Fri Mar 05 20:23:19 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.550369	82.360818	0.000000
-0.154844	83.523055	0.005005
-0.939358	60.060326	0.010010
-2.918918	28.585019	0.015014
-6.870468	13.081706	0.020019
-12.496954	9.748279	0.025024
-17.324903	4.265864	0.030029
-21.944228	10.663921	0.035034
-25.490411	2.733090	0.040038
-29.152077	12.234773	0.045043
-32.940609	10.845888	0.050048
-36.647389	5.243016	0.055053
-40.859316	21.149695	0.060058
-44.278566	17.516287	0.065062
-47.853020	6.516553	0.070067
-51.799495	12.444637	0.075072
-55.033429	15.439503	0.080077
-59.227372	18.522864	0.085082
-62.972135	14.925643	0.090086
-66.559823	21.044096	0.095091
-70.370548	10.558320	0.100096
-74.371862	8.222593	0.105101
-78.333611	17.548296	0.110106
-81.765356	17.066075	0.115110
-85.515958	12.194082	0.120115
-89.571531	16.416043	0.125120
-92.886768	11.001525	0.130125
-97.094702	14.927688	0.135130
-100.309819	7.084499	0.140134
-104.504953	6.747758	0.145139
-108.339459	15.476048	0.150144
-111.552230	14.340775	0.155149
-115.997584	8.319707	0.160154
-119.456801	11.538255	0.165158
-123.195262	15.738060	0.170163
-127.128683	11.426729	0.175168
-130.525210	14.886023	0.180173
-134.597677	17.242087	0.185178
-137.831887	5.238895	0.190182
-142.062681	5.339989	0.195187
-146.249672	2.048428	0.200192
-149.773974	5.379902	0.205197
-153.723490	16.804242	0.210202
-157.207634	11.281150	0.215206
-160.888899	11.657285	0.220211
-164.944765	12.424356	0.225216
-168.453068	3.342850	0.230221
-172.373088	13.988236	0.235226
-175.782628	9.385235	0.240230
-179.528918	8.161727	0.245235
-183.294441	9.167922	0.250240
-187.080494	5.758837	0.255245
-191.234380	12.295817	0.260250
-194.663383	14.541412	0.265254
-198.704388	11.583032	0.270259
-202.517893	7.374116	0.275264
-205.786215	12.665947	0.280269
-209.632100	8.618326	0.285274
-213.626089	8.929332	0.290278
-217.327260	11.087508	0.295283
-221.219242	4.812752	0.300288
-224.726655	10.177457	0.305293
-228.829138	15.654484	0.310298
-231.951456	6.129856	0.315302
-236.085871	12.357878	0.320307
-239.691792	11.367525	0.325312
-243.592896	7.612620	0.330317
-247.698439	10.004112	0.335322
-251.279348	3.572528	0.340326
-254.873905	8.129602	0.345331
-258.520830	6.094009	0.350336
-262.081229	4.697461	0.355341
-266.084542	10.470951	0.360346
-269.883542	8.137954	0.365350
-273.874199	6.160403	0.370355
-277.726894	8.057431	0.375360
-281.258392	10.381007	0.380365
-285.097482	9.204015	0.385370
-288.823375	11.279515	0.390374
-292.325931	7.085766	0.395379
-296.410318	6.766374	0.400384
-300.088079	6.475121	0.405389
-304.004766	19.203301	0.410394
-307.642286	9.895055	0.415398
-311.297244	9.948680	0.420403
-315.249645	15.830817	0.425408
-318.834845	5.161235	0.430413
-322.624578	18.135677	0.435418
-326.154254	14.602309	0.440422
-330.186105	6.333171	0.445427
-334.201552	6.583148	0.450432
-337.405272	11.107911	0.455437
-341.563264	5.213287	0.460442
-345.319885	2.189260	0.465446
-348.981418	17.478703	0.470451
-352.848008	17.949371	0.475456
-356.329833	13.191020	0.480461
-360.521559	13.849224	0.485466
-363.995705	13.740023	0.490470
-367.500062	6.706627	0.495475
-371.629087	7.517263	0.500480
-375.160843	7.901393	0.505485
-379.437394	15.125311	0.510490
-382.978583	10.463211	0.515494
-386.472922	14.819975	0.520499
-390.265447	9.171434	0.525504
-394.146687	2.966218	0.530509
-398.204082	9.537018	0.535514
-401.322984	-0.296990	0.540518
-405.256981	8.821356	0.545523
-409.307196	6.262195	0.550528
-413.014723	7.948604	0.555533
-416.799887	9.507069	0.560538
-420.441129	8.118935	0.565542
-424.132090	7.290671	0.570547
-428.162591	16.276235	0.575552
-431.709410	8.628407	0.580557
-435.857595	12.055182	0.585562
-439.545256	0.744581	0.590566
-442.622199	1.286416	0.595571
-447.084971	7.858951	0.600576
-450.031824	8.044137	0.605581
-454.175994	13.633846	0.610586
-458.113192	9.128138	0.615590
-461.751071	9.295958	0.620595
-465.646306	11.543848	0.625600
-469.470625	19.479436	0.630605
-473.534990	10.673279	0.635610
-477.024445	8.830492	0.640614
-480.584163	6.775007	0.645619
-484.454033	19.320941	0.650624
-487.644157	3.887718	0.655629
-491.714692	2.833178	0.660634
-495.568273	12.066554	0.665638
-499.483852	3.700304	0.670643
-503.607462	14.880169	0.675648
-507.062905	6.910366	0.680653
-511.009270	12.571078	0.685658
-514.541079	4.000060	0.690662
-518.068499	1.198320	0.695667
-521.880134	10.647382	0.700672
-525.703657	0.229088	0.705677
-529.659515	7.627539	0.710682
-533.511498	7.542665	0.715686
-537.211644	4.604541	0.720691
-541.155406	10.156077	0.725696
-544.152313	-1.412910	0.730701
-548.426819	9.840011	0.735706
-551.956402	8.022667	0.740710
-555.636593	7.546119	0.745715
-559.639026	3.451544	0.750720
-563.276379	2.198626	0.755725
-567.024102	10.054314	0.760730
-571.072532	3.797258	0.765734
-574.861460	15.537201	0.770739
-578.732606	12.159686	0.775744
-582.186336	9.521309	0.780749
-586.205828	4.295696	0.785754
-589.809657	11.027740	0.790758
-593.642293	12.537297	0.795763
-597.267009	9.522563	0.800768
-600.634639	9.647423	0.805773
-604.947352	15.358926	0.810778
-608.403452	6.328114	0.815782
-612.400881	14.282109	0.820787
-616.273417	12.251573	0.825792
-619.812127	16.013372	0.830797
-623.393321	19.293117	0.835802
-627.367841	14.080888	0.840806
-630.943788	3.594835	0.845811
-635.089922	17.178589	0.850816
-638.699023	9.425922	0.855821
-642.559052	10.477894	0.860826
-646.213287	0.307146	0.865830
-649.804407	8.693014	0.870835
-653.675901	14.130685	0.875840
-657.495533	6.145186	0.880845
-660.942117	8.111977	0.885850
-665.172081	4.268401	0.890854
-668.904664	7.115091	0.895859
-672.646300	6.676927	0.900864
-676.186558	2.852478	0.905869
-679.964706	11.473273	0.910874
-683.719588	4.622321	0.915878
-687.492359	9.104423	0.920883
-691.461792	10.194456	0.925888
-694.955194	-0.107564	0.930893
-699.118472	10.678413	0.935898
-702.686740	12.395055	0.940902
-706.064278	1.035345	0.945907
-709.849904	8.823187	0.950912
-713.741099	2.706837	0.955917
-717.624932	3.994542	0.960922
-721.024940	2.763864	0.965926
-725.068798	5.438037	0.970931
-729.284047	9.431106	0.975936
-732.702908	0.468656	0.980941
-736.497738	9.902738	0.985946
-740.166278	8.271885	0.990950
-743.878962	6.296439	0.995955
-747.880754	5.125701	1.000960
-751.557659	3.182396	1.005965
-755.499970	9.035235	1.010970
-759.081961	3.271662	1.015974
-762.568639	-0.971216	1.020979
-766.448899	4.475915	1.025984
-769.943324	-8.552311	1.030989
-773.851336	-3.594312	1.035994
-778.031753	-3.421297	1.040998
-781.702661	1.549283	1.046003
-785.550098	10.802617	1.051008
-789.093007	4.655960	1.056013
-793.058159	2.758791	1.061018
-796.911839	10.961335	1.066022
-800.110539	7.932443	1.071027
-804.254779	12.141370	1.076032
-807.575208	1.559574	1.081037
-811.739763	12.420057	1.086042
-815.819907	5.797928	1.091046
-818.899678	-2.830664	1.096051
-822.994248	4.177270	1.101056
-826.737776	9.690950	1.106061
-830.497908	14.811485	1.111066
-834.386318	0.193719	1.116070
-837.858831	-1.611813	1.121075
-841.694527	18.099443	1.126080
-845.348403	6.128120	1.131085
-849.073887	3.648697	1.136090
-853.291098	8.178448	1.141094
-857.113862	0.419294	1.146099
-861.026190	1.227674	1.151104
-864.370865	1.450163	1.156109
-867.873462	8.508617	1.161114
-871.565753	6.910153	1.166118
-875.306756	0.943531	1.171123
-879.853024	10.870112	1.176128
-883.147836	7.271665	1.181133
-887.065198	10.788464	1.186138
-890.781522	3.603694	1.191142
-894.232213	7.758664	1.196147
-898.066302	7.993215	1.201152
-901.773789	1.363703	1.206157
-905.771085	9.378069	1.211162
-909.413277	13.060641	1.216166
-913.035170	0.828863	1.221171
-917.230114	7.834080	1.226176
-920.850817	11.264081	1.231181
-924.613731	13.756481	1.236186
-928.211294	8.132856	1.241190
-931.872447	6.029626	1.246195
-935.919115	7.075648	1.251200
-939.671032	-0.308347	1.256205
-943.060437	4.729428	1.261210
-946.951082	-1.328262	1.266214
-950.539811	-2.258776	1.271219
-954.792844	4.099795	1.276224
-958.778481	0.616652	1.281229
-962.432954	5.617993	1.286234
-965.965896	3.991044	1.291238
-969.501467	0.380761	1.296243
-973.383569	7.058511	1.301248
-976.643869	1.286421	1.306253
-980.940784	8.180323	1.311258
-984.709715	4.116957	1.316262
-988.340965	-0.488800	1.321267
-992.201620	7.574814	1.326272
-996.083956	0.974997	1.331277
-1000.058828	7.587203	1.336282
-1003.598207	5.060922	1.341286
-1007.263600	12.650223	1.346291
-1010.934378	6.546441	1.351296
-1014.231840	4.736831	1.356301
-1018.764525	2.758927	1.361306
-1022.695572	11.280116	1.366310
-1026.174433	-4.968672	1.371315
-1029.920023	4.081092	1.376320
-1033.758460	2.387991	1.381325
-1037.478012	4.105676	1.386330
-1041.220150	10.871534	1.391334
-1044.586054	11.266405	1.396339
-1048.772781	17.237657	1.401344
-1052.477420	1.911244	1.406349
-1056.102843	4.842320	1.411354
-1059.987326	8.108143	1.416358
-1063.521383	13.479877	1.421363
-1067.842403	13.655396	1.426368
-1070.868353	1.103065	1.431373
-1074.916834	3.004304	1.436378
-1078.954907	1.551363	1.441382
-1082.411773	9.298226	1.446387
-1086.318378	13.081706	1.451392
-1089.864488	12.160358	1.456397
-1093.601883	10.400732	1.461402
-1097.558947	8.069138	1.466406
-1101.190073	4.477497	1.471411
