Fri Mar 05 20:20:03 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.025545	108.922492	0.000000
-0.543869	92.420733	0.005005
-1.020767	62.632689	0.010010
-3.012569	36.836317	0.015014
-6.890038	13.939578	0.020019
-11.804066	-6.334903	0.025024
-17.314384	9.980754	0.030029
-21.755316	0.188405	0.035034
-25.841222	8.187179	0.040038
-29.740022	-1.084516	0.045043
-33.079286	11.549620	0.050048
-37.389601	9.091287	0.055053
-40.583474	11.086314	0.060058
-44.239715	10.564203	0.065062
-47.657702	3.868235	0.070067
-51.383157	-4.781378	0.075072
-55.574189	9.951954	0.080077
-59.389682	-1.084956	0.085082
-63.055407	3.696127	0.090086
-66.813745	-0.032913	0.095091
-70.644531	2.741848	0.100096
-74.519939	9.270530	0.105101
-77.901761	-3.024545	0.110106
-81.530858	1.203524	0.115110
-85.718908	7.930336	0.120115
-89.305587	-2.543794	0.125120
-93.387736	10.289368	0.130125
-97.023330	6.536058	0.135130
-100.368981	0.626557	0.140134
-104.246936	1.248498	0.145139
-107.755566	-9.785246	0.150144
-112.213863	-4.685246	0.155149
-115.722213	-1.053551	0.160154
-119.552367	-10.637233	0.165158
-124.203832	10.821174	0.170163
-127.707911	3.538251	0.175168
-131.291505	3.651223	0.180173
-134.941457	2.306665	0.185178
-138.377052	7.371255	0.190182
-141.953045	6.248291	0.195187
-145.797924	1.665873	0.200192
-149.734824	11.164386	0.205197
-153.437579	4.460401	0.210202
-156.861939	7.995176	0.215206
-160.610265	1.735287	0.220211
-164.502397	8.050736	0.225216
-168.701942	1.709904	0.230221
-172.687378	0.887290	0.235226
-176.092373	5.360429	0.240230
-180.008407	7.983387	0.245235
-183.244782	4.529196	0.250240
-187.108783	1.214597	0.255245
-190.930357	7.596095	0.260250
-195.064798	7.213608	0.265254
-198.946503	7.875722	0.270259
-201.999675	-7.996052	0.275264
-205.831587	8.550439	0.280269
-209.754750	4.857393	0.285274
-213.573771	-0.247851	0.290278
-217.530869	9.698683	0.295283
-221.057394	-0.411105	0.300288
-225.127599	4.154079	0.305293
-228.357895	-1.913993	0.310298
-232.378947	7.221189	0.315302
-236.560136	7.082774	0.320307
-239.590892	2.837338	0.325312
-243.917582	8.312382	0.330317
-247.462716	-2.041972	0.335322
-251.102657	5.977441	0.340326
-255.142056	-1.532070	0.345331
-258.437681	1.512371	0.350336
-262.565693	6.887925	0.355341
-266.351322	-5.922712	0.360346
-270.213273	1.179699	0.365350
-274.254996	0.538124	0.370355
-277.287759	1.876969	0.375360
-281.233663	3.900892	0.380365
-285.104179	-2.403942	0.385370
-288.988470	0.042237	0.390374
-292.856425	-4.880024	0.395379
-296.165741	-12.849773	0.400384
-300.216085	4.466565	0.405389
-303.846520	3.975423	0.410394
-307.407755	-2.888095	0.415398
-311.339707	6.401718	0.420403
-314.900095	2.250394	0.425408
-319.237551	4.431504	0.430413
-322.880023	10.685264	0.435418
-326.480075	-1.713359	0.440422
-330.488681	2.927318	0.445427
-333.932774	-0.922426	0.450432
-337.587291	-5.293647	0.455437
-341.430824	0.411927	0.460442
-345.283768	-0.341667	0.465446
-349.606081	7.444639	0.470451
-353.114627	8.635617	0.475456
-356.471745	7.821800	0.480461
-360.205999	6.044776	0.485466
-363.943042	0.056226	0.490470
-367.969067	0.878847	0.495475
-371.635086	3.086883	0.500480
-375.395313	0.779452	0.505485
-379.292011	5.183147	0.510490
-382.915469	-9.938148	0.515494
-386.847131	7.245833	0.520499
-390.205485	-7.583474	0.525504
-394.133206	-0.952912	0.530509
-397.825139	4.780582	0.535514
-401.905392	5.827958	0.540518
-405.657030	0.418962	0.545523
-408.963861	-9.459102	0.550528
-413.138327	9.597658	0.555533
-416.673130	-7.027938	0.560538
-420.415562	-2.410698	0.565542
-424.496111	-2.304662	0.570547
-428.226623	-14.180810	0.575552
-432.097418	-4.897431	0.580557
-435.520812	-7.823094	0.585562
-439.038842	0.170808	0.590566
-443.201624	-4.393464	0.595571
-446.697151	-0.717616	0.600576
-450.706697	-2.594033	0.605581
-454.216609	4.766249	0.610586
-458.439049	-8.114641	0.615590
-462.468073	0.426095	0.620595
-465.673805	2.814648	0.625600
-469.459655	-3.224280	0.630605
-472.821819	-2.920662	0.635610
-476.722805	3.778300	0.640614
-480.915266	-3.096093	0.645619
-484.477348	-2.607567	0.650624
-488.378062	-4.384609	0.655629
-492.507918	4.911860	0.660634
-495.704208	-8.342584	0.665638
-499.842324	5.230261	0.670643
-503.173472	-7.140055	0.675648
-507.240432	10.652332	0.680653
-510.615761	5.378939	0.685658
-514.283522	5.234696	0.690662
-518.338438	-3.287409	0.695667
-522.375694	2.116657	0.700672
-525.693879	-16.751042	0.705677
-529.632629	-0.746846	0.710682
-533.227755	0.292648	0.715686
-537.646055	4.637988	0.720691
-541.021877	-6.055169	0.725696
-544.464836	5.363009	0.730701
-548.212305	-1.380497	0.735706
-552.057206	4.719853	0.740710
-556.525212	3.154968	0.745715
-559.923505	-3.415644	0.750720
-563.509259	0.637478	0.755725
-567.068408	3.781200	0.760730
-570.688998	-0.415304	0.765734
-574.709668	0.712732	0.770739
-578.355111	-2.300250	0.775744
-582.424897	3.697305	0.780749
-586.345541	-7.591552	0.785754
-589.789833	-0.924375	0.790758
-593.744925	-2.604247	0.795763
-597.357494	-8.017797	0.800768
-601.048069	9.262021	0.805773
-604.930717	2.570164	0.810778
-608.668760	-2.323438	0.815782
-612.615252	4.682622	0.820787
-616.096664	1.206684	0.825792
-619.882973	2.494468	0.830797
-623.851290	-8.411396	0.835802
-627.047867	-1.618170	0.840806
-630.920945	5.341498	0.845811
-634.786599	1.226826	0.850816
-638.793093	2.272282	0.855821
-642.739011	-0.012935	0.860826
-646.193332	-8.985577	0.865830
-650.006021	4.183854	0.870835
-653.726486	-0.859138	0.875840
-657.606945	6.232636	0.880845
-661.262050	3.002135	0.885850
-665.183988	-2.711953	0.890854
-669.231641	2.061669	0.895859
-672.441478	-6.130000	0.900864
-676.384972	1.720911	0.905869
-680.163444	8.507847	0.910874
-683.718013	4.652623	0.915878
-687.688671	-7.091676	0.920883
-691.326493	0.316182	0.925888
-695.311112	-8.301988	0.930893
-698.828051	1.305293	0.935898
-702.337613	-3.796553	0.940902
-706.375211	5.881330	0.945907
-710.388497	8.318838	0.950912
-714.373528	3.665146	0.955917
-717.763143	8.597035	0.960922
-721.617077	-3.217898	0.965926
-725.337952	4.058207	0.970931
-728.715629	-3.762790	0.975936
-732.590904	5.002963	0.980941
-736.545705	-2.763633	0.985946
-740.257858	-10.501191	0.990950
-744.256432	-1.810333	0.995955
-747.803266	-11.039260	1.000960
-751.353964	0.434255	1.005965
-755.262128	2.492344	1.010970
-759.161404	-1.388090	1.015974
-763.229980	-0.876540	1.020979
-766.466456	-3.131438	1.025984
-770.511621	0.222725	1.030989
-774.286694	2.351034	1.035994
-777.818417	4.546107	1.040998
-781.312311	3.451988	1.046003
-785.208315	-4.191458	1.051008
-789.014761	0.816615	1.056013
-793.032776	2.064441	1.061018
-796.661155	-4.018034	1.066022
-801.060069	5.362948	1.071027
-804.516864	2.886281	1.076032
-807.987611	6.998649	1.081037
-811.652111	10.984303	1.086042
-815.074012	3.815463	1.091046
-819.093703	3.939257	1.096051
-823.177027	-3.390333	1.101056
-827.015123	3.529356	1.106061
-830.688194	12.751786	1.111066
-833.951672	-4.777485	1.116070
-837.974175	1.723855	1.121075
-841.675289	-2.394695	1.126080
-845.630265	-3.594775	1.131085
-849.409494	-6.521286	1.136090
-853.264866	-12.628877	1.141094
-857.150302	-9.727451	1.146099
-860.548161	-7.427505	1.151104
-864.624589	0.044419	1.156109
-868.359896	-8.619607	1.161114
-871.936091	-11.002965	1.166118
-875.941547	-0.385378	1.171123
-879.090605	-7.205083	1.176128
-882.927138	-3.797356	1.181133
-887.234949	-5.628490	1.186138
-890.738727	-11.711809	1.191142
-894.637428	-1.675799	1.196147
-898.051538	-5.061146	1.201152
-902.155509	-1.768320	1.206157
-905.937184	-0.914475	1.211162
-909.585068	-6.864341	1.216166
-913.426839	-3.925650	1.221171
-917.113428	-4.733293	1.226176
-920.560823	-0.816884	1.231181
-924.469962	4.387591	1.236186
-928.376269	-1.856808	1.241190
-932.428872	-2.758862	1.246195
-935.653003	-11.146551	1.251200
-939.874711	-2.541123	1.256205
-943.365278	-3.222378	1.261210
-946.765857	-5.572204	1.266214
-951.034963	0.801603	1.271219
-954.698928	-9.409604	1.276224
-958.342932	-6.901427	1.281229
-962.696179	11.371088	1.286234
-966.100434	-0.527940	1.291238
-969.904099	3.491245	1.296243
-973.532095	-4.150578	1.301248
-977.024693	-1.584585	1.306253
-981.211338	-6.136180	1.311258
-984.708099	-6.724921	1.316262
-988.700362	-5.873533	1.321267
-992.445556	-9.961132	1.326272
-996.101657	-8.278843	1.331277
-999.875138	-3.408174	1.336282
-1003.247361	-2.433580	1.341286
-1007.538141	7.851394	1.346291
-1011.270376	6.969200	1.351296
-1014.609170	0.531683	1.356301
-1018.615336	-0.581069	1.361306
-1022.346800	-7.028305	1.366310
-1026.355895	2.776416	1.371315
-1030.007288	-12.203691	1.376320
-1033.719457	2.728988	1.381325
-1037.352111	-3.658337	1.386330
-1041.157789	-14.151073	1.391334
-1045.412313	-4.321261	1.396339
-1048.991326	6.285165	1.401344
-1052.669777	7.625772	1.406349
-1056.279200	1.073915	1.411354
-1059.673971	-6.740687	1.416358
-1063.525034	-3.663076	1.421363
-1067.332951	-7.133406	1.426368
-1071.188730	-7.555780	1.431373
-1075.456402	2.941649	1.436378
-1079.084797	-3.205021	1.441382
-1082.521843	-3.464130	1.446387
-1086.071763	-17.034836	1.451392
-1089.874457	-11.514398	1.456397
-1093.975060	-11.325149	1.461402
-1097.984689	-2.187265	1.466406
-1101.821603	-1.690111	1.471411
-1105.295934	-5.600088	1.476416
-1108.697624	-7.053808	1.481421
-1112.326313	-5.210149	1.486426
-1115.899900	-8.528655	1.491430
-1120.478212	2.244047	1.496435
-1124.110444	-1.027221	1.501440
-1127.752268	-10.368066	1.506445
-1131.792113	-5.128155	1.511450
-1135.320918	-9.521366	1.516454
-1138.911744	-2.834713	1.521459
-1142.772268	-7.433455	1.526464
-1146.572008	-16.029926	1.531469
-1150.338125	-2.133948	1.536474
-1153.805307	-6.316223	1.541478
-1158.028794	-3.623561	1.546483
-1161.780725	-7.045922	1.551488
-1165.289302	1.909406	1.556493
-1168.936758	4.115693	1.561498
-1172.320004	-8.048130	1.566502
-1176.556554	3.163566	1.571507
-1180.554888	-2.086405	1.576512
-1184.334983	-8.213358	1.581517
-1187.743883	-2.855120	1.586522
-1191.455380	-7.614816	1.591526
-1195.656065	2.711256	1.596531
-1199.102422	-6.731711	1.601536
-1203.167430	-5.084591	1.606541
-1206.797193	-3.623804	1.611546
-1210.178919	-1.907820	1.616550
-1214.320212	8.462398	1.621555
-1218.122977	-5.720477	1.626560
-1222.047753	-8.157892	1.631565
-1225.646465	-1.668540	1.636570
-1228.779983	-7.950927	1.641574
-1232.854382	0.828546	1.646579
-1236.949908	-9.432965	1.651584
-1240.676671	-12.056572	1.656589
-1244.463959	2.760699	1.661594
-1248.057527	-2.457737	1.666598
-1251.998631	0.511591	1.671603
-1255.388394	-4.504489	1.676608
-1259.297721	-0.534164	1.681613
-1263.086415	-1.042648	1.686618
-1266.811573	-6.148531	1.691622
-1270.980040	5.505005	1.696627
-1274.466834	-6.645237	1.701632
-1278.274587	0.457955	1.706637
-1281.746308	10.908774	1.711642
-1285.493749	-2.292537	1.716646
-1289.439763	2.568357	1.721651
-1293.149345	-12.761514	1.726656
-1296.937223	-10.524670	1.731661
-1300.673996	-8.712304	1.736666
-1304.561215	-9.283795	1.741670
-1308.385550	-6.169065	1.746675
-1311.861408	-7.708380	1.751680
-1316.014855	-0.705910	1.756685
-1319.529882	-7.209368	1.761690
-1323.044752	-8.923766	1.766694
-1327.051849	-4.841490	1.771699
-1330.983405	-1.625983	1.776704
-1334.706805	-10.010430	1.781709
-1338.720192	-6.808620	1.786714
-1341.876264	-23.427025	1.791718
-1346.185368	-5.846913	1.796723
-1349.122181	-5.715784	1.801728
-1353.195751	-4.502260	1.806733
-1357.848062	-2.713546	1.811738
-1360.633585	-11.971890	1.816742
-1364.676564	-4.126029	1.821747
-1368.154370	-0.357067	1.826752
-1372.025739	-3.501345	1.831757
-1376.054086	-8.739851	1.836762
-1379.582358	-15.786699	1.841766
-1383.537372	-6.229753	1.846771
-1387.126022	-12.885312	1.851776
-1391.200205	-12.532615	1.856781
-1394.980181	-8.048205	1.861786
-1398.229006	-8.724899	1.866790
-1402.305431	-4.427974	1.871795
-1405.839907	-2.176332	1.876800
-1409.838973	-8.703069	1.881805
-1413.739294	-3.805133	1.886810
-1417.323778	-15.461687	1.891814
-1421.189450	-9.099610	1.896819
-1424.775803	0.675915	1.901824
-1428.363769	2.083048	1.906829
-1432.722893	-4.841725	1.911834
-1436.084960	-9.111354	1.916838
-1440.337024	4.897560	1.921843
-1443.895670	-3.333317	1.926848
-1447.482682	-4.977626	1.931853
-1450.848732	-3.828337	1.936858
-1454.818174	-6.773847	1.941862
-1458.869495	-10.929917	1.946867
-1462.589934	-3.430423	1.951872
-1466.161767	-6.554696	1.956877
-1470.535145	2.804469	1.961882
-1473.550245	-4.357525	1.966886
-1477.310203	-8.175455	1.971891
-1481.012654	-2.742985	1.976896
-1484.753091	-5.352964	1.981901
-1489.210292	-4.397878	1.986906
-1492.599331	-5.684323	1.991910
-1496.308107	-2.160451	1.996915
-1500.381400	-12.142076	2.006912
-1501.166943	-6.344699	2.016909
-1498.759282	-6.916523	2.026906
-1495.906798	-7.133270	2.036902
-1493.515174	-7.637783	2.046899
-1491.479774	-1.182178	2.056896
-1489.924685	-8.288425	2.066893
-1488.352465	-5.960167	2.076890
-1486.141244	-8.485230	2.086886
-1484.388072	-4.673335	2.096883
-1482.075539	-11.828242	2.106880
-1480.219816	-4.784915	2.116877
-1478.430431	-6.937685	2.126874
-1476.670173	-8.820530	2.136870
-1474.922155	-4.314653	2.146867
-1472.724584	-5.310695	2.156864
-1471.057868	-6.805930	2.166861
-1469.099620	-2.412659	2.176858
-1467.214259	-7.054969	2.186854
-1465.323570	-16.068598	2.196851
-1463.313369	-13.422043	2.206848
-1461.354148	-9.101555	2.216845
-1459.550122	-7.416704	2.226842
-1457.819719	-5.129544	2.236838
-1455.756408	-5.931968	2.246835
-1453.917443	-9.494746	2.256832
-1451.932668	0.240541	2.266829
-1449.939729	-2.344271	2.276826
-1448.468566	-2.263986	2.286822
-1446.763385	-3.002740	2.296819
-1444.450237	-5.158827	2.306816
-1442.457875	-6.690395	2.316813
-1440.658153	-5.390098	2.326810
-1438.817493	-9.966808	2.336806
-1437.001870	-13.162681	2.346803
-1435.289168	-7.983233	2.356800
-1432.984990	-10.865757	2.366797
-1431.352999	-4.083401	2.376794
-1429.397344	-4.578041	2.386790
-1427.651895	-12.257879	2.396787
-1425.933809	-6.501398	2.406784
-1423.854870	-10.667832	2.416781
-1421.770703	-5.622059	2.426778
-1420.176764	-6.843503	2.436774
-1418.148281	-3.958256	2.446771
-1416.370077	-9.788092	2.456768
-1414.458790	-2.488342	2.466765
-1412.317459	-0.852721	2.476762
-1410.760250	-1.144605	2.486758
-1408.745845	-5.981214	2.496755
-1406.985804	-7.273453	2.506752
-1404.935633	-6.420590	2.516749
-1403.079234	-4.766184	2.526746
-1401.355646	-9.275175	2.536742
-1399.588623	-5.125960	2.546739
-1397.528306	-3.600512	2.556736
-1395.782760	-7.096185	2.566733
-1393.701735	-6.344566	2.576730
-1391.722716	-9.624987	2.586726
-1389.966421	-3.658279	2.596723
-1387.996694	-0.092553	2.606720
-1386.242820	-2.582196	2.616717
-1384.386065	-5.929878	2.626714
-1382.494541	-5.779482	2.636710
-1380.839684	-9.456412	2.646707
-1378.823403	-10.306501	2.656704
-1376.913524	-9.769043	2.666701
-1374.883329	-12.078707	2.676698
-1373.090190	-7.879969	2.686694
-1371.198814	-7.246388	2.696691
-1369.032004	-6.481638	2.706688
-1367.542588	-8.208938	2.716685
-1365.610745	-4.075029	2.726682
-1363.718207	-7.474213	2.736678
-1361.850814	-9.347281	2.746675
-1359.895492	-11.360738	2.756672
-1358.067214	-10.031790	2.766669
-1356.191652	-5.847812	2.776666
-1354.508893	-7.332900	2.786662
-1352.779650	-7.195974	2.796659
-1350.219321	-10.155739	2.806656
-1348.363186	-14.201179	2.816653
-1346.731189	-6.976659	2.826650
-1345.070489	-10.248715	2.836646
-1343.062738	-7.072717	2.846643
-1341.162430	-3.418470	2.856640
-1339.353217	-5.752728	2.866637
-1337.403656	-11.936776	2.876634
-1335.471870	-9.454392	2.886630
-1333.855514	-10.020952	2.896627
-1332.006138	-10.784284	2.906624
-1329.623222	-10.451980	2.916621
-1328.115152	-1.889200	2.926618
-1326.275326	-0.263655	2.936614
-1324.191311	-2.299263	2.946611
-1322.177235	1.567315	2.956608
-1320.371806	-5.608903	2.966605
-1318.849101	-3.179442	2.976602
-1316.733253	-1.977016	2.986598
-1314.468684	-7.491478	2.996595
-1312.939058	-3.228405	3.006592
-1311.396093	-6.937904	3.016589
-1309.426998	-1.767814	3.026586
-1307.443730	1.511610	3.036582
-1305.409705	-0.020196	3.046579
-1303.811778	-6.269514	3.056576
-1301.750427	-10.038296	3.066573
-1299.750340	-5.192103	3.076570
-1297.903769	-4.611289	3.086566
-1296.091320	2.525973	3.096563
-1294.159773	-0.997821	3.106560
-1292.236018	-6.104033	3.116557
-1290.583983	-3.709463	3.126554
-1288.589415	-1.224455	3.136550
-1286.680918	-2.625628	3.146547
-1285.004793	-1.202794	3.156544
-1283.021046	-1.730227	3.166541
-1281.283945	3.867018	3.176538
-1279.346593	4.104900	3.186534
-1277.237791	-3.776679	3.196531
-1275.412800	1.907555	3.206528
-1273.754054	-1.867821	3.216525
-1271.683152	-4.706539	3.226522
-1269.731560	3.494781	3.236518
-1267.850630	-3.342962	3.246515
-1265.906318	3.762169	3.256512
-1264.147509	-4.851272	3.266509
-1262.530797	-0.906833	3.276506
-1260.546432	0.608791	3.286502
-1258.641884	2.168770	3.296499
-1256.629669	4.335197	3.306496
-1254.730986	1.432477	3.316493
-1252.833809	-0.364747	3.326490
-1251.165967	5.737813	3.336486
-1249.184623	10.879161	3.346483
-1247.237071	7.403367	3.356480
-1245.458924	5.310989	3.366477
-1243.408958	-1.754313	3.376474
-1241.819766	-0.914371	3.386470
-1239.999791	2.151249	3.396467
-1237.646107	-4.348449	3.406464
-1236.121985	-0.108123	3.416461
-1234.212281	-0.914189	3.426458
-1232.662443	-2.584760	3.436454
-1230.618559	-5.010175	3.446451
-1228.415097	-4.795889	3.456448
-1226.605835	-4.755358	3.466445
-1224.724642	-1.247949	3.476442
-1222.898091	-0.439661	3.486438
-1221.021741	-1.729848	3.496435
-1219.099648	2.255754	3.506432
-1217.380668	6.092284	3.516429
-1215.563911	-0.095685	3.526426
-1213.179725	4.089132	3.536422
-1211.623565	3.006504	3.546419
-1209.861726	3.163585	3.556416
-1207.960006	1.610403	3.566413
-1205.924084	6.965685	3.576410
-1204.327609	3.595052	3.586406
-1202.284581	1.938738	3.596403
-1200.287586	1.638200	3.606400
-1198.383050	3.370335	3.616397
-1196.904094	5.876355	3.626394
-1194.707783	4.370780	3.636390
-1192.835186	4.511729	3.646387
-1190.724598	-2.672177	3.656384
-1189.058664	7.564384	3.666381
-1187.481344	7.872585	3.676378
-1185.548490	8.547051	3.686374
-1183.388118	3.122009	3.696371
-1181.669756	3.742380	3.706368
-1179.666306	2.711359	3.716365
-1177.780493	5.166501	3.726362
-1176.011812	5.448827	3.736358
-1174.175972	3.026748	3.746355
-1172.354722	4.413813	3.756352
-1170.157781	7.487069	3.766349
-1168.710207	11.588116	3.776346
-1166.712050	5.439049	3.786342
-1164.722068	0.721808	3.796339
-1162.790978	3.373400	3.806336
-1160.949136	4.371920	3.816333
-1159.086793	4.912428	3.826330
-1157.469336	6.098430	3.836326
-1155.632379	-1.278507	3.846323
-1153.342532	5.735128	3.856320
-1151.375591	5.679439	3.866317
-1149.976027	7.045570	3.876314
-1147.744344	4.528599	3.886310
-1145.674540	2.808050	3.896307
-1144.045769	0.561228	3.906304
-1142.335460	5.630773	3.916301
-1140.349432	1.368916	3.926298
-1138.498256	5.836458	3.936294
-1136.508256	6.651821	3.946291
-1134.760259	1.239114	3.956288
-1133.236050	4.783191	3.966285
-1131.202902	5.155870	3.976282
-1128.799054	-2.145956	3.986278
-1127.044832	7.626536	3.996275
-1125.357151	0.860865	4.006272
-1123.427962	-2.480838	4.016269
-1121.513574	-0.473902	4.026266
-1119.843514	1.226338	4.036262
-1117.792974	-2.414247	4.046259
-1115.863431	-0.005523	4.056256
-1114.055502	-2.847824	4.066253
-1112.038547	1.733743	4.076250
-1110.338989	6.626614	4.086246
-1108.266130	-4.915363	4.096243
-1106.578109	-3.257461	4.106240
-1105.009557	3.326884	4.116237
-1102.766328	0.411795	4.126234
-1101.056756	-2.342130	4.136230
-1098.996467	0.497267	4.146227
-1097.083905	-5.178578	4.156224
-1095.126068	-1.129114	4.166221
-1093.576291	9.653475	4.176218
-1091.461278	-2.962595	4.186214
-1089.727092	4.924728	4.196211
-1087.709567	0.667349	4.206208
-1085.946218	3.588997	4.216205
-1083.991415	0.263752	4.226202
-1082.168508	2.324830	4.236198
-1080.650245	2.377289	4.246195
-1078.512835	0.189672	4.256192
-1076.515779	3.970777	4.266189
-1074.418512	2.766945	4.276186
-1072.735394	1.523575	4.286182
-1070.922288	-0.894789	4.296179
-1069.139775	-0.965117	4.306176
-1067.214870	-3.865568	4.316173
-1065.196864	2.697437	4.326170
-1063.379168	2.051489	4.336166
-1061.424632	0.878394	4.346163
-1059.628844	0.471215	4.356160
-1057.553711	2.637229	4.366157
-1055.964698	1.162610	4.376154
-1054.070660	2.504969	4.386150
-1052.468785	1.184609	4.396147
-1050.109687	-2.137382	4.406144
-1048.174863	-1.278381	4.416141
-1046.438567	-3.033918	4.426138
-1044.842212	1.706564	4.436134
-1042.651613	-0.622160	4.446131
-1040.927706	-4.295697	4.456128
-1039.073008	-2.967560	4.466125
-1037.184553	-3.798488	4.476122
-1035.396584	0.818196	4.486118
-1033.191643	-0.968081	4.496115
-1031.398974	-7.058906	4.506112
-1029.750434	-1.556241	4.516109
-1027.993768	-1.976085	4.526106
-1025.892691	-2.847328	4.536102
-1024.049997	-5.030390	4.546099
-1022.555945	-6.407693	4.556096
-1020.046132	0.182481	4.566093
-1018.158758	-1.030362	4.576090
-1016.539902	5.648635	4.586086
-1014.735449	5.311156	4.596083
-1012.574277	-1.830168	4.606080
-1010.784104	1.193037	4.616077
-1008.936255	-3.573977	4.626074
-1007.223363	0.339478	4.636070
-1005.099045	0.269795	4.646067
-1003.233709	-6.386840	4.656064
-1001.667937	-3.450896	4.666061
-999.712100	-0.266284	4.676058
-997.640597	-7.034834	4.686054
-995.941303	0.573936	4.696051
-993.908097	-6.835850	4.706048
-992.223589	-3.678891	4.716045
-990.422525	-0.810569	4.726042
-988.262435	2.879806	4.736038
-986.015611	-2.370996	4.746035
-984.858267	2.711317	4.756032
-982.820364	1.918110	4.766029
-980.890465	0.767969	4.776026
-978.844481	4.967651	4.786022
-977.206207	6.243608	4.796019
-975.110918	-1.733458	4.806016
-973.452220	0.502387	4.816013
-971.454436	-4.118052	4.826010
-969.651530	4.974161	4.836006
-967.592718	-1.419708	4.846003
-965.909930	1.195972	4.856000
-964.043135	-8.031376	4.865997
-961.765560	-6.579751	4.875994
-960.343535	-0.576601	4.885990
-958.458187	-3.506955	4.895987
-956.315512	-6.898454	4.905984
-954.304051	-8.571612	4.915981
-952.551543	-3.570248	4.925978
-951.234740	-4.521270	4.935974
-949.004103	-2.629497	4.945971
-947.000244	-12.204010	4.955968
-945.304670	-12.631392	4.965965
-943.131173	-10.956265	4.975962
-941.462281	-11.290958	4.985958
-939.569409	-15.403542	4.995955
-937.685771	-15.279943	5.005952
-935.575786	-11.478880	5.015949
-933.880211	-9.228378	5.025946
-932.295573	-10.318533	5.035942
-930.327044	-11.283758	5.045939
-928.094232	-10.911250	5.055936
-926.579085	-9.484518	5.065933
-924.727566	-8.173149	5.075930
-922.701358	-11.841256	5.085926
-920.699278	-10.749747	5.095923
-919.054860	-12.755761	5.105920
-917.092593	-6.374761	5.115917
-915.167424	-7.430934	5.125914
-913.272526	-12.800657	5.135910
-911.414621	-11.075039	5.145907
-909.381255	-5.671709	5.155904
-907.508320	-5.808477	5.165901
-905.733088	-10.990115	5.175898
-904.235278	-2.494852	5.185894
-901.937356	-9.433735	5.195891
-900.198621	-11.877973	5.205888
-898.366846	-5.799773	5.215885
-896.465603	-6.931052	5.225882
-894.232616	-2.254356	5.235878
-892.656436	2.862094	5.245875
-890.862632	-6.871426	5.255872
-888.966980	0.636563	5.265869
-886.958136	-4.047156	5.275866
-884.694604	-7.418442	5.285862
-883.474951	-2.238669	5.295859
-881.477888	-8.545225	5.305856
-879.591740	-12.157746	5.315853
-877.643906	-9.945955	5.325850
-875.608583	-7.921832	5.335846
-874.040365	-2.646204	5.345843
-872.321746	-4.670367	5.355840
-870.116244	0.626534	5.365837
-868.284154	-10.275188	5.375834
-866.382309	-5.518681	5.385830
-864.443576	-2.692794	5.395827
-862.509289	-9.016141	5.405824
-860.771958	-1.171766	5.415821
-859.263292	-4.649714	5.425818
-857.031952	-1.398498	5.435814
-854.995153	-3.565095	5.445811
-853.024339	-9.872168	5.455808
-851.598713	-6.266350	5.465805
-849.729001	4.659487	5.475802
-847.538338	-1.286419	5.485798
-845.518995	1.161863	5.495795
-844.059603	0.304945	5.505792
-842.043806	-0.369344	5.515789
-840.298838	3.678061	5.525786
-838.014639	-2.800682	5.535782
-836.375641	2.558396	5.545779
-834.450303	3.079621	5.555776
-832.536648	0.507994	5.565773
-830.433912	3.206641	5.575770
-828.782047	3.926324	5.585766
-826.972994	-0.599093	5.595763
-825.101967	0.298714	5.605760
-823.341189	4.029396	5.615757
-821.553279	1.010513	5.625754
-819.721380	4.925617	5.635750
-817.615900	1.333342	5.645747
-815.684079	-3.865372	5.655744
-813.805102	-3.733034	5.665741
-811.599645	-0.521845	5.675738
-810.067425	0.412765	5.685734
-808.261637	-2.446336	5.695731
-806.418240	-7.083015	5.705728
-804.506713	-2.121161	5.715725
-802.663456	-4.013619	5.725722
-800.565596	3.136866	5.735718
-798.864203	1.726557	5.745715
-796.913097	-1.616814	5.755712
-794.980226	-4.260956	5.765709
-793.419399	5.122737	5.775706
-791.563252	1.106130	5.785702
-789.436712	-0.594759	5.795699
-787.632854	-3.769323	5.805696
-785.436518	-4.450317	5.815693
-783.744488	4.950306	5.825690
-782.014175	9.104311	5.835686
-780.307411	3.606858	5.845683
-778.072096	-1.992442	5.855680
-776.049359	1.871668	5.865677
-774.515563	-2.620767	5.875674
-772.623739	2.255845	5.885670
-770.756488	1.488518	5.895667
-768.718893	0.182388	5.905664
-766.848207	1.651873	5.915661
-765.180146	-1.311497	5.925658
-763.336167	7.591176	5.935654
-761.446479	-3.668633	5.945651
-759.313521	1.602079	5.955648
-757.589053	2.845469	5.965645
-755.891090	6.265720	5.975642
-753.783079	1.643625	5.985638
-751.859129	1.230407	5.995635
-749.941118	2.501290	6.005632
-748.027873	-2.454406	6.015629
-746.271903	1.573946	6.025626
-744.455892	0.522725	6.035622
-742.338348	3.817505	6.045619
-740.735324	-1.930180	6.055616
-739.018500	2.685484	6.065613
-737.023736	3.252535	6.075610
-734.940153	-5.597200	6.085606
-733.016631	2.424367	6.095603
-731.144439	-6.189476	6.105600
-729.584973	-0.928133	6.115597
-727.516499	-2.649687	6.125594
-725.701456	4.298176	6.135590
-724.081293	-0.118033	6.145587
-721.768840	-3.354883	6.155584
-719.827105	-3.003553	6.165581
-718.311094	-1.619452	6.175578
-716.225895	-1.418940	6.185574
-714.554177	-2.800761	6.195571
-712.464788	2.183276	6.205568
-710.783773	1.510495	6.215565
-708.808808	-1.615568	6.225562
-706.848669	6.723856	6.235558
-704.955155	6.865012	6.245555
-703.119422	2.575417	6.255552
-701.249743	2.104597	6.265549
-699.396376	4.304797	6.275546
-697.579590	0.622970	6.285542
-695.490195	-1.348215	6.295539
-693.864100	0.545677	6.305536
-691.898087	-3.351044	6.315533
-690.016171	1.195645	6.325530
-688.228336	2.312119	6.335526
-686.227619	3.636154	6.345523
-684.320655	-5.101634	6.355520
-682.464830	-1.349715	6.365517
-680.747736	-0.877192	6.375514
-678.829936	1.085360	6.385510
-676.698448	-5.300940	6.395507
-674.841201	-7.220800	6.405504
-673.074163	-2.499426	6.415501
-671.311256	-1.301588	6.425498
-669.458733	-0.853855	6.435494
-667.421672	-2.614549	6.445491
-665.743747	-0.173131	6.455488
-663.190343	-8.545251	6.465485
-662.297610	-6.807311	6.475482
-660.262898	-3.611325	6.485478
-658.034045	-4.870553	6.495475
-656.072891	-4.263326	6.505472
-654.386337	-4.854848	6.515469
-652.751110	-1.288708	6.525466
-650.570969	3.947729	6.535462
-648.643112	-1.284963	6.545459
-646.890638	-3.415428	6.555456
-644.820389	-3.370359	6.565453
-642.916831	0.110283	6.575450
-641.138199	-2.254883	6.585446
-639.321701	-7.946614	6.595443
-637.442017	-1.313743	6.605440
-635.648050	-2.250834	6.615437
-633.842044	0.705404	6.625434
-632.230611	0.208006	6.635430
-629.833049	-1.829729	6.645427
-627.869157	-4.725010	6.655424
-626.463653	-4.914767	6.665421
-624.214509	-0.436170	6.675418
-622.368669	-3.576270	6.685414
-620.694596	-4.235247	6.695411
-618.802482	-6.204845	6.705408
-616.926846	-1.582882	6.715405
-614.859970	-3.068822	6.725402
-612.919414	0.270145	6.735398
-611.007293	-2.375274	6.745395
-609.398087	-6.435975	6.755392
-607.563745	-1.658986	6.765389
-605.820384	2.264123	6.775386
-603.857965	-0.305643	6.785382
-601.826885	-7.405310	6.795379
-599.786553	2.220868	6.805376
-597.951079	1.806120	6.815373
-596.085451	7.313911	6.825370
-594.430823	1.019649	6.835366
-592.463708	6.331230	6.845363
-590.549791	1.419755	6.855360
-588.752990	-2.828799	6.865357
-586.860000	4.401992	6.875354
-584.949928	4.213756	6.885350
-583.200613	0.804896	6.895347
-581.188195	-2.093365	6.905344
-579.229259	-6.190970	6.915341
-577.393546	-2.844698	6.925338
-575.602618	-2.832314	6.935334
-573.825593	2.317018	6.945331
-571.923000	5.153666	6.955328
-569.838987	-2.792854	6.965325
-567.867227	2.186426	6.975322
-566.188997	4.888395	6.985318
-564.399590	1.297880	6.995315
-562.472286	-1.163611	7.005312
-560.366642	-2.350962	7.015309
-558.689505	-3.986173	7.025306
-556.692472	2.260130	7.035302
-554.976875	-2.303848	7.045299
-553.209121	-4.790371	7.055296
-551.082479	-3.172126	7.065293
-549.393200	0.314403	7.075290
-547.280163	1.759562	7.085286
-545.554846	-1.375438	7.095283
-543.836427	-3.850916	7.105280
-541.627473	-11.244211	7.115277
-540.007046	-3.982476	7.125274
-537.920079	-9.489971	7.135270
-536.279067	-6.320986	7.145267
-534.121199	-4.912977	7.155264
-532.429564	-8.347323	7.165261
-530.662293	-2.267982	7.175258
-528.672773	-3.642018	7.185254
-526.712183	-4.136697	7.195251
-524.826749	-3.743055	7.205248
-523.013754	2.016361	7.215245
-521.240003	0.927847	7.225242
-519.129807	-1.231245	7.235238
-517.366381	-2.567580	7.245235
-515.636332	-3.671214	7.255232
-513.697771	1.248680	7.265229
-511.768978	3.809615	7.275226
-509.981756	5.889480	7.285222
-507.930931	-5.566421	7.295219
-506.240269	2.816227	7.305216
-504.043620	1.514917	7.315213
-502.393443	2.501941	7.325210
-500.548505	0.887337	7.335206
-498.686763	2.115309	7.345203
-496.692986	-2.512008	7.355200
-494.780807	-0.202617	7.365197
-493.082623	-1.729039	7.375194
-491.097090	-4.796616	7.385190
-489.267541	-3.745074	7.395187
-487.537064	-6.162438	7.405184
-485.373203	5.822014	7.415181
-483.401244	2.606611	7.425178
-481.748622	-3.401469	7.435174
-479.853156	4.899545	7.445171
-478.171710	3.217911	7.455168
-475.839669	-0.943942	7.465165
-474.471375	1.194963	7.475162
-472.460432	-3.071919	7.485158
-470.375940	-1.964763	7.495155
-468.467870	-0.219957	7.505152
-466.653462	2.128758	7.515149
-465.112676	-1.275138	7.525146
-462.822590	0.713400	7.535142
-461.143194	-2.447366	7.545139
-459.049279	-5.510121	7.555136
-457.167511	-2.998474	7.565133
-455.587226	2.757109	7.575130
-453.698920	2.814033	7.585126
-451.580783	-4.807843	7.595123
-449.958307	3.506794	7.605120
-448.011155	1.808010	7.615117
-446.052677	5.118996	7.625114
-444.340714	3.344090	7.635110
-442.304848	5.044827	7.645107
-440.408379	1.629934	7.655104
-438.594945	-1.332750	7.665101
-436.620316	-0.148019	7.675098
-434.787970	-5.867401	7.685094
-432.963450	-0.918173	7.695091
-431.033281	1.366293	7.705088
-429.211983	0.210254	7.715085
-427.290802	5.131421	7.725082
-425.605233	6.832848	7.735078
-423.502446	-0.203925	7.745075
-421.832842	-3.748364	7.755072
-419.936479	0.823087	7.765069
-418.092140	3.108639	7.775066
-416.049951	4.454704	7.785062
-414.039417	-3.982065	7.795059
-412.148014	5.818078	7.805056
-410.288383	4.772774	7.815053
-408.616360	5.197429	7.825050
-406.641078	2.387345	7.835046
-404.864070	2.447870	7.845043
-402.936562	8.162259	7.855040
-401.059003	3.517257	7.865037
-399.318903	-0.646320	7.875034
-396.968229	7.211029	7.885030
-395.262325	2.059757	7.895027
-393.539342	-3.108450	7.905024
-392.076600	1.123317	7.915021
-390.000184	-3.269218	7.925018
-388.052646	-4.203804	7.935014
-386.023549	-8.140357	7.945011
-383.892396	-0.620578	7.955008
-382.052414	0.424645	7.965005
-380.732473	-1.402884	7.975002
-378.653843	-0.269447	7.984998
-376.647598	1.120286	7.994995
-374.808601	2.582514	8.004992
-372.726557	1.144884	8.014989
-370.883662	0.474915	8.024986
-369.066593	2.071701	8.034982
-367.240320	-5.317190	8.044979
-365.681433	2.524506	8.054976
-363.625391	3.800510	8.064973
-361.878223	-0.479433	8.074970
-359.846478	4.487297	8.084966
-357.616394	-0.695537	8.094963
-355.751879	-7.968946	8.104960
-354.109579	-0.822666	8.114957
-352.430719	5.089360	8.124954
-350.564014	6.911921	8.134950
-348.569849	3.880973	8.144947
-346.486762	-0.967329	8.154944
-344.629037	-1.404383	8.164941
-342.815101	1.800293	8.174938
-340.885970	0.287630	8.184934
-339.178750	0.397241	8.194931
-337.636430	-0.602084	8.204928
-335.336024	2.660721	8.214925
-333.202272	-2.350395	8.224922
-331.836417	0.821616	8.234918
-329.862004	-2.611952	8.244915
-327.814500	-2.315081	8.254912
-325.661001	-1.379867	8.264909
-324.399299	-2.702278	8.274906
-322.230735	-1.126834	8.284902
-320.226284	0.594813	8.294899
-318.648245	-6.197047	8.304896
-316.628712	-10.015175	8.314893
-314.414637	-0.909093	8.324890
-313.000358	0.564145	8.334886
-311.209270	3.361968	8.344883
-309.224796	-2.542666	8.354880
-307.250100	-0.969417	8.364877
-305.472751	0.611655	8.374874
-303.511253	-2.346146	8.384870
-301.590395	-0.296929	8.394867
-299.651466	-0.969543	8.404864
-297.946760	-7.317401	8.414861
-295.817228	-0.094119	8.424858
-294.079875	6.935984	8.434854
-292.455348	0.335663	8.444851
-290.180534	-1.966354	8.454848
-288.433500	-0.874641	8.464845
-286.561946	-2.559649	8.474842
-284.730036	-3.219905	8.484838
-283.167333	6.482826	8.494835
-280.896707	-4.000629	8.504832
-278.896071	0.762717	8.514829
-277.281918	1.547229	8.524826
-275.521013	0.345682	8.534822
-273.238125	10.871357	8.544819
-271.753560	2.536018	8.554816
-269.688568	2.324884	8.564813
-267.859481	1.374564	8.574810
-265.821625	1.747239	8.584807
-264.034780	-5.287920	8.594803
-262.017543	-3.129317	8.604800
-260.240740	2.666091	8.614797
-258.482096	4.003869	8.624794
-257.056505	11.407452	8.634791
-255.044998	7.636440	8.644787
-252.593788	9.896309	8.654784
-250.778152	3.830771	8.664781
-249.198510	2.023438	8.674778
-247.060876	1.860728	8.684775
-245.256293	1.575917	8.694771
-243.605064	-1.479156	8.704768
-241.389883	0.429975	8.714765
-239.694459	10.515768	8.724762
-237.746267	2.112762	8.734759
-235.902149	-1.239937	8.744755
-234.254788	-4.415965	8.754752
-232.006212	-7.307425	8.764749
-230.562993	-7.708232	8.774746
-228.558192	-3.171298	8.784743
-226.569865	-5.642267	8.794739
-224.850501	-1.985035	8.804736
-222.641162	-0.599165	8.814733
-220.883032	-3.879706	8.824730
-219.005488	-3.339300	8.834727
-217.219043	-5.114882	8.844723
-215.452946	-4.349843	8.854720
-213.114861	-8.142941	8.864717
-211.540718	-8.324632	8.874714
-209.783447	-3.923438	8.884711
-207.862582	1.417966	8.894707
-205.988106	-2.964294	8.904704
-203.658681	-8.161266	8.914701
-201.842631	-10.142088	8.924698
-200.408280	-12.619360	8.934695
-198.517122	-11.326372	8.944691
-196.403964	-10.111445	8.954688
-194.662113	-7.907256	8.964685
-192.914219	-12.359303	8.974682
-190.586783	-8.036458	8.984679
-189.290088	-11.151755	8.994675
-187.400490	-15.877465	9.004672
-185.232094	-8.169230	9.014669
-183.222123	-7.957825	9.024666
-181.496754	-8.847316	9.034663
-179.819066	-10.138145	9.044659
-177.605724	-7.516555	9.054656
-175.740996	-10.030916	9.064653
-174.155183	-13.670767	9.074650
-172.272793	-13.306361	9.084647
-170.307881	-11.049330	9.094643
-168.471317	-11.388135	9.104640
-166.464226	-8.891516	9.114637
-164.730895	-7.963316	9.124634
-162.759955	-10.973039	9.134631
-160.853380	-7.584057	9.144627
-158.981413	-15.780622	9.154624
-157.187641	-7.718892	9.164621
-155.147693	-10.392252	9.174618
-153.316887	-10.313284	9.184615
-151.620278	-5.232891	9.194611
-149.494410	-7.354693	9.204608
-147.860137	-5.089091	9.214605
-146.110831	-3.353425	9.224602
-144.044246	-1.769438	9.234599
-142.007264	-5.804950	9.244595
-140.125712	-7.174073	9.254592
-138.313292	-7.264265	9.264589
-136.721037	-7.665114	9.274586
-134.899631	-6.512525	9.284583
-132.810804	-10.022616	9.294579
-130.717887	-12.285986	9.304576
-128.954417	-13.184678	9.314573
-127.002163	-5.560316	9.324570
-125.286275	-4.532988	9.334567
-123.302041	-5.847429	9.344563
-121.297490	-7.090900	9.354560
-119.780561	-10.127620	9.364557
-117.895118	-7.055757	9.374554
-116.208717	-8.003722	9.384551
-114.082465	-7.384496	9.394547
-111.576843	-5.960535	9.404544
-110.083152	-9.361437	9.414541
-108.364249	-7.639839	9.424538
-106.695072	-8.190311	9.434535
-104.542569	-2.742095	9.444531
-102.660897	0.207225	9.454528
-100.887372	0.663269	9.464525
-98.940228	-4.297352	9.474522
-97.045278	-2.856466	9.484519
-95.512455	-7.368870	9.494515
-93.526714	-11.525640	9.504512
-91.539320	-3.349483	9.514509
-89.364823	-3.734251	9.524506
-87.499024	1.402884	9.534503
-85.762197	-5.098386	9.544499
-84.002090	-3.694397	9.554496
-82.438882	-4.707947	9.564493
-80.375110	-5.989254	9.574490
-78.432961	3.236246	9.584487
-76.342581	-3.746165	9.594483
-74.358571	2.550020	9.604480
-72.564069	-4.781499	9.614477
-71.153967	3.245205	9.624474
-69.027704	-3.687661	9.634471
-67.057907	-0.348160	9.644467
-65.151184	-3.726512	9.654464
-63.303322	-1.717558	9.664461
-61.521286	-2.265479	9.674458
-59.714934	-6.330447	9.684455
-57.738150	0.194274	9.694451
-55.915819	0.355194	9.704448
-54.010118	-7.398263	9.714445
-51.620284	-3.907865	9.724442
-50.391557	3.069363	9.734439
-48.659366	-1.841138	9.744435
-46.607431	-5.354747	9.754432
-44.447810	-1.816563	9.764429
-42.299120	2.306003	9.774426
-40.842304	-3.234775	9.784423
-39.076985	-0.194210	9.794419
-37.347418	-8.304821	9.804416
-35.183106	-3.014739	9.814413
-33.225904	0.437326	9.824410
-31.313101	-2.787232	9.834407
-29.631998	-0.208490	9.844403
-27.641273	-3.028633	9.854400
-25.727932	5.385193	9.864397
-23.970977	2.903925	9.874394
-22.004641	-1.066539	9.884391
-20.144260	6.315211	9.894387
-18.468667	-4.744161	9.904384
-16.558588	5.111778	9.914381
-14.494339	-0.276411	9.924378
-12.718459	0.858272	9.934375
-10.804601	7.582550	9.944371
-9.019441	-6.502202	9.954368
-7.056298	-1.600004	9.964365
-5.570662	12.679989	9.974362
-3.939749	31.356326	9.984359
-2.658378	69.018601	9.994355
-1.148977	112.740989	10.004352
0.000000	150.954963	10.009357
1.189788	181.671910	10.014362
1.472525	200.805779	10.019367
2.024144	221.543128	10.024371
2.333065	245.356448	10.029376
2.472407	248.923421	10.034381
2.835697	264.277163	10.039386
2.592016	267.941509	10.044391
3.238946	277.325368	10.049395
3.473900	297.411589	10.054400
3.211933	291.822063	10.059405
3.435888	294.079284	10.064410
3.420648	301.488765	10.069415
3.613886	304.706530	10.074419
3.261973	307.274810	10.079424
3.582267	310.164801	10.084429
3.553762	306.875096	10.089434
3.613081	309.729444	10.094439
4.192685	304.095559	10.099443
3.626689	293.476692	10.104448
3.419274	300.090496	10.109453
3.574845	303.708511	10.114458
3.842975	311.719353	10.119463
3.875249	313.664951	10.124467
3.834406	317.981358	10.129472
3.985764	321.823979	10.134477
3.788253	318.359378	10.139482
3.682526	324.893894	10.144487
4.015135	326.373689	10.149491
4.013187	322.267605	10.154496
4.206215	317.181086	10.159501
4.157152	325.327688	10.164506
4.047340	336.819279	10.169511
4.204558	320.696521	10.174515
3.632248	335.658678	10.179520
4.210143	328.919600	10.184525
4.186404	335.655511	10.189530
4.255511	344.622223	10.194535
4.182798	360.267968	10.199539
4.415081	363.460595	10.204544
4.529723	371.193174	10.209549
4.608028	376.078804	10.214554
4.590342	368.717186	10.219559
4.857181	378.686874	10.224563
4.662040	372.861149	10.229568
4.685352	371.136986	10.234573
4.588369	387.829013	10.239578
4.484147	379.762091	10.244583
4.713352	375.300571	10.249587
4.932488	379.935077	10.254592
4.648156	388.515064	10.259597
5.271153	389.827118	10.264602
5.006544	400.553386	10.269607
5.093742	390.733864	10.274611
5.267059	416.745326	10.279616
5.459538	421.116010	10.284621
5.325121	397.200518	10.289626
4.917867	408.463640	10.294631
5.602729	397.351852	10.299635
5.656769	414.365178	10.304640
5.817288	414.186642	10.309645
5.374296	399.517316	10.314650
5.015031	409.522241	10.319655
5.680624	407.895898	10.324659
5.765154	430.453770	10.329664
5.861917	418.462777	10.334669
6.017681	418.097338	10.339674
5.635953	400.537097	10.344679
5.463768	412.901304	10.349683
5.695953	418.710168	10.354688
5.798671	418.640202	10.359693
5.742205	424.450956	10.364698
5.668148	437.204815	10.369703
6.293558	429.939284	10.374707
6.116344	443.763029	10.379712
5.701994	434.974400	10.384717
5.997782	439.276571	10.389722
5.743729	434.007432	10.394727
5.641249	441.779413	10.399731
5.863730	447.507833	10.404736
6.208164	461.879179	10.409741
6.417879	464.775801	10.414746
6.258589	463.762012	10.419751
6.697121	462.455740	10.424755
6.579016	466.797131	10.429760
6.242970	463.791417	10.434765
6.601413	463.098752	10.439770
6.693417	479.262411	10.444775
6.546966	469.882237	10.449779
6.847171	473.655424	10.454784
6.541898	479.463308	10.459789
6.681250	480.557622	10.464794
6.315413	482.035301	10.469799
6.760311	477.242871	10.474803
6.814573	474.209591	10.479808
6.569982	489.095975	10.484813
6.764876	491.042466	10.489818
6.763058	511.379645	10.494823
7.063952	514.110341	10.499827
6.989124	518.175179	10.504832
7.140525	517.029823	10.509837
7.382087	507.404802	10.514842
7.466514	530.122121	10.519847
7.305008	517.678645	10.524851
7.646797	518.814789	10.529856
7.323313	530.036256	10.534861
7.436068	522.152270	10.539866
7.262851	527.453396	10.544871
7.475084	517.913472	10.549875
7.702223	525.213441	10.554880
7.448080	520.075174	10.559885
7.806488	516.976023	10.564890
7.471551	535.694762	10.569895
7.484698	527.197442	10.574899
7.518171	535.950754	10.579904
7.742855	549.434518	10.584909
8.152245	560.258402	10.589914
8.221429	562.951949	10.594919
8.047242	547.545718	10.599923
8.005300	544.901516	10.604928
7.812594	532.915601	10.609933
8.283643	545.178895	10.614938
8.092798	574.724423	10.619943
8.357558	570.607265	10.624947
8.562563	573.255495	10.629952
8.159833	562.864283	10.634957
8.167633	555.075870	10.639962
8.230427	567.451614	10.644967
8.547016	571.047166	10.649971
8.514244	576.683886	10.654976
8.350675	575.989324	10.659981
8.599970	569.433443	10.664986
8.421031	584.634314	10.669991
8.433684	578.117752	10.674995
8.582939	577.762810	10.680000
8.465140	579.174124	10.685005
8.551949	581.035363	10.690010
8.362099	588.127480	10.695015
8.614069	575.055012	10.700019
8.760126	584.474812	10.705024
8.595347	606.556258	10.710029
9.154249	606.449796	10.715034
8.625056	610.260696	10.720039
9.098431	607.917496	10.725043
9.155645	610.267598	10.730048
9.353923	613.252809	10.735053
9.138237	610.208942	10.740058
9.285413	609.310266	10.745063
9.346007	611.467435	10.750067
9.305583	615.146755	10.755072
8.812443	617.305517	10.760077
9.392788	608.119991	10.765082
8.708968	625.684936	10.770087
9.235940	616.055319	10.775091
9.652901	644.983628	10.780096
9.502522	644.012560	10.785101
9.786715	648.649391	10.790106
9.481193	656.054892	10.795111
9.837869	654.356370	10.800115
10.014643	644.341033	10.805120
9.528173	654.869480	10.810125
9.902711	654.443908	10.815130
9.849103	659.618766	10.820135
10.001295	654.817774	10.825139
10.040162	660.326400	10.830144
9.992527	663.844451	10.835149
10.083225	654.886815	10.840154
9.799087	663.154684	10.845159
9.977650	661.517690	10.850163
9.796874	669.642916	10.855168
9.829730	665.778773	10.860173
10.231343	672.380758	10.865178
10.014166	688.841558	10.870183
10.189999	698.732940	10.875187
10.241646	697.199768	10.880192
10.189037	702.092197	10.885197
10.295998	698.061678	10.890202
10.412904	699.908670	10.895207
10.907359	692.739596	10.900211
10.718634	699.355330	10.905216
10.416077	704.729192	10.910221
10.654193	697.869096	10.915226
10.571183	705.704347	10.920231
10.538043	704.506409	10.925235
10.940884	721.570117	10.930240
10.815916	740.001727	10.935245
10.868894	733.986462	10.940250
10.803007	746.677786	10.945255
10.989983	731.062357	10.950259
11.200244	739.305027	10.955264
10.944766	742.338988	10.960269
11.329533	736.277107	10.965274
11.197941	742.566768	10.970279
11.321273	738.374348	10.975283
11.274547	733.120915	10.980288
11.199577	728.772465	10.985293
11.296107	735.620269	10.990298
11.201108	741.907246	10.995303
11.556133	726.701850	11.000307
11.629974	742.053383	11.005312
11.457800	744.534718	11.010317
11.376545	733.693119	11.015322
11.506488	741.660008	11.020327
11.456735	733.599970	11.025331
11.645391	743.777932	11.030336
11.607238	761.263704	11.035341
11.934984	767.678811	11.040346
11.517032	775.406670	11.045351
12.006701	768.104276	11.050355
12.171187	773.015719	11.055360
11.857897	772.471191	11.060365
12.162469	767.182212	11.065370
11.960042	774.842575	11.070375
12.095170	779.881711	11.075379
12.163206	774.461718	11.080384
12.247987	775.703537	11.085389
12.140500	771.342913	11.090394
11.980092	775.706914	11.095399
12.321447	776.288039	11.100403
12.049652	772.008819	11.105408
12.010882	778.108640	11.110413
12.410322	786.781650	11.115418
12.765814	805.370104	11.120423
12.833145	812.105902	11.125427
12.760089	801.162016	11.130432
12.809410	805.617156	11.135437
13.057759	793.115953	11.140442
12.633032	787.695704	11.145447
12.470927	773.686122	11.150451
12.635582	791.893396	11.155456
12.505378	799.774074	11.160461
12.875893	814.081684	11.165466
12.753355	816.507802	11.170471
12.553632	811.445910	11.175475
12.776037	808.683798	11.180480
12.687370	822.623093	11.185485
12.810784	822.004173	11.190490
12.815326	846.258134	11.195495
12.999149	831.728095	11.200499
12.847473	842.573874	11.205504
12.918470	846.219709	11.210509
13.012547	840.770306	11.215514
13.413584	851.955304	11.220519
13.599069	850.924340	11.225523
13.558122	851.698919	11.230528
13.597827	859.636110	11.235533
13.535611	848.283586	11.240538
13.622054	865.487823	11.245543
14.012406	868.224820	11.250547
13.670780	855.164779	11.255552
13.673801	865.706766	11.260557
14.120015	876.208032	11.265562
13.698877	869.039830	11.270567
14.046048	868.208591	11.275571
14.026100	867.967368	11.280576
14.089663	865.629570	11.285581
14.272327	846.698214	11.290586
13.767912	858.519676	11.295591
13.965790	857.193409	11.300595
14.216789	875.177270	11.305600
13.927604	877.527474	11.310605
14.007428	881.353268	11.315610
13.710389	893.140104	11.320615
14.298801	889.013813	11.325619
14.079443	885.360161	11.330624
13.799308	892.479443	11.335629
14.243669	888.540141	11.340634
14.312072	915.830857	11.345639
14.477460	913.219752	11.350643
14.630127	918.793908	11.355648
14.444059	923.840170	11.360653
14.555502	910.559570	11.365658
14.946626	925.684060	11.370663
15.076768	914.873265	11.375667
14.842749	919.879864	11.380672
14.825969	912.374315	11.385677
15.055097	916.679378	11.390682
14.992758	925.224269	11.395687
15.133073	921.177329	11.400691
15.111894	927.728593	11.405696
14.703700	916.961085	11.410701
15.029629	917.516290	11.415706
14.767267	928.505952	11.420711
14.953747	921.042098	11.425715
14.848069	932.416799	11.430720
15.032940	940.944346	11.435725
15.517127	946.896163	11.440730
15.526877	954.636323	11.445735
15.526411	963.068860	11.450739
15.917462	953.667295	11.455744
15.745923	942.855712	11.460749
15.468075	939.112023	11.465754
15.308643	928.438875	11.470759
15.447856	947.008390	11.475763
15.780827	959.073276	11.480768
15.293553	960.931512	11.485773
15.772569	959.935727	11.490778
15.307428	960.292246	11.495783
15.488129	966.514842	11.500787
15.540125	965.686523	11.505792
15.741536	970.100107	11.510797
15.974094	974.141274	11.515802
15.633069	979.874629	11.520807
15.872895	987.686924	11.525811
15.946443	991.168376	11.530816
16.034583	998.411903	11.535821
16.669040	995.995639	11.540826
16.500972	997.173724	11.545831
16.222528	990.634019	11.550835
16.392552	1001.947451	11.555840
16.369031	994.797770	11.560845
16.461074	999.824930	11.565850
16.254447	997.821961	11.570855
16.575201	996.368842	11.575859
16.612727	990.360668	11.580864
16.452870	1002.507354	11.585869
16.792169	991.436046	11.590874
16.471584	996.998981	11.595879
16.416516	996.990453	11.600883
16.379578	997.847983	11.605888
16.350170	1010.707193	11.610893
16.934580	1015.125936	11.615898
16.823779	1015.779194	11.620903
17.134096	1016.589221	11.625907
17.509199	1016.572005	11.630912
17.365388	1021.654141	11.635917
17.423447	1001.785192	11.640922
17.041552	1004.137587	11.645927
16.959811	994.026042	11.650931
17.527803	996.219037	11.655936
17.132388	1016.592895	11.660941
17.518909	1014.061624	11.665946
17.434649	1017.623451	11.670951
17.588526	1015.209719	11.675955
17.400436	1004.831262	11.680960
16.852109	1004.314751	11.685965
17.322711	1019.772036	11.690970
17.280372	1017.723934	11.695975
17.428511	1027.700388	11.700979
17.915441	1028.277229	11.705984
17.856954	1029.751669	11.710989
17.810919	1020.982785	11.715994
17.566788	1033.910961	11.720999
17.657528	1022.432972	11.726003
17.857610	1036.257024	11.731008
17.712808	1035.447476	11.736013
17.717938	1032.937611	11.741018
17.812071	1028.639372	11.746023
17.934865	1042.519915	11.751027
18.164680	1054.418398	11.756032
18.442127	1045.895964	11.761037
18.423340	1048.821267	11.766042
18.216957	1037.819616	11.771047
18.314782	1051.338275	11.776051
18.650542	1037.012469	11.781056
18.384344	1039.016811	11.786061
18.415913	1037.108315	11.791066
18.261896	1030.545591	11.796071
18.563353	1036.159141	11.801075
18.502862	1057.917901	11.806080
18.337604	1051.137751	11.811085
18.428657	1050.274810	11.816090
18.544752	1043.504983	11.821095
18.568609	1056.975518	11.826099
18.986162	1061.644832	11.831104
18.596233	1057.682432	11.836109
18.838572	1054.302045	11.841114
18.915330	1052.922535	11.846119
18.867395	1054.423682	11.851123
19.041406	1051.077850	11.856128
18.786313	1054.736325	11.861133
19.216821	1057.026957	11.866138
18.961220	1060.223439	11.871143
19.023068	1061.719692	11.876147
19.256621	1049.476111	11.881152
18.935761	1054.215893	11.886157
19.233232	1054.781952	11.891162
19.351249	1078.366879	11.896167
19.437174	1080.346603	11.901171
19.745594	1085.271466	11.906176
19.272410	1081.774953	11.911181
19.458050	1076.826553	11.916186
19.549260	1097.905122	11.921191
19.041762	1081.100598	11.926195
19.584069	1085.261135	11.931200
19.314160	1086.725146	11.936205
19.344916	1082.351840	11.941210
19.201362	1093.201242	11.946215
19.509097	1091.770693	11.951219
19.912604	1099.243106	11.956224
20.002492	1113.701437	11.961229
20.305312	1106.166889	11.966234
20.357598	1112.296483	11.971239
20.238521	1094.682464	11.976243
20.234464	1090.074996	11.981248
19.912782	1092.359449	11.986253
20.103243	1086.266913	11.991258
20.323345	1091.942350	11.996263
19.896558	1088.375352	12.001267
20.103679	1095.235651	12.006272
20.079412	1118.786565	12.011277
20.285033	1108.206454	12.016282
20.279398	1114.614965	12.021287
20.313280	1125.220031	12.026291
20.778281	1113.450446	12.031296
20.604348	1111.185186	12.036301
20.563135	1116.055435	12.041306
20.290092	1107.480413	12.046311
20.512748	1108.053677	12.051315
20.737931	1092.477501	12.056320
19.912442	1085.577127	12.061325
20.451103	1085.409236	12.066330
20.338958	1086.863854	12.071335
20.348749	1092.077642	12.076339
20.244361	1091.633829	12.081344
20.215571	1085.074761	12.086349
20.747233	1100.441964	12.091354
20.499954	1092.257105	12.096359
20.409985	1097.073620	12.101363
20.560425	1094.944292	12.106368
20.198940	1099.625908	12.111373
20.454330	1081.404938	12.116378
20.409378	1100.565455	12.121383
20.380102	1100.901342	12.126387
20.656448	1098.982181	12.131392
20.494616	1094.399877	12.136397
20.369314	1094.842550	12.141402
20.430084	1095.509448	12.146407
20.176492	1096.890428	12.151411
20.434871	1096.317783	12.156416
20.302906	1106.856244	12.161421
20.603099	1100.839244	12.166426
20.536796	1105.528976	12.171431
20.567238	1106.560281	12.176435
20.605998	1092.523083	12.181440
20.679446	1097.390807	12.186445
20.650270	1086.487017	12.191450
20.401197	1081.021291	12.196455
20.322063	1074.348826	12.201459
20.485897	1064.246950	12.206464
20.229039	1079.200552	12.211469
20.395446	1061.503187	12.216474
20.270687	1070.980695	12.221479
20.274647	1073.940223	12.226483
20.447852	1071.816730	12.231488
20.057250	1071.331832	12.236493
20.177914	1061.336198	12.241498
20.370635	1075.230852	12.246503
20.163934	1081.956866	12.251507
20.488772	1084.185506	12.256512
20.315869	1095.145252	12.261517
20.441521	1087.449727	12.266522
20.550185	1077.156357	12.271527
20.277127	1083.388299	12.276531
20.534194	1073.716274	12.281536
19.961373	1072.096577	12.286541
20.279665	1079.316051	12.291546
20.537049	1090.107806	12.296551
20.370535	1083.994935	12.301555
20.639179	1080.192427	12.306560
20.211060	1074.944508	12.311565
20.470998	1074.475701	12.316570
20.558070	1068.557368	12.321575
20.152705	1078.119064	12.326579
20.504513	1080.144693	12.331584
19.918339	1080.276075	12.336589
20.263599	1079.900898	12.341594
19.932423	1085.481327	12.346599
20.059190	1094.576509	12.351603
20.177518	1102.906595	12.356608
20.192270	1112.924885	12.361613
20.304785	1102.955756	12.366618
20.379230	1111.240803	12.371623
20.504370	1110.481239	12.376627
20.837479	1105.108735	12.381632
20.551709	1112.120205	12.386637
20.815777	1096.769649	12.391642
20.759129	1088.062346	12.396647
20.698607	1079.063911	12.401651
20.558323	1073.867858	12.406656
20.608292	1087.203361	12.411661
20.639725	1080.571608	12.416666
20.407224	1073.406333	12.421671
20.194832	1081.361777	12.426675
20.591663	1069.382314	12.431680
20.403078	1085.621368	12.436685
20.653444	1073.781965	12.441690
20.260137	1078.626356	12.446695
20.391268	1088.503056	12.451699
20.542078	1064.867418	12.456704
20.334509	1079.067213	12.461709
20.380867	1065.839433	12.466714
20.684228	1057.486334	12.471719
20.289538	1066.891770	12.476723
20.191868	1061.198462	12.481728
20.128983	1058.245251	12.486733
20.245321	1054.804532	12.491738
20.306291	1060.096883	12.496743
20.367758	1065.868580	12.501747
20.346420	1067.731362	12.506752
19.903697	1068.595270	12.511757
20.596509	1082.518981	12.516762
20.491698	1087.645384	12.521767
20.640211	1083.507200	12.526771
20.491134	1071.920759	12.531776
20.343197	1065.998909	12.536781
20.069396	1074.590233	12.541786
20.326403	1069.936400	12.546791
20.107396	1071.896947	12.551795
20.442203	1070.110400	12.556800
20.262474	1080.323702	12.561805
20.411589	1074.040634	12.566810
20.424696	1074.230979	12.571815
20.175077	1074.520004	12.576819
20.603965	1079.272676	12.581824
20.168531	1081.412835	12.586829
20.327743	1077.080546	12.591834
20.370705	1080.087475	12.596839
20.453525	1079.380397	12.601843
20.514915	1074.178986	12.606848
20.600387	1075.614698	12.611853
20.795747	1074.422863	12.616858
20.293263	1075.887698	12.621863
20.512850	1074.950634	12.626867
20.560600	1071.935616	12.631872
20.312069	1073.041380	12.636877
20.548071	1068.177996	12.641882
20.365995	1075.787958	12.646887
20.472019	1070.724518	12.651891
20.678588	1069.798993	12.656896
20.356674	1063.808694	12.661901
20.338876	1075.092214	12.666906
20.298229	1069.247873	12.671911
20.168413	1067.906042	12.676915
20.249564	1070.958921	12.681920
20.248994	1063.532715	12.686925
20.176908	1081.913742	12.691930
20.217747	1072.120080	12.696935
20.408265	1077.030629	12.701939
20.653176	1066.062635	12.706944
20.460115	1082.923758	12.711949
20.431830	1075.598167	12.716954
20.614076	1084.419549	12.721959
20.341224	1076.786016	12.726963
20.383852	1072.906013	12.731968
20.462904	1075.443532	12.736973
20.644574	1075.280540	12.741978
20.447513	1067.398365	12.746983
19.907282	1050.900314	12.751987
20.797980	1061.934828	12.756992
20.265749	1060.419051	12.761997
20.219503	1049.505396	12.767002
20.203948	1057.391582	12.772007
20.374240	1067.074352	12.777011
20.335974	1069.942838	12.782016
20.374745	1071.906426	12.787021
20.463182	1073.778509	12.792026
20.214056	1059.768337	12.797031
20.422894	1070.189329	12.802035
20.399823	1054.963470	12.807040
19.962959	1060.503973	12.812045
20.198252	1071.499523	12.817050
20.273382	1079.979998	12.822055
20.265082	1081.801275	12.827059
20.291516	1076.583360	12.832064
20.270721	1086.247734	12.837069
20.503985	1078.142363	12.842074
20.548111	1086.777607	12.847079
20.327192	1075.617386	12.852083
19.994291	1082.578009	12.857088
20.305101	1085.116411	12.862093
20.322727	1083.386763	12.867098
20.363185	1085.258614	12.872103
20.426832	1080.334402	12.877107
20.428170	1089.731881	12.882112
20.222947	1088.055125	12.887117
20.353615	1086.313753	12.892122
20.405955	1091.128068	12.897127
20.467967	1086.216731	12.902131
20.895691	1084.109413	12.907136
20.389266	1079.224088	12.912141
20.198805	1056.414076	12.917146
20.103580	1064.265662	12.922151
20.296126	1080.890224	12.927155
20.781487	1083.859706	12.932160
20.398662	1069.126482	12.937165
20.397913	1060.739882	12.942170
20.512614	1058.546870	12.947175
19.993502	1060.566324	12.952179
20.158087	1061.647196	12.957184
20.369614	1075.385877	12.962189
20.315646	1078.635362	12.967194
20.540810	1091.427228	12.972199
20.408847	1072.391212	12.977203
20.419542	1058.986189	12.982208
20.237295	1069.318164	12.987213
20.311454	1059.555468	12.992218
20.511824	1052.004171	12.997223
20.174318	1064.710711	13.002227
20.472769	1055.170878	13.007232
20.390120	1052.593004	13.012237
20.358479	1054.048971	13.017242
20.429224	1059.316107	13.022247
20.121954	1055.780520	13.027251
20.384173	1055.551061	13.032256
20.318108	1061.112849	13.037261
20.669510	1057.593632	13.042266
20.578289	1050.752784	13.047271
20.573379	1054.830275	13.052275
20.408347	1050.168067	13.057280
20.298216	1060.892257	13.062285
20.543338	1050.835776	13.067290
20.724275	1051.783144	13.072295
20.291894	1060.387138	13.077299
20.560342	1047.023019	13.082304
20.353962	1056.956687	13.087309
20.494098	1056.887059	13.092314
20.596291	1063.789312	13.097319
20.622500	1058.912082	13.102323
20.700240	1048.653628	13.107328
20.483880	1041.673463	13.112333
20.397256	1040.189120	13.117338
20.245799	1032.209798	13.122343
19.878958	1037.614537	13.127347
20.559839	1037.581666	13.132352
20.395204	1032.316968	13.137357
20.036418	1030.447080	13.142362
20.445524	1040.527006	13.147367
20.473916	1058.217000	13.152371
20.367618	1050.812396	13.157376
19.910878	1044.575512	13.162381
20.068669	1052.252685	13.167386
20.355177	1065.738108	13.172391
20.447590	1062.816899	13.177395
20.659292	1059.042404	13.182400
20.527611	1060.525368	13.187405
20.413257	1054.235445	13.192410
20.372669	1032.284713	13.197415
20.272530	1032.797491	13.202419
20.256868	1024.828054	13.207424
20.331020	1044.646053	13.212429
20.382226	1037.626366	13.217434
20.456259	1036.679403	13.222439
20.017245	1039.315320	13.227443
20.609768	1048.716252	13.232448
20.247408	1059.652572	13.237453
20.367689	1049.005686	13.242458
20.576253	1054.913198	13.247463
20.418734	1052.421388	13.252467
20.474279	1043.754566	13.257472
20.207882	1039.895477	13.262477
20.187538	1042.716942	13.267482
20.534258	1041.362186	13.272487
20.143362	1042.553737	13.277491
20.590237	1038.533566	13.282496
20.402796	1039.486072	13.287501
20.294322	1034.146179	13.292506
20.177308	1040.512495	13.297511
20.389474	1037.266242	13.302515
20.366040	1028.750807	13.307520
20.203278	1042.828296	13.312525
20.243046	1040.817560	13.317530
20.724329	1040.108431	13.322535
20.084465	1045.197155	13.327539
20.078305	1045.008927	13.332544
20.112361	1051.652367	13.337549
20.208892	1058.508209	13.342554
20.393493	1073.618485	13.347559
19.967254	1071.683653	13.352563
20.207381	1082.749408	13.357568
20.614592	1082.148293	13.362573
20.336554	1073.749141	13.367578
20.469457	1074.781448	13.372583
20.131169	1078.815921	13.377587
20.583411	1076.520178	13.382592
20.349589	1078.749611	13.387597
20.315289	1070.680614	13.392602
20.540320	1071.351274	13.397607
20.810986	1073.110706	13.402611
20.475027	1058.828939	13.407616
20.055090	1054.738854	13.412621
20.242323	1046.145649	13.417626
20.197242	1053.180204	13.422631
20.133680	1070.966887	13.427635
20.645318	1062.460709	13.432640
20.436615	1064.826491	13.437645
20.476048	1059.627010	13.442650
20.316343	1049.357541	13.447655
19.968491	1054.330300	13.452659
20.497924	1059.521118	13.457664
20.390233	1070.243350	13.462669
20.106033	1069.948073	13.467674
20.527710	1075.767981	13.472679
20.139065	1077.246200	13.477683
20.552508	1081.988720	13.482688
20.570954	1079.017801	13.487693
20.215261	1067.530556	13.492698
20.497900	1054.843875	13.497703
20.231399	1053.605855	13.502707
20.409983	1048.261173	13.507712
20.153291	1049.410817	13.512717
20.484140	1061.014052	13.517722
20.314854	1056.636389	13.522727
19.876423	1054.695619	13.527731
20.239066	1064.943832	13.532736
20.445136	1069.702078	13.537741
20.369127	1081.706137	13.542746
20.420146	1082.361974	13.547751
20.495311	1082.163928	13.552755
20.432140	1068.554622	13.557760
20.199371	1074.117772	13.562765
20.411177	1083.737158	13.567770
20.466411	1075.543483	13.572775
20.278181	1066.601698	13.577779
20.345383	1063.684510	13.582784
20.416775	1076.595514	13.587789
20.198369	1062.859577	13.592794
20.288941	1072.585032	13.597799
20.217413	1082.727457	13.602803
20.720936	1077.892365	13.607808
20.375708	1070.262494	13.612813
20.205672	1065.790326	13.617818
20.185382	1056.208287	13.622823
20.146366	1070.070509	13.627827
20.577538	1079.986084	13.632832
20.441719	1090.201851	13.637837
20.553451	1074.027163	13.642842
20.589913	1056.079279	13.647847
20.170167	1070.182014	13.652851
20.337263	1058.832174	13.657856
20.230761	1054.200055	13.662861
19.965461	1058.536713	13.667866
20.399613	1060.240103	13.672871
20.522064	1075.875990	13.677875
20.164854	1070.384935	13.682880
20.199910	1071.816073	13.687885
20.531503	1087.221481	13.692890
20.533200	1087.448341	13.697895
20.206057	1077.060471	13.702899
20.558734	1059.287663	13.707904
20.268330	1059.767709	13.712909
20.027610	1069.984424	13.717914
20.562530	1064.398383	13.722919
20.263839	1087.291232	13.727923
20.288274	1082.638218	13.732928
20.334026	1077.720015	13.737933
20.335964	1081.279148	13.742938
20.727341	1077.564304	13.747943
20.345155	1075.415851	13.752947
20.474155	1061.416331	13.757952
20.379319	1069.909717	13.762957
20.246760	1070.258923	13.767962
20.422523	1066.725139	13.772967
20.428996	1075.733835	13.777971
20.193562	1064.388269	13.782976
20.389813	1065.541366	13.787981
20.505890	1060.033174	13.792986
20.313099	1064.162714	13.797991
19.898113	1075.982703	13.802995
20.464913	1066.447371	13.808000
20.388479	1070.470039	13.813005
20.304342	1070.146005	13.818010
20.356985	1065.876452	13.823015
20.054854	1071.805502	13.828019
20.315624	1062.681708	13.833024
