Fri Mar 05 20:16:55 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.183864	105.794124	0.000000
-0.519898	95.556906	0.005005
-1.043161	63.196333	0.010010
-2.783769	27.119195	0.015014
-6.417718	-1.140174	0.020019
-11.623789	-4.141684	0.025024
-17.369505	7.554791	0.030029
-21.400174	-5.414348	0.035034
-25.495747	1.299154	0.040038
-29.368729	8.475470	0.045043
-32.964907	1.695902	0.050048
-36.894453	-7.335958	0.055053
-40.474287	-11.470441	0.060058
-44.146547	0.174448	0.065062
-47.565612	1.547795	0.070067
-51.476798	-10.014796	0.075072
-55.181928	3.858833	0.080077
-58.935912	-4.157067	0.085082
-63.030448	-5.889735	0.090086
-66.630537	-2.899509	0.095091
-70.434605	-9.661618	0.100096
-74.452432	-0.243383	0.105101
-77.629412	-2.447257	0.110106
-81.415357	-1.710761	0.115110
-85.473911	-1.501617	0.120115
-89.072601	1.518380	0.125120
-93.257079	-1.666437	0.130125
-96.434905	-5.601626	0.135130
-100.429130	3.718271	0.140134
-103.896835	-5.202659	0.145139
-107.339565	-7.504440	0.150144
-111.844214	-1.148151	0.155149
-115.516261	-6.545125	0.160154
-119.509696	-6.171274	0.165158
-123.094621	-2.915307	0.170163
-126.778784	-5.484465	0.175168
-130.361018	1.377533	0.180173
-134.047357	-4.974332	0.185178
-138.423211	-4.069505	0.190182
-142.187749	-6.064425	0.195187
-145.891131	-0.865665	0.200192
-150.175606	0.023025	0.205197
-153.698602	-0.685795	0.210202
-157.398784	1.382260	0.215206
-160.822021	-1.275789	0.220211
-164.533230	-6.811515	0.225216
-168.414705	4.595701	0.230221
-171.660683	-4.098735	0.235226
-175.550942	-2.446594	0.240230
-179.553821	-1.020900	0.245235
-182.953452	-4.125802	0.250240
-186.732243	-2.295892	0.255245
-191.177199	-8.479294	0.260250
-194.743718	0.581683	0.265254
-198.188390	-2.585394	0.270259
-201.802757	-11.780804	0.275264
-205.931741	-3.849020	0.280269
-209.202887	-11.150103	0.285274
-213.336084	-2.637323	0.290278
-217.384619	-1.652130	0.295283
-220.932872	0.484813	0.300288
-224.601253	3.957672	0.305293
-228.300949	-4.008267	0.310298
-232.440654	0.509639	0.315302
-236.101460	-2.089885	0.320307
-239.541987	-1.294732	0.325312
-243.563663	9.406433	0.330317
-247.178823	-4.084349	0.335322
-250.926023	-9.213650	0.340326
-254.834516	-7.146894	0.345331
-258.391285	-17.638178	0.350336
-262.302794	-8.206662	0.355341
-266.352490	-10.567449	0.360346
-269.920653	-8.241181	0.365350
-273.234326	-1.576390	0.370355
-277.143163	-2.904676	0.375360
-281.370825	0.722192	0.380365
-284.911507	-7.239072	0.385370
-288.692796	2.793015	0.390374
-292.625140	3.351362	0.395379
-296.293056	-3.156147	0.400384
-299.923855	5.555699	0.405389
-303.632906	5.133839	0.410394
-307.368624	-3.896958	0.415398
-311.021674	3.342447	0.420403
-314.967121	-1.050219	0.425408
-318.880074	9.420822	0.430413
-322.450993	-5.278519	0.435418
-326.431110	0.360496	0.440422
-330.250218	0.667442	0.445427
-333.419586	-3.763930	0.450432
-337.355842	5.974429	0.455437
-340.860370	-4.092994	0.460442
-345.106083	-3.199109	0.465446
-349.179898	1.661705	0.470451
-352.607433	-1.695536	0.475456
-356.706884	3.038499	0.480461
-360.137023	-2.220094	0.485466
-363.629260	0.731270	0.490470
-367.553835	3.969281	0.495475
-371.282400	-0.856879	0.500480
-375.376735	3.150982	0.505485
-378.849201	0.103723	0.510490
-382.573743	6.867376	0.515494
-386.379653	3.163747	0.520499
-390.032592	-2.414037	0.525504
-394.128632	7.520231	0.530509
-397.843272	-3.748292	0.535514
-402.001666	1.529808	0.540518
-405.620961	7.054570	0.545523
-408.969562	5.482506	0.550528
-412.609106	-4.697284	0.555533
-416.237826	-5.328912	0.560538
-420.229310	-1.502978	0.565542
-423.807276	-5.023748	0.570547
-427.515059	-5.753119	0.575552
-431.754089	-7.056809	0.580557
-435.452629	-11.625886	0.585562
-439.161029	-3.552728	0.590566
-442.846698	-6.428652	0.595571
-446.508295	-6.326443	0.600576
-450.695380	-3.128380	0.605581
-454.125256	-6.286404	0.610586
-457.786151	-5.540903	0.615590
-461.759885	0.322810	0.620595
-465.286717	-10.196583	0.625600
-469.283315	-8.634221	0.630605
-473.076238	-9.780425	0.635610
-477.222621	-6.808011	0.640614
-480.805634	-11.368657	0.645619
-484.132968	-7.874187	0.650624
-488.002617	-0.144204	0.655629
-491.454365	-9.188505	0.660634
-495.201021	-10.718948	0.665638
-499.223218	-7.037789	0.670643
-503.098667	-13.164891	0.675648
-507.072671	1.329458	0.680653
-510.400094	-9.986522	0.685658
-514.307876	-8.349962	0.690662
-518.577572	-5.564359	0.695667
-522.249144	-7.996139	0.700672
-525.744163	-2.875825	0.705677
-529.292478	-7.675325	0.710682
-533.041157	-8.175652	0.715686
-536.825328	-2.595983	0.720691
-540.586895	-7.784020	0.725696
-544.541592	4.950609	0.730701
-547.620597	1.531676	0.735706
-551.696446	-4.301568	0.740710
-555.692846	0.965107	0.745715
-559.366563	-6.449360	0.750720
-563.509301	-1.167183	0.755725
-566.909212	-4.747713	0.760730
-570.982557	-7.324968	0.765734
-574.854786	-0.375018	0.770739
-578.134966	-8.265473	0.775744
-582.512544	4.126765	0.780749
-585.675565	0.563612	0.785754
-589.516156	0.716711	0.790758
-593.064111	-0.766474	0.795763
-597.053646	-0.299414	0.800768
-601.123982	2.580642	0.805773
-604.718543	-2.626087	0.810778
-608.677241	-2.958704	0.815782
-612.361264	-1.073886	0.820787
-615.806726	-9.738958	0.825792
-619.580680	-1.281329	0.830797
-623.038978	-13.508188	0.835802
-627.088088	-2.314780	0.840806
-631.352692	2.034520	0.845811
-634.731652	2.506594	0.850816
-638.700027	3.506498	0.855821
-642.219541	-5.928859	0.860826
-645.707146	-2.261908	0.865830
-649.601861	-2.011756	0.870835
-653.234767	-4.708124	0.875840
-657.455133	-1.107002	0.880845
-661.188394	-3.437246	0.885850
-665.063763	1.304076	0.890854
-668.844827	-0.592749	0.895859
-672.057862	-12.224795	0.900864
-676.282868	7.915886	0.905869
-679.776932	-6.662677	0.910874
-683.365688	-5.103627	0.915878
-687.445692	0.588198	0.920883
-691.025964	-0.580597	0.925888
-695.076520	7.432501	0.930893
-698.759767	-2.850221	0.935898
-702.191243	5.092346	0.940902
-706.307046	5.871498	0.945907
-709.896870	-4.544403	0.950912
-714.084628	-7.114164	0.955917
-717.699784	-10.680574	0.960922
-721.264250	-2.667847	0.965926
-725.132842	0.651678	0.970931
-728.416121	-0.455713	0.975936
-732.772777	-2.296720	0.980941
-736.193583	-7.929968	0.985946
-739.784753	-6.469793	0.990950
-744.231541	1.415897	0.995955
-747.251445	-5.962406	1.000960
-751.369904	-5.113368	1.005965
-754.852576	-6.918970	1.010970
-758.783254	0.114723	1.015974
-762.908297	-0.752436	1.020979
-766.288534	-7.846045	1.025984
-770.562344	7.592316	1.030989
-774.216247	-1.017124	1.035994
-777.408070	4.504513	1.040998
-781.412123	-2.404220	1.046003
-785.162631	-6.251661	1.051008
-789.232997	1.946100	1.056013
-792.804504	-0.881287	1.061018
-796.663087	-0.909476	1.066022
-800.523042	0.092291	1.071027
-803.657279	-8.399889	1.076032
-807.311983	-5.798804	1.081037
-811.252339	-7.398704	1.086042
-815.150073	-2.371301	1.091046
-819.194488	-2.674095	1.096051
-822.816642	-2.195995	1.101056
-826.893588	4.302958	1.106061
-830.585915	-4.883706	1.111066
-834.082213	1.281173	1.116070
-837.758690	5.122093	1.121075
-841.308727	-1.263033	1.126080
-845.439583	8.228106	1.131085
-849.200077	8.871861	1.136090
-853.009702	4.553017	1.141094
-856.981967	2.007409	1.146099
-860.410336	-4.307250	1.151104
-864.025756	2.412868	1.156109
-867.839278	2.216746	1.161114
-871.341950	2.436127	1.166118
-875.445865	8.061129	1.171123
-879.277371	-9.656423	1.176128
-883.079373	8.869998	1.181133
-886.690105	7.004641	1.186138
-890.415230	2.391659	1.191142
-894.254427	1.900070	1.196147
-897.881470	-4.144654	1.201152
-901.930512	5.281458	1.206157
-905.868492	-5.313418	1.211162
-909.441913	-6.453012	1.216166
-913.210161	-9.576753	1.221171
-916.590303	2.631351	1.226176
-920.645993	4.670685	1.231181
-924.221977	1.921487	1.236186
-927.826806	-7.132350	1.241190
-932.125784	-2.953640	1.246195
-935.693669	-7.702071	1.251200
-939.493628	0.466891	1.256205
-943.116798	-4.611727	1.261210
-946.759162	-1.249173	1.266214
-950.802274	0.304086	1.271219
-954.159191	-12.616528	1.276224
-958.084866	-0.280140	1.281229
-962.079652	-9.028718	1.286234
-965.765408	-0.256672	1.291238
-969.634948	-6.391809	1.296243
-973.126264	-4.491519	1.301248
-977.239707	-5.181962	1.306253
-980.683446	-7.792949	1.311258
-984.404912	-7.694526	1.316262
-988.410724	-7.049165	1.321267
-991.918989	-8.041359	1.326272
-996.064484	7.733237	1.331277
-999.640235	-5.626969	1.336282
-1003.280531	-1.737969	1.341286
-1007.317432	9.004679	1.346291
-1010.421921	-3.889994	1.351296
-1014.883694	9.074685	1.356301
-1018.762734	2.471226	1.361306
-1022.391256	2.792959	1.366310
-1025.987175	13.774190	1.371315
-1029.469908	1.332688	1.376320
-1033.603394	-4.135667	1.381325
-1037.163169	-3.433830	1.386330
-1041.041798	2.590648	1.391334
-1044.948000	13.902223	1.396339
-1048.333750	3.198773	1.401344
-1052.216214	9.436768	1.406349
-1056.009961	8.543945	1.411354
-1059.275319	-3.244736	1.416358
-1063.818264	8.187633	1.421363
-1067.348517	10.654097	1.426368
-1071.153401	4.098789	1.431373
-1074.943768	-1.061682	1.436378
-1078.351249	-0.847756	1.441382
-1082.273722	6.297105	1.446387
-1086.012567	3.000212	1.451392
-1090.201019	7.836448	1.456397
-1093.866192	2.012599	1.461402
-1097.174056	-1.324831	1.466406
-1101.267994	-1.075179	1.471411
-1104.724615	-10.860465	1.476416
-1108.525293	3.561345	1.481421
-1112.604068	-2.727729	1.486426
-1116.329575	-1.672838	1.491430
-1119.870707	1.158134	1.496435
-1123.815080	-4.218885	1.501440
-1127.737855	-0.603044	1.506445
-1131.407049	-1.138784	1.511450
-1134.816515	0.709227	1.516454
-1138.697763	4.211214	1.521459
-1142.087709	-1.235549	1.526464
-1146.285925	2.870656	1.531469
-1150.271836	-1.834213	1.536474
-1153.946734	-2.510928	1.541478
-1158.196558	3.445393	1.546483
-1161.292403	-10.852311	1.551488
-1164.896530	0.179304	1.556493
-1168.702564	-3.871506	1.561498
-1172.444914	-6.552697	1.566502
-1176.319906	-3.460073	1.571507
-1180.421618	-8.326127	1.576512
-1184.091992	-4.764769	1.581517
-1187.701004	1.216803	1.586522
-1190.904572	-2.605521	1.591526
-1195.043924	0.218780	1.596531
-1198.559077	-6.128780	1.601536
-1202.621510	-4.715496	1.606541
-1206.742738	-1.914574	1.611546
-1210.310151	-1.832556	1.616550
-1214.138253	-0.895130	1.621555
-1217.598298	-9.374004	1.626560
-1221.692820	0.083558	1.631565
-1225.441567	-2.738446	1.636570
-1228.864725	-5.609389	1.641574
-1232.991190	7.639479	1.646579
-1236.600946	-3.890396	1.651584
-1240.156681	0.520007	1.656589
-1244.255828	-0.216405	1.661594
-1247.744075	-4.986547	1.666598
-1251.751639	10.868889	1.671603
-1254.997480	-3.324257	1.676608
-1259.235225	5.323680	1.681613
-1262.856612	-2.088543	1.686618
-1266.671861	-6.016290	1.691622
-1270.746429	-1.204274	1.696627
-1274.198144	-8.973203	1.701632
-1277.960084	-0.426615	1.706637
-1281.385328	-1.642963	1.711642
-1285.067842	2.784643	1.716646
-1289.136321	-0.731965	1.721651
-1292.749145	-1.517739	1.726656
-1297.029583	0.539289	1.731661
-1300.722792	-1.313793	1.736666
-1304.147982	-1.675429	1.741670
-1308.012436	-6.003652	1.746675
-1311.578894	-3.037456	1.751680
-1315.532011	0.466860	1.756685
-1319.342853	-5.284415	1.761690
-1323.189694	2.216147	1.766694
-1327.042295	0.325544	1.771699
-1330.388500	-3.986247	1.776704
-1334.653773	-1.018546	1.781709
-1338.324342	1.079707	1.786714
-1341.988033	3.892783	1.791718
-1345.780008	3.692419	1.796723
-1349.287863	-6.133162	1.801728
-1353.113668	2.579879	1.806733
-1356.940548	-8.848802	1.811738
-1360.684444	-9.276028	1.816742
-1364.389711	5.089890	1.821747
-1368.136888	-5.880036	1.826752
-1371.924423	-7.956015	1.831757
-1375.598971	-9.154389	1.836762
-1379.266209	-12.731909	1.841766
-1383.452786	-2.149198	1.846771
-1387.157230	-3.863149	1.851776
-1390.902116	-3.865979	1.856781
-1394.442643	-6.161232	1.861786
-1398.313560	-14.779036	1.866790
-1402.180237	-12.575174	1.871795
-1405.769521	-8.767844	1.876800
-1409.560564	-12.341263	1.881805
-1413.513420	-10.666042	1.886810
-1416.562097	-6.486365	1.891814
-1420.700570	-9.630414	1.896819
-1424.298642	-9.986269	1.901824
-1428.384257	-7.528120	1.906829
-1432.361081	-5.196188	1.911834
-1435.988638	-1.802141	1.916838
-1439.837766	-6.153089	1.921843
-1443.453246	-3.672418	1.926848
-1447.069557	-0.991341	1.931853
-1450.930319	-0.601792	1.936858
-1454.491408	-5.727367	1.941862
-1458.699873	-3.263687	1.946867
-1462.052505	2.603131	1.951872
-1465.941280	-2.594535	1.956877
-1470.009514	7.258194	1.961882
-1473.333915	-10.919492	1.966886
-1477.330030	5.748142	1.971891
-1481.173929	-8.255841	1.976896
-1484.775434	-6.870143	1.981901
-1488.175327	-5.075189	1.986906
-1492.248626	2.581750	1.991910
-1496.353539	-0.122848	1.996915
-1500.076053	0.164336	2.006912
-1500.923147	-4.646724	2.016909
-1498.462349	1.609735	2.026906
-1495.490804	3.595509	2.036902
-1493.555724	-4.438412	2.046899
-1491.445703	0.570030	2.056896
-1489.555282	-4.341508	2.066893
-1487.743135	-1.596916	2.076890
-1486.205543	-1.146751	2.086886
-1483.934252	-2.470369	2.096883
-1482.187059	-4.857943	2.106880
-1480.014377	-10.342033	2.116877
-1478.472561	-2.732098	2.126874
-1476.502082	4.300787	2.136870
-1474.255235	1.247427	2.146867
-1472.516021	-1.042548	2.156864
-1470.583151	-7.631375	2.166861
-1468.879466	-3.584152	2.176858
-1466.957716	-6.656500	2.186854
-1464.877464	-7.096888	2.196851
-1463.086477	-1.025241	2.206848
-1461.465160	-4.987363	2.216845
-1459.409641	-9.290583	2.226842
-1457.355324	-4.402663	2.236838
-1455.522338	-4.467139	2.246835
-1453.608168	-3.065155	2.256832
-1451.718757	-3.143399	2.266829
-1449.987304	-6.621048	2.276826
-1448.177362	-6.986561	2.286822
-1446.202398	-7.247445	2.296819
-1444.409367	-3.868185	2.306816
-1442.247695	-5.100001	2.316813
-1440.450937	-4.842878	2.326810
-1438.787188	-3.108685	2.336806
-1436.516952	-7.632578	2.346803
-1435.019219	-9.283868	2.356800
-1433.080584	-7.871574	2.366797
-1431.276316	-0.491515	2.376794
-1429.184694	-3.838922	2.386790
-1427.197703	-7.226417	2.396787
-1425.450314	-2.613006	2.406784
-1423.803085	-2.391929	2.416781
-1421.990895	-8.032987	2.426778
-1419.501096	-5.537358	2.436774
-1417.822264	-1.828743	2.446771
-1416.077113	-11.930592	2.456768
-1414.513654	-9.070338	2.466765
-1412.228966	-5.539242	2.476762
-1410.365370	-8.272238	2.486758
-1408.648195	-7.558670	2.496755
-1406.723643	-6.158309	2.506752
-1404.783493	-10.040385	2.516749
-1402.729016	-2.817201	2.526746
-1400.928013	-4.472811	2.536742
-1399.285043	3.908880	2.546739
-1397.320289	-6.566009	2.556736
-1395.327855	-6.453861	2.566733
-1393.623245	-12.020832	2.576730
-1391.852675	-5.205340	2.586726
-1389.701240	0.679193	2.596723
-1387.862939	-4.721287	2.606720
-1385.706066	-3.312311	2.616717
-1384.070354	-3.160414	2.626714
-1382.281025	-1.370493	2.636710
-1380.326859	-8.829493	2.646707
-1378.296622	-8.214966	2.656704
-1376.866599	-3.877549	2.666701
-1374.895882	-4.548213	2.676698
-1372.773776	-6.277310	2.686694
-1370.798991	-5.690215	2.696691
-1369.116299	-9.286314	2.706688
-1367.197836	-9.950186	2.716685
-1365.427133	-2.769959	2.726682
-1363.447096	-3.862102	2.736678
-1361.575921	-3.555251	2.746675
-1359.686086	-0.957199	2.756672
-1357.693231	-6.683973	2.766669
-1355.626227	-5.063216	2.776666
-1354.174804	0.205520	2.786662
-1352.578845	-2.277750	2.796659
-1350.441156	-6.290877	2.806656
-1348.456951	-10.899953	2.816653
-1346.611464	-6.741124	2.826650
-1344.573498	-4.803081	2.836646
-1342.760770	-2.206882	2.846643
-1340.767833	0.895730	2.856640
-1339.351424	-0.355644	2.866637
-1337.271930	-2.549990	2.876634
-1335.059571	-4.525602	2.886630
-1333.211849	-3.455509	2.896627
-1331.529357	-2.324230	2.906624
-1329.990574	-2.000465	2.916621
-1327.807827	3.228599	2.926618
-1326.030394	5.936251	2.936614
-1323.955832	-1.884609	2.946611
-1322.155875	-2.690527	2.956608
-1320.242700	-11.357118	2.966605
-1318.271698	-11.118316	2.976602
-1316.413491	-6.022033	2.986598
-1314.855142	-8.196102	2.996595
-1312.714818	-1.799720	3.006592
-1310.876919	-0.006464	3.016589
-1309.073925	2.198167	3.026586
-1306.916873	-3.168010	3.036582
-1305.306203	-3.828356	3.046579
-1303.539706	-2.389979	3.056576
-1301.480994	-1.516259	3.066573
-1299.696669	1.084521	3.076570
-1298.054153	2.391170	3.086566
-1295.723506	-1.877002	3.096563
-1293.737124	-4.815873	3.106560
-1291.779293	-2.315487	3.116557
-1290.487677	-5.430526	3.126554
-1288.722181	-0.939900	3.136550
-1286.516158	-5.462851	3.146547
-1284.826426	-2.141138	3.156544
-1282.400323	-2.857764	3.166541
-1280.724701	-4.949528	3.176538
-1278.901360	-4.826006	3.186534
-1277.152765	-5.022096	3.196531
-1275.204130	-0.415507	3.206528
-1273.170185	0.812726	3.216525
-1271.573959	-5.409446	3.226522
-1269.709876	0.379091	3.236518
-1267.770447	-5.326430	3.246515
-1265.771856	-7.773025	3.256512
-1263.909600	-7.638351	3.266509
-1262.149874	-1.171535	3.276506
-1260.229089	-2.888840	3.286502
-1258.395394	-0.899080	3.296499
-1256.202200	-2.288926	3.306496
-1254.535911	-5.598115	3.316493
-1252.790387	-3.074772	3.326490
-1251.237695	-0.376886	3.336486
-1249.104271	-8.770781	3.346483
-1246.985418	-2.364582	3.356480
-1245.083594	-10.440360	3.366477
-1243.386952	-2.086083	3.376474
-1241.465806	-11.251256	3.386470
-1239.673673	-0.865960	3.396467
-1237.439133	1.580720	3.406464
-1235.840955	-6.918564	3.416461
-1233.904376	-3.854206	3.426458
-1232.230591	3.921115	3.436454
-1229.986116	0.067845	3.446451
-1228.415435	-3.290764	3.456448
-1226.580155	-3.001744	3.466445
-1224.547711	-0.759552	3.476442
-1222.796798	-4.551204	3.486438
-1220.938966	-6.533137	3.496435
-1218.890394	1.965372	3.506432
-1216.975020	-5.225195	3.516429
-1215.110038	-2.021470	3.526426
-1213.374801	-3.865361	3.536422
-1211.479118	-1.874430	3.546419
-1209.226656	-5.050016	3.556416
-1207.398775	-10.241854	3.566413
-1205.853076	0.228694	3.576410
-1204.058493	-0.888902	3.586406
-1202.094656	-6.604593	3.596403
-1200.307139	-4.269506	3.606400
-1198.277789	-6.477811	3.616397
-1196.409254	-0.906238	3.626394
-1194.516656	-6.080003	3.636390
-1192.658163	0.121597	3.646387
-1190.581875	-4.562087	3.656384
-1188.888344	-9.943993	3.666381
-1186.952911	2.058937	3.676378
-1185.260444	0.807694	3.686374
-1182.932442	0.024763	3.696371
-1181.296342	-3.765858	3.706368
-1179.542194	-4.220129	3.716365
-1177.816731	-7.633469	3.726362
-1176.022672	-2.465223	3.736358
-1173.950473	-2.986166	3.746355
-1171.712239	-8.047846	3.756352
-1170.145778	-6.364204	3.766349
-1168.256261	-5.055929	3.776346
-1166.397222	-8.879050	3.786342
-1164.574834	-4.814266	3.796339
-1162.655553	-6.903878	3.806336
-1160.695294	-9.898459	3.816333
-1158.725564	-2.740426	3.826330
-1156.913353	-3.878175	3.836326
-1155.323872	-1.334528	3.846323
-1153.311437	-6.173752	3.856320
-1151.283084	-2.066118	3.866317
-1149.555982	-0.045007	3.876314
-1147.842221	-5.902224	3.886310
-1145.837998	-9.124878	3.896307
-1143.950129	-10.885768	3.906304
-1141.778976	-2.784162	3.916301
-1140.195274	-5.873220	3.926298
-1138.243892	2.659865	3.936294
-1136.301857	-2.727028	3.946291
-1134.625853	-8.586090	3.956288
-1132.391154	3.763751	3.966285
-1130.648206	-5.604941	3.976282
-1128.837178	-5.566173	3.986278
-1127.160202	-4.189126	3.996275
-1125.142580	-13.765960	4.006272
-1123.162140	-13.436923	4.016269
-1121.179212	-13.161966	4.026266
-1119.645923	-11.646666	4.036262
-1117.560964	-4.421767	4.046259
-1115.724463	-8.446505	4.056256
-1113.868005	-8.419730	4.066253
-1112.238447	-4.620894	4.076250
-1109.847936	-2.674299	4.086246
-1108.134924	-5.362446	4.096243
-1106.370785	-5.968260	4.106240
-1104.751480	-8.508783	4.116237
-1102.600350	-14.315933	4.126234
-1100.638359	-7.522923	4.136230
-1098.834104	-7.585679	4.146227
-1096.821375	-10.294919	4.156224
-1094.977340	-8.155104	4.166221
-1093.162915	-6.376864	4.176218
-1091.365662	-3.009045	4.186214
-1089.440464	-2.603248	4.196211
-1087.473032	-1.297896	4.206208
-1085.350377	-8.789940	4.216205
-1083.651741	-3.879509	4.226202
-1082.011894	-12.637994	4.236198
-1080.312606	-4.977160	4.246195
-1078.265590	-13.922349	4.256192
-1076.186576	-7.672242	4.266189
-1074.374515	-14.141969	4.276186
-1072.479408	-13.027140	4.286182
-1070.860978	-13.590673	4.296179
-1068.974693	-16.161244	4.306176
-1066.836250	-17.739523	4.316173
-1064.813409	-10.531481	4.326170
-1063.099282	-15.217127	4.336166
-1061.360077	-11.363162	4.346163
-1059.269179	-9.239120	4.356160
-1057.673099	-9.950647	4.366157
-1055.699267	-10.256807	4.376154
-1053.837236	-3.886708	4.386150
-1051.965116	-6.642896	4.396147
-1050.143934	-10.502504	4.406144
-1048.172815	-12.641368	4.416141
-1046.400807	-11.674197	4.426138
-1044.518251	-10.494180	4.436134
-1042.477791	-11.084140	4.446131
-1040.252719	-12.287833	4.456128
-1038.677997	-15.771700	4.466125
-1037.150806	-15.750622	4.476122
-1035.004285	-11.625468	4.486118
-1033.179698	-5.590414	4.496115
-1031.049807	-6.766244	4.506112
-1029.403735	-10.469937	4.516109
-1027.713662	-4.920204	4.526106
-1025.819872	-5.655639	4.536102
-1023.688760	-6.046926	4.546099
-1021.954554	-7.269990	4.556096
-1019.830312	-9.397005	4.566093
-1018.091405	-11.541338	4.576090
-1016.175081	-4.581473	4.586086
-1014.606218	-8.531755	4.596083
-1012.472848	-12.062319	4.606080
-1010.612287	-7.403516	4.616077
-1008.861216	-8.201376	4.626074
-1006.828382	-8.617983	4.636070
-1005.002305	-12.798865	4.646067
-1002.892301	-13.739385	4.656064
-1001.128323	-6.998301	4.666061
-999.343717	-10.660971	4.676058
-997.844507	-5.486478	4.686054
-995.936383	-13.801501	4.696051
-993.483140	-5.648542	4.706048
-991.916233	-9.887442	4.716045
-989.971533	-8.592582	4.726042
-988.046651	-2.939841	4.736038
-986.127822	-8.888164	4.746035
-984.456097	-5.279134	4.756032
-982.446311	-4.471515	4.766029
-980.429764	-2.839190	4.776026
-978.781183	-11.807430	4.786022
-976.926959	-6.599694	4.796019
-975.009045	-2.336871	4.806016
-973.080683	-15.084034	4.816013
-971.591845	-10.871017	4.826010
-969.465148	-0.756874	4.836006
-967.271297	-11.511238	4.846003
-965.485051	-3.472639	4.856000
-963.902157	-2.025165	4.865997
-961.645254	-8.970156	4.875994
-960.064784	-9.900172	4.885990
-958.021453	-14.022602	4.895987
-956.164061	-8.261149	4.905984
-954.256927	-4.339215	4.915981
-952.503600	-3.711612	4.925978
-950.775521	-7.662050	4.935974
-948.615516	-9.518407	4.945971
-947.013013	-3.169874	4.955968
-945.046553	-6.866322	4.965965
-942.992852	-3.067286	4.975962
-941.327606	1.414388	4.985958
-939.389971	-8.695832	4.995955
-937.269548	-7.860075	5.005952
-935.601292	-12.727773	5.015949
-933.805789	-7.021141	5.025946
-932.021749	-5.956331	5.035942
-929.626926	-6.651802	5.045939
-927.825741	-4.527105	5.055936
-926.158051	-3.450003	5.065933
-924.477381	-6.082323	5.075930
-922.554398	-7.084448	5.085926
-920.635278	-8.313320	5.095923
-918.686525	-7.844833	5.105920
-916.827864	-5.590370	5.115917
-915.037115	-9.432382	5.125914
-913.099183	-12.042669	5.135910
-911.022738	-11.297751	5.145907
-908.980920	-10.720979	5.155904
-907.530708	-10.562772	5.165901
-905.630633	-10.776487	5.175898
-903.560876	-5.843147	5.185894
-901.763584	-13.193019	5.195891
-900.014341	-18.768372	5.205888
-898.094257	-8.695339	5.215885
-896.093647	-18.888222	5.225882
-894.364196	-10.289436	5.235878
-892.557289	-11.181400	5.245875
-890.720278	-12.310279	5.255872
-888.499257	-8.280578	5.265869
-886.988942	-14.286671	5.275866
-884.845641	-2.687737	5.285862
-882.499954	-7.253180	5.295859
-881.348280	-8.951430	5.305856
-879.564494	-8.848113	5.315853
-877.439178	-10.252020	5.325850
-875.504048	-15.110238	5.335846
-873.739092	-13.314442	5.345843
-871.718292	-11.857966	5.355840
-869.526778	-17.772423	5.365837
-868.318113	-16.178216	5.375834
-866.296528	-7.202952	5.385830
-864.148731	-15.373037	5.395827
-862.396956	-16.657214	5.405824
-860.656968	-17.205299	5.415821
-858.538406	-14.030765	5.425818
-856.765075	-15.992591	5.435814
-854.985498	-8.994935	5.445811
-852.949684	-6.552425	5.455808
-851.127797	-13.325144	5.465805
-849.207297	-12.578926	5.475802
-847.457942	-6.211164	5.485798
-845.581260	-5.183202	5.495795
-843.406481	-12.034433	5.505792
-841.676355	-10.735148	5.515789
-840.062176	-7.792597	5.525786
-838.073077	-1.632096	5.535782
-836.257842	-5.364283	5.545779
-834.077290	-2.337001	5.555776
-832.047374	-2.715095	5.565773
-830.578286	-5.323004	5.575770
-828.761718	-2.333849	5.585766
-826.820195	-3.510964	5.595763
-824.641924	-4.141713	5.605760
-822.674751	-9.761327	5.615757
-821.167039	-2.072816	5.625754
-819.343739	-0.499460	5.635750
-817.475935	-5.015297	5.645747
-815.710956	-5.726817	5.655744
-813.636323	-2.305217	5.665741
-811.839167	-5.098185	5.675738
-809.807880	-5.797005	5.685734
-807.812393	-2.474854	5.695731
-806.266715	-1.774477	5.705728
-804.305185	-2.097407	5.715725
-802.348647	-4.622160	5.725722
-800.422428	-4.080499	5.735718
-798.617074	4.282033	5.745715
-796.741850	-4.889695	5.755712
-794.679568	-0.687685	5.765709
-792.982372	3.673733	5.775706
-791.231963	1.019303	5.785702
-789.271535	1.486033	5.795699
-787.430874	-0.488085	5.805696
-785.397757	0.303345	5.815693
-783.644875	5.094816	5.825690
-781.769157	5.314566	5.835686
-779.716300	8.217050	5.845683
-777.897845	-0.375596	5.855680
-776.118942	3.164358	5.865677
-774.197888	3.539499	5.875674
-772.458412	1.892616	5.885670
-770.484391	3.045608	5.895667
-768.355237	1.006449	5.905664
-766.637048	-5.064381	5.915661
-764.667857	-6.271131	5.925658
-763.253862	-2.743900	5.935654
-761.397334	-4.891059	5.945651
-759.060579	-10.920215	5.955648
-757.282636	-9.211667	5.965645
-755.615563	-0.170161	5.975642
-753.449222	-7.889967	5.985638
-751.688740	-5.368627	5.995635
-749.675673	-2.786600	6.005632
-748.024599	-4.929335	6.015629
-746.281904	-3.559355	6.025626
-744.284405	-6.704816	6.035622
-742.115183	-6.235100	6.045619
-740.470188	-6.381075	6.055616
-738.351700	-1.325894	6.065613
-736.821956	-3.439758	6.075610
-735.059110	-1.701938	6.085606
-732.912315	2.311361	6.095603
-731.036881	-4.510888	6.105600
-728.908951	-3.712457	6.115597
-727.541677	-4.870354	6.125594
-725.402802	-0.936309	6.135590
-723.641594	-3.843468	6.145587
-721.688413	-5.565517	6.155584
-719.693355	1.697822	6.165581
-717.960533	-1.027955	6.175578
-715.913245	-2.872407	6.185574
-714.288423	-0.171464	6.195571
-712.071761	-0.876140	6.205568
-710.434942	2.127625	6.215565
-708.659987	-0.439089	6.225562
-706.605638	-2.944660	6.235558
-705.000031	-0.403271	6.245555
-702.779106	-7.326496	6.255552
-701.018734	-6.046149	6.265549
-699.246186	-4.770903	6.275546
-697.359364	-4.794439	6.285542
-695.232547	-2.696329	6.295539
-693.421303	-4.706727	6.305536
-691.647789	-3.510577	6.315533
-689.644072	-4.981729	6.325530
-687.884190	0.994485	6.335526
-685.929207	-0.187825	6.345523
-684.248848	-2.515197	6.355520
-682.456727	-4.773583	6.365517
-680.558202	1.159958	6.375514
-678.467551	-0.440339	6.385510
-676.613497	-1.908093	6.395507
-674.687593	-0.504175	6.405504
-672.815263	-1.349584	6.415501
-670.987609	-1.973117	6.425498
-669.334971	4.853931	6.435494
-667.354072	4.108021	6.445491
-665.284645	-4.292543	6.455488
-663.134413	-6.188135	6.465485
-661.536188	-8.830787	6.475482
-659.900659	-4.130996	6.485478
-657.809369	-6.197165	6.495475
-656.184699	-5.842467	6.505472
-654.313100	-6.403535	6.515469
-652.214433	-13.371917	6.525466
-650.425809	-5.980799	6.535462
-648.400736	-5.697964	6.545459
-646.534432	-1.748716	6.555456
-644.803101	-5.645780	6.565453
-642.820078	-1.675704	6.575450
-640.977292	-1.259529	6.585446
-639.408411	-3.226427	6.595443
-637.084004	-4.404562	6.605440
-635.043122	-8.115812	6.615437
-633.468727	-8.507802	6.625434
-631.687690	-8.871226	6.635430
-629.820793	-1.773645	6.645427
-628.205321	-0.459039	6.655424
-625.862707	-8.047428	6.665421
-624.235271	-5.138419	6.675418
-622.243277	-3.233438	6.685414
-620.535148	-3.411522	6.695411
-618.383432	-2.747843	6.705408
-616.566583	0.653543	6.715405
-614.499751	-0.137632	6.725402
-612.966813	-4.876135	6.735398
-610.762978	-1.943937	6.745395
-609.034934	-7.506237	6.755392
-607.142521	-9.101644	6.765389
-605.507632	-2.393292	6.775386
-603.695838	-11.936854	6.785382
-601.783069	-2.501846	6.795379
-599.582521	-6.582785	6.805376
-597.686406	-9.893509	6.815373
-595.986800	-6.493905	6.825370
-594.270950	-8.023201	6.835366
-592.206985	-5.160220	6.845363
-590.208738	-3.388843	6.855360
-588.302305	-1.247533	6.865357
-586.553343	-2.434746	6.875354
-584.791513	-7.115060	6.885350
-582.973809	-7.981673	6.895347
-580.820827	-11.980784	6.905344
-578.879867	-6.669726	6.915341
-577.410697	-11.194336	6.925338
-575.437200	-10.885832	6.935334
-573.494812	-6.389733	6.945331
-571.581391	-7.094785	6.955328
-569.601383	-12.831516	6.965325
-567.588289	-8.460391	6.975322
-565.919351	-12.049011	6.985318
-564.223356	-2.549342	6.995315
-562.414625	-0.442931	7.005312
-560.171985	-12.010021	7.015309
-558.260998	-7.502577	7.025306
-556.405645	-8.340447	7.035302
-554.672060	-7.693603	7.045299
-552.727966	0.831713	7.055296
-551.027315	-7.519329	7.065293
-549.311371	-5.835455	7.075290
-547.383683	-3.046981	7.085286
-545.042590	-1.216643	7.095283
-543.342308	-11.313933	7.105280
-541.705901	-2.003673	7.115277
-539.648049	-11.960706	7.125274
-537.800033	-3.738980	7.135270
-535.837886	-4.982313	7.145267
-533.994453	0.435944	7.155264
-532.134779	-2.739438	7.165261
-530.527059	-5.044049	7.175258
-528.495185	-4.866409	7.185254
-526.516284	-7.936092	7.195251
-524.570082	-14.256335	7.205248
-522.794456	-2.936196	7.215245
-520.772150	-2.824915	7.225242
-519.160069	-6.609688	7.235238
-517.333340	-6.246115	7.245235
-515.273424	-6.461363	7.255232
-513.479540	-11.552536	7.265229
-511.356899	-7.170435	7.275226
-509.731793	-3.476235	7.285222
-507.704429	-13.180479	7.295219
-505.810836	-10.647053	7.305216
-503.983001	-7.991017	7.315213
-502.195648	-7.867459	7.325210
-500.333027	-11.136444	7.335206
-498.268189	-11.028780	7.345203
-496.461872	-5.105619	7.355200
-494.793935	-8.259824	7.365197
-492.794986	-10.203735	7.375194
-490.728390	-7.663189	7.385190
-489.020355	-12.461160	7.395187
-487.124713	-12.621727	7.405184
-485.222248	-5.870756	7.415181
-483.434639	-6.977224	7.425178
-481.538177	-7.028971	7.435174
-479.558092	-9.587227	7.445171
-477.616177	-9.583071	7.455168
-475.891706	-11.980502	7.465165
-474.100014	-5.557619	7.475162
-471.995761	-12.910433	7.485158
-470.359267	-9.746972	7.495155
-468.603964	-3.394062	7.505152
-466.476025	-9.620129	7.515149
-464.516474	-10.226674	7.525146
-462.823653	-11.125358	7.535142
-461.001138	-1.955281	7.545139
-458.977258	-13.844196	7.555136
-456.875067	-11.558778	7.565133
-455.292712	-15.831392	7.575130
-453.320542	-8.254684	7.585126
-451.426996	-10.604888	7.595123
-449.645343	-3.215645	7.605120
-447.750359	-10.122917	7.615117
-445.747874	-12.648406	7.625114
-443.951339	-9.246799	7.635110
-442.222885	-7.171686	7.645107
-440.429410	-8.898006	7.655104
-438.327530	-5.688837	7.665101
-436.513057	-12.096927	7.675098
-434.558533	-6.865277	7.685094
-432.636901	-10.779951	7.695091
-430.771245	-10.998843	7.705088
-428.922944	-4.558121	7.715085
-426.818847	-3.198242	7.725082
-425.294500	-10.033683	7.735078
-423.597129	-7.220961	7.745075
-421.267942	-6.124388	7.755072
-419.658005	-6.035596	7.765069
-417.455531	-7.156155	7.775066
-415.989740	-6.275397	7.785062
-413.968520	-4.475958	7.795059
-412.032788	-5.929709	7.805056
-410.376790	-4.124055	7.815053
-408.537943	-13.670230	7.825050
-406.326864	-9.096889	7.835046
-404.333810	-2.524521	7.845043
-402.803957	-0.087666	7.855040
-401.018053	-3.055382	7.865037
-398.819863	-7.052083	7.875034
-397.011388	-2.316554	7.885030
-395.126232	1.898315	7.895027
-393.316205	5.589917	7.905024
-391.345728	-1.302530	7.915021
-389.373019	-6.611644	7.925018
-387.931772	-8.660635	7.935014
-386.005711	-2.259133	7.945011
-384.042644	2.241726	7.955008
-382.269680	-6.567600	7.965005
-380.128567	-6.031485	7.975002
-378.003615	-5.559103	7.984998
-376.442107	-10.020974	7.994995
-374.678908	-7.570831	8.004992
-372.683789	-3.397187	8.014989
-370.652669	-4.514030	8.024986
-368.916589	-8.837979	8.034982
-367.002521	-2.295598	8.044979
-365.214139	-7.051053	8.054976
-363.280516	-7.910745	8.064973
-361.497354	-7.140622	8.074970
-359.707610	-0.313122	8.084966
-357.609768	-5.018505	8.094963
-355.533373	-11.630988	8.104960
-354.095078	-8.645801	8.114957
-352.230900	-2.472811	8.124954
-350.066743	-2.886138	8.134950
-348.190260	-1.736166	8.144947
-346.460104	-6.479156	8.154944
-344.472003	-0.865943	8.164941
-342.579150	-5.939641	8.174938
-340.753449	-1.516289	8.184934
-338.688145	-4.457512	8.194931
-337.225665	-3.380387	8.204928
-335.402543	-6.012944	8.214925
-333.335685	-8.720725	8.224922
-331.233495	-3.379926	8.234918
-329.424080	-2.348707	8.244915
-327.711918	-6.528283	8.254912
-325.859647	-7.591274	8.264909
-323.882639	-1.928904	8.274906
-321.802515	-4.769847	8.284902
-320.216471	-2.324540	8.294899
-318.334152	0.476106	8.304896
-316.538088	-5.071597	8.314893
-314.708123	-2.870487	8.324890
-312.539684	-2.682884	8.334886
-310.646632	-4.901849	8.344883
-308.756290	-5.434062	8.354880
-307.088155	-12.660284	8.364877
-305.234551	-4.226090	8.374874
-303.343433	4.030016	8.384870
-301.436441	1.816726	8.394867
-299.348782	-5.751199	8.404864
-297.417580	-2.707288	8.414861
-296.012077	0.456858	8.424858
-293.877971	-1.033203	8.434854
-291.918845	-2.015330	8.444851
-290.056216	-4.469424	8.454848
-288.320795	-8.647950	8.464845
-286.267440	-8.243006	8.474842
-284.292896	-7.793901	8.484838
-282.528295	-4.363384	8.494835
-280.820254	-5.071739	8.504832
-278.900003	-10.877658	8.514829
-277.170093	-5.251595	8.524826
-275.128276	-9.264282	8.534822
-273.262114	-6.862075	8.544819
-271.220719	-11.373638	8.554816
-269.433223	-11.587825	8.564813
-267.411732	-11.708306	8.574810
-265.833305	-15.197019	8.584807
-263.712611	-15.327015	8.594803
-262.089566	-5.085982	8.604800
-260.198653	-12.818261	8.614797
-258.270293	-14.449135	8.624794
-256.246437	-10.505767	8.634791
-254.449064	-5.676772	8.644787
-252.836442	-11.485677	8.654784
-250.810371	-12.004770	8.664781
-248.664589	-7.913487	8.674778
-246.537073	-13.035619	8.684775
-245.387615	-15.162693	8.694771
-243.007038	-14.490990	8.704768
-241.250293	-8.171288	8.714765
-239.773117	-6.786974	8.724762
-237.573995	-14.277900	8.734759
-235.764729	-13.533955	8.744755
-233.816879	-9.673173	8.754752
-231.976156	-9.714248	8.764749
-230.196966	-13.781297	8.774746
-228.149741	-7.645314	8.784743
-225.911019	-16.956763	8.794739
-224.294729	-15.480958	8.804736
-222.578635	-17.396875	8.814733
-220.745609	-14.161969	8.824730
-218.664250	-16.412494	8.834727
-216.993474	-9.906948	8.844723
-214.966990	-5.291329	8.854720
-213.340565	-11.579256	8.864717
-211.422727	-13.476836	8.874714
-209.418933	-18.696032	8.884711
-207.595142	-11.046476	8.894707
-205.603466	-7.672665	8.904704
-203.805863	-13.231586	8.914701
-201.836298	-11.993723	8.924698
-199.854348	-15.924161	8.934695
-198.239137	-17.260276	8.944691
-196.686973	-12.966844	8.954688
-194.500710	-10.978817	8.964685
-192.376013	-15.438873	8.974682
-190.539285	-13.481905	8.984679
-189.033456	-15.230034	8.994675
-187.074223	-18.946836	9.004672
-184.944877	-13.024446	9.014669
-182.842982	-15.968220	9.024666
-181.324722	-15.474639	9.034663
-179.584188	-17.846006	9.044659
-177.513238	-23.058525	9.054656
-175.366970	-19.133043	9.064653
-173.865229	-13.192598	9.074650
-172.026367	-12.848066	9.084647
-170.306169	-13.795126	9.094643
-168.354996	-15.969571	9.104640
-166.388946	-11.071108	9.114637
-164.358577	-9.934495	9.124634
-162.654246	-13.796920	9.134631
-160.720778	-12.389052	9.144627
-158.658989	-6.972172	9.154624
-156.630741	-11.067861	9.164621
-155.138991	-8.152656	9.174618
-153.361801	-11.322490	9.184615
-151.337849	-8.785890	9.194611
-149.304181	-11.066643	9.204608
-147.660093	-5.927313	9.214605
-145.531114	-10.809595	9.224602
-143.605218	-8.641028	9.234599
-142.194504	2.665041	9.244595
-139.988622	-5.221626	9.254592
-138.114105	-12.588044	9.264589
-136.427411	-8.938142	9.274586
-134.476277	-4.136742	9.284583
-132.401434	-5.554049	9.294579
-130.696946	-5.338044	9.304576
-128.928116	-5.204937	9.314573
-126.813710	-4.809597	9.324570
-125.025942	1.217882	9.334567
-122.862619	-7.080401	9.344563
-121.332795	-4.577040	9.354560
-119.422179	-0.912324	9.364557
-117.499708	-2.840572	9.374554
-115.644780	-8.397528	9.384551
-113.937498	-4.692472	9.394547
-111.923241	-8.743262	9.404544
-110.061377	-1.270220	9.414541
-108.191281	-9.927497	9.424538
-106.312773	-7.868181	9.434535
-104.356320	-1.826546	9.444531
-102.114562	-8.878900	9.454528
-100.615448	-10.027482	9.464525
-98.837546	-4.543148	9.474522
-96.796381	1.527611	9.484519
-94.986611	1.955792	9.494515
-93.165712	-2.113084	9.504512
-91.250801	-4.341685	9.514509
-89.473234	-0.624138	9.524506
-87.673278	2.494573	9.534503
-85.786408	0.954136	9.544499
-83.657462	-7.310210	9.554496
-81.846590	-2.116913	9.564493
-79.936517	-5.399475	9.574490
-77.985280	-8.126495	9.584487
-75.956460	-3.826915	9.594483
-74.554291	-5.604227	9.604480
-72.560730	-6.987990	9.614477
-70.767521	-8.096629	9.624474
-68.359825	-5.534334	9.634471
-66.950680	-5.430642	9.644467
-65.076399	-5.949050	9.654464
-62.818449	-6.939192	9.664461
-61.037873	-7.205805	9.674458
-59.626287	-4.516171	9.684455
-57.933735	-2.065570	9.694451
-55.530534	-3.438878	9.704448
-53.518648	-8.725565	9.714445
-51.928590	-5.015972	9.724442
-49.876390	-3.473795	9.734439
-47.930883	-5.484611	9.744435
-46.252945	4.534683	9.754432
-44.413201	-1.179279	9.764429
-42.745601	-12.426852	9.774426
-40.590234	-2.949510	9.784423
-38.616730	-2.774776	9.794419
-36.841725	-3.976803	9.804416
-34.745017	-12.780705	9.814413
-33.175920	-5.341424	9.824410
-31.353873	-1.236189	9.834407
-29.470283	-1.533422	9.844403
-27.399450	-3.028949	9.854400
-25.275951	-1.629176	9.864397
-23.848088	-4.525301	9.874394
-22.044618	-2.918160	9.884391
-20.025139	5.726669	9.894387
-18.131849	0.844188	9.904384
-16.037246	-0.626699	9.914381
-14.201972	-2.638854	9.924378
-12.162802	2.257558	9.934375
-10.632131	2.940322	9.944371
-8.795970	5.865425	9.954368
-6.751625	-0.654834	9.964365
-4.964664	-2.059273	9.974362
-3.840169	18.298925	9.984359
-2.611414	58.353851	9.994355
-0.954428	110.857057	10.004352
0.000000	152.008276	10.009357
0.974254	197.911059	10.014362
1.633944	220.181349	10.019367
2.170495	236.814749	10.024371
2.131420	266.794374	10.029376
2.612350	283.917675	10.034381
2.453967	292.594220	10.039386
2.675355	300.046393	10.044391
3.451979	309.035864	10.049395
3.111126	328.031269	10.054400
3.199362	327.761762	10.059405
3.113420	332.643621	10.064410
3.336848	334.542966	10.069415
3.475746	331.444174	10.074419
3.443244	339.143447	10.079424
3.786012	346.284543	10.084429
3.947488	363.192383	10.089434
3.885088	361.975485	10.094439
4.018950	350.489560	10.099443
3.631373	352.792297	10.104448
3.993333	365.355136	10.109453
3.939136	367.727705	10.114458
4.273207	374.493305	10.119463
3.978845	373.564144	10.124467
3.911019	380.568895	10.129472
4.413999	382.775323	10.134477
4.110051	391.440452	10.139482
4.279083	396.901416	10.144487
4.458765	401.012366	10.149491
4.399860	390.802969	10.154496
4.581156	388.771325	10.159501
4.364837	379.258838	10.164506
4.325534	378.779435	10.169511
4.565186	378.279192	10.174515
4.422818	403.347519	10.179520
4.949237	393.456352	10.184525
4.584908	398.727995	10.189530
4.500924	398.176868	10.194535
4.617225	399.744796	10.199539
4.520327	408.903622	10.204544
4.880385	415.726598	10.209549
4.868034	417.537403	10.214554
5.083871	416.156271	10.219559
5.091575	415.921685	10.224563
4.806463	416.992236	10.229568
4.994458	417.134178	10.234573
5.194191	427.832146	10.239578
5.029771	416.076772	10.244583
4.889233	429.746432	10.249587
4.682129	423.520457	10.254592
5.291743	409.563165	10.259597
5.050908	431.032805	10.264602
5.033896	430.048363	10.269607
5.017512	430.576148	10.274611
5.018455	460.300626	10.279616
5.461387	452.455471	10.284621
5.341043	460.171973	10.289626
5.557344	467.946749	10.294631
5.720292	466.610319	10.299635
5.648049	470.447650	10.304640
5.790012	466.405302	10.309645
5.666253	473.135161	10.314650
5.511999	469.387646	10.319655
5.600988	469.212636	10.324659
5.419436	466.163351	10.329664
5.513892	462.633218	10.334669
5.551693	471.013644	10.339674
5.751609	486.363741	10.344679
5.983823	495.905376	10.349683
6.087287	507.068200	10.354688
6.492897	499.096507	10.359693
6.215897	514.980030	10.364698
6.244042	507.185236	10.369703
6.288453	508.013995	10.374707
6.127148	521.111451	10.379712
6.562390	515.066840	10.384717
6.032577	517.231436	10.389722
6.110347	513.107848	10.394727
6.190804	509.843294	10.399731
6.291116	524.548559	10.404736
6.300799	523.780632	10.409741
6.404014	519.301314	10.414746
6.673504	527.815134	10.419751
6.658682	524.743974	10.424755
6.537378	521.592025	10.429760
6.572542	516.716698	10.434765
6.525459	531.719876	10.439770
6.732724	545.796230	10.444775
7.052397	546.046484	10.449779
6.853399	549.713237	10.454784
7.083007	561.974074	10.459789
6.831735	554.892469	10.464794
6.734426	560.974735	10.469799
7.198737	558.945236	10.474803
6.881187	550.011772	10.479808
6.861785	556.344968	10.484813
7.201448	560.810502	10.489818
7.108791	553.681520	10.494823
7.189883	564.242390	10.499827
7.139805	570.228814	10.504832
7.637112	593.373218	10.509837
7.765122	591.991885	10.514842
7.111670	580.632144	10.519847
7.846402	585.363477	10.524851
7.623486	604.319929	10.529856
7.550528	595.684902	10.534861
7.454406	591.343016	10.539866
7.786801	600.662155	10.544871
7.521449	603.822248	10.549875
7.448261	601.697121	10.554880
7.803801	601.823380	10.559885
7.545890	596.173155	10.564890
7.597704	603.037501	10.569895
7.590731	610.253436	10.574899
7.691703	609.176045	10.579904
8.003762	623.431307	10.584909
7.745058	633.768872	10.589914
7.969132	626.075232	10.594919
8.152518	635.672058	10.599923
8.030155	632.889273	10.604928
8.320282	636.015969	10.609933
8.239472	646.672111	10.614938
8.212579	634.781079	10.619943
8.473074	635.982247	10.624947
8.204565	645.154399	10.629952
8.512745	641.877149	10.634957
8.401050	646.342159	10.639962
8.873071	669.606628	10.644967
8.819908	656.855567	10.649971
8.556972	660.048405	10.654976
9.120415	660.625646	10.659981
8.770869	657.035393	10.664986
8.821821	650.419640	10.669991
8.970911	638.047935	10.674995
8.795509	658.944483	10.680000
8.918254	661.843984	10.685005
8.873309	674.841015	10.690010
9.143529	674.862609	10.695015
9.274072	685.664847	10.700019
9.025459	694.262979	10.705024
9.546677	684.886552	10.710029
9.276768	696.176886	10.715034
9.236106	692.825950	10.720039
9.418594	677.908318	10.725043
9.315534	697.631126	10.730048
9.458899	690.237342	10.735053
9.278027	693.543258	10.740058
9.291443	693.279371	10.745063
9.761217	687.916759	10.750067
9.659980	691.321940	10.755072
9.504751	692.740814	10.760077
9.394960	696.784475	10.765082
9.545515	699.444573	10.770087
9.526115	692.220257	10.775091
9.723846	710.890550	10.780096
9.454546	689.219653	10.785101
9.365276	706.532178	10.790106
9.492840	704.595797	10.795111
9.836780	719.842741	10.800115
9.958060	723.732854	10.805120
10.081968	732.266861	10.810125
10.462485	731.528088	10.815130
10.240279	723.523940	10.820135
10.423772	730.499813	10.825139
10.141029	726.730146	10.830144
10.417304	733.601332	10.835149
10.193326	725.818248	10.840154
9.942632	735.102738	10.845159
10.369524	724.478141	10.850163
9.904881	735.082023	10.855168
10.305440	731.085092	10.860173
10.035545	726.334049	10.865178
10.135187	729.738740	10.870183
10.691286	745.148999	10.875187
10.877052	754.841722	10.880192
10.792670	756.119987	10.885197
11.003911	770.344164	10.890202
10.723242	769.592572	10.895207
11.014170	765.352910	10.900211
11.027370	767.881958	10.905216
11.129979	763.095144	10.910221
10.821054	752.168402	10.915226
11.227246	760.589589	10.920231
11.138383	748.940170	10.925235
10.935646	760.726062	10.930240
11.268587	753.213696	10.935245
11.017191	753.700126	10.940250
11.104606	768.237377	10.945255
11.567389	763.618629	10.950259
11.112266	774.579005	10.955264
10.964508	774.533220	10.960269
11.202948	778.352619	10.965274
11.121135	763.415551	10.970279
11.207334	776.100006	10.975283
11.249347	781.797428	10.980288
11.581201	772.235097	10.985293
11.404150	782.069290	10.990298
11.474041	796.049521	10.995303
11.719415	802.919360	11.000307
11.533508	807.688006	11.005312
11.414324	807.476807	11.010317
11.512920	807.538392	11.015322
11.485059	810.668535	11.020327
11.778715	805.996321	11.025331
11.710138	815.365360	11.030336
12.089276	811.794467	11.035341
12.152695	820.793933	11.040346
12.087144	831.739526	11.045351
12.406579	827.441680	11.050355
12.152499	823.366204	11.055360
12.387348	812.914106	11.060365
12.395363	813.439590	11.065370
12.291945	816.449316	11.070375
12.590226	806.004453	11.075379
11.896441	819.983505	11.080384
12.255707	832.966670	11.085389
12.658088	834.845425	11.090394
12.707244	839.579743	11.095399
12.980629	836.050944	11.100403
12.822797	837.711532	11.105408
12.929854	832.348370	11.110413
12.854196	831.496263	11.115418
12.692127	818.628383	11.120423
12.729939	812.208628	11.125427
13.058219	833.944496	11.130432
13.274456	818.423644	11.135437
13.013606	815.976739	11.140442
12.617246	810.597682	11.145447
13.320735	813.423510	11.150451
12.632590	827.477367	11.155456
13.016817	835.916295	11.160461
13.135577	839.931426	11.165466
13.139133	842.283821	11.170471
13.326242	835.160543	11.175475
12.772633	844.998066	11.180480
12.926242	844.268671	11.185485
13.167853	844.521921	11.190490
12.889857	845.873654	11.195495
13.240703	854.368382	11.200499
13.247527	870.254333	11.205504
13.504958	876.111408	11.210509
13.584412	880.533385	11.215514
13.522277	887.534318	11.220519
13.916327	874.932520	11.225523
13.634737	875.565703	11.230528
14.323528	878.490088	11.235533
14.039043	877.347994	11.240538
13.716125	883.914256	11.245543
13.941162	876.010586	11.250547
14.048535	881.260784	11.255552
14.002157	871.780794	11.260557
13.818072	883.642663	11.265562
14.055599	882.691712	11.270567
14.064538	868.263637	11.275571
13.956278	879.839005	11.280576
13.932017	883.675100	11.285581
14.163748	874.254835	11.290586
14.304602	879.299409	11.295591
14.439555	874.800727	11.300595
14.261289	879.077721	11.305600
14.339350	873.288640	11.310605
14.473364	881.303856	11.315610
14.491515	881.259995	11.320615
14.684439	892.438810	11.325619
14.640574	905.029000	11.330624
14.786804	892.070878	11.335629
14.765029	893.370709	11.340634
14.422638	899.865964	11.345639
14.876393	902.782108	11.350643
14.439082	908.917171	11.355648
14.902396	904.744596	11.360653
14.809941	910.856197	11.365658
14.901242	905.956016	11.370663
15.133373	913.182853	11.375667
15.218319	916.679823	11.380672
15.136220	914.494566	11.385677
15.188014	904.142567	11.390682
15.068674	914.021263	11.395687
15.415599	908.747555	11.400691
15.105636	912.933594	11.405696
15.125031	908.540070	11.410701
14.801889	919.140440	11.415706
15.204418	912.181473	11.420711
15.610083	902.936885	11.425715
15.357629	913.639523	11.430720
15.484263	914.354260	11.435725
15.377582	923.537048	11.440730
15.468680	944.822031	11.445735
15.610945	934.176444	11.450739
15.750194	937.958087	11.455744
16.122921	936.725358	11.460749
15.989917	938.962348	11.465754
16.211053	935.743073	11.470759
16.032318	925.938787	11.475763
16.030144	919.720914	11.480768
16.201347	904.664494	11.485773
16.061519	902.453752	11.490778
15.768001	916.223966	11.495783
15.873854	901.599040	11.500787
15.890109	929.074761	11.505792
15.843867	936.639339	11.510797
16.096301	940.218416	11.515802
16.155449	944.601072	11.520807
16.306258	939.495836	11.525811
16.072649	949.987325	11.530816
16.529461	942.117619	11.535821
16.034653	949.102431	11.540826
16.236838	952.413545	11.545831
16.290885	949.739763	11.550835
16.379242	964.087816	11.555840
16.569055	967.661117	11.560845
17.314069	969.218722	11.565850
17.052748	961.312149	11.570855
17.220150	950.783973	11.575859
16.942860	947.357172	11.580864
16.949884	945.687581	11.585869
16.825974	942.772511	11.590874
16.701505	946.864315	11.595879
16.870052	948.155874	11.600883
16.985530	950.988780	11.605888
17.150273	959.276698	11.610893
16.971600	959.234265	11.615898
17.019153	979.955357	11.620903
17.513137	972.455042	11.625907
17.500763	976.763955	11.630912
17.362922	965.379231	11.635917
17.431086	952.406698	11.640922
17.138912	950.581389	11.645927
17.672356	952.303630	11.650931
17.471098	967.995783	11.655936
17.816541	968.675624	11.660941
17.768409	948.295355	11.665946
17.408071	953.626486	11.670951
17.389786	943.478035	11.675955
17.459671	969.795617	11.680960
17.413156	975.308527	11.685965
17.691046	983.453825	11.690970
17.646924	979.179227	11.695975
18.105728	978.158283	11.700979
18.028360	986.054299	11.705984
18.096872	975.019876	11.710989
18.374074	976.814532	11.715994
17.691116	979.271715	11.720999
18.206189	979.257412	11.726003
18.201883	976.271216	11.731008
18.003560	977.655987	11.736013
18.063294	971.295747	11.741018
17.904653	981.567132	11.746023
18.029235	975.535611	11.751027
18.006273	987.259895	11.756032
18.292186	988.179480	11.761037
18.176721	987.253284	11.766042
18.487462	997.383580	11.771047
18.690383	998.354252	11.776051
18.458110	999.421146	11.781056
18.804730	1008.178429	11.786061
18.856646	1003.804922	11.791066
18.510081	1010.445979	11.796071
19.016286	1001.691525	11.801075
18.591670	1011.986430	11.806080
18.856366	1003.155370	11.811085
19.265843	1002.940278	11.816090
18.777534	1003.759409	11.821095
19.103859	1003.833562	11.826099
19.179965	1008.404355	11.831104
19.070202	1007.464632	11.836109
18.912351	1007.910916	11.841114
18.651527	999.247261	11.846119
18.720296	998.913035	11.851123
19.049554	1001.938949	11.856128
18.821128	1009.499504	11.861133
18.849410	1005.197580	11.866138
18.969281	1018.627550	11.871143
19.310042	1022.709832	11.876147
19.293933	1027.747952	11.881152
19.320969	1030.263800	11.886157
19.338923	1034.216211	11.891162
19.354271	1027.329983	11.896167
19.510327	1021.673491	11.901171
19.325342	1032.422229	11.906176
19.275527	1025.682021	11.911181
19.592071	1040.578838	11.916186
19.905072	1048.523020	11.921191
20.070835	1052.805120	11.926195
20.393630	1052.072386	11.931200
20.347475	1032.391894	11.936205
20.094158	1030.834784	11.941210
19.907704	1035.182519	11.946215
20.369831	1029.138141	11.951219
20.010715	1031.376514	11.956224
19.844968	1024.068135	11.961229
20.047385	1027.037009	11.966234
20.237254	1026.836441	11.971239
19.978591	1024.753450	11.976243
20.091408	1042.712273	11.981248
20.368038	1052.773927	11.986253
20.509685	1051.699479	11.991258
20.467856	1051.341888	11.996263
20.789456	1045.028164	12.001267
20.470510	1057.875261	12.006272
20.355267	1056.609959	12.011277
20.721612	1055.207917	12.016282
20.403166	1058.671484	12.021287
20.790804	1058.280090	12.026291
20.953873	1062.949001	12.031296
20.546734	1050.451183	12.036301
20.797097	1049.788353	12.041306
20.618153	1052.614619	12.046311
20.321559	1030.364054	12.051315
20.467833	1037.065297	12.056320
20.794898	1049.580679	12.061325
20.631612	1042.238781	12.066330
20.494341	1036.146490	12.071335
20.693558	1043.966883	12.076339
20.479586	1033.319691	12.081344
20.841543	1043.495471	12.086349
20.923221	1033.463485	12.091354
20.456703	1039.458172	12.096359
21.003761	1027.967315	12.101363
20.851218	1037.621141	12.106368
20.247043	1031.600168	12.111373
20.642384	1039.253651	12.116378
20.426473	1043.867877	12.121383
20.624993	1039.187108	12.126387
20.714706	1037.931697	12.131392
20.827406	1026.492772	12.136397
20.679046	1035.969301	12.141402
20.242143	1038.994412	12.146407
20.666207	1035.168704	12.151411
20.490833	1043.676507	12.156416
20.769646	1043.039104	12.161421
20.902702	1041.425098	12.166426
20.766059	1039.310026	12.171431
20.795493	1036.960296	12.176435
20.713060	1041.438107	12.181440
20.483101	1042.690727	12.186445
20.683398	1039.014255	12.191450
20.516908	1041.455309	12.196455
20.571254	1039.563680	12.201459
20.521036	1039.593805	12.206464
20.591936	1042.195705	12.211469
20.711663	1038.593589	12.216474
20.487876	1041.586286	12.221479
20.893493	1032.439402	12.226483
20.978611	1038.144243	12.231488
20.606199	1028.484325	12.236493
20.374405	1020.194519	12.241498
20.581202	1023.922831	12.246503
20.777318	1022.885432	12.251507
20.447348	1017.930971	12.256512
20.753856	1019.694148	12.261517
20.445629	1013.837305	12.266522
20.537539	1021.573869	12.271527
20.567658	1021.882934	12.276531
20.409171	1031.917773	12.281536
20.788515	1029.304065	12.286541
20.694737	1020.162718	12.291546
20.420195	1017.489290	12.296551
20.767891	1019.695357	12.301555
20.515926	1016.087870	12.306560
20.544885	1018.155528	12.311565
20.499766	1012.925388	12.316570
20.656501	1021.030104	12.321575
20.542453	1009.327718	12.326579
20.652416	1019.288191	12.331584
20.402882	1013.229587	12.336589
20.968762	1012.656792	12.341594
20.449834	1021.656220	12.346599
20.335685	1017.500018	12.351603
20.454391	1030.234707	12.356608
20.650080	1036.005495	12.361613
20.529176	1044.548769	12.366618
20.653835	1047.031702	12.371623
20.667577	1043.810787	12.376627
20.814697	1030.746738	12.381632
20.407448	1028.274258	12.386637
20.970862	1015.416655	12.391642
20.931276	1022.751544	12.396647
20.905958	1018.328846	12.401651
20.691919	1021.338910	12.406656
20.495947	1017.924354	12.411661
20.564258	1019.518930	12.416666
20.083732	1023.325326	12.421671
20.793176	1020.887641	12.426675
20.507018	1029.652817	12.431680
20.586508	1021.702892	12.436685
20.579983	1019.614382	12.441690
19.946043	1029.117889	12.446695
20.138461	1022.591375	12.451699
20.330056	1037.028695	12.456704
20.554295	1045.138429	12.461709
20.773556	1054.628880	12.466714
20.680548	1060.340061	12.471719
20.813244	1053.110231	12.476723
20.825822	1038.097898	12.481728
20.402170	1039.528076	12.486733
20.432954	1028.971168	12.491738
20.390667	1031.774056	12.496743
20.874302	1041.206562	12.501747
20.739831	1032.103239	12.506752
20.558899	1031.780452	12.511757
20.727011	1031.274252	12.516762
20.651227	1036.768198	12.521767
20.661263	1019.445913	12.526771
20.763593	1027.415798	12.531776
20.828680	1033.895009	12.536781
20.829308	1030.826008	12.541786
20.744080	1038.306965	12.546791
20.862706	1035.141868	12.551795
20.612549	1037.421214	12.556800
20.465845	1025.903807	12.561805
20.797316	1025.582877	12.566810
20.744627	1034.287163	12.571815
20.845674	1035.575302	12.576819
20.839533	1030.439870	12.581824
20.752281	1032.358898	12.586829
20.498300	1012.088646	12.591834
20.176967	1023.625569	12.596839
20.652240	1026.008419	12.601843
20.823235	1048.245965	12.606848
20.711959	1039.736640	12.611853
20.688938	1025.671496	12.616858
20.245286	1022.902030	12.621863
20.851461	1024.122219	12.626867
20.744555	1023.781317	12.631872
20.407472	1017.280907	12.636877
20.817486	1006.400163	12.641882
20.424915	1014.961516	12.646887
20.128379	1014.805410	12.651891
20.515115	1030.567861	12.656896
20.640566	1036.778809	12.661901
20.947039	1038.595614	12.666906
20.526902	1035.932788	12.671911
20.528854	1024.697619	12.676915
20.620626	1024.017505	12.681920
20.605566	1028.699045	12.686925
20.620425	1022.552532	12.691930
20.402454	1017.965008	12.696935
20.716394	1020.791507	12.701939
20.557252	1029.351910	12.706944
20.663296	1020.604496	12.711949
20.737391	1008.506227	12.716954
20.325782	1021.267141	12.721959
20.662226	1007.248767	12.726963
20.237472	1015.279057	12.731968
20.487393	1033.769546	12.736973
20.620026	1040.190674	12.741978
20.738879	1051.469742	12.746983
20.893939	1038.697751	12.751987
20.394089	1033.579558	12.756992
20.258626	1027.214153	12.761997
20.254534	1032.529496	12.767002
20.362123	1048.550968	12.772007
20.886752	1042.700056	12.777011
21.012902	1050.317627	12.782016
20.721463	1041.204639	12.787021
20.923562	1032.334657	12.792026
20.448127	1023.497047	12.797031
20.798623	1025.157009	12.802035
20.635318	1021.541689	12.807040
20.667946	1026.674543	12.812045
20.643135	1007.927446	12.817050
20.582179	1022.996426	12.822055
20.760863	1022.491695	12.827059
20.944859	1017.636620	12.832064
20.559766	1019.795550	12.837069
20.616398	1031.691690	12.842074
20.585261	1023.762563	12.847079
20.718409	1017.079915	12.852083
20.444398	1030.855011	12.857088
20.543608	1022.602301	12.862093
20.827191	1020.898053	12.867098
20.560994	1032.692710	12.872103
20.592626	1025.780229	12.877107
20.483141	1028.114412	12.882112
20.479748	1022.511738	12.887117
20.590451	1028.887471	12.892122
20.650624	1032.953004	12.897127
20.896653	1025.299810	12.902131
20.683953	1029.978179	12.907136
20.777651	1035.006673	12.912141
20.819914	1034.168864	12.917146
20.698499	1032.396738	12.922151
20.582730	1026.999655	12.927155
20.811829	1035.138571	12.932160
20.774507	1024.256618	12.937165
20.462786	1002.743413	12.942170
20.216931	1000.970637	12.947175
20.623407	1010.237223	12.952179
20.912540	1026.004197	12.957184
20.710525	1013.260793	12.962189
20.754622	998.552574	12.967194
20.311424	1003.720309	12.972199
20.871970	1005.066053	12.977203
20.517858	993.558096	12.982208
20.520435	994.931328	12.987213
20.622625	1004.345796	12.992218
20.595671	1006.097499	12.997223
20.579892	999.544273	13.002227
20.683899	1008.671433	13.007232
20.466488	1002.002123	13.012237
20.927984	995.685031	13.017242
20.389885	999.227775	13.022247
20.332047	997.248383	13.027251
20.504272	1001.600405	13.032256
20.230705	998.683960	13.037261
20.614735	1000.059434	13.042266
20.194839	1011.821815	13.047271
20.504671	1020.871996	13.052275
20.829103	1032.447863	13.057280
20.590950	1038.721536	13.062285
20.880511	1032.889196	13.067290
20.366567	1017.085600	13.072295
20.285556	1030.498733	13.077299
20.586198	1034.987988	13.082304
20.632832	1039.850515	13.087309
20.925649	1043.874214	13.092314
20.666644	1027.518981	13.097319
20.877835	1014.731750	13.102323
20.379665	1016.926062	13.107328
20.454678	1007.133292	13.112333
20.750478	998.010252	13.117338
20.428694	1015.158368	13.122343
20.306612	993.447763	13.127347
20.203828	1020.133618	13.132352
20.380390	1036.399557	13.137357
20.564298	1041.535098	13.142362
20.639105	1050.539200	13.147367
20.553991	1040.593739	13.152371
20.548512	1050.476447	13.157376
20.829153	1043.371268	13.162381
20.717517	1045.267377	13.167386
20.825960	1040.277678	13.172391
20.371144	1044.564134	13.177395
20.839008	1052.012079	13.182400
20.593844	1040.563984	13.187405
20.331293	1028.350648	13.192410
20.128429	1035.378829	13.197415
20.467338	1047.201573	13.202419
20.311738	1041.769833	13.207424
20.166251	1046.894831	13.212429
20.573199	1050.517106	13.217434
20.455110	1038.775914	13.222439
20.881702	1047.141975	13.227443
20.976103	1040.014459	13.232448
20.547446	1050.261146	13.237453
20.626196	1047.129217	13.242458
20.493013	1053.329380	13.247463
20.556432	1043.850690	13.252467
20.820455	1053.297729	13.257472
20.212453	1054.309429	13.262477
20.374616	1046.794188	13.267482
20.360519	1047.551880	13.272487
20.258438	1042.365510	13.277491
20.449190	1045.757321	13.282496
20.479084	1047.638741	13.287501
20.673088	1042.406724	13.292506
20.533928	1050.268473	13.297511
20.588434	1048.132375	13.302515
20.873887	1042.363768	13.307520
20.389461	1047.148563	13.312525
20.656979	1042.674421	13.317530
21.161447	1043.956568	13.322535
20.838829	1042.650221	13.327539
20.695625	1052.941273	13.332544
20.794556	1053.737712	13.337549
20.834649	1051.258538	13.342554
20.595701	1056.272282	13.347559
20.580344	1045.382078	13.352563
20.662843	1056.288456	13.357568
20.360813	1052.133824	13.362573
20.638894	1053.835303	13.367578
20.719380	1051.770759	13.372583
20.833683	1060.085704	13.377587
20.715026	1049.205666	13.382592
20.685589	1028.841226	13.387597
20.744278	1025.296160	13.392602
20.529632	1025.529139	13.397607
20.639968	1022.601925	13.402611
20.311615	1023.824502	13.407616
20.404792	1023.480074	13.412621
20.862344	1020.674109	13.417626
20.857054	1019.178372	13.422631
20.660487	1026.524107	13.427635
20.424098	1027.661050	13.432640
20.662913	1034.634554	13.437645
20.890607	1019.024924	13.442650
20.173759	1028.448608	13.447655
20.276851	1027.869196	13.452659
20.460061	1022.971664	13.457664
20.321441	1027.549902	13.462669
20.670673	1039.751061	13.467674
20.924712	1043.377221	13.472679
20.727786	1036.479110	13.477683
20.391355	1032.687960	13.482688
20.367543	1027.214705	13.487693
20.545534	1019.133947	13.492698
20.245386	1034.308902	13.497703
20.742490	1049.211626	13.502707
20.939837	1057.399777	13.507712
20.403807	1040.554093	13.512717
20.373316	1034.110438	13.517722
20.375262	1053.690817	13.522727
20.426815	1052.332676	13.527731
20.685702	1062.168494	13.532736
20.477965	1064.256563	13.537741
21.068285	1052.531691	13.542746
20.807976	1055.404052	13.547751
20.463162	1035.969898	13.552755
20.544451	1028.992722	13.557760
20.608978	1028.925693	13.562765
20.713484	1027.437676	13.567770
20.682761	1033.668800	13.572775
20.648564	1015.587128	13.577779
20.705263	1031.077347	13.582784
20.426217	1035.230103	13.587789
20.569749	1025.136215	13.592794
20.391850	1039.935264	13.597799
20.435828	1027.871748	13.602803
20.748555	1030.072354	13.607808
20.483001	1035.962442	13.612813
20.643560	1028.414348	13.617818
20.663991	1032.311167	13.622823
20.644357	1031.599932	13.627827
20.819793	1028.622906	13.632832
20.633283	1031.820981	13.637837
20.854937	1030.292200	13.642842
20.397565	1033.520860	13.647847
20.631637	1026.732218	13.652851
20.772751	1027.696980	13.657856
20.215781	1030.255508	13.662861
20.567271	1035.339086	13.667866
20.329521	1037.305774	13.672871
20.763674	1032.981687	13.677875
20.770439	1031.706389	13.682880
20.276054	1029.399203	13.687885
20.601559	1031.954184	13.692890
20.699712	1031.465451	13.697895
20.522138	1038.377629	13.702899
20.626586	1030.816405	13.707904
20.580920	1035.040753	13.712909
20.532695	1029.587162	13.717914
20.267915	1038.003559	13.722919
20.600862	1031.747958	13.727923
20.581200	1015.058080	13.732928
20.211326	1037.291983	13.737933
20.614741	1032.712586	13.742938
20.792533	1045.882593	13.747943
20.539044	1045.815820	13.752947
20.827935	1034.837672	13.757952
20.649646	1034.206938	13.762957
20.891955	1035.887311	13.767962
20.699228	1034.949779	13.772967
20.762204	1034.769450	13.777971
