.870608	68.277748
1160.202008	51.324145	68.282753
1159.277658	53.898112	68.287758
1158.859549	49.388272	68.292762
1157.879758	45.256346	68.297767
1157.412243	48.501986	68.302772
1157.216983	55.556853	68.307777
1156.411578	56.271588	68.312782
1155.494116	49.068861	68.317786
1154.602881	59.300033	68.322791
1154.201261	53.439265	68.327796
1154.076993	45.519031	68.332801
1152.946914	46.083551	68.337806
1152.262360	41.433162	68.342810
1151.500992	51.271512	68.347815
1151.063106	51.907298	68.352820
1150.372560	44.543907	68.357825
1149.432759	53.229492	68.362830
1148.941795	44.203779	68.367834
1148.364218	49.602133	68.372839
1147.534501	46.845110	68.377844
1147.111906	47.942092	68.382849
1146.119836	44.521757	68.387854
1146.186946	44.878531	68.392858
1145.256646	50.394486	68.397863
1144.013524	47.755252	68.402868
1143.513079	48.153405	68.407873
1143.007069	51.395709	68.412878
1142.691920	43.177828	68.417882
1141.609741	45.239157	68.422887
1140.751615	47.687479	68.427892
1140.296643	40.091084	68.432897
1139.635958	49.072901	68.437902
1139.470501	47.042871	68.442906
1138.060708	56.579076	68.447911
1137.538454	49.669894	68.452916
1137.241650	59.650411	68.457921
1136.696363	61.550660	68.462926
1135.602445	57.239770	68.467930
1135.007990	57.231828	68.472935
1134.219178	55.364017	68.477940
1134.100416	48.449012	68.482945
1133.239910	55.814688	68.487950
1132.341202	56.459114	68.492954
1131.701014	56.184055	68.497959
1131.260470	49.137300	68.502964
1130.666375	51.095774	68.507969
1129.449367	55.681196	68.512974
1128.773236	50.245720	68.517978
1128.354998	57.873797	68.522983
1127.858252	49.024050	68.527988
1127.727470	48.526044	68.532993
1126.491819	51.576892	68.537998
1126.016135	47.478342	68.543002
1125.374930	46.924324	68.548007
1124.241097	41.724078	68.553012
1123.457617	39.945311	68.558017
1122.766061	44.879247	68.563022
1122.533683	36.186159	68.568026
1122.082478	45.336510	68.573031
1121.464523	45.611430	68.578036
1120.773336	48.760187	68.583041
1119.296671	46.221190	68.588046
1119.026852	47.673925	68.593050
1118.748595	43.898793	68.598055
1117.926383	51.155878	68.603060
1117.133912	49.388005	68.608065
1116.326597	57.071657	68.613070
1116.335468	51.848935	68.618074
1115.586482	51.917616	68.623079
1114.629896	55.947532	68.628084
1114.437834	45.201129	68.633089
1113.313713	50.888271	68.638094
1112.365357	44.956780	68.643098
1111.651879	49.645046	68.648103
1111.110728	49.157119	68.653108
1110.568641	37.045553	68.658113
1109.802326	53.477977	68.663118
1109.735425	47.526136	68.668122
1108.643234	47.129009	68.673127
1107.846161	42.474454	68.678132
1107.651044	30.782371	68.683137
1106.851680	55.073322	68.688142
1105.494112	45.605138	68.693146
1105.218447	46.018008	68.698151
1104.637100	49.325918	68.703156
1104.509232	46.930364	68.708161
1103.536830	54.540928	68.713166
1102.758515	42.006461	68.718170
1102.014436	50.277724	68.723175
1101.446398	49.590647	68.728180
1101.102447	47.267311	68.733185
1099.971496	46.695003	68.738190
1099.389991	47.790460	68.743194
1099.270205	49.927389	68.748199
1097.890495	52.379840	68.753204
1097.138346	42.482626	68.758209
1096.360628	48.974119	68.763214
1096.347329	40.074298	68.768218
1095.803893	38.169049	68.773223
1094.530174	45.912695	68.778228
1094.004549	35.664064	68.783233
1093.201379	40.995805	68.788238
1092.986746	42.755156	68.793242
1092.554492	41.346313	68.798247
1091.131984	36.699785	68.803252
1090.515505	38.051543	68.808257
1089.746870	42.015298	68.813262
1089.916755	44.363195	68.818266
1089.106150	46.089610	68.823271
1087.998699	52.289777	68.828276
1087.649898	43.080620	68.833281
1087.038328	47.576061	68.838286
1086.414661	44.940827	68.843290
1085.440191	46.559267	68.848295
1084.530581	53.628412	68.853300
1084.139872	47.690232	68.858305
1083.755582	46.311608	68.863310
1083.295369	41.970910	68.868314
1082.403812	45.928990	68.873319
1081.428682	47.968585	68.878324
1081.268310	50.140355	68.883329
1079.378230	44.902728	68.888334
1079.288420	42.633588	68.893338
1078.900487	39.342691	68.898343
1078.207161	51.016853	68.903348
1077.869804	45.622126	68.908353
1077.224387	51.783496	68.913358
1076.434701	50.491435	68.918362
1076.006465	41.831085	68.923367
1075.199079	43.148559	68.928372
1074.042644	37.414191	68.933377
1073.233348	51.579477	68.938382
1072.628927	44.095180	68.943386
1072.366932	51.219008	68.948391
1071.625930	42.650987	68.953396
1071.693300	33.864497	68.958401
1070.446448	52.773499	68.963406
1069.990895	51.374673	68.968410
1069.101893	44.139074	68.973415
1067.995186	44.482293	68.978420
1067.811279	37.005227	68.983425
1066.791483	38.567804	68.988430
1066.397394	42.173939	68.993434
1065.849335	42.481910	68.998439
1064.673863	52.668426	69.003444
1064.144854	45.858114	69.008449
1063.623926	60.956833	69.013454
1062.932654	52.246857	69.018458
1063.018849	49.083967	69.023463
1061.893376	45.025719	69.028468
1061.393903	43.774232	69.033473
1060.647586	49.557414	69.038478
1059.647224	43.487562	69.043482
1058.840421	42.822708	69.048487
1058.055958	56.749084	69.053492
1057.903997	46.217087	69.058497
1057.099806	51.545850	69.063502
1056.426332	38.269326	69.068506
1055.805472	42.144927	69.073511
1054.842135	47.707164	69.078516
1054.499350	39.446391	69.083521
1053.922429	49.406806	69.088526
1053.637407	34.346450	69.093530
1052.971144	45.563720	69.098535
1052.086005	50.023839	69.103540
1050.917130	44.181072	69.108545
1050.034054	48.019540	69.113550
1049.336289	47.386229	69.118554
1049.249413	40.079810	69.123559
1048.641933	43.598468	69.128564
1048.439356	43.958717	69.133569
1047.236992	42.338075	69.138574
1046.817375	44.968982	69.143578
1046.268002	46.142917	69.148583
1045.253551	51.021004	69.153588
1044.639156	35.861659	69.158593
1043.463094	47.212069	69.163598
1043.427111	47.859632	69.168602
1042.822497	45.210340	69.173607
1041.827031	51.783796	69.178612
1041.018952	40.791630	69.183617
1040.525282	48.245626	69.188622
1040.338529	42.651906	69.193626
1039.501650	44.888721	69.198631
1038.067832	53.231877	69.203636
1037.981744	42.260473	69.208641
1037.191700	41.848428	69.213646
1037.104518	49.296107	69.218650
1036.275216	42.565115	69.223655
1035.034902	50.178894	69.228660
1034.734566	47.208384	69.233665
1034.279730	51.109619	69.238670
1033.373191	40.369664	69.243674
1032.750449	47.251258	69.248679
1032.143271	49.798464	69.253684
1031.738439	41.271598	69.258689
1030.447766	43.921231	69.263694
1029.629379	47.407213	69.268698
1029.443682	45.203793	69.273703
1029.110530	49.757456	69.278708
1028.396951	41.584062	69.283713
1027.120327	47.826932	69.288718
1026.446241	37.562515	69.293722
1026.308598	33.325059	69.298727
1025.564249	45.100382	69.303732
1024.779201	38.466436	69.308737
1023.688915	43.017546	69.313742
1023.213378	42.333118	69.318746
1023.079548	40.394262	69.323751
1022.371317	52.099190	69.328756
1021.449422	37.430322	69.333761
1020.504652	43.774941	69.338766