20.603913	1069.771913	13.838029
20.324405	1072.224689	13.843034
20.337886	1064.454021	13.848039
20.356569	1063.588430	13.853043
20.271233	1066.313026	13.858048
20.364136	1063.882202	13.863053
20.487842	1075.152613	13.868058
20.609514	1074.718476	13.873063
20.510749	1069.452721	13.878067
20.699752	1058.178240	13.883072
20.531874	1071.381309	13.888077
20.639529	1068.776232	13.893082
20.610232	1067.913563	13.898087
20.200823	1072.512923	13.903091
20.316794	1069.628958	13.908096
20.384943	1070.204786	13.913101
20.354965	1062.980403	13.918106
20.434313	1071.228373	13.923111
20.553975	1073.841420	13.928115
20.359780	1066.545451	13.933120
20.521203	1066.256371	13.938125
20.352088	1070.244933	13.943130
20.441670	1070.382077	13.948135
20.334158	1074.671492	13.953139
20.524940	1060.701545	13.958144
20.337338	1065.595127	13.963149
19.963928	1076.025411	13.968154
20.229773	1070.300927	13.973159
19.978215	1074.761562	13.978163
20.202240	1067.099245	13.983168
20.300522	1066.375508	13.988173
20.173554	1075.501688	13.993178
20.300135	1073.790934	13.998183
20.406052	1078.748096	14.003187
20.236177	1064.174887	14.008192
20.228478	1071.413025	14.013210
20.324415	1075.094375	14.018227
20.696683	1068.107415	14.023245
20.330561	1083.658608	14.028263
20.467936	1067.568244	14.033280
20.538434	1083.985745	14.038298
20.491308	1079.529040	14.043315
20.498151	1079.328210	14.048333
20.276883	1084.328019	14.053351
20.154575	1070.887156	14.058368
20.398642	1076.257906	14.063386
20.095132	1068.224134	14.068403
20.200649	1073.365297	14.073421
20.121533	1081.738600	14.078439
20.523913	1096.718912	14.083456
20.507875	1110.293622	14.088474
20.827368	1107.074610	14.093491
20.945244	1104.551576	14.098509
20.693076	1115.813846	14.103527
20.894771	1104.273406	14.108544
20.790249	1088.462278	14.113562
20.354070	1090.951206	14.118579
20.817074	1106.250622	14.123597
20.468287	1110.284489	14.128615
20.644034	1103.648184	14.133632
20.624392	1115.310667	14.138650
20.988425	1119.572186	14.143667
21.165160	1106.524041	14.148685
20.823424	1120.765766	14.153703
20.834882	1119.717907	14.158720
21.301944	1110.436482	14.163738
20.775608	1113.109682	14.168755
20.844119	1110.416770	14.173773
20.379435	1116.768898	14.178791
21.080314	1110.844783	14.183808
20.756270	1117.945265	14.188826
20.599446	1118.703348	14.193843
20.931362	1112.636736	14.198861
21.136625	1109.209427	14.203879
21.031330	1110.546032	14.208896
20.988579	1119.124342	14.213914
20.759344	1117.759369	14.218931
20.655095	1111.367497	14.223949
20.854069	1126.070397	14.228967
20.873518	1119.059465	14.233984
20.867014	1147.685052	14.239002
21.048250	1151.167196	14.244019
21.306518	1147.311423	14.249037
21.389305	1152.482982	14.254055
21.387060	1147.617973	14.259072
21.198882	1152.867359	14.264090
21.092145	1155.160605	14.269107
21.230875	1139.475790	14.274125
21.003481	1148.840198	14.279143
21.435054	1140.484642	14.284160
21.423256	1141.491729	14.289178
21.321324	1143.877015	14.294195
21.499372	1146.046182	14.299213
21.476560	1144.075696	14.304231
21.322490	1144.347273	14.309248
21.657239	1148.739314	14.314266
21.775100	1147.469986	14.319283
21.710491	1149.838309	14.324301
21.418964	1139.619211	14.329319
21.697074	1135.197129	14.334336
21.529777	1112.495085	14.339354
21.349301	1119.593117	14.344371
21.767133	1123.457517	14.349389
21.400892	1130.582038	14.354407
21.564001	1135.721903	14.359424
21.837395	1134.759678	14.364442
21.704682	1137.082232	14.369459
21.641769	1114.758366	14.374477
21.631634	1119.389454	14.379495
21.652641	1124.765914	14.384512
21.820037	1129.555879	14.389530
21.803176	1130.859503	14.394547
21.787804	1120.074124	14.399565
21.880551	1122.445657	14.404583
21.756630	1112.674901	14.409600
22.224359	1106.075394	14.414618
21.564278	1117.209246	14.419635
21.690654	1115.328225	14.424653
21.620113	1126.684230	14.429671
21.877441	1137.774013	14.434688
22.098941	1144.159849	14.439706
21.866568	1153.691797	14.444723
22.048322	1144.100353	14.449741
21.980409	1146.558865	14.454759
22.047577	1144.671555	14.459776
22.347935	1134.809513	14.464794
22.041602	1126.129642	14.469811
21.825995	1109.030592	14.474829
21.639879	1118.528397	14.479847
21.786954	1134.444527	14.484864
22.172595	1142.841262	14.489882
21.856354	1145.487248	14.494899
21.942371	1142.078952	14.499917
21.859551	1151.146594	14.504935
21.864157	1148.190159	14.509952
22.146454	1139.883582	14.514970
22.196265	1147.089615	14.519987
22.277053	1140.543946	14.525005
22.206407	1144.684469	14.530023
22.056099	1144.170501	14.535040
22.420429	1141.844106	14.540058
21.989343	1146.440099	14.545075
22.311629	1142.681082	14.550093
22.230238	1139.750950	14.555111
22.254519	1145.082850	14.560128
22.727516	1153.854197	14.565146
22.154428	1160.991277	14.570163
22.266676	1154.708001	14.575181
22.437401	1161.828687	14.580199
22.195036	1164.377949	14.585216
22.665574	1160.898877	14.590234
22.666818	1167.952217	14.595251
22.951693	1161.886796	14.600269
22.570810	1151.864415	14.605287
22.663815	1145.242863	14.610304
22.656647	1139.233472	14.615322
22.528688	1141.725156	14.620339
22.788653	1138.990689	14.625357
22.534669	1137.022470	14.630375
22.473998	1139.567916	14.635392
22.424527	1138.663481	14.640410
22.435935	1151.209805	14.645427
22.454508	1155.358123	14.650445
22.832062	1164.950096	14.655463
22.611161	1174.304047	14.660480
22.882050	1164.849384	14.665498
22.635736	1163.548479	14.670515
22.736162	1165.346209	14.675533
23.040492	1160.529824	14.680551
23.014212	1161.355177	14.685568
23.332569	1158.636561	14.690586
23.064778	1157.922679	14.695603
23.090094	1166.601846	14.700621
22.920359	1153.734764	14.705639
23.169888	1154.523989	14.710656
23.077929	1140.568557	14.715674
22.875524	1146.477739	14.720691
22.704684	1142.658951	14.725709
23.110107	1154.270969	14.730727
23.235164	1155.618026	14.735744
23.296164	1153.245630	14.740762
22.922023	1153.899951	14.745779
22.972029	1162.040344	14.750797
23.147003	1156.579198	14.755815
23.151829	1161.893758	14.760832
22.930358	1154.903933	14.765850
23.385840	1155.805027	14.770867
23.266669	1152.355524	14.775885
23.454986	1152.487545	14.780903
23.149992	1163.896705	14.785920
23.467678	1152.362894	14.790938
23.213770	1162.566824	14.795955
23.151153	1158.228971	14.800973
23.242816	1162.244508	14.805991
23.121461	1165.790651	14.811008
23.040632	1159.550753	14.816026
22.992368	1165.419626	14.821043
22.914415	1163.426472	14.826061
23.276857	1163.963305	14.831079
23.309771	1179.565782	14.836096
23.525199	1182.864728	14.841114
23.593945	1190.877878	14.846131
23.666329	1200.752934	14.851149
23.438687	1195.738242	14.856167
23.629998	1199.937671	14.861184
23.733415	1186.142943	14.866202
23.498236	1183.946773	14.871219
23.546182	1189.062554	14.876237
23.965700	1184.237226	14.881255
23.501328	1187.643031	14.886272
23.806892	1194.476382	14.891290
23.755312	1193.079919	14.896307
23.682461	1190.728866	14.901325
23.830092	1193.514805	14.906343
23.605493	1193.722127	14.911360
23.481498	1197.580161	14.916378
23.412551	1200.375478	14.921395
23.642960	1210.472302	14.926413
23.938209	1196.064941	14.931431
23.737742	1205.181269	14.936448
23.869737	1194.789185	14.941466
23.685111	1195.880472	14.946483
23.499951	1200.239052	14.951501
23.803691	1195.089265	14.956519
23.245368	1199.510512	14.961536
23.866967	1209.268084	14.966554
24.016416	1222.819649	14.971571
24.109067	1214.277434	14.976589
24.290256	1230.126879	14.981607
24.108797	1225.189755	14.986624
24.473803	1225.534270	14.991642
24.754261	1216.336027	14.996659
23.859326	1215.821276	15.001677
24.252127	1204.775671	15.006695
24.447094	1216.956142	15.011712
24.488218	1200.456263	15.016730
24.384397	1193.411474	15.021747
24.510426	1193.287586	15.026765
24.483769	1176.251128	15.031783
24.086698	1193.207378	15.036800
24.037237	1194.744298	15.041818
24.243737	1191.908237	15.046835
24.392782	1192.553041	15.051853
24.277925	1188.709581	15.056871
24.583771	1201.264041	15.061888
24.343680	1200.361692	15.066906
24.334276	1201.428177	15.071923
24.335418	1219.697354	15.076941
25.126935	1216.582355	15.081959
24.876727	1205.197287	15.086976
24.727022	1195.161597	15.091994
24.510514	1190.481762	15.097011
24.403994	1185.067078	15.102029
24.525563	1190.473140	15.107047
24.280863	1195.325712	15.112064
24.722610	1209.670646	15.117082
24.817640	1222.104592	15.122099
24.683692	1226.294561	15.127117
24.978420	1213.910201	15.132135
24.543786	1207.891885	15.137152
24.773431	1199.485132	15.142170
24.769337	1224.459456	15.147187
24.708375	1220.070983	15.152205
24.962293	1214.214974	15.157223
25.047625	1221.678076	15.162240
24.777250	1211.354879	15.167258
25.079282	1211.254829	15.172275
24.675303	1209.179962	15.177293
25.257266	1212.634384	15.182311
24.837944	1200.621908	15.187328
24.967833	1218.002227	15.192346
25.322411	1215.715130	15.197363
25.117167	1207.486279	15.202381
24.973294	1198.445393	15.207399
24.800846	1193.373134	15.212416
24.641638	1208.797073	15.217434
25.030510	1215.997822	15.222451
24.833343	1227.485789	15.227469
25.061862	1225.700148	15.232487
24.745899	1231.602309	15.237504
24.756071	1222.672119	15.242522
25.066955	1221.449076	15.247539
24.919609	1215.213471	15.252557
25.414400	1236.450916	15.257575
25.380433	1247.695787	15.262592
25.409438	1254.472603	15.267610
25.279053	1248.347539	15.272627
25.478200	1256.654535	15.277645
25.488486	1250.008376	15.282663
25.566906	1249.511405	15.287680
25.679494	1241.488246	15.292698
25.556887	1221.118023	15.297715
25.263140	1222.854362	15.302733
25.254700	1229.832197	15.307751
25.486394	1241.673346	15.312768
25.440824	1245.916865	15.317786
25.805720	1251.350206	15.322803
25.501315	1252.028014	15.327821
25.479411	1248.680952	15.332839
25.482497	1248.027680	15.337856
25.602078	1253.989369	15.342874
25.915613	1247.524507	15.347891
25.767948	1256.519186	15.352909
25.400716	1246.694338	15.357927
25.878951	1251.233414	15.362944
25.605722	1247.688909	15.367962
25.761966	1249.719996	15.372979
25.527007	1244.725330	15.377997
25.849826	1246.316136	15.383015
25.724875	1249.161294	15.388032
25.745077	1259.445840	15.393050
25.793231	1237.209464	15.398067
25.796322	1261.130337	15.403085
25.970114	1240.259773	15.408103
25.849130	1250.614024	15.413120
26.062508	1250.878904	15.418138
25.997154	1239.624774	15.423155
26.020983	1257.932852	15.428173
26.038005	1255.828580	15.433191
25.984491	1251.215537	15.438208
26.276392	1264.012952	15.443226
26.443762	1263.934381	15.448243
26.006470	1260.708628	15.453261
25.937625	1264.575187	15.458279
26.423136	1272.841236	15.463296
26.273315	1264.208678	15.468314
26.327981	1272.664572	15.473331
26.335007	1273.415405	15.478349
26.222698	1275.541241	15.483367
26.128722	1286.761106	15.488384
26.213387	1280.488467	15.493402
26.293019	1278.155552	15.498419
26.083716	1285.904786	15.503437
26.289479	1275.587396	15.508455
26.510415	1286.524220	15.513472
26.459568	1277.869574	15.518490
26.476800	1286.509203	15.523507
26.578075	1282.108991	15.528525
26.719229	1273.821705	15.533543
27.003404	1282.349539	15.538560
26.584802	1281.527568	15.543578
26.591115	1280.900522	15.548595
26.527972	1282.272891	15.553613
26.595531	1272.422721	15.558631
26.670524	1280.806164	15.563648
26.708100	1284.430807	15.568666
26.934645	1273.351893	15.573683
26.488101	1284.140347	15.578701
26.765129	1272.771805	15.583719
26.736962	1276.455697	15.588736
26.487202	1281.593827	15.593754
26.754353	1285.189718	15.598771
26.702223	1283.395352	15.603789
26.965975	1283.537365	15.608807
26.929092	1290.596846	15.613824
26.697697	1297.405779	15.618842
27.037417	1301.660219	15.623859
27.048815	1316.681100	15.628877
27.084728	1312.992887	15.633895
27.414668	1307.486518	15.638912
26.936013	1314.078490	15.643930
27.218897	1306.128808	15.648947
27.304833	1307.763697	15.653965
27.117056	1292.728556	15.658983
27.035632	1298.447040	15.664000
27.014092	1300.693684	15.669018
27.300601	1305.686509	15.674035
27.125265	1309.900407	15.679053
27.263158	1301.638794	15.684071
27.327305	1306.791359	15.689088
27.025637	1300.857190	15.694106
27.356981	1309.201334	15.699123
27.360616	1307.717399	15.704141
27.405636	1311.123781	15.709159
27.390312	1310.097483	15.714176
27.162833	1312.200795	15.719194
27.565560	1299.649696	15.724211
27.183148	1307.901615	15.729229
27.472407	1305.041320	15.734247
27.750646	1302.900096	15.739264
27.370744	1315.951005	15.744282
27.361163	1304.994675	15.749299
27.310741	1315.359739	15.754317
27.451525	1311.319739	15.759335
27.486615	1315.025012	15.764352
27.670805	1338.624538	15.769370
27.863732	1333.011023	15.774387
27.944713	1334.780415	15.779405
27.680669	1336.977654	15.784423
27.941415	1325.699759	15.789440
27.884819	1329.443256	15.794458
28.070862	1317.052548	15.799475
28.109183	1309.716038	15.804493
27.355183	1313.168067	15.809511
27.901170	1321.989225	15.814528
27.964452	1332.139534	15.819546
28.404558	1329.325961	15.824563
27.775944	1324.691364	15.829581
27.859502	1332.387619	15.834599
28.335328	1324.613223	15.839616
28.083525	1330.385637	15.844634
28.644852	1327.030475	15.849651
27.952305	1312.336953	15.854669
27.865919	1315.740700	15.859687
27.878880	1319.790857	15.864704
28.087658	1330.718642	15.869722
28.114723	1330.604247	15.874739
28.409968	1334.653429	15.879757
28.016459	1330.218862	15.884775
28.036052	1331.593769	15.889792
27.994897	1332.833645	15.894810
27.986953	1325.542260	15.899827
27.930555	1338.816875	15.904845
28.245866	1345.647170	15.909863
29.060645	1350.337096	15.914880
28.713572	1338.223316	15.919898
28.867675	1325.066898	15.924915
28.703867	1327.789279	15.929933
28.768913	1321.747845	15.934951
28.721156	1323.158663	15.939968
28.906409	1321.799918	15.944986
28.486957	1327.172773	15.950003
28.531396	1332.690293	15.955021
28.639153	1325.844505	15.960039
29.016188	1316.586749	15.965056
28.820412	1327.185796	15.970074
28.929733	1319.200869	15.975091
28.942108	1321.679638	15.980109
28.698086	1320.576558	15.985127
29.070911	1317.696639	15.990144
28.565463	1323.087928	15.995162
28.812746	1321.151417	16.000179
28.838139	1319.884239	16.005197
28.734518	1326.049875	16.010215
28.953476	1325.242616	16.015232
28.700926	1325.998674	16.020250
28.713100	1320.179609	16.025267
28.650705	1321.646245	16.030285
28.963373	1328.796285	16.035303
29.104504	1318.088044	16.040320
28.988826	1330.231642	16.045338
28.890600	1346.659048	16.050355
29.029927	1343.600859	16.055373
29.090097	1356.009019	16.060391
29.200010	1355.730395	16.065408
29.169910	1364.800772	16.070426
29.209085	1350.026681	16.075443
29.154218	1358.522119	16.080461
29.156079	1362.183940	16.085479
29.208649	1360.297357	16.090496
29.445044	1357.651555	16.095514
29.347805	1360.292536	16.100531
29.571238	1356.393500	16.105549
29.301114	1359.194193	16.110567
29.423769	1356.816649	16.115584
29.128627	1360.653260	16.120602
29.286643	1352.630660	16.125619
29.153876	1362.398545	16.130637
29.210225	1376.908940	16.135655
29.458717	1375.599880	16.140672
29.577105	1391.978629	16.145690
29.854182	1390.375565	16.150707
29.971879	1381.991283	16.155725
29.858202	1380.039977	16.160743
30.128435	1374.060177	16.165760
29.660214	1380.806247	16.170778
30.062331	1382.710044	16.175795
30.149761	1377.168396	16.180813
29.870264	1365.901133	16.185831
30.088024	1353.392075	16.190848
29.704664	1349.550500	16.195866
29.744913	1358.957298	16.200883
30.269900	1375.032071	16.205901
30.428915	1375.329220	16.210919
30.294913	1351.323715	16.215936
29.991963	1351.010268	16.220954
29.875458	1345.969932	16.225971
30.027879	1342.738191	16.230989
29.633491	1351.917003	16.236007
30.127478	1374.402214	16.241024
30.033710	1374.239450	16.246042
30.160067	1372.399300	16.251059
30.491150	1381.150950	16.256077
30.385783	1380.127998	16.261095
30.609028	1380.204113	16.266112
30.585186	1378.562528	16.271130
30.421573	1368.695681	16.276147
30.434289	1349.765066	16.281165
29.972890	1364.608147	16.286183
30.323162	1371.324337	16.291200
30.337377	1374.702613	16.296218
30.161098	1387.714815	16.301235
30.281583	1382.480932	16.306253
30.266683	1378.352485	16.311271
30.321702	1377.673620	16.316288
29.940733	1381.267517	16.321306
30.464723	1381.646455	16.326323
30.575489	1394.826816	16.331341
30.717343	1407.607392	16.336359
30.943952	1408.732204	16.341376
30.961256	1397.598479	16.346394
30.693224	1393.537144	16.351411
30.541488	1390.256377	16.356429
30.743700	1407.452350	16.361447
30.814638	1413.379391	16.366464
31.097727	1413.733831	16.371482
30.724923	1412.327233	16.376499
31.194720	1412.474137	16.381517
30.937727	1417.498634	16.386535
30.951984	1412.210896	16.391552
31.005454	1412.649153	16.396570
30.735422	1410.389292	16.401587
31.027910	1412.480470	16.406605
30.887390	1415.556238	16.411623
31.221675	1412.084684	16.416640
31.391265	1403.736158	16.421658
31.184025	1409.578576	16.426675
31.538110	1399.459243	16.431693
31.249091	1409.989850	16.436711
31.283855	1404.357489	16.441728
31.339217	1405.616583	16.446746
31.473712	1407.424640	16.451763
31.576558	1408.024913	16.456781
30.938907	1413.372826	16.461799
31.026609	1406.190416	16.466816
31.116641	1407.768033	16.471834
31.106699	1403.503504	16.476851
31.340815	1404.315652	16.481869
31.312718	1417.725827	16.486887
31.677888	1428.913467	16.491904
32.018798	1432.614038	16.496922
31.898336	1416.358343	16.501939
31.573645	1409.650707	16.506957
31.405271	1406.995523	16.511975
31.598196	1408.765945	16.516992
31.879203	1418.422252	16.522010
31.936653	1423.893686	16.527027
31.928868	1410.214013	16.532045
31.886357	1406.132434	16.537063
31.781538	1410.423204	16.542080
31.880567	1406.973444	16.547098
31.746193	1408.110215	16.552115
32.130439	1408.832349	16.557133
31.955320	1413.938169	16.562151
31.920525	1401.853181	16.567168
31.996064	1410.642463	16.572186
32.296513	1433.860223	16.577203
31.793087	1423.879220	16.582221
31.888992	1426.391876	16.587239
31.879922	1431.866058	16.592256
32.236251	1440.475287	16.597274
31.793456	1438.183201	16.602291
32.201880	1432.999331	16.607309
32.366746	1439.185114	16.612327
32.060190	1430.807123	16.617344
32.225071	1430.824905	16.622362
32.042341	1447.460964	16.627379
32.290125	1438.629599	16.632397
31.861357	1443.352731	16.637415
32.192853	1455.171844	16.642432
32.503826	1464.903629	16.647450
32.420784	1476.755844	16.652467
32.668905	1471.102011	16.657485
32.507937	1478.118452	16.662503
32.879963	1467.860926	16.667520
32.602462	1464.622224	16.672538
32.330791	1473.444901	16.677555
32.754225	1471.332406	16.682573
32.700295	1469.802579	16.687591
32.573537	1468.002789	16.692608
32.926703	1464.199440	16.697626
32.654391	1465.388104	16.702643
33.175008	1464.748234	16.707661
32.805361	1464.695540	16.712679
32.934054	1460.548885	16.717696
33.036280	1457.174111	16.722714
32.966844	1471.764440	16.727731
33.068702	1461.572034	16.732749
32.786575	1465.340526	16.737767
33.045250	1469.507267	16.742784
33.168959	1470.455010	16.747802
32.894797	1473.217042	16.752819
33.137416	1461.152252	16.757837
32.823420	1472.648034	16.762855
32.947480	1464.459323	16.767872
33.418783	1459.877339	16.772890
33.016164	1465.535431	16.777907
33.215315	1459.106024	16.782925
33.177760	1467.180328	16.787943
33.225103	1464.611853	16.792960
33.466388	1471.776496	16.797978
33.326505	1473.883162	16.802995
33.457799	1471.941536	16.808013
33.215332	1485.676197	16.813031
33.478221	1479.771460	16.818048
33.676936	1489.982864	16.823066
33.528657	1494.977463	16.828083
33.652065	1481.632312	16.833101
33.466413	1494.090023	16.838119
33.402869	1493.607035	16.843136
33.684173	1485.612676	16.848154
33.581718	1493.692627	16.853171
34.100591	1480.952169	16.858189
33.485189	1486.984778	16.863207
33.417219	1493.207721	16.868224
33.973505	1493.837924	16.873242
33.583086	1495.757245	16.878259
33.536003	1486.311405	16.883277
33.572132	1493.360125	16.888295
33.691290	1503.662095	16.893312
34.156171	1503.897877	16.898330
33.875250	1520.585861	16.903347
34.213145	1514.113851	16.908365
34.588848	1515.501978	16.913383
34.348903	1503.287600	16.918400
34.231948	1489.091206	16.923418
34.133926	1484.309003	16.928435
33.840841	1487.470470	16.933453
34.095360	1496.707898	16.938471
34.398614	1511.997045	16.943488
34.675495	1508.248325	16.948506
34.476500	1504.047741	16.953523
34.121529	1487.899372	16.958541
34.642183	1498.274157	16.963559
34.529848	1507.803707	16.968576
34.548062	1500.206818	16.973594
34.651114	1500.498739	16.978611
34.295142	1489.553473	16.983629
34.812284	1507.708461	16.988647
34.685661	1503.242283	16.993664
34.540349	1502.511206	16.998682
34.415010	1519.452021	17.003699
34.674465	1511.380120	17.008717
34.495732	1515.810129	17.013735
34.559411	1517.990517	17.018752
34.813426	1510.786249	17.023770
34.563226	1519.026636	17.028787
34.773647	1512.732266	17.033805
34.561768	1510.846158	17.038823
34.968473	1514.425354	17.043840
35.065780	1509.901433	17.048858
34.666674	1518.831769	17.053875
34.814179	1511.995285	17.058893
34.696469	1513.690207	17.063911
34.670370	1524.071991	17.068928
35.437598	1523.436830	17.073946
35.320985	1539.447375	17.078963
35.618971	1541.826356	17.083981
35.685937	1518.133025	17.088999
35.533745	1504.471577	17.094016
35.399385	1499.434821	17.099034
35.238868	1513.137560	17.104051
35.637349	1498.453092	17.109069
35.495213	1503.970547	17.114087
35.264638	1507.055192	17.119104
35.757952	1499.863886	17.124122
35.691092	1510.549473	17.129139
35.599323	1501.207494	17.134157
35.625898	1507.984817	17.139175
35.533758	1504.121132	17.144192
35.758837	1501.431491	17.149210
35.578528	1503.330671	17.154227
35.589013	1509.903702	17.159245
35.621645	1498.899592	17.164263
35.461169	1500.248179	17.169280
35.630798	1496.765114	17.174298
35.515588	1498.358959	17.179315
35.527824	1512.112011	17.184333
35.471454	1510.590435	17.189351
35.797249	1524.915638	17.194368
35.907301	1529.352289	17.199386
36.030004	1529.368147	17.204403
35.931157	1533.208887	17.209421
36.097020	1534.204182	17.214439
35.800167	1539.381374	17.219456
36.230264	1535.793046	17.224474
35.987957	1535.757794	17.229491
36.001230	1533.190022	17.234509
35.797283	1543.864464	17.239527
35.687662	1532.073669	17.244544
36.040886	1526.964640	17.249562
35.953753	1548.700428	17.254579
36.177287	1564.331120	17.259597
36.358678	1568.839777	17.264615
36.488983	1565.942649	17.269632
36.413207	1566.783785	17.274650
36.469075	1570.965599	17.279667
36.497666	1572.229765	17.284685
36.741279	1566.043340	17.289703
36.536138	1576.066740	17.294720
36.687079	1568.943380	17.299738
36.761630	1559.568544	17.304755
36.733898	1571.194929	17.309773
36.571274	1559.817635	17.314791
36.513421	1564.229952	17.319808
36.876040	1569.471862	17.324826
36.968631	1567.179307	17.329843
36.921407	1566.548990	17.334861
37.169602	1560.795220	17.339879
36.946498	1564.847703	17.344896
36.817073	1567.081707	17.349914
36.902944	1565.138662	17.354931
36.748397	1567.334200	17.359949
37.125208	1551.074548	17.364967
36.735896	1575.883607	17.369984
37.216337	1572.227463	17.375002
36.972034	1569.068389	17.380019
36.992406	1559.431624	17.385037
37.185547	1557.201687	17.390055
36.990259	1567.043391	17.395072
36.841035	1561.174465	17.400090
36.827312	1568.781751	17.405107
36.972660	1573.820782	17.410125
37.405457	1577.210996	17.415143
37.057678	1584.567967	17.420160
37.449644	1571.159449	17.425178
37.367910	1583.483467	17.430195
37.290070	1573.930787	17.435213
37.558610	1574.226203	17.440231
37.595195	1587.961285	17.445248
37.415628	1576.441956	17.450266
37.189917	1584.443299	17.455283
37.515570	1595.304665	17.460301
37.885126	1593.727730	17.465319
37.952974	1608.030447	17.470336
37.833469	1611.211447	17.475354
38.157238	1604.033761	17.480371
37.762021	1594.766078	17.485389
37.889614	1589.834593	17.490407
38.038366	1602.010176	17.495424
38.079780	1603.511408	17.500442
38.169881	1608.679604	17.505459
38.459229	1602.032821	17.510477
38.293129	1577.482268	17.515495
37.811114	1581.731787	17.520512
37.745489	1579.482555	17.525530
37.990989	1601.167727	17.530547
38.032636	1604.773711	17.535565
38.343351	1603.855844	17.540583
38.326722	1607.262690	17.545600
38.343333	1608.241681	17.550618
38.370967	1609.727808	17.555635
38.405524	1606.869540	17.560653
38.381218	1603.470081	17.565671
38.352526	1603.030296	17.570688
38.225571	1618.728747	17.575706
38.478066	1608.921214	17.580723
38.345829	1611.726703	17.585741
38.516332	1611.841122	17.590759
37.987306	1613.570984	17.595776
38.382428	1626.111575	17.600794
38.633762	1629.127247	17.605811
38.721259	1645.615820	17.610829
39.035415	1630.882531	17.615847
38.972671	1642.703328	17.620864
39.114305	1642.311884	17.625882
38.826421	1640.035169	17.630899
38.706812	1635.998071	17.635917
38.947334	1640.645190	17.640935
38.789862	1639.894809	17.645952
39.114593	1627.576103	17.650970
39.118964	1632.351338	17.655987
38.861493	1646.679239	17.661005
39.306167	1638.227713	17.666023
39.267682	1630.500581	17.671040
39.236082	1636.924646	17.676058
39.272095	1638.006729	17.681075
38.852937	1636.738853	17.686093
39.184796	1630.828561	17.691111
39.074211	1630.324755	17.696128
39.263494	1642.548179	17.701146
39.481663	1650.337968	17.706163
39.297640	1666.460868	17.711181
39.827059	1667.274698	17.716199
39.367497	1670.681415	17.721216
39.572863	1670.828815	17.726234
39.588092	1665.298573	17.731251
39.414847	1672.464936	17.736269
39.612902	1666.481585	17.741287
39.826780	1672.169632	17.746304
39.539133	1669.531850	17.751322
39.785479	1660.440234	17.756339
39.400725	1674.645312	17.761357
39.695829	1664.199350	17.766375
40.104477	1671.003115	17.771392
39.652354	1668.055712	17.776410
40.004870	1670.181401	17.781427
39.758327	1690.074778	17.786445
40.458461	1685.435777	17.791463
40.295122	1698.487879	17.796480
40.187715	1679.647571	17.801498
40.190962	1679.979797	17.806515
40.171270	1700.319946	17.811533
40.374058	1689.624409	17.816551
40.262085	1691.224051	17.821568
40.406297	1693.073068	17.826586
40.345431	1679.923875	17.831603
40.327352	1687.984970	17.836621
40.451314	1684.871743	17.841639
40.117922	1692.542665	17.846656
40.452798	1683.294550	17.851674
40.574870	1690.420111	17.856691
40.236994	1691.364408	17.861709
40.652656	1688.773329	17.866727
40.782555	1676.665777	17.871744
40.765637	1689.114045	17.876762
40.573717	1686.470430	17.881779
40.747353	1684.301003	17.886797
40.887334	1677.812509	17.891815
40.907166	1692.349493	17.896832
40.598062	1684.114912	17.901850
40.768481	1694.194901	17.906867
40.957215	1702.336281	17.911885
41.035182	1706.226733	17.916903
41.073424	1717.452584	17.921920
41.060605	1720.003083	17.926938
41.325804	1709.391963	17.931955
41.180402	1725.994856	17.936973
41.278114	1709.801566	17.941991
41.266943	1727.063416	17.947008
40.978262	1717.383027	17.952026
41.617094	1714.676907	17.957043
41.284155	1716.742037	17.962061
41.585972	1717.025071	17.967079
41.650119	1706.209269	17.972096
41.320419	1719.344556	17.977114
41.589870	1709.667178	17.982131
41.692309	1707.207855	17.987149
41.593327	1706.330158	17.992167
41.502410	1706.752913	17.997184
41.519677	1717.801991	18.002202
41.745197	1704.625188	18.007219
41.837506	1712.597900	18.012237
41.901021	1717.490364	18.017255
41.840791	1702.147365	18.022272
41.797658	1708.836794	18.027290
41.955930	1697.989469	18.032307
41.480833	1716.319496	18.037325
41.619679	1707.864798	18.042343
41.473866	1718.943819	18.047360
41.619566	1740.664781	18.052378
42.076875	1722.917317	18.057395
41.910967	1746.005457	18.062413
41.787400	1740.585419	18.067431
42.127762	1732.863878	18.072448
42.032686	1743.275697	18.077466
42.479056	1734.730246	18.082483
42.380059	1748.623965	18.087501
42.429243	1737.125441	18.092519
42.379040	1728.713468	18.097536
42.328509	1745.382266	18.102554
42.581967	1736.586785	18.107571
42.102992	1757.102518	18.112589
42.150774	1764.936849	18.117607
42.627551	1768.089634	18.122624
42.718228	1767.473495	18.127642
43.005747	1770.987605	18.132659
43.055047	1766.689138	18.137677
43.141836	1765.819563	18.142695
43.112853	1760.901195	18.147712
42.839711	1774.379885	18.152730
43.200584	1751.564283	18.157747
43.356371	1754.319142	18.162765
43.029234	1737.751541	18.167783
42.840973	1735.705898	18.172800
42.886184	1730.228268	18.177818
42.994081	1758.833665	18.182835
43.183180	1759.052877	18.187853
43.271739	1765.334345	18.192871
43.315214	1764.944396	18.197888
43.403942	1768.511449	18.202906
43.272894	1768.278329	18.207923
43.205672	1765.986063	18.212941
43.318038	1763.238056	18.217959
43.677991	1759.028476	18.222976
43.332864	1762.342240	18.227994
43.882168	1761.321813	18.233011
43.664003	1760.332555	18.238029
43.606481	1763.009748	18.243047
43.350503	1755.396680	18.248064
43.368474	1764.150525	18.253082
43.606512	1762.741635	18.258099
43.852961	1765.798229	18.263117
43.497002	1754.794554	18.268135
43.676724	1761.847245	18.273152
43.534141	1766.799340	18.278170
43.382582	1757.081323	18.283187
43.593520	1777.066241	18.288205
44.061580	1778.685070	18.293223
44.259463	1771.742110	18.298240
44.177102	1789.929362	18.303258
44.214906	1780.923632	18.308275
44.533881	1790.867517	18.313293
44.263580	1781.598667	18.318311
44.703638	1791.229856	18.323328
44.551400	1792.372651	18.328346
44.523508	1769.821958	18.333363
44.455393	1760.277829	18.338381
44.295321	1768.371840	18.343399
44.718088	1761.182222	18.348416
44.312793	1773.300018	18.353434
44.361863	1777.954908	18.358451
44.450764	1778.802825	18.363469
44.346346	1781.242096	18.368487
44.764612	1790.704505	18.373504
44.400035	1781.692950	18.378522
44.847532	1772.678513	18.383539
44.674385	1783.375746	18.388557
44.335325	1786.098633	18.393575
44.728428	1778.372589	18.398592
44.560639	1793.243995	18.403610
45.003760	1808.070677	18.408627
45.229026	1812.496118	18.413645
45.082287	1815.138783	18.418663
45.209255	1814.852712	18.423680
45.116837	1811.400357	18.428698
45.157891	1817.138050	18.433715
45.474209	1818.818054	18.438733
45.132448	1819.484538	18.443751
45.469600	1814.182122	18.448768
45.175094	1818.229545	18.453786
44.951715	1812.845062	18.458803
45.100297	1810.539606	18.463821
44.976645	1821.224253	18.468839
45.161000	1810.196496	18.473856
45.123092	1823.717941	18.478874
45.333613	1823.443714	18.483891
45.570215	1845.112579	18.488909
45.460094	1838.981672	18.493927
45.987342	1839.434831	18.498944
45.778632	1837.635480	18.503962
45.939619	1846.036210	18.508979
46.024123	1837.568080	18.513997
45.692022	1828.512775	18.519015
45.885240	1839.704563	18.524032
45.791502	1837.023237	18.529050
45.861025	1841.419255	18.534067
45.744871	1839.512328	18.539085
45.705554	1855.167952	18.544103
46.214782	1834.986333	18.549120
46.002658	1860.484952	18.554138
46.418686	1861.054957	18.559155
46.590415	1866.703397	18.564173
46.657176	1856.846667	18.569191
46.528007	1835.325110	18.574208
46.024510	1843.805078	18.579226
46.440003	1856.248233	18.584243
46.671359	1863.742648	18.589261
46.429945	1867.242039	18.594279
46.810099	1861.939040	18.599296
46.534241	1874.602595	18.604314
46.519363	1870.439396	18.609331
46.838719	1871.208875	18.614349
46.344626	1875.272415	18.619367
46.823324	1864.475326	18.624384
46.292960	1873.098029	18.629402
46.444694	1869.708185	18.634419
47.036526	1871.877538	18.639437
47.130294	1886.249545	18.644455
47.186012	1886.979272	18.649472
47.257969	1875.396778	18.654490
47.074894	1869.172882	18.659507
47.429519	1876.737311	18.664525
47.514054	1871.910919	18.669543
47.511197	1855.679235	18.674560
47.714492	1852.837267	18.679578
47.753759	1846.533084	18.684595
47.917158	1854.971190	18.689613
47.623037	1860.885848	18.694631
47.766208	1850.803777	18.699648
47.808981	1847.793919	18.704666
47.386446	1852.830022	18.709683
47.860318	1848.121662	18.714701
47.777734	1858.039186	18.719719
47.605829	1848.410087	18.724736
47.587355	1863.214488	18.729754
47.225567	1854.881241	18.734771
47.847292	1840.035762	18.739789
47.724316	1849.692294	18.744807
47.689640	1857.086770	18.749824
47.669352	1852.513856	18.754842
47.742907	1868.012272	18.759859
48.042772	1876.191870	18.764877
48.064735	1882.585477	18.769895
48.478900	1871.237073	18.774912
48.371909	1870.194680	18.779930
48.443689	1879.778482	18.784947
48.358020	1883.305735	18.789965
48.175622	1882.198285	18.794983
48.248547	1875.296444	18.800000
48.218731	1886.389340	18.805018
47.735529	1875.173047	18.810035
48.175989	1881.755536	18.815053
48.279798	1871.081946	18.820071
48.559860	1887.143656	18.825088
48.648455	1894.605011	18.830106
48.805277	1897.029378	18.835123
49.092489	1896.112098	18.840141
48.604010	1915.013189	18.845159
48.887650	1903.527480	18.850176
48.951327	1898.344948	18.855194
48.870451	1908.131665	18.860211
48.937073	1898.487300	18.865229
49.057481	1897.083787	18.870247
49.151034	1900.720894	18.875264
49.171225	1903.653934	18.880282
49.078213	1908.473107	18.885299
48.951713	1903.799134	18.890317
48.858727	1907.349583	18.895335
49.097092	1901.771865	18.900352
49.463761	1898.472796	18.905370
49.383436	1907.423313	18.910387
49.456997	1900.788002	18.915405
49.377309	1906.316099	18.920423
49.528611	1920.793802	18.925440
49.315529	1931.755504	18.930458
49.580200	1936.720571	18.935475
49.703819	1931.681846	18.940493
49.561383	1938.860729	18.945511
49.772256	1928.228227	18.950528
49.980006	1939.538905	18.955546
49.687124	1941.111582	18.960563
49.965758	1932.296237	18.965581
49.640545	1934.915476	18.970599
49.612838	1931.749304	18.975616
50.015833	1938.562752	18.980634
50.007784	1951.093205	18.985651
50.210239	1949.529515	18.990669
50.112528	1968.843434	18.995687
50.276645	1967.593403	19.000704
50.161266	1970.651905	19.005722
50.187756	1959.124577	19.010739
50.480253	1956.350950	19.015757
50.186297	1963.236241	19.020775
50.452805	1966.649138	19.025792
50.498267	1964.482809	19.030810
50.423558	1964.924223	19.035827
50.939063	1953.696454	19.040845
50.669302	1964.487098	19.045863
50.490694	1958.861025	19.050880
50.479198	1956.947615	19.055898
50.730043	1960.738200	19.060915
50.947224	1955.302275	19.065933
50.635284	1961.163183	19.070951
51.269836	1966.242311	19.075968
51.254091	1964.619819	19.080986
50.921458	1979.704908	19.086003
51.224295	1961.266021	19.091021
51.104652	1985.536444	19.096039
51.272284	1969.127995	19.101056
51.700770	1971.745015	19.106074
51.317167	1980.467077	19.111091
51.184657	1971.374341	19.116109
51.170447	1978.489531	19.121127
51.092729	1974.885346	19.126144
51.327356	1984.812142	19.131162
51.457961	1979.023478	19.136179
51.601680	1976.722705	19.141197
51.427856	1979.825925	19.146215
51.506243	1978.172688	19.151232
51.662834	1976.035826	19.156250
51.510053	1984.134300	19.161267
51.847046	2002.453933	19.166285
51.717042	2014.148110	19.171303
51.560812	2013.949678	19.176320
52.007405	2003.885181	19.181338
51.841348	2007.512593	19.186355
52.230885	2011.370739	19.191373
51.558274	2012.992975	19.196391
51.788089	2014.231378	19.201408
52.467297	2016.808418	19.206426
52.209374	2030.555495	19.211443
52.646150	2036.596699	19.216461
52.334355	2041.001681	19.221479
52.506553	2047.180263	19.226496
52.683249	2036.710446	19.231514
52.465348	2042.673586	19.236531
52.492294	2036.602537	19.241549
52.730376	2031.463719	19.246567
52.641301	2036.460071	19.251584
52.837761	2034.151663	19.256602
52.800187	2032.412301	19.261619
52.767977	2034.839311	19.266637
52.839147	2030.600203	19.271655
52.799728	2029.198572	19.276672
52.909160	2025.991630	19.281690
52.744184	2032.896496	19.286707
52.884671	2033.035371	19.291725
52.815631	2031.032022	19.296743
52.715672	2035.309615	19.301760
53.307983	2057.693686	19.306778
53.207500	2059.076802	19.311795
53.137884	2061.631700	19.316813
53.322199	2058.058065	19.321831
53.316301	2058.726050	19.326848
53.196993	2057.899554	19.331866
53.104413	2065.746995	19.336883
53.581298	2065.110149	19.341901
53.464826	2061.216373	19.346919
53.752644	2072.918681	19.351936
54.002117	2081.256668	19.356954
53.963534	2093.338263	19.361971
53.891960	2076.733447	19.366989
53.920753	2082.613996	19.372007
54.031839	2083.049378	19.377024
54.030733	2075.226379	19.382042
53.919258	2085.886467	19.387059
54.373596	2078.849760	19.392077
54.426545	2087.468436	19.397095
54.017937	2087.352730	19.402112
54.348132	2079.101696	19.407130
54.541210	2088.068497	19.412147
54.364500	2078.330679	19.417165
54.303574	2093.533010	19.422183
54.277712	2080.195388	19.427200
54.343627	2082.690131	19.432218
54.155105	2079.785547	19.437235
54.295657	2082.286477	19.442253
54.569091	2078.906278	19.447271
54.232929	2106.703013	19.452288
54.833100	2106.125158	19.457306
55.031894	2116.266201	19.462323
54.941425	2115.996713	19.467341
54.856549	2104.793794	19.472359
54.962429	2119.263994	19.477376
55.026345	2102.659563	19.482394
54.662085	2115.250903	19.487411
54.892214	2097.583269	19.492429
55.029168	2103.078461	19.497447
55.240386	2112.834460	19.502464
55.469209	2116.815015	19.507482
55.318873	2122.431545	19.512499
55.610147	2121.528550	19.517517
55.559515	2128.510399	19.522535
55.290893	2124.036786	19.527552
55.515393	2133.338402	19.532570
55.734803	2136.830430	19.537587
55.976187	2134.074362	19.542605
56.139769	2134.874994	19.547623
55.799132	2122.731999	19.552640
55.814070	2115.186439	19.557658
55.853129	2110.430146	19.562675
55.913492	2126.255794	19.567693
55.841009	2128.236177	19.572711
55.981559	2136.890466	19.577728
56.138103	2129.915388	19.582746
55.842612	2136.649195	19.587763
56.095852	2138.056920	19.592781
56.173269	2132.959423	19.597799
55.929703	2137.235566	19.602816
56.218449	2136.475341	19.607834
56.003786	2136.295666	19.612851
56.313344	2147.028657	19.617869
56.463291	2169.719426	19.622887
56.386000	2166.690896	19.627904
56.851779	2157.084166	19.632922
56.599725	2152.090337	19.637939
56.837450	2172.089618	19.642957
56.834945	2166.387396	19.647975
56.778625	2163.545873	19.652992
56.959947	2168.203392	19.658010
56.963014	2165.121144	19.663027
57.023300	2156.477354	19.668045
56.905882	2160.159186	19.673063
56.871448	2163.494276	19.678080
57.162556	2146.867718	19.683098
56.809594	2159.541458	19.688115
57.257159	2176.302779	19.693133
57.353126	2177.521643	19.698151
57.250474	2185.873375	19.703168
57.421417	2185.359258	19.708186
57.660911	2181.783086	19.713203
57.380906	2182.257248	19.718221
57.877534	2182.462816	19.723239
57.280915	2186.914841	19.728256
58.163072	2185.676910	19.733274
57.822505	2180.796296	19.738291
57.467599	2192.723915	19.743309
58.074420	2179.634534	19.748327
57.755212	2182.958415	19.753344
57.821012	2183.172129	19.758362
57.733152	2203.531718	19.763379
58.234276	2205.532321	19.768397
58.134408	2203.519706	19.773415
58.151958	2220.290669	19.778432
58.348456	2201.955750	19.783450
58.267064	2213.744587	19.788467
58.296479	2216.227084	19.793485
58.519018	2212.525397	19.798503
58.778690	2217.717893	19.803520
58.584115	2210.452684	19.808538
58.993773	2210.899444	19.813555
58.559607	2205.230656	19.818573
58.743672	2209.423672	19.823591
58.470523	2211.801042	19.828608
58.955231	2203.026606	19.833626
58.894176	2202.442515	19.838643
58.590436	2208.142537	19.843661
58.885996	2198.297067	19.848679
58.595855	2219.042897	19.853696
59.075197	2218.400934	19.858714
59.471489	2223.120935	19.863731
59.694898	2220.564362	19.868749
59.572001	2221.479909	19.873767
59.124754	2211.041048	19.878784
59.187685	2215.601838	19.883802
59.786206	2215.098969	19.888819
59.487317	2233.116797	19.893837
59.855261	2216.864115	19.898855
59.483934	2219.243772	19.903872
59.199799	2227.201295	19.908890
59.689722	2222.822979	19.913907
59.647400	2227.045814	19.918925
59.728134	2224.301980	19.923943
59.366075	2227.392799	19.928960
59.709809	2225.694067	19.933978
59.977324	2246.051311	19.938995
60.228721	2240.428125	19.944013
60.380841	2243.852253	19.949031
60.416601	2251.473242	19.954048
60.555668	2252.546014	19.959066
60.229126	2252.221358	19.964083
60.285056	2251.409377	19.969101
60.081914	2243.597273	19.974119
60.232874	2251.237644	19.979136
60.614967	2240.596486	19.984154
60.612765	2254.103196	19.989171
60.358257	2255.276495	19.994189
60.669713	2243.479319	19.999207
60.611265	2254.924729	20.004224
60.757565	2256.104109	20.009242
60.825378	2263.104101	20.014259
60.743037	2272.640377	20.019277
61.207654	2262.358093	20.024295
61.304408	2274.680971	20.029312
61.375759	2270.175115	20.034330
61.612020	2269.048844	20.039347
61.350826	2266.825977	20.044365
61.460402	2262.181094	20.049383
61.703696	2268.840044	20.054400
61.790872	2260.024362	20.059418
61.752149	2255.105807	20.064435
61.432332	2248.275080	20.069453
61.913470	2226.487279	20.074471
61.685690	2242.480142	20.079488
61.727885	2232.973956	20.084506
61.612924	2241.532194	20.089523
61.680616	2253.633942	20.094541
62.047613	2254.806440	20.099559
62.181221	2265.383522	20.104576
61.976995	2273.963095	20.109594
62.070468	2262.982528	20.114611
61.953477	2258.634926	20.119629
62.278507	2261.928440	20.124647
62.237826	2263.663863	20.129664
62.182280	2259.646262	20.134682
62.288338	2255.416470	20.139699
62.220943	2257.058617	20.144717
62.299335	2262.782665	20.149735
62.337199	2264.758053	20.154752
62.501586	2259.433478	20.159770
62.496543	2271.099278	20.164787
62.704624	2288.086131	20.169805
62.620554	2289.176402	20.174823
62.584369	2297.623000	20.179840
62.783633	2302.153421	20.184858
62.947955	2287.093343	20.189875
62.942842	2301.323428	20.194893
62.844607	2294.370816	20.199911
62.879606	2299.458376	20.204928
62.705411	2295.726340	20.209946
62.974000	2309.548594	20.214963
63.152136	2322.733212	20.219981
63.519229	2316.391487	20.224999
63.381105	2320.702780	20.230016
63.288506	2318.733826	20.235034
63.144589	2320.759451	20.240051
63.178101	2323.180745	20.245069
63.604237	2340.482124	20.250087
63.936697	2349.735985	20.255104
63.881254	2360.314184	20.260122
64.088879	2357.096228	20.265139
63.713048	2365.052718	20.270157
63.940186	2350.710146	20.275175
63.857554	2363.144300	20.280192
63.779613	2356.176623	20.285210
63.885441	2347.378365	20.290227
64.027129	2360.468147	20.295245
63.936660	2372.482737	20.300263
64.282432	2370.174062	20.305280
64.083999	2373.658063	20.310298
64.417217	2376.848042	20.315315
64.322244	2383.392665	20.320333
64.429760	2368.349429	20.325351
64.604020	2382.493565	20.330368
64.695446	2400.435189	20.335386
65.143193	2396.064337	20.340403
65.133059	2406.835923	20.345421
65.170049	2401.531615	20.350439
65.269419	2395.143671	20.355456
65.338041	2387.398268	20.360474
65.052533	2372.829094	20.365491
64.823413	2379.778962	20.370509
65.308428	2387.786951	20.375527
65.302269	2401.142617	20.380544
65.266012	2404.779316	20.385562
65.449266	2401.608500	20.390579
65.319861	2405.000482	20.395597
65.449595	2400.552920	20.400615
65.439898	2394.681854	20.405632
65.259615	2394.021593	20.410650
65.463150	2395.774716	20.415667
65.563026	2409.519357	20.420685
65.603305	2421.360537	20.425703
65.806716	2423.302464	20.430720
65.647424	2433.865815	20.435738
66.054578	2428.305028	20.440755
66.108122	2433.569806	20.445773
66.101891	2428.594883	20.450791
66.355666	2431.680343	20.455808
66.286311	2422.765247	20.460826
66.424139	2428.184124	20.465843
66.261112	2425.965240	20.470861
66.280196	2419.515365	20.475879
66.837451	2439.785767	20.480896
66.986221	2460.591727	20.485914
67.082021	2442.403927	20.490931
66.946221	2429.664807	20.495949
66.770154	2426.302732	20.500967
67.076648	2426.964174	20.505984
66.842589	2425.410272	20.511002
67.033831	2437.187272	20.516019
67.121419	2449.881457	20.521037
67.287032	2453.774650	20.526055
67.178114	2460.544922	20.531072
66.765766	2457.430542	20.536090
67.115800	2449.903732	20.541107
67.086806	2443.764350	20.546125
66.735427	2444.165738	20.551143
67.041485	2466.386863	20.556160
67.096019	2478.759123	20.561178
67.406590	2480.621827	20.566195
67.367203	2488.999826	20.571213
67.486771	2498.728226	20.576231
67.912079	2511.158582	20.581248
67.730902	2510.618807	20.586266
67.903440	2497.872141	20.591283
68.080331	2511.725731	20.596301
67.872105	2507.909396	20.601319
67.968180	2511.434558	20.606336
67.880830	2511.343121	20.611354
68.429459	2521.336622	20.616371
68.529198	2537.752674	20.621389
68.495739	2533.460887	20.626407
69.078188	2535.244055	20.631424
68.356958	2537.865201	20.636442
68.526567	2533.246056	20.641459
68.384496	2534.924528	20.646477
68.520850	2540.121863	20.651495
68.690251	2539.505723	20.656512
68.913054	2542.809313	20.661530
69.012573	2541.117246	20.666547
68.699963	2543.010127	20.671565
68.773448	2541.422109	20.676583
68.944482	2545.709332	20.681600
69.240348	2568.629948	20.686618
69.445232	2568.348743	20.691635
69.475398	2567.237228	20.696653
69.581919	2567.230501	20.701671
69.690910	2562.253674	20.706688
69.549107	2567.211420	20.711706
69.704452	2560.847514	20.716723
69.566656	2567.111941	20.721741
69.577846	2562.787067	20.726759
69.893116	2559.996326	20.731776
69.260957	2565.350060	20.736794
69.492746	2566.103656	20.741811
69.712802	2580.946257	20.746829
69.704736	2591.044323	20.751847
70.098925	2592.852803	20.756864
69.987610	2603.252092	20.761882
70.182699	2580.930451	20.766899
70.178479	2596.266635	20.771917
70.435493	2612.897600	20.776935
70.789577	2618.920776	20.781952
70.770200	2622.797108	20.786970
70.579568	2621.823848	20.791987
70.886148	2622.369656	20.797005
70.784591	2615.522824	20.802023
70.946951	2619.433886	20.807040
70.810280	2616.613742	20.812058
71.196194	2613.753516	20.817075
71.300048	2620.248442	20.822093
71.158391	2620.064981	20.827111
71.289395	2616.160691	20.832128
71.074205	2622.888992	20.837146
71.154227	2617.546279	20.842163
71.168277	2617.495305	20.847181
71.222426	2614.470103	20.852199
71.612023	2626.930639	20.857216
71.600476	2645.992585	20.862234
71.697494	2641.945042	20.867251
71.891114	2643.982953	20.872269
71.491889	2654.157605	20.877287
71.960037	2639.810923	20.882304
71.715643	2652.673861	20.887322
71.905412	2638.415627	20.892339
71.648776	2637.861137	20.897357
71.873704	2661.311580	20.902375
72.239129	2666.139695	20.907392
72.175041	2676.287658	20.912410
72.346714	2674.696552	20.917427
72.450446	2678.920608	20.922445
72.025840	2684.517379	20.927463
72.379292	2671.832169	20.932480
72.185440	2679.423140	20.937498
72.537102	2691.581434	20.942515
72.655908	2701.243229	20.947533
72.783563	2706.102985	20.952551
72.932593	2698.248629	20.957568
73.120057	2705.928254	20.962586
72.915801	2708.380454	20.967603
72.978479	2694.893640	20.972621
72.848400	2706.671761	20.977639
73.428591	2692.234006	20.982656
73.234504	2697.719291	20.987674
73.464266	2697.866748	20.992691
73.368082	2709.925002	20.997709
73.443849	2723.325319	21.002727
73.466032	2722.016842	21.007744
73.315787	2740.988548	21.012762
73.471555	2727.844762	21.017779
73.681231	2730.148357	21.022797
73.495281	2736.827210	21.027815
74.166473	2755.410709	21.032832
74.237170	2750.674334	21.037850
74.403792	2760.428442	21.042867
74.381355	2760.334517	21.047885
74.213338	2752.136606	21.052903
74.526236	2752.958298	21.057920
74.336066	2764.799538	21.062938
74.328644	2756.709735	21.067955
74.586093	2760.400367	21.072973
74.655368	2761.507906	21.077991
74.876735	2748.559731	21.083008
74.911930	2752.124552	21.088026
74.575137	2747.606554	21.093043
74.635096	2751.763672	21.098061
74.834193	2757.805331	21.103079
74.914009	2760.154812	21.108096
74.783241	2777.890849	21.113114
75.204877	2777.479107	21.118131
75.564671	2773.641333	21.123149
75.345016	2773.600099	21.128167
75.446171	2764.519158	21.133184
75.474222	2778.908819	21.138202
75.554957	2773.718538	21.143219
75.916881	2774.031344	21.148237
75.567057	2784.335863	21.153255
76.014651	2769.186849	21.158272
75.615847	2783.620993	21.163290
75.853002	2794.703466	21.168307
76.125982	2787.162029	21.173325
76.019991	2798.093926	21.178343
76.458416	2796.838623	21.183360
76.259855	2788.195624	21.188378
76.461370	2793.034977	21.193395
76.458079	2792.209600	21.198413
76.104019	2795.405451	21.203431
76.576733	2792.607650	21.208448
76.342064	2794.410256	21.213466
76.389781	2787.610332	21.218483
76.750013	2792.949826	21.223501
76.570713	2820.283969	21.228519
76.798888	2819.156589	21.233536
76.756510	2823.455905	21.238554
76.703927	2827.234542	21.243571
77.147164	2826.070503	21.248589
77.006609	2822.977984	21.253607
77.141647	2820.347303	21.258624
77.236720	2831.549216	21.263642
76.974453	2843.198286	21.268659
77.465801	2855.205436	21.273677
77.098459	2849.012865	21.278695
77.331497	2858.959392	21.283712
77.382430	2859.582166	21.288730
77.256581	2880.928872	21.293747
77.659298	2872.308709	21.298765
77.460955	2895.299216	21.303783
77.898148	2883.624638	21.308800
77.995573	2891.262871	21.313818
77.998838	2891.569164	21.318835
78.620345	2896.944116	21.323853
78.738436	2916.304318	21.328871
78.565889	2895.289186	21.333888
78.966995	2895.263797	21.338906
78.898670	2886.006864	21.343923
78.914726	2884.146361	21.348941
78.335734	2885.107154	21.353959
78.899320	2874.964411	21.358976
78.718512	2902.120387	21.363994
78.873448	2907.458840	21.369011
79.702327	2901.099857	21.374029
79.788189	2904.128817	21.379047
79.412775	2889.254885	21.384064
79.588876	2876.050302	21.389082
79.217629	2875.765795	21.394099
79.615455	2862.270214	21.399117
79.428622	2886.259440	21.404135
79.855697	2882.546992	21.409152
79.710093	2888.329821	21.414170
79.763124	2900.529624	21.419187
79.912390	2892.328230	21.424205
79.504982	2897.651744	21.429223
79.735755	2896.284027	21.434240
79.816793	2895.556894	21.439258
79.659945	2888.867421	21.444275
79.882148	2902.943848	21.449293
80.110118	2913.200359	21.454311
80.163894	2921.812317	21.459328
80.389666	2929.252327	21.464346
80.283053	2918.989893	21.469363
80.701654	2926.891569	21.474381
80.637114	2929.112283	21.479399
80.529224	2933.079902	21.484416
80.498610	2928.161400	21.489434
80.470644	2931.524739	21.494451
80.647162	2944.740069	21.499469
80.575845	2951.081372	21.504487
81.022156	2952.656615	21.509504
81.015464	2945.918784	21.514522
80.654349	2957.324912	21.519539
80.977017	2970.416270	21.524557
81.316202	2987.991085	21.529575
81.262643	2988.328468	21.534592
81.303904	2999.919029	21.539610
81.137590	2996.503348	21.544627
81.842557	3002.086856	21.549645
81.676955	3013.575907	21.554663
81.860916	3010.598357	21.559680
82.288427	3012.385060	21.564698
81.923777	3018.077801	21.569715
82.230086	3010.466432	21.574733
82.078247	3020.774152	21.579751
81.775191	3027.817138	21.584768
82.059178	3020.829967	21.589786
82.214700	3033.892189	21.594803
82.702956	3039.548031	21.599821
82.425843	3052.773661	21.604839
82.387250	3050.106127	21.609856
82.918695	3044.424602	21.614874
82.681870	3059.314595	21.619891
82.551938	3048.724621	21.624909
82.779435	3058.474727	21.629927
83.138869	3073.656661	21.634944
83.108191	3066.375110	21.639962
83.041342	3073.322238	21.644979
83.106374	3077.175790	21.649997
83.140839	3079.391750	21.655015
83.326571	3083.570595	21.660032
83.293383	3077.632204	21.665050
83.280351	3113.697059	21.670067
83.505369	3105.075209	21.675085
83.707314	3117.887822	21.680103
83.326159	3115.382675	21.685120
83.737930	3121.353598	21.690138
83.761600	3131.318755	21.695155
83.942870	3134.882399	21.700173
83.961788	3134.833006	21.705191
84.279183	3141.172182	21.710208
84.602533	3126.192863	21.715226
84.547465	3141.110589	21.720243
84.957374	3130.233086	21.725261
85.091788	3134.708035	21.730279
84.897374	3124.679715	21.735296
84.989195	3130.980918	21.740314
85.050754	3127.802610	21.745331
85.142933	3126.185590	21.750349
85.223484	3124.970817	21.755367
85.207918	3125.530265	21.760384
85.219362	3128.199853	21.765402
84.911225	3125.716098	21.770419
85.207235	3132.489751	21.775437
85.258653	3145.908498	21.780455
85.677405	3147.458268	21.785472
85.825212	3153.773365	21.790490
85.650807	3160.149290	21.795507
85.759052	3158.779851	21.800525
85.802047	3160.369882	21.805543
85.687661	3155.729757	21.810560
85.877804	3156.918740	21.815578
85.619125	3164.336227	21.820595
85.876332	3178.264171	21.825613
85.897159	3185.161184	21.830631
85.954203	3194.972390	21.835648
86.005537	3186.385270	21.840666
86.022594	3203.913389	21.845683
86.393116	3212.145406	21.850701
86.575910	3217.092509	21.855719
86.875319	3226.101266	21.860736
86.884331	3210.322430	21.865754
86.942615	3209.649255	21.870771
86.976518	3211.489317	21.875789
87.572814	3221.928014	21.880807
87.417852	3220.974195	21.885824
87.421502	3213.320528	21.890842
87.500538	3236.537147	21.895859
87.651761	3226.613321	21.900877
87.699223	3236.190093	21.905895
87.737690	3240.951764	21.910912
87.856660	3235.631720	21.915930
87.570811	3249.781638	21.920947
87.808457	3238.022183	21.925965
88.012252	3239.433185	21.930983
87.721526	3246.217867	21.936000
87.998706	3224.971640	21.941018
87.920403	3250.498535	21.946035
88.152108	3253.888972	21.951053
88.188321	3271.903403	21.956071
88.103243	3276.956176	21.961088
88.543721	3264.044974	21.966106
88.439325	3271.315983	21.971123
88.418517	3290.882904	21.976141
88.508477	3291.401930	21.981159
88.455283	3291.180752	21.986176
88.685038	3295.067876	21.991194
88.772416	3315.482873	21.996211
89.353527	3319.430393	22.001229
89.216577	3330.529670	22.006247
89.165224	3331.208108	22.011264
89.391745	3319.094017	22.016282
89.318977	3330.087089	22.021299
89.437342	3323.226091	22.026317
89.762961	3338.026669	22.031335
89.558710	3337.973534	22.036352
90.053360	3346.278655	22.041370
90.017586	3359.010609	22.046387
90.395218	3349.109591	22.051405
90.539424	3348.593408	22.056423
90.363385	3359.894813	22.061440
90.239256	3346.647224	22.066458
90.398019	3346.208956	22.071475
90.458608	3343.275401	22.076493
90.617042	3347.022879	22.081511
90.194363	3355.759061	22.086528
90.585402	3353.827685	22.091546
90.600983	3346.540191	22.096563
90.589562	3354.343912	22.101581
91.075841	3363.041337	22.106599
90.928411	3374.032189	22.111616
91.339132	3379.169550	22.116634
91.024198	3368.518384	22.121651
91.040314	3375.176314	22.126669
91.370200	3371.222802	22.131687
91.393561	3405.021772	22.136704
91.574894	3399.898611	22.141722
91.658291	3406.674834	22.146739
91.724860	3408.208427	22.151757
91.984473	3404.981956	22.156775
92.086360	3403.418422	22.161792
92.258783	3405.647830	22.166810
92.252115	3405.019616	22.171827
92.316202	3407.853921	22.176845
92.249360	3403.718238	22.181863
92.048553	3408.276623	22.186880
92.836050	3419.245846	22.191898
92.358478	3437.366015	22.196915
92.376523	3432.493076	22.201933
93.039221	3424.745995	22.206951
92.884279	3439.737377	22.211968
93.246074	3424.333131	22.216986
93.267828	3426.138971	22.222003
93.046096	3425.509655	22.227021
93.074330	3418.726705	22.232039
92.985790	3443.775717	22.237056
93.678900	3439.141242	22.242074
93.552282	3444.416237	22.247091
93.674646	3446.257953	22.252109
94.232897	3440.608190	22.257127
93.659694	3442.530939	22.262144
93.893749	3439.916610	22.267162
94.275458	3447.218740	22.272179
93.914948	3445.359221	22.277197
94.048216	3446.664282	22.282215
93.982063	3453.779820	22.287232
94.383798	3472.547234	22.292250
94.526624	3469.210364	22.297267
94.307288	3479.703803	22.302285
94.786112	3481.273924	22.307303
94.549726	3479.481923	22.312320
94.384554	3477.999517	22.317338
94.445682	3477.940245	22.322355
94.550261	3498.123054	22.327373
94.977318	3506.809558	22.332391
94.611351	3504.606350	22.337408
94.599852	3517.445487	22.342426
95.057096	3536.959312	22.347443
94.536698	3546.174524	22.352461
95.471193	3538.567329	22.357479
95.191466	3542.188072	22.362496
95.741235	3562.924571	22.367514
95.937381	3561.189446	22.372531
96.059564	3564.538425	22.377549
96.019707	3568.699107	22.382567
95.800797	3572.396689	22.387584
96.092927	3562.952834	22.392602
96.168966	3566.125882	22.397619
95.811331	3580.805966	22.402637
96.551150	3591.498944	22.407655
96.655227	3595.229982	22.412672
96.554422	3608.117266	22.417690
96.772321	3604.166605	22.422707
96.563742	3605.735446	22.427725
97.014192	3607.270773	22.432743
96.723832	3603.632442	22.437760
96.950044	3628.895890	22.442778
97.365976	3631.085712	22.447795
97.377279	3631.511884	22.452813
97.820298	3632.012379	22.457831
97.745826	3627.134462	22.462848
97.771147	3629.684718	22.467866
97.970901	3622.488075	22.472883
97.539137	3630.197713	22.477901
97.670233	3626.193237	22.482919
97.556160	3634.589307	22.487936
98.018778	3645.975519	22.492954
98.232120	3647.702848	22.497971
98.110357	3666.520956	22.502989
98.442439	3658.036679	22.508007
98.207496	3666.345058	22.513024
98.135820	3664.608579	22.518042
98.502104	3671.936882	22.523059
98.693284	3693.718004	22.528077
98.867972	3676.543466	22.533095
98.416937	3688.852630	22.538112
98.479651	3690.083219	22.543130
98.777502	3701.493391	22.548147
98.943005	3720.370382	22.553165
98.933736	3712.616249	22.558183
99.211406	3727.551520	22.563200
99.036445	3748.270913	22.568218
99.557188	3739.230230	22.573235
99.249743	3745.484452	22.578253
99.559221	3746.659960	22.583271
99.345201	3761.382613	22.588288
99.909541	3761.300519	22.593306
100.092242	3782.405025	22.598323
99.905002	3787.295693	22.603341
100.252854	3779.519187	22.608359
100.243290	3785.737721	22.613376
100.433628	3789.122295	22.618394
100.452681	3793.792842	22.623411
100.488954	3801.884980	22.628429
100.670414	3807.654557	22.633447
100.468703	3807.415362	22.638464
100.707454	3806.312970	22.643482
101.062952	3821.386178	22.648499
100.805797	3838.747172	22.653517
101.031565	3841.329219	22.658535
101.567434	3845.045742	22.663552
101.492712	3845.462825	22.668570
101.625199	3839.355319	22.673587
101.572276	3836.257262	22.678605
101.978161	3851.232786	22.683623
101.811419	3869.331448	22.688640
102.015732	3871.222297	22.693658
102.367422	3861.327434	22.698675
102.401159	3876.951543	22.703693
102.529273	3862.716117	22.708711
102.768945	3868.830434	22.713728
102.786952	3860.329262	22.718746
102.689694	3861.686856	22.723763
102.538632	3870.783584	22.728781
102.629771	3857.232951	22.733799
102.534425	3863.072653	22.738816
102.925076	3881.459254	22.743834
103.063320	3883.848373	22.748851
103.207929	3896.270400	22.753869
103.301815	3890.855001	22.758887
103.320602	3888.549470	22.763904
103.317070	3901.615019	22.768922
103.299229	3888.401123	22.773939
103.212143	3897.712651	22.778957
103.385888	3913.947738	22.783975
103.439826	3912.492491	22.788992
103.802212	3922.060397	22.794010
104.211425	3933.234297	22.799027
104.255932	3953.446979	22.804045
104.411254	3941.029851	22.809063
104.755751	3942.043245	22.814080
104.316595	3942.474394	22.819098
104.568866	3939.343379	22.824115
104.840891	3943.174376	22.829133
105.141898	3942.447515	22.834151
104.884764	3942.549129	22.839168
104.847206	3941.992686	22.844186
105.257552	3960.063152	22.849203
105.476280	3983.162702	22.854221
105.837136	3976.610439	22.859239
105.954164	3944.741921	22.864256
105.934500	3937.978956	22.869274
105.937323	3934.038120	22.874291
105.611852	3919.620878	22.879309
105.793431	3919.072756	22.884327
105.783372	3937.109542	22.889344
106.078593	3937.772860	22.894362
106.547948	3942.687886	22.899379
106.313661	3954.898985	22.904397
106.196934	3950.089060	22.909415
106.325636	3947.265669	22.914432
106.497109	3939.894808	22.919450
106.722005	3949.962952	22.924467
106.493476	3941.152554	22.929485
107.098505	3952.023056	22.934503
107.071797	3969.459949	22.939520
107.136831	3978.249307	22.944538
107.258783	3979.505088	22.949555
107.320014	3979.298691	22.954573
107.063624	3980.725726	22.959591
107.205980	3974.431723	22.964608
107.455200	3979.621014	22.969626
107.616389	3986.606154	22.974643
107.585955	4003.538639	22.979661
107.805415	4003.399836	22.984679
107.862476	3997.214613	22.989696
107.341238	4007.627557	22.994714
108.063258	4026.940906	22.999731
108.040369	4039.820863	23.004749
108.131786	4033.232088	23.009767
108.245191	4043.750747	23.014784
108.415710	4066.114710	23.019802
108.669672	4073.960667	23.024819
108.461118	4085.300853	23.029837
108.479167	4073.047107	23.034855
108.896846	4092.322540	23.039872
109.082372	4109.167213	23.044890
109.059941	4104.136877	23.049907
109.110682	4101.378597	23.054925
109.354523	4115.953855	23.059943
109.329818	4130.355616	23.064960
109.416808	4130.476301	23.069978
109.534961	4133.801666	23.074995
109.563710	4137.309638	23.080013
109.590493	4161.015141	23.085031
110.074798	4156.825181	23.090048
109.882694	4167.833188	23.095066
110.246539	4164.149391	23.100083
110.426879	4183.936375	23.105101
110.821291	4188.052367	23.110119
111.044294	4188.701254	23.115136
111.062270	4179.019093	23.120154
111.307127	4176.071721	23.125171
111.392430	4192.278740	23.130189
111.281821	4176.962417	23.135207
111.504401	4178.254089	23.140224
111.632260	4177.944237	23.145242
111.853668	4173.633353	23.150259
111.792069	4181.214231	23.155277
112.069270	4171.076943	23.160295
112.243945	4169.935183	23.165312
112.224881	4167.180156	23.170330
112.448422	4164.558725	23.175347
112.011201	4165.707022	23.180365
112.173329	4161.438635	23.185383
112.299395	4168.766950	23.190400
111.697279	4182.402571	23.195418
112.058669	4168.918691	23.200435
112.114086	4182.444737	23.205453
112.103811	4203.268310	23.210471
112.471493	4199.929246	23.215488
112.490371	4213.476094	23.220506
112.948182	4226.076594	23.225523
112.818053	4232.954905	23.230541
112.917683	4231.144626	23.235559
113.150312	4249.190295	23.240576
113.070576	4265.802895	23.245594
113.528613	4263.308470	23.250611
113.532164	4268.102789	23.255629
113.455632	4290.928154	23.260647
113.967517	4292.935216	23.265664
113.866204	4306.574478	23.270682
114.023053	4296.780412	23.275699
114.271986	4301.194977	23.280717
114.434405	4324.775271	23.285735
114.416076	4319.676551	23.290752
114.533465	4347.534210	23.295770
114.484140	4324.216763	23.300787
114.465884	4341.145334	23.305805
114.636310	4345.215273	23.310823
114.927198	4358.624476	23.315840
115.050487	4368.934892	23.320858
115.457669	4359.871822	23.325875
115.347526	4361.062378	23.330893
115.394523	4392.266916	23.335911
115.709817	4385.918413	23.340928
115.858570	4399.462029	23.345946
116.057052	4396.692721	23.350963
116.097674	4390.823058	23.355981
115.965964	4393.942879	23.360999
116.317813	4383.862771	23.366016
116.566639	4405.664079	23.371034
116.599453	4410.395563	23.376051
116.758015	4420.147345	23.381069
116.555333	4413.963245	23.386087
116.950573	4413.163121	23.391104
116.809663	4408.083132	23.396122
116.906669	4410.253133	23.401139
116.907490	4413.034786	23.406157
117.003122	4434.504980	23.411175