20.563759	1038.798957	13.782976
20.348244	1040.348912	13.787981
20.649558	1027.799623	13.792986
20.342334	1037.676829	13.797991
20.613035	1035.772772	13.802995
20.795917	1027.675458	13.808000
20.382790	1037.806113	13.813005
20.797085	1035.227832	13.818010
20.916152	1032.627248	13.823015
20.628815	1033.319704	13.828019
20.772210	1035.757066	13.833024
20.459614	1040.216390	13.838029
20.664210	1039.885733	13.843034
20.629336	1042.547083	13.848039
20.572305	1036.880415	13.853043
20.785545	1037.008876	13.858048
20.509331	1035.636778	13.863053
20.731144	1032.635007	13.868058
20.404265	1039.017455	13.873063
20.643428	1041.767570	13.878067
20.998749	1038.583645	13.883072
20.684956	1033.763802	13.888077
20.872572	1040.676086	13.893082
20.519078	1031.929414	13.898087
20.514465	1033.105088	13.903091
20.517463	1042.466012	13.908096
20.350894	1042.563583	13.913101
20.674103	1038.738189	13.918106
20.590407	1041.432559	13.923111
20.499153	1035.861241	13.928115
20.531759	1041.028799	13.933120
20.409679	1035.334657	13.938125
20.622631	1037.131683	13.943130
20.217285	1046.565623	13.948135
20.545365	1027.965656	13.953139
20.681693	1037.414127	13.958144
20.517374	1039.031614	13.963149
20.401639	1042.208940	13.968154
20.457938	1043.518411	13.973159
20.361634	1046.831420	13.978163
20.714891	1040.610425	13.983168
20.678452	1039.482375	13.988173
20.775957	1036.278066	13.993178
20.394325	1050.447260	13.998183
20.526118	1049.514741	14.003187
20.743222	1046.251928	14.008192
20.476375	1051.364910	14.013210
20.608566	1046.865454	14.018227
20.265391	1042.312829	14.023245
20.456920	1048.700269	14.028263
20.480067	1045.937524	14.033280
20.283960	1054.559143	14.038298
20.592247	1047.521047	14.043315
20.650917	1046.248585	14.048333
20.761452	1041.373485	14.053351
20.722992	1042.222798	14.058368
20.429075	1052.766524	14.063386
20.373722	1057.087060	14.068403
20.688990	1070.203066	14.073421
20.515510	1080.186480	14.078439
20.758632	1079.696280	14.083456
20.723692	1077.671107	14.088474
20.730143	1078.079103	14.093491
20.809318	1077.696849	14.098509
20.842059	1080.063794	14.103527
20.895790	1083.816379	14.108544
20.574206	1083.424112	14.113562
20.936639	1074.247483	14.118579
20.935155	1081.760550	14.123597
20.732395	1080.794052	14.128615
21.056971	1067.516282	14.133632
20.607975	1083.170370	14.138650
20.478692	1080.273054	14.143667
21.033112	1098.567114	14.148685
21.277390	1108.617625	14.153703
21.412690	1096.950917	14.158720
21.118441	1109.225073	14.163738
21.575932	1109.672816	14.168755
21.252633	1092.210267	14.173773
21.262271	1079.184066	14.178791
21.302260	1070.570103	14.183808
21.283331	1078.702579	14.188826
21.270302	1075.437510	14.193843
21.502099	1081.044610	14.198861
21.190136	1080.823842	14.203879
21.557412	1079.061707	14.208896
21.221543	1076.957115	14.213914
21.350618	1072.263092	14.218931
21.429588	1068.505150	14.223949
21.249612	1083.413186	14.228967
21.621188	1075.134873	14.233984
21.304924	1083.888931	14.239002
21.575592	1078.539964	14.244019
21.571414	1082.761109	14.249037
21.311870	1078.099180	14.254055
21.302954	1078.435694	14.259072
21.316204	1090.667082	14.264090
21.417549	1083.737481	14.269107
21.424334	1078.721612	14.274125
21.366277	1096.971784	14.279143
21.586145	1069.028034	14.284160
21.117445	1081.344148	14.289178
21.365164	1089.869831	14.294195
21.821162	1101.184321	14.299213
21.525377	1105.952207	14.304231
21.859926	1105.837536	14.309248
21.577216	1110.461766	14.314266
21.831704	1106.273122	14.319283
21.666780	1115.583511	14.324301
21.739587	1116.246768	14.329319
21.857860	1107.024117	14.334336
21.821187	1117.457647	14.339354
21.807788	1106.148132	14.344371
21.725929	1099.000777	14.349389
21.564822	1111.132576	14.354407
22.014630	1099.868736	14.359424
21.862928	1110.040608	14.364442
21.956292	1110.286877	14.369459
21.963210	1114.904239	14.374477
21.804877	1116.686609	14.379495
22.020993	1101.804308	14.384512
22.057086	1117.530502	14.389530
21.882459	1112.041758	14.394547
22.136705	1102.075401	14.399565
22.363733	1102.619677	14.404583
22.177523	1088.866502	14.409600
21.826294	1086.676269	14.414618
21.862479	1086.285142	14.419635
22.039949	1086.934849	14.424653
21.838358	1113.694443	14.429671
21.926288	1104.965847	14.434688
22.072992	1109.208553	14.439706
22.136608	1112.734624	14.444723
22.495526	1111.348201	14.449741
22.080586	1124.561845	14.454759
22.590895	1107.675759	14.459776
22.106236	1117.125235	14.464794
22.187379	1113.763339	14.469811
21.931649	1110.694275	14.474829
21.695232	1120.157643	14.479847
22.124009	1114.945467	14.484864
22.226564	1111.100381	14.489882
22.200661	1116.278260	14.494899
22.124805	1118.473768	14.499917
22.256208	1123.774425	14.504935
22.258060	1110.253931	14.509952
22.115437	1125.108862	14.514970
22.564557	1135.785823	14.519987
22.709944	1149.400908	14.525005
22.132661	1146.766943	14.530023
22.505866	1143.400930	14.535040
22.562142	1149.443468	14.540058
22.899741	1136.108502	14.545075
22.854141	1149.003709	14.550093
22.367157	1127.557550	14.555111
22.458058	1116.785100	14.560128
22.509462	1148.648231	14.565146
22.666250	1146.218085	14.570163
22.560478	1139.654976	14.575181
22.646145	1152.793520	14.580199
22.759642	1142.203065	14.585216
22.864651	1154.306613	14.590234
22.592350	1150.530742	14.595251
22.915184	1148.503552	14.600269
22.643827	1159.278140	14.605287
22.720279	1149.502131	14.610304
22.898343	1160.316724	14.615322
22.833942	1152.529478	14.620339
22.994823	1142.669220	14.625357
23.102780	1146.619240	14.630375
23.181418	1144.594819	14.635392
23.045980	1133.811264	14.640410
22.599094	1129.048636	14.645427
23.116050	1127.907568	14.650445
22.731013	1130.229469	14.655463
23.014931	1140.456152	14.660480
23.039565	1150.190938	14.665498
22.934759	1147.080490	14.670515
23.258380	1145.090928	14.675533
22.792280	1157.147140	14.680551
22.773015	1142.434475	14.685568
23.119671	1159.629163	14.690586
22.780899	1152.082307	14.695603
23.278180	1148.794032	14.700621
22.749581	1157.209190	14.705639
23.083374	1148.411466	14.710656
22.993999	1146.505078	14.715674
22.983741	1155.021609	14.720691
23.700043	1143.167814	14.725709
23.244424	1150.404135	14.730727
23.291721	1141.781099	14.735744
23.231771	1140.771369	14.740762
23.572967	1147.801949	14.745779
23.660163	1145.102903	14.750797
23.406153	1150.488636	14.755815
23.409353	1141.071957	14.760832
23.344472	1136.470197	14.765850
23.368731	1140.627048	14.770867
23.485918	1139.197379	14.775885
23.122154	1147.391185	14.780903
22.995921	1142.327297	14.785920
23.508815	1149.802405	14.790938
23.621805	1163.336152	14.795955
24.094370	1160.624403	14.800973
23.812512	1143.052935	14.805991
23.662923	1150.021793	14.811008
23.511280	1145.352070	14.816026
23.553097	1152.406806	14.821043
23.912713	1141.363388	14.826061
23.425210	1144.052421	14.831079
23.687801	1139.884499	14.836096
23.615863	1143.517141	14.841114
23.533395	1150.813498	14.846131
23.560962	1162.249851	14.851149
23.913584	1174.095270	14.856167
23.925952	1174.142098	14.861184
23.742446	1171.039479	14.866202
24.189710	1171.015371	14.871219
23.928737	1162.364411	14.876237
23.920853	1145.156660	14.881255
23.985463	1148.407300	14.886272
23.944396	1140.913642	14.891290
23.545180	1138.900942	14.896307
24.072403	1145.565221	14.901325
23.884078	1166.972896	14.906343
24.154373	1167.113868	14.911360
24.300605	1172.075547	14.916378
23.986087	1172.028219	14.921395
24.140193	1152.768547	14.926413
24.290607	1158.769333	14.931431
24.193346	1160.205336	14.936448
23.830721	1149.461151	14.941466
23.935773	1159.043116	14.946483
24.572657	1161.813944	14.951501
24.507956	1160.627217	14.956519
24.305190	1151.057763	14.961536
24.178509	1135.608752	14.966554
24.116684	1144.814626	14.971571
24.353779	1155.924971	14.976589
24.302965	1166.886187	14.981607
24.543287	1159.585169	14.986624
24.142942	1158.050850	14.991642
24.421287	1157.059523	14.996659
24.374192	1162.385517	15.001677
24.098232	1175.212095	15.006695
24.263018	1166.812553	15.011712
24.293770	1162.360701	15.016730
24.354459	1171.553344	15.021747
24.457337	1174.596537	15.026765
24.710937	1175.449613	15.031783
24.833356	1167.324246	15.036800
24.659460	1171.784846	15.041818
24.702653	1173.067887	15.046835
24.764875	1165.186505	15.051853
24.532121	1167.863226	15.056871
24.433685	1171.078527	15.061888
24.919967	1158.651068	15.066906
24.318384	1171.924410	15.071923
24.915543	1158.675442	15.076941
24.952847	1165.194498	15.081959
24.902622	1158.053080	15.086976
24.962929	1162.907336	15.091994
24.556948	1171.140923	15.097011
25.037099	1163.085918	15.102029
25.041763	1171.118728	15.107047
24.983882	1158.369068	15.112064
24.983725	1166.330284	15.117082
24.761703	1166.268204	15.122099
24.865972	1165.974755	15.127117
24.922607	1160.412928	15.132135
24.722254	1169.312147	15.137152
24.854837	1178.974678	15.142170
24.637326	1176.994340	15.147187
24.929917	1165.481816	15.152205
24.685778	1179.261303	15.157223
24.589851	1172.529866	15.162240
25.044792	1181.776040	15.167258
25.205297	1189.697486	15.172275
25.212492	1195.124947	15.177293
24.850580	1194.360005	15.182311
25.054016	1195.008722	15.187328
25.182255	1191.585813	15.192346
25.022545	1197.908215	15.197363
25.201530	1183.975579	15.202381
25.537791	1198.491507	15.207399
25.494872	1191.344189	15.212416
25.532120	1185.654882	15.217434
25.175779	1202.260167	15.222451
25.216989	1193.027730	15.227469
25.577845	1194.862584	15.232487
25.351854	1194.665854	15.237504
25.351368	1192.062582	15.242522
25.587367	1187.626751	15.247539
25.607755	1190.274112	15.252557
25.320154	1183.857961	15.257575
25.032033	1191.751861	15.262592
25.505700	1183.690014	15.267610
25.572604	1194.528655	15.272627
25.746987	1192.487383	15.277645
25.887772	1187.267632	15.282663
25.587055	1185.972253	15.287680
25.725444	1184.380322	15.292698
25.497108	1198.799108	15.297715
25.548532	1196.215871	15.302733
25.547073	1192.629601	15.307751
25.403097	1193.549236	15.312768
25.687683	1195.397827	15.317786
25.702011	1205.996321	15.322803
25.939789	1207.471703	15.327821
25.638050	1207.724361	15.332839
25.819076	1223.891602	15.337856
26.175013	1217.201334	15.342874
25.811457	1212.776176	15.347891
26.061432	1224.043396	15.352909
26.099596	1216.966504	15.357927
25.902187	1214.028117	15.362944
26.162957	1211.397330	15.367962
26.112976	1214.949409	15.372979
26.209605	1221.315881	15.377997
26.319799	1212.047261	15.383015
25.927468	1213.113475	15.388032
26.146196	1209.034327	15.393050
26.128654	1212.606401	15.398067
26.321302	1211.164690	15.403085
26.576189	1211.303401	15.408103
25.832679	1215.884752	15.413120
26.208797	1208.120025	15.418138
26.382532	1214.438016	15.423155
26.444391	1221.859255	15.428173
26.520064	1214.494806	15.433191
26.340280	1214.352055	15.438208
25.917997	1200.567212	15.443226
26.282321	1220.507263	15.448243
26.487230	1217.698192	15.453261
26.211739	1219.972746	15.458279
26.226880	1218.277771	15.463296
26.253704	1217.320263	15.468314
26.317123	1217.459625	15.473331
26.280039	1219.910089	15.478349
26.470344	1223.247665	15.483367
26.463720	1217.653434	15.488384
26.745076	1218.251972	15.493402
26.486850	1220.182422	15.498419
26.567987	1220.520307	15.503437
26.548453	1216.046571	15.508455
26.283028	1217.820864	15.513472
26.831028	1242.191235	15.518490
26.890743	1240.569373	15.523507
26.940708	1254.948547	15.528525
27.067092	1233.442155	15.533543
26.844096	1223.786216	15.538560
26.805917	1216.831613	15.543578
26.380948	1219.406864	15.548595
26.854586	1239.669284	15.553613
27.044157	1239.203351	15.558631
27.084774	1246.849791	15.563648
27.063692	1249.639060	15.568666
26.709036	1250.162857	15.573683
26.594271	1253.533367	15.578701
26.911587	1248.818702	15.583719
26.970817	1255.305986	15.588736
26.938472	1245.658951	15.593754
26.928772	1241.035773	15.598771
26.962072	1242.557928	15.603789
27.352865	1256.816676	15.608807
26.952077	1257.170077	15.613824
27.155749	1242.715914	15.618842
27.146407	1254.760705	15.623859
27.123082	1254.800641	15.628877
27.558759	1250.224404	15.633895
27.181679	1251.533583	15.638912
27.434473	1248.699566	15.643930
27.314231	1240.699378	15.648947
26.866462	1254.461076	15.653965
27.482516	1247.019862	15.658983
27.198639	1255.852229	15.664000
27.448126	1269.092168	15.669018
27.402895	1266.675346	15.674035
27.713089	1283.817794	15.679053
28.090350	1266.954320	15.684071
27.371630	1259.776324	15.689088
27.309679	1239.670088	15.694106
27.102092	1246.003292	15.699123
27.535712	1260.522632	15.704141
27.954771	1260.229312	15.709159
27.741950	1280.635882	15.714176
27.925165	1277.510930	15.719194
28.048347	1267.003785	15.724211
27.486167	1263.579289	15.729229
27.682456	1250.477547	15.734247
27.561614	1275.346338	15.739264
27.911344	1268.233886	15.744282
27.921082	1272.267246	15.749299
27.933656	1276.919938	15.754317
28.124262	1257.679474	15.759335
27.754169	1282.819270	15.764352
27.692934	1271.460625	15.769370
28.109369	1276.372953	15.774387
27.750408	1269.894211	15.779405
28.232840	1270.693493	15.784423
27.971389	1270.129604	15.789440
28.166561	1271.015602	15.794458
28.039243	1277.422535	15.799475
27.881881	1275.264274	15.804493
27.948185	1268.574558	15.809511
28.110011	1275.731339	15.814528
28.157604	1278.953261	15.819546
28.017467	1275.282122	15.824563
28.077848	1280.026292	15.829581
28.426568	1271.987471	15.834599
27.986936	1286.938702	15.839616
28.058072	1282.761949	15.844634
28.084891	1280.583749	15.849651
27.970189	1290.002645	15.854669
28.461629	1298.052271	15.859687
28.213927	1328.283479	15.864704
28.378714	1307.598282	15.869722
28.776308	1318.933269	15.874739
28.412010	1311.934678	15.879757
28.765960	1310.723639	15.884775
28.852849	1319.559833	15.889792
28.641391	1308.396582	15.894810
28.816975	1302.084258	15.899827
28.408411	1285.940710	15.904845
28.513568	1287.992539	15.909863
28.653613	1307.254314	15.914880
28.817036	1303.386885	15.919898
28.874824	1310.830842	15.924915
28.718079	1311.423751	15.929933
29.153487	1299.886771	15.934951
28.947938	1295.750997	15.939968
28.791940	1281.690793	15.944986
28.737590	1274.650651	15.950003
28.563238	1287.170106	15.955021
29.018276	1291.373127	15.960039
28.606693	1308.075434	15.965056
28.479965	1309.899978	15.970074
28.759410	1301.109258	15.975091
29.020508	1323.804603	15.980109
29.169530	1306.109157	15.985127
28.948758	1305.370462	15.990144
28.904375	1313.961743	15.995162
29.041219	1299.964930	16.000179
28.741960	1311.201838	16.005197
29.047132	1306.454485	16.010215
29.295107	1306.010696	16.015232
29.245693	1307.472117	16.020250
29.384482	1300.364978	16.025267
29.170919	1299.766709	16.030285
29.324347	1298.751250	16.035303
28.955717	1306.917606	16.040320
29.167344	1303.770813	16.045338
29.557022	1307.435268	16.050355
29.524692	1314.973825	16.055373
29.573562	1301.510150	16.060391
29.420073	1315.608796	16.065408
29.040435	1306.034415	16.070426
29.637600	1308.788012	16.075443
29.548941	1323.000596	16.080461
29.884347	1322.848035	16.085479
29.442173	1314.598698	16.090496
29.678131	1320.069946	16.095514
29.826599	1322.882525	16.100531
29.633124	1310.286495	16.105549
29.738613	1324.129908	16.110567
29.758787	1312.350825	16.115584
29.759860	1322.138248	16.120602
29.969082	1317.719233	16.125619
29.516140	1314.720904	16.130637
29.830862	1318.864514	16.135655
29.977097	1328.748342	16.140672
29.946901	1325.677867	16.145690
30.304597	1322.485751	16.150707
29.670485	1316.170425	16.155725
29.872204	1315.743452	16.160743
29.984208	1324.633846	16.165760
30.307305	1330.839975	16.170778
30.284375	1332.740777	16.175795
29.788465	1312.483425	16.180813
30.298414	1320.772362	16.185831
30.253755	1324.863178	16.190848
29.681111	1307.775197	16.195866
29.957658	1316.902043	16.200883
29.917006	1321.067726	16.205901
30.103625	1333.686955	16.210919
29.984210	1325.658273	16.215936
29.976169	1332.044634	16.220954
30.172313	1331.461244	16.225971
30.011998	1333.772503	16.230989
30.346030	1328.328394	16.236007
30.272374	1334.558477	16.241024
29.803127	1341.512341	16.246042
30.413234	1340.642698	16.251059
30.203480	1371.149521	16.256077
30.495218	1357.260086	16.261095
30.475202	1365.809757	16.266112
30.524749	1367.302592	16.271130
30.760137	1362.577363	16.276147
30.642769	1357.592211	16.281165
30.963239	1362.864375	16.286183
30.633875	1359.473511	16.291200
30.492077	1369.376563	16.296218
30.612330	1365.769266	16.301235
30.784146	1362.710610	16.306253
30.685093	1364.397036	16.311271
30.625941	1360.944199	16.316288
30.408763	1365.820757	16.321306
30.725490	1357.094846	16.326323
30.568679	1350.407643	16.331341
30.582140	1351.259705	16.336359
30.742922	1362.459460	16.341376
30.697648	1383.463956	16.346394
31.318690	1374.637587	16.351411
31.144516	1384.424688	16.356429
31.174264	1377.808394	16.361447
31.617098	1382.076312	16.366464
31.142475	1371.352969	16.371482
31.181007	1358.803266	16.376499
31.251789	1345.331337	16.381517
31.421642	1358.771253	16.386535
31.251159	1344.524531	16.391552
30.914707	1358.018456	16.396570
31.254165	1354.190579	16.401587
31.516233	1379.111737	16.406605
31.488357	1374.983783	16.411623
31.233286	1372.119055	16.416640
31.443141	1374.121165	16.421658
31.731083	1379.508637	16.426675
31.613588	1368.569458	16.431693
31.605648	1356.362231	16.436711
31.482462	1340.523898	16.441728
30.927993	1357.354445	16.446746
31.439861	1361.513816	16.451763
31.227543	1365.170476	16.456781
31.553764	1372.795027	16.461799
31.650878	1382.120423	16.466816
31.325578	1377.486187	16.471834
31.685022	1372.881171	16.476851
31.663084	1378.195366	16.481869
31.821681	1375.499047	16.486887
31.690848	1374.933198	16.491904
31.691572	1372.955780	16.496922
32.121315	1368.787876	16.501939
31.962605	1379.727134	16.506957
31.742094	1379.815825	16.511975
31.907064	1372.380424	16.516992
31.783207	1382.143767	16.522010
32.080848	1370.378587	16.527027
31.896092	1376.528877	16.532045
31.829644	1376.753448	16.537063
32.264250	1379.968725	16.542080
32.045776	1406.473567	16.547098
32.388276	1398.040830	16.552115
32.225874	1381.382848	16.557133
32.086171	1395.487237	16.562151
31.983018	1383.713608	16.567168
32.200694	1402.141988	16.572186
32.765952	1399.171588	16.577203
32.587344	1404.609884	16.582221
32.410075	1387.120541	16.587239
32.178608	1370.616735	16.592256
32.184699	1380.176876	16.597274
32.450125	1392.637293	16.602291
32.652714	1410.569428	16.607309
32.640011	1409.265846	16.612327
32.669731	1400.234890	16.617344
32.535720	1405.713265	16.622362
32.746206	1387.092394	16.627379
32.533506	1386.407464	16.632397
32.908058	1388.419489	16.637415
32.495756	1365.627105	16.642432
32.616430	1393.345720	16.647450
32.937316	1394.307632	16.652467
32.730099	1392.690573	16.657485
32.793780	1409.649112	16.662503
32.863456	1399.084337	16.667520
32.794484	1404.361998	16.672538
33.087944	1402.622611	16.677555
33.293464	1408.738985	16.682573
32.601216	1385.995938	16.687591
32.729785	1378.396448	16.692608
32.505415	1400.310449	16.697626
32.804789	1394.527342	16.702643
32.968751	1410.749425	16.707661
32.964805	1393.720082	16.712679
32.791670	1410.533916	16.717696
32.439179	1405.296803	16.722714
33.098151	1412.772348	16.727731
33.258401	1428.471211	16.732749
33.156289	1434.789247	16.737767
33.365798	1418.880463	16.742784
33.288591	1424.341921	16.747802
33.445158	1419.807001	16.752819
33.643663	1425.488761	16.757837
33.121656	1428.770100	16.762855
33.616848	1422.559339	16.767872
33.155025	1431.769413	16.772890
33.618508	1414.594707	16.777907
33.751937	1424.219513	16.782925
33.744179	1424.030446	16.787943
33.664994	1422.654093	16.792960
33.454823	1429.198579	16.797978
33.664837	1429.736145	16.802995
34.141382	1438.258573	16.808013
33.836804	1416.968513	16.813031
33.418697	1415.259241	16.818048
33.560487	1423.279758	16.823066
33.512460	1426.325049	16.828083
33.424314	1427.463888	16.833101
33.396402	1422.159272	16.838119
33.801337	1426.084026	16.843136
33.350698	1431.869320	16.848154
33.352490	1434.420589	16.853171
33.961570	1449.884293	16.858189
34.037767	1461.401217	16.863207
34.249046	1456.335300	16.868224
34.084551	1460.055145	16.873242
34.335411	1457.713768	16.878259
34.354191	1465.256836	16.883277
34.010877	1465.778044	16.888295
34.667415	1458.513532	16.893312
34.213538	1444.613940	16.898330
33.890920	1445.741411	16.903347
33.924000	1450.057397	16.908365
33.930819	1451.138619	16.913383
34.045526	1452.251399	16.918400
34.126012	1460.958135	16.923418
34.110456	1452.914391	16.928435
34.279789	1448.707771	16.933453
33.965094	1462.415406	16.938471
34.440967	1467.039886	16.943488
34.881400	1472.503749	16.948506
34.975703	1476.259402	16.953523
34.981226	1460.863680	16.958541
34.618979	1460.564404	16.963559
34.867288	1449.795704	16.968576
34.573858	1454.638834	16.973594
34.791483	1451.022279	16.978611
34.901851	1446.416065	16.983629
34.491588	1446.339958	16.988647
34.954525	1445.981436	16.993664
35.015971	1451.576524	16.998682
35.014555	1454.070104	17.003699
34.932851	1445.445439	17.008717
34.815726	1449.922239	17.013735
35.337177	1448.188958	17.018752
34.980462	1450.570886	17.023770
35.083280	1448.800550	17.028787
35.056244	1445.856964	17.033805
34.708449	1460.540460	17.038823
35.376149	1454.808701	17.043840
35.112213	1475.200099	17.048858
35.062381	1466.227409	17.053875
35.170174	1467.982320	17.058893
34.757660	1475.003492	17.063911
35.146476	1465.247454	17.068928
35.363613	1472.206741	17.073946
35.378422	1478.392101	17.078963
35.449834	1463.969039	17.083981
35.266528	1475.290615	17.088999
35.620195	1464.702522	17.094016
35.784495	1475.500670	17.099034
35.502807	1472.383755	17.104051
35.929483	1472.880475	17.109069
35.679374	1478.466273	17.114087
35.638781	1467.789256	17.119104
35.705074	1464.811118	17.124122
35.590670	1473.768388	17.129139
35.739441	1463.839057	17.134157
35.327435	1476.233764	17.139175
35.428207	1462.811214	17.144192
35.799915	1476.521862	17.149210
35.507563	1472.351902	17.154227
35.805640	1472.232038	17.159245
36.030234	1493.710407	17.164263
36.078883	1496.566469	17.169280
36.479118	1495.331518	17.174298
36.312818	1483.342143	17.179315
35.975942	1463.037191	17.184333
35.651591	1472.929316	17.189351
36.251269	1487.903761	17.194368
36.210958	1490.320965	17.199386
36.182563	1488.206598	17.204403
36.284981	1488.272886	17.209421
36.045145	1495.503275	17.214439
36.535704	1497.556591	17.219456
36.215403	1503.768666	17.224474
36.419991	1502.698629	17.229491
36.564486	1494.332024	17.234509
36.028856	1510.861644	17.239527
35.981722	1494.114360	17.244544
36.560655	1502.412064	17.249562
36.281275	1506.859701	17.254579
36.371278	1501.150846	17.259597
36.459914	1509.804399	17.264615
36.285346	1500.509438	17.269632
36.173954	1504.902753	17.274650
36.582771	1511.562493	17.279667
36.733660	1515.636332	17.284685
36.940524	1527.100221	17.289703
36.796372	1520.892283	17.294720
37.286811	1523.132818	17.299738
36.881431	1534.086364	17.304755
36.950769	1525.266097	17.309773
36.782268	1526.445288	17.314791
36.915291	1526.855919	17.319808
37.191368	1537.946970	17.324826
37.310889	1528.081251	17.329843
37.413623	1521.522467	17.334861
37.204499	1511.720973	17.339879
37.130289	1488.051754	17.344896
37.362854	1493.767436	17.349914
36.979850	1488.028629	17.354931
37.225672	1485.952327	17.359949
37.374940	1493.712920	17.364967
37.389183	1489.692264	17.369984
37.181167	1497.880301	17.375002
37.527681	1489.531818	17.380019
37.690232	1500.524539	17.385037
37.330401	1485.489878	17.390055
37.358248	1495.278653	17.395072
37.719413	1501.613283	17.400090
37.318354	1509.706269	17.405107
37.389803	1506.293918	17.410125
37.481219	1519.342998	17.415143
37.646079	1512.084516	17.420160
37.768399	1513.960602	17.425178
37.571932	1519.401002	17.430195
37.663761	1518.301756	17.435213
37.540763	1525.526110	17.440231
37.403664	1523.383456	17.445248
37.419892	1521.272192	17.450266
37.518766	1515.644502	17.455283
37.623949	1526.275146	17.460301
37.754328	1546.674544	17.465319
37.802119	1550.832478	17.470336
38.024196	1554.001464	17.475354
37.481055	1561.002610	17.480371
37.717261	1556.285840	17.485389
37.928344	1560.130647	17.490407
37.812896	1553.457990	17.495424
38.240399	1561.317394	17.500442
38.182922	1582.367383	17.505459
38.414304	1573.897997	17.510477
38.500506	1593.619427	17.515495
38.638989	1582.071378	17.520512
38.740103	1577.969200	17.525530
38.309585	1564.306449	17.530547
38.380768	1547.774622	17.535565
38.949179	1573.259971	17.540583
38.420883	1565.140633	17.545600
38.578302	1550.718712	17.550618
38.462269	1564.600044	17.555635
38.866894	1556.723618	17.560653
38.520570	1575.310599	17.565671
38.789273	1582.826454	17.570688
39.104311	1575.459828	17.575706
38.757282	1574.215057	17.580723
38.608208	1563.167506	17.585741
38.927713	1573.620066	17.590759
38.754109	1593.592153	17.595776
39.090691	1578.169462	17.600794
39.000436	1582.497293	17.605811
39.134637	1577.438908	17.610829
39.242231	1584.418080	17.615847
38.968506	1583.976476	17.620864
39.068068	1582.226307	17.625882
38.874536	1583.217579	17.630899
38.889062	1586.144384	17.635917
39.226645	1579.042372	17.640935
38.984374	1578.888345	17.645952
39.291195	1565.532729	17.650970
38.964505	1583.873547	17.655987
39.415821	1582.706737	17.661005
39.283110	1591.121925	17.666023
39.152535	1572.944551	17.671040
39.518279	1579.723668	17.676058
39.218214	1581.081941	17.681075
39.404435	1568.507716	17.686093
39.782430	1587.461343	17.691111
39.737890	1587.680063	17.696128
39.628271	1580.777580	17.701146
39.577882	1578.794128	17.706163
39.849357	1588.259382	17.711181
39.923570	1595.412204	17.716199
40.028766	1592.504130	17.721216
40.158653	1571.854012	17.726234
39.962065	1579.931729	17.731251
39.924407	1568.493583	17.736269
40.116197	1568.381232	17.741287
40.001907	1566.098075	17.746304
40.047577	1573.469378	17.751322
39.990936	1569.894962	17.756339
40.063282	1574.959017	17.761357
39.760376	1574.472515	17.766375
39.876452	1587.041865	17.771392
40.304849	1589.869629	17.776410
40.247117	1597.782060	17.781427
40.195460	1608.783070	17.786445
40.324056	1595.006735	17.791463
40.207794	1614.150127	17.796480
40.302548	1597.557853	17.801498
40.153625	1610.866366	17.806515
39.951378	1606.619072	17.811533
40.232197	1606.847252	17.816551
40.232476	1596.937581	17.821568
40.324768	1613.580324	17.826586
40.438405	1620.010328	17.831603
40.800961	1629.168489	17.836621
40.849342	1618.909770	17.841639
40.785846	1634.325990	17.846656
40.620886	1622.757088	17.851674
41.006405	1621.710885	17.856691
41.074124	1620.263105	17.861709
41.029550	1611.927373	17.866727
40.945534	1614.175382	17.871744
41.135478	1618.093578	17.876762
41.252464	1610.845041	17.881779
41.116014	1617.546961	17.886797
41.120847	1606.885406	17.891815
40.845096	1626.718881	17.896832
41.215837	1611.183738	17.901850
40.744803	1620.785524	17.906867
40.961302	1611.515428	17.911885
41.084939	1620.006156	17.916903
41.026937	1624.637967	17.921920
41.235617	1606.315205	17.926938
41.068645	1615.004869	17.931955
41.011395	1623.415906	17.936973
41.275186	1629.776347	17.941991
41.314641	1642.877873	17.947008
41.746456	1649.140736	17.952026
41.646059	1643.015433	17.957043
41.522775	1646.979660	17.962061
41.617581	1649.979408	17.967079
41.403484	1652.618632	17.972096
41.609170	1649.897449	17.977114
41.435769	1658.492206	17.982131
41.563038	1646.728807	17.987149
41.597537	1645.210813	17.992167
41.644710	1649.077066	17.997184
41.802868	1642.146004	18.002202
42.021670	1653.976194	18.007219
42.088286	1666.494511	18.012237
42.106352	1667.746995	18.017255
42.053722	1678.991257	18.022272
42.488523	1663.522924	18.027290
42.070796	1657.507215	18.032307
42.288980	1660.439309	18.037325
42.147985	1655.585243	18.042343
42.126581	1665.005232	18.047360
42.524082	1663.022698	18.052378
42.231395	1671.630980	18.057395
42.252694	1675.361361	18.062413
42.401187	1664.634379	18.067431
42.407915	1667.083437	18.072448
42.519331	1674.423069	18.077466
42.343274	1672.288179	18.082483
42.316572	1676.212627	18.087501
42.465855	1674.124168	18.092519
42.568823	1679.509792	18.097536
42.766798	1668.804804	18.102554
42.383336	1674.800498	18.107571
42.493566	1666.725563	18.112589
42.782066	1673.763233	18.117607
42.984902	1704.868798	18.122624
42.922613	1701.243339	18.127642
43.243596	1700.865765	18.132659
43.314439	1698.376088	18.137677
43.523527	1681.898410	18.142695
43.159787	1671.531554	18.147712
42.745766	1669.734291	18.152730
42.964034	1670.081779	18.157747
42.914052	1693.296885	18.162765
43.284375	1690.696522	18.167783
43.116263	1703.568499	18.172800
43.308058	1707.145062	18.177818
43.391991	1699.573762	18.182835
43.150847	1701.389858	18.187853
43.594006	1697.850536	18.192871
43.759546	1704.325786	18.197888
43.630432	1692.532450	18.202906
43.535748	1699.878222	18.207923
43.636943	1693.200052	18.212941
43.689112	1690.726725	18.217959
43.761728	1692.926955	18.222976
43.738486	1691.609297	18.227994
43.723720	1692.200813	18.233011
43.663086	1702.049459	18.238029
43.657122	1696.682251	18.243047
43.801104	1702.626871	18.248064
43.782172	1700.925476	18.253082
43.901959	1695.583045	18.258099
43.809300	1707.237212	18.263117
43.856359	1700.212939	18.268135
43.348724	1693.952780	18.273152
43.978115	1715.595804	18.278170
44.519575	1706.959692	18.283187
44.144517	1730.949542	18.288205
44.493429	1722.683919	18.293223
44.313043	1724.644492	18.298240
44.124255	1728.272319	18.303258
44.070364	1727.903406	18.308275
44.224622	1734.261699	18.313293
44.408255	1717.013289	18.318311
44.552502	1731.164743	18.323328
44.618757	1723.333542	18.328346
44.807552	1721.623397	18.333363
44.275705	1728.683384	18.338381
44.182267	1716.928386	18.343399
44.192770	1723.492867	18.348416
44.842709	1732.450309	18.353434
45.278980	1739.354328	18.358451
44.796560	1729.304461	18.363469
44.937979	1718.234845	18.368487
44.848489	1723.856470	18.373504
44.698785	1723.587786	18.378522
44.782988	1734.051246	18.383539
44.789292	1746.977246	18.388557
44.825157	1755.684983	18.393575
44.761907	1753.513999	18.398592
44.780187	1747.065329	18.403610
44.773669	1749.913722	18.408627
44.896036	1771.399367	18.413645
45.529691	1777.987192	18.418663
45.361611	1787.118391	18.423680
45.298271	1792.459004	18.428698
45.801990	1778.315128	18.433715
45.383142	1778.901090	18.438733
45.752274	1770.739186	18.443751
45.779593	1770.266080	18.448768
45.706705	1759.337583	18.453786
45.990216	1745.670113	18.458803
45.506302	1731.732560	18.463821
45.569386	1744.688043	18.468839
45.330440	1757.921380	18.473856
45.506831	1756.565585	18.478874
45.808670	1769.221877	18.483891
45.723509	1770.740958	18.488909
45.937349	1776.575361	18.493927
46.106860	1768.433498	18.498944
46.159408	1771.535970	18.503962
46.083537	1779.880063	18.508979
45.752325	1771.854237	18.513997
46.150730	1766.058338	18.519015
46.004332	1773.072603	18.524032
46.230828	1775.714730	18.529050
46.561905	1773.579960	18.534067
46.305844	1778.317342	18.539085
46.242071	1780.625859	18.544103
46.411939	1762.107734	18.549120
46.466968	1773.745479	18.554138
46.448872	1772.006187	18.559155
46.148964	1769.413597	18.564173
46.491687	1787.744656	18.569191
46.621434	1799.280838	18.574208
46.468395	1806.521133	18.579226
46.950030	1806.172995	18.584243
46.654439	1805.643629	18.589261
46.802435	1812.888616	18.594279
46.777799	1807.533784	18.599296
46.710773	1812.311819	18.604314
47.215218	1801.993608	18.609331
46.832792	1802.711409	18.614349
47.145422	1799.022198	18.619367
46.883241	1800.737837	18.624384
46.966386	1799.281286	18.629402
47.126879	1804.804868	18.634419
47.094716	1807.165766	18.639437
47.279234	1811.942225	18.644455
46.826522	1815.881167	18.649472
46.782965	1808.459925	18.654490
47.385220	1811.000443	18.659507
47.462450	1825.883162	18.664525
47.649647	1827.829958	18.669543
47.848908	1826.251847	18.674560
47.379100	1829.043575	18.679578
47.590504	1822.590814	18.684595
47.580317	1828.538051	18.689613
47.728140	1824.982876	18.694631
47.707124	1821.519914	18.699648
47.945685	1816.951345	18.704666
47.690603	1818.972610	18.709683
47.463478	1820.436467	18.714701
47.620050	1825.753032	18.719719
47.565038	1827.080897	18.724736
47.574358	1825.603082	18.729754
48.014494	1841.418999	18.734771
48.064462	1853.348641	18.739789
48.485559	1848.837471	18.744807
48.387389	1835.641373	18.749824
48.018275	1826.019345	18.754842
48.348864	1819.712755	18.759859
48.140536	1840.642450	18.764877
48.452810	1833.810208	18.769895
48.676843	1832.812557	18.774912
48.745336	1837.576067	18.779930
48.678776	1818.286997	18.784947
48.354850	1821.341763	18.789965
48.727470	1831.266912	18.794983
48.808403	1827.016864	18.800000
48.332038	1820.067359	18.805018
48.481650	1838.390739	18.810035
48.367521	1840.768647	18.815053
48.591942	1841.642938	18.820071
48.779561	1844.181946	18.825088
48.725745	1846.156171	18.830106
49.156749	1835.241641	18.835123
48.863700	1845.607250	18.840141
48.901706	1843.696971	18.845159
48.732199	1852.525614	18.850176
48.766331	1863.860794	18.855194
49.178083	1866.133599	18.860211
49.221106	1879.981999	18.865229
49.410803	1880.602266	18.870247
49.605361	1873.859570	18.875264
49.084979	1888.108522	18.880282
49.286398	1874.656957	18.885299
49.408733	1875.297405	18.890317
49.916763	1866.938681	18.895335
49.791693	1871.139221	18.900352
49.485623	1870.494326	18.905370
49.861204	1861.185329	18.910387
49.655145	1876.214745	18.915405
49.690859	1870.400353	18.920423
49.939684	1863.808678	18.925440
49.780494	1870.527712	18.930458
49.961233	1866.282186	18.935475
49.828859	1868.023536	18.940493
49.803124	1866.793568	18.945511
49.785586	1862.977663	18.950528
49.675383	1865.552375	18.955546
50.056059	1876.801620	18.960563
50.061184	1889.057786	18.965581
50.228792	1898.558687	18.970599
50.464138	1892.721100	18.975616
50.284037	1901.614386	18.980634
50.195787	1897.974927	18.985651
50.486813	1895.065473	18.990669
50.670842	1888.293774	18.995687
50.987146	1896.264698	19.000704
50.666104	1888.793282	19.005722
50.608183	1871.166336	19.010739
50.485950	1880.903798	19.015757
50.658246	1891.910206	19.020775
50.925630	1884.249774	19.025792
50.546436	1893.578313	19.030810
51.027247	1899.419743	19.035827
50.871392	1894.936076	19.040845
50.748302	1893.675224	19.045863
50.989944	1895.511881	19.050880
50.689265	1896.529699	19.055898
50.742504	1896.129538	19.060915
50.953472	1897.720961	19.065933
50.753352	1891.454932	19.070951
50.848599	1895.027276	19.075968
50.858788	1915.591873	19.080986
51.393858	1917.910305	19.086003
51.472525	1919.554293	19.091021
51.731372	1927.290563	19.096039
51.768059	1924.920346	19.101056
51.476814	1930.084985	19.106074
51.291888	1922.927705	19.111091
51.584011	1930.653164	19.116109
51.506535	1932.819949	19.121127
51.653548	1925.579840	19.126144
51.693600	1920.570174	19.131162
51.538714	1908.469295	19.136179
51.631566	1923.047582	19.141197
51.693656	1916.612301	19.146215
51.648425	1910.494605	19.151232
51.473376	1933.862969	19.156250
51.837175	1937.494747	19.161267
52.162661	1947.539972	19.166285
52.173153	1962.729221	19.171303
52.358058	1947.257969	19.176320
52.035361	1953.354203	19.181338
52.376595	1948.147048	19.186355
52.264212	1949.104163	19.191373
51.968786	1953.224136	19.196391
52.392131	1942.866061	19.201408
51.769544	1952.122548	19.206426
52.438796	1961.381455	19.211443
52.320744	1969.698562	19.216461
52.380465	1981.607876	19.221479
52.497877	1973.728267	19.226496
53.075765	1968.966313	19.231514
52.905730	1972.439402	19.236531
52.807641	1970.181127	19.241549
52.736764	1970.953861	19.246567
53.091759	1960.882758	19.251584
53.095517	1964.143286	19.256602
53.447926	1966.597830	19.261619
53.547966	1956.762458	19.266637
53.533871	1974.778616	19.271655
53.545943	1954.377209	19.276672
53.188800	1963.481251	19.281690
53.139695	1958.314320	19.286707
53.397509	1962.703163	19.291725
53.558885	1958.293161	19.296743
53.563132	1965.731835	19.301760
53.489462	1964.587372	19.306778
53.555569	1955.757135	19.311795
53.380232	1959.885487	19.316813
53.587991	1962.657274	19.321831
53.684998	1956.188877	19.326848
53.468561	1954.967291	19.331866
53.706652	1957.272527	19.336883
53.761991	1961.068343	19.341901
53.661888	1964.319479	19.346919
53.898709	1957.484269	19.351936
53.742328	1962.399308	19.356954
53.800320	1976.928936	19.361971
54.122527	1983.343930	19.366989
53.829203	1996.568850	19.372007
54.185343	1988.454520	19.377024
54.308084	1997.093487	19.382042
54.360837	1999.890788	19.387059
54.586655	1998.663165	19.392077
54.152996	1999.516567	19.397095
54.178689	1994.132402	19.402112
54.098810	2002.396246	19.407130
54.172474	2000.558130	19.412147
54.425444	1998.763782	19.417165
54.361267	2016.433238	19.422183
54.633548	2017.347888	19.427200
54.729971	2016.683630	19.432218
54.867524	2016.404522	19.437235
55.100369	2016.827566	19.442253
54.839911	2010.989560	19.447271
55.190869	2007.042485	19.452288
55.088120	2008.153808	19.457306
54.964522	2000.279586	19.462323
55.059409	1998.253243	19.467341
54.970337	2005.691088	19.472359
55.076613	2008.539634	19.477376
54.868911	2012.522142	19.482394
55.214024	2019.890750	19.487411
55.453883	2040.425188	19.492429
55.121042	2039.749159	19.497447
55.181311	2043.453755	19.502464
55.385619	2044.081139	19.507482
55.542498	2047.719202	19.512499
55.817402	2031.137819	19.517517
55.772444	2036.900336	19.522535
55.933708	2040.041374	19.527552
55.689203	2033.390651	19.532570
55.757480	2024.962748	19.537587
55.748535	2029.027615	19.542605
55.760333	2044.697334	19.547623
56.041182	2030.175811	19.552640
56.247859	2054.266124	19.557658
56.258933	2047.672169	19.562675
56.333653	2035.628954	19.567693
56.062636	2042.097681	19.572711
56.059942	2045.298690	19.577728
56.380081	2061.002629	19.582746
56.384044	2063.953239	19.587763
56.433394	2060.841606	19.592781
56.375511	2066.514168	19.597799
56.778797	2061.979032	19.602816
56.468845	2064.732723	19.607834
56.309640	2073.921677	19.612851
56.604711	2051.377222	19.617869
56.575464	2064.071629	19.622887
56.988419	2057.183113	19.627904
56.832799	2058.479062	19.632922
56.853291	2062.205739	19.637939
56.715344	2061.316929	19.642957
56.504531	2070.009135	19.647975
57.314823	2083.235892	19.652992
57.123063	2086.419082	19.658010
57.126972	2094.369932	19.663027
57.170533	2084.046370	19.668045
56.994218	2092.108551	19.673063
57.414200	2089.328728	19.678080
57.240055	2086.725461	19.683098
57.586445	2084.790354	19.688115
57.480911	2090.118928	19.693133
57.108733	2103.542937	19.698151
57.652190	2095.651950	19.703168
57.614364	2099.212531	19.708186
57.465185	2117.798648	19.713203
57.880492	2114.726962	19.718221
57.893251	2121.564204	19.723239
58.074833	2114.827400	19.728256
57.906040	2116.409407	19.733274
57.838461	2118.328444	19.738291
58.028775	2122.952274	19.743309
57.840128	2118.958295	19.748327
58.324639	2114.315801	19.753344
58.383927	2113.360924	19.758362
58.043556	2126.542337	19.763379
58.356465	2115.092688	19.768397
58.298958	2116.505139	19.773415
58.448359	2125.330281	19.778432
58.469620	2136.499399	19.783450
58.501347	2136.728774	19.788467
58.903828	2134.653358	19.793485
58.817565	2130.453484	19.798503
58.801413	2126.995179	19.803520
59.018250	2132.008854	19.808538
58.983854	2135.291237	19.813555
59.049254	2132.453903	19.818573
59.074931	2125.865449	19.823591
59.067592	2132.415656	19.828608
59.391133	2131.910242	19.833626
59.249456	2130.521763	19.838643
59.457188	2113.675699	19.843661
58.962178	2105.407587	19.848679
59.105175	2126.396501	19.853696
59.510399	2121.396175	19.858714
58.832368	2134.687292	19.863731
59.470278	2134.930113	19.868749
59.345238	2136.612119	19.873767
59.260323	2132.828913	19.878784
59.253181	2129.244892	19.883802
59.305143	2138.160306	19.888819
59.615267	2137.082834	19.893837
59.687643	2160.562337	19.898855
59.977414	2165.732720	19.903872
60.215416	2153.436834	19.908890
59.952708	2169.435992	19.913907
60.216570	2159.763135	19.918925
60.253897	2153.968037	19.923943
60.493085	2149.712322	19.928960
60.328685	2152.010200	19.933978
60.202877	2158.542343	19.938995
60.290847	2152.247561	19.944013
60.278358	2153.076278	19.949031
60.333373	2153.677922	19.954048
60.436084	2142.262560	19.959066
60.528230	2148.085060	19.964083
60.459455	2148.125168	19.969101
60.515532	2144.659272	19.974119
60.563337	2141.432242	19.979136
60.895514	2154.898137	19.984154
60.503700	2183.304865	19.989171
60.834967	2176.017942	19.994189
61.120758	2184.763949	19.999207
61.039838	2183.531742	20.004224
61.064328	2177.514508	20.009242
61.245100	2183.077477	20.014259
61.132902	2178.825091	20.019277
61.499017	2178.987768	20.024295
61.535691	2185.249386	20.029312
61.672226	2169.309735	20.034330
60.951516	2177.164603	20.039347
61.686371	2178.084938	20.044365
61.466983	2185.003280	20.049383
61.687720	2182.885263	20.054400
61.947726	2175.371373	20.059418
61.445298	2180.788446	20.064435
61.312100	2178.843288	20.069453
61.561358	2183.924176	20.074471
61.783932	2203.616034	20.079488
61.900677	2211.513557	20.084506
61.601911	2210.826578	20.089523
62.190762	2203.039989	20.094541
61.834789	2209.106239	20.099559
61.635340	2215.323722	20.104576
62.190104	2205.082156	20.109594
62.082259	2211.447063	20.114611
62.033768	2217.639686	20.119629
62.117991	2226.859920	20.124647
62.834159	2237.661083	20.129664
62.667517	2238.432584	20.134682
62.480662	2235.402632	20.139699
62.508469	2230.508081	20.144717
62.579202	2246.642924	20.149735
62.288940	2241.675601	20.154752
62.406421	2237.392862	20.159770
62.273422	2233.915411	20.164787
62.652554	2248.788958	20.169805
63.158965	2257.716134	20.174823
62.966695	2265.348336	20.179840
63.304288	2263.239988	20.184858
63.009621	2269.863610	20.189875
63.055637	2266.887756	20.194893
63.282017	2263.601544	20.199911
63.093886	2271.111169	20.204928
63.742262	2267.823729	20.209946
63.458838	2274.624113	20.214963
63.405706	2284.158896	20.219981
63.639057	2289.984891	20.224999
63.533186	2293.357366	20.230016
64.187995	2288.933073	20.235034
63.794858	2300.887339	20.240051
63.968000	2283.588019	20.245069
64.004242	2283.127633	20.250087
64.115425	2293.307957	20.255104
64.316156	2284.621234	20.260122
64.125281	2286.449047	20.265139
64.040345	2283.922761	20.270157
64.406142	2271.054217	20.275175
64.479645	2279.305554	20.280192
64.706223	2278.183190	20.285210
64.477722	2285.375975	20.290227
64.506658	2283.688115	20.295245
64.717091	2284.895030	20.300263
64.544742	2286.933053	20.305280
64.283890	2287.811611	20.310298
64.427744	2275.541650	20.315315
64.519541	2283.126199	20.320333
64.908511	2284.333744	20.325351
64.982024	2308.555050	20.330368
65.053832	2309.537875	20.335386
65.328422	2310.677926	20.340403
65.256164	2306.154842	20.345421
65.365101	2303.755737	20.350439
64.895251	2310.205162	20.355456
65.111637	2303.623184	20.360474
65.328769	2308.206614	20.365491
65.519010	2309.267301	20.370509
65.257616	2310.964779	20.375527
65.299674	2312.757808	20.380544
65.465132	2304.644610	20.385562
65.298457	2315.299522	20.390579
65.399163	2310.615134	20.395597
65.583375	2323.272579	20.400615
65.864368	2335.614912	20.405632
65.791221	2339.815170	20.410650
65.654745	2344.060139	20.415667
65.697018	2346.758496	20.420685
66.048870	2334.122590	20.425703
66.058109	2336.457305	20.430720
66.648586	2323.777847	20.435738
66.605240	2324.632732	20.440755
66.250168	2318.250430	20.445773
66.447187	2329.946994	20.450791
66.204190	2334.507850	20.455808
66.302092	2336.532670	20.460826
66.578439	2349.768528	20.465843
66.606922	2346.309346	20.470861
66.704587	2356.071835	20.475879
67.008117	2352.714305	20.480896
66.950953	2343.765840	20.485914
66.762241	2357.065645	20.490931
66.797051	2364.922831	20.495949
67.318119	2344.287895	20.500967
66.886753	2357.588642	20.505984
67.066224	2352.838978	20.511002
67.006846	2347.243286	20.516019
67.268333	2367.011751	20.521037
67.351730	2375.030309	20.526055
67.586237	2379.116229	20.531072
67.625983	2383.183655	20.536090
67.549950	2385.609062	20.541107
67.536075	2386.076971	20.546125
67.803341	2373.728252	20.551143
67.537999	2386.318219	20.556160
67.791259	2384.123408	20.561178
67.844798	2369.751855	20.566195
67.624804	2383.722911	20.571213
67.889353	2386.556516	20.576231
68.010582	2403.654915	20.581248
68.152443	2401.788569	20.586266
67.857918	2400.802000	20.591283
68.033606	2405.475449	20.596301
68.393491	2400.351686	20.601319
68.119981	2395.804821	20.606336
68.024704	2397.875403	20.611354
67.908745	2409.149205	20.616371
68.064012	2430.007600	20.621389
68.600349	2432.971707	20.626407
68.480179	2432.180722	20.631424
68.545723	2431.590590	20.636442
68.895780	2446.278622	20.641459
68.855051	2466.531189	20.646477
68.882199	2461.405407	20.651495
68.837031	2455.182855	20.656512
69.221028	2462.714606	20.661530
69.656177	2446.849740	20.666547
69.480469	2460.116101	20.671565
69.600989	2451.238344	20.676583
69.381528	2453.329524	20.681600
69.645387	2451.066940	20.686618
69.562359	2451.791294	20.691635
69.401563	2452.300727	20.696653
69.724492	2444.155260	20.701671
69.955329	2452.577466	20.706688
69.582778	2446.842111	20.711706
70.027687	2445.703007	20.716723
69.711715	2456.300812	20.721741
70.130462	2435.778816	20.726759
69.686662	2450.689417	20.731776
69.823354	2455.428095	20.736794
70.374971	2453.696191	20.741811
70.370188	2479.736277	20.746829
70.840842	2469.105208	20.751847
70.632215	2483.061174	20.756864
70.744388	2472.075884	20.761882
70.517851	2459.062515	20.766899
70.454413	2469.454086	20.771917
70.412803	2473.823977	20.776935
70.582595	2472.680764	20.781952
70.613168	2466.055192	20.786970
70.662913	2485.716000	20.791987
70.650249	2478.199818	20.797005
70.853552	2479.157751	20.802023
71.069597	2487.861576	20.807040
71.051909	2503.943159	20.812058
71.215518	2492.494214	20.817075
70.886722	2510.222199	20.822093
71.179659	2509.403873	20.827111
70.860505	2513.751962	20.832128
71.394939	2511.008087	20.837146
71.340389	2521.458058	20.842163
71.131478	2539.531939	20.847181
71.804193	2525.249487	20.852199
71.822451	2542.202431	20.857216
71.603208	2531.661673	20.862234
71.735636	2530.566104	20.867251
71.662298	2544.889917	20.872269
72.194790	2537.716246	20.877287
71.976198	2565.536821	20.882304
72.186752	2554.281711	20.887322
72.437548	2559.522952	20.892339
72.445862	2552.193743	20.897357
72.450873	2551.097254	20.902375
72.700994	2552.444169	20.907392
72.507441	2547.244217	20.912410
73.173931	2548.553050	20.917427
72.611770	2557.101779	20.922445
73.052975	2546.835612	20.927463
72.874106	2557.506016	20.932480
72.889328	2550.776664	20.937498
73.250199	2539.260042	20.942515
72.823895	2559.618276	20.947533
72.813189	2545.447152	20.952551
72.726917	2552.313760	20.957568
72.719436	2552.929321	20.962586
72.985055	2557.848054	20.967603
72.865242	2581.103239	20.972621
73.284584	2586.747094	20.977639
73.067970	2593.123219	20.982656
72.992496	2593.465663	20.987674
73.903047	2604.961347	20.992691
73.788089	2606.103764	20.997709
74.076189	2608.935232	21.002727
74.267091	2605.325018	21.007744
73.918499	2605.078592	21.012762
74.248288	2608.688436	21.017779
74.222819	2618.113621	21.022797
74.490736	2608.487806	21.027815
73.915314	2602.690349	21.032832
74.003606	2610.676793	21.037850
74.313928	2610.581719	21.042867
74.261691	2601.539491	21.047885
74.334914	2606.535332	21.052903
74.475495	2606.618354	21.057920
74.279354	2610.254648	21.062938
74.839970	2628.117034	21.067955
74.573042	2636.942019	21.072973
74.959269	2628.823326	21.077991
74.892211	2638.548559	21.083008
74.728499	2634.858807	21.088026
74.877404	2632.168526	21.093043
74.455142	2640.245844	21.098061
75.111243	2646.242119	21.103079
75.200544	2660.079947	21.108096
75.145011	2663.409082	21.113114
75.374339	2665.525474	21.118131
75.243574	2682.007573	21.123149
75.740906	2666.643845	21.128167
75.478480	2672.332742	21.133184
75.629127	2680.530314	21.138202
75.999561	2691.427071	21.143219
75.834269	2696.277701	21.148237
76.140233	2696.643485	21.153255
76.187837	2697.417813	21.158272
76.414219	2705.228899	21.163290
76.545029	2693.067647	21.168307
76.338165	2701.878373	21.173325
76.714920	2695.822841	21.178343
76.432484	2697.394714	21.183360
76.138609	2700.314289	21.188378
76.421505	2695.051675	21.193395
76.293269	2700.322736	21.198413
76.579390	2695.093432	21.203431
76.500558	2691.913220	21.208448
76.530163	2707.661045	21.213466
76.731137	2706.012562	21.218483
76.786360	2719.838576	21.223501
77.231543	2725.699400	21.228519
77.163585	2719.569256	21.233536
76.930723	2721.041194	21.238554
77.223137	2723.495213	21.243571
77.021648	2719.241176	21.248589
77.232057	2719.285532	21.253607
77.668520	2724.833891	21.258624
77.468783	2728.991520	21.263642
77.484841	2741.901114	21.268659
77.577750	2744.127372	21.273677
77.846509	2752.911050	21.278695
78.060106	2755.504287	21.283712
77.714724	2752.836960	21.288730
78.001415	2752.898256	21.293747
77.865933	2750.699310	21.298765
77.871333	2753.933795	21.303783
78.190544	2753.910458	21.308800
78.031490	2775.128608	21.313818
77.959649	2768.733976	21.318835
78.381499	2782.899606	21.323853
78.496522	2779.903204	21.328871
79.016666	2776.723421	21.333888
78.374428	2784.821739	21.338906
78.863784	2774.181176	21.343923
78.918140	2783.172903	21.348941
78.830210	2793.775488	21.353959
79.234993	2803.060598	21.358976
79.053292	2805.713737	21.363994
79.402548	2801.982255	21.369011
79.333781	2809.375580	21.374029
79.399225	2808.944345	21.379047
79.385787	2811.207238	21.384064
79.267133	2811.794128	21.389082
79.537736	2801.801985	21.394099
79.626603	2800.316106	21.399117
79.500461	2809.787361	21.404135
79.601735	2803.029225	21.409152
79.915939	2819.207682	21.414170
79.815312	2814.614236	21.419187
79.858226	2828.644475	21.424205
80.357932	2829.385257	21.429223
80.491097	2823.499096	21.434240
79.966069	2833.537406	21.439258
80.376945	2827.448848	21.444275
80.624352	2826.780929	21.449293
80.452838	2827.523346	21.454311
80.526030	2828.881985	21.459328
80.342562	2832.978053	21.464346
80.637226	2823.426493	21.469363
80.735084	2840.291574	21.474381
80.616537	2857.930600	21.479399
80.937637	2853.825236	21.484416
80.960315	2856.706160	21.489434
80.840492	2859.060754	21.494451
80.948063	2862.440225	21.499469
80.640915	2858.399650	21.504487
81.052885	2874.022175	21.509504
80.927575	2889.608473	21.514522
81.271034	2886.061177	21.519539
81.080252	2900.008399	21.524557
81.245921	2889.145631	21.529575
81.522275	2904.879491	21.534592
81.396326	2922.664512	21.539610
81.521811	2925.956186	21.544627
81.802772	2923.643607	21.549645
81.971883	2934.620635	21.554663
81.791086	2927.289931	21.559680
82.010054	2936.511938	21.564698
82.312813	2947.905022	21.569715
82.549126	2950.523777	21.574733
82.890754	2939.919240	21.579751
82.931548	2947.325840	21.584768
82.818633	2950.279535	21.589786
83.126163	2943.378317	21.594803
83.101570	2935.487013	21.599821
82.762580	2942.791346	21.604839
83.275099	2938.892205	21.609856
82.906970	2943.614792	21.614874
82.914662	2939.687602	21.619891
83.067918	2943.946323	21.624909
83.082100	2937.563857	21.629927
83.158197	2940.673050	21.634944
82.827716	2943.692117	21.639962
83.000593	2956.345627	21.644979
83.317937	2970.238630	21.649997
83.086447	2979.452264	21.655015
83.507282	2966.896850	21.660032
83.431406	2989.975768	21.665050
83.713612	2996.851473	21.670067
83.915293	2994.147203	21.675085
83.669894	3013.366510	21.680103
84.286080	2999.975203	21.685120
84.037787	2994.063277	21.690138
84.036203	3006.651044	21.695155
84.402984	3009.591970	21.700173
84.473203	3037.593930	21.705191
84.622336	3030.885481	21.710208
84.519433	3038.343361	21.715226
84.778320	3028.902781	21.720243
84.641622	3038.373506	21.725261
84.660209	3037.615422	21.730279
84.973267	3023.575488	21.735296
85.027800	3028.612211	21.740314
85.222740	3029.976626	21.745331
85.300966	3028.631653	21.750349
85.169729	3049.504370	21.755367
85.211582	3052.847955	21.760384
84.817421	3063.801631	21.765402
85.389727	3055.413112	21.770419
85.482258	3056.988942	21.775437
85.330727	3060.648125	21.780455
85.861043	3066.693741	21.785472
85.712551	3085.423355	21.790490
85.523139	3084.987915	21.795507
85.830152	3092.407199	21.800525
85.846388	3090.291775	21.805543
86.198021	3087.906544	21.810560
85.826481	3090.406724	21.815578
86.457940	3104.311120	21.820595
86.558086	3116.488660	21.825613
86.439728	3122.765176	21.830631
86.919886	3118.727197	21.835648
86.906191	3117.688712	21.840666
86.648446	3121.170551	21.845683
86.789350	3120.785483	21.850701
86.531574	3125.544808	21.855719
86.548481	3121.183456	21.860736
86.720272	3125.650876	21.865754
86.844305	3137.299158	21.870771
87.284330	3141.188902	21.875789
87.065541	3149.595898	21.880807
87.468770	3142.828785	21.885824
87.265145	3141.787548	21.890842
87.575045	3141.148982	21.895859
87.464498	3163.875788	21.900877
87.775226	3169.362561	21.905895
88.058647	3163.342175	21.910912
88.053157	3169.548795	21.915930
88.083720	3172.782506	21.920947
88.279265	3170.777710	21.925965
88.150934	3176.175602	21.930983
88.493880	3173.433828	21.936000
88.474757	3162.172401	21.941018
88.342186	3167.843926	21.946035
88.532578	3173.648023	21.951053
88.718282	3191.473346	21.956071
88.872794	3191.380307	21.961088
88.984495	3198.350160	21.966106
89.175747	3194.242597	21.971123
89.633866	3181.799050	21.976141
89.469406	3186.591497	21.981159
89.457873	3177.358351	21.986176
89.203442	3157.364333	21.991194
89.363265	3177.511958	21.996211
89.584417	3174.835230	22.001229
89.707232	3178.494743	22.006247
89.934186	3183.017101	22.011264
89.917028	3176.156539	22.016282
89.663672	3181.589317	22.021299
90.224826	3176.602318	22.026317
89.756093	3181.226176	22.031335
90.241801	3176.176479	22.036352
90.145184	3176.563211	22.041370
90.025542	3178.631494	22.046387
90.234381	3166.326827	22.051405
89.924542	3171.251007	22.056423
90.252240	3169.481577	22.061440
90.394177	3183.524684	22.066458
90.428250	3203.578337	22.071475
90.494150	3201.235507	22.076493
90.396649	3211.570106	22.081511
90.723601	3204.785237	22.086528
90.696112	3212.347600	22.091546
90.697362	3215.721296	22.096563
90.895135	3233.714659	22.101581
90.928021	3238.348218	22.106599
91.361795	3240.661790	22.111616
90.924093	3244.997532	22.116634
91.048115	3252.979415	22.121651
91.738821	3255.865592	22.126669
91.423440	3266.720326	22.131687
91.498504	3254.183622	22.136704
91.704960	3261.481367	22.141722
91.680508	3263.211963	22.146739
92.097440	3277.518881	22.151757
92.150212	3286.460826	22.156775
92.143283	3292.388472	22.161792
92.206209	3293.322436	22.166810
91.791410	3299.848465	22.171827
92.432004	3287.657345	22.176845
92.610706	3300.112779	22.181863
92.589706	3316.291752	22.186880
92.779777	3322.590753	22.191898
92.644586	3317.468534	22.196915
93.181657	3314.553397	22.201933
93.026122	3313.197690	22.206951
93.044575	3315.103949	22.211968
93.227595	3309.949868	22.216986
93.094906	3313.333146	22.222003
93.440489	3320.143833	22.227021
93.516761	3340.214543	22.232039
93.590593	3335.695375	22.237056
93.826548	3336.428689	22.242074
93.643584	3343.424362	22.247091
93.752991	3337.887905	22.252109
93.811131	3337.465685	22.257127
94.245086	3330.910700	22.262144
94.321069	3334.200921	22.267162
94.067702	3337.177877	22.272179
94.641470	3338.934229	22.277197
94.438196	3345.952807	22.282215
94.684539	3359.236848	22.287232
94.521358	3359.623973	22.292250
94.579228	3368.221394	22.297267
95.015585	3358.029383	22.302285
94.961726	3363.730910	22.307303
95.024387	3356.459496	22.312320
95.180585	3359.972923	22.317338
94.937543	3364.520728	22.322355
95.141840	3346.810855	22.327373
94.827400	3353.767714	22.332391
94.930743	3361.111058	22.337408
95.544044	3379.227132	22.342426
95.477950	3392.396618	22.347443
95.316878	3392.046326	22.352461
95.695819	3393.829032	22.357479
95.691412	3398.394645	22.362496
95.862394	3402.876440	22.367514
95.854165	3418.153571	22.372531
95.967469	3423.933875	22.377549
95.947689	3427.194550	22.382567
96.137989	3427.005339	22.387584
96.230144	3423.013419	22.392602
96.074570	3437.698127	22.397619
96.285989	3446.097260	22.402637
96.501356	3457.123944	22.407655
96.411675	3458.064161	22.412672
97.034288	3453.472392	22.417690
96.761605	3458.650334	22.422707
97.128196	3471.772133	22.427725
96.998918	3487.201582	22.432743
96.918111	3494.374550	22.437760
97.640619	3479.869273	22.442778
97.645449	3487.658685	22.447795
97.606920	3484.890368	22.452813
97.765302	3480.177532	22.457831
97.650979	3487.705112	22.462848
97.743761	3486.455320	22.467866
97.511199	3509.554535	22.472883
98.244258	3502.438098	22.477901
98.403944	3508.051350	22.482919
98.451397	3507.836145	22.487936
98.553995	3507.702611	22.492954
98.475290	3501.849965	22.497971
98.428784	3491.487068	22.502989
98.593208	3498.531255	22.508007
98.454329	3501.446721	22.513024
98.962772	3512.425139	22.518042
98.883193	3527.574526	22.523059
99.095286	3523.890698	22.528077
99.238961	3527.935577	22.533095
99.038850	3532.611891	22.538112
98.990077	3531.833057	22.543130
99.038409	3533.977655	22.548147
99.282619	3540.666161	22.553165
99.647709	3558.533339	22.558183
99.437393	3566.371260	22.563200
99.610945	3562.047730	22.568218
99.564350	3565.348110	22.573235
99.699075	3558.356165	22.578253
99.628425	3572.276215	22.583271
99.974496	3585.753808	22.588288
100.099569	3581.087156	22.593306
100.166808	3593.942140	22.598323
100.305662	3595.454004	22.603341
100.271441	3593.535350	22.608359
100.570310	3609.657345	22.613376
100.896698	3607.453843	22.618394
100.535420	3620.170293	22.623411
101.002977	3614.393331	22.628429
101.251658	3618.004565	22.633447
100.859450	3619.777326	22.638464
101.511878	3614.321730	22.643482
101.316289	3620.750798	22.648499
101.142772	3617.105625	22.653517
101.473152	3634.685010	22.658535
101.437051	3638.074198	22.663552
101.816841	3631.218564	22.668570
101.571937	3647.179516	22.673587
101.992263	3644.093350	22.678605
102.009592	3639.094587	22.683623
102.316228	3647.144325	22.688640
102.411085	3642.754655	22.693658
102.036627	3644.685852	22.698675
102.352026	3665.286840	22.703693
102.532060	3681.895924	22.708711
102.638591	3683.188755	22.713728
102.902543	3674.736568	22.718746
102.590316	3688.152458	22.723763
102.649773	3680.821608	22.728781
103.061638	3681.950898	22.733799
103.038349	3689.296507	22.738816
103.458825	3694.599996	22.743834
103.257552	3697.336652	22.748851
103.425764	3699.880659	22.753869
103.219673	3706.227266	22.758887
103.221485	3705.061188	22.763904
103.760601	3694.192556	22.768922
104.183235	3723.288935	22.773939
104.412408	3719.566936	22.778957
104.506293	3708.043205	22.783975
104.271189	3693.159430	22.788992
104.455748	3706.606250	22.794010
104.504681	3722.601454	22.799027
104.740042	3724.263927	22.804045
104.841145	3720.253194	22.809063
104.510862	3719.202217	22.814080
104.750716	3722.666993	22.819098
104.608870	3723.919195	22.824115
104.655181	3727.897843	22.829133
104.937617	3711.123781	22.834151
104.397060	3732.246030	22.839168
104.884787	3740.207943	22.844186
104.835573	3748.705451	22.849203
105.061362	3756.262319	22.854221
105.117426	3758.994138	22.859239
104.931433	3781.624584	22.864256
105.758807	3782.956664	22.869274
105.499904	3785.678140	22.874291
105.803196	3795.116950	22.879309
105.862344	3812.856225	22.884327
105.768456	3810.320874	22.889344
106.122254	3808.426064	22.894362
106.087025	3815.412561	22.899379
106.077444	3824.127205	22.904397
106.086382	3845.373605	22.909415
106.372802	3852.088564	22.914432
106.790604	3835.628681	22.919450
106.708741	3849.313209	22.924467
106.641920	3863.576696	22.929485
106.927969	3870.855762	22.934503
106.971759	3883.575499	22.939520
107.327234	3874.224391	22.944538
107.001027	3881.746626	22.949555
107.384725	3896.053158	22.954573
107.611485	3908.297700	22.959591
107.614927	3910.809805	22.964608
107.958557	3903.418584	22.969626
107.905855	3908.588350	22.974643
107.964157	3912.851483	22.979661
108.129342	3910.151296	22.984679
107.894057	3921.360324	22.989696
108.299527	3929.744526	22.994714
108.209127	3932.991401	22.999731
108.136334	3930.472331	23.004749
108.389015	3941.572884	23.009767
108.418433	3966.229552	23.014784
108.890782	3955.694697	23.019802
109.120312	3963.745106	23.024819
108.675455	3964.071747	23.029837
108.897833	3960.817267	23.034855
109.314585	3984.092168	23.039872
109.460114	3977.964427	23.044890
109.899658	3979.009875	23.049907
110.195472	3971.503525	23.054925
110.303376	3971.955211	23.059943
110.201782	3979.860188	23.064960
110.307809	3980.696070	23.069978
110.631007	3958.760956	23.074995
110.304982	3975.836538	23.080013
110.161571	3983.140087	23.085031
110.195582	3976.237951	23.090048
110.337899	3976.208214	23.095066
110.208464	3986.937851	23.100083
110.402075	4001.443146	23.105101
110.721598	3999.836980	23.110119
110.361872	4016.312245	23.115136
110.738635	4022.691914	23.120154
110.752815	4033.535565	23.125171
110.589851	4047.093967	23.130189
111.212467	4037.680492	23.135207
110.904842	4050.244794	23.140224
111.305920	4066.527211	23.145242
111.376346	4065.951970	23.150259
111.524239	4080.847745	23.155277
111.948855	4066.389399	23.160295
111.625792	4090.042041	23.165312
112.036361	4093.178387	23.170330
112.112773	4099.524955	23.175347
112.579210	4096.737363	23.180365
112.825167	4094.669339	23.185383
112.816479	4109.411534	23.190400
112.984355	4097.722298	23.195418
112.693627	4095.749292	23.200435
112.746386	4097.344165	23.205453
112.884832	4095.804624	23.210471
112.724373	4106.792605	23.215488
112.937212	4116.771548	23.220506
113.234400	4123.185978	23.225523
113.354937	4127.871136	23.230541
113.555149	4116.391493	23.235559
113.783467	4134.900301	23.240576
114.000406	4123.910446	23.245594
114.445071	4127.058670	23.250611
114.709887	4129.632189	23.255629
114.410467	4119.913347	23.260647
114.191055	4113.205746	23.265664
114.512953	4128.927370	23.270682
114.718795	4128.601152	23.275699
114.410121	4131.672045	23.280717
114.545108	4134.146692	23.285735
114.459491	4131.370028	23.290752
114.438038	4132.241980	23.295770
114.948997	4143.192941	23.300787
115.096224	4157.874923	23.305805
115.360010	4160.782165	23.310823
115.126834	4165.085556	23.315840
115.181605	4159.942977	23.320858
115.413422	4169.465801	23.325875
115.377265	4188.924681	23.330893
115.850662	4184.219604	23.335911
115.520852	4195.940310	23.340928
115.314470	4203.930558	23.345946
116.023408	4213.828101	23.350963