-1105.307277	15.441277	1.476416
-1109.019210	12.442877	1.481421
-1112.296317	14.178212	1.486426
-1116.205071	6.723408	1.491430
-1119.921809	6.602090	1.496435
-1123.802726	9.854832	1.501440
-1127.707172	8.625021	1.506445
-1131.540732	8.891407	1.511450
-1135.694714	4.997120	1.516454
-1138.957410	-3.067181	1.521459
-1142.553047	4.875424	1.526464
-1146.154802	6.364705	1.531469
-1150.273780	11.226183	1.536474
-1154.203353	11.440160	1.541478
-1157.818727	9.637463	1.546483
-1161.749803	5.154065	1.551488
-1165.097480	1.078797	1.556493
-1168.860959	3.114368	1.561498
-1172.862631	5.979665	1.566502
-1176.358826	-5.857044	1.571507
-1180.381149	15.223346	1.576512
-1184.155672	1.710760	1.581517
-1188.006561	1.511669	1.586522
-1191.807232	4.762720	1.591526
-1195.142455	0.113084	1.596531
-1198.989797	10.917146	1.601536
-1202.651459	6.709248	1.606541
-1206.322219	3.020041	1.611546
-1210.436951	4.405425	1.616550
-1214.089654	-1.886987	1.621555
-1218.252725	9.645696	1.626560
-1221.852172	-4.976594	1.631565
-1225.232123	4.415494	1.636570
-1229.121728	1.295916	1.641574
-1232.983990	-0.350463	1.646579
-1237.036743	7.302739	1.651584
-1240.212126	-4.608857	1.656589
-1244.444520	0.977385	1.661594
-1248.466092	5.877058	1.666598
-1251.760166	-5.159264	1.671603
-1255.585394	5.248691	1.676608
-1259.135058	-1.427556	1.681613
-1262.607158	-2.226444	1.686618
-1266.431752	-2.044846	1.691622
-1270.180751	2.134746	1.696627
-1274.732578	5.162375	1.701632
-1278.284161	3.428506	1.706637
-1281.727640	0.325929	1.711642
-1285.839968	1.785175	1.716646
-1289.418874	0.443617	1.721651
-1293.211487	9.518654	1.726656
-1297.172001	2.332647	1.731661
-1300.709934	2.832689	1.736666
-1304.401581	5.826781	1.741670
-1307.973616	0.970794	1.746675
-1312.015480	6.744277	1.751680
-1315.415529	-2.217117	1.756685
-1319.298084	1.605470	1.761690
-1323.134603	-0.716641	1.766694
-1326.691052	-8.867678	1.771699
-1331.035043	6.762576	1.776704
-1334.541655	-4.605442	1.781709
-1338.253809	-1.969128	1.786714
-1342.172107	2.198254	1.791718
-1346.143936	3.513696	1.796723
-1349.501090	10.221558	1.801728
-1353.004433	8.093740	1.806733
-1356.972904	9.716160	1.811738
-1360.815055	7.910663	1.816742
-1364.496943	3.662114	1.821747
-1368.697642	8.988046	1.826752
-1372.216949	-7.157492	1.831757
-1375.921699	0.574268	1.836762
-1379.744285	6.577683	1.841766
-1383.340743	-3.140617	1.846771
-1387.105688	2.423086	1.851776
-1391.163988	4.028406	1.856781
-1394.474083	7.076673	1.861786
-1398.428206	10.884042	1.866790
-1402.086156	9.820234	1.871795
-1406.068134	12.313778	1.876800
-1409.519848	5.043363	1.881805
-1413.643450	0.651153	1.886810
-1417.516151	2.663609	1.891814
-1420.735230	-5.609096	1.896819
-1424.787738	3.491980	1.901824
-1428.598148	-0.611309	1.906829
-1431.981049	3.347504	1.911834
-1435.970814	3.234137	1.916838
-1439.481573	-1.063762	1.921843
-1443.862557	9.483928	1.926848
-1447.607495	0.883881	1.931853
-1451.187925	2.728175	1.936858
-1455.214699	13.315366	1.941862
-1458.348732	6.803116	1.946867
-1462.427777	9.214530	1.951872
-1466.156445	4.825409	1.956877
-1470.205317	5.763903	1.961882
-1473.827295	2.097282	1.966886
-1477.271387	-0.492402	1.971891
-1481.279699	12.625965	1.976896
-1484.742025	5.082986	1.981901
-1488.438971	9.669317	1.986906
-1492.182825	11.192924	1.991910
-1496.069801	4.403918	1.996915
-1500.535325	6.435648	2.006912
-1501.253562	3.915509	2.016909
-1498.434696	5.673109	2.026906
-1495.446186	9.040896	2.036902
-1493.437012	8.439771	2.046899
-1491.780711	2.253646	2.056896
-1490.123335	6.666688	2.066893
-1488.088458	11.158231	2.076890
-1486.120255	11.829973	2.086886
-1483.971684	10.034970	2.096883
-1481.989333	5.225571	2.106880
-1480.512179	12.119555	2.116877
-1478.494261	10.830209	2.126874
-1476.522301	6.038267	2.136870
-1474.294515	-2.089856	2.146867
-1472.770191	6.661291	2.156864
-1471.227181	6.644822	2.166861
-1469.234010	11.360952	2.176858
-1466.749650	5.035938	2.186854
-1465.055849	9.657902	2.196851
-1463.347560	9.439713	2.206848
-1461.548286	8.032235	2.216845
-1459.554355	11.830895	2.226842
-1457.557463	1.432940	2.236838
-1455.710112	6.605055	2.246835
-1453.988980	4.201159	2.256832
-1451.779348	3.444818	2.266829
-1450.004611	5.304921	2.276826
-1448.555139	5.912910	2.286822
-1446.481729	6.727313	2.296819
-1444.204008	3.053270	2.306816
-1442.464780	3.973287	2.316813
-1440.812764	6.516196	2.326810
-1438.708503	13.246649	2.336806
-1436.783506	8.568046	2.346803
-1435.031558	9.894974	2.356800
-1433.042069	11.302293	2.366797
-1431.301509	10.437916	2.376794
-1429.468054	7.965528	2.386790
-1427.722840	13.547175	2.396787
-1425.489241	13.786484	2.406784
-1423.589999	6.947302	2.416781
-1422.069253	6.192334	2.426778
-1420.122074	8.560110	2.436774
-1417.698556	11.688461	2.446771
-1416.168484	16.436151	2.456768
-1414.464919	21.943955	2.466765
-1412.574746	18.115671	2.476762
-1410.279745	7.496339	2.486758
-1408.902814	16.193770	2.496755
-1406.538378	13.972704	2.506752
-1405.242619	11.471154	2.516749
-1403.164300	9.594315	2.526746
-1400.932265	12.863864	2.536742
-1399.340885	10.466568	2.546739
-1397.779030	7.676110	2.556736
-1395.561432	6.113293	2.566733
-1393.417900	10.639634	2.576730
-1391.603593	3.840917	2.586726
-1390.007911	10.971777	2.596723
-1388.012464	8.094546	2.606720
-1386.296499	8.820963	2.616717
-1384.079977	15.298240	2.626714
-1382.568428	10.892704	2.636710
-1380.600042	-0.853771	2.646707
-1378.664670	8.171117	2.656704
-1376.822563	12.063630	2.666701
-1374.780336	4.544762	2.676698
-1373.036466	4.770939	2.686694
-1371.127516	3.953861	2.696691
-1369.252625	15.718413	2.706688
-1367.546862	10.315492	2.716685
-1365.519314	15.498316	2.726682
-1363.464346	14.591555	2.736678
-1361.676100	11.303833	2.746675
-1359.862657	13.830437	2.756672
-1358.164733	18.055517	2.766669
-1356.110470	11.073150	2.776666
-1354.375241	15.015948	2.786662
-1352.252404	9.228911	2.796659
-1350.368469	10.160572	2.806656
-1348.543941	10.790694	2.816653
-1346.944043	16.027779	2.826650
-1345.044845	18.374882	2.836646
-1342.948078	18.137230	2.846643
-1341.041988	16.237487	2.856640
-1339.047458	14.704112	2.866637
-1337.105594	14.863889	2.876634
-1335.404962	13.008089	2.886630
-1334.025398	11.636309	2.896627
-1331.892948	13.785037	2.906624
-1329.683142	6.247276	2.916621
-1327.970812	8.801142	2.926618
-1325.998975	8.989287	2.936614
-1324.000283	3.953192	2.946611
-1322.304749	10.089186	2.956608
-1320.684498	13.084108	2.966605
-1318.855329	9.775657	2.976602
-1316.433876	6.776617	2.986598
-1314.557269	8.629996	2.996595
-1312.919084	9.029448	3.006592
-1311.202724	9.485862	3.016589
-1309.258926	6.143283	3.026586
-1307.255683	8.047453	3.036582
-1305.453862	11.049640	3.046579
-1303.625246	10.134949	3.056576
-1301.525203	9.641024	3.066573
-1299.687190	12.896369	3.076570
-1297.963962	5.663878	3.086566
-1296.120263	7.712011	3.096563
-1294.185350	13.296565	3.106560
-1292.253447	16.157946	3.116557
-1290.423087	5.560979	3.126554
-1288.415929	8.094532	3.136550
-1286.385785	18.604330	3.146547
-1284.994699	12.803409	3.156544
-1283.176680	10.068343	3.166541
-1281.154803	14.907946	3.176538
-1279.073348	10.158637	3.186534
-1277.101030	15.663011	3.196531
-1275.284552	11.770840	3.206528
-1273.353232	14.731803	3.216525
-1271.756995	14.744844	3.226522
-1269.703797	7.836928	3.236518
-1267.845456	10.318527	3.246515
-1265.941230	9.297030	3.256512
-1264.227060	14.039051	3.266509
-1262.348442	3.025437	3.276506
-1260.449917	3.435369	3.286502
-1258.485998	9.888460	3.296499
-1256.668134	7.965010	3.306496
-1254.771274	3.695260	3.316493
-1252.555498	11.146990	3.326490
-1251.111955	8.298192	3.336486
-1248.873496	10.805819	3.346483
-1247.392900	12.979993	3.356480
-1245.442890	16.373776	3.366477
-1243.544123	13.136348	3.376474
-1241.384992	6.503607	3.386470
-1239.822243	8.985162	3.396467
-1237.840782	13.787062	3.406464
-1235.979025	11.802920	3.416461
-1234.189897	16.024555	3.426458
-1232.200420	12.480518	3.436454
-1230.342396	13.833263	3.446451
-1228.477555	15.898596	3.456448
-1226.889745	16.094593	3.466445
-1224.668363	17.014992	3.476442
-1222.673802	12.105952	3.486438
-1220.854328	13.412768	3.496435
-1219.058503	12.699177	3.506432
-1217.219194	15.810701	3.516429
-1215.549492	11.926271	3.526426
-1213.397679	14.659375	3.536422
-1211.225309	15.636577	3.546419
-1209.642116	14.598599	3.556416
-1208.245000	11.937252	3.566413
-1206.112589	10.028247	3.576410
-1203.889838	14.316311	3.586406
-1202.243130	11.308719	3.596403
-1200.402147	14.699460	3.606400
-1198.196502	15.718718	3.616397
-1196.566534	13.736957	3.626394
-1194.607130	8.975669	3.636390
-1192.919171	9.665661	3.646387
-1190.963632	8.399174	3.656384
-1188.880276	6.681189	3.666381
-1187.283690	12.668915	3.676378
-1185.204908	10.637457	3.686374
-1183.550756	15.057569	3.696371
-1181.703060	12.355725	3.706368
-1179.751350	11.039334	3.716365
-1177.751766	3.257449	3.726362
-1175.848876	7.533559	3.736358
-1174.073167	13.811581	3.746355
-1172.037278	14.736445	3.756352
-1170.236737	14.039506	3.766349
-1168.579491	14.068120	3.776346
-1166.565449	10.322840	3.786342
-1164.300307	13.797327	3.796339
-1162.842605	21.585175	3.806336