117.263949	4433.205497	23.416192
117.211517	4450.260794	23.421210
117.684907	4440.514493	23.426227
117.612384	4441.275027	23.431245
117.643535	4453.444995	23.436263
118.061129	4444.609142	23.441280
117.972311	4477.437231	23.446298
118.021275	4452.779896	23.451315
118.183982	4471.013995	23.456333
118.287006	4466.526804	23.461351
118.070793	4464.851826	23.466368
118.182277	4490.592123	23.471386
118.556181	4506.138268	23.476403
118.417210	4506.727674	23.481421
118.370686	4504.991804	23.486439
118.900445	4518.071983	23.491456
118.692908	4542.606885	23.496474
118.715108	4531.443249	23.501491
119.345977	4551.214740	23.506509
119.257870	4571.896265	23.511527
119.735426	4565.687805	23.516544
119.686554	4567.508981	23.521562
119.563352	4577.409643	23.526579
119.892405	4583.436058	23.531597
119.760205	4589.751585	23.536615
120.090654	4589.973485	23.541632
120.049568	4600.905024	23.546650
120.370191	4619.704939	23.551667
120.558498	4618.833959	23.556685
120.576559	4615.172151	23.561703
120.872624	4614.608896	23.566720
120.932076	4623.257137	23.571738
121.280332	4632.170864	23.576755
121.408778	4637.136557	23.581773
121.250030	4654.155546	23.586791
121.911401	4636.340575	23.591808
121.780038	4643.845491	23.596826
121.777449	4646.873971	23.601843
122.147055	4641.890288	23.606861
122.013778	4642.455976	23.611879
121.973140	4640.408403	23.616896
121.988486	4649.471206	23.621914
122.191616	4658.121730	23.626931
122.473082	4672.303695	23.631949
122.215541	4680.348764	23.636967
122.621403	4674.550552	23.641984
122.723950	4686.780919	23.647002
122.249957	4700.545271	23.652019
122.853557	4711.234053	23.657037
122.762574	4709.211806	23.662055
123.187880	4732.991566	23.667072
123.410854	4736.176840	23.672090
123.256721	4741.281247	23.677107
123.494574	4737.912419	23.682125
123.233242	4743.088991	23.687143
123.684019	4754.107418	23.692160
123.843966	4765.465675	23.697178
123.978985	4764.165772	23.702195
124.206733	4774.878346	23.707213
123.821508	4759.912025	23.712231
124.664507	4776.866608	23.717248
124.989919	4793.348325	23.722266
124.960516	4780.426556	23.727283
125.204373	4791.334039	23.732301
125.072174	4791.491257	23.737319
125.114516	4796.548619	23.742336
125.302895	4786.967907	23.747354
125.199579	4796.250335	23.752371
125.350041	4787.543415	23.757389
125.532494	4799.241902	23.762407
125.719729	4812.305374	23.767424
125.745315	4819.382553	23.772442
125.757242	4821.327020	23.777459
125.799609	4827.577050	23.782477
125.650072	4826.944023	23.787495
125.971049	4840.308746	23.792512
126.306190	4862.964716	23.797530
126.224778	4857.506899	23.802547
126.401071	4858.861085	23.807565
126.333634	4870.357955	23.812583
126.830694	4877.685681	23.817600
126.741115	4891.981310	23.822618
126.892606	4889.096677	23.827635
127.463998	4899.418615	23.832653
127.588807	4900.064313	23.837671
127.799234	4901.362711	23.842688
127.717305	4901.607106	23.847706
128.152906	4901.204111	23.852723
128.187377	4893.590284	23.857741
128.141214	4899.910318	23.862759
128.099182	4912.272495	23.867776
128.201655	4918.472069	23.872794
128.521221	4936.446502	23.877811
128.938770	4912.969496	23.882829
128.615515	4930.775009	23.887847
128.684065	4928.104995	23.892864
129.008813	4930.848466	23.897882
129.031778	4951.738601	23.902899
129.031058	4954.393940	23.907917
129.070193	4968.004336	23.912935
129.178310	4963.193626	23.917952
129.343040	4968.543074	23.922970
129.332896	4986.709394	23.927987
129.913145	4983.628924	23.933005
129.425988	4998.849516	23.938023
129.795724	4999.851885	23.943040
129.899681	5022.255451	23.948058
130.136392	5019.404408	23.953075
130.370586	5026.517654	23.958093
130.296140	5020.341171	23.963111
130.879299	5034.997765	23.968128
131.054128	5049.650254	23.973146
130.753489	5050.401564	23.978163
131.359435	5040.374901	23.983181
130.939687	5045.703501	23.988199
131.127796	5053.764249	23.993216
131.241855	5063.323725	23.998234
131.493123	5074.090986	24.003251
131.675299	5075.152378	24.008269
131.297292	5087.345630	24.013287
131.876348	5087.314695	24.018304
132.098663	5098.901642	24.023322
132.052118	5103.339966	24.028339
132.366532	5095.923708	24.033357
132.190727	5106.788989	24.038375
132.453813	5123.022968	24.043392
132.809609	5136.548409	24.048410
132.566190	5148.997181	24.053427
132.694057	5147.477313	24.058445
132.948117	5160.167754	24.063463
132.870265	5171.450166	24.068480
133.066207	5181.178398	24.073498
132.544212	5197.506177	24.078515
133.000063	5195.967047	24.083533
132.957498	5217.744430	24.088551
133.252674	5245.629721	24.093568
133.729202	5244.745790	24.098586
133.938211	5271.578053	24.103603
134.373570	5276.493449	24.108621
134.245441	5271.699069	24.113639
134.432470	5278.944263	24.118656
135.003472	5276.378951	24.123674
135.243494	5293.125815	24.128691
135.499614	5287.942874	24.133709
135.470917	5285.016878	24.138727
135.681762	5293.081211	24.143744
135.938151	5283.801671	24.148762
135.774121	5286.660127	24.153779
136.197800	5280.990227	24.158797
136.318369	5288.072154	24.163815
136.151105	5281.069337	24.168832
136.465643	5282.089970	24.173850
136.107991	5283.102925	24.178867
136.588076	5275.613743	24.183885
136.509687	5286.477784	24.188903
136.690683	5294.257357	24.193920
136.716648	5309.375204	24.198938
136.661457	5308.460405	24.203955
136.835275	5314.816345	24.208973
136.997985	5329.393158	24.213991
137.219698	5338.214990	24.219008
137.517254	5332.988449	24.224026
136.831638	5359.801458	24.229043
137.097233	5346.417541	24.234061
137.237875	5361.219765	24.239079
137.351006	5388.183180	24.244096
137.758354	5392.505156	24.249114
137.654505	5405.041244	24.254131
138.234051	5414.150658	24.259149
138.323584	5416.598935	24.264167
138.459656	5418.645631	24.269184
138.823410	5429.980556	24.274202
138.675717	5436.370508	24.279219
139.149035	5429.310320	24.284237
139.397319	5429.860039	24.289255
138.968312	5424.577024	24.294272
139.581713	5446.365011	24.299290
139.481854	5456.544194	24.304307
139.704344	5456.815584	24.309325
139.729650	5468.011753	24.314343
139.820564	5460.986564	24.319360
140.123019	5482.788783	24.324378
140.325010	5503.050073	24.329395
140.437714	5506.064278	24.334413
140.402280	5499.813714	24.339431
140.147464	5497.527956	24.344448
140.612927	5514.677345	24.349466
140.703832	5512.587433	24.354483
140.565526	5515.823405	24.359501
140.869524	5532.829410	24.364519
141.603035	5549.781108	24.369536
141.464420	5546.102354	24.374554
141.226446	5567.499152	24.379571
141.646750	5573.121196	24.384589
141.658313	5585.459653	24.389607
141.588925	5585.139528	24.394624
141.930988	5601.061686	24.399642
142.378721	5610.639906	24.404659
142.722515	5617.791036	24.409677
142.607469	5620.224763	24.414695
142.672278	5624.464532	24.419712
143.228886	5631.460574	24.424730
143.078107	5642.518945	24.429747
143.295165	5642.418282	24.434765
143.426864	5642.488581	24.439783
143.365831	5645.501409	24.444800
143.617330	5653.494157	24.449818
143.819931	5669.149099	24.454835
144.081815	5670.018445	24.459853
143.999101	5677.587721	24.464871
144.332944	5675.219873	24.469888
144.868506	5657.528384	24.474906
144.649970	5661.765352	24.479923
145.039268	5670.098833	24.484941
145.279774	5692.292033	24.489959
145.189266	5687.065880	24.494976
144.848128	5683.932353	24.499994
145.032653	5699.915143	24.505011
145.354958	5686.740596	24.510029
145.283117	5685.215542	24.515047
145.485598	5699.825716	24.520064
145.932942	5702.632398	24.525082
145.557428	5723.288192	24.530099
145.704133	5726.458308	24.535117
146.211046	5722.660056	24.540135
146.158165	5734.230805	24.545152
146.374510	5738.908274	24.550170
146.324562	5759.566492	24.555187
146.291493	5764.491446	24.560205
146.390325	5776.230793	24.565223
146.776558	5786.754400	24.570240
147.090082	5777.050030	24.575258
147.077768	5796.042221	24.580275
147.222674	5803.170868	24.585293
147.671608	5806.038684	24.590311
147.570703	5807.952494	24.595328
148.101639	5810.820610	24.600346
147.983035	5833.399365	24.605363
148.286901	5842.023510	24.610381
148.465897	5840.558362	24.615399
148.473690	5841.387984	24.620416
148.734825	5849.557113	24.625434
148.633072	5855.214516	24.630451
148.505197	5867.236344	24.635469
148.967228	5867.488431	24.640487
148.968570	5883.012829	24.645504
149.013708	5891.229011	24.650522
149.133572	5914.160103	24.655539
149.426982	5907.875814	24.660557
149.493007	5928.730564	24.665575
149.454763	5937.803489	24.670592
150.068235	5946.028999	24.675610
149.993432	5980.971468	24.680627
150.307742	5979.929260	24.685645
150.728911	5971.981782	24.690663
150.396728	5978.631909	24.695680
150.619300	5997.260392	24.700698
150.888118	6001.176632	24.705715
150.869540	6000.136361	24.710733
150.889623	6018.021395	24.715751
150.713534	6035.431043	24.720768
151.174042	6036.773067	24.725786
151.568442	6057.087048	24.730803
151.438252	6067.692414	24.735821
151.737272	6076.288358	24.740839
152.256464	6089.597434	24.745856
152.671752	6095.491921	24.750874
152.541356	6089.183078	24.755891
153.009047	6091.954334	24.760909
153.232606	6084.489132	24.765927
153.043070	6102.584717	24.770944
153.552601	6102.243869	24.775962
153.250150	6115.504594	24.780979
153.315545	6115.173194	24.785997
153.827334	6106.491287	24.791015
153.967300	6123.576843	24.796032
154.187759	6122.042115	24.801050
154.117082	6116.283928	24.806067
154.203760	6113.231582	24.811085
154.304783	6124.121916	24.816103
154.051498	6141.618742	24.821120
154.251101	6139.697879	24.826138
154.621216	6145.152694	24.831155
154.180490	6147.707673	24.836173
154.652489	6172.254151	24.841191
154.791053	6180.394227	24.846208
154.968150	6206.423671	24.851226
155.005386	6206.931542	24.856243
155.191675	6226.416619	24.861261
155.851804	6232.883457	24.866279
155.788675	6250.135297	24.871296
155.639495	6246.447824	24.876314
156.205864	6259.652757	24.881331
156.359071	6266.523023	24.886349
156.797399	6269.514577	24.891367
156.964134	6271.881450	24.896384
156.769352	6272.083277	24.901402
157.310045	6292.212176	24.906419
157.110233	6296.344054	24.911437
157.625297	6302.406825	24.916455
157.234969	6312.242659	24.921472
157.550463	6314.352928	24.926490
157.669732	6338.199814	24.931507
157.871712	6342.528069	24.936525
157.847495	6334.036141	24.941543
158.256886	6357.503984	24.946560
158.622703	6363.338802	24.951578
158.517150	6369.821571	24.956595
158.624793	6374.375739	24.961613
158.914141	6390.271749	24.966631
158.815633	6400.843189	24.971648
158.945222	6399.212770	24.976666
159.062337	6412.791604	24.981683
159.292494	6429.792321	24.986701
159.565280	6431.415305	24.991719
159.642137	6439.559068	24.996736
159.943801	6454.021205	25.001754
160.094282	6463.797658	25.006771
160.060904	6477.797883	25.011789
160.708263	6472.893625	25.016807
160.637896	6485.114498	25.021824
160.650790	6485.598722	25.026842
161.114438	6485.926887	25.031859
161.101715	6508.000392	25.036877
161.236243	6513.653417	25.041895
161.527224	6523.393346	25.046912
161.501297	6511.340506	25.051930
161.700273	6531.301551	25.056947
161.495952	6555.788127	25.061965
161.967861	6547.294865	25.066983
161.782011	6559.788352	25.072000
161.990789	6573.511653	25.077018
162.160809	6575.833204	25.082035
162.075452	6592.310043	25.087053
162.723220	6589.262553	25.092071
162.617791	6616.466837	25.097088
162.754933	6612.011327	25.102106
162.981148	6641.146326	25.107123
162.821549	6648.312131	25.112141
163.323896	6651.532748	25.117159
163.299364	6679.195548	25.122176
163.562977	6687.347436	25.127194
163.742017	6698.151792	25.132211
163.968188	6717.514706	25.137229
164.328873	6711.463267	25.142247
164.554281	6739.365647	25.147264
165.043495	6734.196972	25.152282
165.031959	6738.479132	25.157299
164.998137	6750.688889	25.162317
165.723353	6759.502892	25.167335
165.790144	6768.139415	25.172352
165.780561	6766.999304	25.177370
166.050152	6758.720724	25.182387
165.893212	6771.694458	25.187405
166.065097	6778.580082	25.192423
166.080124	6789.366593	25.197440
166.238576	6801.840005	25.202458
166.665682	6791.127835	25.207475
166.902312	6825.409700	25.212493
166.884359	6820.957612	25.217511
166.897037	6835.304113	25.222528
166.777809	6828.046627	25.227546
167.207668	6850.075250	25.232563
167.434471	6853.725391	25.237581
167.894036	6870.120374	25.242599
168.017023	6885.889224	25.247616
168.156947	6895.680236	25.252634
168.378250	6896.593897	25.257651
168.273707	6896.613749	25.262669
168.484612	6897.286726	25.267687
168.454537	6927.195685	25.272704
168.746591	6930.412914	25.277722
169.065584	6942.029957	25.282739
169.070038	6955.302291	25.287757
169.228153	6963.372013	25.292775
169.406131	6978.256452	25.297792
169.313507	6983.592588	25.302810
169.217244	6994.441842	25.307827
169.550097	7023.200219	25.312845
169.973932	7027.303675	25.317863
170.245547	7031.964089	25.322880
170.306747	7055.227326	25.327898
170.753105	7048.584557	25.332915
170.908107	7057.684005	25.337933
170.896687	7080.244414	25.342951
171.057437	7085.554350	25.347968
171.051804	7085.812579	25.352986
171.636956	7092.808707	25.358003
171.481013	7114.105734	25.363021
171.941563	7108.112177	25.368039
172.214220	7111.201924	25.373056
172.302525	7130.310392	25.378074
172.479421	7141.920348	25.383091
172.738030	7140.457333	25.388109
172.893520	7153.741957	25.393127
172.787029	7150.554176	25.398144
172.961097	7165.220685	25.403162
173.673233	7169.311262	25.408179
173.311093	7178.198172	25.413197
173.458091	7166.208504	25.418215
173.914580	7188.526090	25.423232
174.099253	7194.508148	25.428250
174.762400	7189.166808	25.433267
174.868324	7192.656119	25.438285
175.060389	7186.209629	25.443303
175.042158	7189.559793	25.448320
175.196410	7197.341487	25.453338
175.270185	7186.790021	25.458355
175.566979	7223.453241	25.463373
175.833358	7216.378791	25.468391
175.751960	7221.924883	25.473408
175.219351	7233.164126	25.478426
175.823940	7237.808498	25.483443
175.865860	7252.145231	25.488461
175.687579	7253.141510	25.493479
176.092256	7275.227500	25.498496
176.196749	7282.117808	25.503514
176.527982	7276.446165	25.508531
176.635236	7313.605247	25.513549
177.055971	7318.747920	25.518567
177.304581	7325.066837	25.523584
177.246453	7348.262217	25.528602
177.248919	7348.552207	25.533619
177.466585	7358.692293	25.538637
177.735019	7375.579405	25.543655
178.024572	7386.309989	25.548672
177.828509	7406.861600	25.553690
178.316560	7409.681799	25.558707
178.335382	7428.257226	25.563725
178.464849	7448.988327	25.568743
178.875958	7456.420757	25.573760
178.596580	7474.008284	25.578778
179.037713	7482.708287	25.583795
179.398627	7477.603881	25.588813
179.482177	7511.307428	25.593831
179.614957	7519.638794	25.598848
179.884590	7521.182147	25.603866
180.210044	7540.276936	25.608883
180.077124	7545.134204	25.613901
180.403990	7547.323888	25.618919
180.799923	7566.686810	25.623936
181.316369	7567.107308	25.628954
181.773165	7571.776138	25.633971
181.640503	7571.316552	25.638989
181.584867	7577.198592	25.644007
181.885340	7573.857705	25.649024
181.903606	7569.896916	25.654042
182.158868	7590.760810	25.659059
182.066452	7604.381222	25.664077
182.142256	7599.374166	25.669095
182.755447	7615.644764	25.674112
182.445012	7633.518340	25.679130
182.950018	7632.824104	25.684148
182.970157	7644.483052	25.689165
183.058431	7661.189907	25.694183
183.617048	7658.023445	25.699200
183.557281	7666.471362	25.704218
184.025331	7683.633089	25.709236
183.870600	7693.228463	25.714253
183.776934	7702.589851	25.719271
184.244213	7717.228253	25.724288
184.033306	7730.726823	25.729306
184.251733	7732.347607	25.734324
184.726755	7766.019216	25.739341
185.078760	7768.285187	25.744359
184.927647	7774.857662	25.749376
185.232083	7787.672162	25.754394
185.730690	7800.382535	25.759412
186.350011	7806.160200	25.764429
186.598984	7814.417338	25.769447
186.746215	7811.939640	25.774464
186.495593	7817.926828	25.779482
186.974465	7815.015406	25.784500
187.093462	7822.093288	25.789517
187.353422	7837.085909	25.794535
187.581674	7842.286209	25.799552
187.496003	7839.529315	25.804570
187.486531	7851.754975	25.809588
187.594702	7861.700405	25.814605
187.588543	7879.982151	25.819623
187.887458	7883.943671	25.824640
188.167999	7899.748278	25.829658
188.173692	7906.225779	25.834676
188.174210	7935.308806	25.839693
188.621109	7943.934982	25.844711
189.056391	7960.320881	25.849728
189.193463	7957.243601	25.854746
189.543705	7964.659238	25.859764
189.839171	7960.318151	25.864781
190.220634	7959.809632	25.869799
190.646015	7953.057288	25.874816
190.618914	7964.922313	25.879834
190.664868	7959.618519	25.884852
190.645895	7964.091069	25.889869
190.951247	7971.845931	25.894887
191.178989	7982.751261	25.899904
191.030103	7998.245948	25.904922
191.276614	8000.402874	25.909940
191.054811	7999.628569	25.914957
191.436218	8006.593096	25.919975
191.622410	8020.156877	25.924992
191.593284	8037.549363	25.930010
192.203352	8058.620164	25.935028
192.484688	8067.082383	25.940045
192.572011	8070.474539	25.945063
192.787844	8079.738817	25.950080
192.522699	8089.254474	25.955098
193.078157	8094.625778	25.960116
193.271555	8118.194582	25.965133
192.914128	8130.936277	25.970151
193.082350	8143.426176	25.975168
193.393772	8161.683600	25.980186
193.741263	8186.821009	25.985204
193.678131	8199.131837	25.990221
193.843587	8220.736448	25.995239
194.314096	8220.693338	26.000256
194.248383	8244.296963	26.005274
194.591705	8262.218141	26.010292
195.069378	8271.015080	26.015309
194.946022	8295.814619	26.020327
195.393752	8304.448349	26.025344
195.372440	8325.998691	26.030362
195.628682	8330.652525	26.035380
196.177525	8353.451705	26.040397
196.429771	8355.548358	26.045415
196.746846	8370.175155	26.050432
196.732464	8387.379201	26.055450
196.947018	8391.208336	26.060468
197.420236	8394.462319	26.065485
197.666112	8413.597277	26.070503
197.692317	8418.530575	26.075520
197.937118	8426.989774	26.080538
198.022762	8423.086477	26.085556
198.308752	8436.823191	26.090573
198.124310	8455.721490	26.095591
198.765771	8455.118390	26.100608
198.644150	8472.361663	26.105626
198.879800	8477.459102	26.110644
199.214443	8487.629310	26.115661
199.403799	8501.337816	26.120679
199.690144	8507.157829	26.125696
199.607766	8519.089550	26.130714
199.885850	8528.812789	26.135732
200.267612	8536.509730	26.140749
200.134660	8549.999362	26.145767
200.427223	8557.475249	26.150784
200.254079	8583.866078	26.155802
200.399347	8596.690912	26.160820
201.104457	8598.119312	26.165837
201.058504	8617.624088	26.170855
201.190928	8620.375710	26.175872
201.602683	8640.477603	26.180890
201.751493	8651.630114	26.185908
201.907416	8665.543978	26.190925
202.040555	8680.751642	26.195943
202.548945	8678.739131	26.200960
202.838605	8710.313414	26.205978
203.055554	8715.452082	26.210996
203.204584	8720.121952	26.216013
203.020177	8722.959124	26.221031
203.183889	8738.611698	26.226048
203.103861	8758.055987	26.231066
203.577117	8773.591572	26.236084
203.771644	8778.246337	26.241101
203.653244	8809.063943	26.246119
203.909463	8803.931323	26.251136
204.384918	8832.138889	26.256154
204.716945	8835.218749	26.261172
205.426155	8847.698926	26.266189
205.333492	8869.055248	26.271207
205.725411	8871.234370	26.276224
205.744470	8878.384165	26.281242
206.250638	8898.219929	26.286260
206.531840	8898.316780	26.291277
206.539528	8906.695228	26.296295
206.902926	8907.788215	26.301312
207.017699	8931.139477	26.306330
206.979989	8939.382352	26.311348
207.259978	8943.782349	26.316365
207.064329	8963.645100	26.321383
207.567675	8969.303609	26.326400
207.751110	8987.080777	26.331418
207.701325	8996.388365	26.336436
207.870496	9003.779486	26.341453
207.824346	9040.809931	26.346471
208.409764	9036.579700	26.351488
208.757664	9064.853290	26.356506
208.744155	9080.734359	26.361524
209.275559	9089.427999	26.366541
209.129843	9108.704579	26.371559
209.401062	9117.784003	26.376576
209.758895	9127.321004	26.381594
209.615793	9145.098087	26.386612
210.082237	9159.915107	26.391629
210.263505	9164.982499	26.396647
210.788734	9170.733998	26.401664
210.912618	9183.979040	26.406682
210.904391	9199.240852	26.411700
211.541893	9214.577191	26.416717
211.745931	9228.223427	26.421735
212.244183	9231.782485	26.426752
212.246028	9233.015374	26.431770
212.743694	9247.310480	26.436788
212.880535	9252.004100	26.441805
212.796418	9260.404070	26.446823
213.217804	9263.509122	26.451840
213.419991	9261.502859	26.456858
213.002950	9264.793516	26.461876
213.623506	9261.512193	26.466893
213.291179	9275.524531	26.471911
213.335096	9284.395946	26.476928
213.527927	9306.412877	26.481946
213.834596	9317.178327	26.486964
214.092216	9338.261879	26.491981
214.244867	9352.234744	26.496999
214.563752	9366.648179	26.502016
214.943909	9385.459996	26.507034
215.118750	9400.274166	26.512052
215.354631	9418.606947	26.517069
215.288216	9432.185132	26.522087
215.593939	9455.468207	26.527104
215.762541	9464.968700	26.532122
216.057704	9483.329883	26.537140
216.193612	9494.365855	26.542157
216.203211	9512.158768	26.547175
216.521182	9524.272600	26.552192
216.670023	9542.790967	26.557210
216.797177	9574.476397	26.562228
216.989028	9586.907859	26.567245
217.389279	9618.363332	26.572263
217.788411	9623.208062	26.577280
218.144474	9631.768645	26.582298
218.444724	9654.740476	26.587316
218.502116	9667.815148	26.592333
218.845568	9686.871648	26.597351
219.177522	9702.425612	26.602368
219.422528	9709.406390	26.607386
219.417002	9723.037301	26.612404
220.188606	9728.494367	26.617421
220.636715	9755.150217	26.622439
220.214056	9759.532623	26.627456
220.513167	9769.466589	26.632474
220.763536	9778.172384	26.637492
221.055059	9781.142428	26.642509
220.941264	9796.346126	26.647527
221.518033	9815.157044	26.652544
221.420111	9818.618872	26.657562
221.449742	9849.141139	26.662580
221.696584	9852.113992	26.667597
221.814093	9886.114159	26.672615
222.251820	9884.197363	26.677632
222.411565	9915.746496	26.682650
222.147995	9927.709793	26.687668
222.734116	9955.745617	26.692685
222.789652	9969.174204	26.697703
223.228768	9999.622445	26.702720
223.298431	10011.340658	26.707738
223.548428	10030.465614	26.712756
223.961293	10041.611298	26.717773
224.544921	10053.741445	26.722791
224.980396	10061.407005	26.727808
225.135138	10061.153357	26.732826
225.472709	10080.531206	26.737844
225.610554	10078.801098	26.742861
225.612011	10094.161042	26.747879
225.775917	10099.719062	26.752896
225.707257	10103.151499	26.757914
225.888405	10121.973144	26.762932
226.395772	10141.346432	26.767949
226.686966	10148.527032	26.772967
226.732100	10153.100979	26.777984
227.072929	10168.780326	26.783002
227.170726	10200.650009	26.788020
227.469218	10195.545990	26.793037
227.474066	10219.309491	26.798055
227.443337	10236.662279	26.803072
228.336888	10245.754539	26.808090
227.991843	10267.903091	26.813108
228.400364	10284.420943	26.818125
228.768611	10299.183918	26.823143
228.912683	10321.259296	26.828160
229.426652	10331.877526	26.833178
229.465114	10356.409510	26.838196
229.846447	10359.967414	26.843213
229.890400	10371.257546	26.848231
229.911896	10394.415820	26.853248
230.424495	10404.654194	26.858266
230.456323	10426.928632	26.863284
230.941070	10436.288049	26.868301
231.099496	10463.699253	26.873319
231.370834	10472.668513	26.878336
231.402823	10482.390544	26.883354
231.366746	10511.538892	26.888372
231.893660	10527.179110	26.893389
231.691451	10542.156432	26.898407
232.163477	10568.333766	26.903424
232.644697	10573.199563	26.908442
232.987640	10598.010014	26.913460
233.224717	10599.810340	26.918477
233.494276	10626.253797	26.923495
233.812195	10634.820643	26.928512
234.235402	10641.425192	26.933530
233.683197	10667.224112	26.938548
234.332163	10680.135311	26.943565
234.820408	10690.371074	26.948583
234.654295	10708.507433	26.953600
235.189658	10718.751838	26.958618
235.528977	10739.214780	26.963636
235.880137	10745.433018	26.968653
236.215894	10763.910497	26.973671
236.071835	10772.016676	26.978688
236.690839	10772.486661	26.983706
236.807179	10789.816640	26.988724
236.820099	10793.965018	26.993741
237.223531	10791.155186	26.998759
237.420295	10801.114023	27.003776
237.620229	10816.119197	27.008794
237.653279	10826.697570	27.013812
237.602315	10832.854024	27.018829
238.099340	10854.426095	27.023847
238.027711	10867.271706	27.028864
238.423875	10885.327692	27.033882
238.443516	10908.838068	27.038900
238.787229	10917.732700	27.043917
239.066425	10933.287300	27.048935
239.025042	10960.625403	27.053952
239.573921	10961.497733	27.058970
240.552008	10965.735492	27.063988
241.040958	10972.476490	27.069005
241.397651	10965.409506	27.074023
241.598378	10961.987372	27.079040
242.019568	10964.299877	27.084058
241.708641	10969.171666	27.089076
242.413115	10984.214241	27.094093
242.676877	10994.850792	27.099111
242.367009	10983.341357	27.104128
242.695913	10997.456474	27.109146
242.868146	10987.967253	27.114164
243.018002	11008.691368	27.119181
243.056206	11021.313002	27.124199
243.034754	11044.302034	27.129216
243.329924	11052.902261	27.134234
243.260079	11071.658853	27.139252
243.587661	11079.162297	27.144269
243.881139	11098.945553	27.149287
243.946462	11122.182563	27.154304
244.536361	11144.646924	27.159322
244.644953	11160.185667	27.164340
244.369349	11173.081762	27.169357
244.837508	11206.421404	27.174375
245.166048	11212.480129	27.179392
245.648073	11230.971464	27.184410
245.829987	11265.913659	27.189428
245.889469	11279.536004	27.194445
246.256432	11300.014978	27.199463
246.132030	11338.646701	27.204480
246.512599	11344.668064	27.209498
246.971583	11369.761746	27.214516
247.052604	11401.225397	27.219533
247.224243	11418.499861	27.224551
247.294117	11449.617901	27.229568
247.844564	11466.633103	27.234586
247.925400	11494.685444	27.239604
248.216319	11513.437412	27.244621
248.761253	11521.576618	27.249639
249.146572	11554.884584	27.254656
249.392581	11565.356328	27.259674
249.628683	11589.608519	27.264692
250.124991	11579.098187	27.269709
250.607828	11609.932117	27.274727
250.471536	11621.021303	27.279744
250.846885	11622.659221	27.284762
251.222328	11641.392167	27.289780
251.196895	11661.796642	27.294797
251.306760	11663.104599	27.299815
251.513873	11685.732515	27.304832
251.797363	11691.131765	27.309850
252.017475	11717.457509	27.314868
252.224094	11718.676258	27.319885
252.300417	11747.414938	27.324903
252.479685	11766.683043	27.329920
252.777886	11787.959736	27.334938
252.825621	11799.688539	27.339956
253.199552	11836.726957	27.344973
253.532677	11848.182246	27.349991
253.586906	11882.082470	27.355008
253.795708	11908.313143	27.360026
253.952811	11932.851202	27.365044
254.331941	11952.169934	27.370061
254.597451	11978.663825	27.375079
254.829611	12013.828187	27.380096
255.594387	12026.260260	27.385114
255.611784	12050.715309	27.390132
255.689579	12073.533054	27.395149
256.492005	12089.255144	27.400167
256.696728	12109.362411	27.405184
257.122263	12135.947755	27.410202
257.266307	12149.499354	27.415220
257.294635	12162.317926	27.420237
257.759541	12169.880703	27.425255
257.849844	12192.218665	27.430272
258.265660	12213.835733	27.435290
258.424490	12227.149109	27.440308
258.544747	12247.194462	27.445325
258.996618	12278.209623	27.450343
259.023742	12292.852224	27.455360
259.225246	12321.537009	27.460378
259.381107	12336.887600	27.465396
259.932307	12356.536571	27.470413
260.979072	12348.062971	27.475431
260.854752	12381.626765	27.480448
261.491460	12376.382708	27.485466
262.051969	12367.166045	27.490484
263.370442	12377.975872	27.495501
264.674377	12328.337090	27.500519
264.758945	12307.659470	27.505536
264.672150	12288.057228	27.510554
264.931930	12262.935083	27.515572
264.843535	12262.994467	27.520589
265.169054	12235.538743	27.525607
265.099999	12232.151461	27.530624
264.996811	12205.373741	27.535642
265.103279	12208.153383	27.540660
264.961809	12203.671573	27.545677
264.898336	12193.058984	27.550695
265.223909	12203.690275	27.555712
264.979546	12207.355841	27.560730
265.224602	12215.624497	27.565748
265.422911	12235.621384	27.570765
265.687716	12244.750558	27.575783
265.414716	12268.410046	27.580800
265.487993	12274.690533	27.585818
265.443030	12300.057950	27.590836
265.709406	12330.200763	27.595853
266.236111	12353.758293	27.600871
266.159747	12382.375914	27.605888
266.411465	12407.642498	27.610906
266.792804	12443.370872	27.615924
266.910440	12472.325124	27.620941
267.685988	12489.474832	27.625959
267.600865	12522.743424	27.630976
267.917304	12538.606030	27.635994
268.420173	12571.205025	27.641012
268.401781	12609.256941	27.646029
269.311117	12617.026760	27.651047
269.661776	12658.619690	27.656064
269.813574	12675.219656	27.661082
270.056793	12687.517973	27.666100
270.485003	12710.117095	27.671117
270.772834	12727.470560	27.676135
270.806897	12742.687487	27.681152
271.383394	12762.252077	27.686170
271.669605	12772.213304	27.691188
271.508275	12803.968997	27.696205
271.760672	12810.984477	27.701223
271.978510	12850.661572	27.706240
272.032378	12872.811329	27.711258
272.740808	12896.889765	27.716276
273.238438	12923.911111	27.721293
273.513379	12941.102362	27.726311
273.663440	12955.417839	27.731328
274.111511	12984.884580	27.736346
274.153975	13007.075707	27.741364
274.366945	13024.583819	27.746381
275.392526	13048.380127	27.751399
275.604853	13058.245579	27.756416
275.855338	13070.633766	27.761434
276.058098	13077.756955	27.766452
276.263960	13102.344822	27.771469
276.861055	13107.977476	27.776487
276.682278	13134.143936	27.781504
276.913907	13144.320539	27.786522
277.207023	13156.152077	27.791540
277.084712	13182.958726	27.796557
277.383236	13198.910187	27.801575
277.391828	13230.557521	27.806592
278.033940	13243.105994	27.811610
278.249608	13272.543821	27.816628
278.157554	13283.059818	27.821645
278.635546	13306.620787	27.826663
278.828213	13327.812261	27.831680
279.051191	13351.102133	27.836698
279.605018	13375.519263	27.841716
279.703314	13401.781468	27.846733
280.012717	13412.342388	27.851751
280.475457	13449.172216	27.856768
280.584130	13463.405424	27.861786
280.820989	13481.677349	27.866804
281.287874	13508.537952	27.871821
281.878179	13513.411926	27.876839
281.977021	13546.236912	27.881856
282.219589	13558.326059	27.886874
282.773103	13573.386924	27.891892
283.171416	13585.936954	27.896909
283.086703	13611.185167	27.901927
283.244186	13625.354266	27.906944
283.850678	13650.047908	27.911962
284.141523	13648.104190	27.916980
284.325911	13683.084117	27.921997
284.620101	13685.925520	27.927015
284.892394	13723.177005	27.932032
284.949345	13739.434294	27.937050
285.488441	13766.506711	27.942068
285.565388	13788.179840	27.947085
286.034601	13785.678981	27.952103
286.043621	13821.607004	27.957120
286.371513	13837.426337	27.962138
286.884352	13859.958773	27.967156
286.800298	13890.362444	27.972173
287.113068	13905.700727	27.977191
287.347200	13934.279341	27.982208
287.455769	13968.385232	27.987226
288.101907	13983.531320	27.992244
288.259126	14014.120146	27.997261
288.633222	14043.685152	28.002279
288.573917	14066.144564	28.007296
289.024261	14076.240779	28.012314
289.231900	14111.716178	28.017332
289.487023	14145.443486	28.022349
290.090881	14171.710635	28.027367
290.391203	14193.605657	28.032384
290.577130	14238.584100	28.037402
291.019046	14244.218596	28.042420
291.255479	14281.638829	28.047437
291.660546	14302.469239	28.052455
291.768426	14315.457506	28.057472
291.875978	14347.416003	28.062490
292.872740	14349.821414	28.067508
292.625004	14378.224376	28.072525
292.991967	14400.143807	28.077543
293.373379	14422.339543	28.082560
293.335040	14447.513548	28.087578
294.022136	14465.919170	28.092596
294.010446	14492.587671	28.097613
294.841453	14499.851393	28.102631
295.072396	14529.591401	28.107648
295.010823	14539.474311	28.112666
295.465435	14565.304810	28.117684
295.776919	14583.855661	28.122701
295.965389	14615.142222	28.127719
296.135024	14628.167948	28.132736
296.438545	14662.479593	28.137754
296.905008	14672.825943	28.142772
296.995891	14693.102468	28.147789
297.544337	14717.170811	28.152807
297.926296	14742.253805	28.157824
298.079483	14748.183473	28.162842
298.276200	14781.759616	28.167860
298.462338	14800.574456	28.172877
299.204456	14818.171016	28.177895
299.501849	14838.380081	28.182912
299.729911	14855.257308	28.187930
300.319838	14875.612079	28.192948
300.242443	14883.600186	28.197965
300.940106	14892.208705	28.202983
301.103472	14917.205789	28.208000
301.625343	14921.218178	28.213018
302.207733	14935.762705	28.218036
301.954079	14962.022153	28.223053
302.320216	14974.148621	28.228071
302.942605	14978.590487	28.233088
302.936717	14991.542058	28.238106
303.492644	15009.242321	28.243124
303.425793	15032.043159	28.248141
303.912562	15046.146526	28.253159
304.115458	15064.216938	28.258176
303.992109	15077.784532	28.263194
304.687421	15101.071358	28.268212
304.669451	15133.559572	28.273229
305.096126	15151.275384	28.278247
305.841500	15166.460959	28.283264
306.630540	15189.392592	28.288282
307.156200	15174.149237	28.293300
307.187362	15192.547018	28.298317
307.390752	15197.560266	28.303335
307.747582	15205.337329	28.308352
307.498286	15217.587962	28.313370
308.231617	15233.797386	28.318388
308.256847	15251.332363	28.323405
308.244155	15269.666767	28.328423
308.717322	15276.077730	28.333440
308.502348	15316.382565	28.338458
309.019195	15315.735164	28.343476
309.246424	15363.459962	28.348493
309.438879	15378.887787	28.353511
309.851828	15401.413423	28.358528
310.167892	15426.627017	28.363546
310.398702	15449.222199	28.368564
310.494546	15469.387855	28.373581
310.718935	15493.092504	28.378599
311.074759	15514.725000	28.383616
310.934274	15545.624324	28.388634
311.586670	15569.944820	28.393652
311.610465	15594.581454	28.398669
312.187960	15627.697244	28.403687
313.100024	15649.045438	28.408704
313.153356	15673.272238	28.413722
313.602598	15683.937031	28.418740
314.034192	15700.403574	28.423757
314.218457	15729.482679	28.428775
314.804796	15741.826984	28.433792
315.016997	15765.532815	28.438810
315.364437	15788.802621	28.443828
315.876893	15805.934441	28.448845
315.739784	15825.554508	28.453863
316.214892	15838.921004	28.458880
316.052322	15861.395362	28.463898
316.622424	15886.036519	28.468916
316.707599	15922.374480	28.473933
317.097526	15936.706083	28.478951
317.943757	15964.240755	28.483968
318.296932	15983.759458	28.488986
318.685969	16005.605827	28.494004
319.105039	16021.366339	28.499021
319.373759	16041.978161	28.504039
319.345518	16054.309859	28.509056
319.404819	16079.351005	28.514074
320.113043	16099.214595	28.519092
320.436190	16124.823726	28.524109
320.378454	16154.743483	28.529127
321.036490	16175.518211	28.534144
321.266869	16207.422222	28.539162
321.492088	16221.275480	28.544180
321.564847	16249.332317	28.549197
321.948139	16274.972068	28.554215
322.431825	16297.549154	28.559232
322.274457	16323.218075	28.564250
322.818594	16352.751376	28.569268
323.493444	16378.865444	28.574285
323.877884	16405.237237	28.579303
324.248104	16421.128963	28.584320
324.632445	16446.423789	28.589338
324.640065	16473.400188	28.594356
324.758124	16494.416314	28.599373
325.456354	16529.468546	28.604391
326.220132	16545.281930	28.609408
326.290152	16573.797229	28.614426
326.534296	16577.469422	28.619444
327.147872	16612.686504	28.624461
327.086840	16624.191674	28.629479
327.726680	16650.415908	28.634496
327.803240	16673.952645	28.639514
328.113632	16695.511568	28.644532
328.638411	16713.762026	28.649549
328.679801	16732.688709	28.654567
329.219294	16738.503646	28.659584
329.450902	16757.481926	28.664602
329.759732	16776.484926	28.669620
330.115315	16802.261652	28.674637
330.042587	16835.182317	28.679655
330.412309	16849.392805	28.684672
330.731731	16879.455018	28.689690
330.839221	16907.869692	28.694708
331.141271	16937.152166	28.699725
331.418660	16960.684101	28.704743
331.959130	16978.586726	28.709760
331.535826	17025.284591	28.714778
331.952615	17065.508155	28.719796
332.448727	17089.028259	28.724813
332.635575	17127.789511	28.729831
333.352415	17154.422187	28.734848
333.843033	17186.274145	28.739866
334.291780	17212.583528	28.744884
335.017374	17234.589996	28.749901
335.286920	17256.467220	28.754919
335.729514	17285.947235	28.759936
335.998307	17311.431964	28.764954
336.183890	17327.479242	28.769972
336.966432	17345.757672	28.774989
336.840254	17368.495331	28.780007
337.415850	17400.969200	28.785024
337.619954	17429.613517	28.790042
337.903470	17453.739493	28.795060
338.449401	17475.729666	28.800077
338.393821	17510.999537	28.805095
338.940265	17526.056076	28.810112
339.070622	17561.722793	28.815130
339.569607	17589.557047	28.820148
339.761060	17610.270085	28.825165
340.026108	17637.746838	28.830183
340.401083	17669.914670	28.835200
340.636485	17702.888261	28.840218
340.922229	17727.345797	28.845236
341.160197	17752.736952	28.850253
341.452868	17790.109790	28.855271
341.992095	17821.048628	28.860288
342.311368	17863.701977	28.865306
342.767406	17874.082371	28.870324
343.368473	17916.054347	28.875341
343.341067	17943.129039	28.880359
343.902817	17975.684665	28.885376
344.025723	18010.330768	28.890394
344.840384	18032.995440	28.895412
345.207984	18051.718002	28.900429
345.252251	18088.474058	28.905447
345.960404	18106.200677	28.910464
346.239644	18139.299310	28.915482
346.799193	18165.352100	28.920500
347.015170	18178.495784	28.925517
346.876231	18205.770206	28.930535
347.360856	18212.285994	28.935552
347.325590	18247.573981	28.940570
347.792869	18272.983774	28.945588
348.229981	18297.284224	28.950605
348.539517	18325.146447	28.955623
349.122076	18347.153675	28.960640
349.504798	18368.856554	28.965658
350.290864	18385.617120	28.970676
351.130163	18391.957562	28.975693
351.403676	18402.950092	28.980711
351.908416	18422.137479	28.985728
351.844576	18435.419283	28.990746
352.093723	18452.528488	28.995764
352.408213	18464.275970	29.000781
352.764339	18479.471253	29.005799
353.093319	18509.924485	29.010816
353.540908	18523.307149	29.015834
353.657664	18553.734444	29.020852
354.174295	18559.848810	29.025869
354.111435	18595.053396	29.030887
354.425850	18605.688751	29.035904
354.807156	18651.740013	29.040922
355.170689	18659.420217	29.045940
355.525873	18687.144707	29.050957
355.710643	18725.414190	29.055975
356.244990	18753.984302	29.060992
356.489954	18778.678349	29.066010
356.498053	18801.242359	29.071028
357.231530	18837.372210	29.076045
357.583354	18871.428599	29.081063
358.029818	18889.004898	29.086080
358.035985	18934.210034	29.091098
358.336323	18960.028680	29.096116
358.724387	18988.467013	29.101133
358.669677	19033.501025	29.106151
359.039736	19063.345209	29.111168
359.630824	19095.914257	29.116186
359.891771	19143.224423	29.121204
361.051910	19156.410609	29.126221
361.401080	19190.807907	29.131239
362.274579	19191.030578	29.136256
363.195406	19205.806634	29.141274
364.019787	19220.090163	29.146292
364.291464	19211.727770	29.151309
364.329692	19224.378184	29.156327
364.737367	19240.382202	29.161344
365.011100	19254.781469	29.166362
365.173885	19268.471996	29.171380
365.420729	19263.235827	29.176397
365.458081	19288.303164	29.181415
365.920163	19298.276041	29.186432
366.369319	19327.836846	29.191450
366.411155	19333.788583	29.196468
366.763910	19345.526697	29.201485
367.342996	19364.295099	29.206503
367.804150	19370.755274	29.211520
368.106970	19394.080723	29.216538
368.048291	19405.693093	29.221556
368.012754	19425.369429	29.226573
368.557041	19448.815549	29.231591
368.273037	19470.353356	29.236608
368.805147	19491.302039	29.241626
369.006775	19536.100960	29.246644
369.257464	19557.087885	29.251661
369.432453	19601.586091	29.256679
370.094303	19632.988571	29.261696
370.681186	19660.914509	29.266714
370.906228	19701.050631	29.271732
371.251019	19734.732427	29.276749
371.589083	19771.213315	29.281767
371.901477	19802.228468	29.286784
372.212730	19839.903294	29.291802
372.747606	19871.473355	29.296820
373.461520	19902.883832	29.301837
373.616779	19951.408310	29.306855
374.133011	19968.106493	29.311872
374.846554	20003.787052	29.316890
375.076649	20035.045731	29.321908
375.469157	20061.760682	29.326925
375.816059	20099.656859	29.331943
376.454356	20121.200177	29.336960
376.999679	20139.434665	29.341978
376.981016	20175.440986	29.346996
377.778187	20187.955093	29.352013
377.845345	20218.396286	29.357031
378.190378	20249.276397	29.362048
378.812483	20273.188588	29.367066
378.802692	20298.217013	29.372084
379.221428	20324.644728	29.377101
379.856930	20364.004437	29.382119
380.090734	20393.356263	29.387136
380.505530	20420.830594	29.392154
380.418077	20456.313006	29.397172
380.599590	20488.488345	29.402189
380.878631	20531.869680	29.407207
381.502924	20566.044241	29.412224
381.732657	20595.406150	29.417242
381.890066	20639.458452	29.422260
382.738899	20676.030947	29.427277
383.469509	20698.251412	29.432295
384.009710	20735.385126	29.437312
384.253972	20756.297897	29.442330
384.219813	20798.529668	29.447348
384.973363	20818.049322	29.452365
385.471665	20855.821606	29.457383
385.618443	20881.482426	29.462400
386.155715	20915.671616	29.467418
386.123261	20951.624420	29.472436
386.795111	20974.170448	29.477453
386.905714	21002.881109	29.482471
387.144944	21040.054053	29.487488
387.194565	21068.730449	29.492506
387.908252	21112.934849	29.497524
388.778109	21141.130208	29.502541
389.000780	21167.657528	29.507559
389.276170	21195.650018	29.512576
389.860914	21220.792692	29.517594
389.866673	21261.700965	29.522612
390.470879	21291.867671	29.527629
390.791805	21327.283818	29.532647
391.201467	21360.127093	29.537664
391.753486	21385.567433	29.542682
392.225970	21414.433035	29.547700
392.985586	21419.903784	29.552717
393.310460	21459.207052	29.557735
393.847968	21486.929107	29.562752
394.223536	21497.493686	29.567770
394.800322	21527.333645	29.572788
395.446137	21549.955532	29.577805
395.664892	21562.715708	29.582823
395.801215	21591.910068	29.587840
396.635456	21613.757759	29.592858
396.889507	21644.526734	29.597876
397.215089	21661.822197	29.602893
397.351969	21682.780088	29.607911
397.581451	21731.058013	29.612928
398.251406	21728.218366	29.617946
398.133765	21763.823517	29.622964
398.624774	21784.378574	29.627981
398.936922	21817.105240	29.632999
398.956329	21863.220451	29.638016
399.611283	21888.051357	29.643034
399.981377	21942.681530	29.648052
400.803192	21953.817201	29.653069
400.876045	21996.606922	29.658087
401.529258	22020.391594	29.663104
402.515354	22037.774395	29.668122
402.748538	22065.668041	29.673140
402.958806	22093.770166	29.678157
403.343884	22118.316796	29.683175
403.697005	22134.586077	29.688192
403.982378	22170.921045	29.693210
404.184082	22208.305137	29.698228
404.818860	22230.465861	29.703245
405.148560	22276.065779	29.708263
405.079393	22310.942193	29.713280
405.763006	22335.539255	29.718298
405.729206	22371.063100	29.723316
406.279935	22412.112771	29.728333
407.110233	22437.574268	29.733351
407.439430	22476.548579	29.738368
407.931402	22512.341031	29.743386
407.721207	22542.719454	29.748404
408.035803	22575.468565	29.753421
408.406141	22612.512476	29.758439
408.389311	22648.208304	29.763456
409.242376	22689.118366	29.768474
409.244184	22736.636975	29.773492
409.887552	22774.171777	29.778509
410.182702	22820.986219	29.783527
410.644875	22868.047497	29.788544
411.448068	22895.791131	29.793562
411.746844	22929.721024	29.798580
412.356748	22961.277852	29.803597
412.834641	22994.394058	29.808615
413.411895	23032.900155	29.813632
414.362499	23051.808329	29.818650
414.458268	23097.489631	29.823668
415.117938	23113.447998	29.828685
415.428302	23141.545484	29.833703
415.817461	23172.911062	29.838720
416.603920	23201.405389	29.843738
416.457065	23239.342102	29.848756
416.944558	23261.634077	29.853773
417.154365	23302.185076	29.858791
417.515929	23332.840955	29.863808
418.077840	23365.041095	29.868826
418.278166	23411.946429	29.873844
418.604339	23430.896268	29.878861
419.331236	23476.929432	29.883879
419.376422	23505.571563	29.888896
420.343587	23540.136677	29.893914
420.417172	23574.444106	29.898932
420.813419	23617.283551	29.903949
421.326890	23639.690071	29.908967
421.560635	23694.524447	29.913984
421.991819	23717.720058	29.919002
422.396124	23773.014316	29.924020
422.693337	23807.505593	29.929037
423.393103	23853.386633	29.934055
423.882263	23883.056745	29.939072
425.256885	23895.751999	29.944090
425.750792	23929.335496	29.949108
426.217976	23941.154520	29.954125
426.734294	23967.910713	29.959143
426.755849	23999.692536	29.964160
427.106442	24012.495911	29.969178
427.786177	24052.395773	29.974196
427.915805	24076.998744	29.979213
428.150196	24101.288884	29.984231
428.544038	24129.934874	29.989248
428.714522	24157.977675	29.994266
428.801870	24189.932929	29.999284
429.534723	24233.814529	30.004301
429.874563	24265.387838	30.009319
429.863626	24313.114837	30.014336
430.430202	24342.647437	30.019354
430.776755	24389.941964	30.024372
430.903476	24414.023659	30.029389
431.661162	24467.146630	30.034407
431.825703	24506.665750	30.039424
432.367773	24536.973010	30.044442
432.420376	24591.989000	30.049460
432.948022	24635.523141	30.054477
433.309991	24682.280420	30.059495
433.748147	24735.042422	30.064512
434.471348	24762.771350	30.069530
434.992947	24809.933673	30.074548
435.479699	24846.404158	30.079565
436.382259	24878.559388	30.084583
436.231227	24940.674289	30.089600
436.866160	24961.613080	30.094618
437.227491	25021.682807	30.099636
437.389943	25063.764610	30.104653
438.194375	25094.821243	30.109671
438.372694	25138.754299	30.114688
439.229262	25175.899225	30.119706
439.485167	25220.024959	30.124724
440.036776	25262.436009	30.129741
440.002947	25298.001038	30.134759
440.974063	25341.614545	30.139776
441.603341	25363.758471	30.144794
441.868634	25415.245717	30.149812
442.957602	25428.888940	30.154829
443.759287	25452.448715	30.159847
443.878777	25493.673520	30.164864
444.564867	25507.437720	30.169882
445.280858	25539.402646	30.174900
445.670130	25569.508545	30.179917
445.886817	25582.451109	30.184935
446.156816	25624.972586	30.189952
446.293163	25661.006032	30.194970
446.636642	25685.901971	30.199988
446.892000	25724.716377	30.205005
447.675097	25765.996859	30.210023
447.959263	25793.223234	30.215040
448.207919	25838.498056	30.220058
448.495924	25877.172130	30.225076
449.345597	25913.153938	30.230093
449.388829	25952.794425	30.235111
449.535136	26005.184064	30.240128
450.285124	26036.236235	30.245146
450.563173	26091.852476	30.250164
450.717807	26125.463921	30.255181
451.486575	26168.145286	30.260199
451.915511	26221.414695	30.265216
452.419277	26266.732798	30.270234
452.876036	26316.693224	30.275252
453.566370	26343.213750	30.280269
454.226681	26383.170585	30.285287
454.307674	26431.570697	30.290304
454.688138	26472.598080	30.295322
455.031167	26512.393862	30.300340
455.458343	26546.152628	30.305357
455.911489	26576.941949	30.310375
455.987766	26634.338821	30.315392
456.754847	26666.679954	30.320410
457.248185	26709.947881	30.325428
457.599351	26747.907298	30.330445
458.077457	26788.981382	30.335463
458.075739	26833.846675	30.340480
458.538549	26891.317599	30.345498
459.354367	26939.238177	30.350516
459.985468	26994.522389	30.355533
460.508706	27032.585057	30.360551
461.001116	27066.184041	30.365568
461.942059	27099.653334	30.370586
463.158847	27117.194060	30.375604
464.120102	27135.941541	30.380621
464.611475	27158.802446	30.385639
464.846839	27179.876346	30.390656
465.610947	27207.553363	30.395674
465.985840	27210.832609	30.400692
466.145749	27235.865768	30.405709
466.704670	27255.047782	30.410727
466.682340	27282.434232	30.415744
467.114981	27308.590086	30.420762
467.636325	27342.785389	30.425780
467.825414	27374.170597	30.430797
468.516043	27414.550611	30.435815
468.505765	27449.574584	30.440832
468.541230	27482.498760	30.445850
469.177475	27522.043111	30.450868
469.262679	27575.181091	30.455885
470.267744	27619.495019	30.460903
470.280813	27659.224077	30.465920
470.511013	27710.952736	30.470938
471.012957	27747.432116	30.475956
471.850875	27794.056437	30.480973
472.203079	27834.206202	30.485991
472.542534	27896.757806	30.491008
473.238401	27934.790373	30.496026
473.350056	27984.854279	30.501044
473.894584	28037.608592	30.506061
474.724622	28082.635570	30.511079
474.947877	28122.086452	30.516096
475.578499	28185.615479	30.521114
476.038201	28225.082520	30.526132
476.253830	28282.874325	30.531149
476.895840	28318.677137	30.536167
477.507983	28368.289021	30.541184
478.120571	28399.964884	30.546202
478.622898	28448.861750	30.551220
478.962985	28488.285454	30.556237
479.532936	28537.707599	30.561255
480.121251	28590.143141	30.566272
480.419538	28630.623365	30.571290
481.006298	28663.221003	30.576308
481.372079	28704.423431	30.581325
481.980747	28745.768493	30.586343
482.044100	28801.815133	30.591360
482.480183	28830.855165	30.596378
483.148857	28871.940425	30.601396
483.550720	28920.768043	30.606413
483.821516	28967.147276	30.611431
484.315600	29008.218146	30.616448
484.492978	29062.323357	30.621466
485.288458	29110.483694	30.626484
486.169184	29154.062051	30.631501
487.516563	29170.812036	30.636519
488.230870	29205.700722	30.641536
488.696965	29223.219946	30.646554
489.219366	29248.549891	30.651572
489.622701	29300.728804	30.656589
489.914951	29327.573747	30.661607
490.292916	29367.007732	30.666624
490.893797	29399.864628	30.671642
491.147209	29432.523221	30.676660
491.222425	29469.372305	30.681677
492.015109	29503.331951	30.686695
492.122105	29548.769735	30.691712
491.989430	29613.833259	30.696730
492.879556	29643.240523	30.701748
493.068229	29701.221316	30.706765
493.492223	29758.504499	30.711783
494.056385	29811.868188	30.716800
494.241665	29867.591752	30.721818
495.059791	29916.072365	30.726836
495.118217	29977.748487	30.731853
496.258379	30039.093341	30.736871
496.447477	30085.955263	30.741888
496.948946	30156.002496	30.746906
497.677059	30192.257488	30.751924
497.865090	30256.158241	30.756941
498.548178	30304.518103	30.761959
499.585968	30340.927398	30.766976
500.054470	30396.803072	30.771994
501.213018	30426.657560	30.777012
501.296347	30481.449112	30.782029
501.924561	30509.363036	30.787047
502.568578	30546.026220	30.792064
502.877404	30599.611250	30.797082
503.305711	30640.545409	30.802100
503.928959	30696.351749	30.807117
504.207690	30728.313859	30.812135
504.513130	30783.952053	30.817152
504.967435	30829.295510	30.822170
505.639193	30884.394990	30.827188
505.846039	30937.696341	30.832205
506.676458	30980.003095	30.837223
506.797045	31024.607486	30.842240
506.899147	31083.035654	30.847258
507.881448	31127.142128	30.852276
508.787519	31168.951883	30.857293
509.583737	31202.660754	30.862311
510.443146	31239.938958	30.867328
511.064703	31260.737545	30.872346
511.565706	31291.492723	30.877364
511.910278	31315.626418	30.882381
512.427966	31337.143019	30.887399
513.244239	31378.742232	30.892416
513.402580	31411.183500	30.897434
514.174508	31434.859993	30.902452
514.405203	31468.705206	30.907469
514.586209	31489.013163	30.912487
514.865710	31537.734119	30.917504
514.962990	31582.507654	30.922522
515.848568	31619.667497	30.927540
516.344111	31674.761452	30.932557
516.795594	31708.409645	30.937575
517.209801	31755.976538	30.942592
517.905190	31809.915314	30.947610
518.077300	31852.348102	30.952628
518.667341	31902.448672	30.957645
519.278527	31951.977028	30.962663
519.919502	31998.320065	30.967680
520.267522	32049.958580	30.972698
521.308892	32091.082411	30.977716
521.481189	32140.641843	30.982733
521.902802	32189.348392	30.987751
522.595223	32231.171247	30.992768
522.601564	32282.351076	30.997786
523.288685	32329.125878	31.002804
523.481048	32387.764964	31.007821
524.206865	32446.855196	31.012839
524.515660	32503.660342	31.017856
524.796996	32558.889100	31.022874
525.744050	32623.918634	31.027892
526.178910	32676.018145	31.032909
526.939748	32738.825347	31.037927
527.593606	32776.814417	31.042944
528.014986	32845.646935	31.047962
528.718184	32877.361182	31.052980
529.339747	32941.471264	31.057997
529.587760	32996.005351	31.063015
530.027024	33041.455026	31.068032
530.977075	33100.152486	31.073050
531.932427	33143.426933	31.078068
532.230228	33191.626527	31.083085
532.514127	33238.066180	31.088103
533.397773	33294.382094	31.093120
533.677325	33346.795342	31.098138
534.136186	33387.867027	31.103156
534.692763	33444.989028	31.108173
535.148711	33491.099331	31.113191
535.336911	33541.272034	31.118208
536.133696	33600.288878	31.123226
536.776792	33636.148866	31.128244
537.222572	33699.526937	31.133261
537.505370	33739.632869	31.138279
538.308911	33781.030523	31.143296
538.634509	33821.687862	31.148314
539.389824	33870.152314	31.153332
540.125482	33912.625149	31.158349
540.506590	33966.662013	31.163367
541.339041	34005.005360	31.168384
541.488139	34048.424788	31.173402
542.266470	34089.190374	31.178420
542.697497	34148.423491	31.183437
543.006966	34181.454602	31.188455
543.519220	34235.460415	31.193472
544.000808	34293.363404	31.198490
544.658630	34345.224561	31.203508
544.990944	34389.922530	31.208525
545.709192	34443.399640	31.213543
546.376487	34503.750318	31.218560
546.273720	34567.247446	31.223578
546.960731	34611.921042	31.228596
547.753323	34679.254874	31.233613
547.942441	34740.409309	31.238631
549.018439	34783.712966	31.243648
549.307727	34862.769721	31.248666
549.719651	34904.095403	31.253684
549.999743	34986.600333	31.258701
550.594172	35039.544164	31.263719
551.195404	35103.779333	31.268736
551.685835	35169.925746	31.273754
552.432792	35236.111962	31.278772
552.878157	35301.443149	31.283789
553.048411	35363.428948	31.288807
553.990435	35424.068683	31.293824
554.189316	35501.916342	31.298842
555.294872	35556.047911	31.303860
555.535041	35620.087179	31.308877
556.312078	35678.989994	31.313895
557.353271	35743.668339	31.318912
558.124163	35796.472951	31.323930
558.965921	35845.575763	31.328948
559.667874	35905.355280	31.333965
559.735487	35966.145716	31.338983
560.521196	36011.950339	31.344000
561.001753	36078.923303	31.349018
561.393976	36120.540486	31.354036
561.922236	36185.587596	31.359053
562.123671	36241.076197	31.364071
562.689445	36302.354496	31.369088
563.263128	36370.781589	31.374106
563.838092	36424.932689	31.379124
564.330140	36480.069932	31.384141
564.845285	36563.771779	31.389159
565.496042	36619.721380	31.394176
565.703649	36674.508835	31.399194
566.328206	36734.373003	31.404212
567.044669	36787.042779	31.409229
567.467805	36838.624265	31.414247
568.216908	36901.091131	31.419264
568.279375	36958.581337	31.424282
569.260096	37021.858419	31.429300
570.123257	37076.288928	31.434317
570.406083	37135.603517	31.439335
571.303724	37188.406513	31.444352
572.168082	37242.279229	31.449370
572.707806	37295.581037	31.454388
573.398614	37343.365794	31.459405
573.906072	37394.344296	31.464423
574.703224	37435.288486	31.469440
574.946473	37503.364451	31.474458
575.655345	37550.333344	31.479476
575.990612	37600.564158	31.484493
576.283226	37666.051851	31.489511
577.265721	37711.307876	31.494528
577.355323	37777.682915	31.499546
578.318330	37840.754615	31.504564
578.843232	37894.957835	31.509581
578.922385	37951.247292	31.514599
579.731454	38017.384118	31.519616
580.020210	38084.412947	31.524634
580.540625	38147.275621	31.529652
581.554573	38214.049131	31.534669
581.794241	38285.722253	31.539687
582.656042	38342.963715	31.544704
582.993927	38425.052142	31.549722
583.562212	38497.487439	31.554740
584.256548	38569.642799	31.559757
584.450888	38628.539944	31.564775
584.978512	38696.556491	31.569792
585.736315	38776.862598	31.574810
586.327060	38835.654753	31.579828
587.007374	38908.712575	31.584845
587.756251	38985.282436	31.589863
588.661456	39044.097765	31.594880
589.192430	39115.090949	31.599898
589.594317	39187.260821	31.604916
590.074034	39249.515936	31.609933
590.654025	39317.227024	31.614951
591.426623	39376.406804	31.619968
591.807991	39455.607611	31.624986
592.742260	39523.510667	31.630004
593.482690	39583.306543	31.635021
593.934293	39660.409317	31.640039
594.352158	39718.270151	31.645056
595.377078	39779.084238	31.650074
595.712347	39855.938349	31.655092
596.380142	39918.419839	31.660109
596.612830	39974.179039	31.665127
597.435535	40040.821463	31.670144
597.946818	40112.082131	31.675162
598.430809	40184.579037	31.680180
599.288088	40229.098492	31.685197
599.706759	40305.520299	31.690215
600.279781	40372.134396	31.695232
601.126092	40426.502660	31.700250
601.367571	40502.288086	31.705268
601.916475	40556.694669	31.710285
602.498756	40614.852483	31.715303
603.269336	40672.882733	31.720320
603.651589	40751.419188	31.725338
604.025934	40814.165160	31.730356
605.133064	40871.524301	31.735373
605.548150	40951.557755	31.740391
606.204063	41009.285697	31.745408
607.206748	41079.864984	31.750426
607.696896	41147.413127	31.755444
608.533435	41206.169578	31.760461
608.932320	41268.793451	31.765479
610.066884	41311.196179	31.770496
611.216956	41370.855801	31.775514
611.109642	41416.503434	31.780532
612.597238	41459.231955	31.785549
612.754977	41530.452322	31.790567
613.706628	41572.260310	31.795584
614.551247	41621.305297	31.800602
614.937134	41678.961795	31.805620
615.449821	41721.666445	31.810637
615.724692	41782.094559	31.815655
616.450422	41828.569489	31.820672
617.125027	41871.027932	31.825690
617.449162	41935.836229	31.830708
618.275195	41983.450046	31.835725
618.927163	42037.381245	31.840743
619.218264	42101.627666	31.845760
619.906977	42158.537303	31.850778
620.533833	42230.158993	31.855796
620.949707	42281.302335	31.860813
621.302422	42354.062730	31.865831
621.987103	42404.753573	31.870848
622.542112	42490.796613	31.875866
622.689980	42553.537686	31.880884
623.672916	42625.227329	31.885901
623.857794	42690.543252	31.890919
624.240865	42782.762950	31.895936
625.250159	42852.812226	31.900954
625.942804	42944.563956	31.905972
626.255160	43013.059350	31.910989
626.445213	43098.939573	31.916007
627.337328	43174.314551	31.921024
628.036215	43249.219072	31.926042
628.116189	43332.114945	31.931060
629.556909	43404.192316	31.936077
630.145716	43502.054832	31.941095
630.922872	43565.200922	31.946112
632.390736	43626.451792	31.951130
633.412458	43679.007494	31.956148
634.130275	43717.873751	31.961165
634.445001	43785.898643	31.966183
635.236154	43811.826107	31.971200
636.027334	43879.087799	31.976218
636.591572	43919.142999	31.981236
637.658106	43956.951109	31.986253
637.857997	44013.140281	31.991271
638.493708	44057.285383	31.996288
638.950089	44109.509705	32.001306
639.352737	44167.824839	32.006324
639.900015	44227.426306	32.011341
640.225777	44278.753941	32.016359
641.076095	44344.752475	32.021376
641.668236	44399.369355	32.026394
641.861188	44482.754316	32.031412
642.760260	44536.029332	32.036429
643.220459	44604.103662	32.041447
643.922525	44661.981589	32.046464
644.891041	44735.401580	32.051482
645.375005	44795.882624	32.056500
646.010620	44864.314914	32.061517
646.551648	44934.049675	32.066535
647.613732	44997.868578	32.071552
648.253107	45054.445410	32.076570
648.813584	45121.278583	32.081588
649.696998	45183.533450	32.086605
650.306066	45245.292754	32.091623
650.718488	45317.879393	32.096640
651.470347	45384.973344	32.101658
651.820622	45448.607536	32.106676
652.484376	45513.974536	32.111693
652.690598	45602.602952	32.116711
653.606773	45664.661870	32.121728
654.467419	45734.913657	32.126746
654.583997	45829.696929	32.131764
655.528551	45900.030664	32.136781
655.776496	45966.206974	32.141799
656.697402	46054.477784	32.146816
657.323728	46136.457610	32.151834
657.731583	46214.765499	32.156852
658.189568	46301.104694	32.161869
659.055785	46390.136792	32.166887
659.402309	46468.752151	32.171904
660.421466	46540.969598	32.176922
660.802098	46640.782198	32.181940
662.280609	46707.427914	32.186957
662.926867	46766.662601	32.191975
664.113591	46851.194179	32.196992
664.895754	46915.727226	32.202010
665.133908	46999.858418	32.207028
666.249447	47047.152903	32.212045
667.181633	47124.630433	32.217063
667.854952	47175.015155	32.222080
668.982424	47224.027778	32.227098
669.263319	47281.703778	32.232116
669.990165	47323.876948	32.237133
670.551696	47378.151463	32.242151
670.580241	47423.550240	32.247168
671.132639	47488.579477	32.252186
671.562117	47568.167807	32.257204
672.362605	47624.153025	32.262221
672.631904	47695.087377	32.267239
673.182778	47764.910700	32.272256
674.143840	47843.800351	32.277274
674.493134	47921.995789	32.282292
675.254927	47992.171370	32.287309
675.900215	48072.743616	32.292327
676.298221	48153.724776	32.297344
677.217665	48229.006765	32.302362
677.393689	48317.145632	32.307380
678.265422	48406.676120	32.312397
678.234800	48497.259493	32.317415
678.896277	48584.208535	32.322432
679.766887	48671.752633	32.327450
680.263484	48769.514077	32.332468
681.009805	48861.335590	32.337485
681.428207	48965.175350	32.342503
682.664487	49057.039769	32.347520
683.577106	49143.973653	32.352538
684.656469	49226.567814	32.357556
685.687440	49313.938080	32.362573
686.983403	49378.439330	32.367591
687.753969	49457.678897	32.372608
688.701124	49526.931704	32.377626
688.737700	49589.204450	32.382644
689.628558	49665.942345	32.387661
690.409970	49739.274158	32.392679
690.750853	49818.555346	32.397696
691.431979	49883.869498	32.402714
691.960235	49968.946828	32.407732
692.740696	50040.654870	32.412749
693.415655	50107.917871	32.417767
694.254730	50189.661704	32.422784
695.172021	50271.500752	32.427802
695.211250	50356.938651	32.432820
695.653239	50439.946027	32.437837
696.689529	50525.576265	32.442855
697.049708	50607.770638	32.447872
698.084548	50688.819718	32.452890
698.617008	50787.340743	32.457908
699.404595	50861.906943	32.462925
700.253400	50945.650310	32.467943
700.384590	51044.953012	32.472960
701.619791	51122.683768	32.477978
702.278798	51209.866913	32.482996
703.208780	51294.192287	32.488013
703.943368	51370.653106	32.493031
704.325051	51456.130077	32.498048
705.384902	51526.559315	32.503066
705.755053	51619.632061	32.508084
706.941686	51676.515334	32.513101
707.721913	51762.315333	32.518119
707.760683	51828.695110	32.523136
708.707659	51900.308342	32.528154
709.236844	51981.626819	32.533172
709.520194	52055.501880	32.538189
710.235986	52144.438418	32.543207
710.953462	52223.417789	32.548224