1020.332422	48.498546	69.343770
1019.837019	43.789721	69.348775
1018.718235	45.642457	69.353780
1018.057625	37.990501	69.358785
1017.477830	46.943698	69.363790
1017.331838	45.438863	69.368794
1016.346976	37.460023	69.373799
1015.249656	47.181532	69.378804
1014.827737	33.582733	69.383809
1014.292725	34.292341	69.388814
1013.758090	38.780284	69.393818
1012.666319	25.228139	69.398823
1012.036492	41.120027	69.403828
1011.622170	41.474542	69.408833
1011.174085	43.329387	69.413838
1010.414160	41.583180	69.418842
1009.445734	36.087019	69.423847
1008.765228	44.371837	69.428852
1008.615376	35.072705	69.433857
1007.501987	47.509144	69.438862
1006.810315	46.035932	69.443866
1006.610126	38.525195	69.448871
1005.970930	48.791991	69.453876
1005.043856	42.757814	69.458881
1003.904068	44.339507	69.463886
1003.474354	41.361200	69.468890
1003.005870	43.129405	69.473895
1002.452145	44.952173	69.478900
1001.892214	43.767087	69.483905
1000.773178	49.943897	69.488910
1000.278774	48.171219	69.493914
1000.034579	38.456585	69.498919
998.600028	46.661100	69.503924
997.544383	44.965100	69.508929
997.084061	41.223686	69.513934
996.876139	44.208850	69.518938
996.825969	47.129493	69.523943
996.054986	51.084187	69.528948
995.647983	48.490200	69.533953
994.607173	49.176205	69.538958
994.170310	47.764959	69.543962
992.743912	49.912654	69.548967
991.954681	46.794428	69.553972
991.595309	38.457461	69.558977
991.075588	50.889341	69.563982
990.734772	42.369646	69.568986
990.033084	44.406770	69.573991
988.699951	46.187965	69.578996
988.508380	43.037731	69.584001
987.931369	51.060085	69.589006
987.072383	46.306612	69.594010
986.536311	45.060964	69.599015
985.590306	53.632462	69.604020
985.641421	43.974922	69.609025
984.869722	46.625585	69.614030
983.915424	48.540475	69.619034
983.547135	46.919624	69.624039
982.268331	47.156219	69.629044
981.151247	41.303673	69.634049
980.494325	41.988530	69.639054
980.016703	36.619296	69.644058
979.666479	39.292786	69.649063
979.296365	48.520134	69.654068
979.140033	40.403178	69.659073
978.512001	35.184033	69.664078
977.402380	41.652665	69.669082
976.878196	36.103182	69.674087
975.786405	46.604419	69.679092
974.949370	42.836214	69.684097
974.266859	48.205561	69.689102
973.761736	45.442686	69.694106
973.677658	40.799316	69.699111
972.768150	46.950683	69.704116
971.918976	41.746223	69.709121
971.395316	50.947541	69.714126
970.584928	41.595812	69.719130
969.962716	41.890370	69.724135
968.920480	48.750411	69.729140
968.493121	48.573995	69.734145
968.135086	43.269313	69.739150
967.789685	46.124966	69.744154
966.746066	45.797444	69.749159
965.775987	50.714230	69.754164
965.429215	44.486811	69.759169
964.896409	47.105776	69.764174
964.001392	43.797811	69.769178
963.383231	40.482066	69.774183
962.443505	52.807313	69.779188
962.272474	44.651694	69.784193
961.454977	41.189470	69.789198
960.684657	38.230675	69.794202
960.253574	35.668914	69.799207
959.603183	47.083945	69.804212
958.824900	42.554188	69.809217
957.852557	46.020532	69.814222
957.500381	46.150701	69.819226
957.123101	43.987234	69.824231
955.826183	45.357405	69.829236
955.293056	37.349294	69.834241
954.704252	39.248615	69.839246
954.041110	40.238821	69.844250
953.997427	35.215287	69.849255
952.356294	34.500297	69.854260
952.088046	40.265779	69.859265
951.263276	38.607180	69.864270
950.804603	45.629838	69.869274
950.443709	45.966400	69.874279
949.513109	45.215623	69.879284
948.945792	41.275200	69.884289
948.273892	43.788567	69.889294
947.223983	44.526502	69.894298
946.497695	38.256976	69.899303
945.847553	41.325124	69.904308
945.739822	42.144953	69.909313
945.172129	48.103166	69.914318
944.355769	42.448793	69.919322
943.785086	44.879823	69.924327
942.615996	46.948754	69.929332
942.582861	40.837016	69.934337
941.369949	41.692354	69.939342
940.383014	40.775503	69.944346
940.072561	39.796741	69.949351
939.341501	51.360233	69.954356
938.945335	41.903181	69.959361
938.984154	38.445056	69.964366
937.604626	45.500703	69.969370
937.218161	29.418888	69.974375
936.261265	43.210282	69.979380
935.317452	38.429329	69.984385
934.568592	39.157212	69.989390
934.053520	36.798055	69.994394
933.871709	34.485218	69.999399
933.324019	36.264460	70.004404
932.714151	34.237357	70.009409
931.650274	40.807537	70.014414
931.118157	36.995560	70.019418
930.468278	34.191077	70.024423
929.240799	46.111104	70.029428
928.809392	31.160813	70.034433
928.153195	34.223620	70.039438
927.558616	37.601476	70.044442
927.259563	34.282272	70.049447
926.350085	35.262798	70.054452
925.509758	40.657265	70.059457
924.968040	37.780378	70.064462
924.956073	41.786195	70.069466
923.931900	37.295580	70.074471
923.116615	39.508492	70.079476
922.481945	35.427408	70.084481
921.899029	41.641934	70.089486
920.387416	36.315828	70.094490
920.020466	42.226329	70.099495
919.477027	41.989545	70.104500
919.367517	27.546281	70.109505
919.151881	40.533743	70.114510
918.005799	41.550346	70.119514
917.404885	43.427948	70.124519
916.773995	53.508934	70.129524
915.639990	45.561755	70.134529
914.936083	45.330007	70.139534
914.342968	50.297210	70.144538
914.112193	40.954196	70.149543
912.941537	46.391773	70.154548
912.152865	41.874725	70.159553
911.602636	37.084767	70.164558
910.865759	41.560757	70.169562
910.963384	38.929063	70.174567
910.075265	51.749158	70.179572
909.193666	48.494271	70.184577
908.775283	49.883934	70.189582
907.787056	45.691957	70.194586
907.567196	31.613183	70.199591
906.331852	40.248087	70.204596
905.608293	41.952820	70.209601
905.040604	41.328812	70.214606
905.070395	37.891048	70.219610
904.016660	36.237364	70.224615
903.246257	43.811106	70.229620
902.381795	45.669151	70.234625
902.158309	49.502048	70.239630
901.430837	55.307501	70.244634
900.356931	44.564279	70.249639
899.922652	54.571402	70.254644
899.376811	45.688536	70.259649
898.789036	45.146574	70.264654
897.598611	47.862320	70.269658
897.227278	43.136935	70.274663
896.874477	43.207288	70.279668
896.406390	39.334667	70.284673
895.148576	41.851401	70.289678
894.347437	47.693808	70.294682
894.273018	45.236148	70.299687
893.585282	47.335732	70.304692
892.485995	44.131265	70.309697
891.956435	41.634074	70.314702
890.989236	45.456016	70.319706
890.988544	43.546444	70.324711
890.133208	37.275398	70.329716
888.877854	44.834856	70.334721
888.334146	43.948415	70.339726
887.737583	41.288422	70.344730
887.571476	46.282291	70.349735
887.159198	45.340240	70.354740
886.544189	39.628616	70.359745
885.551650	42.211948	70.364750
884.437871	42.455446	70.369754
884.151116	43.589198	70.374759
882.994041	37.514409	70.379764
882.842379	37.994301	70.384769
882.522201	34.580694	70.389774
881.467542	40.788301	70.394778
881.177201	36.201420	70.399783
880.037596	44.623981	70.404788
879.888443	45.027780	70.409793
878.742839	37.749525	70.414798
877.463546	46.388283	70.419802
877.455911	40.114797	70.424807
876.938547	40.310690	70.429812