115.955166	4227.777494	23.355981
116.243426	4224.358262	23.360999
116.109570	4243.006772	23.366016
116.379482	4247.705912	23.371034
116.984985	4247.039050	23.376051
116.767682	4248.201058	23.381069
117.054358	4247.183825	23.386087
117.059518	4248.324520	23.391104
117.098562	4246.099877	23.396122
117.633563	4239.092559	23.401139
117.322839	4251.409719	23.406157
117.712960	4258.491447	23.411175
117.858522	4274.471057	23.416192
117.962467	4280.930530	23.421210
118.369870	4266.750862	23.426227
117.957918	4282.368607	23.431245
117.979307	4274.911369	23.436263
118.131195	4276.385826	23.441280
118.177083	4277.322571	23.446298
118.377030	4279.786884	23.451315
118.155309	4285.179619	23.456333
118.353580	4284.031730	23.461351
118.104363	4296.641209	23.466368
118.571919	4309.412533	23.471386
118.977742	4306.240437	23.476403
118.701500	4322.893110	23.481421
119.229006	4333.401816	23.486439
119.260448	4347.616275	23.491456
119.088566	4338.997986	23.496474
119.229463	4344.825389	23.501491
119.407436	4358.442996	23.506509
119.492452	4354.221463	23.511527
119.546806	4368.164027	23.516544
119.793959	4367.993277	23.521562
119.910630	4387.157427	23.526579
119.657489	4406.937550	23.531597
120.097570	4404.759859	23.536615
119.980265	4408.166893	23.541632
120.497067	4431.210998	23.546650
120.975660	4427.272833	23.551667
120.832253	4424.711442	23.556685
120.951873	4429.567556	23.561703
121.067416	4441.829492	23.566720
121.080109	4451.239541	23.571738
121.268785	4459.716047	23.576755
121.479262	4457.304337	23.581773
121.377056	4462.434202	23.586791
121.357883	4473.380260	23.591808
121.400838	4492.295904	23.596826
121.681154	4483.707696	23.601843
121.685433	4500.945197	23.606861
121.962208	4511.254855	23.611879
122.264424	4523.612965	23.616896
122.156303	4530.323492	23.621914
122.490305	4531.426721	23.626931
122.166071	4532.212450	23.631949
122.220816	4559.097157	23.636967
122.757922	4551.392339	23.641984
122.743866	4558.275901	23.647002
123.341414	4559.866561	23.652019
123.287012	4582.365540	23.657037
123.490241	4590.940500	23.662055
123.891763	4591.847305	23.667072
123.529669	4579.873229	23.672090
123.891713	4577.858219	23.677107
123.730340	4584.061971	23.682125
123.941398	4582.005738	23.687143
123.932718	4580.744500	23.692160
123.972128	4584.118718	23.697178
124.445877	4587.538540	23.702195
124.318680	4601.005996	23.707213
124.589749	4591.676550	23.712231
124.990988	4589.328020	23.717248
124.783131	4592.149279	23.722266
125.046611	4591.859492	23.727283
125.085148	4592.865872	23.732301
125.224655	4608.190699	23.737319
125.458529	4615.854502	23.742336
125.466222	4631.611032	23.747354
125.840335	4622.389436	23.752371
125.613731	4626.549518	23.757389
125.652734	4631.771785	23.762407
126.165629	4625.095869	23.767424
125.524110	4629.296936	23.772442
125.956850	4643.192800	23.777459
126.056853	4666.705742	23.782477
126.172010	4661.108083	23.787495
126.270569	4667.128029	23.792512
126.255024	4683.647493	23.797530
126.454819	4682.670834	23.802547
126.480491	4692.099422	23.807565
126.503521	4698.149518	23.812583
126.638891	4716.054739	23.817600
126.898702	4721.329154	23.822618
127.158967	4743.140183	23.827635
127.223220	4750.701295	23.832653
127.620913	4759.888090	23.837671
127.760679	4753.911210	23.842688
127.542228	4781.389796	23.847706
127.761678	4790.001621	23.852723
127.901796	4793.333868	23.857741
127.970716	4790.134360	23.862759
128.498456	4805.266106	23.867776
128.292957	4819.269412	23.872794
128.542372	4820.616660	23.877811
128.827331	4827.160798	23.882829
128.668015	4824.087361	23.887847
128.966524	4832.244470	23.892864
129.213667	4844.418100	23.897882
129.482440	4841.043532	23.902899
129.606925	4847.151463	23.907917
129.594283	4850.660704	23.912935
129.791762	4843.359193	23.917952
129.480952	4859.453903	23.922970
129.659928	4874.036345	23.927987
130.009683	4877.133785	23.933005
129.978094	4894.589879	23.938023
130.076118	4895.272107	23.943040
130.105626	4913.653105	23.948058
130.348170	4904.502664	23.953075
130.597785	4910.475809	23.958093
130.561423	4911.787601	23.963111
131.199707	4919.374492	23.968128
131.060579	4929.997004	23.973146
131.334656	4934.583201	23.978163
131.756015	4938.688829	23.983181
131.557921	4941.464540	23.988199
131.907884	4923.340123	23.993216
131.474050	4942.525902	23.998234
131.654911	4939.492606	24.003251
131.664945	4941.860652	24.008269
131.915874	4956.917898	24.013287
132.348935	4956.826855	24.018304
132.028878	4958.629171	24.023322
132.062400	4959.856659	24.028339
132.307249	4975.515164	24.033357
132.852399	4991.361034	24.038375
133.043222	4990.459739	24.043392
132.767385	4991.691713	24.048410
132.997660	4999.908572	24.053427
133.066995	5014.536958	24.058445
133.241823	5018.187853	24.063463
133.765018	5016.864585	24.068480
133.429404	5018.857417	24.073498
133.566061	5031.133785	24.078515
133.888579	5053.371981	24.083533
133.878207	5052.211673	24.088551
134.072902	5058.979577	24.093568
134.071990	5064.400324	24.098586
134.213802	5066.406724	24.103603
134.269348	5074.864690	24.108621
134.170960	5077.884936	24.113639
134.705329	5086.703983	24.118656
134.711548	5109.616574	24.123674
134.617690	5109.464003	24.128691
135.106297	5118.727002	24.133709
135.264276	5128.225246	24.138727
135.545598	5129.230715	24.143744
135.660087	5134.499342	24.148762
135.415626	5134.934085	24.153779
135.565531	5166.508604	24.158797
135.652033	5171.123209	24.163815
136.087928	5163.067598	24.168832
136.213099	5182.908806	24.173850
136.756523	5202.624346	24.178867
136.749490	5197.636021	24.183885
136.671685	5200.225025	24.188903
137.043269	5188.731388	24.193920
137.072961	5200.685870	24.198938
136.912291	5193.497152	24.203955
137.231344	5208.694846	24.208973
137.004783	5233.675315	24.213991
137.824446	5223.623104	24.219008
137.775269	5222.204626	24.224026
137.784004	5226.542129	24.229043
138.037638	5222.755279	24.234061
138.330818	5236.559882	24.239079
138.738958	5238.582060	24.244096
138.538070	5239.424468	24.249114
138.674371	5237.484703	24.254131
138.651530	5244.144192	24.259149
138.765838	5249.691395	24.264167
138.857185	5242.047071	24.269184
138.881723	5254.428831	24.274202
138.791594	5248.622154	24.279219
139.250714	5264.446633	24.284237
139.266435	5281.574651	24.289255
139.135174	5276.574637	24.294272
139.216476	5286.610753	24.299290
139.350882	5298.616277	24.304307
139.692928	5309.743742	24.309325
139.406117	5312.817682	24.314343
140.028952	5322.962589	24.319360
140.103794	5339.096245	24.324378
140.198911	5347.886357	24.329395
140.246363	5355.077541	24.334413
140.285218	5381.447028	24.339431
140.733340	5379.494504	24.344448
140.509461	5394.251052	24.349466
140.837608	5404.295880	24.354483
141.069540	5406.332803	24.359501
141.169620	5417.447792	24.364519
141.536825	5426.141855	24.369536
141.849781	5441.982750	24.374554
141.850011	5439.523372	24.379571
141.964917	5445.398628	24.384589
142.142794	5448.138088	24.389607
142.222166	5459.871649	24.394624
142.452476	5466.830751	24.399642
142.267000	5462.766897	24.404659
142.952070	5478.294379	24.409677
142.730429	5501.959066	24.414695
143.093233	5487.800294	24.419712
143.227612	5504.773543	24.424730
143.318247	5494.521117	24.429747
143.444017	5498.703145	24.434765
143.673320	5523.185783	24.439783
143.972083	5527.320567	24.444800
143.877367	5527.227921	24.449818
143.869458	5534.638870	24.454835
144.245831	5517.149936	24.459853
144.039207	5538.973645	24.464871
144.128361	5551.881130	24.469888
144.131031	5555.567477	24.474906
144.251708	5561.315192	24.479923
144.500501	5574.724370	24.484941
144.348875	5583.347047	24.489959
145.248206	5597.836592	24.494976
145.000138	5624.625183	24.499994
144.985070	5624.426999	24.505011
145.483855	5618.328801	24.510029
145.168957	5639.332810	24.515047
145.615502	5654.559416	24.520064
145.660491	5663.024122	24.525082
145.814069	5661.987897	24.530099
146.265243	5672.663945	24.535117
146.397645	5684.027318	24.540135
146.696606	5681.720106	24.545152
146.644841	5685.446635	24.550170
146.502169	5689.112130	24.555187
146.796555	5699.888727	24.560205
146.896517	5716.110053	24.565223
147.456501	5715.726554	24.570240
147.207776	5710.284077	24.575258
147.423453	5732.045458	24.580275
147.882834	5733.987155	24.585293
147.776366	5752.927451	24.590311
148.072032	5744.542989	24.595328
148.146147	5748.251823	24.600346
148.239716	5759.398004	24.605363
148.373632	5766.008344	24.610381
148.366382	5779.802350	24.615399
148.508668	5774.963111	24.620416
148.833971	5784.426446	24.625434
149.128702	5797.149522	24.630451
149.335496	5797.923811	24.635469
149.178904	5806.680374	24.640487
149.496740	5796.700714	24.645504
149.555874	5809.575446	24.650522
149.970609	5826.266760	24.655539
150.441835	5820.118588	24.660557
150.450074	5830.129744	24.665575
150.548749	5824.928447	24.670592
150.613018	5820.180309	24.675610
150.444468	5827.366824	24.680627
150.729399	5822.952498	24.685645
150.796880	5836.714973	24.690663
151.232264	5854.116627	24.695680
151.159321	5856.709691	24.700698
150.948266	5858.161141	24.705715
151.180219	5858.963680	24.710733
151.292505	5879.896770	24.715751
151.465868	5895.647902	24.720768
151.762116	5895.006690	24.725786
151.747474	5897.853248	24.730803
152.182575	5910.768044	24.735821
152.158178	5922.242359	24.740839
152.213663	5922.191850	24.745856
152.628135	5935.603265	24.750874
152.503447	5948.922058	24.755891
152.629206	5946.982309	24.760909
152.636534	5953.453987	24.765927
153.037236	5975.426980	24.770944
153.095248	5982.620719	24.775962
153.299594	5985.883989	24.780979
153.040960	5991.747424	24.785997
153.430944	6006.583730	24.791015
153.767010	6012.062819	24.796032
153.785755	6018.462682	24.801050
153.569051	6029.698662	24.806067
154.048260	6033.622287	24.811085
154.273000	6049.052252	24.816103
154.250240	6066.660169	24.821120
154.789841	6078.750425	24.826138
154.578371	6077.131934	24.831155
155.106125	6094.870049	24.836173
155.119827	6097.836438	24.841191
155.306727	6105.388918	24.846208
155.505121	6104.140954	24.851226
155.210227	6140.328218	24.856243
155.820776	6137.212009	24.861261
155.640323	6147.656299	24.866279
155.972331	6155.601879	24.871296
156.407107	6160.417759	24.876314
156.175128	6175.102415	24.881331
156.485450	6172.842099	24.886349
156.629660	6199.553446	24.891367
156.650676	6212.355926	24.896384
156.884099	6203.563346	24.901402
157.149634	6223.636917	24.906419
157.791719	6220.741473	24.911437
158.075765	6225.076287	24.916455
157.964637	6226.455190	24.921472
158.453758	6225.228527	24.926490
158.570240	6225.047913	24.931507
158.683902	6216.836188	24.936525
158.604602	6220.439781	24.941543
158.574560	6228.163028	24.946560
159.042494	6244.275122	24.951578
158.725025	6254.362099	24.956595
158.966234	6247.313357	24.961613
159.092243	6253.616754	24.966631
158.988398	6269.800370	24.971648
159.550564	6280.955632	24.976666
159.434440	6286.211085	24.981683
159.495052	6285.779736	24.986701
159.603108	6314.364118	24.991719
159.574605	6328.366589	24.996736
160.141395	6328.827803	25.001754
159.937819	6353.380832	25.006771
159.884740	6361.553148	25.011789
160.348089	6380.928976	25.016807
160.667091	6386.449478	25.021824
161.014098	6388.916669	25.026842
160.974714	6405.869087	25.031859
161.656361	6415.660760	25.036877
161.533661	6421.033756	25.041895
161.289645	6429.332541	25.046912
161.703985	6436.837126	25.051930
161.376991	6451.501797	25.056947
161.503355	6457.271771	25.061965
162.115671	6477.362783	25.066983
162.047728	6485.905762	25.072000
162.124565	6487.965205	25.077018
162.389170	6513.155124	25.082035
162.932982	6504.151584	25.087053
163.227429	6516.123139	25.092071
163.289882	6515.366539	25.097088
163.773520	6522.479306	25.102106
163.393760	6542.021239	25.107123
163.646575	6542.011653	25.112141
164.051849	6538.652711	25.117159
164.217427	6545.307920	25.122176
164.235544	6560.045137	25.127194
163.823895	6570.067874	25.132211
164.441972	6575.294494	25.137229
164.438977	6577.720742	25.142247
164.221579	6604.747759	25.147264
164.826338	6599.393117	25.152282
164.895474	6636.503128	25.157299
164.816744	6640.467878	25.162317
164.952180	6644.802906	25.167335
165.185387	6669.585020	25.172352
165.480089	6673.795525	25.177370
165.444530	6693.565245	25.182387
165.917330	6699.884354	25.187405
165.998881	6707.109313	25.192423
166.315771	6731.848289	25.197440
166.636623	6738.281339	25.202458
166.760017	6751.019178	25.207475
166.833113	6768.595334	25.212493
167.266886	6762.679355	25.217511
167.093427	6761.273462	25.222528
167.554255	6778.355847	25.227546
167.940963	6792.071460	25.232563
168.538395	6787.999653	25.237581
168.324598	6783.718851	25.242599
168.201565	6795.739883	25.247616
168.422442	6780.146109	25.252634
168.624465	6795.578900	25.257651
168.683293	6812.624705	25.262669
168.987226	6813.935126	25.267687
168.988176	6814.075066	25.272704
169.452234	6826.273974	25.277722
169.413262	6831.525973	25.282739
169.529065	6845.925301	25.287757
169.933571	6840.066676	25.292775
169.818491	6851.110037	25.297792
170.306484	6849.199758	25.302810
170.445144	6872.038879	25.307827
170.461238	6875.076643	25.312845
170.302150	6878.962210	25.317863
170.275351	6881.766832	25.322880
170.563396	6899.773887	25.327898
170.509032	6913.578031	25.332915
170.864956	6911.187591	25.337933
171.347977	6930.354068	25.342951
171.213515	6944.919285	25.347968
171.576143	6945.911137	25.352986
171.580660	6957.874983	25.358003
171.635214	6975.245830	25.363021
171.745030	6976.568331	25.368039
171.982313	6996.424780	25.373056
172.600151	7005.765939	25.378074
172.365553	7015.763892	25.383091
172.642001	7016.891448	25.388109
172.901756	7024.852165	25.393127
172.809959	7042.455720	25.398144
172.919550	7042.890714	25.403162
173.130635	7070.448255	25.408179
172.951766	7075.997250	25.413197
173.286934	7092.760120	25.418215
173.456039	7107.624879	25.423232
173.746795	7125.226554	25.428250
173.927322	7130.172204	25.433267
174.274948	7148.982866	25.438285
174.369970	7160.419426	25.443303
174.472796	7172.337084	25.448320
175.000933	7188.389073	25.453338
175.167646	7194.577010	25.458355
175.235304	7200.708352	25.463373
175.562456	7218.550616	25.468391
175.791126	7228.085364	25.473408
175.763934	7220.408566	25.478426
176.005772	7238.298291	25.483443
176.335743	7251.871515	25.488461
176.835843	7256.266610	25.493479
176.623648	7270.458983	25.498496
176.613634	7274.904725	25.503514
176.539927	7276.171533	25.508531
176.907887	7301.103963	25.513549
177.207319	7308.034817	25.518567
177.256611	7325.997834	25.523584
177.425298	7334.121164	25.528602
177.526725	7354.316065	25.533619
177.823123	7360.922458	25.538637
178.395484	7361.677108	25.543655
178.239540	7392.782659	25.548672
178.372781	7400.465531	25.553690
178.667337	7398.789821	25.558707
178.655983	7421.264209	25.563725
179.005505	7419.992832	25.568743
179.045893	7439.141620	25.573760
179.433791	7451.106902	25.578778
179.306296	7461.258037	25.583795
179.073734	7468.152606	25.588813
179.756697	7490.863408	25.593831
180.108914	7508.897167	25.598848
180.382143	7512.464538	25.603866
180.766610	7521.020176	25.608883
180.573263	7532.489620	25.613901
181.032844	7529.383827	25.618919
180.839306	7530.067026	25.623936
181.192748	7533.941080	25.628954
181.316996	7554.023240	25.633971
181.670105	7552.250837	25.638989
182.283360	7546.453082	25.644007
182.216963	7553.870428	25.649024
182.144216	7553.678265	25.654042
182.501046	7565.962550	25.659059
182.659154	7580.280306	25.664077
182.939660	7583.907911	25.669095
182.664786	7579.827822	25.674112
182.882204	7589.200929	25.679130
183.268852	7607.999658	25.684148
182.980486	7614.516840	25.689165
183.373990	7619.236704	25.694183
183.252182	7646.610751	25.699200
183.442920	7653.334839	25.704218
183.687713	7664.307263	25.709236
183.567330	7684.599350	25.714253
183.967553	7700.064431	25.719271
184.207972	7716.434726	25.724288
184.477325	7722.197347	25.729306
185.304923	7735.033068	25.734324
184.619386	7752.565302	25.739341
185.106615	7755.589510	25.744359
185.423021	7778.674728	25.749376
185.570239	7778.729195	25.754394
185.894589	7794.702988	25.759412
185.756546	7818.365892	25.764429
186.161890	7824.850470	25.769447
186.258938	7844.308643	25.774464
186.564473	7854.331206	25.779482
186.653807	7854.708079	25.784500
186.543839	7888.754187	25.789517
187.029805	7886.317685	25.794535
187.027495	7913.549629	25.799552
187.360863	7920.789325	25.804570
187.583989	7926.449233	25.809588
187.555009	7946.092089	25.814605
188.169110	7946.439597	25.819623
188.014964	7960.035568	25.824640
188.471708	7976.038022	25.829658
188.656155	7989.842858	25.834676
189.023021	7996.795547	25.839693
189.409422	7999.997193	25.844711
189.526322	8002.919181	25.849728
189.625268	8014.580820	25.854746
189.858563	8009.762548	25.859764
190.008287	8025.719577	25.864781
190.405790	8029.335722	25.869799
190.757966	8030.245909	25.874816
190.899558	8025.294317	25.879834
191.251552	8014.173836	25.884852
191.050802	8029.453366	25.889869
191.438439	8014.791722	25.894887
191.407302	8013.086034	25.899904
191.282561	8031.356203	25.904922
191.588364	8034.836673	25.909940
191.632825	8039.207072	25.914957
191.981267	8044.548030	25.919975
191.524764	8053.476081	25.924992
191.932402	8072.513232	25.930010
192.590278	8081.643709	25.935028
192.119398	8096.351418	25.940045
192.320279	8112.343269	25.945063
192.582594	8118.948747	25.950080
192.656069	8148.283413	25.955098
192.945255	8159.714572	25.960116
192.858414	8173.483353	25.965133
193.180359	8185.745384	25.970151
193.271110	8212.289848	25.975168
193.488780	8228.693841	25.980186
194.068293	8248.257004	25.985204
194.105686	8267.030408	25.990221
194.418570	8288.101730	25.995239
194.598106	8301.976885	26.000256
194.450193	8308.580567	26.005274
194.829461	8325.076152	26.010292
195.242485	8340.892392	26.015309
195.928305	8347.097596	26.020327
195.825811	8352.578228	26.025344
196.055452	8364.389275	26.030362
196.837583	8368.684663	26.035380
196.607242	8377.090936	26.040397
196.801164	8382.712394	26.045415
197.097971	8382.612784	26.050432
197.038224	8415.636977	26.055450
197.219593	8413.202133	26.060468
197.261992	8419.467449	26.065485
197.495611	8438.796425	26.070503
197.812079	8445.834477	26.075520
197.953374	8452.422412	26.080538
198.405378	8462.119469	26.085556
198.421065	8478.087333	26.090573
198.351297	8485.677224	26.095591
199.170313	8491.956077	26.100608
199.014387	8511.923661	26.105626
199.564751	8499.377185	26.110644
199.622533	8508.184563	26.115661
200.022344	8514.503896	26.120679
200.005282	8527.163348	26.125696
200.039860	8540.357548	26.130714
200.492924	8522.611297	26.135732
200.328884	8541.332171	26.140749
200.890833	8545.704027	26.145767
201.083912	8541.535299	26.150784
200.880802	8551.752737	26.155802
201.407910	8574.453454	26.160820
201.337172	8579.817365	26.165837
201.390278	8584.634300	26.170855
201.744190	8598.959198	26.175872
201.619251	8613.822367	26.180890
202.158698	8623.987184	26.185908
202.024391	8635.812400	26.190925
202.371110	8652.423312	26.195943
202.290635	8658.999478	26.200960
202.238391	8679.422514	26.205978
202.861905	8688.998734	26.210996
202.790166	8711.879329	26.216013
203.322033	8724.920837	26.221031
203.326035	8737.668785	26.226048
203.247472	8763.503477	26.231066
203.662243	8776.714394	26.236084
203.745751	8793.321782	26.241101
204.068159	8822.155370	26.246119
204.580979	8833.291316	26.251136
204.597726	8842.730255	26.256154
205.056049	8862.584250	26.261172
205.263723	8870.778142	26.266189
205.737484	8884.477091	26.271207
205.990319	8884.561156	26.276224
205.686453	8893.561373	26.281242
206.289627	8906.901725	26.286260
206.113677	8920.269108	26.291277
206.075903	8938.461202	26.296295
206.551201	8946.144246	26.301312
206.752069	8946.188987	26.306330
207.127145	8969.092388	26.311348
207.540868	8990.064423	26.316365
207.661087	8986.749604	26.321383
208.067878	9004.687944	26.326400
207.949264	9024.730528	26.331418
208.039384	9023.939097	26.336436
208.230635	9049.636442	26.341453
208.280085	9064.920812	26.346471
208.859496	9066.276058	26.351488
208.998241	9082.901324	26.356506
209.091033	9098.987796	26.361524
209.190708	9110.800480	26.366541
209.432434	9120.342623	26.371559
210.092349	9128.981191	26.376576
209.719065	9149.593367	26.381594
210.192876	9157.087498	26.386612
210.022706	9191.232724	26.391629
210.229461	9199.599284	26.396647
210.628570	9211.954917	26.401664
210.812258	9233.115452	26.406682
210.978666	9243.529423	26.411700
211.225305	9259.172490	26.416717
211.354412	9276.865039	26.421735
211.895089	9280.304034	26.426752
212.026072	9317.311686	26.431770
212.162899	9314.691389	26.436788
212.565550	9330.307299	26.441805
212.810166	9352.712301	26.446823
213.107859	9351.325876	26.451840
212.880047	9354.625341	26.456858
213.306504	9364.950724	26.461876
213.574791	9374.882274	26.466893
213.340176	9397.106010	26.471911
213.902002	9404.213217	26.476928
213.896524	9420.248020	26.481946
214.111590	9441.883892	26.486964
214.280026	9460.309737	26.491981
214.454146	9473.818152	26.496999
214.714937	9487.725130	26.502016
214.943569	9515.890346	26.507034
215.208776	9525.570264	26.512052
215.518597	9542.746400	26.517069
215.719207	9564.130956	26.522087
216.320296	9563.466981	26.527104
216.150702	9588.112361	26.532122
216.442724	9599.022806	26.537140
216.377290	9608.647672	26.542157
216.693067	9631.576886	26.547175
217.087696	9650.751909	26.552192
216.887913	9659.583710	26.557210
217.235288	9676.493524	26.562228
217.339736	9698.319353	26.567245
217.626158	9715.257422	26.572263
218.278816	9723.877427	26.577280
218.177432	9748.577121	26.582298
218.663232	9762.575189	26.587316
219.054133	9784.945319	26.592333
219.027125	9791.745614	26.597351
219.682391	9795.194402	26.602368
219.790007	9814.684929	26.607386
220.180903	9824.758169	26.612404
219.932758	9836.687862	26.617421
220.248274	9846.484705	26.622439
220.591033	9855.629919	26.627456
220.538810	9868.626244	26.632474
220.779291	9891.165710	26.637492
220.849553	9902.009812	26.642509
220.956843	9931.845456	26.647527
221.332616	9941.446634	26.652544
221.443282	9960.011366	26.657562
221.692483	9969.341947	26.662580
222.125371	9993.357975	26.667597
222.005231	10005.847013	26.672615
222.718605	10020.994252	26.677632
222.832240	10043.680872	26.682650
223.239096	10062.825747	26.687668
223.616016	10064.544303	26.692685
223.536075	10081.371984	26.697703
223.770901	10091.560788	26.702720
223.560310	10098.286996	26.707738
224.277289	10119.063921	26.712756
224.454128	10137.091430	26.717773
224.216848	10143.627918	26.722791
224.944458	10144.610221	26.727808
224.915386	10164.385846	26.732826
224.999996	10176.884491	26.737844
225.098406	10183.247073	26.742861
225.343957	10200.580982	26.747879
225.615820	10233.448485	26.752896
225.659642	10236.343211	26.757914
226.387557	10244.263290	26.762932
226.667008	10258.251037	26.767949
226.690666	10272.000187	26.772967
227.272694	10274.440022	26.777984
227.440514	10290.134504	26.783002
227.381858	10315.336720	26.788020
227.776159	10314.129595	26.793037
228.034379	10328.281735	26.798055
228.238417	10351.888978	26.803072
228.479137	10367.933945	26.808090
228.670253	10382.806715	26.813108
229.054017	10401.264316	26.818125
229.142616	10406.492507	26.823143
229.126508	10423.860514	26.828160
229.122832	10431.009566	26.833178
229.295966	10463.279438	26.838196
229.950091	10469.766443	26.843213
229.670250	10501.377666	26.848231
230.357945	10507.480389	26.853248
230.425158	10538.958256	26.858266
230.671832	10557.067609	26.863284
230.845838	10565.860028	26.868301
230.896550	10597.714875	26.873319
231.251640	10601.763408	26.878336
231.753051	10618.038214	26.883354
231.690678	10637.789861	26.888372
232.296910	10662.687944	26.893389
232.258441	10685.618569	26.898407
232.532792	10695.042396	26.903424
233.046261	10709.061337	26.908442
233.369305	10717.350394	26.913460
233.449258	10735.682508	26.918477
233.394706	10754.664135	26.923495
234.054203	10770.279560	26.928512
234.171060	10783.177313	26.933530
233.670245	10817.160522	26.938548
234.357360	10815.558422	26.943565
234.717102	10840.890789	26.948583
235.620206	10846.928621	26.953600
236.007941	10854.478256	26.958618
236.499065	10855.587639	26.963636
237.152374	10857.209501	26.968653
236.944554	10849.854776	26.973671
237.261103	10856.918748	26.978688
237.386273	10857.225844	26.983706
237.723471	10849.010981	26.988724
237.738985	10851.708070	26.993741
238.003571	10858.707526	26.998759
237.760322	10859.476705	27.003776
237.772259	10871.288230	27.008794
237.735926	10874.975808	27.013812
238.345597	10883.624985	27.018829
238.130008	10883.115152	27.023847
238.222254	10914.838909	27.028864
238.601253	10931.941856	27.033882
238.961295	10949.450415	27.038900
239.211752	10952.005396	27.043917
239.483918	10974.611479	27.048935
239.690273	10997.201721	27.053952
239.906967	10997.969998	27.058970
240.284320	11011.417884	27.063988
240.846088	11015.097125	27.069005
240.819303	11042.484631	27.074023
241.158683	11048.215343	27.079040
241.581149	11051.185241	27.084058
241.840704	11075.668620	27.089076
242.197975	11069.071359	27.094093
242.474431	11075.336677	27.099111
242.545681	11085.933948	27.104128
242.722117	11093.530765	27.109146
242.700145	11116.088321	27.114164
243.004493	11120.727894	27.119181
243.248365	11133.271205	27.124199
243.365396	11145.918565	27.129216
243.691901	11155.159643	27.134234
243.567785	11174.875397	27.139252
243.811017	11187.159522	27.144269
244.011360	11197.936991	27.149287
244.575396	11232.681293	27.154304
244.872395	11233.686672	27.159322
244.773362	11257.261002	27.164340
245.143143	11267.427911	27.169357
244.828956	11306.705325	27.174375
245.251713	11320.334356	27.179392
245.518405	11341.404933	27.184410
245.702552	11366.876166	27.189428
246.139748	11393.109713	27.194445
246.278284	11412.579273	27.199463
246.577829	11440.516207	27.204480
246.563129	11455.750261	27.209498
247.031353	11485.460409	27.214516
247.354327	11498.833970	27.219533
247.772933	11528.615667	27.224551
248.054727	11544.050673	27.229568
248.562200	11561.092731	27.234586
248.566470	11578.366334	27.239604
249.109346	11588.561358	27.244621
249.412325	11608.841812	27.249639
249.578261	11621.280480	27.254656
249.871169	11628.501867	27.259674
249.846885	11652.100510	27.264692
250.458330	11649.530485	27.269709
250.278340	11678.782563	27.274727
250.694566	11694.946576	27.279744
251.146954	11689.569599	27.284762
251.019936	11716.136061	27.289780
251.207175	11727.084039	27.294797
251.283307	11749.992891	27.299815
251.736672	11756.683851	27.304832
251.950155	11773.429647	27.309850
252.134908	11799.228937	27.314868
252.612585	11807.260185	27.319885
252.843495	11828.389681	27.324903
252.807976	11851.770632	27.329920
253.289150	11864.357401	27.334938
253.553118	11878.498274	27.339956
253.984773	11891.003624	27.344973
254.100632	11922.682044	27.349991
254.296397	11933.032591	27.355008
254.604680	11945.297912	27.360026
254.462314	11972.948732	27.365044
254.969403	11979.528315	27.370061
255.068867	12013.884080	27.375079
255.133246	12026.282794	27.380096
255.622281	12055.294362	27.385114
255.958222	12079.840389	27.390132
256.250381	12086.987932	27.395149
256.350458	12108.102072	27.400167
257.069902	12138.969654	27.405184
257.842062	12133.072048	27.410202
257.674138	12156.343520	27.415220
258.073289	12161.472444	27.420237
258.309922	12178.872229	27.425255
258.093507	12199.265190	27.430272
258.790658	12209.742622	27.435290
258.715618	12226.504408	27.440308
259.495447	12228.705056	27.445325
259.823785	12236.461632	27.450343
260.322277	12248.710655	27.455360
260.711063	12257.241958	27.460378
260.886166	12266.896289	27.465396
261.179726	12257.160245	27.470413
261.300809	12260.000738	27.475431
261.562332	12272.944983	27.480448
262.008153	12278.805800	27.485466
261.758329	12287.005806	27.490484
261.743184	12293.061318	27.495501
262.101538	12304.607403	27.500519
262.002257	12319.920349	27.505536
262.021850	12341.072240	27.510554
261.805103	12364.422652	27.515572
262.381970	12379.847489	27.520589
262.886412	12411.419732	27.525607
262.952008	12447.842542	27.530624
263.254237	12454.533897	27.535642
263.169962	12490.210701	27.540660
263.741467	12501.455341	27.545677
264.018742	12522.560704	27.550695
264.318863	12559.542644	27.555712
264.836022	12563.238044	27.560730
264.645801	12598.112593	27.565748
265.113443	12604.178253	27.570765
265.672448	12622.059849	27.575783
265.878082	12638.419405	27.580800
266.578161	12646.987502	27.585818
266.518987	12668.029807	27.590836
266.910525	12671.188955	27.595853
267.281148	12686.334882	27.600871
267.313271	12706.977389	27.605888
267.811381	12723.541907	27.610906
267.957515	12736.464994	27.615924
268.358700	12745.948995	27.620941
268.900130	12754.767167	27.625959
268.744894	12773.572943	27.630976
269.010422	12797.715356	27.635994
269.302136	12800.655285	27.641012
269.596399	12818.208374	27.646029
270.058553	12822.762123	27.651047
270.064553	12852.197172	27.656064
270.260298	12858.922603	27.661082
270.472191	12880.589292	27.666100
270.765982	12897.629923	27.671117
270.921564	12912.251482	27.676135
271.235272	12940.989052	27.681152
271.652972	12959.950506	27.686170
271.684283	12979.362026	27.691188
272.046916	12994.320128	27.696205
272.391902	13013.848668	27.701223
272.459646	13042.101197	27.706240
272.965874	13055.018029	27.711258
273.124273	13077.692908	27.716276
273.214283	13096.840185	27.721293
273.462776	13118.482093	27.726311
273.447580	13148.011514	27.731328
273.718933	13168.270069	27.736346
274.160473	13196.692367	27.741364
274.261571	13221.208894	27.746381
274.613891	13249.340389	27.751399
274.686946	13279.400120	27.756416
275.187748	13305.479247	27.761434
275.288142	13333.528353	27.766452
275.606764	13358.531235	27.771469
276.509145	13378.415681	27.776487
276.783905	13397.216070	27.781504
277.389987	13411.585453	27.786522
277.719616	13419.920507	27.791540
277.964838	13434.216267	27.796557
278.535382	13449.478291	27.801575
278.373812	13486.487364	27.806592
278.958233	13489.348896	27.811610
278.941714	13497.483334	27.816628
279.266554	13505.689709	27.821645
280.048740	13511.895705	27.826663
280.067774	13524.048316	27.831680
279.966514	13522.635086	27.836698
279.996015	13549.719992	27.841716
280.276343	13558.865504	27.846733
280.646730	13575.660011	27.851751
280.717393	13593.338977	27.856768
280.984365	13611.639048	27.861786
281.331134	13634.662183	27.866804
281.320831	13650.620361	27.871821
281.667202	13677.942900	27.876839
281.974648	13708.821389	27.881856
282.540222	13724.251956	27.886874
282.500674	13751.266159	27.891892
282.655867	13772.658882	27.896909
283.225951	13786.188232	27.901927
283.148662	13827.277670	27.906944
283.951877	13844.765484	27.911962
284.177885	13861.095457	27.916980
284.214095	13895.260481	27.921997
285.144883	13899.292741	27.927015
285.243865	13912.250219	27.932032
285.313543	13932.658537	27.937050
285.571406	13952.456333	27.942068
285.827118	13975.515946	27.947085
286.118369	13990.301218	27.952103
286.562388	14010.105432	27.957120
287.086381	14031.911169	27.962138
287.243538	14041.714136	27.967156
287.235129	14064.657654	27.972173
287.681727	14076.866443	27.977191
287.880731	14109.487291	27.982208
288.020414	14128.524821	27.987226
288.278784	14141.405331	27.992244
288.458112	14173.045248	27.997261
288.874357	14194.299118	28.002279
289.366016	14219.534627	28.007296
290.035358	14235.452594	28.012314
290.033558	14254.541071	28.017332
290.412559	14273.109246	28.022349
290.715150	14300.289421	28.027367
291.148685	14318.760694	28.032384
291.765754	14331.366628	28.037402
291.838282	14344.999100	28.042420
291.833301	14360.285282	28.047437
292.474351	14374.746242	28.052455
292.246443	14400.154596	28.057472
293.129562	14403.825685	28.062490
293.362482	14412.169613	28.067508
293.070949	14435.436798	28.072525
293.329979	14452.260351	28.077543
293.686359	14471.859007	28.082560
293.627220	14487.906629	28.087578
294.092900	14516.813256	28.092596
294.463548	14536.969043	28.097613
294.997605	14546.038595	28.102631
295.283545	14561.512810	28.107648
295.414538	14575.252875	28.112666
295.870304	14600.712698	28.117684
296.214070	14614.799117	28.122701
296.422137	14625.087346	28.127719
296.560735	14637.160970	28.132736
297.031826	14660.347786	28.137754
297.245946	14675.017499	28.142772
297.626373	14696.384471	28.147789
298.095710	14717.308556	28.152807
297.904011	14733.417514	28.157824
298.358357	14752.419444	28.162842
298.658324	14774.983943	28.167860
298.771756	14806.714887	28.172877
298.950457	14825.779439	28.177895
299.221549	14855.141056	28.182912
299.580923	14883.780437	28.187930
299.907537	14906.623600	28.192948
300.085371	14934.397405	28.197965
300.523153	14945.249610	28.202983
300.620949	14990.819563	28.208000
301.275779	15011.568452	28.213018
301.829100	15021.058660	28.218036
301.714853	15047.919663	28.223053
302.143538	15066.403733	28.228071
302.379973	15084.231195	28.233088
302.745764	15116.710500	28.238106
303.292142	15137.961007	28.243124
303.529285	15164.573136	28.248141
303.730408	15182.936950	28.253159
303.704674	15208.726939	28.258176
304.176200	15227.600071	28.263194
304.697070	15251.784392	28.268212
304.730408	15287.850665	28.273229
305.107432	15299.627212	28.278247
305.569493	15330.385429	28.283264
305.962371	15350.172863	28.288282
306.103493	15370.757994	28.293300
306.484852	15404.304338	28.298317
307.122437	15419.198759	28.303335
306.872539	15440.932341	28.308352
307.558229	15464.248940	28.313370
307.886117	15483.962567	28.318388
308.215386	15502.818462	28.323405
308.903490	15521.256619	28.328423
309.530560	15533.622823	28.333440
309.577805	15536.302694	28.338458
309.634506	15551.758154	28.343476
309.953078	15581.898508	28.348493
310.651944	15577.886202	28.353511
310.735419	15606.979993	28.358528
310.837947	15617.060350	28.363546
311.492484	15618.623135	28.368564
311.454812	15644.020343	28.373581
311.397822	15643.250055	28.378599
311.648938	15662.265823	28.383616
311.554112	15675.706103	28.388634
312.403307	15708.801837	28.393652
312.315381	15736.423608	28.398669
312.728015	15755.876675	28.403687
312.857192	15784.716309	28.408704
313.306072	15809.618984	28.413722
313.675015	15826.284422	28.418740
313.761236	15858.613422	28.423757
314.295596	15882.128767	28.428775
314.306337	15911.787010	28.433792
314.424533	15936.323161	28.438810
314.902645	15961.295429	28.443828
315.129581	15997.246298	28.448845
315.721254	16025.100784	28.453863
316.123582	16054.025128	28.458880
316.307512	16088.614144	28.463898
317.240905	16098.905664	28.468916
317.826003	16120.718616	28.473933
318.186002	16141.101706	28.478951
318.694198	16145.152339	28.483968
319.030322	16161.055156	28.488986
319.539823	16160.669306	28.494004
319.351508	16180.229312	28.499021
319.935494	16192.655667	28.504039
320.233494	16198.566369	28.509056
320.127992	16228.172298	28.514074
320.893390	16247.869733	28.519092
321.013557	16274.359625	28.524109
321.170375	16276.117934	28.529127
321.403771	16292.444497	28.534144
321.513495	16300.260233	28.539162
321.878809	16326.157466	28.544180
322.202264	16341.556049	28.549197
322.488354	16365.521106	28.554215
323.018418	16382.049474	28.559232
323.069080	16415.288755	28.564250
323.515809	16423.793486	28.569268
323.860753	16454.689732	28.574285
324.097205	16478.713460	28.579303
324.496370	16498.917965	28.584320
324.524052	16527.551365	28.589338
324.758541	16541.000538	28.594356
325.445353	16580.011069	28.599373
325.713310	16606.819875	28.604391
326.132924	16626.851619	28.609408
325.961790	16661.024923	28.614426
326.968136	16674.238025	28.619444
327.095943	16690.393073	28.624461
327.423482	16707.018038	28.629479
327.878642	16720.019439	28.634496
327.886455	16757.814331	28.639514
328.376722	16774.302813	28.644532
328.541612	16794.646017	28.649549
328.839138	16823.484186	28.654567
329.413353	16844.618260	28.659584
329.583407	16863.300817	28.664602
329.820095	16879.592441	28.669620
329.909410	16894.931850	28.674637
330.252807	16929.432773	28.679655
330.504527	16952.519437	28.684672
330.607157	16977.258134	28.689690
331.157531	17006.188031	28.694708
331.499067	17028.728641	28.699725
331.869698	17060.167836	28.704743
332.551186	17080.198393	28.709760
332.670309	17115.680100	28.714778
332.749183	17141.915278	28.719796
333.138922	17161.658006	28.724813
333.477909	17200.389334	28.729831
334.172176	17223.250372	28.734848
334.392526	17250.754855	28.739866
334.934551	17261.558530	28.744884
335.082882	17294.683744	28.749901
335.579086	17317.004072	28.754919
336.020465	17326.287287	28.759936
336.089033	17364.444430	28.764954
336.424569	17375.148814	28.769972
336.548320	17404.857850	28.774989
337.146302	17424.536627	28.780007
337.161713	17460.680115	28.785024
337.278805	17485.694473	28.790042
337.980194	17511.349196	28.795060
338.070206	17546.589292	28.800077
338.235932	17580.472951	28.805095
338.946201	17609.932616	28.810112
338.978355	17649.050173	28.815130
339.755309	17664.964603	28.820148
339.843346	17710.592948	28.825165
340.214947	17733.206563	28.830183
340.722986	17768.432905	28.835200
340.686796	17798.970139	28.840218
341.399430	17829.796362	28.845236
341.396593	17855.391837	28.850253
341.637048	17882.027708	28.855271
342.500467	17914.827691	28.860288
342.686929	17941.947069	28.865306
343.438749	17972.565758	28.870324
344.114330	17984.389600	28.875341
344.234484	18002.309830	28.880359
345.463265	18008.962469	28.885376
345.423705	18032.282593	28.890394
345.658047	18032.457884	28.895412
346.182688	18059.814521	28.900429
346.201467	18079.767931	28.905447
346.782033	18096.329461	28.910464
346.967828	18110.915325	28.915482
347.308668	18122.252063	28.920500
347.552380	18141.507104	28.925517
347.541427	18152.290077	28.930535
347.740427	18175.212554	28.935552
347.980431	18195.156842	28.940570
348.565077	18210.477279	28.945588
348.654531	18240.416609	28.950605
348.487472	18270.841369	28.955623
349.010917	18292.633952	28.960640
349.054482	18328.022198	28.965658
349.443950	18361.807730	28.970676
350.085348	18388.503020	28.975693
350.229308	18418.424163	28.980711
350.561004	18448.558367	28.985728
350.927576	18485.001825	28.990746
351.500224	18514.825705	28.995764
351.904891	18549.008447	29.000781
352.351962	18575.631479	29.005799
352.465777	18601.936783	29.010816
352.692356	18633.611381	29.015834
353.244720	18663.371452	29.020852
353.565265	18698.091570	29.025869
353.774539	18727.644615	29.030887
354.285520	18757.263816	29.035904
354.583806	18788.741861	29.040922
354.902879	18820.767472	29.045940
355.542243	18855.516274	29.050957
355.999924	18885.802122	29.055975
356.396103	18906.988253	29.060992
356.992708	18936.290196	29.066010
357.275116	18961.027023	29.071028
358.019049	18986.472675	29.076045
358.266862	19005.709233	29.081063
358.617198	19023.654592	29.086080
358.773087	19051.538303	29.091098
359.521607	19061.420907	29.096116
359.823238	19085.385919	29.101133
359.876451	19103.700000	29.106151
360.302456	19130.242293	29.111168
360.700824	19160.457413	29.116186
360.957002	19185.511397	29.121204
361.610295	19204.131970	29.126221
361.668475	19232.176073	29.131239
361.898557	19246.244486	29.136256
362.218898	19277.610546	29.141274
362.723690	19301.870314	29.146292
363.082462	19321.843186	29.151309
363.188025	19359.434704	29.156327
363.819650	19389.951711	29.161344
364.301368	19407.280067	29.166362
364.640132	19440.319651	29.171380
365.017066	19462.360077	29.176397
365.313574	19484.248373	29.181415
365.896209	19501.504842	29.186432
366.023426	19535.871769	29.191450
366.239383	19551.634998	29.196468
366.527327	19566.783170	29.201485
366.324720	19604.204676	29.206503
366.982654	19626.926220	29.211520
367.046635	19658.510292	29.216538
367.098115	19697.942929	29.221556
367.515147	19733.188615	29.226573
368.122086	19765.399846	29.231591
368.602516	19800.726536	29.236608
368.476685	19837.668595	29.241626
368.789332	19874.555044	29.246644
369.357246	19907.978835	29.251661
369.519971	19957.570041	29.256679
370.172525	19989.702803	29.261696
370.705100	20037.239405	29.266714
371.006894	20062.231611	29.271732
371.750568	20095.588422	29.276749
372.137723	20131.755635	29.281767
372.798751	20144.906466	29.286784
372.864674	20189.575759	29.291802
373.412785	20214.824276	29.296820
373.778469	20242.858200	29.301837
374.112179	20281.131030	29.306855
374.457441	20299.436196	29.311872
374.887301	20333.772002	29.316890
375.446475	20363.223162	29.321908
375.840733	20388.647680	29.326925
375.898011	20427.931204	29.331943
376.414284	20450.902935	29.336960
376.690024	20485.810174	29.341978
376.965086	20519.281936	29.346996
377.290399	20551.802302	29.352013
377.606685	20593.071279	29.357031
377.940133	20624.361163	29.362048
378.218435	20661.556954	29.367066
378.691426	20705.748999	29.372084
379.553923	20735.400206	29.377101
379.691122	20765.760059	29.382119
380.331433	20785.708052	29.387136
381.225990	20817.335758	29.392154
381.688089	20843.535383	29.397172
381.905244	20862.455429	29.402189
382.061227	20890.243559	29.407207
382.381778	20916.441446	29.412224
383.002488	20938.990877	29.417242
383.125699	20954.805737	29.422260
383.526820	20980.960967	29.427277
383.583375	21005.323548	29.432295
384.455255	21033.749970	29.437312
384.817591	21064.439950	29.442330
384.922654	21101.591144	29.447348
385.362138	21115.853900	29.452365
385.604471	21144.708461	29.457383
386.022076	21174.867699	29.462400
386.322677	21198.641975	29.467418
386.955604	21229.212767	29.472436
387.281096	21252.257813	29.477453
387.622400	21287.093379	29.482471
387.927548	21299.053600	29.487488
388.288604	21318.757733	29.492506
388.359523	21357.723226	29.497524
388.857589	21384.322833	29.502541
389.034594	21414.172761	29.507559
389.032065	21448.552335	29.512576
389.678378	21485.364592	29.517594
389.851607	21521.553734	29.522612
390.550712	21554.194605	29.527629
390.506420	21605.010083	29.532647
391.321413	21637.727960	29.537664
391.529350	21677.420613	29.542682
391.778627	21712.414335	29.547700
392.485378	21759.373538	29.552717
392.835102	21795.649387	29.557735
392.822658	21833.343199	29.562752
393.802989	21864.580518	29.567770
394.368859	21913.600924	29.572788
394.851329	21935.513808	29.577805
394.940814	21958.685703	29.582823
395.454041	21995.020230	29.587840
395.807894	22034.915785	29.592858
396.166146	22076.776602	29.597876
396.436477	22105.156683	29.602893
396.864320	22145.747212	29.607911
397.506322	22180.524236	29.612928
398.013145	22211.168223	29.617946
398.388759	22247.074743	29.622964
398.589146	22281.583682	29.627981
398.958276	22318.686998	29.632999
399.222445	22347.166160	29.638016
399.626936	22378.773495	29.643034
400.135972	22431.967925	29.648052
400.444088	22465.982801	29.653069
400.603625	22499.519705	29.658087
401.241170	22548.475526	29.663104
401.583980	22581.705370	29.668122
401.750470	22621.968577	29.673140
402.573050	22658.711378	29.678157
402.964026	22696.635177	29.683175
403.923761	22718.515636	29.688192
404.723133	22740.513043	29.693210
405.189394	22758.074803	29.698228
406.257102	22771.720698	29.703245
406.847396	22794.301267	29.708263
406.971371	22807.146092	29.713280
407.747957	22802.054740	29.718298
408.107036	22808.812236	29.723316
408.315132	22807.625221	29.728333
408.741915	22820.912511	29.733351
408.930903	22856.076686	29.738368
409.415466	22851.476866	29.743386
409.150350	22871.329181	29.748404
409.625426	22882.338048	29.753421
409.962033	22902.811286	29.758439
410.086504	22924.154831	29.763456
410.662648	22944.159901	29.768474
410.385319	22976.964810	29.773492
410.965968	23006.173719	29.778509
411.099792	23029.376348	29.783527
411.336787	23068.862283	29.788544
412.046273	23087.188276	29.793562
412.267708	23116.965812	29.798580
412.898800	23140.650184	29.803597
413.231473	23177.575436	29.808615
413.516557	23212.017770	29.813632
413.907237	23252.290966	29.818650
414.022796	23292.693168	29.823668
414.590749	23320.820852	29.828685
414.862970	23361.811073	29.833703
415.086385	23403.392052	29.838720
415.889221	23437.508204	29.843738
416.287963	23479.756963	29.848756
416.715937	23510.390825	29.853773
417.473178	23555.656967	29.858791
417.667123	23594.428766	29.863808
418.232888	23628.979306	29.868826
418.444181	23668.592917	29.873844
418.817722	23693.555028	29.878861
419.483882	23728.270168	29.883879
419.529037	23772.402687	29.888896
420.611579	23801.974991	29.893914
420.967010	23838.975346	29.898932
421.699208	23865.507170	29.903949
422.144596	23885.197130	29.908967
422.298056	23910.108001	29.913984
423.325796	23939.522303	29.919002
423.479984	23974.430617	29.924020
424.020591	23988.570374	29.929037
424.780431	24012.087451	29.934055
424.595085	24038.030827	29.939072
425.274712	24054.853464	29.944090
425.644474	24091.738695	29.949108
426.169812	24105.599779	29.954125
426.298616	24145.683013	29.959143
426.433436	24172.950935	29.964160
426.969316	24203.520892	29.969178
427.067419	24249.430459	29.974196
427.476940	24282.802901	29.979213
427.727743	24318.064437	29.984231
427.905633	24362.691820	29.989248
428.793138	24399.348758	29.994266
428.769900	24450.936431	29.999284
429.460626	24479.953278	30.004301
430.074842	24519.474874	30.009319
430.005960	24565.619914	30.014336
430.313520	24601.824610	30.019354
430.769537	24649.846924	30.024372
431.313054	24673.189121	30.029389
431.900278	24714.163355	30.034407
432.548634	24747.597972	30.039424
433.168380	24783.079825	30.044442
433.700604	24811.833429	30.049460
434.086325	24842.456894	30.054477
434.652969	24868.389727	30.059495
434.898748	24903.888104	30.064512
435.195832	24931.324466	30.069530
435.573035	24973.011075	30.074548
436.126436	25001.754558	30.079565
436.333299	25026.549953	30.084583
436.845333	25077.900755	30.089600
437.397748	25108.148408	30.094618
437.561540	25159.361954	30.099636
437.710983	25199.639905	30.104653
438.223935	25241.591543	30.109671
438.531068	25284.642713	30.114688
439.024474	25324.771647	30.119706
439.235508	25380.249637	30.124724
439.830144	25425.463495	30.129741
440.487154	25468.047412	30.134759
440.452637	25510.829059	30.139776
441.440987	25556.986552	30.144794
441.778316	25600.542664	30.149812
442.028908	25643.569931	30.154829
442.593762	25692.001859	30.159847
443.003657	25739.684228	30.164864
443.633178	25777.698675	30.169882
443.962195	25830.157951	30.174900
444.381959	25877.076574	30.179917
444.810433	25925.598685	30.184935
445.463305	25972.025102	30.189952
445.767997	26015.720678	30.194970
446.382929	26055.513020	30.199988
447.037450	26093.904743	30.205005
447.550760	26132.291481	30.210023
448.039123	26170.249780	30.215040
448.575196	26199.436196	30.220058
449.277805	26242.678241	30.225076
449.516686	26286.209355	30.230093
449.862094	26316.325254	30.235111
450.323451	26363.768083	30.240128
450.997913	26395.409703	30.245146
451.465970	26437.023405	30.250164
451.574720	26474.855400	30.255181
452.302138	26518.767036	30.260199
452.241535	26551.740895	30.265216
453.004391	26585.128810	30.270234
453.263092	26637.489262	30.275252
454.143045	26674.760042	30.280269
454.760019	26705.354950	30.285287
455.036695	26748.985287	30.290304
455.562243	26773.814544	30.295322
456.061925	26802.071115	30.300340
456.016991	26840.901433	30.305357
456.541279	26868.263154	30.310375
456.581106	26907.549681	30.315392
457.084728	26945.259207	30.320410
457.684201	26991.909008	30.325428
458.161769	27030.251586	30.330445
458.559420	27068.816555	30.335463
458.819248	27117.021683	30.340480
459.158689	27161.768191	30.345498
459.390195	27202.320132	30.350516
459.694174	27247.767418	30.355533
460.475112	27290.827261	30.360551
460.849567	27347.898747	30.365568
461.495161	27380.199256	30.370586
461.666430	27434.323708	30.375604
462.423733	27485.463491	30.380621
463.193080	27525.144264	30.385639
463.366560	27579.623392	30.390656
464.043305	27621.481085	30.395674
464.789917	27659.238660	30.400692
465.100718	27699.921035	30.405709
466.201056	27741.355435	30.410727
466.534835	27778.679539	30.415744
467.021525	27811.887084	30.420762
467.376713	27852.545438	30.425780
467.636667	27891.956865	30.430797
468.408149	27921.050596	30.435815
468.609869	27964.207662	30.440832
468.917210	27991.645245	30.445850
469.388368	28034.215926	30.450868
469.930555	28075.245301	30.455885
470.327321	28119.526769	30.460903
471.017386	28159.142940	30.465920
471.505740	28191.706494	30.470938
472.113727	28224.329846	30.475956
472.504888	28277.114157	30.480973
473.349789	28296.158904	30.485991
473.593272	28352.526766	30.491008
473.761860	28381.756768	30.496026
474.558995	28423.228614	30.501044
475.040299	28467.729214	30.506061
475.645931	28500.862495	30.511079
476.089227	28537.581536	30.516096
476.276792	28567.049953	30.521114
476.861130	28602.853169	30.526132
477.100237	28647.977486	30.531149
477.715412	28673.450945	30.536167
478.158400	28727.916209	30.541184
478.827511	28761.725411	30.546202
479.616582	28789.560365	30.551220
479.863914	28837.651260	30.556237
480.161884	28864.527651	30.561255
480.591554	28907.113535	30.566272
481.218822	28941.427756	30.571290
481.307648	28974.954784	30.576308
481.380681	29016.991052	30.581325
482.505464	29041.958420	30.586343
482.637781	29089.155937	30.591360
482.895807	29139.556287	30.596378
483.642250	29174.657302	30.601396
483.303157	29216.940968	30.606413
484.154754	29251.853625	30.611431
484.422568	29313.950965	30.616448
485.157012	29341.340127	30.621466
485.603698	29395.796007	30.626484
485.919163	29446.763369	30.631501
486.841970	29496.553049	30.636519
486.941982	29545.211622	30.641536
487.208141	29596.874418	30.646554
487.601838	29647.125496	30.651572
488.125077	29704.033422	30.656589
488.716599	29765.428467	30.661607
489.234978	29816.137720	30.666624
489.604943	29869.664973	30.671642
490.031338	29926.516606	30.676660
490.431623	29977.286147	30.681677
491.403407	30037.423892	30.686695
491.989785	30080.113958	30.691712
492.481795	30145.507243	30.696730
493.172512	30176.304210	30.701748
493.479152	30239.440620	30.706765
493.692535	30293.985514	30.711783
494.076875	30348.577430	30.716800
494.906974	30404.453901	30.721818
496.115007	30443.491954	30.726836
496.771616	30475.415475	30.731853
497.686471	30517.018906	30.736871
498.146118	30551.908530	30.741888
498.220493	30598.099937	30.746906
498.922488	30615.557889	30.751924
499.216171	30667.506522	30.756941
499.797530	30702.435394	30.761959
500.478369	30740.856795	30.766976
501.081823	30776.245666	30.771994
501.384270	30813.072649	30.777012
501.530344	30854.884509	30.782029
502.305395	30887.522841	30.787047
502.958810	30921.868589	30.792064
503.174056	30969.299460	30.797082
503.839529	31017.459401	30.802100
504.164556	31054.631645	30.807117
504.155563	31103.767700	30.812135
504.735382	31150.318301	30.817152
505.066973	31196.054327	30.822170
505.488331	31245.199483	30.827188
506.025116	31312.546240	30.832205
506.494832	31361.220662	30.837223
506.927347	31407.656758	30.842240
507.204923	31469.235866	30.847258
507.923206	31508.359208	30.852276
508.488553	31552.804392	30.857293
509.380143	31601.409173	30.862311
509.724882	31642.050265	30.867328
510.544421	31670.901905	30.872346
511.383364	31706.759640	30.877364
511.654872	31757.189539	30.882381
512.215641	31785.154245	30.887399
513.479368	31803.598931	30.892416
513.755049	31841.545252	30.897434
514.688426	31861.440682	30.902452
515.115539	31893.280585	30.907469
515.612782	31913.255005	30.912487
515.879922	31945.640627	30.917504
516.313586	31981.133224	30.922522
516.752855	32006.283697	30.927540
517.133269	32052.747252	30.932557
517.433059	32086.875937	30.937575
518.138452	32119.704354	30.942592
518.361518	32176.307728	30.947610
519.372142	32196.435572	30.952628
520.701522	32203.737587	30.957645
521.534530	32227.711312	30.962663
521.646496	32265.099917	30.967680
522.242913	32282.923237	30.972698
522.636412	32299.097086	30.977716
522.456395	32339.599665	30.982733
522.871005	32372.531648	30.987751
523.667478	32398.204295	30.992768
523.513657	32438.501188	30.997786
524.121930	32477.861882	31.002804
524.134646	32528.661641	31.007821
524.873333	32572.183521	31.012839
524.966306	32635.886476	31.017856
525.185832	32685.533070	31.022874
525.879670	32730.999715	31.027892
526.097522	32809.717700	31.032909
526.641328	32856.693419	31.037927
527.112880	32933.555732	31.042944
527.458108	32991.425520	31.047962
528.414384	33048.966469	31.052980
528.623004	33120.085014	31.057997
529.583967	33179.794638	31.063015
530.068304	33232.368846	31.068032
530.386415	33301.721043	31.073050
531.532768	33352.661173	31.078068
531.990786	33400.082432	31.083085
532.565771	33457.239437	31.088103
533.143959	33507.698340	31.093120
533.353795	33576.988542	31.098138
534.022218	33615.989267	31.103156
534.658765	33673.058394	31.108173
535.493298	33723.245402	31.113191
535.657597	33780.705386	31.118208
536.073184	33834.438457	31.123226
536.760028	33880.722772	31.128244
536.977817	33929.950903	31.133261
537.532122	33987.008987	31.138279
538.094968	34047.174512	31.143296
538.852394	34096.367628	31.148314
539.389344	34138.391945	31.153332
539.773020	34197.300224	31.158349
539.994739	34252.925662	31.163367
540.766583	34303.740778	31.168384
541.223009	34359.797379	31.173402
542.051303	34406.546162	31.178420
542.751718	34458.851799	31.183437
543.043686	34503.077318	31.188455
544.011323	34559.015332	31.193472
544.150271	34620.967170	31.198490
544.953589	34661.775947	31.203508
545.271129	34720.332454	31.208525
545.950943	34776.728493	31.213543
546.472996	34826.561882	31.218560
546.836829	34883.481544	31.223578
547.597078	34936.501166	31.228596
547.856405	34998.728453	31.233613
548.160376	35055.642471	31.238631
549.406352	35113.246907	31.243648
549.450231	35161.893126	31.248666
550.128123	35224.940570	31.253684
550.850578	35290.823564	31.258701
550.764231	35339.308167	31.263719
551.704321	35400.665500	31.268736
552.056175	35466.504164	31.273754
552.684321	35527.806021	31.278772
553.396865	35597.002475	31.283789
553.651197	35660.030734	31.288807
554.464310	35713.862621	31.293824
555.373972	35775.081135	31.298842
556.136676	35821.377679	31.303860
556.918511	35877.572002	31.308877
557.353598	35930.878321	31.313895
558.129859	35980.102375	31.318912
558.298006	36034.255582	31.323930
559.065659	36089.125411	31.328948
559.672656	36134.388169	31.333965
560.109678	36191.565486	31.338983
560.635676	36236.130385	31.344000
561.314548	36290.997672	31.349018
561.657978	36338.786080	31.354036
562.246407	36400.475838	31.359053
562.971907	36446.425303	31.364071
563.690547	36484.876091	31.369088
564.008636	36555.023798	31.374106
564.621352	36611.408330	31.379124
565.406017	36654.138956	31.384141
565.848992	36725.782615	31.389159
566.523751	36754.215259	31.394176
566.611633	36804.095304	31.399194
567.531594	36845.524646	31.404212
567.860989	36896.090174	31.409229
568.084723	36951.833042	31.414247
568.883021	36999.864636	31.419264
569.028227	37051.152114	31.424282
569.651014	37097.871784	31.429300
570.339025	37157.483037	31.434317
570.631850	37217.795991	31.439335
571.366143	37275.803124	31.444352
571.804866	37322.445519	31.449370
572.135119	37394.565633	31.454388
573.503798	37450.550354	31.459405
573.530170	37502.906630	31.464423
574.474761	37553.387190	31.469440
575.036164	37624.640552	31.474458
575.682003	37679.066690	31.479476
576.400565	37723.303710	31.484493
576.728335	37791.799467	31.489511
577.139204	37843.021812	31.494528
577.619712	37906.626348	31.499546
578.326205	37961.759575	31.504564
579.009018	38021.915533	31.509581
579.338614	38084.568767	31.514599
580.184947	38135.233853	31.519616
580.461605	38209.587628	31.524634
581.101669	38277.745491	31.529652
581.727870	38326.174083	31.534669
582.081041	38399.415918	31.539687
582.478048	38477.841870	31.544704
583.197154	38546.005568	31.549722
583.910983	38604.269657	31.554740
584.758188	38665.390373	31.559757
585.300622	38731.509456	31.564775
586.205282	38785.836441	31.569792
586.707318	38847.742851	31.574810
587.085394	38911.668647	31.579828
587.829272	38970.116849	31.584845
588.184104	39042.104456	31.589863
588.666609	39101.517187	31.594880
589.359129	39168.041393	31.599898
590.134144	39237.977656	31.604916
590.866844	39297.341766	31.609933
591.002086	39371.182282	31.614951
591.954709	39417.102088	31.619968
592.432410	39485.669108	31.624986
592.933169	39543.994007	31.630004
593.816563	39605.317340	31.635021
594.154929	39671.417386	31.640039
595.151482	39731.682401	31.645056
595.473591	39797.725603	31.650074
596.238503	39870.682704	31.655092
596.829211	39931.645402	31.660109
597.348219	39990.128191	31.665127
597.762385	40043.255268	31.670144
598.382075	40113.407518	31.675162
598.758460	40179.334743	31.680180
599.341271	40209.068327	31.685197
600.209048	40283.012171	31.690215
600.869172	40332.048206	31.695232
601.616322	40398.631595	31.700250
602.384408	40450.785785	31.705268
603.205959	40490.467216	31.710285
603.769606	40558.528114	31.715303
604.434740	40595.679993	31.720320
604.911965	40657.018175	31.725338
605.538143	40708.136013	31.730356
606.455304	40748.067753	31.735373
606.831084	40798.282692	31.740391
607.407739	40851.597724	31.745408
607.789187	40895.699569	31.750426
608.507077	40960.993507	31.755444
608.970260	41005.353865	31.760461
609.709011	41067.449842	31.765479
610.188383	41113.835960	31.770496
610.807787	41173.406000	31.775514
611.205905	41231.778239	31.780532
612.043101	41297.852445	31.785549
612.650106	41353.996585	31.790567
612.923472	41411.853105	31.795584
613.715497	41480.322873	31.800602
613.781654	41529.229829	31.805620
614.552133	41609.979454	31.810637
614.961472	41674.214980	31.815655
615.234435	41741.951520	31.820672
616.328182	41816.358055	31.825690
616.529961	41890.080551	31.830708
617.368658	41970.606520	31.835725
617.715318	42045.855332	31.840743
618.189416	42123.743209	31.845760
618.944784	42197.176991	31.850778
619.688350	42280.473227	31.855796
620.542741	42347.750510	31.860813
620.978170	42430.528768	31.865831
621.855638	42498.667244	31.870848
622.345158	42577.295977	31.875866
623.046085	42664.717259	31.880884
624.131303	42712.635700	31.885901
625.080298	42782.959341	31.890919
625.727796	42846.388490	31.895936
626.455864	42905.067150	31.900954
626.654233	42963.609550	31.905972
627.520203	43022.061611	31.910989
628.186989	43079.750675	31.916007
629.114073	43146.271899	31.921024
629.847036	43203.739492	31.926042
630.205320	43278.105422	31.931060
630.774892	43320.710390	31.936077
631.553948	43383.688401	31.941095
631.626475	43450.135522	31.946112
632.424972	43508.984823	31.951130
632.939155	43577.481927	31.956148
633.672280	43621.153052	31.961165
633.789298	43695.527646	31.966183
634.291318	43747.264177	31.971200
634.816938	43818.823474	31.976218
635.402590	43890.203160	31.981236
635.946876	43962.510863	31.986253
636.650204	44035.301432	31.991271
637.067350	44113.762543	31.996288
637.806007	44179.349275	32.001306
638.444305	44250.646347	32.006324
639.164293	44329.710064	32.011341
639.689134	44409.275258	32.016359
640.563558	44475.437720	32.021376
641.552055	44550.945379	32.026394
642.185189	44620.216325	32.031412
642.740949	44685.685819	32.036429
643.385454	44767.997126	32.041447
643.831898	44828.042658	32.046464
644.639024	44900.492226	32.051482
645.444829	44979.277074	32.056500
646.020486	45053.527649	32.061517
646.744079	45135.228689	32.066535
647.075503	45196.644055	32.071552
648.334528	45268.707717	32.076570
648.526947	45356.706208	32.081588
649.179829	45415.875395	32.086605
649.627886	45488.330946	32.091623
650.493170	45565.361177	32.096640
651.280732	45634.788232	32.101658
651.636825	45712.578490	32.106676
652.656706	45772.169991	32.111693
653.357255	45854.259804	32.116711
654.107242	45927.533546	32.121728
654.792674	45991.778947	32.126746
655.401311	46080.979936	32.131764
656.422237	46118.651778	32.136781
657.557078	46191.259590	32.141799
658.185958	46236.840558	32.146816
659.299511	46303.432503	32.151834
659.928516	46359.336944	32.156852
660.519675	46400.324334	32.161869
661.144172	46459.981135	32.166887
661.708204	46514.284194	32.171904
662.581704	46574.053177	32.176922
662.972597	46626.964380	32.181940
663.496501	46690.815284	32.186957
664.237143	46733.871466	32.191975
664.541163	46797.972315	32.196992
665.896339	46837.034363	32.202010
666.194127	46907.497286	32.207028
666.775063	46954.753652	32.212045
667.507743	47018.550419	32.217063
667.884991	47081.040988	32.222080
669.039433	47134.608309	32.227098
669.353209	47189.505453	32.232116
669.786287	47242.771479	32.237133
670.334571	47301.231684	32.242151
671.093526	47349.956324	32.247168
671.884356	47410.309249	32.252186
672.078204	47475.827861	32.257204
672.963129	47519.014445	32.262221
673.286643	47589.441288	32.267239
673.836088	47644.930218	32.272256
674.659890	47702.297188	32.277274
675.299919	47783.004712	32.282292
675.890226	47855.661932	32.287309
676.865707	47916.728682	32.292327
677.031212	47993.701129	32.297344
677.713649	48055.884666	32.302362
678.100970	48138.372628	32.307380
678.546177	48213.461938	32.312397
679.391210	48293.687937	32.317415
679.887076	48372.950709	32.322432
680.939118	48439.140867	32.327450
681.924211	48530.799693	32.332468
682.704224	48589.116824	32.337485
683.680651	48664.893388	32.342503
684.583702	48735.721611	32.347520
685.267003	48799.747245	32.352538
685.541928	48878.365875	32.357556
685.940498	48940.761800	32.362573
687.158858	49013.875982	32.367591
687.431992	49091.508173	32.372608
688.481654	49157.076604	32.377626
689.020277	49235.863095	32.382644
689.729572	49304.405124	32.387661
690.404137	49378.004984	32.392679
690.661925	49456.660453	32.397696
691.532453	49528.039772	32.402714
691.873438	49624.587495	32.407732
692.851865	49691.267386	32.412749
693.554161	49777.243932	32.417767
694.065918	49849.202336	32.422784
694.912063	49934.083819	32.427802
695.678046	50007.605456	32.432820
695.915329	50096.343044	32.437837
696.865280	50169.766634	32.442855
697.672666	50251.623180	32.447872
698.624633	50332.516677	32.452890
699.240894	50420.393982	32.457908
699.916689	50494.683049	32.462925
700.892463	50580.307502	32.467943
701.316814	50657.474308	32.472960
702.097274	50737.541728	32.477978
702.669744	50826.305308	32.482996