711.702563	52308.849777	32.553242
712.223915	52414.413195	32.558260
713.014482	52497.573407	32.563277
713.403921	52595.439074	32.568295
713.948897	52685.607954	32.573312
715.350383	52763.657037	32.578330
716.154638	52853.908566	32.583348
716.864942	52930.834358	32.588365
717.826654	53011.735120	32.593383
718.974241	53099.534512	32.598400
719.862810	53176.369844	32.603418
720.120288	53259.833059	32.608436
721.103770	53335.590306	32.613453
721.833958	53413.322982	32.618471
722.239208	53500.254597	32.623488
723.180364	53569.735427	32.628506
723.775678	53672.052899	32.633524
724.547222	53746.463147	32.638541
725.207235	53837.260175	32.643559
725.500642	53919.439231	32.648576
726.274532	54008.845976	32.653594
727.014132	54110.672648	32.658612
727.633592	54197.444081	32.663629
728.185572	54293.165618	32.668647
728.769345	54388.914161	32.673664
729.784492	54477.350496	32.678682
730.282198	54584.268632	32.683700
731.153144	54674.957344	32.688717
731.806667	54765.141363	32.693735
732.532116	54872.397394	32.698752
733.559931	54958.371970	32.703770
733.989592	55063.990633	32.708788
735.018272	55149.290471	32.713805
736.580302	55243.350511	32.718823
736.927812	55330.107494	32.723840
737.791953	55421.293425	32.728858
738.739347	55494.480149	32.733876
739.286188	55591.273086	32.738893
740.183963	55669.834688	32.743911
740.882975	55746.783650	32.748928
742.072382	55819.746904	32.753946
742.659851	55902.585689	32.758964
743.217494	55986.130384	32.763981
743.953157	56078.018729	32.768999
744.275143	56161.462842	32.774016
745.298740	56245.944693	32.779034
745.989116	56339.113722	32.784052
746.477979	56406.395024	32.789069
747.323525	56490.019291	32.794087
747.704977	56575.454061	32.799104
748.746758	56647.875888	32.804122
749.155890	56736.489067	32.809140
750.020077	56812.289210	32.814157
751.657512	56877.665751	32.819175
751.978649	56956.870795	32.824192
752.832526	57037.816045	32.829210
753.600259	57115.811041	32.834228
754.247912	57189.121691	32.839245
755.054248	57258.079235	32.844263
755.522868	57357.324746	32.849280
756.244242	57427.101466	32.854298
756.725696	57527.302400	32.859316
757.631869	57618.053718	32.864333
758.692283	57702.542706	32.869351
759.502955	57779.188788	32.874368
760.129412	57869.831178	32.879386
761.342226	57955.196811	32.884404
761.623355	58035.732486	32.889421
762.730160	58110.549066	32.894439
763.436919	58204.387886	32.899456
764.235537	58278.951128	32.904474
764.907944	58379.735593	32.909492
765.591914	58451.264854	32.914509
766.732346	58519.684564	32.919527
767.026919	58624.369579	32.924544
767.850686	58709.690122	32.929562
768.464088	58803.493159	32.934580
769.005309	58883.056577	32.939597
769.768967	58983.450927	32.944615
770.609842	59084.288166	32.949632
771.771828	59167.709991	32.954650
772.319822	59268.556965	32.959668
772.981686	59356.337335	32.964685
774.128254	59439.668115	32.969703
774.819195	59537.181790	32.974720
775.483205	59623.586492	32.979738
775.886879	59726.179651	32.984756
776.896805	59821.269714	32.989773
777.803796	59914.103341	32.994791
778.366288	60023.312797	32.999808
779.416026	60104.470733	33.004826
780.123676	60195.875615	33.009844
780.739398	60296.152174	33.014861
781.697504	60395.026537	33.019879
782.091948	60504.221342	33.024896
782.950934	60591.966662	33.029914
784.021338	60693.177047	33.034932
784.777018	60781.081784	33.039949
785.380838	60877.176480	33.044967
786.112044	60990.431611	33.049984
786.774734	61073.988787	33.055002
787.610522	61174.680225	33.060020
788.299458	61268.553065	33.065037
789.241745	61353.162662	33.070055
790.179335	61440.574200	33.075072
790.992694	61527.068101	33.080090
791.782653	61606.372989	33.085108
792.454597	61706.247100	33.090125
793.103359	61801.069974	33.095143
793.911578	61889.202036	33.100160
794.390313	61991.293539	33.105178
795.331527	62080.074758	33.110196
796.015452	62187.790159	33.115213
797.117506	62273.366831	33.120231
797.729098	62375.710830	33.125248
798.246793	62481.234442	33.130266
799.522182	62575.601468	33.135284
800.066581	62686.423944	33.140301
800.456070	62782.208779	33.145319
801.239482	62896.256494	33.150336
802.089552	62992.155390	33.155354
802.960514	63095.355669	33.160372
803.349119	63225.879827	33.165389
804.499947	63327.918917	33.170407
805.531012	63448.221144	33.175424
806.489943	63543.057051	33.180442
807.053198	63653.800060	33.185460
807.863765	63762.628489	33.190477
808.947747	63876.987942	33.195495
809.343815	63990.055404	33.200512
809.962988	64103.887015	33.205530
810.882330	64217.955754	33.210548
811.326457	64342.301500	33.215565
812.290830	64453.692720	33.220583
812.701878	64581.178145	33.225600
813.731259	64710.325097	33.230618
814.782021	64828.728518	33.235636
815.552661	64944.963356	33.240653
816.810836	65064.453227	33.245671
817.653847	65178.018732	33.250688
818.438118	65300.216322	33.255706
819.541983	65416.748389	33.260724
820.312065	65532.639465	33.265741
820.995335	65639.717547	33.270759
822.064071	65756.955259	33.275776
822.464945	65870.235179	33.280794
823.374531	65981.302890	33.285812
824.088467	66102.540834	33.290829
825.119672	66216.707883	33.295847
826.017800	66340.839542	33.300864
826.675742	66453.573464	33.305882
827.574549	66562.473222	33.310900
828.342698	66696.832884	33.315917
829.501828	66805.825238	33.320935
830.284136	66910.096170	33.325952
831.714529	67012.514678	33.330970
832.622634	67106.147619	33.335988
833.434262	67203.125507	33.341005
834.768404	67274.581431	33.346023
835.939031	67360.062565	33.351040
836.711080	67445.310605	33.356058
838.034425	67517.716732	33.361076
838.443798	67605.221603	33.366093
839.278750	67692.892874	33.371111
839.972766	67775.817381	33.376128
840.444973	67862.744851	33.381146
841.202296	67954.889722	33.386164
841.369897	68050.679283	33.391181
842.457536	68140.169679	33.396199
843.015793	68255.046291	33.401216
843.228775	68371.134642	33.406234
844.631291	68471.493146	33.411252
845.282639	68587.576191	33.416269
846.108856	68695.975118	33.421287
846.847576	68800.282086	33.426304
847.259367	68912.001770	33.431322
848.164805	69033.353899	33.436340
848.830170	69161.625060	33.441357
849.763013	69280.434610	33.446375
850.883962	69396.258184	33.451392
851.717090	69531.353630	33.456410
852.554997	69633.861288	33.461428
853.330606	69778.198102	33.466445
854.583195	69877.065053	33.471463
855.529244	70001.291413	33.476480
856.589304	70117.299525	33.481498
858.004013	70220.445029	33.486516
858.719860	70333.545998	33.491533
859.886299	70415.825247	33.496551
860.724723	70522.583286	33.501568
861.130516	70645.945648	33.506586
862.377872	70736.161737	33.511604
863.144277	70858.052737	33.516621
864.065140	70956.219712	33.521639
864.643308	71068.923481	33.526656
865.645977	71182.324865	33.531674
866.289641	71296.624392	33.536692
866.928251	71414.874451	33.541709
867.707063	71518.014218	33.546727
868.679024	71641.488564	33.551744
868.898028	71758.436320	33.556762
870.542207	71885.242533	33.561780
871.205004	72002.140054	33.566797
871.730726	72129.416486	33.571815
872.431583	72252.369092	33.576832
873.033028	72394.199953	33.581850
874.308176	72493.215436	33.586868
875.132572	72646.746728	33.591885
876.095397	72756.321562	33.596903
876.805433	72878.398243	33.601920
877.802186	73020.094821	33.606938
878.591871	73120.479763	33.611956
879.633503	73244.926113	33.616973
880.360371	73360.709252	33.621991
881.225461	73470.587924	33.627008
882.071090	73587.693140	33.632026
883.365915	73700.342008	33.637044
884.267012	73821.888509	33.642061
885.408955	73931.137961	33.647079
886.125099	74027.962436	33.652096
886.793049	74168.120682	33.657114
888.523860	74249.403385	33.662132
889.518590	74368.334705	33.667149
890.092479	74464.830038	33.672167
890.910926	74575.581642	33.677184
892.112673	74695.151821	33.682202
892.852652	74791.186240	33.687220
893.369296	74910.721374	33.692237
894.188268	75027.516934	33.697255
895.261964	75146.275977	33.702272
896.081709	75254.496914	33.707290
896.915937	75371.096125	33.712308
898.055717	75499.888834	33.717325
898.979370	75618.984207	33.722343
899.815734	75735.471424	33.727360
900.276188	75844.296205	33.732378
901.528032	75961.110440	33.737396
902.218582	76097.480215	33.742413
902.941568	76212.553583	33.747431
904.240989	76319.812767	33.752448
904.584162	76459.109556	33.757466
905.749912	76575.890475	33.762484
906.410682	76698.023446	33.767501
907.001197	76842.466044	33.772519
908.762393	76977.135541	33.777536
909.060537	77099.297024	33.782554
910.092102	77225.172652	33.787572
910.801597	77374.991338	33.792589
911.935316	77496.466042	33.797607
913.164827	77627.501720	33.802624
914.176695	77760.380536	33.807642
915.191184	77881.876506	33.812660
915.780606	78002.676048	33.817677
916.606014	78129.759364	33.822695
917.210588	78269.690579	33.827712
918.574374	78391.658608	33.832730
919.905907	78508.683362	33.837748
920.901234	78628.347477	33.842765
921.939518	78765.235977	33.847783
922.941009	78878.680894	33.852800
923.682326	79000.827444	33.857818
924.528419	79125.739253	33.862836
925.759578	79246.431356	33.867853
926.711402	79368.344320	33.872871
927.423793	79475.568103	33.877888
928.319106	79600.822617	33.882906
929.214414	79711.242264	33.887924
929.769919	79828.467543	33.892941
930.524000	79947.431818	33.897959
931.536211	80057.120419	33.902976
931.815001	80184.575212	33.907994
933.084505	80302.359617	33.913012
934.277634	80433.772967	33.918029
934.776010	80551.574028	33.923047
935.865177	80664.774600	33.928064
936.915279	80799.430614	33.933082
938.213597	80927.479997	33.938100
939.332268	81046.771857	33.943117
939.859041	81167.998152	33.948135
941.048665	81287.495037	33.953152
941.716025	81427.804299	33.958170
942.730281	81543.202536	33.963188
944.031546	81673.070357	33.968205
944.962040	81790.392443	33.973223
945.757537	81913.596949	33.978240
946.649333	82044.391993	33.983258
947.696447	82173.816590	33.988276
948.300471	82312.978656	33.993293
948.873885	82444.060767	33.998311
950.194952	82562.595749	34.003328
950.699924	82704.551518	34.008346
951.862041	82830.611211	34.013364
952.845006	82980.553402	34.018381
953.710601	83111.517328	34.023399
954.996021	83247.005167	34.028416
955.449039	83403.344220	34.033434
956.819076	83540.634964	34.038452
957.956748	83672.874122	34.043469
958.434791	83822.264095	34.048487
959.703935	83955.875025	34.053504
960.587137	84093.044509	34.058522
962.039485	84220.223349	34.063540
963.380114	84361.949842	34.068557
964.255400	84493.824927	34.073575
965.460851	84620.040171	34.078592
966.157006	84752.223559	34.083610
967.359469	84871.852608	34.088628
968.205746	85011.822211	34.093645
968.835595	85144.214592	34.098663
970.039244	85269.517191	34.103680
971.044499	85405.727333	34.108698
972.049473	85538.663153	34.113716
972.934293	85668.571285	34.118733
973.485419	85811.330918	34.123751
974.484859	85936.587735	34.128768
974.961971	86090.596935	34.133786
976.324804	86224.283116	34.138804
977.142899	86373.624273	34.143821
977.918077	86516.188565	34.148839
979.199926	86655.625419	34.153856
980.225212	86810.513708	34.158874
980.967155	86927.318874	34.163892
981.818789	87069.229706	34.168909
982.503019	87199.824025	34.173927
983.884079	87336.979444	34.178944
984.755094	87471.845602	34.183962
985.860840	87595.906402	34.188980
987.095164	87732.569166	34.193997
987.817075	87860.600481	34.199015
988.972021	87996.834902	34.204032
989.794484	88140.932750	34.209050
990.509084	88282.544548	34.214068
991.291356	88423.786057	34.219085
992.519814	88568.802338	34.224103
993.392289	88712.080270	34.229120
994.062679	88869.322700	34.234138
995.366371	89011.838387	34.239156
996.106145	89166.131327	34.244173
997.393647	89311.541590	34.249191
998.583373	89455.899625	34.254208
999.756054	89605.668389	34.259226
1000.953506	89755.693532	34.264244
1002.150710	89886.918104	34.269261
1003.111743	90038.538541	34.274279
1004.641777	90175.719867	34.279296
1005.054306	90320.668941	34.284314
1006.496242	90453.907048	34.289332
1007.370725	90596.159874	34.294349
1008.231884	90739.414996	34.299367
1009.225892	90875.206083	34.304384
1010.258311	91014.116180	34.309402
1011.374461	91166.737993	34.314420
1012.146081	91302.661971	34.319437
1013.089667	91457.931616	34.324455
1014.436234	91609.488941	34.329472
1015.191818	91754.260087	34.334490
1016.110742	91906.064574	34.339508
1017.254526	92046.626874	34.344525
1018.483985	92195.487217	34.349543
1019.777824	92337.855366	34.354560
1020.665375	92480.896254	34.359578
1021.556181	92637.593044	34.364596
1022.752068	92766.792085	34.369613
1023.790821	92917.958287	34.374631
1024.913823	93051.104730	34.379648
1026.272746	93196.529367	34.384666
1027.332959	93343.096720	34.389684
1028.426418	93475.845602	34.394701
1029.014697	93619.093239	34.399719
1030.100536	93747.309786	34.404736
1030.893625	93902.297927	34.409754
1032.076119	94043.878773	34.414772
1032.940326	94180.318031	34.419789
1033.707033	94342.486380	34.424807
1035.254682	94465.952797	34.429824
1036.516765	94619.549293	34.434842
1037.419490	94747.225092	34.439860
1038.496337	94866.884748	34.444877
1039.655218	95004.098150	34.449895
1040.569329	95118.275448	34.454912
1041.464126	95234.474282	34.459930
1042.307721	95380.570753	34.464948
1043.178141	95500.899197	34.469965
1044.023554	95645.497901	34.474983
1045.347504	95787.876963	34.480000
1045.899988	95934.706524	34.485018
1046.739999	96075.753719	34.490036
1047.996019	96227.571940	34.495053
1048.639844	96380.348897	34.500071
1050.017904	96520.105017	34.505088
1050.981718	96674.307018	34.510106
1052.046358	96827.513486	34.515124
1052.845700	96989.366744	34.520141
1053.681683	97149.602149	34.525159
1054.857342	97295.069836	34.530176
1056.063711	97476.409879	34.535194
1056.914388	97637.955926	34.540212
1058.072487	97798.929130	34.545229
1058.813168	97967.340141	34.550247
1059.848799	98124.963145	34.555264
1060.931279	98302.059098	34.560282
1061.782282	98478.655485	34.565300
1063.159144	98644.616810	34.570317
1063.536534	98833.248547	34.575335
1065.082146	98992.593175	34.580352
1066.346315	99182.541869	34.585370
1066.858956	99353.352887	34.590388
1068.148865	99532.209498	34.595405
1069.505585	99720.749680	34.600423
1070.755086	99887.771526	34.605440
1071.908726	100071.816786	34.610458
1072.907572	100235.173395	34.615476
1074.275274	100412.113686	34.620493
1074.868655	100603.762547	34.625511
1076.279293	100765.247835	34.630528
1077.685787	100947.285754	34.635546
1078.584207	101126.577618	34.640564
1080.096109	101290.828133	34.645581
1081.282941	101464.375806	34.650599
1082.351130	101620.062355	34.655616
1083.156820	101799.886672	34.660634
1084.457757	101959.828492	34.665652
1085.456233	102127.627715	34.670669
1086.388307	102306.208280	34.675687
1088.386694	102452.862150	34.680704
1089.320054	102609.703057	34.685722
1090.156951	102767.104541	34.690740
1091.669574	102918.090819	34.695757
1093.008128	103089.335766	34.700775
1093.768403	103243.284984	34.705792
1094.827762	103399.509977	34.710810
1095.856327	103547.261468	34.715828
1097.017273	103690.253176	34.720845
1097.542716	103841.275828	34.725863
1098.412707	103987.663133	34.730880
1099.834526	104151.840448	34.735898
1100.152882	104316.738625	34.740916
1101.328174	104462.226008	34.745933
1102.228792	104644.050337	34.750951
1103.320024	104806.012928	34.755968
1103.977897	104971.456509	34.760986
1105.045960	105163.592322	34.766004
1106.378323	105330.816980	34.771021
1107.405095	105527.917445	34.776039
1108.542196	105693.580929	34.781056
1109.541083	105880.904871	34.786074
1110.896560	106064.623219	34.791092
1112.019002	106250.069791	34.796109
1113.151323	106424.282780	34.801127
1114.297509	106603.532511	34.806144
1115.736253	106787.597567	34.811162
1116.655306	106963.354637	34.816180
1118.465528	107147.964612	34.821197
1118.794243	107336.925430	34.826215
1120.189552	107500.737587	34.831232
1121.325511	107693.730956	34.836250
1122.308223	107878.465468	34.841268
1123.906716	108055.527490	34.846285
1124.870902	108230.558753	34.851303
1126.290885	108406.056774	34.856320
1127.424746	108589.304285	34.861338
1128.494227	108767.848076	34.866356
1129.821050	108942.630588	34.871373
1130.995007	109125.299786	34.876391
1132.109521	109305.701203	34.881408
1133.184417	109471.147321	34.886426
1134.217322	109667.381801	34.891444
1135.275750	109833.636842	34.896461
1136.256150	110035.072882	34.901479
1137.534639	110202.643643	34.906496
1138.521087	110385.649564	34.911514
1139.682286	110580.965798	34.916532
1141.523934	110758.780999	34.921549
1142.105361	110941.842805	34.926567
1143.367645	111115.467391	34.931584
1145.070929	111293.492022	34.936602
1146.059664	111489.247994	34.941620
1147.401296	111643.753368	34.946637
1148.692157	111835.533068	34.951655
1149.414004	112008.604196	34.956672
1150.798629	112166.834450	34.961690
1151.618702	112354.135289	34.966708
1152.987955	112532.595424	34.971725
1153.856475	112723.385650	34.976743
1155.035978	112904.841219	34.981760
1156.407047	113076.892294	34.986778
1157.440811	113251.688639	34.991796
1158.434895	113406.646385	34.996813
1159.414500	113584.796173	35.001831
1160.615835	113750.617961	35.006848
1161.353278	113921.876657	35.011866
1162.547273	114098.229750	35.016884
1164.019627	114270.082988	35.021901
1165.249439	114444.286697	35.026919
1166.394543	114630.919794	35.031936
1167.600008	114804.851309	35.036954
1168.696823	114982.226314	35.041972
1169.413527	115168.247765	35.046989
1170.417991	115344.835966	35.052007
1171.407783	115533.127478	35.057024
1172.837325	115738.393736	35.062042
1173.570917	115923.670967	35.067060
1175.177177	116113.571826	35.072077
1176.492203	116310.130211	35.077095
1177.727712	116503.803032	35.082112
1178.937541	116691.143751	35.087130
1180.229747	116874.597946	35.092148
1181.026188	117073.232711	35.097165
1182.186210	117266.024242	35.102183
1183.850137	117459.876766	35.107200
1185.042622	117655.610213	35.112218
1186.325421	117854.661214	35.117236
1187.621617	118037.154344	35.122253
1189.083147	118228.360220	35.127271
1189.855210	118422.482107	35.132288
1191.630133	118597.767200	35.137306
1192.815108	118800.659117	35.142324
1193.807775	118984.270944	35.147341
1195.205331	119175.164730	35.152359
1196.368332	119363.038868	35.157376
1197.590773	119546.447169	35.162394
1198.127141	119756.699845	35.167412
1199.718395	119936.354316	35.172429
1201.122876	120136.707897	35.177447
1202.427285	120314.447608	35.182464
1203.442111	120503.062720	35.187482
1204.547923	120706.393651	35.192500
1205.712128	120898.166667	35.197517
1206.970776	121101.906958	35.202535
1208.258210	121302.984622	35.207552
1209.638200	121482.923915	35.212570
1210.889744	121688.810255	35.217588
1211.838247	121870.733224	35.222605
1213.512288	122066.017913	35.227623
1214.608873	122272.933992	35.232640
1216.079289	122437.540330	35.237658
1217.249165	122632.060767	35.242676
1218.607988	122817.559998	35.247693
1219.952852	123014.930506	35.252711
1221.127364	123200.626365	35.257728
1222.148361	123382.003526	35.262746
1223.183340	123555.235479	35.267764
1224.588273	123721.836058	35.272781
1225.509670	123897.241511	35.277799
1226.466900	124079.773489	35.282816
1228.006171	124244.481359	35.287834
1229.115530	124442.178498	35.292852
1230.542454	124612.163033	35.297869
1231.596305	124801.575104	35.302887
1232.455597	124991.766770	35.307904
1233.840966	125155.922020	35.312922
1235.021594	125356.755875	35.317940
1235.668884	125540.677035	35.322957
1237.351703	125726.892200	35.327975
1238.583971	125932.041548	35.332992
1239.619064	126122.694548	35.338010
1241.018974	126314.570275	35.343028
1242.273351	126514.197574	35.348045
1244.020209	126708.985078	35.353063
1244.849789	126917.043368	35.358080
1246.024216	127110.075277	35.363098
1247.133402	127304.575706	35.368116
1248.097072	127517.329623	35.373133
1249.490273	127716.424235	35.378151
1250.281548	127924.888956	35.383168
1251.777015	128145.265324	35.388186
1253.075184	128367.435700	35.393204
1253.884390	128582.274639	35.398221
1255.550687	128794.533984	35.403239
1256.660252	129012.799651	35.408256
1258.126471	129227.361777	35.413274
1259.174229	129443.765703	35.418292
1260.739975	129663.927605	35.423309
1261.906880	129879.150440	35.428327
1262.990362	130109.730344	35.433344
1264.334253	130324.865128	35.438362
1265.502400	130550.671624	35.443380
1266.743343	130771.058575	35.448397
1268.275843	130993.351990	35.453415
1269.212065	131223.774413	35.458432
1271.019808	131439.224072	35.463450
1272.404933	131659.658401	35.468468
1273.718797	131887.568284	35.473485
1275.310859	132096.076182	35.478503
1276.444090	132312.906712	35.483520
1278.517151	132523.039060	35.488538
1279.704254	132732.756316	35.493556
1281.311495	132948.173297	35.498573
1282.466458	133133.406996	35.503591
1283.293733	133341.057304	35.508608
1285.047370	133550.690506	35.513626
1286.506757	133747.600031	35.518644
1287.689167	133942.831722	35.523661
1289.288207	134141.673039	35.528679
1290.300679	134348.680326	35.533696
1291.563137	134543.700634	35.538714
1292.889030	134727.029466	35.543732
1293.905891	134920.608847	35.548749
1295.162368	135111.718557	35.553767
1296.133973	135293.840176	35.558784
1297.650233	135482.364104	35.563802
1298.696769	135680.695607	35.568820
1300.016195	135880.150864	35.573837
1301.592067	136077.729335	35.578855
1302.595749	136270.914309	35.583872
1303.411604	136456.996191	35.588890
1305.305647	136665.983374	35.593908
1306.476622	136866.419352	35.598925
1307.922931	137067.408519	35.603943
1309.696025	137250.593437	35.608960
1311.112466	137439.171195	35.613978
1312.210396	137636.164512	35.618996
1313.188735	137835.611253	35.624013
1314.689846	138037.485392	35.629031
1315.483726	138249.548018	35.634048
1317.225482	138450.588348	35.639066
1318.663988	138652.425935	35.644084
1319.560255	138870.787747	35.649101
1320.814723	139070.946592	35.654119
1321.882664	139288.688546	35.659136
1323.542852	139504.208866	35.664154
1324.670908	139714.708025	35.669172
1325.469749	139939.847940	35.674189
1326.956204	140155.476596	35.679207
1328.525277	140376.315137	35.684224
1329.611561	140610.450566	35.689242
1330.961471	140839.362377	35.694260
1332.344922	141062.795526	35.699277
1333.447406	141294.170792	35.704295
1334.382469	141535.257334	35.709312
1336.293470	141759.029998	35.714330
1337.400469	141998.521298	35.719348
1338.737215	142240.069213	35.724365
1340.476295	142471.136774	35.729383
1341.794718	142707.596206	35.734400
1342.813296	142937.108774	35.739418
1344.365556	143169.466071	35.744436
1345.693763	143407.310867	35.749453
1347.130041	143644.722051	35.754471
1348.550794	143891.402899	35.759488
1350.248573	144103.933197	35.764506
1351.605347	144343.922736	35.769524
1352.557513	144581.684223	35.774541
1354.436012	144814.166798	35.779559
1355.750847	145045.130919	35.784576
1356.635223	145271.411855	35.789594
1358.339289	145511.228428	35.794612
1359.398334	145754.787275	35.799629
1360.903278	145977.209996	35.804647
1361.989470	146226.244115	35.809664
1364.617795	146441.786040	35.814682
1366.100396	146647.865063	35.819700
1367.230732	146860.516946	35.824717
1368.456459	147048.499868	35.829735
1369.890270	147260.269572	35.834752
1370.908518	147464.589645	35.839770
1372.481769	147677.506192	35.844788
1373.680990	147900.764282	35.849805
1375.104140	148100.840822	35.854823
1376.055949	148322.683368	35.859840
1377.461708	148526.796528	35.864858
1378.901887	148752.063223	35.869876
1380.112948	148983.566946	35.874893
1381.341625	149198.956992	35.879911
1383.053845	149421.370828	35.884928
1384.185655	149655.642907	35.889946
1385.409652	149885.642449	35.894964
1386.624358	150118.560902	35.899981
1387.919968	150346.916942	35.904999
1389.196823	150601.228604	35.910016
1390.416376	150840.528283	35.915034
1392.039510	151071.423591	35.920052
1393.299876	151327.188786	35.925069
1394.820850	151560.144910	35.930087
1396.509014	151811.231106	35.935104
1397.740929	152059.247536	35.940122
1399.408795	152303.266288	35.945140
1401.238643	152536.674676	35.950157
1402.601233	152778.082988	35.955175
1403.538359	153034.331159	35.960192
1404.750526	153264.559081	35.965210
1406.401173	153516.805233	35.970228
1407.686638	153773.295332	35.975245
1409.233844	154020.211257	35.980263
1410.693561	154263.681535	35.985280
1412.050808	154515.842360	35.990298
1413.291080	154768.226527	35.995316
1414.734861	155025.981615	36.000333
1416.162853	155286.568678	36.005351
1416.969277	155541.005531	36.010368
1418.531250	155814.812734	36.015386
1420.051921	156074.199223	36.020404
1421.264682	156353.493145	36.025421
1422.528455	156602.729923	36.030439
1424.165203	156883.875451	36.035456
1425.364241	157148.000089	36.040474
1427.467749	157415.305228	36.045492
1429.229771	157673.866596	36.050509
1431.279140	157927.007762	36.055527
1432.940612	158180.199735	36.060544
1434.282003	158428.828697	36.065562
1435.969921	158671.216220	36.070580
1437.107092	158921.783240	36.075597
1438.961893	159158.035515	36.080615
1440.103880	159400.109052	36.085632
1441.592906	159640.772245	36.090650
1443.061638	159876.799039	36.095668
1444.116384	160099.514583	36.100685
1445.798277	160319.557587	36.105703
1447.151787	160558.130802	36.110720
1448.296681	160776.042739	36.115738
1450.067404	161000.146576	36.120756
1451.164421	161242.797846	36.125773
1452.693852	161472.789190	36.130791
1454.269991	161705.983065	36.135808
1455.853800	161941.878461	36.140826
1457.234483	162174.878168	36.145844
1458.184593	162422.734970	36.150861
1459.725419	162654.862641	36.155879
1461.039948	162906.761161	36.160896
1462.343016	163155.543425	36.165914
1464.108012	163409.149368	36.170932
1465.404373	163652.609526	36.175949
1466.811935	163906.580102	36.180967
1468.040283	164163.650099	36.185984
1469.690195	164416.507685	36.191002
1471.164393	164666.541312	36.196020
1472.567819	164931.858017	36.201037
1474.306624	165185.607242	36.206055
1476.052427	165445.571774	36.211072
1477.320417	165692.448986	36.216090
1479.054073	165942.297814	36.221108
1480.712036	166207.431004	36.226125
1482.253228	166461.207653	36.231143
1483.702669	166719.160771	36.236160
1485.009269	166977.277875	36.241178
1486.641968	167241.039885	36.246196
1488.171211	167493.151164	36.251213
1489.487027	167746.705935	36.256231
1490.939586	168005.047866	36.261248
1492.319677	168271.279811	36.266266
1494.322168	168526.240079	36.271284
1495.275620	168788.788942	36.276301
1496.673847	169053.108152	36.281319
1498.168962	169334.131719	36.286336
1499.824914	169599.618753	36.291354
1501.689681	169855.827445	36.296372
1502.684761	170138.077917	36.301389
1504.379401	170397.881594	36.306407
1506.036726	170660.800702	36.311424
1507.340009	170940.496453	36.316442
1508.763648	171215.025001	36.321460
1510.344912	171482.008214	36.326477
1511.879302	171751.664561	36.331495
1513.686453	172015.266641	36.336512
1515.170856	172297.936989	36.341530
1516.597785	172561.412837	36.346548
1518.144850	172843.696561	36.351565
1519.581947	173101.770373	36.356583
1521.099610	173365.871410	36.361600
1522.445081	173649.055480	36.366618
1524.402482	173899.123209	36.371636
1525.630995	174150.678363	36.376653
1526.986136	174403.749970	36.381671
1528.513847	174652.152659	36.386688
1529.479367	174922.364799	36.391706
1531.341115	175170.806401	36.396724
1532.477233	175433.142081	36.401741
1534.099027	175716.309402	36.406759
1535.792777	175969.451133	36.411776
1537.309896	176232.835129	36.416794
1539.013711	176506.860582	36.421812
1540.742709	176770.125547	36.426829
1542.691655	177019.160762	36.431847
1544.122543	177291.458622	36.436864
1545.808984	177544.699973	36.441882
1547.837169	177801.276002	36.446900
1549.443363	178061.143158	36.451917
1551.158473	178306.505897	36.456935
1552.810193	178552.806306	36.461952
1554.288872	178816.935922	36.466970
1556.046111	179065.734648	36.471988
1557.528998	179318.574963	36.477005
1559.005611	179569.755714	36.482023
1560.306598	179833.336255	36.487040
1561.873365	180103.448423	36.492058
1563.869330	180350.174012	36.497076
1565.094650	180610.941987	36.502093
1566.438058	180869.434332	36.507111
1568.438230	181127.938092	36.512128
1569.713237	181396.214200	36.517146
1571.359103	181655.513292	36.522164
1572.644933	181924.235021	36.527181
1574.294041	182193.611242	36.532199
1575.933208	182461.290456	36.537216
1577.130126	182732.949591	36.542234
1578.964702	182996.946750	36.547252
1580.050982	183291.364739	36.552269
1581.300284	183568.933581	36.557287
1583.271766	183863.202064	36.562304
1584.618734	184145.859871	36.567322
1586.416115	184428.447920	36.572340
1587.726301	184712.777394	36.577357
1589.629700	184991.558126	36.582375
1591.654665	185279.026042	36.587392
1593.081812	185568.494125	36.592410
1595.166020	185831.605462	36.597428
1596.817658	186120.648027	36.602445
1598.321825	186406.733813	36.607463
1599.764463	186677.210302	36.612480
1601.119084	186963.500957	36.617498
1602.608140	187233.376921	36.622516
1604.665146	187519.914769	36.627533
1606.008719	187810.590387	36.632551
1607.477077	188104.458552	36.637568
1608.903699	188394.401282	36.642586
1610.741382	188661.286046	36.647604
1612.133296	188923.623901	36.652621
1613.724410	189179.687976	36.657639
1615.475392	189453.621380	36.662656
1616.971907	189723.053620	36.667674
1618.450395	189990.586677	36.672692
1620.110196	190259.678748	36.677709
1621.891432	190529.603311	36.682727
1623.282652	190790.086022	36.687744
1624.981340	191077.514502	36.692762
1626.857445	191350.030184	36.697780
1628.413310	191620.605786	36.702797
1629.621975	191913.269529	36.707815
1631.631865	192176.707239	36.712832
1633.024511	192475.652557	36.717850
1634.561870	192743.280265	36.722868
1636.344624	193032.394795	36.727885
1637.829988	193321.621697	36.732903
1639.809848	193597.166573	36.737920
1641.237517	193911.649236	36.742938
1643.001773	194175.428472	36.747956
1644.906008	194481.678360	36.752973
1646.763647	194752.159646	36.757991
1648.455043	195039.333045	36.763008
1650.208152	195322.652641	36.768026
1651.876600	195607.954498	36.773044
1653.661042	195903.621549	36.778061
1655.378660	196178.600202	36.783079
1657.061559	196453.319299	36.788096
1658.492978	196761.206359	36.793114
1660.156286	197035.804729	36.798132
1661.577793	197333.251027	36.803149
1663.009302	197629.263186	36.808167
1664.688633	197916.403704	36.813184
1666.202025	198226.583688	36.818202
1667.767652	198517.400974	36.823220
1669.713689	198816.320825	36.828237
1671.323426	199130.006643	36.833255
1673.433604	199420.577364	36.838272
1674.815506	199730.977354	36.843290
1676.679297	200025.842579	36.848308
1678.346312	200321.362613	36.853325
1679.826307	200625.773727	36.858343
1681.827022	200921.205937	36.863360
1683.636057	201235.088055	36.868378
1685.612029	201514.571987	36.873396
1687.551568	201801.996468	36.878413
1689.479412	202099.718665	36.883431
1691.532128	202371.388261	36.888448
1692.932552	202661.530332	36.893466
1694.851135	202939.177255	36.898484
1697.167120	203231.690214	36.903501
1699.171628	203495.045828	36.908519
1700.876170	203764.695644	36.913536
1702.390188	204023.599897	36.918554
1704.300472	204274.826045	36.923572
1705.586216	204502.376652	36.928589
1707.573933	204748.426126	36.933607
1709.131514	204985.037084	36.938624
1710.844272	205243.077441	36.943642
1712.192003	205476.435938	36.948660
1714.807835	205711.130013	36.953677
1716.652235	205940.438201	36.958695
1718.509072	206175.851281	36.963712
1720.088971	206419.332122	36.968730
1721.517520	206641.854096	36.973748
1723.091043	206899.416042	36.978765
1724.656243	207137.240413	36.983783
1726.057118	207389.944487	36.988800
1727.537337	207644.503136	36.993818
1729.157095	207909.348795	36.998836
1730.953056	208174.396140	37.003853
1732.071011	208439.285700	37.008871
1733.741960	208695.786163	37.013888
1735.576763	208976.191602	37.018906
1737.527950	209238.476803	37.023924
1739.535549	209500.652600	37.028941
1741.214458	209777.633376	37.033959
1743.077151	210049.584318	37.038976
1744.475758	210327.856159	37.043994
1746.618535	210596.515032	37.049012
1748.191706	210881.896332	37.054029
1749.854819	211159.330034	37.059047
1751.728525	211442.203233	37.064064
1753.502972	211712.956570	37.069082
1755.045751	211995.948228	37.074100
1756.494001	212278.321355	37.079117
1758.352785	212565.277134	37.084135
1760.422781	212844.303923	37.089152
1762.314863	213146.301364	37.094170
1763.558399	213420.700910	37.099188
1765.531713	213707.453064	37.104205
1766.798439	214009.058592	37.109223
1768.742173	214300.845580	37.114240
1770.541577	214599.576087	37.119258
1772.520212	214903.980005	37.124276
1774.398262	215190.779021	37.129293
1775.917816	215497.543788	37.134311
1777.964992	215797.903435	37.139328
1779.452027	216099.813395	37.144346
1781.381370	216383.193949	37.149364
1783.361302	216683.415766	37.154381
1784.713231	216987.052350	37.159399
1786.876847	217285.025706	37.164416
1788.747650	217591.248794	37.169434
1790.332380	217894.242889	37.174452
1792.509717	218174.074326	37.179469
1794.005453	218486.759931	37.184487
1795.961063	218783.655265	37.189504
1797.746507	219078.001373	37.194522
1799.795990	219355.496077	37.199540
1801.925538	219611.419736	37.204557
1803.732507	219891.354689	37.209575
1805.538771	220151.216821	37.214592
1807.302600	220420.584005	37.219610
1808.731496	220686.539020	37.224628
1810.683683	220951.599292	37.229645
1812.133996	221223.177648	37.234663
1814.396268	221481.461040	37.239680
1815.769013	221825.771032	37.244698
1817.640258	222105.221531	37.249716
1819.619471	222377.532667	37.254733
1821.253381	222667.714086	37.259751
1823.664291	222952.173655	37.264768
1825.563750	223238.289942	37.269786
1827.098752	223520.795522	37.274804
1828.630777	223804.102535	37.279821
1829.845799	224098.495153	37.284839
1831.631277	224383.592456	37.289856
1833.488614	224690.100492	37.294874
1835.234435	224989.872153	37.299892
1837.308515	225303.357294	37.304909
1838.878137	225615.907875	37.309927
1840.643830	225920.593880	37.314944
1842.309276	226236.356877	37.319962
1844.163622	226552.014896	37.324980
1846.045421	226870.996645	37.329997
1847.920573	227196.355123	37.335015
1849.889751	227509.560445	37.340032
1851.876039	227838.027482	37.345050
1853.645486	228160.384216	37.350068
1855.880847	228474.947604	37.355085
1857.532439	228802.684117	37.360103
1859.307725	229121.310139	37.365120
1861.004355	229435.733897	37.370138
1863.021612	229767.428651	37.375156
1865.390394	230078.954306	37.380173
1867.210423	230409.133498	37.385191
1869.011000	230733.297809	37.390208
1871.082109	231044.696227	37.395226
1872.555437	231370.438560	37.400244
1874.688640	231695.696333	37.405261
1876.373004	232025.928219	37.410279
1878.666477	232349.715143	37.415296
1880.852306	232679.564936	37.420314
1882.791241	232988.298581	37.425332
1884.872825	233302.267955	37.430349
1886.743482	233626.024679	37.435367
1888.965655	233932.201948	37.440384
1890.663983	234248.444811	37.445402
1892.484745	234563.145345	37.450420
1894.529767	234871.664859	37.455437
1896.523614	235172.980268	37.460455
1898.517736	235485.776666	37.465472
1900.552748	235789.043040	37.470490
1901.986691	236083.998726	37.475508
1904.021878	236362.147435	37.480525
1905.603223	236661.424539	37.485543
1907.592354	236938.362930	37.490560
1909.332578	237231.444488	37.495578
1911.001319	237524.995371	37.500596
1913.077090	237812.970845	37.505613
1914.829466	238126.422975	37.510631
1916.634831	238420.741953	37.515648
1918.349002	238726.683668	37.520666
1919.779068	239039.071949	37.525684
1922.102681	239344.639232	37.530701
1923.341737	239675.855172	37.535719
1925.257892	239998.328746	37.540736
1927.509793	240312.926838	37.545754
1929.150310	240643.396032	37.550772
1931.377356	240968.947107	37.555789
1933.418696	241300.268910	37.560807
1935.295570	241620.136949	37.565824
1937.328840	241948.820212	37.570842
1939.349091	242279.817825	37.575860
1941.683668	242601.774790	37.580877
1943.100153	242935.181364	37.585895
1945.211745	243263.906459	37.590912
1947.343981	243596.337572	37.595930
1949.242642	243933.429477	37.600948
1950.945577	244262.729964	37.605965
1953.071828	244609.998476	37.610983
1955.421807	244947.072147	37.616000
1957.018783	245284.850362	37.621018
1959.112228	245627.097359	37.626036
1961.450142	245955.183573	37.631053
1963.282920	246298.870629	37.636071
1965.236638	246639.643623	37.641088
1967.763090	246965.466982	37.646106
1969.466416	247305.189041	37.651124
1971.713185	247642.539555	37.656141
1973.641431	247971.584404	37.661159
1975.920145	248303.698709	37.666176
1977.957028	248619.849326	37.671194
1979.906215	248952.880969	37.676212
1982.099380	249275.663267	37.681229
1983.746959	249617.812459	37.686247
1985.557441	249943.400185	37.691264
1988.201679	250286.688131	37.696282
1989.724872	250622.762816	37.701300
1991.965822	250955.777705	37.706317
1993.724394	251277.845468	37.711335
1995.844786	251611.439606	37.716352
1998.075074	251940.190615	37.721370
2000.160173	252270.590990	37.726388
2002.242930	252587.122937	37.731405
2004.385188	252919.014143	37.736423
2006.130770	253246.066311	37.741440
2008.803889	253551.888244	37.746458
2010.341788	253852.988196	37.751476
2012.115966	254158.064658	37.756493
2013.919258	254449.648464	37.761511
2016.221716	254753.803767	37.766528
2018.089760	255059.704999	37.771546
2019.808817	255363.598151	37.776564
2021.805617	255668.590786	37.781581
2023.749162	255971.941164	37.786599
2025.513681	256284.465213	37.791616
2027.697864	256611.504085	37.796634
2029.168206	256927.962286	37.801652
2031.253891	257245.186990	37.806669
2033.155120	257570.443175	37.811687
2034.982531	257907.726910	37.816704
2037.334163	258239.720436	37.821722
2039.050675	258584.719686	37.826740
2041.131979	258909.466471	37.831757
2043.272924	259255.008974	37.836775
2045.361884	259604.472201	37.841792
2048.045932	259928.108542	37.846810
2049.859634	260272.154732	37.851828
2051.812170	260616.255536	37.856845
2053.952487	260956.795981	37.861863
2055.936418	261298.377751	37.866880
2058.400071	261647.911114	37.871898
2060.089439	261996.424584	37.876916
2062.771449	262334.873835	37.881933
2064.756485	262673.129176	37.886951
2066.567575	263012.784221	37.891968
2069.197122	263347.279978	37.896986
2071.264586	263695.659062	37.902004
2073.390405	264041.209491	37.907021
2075.391681	264387.592898	37.912039
2077.408395	264724.371805	37.917056
2079.799793	265068.534674	37.922074
2081.584241	265417.061841	37.927092
2083.685157	265760.661690	37.932109
2086.309730	266099.504559	37.937127
2088.803120	266443.626952	37.942144
2090.947913	266769.641603	37.947162
2092.776716	267107.417481	37.952180
2094.850769	267433.316770	37.957197
2096.781880	267780.399842	37.962215
2099.072832	268116.223210	37.967232
2101.055312	268446.151334	37.972250
2102.994298	268801.439023	37.977268
2105.184708	269134.281308	37.982285
2107.138310	269487.509376	37.987303
2108.728391	269845.139248	37.992320
2111.285148	270184.503366	37.997338
2113.067418	270538.927644	38.002356
2115.075543	270889.683556	38.007373
2117.318830	271244.543043	38.012391
2119.364160	271590.873111	38.017408
2122.256142	271926.679005	38.022426
2124.295350	272249.308873	38.027444
2126.662624	272558.346769	38.032461
2128.770207	272858.687145	38.037479
2130.842253	273187.942282	38.042496
2132.977449	273492.774778	38.047514
2134.800136	273810.815846	38.052532
2137.012886	274118.176451	38.057549
2138.839917	274442.847176	38.062567
2140.645921	274770.061595	38.067584
2142.960741	275099.710259	38.072602
2144.721291	275437.169472	38.077620
2146.825373	275768.274143	38.082637
2148.668128	276115.576814	38.087655
2150.840718	276462.928756	38.092672
2153.301264	276808.837799	38.097690
2155.103486	277158.356874	38.102708
2157.230687	277511.558644	38.107725
2159.144429	277868.376073	38.112743
2161.237130	278238.349390	38.117760
2163.763644	278582.088321	38.122778
2165.255149	278959.676168	38.127796
2167.655953	279330.946652	38.132813
2169.953661	279695.425247	38.137831
2171.909502	280069.992228	38.142848
2174.305368	280443.320701	38.147866
2176.647791	280818.969168	38.152884
2178.843467	281197.714510	38.157901
2181.151707	281567.804669	38.162919
2183.369557	281948.070254	38.167936
2185.687078	282322.350025	38.172954
2187.895403	282697.180334	38.177972
2190.518436	283077.355499	38.182989
2192.766605	283451.315241	38.188007
2194.325555	283837.272682	38.193024
2196.958396	284200.298276	38.198042
2199.028088	284578.019684	38.203060
2202.026473	284950.411252	38.208077
2204.033816	285326.490676	38.213095
2206.203208	285701.451716	38.218112
2208.403531	286068.354722	38.223130
2210.529329	286444.490479	38.228148
2213.268017	286824.542323	38.233165
2215.522073	287190.851395	38.238183
2217.353114	287577.524090	38.243200
2219.748956	287946.629571	38.248218
2221.805247	288321.504111	38.253236
2224.146174	288700.194293	38.258253
2227.084379	289069.060011	38.263271
2228.980062	289436.820440	38.268288
2231.631602	289798.897337	38.273306
2233.836795	290167.877867	38.278324
2236.151918	290531.632916	38.283341
2238.471598	290886.673638	38.288359
2240.412151	291247.362562	38.293376
2242.853245	291597.353331	38.298394
2245.066491	291940.063806	38.303412
2247.207328	292273.767393	38.308429
2249.396487	292605.583069	38.313447
2251.501084	292941.171238	38.318464
2253.851359	293275.932486	38.323482
2255.390886	293620.677897	38.328500
2257.420177	293963.617755	38.333517
2259.908304	294307.881442	38.338535
2261.831643	294675.172326	38.343552
2263.913208	295019.727932	38.348570
2266.183818	295389.274082	38.353588
2268.417249	295750.188741	38.358605
2270.609867	296109.229461	38.363623
2272.867475	296490.536756	38.368640
2275.142457	296846.209980	38.373658
2277.559680	297217.786962	38.378676
2279.800121	297592.160025	38.383693
2282.169167	297964.962416	38.388711
2284.106645	298351.396975	38.393728
2286.758007	298722.425693	38.398746
2289.101781	299104.958510	38.403764
2291.239981	299493.238410	38.408781
2293.694535	299867.521830	38.413799
2295.941923	300256.214459	38.418816
2298.323591	300635.384753	38.423834
2301.001834	301029.316096	38.428852
2303.118594	301416.629539	38.433869
2305.771456	301799.767431	38.438887
2308.018673	302195.313619	38.443904
2310.341756	302576.672951	38.448922
2312.657863	302959.912082	38.453940
2314.954372	303342.264286	38.458957
2317.540561	303730.487953	38.463975
2320.028521	304122.510853	38.468992
2322.493198	304501.099372	38.474010
2325.087495	304887.286504	38.479028
2327.271946	305267.136575	38.484045
2330.646675	305625.739867	38.489063
2333.086832	305998.638398	38.494080
2335.374302	306358.986901	38.499098
2337.603272	306745.480584	38.504116
2339.808447	307108.659482	38.509133
2342.136643	307479.437887	38.514151
2344.083344	307862.137508	38.519168
2346.100553	308221.888586	38.524186
2348.788722	308614.247340	38.529204
2350.756816	308994.730257	38.534221
2353.148896	309376.643347	38.539239
2355.620910	309755.138984	38.544256
2358.393826	310138.284630	38.549274
2360.833066	310507.156589	38.554292
2363.474958	310882.522896	38.559309
2365.863652	311258.055099	38.564327
2368.376061	311627.038834	38.569344
2370.678353	311988.460305	38.574362
2373.063005	312333.408930	38.579380
2375.037546	312671.563743	38.584397
2377.020895	313007.684192	38.589415
2379.007384	313354.115028	38.594432
2381.466701	313707.581446	38.599450
2383.587278	314071.234448	38.604468
2385.620385	314433.553926	38.609485
2387.876952	314800.916418	38.614503
2389.885894	315182.438361	38.619520
2392.133217	315553.914155	38.624538
2394.307540	315938.429436	38.629556
2396.444207	316337.502325	38.634573
2398.736584	316731.647108	38.639591
2400.912126	317131.396363	38.644608
2402.844692	317535.093745	38.649626
2405.629454	317963.239323	38.654644
2407.881426	318381.943330	38.659661
2410.725341	318798.875425	38.664679
2412.733655	319224.497001	38.669696
2415.374914	319653.216351	38.674714
2417.765707	320083.446421	38.679732
2420.150349	320510.551597	38.684749
2422.699256	320937.349341	38.689767
2425.029005	321375.786083	38.694784
2428.176966	321804.643426	38.699802
2430.789417	322231.196265	38.704820
2432.946169	322657.793828	38.709837
2435.445480	323086.899998	38.714855
2437.832458	323531.030903	38.719872
2440.448823	323950.717581	38.724890
2443.326769	324378.588948	38.729908
2445.508476	324811.546005	38.734925
2448.922216	325226.046100	38.739943
2451.875632	325644.426354	38.744960
2454.517117	326064.072849	38.749978
2457.178084	326463.677251	38.754996
2459.307340	326873.801277	38.760013
2462.279751	327276.298043	38.765031
2464.693136	327690.613725	38.770048
2466.965470	328098.931011	38.775066
2469.415946	328502.900830	38.780084
2472.015039	328925.357471	38.785101
2474.513528	329331.880111	38.790119
2476.652568	329748.310430	38.795136
2479.011872	330156.704421	38.800154
2481.927376	330572.245260	38.805172
2484.324245	330983.371255	38.810189
2486.945135	331390.193319	38.815207
2489.557725	331801.534439	38.820224
2492.194717	332206.673385	38.825242
2494.845533	332605.357992	38.830260
2497.187971	333011.656328	38.835277
2499.793137	333418.291578	38.840295
2502.313160	333826.867799	38.845312
2504.607951	334201.603677	38.850330
2507.217899	334586.825423	38.855348
2509.201880	334968.487709	38.860365
2511.679634	335341.182378	38.865383
2513.883243	335720.291818	38.870400
2516.086956	336107.448310	38.875418
2518.814446	336487.206765	38.880436
2520.922710	336879.426838	38.885453
2523.414593	337260.513156	38.890471
2525.808439	337674.951466	38.895488
2528.098867	338075.133754	38.900506
2530.382981	338479.935711	38.905524
2532.687282	338894.938999	38.910541
2535.123450	339320.709688	38.915559
2537.475495	339751.848222	38.920576
2539.714708	340182.976296	38.925594
2542.408556	340603.847961	38.930612
2544.745391	341055.114237	38.935629
2547.349832	341486.937103	38.940647
2550.324951	341936.775527	38.945664
2552.684236	342373.683487	38.950682
2555.319006	342825.600402	38.955700
2557.496862	343281.902434	38.960717
2560.300015	343729.495131	38.965735
2562.914816	344200.014762	38.970752
2565.405135	344649.935030	38.975770
2568.504284	345105.518495	38.980788
2570.985501	345570.031299	38.985805
2573.488739	346033.216721	38.990823
2576.222429	346485.089833	38.995840
2578.832085	346947.007016	39.000858
2581.541600	347409.996263	39.005876
2583.978105	347886.886212	39.010893
2586.533536	348345.982571	39.015911
2589.081201	348812.540000	39.020928
2591.879115	349288.599083	39.025946
2594.636956	349755.902202	39.030964
2597.282589	350224.082214	39.035981
2600.018344	350698.082599	39.040999
2602.690822	351169.017208	39.046016
2605.311022	351639.016706	39.051034
2608.161991	352108.594724	39.056052
2610.716871	352579.332406	39.061069
2613.511151	353040.965688	39.066087
2616.493502	353502.336642	39.071104
2618.904667	353975.445255	39.076122
2621.726379	354442.189316	39.081140
2624.247337	354905.829214	39.086157
2626.837990	355366.763226	39.091175
2629.593277	355841.018489	39.096192
2632.126153	356311.928603	39.101210
2634.863442	356769.120678	39.106228
2637.356919	357240.332885	39.111245
2639.839553	357707.988830	39.116263
2642.671536	358166.802859	39.121280
2645.059354	358633.449746	39.126298
2648.039506	359057.306751	39.131316
2650.632496	359491.018534	39.136333
2653.293298	359925.527870	39.141351
2655.595508	360362.932719	39.146368
2658.079342	360797.360653	39.151386
2660.831646	361224.534085	39.156404
2662.815910	361678.601285	39.161421
2665.448441	362122.485633	39.166439
2668.518323	362566.651812	39.171456
2670.765194	363029.394887	39.176474
2673.425132	363502.879397	39.181492
2675.661172	363970.259131	39.186509
2677.960949	364434.578576	39.191527
2680.519363	364915.373594	39.196544
2683.216962	365402.993532	39.201562
2685.928097	365895.910000	39.206580
2688.216131	366386.477203	39.211597
2691.072735	366883.699289	39.216615
2693.949161	367394.895324	39.221632
2696.408758	367897.345777	39.226650
2699.485534	368387.435975	39.231668
2701.907503	368901.909220	39.236685
2704.632561	369420.160095	39.241703
2707.338425	369938.103283	39.246720
2710.143756	370454.730339	39.251738
2713.022218	370952.866716	39.256756
2715.761982	371478.702781	39.261773
2718.534252	372008.079534	39.266791
2721.637769	372525.623692	39.271808
2724.396886	373047.529482	39.276826
2727.584716	373550.483152	39.281844
2730.006975	374077.935303	39.286861
2733.080136	374593.606225	39.291879
2735.833705	375108.001902	39.296896
2738.465974	375648.797090	39.301914
2741.702345	376154.679564	39.306932
2743.964102	376682.300979	39.311949
2746.788594	377199.424247	39.316967
2749.675636	377725.410614	39.321984
2752.354023	378262.053185	39.327002
2755.326697	378785.880785	39.332020
2758.067004	379312.985496	39.337037
2760.877073	379824.850498	39.342055
2764.214466	380351.770492	39.347072
2766.812779	380858.987489	39.352090
2769.669096	381385.183115	39.357108
2772.111376	381912.477152	39.362125
2774.859658	382448.162819	39.367143
2777.774003	382953.881365	39.372160
2780.430333	383478.456171	39.377178
2783.510006	384010.668017	39.382196
2786.234841	384528.926377	39.387213
2788.959864	385065.821305	39.392231
2791.566449	385580.152007	39.397248
2794.321244	386108.529646	39.402266
2797.482469	386593.664641	39.407284
2800.164512	387085.590608	39.412301
2802.557742	387569.515253	39.417319
2805.466976	388058.246907	39.422336
2807.795003	388562.028305	39.427354
2810.770490	389037.826217	39.432372
2813.605747	389546.028051	39.437389
2816.595599	390053.006114	39.442407
2819.080071	390546.716576	39.447424
2821.375623	391072.481631	39.452442
2824.209865	391563.763805	39.457460
2826.901433	392101.801573	39.462477
2829.264902	392622.840784	39.467495
2832.388303	393145.298792	39.472512
2835.072345	393691.250709	39.477530
2838.006555	394228.709713	39.482548
2840.713065	394772.206337	39.487565
2843.491525	395324.203290	39.492583
2846.272461	395859.987097	39.497600
2848.907360	396421.219131	39.502618
2852.233007	396963.289200	39.507636
2855.178300	397534.824466	39.512653
2857.728206	398096.396761	39.517671
2860.462974	398656.789233	39.522688
2863.049600	399237.632069	39.527706
2865.941905	399818.264078	39.532724
2869.091552	400388.424302	39.537741
2872.091208	400963.009854	39.542759
2875.098696	401536.519088	39.547776
2877.833149	402131.281888	39.552794
2881.111730	402702.521626	39.557812
2883.785895	403285.204590	39.562829
2886.880025	403878.001762	39.567847
2890.000823	404463.178194	39.572864
2893.083819	405044.192175	39.577882
2895.905251	405628.405553	39.582900
2898.910435	406202.540336	39.587917
2901.653220	406806.871769	39.592935
2904.575478	407393.165254	39.597952
2907.255323	407981.868665	39.602970
2910.479448	408580.284218	39.607988
2913.459666	409167.041459	39.613005
2915.956593	409769.959120	39.618023
2918.663531	410373.921379	39.623040
2921.465099	410979.732105	39.628058
2923.975859	411585.830036	39.633076
2926.977979	412201.494229	39.638093
2929.986596	412821.250373	39.643111
2933.449708	413429.212725	39.648128
2936.188414	414046.603458	39.653146
2939.193056	414663.939054	39.658164
2942.435177	415279.120560	39.663181
2945.319165	415898.527050	39.668199
2948.586230	416500.044812	39.673216
2951.401950	417096.173183	39.678234
2954.669825	417679.116750	39.683252
2957.776482	418229.943344	39.688269
2960.827919	418787.254778	39.693287
2964.113442	419344.467486	39.698304
2966.622449	419911.243152	39.703322
2969.583119	420463.746844	39.708340
2972.414868	421014.967814	39.713357
2975.073910	421581.584471	39.718375
2978.116996	422152.207856	39.723392
2980.791920	422733.923975	39.728410
2983.666452	423324.438083	39.733428
2986.354493	423913.499570	39.738445
2988.998761	424501.719239	39.743463
2992.041384	425091.180453	39.748480
2994.620437	425713.026733	39.753498
2997.716339	426321.933472	39.758516
3000.690887	426933.150763	39.763533
3003.132609	427565.336434	39.768551
3006.178103	428191.230927	39.773568
3009.977661	428804.478395	39.778586
3013.317715	429425.053794	39.783604
3016.765257	430038.201579	39.788621
3019.707720	430655.366089	39.793639
3022.703665	431277.117105	39.798656
3025.430502	431911.229946	39.803674
3028.455532	432547.610052	39.808692
3031.693791	433178.571678	39.813709
3034.528938	433818.673199	39.818727
3037.674750	434454.758935	39.823744
3040.164466	435107.848749	39.828762
3043.020112	435758.078298	39.833780
3046.153678	436421.237441	39.838797
3048.835306	437093.237185	39.843815
3052.108520	437746.286499	39.848832
3054.962103	438422.097366	39.853850
3058.087131	439097.416439	39.858868
3061.410604	439777.217727	39.863885
3063.982663	440461.676394	39.868903
3067.286314	441130.252724	39.873920
3070.228723	441819.222562	39.878938
3073.392958	442503.682143	39.883956
3076.714719	443182.325543	39.888973
3080.214811	443871.452484	39.893991
3083.821683	444537.962756	39.899008
3086.720787	445223.348796	39.904026
3089.589671	445907.454260	39.909044
3092.869335	446592.689950	39.914061
3095.970070	447267.961537	39.919079
3099.157234	447944.516189	39.924096
3101.967504	448643.028957	39.929114
3105.267639	449321.044457	39.934132
3108.693003	450001.348692	39.939149
3111.271997	450690.118227	39.944167
3114.341590	451372.412325	39.949184
3117.314070	452052.221545	39.954202
3120.113945	452719.334748	39.959220
3123.401977	453358.567074	39.964237
3125.744663	454018.275033	39.969255
3129.193822	454683.557744	39.974272
3132.256069	455332.385055	39.979290
3135.283589	455994.305204	39.984308
3138.462981	456664.733332	39.989325
3141.349371	457341.866787	39.994343
3144.724859	458005.544308	39.999360
3147.383603	458683.583527	40.004378
3150.259002	459372.040767	40.009396
3153.571331	460064.454759	40.014413
3156.591805	460760.535594	40.019431
3159.659596	461458.053807	40.024448
3162.818865	462160.593972	40.029466
3166.004144	462873.578660	40.034484
3169.148274	463593.021141	40.039501
3172.284911	464306.320070	40.044519
3175.920410	465028.064583	40.049536
3179.064961	465761.748573	40.054554
3181.972441	466477.691693	40.059572
3185.781579	467203.077457	40.064589
3188.704388	467935.709443	40.069607
3191.873368	468663.118422	40.074624
3194.947011	469401.642802	40.079642
3198.338752	470135.539381	40.084660
3201.636337	470876.251474	40.089677
3204.693374	471605.698837	40.094695
3208.163982	472350.224102	40.099712
3211.481882	473102.128515	40.104730
3214.652708	473844.674810	40.109748
3218.318458	474581.099225	40.114765
3221.680307	475319.112159	40.119783
3225.065675	476065.082007	40.124800
3228.347032	476802.547714	40.129818
3231.654838	477546.048178	40.134836
3235.000216	478281.882049	40.139853
3238.260644	479031.956414	40.144871
3241.250885	479764.556390	40.149888
3244.913303	480509.153261	40.154906
3247.754446	481248.747093	40.159924
3251.199643	482002.823386	40.164941
3254.254020	482757.791457	40.169959
3257.585554	483500.456716	40.174976
3260.836068	484266.503396	40.179994
3264.156511	485004.210817	40.185012
3267.913715	485747.985467	40.190029
3270.768773	486500.109914	40.195047
3274.378044	487257.946417	40.200064
3278.079561	488000.277819	40.205082
3281.340208	488756.240197	40.210100
3284.535758	489484.346159	40.215117
3287.598908	490247.504234	40.220135
3291.228437	490969.118704	40.225152
3293.768812	491718.205498	40.230170
3296.778197	492440.972330	40.235188
3300.101944	493151.892462	40.240205
3302.883470	493866.052977	40.245223
3306.240335	494573.680549	40.250240
3309.224466	495292.349653	40.255258
3311.896239	496029.473144	40.260276
3315.200635	496758.386799	40.265293
3318.419844	497500.565624	40.270311
3321.556263	498236.617113	40.275328
3324.710114	498996.165903	40.280346
3327.858619	499768.356829	40.285364
3331.051242	500521.725441	40.290381
3334.247229	501299.749995	40.295399
3337.357879	502080.530690	40.300416
3340.855872	502872.019061	40.305434
3344.210482	503667.886434	40.310452
3347.362074	504447.546415	40.315469
3350.743269	505256.361000	40.320487
3353.814749	506071.950574	40.325504
3357.210054	506893.709170	40.330522
3360.504482	507712.769944	40.335540
3363.707060	508537.509128	40.340557
3366.883215	509379.723971	40.345575
3369.955392	510198.701656	40.350592
3373.656152	511068.352917	40.355610
3376.975029	511902.145666	40.360628
3380.410342	512742.488505	40.365645
3384.072386	513615.193956	40.370663
3387.829177	514454.845730	40.375680
3391.385030	515288.938168	40.380698
3395.089603	516168.970141	40.385716
3398.963941	516988.046436	40.390733
3402.141950	517874.326107	40.395751
3405.601224	518677.597256	40.400768
3409.170765	519565.539941	40.405786
3412.435748	520394.882362	40.410804
3416.080757	521245.100774	40.415821
3419.537425	522117.895215	40.420839
3423.305402	522945.465185	40.425856
3426.784783	523842.819932	40.430874
3430.291165	524676.090493	40.435892
3434.223480	525489.790394	40.440909
3437.470106	526356.843056	40.445927
3440.735070	527220.216244	40.450944
3444.732548	528037.254207	40.455962
3448.147785	528894.010144	40.460980
3451.693244	529763.652165	40.465997
3454.694730	530590.039743	40.471015
3458.828277	531428.703046	40.476032
3462.110596	532269.219666	40.481050
3465.411722	533123.646139	40.486068
3469.002065	533991.685328	40.491085
3472.204230	534814.038075	40.496103
3476.176800	535639.500047	40.501120
3479.583897	536513.542217	40.506125
3482.784775	537267.408964	40.511130
3486.321201	537976.641514	40.516135
3489.641581	538652.190930	40.521140
3492.322498	539254.941243	40.526144
3495.674044	539777.876857	40.531149
3498.168425	540262.401607	40.536154
3501.022084	540681.514401	40.541159
3503.145130	541090.531416	40.546164
3505.092753	541409.235193	40.551168
3507.645320	541638.871388	40.556173
3509.299241	541829.515976	40.561178
3510.764087	541973.585770	40.566183
3512.822272	542073.381959	40.571188
3514.174894	542136.381210	40.576192
3515.358697	542205.919995	40.581197
3516.467257	542171.210120	40.586202
3518.020496	542095.735287	40.591207
3518.454775	542085.922181	40.596212
3519.314369	541962.187122	40.601216
3520.401742	541788.479850	40.606221
3520.778451	541682.742991	40.611226
3521.276088	541490.898217	40.616231
3522.009625	541270.939958	40.621236
3522.290281	541102.906441	40.626240
3522.867175	540881.452464	40.631245
3522.962460	540636.187455	40.636250
3523.318098	540370.679154	40.641255
3523.040168	540109.457513	40.646260
3523.343329	539818.750135	40.651264
3524.101650	539532.459581	40.656269
3524.050478	539283.862902	40.661274
3524.069967	538949.400941	40.666279
3523.902837	538676.572543	40.671284
3523.914822	538338.613749	40.676288
3524.139551	538064.247873	40.681293
3523.416684	537754.976999	40.686298
3523.726299	537407.354728	40.691303
3523.751860	537088.053018	40.696308
3523.403291	536805.118542	40.701312
3523.374338	536466.872253	40.706317
3523.139883	536157.188821	40.711322
3522.923293	535844.162631	40.716327
3522.740167	535499.100480	40.721332
3522.431650	535230.779003	40.726336
3522.357219	534923.166956	40.731341
3521.664630	534598.421036	40.736346
3522.020574	534267.592243	40.741351
3521.584128	533996.036527	40.746356
3521.302347	533655.899386	40.751360
3521.318782	533380.169374	40.756365
3520.828187	533099.563700	40.761370
3520.344185	532789.043864	40.766375
3520.692033	532478.386357	40.771380
3520.311015	532221.239964	40.776384
3520.403425	531891.766331	40.781389
3519.972308	531658.970810	40.786394
3519.955391	531328.441574	40.791399
3519.485084	531076.898747	40.796404
3519.458311	530759.091587	40.801408
3519.132896	530512.923194	40.806413
3519.063120	530241.294655	40.811418
3518.946839	529932.580071	40.816423
3518.126597	529705.779552	40.821428
3518.098362	529455.353618	40.826432
3517.772326	529186.728728	40.831437
3516.955485	528927.272756	40.836442
3516.967217	528663.739936	40.841447
3517.579440	528412.741448	40.846452
3517.099113	528174.191736	40.851456
3517.123524	527971.792939	40.856461
3516.701486	527702.501065	40.861466
3516.518668	527464.247416	40.866471
3515.872841	527253.151864	40.871476
3515.853986	526998.642562	40.876480
3515.968729	526787.167927	40.881485
3515.263643	526585.523805	40.886490
3516.005038	526330.479359	40.891495
3515.307984	526157.788591	40.896500
3514.676196	525912.153083	40.901504
3514.989070	525713.622322	40.906509
3514.576862	525508.531936	40.911514
3514.604882	525297.506200	40.916519
3514.015893	525102.800156	40.921524
3514.035342	524903.497026	40.926528
3514.071397	524727.743327	40.931533
3513.514662	524503.152110	40.936538
3513.415327	524343.388412	40.941543
3512.933961	524141.880372	40.946548
3513.279794	523957.931079	40.951552
3513.095027	523794.131555	40.956557
3512.246232	523607.839635	40.961562
3512.419763	523440.138113	40.966567
3512.454645	523288.936294	40.971572
3512.106256	523103.570482	40.976576
3512.094237	522969.661610	40.981581
3511.943683	522777.436320	40.986586
3512.130270	522643.088941	40.991591
3512.316810	522463.899796	40.996596
3511.341543	522315.527876	41.001600
3511.720750	522146.162742	41.006605
3511.108818	522012.189126	41.011610
3511.343684	521863.520700	41.016615
3511.278526	521701.956107	41.021620
3510.921800	521586.795882	41.026624
3510.710041	521408.871411	41.031629
3510.225125	521308.289750	41.036634
3510.543294	521146.001820	41.041639
3510.425626	521028.575345	41.046644
3510.589813	520876.926192	41.051648
3510.369341	520751.424666	41.056653
3510.204882	520615.700413	41.061658
3510.176077	520481.925409	41.066663
3510.057461	520365.303271	41.071668
3509.674836	520238.154965	41.076672
3509.809508	520100.862360	41.081677
3509.333875	520004.568856	41.086682
3509.517416	519865.345243	41.091687
3509.120615	519766.004201	41.096692
3508.934201	519657.224787	41.101696
3508.928452	519525.208002	41.106701
3508.734674	519447.827546	41.111706
3509.203257	519298.643812	41.116711
3508.775993	519222.057644	41.121716
3508.932261	519107.709034	41.126720
3508.725641	518997.917181	41.131725
3508.684800	518918.436940	41.136730
3508.468574	518801.060661	41.141735
3508.709022	518693.269263	41.146740
3508.552396	518621.592883	41.151744
3508.510065	518500.091202	41.156749
3507.767184	518389.975536	41.161754
3508.199679	518275.223535	41.166759
3508.216547	518234.818484	41.171764
3507.649977	518139.691463	41.176768
3508.091278	518034.999151	41.181773
3508.308646	517924.222937	41.186778