876.147873	39.137125	70.434817
875.680912	46.687814	70.439822
874.515511	40.932898	70.444826
874.484351	39.299413	70.449831
873.669183	47.354952	70.454836
873.070788	36.403610	70.459841
872.087402	40.146131	70.464846
870.799349	41.068655	70.469850
870.705762	37.287827	70.474855
870.508346	43.862058	70.479860
870.061353	39.788967	70.484865
869.266309	36.614941	70.489870
868.522850	39.620687	70.494874
867.816465	32.964823	70.499879
866.197646	46.490995	70.504884
865.963467	47.389300	70.509889
865.893657	40.452348	70.514894
865.154769	40.279798	70.519898
865.043601	27.798544	70.524903
863.643930	36.721390	70.529908
862.876050	40.811240	70.534913
862.633527	44.440586	70.539918
861.279331	40.302145	70.544922
860.879622	39.037977	70.549927
859.609347	41.701791	70.554932
859.662553	43.074753	70.559937
859.460857	41.277598	70.564942
858.493882	43.241858	70.569946
857.503496	49.067085	70.574951
856.837132	49.442815	70.579956
856.552430	46.931892	70.584961
855.906542	47.290171	70.589966
854.386618	46.969116	70.594970
854.114382	36.118836	70.599975
853.756462	43.489745	70.604980
853.259220	39.992359	70.609985
852.723947	38.939003	70.614990
851.767019	44.352050	70.619994
851.058426	41.791899	70.624999
850.455394	46.697613	70.630004
849.815987	43.479898	70.635009
848.855331	44.653100	70.640014
847.941688	52.722745	70.645018
847.778246	38.868389	70.650023
847.445238	49.438136	70.655028
846.321673	43.895773	70.660033
845.963097	43.610659	70.665038
845.066994	44.352541	70.670042
844.886912	43.938093	70.675047
843.257861	46.091314	70.680052
842.425269	45.485828	70.685057
842.496555	39.292824	70.690062
841.804052	47.764087	70.695066
841.580135	49.296274	70.700071
841.123207	48.638883	70.705076
840.024002	44.081398	70.710081
839.568975	41.171809	70.715086
838.382374	41.341763	70.720090
837.542811	42.662853	70.725095
836.826018	47.678139	70.730100
836.430405	40.315228	70.735105
836.241508	40.873589	70.740110
835.311083	44.740160	70.745114
834.578782	28.634576	70.750119
833.904379	40.116519	70.755124
833.211138	34.273861	70.760129
832.711751	37.237614	70.765134
831.678822	42.088751	70.770138
831.196939	42.715823	70.775143
830.690279	42.452704	70.780148
830.107587	41.469979	70.785153
829.296464	45.650300	70.790158
828.154618	45.712210	70.795162
828.062820	48.563783	70.800167
827.739901	44.538760	70.805172
826.822962	42.314554	70.810177
826.241915	41.342607	70.815182
825.219383	41.672533	70.820186
825.156914	36.043293	70.825191
823.856114	42.681183	70.830196
823.170243	47.442392	70.835201
822.738975	44.571602	70.840206
821.962475	48.426293	70.845210
821.383822	39.520293	70.850215
820.205745	39.408200	70.855220
820.022648	44.231308	70.860225
819.578533	38.524042	70.865230
818.917358	42.472340	70.870234
818.198030	37.217313	70.875239
817.289487	45.921663	70.880244
816.977300	36.211583	70.885249
816.263322	38.980837	70.890254
814.890772	48.465523	70.895258
814.382826	44.662342	70.900263
813.706164	44.219705	70.905268
813.606282	43.220058	70.910273
813.346427	41.627707	70.915278
812.093907	49.041668	70.920282
811.749702	45.092576	70.925287
810.788926	58.624432	70.930292
809.818108	58.249117	70.935297
808.880901	42.288111	70.940302
808.207641	50.986555	70.945306
807.868215	50.348313	70.950311
807.549077	45.004355	70.955316
806.991599	48.732724	70.960321
806.833306	39.550083	70.965326
805.665243	50.486141	70.970330
805.289810	50.490722	70.975335
804.242612	53.100133	70.980340
803.125377	46.555415	70.985345
802.705599	38.146106	70.990350
801.934623	51.155735	70.995354
802.077069	45.577455	71.000359
801.130310	47.268859	71.005364
800.081757	43.300999	71.010369
799.518733	43.701295	71.015374
798.987535	49.805110	71.020378
798.531491	44.303174	71.025383
796.921022	43.919296	71.030388
796.472437	41.379276	71.035393
796.101444	45.850670	71.040398
795.808802	41.306746	71.045402
795.375825	39.915421	71.050407
794.237926	44.958323	71.055412
793.629829	48.614327	71.060417
793.244891	43.238269	71.065422
791.974229	52.386626	71.070426
791.382402	45.040764	71.075431
790.696738	43.533543	71.080436
790.128064	43.876394	71.085441
790.076956	40.271737	71.090446
789.280136	46.064596	71.095450
788.630575	42.548893	71.100455
787.769743	48.665758	71.105460
787.010297	46.189415	71.110465
786.204933	32.109255	71.115470
785.258631	41.948723	71.120474
785.172292	38.430099	71.125479
784.689613	41.129427	71.130484
784.079201	45.258887	71.135489
783.176266	37.128345	71.140494
782.439530	50.476303	71.145498
781.450751	45.393488	71.150503
780.697524	51.518458	71.155508
779.950842	39.056373	71.160513
779.459802	36.480538	71.165518
778.854214	47.587263	71.170522
778.586213	39.846082	71.175527
778.232946	39.221088	71.180532
777.153414	42.796021	71.185537
776.901358	32.589101	71.190542
776.135563	41.062578	71.195546
775.074832	37.244903	71.200551
774.157477	43.616772	71.205556
773.671551	43.238400	71.210561
773.840010	33.524358	71.215566
772.069481	49.919559	71.220570
771.699903	35.615489	71.225575
771.246824	37.531090	71.230580
770.592521	41.949814	71.235585
770.314364	37.228548	71.240590
768.838892	33.563632	71.245594
768.335196	32.254533	71.250599
767.970083	34.745912	71.255604
767.116667	40.975139	71.260609
766.196800	32.643875	71.265614
765.552049	49.269874	71.270618
765.520996	36.357984	71.275623
764.557752	44.197422	71.280628
764.094277	40.215287	71.285633
763.256923	38.252828	71.290638
762.629982	46.502356	71.295642
762.290627	37.252353	71.300647
761.150040	35.626751	71.305652
759.937739	37.961261	71.310657
760.044820	34.474927	71.315662
759.227370	43.286216	71.320666
758.925939	42.265041	71.325671
758.012632	40.186941	71.330676
757.252590	36.384485	71.335681
756.966762	31.555634	71.340686
756.206806	40.641620	71.345690
755.254441	34.573735	71.350695
754.596557	35.858044	71.355700
754.000288	38.584921	71.360705
753.659149	30.211997	71.365710
752.564508	47.057847	71.370714
751.869601	37.544327	71.375719
751.134756	40.842047	71.380724
750.639569	39.129472	71.385729
750.389459	39.060494	71.390734
749.210587	37.354259	71.395738
748.764275	39.661448	71.400743
748.191305	31.287584	71.405748
746.890786	37.356181	71.410753
746.354392	30.572374	71.415758
745.604607	46.639503	71.420762
745.475746	36.342012	71.425767
745.200412	34.854637	71.430772
744.324688	40.403023	71.435777
743.697903	35.533836	71.440782
742.411534	40.671357	71.445786
742.270414	29.128451	71.450791
741.479380	38.340812	71.455796
740.366378	39.785890	71.460801
739.955315	36.430931	71.465806
739.267855	40.511164	71.470810
739.263627	37.767950	71.475815
738.360009	28.022740	71.480820
737.526199	43.229611	71.485825
737.020968	35.746982	71.490830
736.079971	46.109170	71.495834
734.946402	43.470055	71.500839
734.293778	41.888205	71.505844
733.946096	41.025784	71.510849
733.842028	34.065918	71.515854
733.026127	37.665128	71.520858
732.690867	39.049468	71.525863
731.647721	40.067112	71.530868