703.141791	50894.853347	32.488013
704.136178	50967.143356	32.493031
704.418329	51060.217844	32.498048
704.802543	51146.936434	32.503066
705.629775	51232.786474	32.508084
706.369588	51311.461718	32.513101
707.174290	51388.833055	32.518119
707.667512	51468.573916	32.523136
709.147122	51513.812097	32.528154
710.145108	51593.081815	32.533172
710.848801	51664.120667	32.538189
711.559085	51734.448657	32.543207
712.009110	51810.464404	32.548224
712.745208	51879.999859	32.553242
713.024895	51965.719653	32.558260
713.647710	52061.699109	32.563277
714.346520	52119.160169	32.568295
715.022282	52218.963459	32.573312
715.655562	52286.127720	32.578330
716.489879	52381.746978	32.583348
716.767875	52457.066939	32.588365
717.893903	52551.283534	32.593383
718.469158	52640.888835	32.598400
719.373508	52721.260977	32.603418
719.847467	52806.786558	32.608436
720.407991	52908.840250	32.613453
721.373831	52990.611454	32.618471
721.461696	53087.082356	32.623488
722.647040	53184.799353	32.628506
723.133143	53276.662909	32.633524
724.166591	53374.676548	32.638541
724.944852	53462.009499	32.643559
725.363501	53569.578247	32.648576
726.303741	53659.300919	32.653594
727.246678	53757.305785	32.658612
727.682505	53837.624904	32.663629
728.955443	53925.692512	32.668647
729.653275	54021.847173	32.673664
730.472853	54106.575802	32.678682
731.228628	54192.817426	32.683700
731.929872	54269.608384	32.688717
733.070273	54365.126252	32.693735
733.327468	54456.577687	32.698752
734.271210	54535.524888	32.703770
734.979972	54630.617299	32.708788
735.539598	54719.929169	32.713805
736.543337	54794.518305	32.718823
736.774292	54894.224041	32.723840
737.485578	54987.985862	32.728858
738.455478	55064.431216	32.733876
739.247731	55156.662716	32.738893
740.235580	55251.047895	32.743911
741.163086	55328.100852	32.748928
741.814630	55421.571375	32.753946
742.404340	55506.759773	32.758964
743.185900	55606.580605	32.763981
743.990390	55671.665683	32.768999
744.574007	55769.811168	32.774016
745.332281	55851.782947	32.779034
746.265897	55933.234735	32.784052
747.325669	55986.101769	32.789069
748.414674	56065.146097	32.794087
748.783260	56146.723504	32.799104
749.492247	56208.230175	32.804122
750.183231	56282.805720	32.809140
750.622375	56367.501219	32.814157
751.574438	56430.336820	32.819175
752.136207	56512.813192	32.824192
752.747230	56592.365203	32.829210
753.278301	56681.189243	32.834228
754.003046	56754.091366	32.839245
755.039967	56843.533326	32.844263
755.706852	56946.634409	32.849280
756.269538	57022.189905	32.854298
756.898881	57119.138853	32.859316
757.045773	57210.918318	32.864333
757.984354	57306.000639	32.869351
758.521265	57409.500670	32.874368
759.107385	57507.055197	32.879386
760.192314	57622.105755	32.884404
760.600273	57721.969117	32.889421
761.625779	57828.793807	32.894439
762.283907	57936.567878	32.899456
762.994456	58037.243486	32.904474
763.457756	58147.846949	32.909492
764.765119	58260.968668	32.914509
766.007765	58350.391488	32.919527
766.747923	58460.637034	32.924544
767.588492	58552.271676	32.929562
768.921438	58644.005196	32.934580
769.456065	58733.735154	32.939597
770.142360	58831.043911	32.944615
770.852437	58928.797715	32.949632
771.942324	59019.807737	32.954650
773.089895	59106.884578	32.959668
773.720732	59191.199398	32.964685
774.654938	59294.343601	32.969703
775.257380	59368.528917	32.974720
775.965888	59460.668962	32.979738
776.836841	59544.075743	32.984756
777.321708	59631.361557	32.989773
778.401021	59729.206022	32.994791
779.071578	59820.766620	32.999808
779.777950	59904.431695	33.004826
780.588942	60002.689715	33.009844
781.116054	60099.559977	33.014861
781.935068	60185.677470	33.019879
783.063022	60277.890548	33.024896
783.688117	60379.021823	33.029914
784.391176	60471.458201	33.034932
785.185703	60551.433689	33.039949
786.112958	60646.699080	33.044967
786.810571	60746.791452	33.049984
787.498556	60827.473413	33.055002
788.279214	60901.907989	33.060020
788.812394	61010.041770	33.065037
789.901219	61077.553992	33.070055
790.542869	61168.497418	33.075072
791.199296	61263.022805	33.080090
792.145387	61334.145701	33.085108
792.844770	61411.206575	33.090125
793.883900	61499.660122	33.095143
794.515862	61594.184750	33.100160
794.929001	61679.590599	33.105178
796.151850	61763.611197	33.110196
796.592949	61863.545088	33.115213
797.535462	61956.228528	33.120231
798.323300	62044.614110	33.125248
799.080754	62153.694492	33.130266
799.891362	62231.710443	33.135284
800.478781	62339.982157	33.140301
801.406327	62434.366052	33.145319
802.043697	62531.269169	33.150336
802.412326	62639.018484	33.155354
803.495194	62729.962361	33.160372
804.020441	62841.565729	33.165389
805.024659	62941.633574	33.170407
806.093654	63056.104277	33.175424
806.843112	63150.169556	33.180442
808.358107	63243.118708	33.185460
808.928130	63345.657818	33.190477
810.206216	63435.241354	33.195495
811.099515	63521.646474	33.200512
811.935502	63609.564311	33.205530
812.869091	63691.833142	33.210548
813.909626	63793.257637	33.215565
814.558358	63873.668307	33.220583
815.369967	63947.232013	33.225600
815.618682	64039.473929	33.230618
816.661624	64137.287050	33.235636
817.402191	64235.028792	33.240653
818.208555	64319.660731	33.245671
819.028804	64409.855444	33.250688
819.434493	64518.433765	33.255706
820.536291	64606.894993	33.260724
820.934884	64730.562155	33.265741
821.429932	64816.310145	33.270759
822.344110	64936.141488	33.275776
823.004888	65047.843577	33.280794
823.677103	65160.157195	33.285812
824.119255	65276.594880	33.290829
824.807005	65388.263074	33.295847
826.133594	65510.979048	33.300864
826.705107	65628.712132	33.305882
827.990377	65739.851422	33.310900
828.871342	65853.803475	33.315917
829.698754	65976.548176	33.320935
830.554245	66065.415388	33.325952
831.265805	66188.069331	33.330970
831.979884	66294.543004	33.335988
832.530459	66405.082941	33.341005
833.699816	66489.082362	33.346023
834.822009	66597.555230	33.351040
835.235208	66706.596370	33.356058
836.377818	66796.526730	33.361076
836.934314	66913.587806	33.366093
837.944576	67008.625454	33.371111
838.341390	67115.296276	33.376128
839.445303	67230.503350	33.381146
840.339861	67339.452493	33.386164
840.996376	67452.824297	33.391181
842.008729	67559.589117	33.396199
842.865684	67687.194802	33.401216
843.375298	67801.735455	33.406234
844.548092	67907.282674	33.411252
845.218186	68024.856718	33.416269
845.666461	68137.716041	33.421287
846.847413	68256.296785	33.426304
847.414844	68382.847545	33.431322
848.379851	68496.485896	33.436340
849.577845	68624.542539	33.441357
850.421763	68742.914542	33.446375
851.354307	68846.394988	33.451392
851.955917	68981.195095	33.456410
853.365208	69084.215548	33.461428
854.416850	69202.127667	33.466445
854.835842	69304.978358	33.471463
856.387608	69409.917432	33.476480
857.232598	69518.697114	33.481498
858.150248	69633.069852	33.486516
859.060866	69738.314895	33.491533
860.140896	69835.560213	33.496551
860.869703	69949.680540	33.501568
861.048216	70058.758820	33.506586
862.495162	70172.930429	33.511604
863.528379	70280.528163	33.516621
864.002973	70387.646747	33.521639
864.745862	70492.840388	33.526656
865.747061	70605.057293	33.531674
866.834866	70715.359250	33.536692
867.774192	70826.696385	33.541709
868.616077	70924.837962	33.546727
870.481627	71009.933931	33.551744
870.854376	71117.982537	33.556762
872.373508	71197.814336	33.561780
873.456826	71304.487197	33.566797
874.094279	71389.489589	33.571815
874.549818	71479.765680	33.576832
875.450987	71574.767059	33.581850
876.421455	71665.625505	33.586868
877.039247	71762.498954	33.591885
877.636688	71856.185193	33.596903
878.655897	71965.405600	33.601920
879.336483	72068.001602	33.606938
879.899866	72165.049961	33.611956
880.461979	72259.078617	33.616973
881.314904	72377.129818	33.621991
881.813133	72476.395334	33.627008
882.646749	72577.933323	33.632026
883.513697	72687.137695	33.637044
884.055951	72803.857020	33.642061
884.586433	72917.381492	33.647079
885.506382	73039.729189	33.652096
886.257062	73172.303555	33.657114
887.253128	73301.850811	33.662132
888.035784	73418.168964	33.667149
888.719043	73548.355275	33.672167
889.856743	73678.659695	33.677184
890.840335	73816.635811	33.682202
891.952166	73944.709056	33.687220
892.888185	74067.547073	33.692237
893.580644	74189.407176	33.697255
894.905709	74314.959015	33.702272
896.128104	74428.407231	33.707290
897.336666	74546.743269	33.712308
898.474432	74660.364251	33.717325
899.383786	74779.747759	33.722343
900.424046	74888.291965	33.727360
901.174763	75002.393562	33.732378
901.995627	75121.603588	33.737396
902.887276	75241.245437	33.742413
903.742488	75356.697471	33.747431
904.823866	75461.787634	33.752448
905.708727	75583.082055	33.757466
906.171864	75701.025260	33.762484
907.120292	75816.370291	33.767501
907.987664	75936.961788	33.772519
909.174854	76059.392787	33.777536
910.288516	76178.145337	33.782554
910.950715	76289.696039	33.787572
911.857212	76407.983615	33.792589
912.454956	76532.426249	33.797607
913.400355	76647.485766	33.802624
914.127204	76789.214041	33.807642
915.231010	76914.305313	33.812660
916.449161	77044.397466	33.817677
916.981077	77164.025740	33.822695
917.849723	77296.412509	33.827712
919.060720	77427.481583	33.832730
920.213355	77533.121014	33.837748
921.089850	77669.124242	33.842765
921.748974	77799.044700	33.847783
922.901668	77910.203886	33.852800
923.693482	78043.334585	33.857818
924.406868	78161.618820	33.862836
925.657705	78291.840135	33.867853
926.621482	78416.969216	33.872871
927.578209	78547.219989	33.877888
927.939831	78667.478299	33.882906
929.369985	78758.162849	33.887924
930.522416	78882.209174	33.892941
931.283655	78989.327945	33.897959
931.962957	79101.763561	33.902976
932.954631	79218.125971	33.907994
933.720752	79336.440186	33.913012
934.641451	79452.044048	33.918029
935.254615	79578.683500	33.923047
936.537905	79680.330933	33.928064
937.317366	79803.228498	33.933082
938.537701	79909.305550	33.938100
939.922060	80046.659650	33.943117
940.385542	80170.488321	33.948135
941.443224	80264.936704	33.953152
941.967431	80390.855693	33.958170
943.350806	80513.667714	33.963188
945.214538	80600.738795	33.968205
946.246913	80715.023428	33.973223
947.440610	80817.025743	33.978240
948.475895	80925.691312	33.983258
949.274744	81004.475386	33.988276
950.351791	81122.314159	33.993293
950.975487	81229.409524	33.998311
952.033275	81335.595601	34.003328
952.618167	81447.022234	34.008346
953.346228	81573.674552	34.013364
954.286519	81667.869843	34.018381
955.061014	81793.517280	34.023399
955.867063	81905.410591	34.028416
956.630450	82042.333015	34.033434
957.359778	82165.246205	34.038452
958.694955	82290.156273	34.043469
958.731538	82426.368675	34.048487
960.195509	82557.360510	34.053504
961.329140	82680.003772	34.058522
962.286907	82827.059868	34.063540
963.200889	82947.602787	34.068557
964.179633	83082.708595	34.073575
964.981823	83224.690268	34.078592
966.014960	83355.414233	34.083610
966.660939	83495.121298	34.088628
968.122969	83611.863350	34.093645
968.922006	83763.617093	34.098663
969.891590	83884.814056	34.103680
970.807266	84024.551267	34.108698
971.438706	84166.515867	34.113716
972.515807	84298.819297	34.118733
973.150930	84440.791473	34.123751
974.400780	84598.043313	34.128768
975.581024	84730.756646	34.133786
976.144415	84875.563034	34.138804
977.181585	85021.376218	34.143821
978.110209	85168.826296	34.148839
979.123329	85311.477599	34.153856
980.463820	85452.231510	34.158874
981.052118	85589.679019	34.163892
982.097839	85721.364020	34.168909
983.212304	85859.741229	34.173927
983.982483	85990.365209	34.178944
984.579729	86131.621227	34.183962
985.542067	86264.612743	34.188980
986.652838	86393.774959	34.193997
987.357264	86557.805251	34.199015
988.568931	86696.355785	34.204032
989.785928	86834.900044	34.209050
990.721965	86989.848236	34.214068
991.875729	87117.724349	34.219085
992.970116	87276.753260	34.224103
994.132327	87403.630639	34.229120
994.936796	87548.669715	34.234138
996.143382	87701.847372	34.239156
997.316930	87827.694718	34.244173
998.114650	87973.085518	34.249191
999.033890	88110.856975	34.254208
1000.238068	88244.214337	34.259226
1000.931115	88393.412487	34.264244
1002.144064	88540.138584	34.269261
1002.724664	88686.947299	34.274279
1003.622032	88838.715088	34.279296
1004.505735	88977.756159	34.284314
1005.940677	89138.711326	34.289332
1007.111279	89291.463290	34.294349
1008.465950	89438.457499	34.299367
1009.456398	89571.268892	34.304384
1010.737722	89720.433173	34.309402
1011.656210	89861.352614	34.314420
1012.663681	89995.042936	34.319437
1013.560458	90152.157578	34.324455
1014.823467	90297.553166	34.329472
1015.818051	90434.707597	34.334490
1016.932906	90571.116457	34.339508
1018.149564	90708.136087	34.344525
1019.416600	90848.740826	34.349543
1020.508634	90985.712448	34.354560
1021.594573	91107.779075	34.359578
1021.874103	91256.284683	34.364596
1022.950584	91393.938050	34.369613
1023.992298	91533.495192	34.374631
1025.224348	91676.412954	34.379648
1026.599248	91802.978576	34.384666
1027.694893	91953.161598	34.389684
1029.787240	92056.263667	34.394701
1031.165228	92177.606702	34.399719
1032.044234	92288.151075	34.404736
1033.591846	92394.105326	34.409754
1034.481800	92507.912684	34.414772
1035.484859	92621.942982	34.419789
1036.249485	92721.243036	34.424807
1037.209910	92824.320026	34.429824
1038.019997	92950.773348	34.434842
1038.710924	93054.596352	34.439860
1039.663513	93152.850109	34.444877
1040.449663	93275.950478	34.449895
1040.708326	93385.536383	34.454912
1042.018232	93509.864041	34.459930
1042.625884	93631.489379	34.464948
1043.579926	93758.563244	34.469965
1044.331643	93905.379595	34.474983
1044.904176	94030.675036	34.480000
1045.993885	94167.186005	34.485018
1046.945043	94326.548218	34.490036
1047.965334	94471.624037	34.495053
1048.726910	94614.078918	34.500071
1049.312707	94789.936160	34.505088
1050.740903	94944.577626	34.510106
1051.509569	95106.055526	34.515124
1052.615302	95267.322831	34.520141
1053.960897	95423.891090	34.525159
1054.831663	95584.970321	34.530176
1056.016267	95748.214816	34.535194
1056.797035	95925.485881	34.540212
1057.781246	96075.176687	34.545229
1059.084447	96255.795884	34.550247
1060.017831	96416.852114	34.555264
1061.190078	96588.986345	34.560282
1062.467089	96751.723636	34.565300
1063.629119	96925.127264	34.570317
1064.763671	97085.036520	34.575335
1066.827421	97223.739130	34.580352
1068.476842	97384.909767	34.585370
1069.259512	97521.015419	34.590388
1070.888568	97664.142354	34.595405
1071.870294	97811.580188	34.600423
1072.737459	97946.719661	34.605440
1074.701611	98076.662255	34.610458
1075.853600	98204.115599	34.615476
1076.863177	98329.245165	34.620493
1078.066409	98452.826242	34.625511
1079.034107	98582.569588	34.630528
1080.133503	98716.031761	34.635546
1080.802435	98857.895394	34.640564
1081.451905	98988.975967	34.645581
1082.698761	99128.326227	34.650599
1083.537189	99275.524233	34.655616
1084.436485	99422.840037	34.660634
1085.064162	99573.958139	34.665652
1086.040337	99739.282656	34.670669
1087.115998	99885.877409	34.675687
1087.715680	100052.788844	34.680704
1088.934659	100209.688518	34.685722
1089.751721	100378.794851	34.690740
1090.696630	100548.793192	34.695757
1092.100425	100713.885835	34.700775
1092.769720	100883.816576	34.705792
1094.118441	101045.010111	34.710810
1095.131048	101209.168784	34.715828
1095.996527	101372.535785	34.720845
1097.258302	101518.022955	34.725863
1098.279857	101686.638056	34.730880
1099.489455	101833.128900	34.735898
1100.503096	102001.367885	34.740916
1101.340414	102156.025522	34.745933
1102.586521	102327.817616	34.750951
1103.531206	102493.976670	34.755968
1105.060445	102658.885966	34.760986
1106.180144	102827.651876	34.766004
1106.914282	102998.631766	34.771021
1108.268056	103161.092001	34.776039
1109.209608	103337.647833	34.781056
1110.409314	103503.634255	34.786074
1111.914775	103676.192283	34.791092
1113.317549	103833.295895	34.796109
1114.272725	103992.990303	34.801127
1115.446609	104156.030216	34.806144
1116.716966	104312.999873	34.811162
1117.710932	104484.626316	34.816180
1119.002859	104652.960230	34.821197
1120.003512	104821.923861	34.826215
1120.712240	104991.871710	34.831232
1122.349641	105144.478906	34.836250
1123.180265	105328.117018	34.841268
1124.258482	105499.250097	34.846285
1125.404608	105659.868285	34.851303
1126.353416	105849.199922	34.856320
1127.549200	106022.634305	34.861338
1128.622414	106196.450169	34.866356
1130.031500	106386.440653	34.871373
1131.134144	106543.597233	34.876391
1132.244380	106725.220704	34.881408
1133.754583	106897.832976	34.886426
1135.026400	107062.187241	34.891444
1136.196951	107233.071188	34.896461
1137.368435	107394.500730	34.901479
1138.194714	107573.112533	34.906496
1139.297027	107733.365486	34.911514
1140.488215	107922.023003	34.916532
1141.289178	108098.731324	34.921549
1142.608612	108261.738071	34.926567
1143.152892	108457.882461	34.931584
1144.371818	108636.192819	34.936602
1145.724431	108815.318698	34.941620
1146.802251	109007.211644	34.946637
1148.464055	109164.922949	34.951655
1149.948837	109351.563767	34.956672
1151.964759	109500.422971	34.961690
1153.057665	109670.165462	34.966708
1154.052345	109829.404964	34.971725
1155.464941	109990.357674	34.976743
1156.036663	110167.965613	34.981760
1157.725684	110319.350359	34.986778
1158.639450	110479.100662	34.991796
1159.544067	110625.440611	34.996813
1160.796322	110767.770005	35.001831
1161.682161	110933.287846	35.006848
1162.223951	111081.890997	35.011866
1163.595409	111240.832860	35.016884
1164.531593	111408.232206	35.021901
1165.570409	111568.957162	35.026919
1166.449868	111743.577712	35.031936
1167.870199	111907.295299	35.036954
1168.896891	112089.535336	35.041972
1170.039199	112273.961242	35.046989
1171.479774	112432.494625	35.052007
1172.498393	112618.335408	35.057024
1173.637413	112774.931204	35.062042
1175.164300	112948.482395	35.067060
1176.397661	113118.447795	35.072077
1177.648655	113291.481829	35.077095
1178.978093	113470.328667	35.082112
1180.455068	113629.066441	35.087130
1181.568614	113798.947893	35.092148
1182.361114	113980.859131	35.097165
1183.878446	114136.808214	35.102183
1185.084966	114308.507897	35.107200
1185.970365	114484.900269	35.112218
1187.393705	114667.975991	35.117236
1188.418896	114846.551790	35.122253
1189.732044	115010.572617	35.127271
1190.729650	115191.282422	35.132288
1191.908983	115382.575378	35.137306
1193.158495	115553.763875	35.142324
1194.069524	115732.351406	35.147341
1195.470671	115910.127853	35.152359
1196.604540	116099.052926	35.157376
1197.625062	116273.043068	35.162394
1199.100930	116467.298034	35.167412
1200.197236	116648.686275	35.172429
1201.112767	116839.145731	35.177447
1202.078895	117034.828303	35.182464
1203.460817	117213.344993	35.187482
1204.431940	117421.338071	35.192500
1205.531092	117620.821859	35.197517
1206.938054	117808.601771	35.202535
1207.980430	118009.788136	35.207552
1209.118174	118210.397386	35.212570
1210.143106	118421.916741	35.217588
1211.098379	118616.796260	35.222605
1212.221918	118816.025800	35.227623
1213.273231	119039.722151	35.232640
1214.383155	119245.966572	35.237658
1215.843326	119466.809203	35.242676
1217.128449	119692.987804	35.247693
1218.757263	119892.848119	35.252711
1219.771193	120109.385319	35.257728
1220.837822	120313.707425	35.262746
1221.989411	120525.173073	35.267764
1223.129257	120718.468559	35.272781
1224.355339	120908.914862	35.277799
1225.520173	121123.942010	35.282816
1226.605320	121327.585160	35.287834
1227.804591	121528.932037	35.292852
1228.806036	121736.593793	35.297869
1230.542366	121941.923935	35.302887
1232.015406	122153.503530	35.307904
1233.069689	122351.270105	35.312922
1234.697548	122552.911266	35.317940
1236.031528	122755.018644	35.322957
1237.615018	122936.468156	35.327975
1238.997578	123141.952486	35.332992
1240.310544	123335.644870	35.338010
1241.776057	123519.105646	35.343028
1242.795596	123711.948123	35.348045
1244.274667	123905.934882	35.353063
1245.808962	124100.040929	35.358080
1246.879108	124299.402694	35.363098
1247.935719	124475.854550	35.368116
1249.151492	124688.521109	35.373133
1250.759939	124865.305784	35.378151
1252.248751	125053.991977	35.383168
1253.587574	125252.165409	35.388186
1254.709097	125430.259866	35.393204
1256.007298	125628.594513	35.398221
1257.136531	125818.622562	35.403239
1258.661998	126006.498875	35.408256
1259.958822	126187.129190	35.413274
1261.457313	126377.457125	35.418292
1262.545159	126566.977619	35.423309
1263.526149	126754.590961	35.428327
1265.378929	126949.933556	35.433344
1265.897151	127153.647665	35.438362
1267.153205	127334.114699	35.443380
1268.085284	127538.183908	35.448397
1269.204425	127743.681705	35.453415
1270.879690	127956.782121	35.458432
1271.860353	128149.966311	35.463450
1273.664491	128349.076350	35.468468
1275.059475	128534.520439	35.473485
1276.594638	128730.394897	35.478503
1277.843231	128929.166700	35.483520
1279.115681	129119.739577	35.488538
1280.817853	129301.592773	35.493556
1281.843882	129503.748586	35.498573
1282.846503	129691.112407	35.503591
1284.028942	129889.673549	35.508608
1285.265019	130082.083115	35.513626
1286.329912	130285.619330	35.518644
1287.468381	130490.652960	35.523661
1288.824370	130691.979423	35.528679
1289.565345	130902.843764	35.533696
1290.492133	131109.005117	35.538714
1291.988774	131298.999747	35.543732
1292.918950	131505.644904	35.548749
1294.198853	131705.039577	35.553767
1295.377001	131917.108974	35.558784
1296.786187	132123.631823	35.563802
1297.916240	132326.057454	35.568820
1299.336862	132529.578648	35.573837
1300.522793	132737.383113	35.578855
1301.999568	132944.636052	35.583872
1303.302507	133163.283447	35.588890
1304.626650	133366.585213	35.593908
1305.767142	133584.349373	35.598925
1307.462482	133788.925544	35.603943
1308.965587	134001.110829	35.608960
1310.082562	134224.775478	35.613978
1311.725945	134433.672581	35.618996
1312.991665	134636.865911	35.624013
1314.323035	134851.733000	35.629031
1315.884637	135060.470240	35.634048
1316.691307	135273.269750	35.639066
1318.426526	135492.778453	35.644084
1319.714542	135705.758050	35.649101
1320.566441	135907.188690	35.654119
1321.941530	136131.688693	35.659136
1323.214034	136358.918486	35.664154
1324.694288	136580.579418	35.669172
1326.398589	136798.062686	35.674189
1327.547151	137015.103671	35.679207
1329.050298	137216.439805	35.684224
1330.187727	137447.906648	35.689242
1332.108734	137653.196454	35.694260
1333.309873	137888.762462	35.699277
1334.515926	138106.347253	35.704295
1336.121415	138322.260736	35.709312
1337.312716	138541.751958	35.714330
1338.514786	138753.018444	35.719348
1339.548736	138973.146151	35.724365
1341.144118	139201.993974	35.729383
1342.583482	139412.682480	35.734400
1343.812193	139632.720726	35.739418
1345.589778	139858.807212	35.744436
1346.718317	140082.261111	35.749453
1348.350195	140303.773676	35.754471
1349.658421	140514.579474	35.759488
1350.920068	140738.853542	35.764506
1352.184481	140948.401968	35.769524
1353.633316	141175.374373	35.774541
1354.777748	141397.846922	35.779559
1356.389010	141618.472548	35.784576
1357.429017	141848.924267	35.789594
1359.049398	142065.103074	35.794612
1360.214083	142292.369782	35.799629
1361.623542	142518.914861	35.804647
1363.098430	142732.054309	35.809664
1364.705449	142938.165215	35.814682
1366.240775	143136.798193	35.819700
1367.927145	143338.881320	35.824717
1369.043833	143541.499926	35.829735
1370.532671	143725.568080	35.834752
1371.934559	143929.614193	35.839770
1373.539875	144112.398643	35.844788
1374.506192	144310.026870	35.849805
1375.565562	144520.709689	35.854823
1376.972024	144717.294567	35.859840
1378.297344	144927.532265	35.864858
1379.812296	145134.939971	35.869876
1380.949457	145337.148748	35.874893
1382.859634	145540.820437	35.879911
1384.289421	145732.008187	35.884928
1385.654061	145944.287253	35.889946
1387.298762	146134.758810	35.894964
1388.697164	146340.659236	35.899981
1390.039678	146552.375501	35.904999
1391.007489	146756.027352	35.910016
1392.032668	146968.430635	35.915034
1392.879198	147200.575329	35.920052
1394.288533	147422.313721	35.925069
1394.993269	147657.501255	35.930087
1396.939199	147876.913809	35.935104
1398.109456	148119.928260	35.940122
1399.430376	148367.015200	35.945140
1400.983503	148609.554191	35.950157
1402.146710	148835.360052	35.955175
1404.050868	149069.163040	35.960192
1405.090569	149328.078999	35.965210
1406.928459	149553.643230	35.970228
1408.329604	149800.474872	35.975245
1409.517134	150046.074598	35.980263
1410.905444	150270.777132	35.985280
1412.341927	150523.161386	35.990298
1413.480311	150767.493926	35.995316
1414.921401	151019.158652	36.000333
1416.484575	151275.991163	36.005351
1418.084910	151513.206964	36.010368
1419.371915	151775.995197	36.015386
1420.988733	152019.982118	36.020404
1422.601606	152263.147383	36.025421
1424.088392	152501.668841	36.030439
1426.085080	152751.141231	36.035456
1427.685235	152967.701659	36.040474
1429.519882	153193.735190	36.045492
1431.289068	153419.577798	36.050509
1432.666857	153645.078405	36.055527
1433.937228	153871.180827	36.060544
1435.516190	154100.126540	36.065562
1436.985224	154321.674047	36.070580
1438.656568	154541.200246	36.075597
1440.048652	154760.708853	36.080615
1441.867817	154973.824066	36.085632
1442.986841	155187.039191	36.090650
1443.916624	155401.769219	36.095668
1445.342165	155602.994227	36.100685
1446.745029	155805.048203	36.105703
1448.149726	156016.156365	36.110720
1448.902586	156234.901171	36.115738
1450.564913	156440.379253	36.120756
1452.428958	156643.531456	36.125773
1453.948355	156867.395305	36.130791
1455.308954	157072.734917	36.135808
1456.348041	157287.941259	36.140826
1457.674790	157517.267038	36.145844
1459.400561	157733.698476	36.150861
1460.326713	157967.186621	36.155879
1461.757660	158179.166148	36.160896
1462.945525	158429.455470	36.165914
1464.461418	158660.698875	36.170932
1466.055095	158901.530759	36.175949
1466.890015	159150.892230	36.180967
1468.329201	159407.070558	36.185984
1469.702424	159646.991518	36.191002
1471.173779	159907.315061	36.196020
1472.616364	160163.396900	36.201037
1473.768225	160429.874698	36.206055
1475.165073	160679.474724	36.211072
1476.321759	160961.680634	36.216090
1477.762012	161225.125747	36.221108
1479.316271	161498.611238	36.226125
1480.602675	161778.279339	36.231143
1482.096448	162063.281095	36.236160
1483.655811	162337.203347	36.241178
1484.857799	162631.716688	36.246196
1486.908077	162896.028285	36.251213
1488.801757	163178.223280	36.256231
1490.855988	163456.539530	36.261248
1492.604675	163721.044552	36.266266
1493.996759	163993.128879	36.271284
1495.950294	164255.677481	36.276301
1496.998684	164522.011699	36.281319
1498.840581	164775.361426	36.286336
1500.825472	165040.256967	36.291354
1501.726865	165295.624064	36.296372
1503.188162	165563.726545	36.301389
1504.742442	165843.294445	36.306407
1506.794970	166095.389474	36.311424
1508.014685	166359.693042	36.316442
1509.795471	166612.012295	36.321460
1511.685547	166862.299207	36.326477
1513.144682	167118.947307	36.331495
1514.860192	167365.828050	36.336512
1516.386813	167619.145711	36.341530
1517.259118	167877.744019	36.346548
1519.345194	168118.507928	36.351565
1520.799223	168365.626982	36.356583
1522.782309	168621.377564	36.361600
1524.204171	168862.581478	36.366618
1525.847724	169089.393124	36.371636
1527.441992	169303.859415	36.376653
1528.798676	169538.190346	36.381671
1530.227710	169750.605134	36.386688
1531.554912	169980.529242	36.391706
1532.752923	170202.877156	36.396724
1534.612473	170436.537473	36.401741
1535.732130	170682.506789	36.406759
1537.276611	170916.017079	36.411776
1538.542561	171172.329762	36.416794
1540.044296	171409.097128	36.421812
1541.172936	171663.925320	36.426829
1542.861985	171912.336243	36.431847
1544.689904	172153.737103	36.436864
1546.364561	172410.969696	36.441882
1547.690474	172670.491987	36.446900
1549.107345	172910.389762	36.451917
1550.488468	173176.490350	36.456935
1551.891182	173427.315758	36.461952
1553.294298	173699.949444	36.466970
1554.718474	173967.443880	36.471988
1556.538089	174230.411843	36.477005
1557.674223	174508.345376	36.482023
1559.826360	174770.122296	36.487040
1561.318281	175044.565067	36.492058
1563.118043	175307.289453	36.497076
1565.436658	175562.663857	36.502093
1566.912755	175822.626608	36.507111
1568.668141	176072.473585	36.512128
1570.356089	176337.455163	36.517146
1571.844166	176592.422378	36.522164
1573.793915	176837.764742	36.527181
1575.259568	177111.844907	36.532199
1576.813330	177357.583101	36.537216
1578.757329	177596.206823	36.542234
1580.514773	177855.642872	36.547252
1582.190730	178099.856273	36.552269
1583.657873	178350.688901	36.557287
1585.375206	178599.466014	36.562304
1586.743560	178856.331096	36.567322
1587.856521	179113.225615	36.572340
1589.459945	179357.381692	36.577357
1591.204149	179619.076373	36.582375
1592.740521	179881.528865	36.587392
1594.381863	180142.989343	36.592410
1595.364209	180410.011827	36.597428
1597.054934	180671.987881	36.602445
1598.426522	180946.564584	36.607463
1600.114556	181207.085199	36.612480
1601.697699	181471.646164	36.617498
1603.042546	181750.736478	36.622516
1604.873019	182025.754648	36.627533
1606.229693	182304.402530	36.632551
1607.816217	182567.079030	36.637568
1610.020738	182839.200690	36.642586
1611.669969	183093.432526	36.647604
1613.440234	183333.562220	36.652621
1615.267936	183579.419384	36.657639
1616.843117	183810.928950	36.662656
1618.521077	184056.000446	36.667674
1619.815844	184295.525648	36.672692
1621.410963	184537.364577	36.677709
1623.060840	184789.613812	36.682727
1624.775883	185032.146940	36.687744
1626.648316	185280.188855	36.692762
1628.045952	185519.564641	36.697780
1629.249917	185777.968350	36.702797
1630.530173	186037.795307	36.707815
1632.241676	186299.547499	36.712832
1634.000622	186566.001468	36.717850
1635.311564	186846.626286	36.722868
1636.943226	187115.565432	36.727885
1638.504105	187390.341982	36.732903
1639.865582	187681.610545	36.737920
1641.488001	187941.622294	36.742938
1643.099209	188230.481610	36.747956
1645.083170	188509.144146	36.752973
1646.977518	188773.634990	36.757991
1648.744858	189055.710738	36.763008
1650.604836	189333.776015	36.768026
1651.659018	189630.270386	36.773044
1653.514973	189893.961395	36.778061
1655.211198	190191.194859	36.783079
1656.590131	190487.439922	36.788096
1658.089415	190763.819492	36.793114
1659.840262	191068.651407	36.798132
1661.278094	191351.681351	36.803149
1662.840829	191653.399485	36.808167
1664.397241	191962.240124	36.813184
1666.073216	192258.651871	36.818202
1667.801470	192575.489825	36.823220
1669.508585	192870.859636	36.828237
1671.503419	193172.315411	36.833255
1672.970905	193474.135964	36.838272
1675.393989	193781.720810	36.843290
1676.649770	194080.037724	36.848308
1678.516891	194385.303164	36.853325
1680.310176	194681.710698	36.858343
1681.928036	194980.610020	36.863360
1683.612259	195286.074922	36.868378
1685.034475	195581.391665	36.873396
1686.884108	195881.604798	36.878413
1688.692749	196181.090055	36.883431
1690.186966	196496.289045	36.888448
1692.011597	196792.170738	36.893466
1693.539257	197100.971223	36.898484
1695.324306	197394.641474	36.903501
1696.678835	197716.774649	36.908519
1698.264345	198026.434478	36.913536
1700.101724	198325.610150	36.918554
1701.881107	198619.300810	36.923572
1703.509080	198910.186657	36.928589
1705.368497	199197.889532	36.933607
1707.325849	199487.317317	36.938624
1709.085546	199754.958946	36.943642
1710.933801	200046.628309	36.948660
1712.498728	200324.876920	36.953677
1714.092274	200605.254846	36.958695
1716.195494	200887.482645	36.963712
1717.483193	201179.234367	36.968730
1719.279410	201477.710499	36.973748
1720.987034	201767.850073	36.978765
1723.019497	202055.337433	36.983783
1724.630569	202343.629403	36.988800
1726.711632	202640.403694	36.993818
1728.035191	202931.562302	36.998836
1730.112359	203217.512590	37.003853
1731.541865	203515.740459	37.008871
1733.123167	203824.405499	37.013888
1735.152045	204100.822137	37.018906
1736.693720	204411.057976	37.023924
1738.494882	204706.224566	37.028941
1740.456628	204994.182315	37.033959
1741.996468	205307.304802	37.038976
1744.196325	205605.801997	37.043994
1745.712945	205908.090526	37.049012
1747.296340	206200.176447	37.054029
1749.321825	206511.374870	37.059047
1751.322178	206813.362725	37.064064
1753.112861	207102.944752	37.069082
1754.826721	207408.675205	37.074100
1756.406961	207708.842772	37.079117
1758.061764	208010.066348	37.084135
1759.517753	208311.056389	37.089152
1762.180517	208615.093516	37.094170
1764.166407	208921.258102	37.099188
1765.932970	209215.284549	37.104205
1767.540199	209512.790736	37.109223
1769.572530	209797.319952	37.114240
1771.438195	210103.915706	37.119258
1773.083206	210403.476754	37.124276
1774.714566	210710.049184	37.129293
1776.599758	210985.314195	37.134311
1778.624121	211292.741115	37.139328
1781.009271	211565.085495	37.144346
1782.893751	211847.184485	37.149364
1784.941841	212120.689238	37.154381
1786.677760	212415.509850	37.159399
1788.133426	212703.203234	37.164416
1790.318082	212970.557876	37.169434
1792.159530	213254.523379	37.174452
1793.880601	213540.223151	37.179469
1795.966759	213803.686495	37.184487
1797.577874	214066.642279	37.189504
1799.731892	214337.676434	37.194522
1801.296408	214599.029317	37.199540
1803.409237	214835.983188	37.204557
1804.933738	215072.040983	37.209575
1806.537975	215317.558280	37.214592
1808.307752	215567.163755	37.219610
1810.159443	215814.840004	37.224628
1811.746225	216080.676820	37.229645
1813.447749	216336.593291	37.234663
1814.917423	216588.611625	37.239680
1816.538352	216855.779112	37.244698
1818.168540	217132.011447	37.249716
1819.696464	217402.433385	37.254733
1821.095496	217681.205783	37.259751
1822.638280	217970.304222	37.264768
1824.549531	218265.185825	37.269786
1826.417667	218554.387340	37.274804
1827.770960	218859.580828	37.279821
1829.551632	219152.366419	37.284839
1831.503604	219462.381091	37.289856
1833.314378	219766.985187	37.294874
1834.930570	220079.112665	37.299892
1836.815440	220395.566602	37.304909
1838.779393	220705.064004	37.309927
1840.325543	221028.062608	37.314944
1842.383238	221339.604685	37.319962
1844.108417	221712.439818	37.324980
1845.980517	222049.713574	37.329997
1848.165362	222359.500093	37.335015
1849.642955	222683.710132	37.340032
1851.802912	223002.632636	37.345050
1854.148390	223334.135664	37.350068
1855.756848	223656.551301	37.355085
1858.220524	223968.674386	37.360103
1860.423963	224273.691190	37.365120
1862.468536	224581.324710	37.370138
1864.402884	224882.704184	37.375156
1866.437401	225188.221074	37.380173
1868.610932	225483.914270	37.385191
1870.294085	225798.822153	37.390208
1872.356033	226095.347919	37.395226
1874.119006	226419.705489	37.400244
1875.792251	226716.701490	37.405261
1878.076652	227016.750676	37.410279
1879.460191	227326.924659	37.415296
1881.366502	227628.178842	37.420314
1883.449071	227929.914038	37.425332
1884.923909	228247.137083	37.430349
1887.396926	228553.485459	37.435367
1888.975901	228857.665687	37.440384
1891.072598	229163.136231	37.445402
1893.269594	229463.233149	37.450420
1895.343758	229761.801349	37.455437
1897.765778	230037.229348	37.460455
1899.749056	230352.017292	37.465472
1901.643962	230623.644950	37.470490
1903.773530	230885.255011	37.475508
1905.661721	231147.818427	37.480525
1907.599093	231397.650635	37.485543
1909.519649	231651.803767	37.490560
1911.482288	231904.604835	37.495578
1913.103908	232157.130527	37.500596
1914.809381	232411.116655	37.505613
1916.759171	232678.525541	37.510631
1918.011833	232949.449120	37.515648
1920.101798	233217.853174	37.520666
1921.827815	233492.004886	37.525684
1923.929382	233772.244116	37.530701
1925.625836	234046.986224	37.535719
1927.162146	234338.618953	37.540736
1928.729613	234634.844687	37.545754
1930.699656	234919.933698	37.550772
1932.382325	235221.324144	37.555789
1934.759894	235521.538469	37.560807
1936.032814	235825.687956	37.565824
1937.855736	236133.637060	37.570842
1939.913647	236441.143400	37.575860
1941.673474	236762.438721	37.580877
1943.734390	237074.848404	37.585895
1945.438775	237399.761087	37.590912
1947.207103	237720.778538	37.595930
1949.121152	238038.141729	37.600948
1951.133822	238385.791478	37.605965
1953.590561	238709.471091	37.610983
1955.503102	239040.502217	37.616000
1957.102765	239370.872771	37.621018
1959.618490	239682.100072	37.626036
1961.518953	240020.349421	37.631053
1963.546247	240350.527930	37.636071
1965.538464	240682.744913	37.641088
1967.500546	241008.262056	37.646106
1969.576427	241337.978409	37.651124
1971.311805	241675.776075	37.656141
1973.357490	242003.924228	37.661159
1975.390973	242356.230682	37.666176
1977.016798	242699.788954	37.671194
1979.183630	243034.219839	37.676212
1980.962560	243374.885423	37.681229
1982.888988	243721.116586	37.686247
1984.735332	244072.670069	37.691264
1986.653484	244429.039193	37.696282
1988.968768	244775.313034	37.701300
1990.774460	245125.580317	37.706317
1993.238966	245466.167909	37.711335
1994.888991	245820.246370	37.716352
1997.313146	246175.295142	37.721370
1999.553237	246515.362085	37.726388
2001.095162	246869.231719	37.731405
2002.989333	247213.038333	37.736423
2005.502159	247550.067120	37.741440
2007.600904	247892.953827	37.746458
2009.958351	248206.538111	37.751476
2011.504686	248526.475030	37.756493
2014.002474	248835.999547	37.761511
2015.946597	249149.371918	37.766528
2017.890719	249455.302308	37.771546
2020.194067	249762.522570	37.776564
2022.387185	250078.905441	37.781581
2024.563349	250386.705898	37.786599
2025.999993	250702.727355	37.791616
2028.137084	251013.024525	37.796634
2030.674170	251313.453762	37.801652
2032.519193	251628.192876	37.806669
2034.846707	251932.923928	37.811687
2036.837061	252247.920520	37.816704
2038.713561	252553.816467	37.821722
2040.683296	252867.064687	37.826740
2042.833187	253184.577788	37.831757
2044.641151	253500.189722	37.836775
2046.384192	253826.811555	37.841792
2048.222059	254160.252056	37.846810
2050.267698	254477.352015	37.851828
2051.963755	254826.590848	37.856845
2054.433882	255164.911561	37.861863
2056.631294	255500.075414	37.866880
2058.348641	255843.419285	37.871898
2060.344923	256177.498424	37.876916
2062.433244	256520.149474	37.881933
2064.333932	256867.428655	37.886951
2066.614998	257219.728521	37.891968
2068.663184	257564.038692	37.896986
2070.962721	257902.212900	37.902004
2072.633505	258270.843364	37.907021
2075.032484	258620.814993	37.912039
2076.937459	258971.271919	37.917056
2078.969818	259332.962498	37.922074
2081.183999	259688.985344	37.927092
2082.923183	260041.629243	37.932109
2085.219982	260399.976978	37.937127
2087.460340	260763.973546	37.942144
2089.410488	261114.984967	37.947162
2091.765073	261474.645834	37.952180
2093.659097	261845.227214	37.957197
2095.955284	262199.817627	37.962215
2098.322827	262556.276937	37.967232
2100.669909	262925.695392	37.972250
2103.094357	263274.144517	37.977268
2105.338690	263627.626957	37.982285
2107.261287	263974.606795	37.987303
2109.372722	264325.951738	37.992320
2111.386030	264681.123033	37.997338
2113.359747	265031.372727	38.002356
2115.285487	265392.528273	38.007373
2117.348686	265745.965173	38.012391
2119.879386	266104.459649	38.017408
2121.827231	266456.645249	38.022426
2123.882627	266790.218907	38.027444
2125.772484	267114.800902	38.032461
2128.041186	267446.994794	38.037479
2130.194106	267769.147568	38.042496
2132.149926	268096.387039	38.047514
2134.191067	268437.457950	38.052532
2136.348099	268772.286862	38.057549
2138.183923	269104.067688	38.062567
2140.592651	269446.859064	38.067584
2142.312791	269792.833614	38.072602
2144.647171	270129.692715	38.077620
2146.689513	270472.390236	38.082637
2148.781077	270826.155947	38.087655
2151.332404	271183.125908	38.092672
2153.289352	271531.045041	38.097690
2155.565029	271879.066150	38.102708
2157.615998	272231.466972	38.107725
2160.200437	272588.533712	38.112743
2162.459454	272928.250808	38.117760
2164.437433	273295.194181	38.122778
2166.721175	273641.309132	38.127796
2169.003907	273996.518708	38.132813
2171.001005	274355.279286	38.137831
2173.403189	274719.589801	38.142848
2175.246782	275077.333218	38.147866
2177.357696	275445.652868	38.152884
2179.474353	275806.579203	38.157901
2181.735460	276166.796714	38.162919
2184.209707	276533.483664	38.167936
2186.212108	276903.344608	38.172954
2188.736697	277269.515399	38.177972
2191.060916	277632.491662	38.182989
2192.738281	278008.145096	38.188007
2195.443630	278371.263968	38.193024
2197.755176	278732.387508	38.198042
2200.824053	279074.262105	38.203060
2203.161023	279431.393050	38.208077
2205.676237	279777.292720	38.213095
2208.057690	280125.296538	38.218112
2210.103563	280469.898566	38.223130
2212.597394	280817.782643	38.228148
2214.778550	281171.304857	38.233165
2217.073051	281506.924998	38.238183
2219.446531	281842.964295	38.243200
2221.293120	282200.374880	38.248218
2223.574184	282520.907055	38.253236
2226.158788	282862.323170	38.258253
2228.260023	283206.025788	38.263271
2230.693344	283536.745290	38.268288
2232.879529	283891.890797	38.273306
2234.827412	284223.677515	38.278324
2237.131614	284562.672784	38.283341
2238.953036	284917.367249	38.288359
2241.098687	285256.006055	38.293376
2242.995577	285597.732386	38.298394
2245.434091	285911.022738	38.303412
2247.277209	286245.542551	38.308429
2249.097581	286579.557604	38.313447
2251.245649	286906.051909	38.318464
2253.266709	287233.709177	38.323482
2255.316259	287584.529076	38.328500
2257.506012	287926.816397	38.333517
2259.410836	288278.801617	38.338535
2261.610291	288629.012329	38.343552
2263.412645	288995.035335	38.348570
2265.651168	289361.827022	38.353588
2267.708564	289736.725028	38.358605
2269.716448	290114.780314	38.363623
2271.996298	290491.674237	38.368640
2274.186423	290881.384776	38.373658
2276.879674	291259.914026	38.378676
2279.177275	291647.015292	38.383693
2281.630334	292051.923869	38.388711
2283.950154	292440.519099	38.393728
2286.151676	292832.053720	38.398746
2288.401308	293217.051634	38.403764
2290.507605	293612.893011	38.408781
2292.577030	294013.997796	38.413799
2295.801555	294416.290431	38.418816
2297.595700	294835.574515	38.423834
2299.962382	295236.198012	38.428852
2302.204703	295642.047862	38.433869
2304.290613	296050.385675	38.438887
2306.883414	296457.016546	38.443904
2309.049299	296878.167929	38.448922
2311.581522	297281.656790	38.453940
2314.200842	297691.506815	38.458957
2316.338397	298120.127976	38.463975
2319.095520	298518.396460	38.468992
2321.436519	298942.309450	38.474010
2323.710160	299352.616822	38.479028
2326.368609	299759.255178	38.484045
2328.713148	300170.514556	38.489063
2331.100014	300584.026907	38.494080
2333.427007	300995.109154	38.499098
2336.050546	301402.409336	38.504116
2338.765275	301811.776889	38.509133
2340.977365	302218.860718	38.514151
2343.291702	302614.369760	38.519168
2345.896787	303016.791526	38.524186
2347.938734	303424.076820	38.529204
2350.685998	303826.473803	38.534221
2353.111883	304222.824404	38.539239
2355.388363	304617.851328	38.544256
2357.706073	305026.815527	38.549274
2360.335939	305424.070170	38.554292
2362.822837	305824.013350	38.559309
2364.804285	306235.795822	38.564327
2367.107739	306624.081474	38.569344
2369.726845	307019.173991	38.574362
2371.714836	307394.934202	38.579380
2374.119421	307758.486024	38.584397
2376.254276	308140.265945	38.589415
2378.317049	308509.279947	38.594432
2380.853756	308894.397418	38.599450
2382.923720	309282.051416	38.604468
2385.444319	309664.806789	38.609485
2387.159297	310049.669779	38.614503
2389.609734	310443.101564	38.619520
2391.986969	310849.878308	38.624538
2393.848944	311261.281749	38.629556
2396.237881	311664.853399	38.634573
2398.517035	312080.226192	38.639591
2401.702977	312475.058264	38.644608
2403.646870	312904.044167	38.649626
2405.590220	313327.643892	38.654644
2408.369468	313739.883205	38.659661
2410.392775	314174.540732	38.664679
2413.179466	314600.084376	38.669696
2415.940982	315034.443515	38.674714
2418.312174	315456.798459	38.679732
2421.397550	315866.415532	38.684749
2424.229787	316284.681010	38.689767
2427.071137	316687.983846	38.694784
2429.640197	317105.754189	38.699802
2432.467618	317505.931909	38.704820
2435.309141	317911.134472	38.709837
2437.718943	318315.006862	38.714855
2440.307274	318707.674340	38.719872
2442.617272	319106.378057	38.724890
2445.030790	319512.352668	38.729908
2447.667697	319907.420102	38.734925
2449.873674	320312.408162	38.739943
2452.614812	320707.506383	38.744960
2454.981713	321118.662153	38.749978
2457.199452	321523.566671	38.754996
2459.763694	321929.557257	38.760013
2462.112213	322328.697696	38.765031
2464.544827	322727.619793	38.770048
2467.400404	323135.818813	38.775066
2469.523830	323542.430352	38.780084
2472.277162	323942.260968	38.785101
2474.516297	324363.452871	38.790119
2476.991527	324762.688713	38.795136
2479.441175	325178.840133	38.800154
2481.727082	325594.507462	38.805172
2484.214234	325990.307007	38.810189
2486.449331	326411.692114	38.815207
2489.153712	326819.871374	38.820224
2491.863583	327240.491170	38.825242
2494.140993	327662.497757	38.830260
2496.822158	328074.788100	38.835277
2499.176678	328501.628265	38.840295
2501.507162	328906.072007	38.845312
2504.017616	329317.290732	38.850330
2506.042870	329714.515751	38.855348
2508.921799	330108.835448	38.860365
2511.337518	330495.303562	38.865383
2513.717902	330876.493353	38.870400
2516.285813	331279.972397	38.875418
2518.408665	331666.836227	38.880436
2520.716169	332062.175479	38.885453
2522.909320	332470.455780	38.890471
2525.384125	332880.593584	38.895488
2527.837566	333291.849674	38.900506
2529.877366	333719.648750	38.905524
2532.860641	334129.013078	38.910541
2535.339381	334557.930883	38.915559
2537.800710	334992.003385	38.920576
2540.646954	335421.924011	38.925594
2542.642515	335853.170099	38.930612
2545.347539	336288.566824	38.935629
2547.912308	336731.651179	38.940647
2550.522379	337169.469368	38.945664
2553.206164	337607.856957	38.950682
2555.910469	338062.869490	38.955700
2558.549737	338493.056847	38.960717
2561.567838	338934.048532	38.965735
2563.927114	339377.528257	38.970752
2566.993939	339825.742343	38.975770
2569.487849	340262.186791	38.980788
2572.142198	340700.050005	38.985805
2574.575702	341142.312169	38.990823
2577.421697	341588.314260	38.995840
2579.894761	342030.969998	39.000858
2582.411558	342480.775362	39.005876
2585.130150	342920.135893	39.010893
2587.632865	343381.412627	39.015911
2590.071351	343831.017175	39.020928
2592.852641	344285.337044	39.025946
2595.371648	344735.962879	39.030964
2597.794371	345198.405961	39.035981
2600.212150	345658.383522	39.040999
2602.686316	346117.002939	39.046016
2605.491077	346583.842640	39.051034
2607.654416	347065.961714	39.056052
2610.434836	347530.360315	39.061069
2613.127423	348001.293415	39.066087
2615.640708	348490.072362	39.071104
2618.353632	348966.731454	39.076122
2620.723269	349444.481637	39.081140
2623.384367	349918.957470	39.086157
2626.111590	350402.430631	39.091175
2628.490435	350887.782412	39.096192
2631.490757	351362.699558	39.101210
2633.793386	351853.334804	39.106228
2636.952913	352332.406616	39.111245
2640.008175	352806.540595	39.116263
2642.582471	353286.508718	39.121280
2645.498990	353753.472308	39.126298
2648.198104	354192.493053	39.131316
2651.354965	354618.466480	39.136333
2653.837021	355049.163042	39.141351
2656.209642	355472.029863	39.146368
2658.897887	355892.127176	39.151386
2661.263025	356339.025689	39.156404
2663.863018	356764.434703	39.161421
2666.515963	357208.792360	39.166439
2668.706876	357658.980966	39.171456
2671.362447	358101.401142	39.176474
2673.924590	358570.685971	39.181492
2676.443641	359015.023135	39.186509
2679.320230	359474.706010	39.191527
2681.700766	359947.178941	39.196544
2684.111362	360404.287119	39.201562
2686.818410	360882.130586	39.206580
2689.808228	361343.757253	39.211597
2692.461168	361823.477924	39.216615
2695.212689	362313.888319	39.221632
2698.137388	362778.505996	39.226650
2700.299245	363271.715291	39.231668
2703.306941	363751.918251	39.236685
2706.040805	364239.341715	39.241703
2708.707016	364735.881528	39.246720
2711.544102	365215.157122	39.251738
2714.367233	365706.890356	39.256756
2717.248144	366201.527476	39.261773
2720.112800	366688.269364	39.266791
2722.740765	367183.620827	39.271808
2725.617563	367664.081961	39.276826
2728.295741	368165.733238	39.281844
2731.207139	368657.343633	39.286861
2733.947793	369147.351458	39.291879
2736.606178	369654.799768	39.296896
2739.758727	370150.313600	39.301914
2742.688311	370650.551372	39.306932
2745.277671	371146.777199	39.311949
2748.038130	371646.167291	39.316967
2750.699904	372142.674450	39.321984
2753.251534	372639.218545	39.327002
2756.103398	373149.131749	39.332020
2758.972324	373655.889716	39.337037
2761.605884	374152.834074	39.342055
2764.362793	374661.931701	39.347072
2767.476791	375154.170041	39.352090
2770.015224	375668.110418	39.357108
2772.688150	376174.817444	39.362125
2775.382521	376678.622373	39.367143
2778.108325	377200.175641	39.372160
2780.928652	377713.563155	39.377178
2783.786905	378229.221340	39.382196
2786.516617	378747.024211	39.387213
2789.095875	379261.241591	39.392231
2791.633265	379791.898112	39.397248
2794.468531	380300.708324	39.402266
2796.654346	380797.336271	39.407284
2799.629734	381279.220671	39.412301
2802.393138	381761.589196	39.417319
2805.340245	382263.303403	39.422336
2808.181834	382749.832675	39.427354
2810.869770	383234.452120	39.432372
2813.669660	383737.895007	39.437389
2816.196388	384253.474090	39.442407
2818.703976	384759.207087	39.447424
2821.519006	385256.310944	39.452442
2824.296303	385769.241995	39.457460
2827.060213	386283.715263	39.462477
2830.091403	386800.218871	39.467495
2832.478855	387331.426822	39.472512
2835.828877	387858.010569	39.477530
2838.807694	388392.026146	39.482548
2841.434415	388923.324949	39.487565
2844.286584	389457.268599	39.492583
2846.814242	390007.588904	39.497600
2850.066600	390531.384211	39.502618
2852.920222	391080.393456	39.507636
2855.803018	391621.730434	39.512653
2858.698465	392177.918378	39.517671
2861.808807	392712.608585	39.522688
2864.738386	393244.935304	39.527706
2867.488712	393808.398276	39.532724
2870.517581	394356.947460	39.537741
2873.784410	394899.338704	39.542759
2876.706278	395458.233399	39.547776
2879.867001	396006.481454	39.552794
2882.691550	396546.583329	39.557812
2885.361333	397110.206945	39.562829
2888.332521	397646.312121	39.567847
2890.892376	398217.744190	39.572864
2893.596089	398774.842961	39.577882
2896.599755	399343.091851	39.582900
2899.211852	399904.749874	39.587917
2902.481974	400476.613300	39.592935
2905.048381	401052.406472	39.597952
2907.807150	401630.871745	39.602970
2910.957129	402206.678661	39.607988
2913.864199	402784.339040	39.613005
2916.437352	403362.853051	39.618023
2919.572369	403955.388441	39.623040
2922.290787	404541.463378	39.628058
2925.381281	405138.850946	39.633076
2928.205772	405724.025032	39.638093
2931.595769	406302.710462	39.643111
2934.115121	406906.770747	39.648128
2937.443380	407484.353786	39.653146
2940.927938	408059.670561	39.658164
2943.395979	408647.507120	39.663181
2946.501551	409236.067876	39.668199
2949.590888	409820.437529	39.673216
2952.752400	410394.874006	39.678234
2955.478074	410941.564037	39.683252
2958.530833	411473.593332	39.688269
2961.599844	412010.654197	39.693287
2964.269419	412559.046860	39.698304
2967.084252	413096.128251	39.703322
2969.826240	413641.219936	39.708340
2972.672226	414192.899571	39.713357
2975.785482	414738.266850	39.718375
2978.888800	415299.438965	39.723392
2981.853006	415839.537960	39.728410
2984.659686	416406.564097	39.733428
2987.883121	416962.109785	39.738445
2990.892897	417508.936130	39.743463
2993.851258	418079.706125	39.748480
2996.935579	418646.466457	39.753498
3000.014675	419199.254643	39.758516
3002.446025	419782.312235	39.763533
3005.332720	420349.550980	39.768551
3008.390293	420942.189624	39.773568
3011.141429	421523.259986	39.778586
3013.831202	422123.203214	39.783604
3016.719355	422730.778650	39.788621
3019.962843	423325.135607	39.793639
3022.654374	423945.357362	39.798656
3025.465801	424558.832582	39.803674
3028.614123	425183.285893	39.808692
3031.351811	425806.193798	39.813709
3034.582575	426439.294055	39.818727
3037.482811	427073.976869	39.823744
3040.314777	427721.016815	39.828762
3043.113848	428363.284137	39.833780
3045.736075	429017.620715	39.838797
3048.998661	429670.395968	39.843815
3051.890508	430334.054139	39.848832
3055.069150	431006.717355	39.853850
3058.336951	431668.331830	39.858868
3061.135556	432348.441192	39.863885
3064.650101	433008.209466	39.868903
3067.415341	433690.036106	39.873920
3070.796913	434352.146018	39.878938
3074.078210	435040.515194	39.883956
3077.064791	435720.732983	39.888973
3080.639678	436394.837971	39.893991
3083.802783	437055.088456	39.899008
3087.052596	437730.677604	39.904026
3090.711378	438385.699641	39.909044
3093.658552	439066.491020	39.914061
3097.074422	439725.567164	39.919079
3100.244034	440389.829526	39.924096
3103.374774	441057.118133	39.929114
3106.541753	441713.040822	39.934132
3109.425136	442372.788098	39.939149
3112.760816	443023.787953	39.944167
3115.828173	443693.849388	39.949184
3118.587524	444340.500032	39.954202
3122.021311	444959.029875	39.959220
3125.117480	445581.393989	39.964237
3127.897527	446193.869457	39.969255
3131.143873	446813.595623	39.974272
3133.955190	447448.763260	39.979290
3137.040701	448055.016842	39.984308
3140.168252	448691.467526	39.989325
3142.978122	449312.158441	39.994343
3145.979067	449945.557806	39.999360
3148.673097	450601.613151	40.004378
3152.015198	451243.274380	40.009396
3154.731927	451899.137306	40.014413
3158.336676	452565.469135	40.019431
3161.363266	453222.915173	40.024448
3164.338364	453893.660066	40.029466
3167.383856	454569.282707	40.034484
3170.225477	455247.346352	40.039501
3173.128843	455942.129274	40.044519
3176.041161	456629.754427	40.049536
3179.171848	457333.515696	40.054554
3182.282574	458035.537470	40.059572
3185.348329	458766.788756	40.064589
3188.248250	459480.586825	40.069607
3191.168352	460207.360873	40.074624
3194.309704	460942.170351	40.079642
3197.339739	461671.357169	40.084660
3200.383987	462435.169877	40.089677
3203.794445	463195.204844	40.094695
3207.213101	463961.231152	40.099712
3210.288934	464731.735509	40.104730
3213.835510	465489.998213	40.109748
3217.212523	466271.071661	40.114765
3220.642505	467028.083842	40.119783
3223.878083	467790.106476	40.124800
3227.150966	468551.792072	40.129818
3230.635261	469325.199577	40.134836
3233.652383	470087.982037	40.139853
3237.249915	470850.088369	40.144871
3240.712576	471618.306330	40.149888
3244.301889	472389.408241	40.154906
3247.659181	473139.332321	40.159924
3251.062178	473901.406574	40.164941
3254.534715	474654.644097	40.169959
3258.429765	475409.758446	40.174976
3261.683322	476154.936157	40.179994
3265.270213	476896.646466	40.185012
3268.444012	477647.038758	40.190029
3272.015633	478383.843342	40.195047
3275.393896	479109.480269	40.200064
3278.391965	479851.224031	40.205082
3281.795837	480600.709887	40.210100
3284.861703	481348.350549	40.215117
3288.454374	482072.277461	40.220135
3292.162346	482811.320475	40.225152
3295.293308	483526.270609	40.230170
3298.760014	484212.791805	40.235188
3301.639526	484898.775022	40.240205
3304.588392	485582.499456	40.245223
3307.735202	486267.633505	40.250240
3310.461184	486962.864284	40.255258
3313.762169	487662.930155	40.260276
3316.709799	488363.480753	40.265293
3319.796128	489075.199087	40.270311
3322.571020	489792.547373	40.275328
3326.000548	490525.879656	40.280346
3329.714696	491245.347578	40.285364
3332.234159	491990.182630	40.290381
3335.479885	492738.964373	40.295399
3339.353602	493496.960676	40.300416
3342.085268	494248.995061	40.305434
3345.292886	494992.893160	40.310452
3348.674285	495766.732164	40.315469
3352.299787	496529.541139	40.320487
3355.599928	497317.113756	40.325504
3358.534509	498090.722491	40.330522
3362.320457	498861.790251	40.335540
3365.075003	499658.789341	40.340557
3368.503451	500444.791193	40.345575
3372.087454	501238.609879	40.350592
3375.410717	502046.216786	40.355610
3379.341215	502830.468829	40.360628
3382.853277	503633.530953	40.365645
3386.171196	504428.258224	40.370663
3389.888444	505236.010086	40.375680
3393.251702	506049.988814	40.380698
3396.773883	506851.589394	40.385716
3399.986968	507649.366163	40.390733
3402.981617	508479.338280	40.395751
3406.543439	509297.624482	40.400768
3409.845449	510111.169343	40.405786
3413.297916	510944.734489	40.410804
3417.465236	511754.229346	40.415821
3420.579715	512571.722914	40.420839
3424.123498	513398.594078	40.425856
3427.612428	514236.834917	40.430874
3431.598209	515022.541012	40.435892
3434.989654	515846.087167	40.440909
3438.311865	516684.484003	40.445927
3441.917290	517499.188102	40.450944
3445.348468	518314.081416	40.455962
3448.486318	519152.180737	40.460980
3451.735970	519978.721206	40.465997
3455.195442	520811.742647	40.471015
3458.426969	521643.950801	40.476032
3461.664138	522492.352100	40.481050
3464.884818	523337.484648	40.486068
3468.948741	524178.910396	40.491085
3472.237732	525005.390601	40.496103
3475.604760	525856.367371	40.501120
3479.064132	526686.605318	40.506125
3482.523642	527469.913808	40.511130
3485.508348	528202.268857	40.516135
3489.068188	528861.681230	40.521140
3491.846509	529521.088524	40.526144
3494.479341	530068.266366	40.531149
3497.299350	530548.295055	40.536154
3499.899993	531009.345909	40.541159
3502.074990	531399.210561	40.546164
3504.654971	531714.883182	40.551168
3506.421258	532006.022860	40.556173
3508.158780	532220.570174	40.561178
3509.466906	532396.735481	40.566183
3511.046311	532549.111003	40.571188
3512.697521	532657.571182	40.576192
3513.576498	532719.067536	40.581197
3514.583353	532746.896824	40.586202
3515.877591	532750.582393	40.591207
3516.651425	532708.831198	40.596212
3517.797170	532666.717990	40.601216
3518.419093	532570.731054	40.606221
3518.807251	532463.211073	40.611226
3519.246325	532331.381319	40.616231
3519.653913	532190.309850	40.621236
3520.002153	532034.443313	40.626240
3520.379494	531870.234275	40.631245
3520.911945	531678.867660	40.636250
3521.270228	531481.210658	40.641255
3520.818514	531268.420549	40.646260
3521.283083	531048.611203	40.651264
3521.002792	530817.800619	40.656269
3521.391943	530583.495497	40.661274
3521.299325	530351.486262	40.666279
3521.233748	530112.041568	40.671284
3521.188406	529859.654406	40.676288
3520.995275	529620.171858	40.681293
3521.469949	529350.564484	40.686298
3521.502985	529091.735148	40.691303
3521.030071	528840.207764	40.696308
3520.906737	528566.790479	40.701312
3520.952995	528313.555583	40.706317
3520.473348	528050.090499	40.711322
3520.550435	527797.600525	40.716327
3520.273076	527530.405685	40.721332
3520.001549	527275.890489	40.726336
3519.775223	527029.450293	40.731341
3519.752417	526756.845116	40.736346
3519.319293	526515.281463	40.741351
3519.205084	526237.223482	40.746356
3519.133228	526011.414545	40.751360
3518.988065	525754.631257	40.756365
3518.799655	525498.204492	40.761370
3518.349978	525255.158655	40.766375
3518.229752	525018.173037	40.771380
3518.354146	524769.620785	40.776384
3517.769866	524535.329778	40.781389
3517.636992	524295.049964	40.786394
3517.795851	524058.814865	40.791399
3517.267660	523830.974916	40.796404
3517.391507	523592.109973	40.801408
3517.171353	523373.667672	40.806413
3516.706302	523145.706977	40.811418
3516.563755	522913.445751	40.816423
3515.951910	522718.411418	40.821428
3516.065227	522489.490688	40.826432
3515.596221	522278.605361	40.831437
3515.716772	522076.370030	40.836442
3515.263527	521857.741926	40.841447
3514.961836	521664.465898	40.846452
3514.713265	521475.173126	40.851456
3514.546973	521282.376729	40.856461
3514.119895	521100.034102	40.861466
3514.746698	520910.545872	40.866471
3514.415200	520717.516125	40.871476
3513.857665	520535.440607	40.876480
3513.793010	520360.110726	40.881485
3513.463158	520179.461495	40.886490
3513.570003	520011.280333	40.891495
3513.594937	519842.250850	40.896500
3513.210457	519660.542749	40.901504
3513.068169	519500.030564	40.906509
3512.750129	519320.785758	40.911514
3512.524336	519168.171343	40.916519
3512.205618	519004.193329	40.921524
3512.642089	518843.987784	40.926528
3512.351221	518708.672403	40.931533
3512.048703	518546.406476	40.936538
3512.011311	518395.575480	40.941543
3511.744921	518235.829078	40.946548
3511.739747	518088.378123	40.951552
3511.079538	517966.363498	40.956557
3511.320816	517811.184925	40.961562
3511.106513	517671.854114	40.966567
3510.676158	517560.621708	40.971572
3511.129276	517410.614438	40.976576
3510.807657	517282.675282	40.981581
3510.437423	517154.692254	40.986586
3510.719480	517013.962658	40.991591
3510.289817	516906.113941	40.996596
3509.939605	516789.553817	41.001600
3509.849399	516654.847351	41.006605
3509.819737	516564.430775	41.011610
3510.102788	516434.214951	41.016615
3509.697057	516322.060065	41.021620
3510.014789	516212.369274	41.026624
3509.670005	516101.821590	41.031629
3509.799768	515977.998594	41.036634
3509.432163	515873.875789	41.041639
3509.377678	515756.857111	41.046644
3509.310251	515647.425776	41.051648
3508.931696	515567.173755	41.056653
3509.184968	515440.950262	41.061658
3509.115655	515346.082772	41.066663
3508.844665	515247.099442	41.071668
3508.824073	515143.574721	41.076672
3508.573861	515070.684074	41.081677
3508.524330	514966.404193	41.086682
3508.252771	514874.297107	41.091687
3508.387793	514786.474854	41.096692
3508.440668	514704.178014	41.101696
3508.275701	514622.016355	41.106701
3508.322247	514522.422209	41.111706
3508.316425	514437.958508	41.116711
3508.033532	514338.668228	41.121716