3508.093841	517864.789738	41.191783
3507.856991	517736.284314	41.196788
3507.560750	517671.199695	41.201792
3507.588644	517599.540287	41.206797
3507.309533	517485.097557	41.211802
3507.612687	517427.148546	41.216807
3507.525369	517339.020798	41.221812
3507.399451	517279.015188	41.226816
3507.538459	517168.044029	41.231821
3507.342866	517111.133567	41.236826
3507.208927	517001.923810	41.241831
3507.150664	516934.927594	41.246836
3506.977344	516861.981978	41.251840
3507.392533	516772.810960	41.256845
3507.154050	516710.039695	41.261850
3507.257736	516636.139028	41.266855
3507.401319	516556.820587	41.271860
3506.773657	516470.139064	41.276864
3506.640998	516415.289712	41.281869
3506.711283	516343.921619	41.286874
3506.853366	516269.406391	41.291879
3506.711443	516186.844116	41.296884
3506.585519	516140.134969	41.301888
3507.178377	516055.028415	41.306893
3506.889644	515994.386458	41.311898
3506.989982	515938.841259	41.316903
3506.900999	515845.648535	41.321908
3506.479497	515791.348519	41.326912
3506.749122	515706.392427	41.331917
3506.446352	515660.063906	41.336922
3506.690170	515564.237729	41.341927
3505.972635	515527.077788	41.346932
3506.416402	515442.042253	41.351936
3506.306640	515424.611326	41.356941
3505.892427	515334.602797	41.361946
3506.200612	515286.103092	41.366951
3506.043515	515209.455688	41.371956
3505.857169	515161.944147	41.376960
3506.037827	515115.638858	41.381965
3505.783181	515039.410700	41.386970
3505.870823	515016.384785	41.391975
3506.173158	514952.712211	41.396980
3506.041599	514878.486917	41.401984
3505.844887	514843.519076	41.406989
3505.751543	514777.177240	41.411994
3505.502991	514735.996422	41.416999
3505.946501	514681.707810	41.422004
3505.640910	514626.374149	41.427008
3505.533544	514576.218447	41.432013
3505.484790	514551.746707	41.437018
3505.719295	514467.497969	41.442023
3505.527070	514459.891149	41.447028
3505.536469	514387.158733	41.452032
3505.914385	514353.818698	41.457037
3505.434567	514281.618354	41.462042
3505.600294	514231.367879	41.467047
3505.527560	514215.396615	41.472052
3505.729468	514134.995328	41.477056
3505.764285	514110.408580	41.482061
3505.581125	514038.463774	41.487066
3505.607290	514008.011076	41.492071
3505.250660	513940.190176	41.497076
3505.614182	513912.212948	41.502080
3505.649020	513847.111665	41.507085
3504.971187	513839.631897	41.512090
3505.206247	513761.499669	41.517095
3505.313199	513748.433192	41.522100
3505.116204	513704.409222	41.527104
3505.442289	513645.229566	41.532109
3505.464413	513617.103489	41.537114
3505.546252	513564.284689	41.542119
3505.218059	513529.284314	41.547124
3505.422292	513456.112437	41.552128
3505.641335	513430.079316	41.557133
3505.445767	513409.827331	41.562138
3505.890120	513321.999031	41.567143
3505.600574	513290.431571	41.572148
3505.435930	513249.891408	41.577152
3505.459910	513168.350262	41.582157
3505.467296	513169.512507	41.587162
3505.538910	513099.293780	41.592167
3505.508794	513069.354102	41.597172
3505.472723	513001.630504	41.602176
3505.373919	512980.249902	41.607181
3505.460252	512927.580146	41.612186
3505.268382	512868.833715	41.617191
3505.573067	512840.813432	41.622196
3505.772577	512775.429075	41.627200
3505.849783	512754.930858	41.632205
3505.605250	512672.873353	41.637210
3505.435970	512650.744727	41.642215
3505.542491	512584.565000	41.647220
3505.141153	512556.655841	41.652224
3505.640489	512481.662683	41.657229
3505.210532	512476.874642	41.662234
3505.283950	512397.598235	41.667239
3504.947352	512396.842129	41.672244
3505.470485	512319.315295	41.677248
3505.433393	512306.270472	41.682253
3505.072998	512241.630149	41.687258
3505.225757	512217.983108	41.692263
3505.112186	512172.171503	41.697268
3505.080498	512125.638645	41.702272
3505.495268	512078.832753	41.707277
3505.029654	512059.127681	41.712282
3505.243762	511999.454122	41.717287
3505.127687	511954.906954	41.722292
3505.188740	511919.032356	41.727296
3505.397742	511873.421886	41.732301
3504.883243	511839.863854	41.737306
3505.071505	511805.435892	41.742311
3505.334897	511743.831389	41.747316
3505.032132	511723.442570	41.752320
3505.319143	511681.714372	41.757325
3504.772245	511642.849534	41.762330
3504.707559	511605.830667	41.767335
3504.677663	511576.191834	41.772340
3504.665483	511529.198982	41.777344
3504.894179	511504.982495	41.782349
3504.692854	511487.764315	41.787354
3505.043455	511419.265067	41.792359
3504.606708	511426.669226	41.797364
3504.777213	511370.440255	41.802368
3504.971134	511320.480204	41.807373
3504.630845	511308.241346	41.812378
3504.660313	511243.687363	41.817383
3504.905614	511244.913309	41.822388
3504.423580	511184.942226	41.827392
3504.950030	511164.371083	41.832397
3504.469558	511154.531888	41.837402
3505.042112	511100.160808	41.842407
3504.838853	511093.464792	41.847412
3504.242238	511038.215969	41.852416
3505.085353	510967.967658	41.857421
3504.677985	510988.419109	41.862426
3504.630265	510930.756125	41.867431
3504.737411	510881.972036	41.872436
3504.228053	510899.454995	41.877440
3504.551850	510826.657590	41.882445
3504.494773	510834.406701	41.887450
3504.697362	510789.654349	41.892455
3504.898185	510762.760013	41.897460
3504.417108	510724.742681	41.902464
3505.051627	510705.519806	41.907469
3504.518244	510667.055313	41.912474
3504.464948	510615.311065	41.917479
3504.789170	510584.248626	41.922484
3504.535626	510579.735696	41.927488
3504.799052	510513.017217	41.932493
3504.438604	510477.560334	41.937498
3504.449633	510490.914286	41.942503
3504.494186	510442.088244	41.947508
3504.594049	510387.890792	41.952512
3504.719724	510388.832170	41.957517
3504.513853	510331.698060	41.962522
3504.548389	510304.373976	41.967527
3504.529472	510309.334835	41.972532
3504.534410	510245.893939	41.977536
3504.491207	510230.723698	41.982541
3504.467923	510182.211179	41.987546
3504.554604	510193.529785	41.992551
3504.580318	510134.031247	41.997556
3504.682579	510138.821230	42.002560
3504.732542	510076.738538	42.007565
3504.809131	510055.275944	42.012570
3503.981676	510031.629032	42.017575
3504.617072	509975.018442	42.022580
3504.587067	509990.453506	42.027584
3504.357920	509953.406458	42.032589
3504.667877	509909.798431	42.037594
3504.639274	509915.519805	42.042599
3504.665438	509849.645703	42.047604
3504.555415	509814.906735	42.052608
3504.971478	509824.959324	42.057613
3504.451156	509767.974217	42.062618
3504.787183	509719.656554	42.067623
3504.705486	509706.515608	42.072628
3504.633555	509655.176139	42.077632
3504.693096	509653.851369	42.082637
3504.622550	509601.044348	42.087642
3504.792025	509562.820420	42.092647
3504.628362	509534.716958	42.097652
3504.531618	509515.911892	42.102656
3504.608923	509476.285750	42.107661
3504.315964	509431.557584	42.112666
3504.300605	509450.734680	42.117671
3504.258235	509406.472766	42.122676
3504.489432	509349.367481	42.127680
3504.490237	509341.525477	42.132685
3504.238033	509345.106884	42.137690
3504.133618	509277.834623	42.142695
3504.687855	509256.902651	42.147700
3503.852891	509248.433808	42.152704
3504.731511	509201.546723	42.157709
3504.395855	509205.697878	42.162714
3503.747297	509155.156362	42.167719
3504.621825	509113.834975	42.172724
3504.261120	509124.314315	42.177728
3504.313074	509083.881777	42.182733
3504.202705	509083.190944	42.187738
3504.118837	509046.776694	42.192743
3504.481031	508986.006738	42.197748
3504.130932	509016.469102	42.202752
3504.212798	508981.951088	42.207757
3504.148902	508934.250964	42.212762
3504.042071	508904.164314	42.217767
3504.351867	508921.519806	42.222772
3503.468990	508874.960852	42.227776
3504.362756	508841.174330	42.232781
3504.402837	508802.918571	42.237786
3504.616452	508775.614342	42.242791
3504.540002	508778.560950	42.247796
3504.270346	508778.856581	42.252800
3504.211760	508723.110482	42.257805
3504.414669	508674.709735	42.262810
3504.551148	508676.357832	42.267815
3504.079051	508678.506880	42.272820
3503.841173	508636.348279	42.277824
3503.539468	508607.405003	42.282829
3504.540450	508573.095059	42.287834
3504.608438	508542.524788	42.292839
3504.539551	508515.669563	42.297844
3504.063763	508505.069164	42.302848
3504.340291	508513.373738	42.307853
3504.227582	508480.808101	42.312858
3504.414707	508419.001312	42.317863
3504.289844	508425.092567	42.322868
3504.099565	508430.991776	42.327872
3504.558956	508367.168537	42.332877
3504.560577	508330.891047	42.337882
3504.454751	508325.848212	42.342887
3504.525609	508264.362823	42.347892
3504.458646	508269.382461	42.352896
3504.880611	508200.909677	42.357901
3504.617050	508183.748605	42.362906
3504.586809	508175.506205	42.367911
3504.198262	508136.456578	42.372916
3504.484305	508089.862526	42.377920
3504.640270	508049.967686	42.382925
3504.242139	508035.559963	42.387930
3504.371453	508049.959649	42.392935
3504.066708	508002.851582	42.397940
3504.586972	507952.425369	42.402944
3504.625151	507911.992261	42.407949
3504.106613	507933.274467	42.412954
3503.850135	507921.829489	42.417959
3503.802524	507881.713452	42.422964
3504.223605	507836.716487	42.427968
3504.202517	507856.351640	42.432973
3504.063123	507818.678638	42.437978
3503.800063	507786.843820	42.442983
3504.511094	507760.471316	42.447988
3503.902276	507775.595073	42.452992
3504.398073	507711.004693	42.457997
3504.000110	507712.787954	42.463002
3504.495056	507662.769682	42.468007
3504.670063	507668.662011	42.473012
3504.097113	507624.378189	42.478016
3504.713286	507568.420513	42.483021
3504.367929	507571.460428	42.488026
3503.935648	507560.093596	42.493031
3503.853886	507512.898350	42.498036
3504.061856	507489.084268	42.503040
3504.484693	507501.515276	42.508045
3503.703661	507446.132237	42.513050
3504.051912	507427.355752	42.518055
3504.377202	507402.258042	42.523060
3503.986238	507405.456991	42.528064
3503.975502	507353.746803	42.533069
3504.042323	507364.159630	42.538074
3503.985378	507312.254226	42.543079
3504.037470	507315.889151	42.548084
3504.021608	507299.143438	42.553088
3504.300838	507248.955673	42.558093
3503.963231	507236.460482	42.563098
3503.972136	507239.748055	42.568103
3504.244501	507190.471990	42.573108
3504.113626	507204.407513	42.578112
3503.987476	507157.420712	42.583117
3504.392859	507123.556242	42.588122
3504.144615	507139.483749	42.593127
3503.661316	507107.378895	42.598132
3503.775365	507065.211433	42.603136
3503.952424	507078.744187	42.608141
3504.207705	507021.829799	42.613146
3503.961666	507042.007429	42.618151
3504.174045	507007.717841	42.623156
3504.294306	506951.077562	42.628160
3504.275556	506973.496346	42.633165
3503.989268	506925.623429	42.638170
3504.529255	506873.774162	42.643175
3504.381378	506855.277879	42.648180
3503.981580	506842.134429	42.653184
3504.485829	506846.962992	42.658189
3504.118630	506831.233765	42.663194
3503.863572	506785.379539	42.668199
3504.368170	506765.009012	42.673204
3504.306901	506765.828340	42.678208
3504.179399	506703.812158	42.683213
3503.871520	506701.938029	42.688218
3504.048745	506673.472421	42.693223
3504.238329	506637.667683	42.698228
3503.962847	506649.956677	42.703232
3504.176746	506579.840550	42.708237
3503.773025	506615.021511	42.713242
3504.292453	506567.121455	42.718247
3504.321949	506538.577775	42.723252
3504.171284	506537.589600	42.728256
3504.457212	506499.391093	42.733261
3504.261590	506486.822316	42.738266
3504.207836	506459.809706	42.743271
3504.395767	506418.286815	42.748276
3504.080088	506432.656979	42.753280
3504.042183	506380.998790	42.758285
3504.279363	506351.511146	42.763290
3504.311748	506306.571656	42.768295
3504.298609	506302.778627	42.773300
3503.885670	506315.241389	42.778304
3504.217304	506289.382043	42.783309
3503.866857	506250.170333	42.788314
3504.608881	506199.602778	42.793319
3504.305728	506201.320601	42.798324
3503.880648	506175.884308	42.803329
3504.495550	506138.290840	42.808333
3504.278236	506120.007159	42.813338
3504.282565	506103.661922	42.818343
3504.272850	506085.193583	42.823348
3504.242244	506038.289859	42.828353
3504.155190	506030.106022	42.833357
3504.215432	506001.151780	42.838362
3504.113465	505990.895569	42.843367
3503.910347	505944.777902	42.848372
3503.970020	505954.636073	42.853377
3504.411459	505909.782713	42.858381
3504.094395	505893.994109	42.863386
3504.346538	505862.074325	42.868391
3504.156279	505829.364155	42.873396
3504.097715	505837.469966	42.878401
3504.151245	505773.144708	42.883405
3504.148760	505787.364692	42.888410
3504.064263	505740.519289	42.893415
3504.257837	505749.900979	42.898420
3504.195685	505713.476287	42.903425
3504.645040	505675.604369	42.908429
3504.336392	505677.424319	42.913434
3504.185930	505629.323951	42.918439
3504.345438	505578.998485	42.923444
3504.190247	505614.597615	42.928449
3504.213383	505552.047483	42.933453
3504.060048	505531.071056	42.938458
3503.975884	505519.141816	42.943463
3504.273183	505501.029166	42.948468
3504.200109	505473.562643	42.953473
3504.077719	505441.751895	42.958477
3504.054794	505440.136213	42.963482
3504.371667	505402.487062	42.968487
3504.094835	505369.384877	42.973492
3504.020809	505356.644251	42.978497
3504.339568	505334.479665	42.983501
3504.244499	505310.609296	42.988506
3504.189478	505281.722684	42.993511
3504.330481	505263.229653	42.998516
3503.900461	505240.221809	43.003521
3504.096524	505214.837747	43.008525
3504.259355	505195.531514	43.013530
3504.175876	505169.280680	43.018535
3503.922809	505148.876214	43.023540
3504.035355	505141.874936	43.028545
3504.201175	505124.997205	43.033549
3504.286284	505094.418160	43.038554
3503.889597	505066.445489	43.043559
3504.124722	505038.170485	43.048564
3503.743799	505034.384708	43.053569
3504.269956	505000.952481	43.058573
3504.272048	504984.201704	43.063578
3504.108142	504969.754408	43.068583
3504.491431	504933.308289	43.073588
3504.120796	504907.608509	43.078593
3504.235981	504900.404295	43.083597
3503.805761	504871.373887	43.088602
3504.043341	504842.541513	43.093607
3504.234460	504843.624674	43.098612
3504.163960	504788.222072	43.103617
3504.221728	504804.761219	43.108621
3503.472525	504759.991896	43.113626
3503.760087	504734.491464	43.118631
3504.219891	504736.443078	43.123636
3503.906071	504711.948585	43.128641
3504.602752	504672.517212	43.133645
3504.109119	504690.864247	43.138650
3503.949092	504628.795225	43.143655
3503.946674	504631.528406	43.148660
3503.577395	504595.554785	43.153665
3503.864521	504589.689650	43.158669
3503.470391	504572.393825	43.163674
3503.750739	504543.908450	43.168679
3503.949890	504546.103713	43.173684
3503.334922	504514.267924	43.178689
3503.607200	504530.267353	43.183693
3503.765456	504486.264821	43.188698
3503.436787	504500.081944	43.193703
3503.430298	504464.708603	43.198708
3503.678198	504443.009557	43.203713
3503.654370	504451.616592	43.208717
3503.802338	504419.407003	43.213722
3503.825238	504415.405438	43.218727
3503.802581	504401.998102	43.223732
3503.580445	504379.006872	43.228737
3504.139482	504354.576343	43.233741
3503.358548	504342.705827	43.238746
3503.708432	504332.832689	43.243751
3504.024984	504330.454740	43.248756
3503.978031	504291.241269	43.253761
3503.999095	504276.106264	43.258765
3503.638280	504276.011507	43.263770
3503.907791	504245.604267	43.268775
3503.918968	504230.268353	43.273780
3503.787945	504227.353841	43.278785
3503.780771	504191.119723	43.283789
3503.651218	504182.182619	43.288794
3503.509990	504190.302258	43.293799
3503.899122	504153.853598	43.298804
3503.812906	504143.138340	43.303809
3503.904024	504142.668500	43.308813
3503.888987	504093.682170	43.313818
3503.713306	504105.299264	43.318823
3503.883919	504076.729261	43.323828
3503.859761	504054.212396	43.328833
3503.951232	504038.661191	43.333837
3503.764415	504029.834277	43.338842
3503.929184	503994.939006	43.343847
3503.668635	504003.583676	43.348852
3503.756935	503967.536441	43.353857
3503.671087	503947.407797	43.358861
3503.701600	503962.231350	43.363866
3503.798236	503904.066673	43.368871
3503.986763	503923.622511	43.373876
3503.690629	503905.855060	43.378881
3504.042889	503865.818406	43.383885
3503.934777	503864.873960	43.388890
3503.842584	503837.913986	43.393895
3503.485681	503810.388501	43.398900
3503.729371	503796.331295	43.403905
3503.790594	503822.182899	43.408909
3503.693077	503767.236828	43.413914
3504.046267	503767.535301	43.418919
3503.653661	503730.855066	43.423924
3503.454802	503737.111478	43.428929
3503.624978	503735.768773	43.433933
3503.263049	503708.901845	43.438938
3503.569584	503658.446412	43.443943
3503.508914	503687.455271	43.448948
3503.446294	503688.426783	43.453953
3503.870696	503649.137377	43.458957
3503.479755	503661.800979	43.463962
3503.372899	503636.816785	43.468967
3504.003829	503598.962301	43.473972
3503.648310	503592.742926	43.478977
3503.688008	503599.973874	43.483981
3503.905531	503575.596247	43.488986
3503.579954	503575.242865	43.493991
3503.838612	503523.326931	43.498996
3503.766117	503562.662284	43.504001
3503.249850	503521.699325	43.509005
3503.737378	503477.844666	43.514010
3503.881767	503496.598195	43.519015
3503.959692	503507.264618	43.524020
3503.609138	503456.203928	43.529025
3503.883054	503453.275891	43.534029
3503.624278	503441.524668	43.539034
3503.509926	503403.230853	43.544039
3503.847899	503427.217324	43.549044
3503.799879	503388.356281	43.554049
3503.931899	503358.171683	43.559053
3503.877245	503357.826084	43.564058
3503.815881	503324.635372	43.569063
3503.705063	503336.647604	43.574068
3503.276902	503322.848046	43.579073
3503.624151	503279.015066	43.584077
3503.731918	503288.107976	43.589082
3503.505291	503266.229433	43.594087
3504.043219	503232.032830	43.599092
3503.462014	503256.569707	43.604097
3503.703253	503215.233248	43.609101
3503.623098	503216.207558	43.614106
3503.386601	503197.265915	43.619111
3503.859081	503166.723511	43.624116
3503.712112	503153.183041	43.629121
3503.741607	503160.061505	43.634125
3503.909835	503111.701420	43.639130
3503.628977	503135.937935	43.644135
3504.211230	503081.388390	43.649140
3503.626102	503093.526369	43.654145
3503.512284	503067.074745	43.659149
3504.078499	503044.412663	43.664154
3503.751226	502996.029359	43.669159
3504.118124	503012.875609	43.674164
3503.507062	503024.461009	43.679169
3503.452297	502980.640222	43.684173
3503.351287	502960.715292	43.689178
3503.794525	502929.569763	43.694183
3503.912075	502955.464346	43.699188
3503.636564	502962.745378	43.704193
3503.894119	502923.885624	43.709197
3503.612421	502875.393562	43.714202
3503.764978	502871.016871	43.719207
3503.825265	502897.021814	43.724212
3503.427502	502854.874505	43.729217
3503.566068	502832.482195	43.734221
3503.853646	502806.321017	43.739226
3503.782474	502816.454693	43.744231
3503.772009	502806.080931	43.749236
3503.596781	502807.525798	43.754241
3503.715275	502781.391310	43.759245
3503.911338	502757.269007	43.764250
3503.449437	502788.266023	43.769255
3503.814402	502768.823956	43.774260
3503.580865	502728.320585	43.779265
3503.717258	502715.544784	43.784269
3503.417621	502698.029729	43.789274
3503.728699	502652.075197	43.794279
3503.560499	502673.865141	43.799284
3503.248549	502685.757769	43.804289
3503.721912	502667.158867	43.809293
3503.611717	502647.235035	43.814298
3503.466472	502611.475008	43.819303
3504.220494	502578.761363	43.824308
3503.887705	502574.157638	43.829313
3504.175680	502579.021580	43.834317
3503.974768	502576.370902	43.839322
3503.575670	502537.512867	43.844327
3503.806322	502494.506178	43.849332
3503.936021	502469.736006	43.854337
3503.669801	502443.965507	43.859341
3503.852108	502495.713755	43.864346
3503.857510	502470.153424	43.869351
3503.773355	502420.262341	43.874356
3504.082074	502403.814936	43.879361
3504.083873	502360.945323	43.884365
3504.009722	502404.686865	43.889370
3503.896572	502381.017830	43.894375
3504.109802	502363.775670	43.899380
3503.829855	502333.502601	43.904385
3503.608444	502293.603678	43.909389
3503.257955	502282.929061	43.914394
3503.625926	502258.930748	43.919399
3503.745603	502244.284549	43.924404
3503.636920	502269.507306	43.929409
3503.556434	502255.803798	43.934413
3503.469573	502216.338955	43.939418
3503.546331	502203.470984	43.944423
3503.468115	502195.182735	43.949428
3503.313768	502167.521442	43.954433
3503.222589	502177.608031	43.959437
3503.614436	502179.418839	43.964442
3503.513146	502139.045057	43.969447
3504.456428	502101.036775	43.974452
3503.912229	502136.552581	43.979457
3503.989607	502111.992635	43.984461
3503.524394	502087.923331	43.989466
3503.149045	502051.034421	43.994471
3504.276738	502023.929473	43.999476
3503.596679	502014.825213	44.004481
3503.637792	502044.579892	44.009485
3503.719277	502030.243238	44.014490
3503.512309	501999.451921	44.019495
3504.074216	501968.134105	44.024500
3503.772776	501952.086411	44.029505
3503.724395	501977.654351	44.034509
3503.901889	501951.306857	44.039514
3503.201230	501911.432210	44.044519
3503.332460	501910.905357	44.049524
3503.229761	501909.352575	44.054529
3503.836889	501881.621090	44.059533
3503.776331	501842.151258	44.064538
3503.612087	501871.230080	44.069543
3503.505149	501858.390895	44.074548
3504.184942	501811.009310	44.079553
3503.630127	501827.192543	44.084557
3503.738949	501812.547704	44.089562
3503.846667	501808.430913	44.094567
3503.857519	501755.637899	44.099572
3503.648504	501779.814294	44.104577
3503.462819	501723.104286	44.109581
3503.583217	501692.817458	44.114586
3503.384636	501734.707559	44.119591
3503.284012	501713.566404	44.124596
3503.059562	501679.537929	44.129601
3503.122425	501671.277751	44.134605
3502.892908	501675.920047	44.139610
3503.175807	501665.701709	44.144615
3503.631230	501656.569631	44.149620
3503.334944	501672.560294	44.154625
3504.074820	501640.403929	44.159629
3503.741193	501656.046202	44.164634
3503.518414	501613.159664	44.169639
3503.944726	501627.264615	44.174644
3503.765317	501581.283609	44.179649
3503.550968	501559.147937	44.184653
3503.477887	501596.210052	44.189658
3503.266331	501552.764824	44.194663
3504.054355	501502.682688	44.199668
3503.462009	501554.859818	44.204673
3503.763128	501540.437438	44.209677
3503.611373	501501.892345	44.214682
3503.815821	501472.654786	44.219687
3503.988732	501484.876504	44.224692
3503.906465	501441.613032	44.229697
3503.967234	501467.518764	44.234701
3503.554663	501425.674089	44.239706
3503.966842	501380.864455	44.244711
3503.658231	501400.349817	44.249716
3503.125104	501372.291612	44.254721
3503.905156	501342.507314	44.259725
3503.425441	501360.653128	44.264730
3503.683593	501337.328941	44.269735
3503.650719	501320.428367	44.274740
3503.734825	501312.873292	44.279745
3503.893176	501309.203928	44.284749
3503.321671	501287.428068	44.289754
3503.602771	501253.369485	44.294759
3503.584555	501256.004452	44.299764
3503.638760	501284.897854	44.304769
3503.725128	501237.861625	44.309773
3503.720700	501192.408738	44.314778
3503.913761	501229.125849	44.319783
3503.844070	501185.151136	44.324788
3503.405711	501169.731776	44.329793
3504.235265	501128.196233	44.334797
3503.760381	501118.147976	44.339802
3503.552517	501147.538576	44.344807
3503.630151	501106.779851	44.349812
3503.757266	501061.255220	44.354817
3503.419312	501091.678813	44.359821
3503.634462	501069.626494	44.364826
3503.659288	501041.833894	44.369831
3503.462000	501050.773703	44.374836
3502.874116	501026.621114	44.379841
3503.936059	500992.236141	44.384845
3503.657635	501036.823212	44.389850
3503.440120	500990.391149	44.394855
3503.659576	500980.789854	44.399860
3503.764457	500969.586912	44.404865
3503.692505	500956.235373	44.409869
3503.417366	500950.306062	44.414874
3503.734168	500926.668364	44.419879
3503.273164	500917.731381	44.424884
3503.329257	500936.805281	44.429889
3503.285404	500882.145483	44.434893
3503.479755	500896.034592	44.439898
3503.644905	500882.696138	44.444903
3503.642071	500877.837345	44.449908
3503.738668	500870.330726	44.454913
3503.742956	500829.380490	44.459917
3503.455337	500849.318693	44.464922
3503.557838	500801.873824	44.469927
3503.922744	500810.977978	44.474932
3503.186583	500786.949736	44.479937
3503.745816	500754.617859	44.484941
3503.576311	500785.977085	44.489946
3503.544730	500737.389030	44.494951
3503.378587	500746.577157	44.499956
3503.542521	500719.268245	44.504961
3503.472966	500742.765971	44.509965
3503.507383	500690.320399	44.514970
3503.536630	500683.026818	44.519975
3503.691384	500708.210147	44.524980
3503.234853	500706.409478	44.529985
3503.283683	500654.265230	44.534989
3503.790529	500620.979648	44.539994
3503.658098	500646.765257	44.544999
3503.672548	500644.181484	44.550004
3503.595677	500603.496649	44.555009
3503.673365	500611.988267	44.560013
3503.754018	500586.261480	44.565018
3503.550221	500582.294883	44.570023
3503.645136	500552.668184	44.575028
3503.565701	500545.594199	44.580033
3503.784955	500545.154631	44.585037
3503.520644	500517.761246	44.590042
3503.799441	500478.335989	44.595047
3503.610047	500506.307403	44.600052
3503.414329	500451.518436	44.605057
3503.529441	500458.333795	44.610061
3503.420905	500427.676056	44.615066
3503.369704	500445.501971	44.620071
3503.604829	500417.219591	44.625076
3503.253197	500383.613692	44.630081
3503.352846	500392.355038	44.635085
3502.886312	500397.490698	44.640090
3502.712874	500398.125573	44.645095
3503.074793	500389.615056	44.650100
3503.467590	500381.757700	44.655105
3503.681039	500353.428026	44.660109
3503.678719	500364.868306	44.665114
3503.546734	500345.704623	44.670119
3504.200364	500339.223352	44.675124
3504.014409	500304.426880	44.680129
3503.791271	500308.258616	44.685133
3503.608346	500248.000142	44.690138
3503.727545	500275.821901	44.695143
3503.821197	500224.074267	44.700148
3503.619669	500225.523497	44.705153
3504.065706	500217.961370	44.710157
3504.035725	500187.189563	44.715162
3503.706852	500165.272738	44.720167
3503.671669	500167.050016	44.725172
3503.644291	500148.780738	44.730177
3503.409449	500145.679482	44.735181
3503.718959	500099.566756	44.740186
3503.605497	500130.766413	44.745191
3503.744100	500096.930629	44.750196
3504.099049	500055.973815	44.755201
3503.796435	500070.802655	44.760205
3503.537506	500028.930416	44.765210
3503.407070	500027.027513	44.770215
3503.577863	500015.256737	44.775220
3503.443684	500021.554848	44.780225
3503.680148	499984.919290	44.785229
3503.554860	499965.096080	44.790234
3503.840201	499934.729579	44.795239
3503.670695	499971.152246	44.800244
3503.465336	499936.661846	44.805249
3503.839806	499897.118947	44.810253
3503.661398	499935.011081	44.815258
3503.426116	499890.198811	44.820263
3503.635025	499856.098358	44.825268
3503.025617	499896.184755	44.830273
3502.662865	499870.577646	44.835277
3503.521449	499845.131795	44.840282
3503.295076	499897.509015	44.845287
3503.369204	499857.001096	44.850292
3503.486282	499818.460494	44.855297
3503.646006	499800.060046	44.860301
3503.777274	499843.117338	44.865306
3503.332691	499817.523087	44.870311
3503.321168	499773.333223	44.875316
3503.488476	499744.706157	44.880321
3503.698775	499756.568805	44.885325
3503.733222	499786.935752	44.890330
3503.512881	499763.128319	44.895335
3503.710038	499712.678983	44.900340
3503.457419	499740.307242	44.905345
3503.219059	499722.931429	44.910349
3503.492497	499677.076422	44.915354
3503.468479	499704.314256	44.920359
3503.566040	499714.321783	44.925364
3503.208679	499692.560744	44.930369
3503.721621	499654.463428	44.935373
3503.791137	499622.206916	44.940378
3503.358146	499653.052943	44.945383
3503.398815	499647.427625	44.950388
3503.422428	499604.396073	44.955393
3503.404249	499594.325386	44.960397
3503.523013	499616.478675	44.965402
3503.243125	499584.226702	44.970407
3503.869709	499602.908124	44.975412
3503.338593	499565.481856	44.980417
3503.203019	499547.330309	44.985421
3503.470243	499568.447766	44.990426
3503.452939	499534.281216	44.995431
3503.455394	499548.606675	45.000436
3503.140618	499524.307639	45.005441
3503.637079	499480.188623	45.010445
3503.699626	499526.801036	45.015450
3503.426998	499510.746587	45.020455
3503.275380	499475.791214	45.025460
3503.328027	499455.179994	45.030465
3504.127548	499424.984465	45.035469
3503.793166	499402.561361	45.040474
3503.719668	499426.972625	45.045479
3503.990717	499387.900547	45.050484
3503.371863	499406.880276	45.055489
3503.735872	499389.510170	45.060493
3503.428107	499376.093482	45.065498
3503.122668	499348.401077	45.070503
3503.766160	499333.872184	45.075508
3503.406497	499361.771053	45.080513
3503.261731	499312.640183	45.085517
3503.857083	499279.338124	45.090522
3503.703021	499264.530264	45.095527
3503.526574	499278.580484	45.100532
3503.648746	499296.835735	45.105537
3503.623452	499291.220733	45.110541
3503.745242	499246.806013	45.115546
3503.489114	499228.521332	45.120551
3503.576521	499234.936560	45.125556
3503.227151	499245.976811	45.130561
3503.200524	499229.731361	45.135565
3503.259182	499211.396907	45.140570
3503.462891	499199.721639	45.145575
3503.296309	499170.994568	45.150580
3502.946547	499154.800126	45.155585
3503.624360	499176.814969	45.160589
3503.799774	499130.214728	45.165594
3503.248939	499144.172362	45.170599
3503.588752	499122.351056	45.175604
3503.558880	499121.140874	45.180609
3503.219786	499114.714836	45.185613
3503.215693	499077.609226	45.190618
3503.298669	499048.994381	45.195623
3503.663899	499079.107750	45.200628
3503.430890	499094.736353	45.205633
3503.812726	499048.457629	45.210637
3503.924133	499045.706432	45.215642
3503.166295	499049.471083	45.220647
3503.441535	499012.270564	45.225652
3503.221430	499040.603476	45.230657
3503.494303	498989.279557	45.235661
3503.367454	499001.550355	45.240666
3503.415886	499002.504567	45.245671
3503.716590	498976.690068	45.250676
3503.345295	498981.102354	45.255681
3503.672201	498951.638833	45.260685
3503.418714	498926.823072	45.265690
3503.526759	498943.714095	45.270695
3503.744860	498939.326083	45.275700
3503.314330	498895.605273	45.280705
3503.732009	498884.199719	45.285709
3503.550183	498903.870244	45.290714
3503.045087	498873.829382	45.295719
3503.784678	498818.685095	45.300724
3503.189199	498856.645426	45.305729
3503.276167	498826.409655	45.310733
3503.326835	498834.096415	45.315738
3503.036562	498853.632267	45.320743
3503.296401	498828.380869	45.325748
3503.711400	498791.309673	45.330753
3503.599539	498772.647361	45.335757
3503.038428	498814.196610	45.340762
3503.155217	498794.435091	45.345767
3503.767162	498778.999519	45.350772
3503.220555	498789.716861	45.355777
3502.810664	498759.002655	45.360781
3503.529942	498720.718879	45.365786
3503.193560	498747.501301	45.370791
3503.276557	498758.068521	45.375796
3503.153777	498735.712384	45.380801
3503.292836	498740.398425	45.385805
3503.145100	498739.409342	45.390810
3502.885736	498714.644840	45.395815
3503.003994	498697.717901	45.400820
3503.413175	498677.049435	45.405825
3503.375852	498688.395069	45.410829
3503.175901	498727.305627	45.415834
3503.247365	498716.764667	45.420839
3503.266782	498692.107940	45.425844
3503.089677	498674.265817	45.430849
3503.255854	498684.668061	45.435853
3503.427792	498643.331969	45.440858
3503.437740	498670.970989	45.445863
3503.737348	498624.046066	45.450868
3503.738398	498641.764265	45.455873
3503.528233	498606.968328	45.460877
3503.605874	498604.779264	45.465882
3503.151477	498628.846825	45.470887
3503.651701	498565.741037	45.475892
3503.206823	498589.300906	45.480897
3503.700045	498543.762640	45.485901
3503.879696	498563.477648	45.490906
3503.625491	498537.851479	45.495911
3503.198934	498507.088854	45.500916
3503.309032	498524.030570	45.505921
3503.722503	498508.879260	45.510925
3503.779809	498490.696158	45.515930
3503.637360	498457.661076	45.520935
3503.665031	498469.199073	45.525940
3503.189701	498469.324864	45.530945
3503.357806	498455.933518	45.535949
3503.418609	498419.170665	45.540954
3503.005746	498436.600119	45.545959
3503.423094	498413.044472	45.550964
3503.191053	498429.736610	45.555969
3503.318634	498401.214936	45.560973
3503.396219	498413.656318	45.565978
3503.619394	498365.527817	45.570983
3503.524746	498363.163459	45.575988
3503.062533	498394.016258	45.580993
3503.642425	498344.920078	45.585997
3503.630732	498367.399273	45.591002
3503.307625	498344.973067	45.596007
3503.567738	498300.331652	45.601012
3503.295430	498333.128902	45.606017
3503.801528	498281.361108	45.611021
3503.580024	498299.165446	45.616026
3503.279617	498264.484361	45.621031
3503.385339	498280.465126	45.626036
3503.334111	498275.562653	45.631041
3503.509819	498247.488752	45.636045
3503.774544	498244.561325	45.641050
3503.730783	498234.038297	45.646055
3503.624399	498218.462665	45.651060
3503.557007	498208.955856	45.656065
3503.200749	498199.444077	45.661069
3503.608756	498193.203368	45.666074
3502.947329	498191.941074	45.671079
3503.092542	498169.592501	45.676084
3503.139848	498190.594463	45.681089
3503.478454	498126.955812	45.686093
3503.340110	498156.644068	45.691098
3503.375307	498135.274720	45.696103
3503.418889	498157.492314	45.701108
3503.418134	498129.243621	45.706113
3503.430921	498106.409649	45.711117
3503.534345	498105.633957	45.716122
3503.236142	498072.673414	45.721127
3503.628123	498098.936666	45.726132
3503.303767	498068.916517	45.731137
3503.517580	498050.151354	45.736141
3503.502351	498059.013246	45.741146
3503.369537	498032.253412	45.746151
3503.354255	498049.417893	45.751156
3503.254231	498043.814314	45.756161
3503.194430	498008.892205	45.761165
3503.359527	498001.322935	45.766170
3503.124715	498015.889619	45.771175
3503.621586	497992.017101	45.776180
3503.222289	497993.953398	45.781185
3503.287024	497981.590551	45.786189
3503.424635	497970.127439	45.791194
3503.507506	497956.850448	45.796199
3503.569870	497945.551091	45.801204
3503.591847	497956.229678	45.806209
3503.551111	497936.694622	45.811213
3503.977191	497918.250151	45.816218
3503.454327	497892.361776	45.821223
3503.775993	497900.562983	45.826228
3503.604051	497878.061677	45.831233
3503.663895	497861.092562	45.836237
3503.593060	497859.331885	45.841242
3503.234365	497845.922103	45.846247
3503.388429	497822.812312	45.851252
3503.295853	497818.574390	45.856257
3503.216306	497804.715446	45.861261
3503.490264	497806.140336	45.866266
3503.250449	497800.457524	45.871271
3503.429449	497766.762855	45.876276
3503.349746	497770.218071	45.881281
3503.385374	497757.049653	45.886285
3503.279934	497769.773540	45.891290
3503.395279	497727.533026	45.896295
3503.237983	497749.884125	45.901300
3503.072090	497716.952646	45.906305
3503.439233	497711.275122	45.911309
3503.247791	497721.481317	45.916314
3503.251738	497713.937399	45.921319
3503.350119	497711.947455	45.926324
3503.455304	497691.427168	45.931329
3503.234009	497686.146404	45.936333
3503.615013	497678.441620	45.941338
3503.483961	497674.310998	45.946343
3503.475099	497669.097905	45.951348
3503.427167	497647.184228	45.956353
3503.563447	497623.823861	45.961357
3503.724567	497623.545296	45.966362
3503.564729	497608.635733	45.971367
3503.599603	497604.833255	45.976372
3503.592471	497572.332059	45.981377
3503.330395	497570.652208	45.986381
3503.359417	497585.835683	45.991386
3503.659463	497531.921366	45.996391
3503.418790	497543.350488	46.001396
3503.449644	497526.031254	46.006401
3503.342611	497510.809503	46.011405
3503.213367	497541.256735	46.016410
3503.347516	497498.354565	46.021415
3503.463503	497483.603810	46.026420
3503.331407	497505.090568	46.031425
3503.420563	497475.965985	46.036429
3503.614070	497502.514611	46.041434
3503.359077	497447.725862	46.046439
3503.476455	497463.756134	46.051444
3503.472096	497429.583550	46.056449
3503.599686	497423.184393	46.061453
3503.689687	497413.652288	46.066458
3503.451207	497412.272456	46.071463
3503.615360	497383.996534	46.076468
3503.578018	497399.798181	46.081473
3503.540763	497361.074214	46.086477
3503.459112	497346.607723	46.091482
3503.394907	497345.554731	46.096487
3503.599196	497343.750516	46.101492
3503.526000	497316.473926	46.106497
3503.622535	497293.878829	46.111501
3503.479701	497314.557469	46.116506
3503.619487	497293.474360	46.121511
3503.566120	497291.812121	46.126516
3503.405358	497250.474807	46.131521
3503.285541	497257.784164	46.136525
3503.206205	497260.682515	46.141530
3503.155420	497233.604768	46.146535
3503.123405	497205.916480	46.151540
3503.195871	497240.028163	46.156545
3503.055326	497214.230267	46.161549
3503.592479	497178.655294	46.166554
3503.236637	497220.378266	46.171559
3503.297956	497188.523722	46.176564
3503.540808	497174.461453	46.181569
3503.243834	497207.315267	46.186573
3503.323926	497169.787410	46.191578
3503.625033	497134.502801	46.196583
3503.512900	497135.229352	46.201588
3503.335488	497185.530956	46.206593
3503.318250	497161.384214	46.211597
3503.265405	497149.444409	46.216602
3503.077664	497133.171911	46.221607
3503.446874	497089.573456	46.226612
3503.166322	497107.033901	46.231617
3502.985102	497114.403649	46.236621
3503.422062	497113.625824	46.241626
3503.210710	497091.382909	46.246631
3503.741561	497028.671949	46.251636
3503.391576	497037.485996	46.256641
3503.210679	497073.460657	46.261645
3503.634927	497038.814564	46.266650
3503.471436	497059.800529	46.271655
3503.943171	496998.111372	46.276660
3503.466983	497021.678226	46.281665
3503.219834	496985.366164	46.286669
3503.376259	496990.303057	46.291674
3503.310782	496953.860959	46.296679
3503.603808	496958.016842	46.301684
3503.380052	496969.747421	46.306689
3503.043070	496953.802123	46.311693
3503.599837	496935.943541	46.316698
3503.273699	496944.045064	46.321703
3503.503095	496920.010903	46.326708
3503.288781	496915.538868	46.331713
3503.260731	496913.467563	46.336717
3503.469311	496910.852570	46.341722
3503.280405	496884.960593	46.346727
3503.310547	496896.549830	46.351732
3503.084170	496865.448995	46.356737
3503.374507	496869.250923	46.361741
3503.642538	496865.107664	46.366746
3503.370098	496846.873775	46.371751
3503.400220	496824.339221	46.376756
3503.415049	496834.462681	46.381761
3503.678510	496815.739024	46.386765
3503.556223	496819.201152	46.391770
3503.077346	496802.569344	46.396775
3503.514663	496782.906852	46.401780
3503.237461	496776.318306	46.406785
3503.143613	496779.067140	46.411789
3503.344362	496773.770028	46.416794
3503.278273	496767.350626	46.421799
3503.108626	496771.731571	46.426804
3502.976386	496735.248958	46.431809
3503.241018	496750.800923	46.436813
3503.255519	496746.242049	46.441818
3503.359527	496743.947335	46.446823
3503.527514	496732.630529	46.451828
3503.269310	496741.531469	46.456833
3503.218241	496715.516206	46.461837
3503.200077	496712.380103	46.466842
3503.329236	496665.021386	46.471847
3502.943189	496697.485166	46.476852
3503.233552	496675.314326	46.481857
3503.365777	496685.925605	46.486861
3502.981171	496706.086232	46.491866
3503.525153	496670.914221	46.496871
3503.295573	496673.127603	46.501876
3503.327104	496634.543102	46.506881
3503.337632	496668.260614	46.511885
3503.535056	496624.991975	46.516890
3503.023380	496657.425054	46.521895
3503.451048	496628.346864	46.526900
3503.114151	496610.376073	46.531905
3503.340598	496608.517655	46.536909
3503.564813	496594.862919	46.541914
3503.180087	496579.785539	46.546919
3503.308552	496595.460419	46.551924
3502.979585	496582.551296	46.556929
3503.178500	496568.647393	46.561933
3503.130361	496566.022299	46.566938
3503.122308	496544.404764	46.571943
3503.201671	496533.911916	46.576948
3503.003259	496562.903460	46.581953
3503.229303	496526.870093	46.586957
3503.230348	496552.184789	46.591962
3503.381417	496546.895465	46.596967
3503.624425	496515.517320	46.601972
3503.477803	496531.185107	46.606977
3503.557261	496492.086431	46.611981
3503.748693	496484.461738	46.616986
3503.055255	496489.330582	46.621991
3503.514854	496456.146057	46.626996
3503.668512	496448.831099	46.632001
3503.769819	496437.980318	46.637005
3503.485484	496433.974901	46.642010
3503.540014	496427.586942	46.647015
3503.393640	496407.459377	46.652020
3503.846067	496397.160633	46.657025
3503.533346	496386.830935	46.662029
3503.506308	496361.722709	46.667034
3503.298856	496362.666877	46.672039
3503.225904	496354.628248	46.677044
3503.376668	496357.389112	46.682049
3503.411190	496354.750921	46.687053
3503.504839	496325.775676	46.692058
3503.274952	496305.053635	46.697063
3503.394819	496316.679690	46.702068
3503.705339	496294.960873	46.707073
3502.907647	496304.099191	46.712077
3503.371110	496255.572702	46.717082
3503.436898	496280.826910	46.722087
3503.343865	496253.248077	46.727092
3503.337538	496258.109635	46.732097
3503.428122	496250.855198	46.737101
3503.342243	496248.489176	46.742106
3502.937713	496231.794462	46.747111
3503.602142	496208.298165	46.752116
3503.623543	496195.181494	46.757121
3503.346496	496218.717908	46.762125
3503.628346	496190.472158	46.767130
3503.347399	496193.351915	46.772135
3503.825955	496154.847631	46.777140
3503.452956	496170.703401	46.782145
3503.387703	496161.752118	46.787149
3503.607192	496107.188112	46.792154
3503.327152	496138.420991	46.797159
3503.601168	496115.087546	46.802164
3503.595618	496099.797941	46.807169
3503.124540	496085.898309	46.812173
3503.400551	496082.310553	46.817178
3503.510427	496066.698889	46.822183
3503.588840	496053.218688	46.827188
3503.559180	496067.501349	46.832193
3503.635780	496034.629751	46.837197
3503.476282	496012.883630	46.842202
3503.343563	496043.536442	46.847207
3503.807490	496005.692359	46.852212
3503.399964	496005.554285	46.857217
3503.500636	495994.399554	46.862221
3503.481907	495985.795249	46.867226
3503.233239	495993.530529	46.872231
3503.391405	495945.861571	46.877236
3503.250477	495961.123897	46.882241
3503.088942	495938.669172	46.887245
3503.405150	495930.467581	46.892250
3503.495292	495942.858043	46.897255
3503.779070	495936.990621	46.902260
3503.493121	495922.150239	46.907265
3503.680115	495903.538995	46.912269
3503.618208	495880.663400	46.917274
3503.519888	495875.008249	46.922279
3503.618261	495852.157915	46.927284
3503.313803	495852.712389	46.932289
3503.467627	495847.675585	46.937293
3503.557727	495837.990745	46.942298
3503.225083	495795.867188	46.947303
3503.242950	495808.978008	46.952308
3503.582241	495791.102053	46.957313
3503.296472	495785.476503	46.962317
3503.695321	495786.780552	46.967322
3503.641731	495761.422537	46.972327
3503.760492	495742.467492	46.977332
3503.515571	495735.670937	46.982337
3503.650253	495738.130646	46.987341
3503.824569	495689.395197	46.992346
3503.584975	495720.065445	46.997351
3503.495164	495657.245346	47.002356
3503.543231	495651.161930	47.007361
3503.458927	495674.871106	47.012365
3503.437119	495641.204242	47.017370
3503.295787	495665.935087	47.022375
3503.657775	495603.549711	47.027380
3503.528527	495639.063349	47.032385
3503.390327	495603.389526	47.037389
3503.565819	495614.855339	47.042394
3503.553464	495579.516004	47.047399
3503.456257	495550.670961	47.052404
3503.171263	495571.070255	47.057409
3503.709341	495555.593002	47.062413
3503.176147	495532.082610	47.067418
3503.263711	495519.917012	47.072423
3503.471925	495511.529775	47.077428
3503.078814	495507.895773	47.082433
3502.971106	495511.406476	47.087437
3503.233288	495511.061274	47.092442
3503.417260	495490.070360	47.097447
3503.260176	495485.538293	47.102452
3503.343784	495469.879640	47.107457
3503.461957	495457.506632	47.112461
3503.557294	495465.187760	47.117466
3503.293197	495469.735843	47.122471
3503.718059	495441.111902	47.127476
3503.158791	495436.238332	47.132481
3503.325579	495415.351314	47.137485
3503.551475	495412.429574	47.142490
3503.199100	495430.561200	47.147495
3503.543038	495401.848724	47.152500
3503.177971	495384.184971	47.157505
3503.277828	495366.042651	47.162509
3503.291523	495371.559507	47.167514
3503.464305	495353.608178	47.172519
3503.397036	495371.745430	47.177524
3503.455338	495333.710909	47.182529
3503.366557	495321.826219	47.187533
3503.364688	495328.155677	47.192538
3503.433932	495316.549803	47.197543
3503.023374	495305.829891	47.202548
3503.141298	495327.988559	47.207553
3503.164028	495294.516549	47.212557
3503.581702	495281.842917	47.217562
3503.124343	495290.168444	47.222567
3502.958938	495262.194489	47.227572
3503.770914	495250.420540	47.232577
3503.332927	495293.274832	47.237581
3503.444167	495252.193787	47.242586
3503.114995	495252.245852	47.247591
3503.501603	495215.171855	47.252596
3503.282563	495252.016903	47.257601
3503.037737	495221.675677	47.262605
3503.626284	495231.557442	47.267610
3503.243394	495189.035361	47.272615
3503.222367	495204.785699	47.277620
3502.994243	495166.846738	47.282625
3503.264766	495185.487749	47.287629
3503.208105	495158.458481	47.292634
3503.154587	495196.239514	47.297639
3503.227148	495161.898617	47.302644
3502.996355	495193.783559	47.307649
3503.154175	495174.467319	47.312653
3503.173213	495144.691859	47.317658
3503.203374	495148.028938	47.322663
3503.442518	495131.990977	47.327668
3503.389656	495124.505600	47.332673
3503.077399	495129.922150	47.337677
3503.469483	495131.986820	47.342682
3503.625435	495109.177090	47.347687
3503.465808	495077.505684	47.352692
3503.181665	495099.778815	47.357697
3503.381818	495078.936774	47.362701
3503.368001	495066.685633	47.367706
3502.974646	495086.191187	47.372711
3503.608822	495044.014344	47.377716
3503.763168	495028.698569	47.382721
3503.197561	495045.446532	47.387725
3503.682415	495035.344435	47.392730
3503.315767	495006.794292	47.397735
3503.527408	494991.317528	47.402740
3503.193942	494997.243808	47.407745
3503.233413	494982.047420	47.412749
3503.637311	494968.109900	47.417754
3503.071973	494981.921106	47.422759
3503.259825	494948.726168	47.427764
3503.562225	494934.247691	47.432769
3502.964712	494940.519531	47.437773
3503.150877	494945.300377	47.442778
3503.207836	494920.683234	47.447783
3503.202149	494950.507651	47.452788
3503.408467	494923.487103	47.457793
3503.105309	494898.673681	47.462797
3503.250043	494902.347135	47.467802
3503.176526	494890.105312	47.472807
3502.983701	494896.718274	47.477812
3503.090299	494889.865840	47.482817
3502.721455	494884.253143	47.487821
3503.109659	494895.989590	47.492826
3503.015891	494873.320308	47.497831
3503.087276	494889.461384	47.502836
3503.366841	494889.974206	47.507841
3503.173674	494878.763973	47.512845
3503.575730	494873.940837	47.517850
3503.511399	494859.165828	47.522855
3503.624815	494841.982897	47.527860
3503.372755	494819.439838	47.532865
3503.357184	494844.000010	47.537869
3503.474006	494793.195256	47.542874
3503.209309	494797.389158	47.547879
3503.359352	494804.403668	47.552884
3503.564035	494774.800801	47.557889
3503.042164	494794.225710	47.562893
3503.383161	494766.170952	47.567898
3503.141455	494744.385682	47.572903
3503.326501	494747.698352	47.577908
3503.357360	494758.833122	47.582913
3503.515520	494726.351359	47.587917
3503.626211	494753.777871	47.592922
3503.774160	494702.613504	47.597927
3503.538050	494711.562572	47.602932
3503.787747	494697.244143	47.607937
3503.326247	494673.265601	47.612941
3503.744320	494663.781474	47.617946
3503.270841	494649.729221	47.622951
3503.454722	494644.687337	47.627956
3503.221754	494647.610385	47.632961
3502.992477	494615.847920	47.637965
3503.417047	494603.476542	47.642970
3503.111870	494610.816255	47.647975
3503.731170	494597.502662	47.652980
3503.341968	494591.741187	47.657985
3503.188119	494598.753175	47.662989
3503.294415	494561.367720	47.667994
3503.194209	494556.674527	47.672999
3502.989094	494564.200983	47.678004
3503.297563	494532.302740	47.683009
3503.267205	494573.575223	47.688013
3503.386138	494542.972836	47.693018
3502.946344	494562.638191	47.698023
3503.334019	494527.739948	47.703028
3503.479982	494545.996218	47.708033
3503.594450	494494.330211	47.713037
3503.486717	494516.221718	47.718042
3503.278389	494501.418546	47.723047
3503.317784	494505.311272	47.728052
3503.294841	494477.161693	47.733057
3502.916762	494470.993339	47.738061
3503.475036	494469.183527	47.743066
3503.296077	494466.173726	47.748071
3504.025754	494463.982374	47.753076
3503.566979	494431.445699	47.758081
3503.280955	494440.757237	47.763085
3503.533323	494392.664265	47.768090
3503.387460	494427.423340	47.773095
3503.085016	494411.014636	47.778100
3503.744584	494384.124195	47.783105
3503.172583	494399.810406	47.788109
3503.350741	494350.311257	47.793114
3502.971125	494381.259054	47.798119
3503.217968	494364.307765	47.803124
3503.739478	494348.629574	47.808129
3503.052609	494353.042214	47.813133
3503.698426	494306.507169	47.818138
3503.196782	494350.943431	47.823143
3503.265840	494344.046093	47.828148
3503.404046	494345.593990	47.833153
3503.268000	494314.879618	47.838157
3502.810499	494277.886518	47.843162
3503.132356	494256.062224	47.848167
3503.471414	494233.475645	47.853172
3503.393828	494244.475960	47.858177
3503.155082	494283.351505	47.863181
3503.352148	494293.751383	47.868186
3503.246909	494268.855189	47.873191
3503.677276	494217.341015	47.878196
3503.340245	494207.165832	47.883201
3503.144404	494236.059380	47.888205
3503.422371	494258.599132	47.893210
3502.915830	494245.311334	47.898215
3502.728213	494224.428344	47.903220
3503.478571	494201.017173	47.908225
3503.023945	494225.445027	47.913229
3503.336277	494183.266447	47.918234
3503.446427	494186.844239	47.923239
3503.317151	494177.497015	47.928244
3503.233724	494147.381681	47.933249
3503.060919	494193.234798	47.938253
3503.234902	494178.522845	47.943258
3503.313482	494132.532746	47.948263
3503.218937	494162.271216	47.953268
3503.241480	494137.304009	47.958273
3502.804075	494121.726560	47.963277
3502.882201	494114.371975	47.968282
3502.809348	494112.509980	47.973287
3503.725926	494096.566584	47.978292
3503.260383	494145.757456	47.983297
3502.792623	494121.779181	47.988301
3503.659826	494095.260590	47.993306
3503.332885	494113.440129	47.998311
3502.927243	494094.009272	48.003316
3503.672960	494068.775755	48.008321
3503.405962	494101.124043	48.013325
3503.603350	494066.761369	48.018330
3503.325200	494059.716259	48.023335
3503.241670	494034.816317	48.028340
3503.587422	494051.421128	48.033345
3503.081707	494021.068516	48.038349
3503.370124	494017.022670	48.043354
3503.004241	494036.018627	48.048359
3502.933872	494007.622643	48.053364
3503.153347	493984.700205	48.058369
3502.965948	493996.376303	48.063373
3503.228476	493967.674455	48.068378
3503.008941	493992.622462	48.073383
3503.063636	493957.522588	48.078388
3502.926930	493978.406578	48.083393
3502.956838	493986.554398	48.088397
3503.381244	493965.574375	48.093402
3503.029768	493992.467434	48.098407
3503.480631	493961.760977	48.103412
3503.622192	493998.703449	48.108417
3503.235969	493948.583515	48.113421
3503.325312	493919.807694	48.118426
3502.783661	493957.820340	48.123431
3502.990858	493910.492801	48.128436
3503.016095	493941.529253	48.133441
3503.308836	493904.366178	48.138445
3502.907827	493939.267779	48.143450
3503.311320	493928.469022	48.148455
3503.028697	493918.082531	48.153460
3503.348822	493887.497889	48.158465
3503.107660	493914.221715	48.163469
3503.421212	493870.826941	48.168474
3503.093203	493888.095405	48.173479
3502.944404	493882.396980	48.178484
3503.700708	493857.566598	48.183489
3503.237291	493895.313822	48.188493
3503.559584	493839.308985	48.193498
3503.341592	493849.268349	48.198503
3503.314688	493827.751861	48.203508
3503.170525	493834.003051	48.208513
3503.240017	493828.979025	48.213517
3503.233091	493828.423146	48.218522
3503.073403	493825.308919	48.223527
3503.609643	493771.498093	48.228532
3503.235631	493815.459735	48.233537
3502.899793	493793.992039	48.238541
3503.692640	493756.800255	48.243546
3503.232276	493801.940237	48.248551
3503.029646	493784.198629	48.253556
3503.389848	493721.351408	48.258561
3503.304720	493754.532393	48.263565
3503.131366	493729.747511	48.268570
3503.283827	493741.319412	48.273575
3503.297099	493724.708279	48.278580
3503.589627	493746.689346	48.283585
3503.281736	493739.800726	48.288589
3503.413868	493698.054619	48.293594
3503.630182	493685.614269	48.298599
3503.289372	493719.747206	48.303604
3503.407407	493684.181063	48.308609
3503.504205	493672.569797	48.313613
3503.306286	493683.741379	48.318618
3503.219444	493671.450213	48.323623
3503.378645	493629.800948	48.328628
3503.458812	493680.071471	48.333633
3502.838851	493636.874340	48.338637
3503.580137	493587.993061	48.343642
3503.131821	493618.041516	48.348647
3503.191908	493585.522605	48.353652
3503.051339	493617.953032	48.358657
3503.303247	493590.163755	48.363661
3503.418220	493597.184270	48.368666
3502.975334	493623.434024	48.373671
3503.556527	493571.084002	48.378676
3503.264339	493585.308815	48.383681
3502.610217	493566.676243	48.388685
3503.477361	493521.268905	48.393690
3503.208367	493569.923865	48.398695
3502.530047	493554.434652	48.403700
3503.247255	493528.749165	48.408705
3503.123571	493556.467698	48.413709
3503.051313	493567.619488	48.418714
3503.218184	493547.236714	48.423719
3502.928485	493562.119445	48.428724
3503.389790	493520.017077	48.433729
3503.047806	493501.537653	48.438733
3503.508025	493524.960981	48.443738
3503.270584	493525.808754	48.448743
3503.467625	493483.748075	48.453748
3503.214494	493534.932524	48.458753
3502.780015	493516.822201	48.463757
3503.211029	493471.281125	48.468762
3502.649556	493512.133557	48.473767
3503.193981	493515.490922	48.478772
3502.718464	493479.866291	48.483777
3502.946594	493446.358449	48.488781
3503.064871	493458.492952	48.493786
3502.623726	493479.577542	48.498791
3502.958204	493462.662211	48.503796
3502.626960	493472.183936	48.508801
3503.038423	493451.205375	48.513805
3503.019686	493492.579720	48.518810
3503.009721	493459.312089	48.523815
3503.126337	493454.989447	48.528820
3503.020534	493490.402254	48.533825
3502.967613	493469.092012	48.538829
3502.938366	493457.449896	48.543834
3503.259278	493421.243520	48.548839
3503.385803	493468.317082	48.553844
3503.600220	493444.837754	48.558849
3503.336422	493455.260314	48.563853
3502.953695	493432.736206	48.568858
3503.102860	493391.746288	48.573863
3502.975647	493429.238768	48.578868
3502.859348	493418.572513	48.583873
3502.942428	493391.062814	48.588877
3503.601610	493393.845041	48.593882
3503.236072	493423.070515	48.598887
3503.438484	493394.377279	48.603892
3503.360636	493427.912168	48.608897
3503.166139	493376.342501	48.613901
3503.697215	493330.987818	48.618906
3503.414660	493381.215212	48.623911
3503.362077	493384.059307	48.628916
3503.355223	493373.274450	48.633921
3503.171562	493327.425072	48.638925
3503.130416	493333.812063	48.643930
3502.845455	493325.704339	48.648935
3503.345204	493277.214887	48.653940
3503.369036	493310.379447	48.658945
3502.997770	493341.327667	48.663949
3503.435976	493307.026790	48.668954
3503.365352	493320.761037	48.673959
3503.236156	493319.515530	48.678964
3503.374199	493280.198194	48.683969
3502.951536	493273.276902	48.688973
3503.206815	493249.233841	48.693978
3502.962894	493252.310755	48.698983
3503.642496	493229.213372	48.703988
3503.245092	493266.242503	48.708993
3502.964928	493279.959263	48.713997
3503.205496	493253.538516	48.719002
3502.900776	493253.232246	48.724007
3502.821027	493218.810521	48.729012
3503.266629	493217.575429	48.734017
3502.816243	493217.241544	48.739021
3503.220898	493218.595504	48.744026
3503.098722	493204.182781	48.749031
3503.154052	493170.651115	48.754036
3503.626066	493181.261357	48.759041
3503.225016	493197.883704	48.764045
3503.441588	493202.761477	48.769050
3503.329408	493201.665188	48.774055
3503.390265	493197.705772	48.779060
3503.406133	493197.399465	48.784065
3503.219093	493193.985621	48.789069
3503.426491	493178.609284	48.794074
3502.664663	493156.195400	48.799079
3502.904477	493132.812939	48.804084
3503.349574	493108.942249	48.809089
3503.299887	493097.910806	48.814093
3503.201216	493130.740578	48.819098
3502.974553	493118.420505	48.824103
3503.351750	493128.488735	48.829108
3503.168453	493120.668686	48.834113
3503.274193	493092.344735	48.839117
3503.467455	493125.584124	48.844122
3503.103624	493085.181003	48.849127
3503.295031	493057.349850	48.854132
3503.112293	493097.383742	48.859137
3502.928933	493082.069091	48.864141
3503.049297	493063.212310	48.869146
3503.267936	493042.820798	48.874151
3503.303148	493060.640293	48.879156
3503.446254	493077.531210	48.884161
3503.409168	493018.947453	48.889165
3503.505383	493003.791103	48.894170
3503.467157	493044.966973	48.899175
3503.427206	493033.731396	48.904180
3503.515674	492986.673454	48.909185
3503.423663	492961.975962	48.914189
3503.932598	492944.475548	48.919194
3503.669397	492962.848701	48.924199
3503.524639	492927.626478	48.929204
3503.718625	492918.024961	48.934209
3503.385187	492908.101688	48.939213
3503.471031	492895.377593	48.944218
3503.208449	492914.712850	48.949223
3503.493017	492921.554896	48.954228
3503.528543	492917.396865	48.959233
3503.017765	492900.412068	48.964237
3503.242966	492882.095569	48.969242
3503.393493	492916.202965	48.974247
3503.155919	492886.261857	48.979252
3503.012017	492875.042614	48.984257
3503.172746	492850.051825	48.989261
3503.303544	492868.514713	48.994266
3502.887818	492851.717406	48.999271
3502.953458	492834.185678	49.004276
3503.588571	492813.981284	49.009281
3503.047518	492859.946558	49.014285
3503.287926	492850.844066	49.019290
3502.866934	492814.196734	49.024295
3503.393238	492789.350638	49.029300
3503.128299	492812.889493	49.034305
3503.152468	492779.767164	49.039309
3504.139278	492766.191609	49.044314
3503.244610	492800.211227	49.049319
3502.940139	492772.964427	49.054324
3503.289442	492731.688211	49.059329
3503.025717	492764.139601	49.064333
3503.321550	492753.914219	49.069338
3503.529201	492733.726664	49.074343
3503.421678	492767.318082	49.079348
3502.900432	492749.119439	49.084353
3503.404759	492727.213859	49.089357
3503.381345	492737.092424	49.094362
3503.251906	492691.941862	49.099367
3503.234840	492729.519629	49.104372
3503.345729	492692.129662	49.109377
3503.248393	492695.740541	49.114381
3503.278134	492701.610143	49.119386
3503.300386	492663.170683	49.124391
3503.140000	492656.055780	49.129396
3503.268266	492661.909821	49.134401
3502.889997	492673.110519	49.139405
3503.381074	492634.596895	49.144410
3503.301350	492676.033347	49.149415
3503.042764	492656.425807	49.154420
3503.396150	492632.366439	49.159425
3503.200365	492647.893383	49.164429
3503.466508	492607.389642	49.169434
3503.350137	492605.686294	49.174439
3503.406934	492605.981194	49.179444
3503.526232	492583.680541	49.184449
3503.343005	492599.154901	49.189453
3503.630539	492559.761766	49.194458
3503.034997	492574.440428	49.199463
3503.527256	492542.357779	49.204468
3503.108984	492569.263463	49.209473
3503.284641	492546.953857	49.214477
3503.776581	492518.517344	49.219482
3503.248979	492518.803338	49.224487
3503.299613	492520.213310	49.229492
3503.518948	492510.151808	49.234497
3503.071825	492499.182829	49.239501
3503.347561	492473.869510	49.244506
3503.157226	492478.609229	49.249511
3503.067549	492463.026053	49.254516
3503.068984	492442.212445	49.259521
3502.961514	492470.031324	49.264525
3503.245827	492454.490307	49.269530
3503.203977	492436.013016	49.274535
3503.317183	492467.848293	49.279540
3503.498136	492440.676198	49.284545
3503.291359	492434.277516	49.289549
3503.348965	492421.962687	49.294554
3503.298086	492393.763707	49.299559
3503.118577	492421.948532	49.304564
3503.467884	492404.067714	49.309569
3503.393718	492392.178822	49.314573
3503.245787	492388.961211	49.319578
3503.304373	492354.921143	49.324583
3502.977219	492370.266520	49.329588
3503.240036	492361.362811	49.334593
3503.108875	492351.711113	49.339597
3503.282617	492378.472855	49.344602
3502.928702	492349.612732	49.349607
3503.098609	492367.006474	49.354612
3503.291783	492314.359747	49.359617
3503.304741	492322.257774	49.364621
3503.501025	492321.821653	49.369626
3503.454838	492296.001922	49.374631
3503.360584	492310.753480	49.379636
3503.329493	492313.290494	49.384641
3503.207105	492292.243084	49.389645
3503.233839	492271.678493	49.394650
3503.348857	492257.126257	49.399655
3503.510157	492286.928585	49.404660
3503.414225	492257.419844	49.409665
3503.475204	492274.780248	49.414669
3503.742992	492219.133615	49.419674
3503.367499	492223.598817	49.424679
3503.240014	492238.102477	49.429684
3503.392246	492210.174962	49.434689
3503.076851	492219.087124	49.439693
3503.237808	492175.408648	49.444698
3503.132405	492180.489510	49.449703
3503.190584	492188.177879	49.454708
3503.146391	492178.309778	49.459713
3503.162300	492193.752999	49.464717
3503.356265	492189.873611	49.469722
3503.140576	492176.740910	49.474727
3503.223150	492188.578040	49.479732
3503.118959	492146.916431	49.484737
3503.173172	492110.648370	49.489741
3503.142240	492155.319350	49.494746
3502.851804	492146.654914	49.499751
3503.076400	492104.586748	49.504756
3503.168333	492131.969480	49.509761
3502.776847	492130.309574	49.514765
3503.227108	492125.174259	49.519770
3502.921725	492119.550681	49.524775
3503.364779	492102.566308	49.529780
3503.209543	492142.040854	49.534785
3503.284733	492100.553355	49.539789
3503.155822	492098.244240	49.544794
3503.321024	492079.126164	49.549799
3502.901028	492085.877319	49.554804
3503.067625	492077.292535	49.559809
3502.522810	492077.733180	49.564813
3503.349822	492061.498350	49.569818
3502.927163	492110.232073	49.574823
3502.668817	492082.673115	49.579828
3503.203003	492054.735635	49.584833
3503.053342	492099.678726	49.589837
3503.378265	492058.658078	49.594842
3503.000415	492098.319831	49.599847
3502.921371	492061.566318	49.604852
3503.139753	492022.588110	49.609857
3502.968091	492051.531888	49.614861
3503.032147	492031.973973	49.619866
3503.483537	492010.582338	49.624871
3503.202496	492040.809475	49.629876
3503.114596	492013.679252	49.634881
3502.674163	492045.704049	49.639885
3502.908341	492008.090648	49.644890
3503.050357	492001.332831	49.649895
3502.985847	492040.590684	49.654900
3502.926438	492036.700672	49.659905
3503.075803	491999.201944	49.664909
3503.141650	492028.158858	49.669914
3502.813219	492028.362733	49.674919
3502.580612	492019.992949	49.679924
3503.182724	492000.451237	49.684929
3503.165173	492038.131765	49.689933
3503.342502	491982.296154	49.694938
3503.338700	492008.630713	49.699943
3503.423829	491961.570699	49.704948