-1161.039638	17.411040	3.816333
-1159.109619	16.424975	3.826330
-1157.155898	12.588302	3.836326
-1155.004225	19.481978	3.846323
-1153.505297	20.000137	3.856320
-1151.628121	14.871514	3.866317
-1149.584440	10.650984	3.876314
-1147.596473	10.181443	3.886310
-1145.773844	14.454632	3.896307
-1144.182354	14.312205	3.906304
-1142.281345	17.309710	3.916301
-1140.340434	18.597164	3.926298
-1138.358379	12.627568	3.936294
-1136.227847	11.675760	3.946291
-1134.673458	11.665590	3.956288
-1132.758053	12.636606	3.966285
-1131.011138	14.531412	3.976282
-1129.110174	10.557939	3.986278
-1127.117913	12.628235	3.996275
-1125.140032	10.848232	4.006272
-1123.487217	12.364943	4.016269
-1121.528278	17.353709	4.026266
-1119.410503	16.583955	4.036262
-1117.586649	9.828112	4.046259
-1115.981438	16.341877	4.056256
-1114.167375	14.709667	4.066253
-1111.866976	13.887022	4.076250
-1110.091308	10.574655	4.086246
-1108.539216	10.860130	4.096243
-1106.765282	13.914308	4.106240
-1104.772303	20.321845	4.116237
-1102.652600	12.160801	4.126234
-1101.022767	19.580108	4.136230
-1098.630663	8.631306	4.146227
-1097.282363	21.831921	4.156224
-1095.181775	15.904976	4.166221
-1093.342056	14.999725	4.176218
-1091.375491	16.477325	4.186214
-1089.593657	11.596103	4.196211
-1087.795713	6.813359	4.206208
-1085.781402	13.162235	4.216205
-1084.275478	10.434608	4.226202
-1082.040122	6.199266	4.236198
-1080.338652	13.155551	4.246195
-1078.047609	7.856576	4.256192
-1076.371312	12.653749	4.266189
-1074.548034	15.044803	4.276186
-1072.637054	5.736128	4.286182
-1071.004145	12.749176	4.296179
-1068.881561	12.084488	4.306176
-1066.963172	11.258252	4.316173
-1065.330275	11.057151	4.326170
-1063.309057	14.823385	4.336166
-1061.644049	8.872983	4.346163
-1059.463706	11.491145	4.356160
-1057.796663	15.996133	4.366157
-1055.825947	12.016296	4.376154
-1054.090082	7.775606	4.386150
-1051.987904	7.859454	4.396147
-1050.302923	11.035271	4.406144
-1048.345651	9.241260	4.416141
-1046.175431	16.528390	4.426138
-1044.714931	9.895448	4.436134
-1042.729472	14.482151	4.446131
-1040.746165	15.031860	4.456128
-1038.781799	12.504096	4.466125
-1037.017512	15.735134	4.476122
-1035.224405	14.507385	4.486118
-1033.082370	13.427516	4.496115
-1031.423544	11.318094	4.506112
-1029.904609	18.002039	4.516109
-1027.739900	16.976968	4.526106
-1025.814922	8.327662	4.536102
-1023.941232	11.328056	4.546099
-1021.954942	11.473097	4.556096
-1020.225225	11.123912	4.566093
-1018.052326	12.628576	4.576090
-1016.481820	12.420119	4.586086
-1014.617249	7.408878	4.596083
-1012.567678	6.159079	4.606080
-1010.953255	6.845174	4.616077
-1008.642827	10.789414	4.626074
-1007.003113	7.511496	4.636070
-1005.427387	6.943792	4.646067
-1003.481839	9.263243	4.656064
-1001.240050	17.012654	4.666061
-999.481968	12.067400	4.676058
-997.773258	17.071030	4.686054
-995.681227	11.893954	4.696051
-993.915216	3.620619	4.706048
-991.907690	13.929061	4.716045
-990.330091	8.357417	4.726042
-988.252667	8.352124	4.736038
-986.261137	8.745829	4.746035
-984.608278	14.148397	4.756032
-982.754762	9.446840	4.766029
-980.598502	13.861023	4.776026
-979.067532	11.798925	4.786022
-976.977611	13.954787	4.796019
-975.076462	9.499827	4.806016
-973.285966	9.868848	4.816013
-971.466646	16.814273	4.826010
-969.545569	14.129277	4.836006
-967.483133	12.852196	4.846003
-965.679717	12.177058	4.856000
-964.002793	20.713146	4.865997
-962.158484	16.939911	4.875994
-959.949472	12.988362	4.885990
-958.268870	13.614965	4.895987
-956.121840	10.593852	4.905984
-954.512567	17.711824	4.915981
-952.924716	12.001195	4.925978
-950.808257	10.115495	4.935974
-948.812212	11.899554	4.945971
-947.007196	11.647330	4.955968
-945.141819	8.170739	4.965965
-943.187400	11.911446	4.975962
-941.191079	4.881838	4.985958
-939.533072	5.818381	4.995955
-937.745894	4.618496	5.005952
-935.825895	12.907316	5.015949
-933.434811	4.500919	5.025946
-932.066344	9.405843	5.035942
-930.163102	7.686883	5.045939
-928.205007	14.780680	5.055936
-926.455328	15.506787	5.065933
-924.546371	13.832706	5.075930
-922.669613	10.756942	5.085926
-920.731444	11.460811	5.095923
-918.847593	18.550700	5.105920
-916.947009	12.581672	5.115917
-915.048316	8.294518	5.125914
-913.306631	5.477198	5.135910
-911.124595	9.364697	5.145907
-909.350000	15.576803	5.155904
-907.970598	9.203217	5.165901
-905.769463	8.796115	5.175898
-903.526467	7.510749	5.185894
-901.642613	6.402802	5.195891
-900.481568	8.738818	5.205888
-898.490106	12.527326	5.215885
-896.172211	15.584705	5.225882
-894.369856	7.008783	5.235878
-892.655934	11.144823	5.245875
-890.678271	10.290307	5.255872
-888.825281	12.114657	5.265869
-887.150920	12.581257	5.275866
-884.850521	5.694131	5.285862
-883.150653	8.034014	5.295859
-881.255999	9.395396	5.305856
-879.510379	9.888504	5.315853
-877.525724	9.776562	5.325850
-875.352599	1.127171	5.335846
-873.837466	2.901334	5.345843
-872.265205	6.387407	5.355840
-870.229272	7.189373	5.365837
-868.122627	1.402180	5.375834
-866.305325	9.991687	5.385830
-864.282153	5.758884	5.395827
-862.642424	11.379958	5.405824
-860.621231	15.135327	5.415821
-858.608223	15.405708	5.425818
-857.013628	4.947770	5.435814
-855.088983	10.482251	5.445811
-853.216508	6.851438	5.455808
-851.241895	10.311104	5.465805
-849.362615	9.938136	5.475802
-847.960757	10.964639	5.485798
-845.456846	6.925001	5.495795
-843.617229	9.160470	5.505792
-842.212653	7.388661	5.515789
-840.022555	4.570766	5.525786
-837.913991	1.527486	5.535782
-836.128880	5.598505	5.545779
-834.557898	4.366941	5.555776
-832.852731	5.813914	5.565773
-830.417194	-2.072125	5.575770
-828.541365	5.696484	5.585766
-826.781696	6.828435	5.595763
-824.965840	6.236679	5.605760
-823.364657	4.815558	5.615757
-821.693024	9.479463	5.625754
-819.753051	3.625792	5.635750
-817.092997	0.475432	5.645747
-815.489274	0.257062	5.655744
-813.904565	4.355394	5.665741
-811.965735	7.768709	5.675738
-809.951639	1.412148	5.685734
-808.155760	-1.660073	5.695731
-806.482217	2.861431	5.705728
-804.585793	3.253123	5.715725
-802.252698	5.466591	5.725722
-800.334324	8.256346	5.735718
-798.861443	4.261551	5.745715
-797.044409	3.707522	5.755712
-795.211475	2.399378	5.765709
-793.294942	3.231547	5.775706
-791.104496	8.502549	5.785702
-789.313767	6.272738	5.795699
-787.304947	4.764384	5.805696
-785.771389	5.948295	5.815693
-783.813737	6.012851	5.825690
-781.495483	5.525567	5.835686
-780.032142	4.047559	5.845683
-778.321723	-0.143082	5.855680
-776.272624	-3.549433	5.865677
-774.053910	-2.648703	5.875674
-772.493177	2.980325	5.885670
-770.716346	0.119595	5.895667
-769.251230	-0.183959	5.905664
-766.826672	5.475963	5.915661
-765.005500	6.692868	5.925658
-762.952349	-3.757771	5.935654
-760.835710	0.044008	5.945651
-759.160697	2.043747	5.955648
-757.386460	5.843410	5.965645
-755.877332	0.418643	5.975642
-753.886432	-2.589969	5.985638
-751.792920	4.583394	5.995635
-749.916347	3.146732	6.005632
-748.143993	-1.047470	6.015629
-746.260712	-0.299948	6.025626
-744.453624	-3.066021	6.035622
-742.562771	4.692367	6.045619
-740.479778	5.998502	6.055616
-738.823858	9.108145	6.065613
-736.912648	-0.355060	6.075610
-735.033673	5.936819	6.085606
-732.893474	1.728053	6.095603
-731.360120	1.745195	6.105600
-729.383376	4.805154	6.115597
-727.284168	2.723461	6.125594
-725.627541	6.245103	6.135590
-723.530527	-4.689355	6.145587
-721.798136	-1.776659	6.155584
-720.053739	0.159915	6.165581
-718.004531	-2.011674	6.175578
-716.397761	2.380043	6.185574
-714.305313	-1.412130	6.195571
-712.309904	6.894839	6.205568
-710.556779	9.298972	6.215565
-708.659478	6.813770	6.225562
-706.824399	5.382193	6.235558
-704.961248	3.180346	6.245555
-702.908508	2.154516	6.255552
-701.217255	4.001702	6.265549
-699.538077	5.768715	6.275546
-697.525667	7.071956	6.285542
-695.181781	-1.680359	6.295539
-693.878737	3.100958	6.305536
-691.631516	4.679314	6.315533
-690.079989	9.810930	6.325530
-688.313381	3.288747	6.335526
-686.239302	4.695828	6.345523
-684.300731	-2.093826	6.355520
-682.330752	4.941449	6.365517
-680.579446	5.806427	6.375514
-678.445211	-1.505538	6.385510
-676.844395	-4.532285	6.395507
-674.906189	6.627532	6.405504
-673.180728	9.980321	6.415501
-671.159837	13.781697	6.425498
-669.159895	13.774855	6.435494
-667.591527	7.301727	6.445491
-665.241835	1.617973	6.455488
-663.646524	3.496305	6.465485
-661.837752	-1.303653	6.475482
-659.996530	2.463279	6.485478
-658.042584	-0.021459	6.495475
-656.430740	-2.189433	6.505472
-654.102599	-1.923438	6.515469
-652.344085	-1.579063	6.525466
-650.660734	-2.719514	6.535462
-648.595959	-1.036177	6.545459
-646.703669	9.126797	6.555456
-644.882627	3.281208	6.565453
-642.891149	11.800451	6.575450
-641.258194	13.536997	6.585446
-639.295621	9.457740	6.595443
-637.606016	7.692616	6.605440
-635.761674	13.393278	6.615437
-633.647348	11.574511	6.625434
-631.530455	4.691667	6.635430
-629.858665	9.197798	6.645427
-628.090598	13.982233	6.655424
-625.957213	10.489906	6.665421
-624.434142	13.268754	6.675418
-622.377288	10.394971	6.685414
-620.352525	8.301578	6.695411
-618.657635	13.637710	6.705408
-616.962130	11.936394	6.715405
-614.868270	8.433024	6.725402
-612.768103	5.249173	6.735398
-611.038135	-0.659210	6.745395