730.727309	44.074048	71.535873
730.512189	34.406883	71.540878
729.443159	44.316368	71.545882
728.920589	42.707506	71.550887
728.352106	34.474858	71.555892
727.366865	43.204057	71.560897
726.685222	41.043355	71.565902
725.972471	43.279427	71.570906
725.473758	42.090968	71.575911
725.236943	40.531230	71.580916
724.533851	42.390449	71.585921
723.922843	29.241322	71.590926
722.878607	42.542043	71.595930
722.511976	33.268009	71.600935
721.400912	39.442074	71.605940
720.405314	40.400113	71.610945
720.149523	36.634083	71.615950
719.372408	50.344870	71.620954
719.170363	40.715045	71.625959
718.865884	38.871190	71.630964
717.505390	46.414344	71.635969
717.251269	33.312475	71.640974
716.325815	37.052134	71.645978
715.793020	31.810024	71.650983
714.950022	36.985776	71.655988
714.240781	32.139189	71.660993
714.110083	35.820123	71.665998
713.166300	35.773280	71.671002
712.087505	33.428234	71.676007
711.510344	27.920377	71.681012
710.869117	38.968122	71.686017
710.922805	27.134010	71.691022
709.494244	41.926220	71.696026
708.697320	38.668971	71.701031
708.232364	38.456008	71.706036
707.979277	40.536897	71.711041
707.543018	35.246302	71.716046
706.523843	36.775804	71.721050
705.977566	38.394017	71.726055
705.139787	29.559281	71.731060
703.722689	38.221624	71.736065
703.287781	35.860797	71.741070
702.730502	45.496424	71.746074
702.602059	32.771942	71.751079
702.530520	32.922119	71.756084
701.502297	35.831321	71.761089
700.643992	27.171744	71.766094
699.848414	34.959270	71.771098
699.100864	35.012076	71.776103
698.124947	31.166742	71.781108
697.519848	45.783696	71.786113
697.327922	37.595181	71.791118
696.743061	41.372082	71.796122
696.056082	35.140543	71.801127
695.172351	37.189380	71.806132
694.406441	35.371688	71.811137
694.194143	32.046594	71.816142
693.251783	38.100767	71.821146
692.422131	41.844105	71.826151
691.899507	34.337451	71.831156
691.189217	39.310732	71.836161
690.946517	35.608854	71.841166
689.631575	40.195861	71.846170
689.033886	31.874836	71.851175
688.751150	29.388859	71.856180
688.066479	35.823050	71.861185
687.378576	32.296138	71.866190
686.401083	46.447262	71.871194
686.149574	34.431506	71.876199
685.649903	38.630084	71.881204
684.337323	44.667516	71.886209
683.518237	34.339588	71.891214
682.961241	43.666088	71.896218
682.800456	35.389039	71.901223
682.597103	30.922384	71.906228
681.095984	44.010436	71.911233
680.528462	36.482548	71.916238
679.924617	41.263841	71.921242
679.632777	36.502191	71.926247
678.908545	31.732120	71.931252
677.979897	38.224084	71.936257
677.504608	34.627052	71.941262
676.820901	33.493292	71.946266
675.864331	35.250957	71.951271
674.893478	38.225151	71.956276
674.431825	46.183446	71.961281
673.969264	33.848061	71.966286
673.595443	47.433135	71.971290
672.995265	39.894678	71.976295
671.965017	36.297702	71.981300
671.036128	38.271736	71.986305
670.873971	33.951486	71.991310
670.671314	37.744804	71.996314
669.432576	38.616999	72.001319
668.780755	33.813323	72.006324
668.141400	36.130762	72.011329
667.761165	25.403386	72.016334
666.742378	28.648565	72.021338
665.949158	35.014888	72.026343
665.458611	32.311268	72.031348
665.210694	30.392183	72.036353
663.880222	24.826096	72.041358
663.274771	37.724223	72.046362
662.915453	33.712913	72.051367
662.725590	29.903279	72.056372
661.673111	35.960803	72.061377
660.629023	23.123518	72.066382
659.981417	27.474963	72.071386
659.449685	31.481529	72.076391
659.032475	32.235529	72.081396
657.636815	37.614418	72.086401
657.450985	28.942396	72.091406
656.657741	36.664905	72.096410
656.344249	28.256063	72.101415
656.098533	29.837464	72.106420
654.869880	34.822330	72.111425
654.309253	34.965233	72.116430
654.080018	37.584800	72.121434
652.978174	27.527420	72.126439
652.277995	29.247420	72.131444
651.570843	37.821970	72.136449
651.343384	38.377022	72.141454
650.127926	30.860858	72.146458
649.341687	39.178344	72.151463
648.994775	34.379738	72.156468
648.589093	30.096693	72.161473
647.732777	26.976659	72.166478
646.504186	33.218349	72.171482
646.191382	29.373101	72.176487
645.859057	26.010356	72.181492
644.978916	39.822706	72.186497
644.276026	27.758995	72.191502
643.927293	37.501763	72.196506
643.312033	36.297189	72.201511
642.502356	36.850337	72.206516
641.442911	38.837285	72.211521
641.059950	37.307137	72.216526
640.616157	32.613847	72.221530
640.102532	36.535533	72.226535
639.052408	33.714445	72.231540
638.191311	44.119126	72.236545
638.148344	32.601608	72.241550
636.839825	38.124326	72.246554
635.960184	35.790178	72.251559
635.794072	33.192595	72.256564
635.047801	29.359605	72.261569
634.614961	23.576478	72.266574
633.521776	29.112212	72.271578
632.597637	29.234159	72.276583
632.105182	35.172551	72.281588
631.929883	34.123423	72.286593
631.677716	32.545640	72.291598
630.510715	32.346717	72.296602
629.725454	40.588359	72.301607
629.447574	38.360235	72.306612
628.420313	43.732514	72.311617
627.634033	34.966878	72.316622
626.606608	38.751191	72.321626
626.560166	37.456038	72.326631
626.157949	34.834554	72.331636
625.327560	37.830552	72.336641
624.723685	33.120180	72.341646
624.067685	39.921981	72.346650
623.214676	43.164434	72.351655
622.610793	32.909495	72.356660
621.615374	36.537325	72.361665
621.185044	31.348310	72.366670
620.810680	32.970701	72.371674
620.048376	36.842106	72.376679
619.392706	32.035905	72.381684
618.323498	31.137017	72.386689
618.421509	25.138468	72.391694
617.415785	27.094793	72.396698
616.248736	32.104557	72.401703
615.492451	28.750986	72.406708
614.819155	31.496464	72.411713
614.484125	31.729606	72.416718
614.329202	33.883178	72.421722
613.353822	31.996371	72.426727
612.950320	23.953535	72.431732
612.106527	33.762526	72.436737
611.247759	35.939878	72.441742
610.462060	33.251734	72.446746
609.660654	35.183409	72.451751
609.616169	27.219016	72.456756
608.842734	30.720034	72.461761
607.981447	21.272500	72.466766
607.471272	24.485588	72.471770
606.568791	28.573282	72.476775
606.418117	28.015398	72.481780
605.146848	32.019900	72.486785
604.594702	26.429243	72.491790
604.020968	28.796169	72.496794
603.204501	31.323178	72.501799
603.176222	26.658343	72.506804
602.035438	34.757910	72.511809
601.154389	33.040588	72.516814
600.878113	32.182585	72.521818
600.461743	29.459282	72.526823
599.458545	25.930573	72.531828
598.810412	29.659220	72.536833
598.209072	34.900598	72.541838
597.771170	32.631732	72.546842
596.919150	29.673458	72.551847
596.366949	32.262462	72.556852
595.499704	43.101793	72.561857
594.487528	38.998926	72.566862
593.831182	34.166032	72.571866
593.245474	36.796643	72.576871
593.179039	32.394926	72.581876
592.321794	42.346418	72.586881
591.576179	31.071698	72.591886
590.602445	31.269369	72.596890
590.128599	41.418421	72.601895
589.779230	30.670376	72.606900
588.534360	35.750894	72.611905
587.753629	29.446017	72.616910
587.417232	37.419060	72.621914
586.765837	33.181468	72.626919