3503.434372	491988.308158	49.709953
3503.446730	491963.592839	49.714957
3503.530815	491961.756462	49.719962
3503.209117	491953.653941	49.724967
3503.299183	491918.088829	49.729972
3503.337351	491934.592237	49.734977
3503.346858	491931.906726	49.739981
3503.495811	491914.006464	49.744986
3503.196687	491912.180012	49.749991
3503.059674	491887.994627	49.754996
3503.274998	491881.478391	49.760001
3503.292329	491864.409166	49.765005
3503.221861	491895.616104	49.770010
3503.198352	491869.589626	49.775015
3503.084469	491897.005236	49.780020
3503.529117	491868.119424	49.785025
3502.945658	491870.186741	49.790029
3503.312875	491836.552722	49.795034
3502.817219	491839.669659	49.800039
3503.254612	491821.774358	49.805044
3503.016838	491824.394751	49.810049
3503.155419	491837.388032	49.815053
3503.533286	491810.386461	49.820058
3503.390456	491824.740941	49.825063
3503.056099	491790.913879	49.830068
3503.212705	491792.408441	49.835073
3503.411583	491782.349780	49.840077
3503.594904	491761.709232	49.845082
3503.371723	491794.712975	49.850087
3503.309060	491759.070415	49.855092
3503.157683	491767.399796	49.860097
3503.130546	491748.767567	49.865101
3503.229332	491734.774560	49.870106
3503.443749	491738.488275	49.875111
3503.306982	491719.620132	49.880116
3503.453631	491728.611423	49.885121
3503.162129	491716.503237	49.890125
3503.309110	491700.324941	49.895130
3503.035423	491692.214717	49.900135
3503.156599	491684.143362	49.905140
3503.211998	491676.436901	49.910145
3502.990136	491683.410099	49.915149
3503.123620	491673.766860	49.920154
3503.056183	491692.160968	49.925159
3502.842097	491680.395023	49.930164
3503.168287	491669.708461	49.935169
3503.088767	491676.051445	49.940173
3503.224732	491651.265531	49.945178
3503.275716	491654.042877	49.950183
3503.162965	491631.676475	49.955188
3503.048474	491642.937383	49.960193
3503.139086	491644.493032	49.965197
3503.590623	491627.304313	49.970202
3503.524948	491631.011680	49.975207
3503.320376	491626.334236	49.980212
3503.409589	491591.426996	49.985217
3502.812646	491609.499736	49.990221
3503.510038	491597.387092	49.995226
3503.122297	491590.054501	50.000231
3503.138529	491595.521442	50.005236
3503.403768	491584.844466	50.010241
3502.813025	491566.959504	50.015245
3503.414197	491556.431987	50.020250
3503.256059	491533.262347	50.025255
3503.124177	491556.325969	50.030260
3503.220543	491541.573549	50.035265
3503.046143	491542.411445	50.040269
3503.300471	491543.839938	50.045274
3503.120536	491529.029895	50.050279
3503.366838	491547.678415	50.055284
3503.449135	491490.995414	50.060289
3502.806592	491527.560321	50.065293
3503.332882	491494.508262	50.070298
3503.398453	491483.406998	50.075303
3503.186454	491500.102264	50.080308
3503.338385	491471.363393	50.085313
3503.405077	491485.127937	50.090317
3503.323317	491439.207139	50.095322
3503.381818	491438.185054	50.100327
3502.965313	491472.536661	50.105332
3503.125611	491443.138057	50.110337
3503.426718	491435.038153	50.115341
3503.303893	491449.440403	50.120346
3503.376947	491407.394617	50.125351
3502.917103	491422.660460	50.130356
3503.010564	491405.983930	50.135361
3502.972046	491402.698209	50.140365
3503.183388	491408.539515	50.145370
3503.052624	491405.876100	50.150375
3502.858643	491422.467300	50.155380
3503.583973	491381.938953	50.160385
3503.133999	491423.993801	50.165389
3503.427461	491383.837584	50.170394
3503.028873	491391.041399	50.175399
3503.553976	491362.952389	50.180404
3503.039785	491365.059455	50.185409
3503.385725	491363.029697	50.190413
3503.187451	491354.502254	50.195418
3503.155617	491369.548555	50.200423
3502.952677	491373.784108	50.205428
3502.755528	491355.330290	50.210433
3503.333545	491333.715290	50.215437
3503.376683	491304.740138	50.220442
3503.439905	491339.573246	50.225447
3503.061404	491295.471537	50.230452
3503.290549	491325.568546	50.235457
3503.397021	491304.990283	50.240461
3503.004248	491307.179451	50.245466
3503.207269	491294.638315	50.250471
3503.073112	491296.482742	50.255476
3503.114241	491249.681104	50.260481
3502.951812	491253.251906	50.265485
3503.057578	491268.529759	50.270490
3503.145398	491246.485700	50.275495
3502.944998	491275.333938	50.280500
3502.585922	491253.664390	50.285505
3503.308118	491228.633318	50.290509
3503.342977	491248.885531	50.295514
3502.967674	491274.570831	50.300519
3502.933279	491246.063641	50.305524
3503.223327	491244.599791	50.310529
3502.936556	491251.887274	50.315533
3503.032579	491251.568266	50.320538
3503.306443	491256.285566	50.325543
3503.265914	491207.977405	50.330548
3503.232591	491229.709100	50.335553
3503.127266	491216.963430	50.340557
3503.253069	491206.308278	50.345562
3503.120823	491224.865024	50.350567
3503.284125	491198.504215	50.355572
3503.071638	491220.365529	50.360577
3503.151598	491219.086818	50.365581
3503.090280	491168.756071	50.370586
3503.003624	491185.279873	50.375591
3503.105925	491185.567604	50.380596
3503.216632	491149.086163	50.385601
3503.044470	491176.258823	50.390605
3502.845260	491170.415596	50.395610
3503.094701	491160.905697	50.400615
3503.188431	491168.487579	50.405620
3503.429046	491147.685362	50.410625
3503.182684	491158.258384	50.415629
3503.423626	491148.344667	50.420634
3503.364376	491132.198476	50.425639
3503.257491	491102.841569	50.430644
3503.363424	491116.600182	50.435649
3503.154502	491126.103768	50.440653
3503.278441	491106.889928	50.445658
3503.134485	491103.975332	50.450663
3503.199338	491092.063635	50.455668
3503.107395	491069.794558	50.460673
3502.756109	491090.715715	50.465677
3502.876754	491075.857800	50.470682
3503.092773	491078.406568	50.475687
3503.246429	491069.823366	50.480692
3503.286613	491066.829014	50.485697
3502.999469	491083.536530	50.490701
3503.638520	491062.418016	50.495706
3503.636784	491067.280215	50.500711
3503.781201	491039.807984	50.505716
3503.413523	491020.418539	50.510721
3503.451242	491031.908981	50.515725
3503.495165	491003.642264	50.520730
3503.373769	490975.401637	50.525735
3503.409317	490961.721916	50.530740
3503.651486	490884.804450	50.535745
3503.354966	490859.427458	50.540749
3503.359441	490785.940388	50.545754
3502.938281	490709.076403	50.550759
3502.746648	490657.600027	50.555764
3502.878746	490543.169984	50.560769
3502.434794	490466.055372	50.565773
3502.644675	490351.409277	50.570778
3502.327996	490234.515953	50.575783
3502.062641	490106.268798	50.580788
3501.919852	489982.053203	50.585793
3501.893594	489824.846519	50.590797
3501.349602	489681.749975	50.595802
3501.526828	489533.726702	50.600807
3501.290200	489358.163833	50.605812
3501.142794	489180.863131	50.610817
3500.645044	489020.837216	50.615821
3500.090549	488799.430238	50.620826
3499.610653	488643.349059	50.625831
3499.536606	488427.636015	50.630836
3499.478892	488212.475105	50.635841
3498.824360	488006.675575	50.640845
3498.576048	487803.291617	50.645850
3498.399599	487546.048827	50.650855
3497.932254	487353.889239	50.655860
3497.561761	487099.102492	50.660865
3497.538684	486872.574113	50.665869
3496.825662	486610.591168	50.670874
3496.742540	486327.684875	50.675879
3495.905501	486103.099686	50.680884
3495.439940	485841.219039	50.685889
3495.201382	485549.713827	50.690893
3494.799606	485318.312917	50.695898
3494.278376	485016.205661	50.700903
3493.496765	484739.921582	50.705908
3493.449781	484444.012409	50.710913
3493.427192	484170.589263	50.715917
3493.058096	483849.846300	50.720922
3492.198869	483589.365144	50.725927
3491.757307	483263.962774	50.730932
3491.165892	482942.378602	50.735937
3490.877403	482636.752029	50.740941
3490.329221	482306.587758	50.745946
3489.788919	481985.993048	50.750951
3489.610881	481677.445841	50.755956
3488.732459	481331.001643	50.760961
3488.000565	481012.346719	50.765965
3487.583179	480675.648280	50.770970
3487.648601	480332.128232	50.775975
3486.502431	479977.189368	50.780980
3485.963487	479652.046286	50.785985
3485.277997	479290.941265	50.790989
3484.448814	478959.751574	50.795994
3484.168202	478616.307038	50.800999
3483.848355	478262.118946	50.806004
3483.204715	477894.545713	50.811009
3482.744221	477566.923416	50.816013
3482.435870	477180.785754	50.821018
3481.582112	476823.007441	50.826023
3480.607828	476481.865779	50.831028
3480.342808	476095.852387	50.836033
3479.720978	475726.259180	50.841037
3479.000630	475350.389729	50.846042
3478.549784	474989.220491	50.851047
3477.748111	474617.709303	50.856052
3477.315964	474242.128488	50.861057
3476.233826	473867.505190	50.866061
3476.056975	473493.999136	50.871066
3475.594091	473113.789501	50.876071
3474.797977	472730.735998	50.881076
3474.125709	472340.254523	50.886081
3473.248632	471981.887395	50.891085
3472.634847	471592.599093	50.896090
3472.320986	471212.989649	50.901095
3471.471146	470813.381931	50.906100
3470.989986	470438.144615	50.911105
3470.250818	470059.290961	50.916109
3469.827201	469662.635564	50.921114
3469.469777	469270.018193	50.926119
3468.809513	468881.649535	50.931124
3468.295849	468481.081823	50.936129
3467.351569	468089.954685	50.941133
3466.621657	467681.952418	50.946138
3465.888796	467318.259355	50.951143
3465.206496	466881.129020	50.956148
3464.588272	466516.998339	50.961153
3463.800162	466109.329744	50.966157
3463.085945	465702.250127	50.971162
3462.370998	465328.530208	50.976167
3461.877051	464909.534359	50.981172
3461.398476	464525.417862	50.986177
3460.845145	464121.173155	50.991181
3459.832771	463723.332641	50.996186
3459.056846	463341.524025	51.001191
3458.683619	462938.800713	51.006196
3457.784592	462520.988631	51.011201
3456.773563	462155.932736	51.016205
3456.324122	461730.883084	51.021210
3455.189045	461367.304340	51.026215
3454.792257	460957.954301	51.031220
3454.231112	460558.665411	51.036225
3453.048902	460195.733919	51.041229
3452.800802	459782.381963	51.046234
3451.980171	459391.279221	51.051239
3451.108493	459001.039906	51.056244
3450.586842	458625.398149	51.061249
3449.845736	458230.153382	51.066253
3449.025442	457835.421339	51.071258
3448.417922	457462.208313	51.076263
3447.502782	457075.289938	51.081268
3447.211671	456684.157009	51.086273
3446.442095	456288.476306	51.091277
3445.528538	455910.567630	51.096282
3444.980081	455522.498972	51.101287
3443.987590	455158.643148	51.106292
3443.688081	454740.436395	51.111297
3442.541559	454395.060046	51.116301
3442.313324	453988.345061	51.121306
3441.126674	453618.457427	51.126311
3440.292644	453232.018092	51.131316
3439.959661	452867.716679	51.136321
3439.190842	452488.053424	51.141325
3438.428783	452119.647220	51.146330
3437.854529	451733.445852	51.151335
3437.000470	451348.956713	51.156340
3436.290659	450974.739209	51.161345
3435.607939	450610.051218	51.166349
3434.960995	450236.674436	51.171354
3434.397595	449859.979947	51.176359
3433.431283	449479.384805	51.181364
3432.691753	449103.467072	51.186369
3431.864191	448732.631999	51.191373
3431.431667	448368.782674	51.196378
3430.902964	448002.760653	51.201383
3430.263749	447620.256461	51.206388
3429.540209	447242.276240	51.211393
3428.352429	446888.876634	51.216397
3427.957420	446506.772495	51.221402
3427.265223	446139.478507	51.226407
3426.351401	445774.903851	51.231412
3425.595410	445408.217672	51.236417
3424.928228	445046.029088	51.241421
3424.049152	444673.717131	51.246426
3423.358746	444330.301387	51.251431
3422.682102	443972.361656	51.256436
3422.074077	443604.000114	51.261441
3421.178502	443252.936754	51.266445
3420.416058	442897.989422	51.271450
3419.999354	442543.134493	51.276455
3419.322588	442191.107392	51.281460
3418.701336	441837.137416	51.286465
3417.990298	441484.597859	51.291469
3417.168695	441123.897625	51.296474
3416.682392	440757.605651	51.301479
3415.796220	440408.174905	51.306484
3415.111362	440057.082818	51.311489
3414.063542	439713.708956	51.316493
3413.467469	439351.347807	51.321498
3412.841204	439000.612149	51.326503
3412.184086	438653.658716	51.331508
3411.651316	438300.309112	51.336513
3410.737236	437961.636776	51.341517
3410.029548	437610.437397	51.346522
3409.457690	437275.890282	51.351527
3408.638628	436925.358914	51.356532
3407.986863	436573.501461	51.361537
3407.357526	436240.752073	51.366541
3406.218470	435899.244023	51.371546
3405.724353	435546.788757	51.376551
3404.843785	435215.563443	51.381556
3404.458080	434875.166456	51.386561
3403.635055	434544.608765	51.391565
3402.800694	434202.801151	51.396570
3402.404901	433861.275061	51.401575
3401.493384	433539.706223	51.406580
3401.095461	433195.099397	51.411585
3400.437984	432864.620732	51.416589
3399.447506	432523.069270	51.421594
3398.962576	432185.826022	51.426599
3397.828411	431854.114811	51.431604
3397.294144	431522.761544	51.436609
3396.476801	431196.958904	51.441613
3395.943774	430852.367555	51.446618
3395.160448	430526.855852	51.451623
3394.244384	430206.592062	51.456628
3393.829812	429872.735735	51.461633
3392.597931	429551.421944	51.466637
3392.084411	429222.804107	51.471642
3391.639222	428912.607697	51.476647
3390.796388	428593.277634	51.481652
3390.281450	428270.615909	51.486657
3389.519208	427941.031038	51.491661
3388.870981	427621.937839	51.496666
3388.167603	427299.852811	51.501671
3387.111360	426982.314820	51.506676
3386.760779	426658.337733	51.511681
3385.913135	426359.628988	51.516685
3385.042698	426044.920334	51.521690
3384.946137	425713.272529	51.526695
3384.051390	425399.398284	51.531700
3383.334722	425087.397083	51.536705
3382.276976	424781.059242	51.541709
3381.701839	424446.703151	51.546714
3380.864242	424129.046145	51.551719
3380.184821	423827.615917	51.556724
3379.937871	423518.519527	51.561729
3379.032489	423215.772103	51.566733
3378.501117	422888.425729	51.571738
3377.719820	422582.171878	51.576743
3376.953280	422275.048662	51.581748
3376.337785	421959.566636	51.586753
3375.623928	421650.345262	51.591757
3375.196999	421340.414625	51.596762
3374.446008	421036.297974	51.601767
3373.541389	420730.576558	51.606772
3372.983587	420411.740142	51.611777
3372.322884	420104.779387	51.616781
3371.717361	419794.453357	51.621786
3370.648922	419491.233775	51.626791
3369.824393	419181.088016	51.631796
3369.316113	418876.960326	51.636801
3368.620609	418582.969760	51.641805
3368.104092	418271.749144	51.646810
3367.517554	417962.390716	51.651815
3366.388096	417663.251299	51.656820
3366.164158	417359.163985	51.661825
3365.355154	417060.297832	51.666829
3364.600257	416759.057275	51.671834
3364.209378	416454.605658	51.676839
3363.139625	416156.025364	51.681844
3362.587791	415851.618220	51.686849
3361.788781	415558.502114	51.691853
3361.149325	415246.632881	51.696858
3360.125414	414951.284967	51.701863
3359.229165	414670.980491	51.706868
3358.934190	414367.177723	51.711873
3358.282692	414076.741953	51.716877
3357.729778	413779.071767	51.721882
3357.180362	413497.583211	51.726887
3356.154382	413194.061714	51.731892
3355.777458	412899.480050	51.736897
3354.908493	412597.477520	51.741901
3354.222312	412302.786347	51.746906
3353.768873	412011.714440	51.751911
3352.612693	411720.445887	51.756916
3352.442175	411425.816915	51.761921
3351.546306	411139.990131	51.766925
3350.685182	410836.901209	51.771930
3350.030733	410554.181578	51.776935
3348.879179	410265.439193	51.781940
3348.800335	409967.096730	51.786945
3347.873316	409691.247775	51.791949
3346.861384	409412.690646	51.796954
3346.915966	409117.469769	51.801959
3345.949330	408837.248387	51.806964
3345.291118	408547.649188	51.811969
3344.283635	408265.548456	51.816973
3343.826043	407973.269127	51.821978
3343.178587	407688.869773	51.826983
3342.339780	407413.341985	51.831988
3341.588459	407121.482184	51.836993
3340.765454	406851.715811	51.841997
3340.084375	406575.342323	51.847002
3339.544536	406288.346156	51.852007
3338.550654	406021.090180	51.857012
3337.910440	405742.822104	51.862017
3337.647348	405467.262159	51.867021
3336.957275	405191.919795	51.872026
3336.201130	404919.432009	51.877031
3335.416548	404650.250413	51.882036
3335.071775	404359.520328	51.887041
3333.886598	404089.761874	51.892045
3333.231512	403809.445650	51.897050
3332.853005	403535.106979	51.902055
3332.145514	403269.154737	51.907060
3331.692049	402990.298972	51.912065
3330.943729	402725.594077	51.917069
3330.051318	402436.076706	51.922074
3329.357924	402158.268305	51.927079
3328.698988	401892.042702	51.932084
3328.024871	401604.618401	51.937089
3327.253351	401337.846800	51.942093
3326.430778	401060.023900	51.947098
3326.088266	400810.134397	51.952103
3325.144249	400530.038436	51.957108
3324.760287	400257.706076	51.962113
3323.938666	399986.050717	51.967117
3323.116592	399713.198431	51.972122
3322.505720	399449.359991	51.977127
3321.726550	399186.664528	51.982132
3321.472547	398905.632024	51.987137
3320.720555	398641.555191	51.992141
3319.867026	398367.146005	51.997146
3319.304759	398104.839743	52.002151
3318.460070	397829.051947	52.007156
3317.985730	397550.991613	52.012161
3317.182624	397293.674206	52.017165
3316.485092	397025.432121	52.022170
3316.042579	396758.520339	52.027175
3315.126866	396491.249083	52.032180
3314.393442	396214.896451	52.037185
3313.876904	395947.761111	52.042189
3312.861671	395675.338284	52.047194
3312.429202	395420.388462	52.052199
3311.177895	395152.702027	52.057204
3311.199960	394880.922287	52.062209
3310.178954	394640.017175	52.067213
3309.434973	394367.718891	52.072218
3308.747538	394105.096070	52.077223
3307.868685	393840.162468	52.082228
3307.193905	393584.271082	52.087233
3306.633646	393335.453156	52.092237
3305.783690	393074.119371	52.097242
3305.549653	392822.271433	52.102247
3304.307163	392560.919566	52.107252
3303.969596	392296.727508	52.112257
3303.228523	392058.607658	52.117261
3302.781056	391798.039624	52.122266
3302.093575	391544.398042	52.127271
3301.305253	391281.286606	52.132276
3300.592495	391035.018913	52.137281
3299.892177	390781.907788	52.142285
3299.075454	390537.229491	52.147290
3298.992322	390268.913593	52.152295
3298.000808	390024.539080	52.157300
3297.346364	389758.140412	52.162305
3296.687014	389505.496773	52.167309
3295.956040	389252.786383	52.172314
3295.256406	388993.636007	52.177319
3294.583365	388745.972997	52.182324
3293.845841	388486.163805	52.187329
3293.314536	388245.365952	52.192333
3292.258740	387989.875469	52.197338
3291.877578	387750.143981	52.202343
3290.923785	387489.751510	52.207348
3290.086120	387235.874067	52.212353
3289.518192	386989.987820	52.217357
3289.241112	386745.986542	52.222362
3288.550595	386492.665509	52.227367
3287.384328	386251.217369	52.232372
3287.205232	385997.023689	52.237377
3286.392172	385761.467055	52.242381
3285.446095	385514.079453	52.247386
3284.918206	385264.386168	52.252391
3284.291845	385022.488532	52.257396
3283.608346	384774.367815	52.262401
3282.904800	384530.114110	52.267405
3282.221537	384298.062516	52.272410
3281.419120	384045.174694	52.277415
3280.760796	383800.603877	52.282420
3280.256170	383559.262395	52.287425
3279.449753	383317.509322	52.292429
3278.728183	383078.513353	52.297434
3278.328095	382832.827246	52.302439
3277.482779	382590.694179	52.307444
3277.011103	382354.375350	52.312449
3276.137367	382108.606863	52.317453
3275.547239	381863.656641	52.322458
3274.735407	381620.062421	52.327463
3274.011578	381373.807690	52.332468
3273.675497	381135.959306	52.337473
3272.911793	380897.108883	52.342477
3272.289643	380658.412621	52.347482
3271.432328	380407.391302	52.352487
3270.641343	380175.814760	52.357492
3270.016601	379928.441453	52.362497
3269.038024	379695.798052	52.367501
3268.681236	379454.636149	52.372506
3268.003846	379224.562027	52.377511
3267.162272	379000.871175	52.382516
3266.549211	378742.144650	52.387521
3266.032439	378519.951200	52.392525
3265.430650	378275.717728	52.397530
3264.616666	378031.083908	52.402535
3263.584397	377809.171473	52.407540
3263.409986	377558.710605	52.412545
3262.591166	377339.101847	52.417549
3262.081929	377101.103671	52.422554
3261.281572	376877.521456	52.427559
3260.583642	376633.827245	52.432564
3260.319175	376396.116826	52.437569
3258.976886	376161.144566	52.442573
3258.222269	375920.049507	52.447578
3257.505724	375705.223130	52.452583
3256.709914	375472.907586	52.457588
3256.477959	375235.185185	52.462593
3255.504052	375026.577115	52.467597
3255.241523	374792.265539	52.472602
3254.519947	374558.584853	52.477607
3253.685078	374338.148297	52.482612
3253.066091	374102.413774	52.487617
3252.313914	373863.366606	52.492621
3251.750478	373640.670278	52.497626
3251.229583	373409.062666	52.502631
3250.325718	373199.798278	52.507636
3249.668803	372952.768592	52.512641
3248.840203	372733.619836	52.517645
3247.918630	372507.667061	52.522650
3247.467366	372278.509692	52.527655
3246.934732	372067.247541	52.532660
3246.268260	371827.157548	52.537665
3245.447263	371612.936910	52.542669
3244.875325	371377.306707	52.547674
3244.293524	371158.517715	52.552679
3243.315722	370933.252243	52.557684
3242.927517	370701.354284	52.562689
3241.994622	370485.059579	52.567693
3241.203484	370274.872405	52.572698
3240.772510	370050.991291	52.577703
3240.048226	369822.194543	52.582708
3239.345137	369604.205414	52.587713
3238.847951	369388.523143	52.592717
3238.403399	369157.465284	52.597722
3237.417346	368934.683800	52.602727
3236.606783	368721.795388	52.607732
3236.115118	368498.399198	52.612737
3235.244452	368278.776236	52.617741
3234.446452	368053.187397	52.622746
3234.084091	367833.303699	52.627751
3233.333091	367626.124856	52.632756
3232.876442	367401.445450	52.637761
3231.749066	367183.358674	52.642765
3231.334982	366964.242076	52.647770
3230.840314	366751.116036	52.652775
3230.051104	366540.656116	52.657780
3229.642282	366307.898412	52.662785
3229.037573	366086.721370	52.667789
3227.819930	365870.423406	52.672794
3227.669558	365644.261884	52.677799
3226.638922	365422.919961	52.682804
3226.177142	365202.275694	52.687809
3225.487301	364994.642411	52.692813
3224.604787	364765.335585	52.697818
3223.730232	364547.959275	52.702823
3222.803057	364342.803115	52.707828
3222.774326	364127.962561	52.712833
3221.857832	363908.528906	52.717837
3221.239162	363694.059521	52.722842
3220.835444	363475.713094	52.727847
3219.769401	363271.515532	52.732852
3219.523411	363061.538732	52.737857
3218.367698	362839.898740	52.742861
3217.960215	362627.273867	52.747866
3217.471499	362403.338056	52.752871
3216.481625	362204.925102	52.757876
3215.950007	361977.228226	52.762881
3215.124484	361773.367705	52.767885
3214.407225	361558.802276	52.772890
3213.748014	361346.516746	52.777895
3213.172527	361144.929454	52.782900
3212.410754	360924.006875	52.787905
3211.828328	360716.540984	52.792909
3210.838287	360512.777387	52.797914
3210.710195	360289.512403	52.802919
3209.532990	360077.226807	52.807924
3209.208628	359876.892152	52.812929
3208.460689	359669.753250	52.817933
3207.519104	359460.124925	52.822938
3206.963154	359244.760174	52.827943
3206.143932	359044.703916	52.832948
3205.536022	358834.892863	52.837953
3204.903900	358639.691053	52.842957
3204.143635	358432.345235	52.847962
3203.705601	358221.308672	52.852967
3202.564586	358024.327298	52.857972
3202.172811	357811.347690	52.862977
3201.463225	357615.568772	52.867981
3200.901430	357419.205859	52.872986
3200.172455	357209.915947	52.877991
3199.522882	357002.088539	52.882996
3198.806304	356803.050248	52.888001
3198.233877	356589.381435	52.893005
3197.625298	356392.640152	52.898010
3197.099336	356190.591883	52.903015
3195.952701	355998.438438	52.908020
3195.537683	355792.960999	52.913025
3194.866901	355597.753326	52.918029
3194.055874	355385.414995	52.923034
3193.672239	355184.129073	52.928039
3192.864981	354993.852190	52.933044
3192.519204	354778.740188	52.938049
3191.657598	354590.073653	52.943053
3191.141042	354371.296908	52.948058
3190.353229	354171.139784	52.953063
3189.440153	353971.536127	52.958068
3188.973350	353757.507849	52.963073
3188.285516	353564.229239	52.968077
3187.449640	353364.381984	52.973082
3187.015174	353162.561756	52.978087
3186.344404	352952.278029	52.983092
3185.531881	352754.918786	52.988097
3184.732124	352548.318572	52.993101
3184.026302	352360.255521	52.998106
3183.453417	352158.758724	53.003111
3182.910196	351954.584226	53.008116
3182.183083	351755.273534	53.013121
3181.784094	351557.768037	53.018125
3180.697167	351352.964644	53.023130
3180.124156	351156.732252	53.028135
3179.262245	350954.793065	53.033140
3178.826366	350757.061393	53.038145
3178.097801	350560.622378	53.043149
3176.823591	350378.495889	53.048154
3176.826129	350173.770139	53.053159
3176.190336	349986.909292	53.058164
3175.629745	349778.835286	53.063169
3174.964777	349590.145226	53.068173
3174.165662	349390.888078	53.073178
3173.683054	349194.608822	53.078183
3172.675998	348998.208231	53.083188
3172.002556	348792.108082	53.088193
3171.798659	348600.567474	53.093197
3170.733144	348402.570570	53.098202
3170.047635	348197.742697	53.103207
3169.407819	348008.839635	53.108212
3168.531312	347815.264794	53.113217
3167.775225	347636.661409	53.118221
3167.191197	347426.953340	53.123226
3166.580699	347236.541369	53.128231
3165.778712	347070.109547	53.133236
3165.307342	346861.908684	53.138241
3164.476339	346672.598697	53.143245
3163.756268	346482.354241	53.148250
3163.350643	346295.648204	53.153255
3162.626611	346103.850511	53.158260
3161.896829	345910.678640	53.163265
3161.105058	345717.465022	53.168269
3160.278793	345532.375676	53.173274
3159.856202	345348.061814	53.178279
3158.977520	345164.201324	53.183284
3158.415205	344969.599895	53.188289
3157.971370	344794.781645	53.193293
3156.973701	344595.717185	53.198298
3156.761296	344406.403702	53.203303
3155.898468	344218.108844	53.208308
3155.177686	344029.027303	53.213313
3154.448770	343836.510210	53.218317
3153.844812	343652.066987	53.223322
3153.348512	343460.911821	53.228327
3152.319677	343276.967373	53.233332
3152.085983	343102.899934	53.238337
3151.441639	342905.250213	53.243341
3150.564883	342717.309161	53.248346
3150.025227	342528.805103	53.253351
3149.195054	342343.451838	53.258356
3148.541000	342152.342920	53.263361
3147.706738	341965.003709	53.268365
3147.131489	341775.586582	53.273370
3146.889807	341575.806999	53.278375
3145.648937	341401.690394	53.283380
3145.242508	341213.161182	53.288385
3144.617117	341030.367907	53.293389
3143.803843	340844.065596	53.298394
3143.529428	340651.644644	53.303399
3142.936777	340469.710002	53.308404
3142.057845	340273.183455	53.313409
3141.267950	340078.602249	53.318413
3140.740085	339889.960960	53.323418
3140.296008	339708.687887	53.328423
3139.103855	339521.397911	53.333428
3138.616037	339328.217545	53.338433
3137.929447	339141.101004	53.343437
3137.292563	338953.085101	53.348442
3136.678084	338766.439705	53.353447
3135.692737	338586.190932	53.358452
3135.207691	338386.312407	53.363457
3134.807799	338206.860887	53.368461
3134.037634	338018.405126	53.373466
3133.155031	337824.391731	53.378471
3132.258474	337654.054166	53.383476
3132.054109	337464.005356	53.388481
3131.332507	337281.445613	53.393485
3130.549850	337089.883474	53.398490
3129.803575	336911.934205	53.403495
3128.923981	336721.608240	53.408500
3128.229309	336543.675268	53.413505
3127.625416	336355.570259	53.418509
3127.008725	336189.384960	53.423514
3126.468872	335997.577585	53.428519
3125.644117	335835.802892	53.433524
3124.991285	335636.120741	53.438529
3124.599814	335469.821647	53.443533
3123.833539	335278.098959	53.448538
3123.370575	335103.485823	53.453543
3122.369718	334914.752249	53.458548
3121.750899	334742.377622	53.463553
3120.828401	334544.644218	53.468557
3120.502249	334379.019466	53.473562
3120.244422	334185.533063	53.478567
3119.134777	334026.115768	53.483572
3118.413965	333838.073185	53.488577
3117.924661	333652.335561	53.493581
3117.091084	333468.713992	53.498586
3116.580035	333285.040905	53.503591
3115.661362	333111.207647	53.508596
3115.213326	332922.228406	53.513601
3114.290640	332745.034434	53.518605
3113.441944	332566.708156	53.523610
3113.205217	332394.241786	53.528615
3112.233450	332223.978880	53.533620
3111.626449	332050.806525	53.538625
3111.267887	331866.876500	53.543629
3110.564597	331685.775513	53.548634
3109.718295	331504.493033	53.553639
3109.094127	331323.938702	53.558644
3108.242822	331154.036074	53.563649
3107.889271	330969.466505	53.568653
3107.003550	330797.506343	53.573658
3106.518479	330612.371134	53.578663
3105.751902	330439.576599	53.583668
3104.924064	330268.828059	53.588673
3104.162999	330094.631606	53.593677
3103.195642	329918.430670	53.598682
3103.039804	329748.898457	53.603687
3102.027138	329572.016476	53.608692
3101.350472	329401.725743	53.613697
3100.658626	329234.899476	53.618701
3100.211928	329064.164239	53.623706
3099.715175	328884.169346	53.628711
3098.592622	328723.163910	53.633716
3098.308781	328559.734062	53.638721
3097.699539	328377.464419	53.643725
3097.086260	328202.578249	53.648730
3096.519307	328032.521673	53.653735
3095.600571	327865.957444	53.658740
3094.970584	327687.406555	53.663745
3094.370427	327516.615765	53.668749
3093.466834	327345.414340	53.673754
3092.902598	327156.769734	53.678759
3092.258360	326999.834966	53.683764
3091.695815	326823.766499	53.688769
3091.040556	326663.370243	53.693773
3089.889460	326494.675752	53.698778
3089.493569	326311.323640	53.703783
3089.072089	326140.272441	53.708788
3088.570431	325970.939400	53.713793
3087.968285	325794.391172	53.718797
3087.209295	325624.156090	53.723802
3086.704681	325437.254727	53.728807
3085.710925	325272.275444	53.733812
3085.190261	325090.162393	53.738817
3084.258439	324918.349164	53.743821
3083.831076	324744.266125	53.748826
3083.297430	324574.273249	53.753831
3082.193808	324405.617800	53.758836
3081.893492	324230.036843	53.763841
3081.010921	324058.646858	53.768845
3080.178597	323894.963226	53.773850
3080.036080	323709.731970	53.778855
3078.931888	323536.313645	53.783860
3078.536909	323371.184882	53.788865
3077.873929	323197.390502	53.793869
3077.146695	323027.043193	53.798874
3076.470411	322855.770874	53.803879
3075.628493	322683.353205	53.808884
3074.883006	322502.237612	53.813889
3074.316147	322341.666169	53.818893
3073.396959	322180.462727	53.823898
3072.921862	322012.594180	53.828903
3072.036083	321833.561765	53.833908
3071.185619	321675.401892	53.838913
3070.461505	321502.912302	53.843917
3069.904961	321348.804646	53.848922
3069.602553	321178.972081	53.853927
3068.863295	321028.813887	53.858932
3068.219075	320860.715282	53.863937
3067.684267	320692.599043	53.868941
3066.796336	320528.230350	53.873946
3066.293185	320360.057552	53.878951
3065.649745	320199.621630	53.883956
3065.117627	320024.297967	53.888961
3064.419165	319856.486147	53.893965
3063.789292	319694.417608	53.898970
3062.928171	319521.614871	53.903975
3062.251401	319359.400387	53.908980
3061.590825	319184.630147	53.913985
3060.892029	319028.071193	53.918989
3060.077439	318862.312920	53.923994
3059.551216	318693.224062	53.928999
3058.780221	318538.941866	53.934004
3058.202499	318378.568751	53.939009
3057.725891	318211.202621	53.944013
3057.261159	318047.271766	53.949018
3056.561761	317872.759844	53.954023
3055.673099	317703.955735	53.959028
3055.043684	317543.156522	53.964033
3054.446559	317373.770973	53.969037
3053.689289	317205.047042	53.974042
3053.237270	317028.813887	53.979047
3052.377574	316866.573145	53.984052
3051.730239	316701.446672	53.989057
3051.038178	316539.815430	53.994061
3050.404569	316375.959386	53.999066
3049.810406	316210.314411	54.004071
3048.862401	316043.910341	54.009076
3048.297944	315873.600351	54.014081
3047.650099	315713.692257	54.019085
3046.926462	315543.228654	54.024090
3046.591195	315375.402406	54.029095
3045.760976	315213.943657	54.034100
3044.721416	315047.679741	54.039105
3044.263390	314887.536590	54.044109
3043.430137	314729.438723	54.049114
3043.320291	314547.748777	54.054119
3042.433518	314390.728328	54.059124
3042.019095	314222.505298	54.064129
3041.243506	314049.526534	54.069133
3040.224482	313900.725561	54.074138
3039.991285	313738.329710	54.079143
3038.980426	313567.093453	54.084148
3038.653322	313394.500976	54.089153
3037.768552	313229.457380	54.094157
3037.053927	313069.377515	54.099162
3036.362755	312895.823298	54.104167
3035.374900	312737.033913	54.109172
3035.024021	312576.539250	54.114177
3034.093888	312407.809297	54.119181
3033.590733	312249.324444	54.124186
3033.210959	312087.254862	54.129191
3032.441460	311932.860498	54.134196
3031.769783	311766.354958	54.139201
3030.950846	311610.643832	54.144205
3029.955627	311452.999644	54.149210
3029.794363	311279.944677	54.154215
3028.877240	311134.408673	54.159220
3028.246622	310968.099161	54.164225
3027.684050	310810.843955	54.169229
3026.694884	310645.329187	54.174234
3026.237237	310487.878677	54.179239
3025.556977	310343.882969	54.184244
3025.050832	310178.647581	54.189249
3024.344980	310017.365108	54.194253
3023.787937	309854.912952	54.199258
3023.226166	309693.327116	54.204263
3022.390324	309540.009521	54.209268
3021.879928	309368.636679	54.214273
3021.272707	309199.698065	54.219277
3020.655729	309042.398153	54.224282
3020.026087	308876.569331	54.229287
3019.190061	308712.224443	54.234292
3018.508982	308543.704033	54.239297
3018.031538	308384.802356	54.244301
3017.181423	308229.855594	54.249306
3016.833375	308054.457195	54.254311
3015.665630	307893.168575	54.259316
3015.145962	307727.702762	54.264321
3014.881009	307566.270824	54.269325
3013.974420	307410.618955	54.274330
3013.123420	307241.308782	54.279335
3012.525174	307085.302124	54.284340
3011.782043	306916.993051	54.289345
3010.903788	306746.795252	54.294349
3010.450245	306600.238165	54.299354
3009.863157	306429.866534	54.304359
3009.098794	306279.895001	54.309364
3008.234648	306116.697104	54.314369
3007.774394	305951.346912	54.319373
3007.165680	305800.535302	54.324378
3006.754450	305637.137795	54.329383
3005.721609	305475.697458	54.334388
3004.987576	305313.827647	54.339393
3004.278652	305153.608927	54.344397
3003.380553	304999.073319	54.349402
3003.085937	304839.170632	54.354407
3002.498138	304690.722768	54.359412
3001.664541	304532.967753	54.364417
3000.759897	304368.220739	54.369421
3000.359453	304216.865086	54.374426
2999.920689	304058.690515	54.379431
2999.061011	303903.943874	54.384436
2998.564791	303743.384260	54.389441
2997.777615	303591.554368	54.394445
2996.782598	303435.911868	54.399450
2996.476123	303274.481319	54.404455
2995.807210	303119.856425	54.409460
2994.873982	302958.804857	54.414465
2994.281240	302805.313539	54.419469
2993.517680	302650.499403	54.424474
2992.817439	302495.496818	54.429479
2992.243058	302357.663731	54.434484
2991.799379	302196.279178	54.439489
2991.385738	302032.215756	54.444493
2990.022419	301882.920038	54.449498
2989.737130	301734.141116	54.454503
2989.186312	301577.636897	54.459508
2988.280732	301415.713440	54.464513
2987.642825	301267.091746	54.469517
2986.732462	301119.990081	54.474522
2986.328903	300958.317742	54.479527
2985.425669	300811.138259	54.484532
2984.854208	300663.269464	54.489537
2984.249839	300506.059589	54.494541
2983.141135	300355.932647	54.499546
2982.803078	300212.814167	54.504551
2982.234490	300065.020764	54.509556
2981.782708	299910.307330	54.514561
2981.151577	299753.992286	54.519565
2980.263282	299606.911206	54.524570
2979.673552	299447.711605	54.529575
2979.135784	299303.630751	54.534580
2978.205044	299143.415246	54.539585
2977.741464	298994.636537	54.544589
2976.781135	298850.927785	54.549594
2976.220532	298692.970726	54.554599
2975.676872	298542.727235	54.559604
2974.903545	298392.188902	54.564609
2974.178823	298249.257288	54.569613
2973.508313	298101.656566	54.574618
2973.076267	297938.508728	54.579623
2972.273580	297796.582292	54.584628
2971.680746	297642.780470	54.589633
2970.892411	297487.939858	54.594637
2970.209215	297347.624028	54.599642
2969.710374	297198.161776	54.604647
2969.004104	297051.253459	54.609652
2968.464100	296899.301728	54.614657
2967.816973	296746.551890	54.619661
2967.105577	296601.757782	54.624666
2966.645724	296438.587541	54.629671
2965.568052	296296.474278	54.634676
2965.085850	296141.354882	54.639681
2964.705938	295977.356650	54.644685
2963.902937	295831.583248	54.649690
2962.947378	295678.295641	54.654695
2962.461282	295532.242646	54.659700
2961.863140	295384.042579	54.664705
2960.918791	295237.094161	54.669709
2960.536368	295084.479381	54.674714
2960.160097	294920.657969	54.679719
2959.264724	294783.277116	54.684724
2958.376245	294629.163143	54.689729
2957.936319	294472.380393	54.694733
2956.803426	294323.372858	54.699738
2956.448638	294174.878721	54.704743
2955.497345	294028.439889	54.709748
2954.977903	293872.509702	54.714753
2954.582195	293729.981076	54.719757
2953.706706	293587.095365	54.724762
2953.281489	293424.426571	54.729767
2952.425069	293287.293262	54.734772
2951.755725	293134.340491	54.739777
2951.283741	292972.646531	54.744781
2950.527665	292827.067354	54.749786
2949.896588	292678.488610	54.754791
2948.962741	292527.105348	54.759796
2948.676544	292376.103342	54.764801
2947.912676	292225.355130	54.769805
2947.233376	292082.488350	54.774810
2946.817520	291923.306054	54.779815
2946.112481	291784.186893	54.784820
2945.315003	291632.756006	54.789825
2945.049576	291478.006419	54.794829
2944.438134	291324.279280	54.799834
2943.675225	291157.638500	54.804839
2942.797819	291001.406511	54.809844
2941.942277	290841.019746	54.814849
2941.255250	290693.543752	54.819853
2940.630824	290545.039059	54.824858
2939.785354	290393.971575	54.829863
2939.109439	290240.381333	54.834868
2938.734906	290088.526027	54.839873
2938.224244	289936.412041	54.844877
2937.321780	289772.874064	54.849882
2936.504560	289640.112965	54.854887
2935.960421	289488.997273	54.859892
2935.578846	289337.753893	54.864897
2935.003004	289183.052104	54.869901
2934.228665	289026.267832	54.874906
2933.422749	288878.300328	54.879911
2932.911815	288719.080219	54.884916
2932.114855	288579.591923	54.889921
2931.392938	288419.590086	54.894925
2930.560049	288266.558452	54.899930
2930.155138	288111.039540	54.904935
2929.281977	287969.933088	54.909940
2928.728176	287815.252572	54.914945
2928.233005	287656.105819	54.919949
2927.521791	287522.104537	54.924954
2926.664622	287354.279457	54.929959
2926.192463	287211.275497	54.934964
2925.604620	287049.647264	54.939969
2925.044208	286901.232474	54.944973
2924.368508	286741.782779	54.949978
2923.622241	286586.011571	54.954983
2923.149516	286438.219399	54.959988
2922.256943	286281.274224	54.964993
2921.761359	286125.947018	54.969997
2921.072178	285978.137991	54.975002
2920.806784	285821.551748	54.980007
2919.791145	285651.535225	54.985012
2918.724204	285499.456251	54.990017
2918.292430	285339.381562	54.995021
2917.502649	285191.053328	55.000026
2917.206890	285033.274575	55.005031
2916.064292	284890.732404	55.010036
2915.556875	284734.489662	55.015041
2915.121023	284563.616841	55.020045
2914.139448	284421.380103	55.025050
2914.000867	284267.829350	55.030055
2913.220294	284105.593680	55.035060
2912.534936	283964.659707	55.040065
2911.766118	283796.589862	55.045069
2911.314505	283643.954372	55.050074
2910.552761	283477.767935	55.055079
2909.664700	283326.092829	55.060084
2908.987235	283168.195566	55.065089
2908.810255	283016.815274	55.070093
2907.872793	282858.806268	55.075098
2907.398040	282709.153931	55.080103
2906.652335	282546.402854	55.085108
2905.709772	282386.076907	55.090113
2904.920929	282228.273398	55.095117
2904.145434	282072.912682	55.100122
2903.797406	281920.744179	55.105127
2903.105454	281764.707980	55.110132
2902.187450	281613.164473	55.115137
2901.902510	281457.318436	55.120141
2901.383291	281314.651077	55.125146
2900.683927	281151.612124	55.130151
2900.067142	280989.349573	55.135156
2899.216297	280844.977306	55.140161
2898.742545	280675.611852	55.145165
2897.608678	280524.509766	55.150170
2897.212635	280367.076566	55.155175
2896.585741	280214.493392	55.160180
2895.957670	280059.923846	55.165185
2895.424140	279903.734799	55.170189
2894.315488	279747.203819	55.175194
2893.789026	279602.346998	55.180199
2892.739002	279419.319621	55.185204
2892.179395	279274.340652	55.190209
2891.721324	279120.915567	55.195213
2890.971450	278964.633267	55.200218
2890.196080	278811.742271	55.205223
2889.804013	278664.062511	55.210228
2888.807245	278512.429007	55.215233
2888.742460	278356.649389	55.220237
2887.568783	278210.621426	55.225242
2887.048117	278050.737139	55.230247
2886.807507	277905.834825	55.235252
2885.852169	277746.223071	55.240257
2885.310559	277594.797545	55.245261
2884.382371	277450.080457	55.250266
2883.946280	277284.172159	55.255271
2883.379808	277136.443441	55.260276
2882.503706	276983.950214	55.265281
2882.330664	276811.582193	55.270285
2881.587687	276667.599771	55.275290
2880.760249	276498.034989	55.280295
2880.223472	276354.427394	55.285300
2879.652921	276186.477364	55.290305
2879.062544	276027.800956	55.295309
2877.843331	275884.199522	55.300314
2877.204616	275707.524606	55.305319
2876.701401	275566.585849	55.310324
2875.910930	275403.993503	55.315329
2875.557818	275251.493792	55.320333
2874.924164	275086.049620	55.325338
2874.425374	274917.655229	55.330343
2873.425623	274764.442914	55.335348
2872.648635	274610.405809	55.340353
2872.122358	274459.130531	55.345357
2871.321210	274297.660487	55.350362
2870.936257	274139.308095	55.355367
2870.120692	273982.704804	55.360372
2869.352466	273839.337585	55.365377
2869.287976	273659.235403	55.370381
2868.356070	273515.308342	55.375386
2867.862398	273344.239007	55.380391
2867.168730	273195.537122	55.385396
2866.614096	273021.192041	55.390401
2865.770924	272861.154953	55.395405
2865.111751	272709.289561	55.400410
2864.547215	272544.929694	55.405415
2864.029675	272381.733945	55.410420
2863.314180	272213.908848	55.415425
2862.672362	272043.321519	55.420429
2861.868828	271883.049036	55.425434
2860.985562	271721.515779	55.430439
2860.330169	271561.449094	55.435444
2859.565919	271391.390605	55.440449
2859.234723	271226.535517	55.445453
2858.377339	271074.268730	55.450458
2858.188027	270905.239884	55.455463
2857.370062	270746.115921	55.460468
2856.605655	270588.282387	55.465473
2855.700709	270416.871048	55.470477
2855.104174	270258.909116	55.475482
2854.636099	270091.936555	55.480487
2853.804128	269927.644886	55.485492
2853.056155	269780.811208	55.490497
2852.564506	269608.672413	55.495501
2851.635818	269454.405200	55.500506
2851.324691	269279.945748	55.505511
2850.695737	269123.950235	55.510516
2849.587727	268965.814875	55.515521
2849.391669	268799.487170	55.520525
2848.413587	268638.300589	55.525530
2847.937252	268475.710246	55.530535
2847.201763	268321.972999	55.535540
2846.593720	268160.753412	55.540545
2845.714416	267989.618741	55.545549
2844.947113	267833.772792	55.550554
2844.623645	267676.786939	55.555559
2843.746588	267511.076787	55.560564
2843.062891	267361.330104	55.565569
2842.400735	267193.421220	55.570573
2841.702626	267041.613985	55.575578
2841.090027	266874.130316	55.580583
2840.573200	266723.236792	55.585588
2839.988032	266560.129412	55.590593
2839.504042	266382.769361	55.595597
2838.296767	266237.410040	55.600602
2837.945458	266074.826093	55.605607
2837.619971	265913.384180	55.610612
2836.573902	265749.662428	55.615617
2836.104543	265580.985001	55.620621
2835.196572	265425.722384	55.625626
2834.480044	265255.963628	55.630631
2833.870468	265097.801452	55.635636
2833.330278	264939.577413	55.640641
2832.658024	264778.878477	55.645645
2831.453568	264623.688580	55.650650
2831.170226	264460.075764	55.655655
2830.797363	264312.572993	55.660660
2829.713982	264150.742421	55.665665
2829.230806	263989.835593	55.670669
2828.878487	263830.716341	55.675674
2828.235326	263663.722668	55.680679
2827.422994	263501.416502	55.685684
2826.477461	263334.598205	55.690689
2826.312189	263173.921544	55.695693
2825.518173	263015.967723	55.700698
2824.539327	262852.465767	55.705703
2823.973466	262675.960785	55.710708
2823.138124	262513.964344	55.715713
2822.522453	262355.065748	55.720717
2821.744192	262205.361416	55.725722
2821.426878	262044.200019	55.730727
2820.874206	261884.222029	55.735732
2820.200292	261724.263321	55.740737
2819.825098	261544.494351	55.745741
2819.192854	261398.154505	55.750746
2818.332368	261227.758328	55.755751
2817.517676	261065.988579	55.760756
2816.866161	260896.654616	55.765761
2816.298879	260730.541818	55.770765
2815.410215	260568.274705	55.775770
2814.836781	260403.945814	55.780775
2814.305124	260241.112998	55.785780
2813.517399	260081.300551	55.790785
2813.097416	259906.531362	55.795789
2811.801595	259753.573976	55.800794
2811.361933	259589.759208	55.805799
2810.539272	259433.849228	55.810804
2810.044352	259271.367725	55.815809
2809.411180	259106.386925	55.820813
2808.615436	258958.775408	55.825818
2808.237772	258773.380282	55.830823
2807.340709	258624.562561	55.835828
2806.469889	258471.844239	55.840833
2806.226968	258311.258976	55.845837
2805.417801	258154.456281	55.850842
2804.975337	257982.977271	55.855847
2804.469676	257821.084162	55.860852
2803.523285	257649.557859	55.865857
2803.074680	257491.170450	55.870861
2802.218216	257333.102414	55.875866
2801.637493	257166.713909	55.880871
2801.267620	256994.714775	55.885876
2800.416762	256843.267710	55.890881
2800.162986	256671.479641	55.895885
2799.335722	256505.054264	55.900890
2798.446799	256335.200691	55.905895
2798.047284	256166.619508	55.910900
2797.232187	256000.650999	55.915905
2796.565489	255829.973141	55.920909
2795.794649	255664.889237	55.925914
2795.282293	255496.224582	55.930919
2794.569122	255326.165703	55.935924
2793.469755	255163.273467	55.940929
2793.188077	254992.280642	55.945933
2792.500859	254828.202844	55.950938
2791.862903	254661.188659	55.955943
2791.380035	254493.156835	55.960948
2790.690499	254335.752183	55.965953
2790.135024	254155.100477	55.970957
2789.184690	253988.467401	55.975962
2788.766030	253809.959043	55.980967
2788.418855	253645.777437	55.985972
2787.328739	253483.419921	55.990977
2786.673319	253305.178731	55.995981
2786.061182	253144.375690	56.000986
2785.346970	252966.551603	56.005991
2784.396902	252804.605431	56.010996
2783.830286	252633.965412	56.016001
2783.516206	252459.287265	56.021005
2782.673165	252297.451925	56.026010
2782.243731	252125.873852	56.031015
2781.449153	251947.223084	56.036020
2780.630360	251792.693317	56.041025
2780.240437	251622.892142	56.046029
2779.482208	251449.558662	56.051034
2778.755759	251272.731391	56.056039
2778.248155	251111.455214	56.061044
2777.468059	250939.831973	56.066049
2776.746365	250767.766724	56.071053
2776.204603	250596.004218	56.076058
2775.706068	250425.406502	56.081063
2774.951992	250251.487855	56.086068
2774.177905	250082.742254	56.091073
2773.359043	249910.158485	56.096077
2772.571488	249749.259025	56.101082
2771.935916	249582.580249	56.106087
2771.425532	249411.730801	56.111092
2770.887500	249243.789076	56.116097
2770.357145	249061.075855	56.121101
2769.433928	248896.989985	56.126106
2768.826541	248720.961524	56.131111
2768.386602	248549.668926	56.136116
2767.308459	248397.118854	56.141121
2766.909876	248212.221130	56.146125
2766.075948	248036.764121	56.151130
2765.450009	247870.009248	56.156135
2765.029806	247710.963663	56.161140
2764.261733	247537.610488	56.166145
2763.703655	247358.596264	56.171149
2762.596726	247188.735081	56.176154
2762.336548	247022.407079	56.181159
2761.864495	246845.111540	56.186164
2760.584933	246680.931727	56.191169
2760.337962	246504.033876	56.196173
2759.452159	246339.970346	56.201178
2759.215942	246170.048846	56.206183
2758.542494	246005.544615	56.211188
2757.719665	245834.112085	56.216193
2757.335537	245656.294781	56.221197
2756.471854	245483.901453	56.226202
2756.054663	245304.001650	56.231207
2755.192734	245123.306691	56.236212
2754.232431	244951.464112	56.241217
2753.740377	244778.121513	56.246221
2753.084284	244602.462290	56.251226
2752.134360	244428.123110	56.256231
2751.629556	244253.993775	56.261236
2750.835904	244091.242534	56.266241
2750.492851	243919.761888	56.271245
2749.670789	243762.974455	56.276250
2749.284153	243580.831167	56.281255
2748.806834	243394.628049	56.286260
2747.732514	243226.498232	56.291265
2747.086313	243049.107878	56.296269
2746.477591	242886.608970	56.301274
2745.821092	242704.713386	56.306279
2745.136463	242540.928220	56.311284
2744.081940	242369.256748	56.316289
2744.004587	242192.566909	56.321293
2743.230467	242026.708456	56.326298
2742.602387	241848.934946	56.331303
2742.288897	241666.655497	56.336308
2740.960485	241501.369381	56.341313
2740.642970	241314.507410	56.346317
2739.832819	241144.810661	56.351322
2739.160565	240967.987629	56.356327
2738.741681	240798.305787	56.361332
2737.948655	240624.685486	56.366337
2737.424669	240437.602935	56.371341
2736.391388	240264.657834	56.376346
2735.940904	240091.951714	56.381351
2735.221919	239916.818315	56.386356
2734.612094	239744.774561	56.391361
2733.878573	239570.306065	56.396365
2733.041378	239398.909988	56.401370
2732.262761	239223.634297	56.406375
2731.477798	239051.695715	56.411380
2730.860114	238889.076309	56.416385
2730.633197	238719.010591	56.421389
2729.924120	238566.006171	56.426394
2729.110429	238381.672058	56.431399
2728.796352	238209.150888	56.436404
2727.831132	238037.547979	56.441409
2727.403827	237859.952457	56.446413
2726.772856	237691.098194	56.451418
2726.320059	237501.844744	56.456423
2725.813530	237329.890180	56.461428
2724.938158	237156.084517	56.466433
2724.147576	236973.251481	56.471437
2723.469584	236798.982242	56.476442
2722.788555	236619.264511	56.481447
2722.362324	236442.587839	56.486452
2721.327335	236271.177029	56.491457
2721.045645	236088.595930	56.496461
2719.955165	235913.909675	56.501466
2719.604916	235737.782349	56.506471
2718.796383	235552.662887	56.511476
2717.966957	235386.008116	56.516481
2717.640183	235207.637182	56.521485
2717.192126	235035.778945	56.526490
2716.329256	234855.074518	56.531495
2715.979692	234665.988053	56.536500
2714.872623	234490.110066	56.541505
2714.127913	234305.135532	56.546509
2713.337912	234141.022879	56.551514
2712.597155	233960.759048	56.556519
2712.169452	233786.378860	56.561524
2711.199435	233617.228426	56.566529
2710.761940	233437.579547	56.571533
2709.870995	233269.944965	56.576538
2709.281231	233098.519908	56.581543
2708.795538	232924.659691	56.586548
2708.008264	232748.301274	56.591553
2707.304488	232573.024852	56.596557
2706.660757	232405.454452	56.601562
2705.909161	232224.711748	56.606567
2705.522424	232046.126839	56.611572
2704.580337	231883.136972	56.616577
2704.534593	231704.524151	56.621581
2703.789817	231535.468998	56.626586
2703.012462	231351.676535	56.631591
2702.396517	231186.039037	56.636596
2701.551268	231006.459309	56.641601
2700.926721	230830.613392	56.646605
2700.086552	230654.038098	56.651610
2699.421199	230469.644005	56.656615
2699.055217	230297.984875	56.661620
2698.133887	230129.393111	56.666625
2697.729537	229953.030212	56.671629
2697.253361	229776.144330	56.676634
2696.255012	229594.809280	56.681639
2695.636557	229414.178273	56.686644
2694.887428	229252.435590	56.691649
2694.725752	229059.078380	56.696653
2693.748600	228889.020997	56.701658
2693.245796	228706.005158	56.706663
2692.658437	228531.074446	56.711668
2691.648875	228361.761602	56.716673
2691.184345	228170.414859	56.721677
2690.470918	227994.843187	56.726682
2689.674589	227812.919635	56.731687
2688.828408	227638.668250	56.736692
2688.120704	227470.786085	56.741697
2687.862117	227288.549298	56.746701
2686.930055	227120.015906	56.751706
2686.363294	226930.266705	56.756711
2685.919589	226757.048187	56.761716
2685.111292	226579.483009	56.766721
2684.392076	226398.288623	56.771725
2683.762262	226225.546247	56.776730
2683.262720	226042.688323	56.781735
2682.497850	225867.218301	56.786740
2681.659415	225689.481558	56.791745
2681.383186	225495.042971	56.796749
2680.570917	225331.713653	56.801754
2680.094008	225154.175397	56.806759
2679.429491	224971.842458	56.811764
2678.695658	224795.886048	56.816769
2677.746700	224607.195655	56.821773
2676.984118	224442.141661	56.826778
2676.459444	224263.479924	56.831783
2675.946847	224087.260861	56.836788
2675.048334	223912.656401	56.841793
2674.677584	223723.227241	56.846797
2673.905124	223545.522927	56.851802
2673.192210	223371.857735	56.856807
2672.845138	223199.344318	56.861812
2671.946428	223012.508313	56.866817
2670.821991	222840.335246	56.871821
2670.399361	222662.933938	56.876826
2669.917620	222475.192980	56.881831
2669.046499	222305.654243	56.886836
2668.290565	222145.695938	56.891841
2667.944467	221956.025269	56.896845
2666.968760	221784.123768	56.901850
2666.446731	221607.186169	56.906855
2665.986259	221433.116147	56.911860
2665.065486	221264.084032	56.916865
2664.340992	221084.175510	56.921869
2663.993225	220910.878068	56.926874
2663.235177	220734.068999	56.931879
2662.663982	220548.090898	56.936884
2661.877897	220389.273993	56.941889
2661.279183	220201.022522	56.946893
2660.767764	220026.900168	56.951898
2660.177190	219843.918323	56.956903
2659.638440	219660.954178	56.961908
2658.264016	219483.227373	56.966913
2658.296492	219306.818358	56.971917
2657.548661	219131.551739	56.976922
2656.945818	218947.708469	56.981927
2656.055083	218769.715827	56.986932
2654.926235	218593.148834	56.991937
2654.738870	218415.605712	56.996941
2654.299942	218243.525517	57.001946
2653.760697	218064.498776	57.006951
2653.040796	217867.693057	57.011956
2652.411940	217688.121373	57.016961
2652.024477	217502.160096	57.021965
2651.248887	217320.015859	57.026970
2650.663350	217132.623094	57.031975
2649.857226	216941.472545	57.036980
2648.890826	216757.590666	57.041985
2648.316754	216556.615858	57.046989
2647.174728	216387.566474	57.051994
2646.773725	216219.011081	57.056999
2646.240767	216032.402115	57.062004
2645.696649	215858.307790	57.067009
2645.049135	215668.752155	57.072013
2644.044130	215489.398447	57.077018
2643.429524	215304.650047	57.082023
2643.135533	215122.231601	57.087028
2642.372806	214945.819431	57.092033
2641.805597	214757.742840	57.097037
2641.338626	214578.611768	57.102042
2640.465930	214389.808160	57.107047
2640.045383	214193.741869	57.112052
2639.220369	214018.767573	57.117057
2638.527206	213824.311150	57.122061
2637.711926	213647.796149	57.127066
2637.254649	213459.031173	57.132071
2636.623122	213277.994947	57.137076
2636.131832	213087.378090	57.142081
2635.462793	212892.207795	57.147085
2634.503879	212706.591943	57.152090
2633.399663	212525.059913	57.157095
2633.002537	212346.318360	57.162100
2632.347830	212161.495913	57.167105
2631.848726	211971.443576	57.172109
2631.075816	211794.875931	57.177114
2630.180322	211611.213266	57.182119
2629.900987	211422.986002	57.187124
2628.855017	211251.885201	57.192129
2628.614336	211061.629139	57.197133
2627.814632	210874.185967	57.202138
2627.269294	210692.035978	57.207143
2626.671825	210516.016810	57.212148
2625.721249	210337.979465	57.217153
2625.287026	210152.682408	57.222157
2624.319988	209965.688451	57.227162
2623.672617	209786.790056	57.232167
2623.108343	209593.165961	57.237172
2622.250017	209423.631320	57.242177
2621.770997	209234.627644	57.247181
2621.198981	209053.377558	57.252186
2620.605042	208867.664159	57.257191
2620.090146	208674.620564	57.262196
2619.230045	208500.901432	57.267201
2618.557220	208322.304022	57.272205
2617.599848	208138.966775	57.277210
2617.296434	207952.739201	57.282215
2616.850927	207770.149227	57.287220
2615.614179	207586.819727	57.292225
2615.481576	207405.581255	57.297229
2614.502191	207215.441290	57.302234
2613.747469	207030.968030	57.307239
2613.125850	206850.203249	57.312244
2612.514948	206670.162751	57.317249
2611.848409	206481.477321	57.322253
2610.919879	206303.511834	57.327258
2610.143869	206124.326393	57.332263
2609.779503	205945.076267	57.337268
2609.023723	205764.768752	57.342273
2608.515104	205582.399079	57.347277
2607.721852	205399.845991	57.352282
2606.994633	205224.015394	57.357287
2606.663734	205044.317278	57.362292
2605.832823	204865.462535	57.367297
2605.325427	204677.495807	57.372301
2604.332948	204495.397092	57.377306
2603.772905	204318.130104	57.382311
2603.408806	204141.023507	57.387316
2602.373740	203962.560242	57.392321
2601.992443	203776.981743	57.397325
2601.152737	203598.946800	57.402330
2600.334308	203420.081835	57.407335
2600.020913	203234.621598	57.412340
2599.055167	203065.465720	57.417345
2598.892098	202874.548772	57.422349
2598.168878	202695.887345	57.427354
2597.535629	202515.926898	57.432359
2596.924872	202318.847015	57.437364
2596.043748	202147.109832	57.442369
2595.210609	201955.424085	57.447373
2594.697379	201768.842276	57.452378
2594.071886	201592.230467	57.457383
2593.603571	201402.283153	57.462388
2592.808297	201231.120574	57.467393
2592.140865	201035.810358	57.472397
2591.548152	200851.000375	57.477402
2590.725164	200665.336709	57.482407
2590.026763	200481.804549	57.487412
2589.182020	200297.723545	57.492417
2588.777189	200127.787809	57.497421
2587.921199	199936.901674	57.502426
2587.626359	199754.160616	57.507431
2586.953732	199563.004957	57.512436
2586.354546	199386.790566	57.517441
2585.894870	199194.482639	57.522445
2584.986005	199013.419316	57.527450
2584.172010	198816.715060	57.532455
2583.758945	198631.031577	57.537460
2582.916630	198452.135602	57.542465
2582.376962	198261.752459	57.547469
2581.333956	198079.911879	57.552474
2580.847659	197895.324189	57.557479
2580.555196	197712.157067	57.562484
2579.401687	197530.755806	57.567489
2579.108719	197338.313638	57.572493
2578.107031	197154.191957	57.577498
2577.557871	196975.089104	57.582503
2577.143893	196775.135141	57.587508
2576.179036	196596.137634	57.592513
2575.581032	196409.435132	57.597517
2575.203778	196226.681102	57.602522
2574.234264	196048.487868	57.607527
2573.994815	195854.719346	57.612532
2573.281263	195667.312538	57.617537
2572.580014	195469.432315	57.622541
2571.613113	195288.569182	57.627546
2570.699141	195104.746272	57.632551
2570.382899	194905.547515	57.637556
2569.938414	194733.026997	57.642561
2569.272170	194541.786840	57.647565
2568.346532	194366.251853	57.652570
2567.899479	194172.522607	57.657575
2567.228667	193973.154666	57.662580
2566.143232	193792.404717	57.667585
2565.764032	193602.611331	57.672589
2564.970752	193420.569482	57.677594
2564.425841	193238.272633	57.682599
2563.922995	193046.236115	57.687604
2562.917706	192868.403268	57.692609
2562.402981	192673.659923	57.697613
2561.841070	192488.263945	57.702618
2561.148098	192299.301388	57.707623
2560.452387	192109.474791	57.712628
2559.790849	191928.142782	57.717633
2559.326087	191738.077444	57.722637
2558.490861	191555.629229	57.727642
2557.650646	191359.403135	57.732647
2557.083086	191181.977777	57.737652
2556.418975	191005.204528	57.742657
2555.832357	190805.187130	57.747661
2555.040415	190613.065983	57.752666
2554.382102	190427.527695	57.757671
2554.101382	190245.530896	57.762676
2553.056158	190073.096385	57.767681
2552.640100	189870.803865	57.772685
2552.046045	189691.505188	57.777690
2551.180469	189509.298517	57.782695
2551.228397	189307.074800	57.787700
2550.074789	189126.899989	57.792705
2549.263044	188930.323051	57.797709
2548.541883	188744.648580	57.802714
2547.703807	188549.693169	57.807719
2547.165192	188360.505295	57.812724
2546.532165	188173.763134	57.817729
2545.829977	187998.915414	57.822733
2545.389890	187811.736999	57.827738
2544.461153	187617.970279	57.832743
2544.378705	187427.492534	57.837748
2543.443575	187246.565137	57.842753
2542.607997	187046.628479	57.847757
2542.003642	186871.095209	57.852762
2541.584735	186680.724735	57.857767
2540.818655	186484.099951	57.862772
2540.173448	186302.061651	57.867777
2539.486158	186115.374525	57.872781
2538.887354	185915.138087	57.877786
2538.182158	185729.231404	57.882791
2537.569142	185531.708639	57.887796
2536.838399	185343.097846	57.892801
2536.122068	185152.742688	57.897805
2535.170736	184966.967176	57.902810
2534.541336	184781.115963	57.907815
2534.386758	184577.558297	57.912820
2533.415233	184397.296726	57.917825
2532.721254	184203.863436	57.922829
2532.056025	184019.598492	57.927834
2531.097081	183842.899121	57.932839
2531.037004	183644.291997	57.937844
2530.094849	183455.977034	57.942849
2529.493002	183264.199677	57.947853
2528.859583	183076.956844	57.952858
2527.723458	182889.463727	57.957863
2527.469779	182701.144619	57.962868
2526.625358	182527.345423	57.967873
2525.955890	182331.359489	57.972877
2525.347763	182146.622594	57.977882
2524.344931	181959.939157	57.982887
2523.923745	181780.669529	57.987892
2523.440012	181598.891864	57.992897
2522.734315	181403.857145	57.997901
2522.350039	181217.625830	58.002906
2521.392500	181039.550937	58.007911
2521.239780	180836.989652	58.012916
2520.405166	180648.402557	58.017921
2519.720227	180452.071350	58.022925
2518.781595	180257.307671	58.027930
2518.079964	180074.985801	58.032935
2517.592129	179885.660194	58.037940
2517.115290	179706.662372	58.042945
2516.409260	179502.783129	58.047949
2515.710176	179317.881917	58.052954
2514.809905	179127.174963	58.057959
2514.372339	178931.994468	58.062964
2513.583376	178748.369240	58.067969
2512.928560	178559.177750	58.072973
2512.239034	178367.359636	58.077978
2511.814183	178174.266644	58.082983
2511.481848	177990.356107	58.087988
2510.443888	177803.747203	58.092993
2509.939128	177603.724654	58.097997
2509.503351	177407.749606	58.103002
2508.649255	177216.815031	58.108007
2507.805402	177022.292876	58.113012
2506.910554	176829.115229	58.118017
2506.422246	176628.039059	58.123021
2505.761641	176445.802685	58.128026
2505.070081	176251.488951	58.133031
2504.456058	176046.378166	58.138036
2503.687194	175865.039123	58.143041
2502.906025	175679.136766	58.148045
2502.320494	175487.976822	58.153050
2501.420536	175290.686307	58.158055
2501.231588	175097.277710	58.163060
2500.476942	174911.374637	58.168065
2500.038112	174722.598839	58.173069
2499.248044	174530.140353	58.178074
2498.422627	174340.422844	58.183079
2497.760400	174139.386453	58.188084
2497.053052	173954.014441	58.193089
2496.387850	173771.930627	58.198093
2495.916285	173576.310231	58.203098
2495.025710	173385.590086	58.208103
2494.715526	173190.798103	58.213108
2493.734841	173007.368774	58.218113