-609.575933	8.644088	6.755392
-607.595854	7.011002	6.765389
-605.366891	7.813940	6.775386
-603.565500	6.826769	6.785382
-601.718209	7.564368	6.795379
-599.851130	6.609337	6.805376
-597.821993	16.842079	6.815373
-596.339966	11.072783	6.825370
-594.258961	2.984653	6.835366
-592.268933	8.737866	6.845363
-590.221176	10.591342	6.855360
-588.824266	8.633009	6.865357
-586.837732	12.436791	6.875354
-584.829649	13.115560	6.885350
-583.159098	8.127734	6.895347
-581.135946	14.313035	6.905344
-579.054309	10.547963	6.915341
-577.286974	6.435206	6.925338
-575.563783	9.051066	6.935334
-573.450001	5.854021	6.945331
-571.831844	5.535616	6.955328
-569.913664	7.651386	6.965325
-568.074012	8.402863	6.975322
-566.011089	7.509733	6.985318
-564.068275	-0.540508	6.995315
-562.415615	4.781884	7.005312
-560.613425	5.940402	7.015309
-558.341397	9.055975	7.025306
-556.763684	3.958261	7.035302
-555.206801	7.105962	7.045299
-552.864023	5.141829	7.055296
-551.082752	5.023172	7.065293
-548.916229	1.149832	7.075290
-547.308736	11.307862	7.085286
-545.544203	3.489792	7.095283
-543.640089	2.931521	7.105280
-541.800659	4.579894	7.115277
-540.015926	4.361219	7.125274
-537.732389	4.097612	7.135270
-535.828987	7.248400	7.145267
-534.144139	8.580418	7.155264
-532.380712	13.766723	7.165261
-530.408916	5.571348	7.175258
-528.626488	7.850940	7.185254
-526.968280	9.135113	7.195251
-524.826427	11.294144	7.205248
-523.019393	13.274549	7.215245
-520.962782	15.652462	7.225242
-519.065000	15.398378	7.235238
-517.362491	17.337061	7.245235
-515.344202	10.320058	7.255232
-513.672648	3.928436	7.265229
-511.754953	14.221690	7.275226
-509.488614	11.268754	7.285222
-508.142094	5.852730	7.295219
-505.967357	11.505468	7.305216
-504.155586	9.161978	7.315213
-502.420886	8.097113	7.325210
-500.534091	10.150059	7.335206
-498.453642	10.132082	7.345203
-496.807032	9.903920	7.355200
-494.773654	11.232409	7.365197
-492.878911	8.785676	7.375194
-490.918010	13.079951	7.385190
-489.103629	15.703420	7.395187
-487.308831	16.075282	7.405184
-485.332802	11.097154	7.415181
-483.494180	11.528335	7.425178
-481.521704	7.104989	7.435174
-479.845330	8.815767	7.445171
-477.918561	12.261295	7.455168
-476.190545	10.786989	7.465165
-474.343592	9.854217	7.475162
-472.381217	14.795641	7.485158
-470.252341	8.469960	7.495155
-468.479389	9.139008	7.505152
-466.719962	13.126005	7.515149
-464.729412	13.665571	7.525146
-462.610416	12.660944	7.535142
-461.097239	14.882534	7.545139
-459.271211	9.091539	7.555136
-457.098741	7.118378	7.565133
-455.361184	18.653083	7.575130
-453.623867	18.292045	7.585126
-451.405955	10.316371	7.595123
-449.848603	13.429335	7.605120
-447.946373	15.378807	7.615117
-446.123614	14.817815	7.625114
-444.238513	12.061606	7.635110
-442.302167	10.399321	7.645107
-440.363614	10.356684	7.655104
-438.482126	15.658423	7.665101
-436.424476	19.706772	7.675098
-434.830083	16.155411	7.685094
-433.042575	12.715321	7.695091
-430.832885	11.574660	7.705088
-429.227835	15.346338	7.715085
-427.365030	11.074755	7.725082
-425.397488	15.405922	7.735078
-423.134044	12.955632	7.745075
-421.545260	11.999387	7.755072
-420.083498	15.359740	7.765069
-417.991889	20.048473	7.775066
-416.007285	18.419555	7.785062
-413.997021	16.085489	7.795059
-412.123729	13.470137	7.805056
-410.357864	18.690889	7.815053
-408.494766	16.841378	7.825050
-406.826551	16.341407	7.835046
-404.620059	12.106543	7.845043
-402.696536	19.689497	7.855040
-400.973467	21.062878	7.865037
-399.033381	19.622661	7.875034
-396.929560	19.847356	7.885030
-395.431273	17.487681	7.895027
-393.701273	18.343644	7.905024
-391.733182	18.920016	7.915021
-389.686963	26.638131	7.925018
-387.687033	18.428888	7.935014
-385.835560	12.535986	7.945011
-384.085563	20.192451	7.955008
-382.196276	23.514573	7.965005
-380.452989	14.346838	7.975002
-378.137202	16.189287	7.984998
-376.746947	17.903190	7.994995
-374.795278	12.987457	8.004992
-372.750709	13.764792	8.014989
-370.811653	10.824761	8.024986
-369.062650	14.139288	8.034982
-367.424436	10.640975	8.044979
-365.574662	11.446257	8.054976
-363.710324	8.679214	8.064973
-361.553737	14.712361	8.074970
-359.708186	8.506213	8.084966
-357.713222	13.431482	8.094963
-355.588706	14.065015	8.104960
-354.204006	9.792446	8.114957
-352.396758	8.864526	8.124954
-350.263246	16.917686	8.134950
-348.515595	12.850860	8.144947
-346.571864	18.134845	8.154944
-344.474080	15.243705	8.164941
-342.767374	14.263949	8.174938
-341.294396	15.497298	8.184934
-339.270795	11.915373	8.194931
-336.968411	17.936323	8.204928
-335.303542	17.729041	8.214925
-333.526714	22.673367	8.224922
-331.335998	19.590560	8.234918
-329.559255	16.131734	8.244915
-328.023853	17.773548	8.254912
-326.040900	17.011810	8.264909
-324.068764	12.992849	8.274906
-322.104218	10.672472	8.284902
-320.089244	5.838256	8.294899
-318.194740	8.804331	8.304896
-316.636099	8.669282	8.314893
-314.848739	12.809833	8.324890
-313.081028	8.600883	8.334886
-310.840473	6.833299	8.344883
-308.623056	10.639941	8.354880
-307.300682	7.997348	8.364877
-305.574828	13.199304	8.374874
-303.308154	4.057025	8.384870
-301.357058	9.043029	8.394867
-299.755944	10.098054	8.404864
-297.786479	13.183234	8.414861
-295.797404	17.376866	8.424858
-294.157260	16.027241	8.434854
-292.183155	14.670100	8.444851
-290.357977	16.182000	8.454848
-288.112787	26.443719	8.464845
-286.751827	19.816019	8.474842
-284.804718	21.366883	8.484838
-282.720104	15.296312	8.494835
-280.834005	19.501658	8.504832
-278.914165	20.640035	8.514829
-277.300610	24.189413	8.524826
-275.213937	17.641675	8.534822
-273.495583	12.682733	8.544819
-271.414756	15.083844	8.554816
-269.578575	13.901893	8.564813
-267.948433	15.887046	8.574810
-265.850412	8.375928	8.584807
-263.810743	11.753089	8.594803
-262.100507	11.931775	8.604800
-260.035909	10.871270	8.614797
-258.546119	7.736191	8.624794
-256.654552	12.799631	8.634791
-254.466304	5.539386	8.644787
-252.876796	2.876291	8.654784
-250.908848	6.858594	8.664781
-248.757021	-0.492147	8.674778
-246.941264	1.425499	8.684775
-245.283159	5.799891	8.694771
-243.412837	0.237243	8.704768
-241.694555	7.098352	8.714765
-239.761433	3.753581	8.724762
-237.511627	8.328808	8.734759
-235.887633	5.450219	8.744755
-234.035458	7.878380	8.754752
-231.771814	0.257175	8.764749
-230.240431	-0.138731	8.774746
-228.170044	-1.826975	8.784743
-226.424682	-3.671767	8.794739
-224.657245	-6.904818	8.804736
-222.981138	-3.516971	8.814733
-220.859835	-0.883857	8.824730
-219.011242	-2.561960	8.834727
-217.090620	-3.709978	8.844723
-215.148762	-4.965594	8.854720
-213.330477	1.213259	8.864717
-211.192957	-6.940429	8.874714
-209.730886	-2.967362	8.884711
-207.860512	3.239499	8.894707
-205.398515	-4.896494	8.904704
-204.427998	-0.104450	8.914701
-202.325856	6.142799	8.924698
-200.189012	2.978706	8.934695
-198.222946	-2.548661	8.944691
-196.311473	0.766909	8.954688
-194.582326	-2.977907	8.964685
-192.769950	2.725063	8.974682
-190.794117	-1.417539	8.984679
-188.956806	-6.311718	8.994675
-187.094071	0.826379	9.004672
-185.327821	0.186179	9.014669
-183.332695	-8.380553	9.024666
-181.416793	-4.056730	9.034663
-179.401927	1.912360	9.044659
-177.830619	-0.147782	9.054656
-176.092814	-1.860280	9.064653
-174.168837	-5.915645	9.074650
-172.220886	-0.663768	9.084647
-169.986321	2.870268	9.094643
-168.221014	-2.157671	9.104640
-166.550664	-2.517291	9.114637
-164.461552	-2.724257	9.124634
-162.902136	-1.286696	9.134631
-160.790684	0.481202	9.144627
-158.927659	-2.078635	9.154624
-157.347103	-4.228661	9.164621
-154.881218	1.649537	9.174618
-153.145442	-1.461572	9.184615
-151.289320	-3.259247	9.194611
-149.690905	-2.753165	9.204608
-148.052995	-1.670751	9.214605
-145.986298	-5.679394	9.224602
-143.794838	-8.878994	9.234599
-141.941982	-9.226665	9.244595
-139.911637	-11.009498	9.254592
-138.372797	-5.073368	9.264589
-136.364825	1.241071	9.274586
-134.779135	2.811828	9.284583
-132.491720	-2.517288	9.294579
-130.652359	0.565105	9.304576
-129.068219	-0.342840	9.314573
-126.984689	1.405858	9.324570
-125.362136	2.760739	9.334567
-123.291915	1.342609	9.344563
-121.381502	0.507349	9.354560
-119.616767	-5.140994	9.364557
-117.676411	2.973202	9.374554
-115.870615	-3.179060	9.384551
-114.138669	0.283643	9.394547
-111.836010	6.911091	9.404544
-109.939194	1.037995	9.414541
-108.323561	3.331889	9.424538
-106.462005	6.579710	9.434535
-104.583019	3.182100	9.444531
-102.626235	2.765773	9.454528
-100.680435	3.008043	9.464525
-99.068607	6.305185	9.474522
-97.012867	7.722028	9.484519
-94.957920	-4.405249	9.494515
-93.328540	5.691219	9.504512
-91.665051	1.127997	9.514509
-90.046586	6.863567	9.524506
-87.439301	1.368194	9.534503
-85.579696	3.083180	9.544499
-83.919334	3.402580	9.554496
-81.922614	2.122528	9.564493
-79.983126	1.290555	9.574490
-78.461121	4.196251	9.584487
-76.418524	6.279947	9.594483
-74.589802	1.998270	9.604480
-72.541315	5.113664	9.614477
-70.825688	0.864244	9.624474
-68.886770	2.373957	9.634471
-67.177637	-0.597053	9.644467
-65.205147	0.686255	9.654464
-63.257953	3.345709	9.664461
-61.305911	6.102287	9.674458
-59.360190	2.447749	9.684455
-57.724577	2.531115	9.694451
-55.500806	0.674861	9.704448