586.760725	28.072974	72.631924
585.222251	39.933839	72.636929
584.687632	36.994404	72.641934
584.555662	42.167341	72.646938
584.042975	34.466748	72.651943
582.992664	27.629220	72.656948
582.163769	40.514059	72.661953
581.880436	33.081291	72.666958
581.188811	29.195462	72.671962
579.959606	29.842254	72.676967
579.407129	29.859297	72.681972
578.552426	37.944851	72.686977
578.341972	35.193486	72.691982
578.049622	34.628205	72.696986
576.908640	34.062465	72.701991
576.193598	27.952134	72.706996
575.346863	35.132825	72.712001
575.364385	34.097146	72.717006
574.790601	31.774233	72.722010
573.808017	31.329923	72.727015
573.356288	35.897773	72.732020
571.919408	37.605818	72.737025
571.216050	30.536418	72.742030
570.765171	35.067863	72.747034
570.215615	41.852721	72.752039
570.001670	31.415849	72.757044
569.263280	40.317089	72.762049
568.330547	30.604980	72.767054
567.511822	31.307827	72.772058
567.151161	34.044525	72.777063
566.950494	31.340489	72.782068
565.649369	39.061910	72.787073
564.806203	32.891564	72.792078
564.416946	30.707997	72.797082
563.916321	33.306139	72.802087
563.160794	29.242836	72.807092
562.253142	43.464864	72.812097
561.704775	32.412629	72.817102
561.440860	38.313054	72.822106
560.378492	45.677910	72.827111
559.672366	33.613167	72.832116
558.964622	38.854154	72.837121
558.752036	32.573913	72.842126
557.899742	36.585823	72.847130
556.967827	37.508552	72.852135
556.358398	36.104375	72.857140
555.889225	36.256388	72.862145
555.106144	35.032834	72.867150
554.357298	27.108094	72.872154
553.523639	35.715426	72.877159
553.372620	33.295220	72.882164
552.742488	30.494009	72.887169
552.213987	38.273725	72.892174
551.141398	34.013344	72.897178
550.315825	41.534450	72.902183
550.067968	42.934853	72.907188
549.342931	45.376354	72.912193
548.479127	38.458670	72.917198
547.465167	41.917593	72.922202
547.144113	44.113400	72.927207
546.862712	35.101801	72.932212
546.067845	41.916273	72.937217
545.073863	41.733987	72.942222
544.632295	40.948050	72.947226
543.795934	33.324255	72.952231
543.590692	42.552166	72.957236
542.509780	36.776086	72.962241
542.039187	32.347284	72.967246
541.321329	29.542703	72.972250
540.763972	50.180754	72.977255
539.934604	38.802697	72.982260
538.927305	42.780956	72.987265
538.463805	41.850280	72.992270
538.440183	45.616665	72.997274
537.492314	46.169782	73.002279
536.693055	34.977744	73.007284
535.976072	47.592460	73.012289
535.589749	40.469415	73.017294
534.725300	42.702891	73.022298
533.840219	43.421049	73.027303
533.433120	38.094310	73.032308
532.955332	42.139616	73.037313
532.214434	42.770154	73.042318
531.174808	43.855128	73.047322
530.753852	42.835675	73.052327
530.208719	40.686404	73.057332
529.572804	45.572183	73.062337
528.470338	44.787441	73.067342
527.984598	42.351166	73.072346
527.375894	49.941816	73.077351
527.198134	41.691146	73.082356
525.926126	39.886316	73.087361
525.225445	34.688345	73.092366
524.867868	39.726906	73.097370
524.377633	37.934745	73.102375
523.723905	41.399374	73.107380
522.869992	47.576711	73.112385
522.206798	38.797817	73.117390
521.883883	33.388287	73.122394
520.476720	39.131776	73.127399
520.121543	32.511556	73.132404
519.503765	41.532366	73.137409
518.695041	34.946544	73.142414
518.185106	39.534713	73.147418
517.293712	46.886541	73.152423
516.721506	43.161479	73.157428
515.976843	42.209362	73.162433
515.819038	40.856258	73.167438
515.252776	39.267020	73.172442
514.261756	43.594356	73.177447
514.037096	40.252327	73.182452
512.393397	42.696671	73.187457
511.586005	39.103691	73.192462
511.087120	42.452195	73.197466
510.626819	47.332082	73.202471
510.576610	28.922883	73.207476
509.732053	36.510098	73.212481
509.489305	32.754638	73.217486
508.312316	35.044215	73.222490
507.562432	43.307058	73.227495
507.232286	35.919607	73.232500
506.387955	40.720317	73.237505
505.545135	45.714754	73.242510
505.298324	36.994120	73.247514
504.317077	40.848393	73.252519
503.330521	43.478222	73.257524
502.564254	45.685030	73.262529
502.045735	48.527309	73.267534
502.055321	43.421204	73.272538
501.450810	46.687188	73.277543
500.474670	44.081457	73.282548
499.620179	40.221595	73.287553
499.193396	35.809478	73.292558
498.503892	34.913235	73.297562
496.851292	41.233574	73.302567
496.733874	31.285965	73.307572
496.096244	37.151307	73.312577
495.756564	33.737719	73.317582
495.800584	37.680983	73.322586
494.800741	45.076901	73.327591
494.271725	41.606739	73.332596
493.100675	38.806557	73.337601
491.982659	41.003169	73.342606
491.173689	45.550671	73.347610
490.654481	42.700266	73.352615
490.534062	39.781604	73.357620
490.284341	48.499364	73.362625
489.405401	43.441763	73.367630
488.486379	37.903271	73.372634
487.581411	45.709854	73.377639
487.223540	34.644644	73.382644
486.414171	41.075088	73.387649
485.687152	39.610814	73.392654
485.188214	37.616622	73.397658
484.494518	44.414994	73.402663
484.082451	35.091487	73.407668
483.446100	48.384071	73.412673
482.746374	43.927126	73.417678
482.117104	32.277527	73.422682
480.471932	45.574700	73.427687
480.082395	42.325173	73.432692
479.428587	48.704032	73.437697
478.858688	46.054093	73.442702
478.663354	37.323687	73.447706
478.158999	47.285223	73.452711
477.905448	39.579647	73.457716
476.778200	48.533396	73.462721
475.936299	44.990080	73.467726
475.425401	36.439256	73.472730
474.045286	34.077666	73.477735
473.666778	27.748180	73.482740
473.163976	39.713767	73.487745
472.807428	47.106560	73.492750
472.364459	35.195471	73.497754
471.099342	39.799875	73.502759
471.123517	36.702062	73.507764
469.912356	40.567743	73.512769
468.788328	37.323267	73.517774
468.355775	43.655840	73.522778
467.781804	46.626807	73.527783
467.345440	31.535537	73.532788
466.828072	42.727589	73.537793
466.078745	36.889261	73.542798
465.649389	35.298725	73.547802
464.952834	45.961085	73.552807
464.359713	35.310250	73.557812
463.074209	42.477297	73.562817
462.498492	36.381077	73.567822
462.032951	37.701049	73.572826
461.704040	34.175364	73.577831
461.095312	31.118457	73.582836
460.251959	33.632446	73.587841
459.582600	36.516108	73.592846
458.517594	35.471541	73.597850
457.210182	39.440872	73.602855
457.171740	37.242434	73.607860
456.826124	36.788156	73.612865
456.384350	39.838988	73.617870
455.832578	35.218135	73.622874
454.655751	44.143518	73.627879
454.339635	34.859927	73.632884
453.715389	36.818618	73.637889
452.560635	40.148619	73.642894
451.880225	40.667041	73.647898
451.133098	45.838636	73.652903
451.195151	32.328494	73.657908
450.492416	40.719454	73.662913
449.602377	38.030642	73.667918
449.214749	40.678611	73.672922
448.036777	35.353280	73.677927
447.085587	35.706687	73.682932
446.663970	35.464791	73.687937
445.739492	42.340939	73.692942
445.787519	32.769101	73.697946
444.977825	40.063775	73.702951
444.665651	26.078676	73.707956
443.737916	32.346636	73.712961
442.872208	33.659403	73.717966
442.402939	29.604152	73.722970
441.101477	34.062971	73.727975