2493.296355	172816.236299	58.223117
2492.493124	172624.971784	58.228122
2491.920748	172432.794068	58.233127
2490.936301	172240.669878	58.238132
2490.134955	172062.888597	58.243137
2489.780697	171862.120061	58.248141
2489.173254	171684.195289	58.253146
2488.460683	171493.646768	58.258151
2487.736375	171298.929703	58.263156
2486.669251	171110.410442	58.268161
2486.424452	170920.744359	58.273165
2485.651703	170739.212911	58.278170
2485.028574	170553.093110	58.283175
2484.601650	170358.931291	58.288180
2483.537971	170178.415070	58.293185
2483.344882	169984.446963	58.298189
2482.673433	169795.019302	58.303194
2481.757874	169607.182724	58.308199
2481.500446	169416.597637	58.313204
2480.632195	169235.520727	58.318209
2479.904448	169032.918427	58.323213
2479.368108	168852.121346	58.328218
2478.374457	168658.426678	58.333223
2477.774521	168457.307715	58.338228
2476.977986	168270.501556	58.343233
2476.464185	168086.945043	58.348237
2475.791917	167891.295863	58.353242
2475.031673	167705.987247	58.358247
2474.507251	167524.736776	58.363252
2473.759054	167334.990104	58.368257
2473.462067	167147.919537	58.373261
2472.940686	166955.799056	58.378266
2472.090205	166757.310160	58.383271
2471.555222	166568.245640	58.388276
2470.691785	166386.265988	58.393281
2470.204377	166182.216626	58.398285
2469.769536	165982.585104	58.403290
2469.005200	165799.778790	58.408295
2468.369217	165596.900580	58.413300
2467.657365	165409.866293	58.418305
2466.935419	165204.257304	58.423309
2466.429944	165017.573741	58.428314
2465.558026	164822.785985	58.433319
2465.061002	164612.643411	58.438324
2464.036736	164431.029414	58.443329
2463.534853	164232.651302	58.448333
2462.796140	164039.944557	58.453338
2462.142094	163847.555992	58.458343
2461.626343	163656.405289	58.463348
2460.911076	163455.166210	58.468353
2460.273343	163205.460057	58.473357
2459.696668	163018.187632	58.478362
2458.719468	162819.282226	58.483367
2458.216040	162622.031986	58.488372
2457.873469	162433.225153	58.493377
2457.092957	162239.301251	58.498381
2456.391741	162037.521080	58.503386
2455.663996	161830.151972	58.508391
2455.124884	161641.202437	58.513396
2454.324849	161455.562786	58.518401
2453.876958	161255.742962	58.523405
2453.000140	161062.260238	58.528410
2452.281759	160867.710905	58.533415
2451.641848	160664.670062	58.538420
2450.720992	160482.741631	58.543425
2450.060483	160285.834254	58.548429
2449.411687	160088.748122	58.553434
2448.897317	159901.876197	58.558439
2448.225396	159701.579353	58.563444
2447.512246	159512.325433	58.568449
2447.138099	159316.852811	58.573453
2446.412533	159130.743109	58.578458
2445.641810	158940.929289	58.583463
2445.141058	158737.216368	58.588468
2444.509782	158546.874051	58.593473
2443.606778	158343.634005	58.598477
2443.197781	158149.559132	58.603482
2442.437769	157951.078769	58.608487
2441.890445	157755.235509	58.613492
2440.984031	157578.519358	58.618497
2440.608018	157360.200505	58.623501
2439.822445	157179.780566	58.628506
2438.516475	156988.829120	58.633511
2438.397402	156790.139391	58.638516
2437.794134	156603.833133	58.643521
2437.165249	156403.662831	58.648525
2436.807617	156212.082293	58.653530
2435.519306	156025.786071	58.658535
2435.194703	155817.409756	58.663540
2434.357426	155618.179638	58.668545
2433.486230	155421.434888	58.673549
2433.042348	155234.500645	58.678554
2432.111943	155053.479269	58.683559
2431.443563	154854.252275	58.688564
2430.558816	154671.801987	58.693569
2429.954970	154476.405903	58.698573
2429.613500	154287.973392	58.703578
2428.734486	154109.402242	58.708583
2428.051499	153921.051346	58.713588
2427.516284	153732.690790	58.718593
2426.991380	153552.541105	58.723597
2426.236268	153353.082511	58.728602
2425.454835	153167.802127	58.733607
2425.248992	152982.723875	58.738612
2424.364965	152787.343907	58.743617
2423.580419	152593.004316	58.748621
2423.074393	152395.571118	58.753626
2422.198848	152211.823556	58.758631
2421.743245	152013.253386	58.763636
2420.970953	151833.609801	58.768641
2420.498764	151631.333067	58.773645
2419.850336	151437.105784	58.778650
2418.975612	151254.659879	58.783655
2418.613030	151053.754742	58.788660
2417.607607	150866.184056	58.793665
2416.758908	150676.314487	58.798669
2416.233596	150485.581307	58.803674
2415.461285	150294.113091	58.808679
2415.105722	150115.200859	58.813684
2413.967424	149925.839122	58.818689
2413.573876	149740.529218	58.823693
2413.215521	149548.300723	58.828698
2412.673307	149356.242321	58.833703
2412.126769	149158.199554	58.838708
2411.538713	148974.157691	58.843713
2410.620357	148775.782222	58.848717
2409.820892	148586.641497	58.853722
2409.273231	148400.982420	58.858727
2408.601336	148202.914558	58.863732
2407.786101	148008.848584	58.868737
2407.102751	147814.356189	58.873741
2406.599162	147629.660474	58.878746
2405.496735	147441.883553	58.883751
2405.182459	147244.362245	58.888756
2404.602849	147056.987638	58.893761
2403.853724	146863.121489	58.898765
2403.401816	146681.028348	58.903770
2402.300428	146487.334720	58.908775
2402.124498	146291.513045	58.913780
2401.112402	146097.350148	58.918785
2400.514378	145910.951070	58.923789
2400.080699	145719.443775	58.928794
2399.099443	145528.113416	58.933799
2398.764761	145328.942539	58.938804
2398.032355	145138.019884	58.943809
2397.292492	144948.370360	58.948813
2396.659200	144752.745146	58.953818
2395.832046	144569.351276	58.958823
2395.535804	144374.653487	58.963828
2394.690021	144197.555029	58.968833
2394.014967	143993.757544	58.973837
2393.494587	143797.612130	58.978842
2392.838226	143611.896794	58.983847
2391.634295	143416.370460	58.988852
2391.250642	143224.984912	58.993857
2390.773322	143027.566838	58.998861
2389.888465	142836.377528	59.003866
2389.264863	142639.302810	59.008871
2388.722638	142444.948420	59.013876
2388.022785	142274.394574	59.018881
2387.333892	142070.942363	59.023885
2386.936997	141882.095901	59.028890
2386.079301	141696.817956	59.033895
2385.530694	141496.485836	59.038900
2384.884736	141306.996275	59.043905
2383.824660	141113.050121	59.048909
2383.643598	140907.517567	59.053914
2382.729422	140724.478082	59.058919
2382.309172	140533.432831	59.063924
2381.362161	140351.264820	59.068929
2380.647400	140156.355216	59.073933
2380.271475	139948.941484	59.078938
2379.169300	139766.191733	59.083943
2378.895784	139564.100810	59.088948
2378.268988	139371.342299	59.093953
2377.643411	139188.024987	59.098957
2376.784429	138992.269124	59.103962
2375.867154	138809.622944	59.108967
2375.250643	138606.322337	59.113972
2374.413921	138425.762096	59.118977
2374.108064	138236.339587	59.123981
2373.452160	138047.609034	59.128986
2372.807461	137860.084869	59.133991
2371.907967	137666.847011	59.138996
2371.299043	137482.800679	59.144001
2370.723622	137286.236104	59.149005
2369.980875	137099.990063	59.154010
2369.331478	136909.588736	59.159015
2369.048556	136718.037956	59.164020
2368.394427	136527.919346	59.169025
2367.380617	136339.955196	59.174029
2366.976725	136146.165971	59.179034
2366.225471	135961.567333	59.184039
2365.847225	135769.669442	59.189044
2365.245938	135567.213121	59.194049
2364.495682	135366.077616	59.199053
2363.915762	135174.507806	59.204058
2362.410779	134983.047825	59.209063
2362.376558	134790.784245	59.214068
2361.237890	134607.182983	59.219073
2360.780997	134403.479639	59.224077
2360.507528	134222.093764	59.229082
2359.545694	134035.089017	59.234087
2359.003069	133842.836131	59.239092
2358.234203	133651.789082	59.244097
2357.508797	133458.830966	59.249101
2357.115782	133259.279454	59.254106
2356.211855	133067.940134	59.259111
2356.008249	132882.258083	59.264116
2355.098903	132678.460861	59.269121
2354.195700	132485.423173	59.274125
2353.761796	132294.573416	59.279130
2352.885111	132119.660415	59.284135
2352.350664	131918.832348	59.289140
2351.704350	131726.432297	59.294145
2350.921883	131535.388863	59.299149
2350.609498	131343.446547	59.304154
2349.496034	131148.787320	59.309159
2348.663679	130956.269581	59.314164
2348.024559	130769.298594	59.319169
2347.646538	130576.546284	59.324173
2347.101433	130390.655249	59.329178
2346.255900	130196.823826	59.334183
2345.655047	130001.405371	59.339188
2344.900638	129818.053500	59.344193
2344.536506	129629.344519	59.349197
2344.100462	129425.508420	59.354202
2343.063593	129238.979041	59.359207
2342.553128	129045.762922	59.364212
2341.803324	128848.572610	59.369217
2341.132747	128661.074558	59.374221
2340.776932	128461.665379	59.379226
2339.588561	128275.369704	59.384231
2339.190099	128067.892514	59.389236
2338.386932	127887.672734	59.394241
2337.893569	127694.272814	59.399245
2337.311457	127499.986603	59.404250
2336.530159	127312.972459	59.409255
2336.200570	127115.842173	59.414260
2335.482280	126914.837932	59.419265
2334.612535	126727.752898	59.424269
2333.778466	126523.594904	59.429274
2333.134292	126338.153142	59.434279
2332.964175	126126.260283	59.439284
2331.917422	125942.332808	59.444289
2331.503378	125748.489551	59.449293
2331.026282	125548.041294	59.454298
2329.950328	125352.616802	59.459303
2329.505711	125148.712135	59.464308
2328.728034	124958.805430	59.469313
2327.768456	124757.525188	59.474317
2327.284456	124570.698595	59.479322
2326.612732	124376.931403	59.484327
2325.984238	124170.307628	59.489332
2325.240953	123985.977057	59.494337
2324.688128	123791.915851	59.499341
2324.371027	123584.701156	59.504346
2323.170721	123411.113711	59.509351
2322.920284	123201.275544	59.514356
2322.149187	123002.099168	59.519361
2321.271680	122809.391781	59.524365
2320.951210	122614.819733	59.529370
2320.058706	122427.933164	59.534375
2319.546685	122219.083844	59.539380
2318.839864	122032.830893	59.544385
2317.950868	121835.015205	59.549389
2317.637520	121636.563714	59.554394
2316.770157	121446.086673	59.559399
2316.099950	121245.739298	59.564404
2315.061693	121057.323735	59.569409
2314.809608	120861.928383	59.574413
2314.273531	120665.132049	59.579418
2313.371236	120477.498989	59.584423
2312.668440	120274.561291	59.589428
2312.096954	120091.335134	59.594433
2311.458322	119882.664044	59.599437
2310.858313	119691.916073	59.604442
2310.097038	119495.532430	59.609447
2309.603365	119304.072120	59.614452
2308.798642	119113.386233	59.619457
2308.140641	118924.697174	59.624461
2307.783924	118712.442143	59.629466
2306.670490	118526.532471	59.634471
2306.381205	118330.527131	59.639476
2305.600630	118143.386701	59.644481
2304.501825	117945.995497	59.649485
2304.356865	117739.948457	59.654490
2303.452741	117540.802871	59.659495
2302.647638	117356.401575	59.664500
2302.133535	117159.615568	59.669505
2301.463407	116962.424170	59.674509
2300.666640	116764.162587	59.679514
2300.103373	116576.104073	59.684519
2299.868259	116379.495618	59.689524
2299.132185	116184.516892	59.694529
2298.414342	115985.728331	59.699533
2298.071839	115791.464572	59.704538
2297.002755	115593.007711	59.709543
2296.446197	115384.791581	59.714548
2295.628131	115201.943904	59.719553
2295.391105	114989.459458	59.724557
2294.611916	114799.715524	59.729562
2293.708192	114600.713388	59.734567
2293.364448	114403.972398	59.739572
2292.552611	114196.688744	59.744577
2291.929429	113996.117268	59.749581
2291.228153	113792.348274	59.754586
2290.171979	113596.983237	59.759591
2289.887170	113396.159782	59.764596
2289.098581	113192.530086	59.769601
2288.633360	112993.826521	59.774605
2287.792638	112794.657317	59.779610
2287.036194	112610.625514	59.784615
2286.600195	112402.738572	59.789620
2285.794630	112204.196803	59.794625
2285.149408	112015.785403	59.799629
2284.638634	111815.346838	59.804634
2283.749209	111617.356143	59.809639
2283.104604	111412.994660	59.814644
2282.800688	111212.344115	59.819649
2281.910412	111014.415485	59.824653
2281.335106	110807.173214	59.829658
2280.552642	110623.172954	59.834663
2280.277516	110410.860347	59.839668
2279.340373	110213.193068	59.844673
2278.573073	110016.261945	59.849677
2277.793471	109802.276787	59.854682
2277.299543	109615.833233	59.859687
2276.361145	109415.094879	59.864692
2275.552499	109211.317055	59.869697
2275.185586	109027.237462	59.874701
2274.862461	108816.900703	59.879706
2273.847635	108632.406507	59.884711
2273.176830	108422.115602	59.889716
2272.700372	108219.257888	59.894721
2271.515315	108021.520735	59.899725
2271.262154	107823.573941	59.904730
2270.696577	107634.878929	59.909735
2270.051607	107430.569742	59.914740
2269.312405	107233.758155	59.919745
2268.690920	107030.831863	59.924750
2268.370121	106829.534680	59.929754
2267.279070	106634.109900	59.934759
2266.691168	106426.665733	59.939764
2266.351221	106230.592130	59.944769
2265.153885	106033.399833	59.949774
2264.733516	105835.178626	59.954778
2264.005829	105637.261588	59.959783
2263.421569	105431.843066	59.964788
2262.783283	105241.903066	59.969793
2262.132871	105033.389596	59.974798
2261.619916	104824.538923	59.979802
2260.578739	104623.793253	59.984807
2259.946920	104434.099753	59.989812
2259.340014	104232.343195	59.994817
2258.553048	104033.490878	59.999822
2257.806684	103830.744766	60.004826
2257.319488	103643.020404	60.009831
2256.699590	103437.174325	60.014836
2255.976209	103249.725279	60.019841
2255.377586	103042.343998	60.024846
2255.007462	102844.463303	60.029850
2254.244793	102645.168396	60.034855
2253.474961	102436.696729	60.039860
2252.774861	102236.551628	60.044865
2251.856516	102046.459657	60.049870
2251.751452	101835.255234	60.054874
2250.865229	101640.968268	60.059879
2250.247365	101430.223111	60.064884
2249.497142	101234.040253	60.069889
2248.821693	101046.683675	60.074894
2248.222240	100830.606136	60.079898
2247.806410	100626.249419	60.084903
2246.683247	100438.461280	60.089908
2246.216412	100231.242600	60.094913
2245.893080	100030.777565	60.099918
2245.448788	99827.605891	60.104922
2244.622848	99627.224070	60.109927
2243.904236	99410.760017	60.114932
2242.991818	99213.681202	60.119937
2242.246126	99002.572421	60.124942
2241.753213	98805.468619	60.129946
2240.904566	98608.226302	60.134951
2240.535171	98402.442063	60.139956
2239.642231	98196.558772	60.144961
2239.051027	97991.859947	60.149966
2238.786703	97795.952692	60.154970
2237.790806	97588.296247	60.159975
2237.442438	97362.570724	60.164980
2236.586775	97164.739426	60.169985
2235.883305	96970.500860	60.174990
2235.372417	96754.973961	60.179994
2234.588024	96560.009687	60.184999
2234.053815	96342.885805	60.190004
2233.224778	96133.554518	60.195009
2232.846698	95922.821801	60.200014
2232.255207	95723.629327	60.205018
2231.424018	95521.965210	60.210023
2230.772233	95300.811120	60.215028
2230.163520	95087.034276	60.220033
2229.221120	94886.097434	60.225038
2228.782090	94667.560344	60.230042
2227.964323	94479.411323	60.235047
2227.324732	94264.860830	60.240052
2226.912037	94050.263718	60.245057
2226.159098	93842.799739	60.250062
2225.443005	93631.482591	60.255066
2224.857083	93430.178851	60.260071
2224.153402	93219.478749	60.265076
2223.367517	93004.988925	60.270081
2222.871963	92797.633351	60.275086
2222.335947	92584.598129	60.280090
2221.446386	92385.723588	60.285095
2220.701364	92170.081270	60.290100
2220.078581	91953.299312	60.295105
2219.323972	91752.823811	60.300110
2218.905396	91544.687820	60.305114
2218.024550	91339.537534	60.310119
2217.821298	91118.188933	60.315124
2217.041981	90906.343464	60.320129
2216.186972	90705.893412	60.325134
2215.472661	90485.722824	60.330138
2214.482047	90290.421229	60.335143
2213.846711	90075.815511	60.340148
2213.313752	89873.248671	60.345153
2212.455230	89661.890637	60.350158
2212.368816	89458.857365	60.355162
2211.215105	89259.057589	60.360167
2210.918907	89043.970740	60.365172
2210.116418	88839.142114	60.370177
2209.426887	88629.067004	60.375182
2208.939693	88424.179596	60.380186
2208.250684	88214.577570	60.385191
2207.520157	88010.296921	60.390196
2206.711554	87797.243689	60.395201
2206.089545	87586.933401	60.400206
2205.422205	87373.950690	60.405210
2204.999450	87170.364559	60.410215
2204.287482	86961.786320	60.415220
2203.885797	86751.950049	60.420225
2202.985821	86548.432823	60.425230
2202.460747	86325.871788	60.430234
2201.908245	86126.094361	60.435239
2201.012022	85912.534851	60.440244
2200.191789	85702.781577	60.445249
2199.573502	85490.025303	60.450254
2199.248405	85271.842823	60.455258
2198.185159	85081.030794	60.460263
2197.696487	84857.813680	60.465268
2197.140840	84645.315795	60.470273
2196.197123	84443.061640	60.475278
2195.965613	84226.440704	60.480282
2194.913009	84011.416456	60.485287
2194.279888	83817.428945	60.490292
2193.620820	83598.917293	60.495297
2193.032715	83391.818517	60.500302
2192.579529	83161.818820	60.505306
2191.372945	82958.574729	60.510311
2191.027493	82747.495018	60.515316
2190.483457	82546.254105	60.520321
2189.768585	82335.344883	60.525326
2189.323137	82120.560511	60.530330
2188.401762	81918.986173	60.535335
2187.649819	81704.806090	60.540340
2187.220248	81492.269272	60.545345
2186.437419	81287.972765	60.550350
2185.534201	81064.557365	60.555354
2184.681622	80860.187385	60.560359
2184.303258	80652.074702	60.565364
2183.825592	80457.979512	60.570369
2183.012142	80240.034373	60.575374
2182.799638	80024.093875	60.580378
2181.637302	79819.060807	60.585383
2180.969716	79615.459561	60.590388
2180.379760	79403.768026	60.595393
2179.461824	79197.099032	60.600398
2179.205071	78975.618792	60.605402
2177.939140	78781.157404	60.610407
2177.429073	78573.618812	60.615412
2176.883208	78367.127246	60.620417
2176.127266	78171.025502	60.625422
2175.686906	77963.025760	60.630426
2174.687190	77752.030878	60.635431
2174.112609	77546.515305	60.640436
2173.603640	77349.235304	60.645441
2172.610467	77142.750990	60.650446
2172.519744	76926.956720	60.655450
2171.694367	76732.223107	60.660455
2171.045910	76524.144282	60.665460
2170.785676	76316.741002	60.670465
2169.776866	76117.093737	60.675470
2169.342714	75909.120265	60.680474
2168.539206	75698.812477	60.685479
2167.981077	75486.573472	60.690484
2167.108220	75269.964123	60.695489
2166.411503	75062.459166	60.700494
2165.840492	74850.982842	60.705498
2164.877777	74656.031181	60.710503
2164.511384	74437.418004	60.715508
2164.018795	74235.420228	60.720513
2163.143942	74028.144243	60.725518
2162.590559	73805.005992	60.730522
2161.854233	73610.630416	60.735527
2161.081839	73393.315739	60.740532
2160.558421	73194.253929	60.745537
2159.880001	72986.628106	60.750542
2159.308230	72774.483213	60.755546
2158.608385	72569.297829	60.760551
2157.829262	72362.841120	60.765556
2157.340982	72153.115905	60.770561
2156.643076	71949.393638	60.775566
2155.767201	71738.752371	60.780570
2155.168663	71539.668311	60.785575
2154.631356	71328.534246	60.790580
2153.849345	71117.738979	60.795585
2153.469069	70915.224856	60.800590
2152.244378	70704.402870	60.805594
2151.771816	70487.800816	60.810599
2151.172301	70285.853680	60.815604
2150.382065	70078.174648	60.820609
2149.848802	69871.590865	60.825614
2149.395162	69665.756717	60.830618
2148.616110	69464.929626	60.835623
2147.942087	69257.646200	60.840628
2147.288433	69047.663457	60.845633
2146.076234	68848.051517	60.850638
2145.847312	68632.748686	60.855642
2144.796148	68428.802127	60.860647
2144.443040	68232.733757	60.865652
2143.773741	68033.975051	60.870657
2143.203752	67836.792343	60.875662
2142.519807	67625.201954	60.880666
2141.736202	67416.961070	60.885671
2141.295037	67204.171385	60.890676
2140.646466	67013.456869	60.895681
2139.744471	66806.305311	60.900686
2139.086270	66598.287641	60.905690
2138.306201	66402.872274	60.910695
2137.789545	66203.759750	60.915700
2137.322082	65998.311651	60.920705
2136.523337	65791.173579	60.925710
2136.000433	65596.536179	60.930714
2134.898692	65394.918858	60.935719
2134.425026	65201.392209	60.940724
2133.777256	64982.627832	60.945729
2132.799260	64788.742068	60.950734
2132.456653	64586.844964	60.955738
2131.737540	64384.854576	60.960743
2131.218215	64181.707454	60.965748
2130.316355	63997.620151	60.970753
2129.530970	63794.718820	60.975758
2129.202896	63585.209099	60.980762
2128.372706	63385.770265	60.985767
2127.927567	63180.975659	60.990772
2126.915631	62992.302619	60.995777
2126.256622	62791.889879	61.000782
2125.815339	62590.653223	61.005786
2125.047723	62401.542043	61.010791
2124.270356	62195.310129	61.015796
2123.796099	61994.626387	61.020801
2122.668955	61811.666029	61.025806
2122.151854	61610.850692	61.030810
2121.444451	61415.623544	61.035815
2120.861608	61220.593918	61.040820
2120.330732	61031.908393	61.045825
2119.545506	60838.887037	61.050830
2119.101227	60639.108813	61.055834
2118.375292	60450.099187	61.060839
2117.411929	60243.636370	61.065844
2117.206124	60047.235880	61.070849
2116.537605	59860.078066	61.075854
2115.779439	59659.878908	61.080858
2115.251477	59463.690751	61.085863
2114.461567	59259.059855	61.090868
2113.913524	59065.784868	61.095873
2112.774859	58875.413221	61.100878
2112.245787	58677.802773	61.105882
2111.561215	58489.369799	61.110887
2111.052538	58292.769909	61.115892
2110.037747	58098.024899	61.120897
2109.446157	57915.723418	61.125902
2108.933226	57724.333708	61.130906
2107.848509	57537.366525	61.135911
2107.396346	57337.105788	61.140916
2107.065821	57146.449545	61.145921
2106.146961	56974.039778	61.150926
2105.226742	56772.425682	61.155930
2104.632052	56598.616549	61.160935
2103.925512	56412.895179	61.165940
2103.186513	56216.942531	61.170945
2102.508745	56042.683423	61.175950
2101.956440	55847.208292	61.180954
2100.978341	55667.674052	61.185959
2099.963171	55497.410607	61.190964
2099.769765	55316.068493	61.195969
2098.907087	55145.562587	61.200974
2098.482065	54957.406101	61.205978
2097.608126	54775.832368	61.210983
2096.891466	54606.767192	61.215988
2096.291752	54433.760987	61.220993
2095.285748	54261.558221	61.225998
2095.182226	54079.138159	61.231002
2094.023031	53907.652899	61.236007
2093.490379	53731.253583	61.241012
2092.814746	53551.350367	61.246017
2091.765742	53388.684331	61.251022
2090.977623	53219.127571	61.256026
2090.106822	53061.657338	61.261031
2089.875977	52903.931873	61.266036
2089.171952	52739.565159	61.271041
2088.356930	52583.279987	61.276046
2087.489936	52411.942846	61.281050
2086.748396	52257.534686	61.286055
2086.010037	52100.191019	61.291060
2085.598970	51939.129582	61.296065
2084.451030	51795.762994	61.301070
2084.069998	51624.849801	61.306074
2083.355730	51477.933300	61.311079
2082.718834	51334.489287	61.316084
2081.886418	51180.240819	61.321089
2080.989120	51034.882015	61.326094
2080.540482	50873.870863	61.331098
2079.528510	50745.314055	61.336103
2078.760908	50585.447648	61.341108
2078.022898	50445.165341	61.346113
2076.988242	50315.365497	61.351118
2076.279375	50168.462011	61.356122
2075.829648	50037.271041	61.361127
2074.910445	49908.287901	61.366132
2074.514659	49781.044941	61.371137
2073.552113	49652.089510	61.376142
2072.959868	49520.491519	61.381146
2072.408479	49391.403125	61.386151
2071.504207	49263.599155	61.391156
2070.916341	49134.762007	61.396161
2070.265286	49007.875100	61.401166
2069.761346	48880.073625	61.406170
2069.210785	48755.380743	61.411175
2068.493981	48618.076831	61.416180
2067.677129	48499.805665	61.421185
2067.177630	48373.421211	61.426190
2066.622671	48240.406359	61.431194
2065.592757	48104.196886	61.436199
2064.731910	47993.211974	61.441204
2064.305666	47865.905283	61.446209
2063.481690	47741.588739	61.451214
2062.807459	47622.367599	61.456218
2062.098296	47501.058684	61.461223
2061.731114	47372.439714	61.466228
2061.283974	47263.680794	61.471233
2060.072540	47138.088747	61.476238
2059.509328	47006.375087	61.481242
2058.745759	46895.625197	61.486247
2058.320046	46779.429138	61.491252
2057.788610	46653.979358	61.496257
2056.882867	46531.699249	61.501262
2056.440095	46416.975988	61.506266
2055.644061	46287.920553	61.511271
2054.988239	46174.013974	61.516276
2054.578184	46048.495474	61.521281
2053.375158	45929.021763	61.526286
2052.837434	45809.383189	61.531290
2052.233918	45699.403024	61.536295
2051.658151	45584.896080	61.541300
2051.491802	45465.273664	61.546305
2050.410611	45336.305271	61.551310
2049.964773	45225.642001	61.556314
2049.104452	45104.651933	61.561319
2048.329788	44982.055021	61.566324
2047.839753	44871.473751	61.571329
2046.833795	44753.602495	61.576334
2046.257761	44639.541413	61.581338
2045.661208	44527.815308	61.586343
2045.144528	44410.109097	61.591348
2044.725691	44294.826630	61.596353
2043.646196	44177.758461	61.601358
2043.597898	44051.216425	61.606362
2042.585740	43938.418319	61.611367
2041.886711	43826.320801	61.616372
2041.618398	43708.674792	61.621377
2040.303148	43595.639210	61.626382
2040.032880	43477.836942	61.631386
2039.356838	43356.564106	61.636391
2038.850977	43245.638295	61.641396
2038.302734	43118.913565	61.646401
2037.533939	43005.036101	61.651406
2036.930982	42868.072183	61.656410
2036.403054	42744.338681	61.661415
2035.647422	42632.415982	61.666420
2035.241445	42507.080436	61.671425
2034.126516	42393.818513	61.676430
2033.444420	42273.645248	61.681434
2033.001475	42144.947097	61.686439
2032.434905	42030.405160	61.691444
2031.583181	41916.585973	61.696449
2030.552453	41792.069449	61.701454
2030.207811	41660.095827	61.706458
2029.199575	41555.901349	61.711463
2028.608917	41440.377371	61.716468
2028.373639	41324.617522	61.721473
2027.927451	41213.366415	61.726478
2026.985911	41076.906825	61.731482
2026.581097	40961.736026	61.736487
2025.764666	40845.138805	61.741492
2025.325195	40725.601880	61.746497
2024.394538	40595.813249	61.751502
2023.869530	40468.993625	61.756506
2022.881681	40361.492496	61.761511
2022.434751	40242.649443	61.766516
2021.889710	40108.066620	61.771521
2021.130584	40002.828624	61.776526
2020.293621	39878.643045	61.781530
2019.895125	39760.187736	61.786535
2019.134997	39634.608396	61.791540
2018.399940	39518.555886	61.796545
2017.323407	39402.356002	61.801550
2017.059005	39280.758827	61.806554
2016.235591	39171.090629	61.811559
2015.625454	39040.178442	61.816564
2015.320891	38931.309997	61.821569
2014.370147	38808.323285	61.826574
2013.671519	38693.372480	61.831578
2012.797978	38570.934856	61.836583
2012.251388	38455.022509	61.841588
2011.835335	38341.336589	61.846593
2011.188831	38226.186230	61.851598
2010.767514	38095.482146	61.856602
2009.820209	37982.964214	61.861607
2009.030946	37870.377685	61.866612
2008.673457	37738.603934	61.871617
2007.628472	37631.609668	61.876622
2007.125335	37512.396236	61.881626
2006.296175	37394.036823	61.886631
2005.973090	37277.023734	61.891636
2005.300109	37168.914266	61.896641
2004.089949	37049.109736	61.901646
2003.613703	36932.300383	61.906650
2003.198589	36819.116130	61.911655
2002.281502	36703.402614	61.916660
2001.703596	36575.640406	61.921665
2001.155703	36469.282749	61.926670
2000.529728	36344.989968	61.931674
1999.889389	36229.967617	61.936679
1999.235918	36119.848058	61.941684
1998.801601	36012.661240	61.946689
1997.790633	35896.127293	61.951694
1997.375246	35777.139806	61.956698
1996.615196	35657.289551	61.961703
1995.610068	35540.058535	61.966708
1995.375246	35414.977165	61.971713
1994.581600	35305.427326	61.976718
1994.109548	35182.948982	61.981722
1993.199613	35072.126252	61.986727
1992.713450	34957.288878	61.991732
1992.034736	34827.359060	61.996737
1991.155680	34724.142255	62.001742
1990.529524	34601.457134	62.006746
1990.089028	34479.936695	62.011751
1989.379199	34360.928559	62.016756
1988.499423	34241.335035	62.021761
1987.806043	34131.789618	62.026766
1987.133827	34015.178657	62.031770
1986.471092	33910.454858	62.036775
1985.913987	33795.666761	62.041780
1985.304898	33675.285225	62.046785
1984.215508	33570.885727	62.051790
1984.036422	33450.756800	62.056794
1983.525322	33334.395278	62.061799
1982.746392	33230.787807	62.066804
1982.384394	33104.106693	62.071809
1981.515430	32983.831467	62.076814
1980.827321	32867.610354	62.081818
1980.017933	32753.940948	62.086823
1979.282482	32641.978363	62.091828
1978.995847	32516.727836	62.096833
1977.566670	32413.609534	62.101838
1977.383454	32294.134382	62.106842
1976.831519	32182.826865	62.111847
1975.964357	32066.130959	62.116852
1975.480911	31951.038948	62.121857
1974.545244	31839.426460	62.126862
1973.933207	31717.978740	62.131866
1973.332352	31618.335211	62.136871
1972.726255	31506.018467	62.141876
1972.215092	31384.830559	62.146881
1971.323333	31280.458392	62.151886
1970.783201	31158.186438	62.156890
1970.323543	31042.074636	62.161895
1969.360868	30918.335641	62.166900
1968.617937	30817.806194	62.171905
1968.019344	30707.903383	62.176910
1967.170785	30583.734806	62.181914
1966.161084	30483.799622	62.186919
1965.406987	30369.603808	62.191924
1965.130179	30263.263363	62.196929
1964.077279	30156.953575	62.201934
1963.705766	30047.284591	62.206938
1963.471125	29930.170046	62.211943
1962.711745	29827.753242	62.216948
1962.109315	29714.337410	62.221953
1961.026747	29611.783658	62.226958
1960.529221	29503.127401	62.231962
1959.910595	29395.524396	62.236967
1959.048872	29289.515377	62.241972
1958.740166	29175.925518	62.246977
1957.951172	29072.190986	62.251982
1957.308052	28960.486870	62.256986
1956.313714	28857.389836	62.261991
1955.681919	28746.032977	62.266996
1955.169165	28637.993164	62.272001
1954.457147	28551.358541	62.277006
1953.730783	28433.989938	62.282010
1952.948670	28333.622596	62.287015
1952.116707	28226.953800	62.292020
1951.831525	28113.986915	62.297025
1951.171196	28024.035522	62.302030
1950.528318	27909.520135	62.307034
1949.657945	27811.095851	62.312039
1948.912739	27697.955271	62.317044
1948.125588	27613.389759	62.322049
1947.422015	27508.400437	62.327054
1946.962264	27401.320949	62.332058
1946.389972	27306.084658	62.337063
1945.402168	27216.335069	62.342068
1945.344625	27118.318347	62.347073
1944.503409	27013.878561	62.352078
1943.750022	26911.932552	62.357082
1942.816792	26803.869013	62.362087
1942.083027	26702.818495	62.367092
1941.734582	26612.658772	62.372097
1940.792918	26512.400708	62.377102
1940.281247	26420.935490	62.382106
1939.269378	26323.992876	62.387111
1938.715421	26227.268814	62.392116
1938.408840	26122.418195	62.397121
1937.466560	26043.744491	62.402126
1936.823238	25933.140175	62.407130
1936.490868	25854.878429	62.412135
1935.531190	25748.243888	62.417140
1934.934960	25661.250949	62.422145
1934.160146	25558.127453	62.427150
1933.342639	25470.352438	62.432154
1932.442903	25377.247998	62.437159
1931.853338	25290.173082	62.442164
1931.458985	25200.907585	62.447169
1930.451128	25111.736817	62.452174
1929.913592	25027.047315	62.457178
1929.245526	24922.138701	62.462183
1928.604369	24848.920653	62.467188
1928.420521	24751.788160	62.472193
1927.045979	24664.200759	62.477198
1926.723908	24569.128105	62.482202
1925.983534	24488.856785	62.487207
1925.009739	24401.235639	62.492212
1924.783765	24312.350341	62.497217
1924.248059	24235.544779	62.502222
1923.346015	24147.910472	62.507226
1922.742858	24055.888057	62.512231
1921.805530	23953.650439	62.517236
1921.263710	23872.387234	62.522241
1920.368297	23793.476280	62.527246
1920.007965	23694.570563	62.532250
1919.352724	23614.658130	62.537255
1918.752970	23538.745822	62.542260
1918.032843	23440.360776	62.547265
1917.481036	23354.893491	62.552270
1916.650540	23264.479277	62.557274
1915.874872	23178.440417	62.562279
1915.268377	23100.900567	62.567284
1914.752067	23022.876130	62.572289
1913.924283	22934.001657	62.577294
1913.288084	22848.394924	62.582298
1912.458670	22770.123730	62.587303
1911.590707	22684.066664	62.592308
1911.167262	22599.012639	62.597313
1910.719370	22529.768645	62.602318
1909.918712	22437.307620	62.607322
1909.379770	22367.376792	62.612327
1908.429312	22279.563843	62.617332
1907.810993	22188.768312	62.622337
1907.126193	22117.517781	62.627342
1906.566472	22034.749925	62.632346
1906.047840	21957.801040	62.637351
1905.060917	21880.310180	62.642356
1904.485566	21791.885283	62.647361
1903.808648	21718.087997	62.652366
1903.075952	21638.879243	62.657370
1902.226329	21554.482795	62.662375
1901.672747	21489.923533	62.667380
1901.194881	21397.453660	62.672385
1900.045539	21341.915983	62.677390
1899.969507	21246.997042	62.682394
1899.212096	21169.673789	62.687399
1898.071000	21094.174965	62.692404
1897.728733	21027.955928	62.697409
1897.081913	20951.074935	62.702414
1896.456246	20869.625661	62.707418
1895.765277	20814.061291	62.712423
1895.158750	20729.225617	62.717428
1894.635170	20650.478947	62.722433
1893.911833	20577.153892	62.727438
1893.350359	20502.128841	62.732442
1892.821645	20416.811134	62.737447
1891.807813	20342.780063	62.742452
1891.370717	20259.784134	62.747457
1890.649829	20187.771933	62.752462
1890.113578	20105.149433	62.757466
1889.279798	20027.479943	62.762471
1888.849864	19954.252144	62.767476
1888.171214	19866.347113	62.772481
1887.280958	19806.827712	62.777486
1886.479297	19726.103526	62.782490
1886.334984	19646.617557	62.787495
1885.191307	19566.461676	62.792500
1884.609902	19490.473531	62.797505
1883.791704	19427.338085	62.802510
1883.202896	19338.848178	62.807514
1882.416944	19264.959314	62.812519
1881.725892	19205.263728	62.817524
1881.475899	19122.939645	62.822529
1880.366614	19052.555528	62.827534
1879.790165	18991.570318	62.832538
1879.379306	18908.847768	62.837543
1878.528076	18838.367988	62.842548
1878.206127	18762.054426	62.847553
1877.167300	18693.601247	62.852558
1876.412910	18618.152034	62.857562
1875.684602	18557.510781	62.862567
1875.161234	18492.931021	62.867572
1874.857663	18413.135951	62.872577
1873.956244	18344.444996	62.877582
1873.214044	18272.407891	62.882586
1872.810191	18195.338820	62.887591
1871.873160	18133.800426	62.892596
1871.289417	18055.830655	62.897601
1870.559966	17972.616969	62.902606
1869.972521	17915.248543	62.907610
1869.288920	17843.742109	62.912615
1868.476685	17771.720414	62.917620
1868.044112	17697.608803	62.922625
1867.141708	17635.477589	62.927630
1866.702770	17567.896010	62.932634
1865.859267	17483.962982	62.937639
1865.239800	17424.575061	62.942644
1864.751567	17358.022517	62.947649
1864.047232	17284.884349	62.952654
1863.629732	17207.936796	62.957658
1862.822391	17136.670344	62.962663
1861.713705	17068.118193	62.967668
1861.471209	16996.977411	62.972673
1860.405481	16921.416542	62.977678
1859.975254	16859.400549	62.982682
1859.046162	16787.847574	62.987687
1858.392690	16721.972260	62.992692
1858.225958	16659.661056	62.997697
1857.646932	16591.496586	63.002702
1856.919114	16511.546168	63.007706
1856.284112	16447.671080	63.012711
1855.209458	16380.703161	63.017716
1855.039635	16303.728861	63.022721
1854.066831	16244.146809	63.027726
1853.556970	16166.731280	63.032730
1852.987555	16100.268068	63.037735
1852.551739	16027.408344	63.042740
1851.926910	15943.158276	63.047745
1850.952161	15883.437822	63.052750
1850.599413	15797.720626	63.057754
1849.505940	15722.507261	63.062759
1848.677080	15664.629434	63.067764
1848.310757	15582.011650	63.072769
1847.250844	15520.276631	63.077774
1846.272148	15454.728500	63.082778
1845.906603	15388.421468	63.087783
1845.361323	15329.140317	63.092788
1844.797214	15256.566451	63.097793
1843.728825	15193.360887	63.102798
1843.348847	15139.570226	63.107802
1842.750192	15065.045333	63.112807
1841.730934	14999.832046	63.117812
1841.448908	14933.719810	63.122817
1840.723680	14876.829682	63.127822
1839.641729	14806.756406	63.132826
1839.277129	14742.792764	63.137831
1838.892051	14684.266181	63.142836
1838.309400	14610.494296	63.147841
1837.455866	14549.536731	63.152846
1836.883094	14480.155293	63.157850
1836.345853	14398.766116	63.162855
1835.586150	14354.205455	63.167860
1835.119173	14275.596823	63.172865
1834.300685	14215.251712	63.177870
1833.506305	14135.864327	63.182874
1832.668898	14069.869941	63.187879
1832.119485	14011.943515	63.192884
1831.792946	13932.791308	63.197889
1830.883222	13881.510789	63.202894
1830.176375	13806.846508	63.207898
1829.674273	13736.548633	63.212903
1828.750893	13675.397585	63.217908
1828.189867	13606.380779	63.222913
1827.623608	13545.297744	63.227918
1826.684383	13472.599810	63.232922
1826.198086	13408.336205	63.237927
1825.487436	13346.338841	63.242932
1825.075084	13270.533148	63.247937
1824.061439	13214.502725	63.252942
1823.457596	13149.851261	63.257946
1823.005217	13077.905328	63.262951
1822.042924	13020.860082	63.267956
1821.877165	12959.031979	63.272961
1821.059312	12877.879719	63.277966
1820.383521	12820.529009	63.282970
1819.537792	12752.918824	63.287975
1818.793478	12680.197464	63.292980
1818.234650	12620.400610	63.297985
1817.766902	12563.032334	63.302990
1817.085318	12491.394589	63.307994
1816.407790	12423.601624	63.312999
1815.981254	12372.453055	63.318004
1815.131411	12295.517847	63.323009
1814.323365	12235.769180	63.328014
1813.914690	12149.456069	63.333018
1813.013263	12098.898933	63.338023
1812.355155	12033.543609	63.343028
1811.921160	11961.265169	63.348033
1811.012654	11903.980615	63.353038
1810.541704	11830.287276	63.358042
1810.008451	11762.374922	63.363047
1809.000274	11705.725801	63.368052
1808.570640	11628.731582	63.373057
1807.845173	11576.228565	63.378062
1807.229866	11500.980962	63.383066
1806.464322	11440.564458	63.388071
1805.445065	11366.421888	63.393076
1805.261761	11305.003847	63.398081
1804.101499	11252.936341	63.403086
1803.497194	11184.761285	63.408090
1803.316237	11123.536535	63.413095
1802.373830	11067.159482	63.418100
1801.915999	10986.119549	63.423105
1801.166122	10930.720857	63.428110
1800.642926	10857.616557	63.433114
1799.909634	10790.827252	63.438119
1798.969361	10738.743157	63.443124
1798.582769	10657.741801	63.448129
1797.876866	10611.874535	63.453134
1797.298886	10541.922050	63.458138
1796.944715	10484.815817	63.463143
1795.976010	10408.449953	63.468148
1795.591029	10333.758422	63.473153
1794.745517	10277.921646	63.478158
1794.106769	10199.600316	63.483162
1793.445897	10140.453568	63.488167
1792.712711	10081.055002	63.493172
1791.939842	10008.158183	63.498177
1790.990631	9929.768613	63.503182
1790.658715	9882.024718	63.508186
1790.115503	9804.372564	63.513191
1789.232919	9744.233718	63.518196
1788.351803	9676.887382	63.523201
1787.793925	9625.215076	63.528206
1787.236362	9556.847037	63.533210
1786.742120	9497.991158	63.538215
1785.744461	9440.029293	63.543220
1785.389704	9370.757274	63.548225
1784.558629	9302.507990	63.553230
1784.103343	9242.672141	63.558234
1783.638828	9165.000925	63.563239
1782.756720	9117.311326	63.568244
1782.193267	9036.685625	63.573249
1781.467635	8985.905680	63.578254
1780.574681	8911.619031	63.583258
1779.939332	8843.231087	63.588263
1778.993440	8783.033562	63.593268
1778.700331	8732.693869	63.598273
1778.012040	8664.050458	63.603278
1777.217702	8604.474544	63.608282
1776.618089	8538.119364	63.613287
1776.017986	8479.999458	63.618292
1775.587037	8418.899942	63.623297
1774.818836	8350.942036	63.628302
1774.501018	8287.518657	63.633306
1773.437321	8216.205263	63.638311
1772.578154	8165.679277	63.643316
1772.227080	8088.392050	63.648321
1771.836487	8029.805138	63.653326
1770.876581	7962.854535	63.658330
1770.510540	7895.773629	63.663335
1769.699747	7832.501470	63.668340
1768.821532	7761.586007	63.673345
1767.897683	7700.555474	63.678350
1767.341671	7626.850835	63.683354
1766.588687	7571.471339	63.688359
1765.660898	7517.057794	63.693364
1765.359506	7452.489885	63.698369
1764.673175	7389.096496	63.703374
1763.902262	7330.961247	63.708378
1763.703868	7265.685156	63.713383
1762.982410	7204.369706	63.718388
1762.371177	7135.762095	63.723393
1761.453128	7071.001891	63.728398
1760.698346	7011.537673	63.733402
1760.359888	6946.380675	63.738407
1759.529299	6888.244404	63.743412
1759.067832	6819.197162	63.748417
1758.131220	6762.636589	63.753422
1757.465508	6691.767014	63.758426
1756.568160	6629.382224	63.763431
1755.853150	6581.440697	63.768436
1755.658515	6511.114824	63.773441
1754.939530	6466.707475	63.778446
1754.557162	6395.742247	63.783450
1753.913934	6341.986707	63.788455
1752.836433	6275.624008	63.793460
1752.570283	6204.496092	63.798465
1751.560444	6134.818931	63.803470
1751.094485	6067.008018	63.808474
1750.316395	6011.760582	63.813479
1749.646879	5934.240867	63.818484
1749.046290	5883.287559	63.823489
1747.975087	5822.415925	63.828494
1747.433996	5764.290532	63.833498
1746.841978	5695.376521	63.838503
1745.765001	5647.646949	63.843508
1744.966023	5587.917012	63.848513
1744.665451	5531.544080	63.853518
1744.114660	5480.028160	63.858522
1743.754528	5411.600810	63.863527
1743.008546	5356.425653	63.868532
1742.406644	5293.162678	63.873537
1741.717427	5225.596150	63.878542
1740.841782	5172.284825	63.883546
1740.318576	5112.057107	63.888551
1739.579788	5051.001765	63.893556
1739.063791	4988.591711	63.898561
1738.468560	4925.852977	63.903566
1737.689742	4868.081994	63.908570
1736.866271	4807.489905	63.913575
1735.902513	4757.371911	63.918580
1735.658538	4678.900697	63.923585
1734.663100	4636.254305	63.928590
1734.143172	4574.841214	63.933594
1733.501378	4525.929315	63.938599
1732.941562	4470.695563	63.943604
1732.028733	4411.441193	63.948609
1731.573073	4352.463852	63.953614
1730.914842	4288.556337	63.958618
1730.126373	4226.764597	63.963623
1729.450095	4185.848937	63.968628
1729.066856	4117.572426	63.973633
1728.445668	4061.176365	63.978638
1727.546468	4008.763434	63.983642
1727.189020	3945.077793	63.988647
1726.443336	3886.476478	63.993652
1725.777393	3831.177590	63.998657
1725.198287	3767.177747	64.003662
1724.197061	3707.225705	64.008666
1723.712943	3646.504048	64.013671
1722.916877	3598.160770	64.018676
1722.460228	3525.763633	64.023681
1721.640152	3482.627422	64.028686
1720.940245	3424.566438	64.033690
1720.536896	3358.735987	64.038695
1719.593958	3305.942914	64.043700
1718.757598	3250.087307	64.048705
1718.141524	3194.127522	64.053710
1717.522270	3132.387641	64.058714
1717.406960	3082.919785	64.063719
1716.265180	3022.732613	64.068724
1715.810926	2964.830015	64.073729
1714.976931	2907.297897	64.078734
1714.084928	2858.463625	64.083738
1713.506151	2799.035733	64.088743
1712.863019	2746.069299	64.093748
1712.249640	2692.304973	64.098753
1711.163046	2658.952288	64.103758
1710.760242	2591.719072	64.108762
1710.141757	2543.213061	64.113767
1709.345856	2490.379071	64.118772
1709.239486	2429.874521	64.123777
1708.686958	2386.210105	64.128782
1707.852547	2336.861351	64.133786
1707.068628	2265.894594	64.138791
1706.250743	2215.842555	64.143796
1705.840187	2158.510306	64.148801
1705.109422	2104.929235	64.153806
1704.191975	2051.097275	64.158810
1703.786122	1989.767563	64.163815
1702.880802	1943.764772	64.168820
1702.302936	1881.787016	64.173825
1701.691064	1833.298083	64.178830
1700.784593	1787.191088	64.183834
1700.245177	1729.326621	64.188839
1699.512594	1673.560703	64.193844
1699.055172	1627.408121	64.198849
1698.236222	1582.786155	64.203854
1697.371207	1528.152922	64.208858
1697.103015	1469.665231	64.213863
1695.787127	1435.347148	64.218868
1695.304722	1382.796203	64.223873
1695.043924	1330.572983	64.228878
1694.203627	1281.543371	64.233882
1693.662125	1228.753187	64.238887
1692.644299	1186.834842	64.243892
1692.184574	1136.727254	64.248897
1691.592569	1090.633235	64.253902
1690.880739	1039.661570	64.258906
1690.447924	974.977290	64.263911
1689.682584	943.361972	64.268916
1688.586252	886.383370	64.273921
1688.178692	843.304564	64.278926
1687.309519	804.423200	64.283930
1686.958006	748.758790	64.288935
1685.943106	709.967064	64.293940
1685.474044	657.207662	64.298945
1684.608834	626.066241	64.303950
1684.126063	580.369672	64.308954
1683.478890	530.006144	64.313959
1682.291604	496.813993	64.318964
1681.621475	458.800840	64.323969
1681.061044	411.700980	64.328974
1679.975160	387.007249	64.333978
1679.458797	331.754625	64.338983
1678.797874	319.093835	64.343988
1678.089993	271.595217	64.348993
1677.493943	245.442472	64.353998
1676.805211	216.948478	64.359002
1676.145500	175.660588	64.364007
1675.410404	156.325316	64.369012
1674.890411	127.175479	64.374017
1674.156214	83.420676	64.379022
1672.821113	66.707149	64.384026
1672.226826	46.646328	64.389031
1671.238805	32.134350	64.394036
1669.953828	36.148463	64.399041
1668.033007	57.216006	64.404046
1666.663947	65.234797	64.409050
1666.765222	61.744677	64.414055
1666.417599	66.354226	64.419060
1666.036790	65.140562	64.424065
1665.835235	71.620852	64.429070
1665.538726	72.352395	64.434074
1665.055801	64.397629	64.439079
1663.789384	73.415690	64.444084
1662.796772	75.300192	64.449089
1661.992098	68.606073	64.454094
1661.537051	75.159750	64.459098
1661.492383	70.235690	64.464103
1660.458723	68.881305	64.469108
1659.534957	69.348212	64.474113
1659.045017	77.041276	64.479118
1658.716522	78.880205	64.484122
1658.513976	69.422197	64.489127
1657.586863	82.459684	64.494132
1656.598852	68.086450	64.499137
1655.848117	78.213210	64.504142
1655.060446	73.867657	64.509146
1655.024293	74.124174	64.514151
1654.253527	70.353109	64.519156
1653.651035	72.194564	64.524161
1652.783766	77.512726	64.529166
1651.814064	79.084506	64.534170
1651.356171	80.649099	64.539175
1650.563073	83.941687	64.544180
1650.484411	73.804824	64.549185
1650.263097	78.465277	64.554190
1648.877149	81.784236	64.559194
1648.404365	74.135368	64.564199
1647.780749	83.086018	64.569204
1647.256299	79.547062	64.574209
1646.717878	82.843348	64.579214
1645.416029	75.977476	64.584218
1644.823708	78.047555	64.589223
1644.117248	80.399122	64.594228
1643.049945	81.590591	64.599233
1642.702692	77.000031	64.604238
1642.151993	78.353861	64.609242
1642.071127	75.927167	64.614247
1641.498608	74.195175	64.619252
1640.425830	76.231194	64.624257
1639.541748	78.473783	64.629262
1639.283868	78.101619	64.634266
1639.208234	73.983580	64.639271
1637.387421	86.879197	64.644276
1636.696827	84.568291	64.649281
1636.709412	68.328246	64.654286
1635.943797	81.835248	64.659290
1635.366747	73.915939	64.664295
1634.757779	85.065718	64.669300
1634.095213	73.342144	64.674305
1633.477943	83.367282	64.679310
1632.411319	77.418117	64.684314
1632.088940	85.040412	64.689319
1631.093497	84.690806	64.694324
1630.343409	82.195386	64.699329
1629.802294	86.553406	64.704334
1628.986226	79.331243	64.709338
1628.382985	79.351420	64.714343
1627.523052	72.539934	64.719348
1626.978351	77.983478	64.724353
1626.698344	76.269674	64.729358
1625.740571	85.588811	64.734362
1625.681905	73.846570	64.739367
1624.649586	76.461224	64.744372
1623.969033	80.844550	64.749377
1623.503705	79.475583	64.754382
1622.347060	85.388517	64.759386
1622.677016	76.893022	64.764391
1621.296745	80.118051	64.769396
1620.407743	73.789009	64.774401
1620.078479	85.652876	64.779406
1620.082892	80.547550	64.784410
1618.985478	72.166863	64.789415
1617.833947	76.618707	64.794420
1616.918684	75.213990	64.799425
1616.951161	85.545917	64.804430
1616.391683	86.640947	64.809434
1615.875330	76.617779	64.814439
1614.682494	85.111661	64.819444
1613.896795	74.383802	64.824449
1613.358733	78.572602	64.829454
1612.558106	73.648797	64.834458
1612.481148	84.644668	64.839463
1611.637924	83.198545	64.844468
1610.759598	84.465660	64.849473
1610.235561	77.392653	64.854478
1609.189939	85.998767	64.859482
1609.073479	77.083758	64.864487
1608.373279	89.536424	64.869492
1607.771206	77.948327	64.874497
1607.140832	81.204035	64.879502
1606.540551	88.719096	64.884506
1606.194540	77.397827	64.889511
1605.274595	81.328753	64.894516
1604.775327	79.132541	64.899521
1603.892826	84.919923	64.904526
1602.156122	85.713131	64.909530
1602.535485	79.559473	64.914535
1602.159622	83.572694	64.919540
1601.058682	71.398382	64.924545
1600.309354	76.715167	64.929550
1599.355392	79.279534	64.934554
1598.842935	80.895382	64.939559
1598.031499	79.387442	64.944564
1597.850997	75.921587	64.949569
1597.141509	76.357626	64.954574
1596.209365	76.428489	64.959578
1595.791437	66.935329	64.964583
1594.859692	87.601376	64.969588
1594.483333	87.412046	64.974593
1594.209933	73.292737	64.979598
1593.258807	82.836331	64.984602
1592.774023	83.058471	64.989607
1592.243267	80.657527	64.994612
1591.596251	84.931453	64.999617
1590.637492	71.173354	65.004622
1589.383348	85.644244	65.009626
1589.087136	73.080302	65.014631
1588.333470	79.457504	65.019636
1587.826519	79.645320	65.024641
1587.304267	82.456494	65.029646
1586.325581	82.113705	65.034650
1585.971627	77.295559	65.039655
1585.348262	80.666854	65.044660
1584.834863	75.063479	65.049665
1584.183284	73.216328	65.054670
1583.606371	70.393785	65.059674
1583.218506	73.352342	65.064679
1581.776239	72.021910	65.069684
1580.769919	75.599133	65.074689
1580.644840	69.188155	65.079694
1580.029642	85.143959	65.084698
1579.452138	76.388943	65.089703
1578.329425	78.156951	65.094708
1577.759653	68.911850	65.099713
1577.344826	79.101948	65.104718
1576.725087	82.644558	65.109722
1576.419499	67.505342	65.114727
1575.550203	76.602268	65.119732
1574.991655	75.912027	65.124737
1574.706126	69.638509	65.129742
1573.173446	77.087251	65.134746
1572.368141	64.019154	65.139751
1571.714255	80.082026	65.144756
1571.434001	70.809848	65.149761
1570.882621	77.973360	65.154766
1569.894535	75.222459	65.159770
1569.839627	72.154549	65.164775
1568.983904	79.437383	65.169780
1568.309652	72.804579	65.174785
1568.119685	65.046143	65.179790
1566.853050	78.804651	65.184794
1566.049669	68.483331	65.189799
1564.877580	74.826095	65.194804
1564.153415	74.077016	65.199809
1564.399543	67.799449	65.204814
1563.730256	74.234211	65.209818
1562.505859	69.530726	65.214823
1561.882859	67.521344	65.219828
1561.452261	71.150597	65.224833
1561.224607	63.819203	65.229838
1560.589598	76.900178	65.234842
1560.259191	56.436339	65.239847
1559.275217	73.108324	65.244852
1558.279868	60.926728	65.249857
1557.394164	68.264787	65.254862
1556.653879	80.159265	65.259866
1556.624100	68.926541	65.264871
1555.810649	74.573649	65.269876
1555.173655	81.353372	65.274881
1555.076822	70.803091	65.279886
1553.598815	71.105788	65.284890
1552.967714	64.611217	65.289895
1552.134304	73.122120	65.294900
1551.648130	61.957191	65.299905
1551.214784	62.322555	65.304910
1550.334682	71.205156	65.309914
1550.083610	67.614902	65.314919
1548.570532	72.548426	65.319924
1547.668586	72.817938	65.324929
1547.960790	70.188466	65.329934
1547.147853	73.263457	65.334938
1546.182456	75.003326	65.339943
1545.586706	71.057829	65.344948
1544.919367	71.559724	65.349953
1544.670276	61.246537	65.354958
1543.927626	70.594581	65.359962
1543.533174	62.518557	65.364967
1542.854414	69.128292	65.369972
1541.659248	80.204067	65.374977
1540.830791	66.360638	65.379982
1540.066638	69.702271	65.384986
1539.828782	69.162932	65.389991
1539.012281	82.066170	65.394996
1538.420976	69.561751	65.400001
1538.005047	73.496186	65.405006
1537.370910	84.785594	65.410010
1537.231102	70.854811	65.415015
1535.663155	76.290654	65.420020
1534.921614	67.213213	65.425025
1534.635632	71.713631	65.430030
1533.896096	76.423319	65.435034
1533.616086	70.633061	65.440039
1532.636200	74.535686	65.445044
1531.821809	73.094471	65.450049
1530.777610	67.332607	65.455054
1530.003238	75.028303	65.460058
1530.256334	74.921887	65.465063
1529.091916	71.333268	65.470068
1528.668684	83.257797	65.475073
1528.469051	72.790087	65.480078
1527.768678	78.622664	65.485082
1527.110020	64.853187	65.490087
1525.839511	69.459591	65.495092
1525.356902	85.417984	65.500097
1524.520412	81.400357	65.505102
1523.817208	79.719123	65.510106
1523.699145	72.720403	65.515111
1522.900646	78.417185	65.520116
1521.727650	72.347781	65.525121
1521.022510	66.770165	65.530126
1519.903954	72.278107	65.535130
1519.696103	66.807549	65.540135
1519.517295	80.232356	65.545140
1518.642455	75.209990	65.550145
1518.694063	64.610899	65.555150
1517.945277	83.459593	65.560154
1517.351528	70.433592	65.565159
1515.809596	81.001503	65.570164
1515.188241	68.090280	65.575169
1514.656925	68.846537	65.580174
1514.239701	73.601204	65.585178
1513.646776	73.673385	65.590183
1513.041517	68.772188	65.595188
1511.918703	83.318426	65.600193
1511.334497	70.817618	65.605198
1510.744438	79.643103	65.610202
1510.274263	73.100891	65.615207
1509.882650	82.038346	65.620212
1509.338714	68.318451	65.625217
1508.041598	73.622959	65.630222
1507.012591	71.263369	65.635226
1506.479938	72.846172	65.640231
1505.965813	72.513167	65.645236
1505.453632	68.614326	65.650241
1505.220743	73.713442	65.655246
1504.535023	73.084428	65.660250
1504.014362	73.324902	65.665255
1502.789439	73.934341	65.670260
1502.200247	71.536398	65.675265
1501.424693	71.293825	65.680270
1500.790337	70.084210	65.685274
1500.501236	66.337579	65.690279
1499.742671	72.748693	65.695284
1498.950486	75.930788	65.700289
1497.992911	70.051093	65.705294
1497.313173	80.961392	65.710298
1496.823161	69.049602	65.715303
1496.148197	73.357947	65.720308
1495.721154	61.937632	65.725313
1495.592148	67.198435	65.730318
1494.438904	76.375198	65.735322
1493.393895	64.786581	65.740327
1493.104219	75.631734	65.745332
1492.353123	69.539453	65.750337
1491.851933	67.119643	65.755342
1491.112068	74.532317	65.760346
1490.657053	65.045080	65.765351
1489.470597	69.187129	65.770356
1488.918981	67.223193	65.775361
1488.515282	62.807218	65.780366
1487.381898	72.488609	65.785370
1487.183422	63.471542	65.790375
1486.967881	60.386589	65.795380
1485.628997	70.135331	65.800385
1485.017805	57.596256	65.805390
1484.073755	67.479369	65.810394
1483.584782	67.762120	65.815399
1483.201874	69.224934	65.820404
1482.817715	68.847624	65.825409
1482.200071	59.252196	65.830414
1480.739916	67.276086	65.835418
1480.239040	70.668934	65.840423
1479.961816	67.046576	65.845428
1479.384823	69.967392	65.850433
1478.977273	63.333236	65.855438
1477.632667	72.526223	65.860442
1476.989643	72.158516	65.865447
1476.311363	76.028996	65.870452
1475.627993	75.787551	65.875457
1475.411616	80.223296	65.880462
1474.615545	77.046098	65.885466
1474.270431	67.975064	65.890471
1472.649598	76.768827	65.895476
1471.811635	75.454382	65.900481
1471.679891	74.311552	65.905486
1471.613264	78.475913	65.910490
1470.742917	63.358679	65.915495
1470.178709	68.133555	65.920500
1469.767087	67.708572	65.925505
1468.689150	70.180721	65.930510
1467.846526	80.943446	65.935514
1467.081407	68.288481	65.940519
1466.568555	72.466988	65.945524
1466.012723	66.443033	65.950529
1465.793237	73.743045	65.955534
1464.383246	72.626750	65.960538
1463.929959	68.122465	65.965543
1463.183448	70.882566	65.970548
1462.658008	66.765068	65.975553
1462.388249	64.333715	65.980558
1461.562861	73.316453	65.985562
1460.223644	69.613723	65.990567
1459.703942	69.268998	65.995572
1459.023951	65.896739	66.000577
1458.656730	64.855991	66.005582
1457.888727	75.944326	66.010586
1458.022863	65.398356	66.015591
1457.235901	68.488166	66.020596
1455.976418	63.558502	66.025601
1455.668174	62.809583	66.030606
1454.734794	64.913405	66.035610
1454.211125	68.119066	66.040615
1453.170361	66.735934	66.045620
1452.120428	68.673777	66.050625
1451.570717	62.175765	66.055630
1451.219907	71.158771	66.060634
1450.884715	62.081438	66.065639
1450.350804	65.887975	66.070644
1450.198497	71.655535	66.075649
1449.490918	61.598166	66.080654
1448.303749	62.985383	66.085658
1447.603274	54.630017	66.090663
1447.255813	59.174901	66.095668
1445.861983	64.974203	66.100673
1445.689347	64.825056	66.105678
1444.740331	72.666799	66.110682
1444.545030	65.779718	66.115687
1443.757785	70.656282	66.120692
1442.149736	61.852223	66.125697
1441.973502	62.183046	66.130702
1441.176038	68.871593	66.135706
1440.731852	66.251921	66.140711
1440.244390	66.961798	66.145716
1439.929954	64.444507	66.150721
1439.341691	64.146954	66.155726
1438.252101	72.175047	66.160730
1437.318144	67.234652	66.165735
1437.012281	66.674593	66.170740
1436.242696	75.356730	66.175745
1436.062086	69.257374	66.180750
1434.779665	63.889816	66.185754
1433.854810	60.753606	66.190759
1432.930849	69.963330	66.195764
1432.401661	72.939636	66.200769
1432.571608	63.493432	66.205774
1432.083285	65.550177	66.210778
1431.660046	70.447735	66.215783
1430.593689	74.482411	66.220788
1429.762110	73.207967	66.225793
1429.408859	67.298481	66.230798
1428.226420	75.464340	66.235802
1427.601593	68.404255	66.240807
1426.589450	74.985003	66.245812
1425.972265	71.916587	66.250817
1425.277563	66.184378	66.255822
1424.677592	72.516684	66.260826
1424.647382	78.170220	66.265831
1424.520240	71.366924	66.270836
1423.050594	75.374240	66.275841
1422.142606	61.732750	66.280846
1421.532424	62.397481	66.285850
1421.168775	64.182096	66.290855
1420.644347	61.879538	66.295860
1420.026534	68.514302	66.300865
1419.023771	63.455542	66.305870
1418.245622	69.078149	66.310874
1417.777859	62.461464	66.315879
1417.376257	66.379441	66.320884
1416.747940	74.637000	66.325889
1415.748025	62.184965	66.330894
1414.697788	79.316954	66.335898
1414.495966	63.082649	66.340903
1414.161196	61.588892	66.345908
1413.503300	74.233543	66.350913
1412.901848	58.614705	66.355918
1411.333461	67.415929	66.360922
1410.898522	73.330917	66.365927
1410.498773	67.001468	66.370932
1409.711008	72.330713	66.375937
1409.709039	66.314931	66.380942
1408.421065	74.079676	66.385946
1407.842484	61.800372	66.390951
1407.198047	65.920954	66.395956
1406.607692	67.132899	66.400961
1406.222868	64.344524	66.405966
1404.830991	65.928305	66.410970
1404.025879	59.628602	66.415975
1403.492381	61.208403	66.420980
1402.919176	58.861563	66.425985
1402.603660	62.461502	66.430990
1402.078056	58.933833	66.435994
1401.768507	73.409165	66.440999
1401.124526	64.434543	66.446004
1399.845645	66.629574	66.451009
1399.383137	55.255931	66.456014
1398.854460	71.336750	66.461018
1398.360295	67.487112	66.466023
1397.303647	62.168843	66.471028
1396.312279	64.978922	66.476033
1396.159926	65.924124	66.481038
1395.252230	63.926925	66.486042
1394.892901	62.380304	66.491047
1394.150822	66.440715	66.496052
1392.985632	75.050127	66.501057
1392.776364	64.546134	66.506062
1391.985372	72.424274	66.511066
1391.778597	60.634660	66.516071
1390.810026	63.805396	66.521076
1389.776702	76.744699	66.526081
1389.291384	65.759457	66.531086
1388.678774	70.316535	66.536090
1388.066704	57.260390	66.541095
1387.982023	67.681863	66.546100
1386.927499	61.751399	66.551105
1386.449685	67.411426	66.556110
1385.493379	63.876531	66.561114
1384.874531	67.953626	66.566119
1383.928266	67.265136	66.571124
1383.111803	69.012927	66.576129
1382.598643	66.028913	66.581134
1381.865750	73.689661	66.586138
1381.394316	69.708678	66.591143
1381.082103	76.465186	66.596148
1380.413319	72.862507	66.601153
1379.762067	57.633225	66.606158
1378.801732	67.736575	66.611162
1378.221824	66.986696	66.616167
1377.716437	62.829762	66.621172
1376.658912	76.495166	66.626177
1375.952829	57.890430	66.631182
1375.382738	74.014107	66.636186
1375.228071	61.700543	66.641191
1374.835279	70.493105	66.646196
1373.246347	76.219381	66.651201
1372.680147	68.421435	66.656206
1371.991118	73.156247	66.661210
1371.684102	69.581218	66.666215
1371.337021	65.119996	66.671220
1370.115420	69.277144	66.676225
1369.634644	58.980326	66.681230
1368.724628	67.599640	66.686234
1368.327387	65.119178	66.691239
1367.701320	75.893226	66.696244
1366.912169	71.861827	66.701249
1366.112988	68.103263	66.706254
1365.044744	63.302520	66.711258
1364.677154	58.835100	66.716263
1364.487565	63.993567	66.721268
1363.971334	68.254628	66.726273
1363.756266	61.629325	66.731278
1362.491672	63.218125	66.736282
1361.737954	60.286551	66.741287
1361.263905	61.614058	66.746292
1360.086943	60.474969	66.751297
1359.112817	66.792646	66.756302
1358.574255	69.459792	66.761306
1358.121765	61.776243	66.766311
1357.955852	60.935323	66.771316
1357.461707	68.469808	66.776321
1357.345273	62.331878	66.781326
1355.785362	66.684741	66.786330
1355.510638	58.402072	66.791335
1354.471764	63.340736	66.796340
1352.819613	71.893533	66.801345
1352.406261	55.946772	66.806350
1352.719592	61.755420	66.811354
1351.923292	61.841047	66.816359
1351.103073	64.582932	66.821364
1350.680201	72.397828	66.826369
1350.006484	60.316599	66.831374
1348.667371	67.387746	66.836378
1348.181165	66.673440	66.841383
1347.987866	61.935461	66.846388
1347.537931	66.607034	66.851393
1346.703988	65.922780	66.856398
1345.169615	66.590950	66.861402
1344.735300	66.891846	66.866407
1344.570420	68.239591	66.871412
1343.780623	67.871597	66.876417
1343.643119	66.307065	66.881422
1342.729130	74.979062	66.886426
1341.992833	75.670169	66.891431
1341.352343	66.176190	66.896436
1340.594184	73.255908	66.901441
1340.351442	66.942515	66.906446
1338.797887	68.168831	66.911450
1338.103078	65.117512	66.916455
1337.807651	75.194018	66.921460
1337.139845	72.909541	66.926465
1337.062153	55.990050	66.931470
1336.049807	65.723208	66.936474
1335.201751	64.755770	66.941479
1334.714805	68.966448	66.946484
1334.039086	66.254296	66.951489
1333.722266	63.354198	66.956494
1332.530682	67.303160	66.961498
1331.963263	59.735663	66.966503
1331.613461	70.120434	66.971508
1330.958341	67.316698	66.976513
1330.219040	62.700220	66.981518
1329.134572	57.394293	66.986522
1328.253046	68.642620	66.991527
1327.964304	71.730528	66.996532
1327.366612	69.633604	67.001537
1326.693526	59.875156	67.006542
1325.694129	68.757852	67.011546
1325.140203	64.422566	67.016551
1324.988499	69.475663	67.021556
1324.146246	61.682200	67.026561
1323.820467	68.037160	67.031566
1322.707968	56.768456	67.036570
1321.944253	59.979186	67.041575
1321.501206	54.959219	67.046580
1320.849772	62.812028	67.051585
1320.218763	63.976838	67.056590
1318.908496	68.192259	67.061594
1318.366789	56.577340	67.066599
1318.030759	56.096209	67.071604
1317.588772	66.281167	67.076609
1317.422151	56.011691	67.081614
1315.850717	64.187392	67.086618
1315.387158	61.670175	67.091623
1314.886779	64.570955	67.096628
1314.182827	75.551359	67.101633
1314.025478	56.837334	67.106638
1312.644495	60.701297	67.111642
1311.715922	67.521106	67.116647
1311.224369	59.555196	67.121652
1310.677963	65.677150	67.126657
1310.285607	64.127908	67.131662
1309.725669	73.346022	67.136666
1309.017864	64.706435	67.141671
1308.474761	57.753249	67.146676
1307.825116	67.960186	67.151681
1306.800684	63.363819	67.156686
1305.893135	60.149214	67.161690
1305.431398	58.652006	67.166695
1305.257002	57.698897	67.171700
1304.478958	69.705066	67.176705
1303.512038	65.683033	67.181710
1302.491630	69.961187	67.186714
1301.735779	68.882905	67.191719
1301.672366	59.588930	67.196724