-54.102593	0.410836	9.714445
-51.986224	2.282258	9.724442
-50.119173	5.799248	9.734439
-48.382483	2.140167	9.744435
-46.388994	5.329095	9.754432
-44.409102	0.797535	9.764429
-42.480225	-1.630615	9.774426
-40.816331	0.319310	9.784423
-39.039889	0.749699	9.794419
-37.010848	4.555071	9.804416
-35.116749	6.878807	9.814413
-33.410500	-2.167531	9.824410
-31.373616	-0.248676	9.834407
-29.296791	5.344350	9.844403
-27.405684	6.200143	9.854400
-26.057781	2.429409	9.864397
-23.638389	5.965684	9.874394
-21.829994	3.972033	9.884391
-20.178770	3.304510	9.894387
-18.138674	5.598656	9.904384
-16.380120	2.750850	9.914381
-14.382686	6.856548	9.924378
-12.734282	3.198942	9.934375
-10.839129	6.915167	9.944371
-8.833202	1.980005	9.954368
-6.924495	4.983542	9.964365
-5.283570	11.563492	9.974362
-3.854703	29.806280	9.984359
-2.487011	61.802110	9.994355
-1.010179	104.883879	10.004352
0.000000	154.246801	10.009357
1.118037	175.838334	10.014362
1.359151	213.807690	10.019367
1.904293	226.099897	10.024371
2.585613	240.311633	10.029376
2.553266	255.181265	10.034381
2.936535	255.208482	10.039386
3.315654	268.918088	10.044391
3.559536	269.431164	10.049395
3.379657	265.083820	10.054400
3.063378	269.015210	10.059405
3.551858	269.825166	10.064410
3.693153	285.297919	10.069415
3.606113	275.831129	10.074419
3.597062	267.725440	10.079424
3.146852	276.193041	10.084429
3.477609	279.388870	10.089434
3.628122	293.216963	10.094439
3.876445	301.787631	10.099443
4.103135	298.775776	10.104448
3.467463	301.135419	10.109453
3.828341	295.661018	10.114458
4.039646	307.334755	10.119463
3.873360	308.268071	10.124467
4.047782	306.819442	10.129472
4.011556	314.011500	10.134477
3.954764	311.699299	10.139482
4.076211	319.045986	10.144487
4.276258	321.901547	10.149491
4.541320	317.434333	10.154496
4.123457	307.692278	10.159501
4.053435	295.852578	10.164506
4.037615	321.416208	10.169511
4.340150	329.175568	10.174515
4.744564	321.819195	10.179520
4.459882	329.624907	10.184525
4.573409	331.721554	10.189530
4.555531	339.454754	10.194535
4.738466	333.734326	10.199539
4.742549	332.837994	10.204544
4.367146	335.160861	10.209549
4.975222	330.982712	10.214554
4.886620	339.900458	10.219559
4.543645	331.288170	10.224563
4.938603	335.795273	10.229568
4.844939	340.060186	10.234573
4.774765	339.539978	10.239578
4.902670	355.587382	10.244583
5.113368	355.859746	10.249587
5.079936	350.192747	10.254592
4.831441	359.851953	10.259597
4.958251	352.913585	10.264602
5.054435	359.106823	10.269607
5.110873	361.445973	10.274611
5.282573	360.426709	10.279616
5.233256	364.041151	10.284621
5.234278	355.459138	10.289626
5.184841	353.093717	10.294631
5.225394	353.623458	10.299635
5.328019	357.451787	10.304640
5.538817	364.967174	10.309645
5.675148	354.695142	10.314650
5.517705	361.942828	10.319655
5.551693	367.489970	10.324659
5.549935	358.192452	10.329664
5.815291	371.767335	10.334669
5.664568	368.833009	10.339674
6.011527	389.387198	10.344679
5.680838	389.264936	10.349683
6.253465	384.587794	10.354688
5.772860	389.805430	10.359693
5.787897	382.168929	10.364698
5.626296	387.091252	10.369703
5.654674	387.585088	10.374707
6.140102	385.638985	10.379712
6.049602	393.733885	10.384717
6.125355	393.917385	10.389722
6.048590	400.918831	10.394727
6.119922	395.477958	10.399731
6.201045	396.151042	10.404736
6.258399	415.586074	10.409741
6.456765	414.832216	10.414746
6.596133	424.603069	10.419751
6.461308	425.922466	10.424755
6.511250	422.084054	10.429760
6.661673	424.964897	10.434765
6.816284	432.590208	10.439770
6.851537	431.291499	10.444775
6.908214	427.108229	10.449779
6.905566	421.623952	10.454784
6.818948	425.069315	10.459789
6.944256	425.337954	10.464794
7.026200	432.161133	10.469799
6.859139	439.192769	10.474803
7.131193	432.764216	10.479808
6.644686	432.132210	10.484813
7.125585	432.126510	10.489818
7.372834	439.869515	10.494823
7.366908	438.118472	10.499827
7.140262	439.313741	10.504832
7.171742	448.661840	10.509837
7.330617	443.665889	10.514842
7.754660	439.852961	10.519847
7.429999	446.610110	10.524851
7.345663	434.274253	10.529856
7.433558	453.031093	10.534861
7.525576	440.894189	10.539866
7.026072	441.467492	10.544871
7.056870	440.759284	10.549875
7.641834	442.042726	10.554880
7.198387	448.869286	10.559885
7.681093	454.753330	10.564890
7.638283	471.919364	10.569895
7.775047	477.013330	10.574899
7.700930	476.304507	10.579904
7.688764	485.240113	10.584909
7.915941	485.197609	10.589914
7.923247	483.114860	10.594919
7.645561	480.311150	10.599923
7.982244	478.242100	10.604928
7.950711	485.715775	10.609933
8.050359	480.502172	10.614938
8.224502	486.878577	10.619943
8.010084	494.189034	10.624947
8.571122	494.761923	10.629952
8.398396	498.050722	10.634957
8.182420	495.399597	10.639962
8.588056	500.994748	10.644967
8.607568	514.922797	10.649971
8.916268	504.731979	10.654976
8.403409	504.583576	10.659981
8.536099	504.761151	10.664986
8.721761	513.401864	10.669991
8.645543	520.803835	10.674995
8.875210	519.455186	10.680000
8.713529	524.492688	10.685005
8.877218	522.064861	10.690010
8.967686	522.135627	10.695015
8.860062	524.135109	10.700019
9.284176	515.291549	10.705024
9.195722	522.749090	10.710029
9.424984	524.480369	10.715034
9.175763	513.047551	10.720039
9.071079	510.591566	10.725043
9.392029	511.417220	10.730048
9.044842	511.633486	10.735053
9.297399	518.733853	10.740058
9.390068	529.026324	10.745063
9.101764	532.447108	10.750067
9.469425	525.345661	10.755072
9.192845	529.486836	10.760077
9.438987	532.752990	10.765082
9.514779	530.414876	10.770087
9.371633	523.388594	10.775091
9.469745	524.200904	10.780096
9.372399	534.041126	10.785101
9.699856	527.472806	10.790106
9.228494	529.757390	10.795111
9.331361	534.456227	10.800115
9.937267	544.690504	10.805120
9.629778	559.926039	10.810125
9.972300	562.572838	10.815130
10.207357	553.060801	10.820135
10.015511	563.135318	10.825139
10.338769	556.771086	10.830144
10.220317	559.153932	10.835149
10.306728	557.979520	10.840154
10.371588	554.955576	10.845159
9.611138	563.947500	10.850163
10.275050	556.537005	10.855168
10.262857	570.443356	10.860173
10.048457	569.094565	10.865178
10.233955	558.270483	10.870183
10.034829	554.728811	10.875187
10.592558	560.329690	10.880192
10.251729	564.462199	10.885197
10.519847	575.100467	10.890202
10.999750	590.178907	10.895207
10.738363	584.850958	10.900211
10.946755	563.987211	10.905216
10.565879	568.414698	10.910221
10.874452	579.371378	10.915226
10.611369	576.614207	10.920231
11.264638	587.801353	10.925235
11.329816	590.457699	10.930240
10.842924	575.596497	10.935245
11.195244	565.868624	10.940250
10.945385	576.345075	10.945255
11.042556	595.838654	10.950259
11.738431	585.604950	10.955264
11.042398	577.083520	10.960269
11.173615	577.031089	10.965274
11.327622	590.508817	10.970279
11.144525	593.485468	10.975283
11.554513	596.198786	10.980288
11.360076	600.337919	10.985293
11.537281	597.152541	10.990298
11.557823	600.893099	10.995303
11.240220	606.801559	11.000307
11.493595	602.810012	11.005312
11.599581	599.090351	11.010317
11.385604	603.259410	11.015322
11.278735	601.645875	11.020327
11.304260	615.089712	11.025331
11.624455	609.673723	11.030336
11.505126	620.779111	11.035341
12.277572	632.551274	11.040346
12.445585	629.739528	11.045351
12.048770	615.179319	11.050355
12.069156	601.904860	11.055360
12.206423	611.172323	11.060365
11.974535	620.296027	11.065370
11.952105	625.066919	11.070375
12.063609	626.541016	11.075379
12.298311	621.269551	11.080384
12.303715	625.766336	11.085389
12.413468	627.429953	11.090394
12.778219	634.608680	11.095399
12.380986	635.468462	11.100403
12.667883	627.517226	11.105408
12.647044	633.574701	11.110413
12.833780	633.202746	11.115418
12.700608	633.239795	11.120423
12.553839	636.625412	11.125427
12.763188	620.476672	11.130432
12.576644	622.512409	11.135437
12.527804	625.398265	11.140442
12.560284	628.304269	11.145447
12.609426	639.237716	11.150451
12.703881	635.737511	11.155456
12.465396	631.441983	11.160461
12.832269	635.406440	11.165466
12.835518	640.703115	11.170471
12.889134	655.948967	11.175475
13.216451	650.837767	11.180480
13.368613	659.722039	11.185485
13.499971	660.691485	11.190490
13.732936	645.732744	11.195495
13.135664	642.828582	11.200499
13.204682	635.970263	11.205504
13.072836	648.785562	11.210509
13.836125	653.497379	11.215514
13.489184	657.020587	11.220519
13.303386	661.620422	11.225523
13.940297	656.947136	11.230528
13.714864	667.377177	11.235533
13.571548	664.296524	11.240538
13.996169	664.567893	11.245543
13.786235	661.373283	11.250547
13.727370	659.731585	11.255552
13.755765	663.898275	11.260557
13.695008	665.123875	11.265562
13.812340	660.233827	11.270567
13.848614	670.948570	11.275571
14.227122	662.219433	11.280576
13.948410	660.950278	11.285581
13.945688	667.899040	11.290586
14.216137	660.229540	11.295591
14.060090	666.579839	11.300595
14.314565	667.091242	11.305600
13.977842	667.454079	11.310605
13.800106	670.929802	11.315610
14.143383	666.287576	11.320615
14.105565	680.816306	11.325619
14.806317	680.471180	11.330624
14.668613	687.372092	11.335629
14.734926	692.007423	11.340634
15.022004	678.861463	11.345639