3507.954696	514247.791695	41.126720
3507.850593	514167.995377	41.131725
3507.906866	514096.367099	41.136730
3507.941501	514010.074017	41.141735
3507.814365	513931.645852	41.146740
3507.733172	513852.249050	41.151744
3507.466093	513772.021396	41.156749
3507.172612	513704.594270	41.161754
3507.503780	513618.505215	41.166759
3507.267190	513548.387720	41.171764
3507.495376	513470.609376	41.176768
3507.085687	513418.879475	41.181773
3507.142524	513332.478252	41.186778
3507.065125	513272.956477	41.191783
3507.228075	513194.377871	41.196788
3507.052147	513125.665313	41.201792
3507.048772	513071.341042	41.206797
3506.932707	512992.906761	41.211802
3507.325279	512931.134472	41.216807
3507.060775	512866.936684	41.221812
3507.121066	512790.800386	41.226816
3506.878020	512728.571407	41.231821
3506.788699	512674.461777	41.236826
3506.762644	512602.941339	41.241831
3506.691773	512550.295310	41.246836
3506.653664	512491.978577	41.251840
3506.607874	512419.044141	41.256845
3506.688581	512348.669182	41.261850
3506.566531	512296.384542	41.266855
3506.433594	512250.475087	41.271860
3506.605453	512185.598735	41.276864
3506.417744	512113.545351	41.281869
3506.065564	512082.238488	41.286874
3506.475706	512017.880268	41.291879
3506.325796	511967.318907	41.296884
3506.341148	511908.030598	41.301888
3506.065740	511863.204904	41.306893
3505.949646	511806.011019	41.311898
3506.375950	511749.742931	41.316903
3506.276992	511713.083853	41.321908
3506.027116	511641.594736	41.326912
3505.975834	511595.012983	41.331917
3505.963264	511552.724827	41.336922
3506.406613	511492.456869	41.341927
3506.258188	511456.412094	41.346932
3506.173711	511388.639187	41.351936
3506.402252	511343.530125	41.356941
3505.857816	511299.858380	41.361946
3506.045505	511243.575746	41.366951
3506.008156	511201.189459	41.371956
3505.865955	511139.899877	41.376960
3505.721525	511107.293690	41.381965
3505.875945	511062.195598	41.386970
3505.600557	511014.180627	41.391975
3505.760756	510964.123738	41.396980
3505.932916	510921.248349	41.401984
3505.433456	510878.074295	41.406989
3505.423553	510841.551030	41.411994
3505.684623	510796.182436	41.416999
3505.564513	510760.890544	41.422004
3505.825766	510709.552218	41.427008
3505.439906	510668.231467	41.432013
3505.667135	510622.260692	41.437018
3506.023503	510593.823861	41.442023
3505.368384	510539.139198	41.447028
3505.893933	510492.867978	41.452032
3505.702316	510455.209048	41.457037
3505.348896	510417.879145	41.462042
3505.419684	510371.072395	41.467047
3505.222339	510336.398911	41.472052
3505.474739	510284.554808	41.477056
3505.379333	510246.627261	41.482061
3505.150655	510217.675188	41.487066
3505.480897	510184.536902	41.492071
3505.284570	510145.157957	41.497076
3505.484073	510099.443112	41.502080
3505.416061	510064.293319	41.507085
3505.021737	510025.046573	41.512090
3505.435390	509979.398743	41.517095
3504.895601	509948.623517	41.522100
3505.377840	509916.725469	41.527104
3505.699815	509889.152955	41.532109
3505.006639	509849.750675	41.537114
3504.776276	509822.720675	41.542119
3505.068601	509790.093535	41.547124
3505.353942	509749.069210	41.552128
3505.291243	509713.462531	41.557133
3505.322635	509691.551322	41.562138
3505.415373	509648.179376	41.567143
3505.269359	509617.341317	41.572148
3505.136485	509559.636635	41.577152
3504.877797	509542.627943	41.582157
3505.013550	509522.015423	41.587162
3505.283854	509462.020623	41.592167
3504.993111	509437.276225	41.597172
3505.122046	509401.689204	41.602176
3504.690146	509378.889557	41.607181
3504.901846	509347.589733	41.612186
3505.252080	509313.890085	41.617191
3504.808836	509276.015365	41.622196
3505.063346	509246.276978	41.627200
3505.093233	509217.788281	41.632205
3504.817021	509184.946290	41.637210
3505.189657	509167.280916	41.642215
3504.995994	509151.071054	41.647220
3504.828996	509084.971645	41.652224
3504.872687	509088.708709	41.657229
3505.042792	509034.394746	41.662234
3504.968084	508997.371853	41.667239
3504.675476	508993.168243	41.672244
3505.139388	508949.179335	41.677248
3504.801909	508913.007297	41.682253
3504.778098	508891.862706	41.687258
3505.040674	508854.330848	41.692263
3504.620518	508828.290571	41.697268
3504.735526	508807.478097	41.702272
3504.493993	508787.885624	41.707277
3505.113825	508733.499631	41.712282
3504.957381	508736.813051	41.717287
3505.037773	508676.086606	41.722292
3504.863739	508669.992164	41.727296
3505.107274	508632.209858	41.732301
3505.195189	508608.163342	41.737306
3505.161388	508573.055685	41.742311
3504.698338	508543.682473	41.747316
3504.828174	508496.608303	41.752320
3504.847343	508486.890985	41.757325
3504.754831	508452.804271	41.762330
3504.957980	508424.337472	41.767335
3504.935251	508380.677007	41.772340
3505.113166	508374.628026	41.777344
3504.815104	508321.751897	41.782349
3504.855739	508328.221790	41.787354
3505.077053	508255.783930	41.792359
3504.727489	508253.107024	41.797364
3504.808805	508220.712646	41.802368
3504.853105	508167.225374	41.807373
3504.781946	508170.373633	41.812378
3504.819897	508107.526845	41.817383
3504.769653	508124.535262	41.822388
3504.770506	508060.328060	41.827392
3504.743561	508062.912787	41.832397
3504.596493	507995.085759	41.837402
3505.047752	508001.895649	41.842407
3504.445066	507955.087571	41.847412
3504.585263	507940.392308	41.852416
3505.023485	507893.571336	41.857421
3504.694046	507869.893339	41.862426
3504.542242	507845.934248	41.867431
3504.452822	507817.917470	41.872436
3504.680476	507803.562450	41.877440
3504.963080	507774.272464	41.882445
3504.800553	507753.907365	41.887450
3505.027303	507721.944444	41.892455
3504.559480	507697.276129	41.897460
3504.861392	507666.566171	41.902464
3504.945366	507640.899801	41.907469
3504.549782	507603.570445	41.912474
3504.801652	507571.502081	41.917479
3504.543268	507550.241126	41.922484
3504.926173	507522.705798	41.927488
3504.641647	507492.341211	41.932493
3504.653899	507462.739239	41.937498
3504.821254	507443.586597	41.942503
3504.611226	507428.136678	41.947508
3504.845741	507390.100090	41.952512
3504.632655	507369.793128	41.957517
3504.690807	507344.029202	41.962522
3504.825007	507320.074777	41.967527
3504.905806	507287.830531	41.972532
3504.587274	507252.056806	41.977536
3504.732965	507225.874076	41.982541
3504.646570	507201.498961	41.987546
3504.578449	507183.597631	41.992551
3504.592087	507151.262547	41.997556
3504.827422	507125.267894	42.002560
3504.589851	507106.634275	42.007565
3504.632485	507075.913652	42.012570
3504.485626	507052.053879	42.017575
3504.351178	507025.206727	42.022580
3504.488286	507017.089134	42.027584
3504.388060	506978.244354	42.032589
3504.229160	506963.140137	42.037594
3504.904164	506940.921311	42.042599
3504.735608	506920.201984	42.047604
3504.486711	506888.363305	42.052608
3504.363404	506862.981545	42.057613
3504.180687	506852.333814	42.062618
3504.666796	506817.089818	42.067623
3504.661714	506809.956009	42.072628
3504.852501	506769.850359	42.077632
3504.571154	506763.772204	42.082637
3504.692040	506726.460529	42.087642
3504.974009	506690.540134	42.092647
3504.719319	506683.293921	42.097652
3504.352599	506633.864334	42.102656
3504.891075	506617.333971	42.107661
3504.776687	506594.885263	42.112666
3504.648084	506562.976374	42.117671
3504.612468	506543.905422	42.122676
3504.470018	506507.039706	42.127680
3504.631410	506486.166509	42.132685
3504.296446	506460.109196	42.137690
3504.520891	506439.225977	42.142695
3504.794109	506414.033897	42.147700
3504.690144	506397.301256	42.152704
3504.567086	506354.461166	42.157709
3504.255042	506364.529653	42.162714
3504.697321	506304.597923	42.167719
3504.594846	506311.546605	42.172724
3504.654050	506283.554460	42.177728
3504.545006	506240.357661	42.182733
3504.272679	506233.265853	42.187738
3504.630947	506208.262442	42.192743
3504.354092	506184.624432	42.197748
3504.505061	506147.913988	42.202752
3504.748582	506137.350256	42.207757
3504.237890	506123.869582	42.212762
3504.314881	506074.621288	42.217767
3504.232147	506068.106677	42.222772
3504.560434	506060.059626	42.227776
3504.838913	506033.854115	42.232781
3503.995386	506016.681369	42.237786
3504.638868	505980.854181	42.242791
3504.564534	505960.979065	42.247796
3504.315507	505940.726715	42.252800
3504.245984	505907.238596	42.257805
3504.482054	505891.514388	42.262810
3504.929448	505866.850622	42.267815
3504.364222	505861.980889	42.272820
3504.688130	505809.960253	42.277824
3504.575782	505800.869455	42.282829
3504.308867	505786.843957	42.287834
3504.602144	505753.399407	42.292839
3504.386655	505716.492958	42.297844
3503.907835	505723.045925	42.302848
3503.957085	505698.748471	42.307853
3504.192353	505679.178326	42.312858
3503.882347	505667.183687	42.317863
3503.831815	505643.509171	42.322868
3503.891389	505644.056433	42.327872
3504.294553	505624.409086	42.332877
3504.088101	505595.951787	42.337882
3503.975922	505601.789000	42.342887
3503.988276	505578.357476	42.347892
3504.094800	505547.624057	42.352896
3504.317759	505535.949924	42.357901
3504.026610	505539.032221	42.362906
3504.458169	505516.850063	42.367911
3504.030490	505492.728910	42.372916
3504.107267	505469.742496	42.377920
3504.253126	505461.015545	42.382925
3503.915760	505432.275045	42.387930
3504.152499	505420.598656	42.392935
3504.321291	505413.183771	42.397940
3504.095097	505385.538920	42.402944
3504.176568	505372.520719	42.407949
3503.939703	505365.473556	42.412954
3504.291472	505337.028816	42.417959
3504.273295	505338.347445	42.422964
3504.122747	505292.877651	42.427968
3504.520850	505284.060139	42.432973
3504.038272	505272.902181	42.437978
3504.276112	505245.639210	42.442983
3504.330324	505225.844150	42.447988
3504.669517	505212.026022	42.452992
3504.380337	505181.759343	42.457997
3504.183775	505159.827825	42.463002
3504.886886	505133.604455	42.468007
3504.471568	505117.324638	42.473012
3504.335719	505091.335016	42.478016
3504.449659	505063.281658	42.483021
3504.287187	505044.735172	42.488026
3504.584323	505023.788168	42.493031
3504.423120	505012.174404	42.498036
3504.656351	504988.099911	42.503040
3504.509362	504969.500292	42.508045
3504.409158	504942.644518	42.513050
3504.834803	504904.116846	42.518055
3504.400394	504883.234692	42.523060
3504.477539	504862.221053	42.528064
3504.396610	504842.851768	42.533069
3504.039285	504824.740694	42.538074
3504.298755	504805.823627	42.543079
3504.187026	504777.451236	42.548084
3504.276163	504755.980119	42.553088
3504.010169	504746.255175	42.558093
3503.907761	504730.330391	42.563098
3504.118209	504709.143681	42.568103
3504.230312	504691.464338	42.573108
3504.387813	504679.648161	42.578112
3504.437415	504665.571735	42.583117
3504.471767	504641.072741	42.588122
3504.513235	504618.445036	42.593127
3504.293240	504592.164333	42.598132
3503.997482	504575.662686	42.603136
3504.298174	504544.896820	42.608141
3504.095850	504533.592879	42.613146
3504.388559	504506.067051	42.618151
3504.083398	504496.854229	42.623156
3504.379831	504480.764966	42.628160
3504.376302	504468.113778	42.633165
3504.312493	504453.802071	42.638170
3504.221543	504415.456191	42.643175
3504.220753	504402.450271	42.648180
3504.391232	504369.073096	42.653184
3504.500045	504359.541734	42.658189
3503.948754	504331.035665	42.663194
3504.004686	504305.470034	42.668199
3504.409770	504305.051792	42.673204
3504.365720	504279.147671	42.678208
3504.189353	504269.003433	42.683213
3504.306066	504250.665018	42.688218
3504.268264	504226.682928	42.693223
3503.872241	504212.170492	42.698228
3503.967792	504201.224119	42.703232
3504.211345	504186.813007	42.708237
3503.955824	504161.853080	42.713242
3504.296519	504144.491314	42.718247
3504.455757	504136.368887	42.723252
3504.151431	504119.564517	42.728256
3504.322962	504091.551112	42.733261
3504.108163	504080.805541	42.738266
3504.385655	504052.927152	42.743271
3504.167431	504027.758706	42.748276
3504.076231	504013.197927	42.753280
3504.390402	504000.597405	42.758285
3504.150532	503976.596303	42.763290
3504.198815	503958.825093	42.768295
3504.131867	503958.127190	42.773300
3504.210097	503925.978361	42.778304
3504.401271	503902.364507	42.783309
3504.418771	503883.788347	42.788314
3504.421238	503851.297094	42.793319
3503.936442	503841.606229	42.798324
3504.298199	503809.412375	42.803329
3504.363084	503794.320655	42.808333
3504.148485	503799.719171	42.813338
3504.306020	503757.486292	42.818343
3504.445031	503752.808311	42.823348
3504.228027	503717.567993	42.828353
3504.669506	503685.411922	42.833357
3504.246174	503696.461103	42.838362
3504.393370	503636.364452	42.843367
3503.966115	503650.197807	42.848372
3504.066527	503599.623008	42.853377
3503.749475	503612.224344	42.858381
3504.094595	503602.705833	42.863386
3503.921052	503574.999195	42.868391
3504.116484	503586.051867	42.873396
3503.778654	503576.995552	42.878401
3504.107941	503534.532554	42.883405
3503.897718	503539.626799	42.888410
3503.944849	503501.459542	42.893415
3503.710392	503511.011299	42.898420
3503.849720	503481.180056	42.903425
3504.108454	503495.006330	42.908429
3504.084667	503433.974424	42.913434
3504.080236	503459.381424	42.918439
3504.313483	503419.463830	42.923444
3504.113717	503409.980727	42.928449
3504.379316	503403.916170	42.933453
3503.703896	503377.503190	42.938458
3504.212634	503352.876813	42.943463
3503.977291	503353.015267	42.948468
3503.870275	503331.421583	42.953473
3504.178215	503317.505689	42.958477
3504.086113	503313.167782	42.963482
3504.235597	503279.336366	42.968487
3504.187022	503278.635532	42.973492
3504.213659	503251.908958	42.978497
3504.284925	503234.740714	42.983501
3503.937408	503234.036516	42.988506
3504.185704	503202.314984	42.993511
3504.040105	503180.980268	42.998516
3504.061914	503172.322400	43.003521
3504.337819	503150.010030	43.008525
3503.955545	503134.279867	43.013530
3503.917711	503102.755213	43.018535
3504.022147	503102.384465	43.023540
3503.762002	503096.453511	43.028545
3504.192055	503052.505705	43.033549
3504.026512	503047.470784	43.038554
3504.165255	503054.585074	43.043559
3503.915750	503028.104251	43.048564
3504.092075	503003.580539	43.053569
3504.135948	503006.407877	43.058573
3504.206146	502973.145131	43.063578
3504.234352	502963.018417	43.068583
3504.241832	502929.259387	43.073588
3504.028453	502934.708586	43.078593
3504.483093	502891.465056	43.083597
3504.058092	502922.759643	43.088602
3504.013811	502882.024303	43.093607
3503.774896	502844.558788	43.098612
3503.923644	502847.268351	43.103617
3504.090063	502844.711494	43.108621
3503.772948	502796.680365	43.113626
3504.072118	502799.214326	43.118631
3504.107457	502787.770474	43.123636
3503.978611	502758.132233	43.128641
3504.024405	502765.008270	43.133645
3503.954368	502734.196617	43.138650
3504.225011	502729.345725	43.143655
3504.182384	502688.002330	43.148660
3504.126876	502714.886229	43.153665
3503.980128	502645.317572	43.158669
3504.022580	502669.908499	43.163674
3504.060359	502611.748922	43.168679
3503.843807	502633.394700	43.173684
3504.308734	502594.805163	43.178689
3503.951614	502602.959645	43.183693
3503.649833	502555.735238	43.188698
3504.024864	502578.704735	43.193703
3503.886431	502556.001592	43.198708
3503.941514	502510.846392	43.203713
3504.096590	502538.760143	43.208717
3504.269975	502511.098226	43.213722
3503.844294	502485.859142	43.218727
3504.446079	502482.828519	43.223732
3504.113231	502440.923064	43.228737
3503.844717	502453.365713	43.233741
3504.006059	502438.257588	43.238746
3503.993180	502399.287628	43.243751
3504.135767	502358.825226	43.248756
3503.981330	502394.531943	43.253761
3504.225668	502356.786562	43.258765
3503.957607	502343.871980	43.263770
3503.960560	502328.991250	43.268775
3503.996985	502307.677323	43.273780
3504.020382	502287.124631	43.278785
3503.890682	502303.695742	43.283789
3504.015530	502276.192971	43.288794
3504.123759	502252.994932	43.293799
3504.179176	502223.782195	43.298804
3503.825080	502225.457832	43.303809
3504.261027	502212.431883	43.308813
3504.108179	502195.753576	43.313818
3504.188380	502193.513934	43.318823
3504.079344	502174.348612	43.323828
3503.892710	502136.114128	43.328833
3503.841312	502137.792544	43.333837
3503.880409	502122.551631	43.338842
3503.483408	502097.509915	43.343847
3503.740286	502090.737694	43.348852
3503.579088	502089.244790	43.353857
3503.899836	502081.855103	43.358861
3503.910607	502062.721338	43.363866
3504.182502	502047.747250	43.368871
3503.803821	502044.922135	43.373876
3503.666456	502043.374846	43.378881
3503.869689	502009.076981	43.383885
3503.526551	502008.068353	43.388890
3503.654404	502002.581847	43.393895
3504.123387	501997.699407	43.398900
3503.952318	501973.836548	43.403905
3504.231330	501950.611122	43.408909
3503.998745	501945.940782	43.413914
3504.047947	501928.673530	43.418919
3504.128700	501917.373782	43.423924
3504.216819	501891.748956	43.428929
3504.303803	501876.702721	43.433933
3503.762606	501883.520033	43.438938
3504.360768	501848.653293	43.443943
3504.073251	501815.242453	43.448948
3504.027816	501821.171595	43.453953
3504.142510	501791.341400	43.458957
3503.719184	501788.472685	43.463962
3503.682535	501777.292634	43.468967
3504.105271	501744.427395	43.473972
3503.726458	501729.150967	43.478977
3504.206463	501732.871261	43.483981
3503.806122	501706.564146	43.488986
3503.792774	501687.281943	43.493991
3504.051207	501673.726892	43.498996
3503.855485	501668.240810	43.504001
3503.833252	501642.177529	43.509005
3503.857116	501638.630726	43.514010
3503.963290	501624.239243	43.519015
3503.948004	501615.485247	43.524020
3503.689465	501599.531698	43.529025
3504.090202	501589.244089	43.534029
3503.860641	501578.094403	43.539034
3504.285128	501569.777030	43.544039
3504.411029	501547.638202	43.549044
3503.953131	501526.300236	43.554049
3503.727728	501523.400195	43.559053
3504.006504	501510.651653	43.564058
3503.616802	501495.427360	43.569063
3503.549222	501480.506451	43.574068
3503.759701	501469.388378	43.579073
3504.034836	501458.361310	43.584077
3503.852709	501457.580280	43.589082
3504.153517	501433.591497	43.594087
3504.167311	501416.835503	43.599092
3503.822754	501412.283951	43.604097
3503.944045	501381.945868	43.609101
3503.837346	501387.074982	43.614106
3503.924313	501360.032324	43.619111
3503.677435	501327.677081	43.624116
3503.683843	501342.354779	43.629121
3503.869303	501328.659151	43.634125
3503.799502	501305.083085	43.639130
3503.850424	501294.698748	43.644135
3504.023355	501302.516966	43.649140
3503.870226	501283.104569	43.654145
3503.948341	501260.618623	43.659149
3503.880826	501253.188728	43.664154
3504.021057	501237.171826	43.669159
3503.643632	501211.568985	43.674164
3503.506686	501213.817791	43.679169
3503.997714	501203.363840	43.684173
3503.418843	501186.296370	43.689178
3503.476396	501176.619548	43.694183
3503.531978	501166.133166	43.699188
3503.698163	501152.541683	43.704193
3503.531286	501152.061928	43.709197
3503.354036	501159.075075	43.714202
3503.759782	501152.582669	43.719207
3503.945076	501126.485832	43.724212
3503.808613	501128.633339	43.729217
3503.805855	501109.753770	43.734221
3503.830571	501106.814128	43.739226
3503.793557	501082.270865	43.744231
3503.375360	501083.653037	43.749236
3503.581831	501074.813109	43.754241
3503.914820	501073.545710	43.759245
3503.878423	501060.087409	43.764250
3503.840924	501041.972513	43.769255
3503.763957	501031.152683	43.774260
3503.581431	501020.855701	43.779265
3503.601239	500996.252723	43.784269
3503.676980	500991.280313	43.789274
3503.655030	500979.338180	43.794279
3503.869133	500981.075976	43.799284
3503.823081	500969.593200	43.804289
3503.704175	500955.894775	43.809293
3503.818900	500944.993979	43.814298
3503.783370	500942.873707	43.819303
3503.862236	500926.208201	43.824308
3503.722135	500911.095808	43.829313
3504.136484	500892.200701	43.834317
3503.671120	500887.870577	43.839322
3503.742137	500864.119818	43.844327
3503.747328	500859.765932	43.849332
3503.799569	500853.076205	43.854337
3503.760816	500847.615677	43.859341
3503.477528	500818.555400	43.864346
3503.759191	500815.980039	43.869351
3503.849948	500807.866914	43.874356
3503.662560	500813.160799	43.879361
3503.708724	500792.906487	43.884365
3503.497954	500786.815099	43.889370
3503.421489	500773.970327	43.894375
3503.536596	500777.039850	43.899380
3503.534404	500776.280967	43.904385
3504.102881	500762.979927	43.909389
3503.718624	500750.892435	43.914394
3503.644983	500729.340925	43.919399
3503.848546	500724.905034	43.924404
3503.769875	500717.932240	43.929409
3504.069681	500687.868468	43.934413
3503.860530	500688.812685	43.939418
3503.587093	500685.312682	43.944423
3503.692434	500659.531507	43.949428
3503.432227	500646.108268	43.954433
3503.749534	500633.808574	43.959437
3503.750246	500642.565428	43.964442
3503.662673	500634.531029	43.969447
3503.806193	500621.752614	43.974452
3503.640604	500609.832936	43.979457
3503.979340	500598.592813	43.984461
3503.492983	500595.075827	43.989466
3503.805413	500581.308940	43.994471
3503.922780	500548.692239	43.999476
3503.636046	500559.013116	44.004481
3504.196175	500522.934960	44.009485
3503.537279	500546.779162	44.014490
3503.676809	500519.170120	44.019495
3503.920894	500505.211503	44.024500
3503.797424	500524.364827	44.029505
3503.848835	500483.507626	44.034509
3503.665425	500470.122735	44.039514
3503.819182	500467.770015	44.044519
3503.861150	500467.155995	44.049524
3503.585245	500439.561872	44.054529
3503.768133	500425.967197	44.059533
3503.972129	500434.793260	44.064538
3503.472161	500418.370624	44.069543
3503.825012	500395.232740	44.074548
3503.886271	500396.387326	44.079553
3503.738405	500372.164320	44.084557
3503.557179	500392.794860	44.089562
3503.517430	500345.826879	44.094567
3503.480029	500349.072437	44.099572
3503.631383	500328.851593	44.104577
3503.851182	500318.794329	44.109581
3503.419055	500334.959500	44.114586
3503.406676	500320.535085	44.119591
3503.761047	500294.460928	44.124596
3503.913887	500282.743799	44.129601
3503.837820	500283.211430	44.134605
3503.174005	500270.864082	44.139610
3503.445776	500289.600853	44.144615
3503.667080	500260.814249	44.149620
3503.262884	500249.843189	44.154625
3503.487291	500249.250945	44.159629
3503.653458	500241.378741	44.164634
3503.571012	500236.329885	44.169639
3503.764536	500243.942837	44.174644
3503.661162	500240.871440	44.179649
3503.607799	500202.510499	44.184653
3503.516084	500194.425937	44.189658
3503.421179	500188.012314	44.194663
3503.782243	500190.385012	44.199668
3503.506953	500190.327321	44.204673
3503.739448	500157.236134	44.209677
3503.601584	500157.713536	44.214682
3503.774598	500159.711005	44.219687
3503.683299	500161.750249	44.224692
3503.666695	500140.442111	44.229697
3503.642962	500112.858246	44.234701
3503.722861	500113.604948	44.239706
3503.651838	500115.286656	44.244711
3504.102145	500107.065765	44.249716
3503.733040	500087.838062	44.254721
3504.000341	500075.394031	44.259725
3503.720073	500070.224536	44.264730
3503.610256	500044.020904	44.269735
3503.667008	500030.496484	44.274740
3503.497058	500030.877720	44.279745
3503.575555	500028.688698	44.284749
3503.705576	500036.362395	44.289754
3503.576082	500019.728976	44.294759
3503.676446	499992.631511	44.299764
3503.557337	500000.749559	44.304769
3503.618498	499984.339073	44.309773
3503.778116	499990.185794	44.314778
3503.758740	499976.875846	44.319783
3503.940444	499945.462756	44.324788
3503.753559	499943.670008	44.329793
3503.642067	499942.776505	44.334797
3503.789864	499926.048552	44.339802
3503.737385	499899.633165	44.344807
3503.779254	499897.905498	44.349812
3503.633170	499908.305759	44.354817
3503.869022	499880.882990	44.359821
3503.571704	499864.225332	44.364826
3503.563582	499869.288680	44.369831
3503.768634	499851.842925	44.374836
3503.348319	499849.479618	44.379841
3503.558729	499847.320344	44.384845
3503.703169	499823.657839	44.389850
3503.927879	499812.485868	44.394855
3503.814617	499811.744499	44.399860
3503.498239	499810.680891	44.404865
3503.611329	499789.604938	44.409869
3503.663690	499764.387673	44.414874
3503.658405	499780.334017	44.419879
3503.686230	499763.827357	44.424884
3503.801054	499760.367046	44.429889
3503.510283	499748.972785	44.434893
3503.735511	499730.055725	44.439898
3503.613429	499738.883051	44.444903
3503.861855	499728.466588	44.449908
3503.696368	499710.066847	44.454913
3503.722525	499679.639670	44.459917
3503.645839	499685.473218	44.464922
3503.406976	499692.851021	44.469927
3503.738045	499676.144490	44.474932
3503.469021	499662.165075	44.479937
3503.612309	499639.616168	44.484941
3503.733344	499649.518772	44.489946
3503.580201	499626.966081	44.494951
3503.773474	499627.998610	44.499956
3503.387282	499623.908767	44.504961
3503.409428	499605.884230	44.509965
3503.545085	499572.756651	44.514970
3503.478869	499597.520858	44.519975
3503.522212	499566.989531	44.524980
3503.480746	499606.126208	44.529985
3503.739748	499577.788139	44.534989
3503.287083	499566.874940	44.539994
3503.511508	499550.438252	44.544999
3503.681600	499546.108605	44.550004
3503.488301	499548.973979	44.555009
3503.582281	499539.138650	44.560013
3503.775555	499540.171184	44.565018
3503.926774	499531.541713	44.570023
3503.911373	499512.206865	44.575028
3503.961513	499488.457581	44.580033
3503.471753	499476.183414	44.585037
3503.511952	499469.393830	44.590042
3503.750339	499464.699018	44.595047
3503.870541	499456.884357	44.600052
3503.703245	499472.856580	44.605057
3503.706873	499427.853570	44.610061
3503.713484	499421.980465	44.615066
3503.504468	499422.722238	44.620071
3503.815143	499413.510671	44.625076
3503.668393	499413.533902	44.630081
3503.698325	499382.447544	44.635085
3503.672382	499382.249194	44.640090
3503.682916	499387.512216	44.645095
3503.772222	499368.312529	44.650100
3503.574497	499367.128896	44.655105
3503.763148	499346.698563	44.660109
3503.783391	499325.231767	44.665114
3503.799988	499329.532033	44.670119
3503.962230	499323.178701	44.675124
3503.466307	499308.222435	44.680129
3503.819023	499287.816726	44.685133
3503.723882	499294.412647	44.690138
3503.701649	499283.532487	44.695143
3503.903464	499246.951559	44.700148
3503.703770	499239.896073	44.705153
3503.648163	499244.157150	44.710157
3503.472951	499253.144977	44.715162
3503.759078	499221.663494	44.720167
3503.936787	499212.118485	44.725172
3503.793480	499200.599324	44.730177
3503.633252	499198.903531	44.735181
3503.865328	499180.997255	44.740186
3503.941102	499174.708159	44.745191
3504.093326	499150.638560	44.750196
3503.789926	499153.318910	44.755201
3503.644969	499128.486295	44.760205
3503.810483	499127.295857	44.765210
3504.022434	499106.355345	44.770215
3503.892140	499080.811633	44.775220
3503.396734	499075.827720	44.780225
3503.825176	499064.673706	44.785229
3503.934886	499075.287133	44.790234
3503.555463	499055.249991	44.795239
3503.776448	499036.434117	44.800244
3503.822811	499025.998563	44.805249
3503.613831	499019.096325	44.810253
3503.553796	499031.964004	44.815258
3503.602573	498979.916189	44.820263
3503.779275	498989.607868	44.825268
3504.079595	498980.903944	44.830273
3504.079597	498949.619078	44.835277
3503.816849	498955.229157	44.840282
3503.732821	498934.233980	44.845287
3503.930387	498928.128040	44.850292
3503.660800	498894.759525	44.855297
3503.842764	498903.437958	44.860301
3503.828983	498892.404356	44.865306
3503.504006	498884.761055	44.870311
3503.645622	498871.070481	44.875316
3503.159371	498861.073375	44.880321
3503.633544	498842.622266	44.885325
3503.505584	498843.908106	44.890330
3503.113063	498844.982645	44.895335
3503.654826	498841.150939	44.900340
3503.488985	498846.695112	44.905345
3503.637163	498842.672499	44.910349
3503.887700	498799.957558	44.915354
3503.672318	498814.773629	44.920359
3504.022111	498796.898989	44.925364
3503.322271	498791.694192	44.930369
3503.541684	498784.116674	44.935373
3503.786720	498770.612171	44.940378
3503.584421	498763.708779	44.945383
3503.542797	498755.008169	44.950388
3503.950224	498756.715629	44.955393
3503.771731	498721.965563	44.960397
3503.696687	498710.131557	44.965402
3503.712502	498697.270710	44.970407
3503.859591	498709.447776	44.975412
3504.010778	498692.009410	44.980417
3504.036316	498670.743491	44.985421
3503.873333	498667.529373	44.990426
3503.828886	498657.411701	44.995431
3503.990849	498628.075000	45.000436
3503.557575	498623.840497	45.005441
3503.684003	498635.059026	45.010445
3503.418946	498589.134534	45.015450
3503.474541	498600.769271	45.020455
3504.014770	498586.610487	45.025460
3503.881164	498593.921479	45.030465
3503.854074	498566.993881	45.035469
3503.853205	498552.211858	45.040474
3503.587754	498548.001436	45.045479
3503.732562	498527.577104	45.050484
3503.630256	498530.478881	45.055489
3503.600507	498524.661853	45.060493
3503.634781	498499.648170	45.065498
3503.734390	498492.038842	45.070503
3503.933175	498489.779997	45.075508
3503.639162	498492.155214	45.080513
3503.630098	498449.936093	45.085517
3503.938548	498452.317342	45.090522
3503.616645	498447.609575	45.095527
3503.842808	498428.539128	45.100532
3503.885663	498420.888116	45.105537
3503.596462	498417.238284	45.110541
3503.659278	498404.015429	45.115546
3503.639715	498404.271680	45.120551
3503.818631	498372.653787	45.125556
3503.776871	498374.280407	45.130561
3503.795960	498358.988826	45.135565
3503.715287	498351.256060	45.140570
3503.772006	498335.249768	45.145575
3503.840967	498327.898338	45.150580
3503.671636	498330.506993	45.155585
3503.904680	498314.928435	45.160589
3503.894295	498276.607215	45.165594
3503.347548	498276.035546	45.170599
3503.762674	498274.299352	45.175604
3503.677736	498292.638967	45.180609
3503.887601	498259.041620	45.185613
3503.872486	498237.376616	45.190618
3503.667144	498246.470956	45.195623
3503.763334	498218.105858	45.200628
3503.488147	498214.099395	45.205633
3503.725438	498174.371938	45.210637
3503.840759	498187.870628	45.215642
3503.859579	498183.108938	45.220647
3504.109579	498155.124431	45.225652
3503.548603	498145.746237	45.230657
3503.566299	498159.766629	45.235661
3503.809634	498131.125011	45.240666
3503.458921	498125.156084	45.245671
3503.673841	498117.427123	45.250676
3503.778012	498098.476859	45.255681
3503.584701	498085.547380	45.260685
3503.580650	498105.950037	45.265690
3503.609660	498090.808537	45.270695
3503.820074	498070.930198	45.275700
3503.553055	498062.771132	45.280705
3503.614235	498041.903841	45.285709
3503.646667	498039.924360	45.290714
3503.368021	498045.587858	45.295719
3503.727004	498006.195176	45.300724
3503.320106	497996.792551	45.305729
3503.181925	497999.649457	45.310733
3503.363192	497981.547520	45.315738
3503.121336	498005.481041	45.320743
3503.579856	497993.663483	45.325748
3503.614824	498000.492440	45.330753
3503.552473	497993.465381	45.335757
3503.516056	498000.913128	45.340762
3503.395203	497971.822564	45.345767
3503.729844	497958.556420	45.350772
3503.612022	497966.624555	45.355777
3503.623960	497962.167648	45.360781
3503.911482	497966.526670	45.365786
3503.472424	497922.349253	45.370791
3503.834417	497934.695378	45.375796
3503.696788	497932.287133	45.380801
3503.846922	497920.872650	45.385805
3503.880796	497892.668767	45.390810
3503.590745	497884.614513	45.395815
3503.523852	497874.348071	45.400820
3503.784031	497879.015191	45.405825
3503.979361	497866.176005	45.410829
3504.058043	497854.215888	45.415834
3503.678172	497831.696783	45.420839
3503.916256	497831.254181	45.425844
3503.886243	497809.388515	45.430849
3503.815241	497800.287080	45.435853
3503.784871	497806.164542	45.440858
3503.765862	497793.561686	45.445863
3503.855491	497756.792965	45.450868
3503.335232	497764.165404	45.455873
3503.608674	497761.388407	45.460877
3503.994927	497740.773146	45.465882
3503.346270	497721.283335	45.470887
3503.392044	497728.819455	45.475892
3503.323232	497709.440488	45.480897
3503.659693	497697.844535	45.485901
3503.715908	497699.050720	45.490906
3503.940930	497701.951519	45.495911
3503.620589	497666.411819	45.500916
3503.366210	497675.159810	45.505921
3503.995226	497658.049936	45.510925
3503.713175	497654.955710	45.515930
3503.389152	497650.298695	45.520935
3503.706644	497624.429013	45.525940
3503.842329	497614.029151	45.530945
3503.658283	497620.589108	45.535949
3503.934450	497610.521427	45.540954
3503.415802	497592.681607	45.545959
3503.792616	497579.408520	45.550964
3503.592285	497584.705396	45.555969
3503.674978	497566.669251	45.560973
3503.847806	497567.046985	45.565978
3503.343188	497546.926698	45.570983
3503.791407	497519.719908	45.575988
3503.312818	497536.704955	45.580993
3503.245690	497528.058412	45.585997
3503.766692	497518.356997	45.591002
3503.462558	497527.214178	45.596007
3503.596359	497506.385418	45.601012
3503.343557	497491.237332	45.606017
3503.321941	497486.380597	45.611021
3503.766162	497479.779542	45.616026
3503.347486	497486.326005	45.621031
3503.818800	497475.366746	45.626036
3503.858082	497463.007582	45.631041
3503.889281	497446.447641	45.636045
3503.695153	497431.593993	45.641050
3503.279382	497442.595199	45.646055
3503.900011	497433.131127	45.651060
3503.663632	497396.261320	45.656065
3503.927786	497402.497380	45.661069
3504.155306	497371.882601	45.666074
3503.650932	497374.797484	45.671079
3503.363138	497363.958139	45.676084
3503.897973	497338.357461	45.681089
3503.353663	497350.543468	45.686093
3503.990958	497348.721447	45.691098
3503.410800	497317.171058	45.696103
3503.596389	497315.926703	45.701108
3503.678828	497309.028376	45.706113
3503.496696	497281.060191	45.711117
3503.736577	497300.665788	45.716122
3503.691094	497297.179716	45.721127
3503.195687	497253.617101	45.726132
3503.435139	497252.364228	45.731137
3503.401630	497252.875837	45.736141
3503.803434	497224.511505	45.741146
3503.440238	497246.946375	45.746151
3503.870131	497232.955860	45.751156
3503.516985	497210.431756	45.756161
3503.764477	497191.306008	45.761165
3503.563194	497198.678886	45.766170
3503.341986	497209.041948	45.771175
3503.417717	497179.412762	45.776180
3503.803995	497185.325827	45.781185
3503.804144	497173.428301	45.786189
3503.390818	497163.013700	45.791194
3503.675971	497146.919625	45.796199
3503.649430	497138.772760	45.801204
3503.626955	497161.153883	45.806209
3503.229355	497117.423598	45.811213
3503.928684	497105.111751	45.816218
3504.035757	497102.006553	45.821223
3503.734014	497102.813702	45.826228
3503.749530	497085.344605	45.831233
3503.669334	497046.525534	45.836237
3503.457490	497076.227151	45.841242
3503.615772	497070.177423	45.846247
3503.728882	497039.580167	45.851252
3503.769163	497038.358759	45.856257
3503.817217	497014.606552	45.861261
3503.883909	496998.040591	45.866266
3503.632798	497027.140954	45.871271
3503.479019	496966.968210	45.876276
3503.749664	496988.037506	45.881281
3503.635423	496970.436922	45.886285
3503.636442	496955.957067	45.891290
3503.607357	496963.049682	45.896295
3503.638392	496939.148180	45.901300
3503.815283	496922.615361	45.906305
3503.927085	496914.244016	45.911309
3503.711470	496929.416065	45.916314
3503.434937	496907.841418	45.921319
3503.328950	496877.734176	45.926324
3503.588794	496880.376461	45.931329
3503.620340	496881.637228	45.936333
3503.545780	496872.232117	45.941338
3503.285723	496883.259677	45.946343
3503.768624	496880.044411	45.951348
3503.528558	496838.009928	45.956353
3503.196048	496847.479469	45.961357
3503.852286	496830.870804	45.966362
3503.441144	496834.226695	45.971367
3503.545493	496837.146707	45.976372
3503.299356	496823.920903	45.981377
3503.370140	496803.050668	45.986381
3503.499178	496793.866481	45.991386
3503.404372	496796.159802	45.996391
3503.363181	496795.660059	46.001396
3503.381200	496788.316057	46.006401
3503.269342	496790.510816	46.011405
3503.531315	496769.053406	46.016410
3503.431797	496779.751880	46.021415
3503.458481	496782.684177	46.026420
3503.449883	496756.206623	46.031425
3503.441980	496752.714507	46.036429
3503.724392	496743.303537	46.041434
3503.363424	496745.284529	46.046439
3503.480787	496736.709707	46.051444
3503.622332	496737.041775	46.056449
3503.566930	496728.342368	46.061453
3503.836637	496702.124522	46.066458
3503.440796	496698.744341	46.071463
3503.496426	496697.672372	46.076468
3503.478571	496686.486181	46.081473
3503.650631	496684.231338	46.086477
3503.652701	496672.586326	46.091482
3503.048740	496663.821704	46.096487
3503.420457	496655.105382	46.101492
3503.640117	496654.108744	46.106497
3503.317283	496647.021075	46.111501
3503.439353	496646.495524	46.116506
3503.216176	496649.720481	46.121511
3503.720191	496634.755835	46.126516
3503.480595	496641.983106	46.131521
3503.661664	496617.854950	46.136525
3503.593708	496588.956324	46.141530
3503.245928	496613.971639	46.146535
3503.519573	496598.233304	46.151540
3503.459309	496596.268317	46.156545
3503.068389	496618.961490	46.161549
3503.276413	496597.006110	46.166554
3503.407947	496619.464816	46.171559
3503.582438	496587.591364	46.176564
3503.501016	496570.238352	46.181569
3503.384021	496549.853172	46.186573
3503.599651	496565.716807	46.191578
3503.570955	496556.405542	46.196583
3503.478484	496572.874793	46.201588
3503.648797	496548.596358	46.206593
3503.574552	496549.468831	46.211597
3503.768961	496542.451257	46.216602
3503.729999	496515.168078	46.221607
3503.843716	496523.504035	46.226612
3503.925413	496481.671019	46.231617
3503.754893	496499.367787	46.236621
3504.130913	496459.462760	46.241626
3503.350149	496488.951477	46.246631
3503.284819	496449.116185	46.251636
3503.862304	496439.860940	46.256641
3503.264686	496444.258973	46.261645
3503.968889	496434.679918	46.266650
3503.556482	496427.302541	46.271655
3503.256325	496432.666159	46.276660
3503.574318	496402.237968	46.281665
3503.282488	496381.070152	46.286669
3503.483522	496389.949300	46.291674
3503.606477	496391.246283	46.296679
3503.672366	496375.895003	46.301684
3503.416279	496404.946517	46.306689
3503.657647	496364.100594	46.311693
3503.715580	496369.660783	46.316698
3503.812220	496347.570818	46.321703
3503.913149	496336.061856	46.326708
3503.692391	496348.906214	46.331713
3503.553518	496321.182864	46.336717
3504.032685	496294.526284	46.341722
3503.751301	496298.013654	46.346727
3503.371743	496304.756877	46.351732
3503.580056	496271.611769	46.356737
3503.507603	496255.219016	46.361741
3503.532320	496249.747062	46.366746
3503.488389	496249.602150	46.371751
3503.484872	496267.930942	46.376756
3503.557345	496242.604326	46.381761
3503.600885	496234.547240	46.386765
3503.910111	496201.588577	46.391770
3503.787014	496199.937261	46.396775
3503.500050	496211.880829	46.401780
3503.625276	496212.266117	46.406785
3503.562744	496199.820925	46.411789
3503.553793	496180.835910	46.416794
3503.403209	496165.164254	46.421799
3503.702303	496164.003142	46.426804
3503.766919	496164.499272	46.431809
3503.433533	496145.565499	46.436813
3503.557279	496127.318915	46.441818
3503.671583	496127.807193	46.446823
3503.454205	496119.082465	46.451828
3503.709840	496120.510389	46.456833
3503.219417	496123.170108	46.461837
3503.812051	496109.304903	46.466842
3503.412559	496090.584044	46.471847
3503.669404	496068.670943	46.476852
3503.702064	496082.791836	46.481857
3503.557054	496080.181987	46.486861
3503.605274	496062.504215	46.491866
3503.470687	496059.285144	46.496871
3503.292695	496044.022762	46.501876
3503.927169	496028.125643	46.506881
3503.741141	496019.345281	46.511885
3503.726066	496036.207832	46.516890
3503.666178	496005.838706	46.521895
3503.703727	495984.719632	46.526900
3503.757954	495984.508572	46.531905
3503.405420	495990.791959	46.536909
3503.773212	495978.531757	46.541914
3503.580691	495959.980575	46.546919
3503.438643	495940.864454	46.551924
3503.567980	495936.287233	46.556929
3503.412948	495937.476292	46.561933
3503.469534	495924.201985	46.566938
3503.297078	495935.975740	46.571943
3503.491652	495933.767878	46.576948
3503.598096	495911.372046	46.581953
3503.211310	495909.458594	46.586957
3503.036407	495897.739796	46.591962
3503.605302	495898.966331	46.596967
3503.564262	495897.605807	46.601972
3503.678733	495896.575122	46.606977
3503.703665	495893.938385	46.611981
3503.690691	495872.827167	46.616986
3503.664653	495856.325456	46.621991
3503.636292	495847.773249	46.626996
3503.822332	495843.946515	46.632001
3503.413063	495844.466923	46.637005
3503.881423	495815.836723	46.642010
3503.551022	495813.256137	46.647015
3503.803015	495817.671927	46.652020
3503.812501	495807.442875	46.657025
3503.794041	495808.559725	46.662029
3503.893445	495760.140142	46.667034
3503.376896	495774.550607	46.672039
3503.571587	495771.532599	46.677044
3503.657449	495765.139464	46.682049
3503.116543	495750.035461	46.687053
3503.641366	495737.699647	46.692058
3503.792351	495724.359642	46.697063
3503.590568	495732.492669	46.702068
3503.614233	495725.451136	46.707073
3503.550811	495725.106774	46.712077
3503.849382	495690.579285	46.717082
3503.792979	495679.601097	46.722087
3503.612760	495680.996682	46.727092
3503.721625	495661.891241	46.732097
3503.644040	495662.764285	46.737101
3503.834028	495640.304285	46.742106
3503.635989	495638.968556	46.747111
3503.721750	495637.790499	46.752116
3503.797979	495620.057240	46.757121
3503.570855	495591.941673	46.762125
3503.736167	495588.523220	46.767130
3503.989412	495595.470478	46.772135
3504.103805	495576.212178	46.777140
3503.981836	495549.446997	46.782145
3503.579653	495539.232230	46.787149
3503.813695	495532.258637	46.792154
3503.643220	495513.197192	46.797159
3503.751552	495492.370155	46.802164
3503.469546	495512.617125	46.807169
3503.333382	495479.525027	46.812173
3503.753576	495491.610457	46.817178
3503.465285	495477.732112	46.822183
3503.075638	495445.996464	46.827188
3503.077539	495442.198751	46.832193
3502.929921	495451.133464	46.837197
3503.424062	495437.840278	46.842202
3503.260826	495448.296440	46.847207
3503.478315	495444.262123	46.852212
3503.662213	495450.005213	46.857217
3503.589289	495449.510450	46.862221
3503.553027	495443.440301	46.867226
3503.384716	495446.403633	46.872231
3503.723518	495421.135047	46.877236
3503.833918	495408.560718	46.882241
3503.546340	495409.416332	46.887245
3503.456417	495396.721758	46.892250
3503.512548	495396.155962	46.897255
3503.486661	495382.590501	46.902260
3503.816788	495374.892802	46.907265
3503.709044	495363.264311	46.912269
3503.707559	495346.251930	46.917274
3503.637052	495359.174500	46.922279
3503.375602	495343.215862	46.927284
3503.713686	495317.137121	46.932289
3503.562379	495318.376264	46.937293
3503.646960	495298.109723	46.942298
3503.637279	495315.022720	46.947303
3503.350056	495305.852945	46.952308
3503.775291	495276.773022	46.957313
3503.306269	495266.619299	46.962317
3503.454781	495257.026197	46.967322
3503.455105	495273.330054	46.972327
3503.387026	495266.758544	46.977332
3503.636991	495240.086022	46.982337
3503.527158	495280.964373	46.987341
3503.424420	495232.018377	46.992346
3503.369154	495219.318203	46.997351
3503.409186	495212.780219	47.002356
3503.777673	495218.443575	47.007361
3503.431306	495217.283158	47.012365
3503.512504	495222.384320	47.017370
3503.680628	495203.319668	47.022375
3503.362138	495195.977579	47.027380
3503.672614	495169.346024	47.032385
3503.235657	495166.275852	47.037389
3503.448263	495178.495567	47.042394
3503.568985	495164.197904	47.047399
3503.356662	495176.282249	47.052404
3503.659127	495178.867414	47.057409
3503.440023	495144.927053	47.062413
3503.677974	495134.560248	47.067418
3503.366749	495130.761329	47.072423
3503.329890	495112.944186	47.077428
3503.381956	495130.556464	47.082433
3503.454191	495119.506974	47.087437
3503.692675	495110.861612	47.092442
3503.348934	495098.763918	47.097447
3503.225474	495087.542805	47.102452
3503.631926	495085.655788	47.107457
3503.146063	495093.428929	47.112461
3503.633889	495083.377037	47.117466
3503.401309	495091.363314	47.122471
3503.457090	495086.898774	47.127476
3503.544337	495085.366012	47.132481
3503.500817	495058.030742	47.137485
3503.364515	495041.596357	47.142490
3503.369768	495052.329917	47.147495
3503.148920	495040.010226	47.152500
3503.640820	495033.907095	47.157505
3503.021497	495029.447979	47.162509
3503.600223	495041.711185	47.167514
3503.486747	495040.665848	47.172519
3503.507686	495042.181587	47.177524
3503.613608	495035.126789	47.182529
3503.177545	495007.296515	47.187533
3503.419469	494999.764502	47.192538
3503.290292	495002.266015	47.197543
3503.419144	494999.055752	47.202548
3503.410091	494987.816495	47.207553
3503.285708	494987.481753	47.212557
3503.660910	494989.295941	47.217562
3503.623744	494989.656289	47.222567
3503.780499	494954.289051	47.227572
3503.411230	494964.423616	47.232577
3503.827246	494935.395244	47.237581
3503.525221	494938.531694	47.242586
3503.492778	494948.815566	47.247591
3503.531826	494938.075016	47.252596
3503.611970	494903.023593	47.257601
3503.742738	494911.458860	47.262605
3503.484673	494912.512367	47.267610
3503.835512	494902.532662	47.272615
3503.490369	494887.498270	47.277620
3503.721811	494862.954764	47.282625
3503.568181	494868.346312	47.287629
3504.115951	494859.196239	47.292634
3503.791266	494850.487865	47.297639
3503.565626	494833.409168	47.302644
3503.858462	494813.261078	47.307649
3503.489483	494805.876177	47.312653
3503.584557	494819.684375	47.317658
3503.900459	494800.646582	47.322663
3503.534329	494767.437641	47.327668
3503.335020	494773.089609	47.332673
3503.483784	494757.420065	47.337677
3503.464764	494782.790996	47.342682
3503.524492	494764.755711	47.347687
3503.097622	494766.646059	47.352692
3503.447486	494768.261736	47.357697
3503.162105	494751.243040	47.362701
3503.516723	494725.414018	47.367706
3503.612723	494718.208761	47.372711
3503.607573	494722.564191	47.377716
3503.597617	494716.489643	47.382721
3503.466096	494732.662915	47.387725
3503.752923	494705.173637	47.392730
3503.524359	494691.892872	47.397735
3503.562858	494676.291321	47.402740
3503.524473	494674.069495	47.407745
3503.307110	494679.876250	47.412749
3503.607593	494665.853594	47.417754
3503.591626	494654.969670	47.422759
3503.450524	494656.561688	47.427764
3503.713132	494629.076124	47.432769
3503.425087	494631.906606	47.437773
3503.616072	494621.850745	47.442778
3503.546450	494632.798925	47.447783
3503.328223	494624.731869	47.452788
3503.626976	494593.088475	47.457793
3503.425114	494593.120417	47.462797
3503.419051	494580.513293	47.467802
3503.567973	494592.439655	47.472807
3503.307488	494588.936412	47.477812
3503.200257	494593.611817	47.482817
3503.175937	494587.792672	47.487821
3503.643785	494582.705895	47.492826
3503.694407	494574.039339	47.497831
3503.499431	494559.841738	47.502836
3503.538344	494555.632911	47.507841
3503.488921	494550.526613	47.512845
3503.678417	494544.623024	47.517850
3503.617087	494536.683037	47.522855
3503.473273	494510.122330	47.527860
3503.416953	494504.713298	47.532865
3503.147702	494496.147898	47.537869
3503.429260	494487.394165	47.542874
3503.614907	494501.238923	47.547879
3503.389662	494503.806323	47.552884
3503.626376	494494.046976	47.557889
3503.297217	494481.997204	47.562893
3503.224442	494484.439237	47.567898
3503.448144	494477.314973	47.572903
3503.433618	494454.126316	47.577908
3503.506357	494434.721495	47.582913
3503.036219	494468.012654	47.587917
3503.496890	494448.495897	47.592922
3503.409603	494446.990667	47.597927
3503.044234	494437.934078	47.602932
3503.542426	494441.906206	47.607937
3503.364994	494452.365178	47.612941
3503.483924	494449.004481	47.617946
3503.591110	494411.567982	47.622951
3503.486039	494400.951168	47.627956
3503.552909	494399.927925	47.632961
3503.397894	494401.724705	47.637965
3503.509114	494384.744254	47.642970
3503.319809	494391.053021	47.647975
3503.322552	494413.180347	47.652980
3503.552706	494393.750603	47.657985
3503.192718	494375.274918	47.662989
3503.653820	494366.492750	47.667994
3503.630752	494363.205116	47.672999
3503.339120	494355.655901	47.678004
3503.539584	494365.396930	47.683009
3503.224181	494371.725634	47.688013
3503.164638	494361.709229	47.693018
3503.429373	494365.161281	47.698023
3503.173064	494361.657334	47.703028
3503.395682	494350.482341	47.708033
3503.522886	494330.157359	47.713037
3503.366824	494320.257458	47.718042
3503.366152	494320.358872	47.723047
3503.416911	494303.894260	47.728052
3503.515645	494310.258800	47.733057
3503.419970	494317.666780	47.738061
3503.164964	494313.453717	47.743066
3503.350252	494307.601354	47.748071
3503.191175	494319.981660	47.753076
3503.093905	494307.034314	47.758081
3503.268829	494320.678359	47.763085
3503.587753	494302.753560	47.768090
3503.464832	494280.594533	47.773095
3503.202661	494276.483866	47.778100
3503.568647	494265.691248	47.783105
3503.373246	494273.013737	47.788109
3503.581982	494268.322280	47.793114
3503.475606	494262.212186	47.798119
3503.405935	494272.603592	47.803124
3503.353961	494256.813442	47.808129
3503.597753	494212.924184	47.813133
3503.358171	494232.153138	47.818138
3503.428715	494230.622945	47.823143
3503.069142	494222.274237	47.828148
3503.622581	494229.832836	47.833153
3503.648835	494222.030777	47.838157
3503.670441	494226.331459	47.843162
3503.606615	494194.339600	47.848167
3503.324974	494180.509856	47.853172
3503.590464	494173.328234	47.858177
3503.406236	494180.800901	47.863181
3503.378524	494178.222875	47.868186
3503.499541	494179.925412	47.873191
3503.511896	494177.999322	47.878196
3503.311113	494153.624458	47.883201
3503.494132	494139.822514	47.888205
3503.284409	494124.563545	47.893210
3503.350738	494140.807339	47.898215
3502.943209	494146.289865	47.903220
3503.314959	494129.926271	47.908225
3502.897543	494132.676005	47.913229
3502.863650	494135.668938	47.918234
3502.978888	494134.739307	47.923239
3503.432267	494140.187036	47.928244
3503.320401	494122.785877	47.933249
3503.047602	494137.311005	47.938253
3503.243427	494133.836824	47.943258
3503.421932	494129.403291	47.948263
3503.190556	494135.566886	47.953268
3503.469857	494130.864241	47.958273
3503.197680	494132.426384	47.963277
3503.369488	494129.918088	47.968282
3503.774538	494123.828386	47.973287
3503.280613	494120.412586	47.978292
3503.497825	494094.655033	47.983297
3503.250500	494097.782979	47.988301
3503.426032	494096.590635	47.993306
3503.681483	494091.334749	47.998311
3503.354860	494088.095046	48.003316
3503.606885	494089.928794	48.008321
3503.291414	494097.624784	48.013325
3503.258401	494072.716932	48.018330
3503.497521	494058.045240	48.023335
3503.585205	494049.524489	48.028340
3503.625303	494044.150718	48.033345
3503.530262	494053.128436	48.038349
3503.287906	494035.444000	48.043354
3503.351579	494051.283200	48.048359
3503.288532	494033.924878	48.053364
3503.442826	494015.570092	48.058369
3503.358996	494014.520009	48.063373
3503.243086	494003.246403	48.068378
3503.379517	494006.263073	48.073383
3503.537161	494004.972277	48.078388
3503.621619	494001.971404	48.083393
3503.665423	494002.369609	48.088397
3502.946740	494008.660905	48.093402
3503.620521	494000.250041	48.098407
3503.363218	493979.276532	48.103412
3503.478265	493954.598302	48.108417
3503.314743	493972.448313	48.113421
3503.445456	493949.337337	48.118426
3503.603803	493945.717134	48.123431
3503.135371	493970.096847	48.128436
3503.673554	493953.959975	48.133441
3503.223351	493961.474771	48.138445
3503.517627	493930.286676	48.143450
3503.171527	493936.316560	48.148455
3503.455075	493920.118632	48.153460
3503.217693	493907.547608	48.158465
3503.477079	493920.368411	48.163469
3503.722960	493915.063351	48.168474
3503.822851	493911.452381	48.173479
3503.568196	493907.340443	48.178484
3503.794179	493876.517510	48.183489
3503.411754	493877.489457	48.188493
3503.761704	493872.016025	48.193498
3503.804144	493859.299467	48.198503
3503.500522	493848.409893	48.203508
3503.605178	493831.885704	48.208513
3503.332416	493833.701150	48.213517
3503.211529	493824.909438	48.218522
3503.716956	493817.284657	48.223527
3503.203552	493828.202183	48.228532
3503.310745	493814.158794	48.233537
3503.414610	493810.851000	48.238541
3503.404963	493825.182868	48.243546
3503.613655	493804.743153	48.248551
3503.268117	493785.251847	48.253556
3503.549540	493777.966279	48.258561
3503.509530	493790.226847	48.263565
3503.616889	493778.462079	48.268570
3503.549993	493780.852639	48.273575
3503.443100	493773.628444	48.278580
3503.673075	493743.716129	48.283585
3503.684230	493737.283460	48.288589
3503.507771	493737.412661	48.293594
3503.514113	493738.272530	48.298599
3503.204563	493729.409317	48.303604
3503.742005	493727.045725	48.308609
3503.528706	493717.205183	48.313613
3503.481193	493697.818592	48.318618
3503.652904	493686.600607	48.323623
3503.398214	493688.868948	48.328628
3503.452422	493691.848027	48.333633
3503.478269	493699.844698	48.338637
3503.394763	493683.755215	48.343642
3503.543009	493669.502678	48.348647
3503.466383	493654.374195	48.353652
3503.548650	493659.121161	48.358657
3503.125273	493658.884289	48.363661
3503.489812	493671.789920	48.368666
3503.716640	493658.031329	48.373671
3503.330075	493656.421424	48.378676
3503.753319	493632.251063	48.383681
3503.557457	493622.559628	48.388685
3503.490719	493607.632095	48.393690
3503.689602	493601.422895	48.398695
3503.715569	493599.747782	48.403700
3503.256321	493590.604336	48.408705
3503.124080	493573.712256	48.413709
3503.292281	493567.811722	48.418714
3503.735060	493558.323138	48.423719
3503.441906	493560.040557	48.428724
3503.475325	493552.135807	48.433729
3503.641700	493559.755862	48.438733
3503.740220	493558.221191	48.443738
3503.648941	493518.484906	48.448743
3503.363550	493526.784034	48.453748
3503.636478	493506.435111	48.458753
3503.613421	493515.148523	48.463757
3503.727902	493528.650796	48.468762
3503.677111	493480.704684	48.473767
3503.347447	493480.807463	48.478772
3503.448134	493489.906433	48.483777
3503.370524	493471.840950	48.488781
3503.363046	493450.624801	48.493786
3503.296952	493492.918081	48.498791
3503.461994	493455.116028	48.503796
3503.498890	493479.264603	48.508801
3503.259810	493456.616563	48.513805
3503.330413	493435.388054	48.518810
3503.861917	493412.921994	48.523815
3503.526654	493424.672451	48.528820
3503.356473	493430.472140	48.533825
3503.707159	493421.352509	48.538829
3503.293158	493408.809061	48.543834
3503.690758	493400.087110	48.548839
3503.660268	493413.105998	48.553844
3503.791872	493375.359706	48.558849
3503.781221	493393.743135	48.563853
3503.425347	493369.037277	48.568858
3503.655556	493376.090297	48.573863
3503.451745	493325.939881	48.578868
3503.621083	493358.169836	48.583873
3503.628724	493326.063897	48.588877
3503.448569	493341.283945	48.593882
3503.644981	493331.226524	48.598887
3503.177876	493341.579995	48.603892
3503.692914	493275.111516	48.608897
3503.386735	493309.847367	48.613901
3503.445821	493271.909771	48.618906
3503.579781	493310.930975	48.623911
3503.200567	493304.509216	48.628916
3503.653798	493264.635682	48.633921
3503.717489	493276.019344	48.638925
3503.484251	493262.231898	48.643930
3503.645155	493252.838348	48.648935
3503.687215	493231.209008	48.653940
3503.488253	493245.824442	48.658945
3503.671686	493240.883531	48.663949
3503.216517	493224.295366	48.668954
3503.560943	493206.314834	48.673959
3503.156908	493205.872343	48.678964
3503.533581	493196.596578	48.683969
3503.335995	493197.741898	48.688973
3503.462205	493199.798178	48.693978
3503.587789	493180.029213	48.698983
3503.254358	493205.452011	48.703988
3503.661484	493183.562359	48.708993
3503.685911	493150.693878	48.713997
3503.150114	493155.690579	48.719002
3503.469447	493154.222252	48.724007
3503.397779	493146.131382	48.729012
3503.574194	493146.761841	48.734017
3503.338186	493166.902841	48.739021
3503.162926	493140.547684	48.744026
3503.457281	493159.845279	48.749031
3503.238001	493117.950888	48.754036
3503.304881	493132.726950	48.759041
3502.696158	493117.277017	48.764045
3503.281504	493099.258302	48.769050
3503.465789	493132.245875	48.774055
3502.859825	493106.920887	48.779060
3503.213998	493103.269569	48.784065
3503.265360	493121.947302	48.789069
3503.535904	493089.394286	48.794074
3503.833627	493121.300527	48.799079
3503.609979	493100.573894	48.804084
3503.594785	493118.249368	48.809089
3503.786762	493092.139933	48.814093
3503.159520	493064.893964	48.819098
3503.194735	493075.775858	48.824103
3503.370045	493044.554433	48.829108
3503.063602	493074.631956	48.834113
3503.251129	493064.120041	48.839117
3503.191918	493061.192363	48.844122
3503.498958	493059.371497	48.849127
3503.379472	493054.782250	48.854132
3503.705570	493051.287277	48.859137
3503.688342	493060.658292	48.864141
3503.424228	493036.089402	48.869146
3503.799234	493020.483903	48.874151
3503.762319	493019.831463	48.879156
3503.619453	493008.915984	48.884161
3503.663740	493013.010807	48.889165
3503.546597	492996.014533	48.894170
3503.649351	492974.780415	48.899175
3503.145440	492975.113295	48.904180
3503.472178	492957.996189	48.909185
3503.498201	492981.539458	48.914189
3503.548375	492966.592929	48.919194
3503.705206	492953.249993	48.924199
3503.444691	492947.265104	48.929204
3503.534161	492940.465302	48.934209
3503.427453	492932.329237	48.939213
3503.306744	492935.285446	48.944218
3503.530381	492923.197919	48.949223
3503.340372	492935.634681	48.954228
3503.183220	492939.406882	48.959233
3503.667896	492908.186970	48.964237
3503.150659	492904.673345	48.969242
3503.748014	492888.070438	48.974247
3503.117526	492878.396666	48.979252
3503.392128	492882.708314	48.984257
3503.216987	492889.065993	48.989261
3503.398459	492899.114639	48.994266
3503.706712	492873.948671	48.999271
3503.304041	492887.887630	49.004276
3503.631795	492877.454725	49.009281
3503.423982	492852.977973	49.014285
3503.421759	492848.471420	49.019290
3503.375812	492839.363554	49.024295
3503.567541	492843.992149	49.029300
3503.737881	492836.116091	49.034305
3503.234895	492821.763273	49.039309
3503.187319	492833.468633	49.044314
3503.422127	492788.007575	49.049319
3503.314662	492793.037951	49.054324
3503.272196	492805.856599	49.059329
3503.492786	492772.450043	49.064333
3503.292497	492806.157303	49.069338
3503.256407	492789.705067	49.074343
3503.665861	492789.589747	49.079348
3503.139356	492783.039166	49.084353
3503.208711	492790.269754	49.089357
3502.927788	492783.579078	49.094362
3503.244316	492777.502928	49.099367
3502.954201	492783.473696	49.104372
3503.169611	492791.440798	49.109377
3503.113180	492774.181525	49.114381
3503.357642	492801.387217	49.119386
3503.978777	492756.979100	49.124391
3503.331558	492773.286238	49.129396
3503.458354	492732.703555	49.134401
3503.376134	492756.416140	49.139405
3503.264296	492754.155051	49.144410
3503.852652	492730.311897	49.149415
3503.138847	492741.869416	49.154420
3503.064432	492753.123308	49.159425
3503.287728	492715.614378	49.164429
3503.308097	492760.377034	49.169434
3503.822051	492728.443231	49.174439
3503.200969	492711.475707	49.179444
3503.454378	492713.106815	49.184449
3503.417276	492683.640121	49.189453
3503.349818	492710.287565	49.194458
3503.748253	492664.243299	49.199463
3503.251637	492711.721080	49.204468
3503.148346	492681.961004	49.209473
3503.106576	492707.642227	49.214477
3503.372388	492686.685847	49.219482
3503.452917	492690.268611	49.224487
3503.401902	492661.006641	49.229492
3503.311690	492667.097770	49.234497
3503.256661	492650.243282	49.239501
3502.980276	492655.654877	49.244506
3503.464562	492671.833903	49.249511
3503.334676	492655.801496	49.254516
3503.181134	492654.104030	49.259521
3503.358805	492645.872250	49.264525
3503.303212	492658.338593	49.269530
3503.302189	492659.604799	49.274535
3503.144483	492632.587820	49.279540
3503.255666	492659.308383	49.284545
3503.743178	492633.911195	49.289549
3503.177065	492647.521684	49.294554
3503.465755	492595.063268	49.299559
3503.195959	492618.957599	49.304564
3502.898500	492579.758287	49.309569
3503.057658	492624.246133	49.314573
3503.130386	492595.369623	49.319578
3503.329136	492620.354626	49.324583
3503.122758	492602.561848	49.329588
3503.131666	492615.980193	49.334593
3503.586488	492600.260445	49.339597
3502.875008	492607.665161	49.344602
3503.378879	492597.963870	49.349607
3503.124809	492598.662390	49.354612
3503.422774	492609.958792	49.359617
3503.319974	492603.493100	49.364621
3503.086820	492591.477555	49.369626
3503.012857	492598.882791	49.374631
3503.286571	492608.967656	49.379636
3502.992744	492590.834206	49.384641
3503.333348	492600.148897	49.389645
3503.332620	492612.353396	49.394650
3503.443240	492592.484888	49.399655
3503.466641	492614.307263	49.404660
3503.532124	492577.430681	49.409665
3503.496029	492573.638382	49.414669
3503.411146	492577.348594	49.419674
3503.530189	492544.717286	49.424679
3503.299516	492585.873917	49.429684
3503.155185	492565.792474	49.434689
3503.816125	492545.836935	49.439693
3503.474290	492577.034952	49.444698
3503.697698	492515.319410	49.449703
3503.264890	492545.822889	49.454708
3503.133958	492516.826525	49.459713
3503.247335	492530.734827	49.464717
3503.099976	492520.933864	49.469722
3503.834044	492519.855703	49.474727
3503.430995	492518.552145	49.479732
3503.551443	492519.849802	49.484737
3503.628034	492516.748651	49.489741
3503.479265	492485.678789	49.494746
3503.497351	492479.497790	49.499751
3503.254609	492470.623411	49.504756
3503.307340	492489.757333	49.509761
3503.856237	492450.423976	49.514765
3503.282593	492496.952305	49.519770
3503.358864	492462.707109	49.524775
3503.481328	492474.233897	49.529780
3503.752438	492409.826502	49.534785
3503.533558	492445.765557	49.539789
3503.259445	492411.676929	49.544794
3503.128689	492438.081565	49.549799
3503.347277	492398.850947	49.554804
3503.396074	492435.963098	49.559809
3503.629904	492410.960188	49.564813
3503.409034	492418.287434	49.569818
3503.406739	492386.687846	49.574823
3503.733472	492380.964442	49.579828
3502.991062	492383.360668	49.584833
3503.566897	492382.915203	49.589837
3503.319025	492378.649926	49.594842
3503.491858	492396.093806	49.599847
3503.849921	492359.980805	49.604852
3503.254579	492376.128168	49.609857
3503.753991	492331.434425	49.614861
3503.807799	492368.545919	49.619866
3503.730284	492328.197208	49.624871
3503.763844	492306.163001	49.629876