1300.892651	64.207285	67.201729
1300.671200	66.158543	67.206734
1299.452994	69.824745	67.211738
1298.742566	65.861281	67.216743
1298.357076	65.151472	67.221748
1297.917882	68.088260	67.226753
1297.463707	65.121696	67.231758
1295.970994	71.878242	67.236762
1295.262355	65.230500	67.241767
1295.065162	69.612735	67.246772
1294.363883	66.122484	67.251777
1294.088633	63.173204	67.256782
1292.710254	63.387669	67.261786
1292.079214	65.411936	67.266791
1291.705772	67.616020	67.271796
1290.894792	77.407068	67.276801
1291.087348	70.762693	67.281806
1289.941673	70.982737	67.286810
1289.191403	64.038840	67.291815
1288.500894	64.170743	67.296820
1287.401226	71.812556	67.301825
1286.538855	71.839321	67.306830
1285.890874	70.972553	67.311834
1285.407980	63.082542	67.316839
1285.191638	57.950842	67.321844
1284.506302	63.331638	67.326849
1284.672702	65.839397	67.331854
1283.556185	70.454540	67.336858
1282.605200	65.512188	67.341863
1282.026449	70.447105	67.346868
1280.792605	78.157566	67.351873
1280.478066	67.009584	67.356878
1279.499411	70.450047	67.361882
1279.076736	72.693501	67.366887
1279.188789	59.924383	67.371892
1277.940188	70.136676	67.376897
1277.381900	63.368839	67.381902
1276.476277	72.446378	67.386906
1275.995472	70.766125	67.391911
1275.017239	58.693923	67.396916
1273.748405	71.019412	67.401921
1273.441580	64.993766	67.406926
1272.887883	66.840158	67.411930
1272.567179	64.440585	67.416935
1272.068773	62.715823	67.421940
1271.610380	68.754402	67.426945
1271.206573	59.852027	67.431950
1270.192075	61.744881	67.436954
1269.257507	58.176616	67.441959
1268.627381	66.434481	67.446964
1267.674824	70.242962	67.451969
1267.052870	56.183910	67.456974
1266.591771	64.481130	67.461978
1266.278219	69.295032	67.466983
1265.329593	64.063728	67.471988
1264.004053	65.460414	67.476993
1263.852442	55.549686	67.481998
1263.301489	68.838093	67.487002
1262.776783	62.252580	67.492007
1262.679196	55.655924	67.497012
1261.760255	65.784261	67.502017
1261.142820	61.080620	67.507022
1259.782719	68.279724	67.512026
1258.883378	61.793208	67.517031
1258.529115	58.692494	67.522036
1257.756791	66.769544	67.527041
1257.813295	61.682770	67.532046
1257.144128	62.656541	67.537050
1255.965048	62.937106	67.542055
1255.310506	59.792677	67.547060
1254.327423	67.097413	67.552065
1254.411305	63.417668	67.557070
1253.513594	60.108479	67.562074
1251.949413	58.371845	67.567079
1251.486033	63.983860	67.572084
1251.040632	67.221264	67.577089
1250.817350	64.604351	67.582094
1250.268025	70.529659	67.587098
1249.879859	67.237215	67.592103
1249.008600	64.918884	67.597108
1248.054336	63.433774	67.602113
1247.696426	61.549481	67.607118
1246.891447	63.251331	67.612122
1245.998799	68.504252	67.617127
1245.347545	61.692861	67.622132
1244.596586	70.450921	67.627137
1244.361505	57.757510	67.632142
1243.918994	61.622086	67.637146
1242.770676	63.943087	67.642151
1242.156291	60.959434	67.647156
1241.164207	69.610756	67.652161
1241.137943	64.366831	67.657166
1240.296616	70.852665	67.662170
1239.259885	63.883375	67.667175
1238.650499	66.402531	67.672180
1237.914774	71.400266	67.677185
1237.758240	62.778699	67.682190
1237.033669	62.692105	67.687194
1235.961420	61.096451	67.692199
1235.321197	59.394249	67.697204
1235.022113	67.250968	67.702209
1234.903150	61.996555	67.707214
1233.856646	59.330781	67.712218
1232.773596	51.138835	67.717223
1232.108661	57.069909	67.722228
1231.568254	63.265036	67.727233
1231.190238	58.968035	67.732238
1230.364302	58.383472	67.737242
1229.670485	57.128191	67.742247
1229.151847	52.727397	67.747252
1228.508255	64.258029	67.752257
1227.833971	65.117503	67.757262
1226.879416	66.155589	67.762266
1226.443617	64.906585	67.767271
1225.845973	62.147357	67.772276
1224.923302	68.344929	67.777281
1223.848091	60.810907	67.782286
1223.218855	64.919647	67.787290
1222.636898	61.408868	67.792295
1222.428171	61.046278	67.797300
1222.018415	70.697837	67.802305
1221.445113	59.674604	67.807310
1220.877808	60.075517	67.812314
1219.954370	62.513731	67.817319
1219.055817	68.270651	67.822324
1217.906387	69.476927	67.827329
1217.411693	60.557479	67.832334
1217.061973	63.163079	67.837338
1216.490206	60.409200	67.842343
1216.499404	51.778634	67.847348
1214.976034	64.646092	67.852353
1214.395920	54.044998	67.857358
1213.666478	66.494462	67.862362
1213.335077	56.893033	67.867367
1212.550883	55.984868	67.872372
1211.398767	55.127329	67.877377
1211.044346	52.447699	67.882382
1210.309999	46.255095	67.887386
1209.728326	52.338511	67.892391
1209.758021	46.830228	67.897396
1208.374387	53.151569	67.902401
1208.105556	53.162817	67.907406
1207.246394	53.414605	67.912410
1206.181328	59.298931	67.917415
1205.464774	49.799762	67.922420
1204.687085	55.881237	67.927425
1204.303772	53.505825	67.932430
1204.191449	57.494514	67.937434
1203.568859	60.365862	67.942439
1202.925002	58.180120	67.947444
1201.924471	51.463719	67.952449
1201.461042	50.562893	67.957454
1200.542381	56.520131	67.962458
1199.165700	59.900917	67.967463
1199.011114	52.744051	67.972468
1198.442602	51.383695	67.977473
1197.955959	39.070942	67.982478
1197.632997	43.458981	67.987482
1196.958141	49.137746	67.992487
1195.744467	44.812806	67.997492
1195.209927	44.192951	68.002497
1194.775671	49.453405	68.007502
1194.223842	53.288062	68.012506
1193.363807	56.854767	68.017511
1192.793543	49.484890	68.022516
1192.123904	53.508595	68.027521
1191.492191	45.429399	68.032526
1190.355185	53.625956	68.037530
1189.398599	51.915734	68.042535
1189.162932	53.303129	68.047540
1188.640659	57.744948	68.052545
1188.357706	55.601161	68.057550
1187.767395	51.298510	68.062554
1186.708913	52.402024	68.067559
1186.343556	50.233496	68.072564
1185.571145	52.827475	68.077569
1184.536017	49.015041	68.082574
1183.525860	47.141453	68.087578
1183.133126	47.946698	68.092583
1182.809402	48.570656	68.097588
1182.298126	53.781860	68.102593
1181.912056	46.980362	68.107598
1180.947554	54.865634	68.112602
1179.850313	54.508742	68.117607
1179.834585	46.987596	68.122612
1178.618170	55.116363	68.127617
1177.772642	59.835102	68.132622
1177.011932	57.817763	68.137626
1176.778836	62.175747	68.142631
1176.827645	45.092681	68.147636
1175.797882	56.236874	68.152641
1174.782225	50.366567	68.157646
1174.136632	48.528041	68.162650
1173.600966	56.573772	68.167655
1172.972722	53.926660	68.172660
1171.820144	51.776105	68.177665
1171.608908	56.572160	68.182670
1170.627230	53.314205	68.187674
1170.208530	61.833348	68.192679
1169.899059	59.543969	68.197684
1168.496534	62.777492	68.202689
1167.998749	55.703600	68.207694
1167.686234	56.169658	68.212698
1166.937968	63.336146	68.217703
1166.488439	63.913883	68.222708
1165.377722	61.162157	68.227713
1164.561787	55.950796	68.232718
1164.236697	60.572571	68.237722
1163.832345	51.107340	68.242727
1163.228597	53.653998	68.247732
1162.204775	59.052384	68.252737
1161.688269	61.121542	68.257742
1161.192973	57.767308	68.262746
1160.377615	58.551465	68.267751
1159.639997	55.234197	68.272756
1158.563099	60.336672	68.277761
1158.497985	55.590948	68.282766
1157.958375	56.656102	68.287770
1156.674753	61.920769	68.292775
1156.438376	58.255695	68.297780
1155.668794	61.781217	68.302785
1155.296905	57.210442	68.307790
1153.965198	57.721912	68.312794
1153.173089	60.615502	68.317799
1152.682476	55.801836	68.322804
1152.271030	60.241805	68.327809
1151.787750	48.049950	68.332814
1151.819787	52.021985	68.337818
1150.340073	57.570156	68.342823
1149.666683	53.296499	68.347828
1148.801014	66.433118	68.352833
1148.730979	53.000695	68.357838
1147.487534	51.558467	68.362842
1146.521703	53.118773	68.367847
1146.219332	52.573964	68.372852
1145.700061	58.298959	68.377857
1145.542291	46.121567	68.382862
1145.013849	54.566699	68.387866
1144.102156	59.840023	68.392871
1143.472108	52.675212	68.397876
1142.119515	49.599270	68.402881
1141.088962	55.490744	68.407886
1140.614522	57.293015	68.412890
1140.044160	52.263379	68.417895
1139.607919	53.335749	68.422900
1139.074064	64.424735	68.427905
1139.060480	51.801779	68.432910
1138.610896	52.598726	68.437914
1137.633852	57.576516	68.442919
1137.011438	60.006300	68.447924
1135.771835	54.764568	68.452929
1135.152383	48.992109	68.457934
1134.517024	52.420591	68.462938
1133.666306	54.224367	68.467943
1133.309708	51.417362	68.472948
1132.482711	53.934882	68.477953
1131.924138	52.831582	68.482958
1131.562249	53.701315	68.487962
1130.902328	61.451426	68.492967
1129.938953	48.284110	68.497972
1129.039486	56.297826	68.502977
1128.455533	51.437513	68.507982
1128.077510	50.061067	68.512986
1126.916072	53.820814	68.517991
1126.163833	48.704995	68.522996
1125.673082	57.907384	68.528001
1125.161304	41.837600	68.533006
1124.928694	53.039510	68.538010
1124.295566	58.746349	68.543015
1123.633100	48.669326	68.548020
1122.622650	52.253668	68.553025
1122.299229	47.041256	68.558030
1121.180583	53.728921	68.563034
1120.071156	60.124962	68.568039
1119.648207	51.088480	68.573044
1119.057526	57.723705	68.578049
1118.686009	47.147816	68.583054
1118.597924	46.185724	68.588058
1117.642649	56.272561	68.593063
1116.838609	39.052359	68.598068
1115.829484	50.639561	68.603073
1115.539626	54.213364	68.608078
1114.700067	54.808995	68.613082
1113.598186	48.607078	68.618087
1113.184479	46.089862	68.623092
1112.792252	56.982850	68.628097
1112.388620	55.970026	68.633102
1111.679431	51.568034	68.638106
1110.551148	48.768668	68.643111
1110.266091	48.189571	68.648116
1109.503935	53.265651	68.653121
1109.091620	46.794775	68.658126
1108.047282	52.207479	68.663130
1107.219813	49.456458	68.668135
1107.244874	47.214801	68.673140
1106.030013	51.457718	68.678145
1105.004516	46.364875	68.683150
1104.622998	43.549225	68.688154
1104.000906	54.406237	68.693159
1103.655469	42.255555	68.698164
1103.236483	55.232807	68.703169
1102.233100	55.163795	68.708174
1101.333699	50.306360	68.713178
1100.899696	54.999081	68.718183
1100.626478	45.826825	68.723188
1099.254828	57.971602	68.728193
1098.830866	48.083730	68.733198
1098.378063	47.122886	68.738202
1097.722007	61.050916	68.743207
1096.973748	52.626009	68.748212
1095.933822	60.804007	68.753217
1095.337841	51.405547	68.758222
1095.149294	50.558786	68.763226
1094.380614	55.090280	68.768231
1093.589389	53.427908	68.773236
1092.585616	55.916790	68.778241
1092.100763	53.256351	68.783246
1091.776182	55.496841	68.788250
1091.032020	55.815529	68.793255
1090.209471	53.834864	68.798260
1089.234128	57.366327	68.803265
1089.022585	62.815296	68.808270
1088.706709	51.877322	68.813274
1087.525409	50.836825	68.818279
1086.955503	54.138210	68.823284
1086.158337	62.783798	68.828289
1085.579453	54.861809	68.833294
1085.443311	49.758383	68.838298
1084.618653	65.302814	68.843303
1083.575922	59.242886	68.848308
1082.915033	57.626015	68.853313
1082.524595	51.033391	68.858318
1081.764266	54.191605	68.863322
1080.607464	55.235109	68.868327
1080.256570	61.996200	68.873332
1079.954416	60.098333	68.878337
1079.267614	55.552440	68.883342
1078.514797	47.976673	68.888346
1077.636148	53.504956	68.893351
1077.427432	46.005060	68.898356
1076.358703	62.655918	68.903361
1075.358185	56.676013	68.908366
1074.852904	57.120708	68.913370
1074.203261	57.771296	68.918375
1074.280800	46.162036	68.923380
1073.409179	55.980109	68.928385
1072.488131	50.679851	68.933390
1071.480352	52.639519	68.938394
1070.971647	64.501951	68.943399
1071.002707	51.920789	68.948404
1069.501566	59.566614	68.953409
1068.703008	64.883466	68.958414
1068.354402	60.152884	68.963418
1067.613535	63.117195	68.968423
1067.329712	55.212927	68.973428
1067.055439	57.672498	68.978433
1065.739172	57.170726	68.983438
1065.393008	59.304264	68.988442
1064.725333	60.030264	68.993447
1064.180782	52.989072	68.998452
1062.939506	58.712247	69.003457
1062.586093	56.321065	69.008462
1061.999951	58.305123	69.013466
1060.912517	63.125459	69.018471
1060.252270	49.525176	69.023476
1059.420904	54.350504	69.028481
1059.073671	50.677849	69.033486
1058.873921	58.190758	69.038490
1058.305576	53.717490	69.043495
1057.532528	45.928907	69.048500
1056.777470	56.826004	69.053505
1056.339324	51.245499	69.058510
1055.604849	48.345660	69.063514
1054.432162	50.197529	69.068519
1053.982301	43.757872	69.073524
1053.084432	51.949548	69.078529
1052.861957	47.351872	69.083534
1052.025616	50.470146	69.088538
1050.938599	48.569417	69.093543
1050.730018	47.132911	69.098548
1050.205565	53.175711	69.103553
1049.111835	42.845631	69.108558
1048.586552	49.533537	69.113562
1047.689650	55.690786	69.118567
1047.413153	51.647332	69.123572
1046.937692	53.615362	69.128577
1046.159330	48.390186	69.133582
1045.172878	52.461173	69.138586
1044.390245	58.686977	69.143591
1044.124302	44.869431	69.148596
1043.608846	58.420279	69.153601
1043.114033	50.626857	69.158606
1042.263352	41.425063	69.163610
1041.474835	53.486547	69.168615
1041.101538	44.065298	69.173620
1039.971500	48.513946	69.178625
1039.103436	51.403881	69.183630
1038.866140	44.471513	69.188634
1038.003732	56.800223	69.193639
1037.537754	48.794058	69.198644
1036.525904	56.683753	69.203649
1036.124174	53.123851	69.208654
1035.897059	42.564437	69.213658
1034.956999	52.793952	69.218663
1034.085814	44.943722	69.223668
1033.643305	52.290246	69.228673
1033.093626	51.343250	69.233678
1031.961720	42.585174	69.238682
1030.984876	50.869845	69.243687
1030.711797	50.386623	69.248692
1030.101455	56.346898	69.253697
1029.277855	52.780000	69.258702
1029.325370	49.389900	69.263706
1028.571374	47.735819	69.268711
1027.897933	48.155238	69.273716
1027.009577	55.219461	69.278721
1025.973553	52.064833	69.283726
1025.267171	49.663584	69.288730
1024.740026	49.998226	69.293735
1024.151288	46.848129	69.298740
1023.648408	58.209736	69.303745
1023.040653	52.228868	69.308750
1022.303614	46.033606	69.313754
1021.190076	48.674019	69.318759
1021.059550	44.466997	69.323764
1020.448175	45.229781	69.328769
1019.914696	46.502145	69.333774
1018.850639	44.323388	69.338778
1018.033052	51.606588	69.343783
1018.021535	53.256377	69.348788
1016.913763	49.695275	69.353793
1016.386229	48.184940	69.358798
1015.839139	50.244795	69.363802
1015.165966	55.937524	69.368807
1014.309131	55.078828	69.373812
1013.418039	45.320499	69.378817
1012.806029	50.199247	69.383822
1012.199006	48.146471	69.388826
1011.905710	55.390409	69.393831
1011.155368	44.619358	69.398836
1010.273247	55.427868	69.403841
1009.622960	54.408576	69.408846
1009.680853	50.177882	69.413850
1008.491263	50.922282	69.418855
1007.906280	42.807329	69.423860
1006.795482	49.537940	69.428865
1006.285406	43.972048	69.433870
1006.233177	44.016664	69.438874
1004.547362	49.577201	69.443879
1004.025290	46.687739	69.448884
1003.619177	52.394747	69.453889
1003.084730	50.265770	69.458894
1003.065978	47.368763	69.463898
1001.769679	55.377845	69.468903
1001.441646	49.514904	69.473908
1000.696811	45.998564	69.478913
999.827287	44.645151	69.483918
998.925581	46.146420	69.488922
998.303172	56.328559	69.493927
998.084743	50.079171	69.498932
996.997453	51.712472	69.503937
996.197049	53.008390	69.508942
995.820113	49.286856	69.513946
995.229401	49.313073	69.518951
994.778906	42.884571	69.523956
993.720128	55.335998	69.528961
992.757319	50.204845	69.533966
992.373628	44.945277	69.538970
991.566554	53.284949	69.543975
991.791490	44.746238	69.548980
991.220535	50.848484	69.553985
989.970621	47.685328	69.558990
989.750378	46.685923	69.563994
987.969092	55.122265	69.568999
987.456846	44.264452	69.574004
986.744619	52.257873	69.579009
986.301984	49.472469	69.584014
986.091321	55.681392	69.589018
985.598543	53.183088	69.594023
985.152394	46.422734	69.599028
984.044463	55.907844	69.604033
983.426333	49.780406	69.609038
982.835900	50.703871	69.614042
981.716947	55.822563	69.619047
981.263690	48.061972	69.624052
980.474474	43.090862	69.629057
979.874035	49.267187	69.634062
979.624619	47.826147	69.639066
978.265673	53.683197	69.644071
977.977654	48.696991	69.649076
977.318332	52.290169	69.654081
976.575925	50.875535	69.659086
976.467535	49.175510	69.664090
975.510330	46.902499	69.669095
974.494481	42.919936	69.674100
974.242997	48.968195	69.679105
973.519145	53.584049	69.684110
972.560906	52.287339	69.689114
971.741428	54.780056	69.694119
971.425941	48.008374	69.699124
970.918373	53.729953	69.704129
970.316254	55.689765	69.709134
969.311729	42.672590	69.714138
968.448892	46.993591	69.719143
968.294139	49.795273	69.724148
967.657758	45.993604	69.729153
966.714372	52.030539	69.734158
966.111940	50.150509	69.739162
965.410862	55.683685	69.744167
965.157128	44.075113	69.749172
963.889758	47.244654	69.754177
963.442520	52.786322	69.759182
962.926636	51.302530	69.764186
962.322342	53.508694	69.769191
961.617245	47.171175	69.774196
960.198868	50.295362	69.779201
959.714853	53.889034	69.784206
959.552737	48.632059	69.789210
959.042195	59.545459	69.794215
958.720403	44.382215	69.799220
957.562111	47.990143	69.804225
956.757704	46.389839	69.809230
956.687046	48.954211	69.814234
955.633427	44.100879	69.819239
954.502265	41.997485	69.824244
954.117981	44.621226	69.829249
953.714272	56.828074	69.834254
953.468773	43.940858	69.839258
951.984210	48.851235	69.844263
951.295551	43.737977	69.849268
950.721841	51.163734	69.854273
949.891763	47.582129	69.859278
950.064370	45.039451	69.864282
948.554958	54.161105	69.869287
948.323284	47.631558	69.874292
947.665094	57.166539	69.879297
947.014235	54.355930	69.884302
946.683518	45.935604	69.889306
945.646010	50.900999	69.894311
944.955047	49.326800	69.899316
944.580144	43.979112	69.904321
943.744158	47.543639	69.909326
943.103608	44.028071	69.914330
942.515706	53.780523	69.919335
941.985480	54.918344	69.924340
940.642147	51.320646	69.929345
939.974603	39.109307	69.934350
939.646642	47.006889	69.939354
938.816310	56.315374	69.944359
938.880978	44.876912	69.949364
938.016957	47.558076	69.954369
937.044592	50.049901	69.959374
936.786389	52.735583	69.964378
935.291429	54.443248	69.969383
934.746037	40.148234	69.974388
933.917850	48.112807	69.979393
933.573680	52.680864	69.984398
933.579398	46.832633	69.989402
932.477886	48.452455	69.994407
931.949775	42.722296	69.999412
930.969082	49.214610	70.004417
930.310232	49.328957	70.009422
929.882977	47.082014	70.014426
929.328035	47.909955	70.019431
928.760275	37.775363	70.024436
927.892927	48.072179	70.029441
927.147626	39.039748	70.034446
926.697917	49.743188	70.039450
925.399001	42.948251	70.044455
925.060021	45.886485	70.049460
924.486639	44.296734	70.054465
924.184534	48.419702	70.059470
923.347195	43.058880	70.064474
922.414735	47.878254	70.069479
921.886765	51.294421	70.074484
921.415711	42.893283	70.079489
920.442054	45.659709	70.084494
919.633879	43.274694	70.089498
918.927568	43.447059	70.094503
918.608917	42.272512	70.099508
918.266816	47.485214	70.104513
917.222944	48.771016	70.109518
916.723579	47.322452	70.114522
915.644887	54.256147	70.119527
915.471251	46.069450	70.124532
914.873910	44.876177	70.129537
913.393475	42.295377	70.134542
913.076029	42.415319	70.139546
912.620673	47.480465	70.144551
912.316315	37.695043	70.149556
911.235431	34.359952	70.154561
910.354911	44.316666	70.159566
910.045665	39.463163	70.164570
909.170053	50.675935	70.169575
909.077680	47.112557	70.174580
907.872261	37.181958	70.179585
907.127637	44.030945	70.184590
906.629839	42.744561	70.189594
906.204397	52.742398	70.194599
905.828546	36.589568	70.199604
904.740813	43.087884	70.204609
904.040159	45.344089	70.209614
903.558696	39.786288	70.214618
902.551612	47.506527	70.219623
901.822273	38.678147	70.224628
901.312649	39.837927	70.229633
900.786548	43.023563	70.234638
900.553624	48.431780	70.239642
899.306340	46.864134	70.244647
898.843131	41.574665	70.249652
898.176700	52.165943	70.254657
897.591847	46.424323	70.259662
897.056724	34.160390	70.264666
896.126897	50.759209	70.269671
895.498521	44.012111	70.274676
894.335911	44.421109	70.279681
893.408907	46.229216	70.284686
892.995870	42.451948	70.289690
892.546638	50.118099	70.294695
892.461511	35.593732	70.299700
892.161878	39.796731	70.304705
890.997995	43.416614	70.309710
890.171150	39.200582	70.314714
889.456480	43.586333	70.319719
889.311198	37.129783	70.324724
888.222855	36.068281	70.329729
887.167834	35.990226	70.334734
887.044689	35.675546	70.339738
886.393487	45.597347	70.344743
885.714469	50.551438	70.349748
884.595793	43.415601	70.354753
883.873808	45.288852	70.359758
883.728506	43.831252	70.364762
883.007370	48.763662	70.369767
882.447304	45.241609	70.374772
881.171616	47.900002	70.379777
880.963792	51.903890	70.384782
880.494118	40.384902	70.389786
879.257410	53.443422	70.394791
878.711348	40.504717	70.399796
878.254232	47.167603	70.404801
877.506282	53.714355	70.409806
877.668403	48.326936	70.414810
876.535326	51.330065	70.419815
875.632172	50.038819	70.424820
875.220925	48.590432	70.429825
874.002896	48.295476	70.434830
873.378946	48.014775	70.439834
872.752605	47.641414	70.444839
872.200072	45.166840	70.449844
871.803605	46.756471	70.454849
871.252252	48.077441	70.459854
870.395204	38.351612	70.464858
869.452010	48.815056	70.469863
869.356941	44.417902	70.474868
868.693737	48.473769	70.479873
867.627119	46.355410	70.484878
866.969661	46.677710	70.489882
866.169234	51.622745	70.494887
865.659142	43.152142	70.499892
865.306315	47.455075	70.504897
864.241357	52.779684	70.509902
863.797395	43.303496	70.514906
862.896396	48.789665	70.519911
862.710596	52.318538	70.524916
861.662791	47.800215	70.529921
860.761584	49.903849	70.534926
860.325251	45.620938	70.539930
859.877061	61.785146	70.544935
859.427482	42.244142	70.549940
858.471707	43.989032	70.554945
857.544448	47.787309	70.559950
857.238663	47.788707	70.564954
856.819453	50.430636	70.569959
856.105433	46.034230	70.574964
855.068915	51.143003	70.579969
854.549258	54.748672	70.584974
853.860133	51.078433	70.589978
852.545264	55.238032	70.594983
852.189681	45.791933	70.599988
851.640733	47.926232	70.604993
851.196620	49.277446	70.609998
851.141021	45.839107	70.615002
850.301753	58.328177	70.620007
849.585760	58.831687	70.625012
849.142120	60.715837	70.630017
847.741258	53.919821	70.635022
847.267485	54.984020	70.640026
846.325277	55.512499	70.645031
846.211323	53.103738	70.650036
844.843822	45.389360	70.655041
844.126203	55.216090	70.660046
844.151349	42.862987	70.665050
843.316352	60.101168	70.670055
842.976926	48.523606	70.675060
841.965467	46.182014	70.680065
841.134806	56.870409	70.685070
841.019076	56.538782	70.690074
840.233019	55.432336	70.695079
839.321964	55.935359	70.700084
838.368058	52.580085	70.705089
838.082138	55.394766	70.710094
837.872289	51.408545	70.715098
836.468034	56.744596	70.720103
835.651373	48.748575	70.725108
835.078369	45.908262	70.730113
834.708803	51.521159	70.735118
834.369433	43.610016	70.740122
833.182781	50.857391	70.745127
832.556122	45.045174	70.750132
832.120847	55.408858	70.755137
831.778444	55.201623	70.760142
830.717664	45.290617	70.765146
829.740847	55.667964	70.770151
829.305877	51.328071	70.775156
828.827555	56.901513	70.780161
828.263385	53.113620	70.785166
827.516035	48.624757	70.790170
826.712486	59.884430	70.795175
826.261013	46.481250	70.800180
825.586991	51.127053	70.805185
824.322116	54.928623	70.810190
824.078174	51.815156	70.815194
823.474132	57.034872	70.820199
822.871622	51.261389	70.825204
821.809120	47.781484	70.830209
820.654912	53.749521	70.835214
820.327631	51.743728	70.840218
819.840986	50.143350	70.845223
819.682701	47.391565	70.850228
819.509359	53.820053	70.855233
818.684426	56.032986	70.860238
817.751888	44.065724	70.865242
816.903741	48.004386	70.870247
816.379235	49.877759	70.875252
815.296582	54.697423	70.880257
814.521985	56.899191	70.885262
814.508875	42.396485	70.890266
813.989495	50.149504	70.895271
812.670879	45.688507	70.900276
811.860279	46.074623	70.905281
811.359638	49.615769	70.910286
811.210554	43.472069	70.915290
810.387626	53.873809	70.920295
809.427880	49.756231	70.925300
809.210830	45.594543	70.930305
808.611637	46.044778	70.935310
807.676684	45.895603	70.940314
806.491026	45.786339	70.945319
806.095880	48.757181	70.950324
805.489043	40.981665	70.955329
805.028758	47.231901	70.960334
804.710099	43.370241	70.965338
803.585153	50.450109	70.970343
803.077298	43.899898	70.975348
802.905713	48.937231	70.980353
801.839843	45.836340	70.985358
801.041681	52.257061	70.990362
800.472326	43.486828	70.995367
799.613074	47.684306	71.000372
798.558119	51.009345	71.005377
797.820967	51.759089	71.010382
797.665433	41.779688	71.015386
797.083264	48.728996	71.020391
796.796870	48.673698	71.025396
796.006979	45.703918	71.030401
794.864155	57.053876	71.035406
794.769049	44.119103	71.040410
793.572249	54.865794	71.045415
792.695578	53.922023	71.050420
792.215481	50.603304	71.055425
791.511065	49.510687	71.060430
791.217128	48.510418	71.065434
790.929564	50.245150	71.070439
790.075422	48.648089	71.075444
789.502690	53.736669	71.080449
788.301746	53.483190	71.085454
787.584976	45.119628	71.090458
786.654231	51.200336	71.095463
786.225837	49.496074	71.100468
785.964073	54.902581	71.105473
785.334665	53.581980	71.110478
784.905470	41.326449	71.115482
784.022577	49.272959	71.120487
783.170810	44.143147	71.125492
782.858473	44.408948	71.130497
781.549428	40.766463	71.135502
781.084016	35.701303	71.140506
780.374698	48.936089	71.145511
779.968132	41.445666	71.150516
779.563160	48.887161	71.155521
778.118346	45.952266	71.160526
777.400673	45.230770	71.165530
776.856032	46.866082	71.170535
776.831055	41.680340	71.175540
776.296813	42.429324	71.180545
774.971439	45.658651	71.185550
774.493220	42.066826	71.190554
773.742952	41.822030	71.195559
773.681907	42.349025	71.200564
772.691337	44.438529	71.205569
771.679161	49.540302	71.210574
771.478397	43.094175	71.215578
771.025359	46.588324	71.220583
770.074727	42.707435	71.225588
769.186885	39.712259	71.230593
768.314026	46.856083	71.235598
768.296984	30.270867	71.240602
767.138203	44.463455	71.245607
766.224642	39.583186	71.250612
765.607265	38.134521	71.255617
765.361785	53.616742	71.260622
765.167957	39.153857	71.265626
763.955171	44.156682	71.270631
763.221981	47.856284	71.275636
762.597086	42.332392	71.280641
762.045195	47.606892	71.285646
761.965855	34.980282	71.290650
760.672835	43.283827	71.295655
759.575494	41.288681	71.300660
759.186064	41.375948	71.305665
758.959160	43.594611	71.310670
758.643093	39.685239	71.315674
757.436392	43.606885	71.320679
757.144809	41.628536	71.325684
756.260631	40.641820	71.330689
754.950663	38.781454	71.335694
754.345689	30.385921	71.340698
753.761222	36.756855	71.345703
753.581900	33.786077	71.350708
753.202689	32.044031	71.355713
752.136274	38.404965	71.360718
751.485096	32.522566	71.365722
750.871331	41.804489	71.370727
750.249637	33.993513	71.375732
749.460495	35.869606	71.380737
748.620951	41.653528	71.385742
748.356939	38.186878	71.390746
747.693096	42.849998	71.395751
746.904562	39.490514	71.400756
746.423155	38.400251	71.405761
745.299271	42.729763	71.410766
744.877738	38.876609	71.415770
744.241097	45.703709	71.420775
743.345399	40.002166	71.425780
742.714430	46.915097	71.430785
742.043278	48.449132	71.435790
742.049695	37.204474	71.440794
740.848439	47.340031	71.445799
740.415595	39.587297	71.450804
739.514124	38.335258	71.455809
739.151834	43.836616	71.460814
738.518648	34.940953	71.465818
737.590777	37.168720	71.470823
737.009066	37.611457	71.475828
736.681154	43.676621	71.480833
735.263259	46.464959	71.485838
734.798051	47.521505	71.490842
734.362708	44.824880	71.495847
733.867489	36.239988	71.500852
732.850742	42.506290	71.505857
731.649735	39.381218	71.510862
731.570195	27.087390	71.515866
730.960404	45.962857	71.520871
730.561841	38.337132	71.525876
729.668309	37.539572	71.530881
728.919908	36.075508	71.535886
728.367045	35.595869	71.540890
727.671254	39.888765	71.545895
727.257533	41.000192	71.550900
726.063407	30.620052	71.555905
725.015466	33.459875	71.560910
725.146454	31.010549	71.565914
724.733103	36.527920	71.570919
724.249513	35.147850	71.575924
723.074511	31.747408	71.580929
722.338852	43.232822	71.585934
722.384731	31.642842	71.590938
720.812327	35.308918	71.595943
720.328642	34.712609	71.600948
719.882092	30.488131	71.605953
719.259127	31.629723	71.610958
718.108911	33.465545	71.615962
717.487748	39.938523	71.620967
717.209595	31.981396	71.625972
716.995672	35.689790	71.630977
715.644672	30.311494	71.635982
714.918741	27.117097	71.640986
714.463416	39.310078	71.645991
713.712719	36.496514	71.650996
713.746149	34.477459	71.656001
712.297335	36.794492	71.661006
711.930234	39.166367	71.666010
711.706430	33.089775	71.671015
710.736157	39.776037	71.676020
709.644164	33.377215	71.681025
709.022348	40.277653	71.686030
708.821953	30.937775	71.691034
707.861225	34.957470	71.696039
706.737592	32.572298	71.701044
706.181187	35.117820	71.706049
705.342223	38.563041	71.711054
705.402992	34.745062	71.716058
704.913674	39.670560	71.721063
704.009755	44.337225	71.726068
703.151361	38.856841	71.731073
702.469548	37.642380	71.736078
702.229065	31.475405	71.741082
701.384534	37.201784	71.746087
700.629919	33.624028	71.751092
699.905062	36.970657	71.756097
699.143962	35.801938	71.761102
698.882646	35.824660	71.766106
697.657856	33.275827	71.771111
697.129846	42.383254	71.776116
696.733031	44.641593	71.781121
696.083082	41.630642	71.786126
695.629822	35.311468	71.791130
694.397760	36.395513	71.796135
693.851006	37.394088	71.801140
693.730668	38.040912	71.806145
692.596696	41.591460	71.811150
691.618297	27.980511	71.816154
691.009187	33.707251	71.821159
690.619193	36.182122	71.826164
690.289283	27.484193	71.831169
689.630917	40.988414	71.836174
688.968770	31.747299	71.841178
688.146525	52.118439	71.846183
687.688401	40.206589	71.851188
686.396263	35.228943	71.856193
685.230148	43.617969	71.861198
685.166006	35.894849	71.866202
684.683337	36.425905	71.871207
683.795274	43.890716	71.876212
684.005337	37.956349	71.881217
683.238754	40.275147	71.886222
682.505504	39.144576	71.891226
681.791487	40.450486	71.896231
680.760628	38.966761	71.901236
679.991058	31.600404	71.906241
678.992037	46.896677	71.911246
678.802871	36.086872	71.916250
678.481387	36.953384	71.921255
677.774181	39.732660	71.926260
676.985635	35.762923	71.931265
676.019404	39.789813	71.936270
675.561673	36.631566	71.941274
674.328919	46.466234	71.946279
673.805664	31.789333	71.951284
673.525394	30.890983	71.956289
672.936875	35.871705	71.961294
672.721603	30.583813	71.966298
671.578752	30.518259	71.971303
670.837194	40.213203	71.976308
670.557603	35.818645	71.981313
669.701756	27.415784	71.986318
669.178856	33.893620	71.991322
668.176094	35.787986	71.996327
667.641609	38.162867	72.001332
666.990253	33.780204	72.006337
666.096418	43.354321	72.011342
666.037646	31.224350	72.016346
665.122880	40.333444	72.021351
663.993897	36.063111	72.026356
663.443936	29.106490	72.031361
662.422077	43.904931	72.036366
662.208636	40.201582	72.041370
662.068585	41.048665	72.046375
661.102268	45.983900	72.051380
660.445603	37.311198	72.056385
659.675753	40.447384	72.061390
659.325768	27.001306	72.066394
658.166917	37.111210	72.071399
657.291818	41.284444	72.076404
656.957196	42.944681	72.081409
656.298127	37.326918	72.086414
656.173585	38.822812	72.091418
655.238431	35.597097	72.096423
654.260765	45.422688	72.101428
653.961920	31.878578	72.106433
652.842723	40.152909	72.111438
651.948838	36.944276	72.116442
651.258959	43.385633	72.121447
650.851495	41.555063	72.126452
650.863676	38.288870	72.131457
650.125218	40.978513	72.136462
649.268603	40.123064	72.141466
648.437711	39.291904	72.146471
648.219531	40.946214	72.151476
647.497901	40.441429	72.156481
645.889013	40.651954	72.161486
645.713659	36.836887	72.166490
645.193184	39.160656	72.171495
644.395671	41.016037	72.176500
643.652635	33.986088	72.181505
642.669187	45.269705	72.186510
642.458304	40.212927	72.191514
642.022481	41.163885	72.196519
641.630131	37.515840	72.201524
640.589586	42.502326	72.206529
639.857953	49.167956	72.211534
639.346058	44.714202	72.216538
638.340203	39.866031	72.221543
637.184290	37.126488	72.226548
636.755288	41.383225	72.231553
636.283819	47.480721	72.236558
636.001532	41.091753	72.241562
635.678202	44.287720	72.246567
634.649497	36.352368	72.251572
634.060890	41.098147	72.256577
633.578030	42.190638	72.261582
632.991804	39.623720	72.266586
631.825811	41.086780	72.271591
631.005162	44.079677	72.276596
630.940264	34.450151	72.281601
629.893899	43.425674	72.286606
628.760939	42.527511	72.291610
628.447729	39.697917	72.296615
627.620948	45.825192	72.301620
627.505638	36.467045	72.306625
626.954200	44.348191	72.311630
626.225541	33.004577	72.316634
625.500193	39.547781	72.321639
624.932436	44.320204	72.326644
623.800649	33.043948	72.331649
622.802878	41.491340	72.336654
622.337963	42.681900	72.341658
622.012847	43.063297	72.346663
621.620943	41.922535	72.351668
621.194300	43.296234	72.356673
619.734297	45.481060	72.361678
619.362754	30.825749	72.366682
618.844327	40.715401	72.371687
618.061152	44.593311	72.376692
616.980953	41.248785	72.381697
616.369484	49.191535	72.386702
616.133458	40.216889	72.391706
615.674906	46.651374	72.396711
615.023198	53.077201	72.401716
614.169099	42.554655	72.406721
613.536280	47.596063	72.411726
613.008295	42.302787	72.416730
611.690949	44.412858	72.421735
611.058830	42.223838	72.426740
610.633734	39.448336	72.431745
610.234350	41.027429	72.436750
610.034955	43.389954	72.441754
608.642987	43.524954	72.446759
608.021975	50.515171	72.451764
607.649492	44.138996	72.456769
607.032988	44.924772	72.461774
606.159607	35.851369	72.466778
605.286583	41.713201	72.471783
604.627985	45.661159	72.476788
604.212547	40.036148	72.481793
603.796719	50.472438	72.486798
602.833560	41.345523	72.491802
602.232704	42.582969	72.496807
601.661278	40.687060	72.501812
601.033301	45.286153	72.506817
599.831920	42.623254	72.511822
599.330673	39.587072	72.516826
598.825192	44.204501	72.521831
598.774667	42.520516	72.526836
598.005415	35.993075	72.531841
596.695868	48.777863	72.536846
596.503193	43.464301	72.541850
595.458067	44.154345	72.546855
594.451192	42.580105	72.551860
593.916086	37.051428	72.556865
593.280068	45.844912	72.561870
593.003768	36.088212	72.566874
592.459062	33.978316	72.571879
591.887161	45.855562	72.576884
591.145839	40.993664	72.581889
590.245188	44.316282	72.586894
590.257321	41.734495	72.591898
589.011230	42.000812	72.596903
588.007550	38.131604	72.601908
587.398433	38.375314	72.606913
587.083701	54.081441	72.611918
586.703340	36.221598	72.616922
585.587742	41.727835	72.621927
584.866199	44.066296	72.626932
585.005045	30.130793	72.631937
583.565671	42.472636	72.636942
582.830722	36.065893	72.641946
582.148605	37.456635	72.646951
581.394142	41.451406	72.651956
581.312702	51.976362	72.656961
580.490634	48.299001	72.661966
579.554574	41.664094	72.666970
579.298044	36.636674	72.671975
578.139898	42.987052	72.676980
578.240663	32.304553	72.681985
576.846555	42.357344	72.686990
576.328430	43.990049	72.691994
576.016350	40.250383	72.696999
575.399284	45.814413	72.702004
575.009089	41.049556	72.707009
573.994813	47.824875	72.712014
572.963307	33.705204	72.717018
572.050794	40.956320	72.722023
571.173306	43.395317	72.727028
571.176771	39.099190	72.732033
570.734960	51.939739	72.737038
570.420176	49.223943	72.742042
569.519852	48.547372	72.747047
568.367572	44.279218	72.752052
567.876983	35.165360	72.757057
566.921304	45.399057	72.762062
566.452774	44.313087	72.767066
565.748406	43.048641	72.772071
565.290692	39.188673	72.777076
565.176258	42.195254	72.782081
563.770883	45.398005	72.787086
563.372251	42.334446	72.792090
562.391788	46.251681	72.797095
561.830513	44.690054	72.802100
561.300003	44.145390	72.807105
560.089076	41.632266	72.812110
559.693150	36.340049	72.817114
559.334941	38.226404	72.822119
558.791764	42.044022	72.827124
558.242524	34.641038	72.832129
557.289863	41.639934	72.837134
556.475993	36.275520	72.842138
555.959237	36.569180	72.847143
555.293664	44.640404	72.852148
554.685471	41.231761	72.857153
553.856598	40.067575	72.862158
553.300811	39.522209	72.867162
553.267872	34.720952	72.872167
552.264718	37.875406	72.877172
551.582349	32.458509	72.882177
550.255359	40.800670	72.887182
549.708838	35.515098	72.892186
548.879295	45.307662	72.897191
547.893196	44.934921	72.902196
548.160236	29.668557	72.907201
547.332334	40.082175	72.912206
547.318420	37.378382	72.917210
546.415678	44.307830	72.922215
545.135741	41.420931	72.927220
544.928788	38.681657	72.932225
544.215797	43.849389	72.937230
543.484094	38.411966	72.942234
542.662737	42.661830	72.947239
542.075102	53.335228	72.952244
541.875755	33.511652	72.957249
540.416253	52.918303	72.962254
539.770290	47.470375	72.967258
539.461228	44.233280	72.972263
539.138445	48.799540	72.977268
538.760655	37.146178	72.982273
537.590586	41.673942	72.987278
537.057503	34.657897	72.992282
535.892838	41.531299	72.997287
534.817362	40.056321	73.002292
534.507732	43.261154	73.007297
533.695456	41.253818	73.012302
533.591548	30.824701	73.017306
533.407407	40.545993	73.022311
532.734079	38.888684	73.027316
532.037225	34.543272	73.032321
530.950816	39.166519	73.037326
529.901755	49.050830	73.042330
529.269480	34.687813	73.047335
528.505523	34.339617	73.052340
528.470437	37.130132	73.057345
527.904529	45.273793	73.062350
526.886795	38.647191	73.067354
526.333569	36.861941	73.072359
525.301890	48.290470	73.077364
525.356006	38.359723	73.082369
524.200628	44.298098	73.087374
523.490292	44.986878	73.092378
522.968976	40.630849	73.097383
522.241622	45.472870	73.102388
521.612585	42.953801	73.107393
520.678332	42.233768	73.112398
520.426408	42.146203	73.117402
519.926381	42.033507	73.122407
518.600199	40.959596	73.127412
518.101802	34.059456	73.132417
517.240836	44.140883	73.137422
517.208849	37.294173	73.142426
516.756472	34.251803	73.147431
515.883294	33.171960	73.152436
515.283533	32.094292	73.157441
514.310072	41.999675	73.162446
513.926060	38.027052	73.167450
512.903463	24.087355	73.172455
511.783384	35.440074	73.177460
511.514933	36.306042	73.182465
511.068800	43.616919	73.187470
510.955811	31.517687	73.192474
509.977372	38.503356	73.197479
509.191623	41.041298	73.202484
508.815690	31.030834	73.207489
507.561830	43.578123	73.212494
506.601220	34.096040	73.217498
506.383971	35.917367	73.222503
505.909380	28.873092	73.227508
505.312973	35.145043	73.232513
504.048467	41.613318	73.237518
503.523915	34.854544	73.242522
502.975108	35.791985	73.247527
502.495584	35.622410	73.252532
502.381014	32.113066	73.257537
501.299286	36.801811	73.262542
500.251826	35.950011	73.267546
500.030767	36.759545	73.272551
499.245849	39.978599	73.277556
498.327351	19.329764	73.282561
497.277283	34.828164	73.287566
496.875420	35.720119	73.292570
497.110983	27.198651	73.297575
495.871693	46.269030	73.302580
495.294810	38.480961	73.307585
494.285733	47.545207	73.312590
494.008082	36.437299	73.317594
493.181271	35.801084	73.322599
492.000473	42.957771	73.327604
491.634248	41.185315	73.332609
490.802265	34.188518	73.337614
490.722303	35.130115	73.342618
490.569676	38.606404	73.347623
489.320505	40.592134	73.352628
488.752297	32.684417	73.357633
488.095426	45.371569	73.362638
487.364863	34.957138	73.367642
486.498128	34.910757	73.372647
485.788252	45.091122	73.377652
485.360473	36.465597	73.382657
484.808707	29.632318	73.387662
484.298561	35.776990	73.392666
483.272841	34.946966	73.397671
483.010553	38.305109	73.402676
482.062311	36.309992	73.407681
480.972040	30.697910	73.412686
480.343175	38.097824	73.417690
479.933543	35.999551	73.422695
479.346442	38.851204	73.427700
479.219824	33.227518	73.432705
477.879498	51.713191	73.437710
477.239113	29.610253	73.442714
477.150793	30.248830	73.447719
476.022754	33.087319	73.452724
475.751351	23.079139	73.457729
474.789943	34.930136	73.462734
473.655348	34.751394	73.467738
472.900284	27.583081	73.472743
472.157573	37.554211	73.477748
471.846105	27.688030	73.482753
471.414134	36.606713	73.487758
471.154375	30.603697	73.492762
470.906905	33.797053	73.497767
469.740745	38.846191	73.502772
469.062521	31.485863	73.507777
467.784448	31.823568	73.512782
466.767203	29.467293	73.517786
466.302575	30.408676	73.522791
465.890910	39.491282	73.527796
465.667779	34.251980	73.532801
465.401123	39.952587	73.537806
464.287100	32.828851	73.542810
463.599315	36.289481	73.547815
463.129494	32.754740	73.552820
462.411670	31.055656	73.557825
461.060543	27.836374	73.562830
460.818622	32.537984	73.567834
460.316699	25.122765	73.572839
459.389088	32.281698	73.577844
458.627459	28.381870	73.582849
457.812440	36.163105	73.587854
457.202228	36.474830	73.592858
456.957134	30.543596	73.597863
456.644250	37.710243	73.602868
456.127766	30.749927	73.607873
454.986754	38.676144	73.612878
454.564320	40.640554	73.617882
453.386917	32.653293	73.622887
452.513177	30.569048	73.627892
452.168815	31.060766	73.632897
451.381802	34.163472	73.637902
450.973524	35.091148	73.642906
450.518735	34.804103	73.647911
449.466553	38.609801	73.652916
449.189954	29.758352	73.657921
448.629954	44.896417	73.662926
447.473053	33.733075	73.667930
446.505589	30.957293	73.672935
445.753848	37.523664	73.677940
445.592488	28.969244	73.682945
445.180443	31.922320	73.687950
444.541465	28.939661	73.692954
443.725571	20.869580	73.697959
442.643433	33.063094	73.702964
442.997814	25.442055	73.707969
442.203306	29.476355	73.712974
440.993918	32.419283	73.717978
440.593827	30.257996	73.722983
439.755685	34.305558	73.727988
439.130893	28.404866	73.732993
438.135755	29.955907	73.737998
437.758040	34.072032	73.743002
437.714267	37.079971	73.748007
436.230993	36.713954	73.753012
435.420285	32.602757	73.758017
434.838129	41.229987	73.763022
434.612506	31.194016	73.768026
434.071654	34.093502	73.773031
432.821240	44.927706	73.778036
432.625513	34.710351	73.783041
432.052861	32.043554	73.788046
430.888281	37.056185	73.793050
430.098319	34.310474	73.798055
429.277263	47.168875	73.803060
429.114234	36.850115	73.808065
428.580936	36.369003	73.813070
428.281883	35.653448	73.818074
427.320273	37.191266	73.823079
426.645731	41.878237	73.828084
426.392384	36.178556	73.833089
424.869287	42.580838	73.838094
424.018466	39.415896	73.843098
424.061910	32.008400	73.848103
423.198231	45.242598	73.853108
422.788508	33.659015	73.858113
421.495372	37.706544	73.863118
420.943254	27.479754	73.868122
420.670961	26.405123	73.873127
420.008419	43.853984	73.878132
419.494660	27.415796	73.883137
418.463844	31.341102	73.888142
417.763545	36.812766	73.893146
417.546673	37.659486	73.898151
416.231427	40.682372	73.903156
415.706256	34.144494	73.908161
415.109834	40.416466	73.913166
414.967080	37.709554	73.918170
414.533904	41.929138	73.923175
413.521194	36.394615	73.928180
412.605877	32.205479	73.933185
411.992096	38.232636	73.938190
411.000142	37.113411	73.943194
410.201348	38.040244	73.948199
409.607932	41.030113	73.953204
409.240631	38.753219	73.958209
408.737079	40.894564	73.963214
408.423268	35.422140	73.968218
407.681451	39.624673	73.973223
406.532229	46.396320	73.978228
406.301344	39.464620	73.983233
405.587157	39.507498	73.988238
404.238472	43.330501	73.993242
403.789359	44.564312	73.998247
403.260024	43.790839	74.003252
402.986030	39.169928	74.008257
402.086284	36.206755	74.013262
401.286644	37.259882	74.018266
400.587696	40.200338	74.023271
399.853029	41.665733	74.028276
399.907951	40.332381	74.033281
398.616249	39.448583	74.038286
397.652234	41.242262	74.043290
397.157422	28.970509	74.048295
396.624691	45.736370	74.053300
396.666275	31.250261	74.058305
396.100552	30.053659	74.063310
394.937306	39.689698	74.068314
394.514747	34.095834	74.073319
393.508218	43.516092	74.078324
393.182936	28.914983	74.083329
392.540503	47.600124	74.088334
391.039563	47.568109	74.093338
390.414963	38.012035	74.098343
389.564253	46.126985	74.103348
389.514157	28.470057	74.108353
389.085965	36.378899	74.113358
388.804929	36.294410	74.118362
387.847165	28.721617	74.123367
386.685437	43.577108	74.128372
386.107072	33.182621	74.133377
385.261517	43.411432	74.138382
384.453831	44.450078	74.143386
383.873916	31.477532	74.148391
383.477216	42.349170	74.153396
383.079879	27.008923	74.158401
383.025537	40.498923	74.163406
381.438326	44.095022	74.168410
381.207044	36.595689	74.173415
380.285410	34.897571	74.178420
379.588745	35.778176	74.183425
378.524304	41.694232	74.188430
377.750966	35.224298	74.193434
377.902959	39.984564	74.198439
377.219575	33.113944	74.203444
376.759267	30.445028	74.208449
375.365947	39.329266	74.213454
374.986113	40.741275	74.218458
374.608889	36.967871	74.223463
373.841639	42.308291	74.228468
372.897644	35.036082	74.233473
372.523990	36.978536	74.238478
371.878940	42.479254	74.243482
370.947105	37.803914	74.248487
369.947191	47.347705	74.253492
369.941429	32.941683	74.258497
369.244917	34.907205	74.263502
367.986396	29.897579	74.268506
367.382243	35.229353	74.273511
366.868736	36.629550	74.278516
366.451557	31.664038	74.283521
366.273707	38.361317	74.288526
364.858373	35.059283	74.293530
364.425239	28.338021	74.298535
363.739235	37.893283	74.303540
363.511017	29.504072	74.308545
361.932548	37.495309	74.313550
361.467714	30.645059	74.318554
361.124603	30.825931	74.323559
360.525594	40.761567	74.328564
360.205561	38.093951	74.333569
359.201859	31.263349	74.338574
358.639271	37.906826	74.343578
358.107085	38.015330	74.348583
357.131090	42.338776	74.353588
356.406087	28.283928	74.358593
355.850893	38.564238	74.363598
355.116084	38.142065	74.368602
354.649812	33.507653	74.373607
353.388965	33.462628	74.378612
353.110362	35.979714	74.383617
352.551209	34.985501	74.388622
352.034253	36.756833	74.393626
351.630103	31.882287	74.398631
350.290716	40.956638	74.403636
349.720253	29.944320	74.408641
348.820445	33.788850	74.413646
348.616997	29.901025	74.418650
348.029632	29.688744	74.423655
347.289622	42.151041	74.428660
346.611873	34.390136	74.433665
346.455295	29.890873	74.438670
345.064938	33.521849	74.443674
344.495018	22.955728	74.448679
343.795242	37.474252	74.453684
343.533902	37.331436	74.458689
342.300819	48.483035	74.463694
341.793304	28.598255	74.468698
341.118652	26.066010	74.473703
340.498763	28.251138	74.478708
340.388562	22.656394	74.483713
339.609709	27.344235	74.488718
338.784143	29.951649	74.493722
338.362310	23.526638	74.498727
337.113517	31.383342	74.503732
336.296567	24.663337	74.508737
335.864856	31.981389	74.513742
335.165177	34.070426	74.518746
335.166114	34.220122	74.523751
333.930612	30.627673	74.528756
333.105252	25.566378	74.533761
332.740222	30.662927	74.538766
331.830177	29.194792	74.543770
331.862567	24.911416	74.548775
330.384141	32.539797	74.553780
329.745482	31.130909	74.558785
329.409172	31.007928	74.563790
329.079908	28.854298	74.568794
328.723476	27.115003	74.573799
327.423978	36.602470	74.578804
326.919424	28.372427	74.583809
326.007306	39.983799	74.588814
325.002800	26.113864	74.593818
324.313239	33.949251	74.598823
323.599694	31.205591	74.603828
323.413290	23.779547	74.608833
323.034173	25.562029	74.613838
322.843218	31.207996	74.618842
321.678654	27.735134	74.623847
320.754771	38.703413	74.628852
320.353811	24.199547	74.633857
319.331060	38.037851	74.638862
318.517287	31.609079	74.643866
318.284157	19.666234	74.648871
317.446413	34.749217	74.653876
317.006993	29.142292	74.658881
316.032171	23.494549	74.663886
315.088134	30.482678	74.668890
314.913948	29.258383	74.673895
314.202750	34.146759	74.678900
314.210007	27.191316	74.683905
312.970472	25.061350	74.688910
312.355228	30.281360	74.693914
311.764854	32.397136	74.698919
310.763226	27.909566	74.703924
310.268430	24.746271	74.708929
309.703601	27.682716	74.713934
308.881934	27.127746	74.718938
307.993795	23.580872	74.723943
307.191721	34.102384	74.728948
306.650808	34.158673	74.733953
306.089661	37.711119	74.738958
305.809814	32.383111	74.743962
305.532061	25.116708	74.748967
304.372230	31.986273	74.753972
304.044744	24.762491	74.758977
303.396636	37.859844	74.763982
302.366179	35.168280	74.768986
302.114901	24.839964	74.773991
300.742242	38.150576	74.778996
299.932939	32.526917	74.784001
299.212629	32.819960	74.789006
298.562010	30.001623	74.794010
298.324290	22.599533	74.799015
297.728442	34.337114	74.804020
297.896537	44.191489	74.809025
296.504566	32.502737	74.814030
295.220879	32.082915	74.819034
295.073256	26.454716	74.824039
294.703290	47.826121	74.829044
293.628168	22.785348	74.834049
293.022793	28.000634	74.839054
292.370307	41.636427	74.844058
292.196594	36.037615	74.849063
291.092449	41.422293	74.854068
290.233026	30.345670	74.859073
289.725187	29.773799	74.864078
289.365352	35.817269	74.869082
288.544224	23.523455	74.874087
287.312908	32.754066	74.879092
286.983225	28.922641	74.884097
286.622107	27.045329	74.889102
286.002229	29.591587	74.894106
285.380259	32.843073	74.899111
284.342162	35.763501	74.904116
283.929545	27.979283	74.909121
283.389913	27.470828	74.914126
282.548227	26.628901	74.919130
281.807748	23.058500	74.924135
281.245999	30.148127	74.929140
280.556083	26.514473	74.934145
279.485070	33.690010	74.939150
278.829117	39.097867	74.944154
278.623339	32.731466	74.949159
277.887172	38.707193	74.954164
277.761894	32.580272	74.959169
276.610243	28.651216	74.964174
275.764966	43.189793	74.969178
275.471849	27.203768	74.974183
274.493802	35.539311	74.979188
273.535569	26.208356	74.984193
272.936584	36.689619	74.989198
272.345467	36.488993	74.994202
272.543787	27.654918	74.999207
271.363633	36.118873	75.004212
270.689206	32.547406	75.009217
270.112815	38.439319	75.014222
269.329139	37.468301	75.019226
268.997484	34.223815	75.024231
267.802859	37.505089	75.029236
267.451465	32.081261	75.034241
267.067444	32.891560	75.039246
265.882461	37.634702	75.044250
265.118559	24.022913	75.049255
264.432640	31.737883	75.054260
264.023976	31.635906	75.059265
263.775888	31.396370	75.064270
262.411996	34.479126	75.069274
261.859796	22.285958	75.074279
261.367733	31.299388	75.079284
260.949488	29.681920	75.084289
259.873603	28.427905	75.089294
259.027897	37.603368	75.094298
258.555589	35.215508	75.099303
258.110320	39.996854	75.104308
257.681083	36.534537	75.109313
256.992167	40.208286	75.114318
256.125266	43.263860	75.119322
255.848929	29.072880	75.124327
254.489619	43.847945	75.129332
253.949098	33.756552	75.134337
253.477089	32.176041	75.139342
252.752738	32.797745	75.144346
252.476840	26.592339	75.149351
251.259429	37.467078	75.154356
250.556016	31.066472	75.159361
250.116173	28.902097	75.164366
249.561598	37.662147	75.169370
249.046744	29.440076	75.174375
247.900311	36.488878	75.179380
247.398585	30.600167	75.184385
247.149094	20.191157	75.189390
246.270211	40.262275	75.194394
245.347903	31.108530	75.199399
244.658772	31.500696	75.204404
244.253219	36.647870	75.209409
243.988765	25.471694	75.214414
242.914443	30.693939	75.219418
242.481648	25.292557	75.224423
241.696208	32.176579	75.229428
241.045202	31.600733	75.234433
240.032767	35.647755	75.239438
239.144900	37.312659	75.244442
238.776276	30.959610	75.249447
238.288662	33.358639	75.254452
237.770749	32.305841	75.259457
237.118630	29.741649	75.264462
236.085310	35.860950	75.269466
236.072331	33.647450	75.274471
234.828881	31.134951	75.279476
234.108447	35.846625	75.284481
233.348614	29.918642	75.289486
233.060358	35.094425	75.294490
232.825582	35.751626	75.299495
231.557815	45.448546	75.304500
231.138877	33.915374	75.309505
230.530592	41.493400	75.314510
229.659123	43.089462	75.319514
228.890268	29.891634	75.324519
228.005094	38.694931	75.329524
227.431918	36.288466	75.334529
226.757699	29.033243	75.339534
226.792391	34.800933	75.344538
225.941327	31.429528	75.349543
225.021862	34.222257	75.354548
224.309760	23.920116	75.359553
224.001877	31.716750	75.364558
222.945550	33.359631	75.369562
222.475598	32.529423	75.374567
221.882557	35.579194	75.379572
221.234326	40.815522	75.384577
220.031052	35.631592	75.389582
219.322404	34.943517	75.394586
218.863166	37.642376	75.399591
218.075388	39.638258	75.404596
218.093490	35.989516	75.409601
217.547372	35.836921	75.414606
216.545871	33.456168	75.419610
216.247898	26.262391	75.424615
215.132601	30.977097	75.429620
214.290856	28.403721	75.434625
213.920815	29.237029	75.439630
213.327002	33.513785	75.444634
213.116157	42.381468	75.449639
211.588717	36.169017	75.454644
211.294127	48.544560	75.459649
211.099183	35.792974	75.464654
209.749404	39.274052	75.469658
208.908272	35.823799	75.474663
208.174343	32.813768	75.479668
207.708689	34.185866	75.484673
207.561068	36.106498	75.489678
206.555455	36.366206	75.494682
206.090135	31.072517	75.499687
205.367898	36.281223	75.504692
204.864008	31.444688	75.509697
203.559372	36.946519	75.514702
203.016399	38.286791	75.519706
202.543466	35.910082	75.524711
201.956314	42.508617	75.529716
201.140242	44.341859	75.534721
200.126944	31.645059	75.539726
199.393174	40.804269	75.544730
199.092444	37.848176	75.549735
198.856374	35.619782	75.554740
198.546528	39.075413	75.559745
197.767110	31.051655	75.564750
196.776846	37.775959	75.569754
196.274525	29.378442	75.574759
194.876362	32.373658	75.579764
194.271973	36.764067	75.584769
193.939599	34.890072	75.589774
193.521946	37.628036	75.594778
193.075472	35.923619	75.599783
192.037715	38.173828	75.604788
191.091200	28.021036	75.609793
190.770836	38.803238	75.614798
190.377353	35.776779	75.619802
189.555146	37.144228	75.624807
188.572836	40.543074	75.629812
187.855636	33.326255	75.634817
187.565633	38.828747	75.639822
186.616773	40.911822	75.644826
185.898533	34.053135	75.649831
185.345684	38.129403	75.654836
184.795340	28.545801	75.659841
184.315154	33.555070	75.664846
183.206343	43.644554	75.669850
182.381958	42.210125	75.674855
181.920080	35.529759	75.679860
181.588151	37.963900	75.684865
181.389259	32.495274	75.689870
179.735691	42.770962	75.694874
179.541299	34.188733	75.699879
178.942096	35.758747	75.704884
178.534805	40.138236	75.709889
177.475911	38.810586	75.714894
176.260032	39.751955	75.719898
176.325530	38.293914	75.724903
175.931164	39.137415	75.729908
174.942371	37.707126	75.734913
174.200986	48.744121	75.739918
173.086646	38.966593	75.744922
173.106210	38.028382	75.749927
172.335682	43.897652	75.754932
171.243636	38.602973	75.759937
171.007075	28.559340	75.764942
170.403160	44.726281	75.769946
169.823997	34.497575	75.774951
168.671659	42.878291	75.779956
168.020182	42.318309	75.784961
167.747218	36.869378	75.789966
166.930556	46.079661	75.794970
166.612006	29.530022	75.799975
165.631345	45.485801	75.804980
165.428076	34.351920	75.809985
164.417318	41.651935	75.814990
163.141332	36.407090	75.819994
162.841171	33.944494	75.824999
162.429606	32.538867	75.830004
162.016076	34.110818	75.835009
160.961631	34.875068	75.840014
160.277414	42.044170	75.845018
160.193572	28.808111	75.850023
158.708609	33.152856	75.855028
157.810751	40.903221	75.860033
157.356324	31.695414	75.865038
156.623083	34.237701	75.870042
156.511989	31.465842	75.875047
156.017480	37.362064	75.880052
155.316019	41.096184	75.885057
154.468831	39.939789	75.890062
153.721392	39.352536	75.895066
153.398022	25.222702	75.900071
151.926003	35.967766	75.905076
151.279589	36.493495	75.910081
150.760561	27.772229	75.915086
150.129208	38.783792	75.920090
150.214758	32.825117	75.925095
149.240707	35.244956	75.930100
148.320255	40.326012	75.935105
148.187561	29.594043	75.940110
147.282691	45.608704	75.945114
146.248853	32.588781	75.950119
145.500524	42.051520	75.955124
145.192107	42.294698	75.960129
144.943960	32.610881	75.965134
143.425845	34.412584	75.970138
143.363565	26.755465	75.975143
142.270005	37.678305	75.980148
142.081699	29.825239	75.985153
141.327188	33.891092	75.990158
139.920504	42.031680	75.995162
139.990747	32.125208	76.000167
139.324629	40.395286	76.005172
138.804682	38.068664	76.010177
137.652405	33.195190	76.015182
136.686564	36.878432	76.020186
136.622108	32.523773	76.025191
136.085155	35.017419	76.030196
135.414414	34.290209	76.035201
134.485768	37.133319	76.040206
133.756617	41.065823	76.045210
133.514521	33.345912	76.050215
132.838745	35.334998	76.055220
131.743747	35.001868	76.060225
131.418165	32.937566	76.065230
130.489759	37.925279	76.070234
130.139187	28.104837	76.075239
129.083889	39.172968	76.080244
128.598167	36.839314	76.085249
127.992329	31.544398	76.090254
127.395429	43.537637	76.095258
126.928120	26.880849	76.100263
125.974905	41.143353	76.105268
125.317549	44.873602	76.110273
125.069830	38.299447	76.115278
123.737413	37.743985	76.120282
123.298068	34.221809	76.125287
122.528256	45.602386	76.130292
122.269712	36.942087	76.135297
121.556963	43.250007	76.140302
120.320871	43.527581	76.145306
120.327988	45.409350	76.150311
119.563547	43.744612	76.155316
118.266741	33.704482	76.160321
117.964877	32.743413	76.165326
117.240613	38.039195	76.170330
116.921749	40.644723	76.175335
116.190212	36.008514	76.180340
115.311200	39.059757	76.185345
114.688135	38.996726	76.190350
114.132332	44.292455	76.195354
113.737623	38.534944	76.200359
112.685303	37.885936	76.205364
112.074787	38.555760	76.210369
111.771992	27.929772	76.215374
110.690210	38.655204	76.220378
110.179050	36.748232	76.225383
109.491722	39.157055	76.230388
109.336770	47.416589	76.235393
108.334787	34.661263	76.240398
107.015716	36.328745	76.245402
106.594627	26.189976	76.250407
106.129634	41.888490	76.255412
105.398367	36.932123	76.260417
104.828035	33.478148	76.265422
104.220287	42.336586	76.270426
103.624762	37.610883	76.275431
103.033261	42.819266	76.280436
101.963458	35.501014	76.285441
101.385669	34.738490	76.290446
100.754038	42.821728	76.295450
100.286154	33.343272	76.300455
100.052349	40.276555	76.305460
98.668861	33.650145	76.310465
98.091131	36.517729	76.315470
97.787539	29.615028	76.320474
97.259817	30.684809	76.325479
95.811637	45.688574	76.330484
95.261362	36.562299	76.335489
94.928472	22.284195	76.340494
94.537433	32.008500	76.345498
93.924773	38.518079	76.350503
92.974891	43.152842	76.355508
91.997651	33.776119	76.360513
91.926790	37.926924	76.365518
91.227640	33.734988	76.370522
90.333417	31.728263	76.375527
89.670481	33.082959	76.380532
88.744153	27.962168	76.385537
88.189005	33.661490	76.390542
87.261519	36.472892	76.395546
86.774028	40.750065	76.400551
86.325733	38.646993	76.405556
86.094325	39.519712	76.410561
85.517908	36.782643	76.415566
84.182307	40.416065	76.420570
83.885634	44.033608	76.425575
83.303068	37.066588	76.430580
81.945534	33.288736	76.435585
81.439109	31.768943	76.440590
80.514980	34.496234	76.445594
80.717115	25.630017	76.450599
80.405250	33.786835	76.455604
79.035858	36.927335	76.460609
78.442514	32.765837	76.465614
77.625439	45.885441	76.470618
77.160695	34.238196	76.475623
76.118311	41.158510	76.480628
75.420252	34.206760	76.485633
75.392429	37.256304	76.490638
74.662483	31.787233	76.495642
73.904303	33.357394	76.500647
73.115129	35.058654	76.505652
72.370751	39.149719	76.510657
72.312003	27.428269	76.515662
70.695548	38.967533	76.520666
70.397070	35.504903	76.525671
69.801672	33.280218	76.530676
69.098252	36.967362	76.535681
68.948392	30.185227	76.540686
67.697501	41.295610	76.545690
67.100896	31.058686	76.550695
66.482866	32.336841	76.555700
66.180870	35.450612	76.560705
65.460401	32.954141	76.565710
64.242015	34.302815	76.570714
63.861310	29.736829	76.575719
63.354934	36.872853	76.580724
62.441086	36.537671	76.585729
61.874502	36.311106	76.590734
61.053952	35.128420	76.595738
60.567456	33.111871	76.600743
60.419156	35.072041	76.605748
58.984598	37.431321	76.610753
58.614124	35.872503	76.615758
58.083599	35.261722	76.620762
57.280430	34.893120	76.625767
56.370288	40.097139	76.630772
55.858021	40.182031	76.635777
55.512724	31.297468	76.640782
54.653928	37.595577	76.645786
54.023252	33.473157	76.650791
53.190728	39.415420	76.655796
52.587659	40.303265	76.660801
52.153208	37.117789	76.665806
51.384051	38.260780	76.670810
50.456958	40.863977	76.675815
50.024381	36.080762	76.680820
49.305067	40.593610	76.685825
49.086971	38.646217	76.690830
47.663255	40.781426	76.695834
47.281510	28.004485	76.700839
46.694179	29.733482	76.705844
45.843718	41.973751	76.710849
45.844960	42.891367	76.715854
44.521175	37.846601	76.720858
44.172608	33.963037	76.725863
43.682470	27.700377	76.730868
42.860443	35.087020	76.735873
42.124788	39.771207	76.740878
41.323978	28.579701	76.745882
40.835271	32.488069	76.750887
40.290717	45.846484	76.755892
39.223127	34.708564	76.760897
38.553522	30.532434	76.765902
37.879216	47.038617	76.770906
37.558371	34.449077	76.775911
37.066453	42.010152	76.780916
35.946783	34.654157	76.785921
35.257755	29.126536	76.790926
34.736303	37.089708	76.795930
34.645114	27.726232	76.800935
33.935982	37.882899	76.805940
33.035073	34.265631	76.810945
32.573393	34.235227	76.815950
31.507399	42.950726	76.820954
31.100354	29.149659	76.825959
30.555215	40.989573	76.830964
29.375261	35.109752	76.835969
28.411204	45.896862	76.840974
27.732784	44.070203	76.845978
27.470094	43.206974	76.850983
27.220967	36.581023	76.855988
26.352597	47.802300	76.860993
25.355370	32.488466	76.865998
24.601570	37.703827	76.871002
24.394295	36.672490	76.876007
24.323898	41.405110	76.881012
23.109723	39.406867	76.886017
22.513409	33.962231	76.891022
21.301510	38.397538	76.896026
20.974067	35.866776	76.901031
19.943382	40.506567	76.906036
19.374211	51.866204	76.911041
19.162258	41.918015	76.916046
18.610807	51.073417	76.921050
17.904807	39.365323	76.926055
17.030095	40.574047	76.931060
16.543441	41.504832	76.936065
15.852565	40.161129	76.941070
14.634704	42.634103	76.946074
14.180857	34.526947	76.951079
13.372853	44.347736	76.956084
12.871910	44.773026	76.961089
12.857025	33.166009	76.966094
11.609249	42.812520	76.971098
10.746877	40.171546	76.976103
10.106472	41.248281	76.981108
9.914114	39.825061	76.986113
9.665888	47.900777	76.991118
8.449238	54.782687	76.996122
7.897064	49.085005	77.001127
7.175351	46.487826	77.006132
5.862728	36.201132	77.011137
5.841910	42.207896	77.016142
4.573657	36.167132	77.021147
4.492721	42.099907	77.026151
4.419203	39.255833	77.031156
3.249117	45.878003	77.036161