14.711424	671.650494	11.350643
14.683598	666.111791	11.355648
14.498206	660.235510	11.360653
14.939927	661.713715	11.365658
14.888664	669.502880	11.370663
14.618723	679.588355	11.375667
15.038568	678.474297	11.380672
15.009057	685.345335	11.385677
15.191600	690.099327	11.390682
15.156997	689.899873	11.395687
14.790610	683.446878	11.400691
15.237695	689.120651	11.405696
15.173545	701.647647	11.410701
15.179722	697.579591	11.415706
15.270197	696.413981	11.420711
14.851464	695.332742	11.425715
15.157629	696.398894	11.430720
15.176532	703.856752	11.435725
15.103097	700.875337	11.440730
15.175830	694.551003	11.445735
15.372968	691.980614	11.450739
15.682289	693.196078	11.455744
15.630910	701.160326	11.460749
15.667497	699.077606	11.465754
15.816817	695.018260	11.470759
15.808962	706.049161	11.475763
15.871131	700.943962	11.480768
15.847412	695.343089	11.485773
15.708743	696.309873	11.490778
15.745217	695.630711	11.495783
15.919138	710.985170	11.500787
16.296463	718.844781	11.505792
15.783409	717.717080	11.510797
15.997156	733.114098	11.515802
16.459764	725.134785	11.520807
16.208265	731.919821	11.525811
16.503982	724.173715	11.530816
16.065750	708.265363	11.535821
16.205308	720.230009	11.540826
16.517550	718.256291	11.545831
16.178171	723.866273	11.550835
16.404928	724.483028	11.555840
16.412939	731.190403	11.560845
16.366464	729.259704	11.565850
16.608885	729.556981	11.570855
16.281762	732.618135	11.575859
16.621412	731.016950	11.580864
16.810006	734.000582	11.585869
16.505635	734.629507	11.590874
16.640550	724.053076	11.595879
16.596498	735.703230	11.600883
16.506468	733.218060	11.605888
16.424707	741.619278	11.610893
16.727841	754.677543	11.615898
17.213161	754.188574	11.620903
17.131816	758.260826	11.625907
17.150836	749.522739	11.630912
17.222375	754.868490	11.635917
17.353946	757.985805	11.640922
17.427262	753.244678	11.645927
17.302859	763.403197	11.650931
17.365149	749.488747	11.655936
17.433526	759.625978	11.660941
17.539269	751.350317	11.665946
18.123453	750.189541	11.670951
17.432032	732.164188	11.675955
17.378584	721.080040	11.680960
17.417564	725.230867	11.685965
17.530820	738.846124	11.690970
17.577405	748.726616	11.695975
17.798950	751.082075	11.700979
17.817826	748.721464	11.705984
17.926827	755.228232	11.710989
17.705827	747.840504	11.715994
18.214084	748.344551	11.720999
17.973535	754.555395	11.726003
18.051486	755.115457	11.731008
17.844989	756.563014	11.736013
17.840153	749.462520	11.741018
17.925985	749.172891	11.746023
17.873308	755.405812	11.751027
18.209641	753.907661	11.756032
18.166310	754.605343	11.761037
17.550077	754.520732	11.766042
18.152327	754.331671	11.771047
17.683022	770.706608	11.776051
18.247484	778.478054	11.781056
18.431765	788.000707	11.786061
18.477060	787.512529	11.791066
18.750697	789.813953	11.796071
18.366860	791.299259	11.801075
18.944518	781.546342	11.806080
18.792177	793.365208	11.811085
18.460713	791.904173	11.816090
18.888854	791.794923	11.821095
18.644181	795.625142	11.826099
18.639775	784.176717	11.831104
18.524271	790.708269	11.836109
18.688070	795.525212	11.841114
18.816308	783.978358	11.846119
18.902364	793.209160	11.851123
19.014620	788.624244	11.856128
19.166824	797.453399	11.861133
19.568002	806.159267	11.866138
19.535681	787.710163	11.871143
19.109773	792.550193	11.876147
19.168582	783.911399	11.881152
19.235467	780.289396	11.886157
19.510736	801.070080	11.891162
19.601541	799.409225	11.896167
19.549113	801.567105	11.901171
19.351177	788.807499	11.906176
19.311624	791.174644	11.911181
19.612671	802.476486	11.916186
20.003093	805.297049	11.921191
19.877075	808.040703	11.926195
19.603783	799.773426	11.931200
19.815900	793.002600	11.936205
19.892195	805.933082	11.941210
20.626686	797.647003	11.946215
19.736990	796.569904	11.951219
19.711650	787.261679	11.956224
19.967303	787.238290	11.961229
19.711186	788.687455	11.966234
20.423204	793.498965	11.971239
20.401959	791.543733	11.976243
20.245132	789.204830	11.981248
19.982840	782.755689	11.986253
20.104736	788.213275	11.991258
20.731136	800.746918	11.996263
20.320827	806.593758	12.001267
20.178948	792.699214	12.006272
20.451372	799.307675	12.011277
20.223445	801.176565	12.016282
20.493978	800.792818	12.021287
20.372656	811.207933	12.026291
20.578969	800.908654	12.031296
20.335316	813.048042	12.036301
20.369365	808.650642	12.041306
20.672199	811.086190	12.046311
20.660832	818.810722	12.051315
20.483041	789.080720	12.056320
20.300688	784.750959	12.061325
20.042694	787.810561	12.066330
20.551498	797.357157	12.071335
20.320347	807.807134	12.076339
20.576693	810.433032	12.081344
20.464004	805.303643	12.086349
20.445801	813.526024	12.091354
20.519463	802.101405	12.096359
19.989511	803.136911	12.101363
20.229645	798.282426	12.106368
20.426608	810.777333	12.111373
20.657660	815.987274	12.116378
20.752992	809.933688	12.121383
20.336310	809.415108	12.126387
20.492324	793.989073	12.131392
20.395092	792.552183	12.136397
20.110674	790.049119	12.141402
20.658651	789.539117	12.146407
20.466461	817.366389	12.151411
20.356536	806.816332	12.156416
20.469477	793.800549	12.161421
20.452020	799.660426	12.166426
20.594030	786.968033	12.171431
20.301557	799.134119	12.176435
20.503617	787.883007	12.181440
20.809481	788.193823	12.186445
20.808986	788.072509	12.191450
20.960355	792.008302	12.196455
20.781447	796.012543	12.201459
20.753560	789.332040	12.206464
20.748347	785.267352	12.211469
20.527640	794.681130	12.216474
20.598994	780.591732	12.221479
20.397303	771.054590	12.226483
20.286221	759.793516	12.231488
20.599325	772.547421	12.236493
20.443403	760.211665	12.241498
20.507080	754.055913	12.246503
20.260600	766.782364	12.251507
20.151827	763.114261	12.256512
20.664240	769.659200	12.261517
20.551427	775.808677	12.266522
20.351541	761.070248	12.271527
20.544652	757.218375	12.276531
20.268900	756.372956	12.281536
20.436720	764.959894	12.286541
20.101127	769.749240	12.291546
20.639821	774.678278	12.296551
20.370778	775.990726	12.301555
20.469539	775.833081	12.306560
20.405750	771.788779	12.311565
20.352588	773.825341	12.316570
20.648590	775.520775	12.321575
20.599040	774.549387	12.326579
20.265034	767.074013	12.331584
20.441202	761.780293	12.336589
20.185174	772.951755	12.341594
20.323201	761.363932	12.346599
20.578378	780.548698	12.351603
20.445586	788.623753	12.356608
20.633853	776.091156	12.361613
20.299391	771.771466	12.366618
20.557360	767.007192	12.371623
20.571679	771.553065	12.376627
20.593792	769.220321	12.381632
20.642016	764.295527	12.386637
20.309122	763.762009	12.391642
20.580963	763.860622	12.396647
20.369274	771.935636	12.401651
20.427848	764.886524	12.406656
20.647966	764.480856	12.411661
20.272572	765.488554	12.416666
20.614324	764.415332	12.421671
20.422092	770.121716	12.426675
20.556658	765.009679	12.431680
20.484036	768.186374	12.436685
20.210255	770.518331	12.441690
20.424761	773.683926	12.446695
20.407709	766.607451	12.451699
20.400549	767.958558	12.456704
20.573530	778.585342	12.461709
20.385455	779.225682	12.466714
20.403943	773.758402	12.471719
20.471324	773.082192	12.476723
20.755805	776.212972	12.481728
20.704349	775.664530	12.486733
20.126820	787.166412	12.491738
20.723695	771.722128	12.496743
20.514083	769.256025	12.501747
20.609759	768.843394	12.506752
20.713834	769.260513	12.511757
20.517341	775.262481	12.516762
20.821040	755.436706	12.521767
20.386842	755.576961	12.526771
20.384765	745.530163	12.531776
20.487057	742.486018	12.536781
20.191343	753.402011	12.541786
20.212236	745.521523	12.546791
20.093561	753.159051	12.551795
19.931232	772.714760	12.556800
20.212479	780.744276	12.561805
19.762345	780.385581	12.566810
20.088906	783.839248	12.571815
20.076286	784.836398	12.576819
20.309904	775.067392	12.581824
20.361562	780.960395	12.586829
20.670438	792.726201	12.591834
20.811318	780.513408	12.596839
20.342820	784.560679	12.601843
20.490780	782.568999	12.606848
20.827589	782.824414	12.611853
20.398417	781.511433	12.616858
20.677866	782.406804	12.621863
20.668014	787.836515	12.626867
20.440663	777.740465	12.631872
20.753243	780.198109	12.636877
20.552278	778.186383	12.641882
20.725697	775.824774	12.646887
20.709602	784.551448	12.651891
20.335692	769.755606	12.656896
20.701327	764.537327	12.661901
20.301019	757.695454	12.666906
20.347897	746.183684	12.671911
20.307742	754.393762	12.676915
20.154799	773.284051	12.681920
20.430204	774.143795	12.686925
19.957629	776.975833	12.691930
20.384459	782.556677	12.696935
20.445222	785.746796	12.701939
20.616893	777.408563	12.706944
20.537922	776.648457	12.711949
20.242618	784.476606	12.716954
20.454149	774.897211	12.721959
20.460775	782.473767	12.726963
20.681659	782.138942	12.731968
21.171878	771.784941	12.736973
20.426868	768.382321	12.741978
20.524168	758.113075	12.746983
20.326325	751.372960	12.751987
20.420876	755.128563	12.756992
20.518254	749.672365	12.761997
20.338547	753.656221	12.767002
20.793421	747.557933	12.772007
20.626859	750.109338	12.777011
20.459514	751.383486	12.782016
20.457932	749.212225	12.787021
20.267634	755.687879	12.792026
20.687960	760.033370	12.797031
20.354377	760.543947	12.802035