3503.533565	492324.582206	49.634881
3503.468914	492312.185358	49.639885
3503.498996	492263.159843	49.644890
3503.485643	492307.776997	49.649895
3503.402005	492289.356823	49.654900
3503.372232	492304.452671	49.659905
3503.773467	492269.345495	49.664909
3503.504696	492277.136140	49.669914
3503.550604	492243.351111	49.674919
3503.165032	492266.808420	49.679924
3503.405628	492237.246483	49.684929
3503.135049	492254.102242	49.689933
3503.152666	492253.694362	49.694938
3503.347135	492252.904040	49.699943
3503.317440	492243.843955	49.704948
3503.595083	492243.546900	49.709953
3503.414987	492239.068313	49.714957
3503.342498	492237.915054	49.719962
3503.588554	492213.365719	49.724967
3503.492094	492221.331719	49.729972
3503.413123	492224.939783	49.734977
3503.605015	492199.588727	49.739981
3503.412764	492224.281573	49.744986
3503.515176	492220.011536	49.749991
3503.716659	492186.455021	49.754996
3503.581759	492178.019231	49.760001
3503.636758	492167.780965	49.765005
3503.576699	492159.181412	49.770010
3503.767491	492165.228292	49.775015
3503.797089	492152.360666	49.780020
3503.365329	492119.916952	49.785025
3503.529464	492127.132819	49.790029
3503.700434	492128.422518	49.795034
3503.561544	492117.809735	49.800039
3503.281883	492126.918850	49.805044
3503.506022	492111.539001	49.810049
3503.477792	492075.587787	49.815053
3503.297279	492105.900185	49.820058
3503.634652	492062.548095	49.825063
3503.659009	492075.964389	49.830068
3503.106911	492086.686483	49.835073
3503.642099	492073.181829	49.840077
3503.275884	492062.250452	49.845082
3503.403288	492078.942182	49.850087
3503.409854	492030.122336	49.855092
3503.483776	492054.469485	49.860097
3503.789693	492025.251380	49.865101
3503.161789	492030.009727	49.870106
3503.596562	492026.953165	49.875111
3503.511097	492023.320483	49.880116
3503.120487	492034.169009	49.885121
3503.502511	492009.192779	49.890125
3503.765108	492005.758290	49.895130
3503.559230	491989.737318	49.900135
3503.494272	491991.722664	49.905140
3503.634081	491983.294008	49.910145
3503.442595	491978.361379	49.915149
3503.228009	491976.167077	49.920154
3503.511277	491949.636468	49.925159
3503.369995	491947.076080	49.930164
3503.036360	491946.875638	49.935169
3503.326897	491946.019477	49.940173
3503.075270	491939.222580	49.945178
3503.247139	491944.209035	49.950183
3503.025459	491935.685566	49.955188
3503.233883	491949.174143	49.960193
3503.879952	491940.361596	49.965197
3503.506328	491948.877943	49.970202
3503.726798	491921.344374	49.975207
3503.739436	491923.418748	49.980212
3503.509724	491909.984232	49.985217
3503.567479	491899.998594	49.990221
3503.311438	491901.153232	49.995226
3503.177611	491887.298405	50.000231
3502.868404	491900.058554	50.005236
3503.053550	491908.334675	50.010241
3503.148139	491881.124797	50.015245
3502.939076	491892.704347	50.020250
3503.048881	491899.371823	50.025255
3503.117596	491880.370097	50.030260
3503.174272	491890.996083	50.035265
3503.476245	491898.747318	50.040269
3503.195028	491881.117604	50.045274
3503.376175	491903.675517	50.050279
3503.218372	491874.277258	50.055284
3502.891839	491900.004607	50.060289
3503.547135	491872.149027	50.065293
3502.809245	491893.636794	50.070298
3502.851048	491885.679365	50.075303
3503.002088	491895.024373	50.080308
3503.047379	491893.801833	50.085313
3503.423917	491882.195886	50.090317
3503.104010	491883.968328	50.095322
3503.215561	491907.600728	50.100327
3503.183982	491890.640559	50.105332
3503.329467	491887.528414	50.110337
3503.664443	491894.616083	50.115341
3503.299322	491866.212784	50.120346
3503.346142	491845.593924	50.125351
3503.329265	491855.066778	50.130356
3503.292447	491860.592665	50.135361
3503.402512	491849.788453	50.140365
3503.214951	491844.601955	50.145370
3503.376349	491848.374670	50.150375
3503.306912	491855.880772	50.155380
3503.148795	491854.791665	50.160385
3503.462118	491843.448898	50.165389
3503.395870	491853.081483	50.170394
3503.410979	491821.680753	50.175399
3503.578802	491803.068424	50.180404
3503.487876	491798.221138	50.185409
3503.486530	491809.464052	50.190413
3503.104354	491788.558437	50.195418
3503.569098	491802.715604	50.200423
3503.675264	491804.775209	50.205428
3503.030421	491785.227814	50.210433
3503.658750	491779.253986	50.215437
3503.693024	491766.891781	50.220442
3503.222922	491761.547346	50.225447
3503.609808	491765.892152	50.230452
3503.802309	491760.493631	50.235457
3503.516245	491748.941687	50.240461
3503.389234	491731.084886	50.245466
3503.729884	491713.761865	50.250471
3503.597989	491708.363959	50.255476
3503.406369	491706.165995	50.260481
3503.636734	491697.165824	50.265485
3503.441185	491702.818132	50.270490
3503.618334	491702.334383	50.275495
3503.615906	491673.468320	50.280500
3503.219343	491664.871082	50.285505
3503.475305	491669.591104	50.290509
3503.090349	491664.283827	50.295514
3503.456411	491661.592567	50.300519
3503.251643	491664.764836	50.305524
3503.083569	491668.640306	50.310529
3503.313167	491657.006801	50.315533
3503.485471	491660.068828	50.320538
3503.309813	491667.845010	50.325543
3503.595967	491647.694533	50.330548
3503.233947	491631.039571	50.335553
3503.434048	491622.348007	50.340557
3503.111705	491620.221337	50.345562
3503.314646	491609.756808	50.350567
3503.312001	491614.112574	50.355572
3503.075466	491619.872671	50.360577
3503.495410	491611.450213	50.365581
3503.388897	491618.202624	50.370586
3503.200080	491620.612731	50.375591
3503.412420	491619.313127	50.380596
3503.144830	491606.340167	50.385601
3503.486255	491607.451031	50.390605
3503.137153	491610.443549	50.395610
3503.274234	491579.580207	50.400615
3503.334138	491579.621418	50.405620
3503.245732	491579.179638	50.410625
3503.542254	491566.725207	50.415629
3503.459256	491573.271344	50.420634
3503.506319	491569.364410	50.425639
3503.389806	491565.331400	50.430644
3503.087231	491576.267563	50.435649
3503.451344	491561.979289	50.440653
3503.164203	491569.773132	50.445658
3503.382540	491566.345559	50.450663
3503.587337	491552.436961	50.455668
3503.163927	491527.587389	50.460673
3503.072182	491525.880051	50.465677
3503.041211	491528.872943	50.470682
3503.128157	491525.263556	50.475687
3503.124344	491527.593791	50.480692
3503.492627	491524.699587	50.485697
3503.408146	491525.270054	50.490701
3503.405346	491538.083307	50.495706
3503.080303	491523.600069	50.500711
3503.293125	491527.263435	50.505716
3503.126258	491521.719072	50.510721
3503.119242	491514.984643	50.515725
3503.244124	491532.335627	50.520730
3503.019399	491499.959394	50.525735
3503.198210	491482.408521	50.530740
3502.961885	491470.139533	50.535745
3503.099614	491411.725701	50.540749
3502.874016	491358.534786	50.545754
3502.868302	491286.570679	50.550759
3502.991939	491221.676041	50.555764
3502.628563	491149.514714	50.560769
3502.608602	491048.532667	50.565773
3502.372003	490956.345892	50.570778
3502.336954	490837.740643	50.575783
3501.895506	490729.530572	50.580788
3501.701598	490606.188279	50.585793
3501.907745	490468.145178	50.590797
3501.581763	490317.827383	50.595802
3501.264687	490162.239678	50.600807
3501.408655	490027.951046	50.605812
3500.912899	489836.935634	50.610817
3500.437894	489668.250966	50.615821
3500.337079	489471.547438	50.620826
3500.217707	489309.286402	50.625831
3500.092037	489095.210121	50.630836
3499.592094	488891.573923	50.635841
3499.466593	488683.571002	50.640845
3498.938176	488461.092451	50.645850
3498.745065	488241.040243	50.650855
3498.391594	488023.594117	50.655860
3497.994341	487774.443348	50.660865
3497.572074	487551.177522	50.665869
3497.334720	487277.984902	50.670874
3497.072257	487021.964550	50.675879
3496.378083	486774.873821	50.680884
3495.932506	486497.751732	50.685889
3495.859958	486239.259314	50.690893
3495.306732	485950.039121	50.695898
3494.538193	485685.975495	50.700903
3494.392884	485394.149474	50.705908
3493.534630	485128.775194	50.710913
3493.577678	484829.869008	50.715917
3493.119833	484525.819155	50.720922
3492.616467	484226.230033	50.725927
3492.166208	483930.934277	50.730932
3490.887140	483604.910337	50.735937
3490.980383	483314.079058	50.740941
3490.484250	483001.651494	50.745946
3489.914747	482669.470388	50.750951
3489.296492	482371.948081	50.755956
3488.999852	482024.816514	50.760961
3488.258462	481717.169939	50.765965
3487.717208	481387.749334	50.770970
3487.433776	481043.385104	50.775975
3486.724705	480719.046892	50.780980
3486.208666	480395.078191	50.785985
3485.874022	480032.816798	50.790989
3485.174037	479697.261380	50.795994
3484.465729	479345.232018	50.800999
3484.148574	478998.860996	50.806004
3483.143470	478658.876645	50.811009
3482.887486	478290.033498	50.816013
3482.011621	477929.440837	50.821018
3481.631700	477590.910440	50.826023
3481.204000	477231.805391	50.831028
3480.327707	476877.579571	50.836033
3480.013761	476512.463161	50.841037
3479.047115	476146.530966	50.846042
3478.453262	475780.533176	50.851047
3477.971696	475412.635613	50.856052
3477.163285	475055.528530	50.861057
3476.851541	474681.407045	50.866061
3476.131605	474302.831906	50.871066
3475.495014	473939.646056	50.876071
3475.009660	473562.337941	50.881076
3474.035064	473202.842050	50.886081
3473.675121	472827.781603	50.891085
3473.107197	472447.221617	50.896090
3472.452494	472065.350232	50.901095
3471.882411	471689.338959	50.906100
3470.795793	471300.424342	50.911105
3470.302033	470925.147471	50.916109
3469.633368	470550.550492	50.921114
3469.348145	470165.391511	50.926119
3468.737183	469791.278651	50.931124
3467.967599	469405.827230	50.936129
3467.380911	469012.024729	50.941133
3466.625325	468624.984893	50.946138
3466.054955	468229.238346	50.951143
3465.108971	467844.242280	50.956148
3464.351438	467463.975637	50.961153
3463.810377	467071.904085	50.966157
3463.037152	466698.674227	50.971162
3462.370837	466300.371163	50.976167
3461.599333	465924.236992	50.981172
3460.858813	465556.813315	50.986177
3460.393786	465160.231831	50.991181
3459.765466	464778.375126	50.996186
3458.646620	464389.185098	51.001191
3458.348642	463999.401793	51.006196
3457.114494	463630.653676	51.011201
3456.877793	463235.927509	51.016205
3456.060303	462856.196447	51.021210
3455.356570	462491.909386	51.026215
3454.595323	462106.019463	51.031220
3453.408235	461729.268630	51.036225
3453.462343	461358.046351	51.041229
3452.676004	460979.849718	51.046234
3451.769706	460596.897662	51.051239
3451.207126	460216.065601	51.056244
3450.497270	459842.148534	51.061249
3449.841893	459460.303519	51.066253
3449.002344	459088.169430	51.071258
3448.269649	458705.258286	51.076263
3448.072646	458326.313935	51.081268
3447.135655	457954.531186	51.086273
3446.497423	457570.773792	51.091277
3445.572262	457188.678451	51.096282
3444.665188	456817.125542	51.101287
3444.552896	456458.427905	51.106292
3443.718940	456069.044406	51.111297
3443.075017	455683.834895	51.116301
3442.000030	455334.707695	51.121306
3441.227391	454952.347041	51.126311
3440.940691	454570.258214	51.131316
3439.876693	454203.252924	51.136321
3439.278787	453835.609881	51.141325
3438.660473	453469.181799	51.146330
3437.715841	453094.579752	51.151335
3437.089731	452729.866084	51.156340
3436.268352	452357.566428	51.161345
3436.012055	451988.875458	51.166349
3435.145949	451622.406108	51.171354
3434.610299	451269.223950	51.176359
3433.794792	450893.753535	51.181364
3432.950710	450530.612350	51.186369
3432.324694	450158.855074	51.191373
3431.666067	449804.908747	51.196378
3430.990293	449427.007346	51.201383
3430.261734	449072.198203	51.206388
3429.509387	448708.557233	51.211393
3428.887230	448333.522244	51.216397
3427.785026	447967.083092	51.221402
3427.309302	447611.044525	51.226407
3426.750413	447249.532565	51.231412
3425.621347	446901.706749	51.236417
3425.097882	446530.789019	51.241421
3424.104029	446182.931229	51.246426
3423.644198	445828.132059	51.251431
3423.005113	445478.177660	51.256436
3422.227381	445134.127707	51.261441
3421.506413	444765.396098	51.266445
3420.802819	444420.918079	51.271450
3420.088456	444075.066334	51.276455
3419.391146	443714.131525	51.281460
3418.262428	443374.121694	51.286465
3418.052990	443034.418565	51.291469
3417.404131	442682.902046	51.296474
3416.486719	442339.443231	51.301479
3415.722491	441981.335730	51.306484
3415.015255	441646.869600	51.311489
3414.526682	441292.718663	51.316493
3413.631311	440960.151111	51.321498
3412.632104	440619.320697	51.326503
3412.572950	440275.697078	51.331508
3411.918303	439936.173370	51.336513
3410.998329	439594.148548	51.341517
3410.167401	439256.902488	51.346522
3409.277203	438908.974346	51.351527
3408.720364	438576.143321	51.356532
3407.971167	438245.292893	51.361537
3407.515410	437903.425147	51.366541
3406.816865	437570.425352	51.371546
3405.929574	437232.678359	51.376551
3405.507740	436893.152315	51.381556
3404.578650	436561.241758	51.386561
3404.067735	436228.397532	51.391565
3403.133452	435892.366239	51.396570
3402.720066	435555.232596	51.401575
3401.608863	435222.469996	51.406580
3401.006409	434898.787834	51.411585
3400.305128	434563.057474	51.416589
3399.616183	434234.556641	51.421594
3398.734050	433906.158284	51.426599
3398.110608	433574.490295	51.431604
3397.276033	433263.798249	51.436609
3397.039197	432935.386963	51.441613
3396.098261	432619.651233	51.446618
3395.169394	432283.114423	51.451623
3394.665868	431966.336667	51.456628
3393.819322	431649.812397	51.461633
3393.273043	431321.988113	51.466637
3392.473354	431004.636012	51.471642
3391.715939	430692.123350	51.476647
3391.553558	430365.318194	51.481652
3390.642369	430036.189589	51.486657
3389.697983	429725.142336	51.491661
3389.087451	429416.349450	51.496666
3388.128820	429088.359174	51.501671
3387.976741	428778.191207	51.506676
3386.979445	428457.614389	51.511681
3386.546517	428143.267835	51.516685
3385.779407	427827.192712	51.521690
3385.031955	427507.250569	51.526695
3384.369240	427180.256481	51.531700
3383.649993	426873.838353	51.536705
3383.078600	426553.831538	51.541709
3382.360503	426246.948908	51.546714
3381.514691	425926.317672	51.551719
3380.896666	425603.056048	51.556724
3379.731344	425303.370067	51.561729
3379.356594	424997.612604	51.566733
3378.519575	424703.506438	51.571738
3377.725445	424382.340728	51.576743
3377.414138	424077.782000	51.581748
3376.528614	423772.523283	51.586753
3375.828995	423458.570516	51.591757
3375.117865	423162.065639	51.596762
3374.706620	422845.291663	51.601767
3374.141192	422544.769259	51.606772
3373.105519	422247.797817	51.611777
3372.650782	421931.223402	51.616781
3371.548897	421629.709009	51.621786
3370.630595	421329.330773	51.626791
3370.398372	421027.570713	51.631796
3369.322882	420734.120176	51.636801
3368.780719	420435.044513	51.641805
3368.194216	420132.390893	51.646810
3367.419735	419842.871597	51.651815
3366.943536	419528.534101	51.656820
3366.066899	419242.174749	51.661825
3365.373203	418936.425968	51.666829
3364.849241	418652.773861	51.671834
3364.066775	418343.171298	51.676839
3363.517575	418067.443426	51.681844
3362.505553	417763.231167	51.686849
3362.075436	417458.720401	51.691853
3361.425614	417178.782598	51.696858
3360.761877	416877.605254	51.701863
3360.096674	416582.446142	51.706868
3358.895695	416299.233326	51.711873
3358.509880	415999.019053	51.716877
3357.905975	415715.883927	51.721882
3357.055328	415420.589782	51.726887
3356.378395	415122.394156	51.731892
3355.496900	414852.379103	51.736897
3354.796669	414557.281043	51.741901
3354.116399	414265.429034	51.746906
3353.695871	413984.992065	51.751911
3353.071891	413702.628138	51.756916
3351.780954	413424.432320	51.761921
3351.295081	413137.518393	51.766925
3350.630125	412854.720839	51.771930
3349.952714	412576.902758	51.776935
3349.204656	412289.259754	51.781940
3348.927570	412037.900823	51.786945
3347.910884	411732.762177	51.791949
3347.501035	411468.409500	51.796954
3346.590492	411178.087940	51.801959
3346.066705	410889.913128	51.806964
3345.377857	410613.679374	51.811969
3344.591547	410341.092284	51.816973
3344.142886	410061.029195	51.821978
3343.194019	409784.600228	51.826983
3342.656219	409500.632630	51.831988
3341.830385	409225.424268	51.836993
3341.411948	408932.436572	51.841997
3340.981273	408670.629232	51.847002
3340.243796	408388.537909	51.852007
3339.518876	408104.485185	51.857012
3338.260065	407837.871512	51.862017
3337.395287	407557.292022	51.867021
3336.980315	407278.036589	51.872026
3336.109722	407008.812942	51.877031
3336.060635	406743.065844	51.882036
3334.857965	406461.564051	51.887041
3334.659109	406180.815882	51.892045
3333.730313	405905.060254	51.897050
3333.107141	405633.040695	51.902055
3332.442663	405361.711503	51.907060
3331.728680	405102.231413	51.912065
3331.015568	404826.279632	51.917069
3330.244391	404551.147913	51.922074
3329.711605	404287.489614	51.927079
3329.219885	404002.040755	51.932084
3328.449536	403741.465420	51.937089
3327.879133	403463.445782	51.942093
3327.287285	403178.132394	51.947098
3326.243404	402919.576078	51.952103
3325.797579	402640.411165	51.957108
3324.998847	402371.720879	51.962113
3324.479784	402102.475746	51.967117
3323.774594	401835.443741	51.972122
3323.117391	401559.505498	51.977127
3322.331831	401285.415321	51.982132
3321.443075	401023.057192	51.987137
3320.848078	400746.364997	51.992141
3319.952746	400485.147393	51.997146
3319.089480	400226.515392	52.002151
3318.667126	399949.738254	52.007156
3318.140966	399690.667384	52.012161
3317.392828	399428.147016	52.017165
3316.618310	399158.866928	52.022170
3315.844832	398906.336533	52.027175
3315.445749	398641.060089	52.032180
3314.490073	398369.031319	52.037185
3313.738786	398105.636561	52.042189
3313.371884	397852.245732	52.047194
3312.323193	397582.869006	52.052199
3311.787216	397322.306590	52.057204
3310.771502	397086.350082	52.062209
3310.116239	396824.023101	52.067213
3309.497443	396582.865007	52.072218
3309.033584	396314.732914	52.077223
3308.420961	396059.180978	52.082228
3307.938253	395810.775785	52.087233
3307.216687	395548.525578	52.092237
3306.843577	395286.269071	52.097242
3305.633903	395031.032571	52.102247
3305.380892	394767.431036	52.107252
3304.440754	394514.309026	52.112257
3303.763922	394248.100994	52.117261
3303.000966	393996.192888	52.122266
3302.181363	393748.029264	52.127271
3301.888141	393483.483465	52.132276
3300.867763	393221.898200	52.137281
3300.163749	392971.651279	52.142285
3299.662062	392718.599207	52.147290
3298.752886	392471.686372	52.152295
3298.361572	392205.493640	52.157300
3297.704824	391960.698410	52.162305
3296.790512	391707.068571	52.167309
3296.106566	391454.875163	52.172314
3295.609305	391202.726689	52.177319
3295.237121	390943.564357	52.182324
3294.477186	390705.489221	52.187329
3293.286318	390444.698252	52.192333
3292.802190	390186.565117	52.197338
3292.019696	389930.918288	52.202343
3291.560575	389686.686189	52.207348
3290.873417	389443.200443	52.212353
3290.035883	389189.514893	52.217357
3289.292098	388932.710512	52.222362
3288.520435	388700.472162	52.227367
3287.877443	388446.928564	52.232372
3286.880217	388206.661949	52.237377
3286.437700	387954.990298	52.242381
3285.826547	387713.209901	52.247386
3285.288932	387479.350065	52.252391
3284.839338	387228.310190	52.257396
3284.120249	386987.813469	52.262401
3283.305394	386739.625197	52.267405
3282.865924	386490.307822	52.272410
3282.049137	386248.219606	52.277415
3281.461236	385996.506512	52.282420
3280.378561	385760.153422	52.287425
3279.897525	385516.379746	52.292429
3279.262782	385264.313021	52.297434
3278.131800	385021.630655	52.302439
3277.826937	384783.698741	52.307444
3276.981729	384544.324907	52.312449
3276.259701	384308.363243	52.317453
3275.589097	384067.102253	52.322458
3274.716228	383836.832627	52.327463
3274.592928	383595.939797	52.332468
3273.657402	383367.177653	52.337473
3273.060576	383123.381173	52.342477
3272.525612	382883.718753	52.347482
3271.890589	382639.721729	52.352487
3271.215159	382404.554553	52.357492
3270.709504	382155.854395	52.362497
3269.716152	381918.165801	52.367501
3269.142002	381682.978138	52.372506
3268.190129	381450.646398	52.377511
3267.878629	381210.200517	52.382516
3267.042689	380965.741312	52.387521
3266.347877	380737.891723	52.392525
3265.852349	380497.877426	52.397530
3264.825722	380261.430067	52.402535
3264.223532	380030.891106	52.407540
3263.515765	379791.134897	52.412545
3262.860802	379555.972456	52.417549
3262.301861	379304.744297	52.422554
3261.853857	379090.606001	52.427559
3261.039437	378847.071106	52.432564
3260.404422	378606.329592	52.437569
3259.544220	378375.363832	52.442573
3258.707705	378141.976631	52.447578
3258.016389	377904.495432	52.452583
3257.773975	377674.953978	52.457588
3256.608264	377445.455490	52.462593
3255.966484	377211.218063	52.467597
3255.425019	376982.177752	52.472602
3254.180563	376764.083077	52.477607
3254.290688	376533.817948	52.482612
3253.693262	376302.467905	52.487617
3252.819698	376069.735764	52.492621
3252.256529	375842.676424	52.497626
3251.515806	375610.683721	52.502631
3250.904488	375368.214644	52.507636
3249.835178	375151.202756	52.512641
3248.952104	374913.988548	52.517645
3248.717099	374680.206245	52.522650
3247.781237	374470.597331	52.527655
3247.344314	374229.671020	52.532660
3246.449569	374022.164632	52.537665
3245.558057	373795.883516	52.542669
3245.285560	373564.008628	52.547674
3244.549471	373343.373131	52.552679
3243.783083	373117.526395	52.557684
3243.236055	372907.746274	52.562689
3242.593501	372668.496884	52.567693
3242.408676	372447.082589	52.572698
3241.160901	372217.822011	52.577703
3240.774159	371994.325832	52.582708
3240.071235	371767.673145	52.587713
3239.482485	371544.766191	52.592717
3238.488396	371306.098857	52.597722
3237.907656	371093.160503	52.602727
3237.115251	370862.624861	52.607732
3236.487026	370636.437648	52.612737
3235.903237	370419.298829	52.617741
3235.166988	370192.693869	52.622746
3234.661146	369982.434763	52.627751
3233.675230	369752.279895	52.632756
3232.931977	369529.997400	52.637761
3232.423836	369315.664919	52.642765
3231.630622	369102.826589	52.647770
3231.394577	368875.117939	52.652775
3231.036860	368656.306248	52.657780
3230.158960	368432.945455	52.662785
3229.280081	368210.448675	52.667789
3228.954737	367974.786330	52.672794
3228.039868	367750.664656	52.677799
3227.079930	367517.211880	52.682804
3226.419814	367307.880133	52.687809
3225.464107	367087.603249	52.692813
3225.109321	366868.171568	52.697818
3224.279724	366652.477579	52.702823
3223.610068	366445.636595	52.707828
3222.584307	366228.037965	52.712833
3222.020486	366008.533341	52.717837
3221.575025	365801.552139	52.722842
3220.534151	365591.102183	52.727847
3220.296040	365375.410237	52.732852
3219.512588	365163.060229	52.737857
3218.986682	364949.243668	52.742861
3218.139494	364736.291103	52.747866
3217.349879	364526.992275	52.752871
3216.665404	364302.282549	52.757876
3215.676205	364100.061174	52.762881
3215.061227	363880.503428	52.767885
3214.981250	363678.925121	52.772890
3214.075303	363478.061798	52.777895
3213.503307	363252.082377	52.782900
3212.690774	363064.306165	52.787905
3212.072825	362840.443866	52.792909
3211.585410	362631.470260	52.797914
3210.751216	362418.479448	52.802919
3210.242904	362202.051975	52.807924
3209.481815	362001.362898	52.812929
3208.955699	361785.419764	52.817933
3208.583877	361576.753938	52.822938
3207.419829	361366.329572	52.827943
3206.837058	361157.364473	52.832948
3206.126073	360935.696073	52.837953
3205.239461	360738.456590	52.842957
3205.312625	360510.580701	52.847962
3204.311351	360312.925019	52.852967
3203.783577	360095.116906	52.857972
3202.960075	359883.054461	52.862977
3202.006580	359674.243285	52.867981
3201.483123	359452.436551	52.872986
3200.628747	359247.424762	52.877991
3200.192375	359038.808938	52.882996
3199.468322	358837.006477	52.888001
3198.820927	358619.388749	52.893005
3198.441022	358423.662750	52.898010
3197.581683	358207.908873	52.903015
3196.861099	357984.472585	52.908020
3196.236056	357780.334430	52.913025
3195.486207	357564.026015	52.918029
3195.098386	357353.181425	52.923034
3193.951622	357156.528359	52.928039
3193.411413	356942.499767	52.933044
3192.890279	356726.075170	52.938049
3192.057941	356531.940092	52.943053
3191.240004	356319.148798	52.948058
3190.655842	356121.893694	52.953063
3190.041877	355919.323911	52.958068
3189.364430	355701.901700	52.963073
3188.589113	355516.049738	52.968077
3188.227026	355302.851208	52.973082
3187.409549	355100.132200	52.978087
3186.578280	354895.607727	52.983092
3185.953361	354684.433164	52.988097
3185.331803	354487.101267	52.993101
3184.735776	354276.327630	52.998106
3183.922058	354076.785064	53.003111
3183.258712	353877.803263	53.008116
3182.615421	353670.521131	53.013121
3181.811488	353478.889364	53.018125
3181.321593	353258.754946	53.023130
3180.284417	353070.390628	53.028135
3179.647369	352864.402212	53.033140
3179.124797	352666.665977	53.038145
3178.520610	352465.786153	53.043149
3178.056483	352272.874622	53.048154
3177.092046	352081.593976	53.053159
3176.572255	351874.616040	53.058164
3176.260060	351685.572169	53.063169
3175.130995	351472.479249	53.068173
3174.721104	351279.428272	53.073178
3174.042789	351072.930401	53.078183
3173.360373	350873.914803	53.083188
3172.842352	350664.285050	53.088193
3172.000230	350465.013249	53.093197
3171.148875	350262.077273	53.098202
3170.489069	350062.266131	53.103207
3170.191698	349862.778676	53.108212
3169.243266	349663.749807	53.113217
3168.533942	349466.438507	53.118221
3167.893481	349253.743100	53.123226
3167.410423	349066.880442	53.128231
3166.553499	348854.141381	53.133236
3165.836139	348664.616585	53.138241
3165.202125	348463.624768	53.143245
3164.516123	348267.603512	53.148250
3163.850051	348073.563646	53.153255
3163.404771	347869.231100	53.158260
3162.606603	347680.428385	53.163265
3161.714022	347483.291725	53.168269
3161.171152	347276.707234	53.173274
3160.536226	347083.448028	53.178279
3159.997485	346881.341016	53.183284
3159.322417	346695.926130	53.188289
3158.615554	346494.353386	53.193293
3158.179105	346291.184543	53.198298
3157.143484	346100.148853	53.203303
3156.486586	345897.955238	53.208308
3155.985854	345701.997587	53.213313
3155.167932	345509.143796	53.218317
3154.852193	345308.548574	53.223322
3153.731013	345110.319956	53.228327
3153.167553	344912.918735	53.233332
3152.317758	344717.929296	53.238337
3151.893792	344524.271766	53.243341
3151.434768	344325.706641	53.248346
3150.503935	344139.356792	53.253351
3149.677074	343941.815801	53.258356
3149.313586	343748.629768	53.263361
3148.289301	343553.155006	53.268365
3147.839878	343347.636216	53.273370
3147.030725	343164.293051	53.278375
3146.540704	342971.099061	53.283380
3145.871358	342779.663695	53.288385
3145.303060	342583.349996	53.293389
3144.438852	342389.475171	53.298394
3143.620849	342203.177789	53.303399
3143.037638	342002.359157	53.308404
3142.418293	341810.250998	53.313409
3141.524746	341619.865617	53.318413
3141.423387	341428.794303	53.323418
3140.318201	341235.539388	53.328423
3139.931524	341045.377484	53.333428
3139.440393	340857.700640	53.338433
3138.578391	340653.612575	53.343437
3138.116142	340451.827906	53.348442
3137.190869	340268.570776	53.353447
3136.411193	340075.998941	53.358452
3135.949672	339879.430614	53.363457
3134.852065	339686.755156	53.368461
3134.277775	339492.672628	53.373466
3133.858281	339315.060154	53.378471
3133.260486	339129.482356	53.383476
3132.374476	338939.138507	53.388481
3131.454757	338745.642918	53.393485
3131.003424	338553.854537	53.398490
3130.218567	338366.674950	53.403495
3129.591551	338176.211487	53.408500
3129.091026	337987.076615	53.413505
3128.191729	337808.084887	53.418509
3127.655607	337614.245189	53.423514
3127.151490	337434.349852	53.428519
3126.437826	337241.504472	53.433524
3125.591396	337057.487431	53.438529
3124.939246	336876.137515	53.443533
3124.414191	336672.492554	53.448538
3123.511093	336492.377745	53.453543
3122.804230	336310.703999	53.458548
3122.165077	336122.298471	53.463553
3121.372622	335949.878069	53.468557
3120.965584	335767.977207	53.473562
3120.096196	335571.511278	53.478567
3119.679017	335387.956292	53.483572
3119.353736	335203.266154	53.488577
3118.564033	335011.571915	53.493581
3118.080807	334818.377581	53.498586
3117.200066	334628.427758	53.503591
3116.533730	334439.639976	53.508596
3115.967503	334235.383181	53.513601
3115.135500	334063.677051	53.518605
3114.472173	333877.916693	53.523610
3113.435668	333692.596749	53.528615
3113.204353	333497.984135	53.533620
3112.644953	333310.525608	53.538625
3111.789960	333128.917734	53.543629
3111.551248	332944.258760	53.548634
3110.230644	332746.786929	53.553639
3109.417034	332563.669029	53.558644
3109.139501	332379.829378	53.563649
3108.580828	332196.975689	53.568653
3107.820960	332010.003675	53.573658
3107.061451	331822.496491	53.578663
3106.203482	331625.915760	53.583668
3105.756890	331452.334738	53.588673
3104.836497	331262.076583	53.593677
3104.743742	331085.180004	53.598682
3103.808513	330891.562695	53.603687
3102.888372	330709.144309	53.608692
3102.158318	330526.237131	53.613697
3101.577651	330350.281575	53.618701
3101.154575	330173.256848	53.623706
3100.250906	329982.305328	53.628711
3099.842553	329794.330021	53.633716
3099.110286	329612.286538	53.638721
3098.201422	329432.383663	53.643725
3097.871860	329245.463789	53.648730
3097.131871	329062.529120	53.653735
3096.534035	328873.537656	53.658740
3095.878619	328698.659326	53.663745
3095.075874	328512.474457	53.668749
3094.388717	328325.176085	53.673754
3093.352050	328147.938167	53.678759
3092.850640	327968.603831	53.683764
3092.366211	327789.393688	53.688769
3091.201876	327608.915892	53.693773
3090.837418	327430.144208	53.698778
3090.269283	327254.204927	53.703783
3089.485285	327076.873652	53.708788
3088.995324	326898.502509	53.713793
3088.140667	326719.806770	53.718797
3087.892688	326541.091004	53.723802
3087.077625	326369.873472	53.728807
3086.119834	326180.397734	53.733812
3085.650952	325995.961693	53.738817
3084.653758	325830.271237	53.743821
3084.511299	325646.775688	53.748826
3083.736484	325466.307737	53.753831
3082.642468	325282.172664	53.758836
3082.457767	325109.732429	53.763841
3081.627380	324930.901554	53.768845
3081.015488	324755.141911	53.773850
3080.172720	324572.391272	53.778855
3079.696033	324389.735060	53.783860
3078.765734	324211.020271	53.788865
3077.995596	324050.000515	53.793869
3077.615101	323865.341978	53.798874
3076.896695	323692.143022	53.803879
3076.314930	323518.056411	53.808884
3075.481418	323327.637801	53.813889
3074.851963	323163.411442	53.818893
3074.319459	322991.607450	53.823898
3073.498776	322814.552777	53.828903
3073.003609	322637.879066	53.833908
3072.194910	322462.222137	53.838913
3071.790602	322283.420026	53.843917
3070.779279	322100.232388	53.848922
3070.189398	321922.731969	53.853927
3069.753966	321748.236672	53.858932
3069.077880	321570.876485	53.863937
3068.470741	321399.997751	53.868941
3067.912951	321211.083986	53.873946
3066.892438	321046.915489	53.878951
3066.327291	320869.790951	53.883956
3065.619387	320690.244313	53.888961
3064.997479	320515.928859	53.893965
3064.424391	320333.202893	53.898970
3063.595256	320162.127752	53.903975
3062.852587	319990.529363	53.908980
3062.586263	319804.418251	53.913985
3061.774238	319632.651926	53.918989
3061.365290	319452.749970	53.923994
3060.082474	319283.960187	53.928999
3059.413770	319106.848584	53.934004
3059.036749	318927.118786	53.939009
3057.996613	318757.500302	53.944013
3057.260655	318578.310418	53.949018
3056.805526	318409.158896	53.954023
3056.175955	318236.444458	53.959028
3055.698135	318074.578212	53.964033
3054.960650	317894.572464	53.969037
3054.853814	317715.179527	53.974042
3053.716119	317542.798866	53.979047
3052.999933	317370.249337	53.984052
3052.663036	317181.445120	53.989057
3051.821888	317016.095249	53.994061
3051.426430	316841.024120	53.999066
3050.737708	316659.658811	54.004071
3050.011688	316485.021301	54.009076
3049.203920	316305.049178	54.014081
3048.187258	316124.575061	54.019085
3047.903620	315934.512318	54.024090
3047.090700	315766.151226	54.029095
3046.304964	315594.424402	54.034100
3045.999423	315418.649017	54.039105
3045.245311	315251.958332	54.044109
3044.354522	315070.520253	54.049114
3043.614396	314899.039662	54.054119
3042.812957	314725.302240	54.059124
3042.343680	314554.363867	54.064129
3041.559848	314381.692544	54.069133
3041.310528	314203.945480	54.074138
3040.017427	314030.895827	54.079143
3039.276692	313867.943933	54.084148
3039.051498	313693.986268	54.089153
3038.145110	313518.608298	54.094157
3037.639783	313350.016323	54.099162
3037.240704	313180.516032	54.104167
3036.407403	313011.007801	54.109172
3035.648471	312835.961865	54.114177
3034.839362	312670.778133	54.119181
3034.328649	312488.944404	54.124186
3033.474596	312328.223462	54.129191
3032.623336	312156.348580	54.134196
3032.120082	311995.367918	54.139201
3031.475977	311833.543531	54.144205
3031.066849	311652.838224	54.149210
3030.493711	311481.172917	54.154215
3029.672146	311305.930738	54.159220
3029.006275	311139.296042	54.164225
3028.072562	310974.562387	54.169229
3028.048628	310803.853163	54.174234
3027.289917	310629.185668	54.179239
3026.356026	310453.399731	54.184244
3026.036678	310275.326316	54.189249
3025.243899	310109.448673	54.194253
3024.882110	309929.522533	54.199258
3023.846230	309762.104067	54.204263
3023.104333	309577.755774	54.209268
3022.556317	309405.268515	54.214273
3021.908654	309231.905511	54.219277
3021.330274	309055.653772	54.224282
3020.548545	308881.904042	54.229287
3019.758953	308708.104375	54.234292
3019.749702	308527.763808	54.239297
3018.966251	308369.241604	54.244301
3018.498955	308185.382474	54.249306
3017.192486	308009.015263	54.254311
3016.951059	307833.905276	54.259316
3016.256994	307646.465202	54.264321
3015.213458	307481.311179	54.269325
3014.806899	307305.004261	54.274330
3014.175824	307123.588670	54.279335
3013.072435	306950.854809	54.284340
3012.611854	306769.462658	54.289345
3011.846186	306608.643539	54.294349
3011.095335	306424.750318	54.299354
3010.375848	306253.202558	54.304359
3010.014283	306080.579308	54.309364
3009.223782	305912.047253	54.314369
3008.419227	305744.026515	54.319373
3007.897375	305573.592532	54.324378
3007.140677	305397.338437	54.329383
3006.447873	305229.503087	54.334388
3005.832947	305055.823589	54.339393
3005.101071	304888.605174	54.344397
3004.428848	304714.806981	54.349402
3003.899713	304554.177129	54.354407
3003.314776	304385.483301	54.359412
3002.951878	304212.399487	54.364417
3001.886019	304040.292556	54.369421
3001.350782	303861.836847	54.374426
3000.503803	303690.764407	54.379431
2999.873329	303531.244450	54.384436
2999.013983	303355.615180	54.389441
2998.543963	303184.838993	54.394445
2997.833265	303014.584550	54.399450
2997.286149	302834.626952	54.404455
2996.636779	302672.893500	54.409460
2996.191788	302499.489552	54.414465
2995.173424	302335.522193	54.419469
2994.797226	302158.694508	54.424474
2994.075027	301985.741296	54.429479
2993.282324	301820.082359	54.434484
2992.488920	301643.523835	54.439489
2991.910345	301470.954763	54.444493
2991.400808	301299.622414	54.449498
2990.579295	301127.244207	54.454503
2990.254397	300962.172424	54.459508
2989.543459	300791.100591	54.464513
2988.515049	300623.542244	54.469517
2988.195137	300440.846426	54.474522
2987.754106	300270.317037	54.479527
2986.844489	300097.289529	54.484532
2986.292981	299925.962339	54.489537
2985.576764	299754.737439	54.494541
2984.957861	299567.733197	54.499546
2984.237367	299403.002566	54.504551
2983.751526	299221.019244	54.509556
2983.057044	299040.825943	54.514561
2982.257556	298876.743965	54.519565
2981.523678	298699.561597	54.524570
2980.786696	298522.048471	54.529575
2980.370948	298351.054720	54.534580
2979.590448	298171.459857	54.539585
2978.893975	298006.291146	54.544589
2978.231611	297822.831753	54.549594
2977.826117	297652.064902	54.554599
2977.117116	297481.957133	54.559604
2976.616938	297293.403634	54.564609
2975.682642	297137.745429	54.569613
2975.069233	296946.280808	54.574618
2974.550944	296763.765283	54.579623
2974.045285	296594.872386	54.584628
2973.224128	296401.988476	54.589633
2972.328635	296237.970221	54.594637
2971.828314	296054.075951	54.599642
2971.152103	295878.435195	54.604647
2970.518432	295698.814689	54.609652
2969.934655	295519.186121	54.614657
2968.897503	295354.425534	54.619661
2968.421641	295178.217633	54.624666
2967.802327	294990.724878	54.629671
2967.132569	294828.019478	54.634676
2966.299988	294639.923481	54.639681
2965.786078	294481.700829	54.644685
2965.053250	294298.682173	54.649690
2964.603428	294125.245177	54.654695
2963.610684	293956.885564	54.659700
2963.174159	293759.532408	54.664705
2962.127887	293587.895700	54.669709
2961.750111	293426.874782	54.674714
2961.279146	293242.667750	54.679719
2960.480158	293076.798056	54.684724
2959.916896	292889.472857	54.689729
2959.002687	292715.547977	54.694733
2958.729605	292540.146236	54.699738
2957.882727	292374.436418	54.704743
2956.907149	292197.159161	54.709748
2956.383591	292010.794731	54.714753
2955.618637	291831.828475	54.719757
2954.775944	291665.480813	54.724762
2954.492415	291497.108992	54.729767
2953.474436	291323.657936	54.734772
2953.074922	291147.129152	54.739777
2952.197626	290974.037598	54.744781
2951.827927	290802.724710	54.749786
2950.798048	290627.186718	54.754791
2950.430375	290468.556162	54.759796
2950.169383	290284.950324	54.764801
2949.277717	290110.994570	54.769805
2948.657264	289931.061800	54.774810
2947.423617	289761.387594	54.779815
2947.296098	289587.794428	54.784820
2946.849305	289411.144632	54.789825
2945.418560	289244.149956	54.794829
2945.515802	289062.524013	54.799834
2944.653896	288880.056546	54.804839
2943.970015	288719.437623	54.809844
2943.577808	288528.745890	54.814849
2942.790515	288361.088559	54.819853
2942.294287	288169.317949	54.824858
2941.391099	287994.649640	54.829863
2940.590628	287814.234702	54.834868
2940.466824	287636.921496	54.839873
2939.480846	287463.030036	54.844877
2939.067929	287278.554986	54.849882
2938.523694	287097.207708	54.854887
2937.395337	286919.925800	54.859892
2936.875572	286735.518302	54.864897
2935.980101	286561.815791	54.869901
2935.448668	286378.097586	54.874906
2934.584069	286194.788580	54.879911
2933.743351	286013.716885	54.884916
2933.639960	285850.203183	54.889921
2932.680429	285677.885663	54.894925
2932.267497	285490.328051	54.899930
2931.771027	285311.595519	54.904935
2930.563176	285135.216711	54.909940
2930.261199	284962.794780	54.914945
2929.736326	284781.774381	54.919949
2928.963113	284597.966258	54.924954
2928.458818	284416.000123	54.929959
2927.692057	284228.727156	54.934964
2926.943578	284049.651953	54.939969
2926.060220	283878.493155	54.944973
2925.626680	283693.866836	54.949978
2925.576736	283507.320541	54.954983
2924.119856	283329.936232	54.959988
2923.816927	283145.136213	54.964993
2922.864269	282965.048727	54.969997
2922.292279	282780.545852	54.975002
2921.663519	282605.245920	54.980007
2920.898055	282419.856692	54.985012
2920.709112	282234.885495	54.990017
2919.568992	282059.946493	54.995021
2918.986297	281882.245026	55.000026
2918.489498	281688.994276	55.005031
2917.567462	281519.241579	55.010036
2917.205489	281332.642054	55.015041
2916.333208	281157.405706	55.020045
2915.649433	280965.406811	55.025050
2915.058692	280793.003711	55.030055
2914.285596	280611.690068	55.035060
2913.883831	280426.217197	55.040065
2912.940720	280243.122129	55.045069
2912.314716	280075.690761	55.050074
2911.710577	279887.728436	55.055079
2910.766543	279710.465636	55.060084
2910.382318	279528.657216	55.065089
2909.471691	279346.753818	55.070093
2908.860836	279172.137806	55.075098
2908.171812	278999.495200	55.080103
2907.321216	278821.096830	55.085108
2907.360594	278632.090041	55.090113
2906.684382	278470.269367	55.095117
2905.805194	278293.658222	55.100122
2905.044509	278106.229707	55.105127
2904.550427	277927.851161	55.110132
2904.062567	277740.048312	55.115137
2903.450482	277558.530324	55.120141
2902.457306	277351.324125	55.125146
2901.622628	277172.795666	55.130151
2901.067348	276989.587711	55.135156
2900.776284	276797.627722	55.140161
2900.152708	276621.587161	55.145165
2899.144663	276441.990946	55.150170
2898.527421	276255.736536	55.155175
2897.952974	276075.154789	55.160180
2897.098033	275890.236878	55.165185
2896.345072	275706.932791	55.170189
2895.762869	275529.306581	55.175194
2895.056067	275353.508350	55.180199
2894.516244	275172.742811	55.185204
2894.119437	274990.579334	55.190209
2893.081925	274797.795103	55.195213
2892.379199	274630.324385	55.200218
2891.868344	274451.642669	55.205223
2891.017534	274264.941299	55.210228
2890.615935	274078.729119	55.215233
2890.234074	273900.383553	55.220237
2889.733468	273719.408083	55.225242
2889.223194	273533.569691	55.230247
2888.023295	273352.730426	55.235252
2887.346543	273147.842599	55.240257
2886.675161	272958.744335	55.245261
2885.891664	272783.416763	55.250266
2885.655977	272600.158215	55.255271
2884.576727	272414.078913	55.260276
2884.006682	272232.605191	55.265281
2883.219880	272052.872190	55.270285
2882.413551	271864.966960	55.275290
2882.300542	271692.232999	55.280295
2881.367236	271512.930760	55.285300
2880.602588	271317.913341	55.290305
2879.993565	271131.326807	55.295309
2879.216739	270954.775931	55.300314
2878.620068	270775.293171	55.305319
2878.103218	270593.836745	55.310324
2877.413677	270407.161220	55.315329
2876.844673	270222.911607	55.320333
2875.979529	270048.030326	55.325338
2875.627931	269857.277418	55.330343
2874.605087	269678.397192	55.335348
2874.004396	269482.386405	55.340353
2873.337933	269304.213889	55.345357
2872.606839	269122.638899	55.350362
2872.343135	268944.122552	55.355367
2871.173007	268760.605176	55.360372
2870.841341	268571.148331	55.365377
2870.021366	268408.459592	55.370381
2869.181395	268218.803183	55.375386
2868.448629	268033.510396	55.380391
2867.952582	267860.888836	55.385396
2867.607960	267681.010376	55.390401
2867.301176	267496.669043	55.395405
2865.973634	267311.317855	55.400410
2865.405874	267122.128074	55.405415
2864.695154	266949.413450	55.410420
2864.438615	266753.782009	55.415425
2863.684813	266574.605416	55.420429
2863.190044	266390.014091	55.425434
2862.540680	266194.215858	55.430439
2861.849335	266017.347187	55.435444
2861.372056	265823.890401	55.440449
2860.697976	265639.124021	55.445453
2859.693082	265440.173425	55.450458
2859.149710	265253.731086	55.455463
2858.376628	265069.209839	55.460468
2858.086787	264874.348524	55.465473
2857.179450	264690.612748	55.470477
2856.330248	264488.658193	55.475482
2856.027961	264301.337672	55.480487
2854.846956	264118.817026	55.485492
2854.765811	263931.232459	55.490497
2854.194159	263741.739148	55.495501
2853.349479	263546.813549	55.500506
2852.752060	263353.580727	55.505511
2851.726799	263165.458412	55.510516
2851.096503	262979.260160	55.515521
2850.367457	262796.694092	55.520525
2849.806034	262602.437274	55.525530
2849.296582	262415.023207	55.530535
2848.295633	262236.677237	55.535540
2847.901900	262043.845869	55.540545
2847.333328	261860.439942	55.545549
2846.352083	261669.255370	55.550554
2846.161224	261478.022169	55.555559
2844.930893	261291.104934	55.560564
2844.917730	261103.740408	55.565569
2844.017573	260902.993058	55.570573
2843.312343	260714.617782	55.575578
2842.676504	260521.163561	55.580583
2841.712879	260336.063854	55.585588
2841.217816	260147.044450	55.590593
2840.273759	259957.485048	55.595597
2839.756028	259774.505334	55.600602
2839.133860	259581.762699	55.605607
2838.550991	259405.618884	55.610612
2837.770433	259215.652103	55.615617
2837.121505	259028.236845	55.620621
2836.547978	258839.842015	55.625626
2835.972469	258648.162323	55.630631
2835.082090	258470.463386	55.635636
2834.313997	258278.636200	55.640641
2833.750582	258095.079163	55.645645
2833.111979	257911.559637	55.650650
2832.923513	257724.301657	55.655655
2831.938976	257540.811727	55.660660
2831.272484	257345.454690	55.665665
2830.767777	257166.091200	55.670669
2830.244501	256971.450355	55.675674
2829.586447	256773.392925	55.680679
2828.830234	256586.276704	55.685684
2828.056796	256399.468975	55.690689
2827.899526	256198.938827	55.695693
2826.710962	256014.463752	55.700698
2826.195141	255812.335364	55.705703
2825.289894	255625.192633	55.710708
2824.802832	255429.834339	55.715713
2824.259179	255244.722997	55.720717
2823.116423	255059.477486	55.725722
2822.886481	254857.712224	55.730727
2821.827785	254681.647381	55.735732
2821.707559	254491.070641	55.740737
2821.152982	254286.046635	55.745741
2820.302548	254100.220907	55.750746
2819.527632	253908.194910	55.755751
2818.652580	253717.534712	55.760756
2818.185458	253520.952701	55.765761
2817.567612	253335.065410	55.770765
2816.699852	253148.479335	55.775770
2816.211225	252948.004887	55.780775
2815.442284	252766.471457	55.785780
2815.002743	252572.789295	55.790785
2814.144461	252383.197404	55.795789
2813.530583	252185.672306	55.800794
2812.981887	251990.047110	55.805799
2812.141447	251810.563301	55.810804
2811.741495	251609.134022	55.815809
2811.182782	251425.556786	55.820813
2810.131923	251235.894751	55.825818
2809.831018	251043.567502	55.830823
2809.121088	250846.924988	55.835828
2808.249598	250659.170649	55.840833
2807.574308	250460.383909	55.845837
2807.051181	250271.989107	55.850842
2806.462419	250074.844446	55.855847
2805.632832	249887.797404	55.860852
2804.839134	249689.157675	55.865857
2804.053769	249502.435137	55.870861
2803.177841	249322.093745	55.875866
2802.881172	249124.012664	55.880871
2802.351984	248946.723679	55.885876
2801.763443	248748.027167	55.890881
2801.150944	248559.215599	55.895885
2800.605121	248361.225870	55.900890
2799.933586	248168.145808	55.905895
2798.947940	247975.446794	55.910900
2798.306972	247776.326916	55.915905
2798.032977	247579.772190	55.920909
2797.063520	247395.908079	55.925914
2796.492276	247195.581029	55.930919
2796.014471	247007.794175	55.935924
2795.194498	246807.557976	55.940929
2794.553456	246614.245907	55.945933
2793.749228	246423.506526	55.950938
2793.258401	246216.470568	55.955943
2792.508063	246033.413854	55.960948
2791.944629	245831.355787	55.965953
2791.305108	245643.316207	55.970957
2790.549992	245448.648642	55.975962
2790.031355	245238.486250	55.980967
2788.974019	245052.016115	55.985972
2788.449841	244854.664393	55.990977
2787.905891	244658.971350	55.995981
2787.507265	244478.331154	56.000986
2786.768202	244275.106313	56.005991
2785.488053	244088.520004	56.010996
2785.222775	243886.366669	56.016001
2784.791719	243696.386873	56.021005
2783.653113	243507.334298	56.026010
2783.186972	243298.821885	56.031015
2782.561651	243117.022592	56.036020
2781.791752	242919.687211	56.041025
2781.317368	242725.564876	56.046029
2780.616828	242533.846911	56.051034
2780.094604	242329.826826	56.056039
2779.146078	242140.898963	56.061044
2778.733288	241941.522284	56.066049
2778.135845	241752.743131	56.071053
2777.288062	241557.739541	56.076058
2777.043152	241353.065987	56.081063
2776.019484	241157.276017	56.086068
2775.447251	240957.365965	56.091073
2774.332463	240772.617310	56.096077
2773.720048	240575.744565	56.101082
2773.031783	240389.401071	56.106087
2772.337917	240193.942416	56.111092
2772.048520	239997.579698	56.116097
2771.430780	239811.938958	56.121101
2770.819528	239625.278906	56.126106
2770.175685	239421.970552	56.131111
2769.592373	239226.317764	56.136116
2768.624555	239027.135728	56.141121
2768.267017	238829.639891	56.146125
2767.057261	238644.247588	56.151130
2766.693957	238439.776130	56.156135
2765.956287	238245.346303	56.161140
2765.130822	238055.030451	56.166145
2764.432319	237857.870434	56.171149
2763.629432	237669.206838	56.176154
2763.201981	237479.567401	56.181159
2762.519772	237293.584528	56.186164
2762.044904	237095.932114	56.191169
2761.511036	236907.812902	56.196173
2760.568782	236713.392737	56.201178
2760.327712	236513.667258	56.206183
2759.383518	236328.491462	56.211188
2758.829780	236127.110159	56.216193
2758.124749	235931.100571	56.221197
2757.316063	235744.376522	56.226202
2756.673074	235543.672530	56.231207
2756.228753	235349.456121	56.236212
2755.490430	235149.837460	56.241217
2754.721273	234957.328364	56.246221
2754.235318	234775.902271	56.251226
2753.755833	234572.729795	56.256231
2752.837285	234380.219990	56.261236
2752.086062	234183.202523	56.266241
2751.657678	233973.046240	56.271245
2750.719612	233790.012960	56.276250
2750.198879	233594.029602	56.281255
2749.442061	233399.229861	56.286260
2748.906591	233191.001925	56.291265
2748.337761	233002.513477	56.296269
2746.860769	232813.634513	56.301274
2747.049361	232609.978305	56.306279
2746.337374	232427.140932	56.311284
2745.387137	232223.003885	56.316289
2744.988937	232028.150098	56.321293
2743.947864	231839.051232	56.326298
2743.651586	231643.825614	56.331303
2742.981345	231458.131683	56.336308
2742.257207	231259.791815	56.341313
2741.732021	231063.075911	56.346317
2740.723681	230875.985330	56.351322
2740.683213	230672.318646	56.356327
2739.912835	230476.788625	56.361332
2739.175810	230273.487770	56.366337
2738.278279	230066.291623	56.371341
2737.668905	229877.077453	56.376346
2737.267539	229693.355991	56.381351
2736.306847	229485.687396	56.386356
2735.674791	229278.043614	56.391361
2735.251458	229083.607416	56.396365
2734.496935	228892.406823	56.401370
2734.224601	228679.182251	56.406375
2733.298683	228489.282763	56.411380
2732.362173	228284.006544	56.416385
2731.477578	228086.844822	56.421389
2730.944093	227898.386690	56.426394
2730.563556	227695.722714	56.431399
2730.016721	227504.237642	56.436404
2729.140023	227299.539889	56.441409
2728.432598	227098.023934	56.446413
2727.605322	226910.251031	56.451418
2727.190246	226712.788936	56.456423
2726.515221	226516.896141	56.461428
2725.907934	226309.535605	56.466433
2725.567562	226114.570989	56.471437
2724.613411	225916.636006	56.476442
2723.933088	225714.966296	56.481447
2722.883157	225509.409199	56.486452
2722.234768	225317.206815	56.491457
2721.942964	225118.455926	56.496461
2721.254622	224927.075524	56.501466
2720.474482	224721.401284	56.506471
2719.800672	224519.962621	56.511476
2719.021983	224327.821396	56.516481
2718.164120	224125.521755	56.521485
2717.936070	223928.889619	56.526490
2717.171856	223743.125302	56.531495
2716.313424	223551.138599	56.536500
2715.997271	223348.449597	56.541505
2715.531472	223142.424091	56.546509
2714.343275	222948.467011	56.551514
2713.934030	222750.428008	56.556519
2713.615681	222552.336918	56.561524
2712.681487	222341.919505	56.566529
2711.868218	222142.533025	56.571533
2711.098416	221953.985986	56.576538
2710.718916	221749.872694	56.581543
2710.167386	221556.862086	56.586548
2709.385886	221357.141636	56.591553
2708.664354	221164.629948	56.596557
2707.792762	220965.026636	56.601562
2707.286528	220759.981343	56.606567
2706.968401	220571.646230	56.611572
2706.206597	220362.861812	56.616577
2705.427710	220155.455472	56.621581
2704.537977	219965.150246	56.626586
2704.225423	219763.984957	56.631591
2703.661248	219560.645152	56.636596
2702.708473	219357.138335	56.641601
2702.480825	219149.278343	56.646605
2701.630279	218958.091184	56.651610
2701.038021	218752.695918	56.656615
2700.461454	218540.501328	56.661620
2699.200549	218333.125571	56.666625
2698.982896	218132.764407	56.671629
2698.197617	217945.808398	56.676634
2697.657335	217743.399119	56.681639
2697.094782	217539.542827	56.686644
2695.846094	217326.910944	56.691649
2695.573723	217127.134076	56.696653
2694.848306	216933.106654	56.701658
2694.196121	216730.577974	56.706663
2693.648371	216522.547185	56.711668
2692.901644	216324.375207	56.716673
2692.381858	216114.839199	56.721677
2691.169309	215921.693666	56.726682
2690.738760	215712.717533	56.731687
2690.251867	215523.124041	56.736692
2689.361061	215320.802747	56.741697
2688.871745	215119.805870	56.746701
2687.970912	214926.410100	56.751706
2687.434421	214718.968483	56.756711
2686.734809	214529.920588	56.761716
2686.011196	214325.080981	56.766721
2685.251683	214128.763010	56.771725
2684.627117	213937.897451	56.776730
2683.994588	213732.077865	56.781735
2683.463170	213539.607641	56.786740
2682.532132	213341.766299	56.791745
2682.407957	213140.615666	56.796749
2681.509620	212942.261207	56.801754
2681.010486	212739.860189	56.806759
2679.946408	212549.437369	56.811764
2679.569621	212344.548931	56.816769
2679.066822	212143.944997	56.821773
2677.804102	211958.532043	56.826778
2677.513910	211747.509589	56.831783
2676.706242	211554.490741	56.836788
2675.994548	211367.515751	56.841793
2675.655261	211163.019676	56.846797
2675.078020	210962.749405	56.851802
2674.508966	210767.047740	56.856807
2673.671572	210565.687156	56.861812
2672.841636	210358.063999	56.866817
2672.331286	210153.241892	56.871821
2671.496895	209961.810335	56.876826
2671.160840	209759.354692	56.881831
2670.177806	209558.134949	56.886836
2669.517711	209355.884677	56.891841
2669.067359	209151.298164	56.896845
2668.536166	208956.092512	56.901850
2668.050568	208752.760186	56.906855
2667.245823	208557.306401	56.911860
2666.082411	208342.271841	56.916865
2665.448611	208142.948652	56.921869
2665.258981	207949.282992	56.926874
2664.495942	207750.363376	56.931879
2663.815277	207551.685904	56.936884
2662.644831	207353.646668	56.941889
2662.565964	207148.002557	56.946893
2661.564213	206962.690379	56.951898
2661.091699	206749.639241	56.956903
2660.506879	206552.808017	56.961908
2659.479586	206342.760684	56.966913
2659.307445	206140.214713	56.971917
2658.311085	205956.202943	56.976922
2658.073588	205750.894216	56.981927
2657.336067	205549.203442	56.986932
2656.454712	205340.511032	56.991937
2656.036994	205136.836558	56.996941
2654.893983	204939.450083	57.001946
2654.782672	204737.115656	57.006951
2653.685900	204534.403543	57.011956
2653.125891	204323.920334	57.016961
2652.288663	204123.815639	57.021965
2651.816979	203940.363422	57.026970
2651.124577	203730.692388	57.031975
2650.497192	203526.814994	57.036980
2649.954773	203334.314828	57.041985
2649.191951	203125.178946	57.046989
2648.579572	202919.316066	57.051994
2647.972647	202713.363986	57.056999
2647.253990	202522.777953	57.062004
2646.496861	202316.354804	57.067009
2646.106652	202112.534003	57.072013
2645.139633	201918.171587	57.077018
2644.654966	201711.720224	57.082023
2643.735300	201515.366477	57.087028
2642.714033	201319.042245	57.092033
2642.247506	201114.651800	57.097037
2641.652631	200922.537261	57.102042
2641.273325	200719.190691	57.107047
2640.468920	200523.522115	57.112052
2639.602009	200320.165196	57.117057
2639.275348	200116.850695	57.122061
2638.709145	199926.554846	57.127066
2638.245811	199716.099073	57.132071
2637.576212	199511.594078	57.137076
2636.590235	199313.400824	57.142081
2636.269242	199107.798653	57.147085
2635.680878	198896.449663	57.152090
2635.071090	198693.694373	57.157095
2633.899314	198500.636339	57.162100
2633.179118	198293.051798	57.167105
2632.798274	198089.575377	57.172109
2631.870480	197884.328549	57.177114
2631.322007	197685.448495	57.182119
2630.707036	197484.301977	57.187124
2630.075979	197282.408011	57.192129
2629.649609	197073.801893	57.197133
2628.563747	196873.152237	57.202138
2628.326643	196668.640553	57.207143
2627.389469	196460.703146	57.212148
2626.845025	196261.407946	57.217153
2626.094789	196048.530893	57.222157
2625.207897	195856.150019	57.227162
2624.722861	195645.383043	57.232167
2624.529425	195443.821336	57.237172
2623.636694	195242.091282	57.242177
2623.010893	195032.926937	57.247181
2622.180214	194834.560587	57.252186
2621.748840	194627.937388	57.257191
2621.120380	194426.588586	57.262196
2619.742691	194214.709262	57.267201
2619.738647	194003.847412	57.272205
2618.994874	193815.803169	57.277210
2618.349062	193601.825525	57.282215
2617.659239	193401.775652	57.287220
2616.859905	193182.989062	57.292225
2616.441934	192979.335146	57.297229
2615.638852	192779.432951	57.302234
2614.947899	192575.467678	57.307239
2614.633341	192363.376858	57.312244
2613.610263	192165.178789	57.317249
2613.104084	191951.987704	57.322253
2612.160741	191752.340911	57.327258
2611.711128	191543.901195	57.332263
2611.040344	191331.400504	57.337268
2610.086627	191131.796059	57.342273
2609.433889	190918.976226	57.347277
2608.665699	190723.440934	57.352282
2608.109863	190524.602949	57.357287
2607.722682	190323.347125	57.362292
2606.960773	190117.685745	57.367297
2606.253282	189905.578815	57.372301
2605.594213	189720.603064	57.377306
2604.890095	189511.563561	57.382311
2604.215698	189308.372741	57.387316
2603.540783	189097.180277	57.392321
2603.155793	188887.609483	57.397325
2602.306619	188692.375212	57.402330
2601.344829	188488.788147	57.407335
2600.962676	188293.774144	57.412340
2599.986025	188100.788959	57.417345
2600.045932	187887.271765	57.422349
2599.078765	187682.442250	57.427354
2598.492844	187486.560603	57.432359
2597.720991	187273.457893	57.437364
2596.898234	187062.755995	57.442369
2596.394258	186861.431629	57.447373
2595.650799	186666.876055	57.452378
2595.252368	186455.740743	57.457383
2594.513286	186248.286130	57.462388
2593.435097	186044.066658	57.467393
2593.130965	185841.417448	57.472397
2592.524206	185637.595797	57.477402
2591.827513	185438.165577	57.482407
2591.245057	185225.792918	57.487412
2590.340421	185028.700064	57.492417
2589.773198	184824.659521	57.497421
2589.054015	184622.908403	57.502426
2588.615692	184418.251359	57.507431
2587.847140	184211.561265	57.512436
2587.268725	184011.940491	57.517441
2586.849724	183797.487795	57.522445
2585.879501	183583.021702	57.527450
2585.266262	183385.317421	57.532455
2584.645406	183175.924548	57.537460
2583.951824	182968.719481	57.542465
2583.278561	182753.968631	57.547469
2582.293931	182550.704253	57.552474
2581.517469	182347.903939	57.557479
2581.071994	182145.344689	57.562484
2580.224301	181941.221855	57.567489
2580.106281	181731.692551	57.572493
2579.209823	181538.048434	57.577498
2578.495512	181332.164583	57.582503
2578.034578	181122.908787	57.587508
2577.318749	180913.058367	57.592513
2576.716009	180707.058034	57.597517
2575.571978	180508.674878	57.602522
2575.101203	180291.118299	57.607527
2574.507556	180098.361207	57.612532
2573.538173	179897.231073	57.617537
2573.678996	179686.093346	57.622541
2572.679489	179487.920962	57.627546
2572.030802	179283.766412	57.632551
2571.264977	179080.661713	57.637556
2570.536600	178870.428949	57.642561
2570.098073	178658.675803	57.647565
2569.375870	178457.309782	57.652570
2568.724747	178246.202936	57.657575
2568.193632	178033.475464	57.662580
2567.361120	177838.527823	57.667585
2566.964613	177624.661773	57.672589
2565.821421	177420.136689	57.677594
2565.186101	177219.653189	57.682599
2564.406577	177008.496605	57.687604
2563.607839	176806.998007	57.692609
2563.452792	176602.765522	57.697613
2562.666917	176410.043018	57.702618
2562.036756	176201.143588	57.707623
2561.517717	175990.892116	57.712628
2560.601160	175789.633367	57.717633
2560.344624	175579.711246	57.722637
2559.533924	175382.571334	57.727642
2558.930763	175176.114836	57.732647
2558.397887	174957.972542	57.737652
2557.537430	174740.188572	57.742657
2556.872685	174541.045502	57.747661
2556.167891	174322.857547	57.752666
2555.418608	174130.648715	57.757671
2555.017890	173915.708825	57.762676
2554.162141	173715.315539	57.767681
2553.131214	173503.491939	57.772685
2553.043113	173296.429234	57.777690
2552.037066	173089.614810	57.782695
2551.789260	172874.668974	57.787700
2550.750623	172678.328734	57.792705
2550.223725	172463.124113	57.797709
2549.256253	172262.565042	57.802714
2548.808174	172058.529048	57.807719
2547.909033	171842.343932	57.812724
2547.135053	171644.326293	57.817729
2546.735570	171441.379494	57.822733
2545.811020	171244.888391	57.827738
2545.626325	171044.834612	57.832743
2544.859054	170834.166196	57.837748
2544.111545	170634.369029	57.842753
2543.665706	170419.442499	57.847757
2542.935675	170223.307215	57.852762
2542.092649	170011.943085	57.857767
2541.366079	169807.441535	57.862772
2540.817517	169603.167194	57.867777
2540.229965	169400.222661	57.872781
2539.719704	169188.772140	57.877786
2539.216597	168973.392183	57.882791
2538.442882	168768.166043	57.887796
2537.411945	168562.231486	57.892801
2537.044896	168350.381386	57.897805
2536.150537	168152.209890	57.902810
2535.674898	167937.925016	57.907815
2534.958542	167727.430801	57.912820
2534.300798	167522.294709	57.917825
2533.629190	167318.713294	57.922829
2532.849799	167116.497960	57.927834
2532.162558	166913.391700	57.932839
2531.866270	166702.951054	57.937844
2530.865322	166495.611490	57.942849
2530.721913	166287.043607	57.947853
2530.048887	166081.879626	57.952858
2529.094739	165871.446173	57.957863
2528.634990	165648.830312	57.962868
2527.537955	165449.662466	57.967873
2526.892828	165238.662277	57.972877
2526.220561	165032.384993	57.977882
2525.672961	164833.057088	57.982887
2525.322627	164586.538196	57.987892
2524.307700	164360.928251	57.992897
2524.204682	164133.865514	57.997901
2523.396354	163936.058726	58.002906
2522.081939	163726.775340	58.007911
2521.959701	163514.405225	58.012916
2521.025745	163305.496259	58.017921
2520.766584	163095.349936	58.022925
2519.794051	162888.420254	58.027930
2519.118047	162677.833821	58.032935
2518.368817	162464.602887	58.037940
2517.936721	162269.835136	58.042945
2517.064937	162050.879148	58.047949
2516.666865	161838.460829	58.052954
2515.584586	161640.964238	58.057959
2515.419534	161425.701588	58.062964
2514.582818	161213.267485	58.067969
2514.073995	161009.885879	58.072973
2513.031349	160800.703499	58.077978
2512.399706	160593.262570	58.082983
2511.818545	160384.022210	58.087988
2510.941345	160182.763334	58.092993
2510.977859	159970.261811	58.097997
2509.988725	159762.259428	58.103002
2508.964711	159549.381832	58.108007
2508.378340	159344.928695	58.113012
2507.796350	159136.979891	58.118017
2506.716627	158938.252014	58.123021
2506.503538	158730.539552	58.128026
2505.844032	158520.191189	58.133031
2505.230861	158312.442913	58.138036
2504.620949	158115.450493	58.143041