440.869141	27.700743	73.732980
440.433230	28.128175	73.737985
439.701203	36.478069	73.742990
439.226466	23.414581	73.747994
438.011470	31.048215	73.752999
437.764539	30.117748	73.758004
437.380986	29.732595	73.763009
436.172974	24.954531	73.768014
435.187503	30.397487	73.773018
434.585481	34.049438	73.778023
434.530858	24.853505	73.783028
433.859387	36.689848	73.788033
432.707061	41.539651	73.793038
432.019508	26.453726	73.798042
431.642861	38.500141	73.803047
431.403361	26.946161	73.808052
430.211348	27.676986	73.813057
429.418383	32.633535	73.818062
428.869877	28.174597	73.823066
428.169537	32.493494	73.828071
428.014262	26.842810	73.833076
426.820639	35.621064	73.838081
425.956046	26.136290	73.843086
425.783369	30.169266	73.848090
425.175034	37.886024	73.853095
424.787944	26.226251	73.858100
423.712556	33.290448	73.863105
422.545489	27.848279	73.868110
422.477338	32.976351	73.873114
422.018847	33.093572	73.878119
421.340516	25.749005	73.883124
420.445383	29.215848	73.888129
419.882751	38.797163	73.893134
419.587133	33.810656	73.898138
418.285546	28.282690	73.903143
417.522563	28.090458	73.908148
417.149700	33.227657	73.913153
416.515558	37.458740	73.918158
415.641876	30.102721	73.923162
414.801086	39.048691	73.928167
414.655784	32.525941	73.933172
414.524412	34.565382	73.938177
413.179835	39.242398	73.943182
412.979245	26.879555	73.948186
412.001078	30.779099	73.953191
411.213044	31.516530	73.958196
410.356634	29.560388	73.963201
409.622047	33.998287	73.968206
409.320094	27.519423	73.973210
408.443420	33.419715	73.978215
407.715169	25.800833	73.983220
407.104755	36.171927	73.988225
406.704834	32.290138	73.993230
406.319877	19.951947	73.998234
405.068149	37.333835	74.003239
404.201409	33.166881	74.008244
404.002362	32.700296	74.013249
403.486151	30.759337	74.018254
402.631730	34.516166	74.023258
401.519846	40.286783	74.028263
401.079183	32.656770	74.033268
400.578420	30.189803	74.038273
400.190584	38.308246	74.043278
399.529673	27.600432	74.048282
398.443927	30.886343	74.053287
398.014028	28.589435	74.058292
397.644506	33.070092	74.063297
396.700684	32.063014	74.068302
396.034936	29.329025	74.073306
395.351213	32.823692	74.078311
395.011202	22.263447	74.083316
393.778409	21.617805	74.088321
392.733216	24.703291	74.093326
392.463533	20.677753	74.098330
391.909491	29.776728	74.103335
391.406920	21.450115	74.108340
391.085723	32.450058	74.113345
390.006203	33.818989	74.118350
389.627839	22.069530	74.123354
389.056577	30.089464	74.128359
387.980451	26.957245	74.133364
387.343313	30.373528	74.138369
386.820639	35.848414	74.143374
386.526991	22.424930	74.148378
384.947625	32.914151	74.153383
384.577744	28.723229	74.158388
383.896226	29.582466	74.163393
383.596420	34.767951	74.168398
383.085550	35.355571	74.173402
381.565059	39.497662	74.178407
381.178577	35.140650	74.183412
380.893701	28.217525	74.188417
380.417685	38.417399	74.193422
379.821428	23.197105	74.198426
378.811585	41.467707	74.203431
378.235036	34.088010	74.208436
377.630576	37.489627	74.213441
376.491612	35.789833	74.218446
376.303695	29.642886	74.223450
375.418810	32.858953	74.228455
374.877811	33.421413	74.233460
374.151927	35.465704	74.238465
373.245742	38.229429	74.243470
372.760447	41.522174	74.248474
372.194655	30.239395	74.253479
371.875409	29.700502	74.258484
371.026175	30.841935	74.263489
370.183065	35.686643	74.268494
369.780122	28.517406	74.273498
369.254190	38.412999	74.278503
367.939076	34.960903	74.283508
367.094634	31.350229	74.288513
366.596023	33.845582	74.293518
366.722166	28.206831	74.298522
365.931886	29.037673	74.303527
364.938598	30.411797	74.308532
364.520233	35.513674	74.313537
363.523854	34.172786	74.318542
362.497864	25.814469	74.323546
361.828662	35.363886	74.328551
361.401072	28.510815	74.333556
361.186243	25.485786	74.338561
360.773982	32.477449	74.343566
360.298509	38.870487	74.348570
358.864280	36.254237	74.353575
358.389970	35.952944	74.358580
357.852469	38.732040	74.363585
356.402610	40.068538	74.368590
356.195290	30.620978	74.373594
355.739169	41.076305	74.378599
355.295806	24.790869	74.383604
354.552246	23.505892	74.388609
353.601895	31.609895	74.393614
352.946950	23.331229	74.398618
352.421922	38.132562	74.403623
351.675891	24.554095	74.408628
350.987977	26.705880	74.413633
350.516932	27.676665	74.418638
349.865280	25.550723	74.423642
349.117722	29.132843	74.428647
348.470083	18.465518	74.433652
347.945198	31.839686	74.438657
347.010699	33.292757	74.443662
346.577356	29.048878	74.448666
345.507680	25.305373	74.453671
344.817202	23.977246	74.458676
344.172062	20.673866	74.463681
343.767478	35.877048	74.468686
343.899375	20.253729	74.473690
342.420006	24.523326	74.478695
341.927168	30.144849	74.483700
341.302809	36.145300	74.488705
340.664840	29.414069	74.493710
339.665629	26.454118	74.498714
338.912460	32.445134	74.503719
338.272597	34.778500	74.508724
337.832947	35.192353	74.513729
337.216925	32.294338	74.518734
336.506089	23.579885	74.523738
335.923541	26.798245	74.528743
335.185410	32.272780	74.533748
334.891391	26.999031	74.538753
333.534707	34.537019	74.543758
333.210763	31.371686	74.548762
332.629424	30.310020	74.553767
332.403141	27.416129	74.558772
331.484396	29.866479	74.563777
330.441540	33.844171	74.568782
330.310633	19.858607	74.573786
329.443949	28.685717	74.578791
328.390407	27.877500	74.583796
328.061060	19.330914	74.588801
327.284400	31.365379	74.593806
326.796124	26.452172	74.598810
325.639010	33.136769	74.603815
325.189345	31.492727	74.608820
324.948939	24.076828	74.613825
324.182705	28.988142	74.618830
323.318442	34.206817	74.623834
322.698930	32.990389	74.628839
321.932066	38.876361	74.633844
321.567066	22.611567	74.638849
320.356081	34.403019	74.643854
319.853465	26.551093	74.648858
319.448839	30.807117	74.653863
318.967907	25.927435	74.658868
318.382481	28.679481	74.663873
316.849146	36.086358	74.668878
316.545193	29.868027	74.673882
316.132510	30.290202	74.678887
315.614880	34.094307	74.683892
314.912627	24.900678	74.688897
314.116660	31.716955	74.693902
313.534508	24.599949	74.698906
312.704175	29.152477	74.703911
311.544472	36.236461	74.708916
311.062497	29.273798	74.713921
310.407815	35.731671	74.718926
310.140316	34.821842	74.723930
309.876694	41.624246	74.728935
309.128488	37.876830	74.733940
308.272213	29.901497	74.738945
307.513867	34.119281	74.743950
307.380285	30.398490	74.748954
305.844692	32.770542	74.753959
305.126201	30.965923	74.758964
305.043395	28.124862	74.763969
304.228078	31.000282	74.768974
303.866117	27.495663	74.773978
302.682698	38.516335	74.778983
302.303897	35.832834	74.783988
301.770456	29.091264	74.788993
300.625132	26.880013	74.793998
300.018806	29.308967	74.799002
299.399103	32.249406	74.804007
298.809615	32.639839	74.809012
298.484587	27.539772	74.814017
297.315192	37.142112	74.819022
297.070468	28.933699	74.824026