20.336657	758.174978	12.807040
20.302396	757.455053	12.812045
20.163910	761.834476	12.817050
20.585733	747.891070	12.822055
20.631360	761.689031	12.827059
20.776260	763.102621	12.832064
20.484740	756.571418	12.837069
20.285599	762.887629	12.842074
20.421696	757.920436	12.847079
20.642003	754.764421	12.852083
20.508213	766.816859	12.857088
20.485359	759.903745	12.862093
20.508108	766.465277	12.867098
20.548861	758.072239	12.872103
20.488183	761.638127	12.877107
20.376759	769.380168	12.882112
20.584681	762.805575	12.887117
20.318363	769.850047	12.892122
20.406874	769.200430	12.897127
20.610516	762.948231	12.902131
20.318730	760.517313	12.907136
20.563686	764.379823	12.912141
20.317688	766.516529	12.917146
20.589066	758.689128	12.922151
20.609756	754.814291	12.927155
20.460513	761.936284	12.932160
20.602945	755.996638	12.937165
20.274426	752.532327	12.942170
20.384529	748.745736	12.947175
20.378917	752.679747	12.952179
20.348062	750.495808	12.957184
20.622855	762.142441	12.962189
20.384542	762.494314	12.967194
20.686976	750.746232	12.972199
20.335627	737.506493	12.977203
19.880065	752.765846	12.982208
20.360559	753.446217	12.987213
20.308904	763.058524	12.992218
20.892628	767.541967	12.997223
20.721529	762.180626	13.002227
20.185726	746.199480	13.007232
20.564002	748.939965	13.012237
20.293805	745.840106	13.017242
20.485407	736.878950	13.022247
20.458154	746.490509	13.027251
20.230224	745.899248	13.032256
20.397816	753.599933	13.037261
20.653246	753.915638	13.042266
20.594187	750.097677	13.047271
20.267602	738.773216	13.052275
20.347668	734.899954	13.057280
20.447323	735.852384	13.062285
20.228359	743.859154	13.067290
20.554618	755.166400	13.072295
20.740056	756.778536	13.077299
20.474047	746.100446	13.082304
20.518978	733.841492	13.087309
20.332049	736.445031	13.092314
20.335747	728.737612	13.097319
20.406788	733.608754	13.102323
20.469258	731.747414	13.107328
20.262651	730.890969	13.112333
19.968887	747.479166	13.117338
20.489276	748.097977	13.122343
20.568820	763.500663	13.127347
20.537399	760.941483	13.132352
20.648281	746.115655	13.137357
20.498885	743.609988	13.142362
20.541252	740.165377	13.147367
20.637671	742.324740	13.152371
20.561194	741.482233	13.157376
20.888515	733.929786	13.162381
20.793588	737.627292	13.167386
20.836876	736.484976	13.172391
20.689880	737.736953	13.177395
20.664477	735.918014	13.182400
20.434907	723.023156	13.187405
20.348525	718.703341	13.192410
20.598019	711.991248	13.197415
20.339702	709.378376	13.202419
20.212900	712.076403	13.207424
20.504089	721.063124	13.212429
20.308881	734.976745	13.217434
20.674620	735.762153	13.222439
20.214967	726.409691	13.227443
20.335950	730.785570	13.232448
20.789136	735.871740	13.237453
20.685624	731.625619	13.242458
20.458523	722.384309	13.247463
20.296861	721.210024	13.252467
20.280584	716.655093	13.257472
20.348307	711.765055	13.262477
20.551387	718.687326	13.267482
20.537916	712.346770	13.272487
20.333754	716.411790	13.277491
20.253865	712.114596	13.282496
20.274260	712.382627	13.287501
19.785853	715.789635	13.292506
20.426319	726.725034	13.297511
20.501641	737.433598	13.302515
20.255374	744.906962	13.307520
20.522726	739.483584	13.312525
20.380370	753.423487	13.317530
20.577148	742.781980	13.322535
20.662288	734.918061	13.327539
20.432517	740.813354	13.332544
20.846383	738.925932	13.337549
20.279048	730.051131	13.342554
20.384316	715.104800	13.347559
20.473913	723.901316	13.352563
20.282351	729.826782	13.357568
20.687259	724.258464	13.362573
20.043615	718.857385	13.367578
20.381883	727.991148	13.372583
20.826053	744.272405	13.377587
20.404034	738.284015	13.382592
20.219273	730.207669	13.387597
20.373415	731.173487	13.392602
20.267563	740.333936	13.397607
20.416786	733.964268	13.402611
20.262036	745.733015	13.407616
20.579022	748.907493	13.412621
20.540768	751.772762	13.417626
20.367500	747.231820	13.422631
20.432482	745.261264	13.427635
20.392830	751.476337	13.432640
20.712983	746.156504	13.437645
20.567459	741.481824	13.442650
20.355457	731.545791	13.447655
20.343527	729.032395	13.452659
20.063865	726.717825	13.457664
20.668462	736.545581	13.462669
20.348179	742.784907	13.467674
20.318952	739.365908	13.472679
20.438425	748.495155	13.477683
20.663588	751.536039	13.482688
20.247217	741.921188	13.487693
20.068977	738.753045	13.492698
20.483779	742.840782	13.497703
20.585487	756.703913	13.502707
20.464271	757.100191	13.507712
20.652494	755.723437	13.512717
20.648587	739.821474	13.517722
20.421655	731.556304	13.522727
20.294663	724.681894	13.527731
20.157890	719.072234	13.532736
20.584175	731.642465	13.537741
20.055352	734.663246	13.542746
20.395915	737.854462	13.547751
20.657351	745.090726	13.552755
20.433838	750.131860	13.557760
20.179268	743.072777	13.562765
20.507171	751.889652	13.567770
20.788183	749.184445	13.572775
20.392375	740.455752	13.577779
20.338208	725.528531	13.582784
20.547970	727.256637	13.587789
20.287096	734.680283	13.592794
20.078427	738.179880	13.597799
20.126051	739.094876	13.602803
20.220035	748.638212	13.607808
20.658620	743.804136	13.612813
20.103931	757.672607	13.617818
20.506726	756.536030	13.622823
20.493567	759.581809	13.627827
20.882326	755.067926	13.632832
20.866267	757.576404	13.637837
20.788624	756.037041	13.642842
20.776926	737.151032	13.647847
20.717910	733.268412	13.652851
20.333098	734.990420	13.657856
20.476049	727.032126	13.662861
20.370135	728.891008	13.667866
20.422311	727.838742	13.672871
20.090493	734.302263	13.677875
20.123554	741.261123	13.682880
20.454945	732.468494	13.687885
20.353708	739.565472	13.692890
20.298406	733.753571	13.697895
20.203621	738.468228	13.702899
20.213737	739.523253	13.707904
20.386473	741.894380	13.712909
20.589132	755.616825	13.717914
20.510079	745.121816	13.722919
20.580040	743.002226	13.727923
20.316454	743.441712	13.732928
20.605852	726.797520	13.737933
20.212965	738.290416	13.742938
20.528272	735.382615	13.747943
20.360650	733.379771	13.752947
20.140335	740.970423	13.757952
20.278159	735.849992	13.762957
20.504196	763.448024	13.767962
20.576453	757.849167	13.772967
20.509094	748.121874	13.777971
20.322982	744.556000	13.782976
20.603549	737.596081	13.787981
20.412067	738.470361	13.792986
20.391039	739.882027	13.797991
20.126135	739.854927	13.802995
20.326859	744.184974	13.808000
20.599636	747.795450	13.813005
20.542340	752.398473	13.818010
20.425069	744.352358	13.823015
20.113853	741.784188	13.828019
20.448147	750.776668	13.833024
20.656020	761.528767	13.838029
20.132702	752.511308	13.843034
20.419720	751.796914	13.848039
20.758850	755.928264	13.853043
20.143624	750.603068	13.858048
20.621683	756.205694	13.863053
20.518478	750.262649	13.868058
20.510343	743.230496	13.873063
20.550883	748.716812	13.878067
20.449036	741.948775	13.883072
20.409556	749.135260	13.888077
20.275803	745.111586	13.893082
20.417938	740.854669	13.898087
20.659450	735.145244	13.903091
20.054159	745.577576	13.908096
20.468317	737.083991	13.913101
20.168502	743.122926	13.918106
20.403519	749.718407	13.923111
20.560730	755.894198	13.928115
20.649679	764.441674	13.933120
20.651572	747.144695	13.938125
20.399067	745.584335	13.943130
20.379051	751.624381	13.948135
20.465524	746.669837	13.953139
20.761554	753.252435	13.958144
20.652958	744.386464	13.963149
20.491300	745.670743	13.968154
20.601540	745.374067	13.973159
20.814784	744.291379	13.978163
20.396350	751.356949	13.983168
20.721478	736.034895	13.988173
20.323971	742.202956	13.993178
20.736204	742.790130	13.998183
20.714597	741.382186	14.003187
20.430625	748.062018	14.008192
20.639988	744.280753	14.013210
20.285264	731.402658	14.018227
20.258807	732.515875	14.023245
20.259059	742.329766	14.028263
20.433359	749.034411	14.033280
20.813739	747.120796	14.038298
20.480324	749.895288	14.043315
20.401495	746.769779	14.048333
20.428434	753.027605	14.053351
20.289037	759.313535	14.058368
20.640394	743.598390	14.063386
20.682604	757.448190	14.068403
20.515341	753.097265	14.073421
20.613383	756.108105	14.078439
20.299213	754.309984	14.083456
20.514965	752.295212	14.088474
20.281044	743.226506	14.093491
20.239902	751.838948	14.098509
20.530369	754.627192	14.103527
20.152687	774.074621	14.108544
20.526621	779.468596	14.113562
20.714391	785.431801	14.118579
20.516152	780.074372	14.123597
21.235109	775.303674	14.128615
20.898650	780.230516	14.133632
21.000475	771.363068	14.138650
21.109320	783.821175	14.143667
20.463315	790.644088	14.148685
20.973065	786.937067	14.153703
20.819654	783.724346	14.158720
20.865992	779.026319	14.163738
20.821582	790.130930	14.168755
20.934129	788.374857	14.173773
21.029779	782.717301	14.178791
20.763757	792.784476	14.183808
20.575327	786.085286	14.188826
20.647104	793.243597	14.193843
20.748077	811.480603	14.198861
20.912184	817.650513	14.203879
20.691387	820.657164	14.208896
21.220440	814.748003	14.213914
21.097128	824.934009	14.218931
21.138437	820.480586	14.223949
21.583514	810.279519	14.228967
21.367342	813.651940	14.233984
21.338884	809.192345	14.239002
21.449898	819.592654	14.244019
21.218533	821.400791	14.249037
21.545139	807.542520	14.254055
21.139927	820.757463	14.259072
21.358984	805.132565	14.264090