2503.985348	157899.025304	58.148045
2503.390455	157694.977251	58.153050
2502.319099	157488.031142	58.158055
2501.872395	157275.342860	58.163060
2501.565941	157075.447905	58.168065
2501.076435	156861.726521	58.173069
2499.623357	156655.850181	58.178074
2499.111157	156444.524914	58.183079
2498.762162	156237.560802	58.188084
2497.813892	156027.425895	58.193089
2497.176588	155829.332185	58.198093
2496.438738	155614.157904	58.203098
2495.702386	155410.527177	58.208103
2495.167831	155205.492802	58.213108
2494.480245	154997.013603	58.218113
2494.080710	154794.489952	58.223117
2493.375693	154581.058510	58.228122
2492.514919	154376.474913	58.233127
2491.814837	154175.032242	58.238132
2491.442774	153969.178778	58.243137
2490.811507	153754.469737	58.248141
2489.972363	153547.892071	58.253146
2489.195687	153349.580740	58.258151
2488.599193	153125.502094	58.263156
2487.856225	152926.959127	58.268161
2487.430864	152712.783416	58.273165
2486.688706	152519.301695	58.278170
2485.941727	152312.424717	58.283175
2485.413559	152098.421788	58.288180
2484.560562	151900.347267	58.293185
2483.992974	151688.984328	58.298189
2483.350176	151476.757641	58.303194
2482.839193	151280.030781	58.308199
2482.154196	151060.225380	58.313204
2481.284142	150854.152376	58.318209
2481.071862	150639.676700	58.323213
2480.070853	150435.647993	58.328218
2479.250556	150240.171142	58.333223
2478.717441	150023.678636	58.338228
2477.886552	149821.050316	58.343233
2477.268296	149612.479537	58.348237
2476.862946	149404.448285	58.353242
2475.816807	149206.115650	58.358247
2475.525135	149007.804449	58.363252
2474.834679	148797.598129	58.368257
2473.960376	148569.819923	58.373261
2473.135335	148377.837408	58.378266
2472.676615	148171.017231	58.383271
2471.991948	147962.734529	58.388276
2471.412017	147758.261986	58.393281
2470.798890	147550.135846	58.398285
2469.731962	147348.882213	58.403290
2469.332842	147141.500056	58.408295
2468.954232	146943.825414	58.413300
2467.892709	146736.919441	58.418305
2467.465233	146534.870630	58.423309
2466.684013	146321.111187	58.428314
2466.229656	146122.157415	58.433319
2465.574811	145915.179645	58.438324
2464.945939	145713.396757	58.443329
2464.344312	145505.472838	58.448333
2463.621846	145288.673850	58.453338
2463.045005	145086.492792	58.458343
2462.308440	144877.895486	58.463348
2461.398804	144673.698470	58.468353
2460.695056	144456.800616	58.473357
2460.227336	144248.025119	58.478362
2459.424193	144057.526735	58.483367
2458.896864	143836.195740	58.488372
2458.147706	143642.959251	58.493377
2457.489977	143427.255777	58.498381
2456.685867	143227.588023	58.503386
2456.296103	143016.152669	58.508391
2455.704732	142818.486972	58.513396
2454.772182	142602.044998	58.518401
2454.371766	142405.508014	58.523405
2453.722766	142192.924969	58.528410
2452.669621	141991.741789	58.533415
2452.330689	141782.352640	58.538420
2451.686656	141584.220399	58.543425
2451.153795	141372.590342	58.548429
2450.492112	141158.555274	58.553434
2449.749858	140948.676709	58.558439
2449.365344	140733.723970	58.563444
2448.248193	140541.137158	58.568449
2447.706749	140304.904319	58.573453
2446.951107	140113.457286	58.578458
2446.014487	139905.179592	58.583463
2445.558464	139707.017117	58.588468
2444.741301	139497.783088	58.593473
2444.097098	139305.624723	58.598477
2443.531989	139090.229523	58.603482
2442.891563	138891.733207	58.608487
2442.598370	138667.671018	58.613492
2441.437727	138472.715781	58.618497
2441.060610	138264.170232	58.623501
2440.505703	138052.160457	58.628506
2439.744728	137856.955327	58.633511
2439.189463	137649.890690	58.638516
2438.454087	137439.120863	58.643521
2437.978545	137225.427398	58.648525
2437.198311	137011.135849	58.653530
2436.468326	136813.544244	58.658535
2435.750248	136600.427345	58.663540
2434.886584	136390.892266	58.668545
2434.508881	136195.192727	58.673549
2433.652718	135978.697513	58.678554
2432.925200	135773.642516	58.683559
2432.495285	135573.648756	58.688564
2431.775515	135367.528255	58.693569
2431.004583	135156.145275	58.698573
2430.471303	134959.119386	58.703578
2429.687989	134750.205830	58.708583
2429.235987	134529.134858	58.713588
2428.507449	134328.180732	58.718593
2428.146332	134127.461933	58.723597
2427.447469	133916.051170	58.728602
2426.556591	133695.170483	58.733607
2426.080451	133495.643002	58.738612
2425.328035	133281.984253	58.743617
2424.475786	133080.994929	58.748621
2424.004057	132866.646935	58.753626
2423.082027	132657.262446	58.758631
2422.969299	132448.360917	58.763636
2421.931458	132238.235709	58.768641
2421.523413	132037.793026	58.773645
2421.136570	131804.601967	58.778650
2420.196049	131605.085097	58.783655
2419.605936	131387.019869	58.788660
2418.702713	131166.757710	58.793665
2417.980868	130973.332977	58.798669
2417.400885	130751.854237	58.803674
2416.710172	130542.004131	58.808679
2416.445104	130326.893162	58.813684
2415.327793	130127.529083	58.818689
2414.855463	129901.619853	58.823693
2414.332066	129683.481031	58.828698
2413.198811	129488.239253	58.833703
2412.662890	129257.734766	58.838708
2412.116261	129061.018557	58.843713
2411.340992	128844.513850	58.848717
2410.427619	128639.107837	58.853722
2410.109001	128426.153729	58.858727
2409.433747	128224.307342	58.863732
2408.541148	128013.161989	58.868737
2407.904881	127803.679471	58.873741
2407.121296	127601.702399	58.878746
2406.309397	127388.707480	58.883751
2405.760884	127181.730424	58.888756
2405.352230	126983.571995	58.893761
2404.650307	126781.422899	58.898765
2403.900125	126571.510624	58.903770
2403.277969	126367.027865	58.908775
2402.838657	126141.347290	58.913780
2402.067503	125946.301759	58.918785
2401.213904	125740.742820	58.923789
2400.953995	125521.655364	58.928794
2400.061681	125327.116056	58.933799
2399.423390	125101.970915	58.938804
2398.625837	124910.594368	58.943809
2398.233084	124695.915828	58.948813
2397.605781	124487.371648	58.953818
2396.628614	124281.614788	58.958823
2396.624417	124054.447626	58.963828
2395.991559	123849.947442	58.968833
2395.048197	123635.631310	58.973837
2394.704774	123410.186874	58.978842
2393.556294	123208.224117	58.983847
2392.792217	122990.646657	58.988852
2392.156048	122779.285450	58.993857
2391.431735	122573.577799	58.998861
2390.987185	122357.173853	59.003866
2389.900195	122163.043860	59.008871
2389.525267	121934.582110	59.013876
2389.026781	121733.454415	59.018881
2388.178964	121522.428798	59.023885
2387.883405	121304.130588	59.028890
2386.924495	121108.464332	59.033895
2386.487104	120885.633740	59.038900
2385.691421	120679.660072	59.043905
2384.907486	120467.807452	59.048909
2384.268224	120253.686256	59.053914
2383.562889	120058.178062	59.058919
2383.468962	119834.705175	59.063924
2382.440075	119622.872824	59.068929
2381.939522	119409.885574	59.073933
2381.288386	119200.618578	59.078938
2380.601484	118978.465880	59.083943
2379.831329	118762.720791	59.088948
2379.314962	118553.653464	59.093953
2378.735728	118336.402556	59.098957
2378.032794	118124.149850	59.103962
2377.028163	117909.496442	59.108967
2376.813629	117683.217310	59.113972
2375.847519	117474.160184	59.118977
2375.147162	117259.286205	59.123981
2374.817682	117044.183831	59.128986
2373.845909	116828.689979	59.133991
2373.233607	116608.304112	59.138996
2372.603276	116402.077909	59.144001
2371.954779	116180.127286	59.149005
2371.562944	115967.995387	59.154010
2370.567921	115755.802204	59.159015
2370.008738	115528.936592	59.164020
2369.182592	115322.921533	59.169025
2368.418323	115094.626102	59.174029
2368.227369	114890.329130	59.179034
2367.357351	114675.586299	59.184039
2366.611480	114453.285357	59.189044
2366.067449	114245.495243	59.194049
2365.393639	114031.247227	59.199053
2364.916032	113793.657954	59.204058
2364.267645	113587.914449	59.209063
2363.604709	113360.970484	59.214068
2362.954076	113141.090473	59.219073
2362.034253	112932.298199	59.224077
2361.474654	112706.137105	59.229082
2361.000052	112490.353821	59.234087
2360.137761	112267.754311	59.239092
2359.612234	112058.310256	59.244097
2358.821725	111831.019620	59.249101
2358.113749	111607.183049	59.254106
2357.320444	111401.696297	59.259111
2356.824846	111175.132798	59.264116
2356.559085	110959.494682	59.269121
2355.960736	110734.430155	59.274125
2355.383895	110506.870287	59.279130
2354.496771	110286.240726	59.284135
2353.408169	110055.618578	59.289140
2353.070700	109848.987320	59.294145
2352.350167	109624.808993	59.299149
2351.952106	109395.289251	59.304154
2350.544824	109186.250497	59.309159
2350.062352	108953.017035	59.314164
2349.456401	108740.783759	59.319169
2349.070301	108521.366097	59.324173
2348.277602	108300.650612	59.329178
2347.565306	108092.247109	59.334183
2347.036921	107859.659583	59.339188
2346.513548	107657.714771	59.344193
2345.834802	107414.793531	59.349197
2345.274583	107202.877349	59.354202
2344.397773	106984.300116	59.359207
2344.008355	106758.661699	59.364212
2343.243927	106533.402105	59.369217
2342.491965	106313.078985	59.374221
2341.847699	106080.628479	59.379226
2341.210482	105867.587833	59.384231
2340.771456	105633.154921	59.389236
2339.836682	105413.465455	59.394241
2339.140217	105186.805554	59.399245
2338.519722	104965.376363	59.404250
2338.024903	104748.440238	59.409255
2337.605792	104527.725486	59.414260
2336.946884	104296.201912	59.419265
2335.977725	104066.620398	59.424269
2335.253970	103842.496320	59.429274
2334.496538	103625.535961	59.434279
2333.972047	103392.800842	59.439284
2333.153970	103167.473698	59.444289
2333.027236	102935.580873	59.449293
2332.427462	102710.388424	59.454298
2331.468841	102488.090754	59.459303
2330.797318	102256.316382	59.464308
2330.271260	102026.614677	59.469313
2329.539725	101793.033737	59.474317
2328.881175	101567.944039	59.479322
2328.074671	101345.823394	59.484327
2327.495514	101110.747055	59.489332
2326.472728	100893.619303	59.494337
2326.162900	100666.573623	59.499341
2325.419277	100436.941088	59.504346
2324.527509	100222.482062	59.509351
2323.903526	99991.439443	59.514356
2323.058217	99766.136721	59.519361
2322.698298	99541.063692	59.524365
2322.231109	99320.614906	59.529370
2321.512304	99098.539925	59.534375
2320.794971	98854.818509	59.539380
2320.254816	98643.426412	59.544385
2319.449853	98406.542204	59.549389
2319.340565	98184.607735	59.554394
2318.056720	97949.586491	59.559399
2317.683789	97721.704506	59.564404
2316.911250	97488.357477	59.569409
2316.176700	97267.013091	59.574413
2315.677523	97029.289164	59.579418
2314.828097	96817.220926	59.584423
2314.110563	96573.251133	59.589428
2313.594183	96357.849073	59.594433
2312.808437	96115.112726	59.599437
2312.439122	95898.702333	59.604442
2311.569600	95665.744557	59.609447
2311.150355	95433.516866	59.614452
2310.231402	95211.562222	59.619457
2309.466279	94976.464134	59.624461
2308.856037	94749.810189	59.629466
2308.022114	94521.855903	59.634471
2307.495463	94298.884119	59.639476
2307.181818	94074.599778	59.644481
2306.184133	93851.066649	59.649485
2305.661045	93607.675204	59.654490
2305.093880	93385.961864	59.659495
2304.363680	93155.652401	59.664500
2303.609718	92931.905934	59.669505
2302.998452	92707.485947	59.674509
2302.345008	92459.891806	59.679514
2301.836031	92242.143832	59.684519
2301.140112	91995.639589	59.689524
2300.609449	91778.806368	59.694529
2299.709893	91553.917485	59.699533
2299.302608	91306.785452	59.704538
2298.507535	91087.122243	59.709543
2297.865847	90852.460286	59.714548
2297.384370	90620.647708	59.719553
2296.438025	90393.394042	59.724557
2296.002844	90154.097242	59.729562
2295.038275	89936.932513	59.734567
2294.575734	89704.017058	59.739572
2293.856149	89463.378045	59.744577
2293.298765	89240.734752	59.749581
2292.660935	89004.665447	59.754586
2291.644092	88773.407503	59.759591
2291.220081	88545.411853	59.764596
2290.371298	88312.001936	59.769601
2289.692016	88093.662823	59.774605
2289.294424	87845.072191	59.779610
2288.231760	87622.525624	59.784615
2287.576672	87386.971164	59.789620
2286.986041	87165.267360	59.794625
2286.573256	86936.583192	59.799629
2285.806942	86694.169240	59.804634
2285.173619	86486.425963	59.809639
2284.259952	86248.040561	59.814644
2283.599264	86026.023634	59.819649
2282.914807	85795.549984	59.824653
2282.552375	85564.520618	59.829658
2281.754924	85339.889097	59.834663
2281.312854	85113.644194	59.839668
2280.541398	84890.357148	59.844673
2279.683327	84663.010309	59.849677
2279.123502	84427.904326	59.854682
2278.629857	84207.160274	59.859687
2277.768150	83978.458523	59.864692
2277.018051	83743.523413	59.869697
2276.290446	83512.726380	59.874701
2275.992381	83282.554632	59.879706
2275.152857	83064.748659	59.884711
2274.467731	82827.861219	59.889716
2273.706587	82610.326398	59.894721
2272.752948	82378.164213	59.899725
2272.541079	82157.092681	59.904730
2272.084347	81936.220762	59.909735
2271.283104	81706.811551	59.914740
2270.782084	81462.856184	59.919745
2269.794474	81242.747593	59.924750
2269.388853	81013.352966	59.929754
2268.277892	80785.365610	59.934759
2267.882544	80552.317594	59.939764
2267.224360	80312.893962	59.944769
2266.563627	80102.391296	59.949774
2265.940083	79859.976112	59.954778
2265.365319	79648.881376	59.959783
2264.470861	79407.338308	59.964788
2263.974365	79168.485279	59.969793
2263.293429	78952.927769	59.974798
2262.791801	78724.365819	59.979802
2261.775044	78497.801867	59.984807
2261.296473	78263.753560	59.989812
2260.834182	78023.831102	59.994817
2259.703048	77802.121620	59.999822
2259.179482	77578.017960	60.004826
2258.479373	77349.597835	60.009831
2257.915563	77116.336535	60.014836
2257.253046	76898.611569	60.019841
2256.336148	76679.902775	60.024846
2256.211239	76441.757570	60.029850
2255.344501	76207.186065	60.034855
2254.818384	75979.469685	60.039860
2254.141959	75741.515192	60.044865
2253.396593	75520.973193	60.049870
2252.431329	75298.567680	60.054874
2251.851283	75071.174180	60.059879
2251.253819	74842.620208	60.064884
2250.573058	74613.777917	60.069889
2250.057510	74395.765054	60.074894
2249.512057	74159.189591	60.079898
2248.492503	73940.190881	60.084903
2247.908617	73720.529922	60.089908
2247.450540	73484.347679	60.094913
2246.745290	73259.458967	60.099918
2246.195546	73036.930174	60.104922
2245.222995	72810.638126	60.109927
2244.822066	72574.932684	60.114932
2244.069355	72351.221041	60.119937
2243.054709	72136.137345	60.124942
2243.090777	71894.599468	60.129946
2242.380880	71669.285964	60.134951
2241.532032	71432.835217	60.139956
2240.857029	71202.884433	60.144961
2239.900366	70973.886839	60.149966
2239.622163	70748.895395	60.154970
2238.853633	70520.405309	60.159975
2237.887878	70286.425563	60.164980
2237.553453	70060.842769	60.169985
2236.923023	69826.644265	60.174990
2236.267428	69597.393186	60.179994
2235.510104	69377.636717	60.184999
2234.986997	69144.278085	60.190004
2234.445901	68910.627385	60.195009
2233.599522	68684.938894	60.200014
2233.227274	68450.316822	60.205018
2232.338589	68225.501738	60.210023
2231.485661	67984.089419	60.215028
2231.014948	67757.788356	60.220033
2230.145053	67533.959966	60.225038
2229.484486	67297.909110	60.230042
2229.136022	67066.726290	60.235047
2228.302912	66839.157058	60.240052
2227.911758	66618.189252	60.245057
2226.851962	66389.730272	60.250062
2226.243608	66148.485626	60.255066
2225.221515	65923.658174	60.260071
2224.623182	65693.541486	60.265076
2224.475763	65470.831914	60.270081
2223.571119	65241.510147	60.275086
2223.193967	65001.864349	60.280090
2222.466505	64780.214171	60.285095
2221.522762	64556.941737	60.290100
2221.143623	64320.945950	60.295105
2220.074888	64094.238052	60.300110
2219.610196	63860.154890	60.305114
2218.986308	63643.143008	60.310119
2218.279780	63414.239100	60.315124
2217.842848	63185.690928	60.320129
2216.539303	62955.440352	60.325134
2216.172484	62725.227603	60.330138
2215.629980	62503.267401	60.335143
2214.990626	62280.929421	60.340148
2214.423682	62049.680202	60.345153
2213.531474	61814.797235	60.350158
2213.168107	61590.017569	60.355162
2212.241443	61368.543144	60.360167
2211.539283	61142.483437	60.365172
2211.052700	60902.194285	60.370177
2210.166643	60676.818290	60.375182
2209.706456	60460.402503	60.380186
2208.813716	60230.145266	60.385191
2208.113445	60015.032575	60.390196
2207.532940	59783.734151	60.395201
2206.517938	59566.593652	60.400206
2206.139027	59332.856761	60.405210
2205.528924	59117.626116	60.410215
2204.693854	58886.432973	60.415220
2204.227949	58672.463370	60.420225
2203.398665	58454.429556	60.425230
2202.674041	58223.062526	60.430234
2202.069399	58002.719425	60.435239
2201.294226	57783.478964	60.440244
2200.726646	57554.570472	60.445249
2199.960938	57342.914097	60.450254
2199.624769	57120.206243	60.455258
2198.678815	56899.344863	60.460263
2197.970645	56684.414308	60.465268
2197.674680	56459.017841	60.470273
2196.633635	56240.166985	60.475278
2196.153504	56010.880780	60.480282
2195.449220	55807.615870	60.485287
2194.991854	55578.901095	60.490292
2194.141343	55357.463903	60.495297
2193.720295	55140.081659	60.500302
2193.221689	54904.384739	60.505306
2192.150386	54683.873639	60.510311
2191.609526	54464.012064	60.515316
2191.035135	54243.633142	60.520321
2190.228687	54007.436494	60.525326
2189.554526	53787.385862	60.530330
2189.080462	53572.748913	60.535335
2188.433539	53343.364343	60.540340
2187.854071	53116.936935	60.545345
2186.738955	52904.055018	60.550350
2186.314140	52673.029893	60.555354
2185.813897	52462.406654	60.560359
2184.750472	52245.094387	60.565364
2184.547918	52012.185063	60.570369
2183.632678	51792.563899	60.575374
2182.910580	51561.343835	60.580378
2182.380853	51355.364013	60.585383
2181.440054	51135.691623	60.590388
2181.318715	50914.936409	60.595393
2180.317171	50687.176294	60.600398
2179.913619	50459.656408	60.605402
2178.851372	50240.023725	60.610407
2178.338591	50023.422890	60.615412
2177.715082	49793.092627	60.620417
2176.958493	49567.883159	60.625422
2176.409960	49346.636060	60.630426
2175.603202	49139.874600	60.635431
2174.775819	48914.931362	60.640436
2174.577546	48683.715926	60.645441
2173.368313	48482.843695	60.650446
2172.765188	48259.227147	60.655450
2172.036718	48046.543960	60.660455
2171.491885	47836.630627	60.665460
2171.196321	47602.012418	60.670465
2170.082834	47393.184678	60.675470
2169.774704	47171.357117	60.680474
2168.696858	46966.125408	60.685479
2167.984548	46748.400402	60.690484
2167.550361	46526.705319	60.695489
2166.547836	46324.410864	60.700494
2165.846786	46104.041336	60.705498
2165.321992	45896.362037	60.710503
2164.427188	45689.212017	60.715508
2164.291584	45470.101845	60.720513
2163.113135	45263.435177	60.725518
2162.711351	45047.124266	60.730522
2161.992540	44842.442362	60.735527
2161.386149	44632.017158	60.740532
2160.782423	44413.177915	60.745537
2159.765319	44211.792567	60.750542
2159.432813	43992.539204	60.755546
2158.572610	43795.618482	60.760551
2157.931280	43584.344887	60.765556
2157.108520	43365.752791	60.770561
2156.600229	43164.428505	60.775566
2156.015565	42946.164445	60.780570
2155.038117	42740.454045	60.785575
2154.350565	42542.305753	60.790580
2153.996489	42340.122199	60.795585
2153.209424	42139.454901	60.800590
2152.788303	41915.589991	60.805594
2151.724094	41716.859477	60.810599
2150.901359	41513.947237	60.815604
2150.369615	41311.288468	60.820609
2149.492430	41105.793499	60.825614
2149.190301	40908.779140	60.830618
2148.375603	40697.473455	60.835623
2147.724489	40497.995819	60.840628
2146.988019	40298.954593	60.845633
2146.289376	40113.939422	60.850638
2145.870281	39901.445627	60.855642
2145.227483	39690.643640	60.860647
2144.147574	39496.415425	60.865652
2143.972647	39293.782374	60.870657
2142.990958	39097.166997	60.875662
2142.045981	38901.253139	60.880666
2141.679731	38701.945708	60.885671
2140.821895	38504.784769	60.890676
2140.213780	38304.048603	60.895681
2139.309116	38112.786644	60.900686
2138.869411	37917.803022	60.905690
2138.156747	37725.332535	60.910695
2137.147664	37539.645284	60.915700
2136.917643	37335.424026	60.920705
2136.156803	37150.273888	60.925710
2135.627653	36949.436906	60.930714
2134.750794	36758.647394	60.935719
2133.964043	36572.113541	60.940724
2133.770172	36376.324669	60.945729
2132.794198	36198.717696	60.950734
2132.175066	35990.973756	60.955738
2131.264748	35799.620329	60.960743
2130.260158	35610.349851	60.965748
2129.749440	35427.929156	60.970753
2129.044682	35246.095999	60.975758
2128.799291	35056.439460	60.980762
2127.777878	34873.298177	60.985767
2126.894943	34694.314161	60.990772
2126.144172	34510.280447	60.995777
2125.415865	34344.145435	61.000782
2124.721671	34151.354135	61.005786
2124.247744	33975.165620	61.010791
2122.987232	33808.404452	61.015796
2122.531000	33627.940223	61.020801
2121.587202	33468.667502	61.025806
2120.834574	33300.014998	61.030810
2120.209710	33130.466844	61.035815
2119.616301	32968.940321	61.040820
2118.719302	32806.983125	61.045825
2117.919498	32641.026586	61.050830
2117.234938	32485.009183	61.055834
2116.684194	32329.551974	61.060839
2115.720592	32181.592069	61.065844
2114.939900	32031.749269	61.070849
2114.091064	31881.322895	61.075854
2113.617187	31727.652699	61.080858
2112.877151	31572.531301	61.085863
2112.148797	31435.372979	61.090868
2111.344244	31279.185315	61.095873
2110.657629	31135.098589	61.100878
2109.715649	30998.864261	61.105882
2109.141582	30863.165232	61.110887
2107.934864	30732.113687	61.115892
2107.056196	30593.812204	61.120897
2106.242518	30473.396053	61.125902
2105.594736	30351.206898	61.130906
2104.901366	30233.669695	61.135911
2103.922619	30125.690536	61.140916
2103.241863	30003.441262	61.145921
2102.289345	29900.776267	61.150926
2101.050827	29789.859023	61.155930
2100.775477	29692.629022	61.160935
2099.667255	29597.606296	61.165940
2099.312571	29502.369758	61.170945
2098.243451	29401.285856	61.175950
2097.756849	29308.907448	61.180954
2097.112285	29213.186139	61.185959
2096.145043	29127.269667	61.190964
2095.605423	29038.302852	61.195969
2094.627979	28949.099485	61.200974
2093.829483	28868.974940	61.205978
2093.470680	28773.751205	61.210983
2092.601261	28699.775169	61.215988
2091.739121	28614.154392	61.220993
2091.009081	28546.042097	61.225998
2090.642651	28459.261244	61.231002
2089.947021	28389.058688	61.236007
2088.850408	28315.989388	61.241012
2088.996536	28235.653296	61.246017
2088.048486	28166.408082	61.251022
2087.331540	28092.875096	61.256026
2086.815346	28019.132065	61.261031
2086.202531	27945.439457	61.266036
2085.521809	27860.816021	61.271041
2084.837428	27790.497361	61.276046
2084.005496	27712.971582	61.281050
2083.459249	27641.631623	61.286055
2082.870723	27570.562514	61.291060
2082.714419	27487.529247	61.296065
2081.619944	27413.815959	61.301070
2081.084707	27332.063216	61.306074
2080.313077	27255.139857	61.311079
2079.506801	27181.937976	61.316084
2079.035321	27101.782904	61.321089
2078.387891	27031.815543	61.326094
2077.618577	26956.411381	61.331098
2077.101842	26882.923208	61.336103
2076.314266	26812.061210	61.341108
2075.952555	26725.704353	61.346113
2075.105506	26661.789811	61.351118
2074.539788	26584.990201	61.356122
2073.976172	26508.136122	61.361127
2073.109610	26433.782960	61.366132
2072.536198	26361.151293	61.371137
2071.718107	26292.166773	61.376142
2071.249561	26213.240690	61.381146
2070.562306	26137.387396	61.386151
2069.810714	26067.720348	61.391156
2069.206943	25997.959849	61.396161
2068.454372	25921.659049	61.401166
2067.864320	25849.258221	61.406170
2067.457235	25779.784964	61.411175
2066.826437	25715.974132	61.416180
2066.452192	25623.639179	61.421185
2065.521582	25554.483756	61.426190
2064.842159	25489.322286	61.431194
2064.192487	25405.978374	61.436199
2063.435767	25338.510148	61.441204
2062.867304	25259.072281	61.446209
2062.387852	25177.336619	61.451214
2061.628394	25116.534768	61.456218
2061.449328	25023.016842	61.461223
2060.383917	24957.438600	61.466228
2059.949347	24873.996976	61.471233
2058.906385	24794.432948	61.476238
2058.274247	24726.464192	61.481242
2057.745893	24641.315397	61.486247
2056.714283	24579.593688	61.491252
2056.212056	24499.888453	61.496257
2055.901332	24436.416531	61.501262
2055.105512	24351.981429	61.506266
2054.683244	24280.567983	61.511271
2053.714497	24202.420609	61.516276
2053.755524	24125.600445	61.521281
2052.717162	24061.026923	61.526286
2051.745047	23963.618934	61.531290
2051.326625	23897.025503	61.536295
2050.298241	23817.363735	61.541300
2049.808324	23744.681707	61.546305
2049.181854	23670.694175	61.551310
2048.338367	23594.145656	61.556314
2047.718198	23514.998685	61.561319
2047.057023	23456.096275	61.566324
2046.894149	23367.471339	61.571329
2045.842893	23303.759757	61.576334
2045.215006	23232.574740	61.581338
2044.781670	23151.722624	61.586343
2043.668539	23084.878000	61.591348
2043.234491	23015.741637	61.596353
2042.558650	22947.834777	61.601358
2042.123004	22866.121363	61.606362
2041.334795	22790.292071	61.611367
2040.687527	22715.995622	61.616372
2039.999546	22647.121478	61.621377
2039.285297	22564.909751	61.626382
2038.126830	22500.556678	61.631386
2037.762528	22421.429823	61.636391
2037.040848	22361.750634	61.641396
2036.284993	22284.461728	61.646401
2035.635096	22221.064304	61.651406
2035.248842	22156.453473	61.656410
2034.632011	22089.852509	61.661415
2033.808554	22026.237834	61.666420
2033.371281	21930.781250	61.671425
2032.501428	21874.958676	61.676430
2031.582346	21803.711000	61.681434
2031.289948	21725.072880	61.686439
2030.443979	21656.839279	61.691444
2030.027665	21592.787458	61.696449
2029.420334	21528.084782	61.701454
2028.804941	21450.595259	61.706458
2028.639888	21372.193725	61.711463
2027.716045	21303.823985	61.716468
2026.944363	21223.093041	61.721473
2026.317492	21146.135860	61.726478
2025.519416	21065.398859	61.731482
2024.951248	21001.404330	61.736487
2023.989449	20939.948642	61.741492
2023.313953	20859.795688	61.746497
2022.528148	20789.877660	61.751502
2021.850770	20725.716035	61.756506
2021.451386	20656.684750	61.761511
2020.542556	20592.527240	61.766516
2020.083445	20518.356540	61.771521
2019.466247	20448.046920	61.776526
2018.549625	20383.213276	61.781530
2017.911928	20307.093308	61.786535
2017.050106	20253.009839	61.791540
2016.547624	20182.687937	61.796545
2016.098862	20114.738270	61.801550
2015.398087	20047.946474	61.806554
2014.777974	19977.712848	61.811559
2013.920519	19916.419881	61.816564
2013.674826	19848.345579	61.821569
2013.099081	19784.035873	61.826574
2011.931424	19710.202111	61.831578
2011.348336	19642.653589	61.836583
2010.651294	19571.495657	61.841588
2010.135990	19501.263320	61.846593
2009.779676	19443.291484	61.851598
2008.983001	19374.966012	61.856602
2008.084846	19289.138873	61.861607
2007.512370	19229.914470	61.866612
2006.655991	19155.188381	61.871617
2006.203595	19087.797566	61.876622
2005.066129	19027.068846	61.881626
2004.405456	18962.737703	61.886631
2003.703090	18898.454101	61.891636
2003.531269	18842.241787	61.896641
2002.810874	18774.654858	61.901646
2002.071800	18717.249746	61.906650
2001.772576	18641.566513	61.911655
2000.902759	18574.134033	61.916660
2000.303665	18507.160970	61.921665
1999.917653	18443.603090	61.926670
1998.551145	18378.106289	61.931674
1998.482326	18302.096037	61.936679
1997.806955	18238.835565	61.941684
1997.168066	18161.555481	61.946689
1996.243892	18098.402171	61.951694
1995.379169	18026.430041	61.956698
1995.207432	17950.736634	61.961703
1994.179036	17900.516466	61.966708
1993.493198	17824.400828	61.971713
1992.895247	17756.998997	61.976718
1992.250603	17692.850932	61.981722
1991.696590	17623.885588	61.986727
1991.114290	17566.533252	61.991732
1990.444841	17489.358454	61.996737
1989.736521	17426.087571	62.001742
1989.130178	17362.678800	62.006746
1988.614847	17280.746965	62.011751
1987.784579	17219.144926	62.016756
1987.084608	17145.121213	62.021761
1986.655716	17074.100259	62.026766
1985.674529	17010.574021	62.031770
1985.130014	16937.259563	62.036775
1984.279019	16872.724141	62.041780
1983.648185	16812.715801	62.046785
1982.897581	16749.824406	62.051790
1982.256073	16691.624689	62.056794
1981.842045	16621.230204	62.061799
1980.870230	16561.057124	62.066804
1980.385348	16498.660348	62.071809
1979.998413	16422.222743	62.076814
1979.065781	16358.319300	62.081818
1978.585449	16299.663705	62.086823
1977.854576	16226.918350	62.091828
1977.431393	16157.919619	62.096833
1976.519323	16084.137897	62.101838
1975.985765	16014.904146	62.106842
1975.106418	15949.048446	62.111847
1974.239708	15887.177288	62.116852
1973.586788	15821.962837	62.121857
1973.012459	15771.405793	62.126862
1972.202462	15694.238769	62.131866
1971.687495	15643.106787	62.136871
1971.008685	15579.021842	62.141876
1970.366354	15517.784502	62.146881
1969.606447	15456.607704	62.151886
1969.118476	15382.085203	62.156890
1968.709641	15313.887129	62.161895
1967.523784	15258.858639	62.166900
1967.109353	15195.398302	62.171905
1966.540253	15126.338748	62.176910
1965.737790	15062.813080	62.181914
1965.478340	15000.116154	62.186919
1964.379700	14936.705404	62.191924
1963.891851	14863.279129	62.196929
1963.435168	14809.494544	62.201934
1962.452240	14746.370376	62.206938
1961.959903	14675.382164	62.211943
1961.092380	14611.125012	62.216948
1960.359568	14541.468192	62.221953
1960.097571	14487.647913	62.226958
1959.335749	14424.464126	62.231962
1958.926285	14352.271208	62.236967
1958.147672	14300.167517	62.241972
1957.493573	14211.871786	62.246977
1956.868453	14157.150495	62.251982
1955.969625	14093.516182	62.256986
1955.488162	14021.086954	62.261991
1954.691671	13962.361510	62.266996
1953.841735	13889.027188	62.272001
1953.104792	13816.319946	62.277006
1952.492103	13767.788477	62.282010
1951.774472	13701.446574	62.287015
1951.139567	13641.600206	62.292020
1950.650153	13576.247206	62.297025
1949.947509	13512.204859	62.302030
1949.259723	13453.146761	62.307034
1948.816907	13387.178998	62.312039
1947.946055	13328.723491	62.317044
1947.443504	13263.301308	62.322049
1946.897185	13190.472279	62.327054
1945.726747	13124.247967	62.332058
1945.199459	13069.453263	62.337063
1944.474838	13005.642531	62.342068
1943.860665	12935.055892	62.347073
1943.518712	12883.105729	62.352078
1942.800622	12823.782515	62.357082
1942.198995	12752.941109	62.362087
1941.463213	12703.567744	62.367092
1940.527987	12630.267384	62.372097
1940.220983	12572.234181	62.377102
1939.318030	12505.651481	62.382106
1938.856836	12438.219274	62.387111
1937.806321	12381.569818	62.392116
1937.305647	12312.739961	62.397121
1937.095030	12244.245918	62.402126
1936.059573	12194.790089	62.407130
1935.740627	12111.761483	62.412135
1934.792541	12068.629869	62.417140
1934.321971	11997.936889	62.422145
1933.274108	11926.079603	62.427150
1932.842479	11873.857019	62.432154
1932.119261	11808.025728	62.437159
1931.427313	11744.796969	62.442164
1930.804543	11688.581705	62.447169
1930.369209	11617.624497	62.452174
1929.280868	11557.793591	62.457178
1928.861330	11496.644310	62.462183
1928.467102	11443.375271	62.467188
1927.988629	11365.327420	62.472193
1927.013767	11298.506160	62.477198
1926.146512	11236.070594	62.482202
1925.756260	11178.039554	62.487207
1924.567997	11104.125486	62.492212
1923.981719	11049.515131	62.497217
1923.773697	10975.876322	62.502222
1922.823628	10918.388662	62.507226
1922.215271	10854.765285	62.512231
1921.576206	10793.322877	62.517236
1921.124507	10747.209542	62.522241
1920.664710	10670.266592	62.527246
1919.904438	10611.958550	62.532250
1919.419154	10547.403999	62.537255
1918.411955	10484.077081	62.542260
1917.722106	10405.911502	62.547265
1917.341300	10351.099633	62.552270
1916.444262	10282.667193	62.557274
1915.544669	10213.742721	62.562279
1915.089879	10148.609636	62.567284
1914.434369	10083.404347	62.572289
1913.598346	10021.871286	62.577294
1912.645999	9957.952420	62.582298
1912.283111	9896.626439	62.587303
1911.560408	9845.181377	62.592308
1911.065773	9775.479781	62.597313
1910.246085	9706.094426	62.602318
1909.233945	9644.114311	62.607322
1908.953631	9586.360902	62.612327
1908.032511	9524.522263	62.617332
1907.526716	9460.510163	62.622337
1906.729366	9399.784192	62.627342
1906.159366	9348.115002	62.632346
1905.754263	9270.209134	62.637351
1904.551971	9227.194057	62.642356
1904.520740	9163.685806	62.647361
1903.979341	9103.673080	62.652366
1902.996716	9039.517952	62.657370
1902.379120	8971.924838	62.662375
1901.814537	8922.695725	62.667380
1901.103844	8852.515148	62.672385
1900.238917	8800.554229	62.677390
1899.639286	8735.115540	62.682394
1899.147497	8672.416598	62.687399
1898.282001	8616.964920	62.692404
1898.030916	8562.430092	62.697409
1897.404367	8490.951085	62.702414
1896.556916	8430.659468	62.707418
1896.134060	8369.707805	62.712423
1895.606878	8296.327617	62.717428
1894.663681	8239.354421	62.722433
1894.153211	8174.388031	62.727438
1892.999390	8116.797092	62.732442
1892.612012	8040.205186	62.737447
1891.711491	7979.183418	62.742452
1890.909031	7918.852799	62.747457
1890.366276	7855.986283	62.752462
1889.467691	7816.410462	62.757466
1889.351416	7734.382963	62.762471
1888.759284	7687.637058	62.767476
1888.016108	7623.692179	62.772481
1887.344183	7554.216409	62.777486
1886.198319	7497.774431	62.782490
1885.793309	7423.576438	62.787495
1885.139854	7386.085329	62.792500
1884.687982	7315.450004	62.797505
1884.101170	7243.188483	62.802510
1882.953445	7196.477892	62.807514
1882.323814	7125.410199	62.812519
1881.873986	7068.554054	62.817524
1881.462042	7011.127287	62.822529
1880.746306	6947.511484	62.827534
1879.670760	6897.017670	62.832538
1879.389075	6830.830422	62.837543
1878.520369	6774.819706	62.842548
1877.970037	6712.275146	62.847553
1877.462302	6647.636814	62.852558
1876.424020	6583.811090	62.857562
1875.953828	6529.741675	62.862567
1874.997554	6465.943669	62.867572
1874.538771	6413.329047	62.872577
1874.011086	6346.468329	62.877582
1873.327469	6295.444594	62.882586
1872.599555	6224.122299	62.887591
1871.819503	6173.104829	62.892596
1870.931519	6113.911276	62.897601
1870.652748	6053.954693	62.902606
1869.822395	5995.496310	62.907610
1869.471892	5938.700494	62.912615
1868.759754	5879.724487	62.917620
1868.181567	5819.484303	62.922625
1867.459598	5744.818082	62.927630
1866.478428	5705.099695	62.932634
1866.111102	5632.596601	62.937639
1865.077930	5571.155774	62.942644
1864.277377	5525.043714	62.947649
1864.034812	5467.697771	62.952654
1863.332242	5406.133362	62.957658
1862.620051	5349.162174	62.962663
1861.925319	5301.332631	62.967668
1861.390948	5231.571387	62.972673
1860.833445	5168.763923	62.977678
1859.981377	5118.326277	62.982682
1859.629792	5047.603776	62.987687
1858.714962	4997.991289	62.992692
1858.170482	4940.446077	62.997697
1857.600752	4873.707525	63.002702
1856.640752	4815.134783	63.007706
1856.210752	4769.583835	63.012711
1855.085878	4709.842746	63.017716
1854.441951	4654.401439	63.022721
1854.285553	4585.157431	63.027726
1853.014859	4537.849301	63.032730
1852.532215	4475.305801	63.037735
1852.219724	4425.298314	63.042740
1851.560912	4372.452960	63.047745
1850.982832	4295.311197	63.052750
1849.937219	4244.159570	63.057754
1849.490339	4183.010806	63.062759
1848.786820	4122.379423	63.067764
1848.116029	4068.980233	63.072769
1847.659612	4012.304063	63.077774
1846.754994	3962.327488	63.082778
1846.022004	3898.923912	63.087783
1845.567069	3840.013011	63.092788
1844.539677	3784.418183	63.097793
1843.867036	3721.992437	63.102798
1843.231436	3680.239527	63.107802
1842.927176	3618.421377	63.112807
1841.868471	3563.477498	63.117812
1841.272424	3509.880767	63.122817
1840.412335	3455.556412	63.127822
1839.847801	3402.294198	63.132826
1839.415573	3347.093136	63.137831
1838.857195	3298.868310	63.142836
1837.908681	3236.208456	63.147841
1837.075988	3179.114950	63.152846
1836.322268	3136.589743	63.157850
1835.964590	3082.694890	63.162855
1835.521919	3035.845314	63.167860
1834.746328	2985.895745	63.172865
1834.332663	2915.705950	63.177870
1833.268478	2875.412969	63.182874
1832.723746	2815.290158	63.187879
1832.236377	2759.399754	63.192884
1831.109536	2709.816043	63.197889
1830.808311	2654.681169	63.202894
1829.772327	2607.283651	63.207898
1829.592107	2558.583245	63.212903
1828.994781	2498.270564	63.217908
1828.089089	2453.237643	63.222913
1827.737208	2379.982347	63.227918
1826.721567	2334.882867	63.232922
1825.982110	2285.818714	63.237927
1825.643727	2228.326311	63.242932
1824.949563	2176.813813	63.247937
1824.169690	2114.094923	63.252942
1823.116626	2073.304000	63.257946
1822.743288	2026.339396	63.262951
1821.858651	1966.947502	63.267956
1821.313579	1921.146076	63.272961
1821.171473	1862.781732	63.277966
1820.143423	1815.960405	63.282970
1819.179874	1758.808845	63.287975
1818.712244	1710.540936	63.292980
1817.988894	1658.362247	63.297985
1817.331570	1610.389752	63.302990
1816.573766	1557.372336	63.307994
1815.829205	1504.267845	63.312999
1815.356219	1461.635913	63.318004
1814.732500	1412.076876	63.323009
1814.010034	1359.217014	63.328014
1813.455786	1318.632094	63.333018
1812.310766	1269.368442	63.338023
1811.831140	1215.596037	63.343028
1811.234289	1170.291728	63.348033
1810.704992	1115.012781	63.353038
1809.721775	1080.900412	63.358042
1809.428132	1031.835141	63.363047
1808.398658	991.052974	63.368052
1807.793870	947.188126	63.373057
1807.214565	896.549020	63.378062
1806.319231	859.762708	63.383066
1805.654791	811.425734	63.388071
1804.836229	769.429485	63.393076
1804.221794	735.213638	63.398081
1803.792976	692.505979	63.403086
1803.133085	647.906421	63.408090
1802.638437	603.839030	63.413095
1801.590508	563.636615	63.418100
1800.637026	533.876572	63.423105
1800.322874	485.335243	63.428110
1799.435936	445.258987	63.433114
1798.760544	412.321504	63.438119
1798.113863	376.452607	63.443124
1797.492876	344.720935	63.448129
1797.017691	304.898239	63.453134
1795.701452	281.859941	63.458138
1795.063474	240.317537	63.463143
1794.583445	216.584359	63.468148
1793.172400	188.695459	63.473153
1792.923357	153.241800	63.478158
1791.983283	139.453732	63.483162
1791.532358	117.821368	63.488167
1791.064684	85.996533	63.493172
1790.063302	70.884144	63.498177
1789.239157	53.715637	63.503182
1788.167141	45.796034	63.508186
1786.891073	31.913191	63.513191
1786.058813	42.044971	63.518196
1784.721372	55.655360	63.523201
1784.191328	55.961921	63.528206
1783.432610	70.136443	63.533210
1782.966159	72.069807	63.538215
1783.010587	71.249068	63.543220
1782.425054	63.283744	63.548225
1781.719037	65.639932	63.553230
1780.637264	81.948952	63.558234
1780.557683	76.822259	63.563239
1780.046534	74.107488	63.568244
1778.991549	79.799207	63.573249
1778.349615	81.809326	63.578254
1777.370170	87.883297	63.583258
1776.529647	82.536815	63.588263
1776.424698	79.656611	63.593268
1775.997904	90.802689	63.598273
1775.317720	77.154770	63.603278
1774.384165	79.249048	63.608282
1773.567163	81.346894	63.613287
1773.586093	81.717668	63.618292
1773.126276	89.246674	63.623297
1772.743930	77.364982	63.628302
1771.014434	82.417911	63.633306
1770.263383	86.951177	63.638311
1769.988989	81.238823	63.643316
1768.789165	88.729225	63.648321
1768.347003	78.268428	63.653326
1767.999585	83.368385	63.658330
1767.806563	85.404989	63.663335
1767.213879	87.744764	63.668340
1765.718188	90.559108	63.673345
1765.607162	88.164000	63.678350
1765.081754	85.919857	63.683354
1764.370770	90.940357	63.688359
1763.649405	87.360094	63.693364
1762.503345	87.718756	63.698369
1762.159128	86.119208	63.703374
1761.146306	89.271616	63.708378
1760.554808	82.368540	63.713383
1759.953831	79.223331	63.718388
1759.057717	92.125000	63.723393
1759.398597	86.986726	63.728398
1758.581056	87.534495	63.733402
1757.415353	94.007067	63.738407
1756.983910	87.324581	63.743412
1756.452507	95.459480	63.748417
1756.056129	89.932080	63.753422
1754.834780	94.025946	63.758426
1754.332159	90.382560	63.763431
1754.103328	85.560271	63.768436
1752.590597	94.434499	63.773441
1752.476845	88.073727	63.778446
1751.935697	97.897541	63.783450
1751.046348	98.751612	63.788455
1750.656436	85.322529	63.793460
1748.947275	92.408121	63.798465
1749.083050	82.935772	63.803470
1748.859924	95.061928	63.808474
1747.761858	103.360944	63.813479
1747.353204	87.148316	63.818484
1746.088064	96.563554	63.823489
1746.021705	90.149523	63.828494
1745.110612	95.305889	63.833498
1744.280886	101.961658	63.838503
1743.956552	89.641812	63.843508
1743.183234	100.677350	63.848513
1742.759283	91.442125	63.853518
1741.949050	94.784719	63.858522
1741.252312	83.383477	63.863527
1740.777707	88.519407	63.868532
1739.858273	93.263931	63.873537
1739.161903	90.677932	63.878542
1738.722984	91.039417	63.883546
1737.642056	89.085359	63.888551
1737.194467	96.975135	63.893556
1736.451760	98.490329	63.898561
1736.102167	86.415778	63.903566
1735.612141	87.495020	63.908570
1734.138301	95.128308	63.913575
1733.871170	90.370451	63.918580
1733.384931	96.328260	63.923585
1732.801918	89.218835	63.928590
1732.066673	95.058494	63.933594
1731.083363	81.887669	63.938599
1730.841253	87.883975	63.943604
1729.702494	90.677921	63.948609
1729.764152	93.044669	63.953614
1728.706188	91.332976	63.958618
1727.490682	97.528037	63.963623
1727.571299	89.258217	63.968628
1726.589665	98.548011	63.973633
1726.120535	87.351900	63.978638
1725.372570	93.802293	63.983642
1724.665279	86.660570	63.988647
1723.896858	88.559902	63.993652
1723.620830	91.697807	63.998657
1723.213593	84.672435	64.003662
1722.166367	86.100377	64.008666
1721.188871	92.916813	64.013671
1720.935934	86.650692	64.018676
1719.768480	99.355770	64.023681
1719.456137	88.915362	64.028686
1718.980228	93.017007	64.033690
1718.692789	89.755776	64.038695
1718.018780	90.246067	64.043700
1717.084377	94.188718	64.048705
1716.627156	86.829081	64.053710
1715.417045	89.369433	64.058714
1714.379053	86.872394	64.063719
1714.323766	89.902699	64.068724
1713.658650	99.404004	64.073729
1712.595785	92.198907	64.078734
1711.969623	82.609452	64.083738
1712.056298	82.614646	64.088743
1711.178241	80.454912	64.093748
1710.108308	89.599455	64.098753
1709.599332	80.231091	64.103758
1708.913621	90.409031	64.108762
1708.031774	89.030502	64.113767
1707.896836	86.136141	64.118772
1707.116112	92.467159	64.123777
1706.693415	84.613180	64.128782
1706.314608	87.601828	64.133786
1705.166601	87.861474	64.138791
1704.016417	78.334755	64.143796
1703.363616	94.197199	64.148801
1703.275959	83.287443	64.153806
1702.405024	92.247416	64.158810
1701.491749	92.395664	64.163815
1701.428233	87.944522	64.168820
1700.170758	86.978901	64.173825
1699.982730	89.069910	64.178830
1699.420682	88.446425	64.183834
1698.760256	87.827527	64.188839
1698.700506	82.036936	64.193844
1696.709684	89.608848	64.198849
1696.570826	79.572988	64.203854
1695.666240	82.828076	64.208858
1694.812764	92.846583	64.213863
1694.025237	84.022367	64.218868
1693.404902	86.932682	64.223873
1692.898772	84.568797	64.228878
1692.897270	84.696807	64.233882
1692.055466	87.032010	64.238887
1691.703780	78.296269	64.243892
1691.004065	86.746491	64.248897
1690.204391	87.628916	64.253902
1689.154679	88.197814	64.258906
1687.743346	95.387527	64.263911
1688.328194	85.164173	64.268916
1687.155992	89.250260	64.273921
1686.044092	79.933515	64.278926
1685.884100	88.216008	64.283930
1685.297430	91.931544	64.288935
1685.130126	82.606688	64.293940
1684.035510	88.285814	64.298945
1683.620812	88.995126	64.303950
1683.339377	81.733738	64.308954
1682.237840	84.200086	64.313959
1681.390496	83.175638	64.318964
1680.306268	88.747457	64.323969
1679.624013	88.286575	64.328974
1679.235797	83.188412	64.333978
1678.757163	90.373481	64.338983
1678.496496	84.084941	64.343988
1677.929250	82.112396	64.348993
1677.182689	90.554294	64.353998
1676.051604	91.093545	64.359002
1675.030549	93.296375	64.364007
1674.293900	81.754841	64.369012
1673.768424	88.228249	64.374017
1673.530219	89.075111	64.379022
1673.216819	83.509319	64.384026
1672.483239	92.274015	64.389031
1672.079610	80.004639	64.394036
1670.667989	84.142955	64.399041
1670.158075	85.140210	64.404046
1669.233802	81.686828	64.409050
1668.771046	91.053487	64.414055
1668.432808	81.359966	64.419060
1667.689953	85.508749	64.424065
1666.966392	78.511563	64.429070
1666.382583	74.890560	64.434074
1665.038513	85.256659	64.439079
1664.466798	81.406649	64.444084
1663.869991	84.401544	64.449089
1663.877105	80.205697	64.454094
1663.112920	81.167649	64.459098
1662.409469	81.146960	64.464103
1662.074542	83.294421	64.469108
1661.144536	91.099979	64.474113
1660.363321	86.712383	64.479118
1659.511773	86.019774	64.484122
1658.733686	90.622018	64.489127
1657.966605	80.425756	64.494132
1657.593572	86.706214	64.499137
1657.107239	71.371733	64.504142
1656.746411	77.867871	64.509146
1655.717523	82.170904	64.514151
1654.625325	81.407713	64.519156
1653.798414	85.833207	64.524161
1653.531639	83.882324	64.529166
1653.088340	78.184206	64.534170
1652.105023	83.932395	64.539175
1651.647503	75.472100	64.544180
1651.042082	85.364474	64.549185
1650.639070	85.971009	64.554190
1650.242713	78.988084	64.559194
1649.308032	92.124563	64.564199
1648.388018	82.422535	64.569204
1647.599695	85.793213	64.574209
1647.053931	85.745902	64.579214
1646.613561	86.238522	64.584218
1645.763441	84.752472	64.589223
1645.350178	82.209841	64.594228
1644.189180	87.306583	64.599233
1643.455565	84.501022	64.604238
1643.009694	73.395871	64.609242
1641.946257	84.687239	64.614247
1641.605333	82.901103	64.619252
1640.996043	93.109493	64.624257
1640.731514	82.803440	64.629262
1640.532822	79.349926	64.634266
1639.530672	79.476043	64.639271
1638.865926	78.340600	64.644276
1637.970421	87.712925	64.649281
1636.892355	80.079772	64.654286
1636.725062	77.062824	64.659290
1635.868735	94.421036	64.664295
1635.622522	79.444230	64.669300
1634.217769	81.200240	64.674305
1633.160160	88.122469	64.679310
1632.873727	82.976607	64.684314
1632.344176	84.631434	64.689319
1632.139160	85.789998	64.694324
1631.297014	84.819935	64.699329
1630.964622	89.469656	64.704334
1630.559715	88.045352	64.709338
1629.276498	86.506682	64.714343
1628.813629	85.640373	64.719348
1627.974357	82.216081	64.724353
1627.272084	78.801567	64.729358
1626.977665	77.668798	64.734362
1625.979870	85.677523	64.739367
1625.155931	80.240155	64.744372
1624.387571	78.490386	64.749377
1623.797464	86.546311	64.754382
1623.431320	80.651435	64.759386
1623.073890	80.878567	64.764391
1622.644846	81.776251	64.769396
1621.084580	81.861726	64.774401
1620.158852	80.471277	64.779406
1619.802118	79.655919	64.784410
1618.886241	82.051796	64.789415
1618.987889	69.257469	64.794420
1618.281813	87.880193	64.799425
1617.673143	79.221564	64.804430
1617.411207	73.780076	64.809434
1615.992460	83.921512	64.814439
1615.466510	83.954640	64.819444
1614.771242	81.862097	64.824449
1614.108076	84.116903	64.829454
1613.811472	79.480447	64.834458
1612.713111	83.553255	64.839463
1611.875905	81.505340	64.844468
1610.910298	83.909121	64.849473
1610.618336	85.336970	64.854478
1610.371009	72.741586	64.859482
1609.593876	85.651186	64.864487
1609.326334	84.364336	64.869492
1608.651329	80.287897	64.874497
1607.157248	79.424567	64.879502
1606.454584	76.757607	64.884506
1606.036487	81.088203	64.889511
1605.852239	75.145512	64.894516
1605.321721	74.677891	64.899521
1604.017218	78.934840	64.904526
1603.196689	72.885075	64.909530
1602.397003	87.616510	64.914535
1601.970273	76.375862	64.919540
1601.613339	79.048804	64.924545
1601.190647	86.001061	64.929550
1600.679495	83.637995	64.934554
1600.192447	75.920428	64.939559
1598.925699	79.758215	64.944564
1598.430586	86.138498	64.949569
1597.764832	88.688614	64.954574
1597.442163	79.970361	64.959578
1596.454882	81.084472	64.964583
1595.956279	73.446016	64.969588
1595.130674	81.391121	64.974593
1594.211695	83.740190	64.979598
1593.710074	74.454276	64.984602
1592.069865	80.852478	64.989607
1592.296322	77.105918	64.994612
1591.504812	78.915912	64.999617
1590.969934	79.526059	65.004622
1590.538553	78.501788	65.009626
1589.560910	81.287539	65.014631
1589.310121	72.747109	65.019636
1588.921157	80.998163	65.024641
1587.608600	83.351417	65.029646
1587.044575	76.421955	65.034650
1586.280702	75.661824	65.039655
1586.120550	73.132609	65.044660
1585.417110	74.291516	65.049665
1584.102701	80.123867	65.054670
1583.314173	73.122842	65.059674
1582.833522	82.598002	65.064679
1582.681695	77.432341	65.069684
1582.190655	80.840960	65.074689
1581.388269	78.029000	65.079694
1580.383718	72.450034	65.084698
1579.506296	78.031607	65.089703
1578.852575	77.440061	65.094708
1578.655258	78.266241	65.099713
1578.482002	88.749139	65.104718
1577.796298	71.817347	65.109722
1576.279241	94.416743	65.114727
1575.698274	82.691240	65.119732
1575.358038	82.595521	65.124737
1575.004558	78.266156	65.129742
1573.603106	79.662124	65.134746
1572.483001	84.744511	65.139751
1572.117105	80.544854	65.144756
1571.556747	75.007282	65.149761
1570.983863	89.073476	65.154766
1570.999809	80.839177	65.159770
1570.125775	85.735811	65.164775
1569.676987	77.532773	65.169780
1568.736224	81.981109	65.174785
1567.769376	81.098690	65.179790
1567.609785	78.373841	65.184794
1566.762903	92.010481	65.189799
1566.315071	81.752493	65.194804
1565.398827	75.254319	65.199809
1564.545434	75.098207	65.204814
1563.802729	77.342006	65.209818
1563.432779	88.663565	65.214823
1562.789688	80.177582	65.219828
1561.508134	86.387930	65.224833
1560.688902	81.861328	65.229838
1560.643013	86.315721	65.234842
1559.675695	82.490747	65.239847
1559.334475	78.958962	65.244852
1558.630612	82.205855	65.249857
1558.448293	82.157588	65.254862
1558.091759	75.042201	65.259866
1556.745332	78.676621	65.264871
1555.888165	77.462962	65.269876
1555.459073	81.230754	65.274881
1554.839994	79.406825	65.279886
1554.563871	75.702270	65.284890
1553.042322	81.179613	65.289895
1552.336880	81.257043	65.294900
1551.807693	83.435381	65.299905
1551.340670	80.521259	65.304910
1551.242913	72.606234	65.309914
1550.337176	85.225613	65.314919
1549.572238	85.131145	65.319924
1548.774747	86.394893	65.324929
1548.152972	82.469288	65.329934
1547.816777	78.220762	65.334938
1546.643926	81.914341	65.339943
1545.935839	79.194643	65.344948
1545.523618	76.759100	65.349953
1544.670369	78.433836	65.354958
1544.646504	80.675388	65.359962
1543.785764	78.134490	65.364967
1542.861474	75.947471	65.369972
1541.900101	73.889348	65.374977
1541.050362	75.262325	65.379982
1540.840906	67.149008	65.384986
1540.446779	80.928170	65.389991
1540.075553	73.715773	65.394996
1539.004319	73.054958	65.400001
1537.858726	71.690014	65.405006
1537.572050	69.696577	65.410010
1536.760902	71.818793	65.415015
1536.683086	63.608867	65.420020
1535.800647	77.820435	65.425025
1534.728886	78.004962	65.430030
1534.331378	73.259973	65.435034
1533.767606	83.088972	65.440039
1533.297604	76.056275	65.445044
1532.243324	74.702055	65.450049
1531.058918	81.146139	65.455054
1530.800806	69.533367	65.460058
1530.122294	76.941019	65.465063
1529.868881	83.751264	65.470068
1529.724323	82.608888	65.475073
1527.976296	80.929660	65.480078
1527.590301	71.850901	65.485082
1527.025809	67.236530	65.490087
1526.870642	70.337893	65.495092
1525.711318	78.712936	65.500097
1524.674009	82.875425	65.505102
1524.202238	71.717655	65.510106
1523.553231	78.071934	65.515111
1523.432613	74.303250	65.520116
1522.934550	76.202255	65.525121
1521.178190	77.932192	65.530126
1520.634475	74.267010	65.535130
1520.251684	88.394465	65.540135
1519.651601	74.216680	65.545140
1519.501290	78.069488	65.550145
1518.901530	88.322107	65.555150
1517.953715	76.553996	65.560154
1516.898369	82.592797	65.565159
1516.361924	81.017524	65.570164
1515.932600	80.956470	65.575169
1515.242714	84.526009	65.580174
1514.181490	72.717576	65.585178
1513.364989	81.907061	65.590183
1512.961488	81.349888	65.595188
1512.472137	70.727932	65.600193
1511.817967	79.380682	65.605198
1511.696985	66.213309	65.610202
1510.568742	81.869026	65.615207
1509.856442	73.349908	65.620212
1509.381105	63.933691	65.625217
1508.835370	67.757868	65.630222
1508.315224	71.429744	65.635226
1506.999222	72.651317	65.640231
1506.506477	69.693985	65.645236
1505.854332	66.599555	65.650241
1505.184116	67.221763	65.655246
1504.865230	66.174901	65.660250
1503.471876	75.651595	65.665255
1503.014267	68.680019	65.670260
1502.404211	73.460602	65.675265
1501.600185	84.403277	65.680270
1501.669405	65.818746	65.685274
1500.857070	71.918281	65.690279
1500.167318	75.396335	65.695284
1499.119128	70.791025	65.700289
1498.083723	69.247738	65.705294
1497.965408	67.628103	65.710298
1497.650927	76.745697	65.715303
1496.792275	77.076149	65.720308
1496.001290	66.439056	65.725313
1495.121614	71.860157	65.730318
1494.850587	66.838033	65.735322
1494.292233	77.410501	65.740327
1493.715331	89.310580	65.745332
1492.676307	80.231519	65.750337
1491.957854	79.301771	65.755342
1491.684944	74.029206	65.760346
1490.199365	75.219388	65.765351
1489.511771	71.146565	65.770356
1488.943659	67.264494	65.775361
1488.127370	84.446039	65.780366
1488.380340	70.173709	65.785370
1487.598996	77.383242	65.790375
1487.221614	69.746055	65.795380
1486.417302	68.172357	65.800385
1485.402188	78.992456	65.805390
1485.176557	66.869904	65.810394
1484.211340	76.207605	65.815399
1483.276259	69.785003	65.820404
1482.693981	64.364485	65.825409
1481.868151	71.770323	65.830414
1481.630385	66.832803	65.835418
1480.875043	75.176777	65.840423
1480.266325	72.469695	65.845428
1479.465494	71.286534	65.850433
1478.599625	69.640619	65.855438
1478.520204	59.555939	65.860442
1478.071471	72.261970	65.865447
1477.043941	60.263708	65.870452
1476.254714	58.339107	65.875457
1475.172308	81.558579	65.880462
1475.195349	67.545145	65.885466
1474.117967	79.428559	65.890471
1473.215927	75.973299	65.895476
1472.691974	73.779456	65.900481
1471.924363	72.764486	65.905486
1471.529010	73.738841	65.910490
1470.716661	74.514534	65.915495
1470.602805	74.269310	65.920500
1469.963425	66.404104	65.925505
1469.059544	77.610234	65.930510
1468.564391	72.898123	65.935514
1467.737796	74.737383	65.940519
1466.412383	67.747610	65.945524
1466.001164	69.125037	65.950529
1465.285132	80.921066	65.955534
1465.454901	68.743564	65.960538
1464.653134	68.483085	65.965543
1464.120957	68.834204	65.970548
1463.230105	66.580400	65.975553
1462.084870	69.334480	65.980558
1461.581225	65.697640	65.985562
1461.011003	67.674354	65.990567
1459.780286	61.749763	65.995572
1459.278606	69.468370	66.000577
1458.604650	72.977039	66.005582
1458.421873	67.590808	66.010586
1457.816136	64.870644	66.015591
1457.342118	71.779024	66.020596
1456.915329	63.165670	66.025601
1455.768146	63.344870	66.030606
1455.360412	65.090756	66.035610
1454.407461	61.752409	66.040615
1453.577525	67.533049	66.045620
1452.537449	66.097757	66.050625
1451.863341	69.885576	66.055630
1451.843768	61.289509	66.060634
1451.469411	67.891886	66.065639
1450.737601	72.575133	66.070644
1450.014784	73.598380	66.075649
1448.968666	73.887679	66.080654
1448.409884	62.343217	66.085658
1447.852910	67.361379	66.090663
1447.197947	60.851700	66.095668
1446.530979	76.271689	66.100673
1445.354086	65.561908	66.105678
1445.290340	64.752051	66.110682
1444.731705	73.552052	66.115687
1444.052553	68.851846	66.120692
1443.378545	80.641199	66.125697
1442.186577	70.400595	66.130702
1441.843414	65.263787	66.135706
1441.414025	77.470004	66.140711
1440.719243	71.572207	66.145716
1439.659280	76.757048	66.150721
1438.894393	65.037184	66.155726
1438.427734	76.452954	66.160730
1438.160973	69.492064	66.165735
1437.424159	75.011904	66.170740
1436.610277	64.711217	66.175745
1435.503028	72.486648	66.180750
1435.428104	63.096701	66.185754
1434.692335	70.791014	66.190759
1434.119696	62.897868	66.195764
1433.281332	67.930792	66.200769
1432.368583	66.156725	66.205774
1432.231982	66.804529	66.210778
1431.690920	65.862376	66.215783
1430.708770	75.257976	66.220788
1429.790406	64.585963	66.225793
1428.960708	79.560307	66.230798
1428.974318	66.133437	66.235802
1428.203565	68.370690	66.240807
1427.323689	80.329961	66.245812
1426.929996	72.130824	66.250817
1426.029650	75.279664	66.255822
1425.669616	71.487540	66.260826
1424.411518	79.504576	66.265831
1423.652949	75.145006	66.270836
1423.216739	71.625191	66.275841
1422.756104	77.102715	66.280846
1422.812359	71.268484	66.285850
1421.668000	66.341024	66.290855
1420.126219	77.856712	66.295860
1419.959884	62.573968	66.300865
1419.319031	73.473369	66.305870
1419.281899	59.122582	66.310874
1418.039622	73.131161	66.315879
1416.857679	69.188974	66.320884
1416.495622	72.854662	66.325889
1415.571369	71.867759	66.330894
1415.790035	56.476521	66.335898
1415.210435	65.470665	66.340903
1414.075151	68.672619	66.345908
1413.605432	70.530866	66.350913
1412.804080	71.951386	66.355918
1412.458319	74.594186	66.360922
1411.130677	70.522193	66.365927
1410.248744	78.290210	66.370932
1409.865451	60.007864	66.375937
1409.264808	77.270254	66.380942
1409.173571	74.570827	66.385946
1408.686118	74.694074	66.390951
1407.605062	83.567659	66.395956
1407.362763	69.506521	66.400961
1406.314219	74.569708	66.405966
1405.685223	71.331276	66.410970
1404.539100	73.643970	66.415975
1403.883768	66.131409	66.420980
1403.281092	65.973346	66.425985
1402.806238	75.666794	66.430990
1402.678389	70.565155	66.435994
1401.924223	70.913725	66.440999
1400.740007	71.242339	66.446004
1400.370205	75.502201	66.451009
1399.911187	74.285237	66.456014
1398.965785	71.276874	66.461018
1397.928976	74.835347	66.466023
1397.071372	71.380940	66.471028
1396.765301	67.465126	66.476033
1396.143997	72.551871	66.481038
1395.972652	74.862594	66.486042
1395.493189	67.304734	66.491047
1394.087238	78.194866	66.496052
1393.513548	67.165304	66.501057
1393.107863	82.258342	66.506062
1392.789381	63.557262	66.511066
1391.781755	75.241949	66.516071
1390.827181	70.032021	66.521076
1390.236800	74.356908	66.526081
1389.815329	79.154846	66.531086
1388.962363	79.948060	66.536090
1388.113251	76.777736	66.541095
1387.217688	74.918951	66.546100
1387.535420	79.875361	66.551105
1386.827102	72.487920	66.556110
1386.263048	77.396833	66.561114
1384.921430	76.826370	66.566119
1383.907854	74.585794	66.571124
1383.548810	74.436319	66.576129
1383.187616	66.965320	66.581134
1382.699305	66.035293	66.586138
1381.902857	74.603442	66.591143
1381.159533	76.115675	66.596148
1380.982038	65.370075	66.601153
1379.622232	72.520190	66.606158
1378.951453	64.319381	66.611162
1378.261857	70.945067	66.616167
1377.400626	73.166754	66.621172
1377.109327	71.825362	66.626177
1376.783779	66.375104	66.631182
1375.982298	80.752032	66.636186
1375.432403	69.873235	66.641191
1374.982406	81.868266	66.646196
1373.751472	80.520116	66.651201
1372.757019	71.205375	66.656206
1371.911023	62.215552	66.661210
1371.697279	73.431847	66.666215
1371.260954	78.419808	66.671220
1371.049309	77.745428	66.676225
1369.750896	66.689149	66.681230
1369.170485	62.883183	66.686234
1368.666552	75.739922	66.691239
1367.727794	72.937098	66.696244
1367.926693	72.456081	66.701249
1366.245427	69.085307	66.706254
1365.412411	74.089016	66.711258
1365.137175	72.713533	66.716263
1364.509283	74.924941	66.721268
1364.618886	65.381089	66.726273
1363.610081	76.665422	66.731278
1362.330953	83.779072	66.736282
1361.839068	80.906789	66.741287
1361.639364	69.628551	66.746292
1360.886052	78.345969	66.751297
1359.747704	80.004581	66.756302
1359.153327	80.001330	66.761306
1358.497015	64.962068	66.766311
1357.940655	77.048121	66.771316
1357.516945	60.497422	66.776321
1356.483635	78.500382	66.781326
1355.965889	70.045014	66.786330
1355.630687	71.208521	66.791335
1354.882199	81.997313	66.796340
1353.860281	66.591965	66.801345
1352.829756	71.705922	66.806350
1352.342301	78.969694	66.811354
1352.336438	78.868160	66.816359
1351.810785	79.306575	66.821364
1351.255068	71.171060	66.826369
1349.798381	81.206677	66.831374
1349.334397	84.030707	66.836378
1349.079629	74.087452	66.841383
1347.761440	79.614577	66.846388
1347.232766	79.056829	66.851393
1346.386119	72.531917	66.856398
1346.001929	70.809477	66.861402
1345.578943	68.147023	66.866407
1344.920105	67.608392	66.871412
1344.365814	63.575928	66.876417
1343.509700	82.618333	66.881422
1342.764290	74.533475	66.886426
1342.349267	75.373780	66.891431
1341.509938	72.734934	66.896436
1340.904639	76.332065	66.901441
1339.996942	79.004280	66.906446
1339.361222	70.848371	66.911450
1339.073574	69.072737	66.916455
1338.047022	73.304544	66.921460
1337.316577	66.228151	66.926465
1336.358436	76.935152	66.931470
1336.186719	75.563716	66.936474
1336.074256	72.749396	66.941479
1335.038670	81.372922	66.946484
1334.482784	66.751369	66.951489
1333.555154	76.671345	66.956494
1333.278845	66.441361	66.961498
1332.190308	75.699359	66.966503
1330.772342	73.393781	66.971508
1330.736751	74.793516	66.976513
1329.953562	74.287272	66.981518
1329.821483	66.366696	66.986522
1329.470750	69.382459	66.991527
1328.245709	61.572561	66.996532
1327.590455	68.165987	67.001537
1327.027509	63.666544	67.006542
1326.577828	68.569896	67.011546
1325.642560	64.012948	67.016551
1324.499730	74.135871	67.021556
1324.568853	69.898645	67.026561
1324.211023	84.932038	67.031566
1323.526606	68.561562	67.036570
1322.543455	81.226409	67.041575
1321.331344	74.442636	67.046580
1321.076497	79.627258	67.051585
1319.920857	81.223981	67.056590
1319.486320	78.766796	67.061594
1318.840309	65.197224	67.066599
1317.765063	79.363792	67.071604
1317.821195	79.255555	67.076609
1317.328046	76.046014	67.081614
1316.733711	81.224684	67.086618
1316.046255	76.978425	67.091623
1314.858026	76.389922	67.096628
1314.748210	78.921104	67.101633
1313.513023	80.457935	67.106638
1312.527006	73.313368	67.111642
1311.942778	73.161856	67.116647
1311.586601	82.005385	67.121652
1311.299008	68.415102	67.126657
1310.629087	83.665268	67.131662
1310.381227	81.402336	67.136666
1309.266709	73.693144	67.141671
1308.427504	85.470934	67.146676
1307.970103	69.818163	67.151681
1307.028191	70.540387	67.156686
1306.300916	75.697615	67.161690
1305.759619	70.866724	67.166695
1305.225233	69.251749	67.171700
1304.906458	72.450092	67.176705
1303.758112	73.769692	67.181710
1303.152420	74.474734	67.186714
1302.648585	70.741766	67.191719
1301.859481	82.543129	67.196724
1301.394237	68.856512	67.201729