296.227326	33.286426	74.829031
295.695467	31.595566	74.834036
294.852681	34.186787	74.839041
293.818552	38.951576	74.844046
293.606471	29.459057	74.849050
293.294303	35.766149	74.854055
292.792620	35.298922	74.859060
291.729412	33.514555	74.864065
290.624744	37.754426	74.869070
290.491647	32.089183	74.874074
289.525101	35.770878	74.879079
288.746556	32.469851	74.884084
288.590454	30.790067	74.889089
287.657950	37.249647	74.894094
287.312441	21.235648	74.899098
286.345403	39.280249	74.904103
285.589133	30.659784	74.909108
285.457554	26.407247	74.914113
284.463412	31.205088	74.919118
283.557096	23.959986	74.924122
282.794261	30.249021	74.929127
282.403984	28.986605	74.934132
282.167038	26.323077	74.939137
280.960513	43.002372	74.944142
280.852668	31.197205	74.949146
279.923147	31.982458	74.954151
278.590613	32.161745	74.959156
278.009708	27.094581	74.964161
277.510495	30.380095	74.969166
277.038034	26.475202	74.974170
276.925667	37.579060	74.979175
275.970519	34.016027	74.984180
275.163928	30.109197	74.989185
274.313151	22.776400	74.994190
274.205460	28.033770	74.999194
272.873029	35.552151	75.004199
272.020878	26.617395	75.009204
272.078919	26.488311	75.014209
271.006011	32.238571	75.019214
270.776444	35.712920	75.024218
269.793802	40.535744	75.029223
268.779147	37.075238	75.034228
268.648702	21.252469	75.039233
267.791150	34.123006	75.044238
267.874755	28.595115	75.049242
266.582550	30.821163	75.054247
266.017425	21.678238	75.059252
265.247164	28.257041	75.064257
263.799712	34.855476	75.069262
263.622642	30.419380	75.074266
262.909078	27.663091	75.079271
262.711272	27.483324	75.084276
262.604178	20.738468	75.089281
261.422623	30.713338	75.094286
260.712046	23.449663	75.099290
259.919021	34.931667	75.104295
258.736502	27.881987	75.109300
258.224888	16.729394	75.114305
257.347840	30.844094	75.119310
257.379581	23.637139	75.124314
256.855965	29.441774	75.129319
256.287788	31.158185	75.134324
255.739394	25.127063	75.139329
254.747737	28.959427	75.144334
254.148772	30.422126	75.149338
253.141332	31.024268	75.154343
252.532977	39.318220	75.159348
252.393326	26.357498	75.164353
251.499757	30.992663	75.169358
250.330650	27.190936	75.174362
249.558813	31.352538	75.179367
249.048557	36.715079	75.184372
248.476209	27.516537	75.189377
248.228069	39.436817	75.194382
248.059231	26.261553	75.199386
246.910928	32.958968	75.204391
246.108783	38.628234	75.209396
245.474735	26.642026	75.214401
244.405194	36.252122	75.219406
243.676978	28.691643	75.224410
243.024787	30.632759	75.229415
242.698018	32.078882	75.234420
242.661215	26.259527	75.239425
241.476314	39.097098	75.244430
240.839667	33.549975	75.249434
240.491475	29.194775	75.254439
239.824241	36.668639	75.259444
238.870346	29.137828	75.264449
237.816233	36.436820	75.269454
237.303405	28.479312	75.274458
237.150226	28.634630	75.279463
235.977483	30.530993	75.284468
235.803095	22.087458	75.289473
234.979988	36.163607	75.294478
234.516376	22.779872	75.299482
233.475563	32.199311	75.304487
232.808767	36.593332	75.309492
232.358190	26.925956	75.314497
230.953403	27.430597	75.319502
230.731273	32.081740	75.324506
230.179962	29.394213	75.329511
229.495948	26.573300	75.334516
229.440248	24.702476	75.339521
227.900890	32.884640	75.344526
227.275810	23.487934	75.349530
227.265647	21.748622	75.354535
226.218778	28.082946	75.359540
225.713278	28.840051	75.364545
224.499852	22.170633	75.369550
224.068822	26.131257	75.374554
223.568963	26.993118	75.379559
223.008703	28.034918	75.384564
222.428667	24.484654	75.389569
221.387681	33.071498	75.394574
221.052055	28.268024	75.399578
220.230360	19.356826	75.404583
219.804422	30.433389	75.409588
218.701341	19.580097	75.414593
218.216735	25.750676	75.419598
217.772498	25.066151	75.424602
217.413339	23.841364	75.429607
216.371285	29.168834	75.434612
215.790812	23.854040	75.439617
215.000979	25.959029	75.444622
214.415042	23.996114	75.449626
213.681585	24.623981	75.454631
212.544967	28.867397	75.459636
212.267835	29.272711	75.464641
211.786541	36.630207	75.469646
211.765728	27.578721	75.474650
210.510139	25.741481	75.479655
209.807803	24.913600	75.484660
209.260384	23.863904	75.489665
208.046761	27.592898	75.494670
207.415640	31.192764	75.499674
207.072026	31.140324	75.504679
206.718972	28.113694	75.509684
206.121678	24.900497	75.514689
204.784893	28.923515	75.519694
204.147919	24.136546	75.524698
203.715061	23.559019	75.529703
203.318662	26.982695	75.534708
202.628123	23.145702	75.539713
201.428246	32.054348	75.544718
201.394345	30.493861	75.549722
200.893278	27.143900	75.554727
199.517914	23.056539	75.559732
198.921059	20.459860	75.564737
198.417172	33.737652	75.569742
198.220506	29.504960	75.574746
196.906574	28.638965	75.579751
196.100902	35.165085	75.584756
195.859624	29.425639	75.589761
195.260863	35.910889	75.594766
194.754707	31.667612	75.599770
193.964513	28.336938	75.604775
192.794018	24.928121	75.609780
193.044258	30.940555	75.614785
192.126241	32.487249	75.619790
191.043271	33.465731	75.624794
190.395546	29.025830	75.629799
189.586440	35.877351	75.634804
189.600196	29.985283	75.639809
188.765266	36.484532	75.644814
187.710541	31.727895	75.649818
187.216673	33.588592	75.654823
186.731953	32.697638	75.659828
186.279829	30.547818	75.664833
184.981483	34.623066	75.669838
184.501028	30.984395	75.674842
184.233407	31.872318	75.679847
183.702632	40.314760	75.684852
182.913859	17.653680	75.689857
182.153265	33.744664	75.694862
181.497203	39.532583	75.699866
180.380212	39.128782	75.704871
179.698940	39.940728	75.709876
179.390955	36.602565	75.714881
178.816976	36.498546	75.719886
178.097186	29.051866	75.724890
177.093945	35.256253	75.729895
176.258803	43.427104	75.734900
176.072198	30.171106	75.739905
175.499090	33.704961	75.744910
174.882575	30.210986	75.749914
174.199417	30.220569	75.754919
173.030677	26.880867	75.759924
172.860833	30.186427	75.764929
172.263301	34.965232	75.769934
171.308472	29.577669	75.774938
170.645815	28.163157	75.779943
169.991169	31.891360	75.784948
169.847724	27.284337	75.789953
168.567787	32.086782	75.794958
167.488716	23.743337	75.799962
167.110490	20.766461	75.804967
166.499384	32.577444	75.809972
166.393258	26.955227	75.814977
165.722227	33.330579	75.819982
165.325902	34.343101	75.824986
164.339650	30.990078	75.829991
163.754723	29.064862	75.834996
162.949883	32.162581	75.840001
162.170226	36.590381	75.845006
161.653658	24.870904	75.850010
160.935285	28.987735	75.855015
159.828224	27.368115	75.860020
159.200399	25.082311	75.865025
158.351787	30.388423	75.870030
158.300593	26.671859	75.875034
158.218837	28.547279	75.880039
157.039948	28.459286	75.885044
156.654487	19.218368	75.890049
155.784130	25.418919	75.895054
154.542336	30.614256	75.900058
153.999751	27.516929	75.905063
153.454028	26.709826	75.910068
153.096401	24.658486	75.915073
152.646662	36.338091	75.920078
151.638921	29.908728	75.925082