1300.097478	82.389670	67.206734
1299.624840	75.560883	67.211738
1299.371635	75.205357	67.216743
1298.908659	78.619019	67.221748
1298.329501	73.980230	67.226753
1297.000358	71.321503	67.231758
1296.440470	82.897190	67.236762
1296.254811	75.360451	67.241767
1295.272057	77.136279	67.246772
1294.114427	66.521294	67.251777
1293.850081	70.624048	67.256782
1293.251512	73.038970	67.261786
1292.837633	68.635684	67.266791
1291.936828	72.525813	67.271796
1291.217225	59.335391	67.276801
1290.431407	74.339046	67.281806
1290.214864	75.051607	67.286810
1289.743897	60.145338	67.291815
1288.562183	78.006325	67.296820
1287.798723	66.617461	67.301825
1287.087697	77.154297	67.306830
1286.776405	69.699039	67.311834
1286.472831	77.291553	67.316839
1285.223706	72.338238	67.321844
1284.790992	67.901678	67.326849
1283.781148	64.827914	67.331854
1283.735311	68.088520	67.336858
1282.865605	72.828424	67.341863
1281.620302	75.812957	67.346868
1281.111886	72.298343	67.351873
1280.494521	74.047621	67.356878
1279.997155	68.097991	67.361882
1280.033074	58.794525	67.366887
1278.491484	65.508380	67.371892
1278.143900	54.619539	67.376897
1277.481293	65.864613	67.381902
1276.885497	71.023018	67.386906
1276.356122	71.930400	67.391911
1275.196042	78.321828	67.396916
1274.805774	73.045881	67.401921
1274.768430	71.525351	67.406926
1273.664134	67.410040	67.411930
1272.934818	63.482694	67.416935
1271.727733	72.739058	67.421940
1271.740733	77.639818	67.426945
1270.641089	74.596106	67.431950
1269.674752	70.422591	67.436954
1269.532465	64.999985	67.441959
1268.863911	70.393890	67.446964
1268.867854	69.742012	67.451969
1267.849908	63.572381	67.456974
1266.940183	78.110038	67.461978
1266.559556	67.587569	67.466983
1265.496475	76.357413	67.471988
1264.558672	76.880301	67.476993
1263.725128	73.018414	67.481998
1263.091885	77.801152	67.487002
1263.191567	70.121280	67.492007
1262.635715	78.890901	67.497012
1261.569040	72.632822	67.502017
1260.935948	79.066621	67.507022
1260.185418	83.134721	67.512026
1259.879165	73.109784	67.517031
1258.958831	80.795637	67.522036
1258.345972	70.269092	67.527041
1257.485989	69.839738	67.532046
1256.900325	75.318238	67.537050
1256.649487	71.494590	67.542055
1255.144215	75.170181	67.547060
1254.737241	69.800701	67.552065
1254.192116	59.879989	67.557070
1253.854601	72.374377	67.562074
1253.641668	63.971501	67.567079
1252.396230	78.120991	67.572084
1251.825436	77.886932	67.577089
1251.384571	68.550462	67.582094
1250.095314	67.057105	67.587098
1249.265654	74.848389	67.592103
1248.379849	79.434744	67.597108
1248.260330	75.607562	67.602113
1247.865916	75.484231	67.607118
1247.494951	65.322935	67.612122
1246.751273	74.658589	67.617127
1245.389422	79.399489	67.622132
1245.212001	68.190273	67.627137
1244.374632	75.271571	67.632142
1243.857321	65.545135	67.637146
1242.849959	62.885736	67.642151
1241.987856	73.894458	67.647156
1241.690427	71.697765	67.652161
1241.615356	72.646457	67.657166
1240.504379	76.563714	67.662170
1239.799676	70.418403	67.667175
1238.842731	77.201747	67.672180
1238.722312	69.154748	67.677185
1238.044762	76.587531	67.682190
1236.632050	69.003067	67.687194
1236.203687	76.229068	67.692199
1235.520606	77.141976	67.697204
1235.162826	77.512720	67.702209
1235.280667	80.209556	67.707214
1234.259950	75.500648	67.712218
1233.276002	78.497261	67.717223
1232.802517	70.809182	67.722228
1231.717412	59.252295	67.727233
1231.164764	74.542159	67.732238
1230.404877	68.162773	67.737242
1230.124581	73.611643	67.742247
1229.440537	64.838980	67.747252
1228.822541	66.645141	67.752257
1228.242770	75.183599	67.757262
1227.364999	76.499631	67.762266
1226.789825	74.976315	67.767271
1225.307315	78.834386	67.772276
1224.703059	69.173819	67.777281
1224.277343	62.498446	67.782286
1224.089760	77.295020	67.787290
1223.616813	71.324174	67.792295
1222.301276	69.633159	67.797300
1221.874273	73.621433	67.802305
1221.166659	69.542417	67.807310
1220.910449	73.954545	67.812314
1220.619862	65.811607	67.817319
1219.144066	82.593428	67.822324
1218.691001	65.793548	67.827329
1218.232536	70.851277	67.832334
1216.915213	66.970144	67.837338
1216.308406	72.415742	67.842343
1215.721644	69.872398	67.847348
1215.547242	77.764498	67.852353
1215.401419	66.597573	67.857358
1213.936800	76.472082	67.862362
1212.958128	62.367247	67.867367
1212.333450	82.486203	67.872372
1212.017073	82.990717	67.877377
1211.585032	69.177422	67.882382
1211.278477	77.177270	67.887386
1210.650053	61.961749	67.892391
1209.501704	68.799191	67.897396
1208.972408	76.186326	67.902401
1207.763914	71.001086	67.907406
1206.910842	76.108954	67.912410
1206.647012	66.622919	67.917415
1205.691631	81.943719	67.922420
1205.738667	59.502363	67.927425
1204.617274	70.306318	67.932430
1203.593428	66.946229	67.937434
1203.354593	58.754068	67.942439
1202.512597	68.871766	67.947444
1202.318926	67.451793	67.952449
1202.320814	61.209902	67.957454
1200.942265	67.043157	67.962458
1200.026051	60.365369	67.967463
1199.555795	74.058859	67.972468
1199.139017	66.388581	67.977473
1198.256889	67.744739	67.982478
1197.609682	60.570006	67.987482
1197.208120	60.305893	67.992487
1195.969029	68.696888	67.997492
1195.217232	66.507803	68.002497
1194.813207	66.256698	68.007502
1194.187945	78.058830	68.012506
1194.002575	59.107993	68.017511
1192.973584	66.147233	68.022516
1192.416802	59.342902	68.027521
1192.156310	72.186165	68.032526
1190.680051	63.397575	68.037530
1190.025225	69.062126	68.042535
1188.873114	65.697211	68.047540
1188.345877	71.324127	68.052545
1188.047679	65.494237	68.057550
1187.684170	65.408578	68.062554
1187.480877	68.033475	68.067559
1186.471328	61.845201	68.072564
1185.408753	73.246941	68.077569
1185.031032	65.497916	68.082574
1184.480753	61.315044	68.087578
1184.002298	66.380686	68.092583
1182.541462	71.017506	68.097588
1182.033747	62.013391	68.102593
1182.065159	70.071453	68.107598
1181.338663	75.644903	68.112602
1180.522408	51.929472	68.117607
1179.797490	71.279027	68.122612
1179.332145	71.417724	68.127617
1178.490636	65.480274	68.132622
1177.723100	74.852852	68.137626
1177.131007	58.259612	68.142631
1176.366089	56.220857	68.147636
1175.726375	64.565421	68.152641
1174.938478	63.180029	68.157646
1174.074427	62.230952	68.162650
1173.713953	70.650960	68.167655
1173.110463	65.760610	68.172660
1172.472087	64.644755	68.177665
1171.823066	54.808407	68.182670
1170.951063	70.909155	68.187674
1170.847334	61.899143	68.192679
1169.856457	71.717251	68.197684
1168.890201	65.365979	68.202689
1168.535346	64.670239	68.207694
1167.863232	69.966957	68.212698
1167.401107	62.802222	68.217703
1166.307288	74.538523	68.222708
1165.653028	77.654617	68.227713
1165.006307	74.322876	68.232718
1164.508750	80.470208	68.237722
1164.317783	63.849442	68.242727
1162.975463	78.727157	68.247732
1162.204598	60.342534	68.252737
1161.977130	64.237578	68.257742
1161.348680	70.527149	68.262746
1160.770885	66.548933	68.267751
1159.720750	65.608955	68.272756
1159.069716	71.337566	68.277761
1158.702075	72.034743	68.282766
1157.914310	77.427131	68.287770
1157.325786	66.117735	68.292775
1156.527595	75.515693	68.297780
1155.925026	70.584199	68.302785
1155.607489	68.690341	68.307790
1154.331910	68.306618	68.312794
1153.652179	57.290859	68.317799
1152.862583	69.849259	68.322804
1152.596748	67.288007	68.327809
1152.665965	60.921870	68.332814
1151.332715	59.120170	68.337818
1151.009125	61.442499	68.342823
1150.360664	73.273553	68.347828
1149.208321	65.163608	68.352833
1148.348559	54.230103	68.357838
1147.442880	65.662088	68.362842
1147.174552	65.029861	68.367847
1146.317266	64.652155	68.372852
1146.228535	55.311757	68.377857
1145.965616	69.473743	68.382862
1144.602521	67.016044	68.387866
1144.317965	59.296369	68.392871
1143.355056	66.157957	68.397876
1142.277172	63.352121	68.402881
1141.599276	58.342730	68.407886
1141.184221	61.991641	68.412890
1141.192523	62.807224	68.417895
1140.672268	74.897012	68.422900
1139.906771	65.960716	68.427905
1139.391270	57.186516	68.432910
1138.125308	64.198808	68.437914
1137.467493	57.369562	68.442919
1136.879098	55.315359	68.447924
1135.834360	65.725515	68.452929
1135.201899	72.678055	68.457934
1134.464234	65.099833	68.462938
1134.051070	56.599519	68.467943
1133.736947	58.925075	68.472948
1133.078167	66.012685	68.477953
1131.957365	58.780836	68.482958
1131.135448	69.557682	68.487962
1130.916155	67.354886	68.492967
1129.932093	67.271741	68.497972
1129.943401	66.016293	68.502977
1129.249161	72.816232	68.507982
1128.106567	68.211916	68.512986
1127.421677	68.314579	68.517991
1127.297608	68.433698	68.522996
1126.277118	62.089496	68.528001
1125.610557	66.111152	68.533006
1124.709424	63.422292	68.538010
1124.202873	69.124773	68.543015
1123.393911	71.522731	68.548020
1122.172565	68.917918	68.553025
1121.965157	78.543619	68.558030
1121.590685	72.967146	68.563034
1121.085324	60.113307	68.568039
1120.424011	76.098556	68.573044
1119.286066	64.559593	68.578049
1118.612602	69.153211	68.583054
1117.882831	67.140422	68.588058
1117.610362	62.309402	68.593063
1117.496835	61.997911	68.598068
1116.438185	63.891532	68.603073
1115.684751	67.934894	68.608078
1114.808119	59.274911	68.613082
1114.502842	59.443354	68.618087
1113.697607	72.425300	68.623092
1112.949164	66.446264	68.628097
1112.346900	61.961018	68.633102
1111.435380	70.790379	68.638106
1111.337672	60.803278	68.643111
1110.205152	57.307554	68.648116
1109.523305	62.246282	68.653121
1109.123412	59.214348	68.658126
1108.538599	69.305353	68.663130
1107.960109	64.228118	68.668135
1106.992729	75.756668	68.673140
1106.328465	78.300351	68.678145
1105.806583	70.069644	68.683150
1104.366011	71.319117	68.688154
1103.938529	69.122630	68.693159
1103.256979	69.309924	68.698164
1102.998500	78.104803	68.703169
1102.870244	71.560338	68.708174
1102.104020	72.114341	68.713178
1101.629952	65.366264	68.718183
1100.546927	71.456915	68.723188
1099.862625	81.429712	68.728193
1099.693330	65.029443	68.733198
1098.139256	75.017583	68.738202
1097.793193	65.618769	68.743207
1096.999228	78.438080	68.748212
1096.636106	66.324870	68.753217
1095.487396	57.730252	68.758222
1094.816307	75.664606	68.763226
1094.016548	61.269602	68.768231
1093.910865	63.385386	68.773236
1093.496326	70.192880	68.778241
1092.991407	71.731924	68.783246
1091.855224	67.178646	68.788250
1091.556682	69.017602	68.793255
1090.732206	64.777444	68.798260
1089.398892	66.449837	68.803265
1088.856808	62.221531	68.808270
1088.298142	70.701455	68.813274
1088.337618	56.568779	68.818279
1087.548716	71.733801	68.823284
1086.322484	70.798211	68.828289
1086.255457	63.409798	68.833294
1085.503253	76.392779	68.838298
1084.586635	68.371527	68.843303
1083.888444	68.457394	68.848308
1083.168017	61.876246	68.853313
1083.020527	59.042288	68.858318
1081.729494	75.004706	68.863322
1081.187552	63.776238	68.868327
1080.660540	62.220067	68.873332
1079.857299	67.506122	68.878337
1079.653080	56.247593	68.883342
1078.103763	61.847870	68.888346
1077.658151	58.058388	68.893351
1077.206299	61.862972	68.898356
1076.722827	71.354385	68.903361
1076.462002	64.528238	68.908366
1075.353175	76.478268	68.913370
1074.832355	64.951550	68.918375
1074.267286	77.007472	68.923380
1073.198063	67.474539	68.928385
1072.179855	60.136514	68.933390
1071.345970	59.149558	68.938394
1071.291744	61.559934	68.943399
1070.939913	70.938942	68.948404
1070.337044	69.508380	68.953409
1070.050226	53.030633	68.958414
1068.838770	77.748307	68.963418
1068.110532	70.703197	68.968423
1067.692915	61.178580	68.973428
1066.285951	74.811349	68.978433
1065.910194	59.614045	68.983438
1065.452790	71.266481	68.988442
1064.937736	64.099153	68.993447
1064.492954	74.637825	68.998452
1063.454435	66.505088	69.003457
1062.820045	68.179852	69.008462
1062.375794	63.024506	69.013466
1061.592518	66.779313	69.018471
1060.544820	58.307418	69.023476
1059.439244	66.762381	69.028481
1059.599455	65.880641	69.033486
1059.140092	71.840555	69.038490
1058.524314	67.075197	69.043495
1057.424861	74.969370	69.048500
1057.163296	71.801896	69.053505
1056.490060	64.705466	69.058510
1054.805282	68.578457	69.063514
1054.377652	61.870315	69.068519
1054.119086	72.171203	69.073524
1053.412300	65.643087	69.078529
1053.438386	61.854264	69.083534
1052.360955	67.485145	69.088538
1051.612332	61.036228	69.093543
1051.184456	68.372552	69.098548
1050.542213	67.131187	69.103553
1049.304739	63.234292	69.108558
1048.330265	73.705842	69.113562
1048.032486	64.594251	69.118567
1048.075190	70.390716	69.123572
1047.229697	69.828240	69.128577
1046.611635	60.532638	69.133582
1045.669835	66.843692	69.138586
1045.211987	60.023665	69.143591
1043.951281	76.500092	69.148596
1043.194692	62.945072	69.153601
1043.068722	62.955687	69.158606
1042.229480	71.590640	69.163610
1041.604451	66.676947	69.168615
1041.089241	71.054593	69.173620
1040.067236	59.893053	69.178625
1039.768978	58.363578	69.183630
1039.120045	71.063625	69.188634
1038.758145	57.330703	69.193639
1037.622897	61.964684	69.198644
1037.007201	64.667812	69.203649
1036.728588	56.352700	69.208654
1035.929836	62.667806	69.213658
1034.800598	57.608827	69.218663
1034.139018	65.296146	69.223668
1033.480470	65.288987	69.228673
1033.204154	54.745264	69.233678
1032.786337	67.410117	69.238682
1031.903257	53.173486	69.243687
1031.092122	69.603619	69.248692
1030.551576	61.527297	69.253697
1029.764066	65.760605	69.258702
1028.811083	62.496555	69.263706
1028.141875	61.300487	69.268711
1027.693425	62.053116	69.273716
1027.319340	67.450683	69.278721
1027.026921	62.701701	69.283726
1025.607945	63.496770	69.288730
1025.101298	71.127906	69.293735
1024.615810	63.462297	69.298740
1023.740461	64.281267	69.303745
1023.264153	62.575115	69.308750
1022.379750	61.608829	69.313754
1021.834953	60.025538	69.318759
1021.302356	55.478774	69.323764
1020.516660	62.627596	69.328769
1019.767917	54.759446	69.333774
1018.968463	65.389235	69.338778
1018.741146	61.956121	69.343783
1017.809232	56.676522	69.348788
1016.941055	68.417965	69.353793
1016.641655	56.901777	69.358798
1015.881785	72.751323	69.363802
1015.528116	60.917335	69.368807
1014.244373	67.393188	69.373812
1013.511927	61.572496	69.378817
1013.033150	64.280654	69.383822
1012.442875	74.560200	69.388826
1012.261074	63.624544	69.393831
1011.585395	76.076540	69.398836
1010.616836	66.190155	69.403841
1010.382223	72.592137	69.408846
1009.530013	65.175690	69.413850
1008.176237	71.717884	69.418855
1007.918617	58.370505	69.423860
1007.354671	66.026525	69.428865
1007.017453	57.848476	69.433870
1005.757313	65.918039	69.438874
1004.782070	68.083865	69.443879
1004.431750	67.354311	69.448884
1003.727897	73.521866	69.453889
1004.078036	64.668324	69.458894
1003.203370	75.819448	69.463898
1002.142564	65.534581	69.468903
1001.512454	67.973504	69.473908
1000.747553	63.020577	69.478913
999.969935	63.691541	69.483918
998.779114	74.189641	69.488922
998.345200	69.817990	69.493927
998.220376	70.635829	69.498932
997.737999	67.087179	69.503937
997.239810	65.778754	69.508942
995.920423	75.627103	69.513946
995.403912	66.096160	69.518951
994.980710	75.297293	69.523956
994.004411	74.211595	69.528961
993.795946	66.481417	69.533966
993.162391	68.611806	69.538970
992.180166	71.559343	69.543975
991.398025	64.261066	69.548980
990.330257	76.452172	69.553985
990.269991	61.999482	69.558990
989.543252	73.164918	69.563994
988.901096	57.950102	69.568999
987.911779	71.068591	69.574004
987.299629	68.731197	69.579009
987.362596	64.272607	69.584014
985.957503	70.707858	69.589018
984.783543	67.628795	69.594023
985.036691	58.595145	69.599028
984.477539	60.989665	69.604033
984.053863	62.271372	69.609038
982.524361	61.172775	69.614042
981.870061	71.853597	69.619047
981.667707	71.644555	69.624052
980.874767	72.111381	69.629057
980.770765	68.086213	69.634062
979.562453	74.308807	69.639066
978.766947	73.717901	69.644071
978.537545	64.237476	69.649076
977.508520	68.135487	69.654081
976.576173	61.450900	69.659086
975.883557	63.835118	69.664090
975.514661	71.505843	69.669095
975.329166	69.967895	69.674100
974.725709	71.295556	69.679105
973.963000	64.487783	69.684110
973.020204	69.947460	69.689114
972.464169	72.655303	69.694119
971.133869	64.647888	69.699124
970.450462	71.114973	69.704129
970.157667	63.396641	69.709134
969.737830	66.994296	69.714138
969.599143	70.861031	69.719143
968.563181	61.792800	69.724148
967.345080	72.459254	69.729153
966.887368	67.067950	69.734158
966.524276	62.257682	69.739162
965.835343	69.686015	69.744167
964.843761	66.008661	69.749172
963.896936	61.534129	69.754177
964.027216	63.025740	69.759182
963.343163	68.663447	69.764186
962.572402	67.325860	69.769191
961.822350	71.843389	69.774196
961.159021	62.846755	69.779201
960.599947	64.648330	69.784206
959.337049	70.706151	69.789210
958.746844	63.227535	69.794215
958.510389	74.412734	69.799220
957.868300	76.066670	69.804225
957.579302	53.330343	69.809230
956.372630	68.539778	69.814234
955.554390	64.131521	69.819239
955.271285	61.011646	69.824244
954.699716	71.233027	69.829249
953.732686	62.735732	69.834254
953.059400	76.330652	69.839258
952.351818	63.726666	69.844263
952.360137	55.190872	69.849268
950.970169	73.364202	69.854273
950.479067	67.155040	69.859278
949.753075	71.298158	69.864282
949.303628	60.916040	69.869287
948.690475	69.663272	69.874292
947.424663	66.031139	69.879297
946.844381	56.623905	69.884302
946.469294	70.067289	69.889306
946.037208	71.239954	69.894311
945.733926	60.880311	69.899316
944.346950	72.138198	69.904321
943.774132	55.783266	69.909326
943.512798	72.442895	69.914330
942.790613	65.289638	69.919335
941.873229	64.200895	69.924340
940.911662	57.489436	69.929345
940.845471	63.836230	69.934350
940.418232	53.348084	69.939354
938.768020	64.662048	69.944359
938.445161	62.898380	69.949364
937.497553	73.531265	69.954369
937.259271	64.585274	69.959374
937.139158	70.134824	69.964378
936.344768	65.740125	69.969383
935.480399	68.752507	69.974388
934.440205	70.824615	69.979393
934.122425	70.685984	69.984398
933.078632	78.227567	69.989402
932.486616	74.284790	69.994407
932.284508	57.684788	69.999412
931.572189	72.268363	70.004417
930.534891	66.896757	70.009422
929.845279	57.634660	70.014426
929.218557	69.700401	70.019431
929.269738	61.351750	70.024436
927.969766	62.605755	70.029441
927.387349	52.216425	70.034446
926.809814	64.826270	70.039450
926.168909	66.768608	70.044455
925.864411	65.762114	70.049460
924.387406	73.547678	70.054465
923.655847	60.901791	70.059470
923.640878	62.220971	70.064474
923.165139	58.933059	70.069479
922.053777	62.913578	70.074484
921.002983	75.617668	70.079489
920.663113	58.755738	70.084494
920.471874	58.587510	70.089498
919.499719	60.700835	70.094503
918.853729	59.854342	70.099508
918.034863	67.894720	70.104513
917.721784	63.171121	70.109518
917.165809	54.958520	70.114522
915.649068	72.232668	70.119527
915.489171	58.079703	70.124532
914.660119	68.558105	70.129537
914.553404	54.456606	70.134542
913.710322	68.215739	70.139546
912.678311	72.401256	70.144551
912.409605	67.445090	70.149556
911.281704	65.606111	70.154561
911.040251	61.535015	70.159566
910.075727	63.968828	70.164570
909.308875	63.359192	70.169575
909.031828	61.127765	70.174580
908.292996	67.067515	70.179585
907.683265	56.636803	70.184590
906.896065	65.170462	70.189594
906.133223	62.853918	70.194599
905.997385	58.157310	70.199604
904.927122	63.952683	70.204609
904.188425	62.898596	70.209614
903.587743	67.311942	70.214618
902.983963	61.540198	70.219623
902.818011	64.646447	70.224628
901.360754	65.207979	70.229633
900.915992	65.953735	70.234638
900.596924	72.842248	70.239642
899.806401	70.348760	70.244647
898.889440	71.532365	70.249652
897.872894	76.018204	70.254657
897.642879	67.674879	70.259662
897.109093	72.476553	70.264666
896.542913	73.650065	70.269671
895.870915	63.383805	70.274676
895.027623	67.709606	70.279681
894.602590	66.498370	70.284686
893.661582	65.720911	70.289690
893.025829	68.151295	70.294695
892.339218	68.270065	70.299700
891.797860	67.831129	70.304705
891.255813	64.098034	70.309710
890.142541	67.019154	70.314714
889.411175	68.619505	70.319719
889.286029	72.553473	70.324724
888.569766	68.638368	70.329729
887.792581	65.882564	70.334734
886.899249	63.009627	70.339738
886.431754	60.444235	70.344743
885.797582	65.488966	70.349748
885.233943	70.325354	70.354753
884.771241	61.746253	70.359758
883.790651	70.197156	70.364762
883.130769	67.709691	70.369767
882.572923	73.086056	70.374772
881.260298	72.471824	70.379777
880.849419	56.699851	70.384782
880.566990	75.111682	70.389786
879.584300	71.287867	70.394791
879.869072	62.419494	70.399796
878.540927	76.058718	70.404801
877.993640	57.403694	70.409806
877.550361	60.976705	70.414810
876.339923	71.776014	70.419815
875.645228	61.947038	70.424820
874.814532	67.833606	70.429825
874.451451	62.755272	70.434830
874.102262	62.050789	70.439834
873.427311	66.966395	70.444839
872.440477	60.197487	70.449844
871.544713	64.258830	70.454849
871.508846	58.188554	70.459854
871.435023	55.066924	70.464858
869.993069	66.421897	70.469863
869.180254	63.247568	70.474868
868.765725	66.082719	70.479873
867.897500	64.415321	70.484878
867.009268	60.828795	70.489882
866.212365	68.912999	70.494887
866.184866	61.945676	70.499892
865.700196	63.811122	70.504897
864.654783	64.663521	70.509902
864.105494	60.285034	70.514906
863.367327	70.537671	70.519911
863.093875	71.680370	70.524916
861.480916	62.656718	70.529921
861.129635	58.972118	70.534926
860.563007	54.227385	70.539930
859.998809	58.825742	70.544935
860.030099	62.600768	70.549940
858.473257	67.800241	70.554945
857.868865	63.255483	70.559950
857.236335	63.529658	70.564954
857.003979	53.879423	70.569959
856.338500	61.926938	70.574964
855.291186	58.947634	70.579969
855.140065	55.166524	70.584974
853.807998	51.548144	70.589978
852.855928	51.833755	70.594983
852.683014	55.038882	70.599988
851.881304	69.291338	70.604993
851.771332	60.203518	70.609998
851.191638	62.295403	70.615002
849.875654	71.561371	70.620007
849.328340	61.801988	70.625012
848.630687	58.521029	70.630017
848.443069	61.696959	70.635022
847.889278	66.098120	70.640026
846.586200	70.113916	70.645031
846.472091	64.201173	70.650036
845.578175	58.898252	70.655041
844.458398	61.072947	70.660046
844.076155	67.171997	70.665050
843.372593	65.446860	70.670055
843.292739	59.706862	70.675060
842.363534	68.230023	70.680065
841.341077	64.322670	70.685070
841.219495	49.283690	70.690074
840.274408	68.253568	70.695079
839.474274	62.248168	70.700084
838.366400	62.579084	70.705089
838.224722	61.876270	70.710094
837.659339	62.827317	70.715098
837.151758	64.224904	70.720103
836.515475	55.452674	70.725108
835.428637	59.899257	70.730113
834.791296	59.560767	70.735118
834.400425	55.218576	70.740122
833.627560	58.776242	70.745127
832.824921	59.724053	70.750132
831.928021	63.415004	70.755137
831.825865	65.445077	70.760142
831.340583	61.600461	70.765146
830.166963	62.471703	70.770151
829.289135	63.324250	70.775156
828.716872	58.638769	70.780161
828.299966	50.383562	70.785166
827.979228	62.533068	70.790170
827.246602	60.959219	70.795175
826.383469	56.930320	70.800180
825.827637	57.119755	70.805185
825.085113	52.587535	70.810190
824.139449	62.059491	70.815194
823.334318	63.767795	70.820199
822.571793	63.529659	70.825204
822.461495	56.830989	70.830209
821.958613	64.209232	70.835214
821.268822	48.606263	70.840218
820.229390	61.978767	70.845223
820.095314	54.123243	70.850228
818.931330	68.430214	70.855233
818.248353	53.682445	70.860238
817.801749	52.045726	70.865242
817.148393	65.560207	70.870247
817.032582	57.305958	70.875252
815.719292	59.880475	70.880257
815.121058	57.446297	70.885262
814.685489	62.036803	70.890266
813.832089	58.873687	70.895271
812.986504	53.793324	70.900276
812.253197	50.273625	70.905281
811.672910	58.474743	70.910286
811.622978	51.430576	70.915290
810.195306	61.297806	70.920295
810.001970	56.482628	70.925300
809.503581	58.359728	70.930305
808.603986	63.263797	70.935310
807.666254	52.213551	70.940314
806.867391	69.979021	70.945319
806.716166	51.563765	70.950324
806.142243	66.268822	70.955329
805.045206	58.022532	70.960334
804.242307	51.558696	70.965338
803.620247	58.651556	70.970343
803.469274	56.594042	70.975348
802.946246	54.937951	70.980353
801.943697	64.688630	70.985358
801.382813	56.569886	70.990362
800.540307	61.193632	70.995367
800.311722	56.511799	71.000372
799.007108	53.619211	71.005377
798.344794	67.206085	71.010382
798.065193	59.268070	71.015386
797.454665	61.323874	71.020391
796.816784	65.167571	71.025396
795.707953	57.552370	71.030401
794.994876	57.602839	71.035406
794.678534	61.346467	71.040410
794.165247	57.995175	71.045415
793.218218	53.743102	71.050420
792.684481	59.077791	71.055425
792.042938	55.489873	71.060430
791.686813	52.597691	71.065434
790.511887	57.818405	71.070439
789.889007	48.895828	71.075444
789.184984	45.808293	71.080449
788.728299	48.435696	71.085454
788.438308	45.736416	71.090458
787.311420	51.949272	71.095463
787.208156	43.934312	71.100468
786.016627	50.201613	71.105473
784.954251	59.698465	71.110478
784.048782	50.199554	71.115482
783.344582	56.720442	71.120487
783.470466	45.404703	71.125492
782.882706	52.717608	71.130497
782.477230	53.379859	71.135502
782.048921	44.645511	71.140506
780.919773	57.461445	71.145511
780.633694	51.337970	71.150516
779.327757	48.253216	71.155521
778.218864	50.240124	71.160526
778.023516	46.063940	71.165530
777.495080	48.411031	71.170535
777.461503	42.628986	71.175540
776.057179	48.013955	71.180545
775.469011	55.372659	71.185550
775.270894	51.681041	71.190554
773.702074	55.406435	71.195559
773.196687	59.410393	71.200564
772.522524	50.863416	71.205569
772.102974	51.829107	71.210574
771.976612	46.610613	71.215578
771.040983	51.960396	71.220583
770.323290	41.851284	71.225588
769.743281	61.666642	71.230593
768.973397	49.482674	71.235598
768.489569	45.629961	71.240602
767.159877	48.353768	71.245607
766.745181	44.469550	71.250612
766.385519	48.895009	71.255617
765.515847	58.449499	71.260622
764.959876	42.492521	71.265626
764.081186	58.290034	71.270631
763.795955	52.174311	71.275636
763.300318	53.232542	71.280641
762.105115	52.367868	71.285646
761.762351	45.457060	71.290650
760.743644	53.502473	71.295655
760.521700	35.142664	71.300660
759.540672	56.117840	71.305665
758.721797	41.429591	71.310670
758.201994	43.817887	71.315674
757.745357	52.101826	71.320679
757.417828	42.569272	71.325684
756.214769	43.153497	71.330689
755.204329	49.265825	71.335694
755.247149	43.586737	71.340698
754.422749	46.602269	71.345703
753.658436	40.357819	71.350708
752.631859	48.026016	71.355713
751.885520	43.678935	71.360718
752.255081	37.902100	71.365722
751.170393	49.384740	71.370727
750.461259	37.616896	71.375732
749.576693	40.154728	71.380737
749.351024	52.246512	71.385742
748.589472	48.056395	71.390746
747.424098	52.365701	71.395751
747.114620	35.342897	71.400756
746.537940	50.879436	71.405761
745.605068	55.408773	71.410766
744.768084	41.030921	71.415770
744.119458	42.939834	71.420775
743.738680	47.236193	71.425780
743.051922	46.222773	71.430785
742.792561	40.002015	71.435790
742.477374	40.318737	71.440794
741.352792	53.515576	71.445799
740.802283	36.868614	71.450804
739.514431	44.119516	71.455809
738.545875	55.711409	71.460814
738.325665	39.119093	71.465818
737.727241	55.445999	71.470823
737.385689	40.598190	71.475828
736.997633	45.419256	71.480833
735.767418	44.061853	71.485838
735.296154	40.552502	71.490842
734.455680	50.140192	71.495847
733.615380	41.509298	71.500852
732.646065	48.119710	71.505857
731.994567	46.414705	71.510862
731.801018	41.471842	71.515866
731.107526	54.467587	71.520871
730.887254	44.801266	71.525876
730.672507	55.874178	71.530881
729.502720	54.093994	71.535886
729.090669	48.851602	71.540890
727.937201	52.096154	71.545895
726.902891	43.280108	71.550900
726.397769	57.051689	71.555905
725.954816	40.423875	71.560910
725.453492	52.162153	71.565914
724.682273	55.386848	71.570919
724.174606	46.393913	71.575924
723.871374	47.241744	71.580929
722.792028	54.063646	71.585934
721.928251	40.855441	71.590938
721.163316	50.073139	71.595943
720.840690	58.018780	71.600948
719.997387	48.491079	71.605953
719.056469	51.856334	71.610958
718.770535	37.040679	71.615962
718.217036	55.410473	71.620967
717.610986	38.209390	71.625972
716.469468	44.549179	71.630977
715.753353	50.444347	71.635982
715.403475	41.484643	71.640986
714.845413	51.304917	71.645991
714.182377	47.390863	71.650996
713.261108	39.626003	71.656001
712.772151	43.843394	71.661006
712.389973	46.056822	71.666010
711.193859	53.435061	71.671015
710.350157	40.885987	71.676020
710.084671	52.711296	71.681025
709.578838	41.641227	71.686030
709.064413	41.116042	71.691034
707.895153	50.582623	71.696039
707.218324	42.846653	71.701044
706.669557	53.494928	71.706049
706.351737	45.540947	71.711054
705.931810	47.383495	71.716058
704.499595	43.492565	71.721063
703.976724	43.407120	71.726068
703.335697	37.808535	71.731073
702.992131	56.490257	71.736078
702.497813	48.449260	71.741082
701.480586	48.100328	71.746087
700.950060	48.484457	71.751092
700.466714	41.168693	71.756097
699.240553	49.026382	71.761102
698.964974	41.497764	71.766106
698.000612	32.921338	71.771111
697.665858	45.700688	71.776116
696.975495	36.255886	71.781121
695.819198	49.766868	71.786126
695.586469	33.673303	71.791130
694.942547	39.952793	71.796135
694.425069	45.992955	71.801140
693.531638	37.737971	71.806145
692.766651	44.175511	71.811150
692.917688	33.024518	71.816154
691.425191	51.323046	71.821159
690.721101	43.529922	71.826164
690.136712	36.422641	71.831169
689.555949	41.162431	71.836174
689.442687	32.313296	71.841178
688.230324	49.751935	71.846183
687.086391	44.020540	71.851188
686.934172	40.949254	71.856193
686.408292	39.952813	71.861198
685.988634	35.288812	71.866202
685.050491	38.518017	71.871207
684.137797	48.397914	71.876212
683.702210	41.254323	71.881217
683.290606	39.878564	71.886222
682.613113	45.098960	71.891226
681.565313	44.858984	71.896231
680.889321	47.817791	71.901236
680.817177	41.072069	71.906241
679.489083	48.230059	71.911246
678.937393	26.322605	71.916250
678.198155	52.068990	71.921255
677.881069	35.673470	71.926260
677.482379	47.573601	71.931265
676.165814	54.028015	71.936270
675.836847	46.353359	71.941274
675.308080	44.223549	71.946279
674.588149	53.746329	71.951284
673.921826	48.298434	71.956289
673.108175	55.576364	71.961294
672.913009	37.732709	71.966298
671.547867	49.752040	71.971303
670.760232	39.920612	71.976308
670.470797	52.855177	71.981313
670.018638	38.693631	71.986318
669.436905	51.222154	71.991322
668.224027	49.896717	71.996327
667.573776	43.050663	72.001332
667.176787	45.607077	72.006337
666.490038	45.159804	72.011342
665.702990	35.722525	72.016346
664.747020	56.266372	72.021351
664.278460	40.983069	72.026356
664.035093	35.521448	72.031361
663.343736	41.459990	72.036366
663.022495	48.129653	72.041370
661.808863	45.555393	72.046375
661.485626	44.110372	72.051380
660.631324	45.613665	72.056385
659.489662	47.933847	72.061390
659.071453	45.532546	72.066394
658.464186	46.674804	72.071399
657.797246	47.853372	72.076404
657.575877	51.175030	72.081409
656.696101	56.643690	72.086414
656.353969	47.321640	72.091418
655.342307	57.012306	72.096423
654.321372	44.239166	72.101428
653.726100	43.334206	72.106433
652.975520	51.180837	72.111438
652.595034	40.557605	72.116442
652.075487	58.639723	72.121447
651.532966	48.393949	72.126452
650.780415	43.149029	72.131457
649.842375	52.777508	72.136462
649.623797	41.365248	72.141466
648.609474	54.542981	72.146471
647.800507	48.759841	72.151476
647.319497	51.190867	72.156481
646.811707	50.869643	72.161486
646.400506	49.672021	72.166490
645.068601	51.964157	72.171495
644.480330	56.605808	72.176500
643.988853	43.344660	72.181505
643.597699	48.924745	72.186510
643.033868	44.400404	72.191514
642.286212	50.381037	72.196519
641.662434	50.655449	72.201524
640.834186	53.720515	72.206529
639.767720	50.059962	72.211534
639.209407	47.102234	72.216538
638.697409	47.631660	72.221543
638.225595	54.128186	72.226548
637.456275	49.644453	72.231553
636.570473	55.155079	72.236558
636.299449	47.726670	72.241562
635.377073	38.720961	72.246567
634.778173	50.246124	72.251572
633.677360	37.421067	72.256577
632.955600	45.092799	72.261582
632.680217	51.089688	72.266586
632.404050	46.514808	72.271591
631.920586	49.651125	72.276596
631.184559	46.149267	72.281601
630.350349	44.109111	72.286606
629.935299	42.008511	72.291610
628.584437	51.603389	72.296615
627.934725	48.560872	72.301620
627.920927	39.486167	72.306625
627.175382	56.628140	72.311630
626.277593	42.028217	72.316634
625.419759	49.213844	72.321639
624.942439	46.172259	72.326644
624.498687	45.500220	72.331649
623.423882	50.334472	72.336654
622.555457	46.361692	72.341658
621.749328	47.653898	72.346663
621.554779	42.608708	72.351668
621.462448	42.363251	72.356673
620.276521	44.785116	72.361678
619.466515	40.831420	72.366682
618.879012	39.524686	72.371687
618.551374	41.188546	72.376692
618.087769	34.114092	72.381697
616.641029	52.383287	72.386702
616.419508	42.420722	72.391706
615.976849	44.465599	72.396711
614.763546	50.687552	72.401716
614.300958	44.566989	72.406721
613.341694	48.977567	72.411726
613.225209	33.972533	72.416730
612.621638	53.957214	72.421735
611.718132	39.501715	72.426740
610.674747	51.338943	72.431745
610.389943	51.873193	72.436750
610.268087	46.247145	72.441754
609.189641	51.815266	72.446759
608.342557	44.112754	72.451764
608.022921	39.879117	72.456769
606.636464	47.418595	72.461774
605.819000	35.702758	72.466778
605.406643	46.963248	72.471783
604.993635	46.835095	72.476788
604.761936	44.276369	72.481793
604.250831	44.886084	72.486798
603.306010	40.513895	72.491802
602.471298	53.726113	72.496807
601.823943	47.917252	72.501812
600.490390	42.223987	72.506817
599.541017	44.789537	72.511822
599.502062	44.136611	72.516826
598.934701	53.900034	72.521831
598.676279	51.008096	72.526836
598.106704	41.236585	72.531841
597.429064	54.739179	72.536846
596.872616	50.456524	72.541850
596.020733	43.953266	72.546855
595.357377	43.872871	72.551860
594.493813	44.563953	72.556865
593.710823	49.408510	72.561870
593.379331	41.534004	72.566874
592.720527	41.383499	72.571879
591.323091	42.277881	72.576884
591.137828	38.081194	72.581889
590.255859	49.992067	72.586894
590.430387	38.354787	72.591898
589.835848	34.284786	72.596903
588.404750	34.872294	72.601908
588.234546	40.656887	72.606913
587.707518	35.786082	72.611918
586.426478	36.740775	72.616922
585.682146	46.193336	72.621927
585.358540	47.437089	72.626932
584.772070	44.788212	72.631937
583.162216	49.010683	72.636942
582.514346	41.028873	72.641946
581.850630	53.967856	72.646951
581.254201	41.680658	72.651956
581.639376	51.156753	72.656961
581.090508	49.717718	72.661966
580.740924	51.359847	72.666970
579.622168	47.822769	72.671975
578.661957	50.941986	72.676980
578.348935	44.835457	72.681985
576.940162	47.043677	72.686990
576.136259	56.505734	72.691994
575.632165	47.272578	72.696999
574.989627	49.208948	72.702004
575.212946	37.240624	72.707009
574.366620	50.982972	72.712014
573.647939	45.797340	72.717018
573.206057	41.307212	72.722023
572.160947	47.538663	72.727028
571.307643	48.371622	72.732033
570.322190	50.848312	72.737038
570.253789	39.762234	72.742042
569.535484	54.457175	72.747047
568.589351	48.107710	72.752052
567.723551	52.441917	72.757057
567.081508	51.208536	72.762062
567.050395	50.443976	72.767066
566.750097	51.701365	72.772071
565.729910	52.414249	72.777076
565.367994	43.724579	72.782081
564.142726	52.050536	72.787086
563.222237	48.350999	72.792090
562.237482	56.663882	72.797095
562.160115	44.322399	72.802100
561.861961	49.770984	72.807105
560.913003	55.206536	72.812110
560.097933	47.085782	72.817114
559.549808	53.931940	72.822119
559.041622	64.602159	72.827124
558.181693	42.811642	72.832129
557.086757	60.375130	72.837134
556.931892	48.544305	72.842138
556.452341	53.578662	72.847143
555.742830	53.819443	72.852148
554.774313	45.650593	72.857153
553.963101	51.537291	72.862158
553.577321	46.885266	72.867162
553.084937	49.111539	72.872167
552.452025	60.747793	72.877172
551.704344	49.572788	72.882177
551.120347	49.580690	72.887182
550.524225	54.356072	72.892186
549.622843	54.010828	72.897191
548.787622	44.360492	72.902196
548.481342	47.320366	72.907201
547.240418	51.761639	72.912206
546.121180	46.896860	72.917210
545.471719	47.161195	72.922215
545.552527	52.494226	72.927220
544.869033	54.225817	72.932225
544.357387	51.664379	72.937230
543.813521	45.965210	72.942234
543.583664	47.578811	72.947239
542.307881	56.040558	72.952244
542.074034	55.043362	72.957249
541.048226	58.367008	72.962254
540.043724	55.398375	72.967258
539.321072	53.413020	72.972263
539.042438	54.102413	72.977268
538.979299	57.337374	72.982273
538.046099	61.401630	72.987278
537.544888	53.582549	72.992282
536.849129	47.981693	72.997287
535.563296	54.445468	73.002292
534.664627	43.337104	73.007297
534.126315	59.588220	73.012302
533.835825	51.043293	73.017306
533.551221	39.766156	73.022311
532.461177	55.780300	73.027316
531.800347	51.104282	73.032321
531.000258	44.671648	73.037326
530.206746	57.968783	73.042330
529.556101	58.903515	73.047335
528.640217	56.002772	73.052340
528.467959	53.259543	73.057345
528.115242	49.956858	73.062350
527.495239	52.720704	73.067354
526.537228	49.968599	73.072359
525.667535	61.221528	73.077364
525.475162	48.143007	73.082369
524.248837	61.084890	73.087374
523.493681	58.999062	73.092378
523.147976	45.710003	73.097383
522.469022	58.047451	73.102388
522.189723	56.704260	73.107393
521.238026	47.532959	73.112398
520.428960	47.376447	73.117402
520.006867	50.887782	73.122407
519.210278	54.718971	73.127412
518.671612	38.820840	73.132417
517.605248	57.477340	73.137422
516.961352	52.607818	73.142426
516.543032	55.367924	73.147431
516.204861	49.861499	73.152436
515.336773	52.598635	73.157441
514.431222	58.304832	73.162446
514.152739	55.748836	73.167450
513.597503	52.620339	73.172455
512.178233	48.244918	73.177460
511.575574	51.431781	73.182465
510.658497	52.995585	73.187470
510.828145	45.512773	73.192474
510.538588	51.709044	73.197479
509.367430	56.708501	73.202484
508.741099	50.019535	73.207489
507.964833	56.550384	73.212494
507.505094	58.415074	73.217498
506.583943	48.877791	73.222503
505.652677	54.058230	73.227508
505.381014	52.945637	73.232513
504.886407	54.473683	73.237518
504.063259	45.499533	73.242522
502.982781	49.847457	73.247527
502.243375	59.322912	73.252532
502.163610	44.488660	73.257537
501.640980	67.469289	73.262542
501.404975	48.206609	73.267546
500.743927	49.653937	73.272551
499.123013	49.254601	73.277556
498.377005	39.702043	73.282561
497.527987	47.725236	73.287566
496.943799	48.373423	73.292570
496.599187	40.953613	73.297575
496.315240	54.770393	73.302580
496.197532	42.400657	73.307585
494.957864	58.643653	73.312590
494.112568	54.875394	73.317594
493.938793	45.840378	73.322599
492.519328	56.293069	73.327604
492.010268	43.928907	73.332609
491.583554	56.431178	73.337614
490.872901	45.310228	73.342618
490.593723	45.118197	73.347623
489.133313	48.413325	73.352628
488.668172	49.901986	73.357633
487.963478	42.760314	73.362638
487.728472	48.608851	73.367642
486.804957	37.911326	73.372647
485.853297	50.082482	73.377652
485.740987	32.640424	73.382657
485.003786	53.753414	73.387662
484.336720	53.310941	73.392666
483.901697	48.759815	73.397671
482.896283	55.232557	73.402676
482.333198	47.495892	73.407681
481.419833	48.060906	73.412686
480.686902	52.228892	73.417690
480.266485	50.296332	73.422695
479.641861	54.208945	73.427700
479.095973	47.021474	73.432705
477.813331	53.183569	73.437710
477.315126	54.131875	73.442714
477.069523	46.388789	73.447719
476.562615	59.290192	73.452724
475.895461	52.243464	73.457729
474.942747	55.616991	73.462734
474.167081	54.726621	73.467738
473.747149	46.527184	73.472743
472.548537	55.273132	73.477748
472.184439	52.123656	73.482753
471.437009	53.606832	73.487758
471.157066	48.452261	73.492762
470.908328	57.220347	73.497767
469.546924	56.103175	73.502772
469.040412	52.992158	73.507777
468.299453	47.169869	73.512782
467.577262	46.299368	73.517786
466.824461	49.158500	73.522791
465.788866	46.529168	73.527796
465.497351	50.272019	73.532801
465.141797	46.570829	73.537806
464.800783	46.185225	73.542810
464.189637	44.002359	73.547815
463.001403	50.132072	73.552820
463.042877	50.076615	73.557825
461.582003	51.429030	73.562830
460.937014	56.037173	73.567834
460.264267	39.654225	73.572839
459.559798	60.831398	73.577844
459.385692	40.004006	73.582849
458.542029	52.643666	73.587854
457.524999	50.416655	73.592858
456.953924	46.294065	73.597863
456.453328	53.452786	73.602868
456.076544	42.393778	73.607873
454.852830	54.791216	73.612878
454.558338	49.479694	73.617882
454.003720	50.110564	73.622887
453.348354	58.751048	73.627892
452.444083	51.395177	73.632897
451.752747	57.060955	73.637902
451.063785	44.917856	73.642906
450.859893	44.515139	73.647911
449.385946	51.038885	73.652916
448.916856	38.938031	73.657921
448.453152	50.818567	73.662926
448.437680	56.684170	73.667930
447.577271	46.585307	73.672935
446.727850	40.860733	73.677940
446.513510	49.498755	73.682945
445.126578	43.546007	73.687950
444.117955	42.949806	73.692954
443.831922	34.129810	73.697959
442.804635	48.847181	73.702964
443.015267	46.514466	73.707969
441.883786	45.431641	73.712974
440.945491	46.476879	73.717978
440.747423	37.272283	73.722983
440.176315	55.556578	73.727988
439.670967	45.904196	73.732993
438.603729	45.798306	73.737998
437.891086	48.624239	73.743002
437.512146	39.673964	73.748007
436.330438	59.753924	73.753012
435.804056	43.055927	73.758017
435.258071	54.826575	73.763022
434.387986	47.772773	73.768026
434.611246	47.300422	73.773031
433.276027	45.996173	73.778036
432.704221	42.517102	73.783041
432.350189	46.530112	73.788046
431.526864	48.999945	73.793050
430.602635	39.966242	73.798055
429.692060	49.191434	73.803060
429.320268	49.840488	73.808065
428.733966	52.900183	73.813070
427.897586	53.553875	73.818074
426.986433	48.848390	73.823079
426.502836	44.631446	73.828084
426.149646	37.504756	73.833089
425.853847	48.483332	73.838094
424.783212	56.776825	73.843098
424.169107	39.573997	73.848103
423.433472	58.810180	73.853108
423.091809	46.589678	73.858113
422.255567	45.850903	73.863118
421.161604	48.747060	73.868122
420.658821	48.912362	73.873127
420.006587	54.901498	73.878132
419.684360	40.437059	73.883137
418.748946	51.563283	73.888142
418.185563	47.157203	73.893146
417.529478	41.696725	73.898151
416.968638	45.186025	73.903156
416.371537	48.621180	73.908161
415.243138	52.473727	73.913166
414.716644	58.318252	73.918170
414.580406	45.713360	73.923175
413.527201	54.921863	73.928180
412.917132	53.311270	73.933185
412.109313	57.183702	73.938190
411.547454	56.689792	73.943194
411.332913	37.288117	73.948199
410.181843	50.836203	73.953204
409.580475	50.276050	73.958209
409.227060	41.703335	73.963214
407.667565	60.504671	73.968218
407.289928	46.003327	73.973223
406.738288	45.503060	73.978228
406.376041	49.706617	73.983233
405.866920	52.142162	73.988238
404.829773	52.570809	73.993242
404.351646	46.984206	73.998247
403.410426	54.090141	74.003252
403.279675	44.930014	74.008257
402.673997	53.419084	74.013262
401.679007	54.888109	74.018266
401.579078	45.372988	74.023271
400.209938	50.850311	74.028276
399.604136	44.719507	74.033281
398.749301	48.273004	74.038286
398.136772	50.490062	74.043290
397.950245	39.960573	74.048295
396.715531	48.805339	74.053300
396.118496	51.657017	74.058305
395.590973	41.254403	74.063310
395.138411	49.501454	74.068314
394.741696	52.220288	74.073319
393.702267	48.820470	74.078324
393.230290	50.657166	74.083329
392.419573	63.422486	74.088334
391.411627	63.012279	74.093338
390.547204	51.513746	74.098343
389.766190	56.987247	74.103348
389.509966	50.133689	74.108353
388.815225	55.263861	74.113358
388.733401	60.343675	74.118362
388.730173	55.080368	74.123367
386.991234	66.243187	74.128372
386.799415	52.634750	74.133377
386.087501	59.710461	74.138382
384.846531	58.425912	74.143386
384.223919	45.742412	74.148391
383.840638	61.516246	74.153396
383.513379	51.103794	74.158401
382.513726	43.170225	74.163406
381.551144	56.306669	74.168410
381.161975	45.798431	74.173415
380.606451	52.581138	74.178420
380.119667	39.235760	74.183425
379.127803	51.047499	74.188430
378.500000	57.389142	74.193434
378.161236	45.893587	74.198439
377.282271	50.997922	74.203444
376.271440	48.334722	74.208449
375.767734	48.296754	74.213454
375.282727	52.054676	74.218458
374.639360	46.174292	74.223463
373.815568	60.383027	74.228468
373.138040	53.144023	74.233473
372.724970	44.292240	74.238478
371.956782	44.695387	74.243482
371.319371	49.583036	74.248487
370.058000	48.527250	74.253492
369.790397	50.325074	74.258497
369.392157	52.377105	74.263502
368.779000	58.834687	74.268506
368.295991	47.248580	74.273511
367.197584	47.650735	74.278516
366.977876	49.781548	74.283521
365.968078	50.611128	74.288526
364.916441	46.893150	74.293530
364.212092	43.296448	74.298535
363.758661	58.576834	74.303540
363.549754	48.057220	74.308545
363.009272	44.510098	74.313550
362.032235	53.812134	74.318554
361.492831	44.936331	74.323559
360.640359	49.596481	74.328564
360.228765	48.451012	74.333569
359.403240	48.120558	74.338574
358.491053	56.800407	74.343578
358.528808	41.947458	74.348583
357.379404	59.204284	74.353588
356.824929	53.426432	74.358593
356.301155	49.313677	74.363598
355.664936	50.034843	74.368602
354.759507	48.513912	74.373607
353.980376	50.826916	74.378612
353.889100	44.934251	74.383617
352.728547	49.495266	74.388622
351.646104	41.961259	74.393626
351.303028	28.455805	74.398631
350.663312	44.393488	74.403636
350.389717	41.738968	74.408641
349.886134	41.661563	74.413646
349.035550	43.571217	74.418650
348.340892	46.416384	74.423655
346.814961	42.592651	74.428660
346.138549	42.515981	74.433665
345.984734	39.977991	74.438670
345.070021	52.621112	74.443674
344.710585	45.399238	74.448679
344.127053	44.197595	74.453684
344.024472	44.327520	74.458689
343.341756	38.999044	74.463694
342.396870	44.270011	74.468698
341.908029	44.135064	74.473703
340.768879	54.715039	74.478708
339.719502	54.046529	74.483713
339.440099	46.638436	74.488718
338.923499	51.522609	74.493722
338.674137	56.654352	74.498727
337.028594	48.945162	74.503732
336.384745	46.542037	74.508737
336.057348	46.397132	74.513742
335.143021	49.909668	74.518746
335.340326	45.284611	74.523751
334.578887	51.841522	74.528756
334.109638	54.179263	74.533761
333.145467	48.006244	74.538766
332.168654	56.057735	74.543770
331.390159	37.841940	74.548775
330.786385	46.398521	74.553780
330.408967	45.484154	74.558785
330.293673	42.659329	74.563790
328.806547	44.574243	74.568794
328.311088	52.071203	74.573799
327.405999	50.312110	74.578804
327.089533	50.928706	74.583809
326.755776	41.927102	74.588814
325.660077	51.088787	74.593818
325.117421	48.596999	74.598823
324.201918	52.768890	74.603828
323.315299	60.118462	74.608833
322.672530	50.002314	74.613838
322.247990	55.061052	74.618842
321.958543	51.811397	74.623847
321.483822	60.035185	74.628852
320.435947	47.438408	74.633857
319.914048	43.169248	74.638862
319.039155	58.731271	74.643866
318.627146	49.759481	74.648871
317.483679	59.764570	74.653876
316.977489	49.002185	74.658881
316.327304	53.874537	74.663886
315.774899	55.096439	74.668890
315.764817	53.429672	74.673895
314.392147	57.538812	74.678900
313.887944	46.252567	74.683905
313.304061	45.784269	74.688910
312.133249	50.359552	74.693914
311.377217	48.920482	74.698919
310.681059	62.974848	74.703924
310.458815	43.151801	74.708929
310.304333	57.741147	74.713934
309.369483	48.154103	74.718938
308.615177	42.887509	74.723943
308.009638	55.506596	74.728948
307.451765	45.304387	74.733953
306.514942	53.556091	74.738958
305.492704	52.924271	74.743962
304.953718	54.874164	74.748967
304.762324	53.774034	74.753972
303.968323	53.120030	74.758977
303.155180	43.193475	74.763982
301.793079	53.711225	74.768986
302.036609	41.955730	74.773991
301.506694	56.114480	74.778996
301.149650	45.448181	74.784001
300.128242	48.558327	74.789006
299.312948	53.042260	74.794010
298.868051	52.007765	74.799015
297.493654	57.758792	74.804020
296.807625	49.164996	74.809025
296.679071	49.187100	74.814030
295.727135	48.345384	74.819034
295.669832	51.547872	74.824039
294.626548	55.760640	74.829044
293.663130	50.109488	74.834049
293.221939	50.898932	74.839054
292.899817	52.798493	74.844058
292.356217	45.762101	74.849063
291.478454	52.356486	74.854068
290.536084	43.250046	74.859073
290.187637	46.767018	74.864078
288.854540	44.404380	74.869082
288.335987	40.191466	74.874087
287.730272	50.743202	74.879092
287.284243	47.778708	74.884097
287.122866	49.390875	74.889102
286.253814	50.246939	74.894106
285.456567	44.797964	74.899111
284.565576	54.217195	74.904116
284.144470	48.079064	74.909121
283.792515	38.414901	74.914126
282.342891	49.724042	74.919130
281.998361	48.572629	74.924135
281.527673	52.131165	74.929140
281.138773	49.067680	74.934145
280.288532	40.000178	74.939150
279.274580	44.400661	74.944154
278.937881	44.976334	74.949159
278.091726	37.147664	74.954164
277.041987	48.877190	74.959169
276.573589	50.227636	74.964174
275.900384	50.763907	74.969178
275.908305	42.813293	74.974183
275.568414	45.770664	74.979188
274.033494	49.404215	74.984193
273.628607	33.557403	74.989198
272.702856	48.845257	74.994202
271.894516	40.572169	74.999207
271.123846	49.306750	75.004212
270.668968	40.080040	75.009217
270.413160	44.056908	75.014222
269.596151	44.001093	75.019226
269.401706	40.192259	75.024231
268.217181	35.256032	75.029236
267.578403	44.187206	75.034241
267.183595	41.493672	75.039246
265.858915	50.179368	75.044250
265.625734	39.638418	75.049255
265.069154	43.795692	75.054260
264.571605	36.293082	75.059265
263.320124	42.748345	75.064270
262.149739	42.394047	75.069274
261.929393	34.637519	75.074279
261.685312	35.684130	75.079284
261.677513	40.441477	75.084289
260.692171	38.739357	75.089294
259.623578	42.203966	75.094298
259.200395	44.269449	75.099303
258.012006	41.620412	75.104308
257.307437	49.079749	75.109313
256.779144	44.996127	75.114318
256.334212	45.462900	75.119322
256.236288	38.637755	75.124327
255.038307	50.561229	75.129332
254.506547	50.508835	75.134337
254.054151	41.310118	75.139342
252.793469	50.744130	75.144346
252.020523	40.872692	75.149351
251.610424	37.963980	75.154356
251.324713	44.096570	75.159361
250.918486	36.557329	75.164366
249.420367	55.218055	75.169370
249.056824	38.565144	75.174375
248.520261	34.714656	75.179380
247.929385	44.035587	75.184385
246.915403	37.738089	75.189390
246.034207	48.745325	75.194394
245.734234	40.709755	75.199399
245.252214	38.175207	75.204404
244.671484	44.488865	75.209409
244.026635	35.629914	75.214414
242.955784	52.590392	75.219418
242.315501	44.230601	75.224423
242.049744	51.019176	75.229428
240.795147	46.464711	75.234433
240.382682	39.787479	75.239438
239.798238	48.055566	75.244442
239.662168	47.205242	75.249447
238.568963	42.544629	75.254452
237.697153	54.223731	75.259457
236.958295	43.441696	75.264462
236.391773	43.092074	75.269466
236.275007	45.089791	75.274471
234.859234	37.970104	75.279476
234.280514	37.601926	75.284481
233.969808	39.696790	75.289486
233.217712	49.002426	75.294490
232.875063	39.021403	75.299495
232.182491	40.842829	75.304500
231.512607	41.619854	75.309505
230.484743	28.155789	75.314510
229.682130	48.618476	75.319514
229.256672	35.760115	75.324519
228.574696	38.835100	75.329524
227.880437	46.948807	75.334529
227.218979	37.460154	75.339534
226.126416	48.023275	75.344538
225.736613	39.166248	75.349543
225.613279	43.724394	75.354548
224.935483	39.259340	75.359553
224.392718	40.017679	75.364558
223.306281	48.739530	75.369562
222.791238	33.421227	75.374567
221.505802	42.543804	75.379572
220.787141	42.021320	75.384577
220.525117	39.514784	75.389582
219.418944	42.397200	75.394586
219.553401	30.312177	75.399591
219.208231	43.949462	75.404596
218.834079	44.731386	75.409601
217.849510	38.629484	75.414606
216.705316	43.618452	75.419610
215.537590	38.614919	75.424615
215.289059	44.061920	75.429620
214.460315	42.547742	75.434625
214.178886	44.779867	75.439630
213.226366	43.236537	75.444634
212.567100	39.173807	75.449639
211.955879	37.598146	75.454644
211.462826	49.497565	75.459649
211.243056	26.189128	75.464654
210.236170	45.347129	75.469658
209.569072	48.238400	75.474663
208.790252	43.942418	75.479668
208.462333	48.760261	75.484673
207.518332	47.944123	75.489678
206.345030	50.275855	75.494682
205.913322	39.597834	75.499687
205.819166	49.333170	75.504692
204.471434	46.965028	75.509697
204.129549	40.874214	75.514702
203.123512	48.954054	75.519706
202.941522	31.357594	75.524711
202.661227	41.778609	75.529716
201.313791	45.180464	75.534721
201.080272	46.431976	75.539726
200.157516	48.055143	75.544730
199.970318	38.356850	75.549735
198.950809	43.450527	75.554740
198.019379	50.835658	75.559745
197.786158	44.241821	75.564750
196.688642	44.161364	75.569754
196.114334	33.655894	75.574759
195.141858	48.968559	75.579764
194.683321	49.382319	75.584769
194.667230	38.327384	75.589774
193.635630	46.994770	75.594778
192.774719	47.534180	75.599783
192.232576	52.480795	75.604788
191.650762	41.038235	75.609793
191.541107	40.956406	75.614798
190.423352	40.771946	75.619802
189.724461	40.159588	75.624807
189.338553	47.773138	75.629812
187.888264	43.112709	75.634817
187.315529	38.917921	75.639822
186.644275	53.212749	75.644826
186.654668	43.982845	75.649831
185.950227	39.471589	75.654836
184.417792	49.522961	75.659841
183.979931	53.210319	75.664846
183.629059	52.179780	75.669850
182.879465	38.376479	75.674855
182.700994	38.934823	75.679860
182.015820	44.743174	75.684865
181.324581	43.708554	75.689870
180.461031	38.494119	75.694874
179.695664	43.682902	75.699879
178.839611	45.631330	75.704884
178.070809	48.636594	75.709889
177.881723	39.378574	75.714894
177.396116	43.882515	75.719898
176.751916	44.403149	75.724903
176.085382	42.989279	75.729908
175.290753	43.201161	75.734913
174.210832	42.647979	75.739918
173.358671	44.922216	75.744922
172.968718	48.865286	75.749927
172.521716	41.785147	75.754932
172.183467	45.114426	75.759937
171.390179	47.030773	75.764942
170.501266	48.268510	75.769946
169.937592	39.092292	75.774951
169.028184	45.489905	75.779956
167.924135	48.261618	75.784961
167.412358	40.658801	75.789966
166.954444	47.673555	75.794970
166.498946	47.328325	75.799975
166.314278	46.205058	75.804980
165.225545	51.711907	75.809985
164.692052	44.953063	75.814990
163.837245	46.393522	75.819994
163.377496	47.570721	75.824999
162.582284	46.312988	75.830004
161.653955	48.146791	75.835009
161.290859	47.222283	75.840014
160.781240	53.658661	75.845018
160.048717	52.427203	75.850023
158.945468	41.763225	75.855028
158.381982	44.713681	75.860033
158.088088	45.038118	75.865038
157.462647	46.880399	75.870042
156.314621	38.713560	75.875047
155.674972	43.593723	75.880052
155.088632	51.587739	75.885057
155.257666	53.632931	75.890062
153.825006	51.191626	75.895066
153.147288	47.158663	75.900071
152.856881	48.384558	75.905076
151.991861	44.442961	75.910081
151.663042	40.963071	75.915086
150.513017	53.170673	75.920090
150.094794	47.005307	75.925095
149.625934	53.424150	75.930100
148.112410	51.481441	75.935105
148.017270	41.796862	75.940110
147.169244	51.625589	75.945114
146.729908	50.330042	75.950119
146.289044	47.651758	75.955124
145.223821	41.217399	75.960129
144.633282	38.372172	75.965134
144.083148	44.619467	75.970138
143.678871	44.490001	75.975143
142.506850	49.425092	75.980148
141.643521	56.589650	75.985153
141.348651	46.113751	75.990158
140.832070	52.111274	75.995162
140.527791	47.260261	76.000167
139.480665	50.478647	76.005172
138.628756	52.703971	76.010177
138.203876	46.814058	76.015182
137.192718	57.231772	76.020186
136.527777	54.934569	76.025191
136.233328	37.671440	76.030196
135.491246	52.360763	76.035201
135.621060	41.023950	76.040206
134.289867	46.731895	76.045210
133.323668	59.372242	76.050215
133.053008	40.610373	76.055220
132.213360	50.220149	76.060225
131.576865	50.493562	76.065230
130.942707	50.930606	76.070234
130.100530	47.125722	76.075239
129.081387	51.233779	76.080244
128.410385	55.715253	76.085249
128.146804	44.740785	76.090254
127.572511	46.995962	76.095258
127.128076	43.657513	76.100263
126.857361	42.262543	76.105268
125.571116	51.528796	76.110273
125.269407	41.604349	76.115278
123.879377	44.120485	76.120282
123.062545	52.543918	76.125287
122.574884	35.794150	76.130292
121.838707	50.282260	76.135297
121.770509	44.203013	76.140302
121.141910	58.486321	76.145306
120.410899	52.824996	76.150311
119.871686	57.473115	76.155316
118.650262	41.384391	76.160321
118.656098	46.454947	76.165326
117.456081	44.810773	76.170330
116.698235	42.843781	76.175335
116.344167	33.358195	76.180340
115.487917	59.648380	76.185345
115.445031	49.750466	76.190350
114.198337	54.747940	76.195354
113.496220	44.827417	76.200359
113.178614	46.699469	76.205364
112.486161	51.741028	76.210369
111.733722	39.158768	76.215374
110.937865	45.508329	76.220378
110.264229	51.652325	76.225383
110.078534	47.271261	76.230388
108.782163	52.391775	76.235393
108.385748	38.046492	76.240398
107.747011	52.985844	76.245402
107.131436	41.468274	76.250407
106.630938	49.191566	76.255412
105.409732	57.619565	76.260417
104.934389	44.501110	76.265422
104.200009	46.546854	76.270426
103.938876	51.667868	76.275431
103.159975	52.124846	76.280436
102.072769	51.159699	76.285441
101.919724	45.415680	76.290446
101.432265	56.839561	76.295450
100.616187	50.762880	76.300455
99.593539	45.723656	76.305460
98.966669	45.211802	76.310465
98.933938	48.296829	76.315470
97.644522	41.809936	76.320474
96.696650	56.672433	76.325479
96.192538	48.969062	76.330484
95.430951	51.619964	76.335489
95.284014	52.662138	76.340494
94.955237	56.727927	76.345498
94.029659	45.237717	76.350503
93.579267	37.532095	76.355508
92.826323	56.701677	76.360513
91.681581	46.869093	76.365518
90.996017	46.571604	76.370522
90.831077	50.237529	76.375527
90.481390	36.685889	76.380532
89.136548	45.256605	76.385537
88.160122	39.361622	76.390542
87.865531	45.905641	76.395546
87.368318	51.225151	76.400551
86.692185	50.233881	76.405556
85.923935	50.733320	76.410561
85.414251	55.233233	76.415566
84.958021	46.553987	76.420570
83.781904	48.607104	76.425575
83.339492	52.288894	76.430580
82.552357	45.677754	76.435585
82.105877	44.432244	76.440590
81.225428	46.069207	76.445594
80.499785	44.936025	76.450599
80.090080	37.294880	76.455604
79.580425	51.647526	76.460609
78.340048	43.878652	76.465614
77.342002	44.971401	76.470618
77.028399	52.002577	76.475623
76.732869	39.047848	76.480628
76.177960	39.387112	76.485633
75.729867	45.550337	76.490638
74.895102	44.603292	76.495642
74.039419	49.469041	76.500647
73.781266	37.834563	76.505652
72.268308	57.290931	76.510657
71.870042	38.521050	76.515662
71.169886	46.925886	76.520666
70.899371	49.099513	76.525671
70.235429	40.858675	76.530676
69.056280	37.839258	76.535681
68.448310	44.657181	76.540686
68.033776	41.924253	76.545690
67.518630	42.476373	76.550695
67.247301	44.661169	76.555700
66.076541	46.229318	76.560705
65.466970	38.236854	76.565710
65.014651	50.855181	76.570714
64.175205	39.844838	76.575719
63.519009	38.407275	76.580724
62.743855	39.708908	76.585729
62.278085	35.741524	76.590734
61.269253	44.728594	76.595738
60.280078	39.967902	76.600743
60.160369	31.862627	76.605748
59.309733	40.318268	76.610753
59.195349	35.239871	76.615758
58.345791	34.675234	76.620762
57.245320	40.800577	76.625767
56.924821	38.629816	76.630772
56.148401	39.441225	76.635777
55.866203	39.639230	76.640782
54.825512	43.968367	76.645786
53.970436	46.877038	76.650791
53.533938	34.350077	76.655796
53.100839	49.955220	76.660801
52.418671	39.881734	76.665806
51.410651	34.192080	76.670810
50.853283	42.113678	76.675815
50.679026	40.250752	76.680820
49.415343	47.248949	76.685825
48.869691	36.198067	76.690830
48.226860	44.207413	76.695834
47.777831	39.603430	76.700839
46.975720	35.049453	76.705844
46.013997	40.622819	76.710849
45.735265	36.835342	76.715854
45.462158	39.315310	76.720858
44.108727	36.933979	76.725863
43.528770	38.453643	76.730868
42.538796	51.126183	76.735873
42.530417	43.217612	76.740878
41.821893	47.277736	76.745882
40.903004	49.630468	76.750887
40.459409	44.224532	76.755892
39.776489	41.551761	76.760897
39.647800	45.848989	76.765902
38.352480	47.943216	76.770906
37.260417	44.042607	76.775911
37.387129	37.271547	76.780916
36.545240	45.016177	76.785921
35.609121	35.325400	76.790926
34.853664	37.838146	76.795930
34.310323	50.491491	76.800935
34.039797	42.935390	76.805940
33.047601	40.594221	76.810945
32.497793	37.176407	76.815950
31.751808	45.082360	76.820954
31.208665	36.503730	76.825959
30.537156	31.402232	76.830964
29.409247	41.240926	76.835969
29.074586	40.911142	76.840974
28.308640	37.188759	76.845978
27.916489	42.633443	76.850983
27.222323	43.540551	76.855988
26.345131	50.647425	76.860993
25.768706	40.771548	76.865998
25.790273	41.715887	76.871002
24.250300	43.767140	76.876007
23.998869	35.654492	76.881012
23.011197	49.985610	76.886017
22.860891	38.999412	76.891022
21.719028	50.362089	76.896026
20.815314	44.720465	76.901031
20.335278	39.176846	76.906036
19.936683	45.794227	76.911041
19.438592	46.662178	76.916046
18.525587	50.191955	76.921050
17.488651	48.037699	76.926055
17.565654	43.851289	76.931060
16.748193	48.043911	76.936065
15.832760	45.422425	76.941070
14.922217	46.490204	76.946074
14.172825	49.848807	76.951079
14.077261	38.495914	76.956084
13.350894	43.941868	76.961089
12.402806	39.078451	76.966094
11.839238	43.085499	76.971098
11.410796	43.209066	76.976103
11.205257	43.229270	76.981108
9.670885	43.210692	76.986113
9.117783	33.840457	76.991118
8.960927	38.963762	76.996122
8.038362	49.693805	77.001127
7.585233	40.418006	77.006132
6.558045	45.803135	77.011137
6.124200	47.977589	77.016142
5.633896	49.448270	77.021147
4.152015	37.762995	77.026151
3.878709	39.440335	77.031156
3.093001	49.863124	77.036161