151.097724	29.662295	75.930087
150.384138	32.778585	75.935092
149.627491	24.659707	75.940097
148.529020	36.073741	75.945102
147.859102	32.261860	75.950106
147.537695	28.400722	75.955111
147.342817	32.676942	75.960116
146.922747	24.103858	75.965121
145.930388	22.808153	75.970126
145.336053	31.557195	75.975130
144.074303	33.827335	75.980135
142.968577	27.929261	75.985140
142.800485	27.404146	75.990145
142.090897	34.399082	75.995150
141.935678	34.108456	76.000154
141.539600	24.984349	76.005159
140.267218	28.613933	76.010164
139.814334	24.152445	76.015169
139.238866	25.327575	76.020174
138.384168	28.942602	76.025178
137.223679	35.777622	76.030183
136.742779	34.307332	76.035188
136.434036	24.866527	76.040193
136.239692	30.825260	76.045198
135.461459	30.862627	76.050202
134.459408	32.045851	76.055207
133.725630	33.818654	76.060212
133.485394	27.905588	76.065217
132.202108	32.137731	76.070222
131.559852	35.876584	76.075226
131.071264	30.050425	76.080231
130.531131	38.183707	76.085236
130.158695	32.760071	76.090241
128.879869	35.215867	76.095246
128.308307	31.777815	76.100250
128.293522	29.652891	76.105255
127.165638	34.088915	76.110260
126.592351	25.873002	76.115265
125.636424	25.109234	76.120270
125.304018	29.360073	76.125274
124.787807	29.652131	76.130279
123.731572	31.646662	76.135284
123.265254	32.823315	76.140289
122.763681	30.681391	76.145294
121.636903	29.812404	76.150298
120.948021	26.571257	76.155303
120.055243	35.024118	76.160308
120.223638	22.996744	76.165313
119.870700	30.010508	76.170318
118.461479	30.378726	76.175322
117.858708	27.425046	76.180327
117.140700	31.343136	76.185332
116.914051	25.855258	76.190337
115.835949	40.109286	76.195342
115.087015	31.700607	76.200346
114.668143	26.401075	76.205351
113.927067	38.163408	76.210356
113.647084	25.928408	76.215361
112.165833	31.934649	76.220366
111.791248	32.311359	76.225370
111.410196	30.154952	76.230375
110.836457	31.361351	76.235380
109.777908	28.395194	76.240385
108.817742	33.001600	76.245390
108.591145	31.158030	76.250394
108.377168	36.091729	76.255399
107.601270	25.437058	76.260404
106.864015	20.368069	76.265409
106.088369	25.378710	76.270414
105.446634	27.283500	76.275418
104.721944	26.626369	76.280423
103.569268	39.329541	76.285428
103.217002	34.289045	76.290433
102.715857	41.479411	76.295438
102.486762	33.569737	76.300442
101.700312	34.023162	76.305447
100.584475	36.575984	76.310452
100.696910	29.143282	76.315457
99.316504	33.018770	76.320462
98.261551	33.374663	76.325466
97.707170	36.164384	76.330471
97.299581	32.350112	76.335476
97.061497	29.442362	76.340481
96.679675	32.215605	76.345486
95.520030	22.286027	76.350490
94.924843	24.030433	76.355495
94.210213	34.113836	76.360500
93.361358	28.075479	76.365505
92.365588	30.082458	76.370510
91.701510	32.646823	76.375514
91.599989	23.836878	76.380519
90.989643	31.312735	76.385524
90.550128	31.508991	76.390529
89.559202	33.606662	76.395534
88.718457	35.055916	76.400538
88.769947	27.468933	76.405543
87.220195	34.101119	76.410548
86.537778	31.197994	76.415553
86.061518	30.370367	76.420558
85.242357	34.908565	76.425562
85.101142	24.597393	76.430567
84.440709	34.022455	76.435572
83.450105	32.001102	76.440577
83.247743	32.959052	76.445582
82.309106	31.128108	76.450586
81.560090	29.293734	76.455591
80.756628	32.280871	76.460596
80.534324	25.237441	76.465601
79.722537	28.517640	76.470606
78.933911	32.470655	76.475610
78.367956	25.791108	76.480615
77.599079	33.123515	76.485620
77.235721	28.966306	76.490625
75.960308	31.946705	76.495630
75.125391	38.256750	76.500634
74.749162	27.719706	76.505639
74.227051	33.546206	76.510644
74.391535	23.664101	76.515649
73.170036	33.768414	76.520654
72.380273	40.735153	76.525658
71.763805	29.260291	76.530663
71.138263	30.304650	76.535668
70.262096	26.418455	76.540673
69.342246	30.780326	76.545678
68.586303	28.456632	76.550682
68.576406	27.567253	76.555687
67.938032	40.678849	76.560692
67.229084	21.409721	76.565697
66.350608	29.691580	76.570702
65.791943	26.842843	76.575706
65.538248	27.947752	76.580711
64.079033	24.793201	76.585716
63.509299	32.566936	76.590721
63.029644	27.144646	76.595726
62.706117	30.504680	76.600730
61.784780	24.868978	76.605735
60.783012	26.455882	76.610740
60.257970	28.176494	76.615745
60.060768	28.766195	76.620750
59.155236	23.869137	76.625754
58.369712	28.234820	76.630759
57.599273	29.477331	76.635764
57.453413	18.853097	76.640769
56.871846	24.872004	76.645774
56.270051	29.492238	76.650778
55.382969	23.799037	76.655783
54.399336	25.102356	76.660788
53.487408	26.255469	76.665793
52.895100	28.850974	76.670798
52.271888	25.266641	76.675802
51.977190	19.501049	76.680807
51.663546	20.254399	76.685812
50.849594	24.613579	76.690817
50.191672	29.256957	76.695822
49.202516	31.589325	76.700826
48.421226	19.767030	76.705831
47.486788	23.036836	76.710836
47.120661	24.432488	76.715841
46.528946	17.544175	76.720846
46.122333	24.814080	76.725850
45.704076	23.843172	76.730855
44.718862	32.580451	76.735860
44.444590	29.173858	76.740865
42.956503	31.902764	76.745870
41.978646	28.289839	76.750874
41.831139	20.188977	76.755879
41.038281	22.261384	76.760884
40.944981	18.315003	76.765889
40.478266	24.227287	76.770894
39.594971	27.747559	76.775898
39.023167	20.324642	76.780903
38.001690	22.447704	76.785908
36.662529	25.206477	76.790913
36.189252	29.989144	76.795918
35.825902	28.455973	76.800922
35.613642	22.333462	76.805927
34.789663	28.474613	76.810932
34.248748	27.281996	76.815937
33.485534	17.787547	76.820942
32.721153	27.323808	76.825946
32.351670	25.236533	76.830951
30.832158	31.409768	76.835956
30.430389	22.784912	76.840961
30.161097	19.275028	76.845966
29.291326	35.686220	76.850970
29.105567	27.635611	76.855975
28.121347	32.584923	76.860980
27.570860	31.146255	76.865985
26.913393	31.574401	76.870990
26.090436	37.480431	76.875994
25.080687	29.378314	76.880999
24.281192	39.192996	76.886004
23.983652	32.899580	76.891009
23.845084	23.609856	76.896014
23.186154	37.374433	76.901018
22.382694	22.401799	76.906023
21.703105	26.807367	76.911028
21.093323	31.441497	76.916033
20.300052	31.861343	76.921038
19.337798	38.136519	76.926042
18.942365	27.359704	76.931047
17.916238	36.761103	76.936052
17.257041	27.557568	76.941057
16.215750	31.609245	76.946062
16.056341	34.190908	76.951066
15.646066	24.965020	76.956071
15.253063	33.939012	76.961076
14.701611	18.021029	76.966081
13.681788	24.083034	76.971086
13.115075	27.600129	76.976090
12.501575	24.372225	76.981095
11.030926	36.954253	76.986100
10.848172	24.389962	76.991105
10.571056	25.400841	76.996110
9.768594	32.446886	77.001114
8.916049	30.351506	77.006119
8.211388	28.483274	77.011124
7.911502	27.031449	77.016129
7.280858	35.026218	77.021134
5.945478	42.379617	77.026139
5.572490	33.393782	77.031143
4.746362	29.513824	77.036148
4.373636	25.064813	77.041153
3.454779	28.606538	77.046158