21.438389	809.338722	14.269107
21.620395	824.037730	14.274125
21.793144	804.822766	14.279143
21.280363	805.236491	14.284160
21.287536	815.628191	14.289178
21.472092	819.087708	14.294195
21.579359	817.956954	14.299213
21.706561	814.892949	14.304231
21.361867	797.876208	14.309248
21.188100	796.003779	14.314266
21.552980	799.138807	14.319283
21.394437	807.389341	14.324301
21.429453	802.636484	14.329319
21.515306	805.677592	14.334336
21.600201	806.483623	14.339354
21.624126	812.389603	14.344371
21.580781	809.587177	14.349389
21.776030	809.139230	14.354407
21.607596	813.937039	14.359424
21.310763	807.992865	14.364442
21.736939	814.138279	14.369459
21.441328	819.863995	14.374477
21.969948	808.468281	14.379495
21.609406	814.232665	14.384512
21.772595	820.566315	14.389530
21.846798	811.756730	14.394547
21.638976	815.999261	14.399565
21.759334	815.929767	14.404583
21.703974	819.040590	14.409600
21.536919	813.143355	14.414618
21.628404	816.255925	14.419635
21.687256	819.641111	14.424653
22.079835	828.752276	14.429671
22.043947	841.695979	14.434688
22.034271	844.425147	14.439706
22.344668	835.461475	14.444723
22.052193	837.663173	14.449741
22.284301	807.183912	14.454759
21.983843	811.645706	14.459776
22.104674	810.861995	14.464794
22.527269	810.143411	14.469811
21.969148	812.870385	14.474829
21.986349	810.527057	14.479847
21.510253	818.048036	14.484864
22.124319	828.388567	14.489882
22.306876	834.879580	14.494899
22.204227	840.801041	14.499917
22.111098	833.526640	14.504935
22.389720	849.350690	14.509952
22.448923	846.060001	14.514970
22.434578	842.342176	14.519987
22.209886	836.495021	14.525005
22.472255	830.233565	14.530023
22.523141	839.543950	14.535040
22.377166	832.436852	14.540058
22.285638	816.590921	14.545075
22.155302	830.042026	14.550093
22.614228	838.200388	14.555111
22.878054	844.483392	14.560128
22.581189	832.437536	14.565146
22.619114	819.591118	14.570163
22.331058	818.782960	14.575181
22.436620	812.861120	14.580199
22.222912	819.873071	14.585216
22.394678	832.879600	14.590234
22.724129	840.530084	14.595251
22.543090	844.755768	14.600269
22.984812	845.791176	14.605287
22.918713	833.211445	14.610304
22.540616	823.775578	14.615322
22.436830	814.209452	14.620339
22.242506	828.730964	14.625357
22.653675	833.032076	14.630375
22.581864	847.546650	14.635392
22.573197	841.370888	14.640410
22.853572	841.019473	14.645427
22.844533	840.325686	14.650445
22.862125	845.993593	14.655463
23.010520	846.471751	14.660480
22.857500	838.974096	14.665498
23.110171	835.116159	14.670515
22.566956	845.985767	14.675533
22.948174	847.729239	14.680551
22.944634	841.162555	14.685568
22.944503	844.181206	14.690586
23.155923	841.361736	14.695603
22.867448	844.874682	14.700621
22.827048	832.693542	14.705639
22.836399	842.243357	14.710656
22.888766	851.769016	14.715674
23.013135	837.019619	14.720691
22.792670	843.205259	14.725709
22.758269	842.831690	14.730727
23.044077	837.935004	14.735744
23.022902	842.108449	14.740762
23.162429	852.332777	14.745779
23.213558	867.422359	14.750797
23.243891	872.226237	14.755815
23.491004	871.872262	14.760832
23.422014	862.442125	14.765850
23.484270	844.691895	14.770867
23.339165	851.016528	14.775885
23.213753	844.713095	14.780903
23.252104	836.138871	14.785920
23.292040	850.976968	14.790938
23.630337	845.228779	14.795955
23.141962	851.677372	14.800973
23.185439	858.692366	14.805991
23.536818	873.686877	14.811008
23.459887	873.831317	14.816026
23.825602	874.480880	14.821043
23.079650	876.602328	14.826061
23.360303	874.600784	14.831079
23.644891	872.785801	14.836096
23.648280	876.617142	14.841114
23.999226	877.519168	14.846131
23.526222	881.574353	14.851149
23.558594	888.205746	14.856167
23.802766	882.475700	14.861184
23.559041	878.418501	14.866202
23.864829	872.754136	14.871219
23.805863	878.868416	14.876237
23.928021	871.158544	14.881255
23.777853	861.797982	14.886272
23.690034	853.852625	14.891290
23.858673	848.243176	14.896307
23.952022	847.304973	14.901325
23.809287	847.579457	14.906343
23.936176	838.847968	14.911360
23.919093	846.654397	14.916378
23.801855	835.341223	14.921395
23.993434	846.603291	14.926413
23.605699	852.996509	14.931431
23.985501	869.181965	14.936448
23.917726	873.891381	14.941466
23.891265	881.155065	14.946483
23.789906	880.202296	14.951501
23.469302	881.994787	14.956519
23.867366	874.198437	14.961536
23.997101	869.759210	14.966554
24.281225	874.794742	14.971571
23.984546	873.525491	14.976589
23.791913	871.958079	14.981607
24.272323	874.616953	14.986624
23.940305	875.261395	14.991642
24.111508	878.062394	14.996659
24.140849	880.679954	15.001677
24.389813	891.047302	15.006695
24.519424	888.025369	15.011712
24.094253	887.213907	15.016730
24.392404	884.519021	15.021747
24.097392	889.329178	15.026765
24.753445	895.076172	15.031783
24.999943	883.366751	15.036800
24.372202	883.386685	15.041818
24.643631	872.008347	15.046835
24.502842	868.104618	15.051853
24.358731	865.546338	15.056871
24.301309	864.402522	15.061888
24.091401	870.570760	15.066906
24.452389	878.386120	15.071923
24.468387	886.470435	15.076941
24.698831	900.312371	15.081959
24.953593	885.914931	15.086976
24.803850	899.265377	15.091994
24.491353	874.018149	15.097011
24.983716	881.927387	15.102029
24.762262	884.688766	15.107047
24.958472	868.040271	15.112064
24.816694	873.010025	15.117082
24.700034	865.736215	15.122099
24.949161	866.023704	15.127117
24.432905	874.144140	15.132135
24.980355	857.592219	15.137152
24.801600	864.499516	15.142170
24.986406	865.129169	15.147187
24.872758	863.126021	15.152205
24.862302	867.038218	15.157223
24.798965	861.333630	15.162240
24.757756	862.669430	15.167258
25.203621	882.024980	15.172275
24.553082	877.249306	15.177293
24.574967	891.165395	15.182311
25.295686	886.216632	15.187328
24.863149	892.874986	15.192346
25.059033	891.470546	15.197363
25.136163	889.292251	15.202381
25.335359	891.476887	15.207399
25.456590	891.319166	15.212416
25.003183	901.325067	15.217434
25.341089	897.403183	15.222451
25.624429	892.568221	15.227469
25.017724	890.212703	15.232487
25.386812	886.988984	15.237504
25.255836	892.801726	15.242522
25.196269	889.990861	15.247539
25.171562	887.220054	15.252557
24.788312	889.271072	15.257575
25.330889	894.856841	15.262592
25.163665	900.271105	15.267610
24.948100	895.339535	15.272627
25.219035	893.317517	15.277645
25.070021	910.479256	15.282663
25.568146	914.577763	15.287680
25.400363	919.611455	15.292698
25.671091	920.362685	15.297715
26.050323	914.063678	15.302733
25.700909	920.161379	15.307751
25.870461	899.650638	15.312768
25.471801	895.544213	15.317786
25.464879	897.788465	15.322803
25.939306	909.521418	15.327821
25.595426	914.611508	15.332839
26.146571	912.137387	15.337856
25.865881	896.469401	15.342874
25.484607	891.834819	15.347891
25.748224	899.673585	15.352909
25.712233	911.541429	15.357927
26.004266	908.287523	15.362944
25.993497	926.194861	15.367962
25.824195	912.631085	15.372979
26.136605	903.088183	15.377997
25.958023	904.813980	15.383015
25.903577	885.638291	15.388032
25.619035	895.477258	15.393050
25.670844	903.390706	15.398067
25.997573	910.261450	15.403085
26.003009	914.679207	15.408103
26.352716	913.780336	15.413120
26.038348	919.636496	15.418138
26.112752	917.902220	15.423155
26.257877	918.421801	15.428173
26.176082	919.786101	15.433191
26.238985	914.578879	15.438208
26.183184	912.207852	15.443226
26.382808	913.745917	15.448243
26.137791	912.867967	15.453261
26.348614	919.565294	15.458279
26.251635	916.890951	15.463296
26.244043	912.775631	15.468314
26.336596	920.421470	15.473331
26.350425	908.434535	15.478349
26.034063	925.918709	15.483367
26.289499	916.649151	15.488384
26.247508	916.710941	15.493402
26.207268	912.890263	15.498419
26.563033	912.646371	15.503437
26.260658	921.229792	15.508455
26.429630	917.580236	15.513472
26.486954	928.201543	15.518490
26.188339	928.628303	15.523507
26.588872	928.166488	15.528525
26.474501	943.238500	15.533543
26.845844	943.979977	15.538560
27.076291	938.156145	15.543578
26.972029	935.451499	15.548595
26.963567	920.361410	15.553613
26.487634	922.691479	15.558631
26.476986	912.143032	15.563648
26.790038	934.821585	15.568666
26.987601	946.858272	15.573683
27.174851	940.102239	15.578701
26.816120	925.892268	15.583719
26.760625	914.451208	15.588736
26.947027	928.649405	15.593754
27.053047	945.394560	15.598771
27.208369	942.758623	15.603789
26.860739	933.855795	15.608807
27.196556	929.419861	15.613824
27.086818	912.884604	15.618842
26.596166	923.994422	15.623859
26.770817	924.032671	15.628877
26.965313	939.487996	15.633895
27.159084	936.374024	15.638912
27.302228	938.668281	15.643930
27.271519	936.386056	15.648947
27.456252	935.903603	15.653965
27.323081	931.515726	15.658983
27.336001	930.741354	15.664000
27.302552	935.069366	15.669018
27.064218	942.503724	15.674035
27.592654	938.796832	15.679053
27.392703	955.685179	15.684071
27.322221	943.595259	15.689088
27.342032	945.902895	15.694106
27.360239	949.410997	15.699123
27.290717	937.095988	15.704141
27.322592	940.793815	15.709159
27.320926	939.991882	15.714176
27.722886	944.749098	15.719194
27.275890	941.340922	15.724211
27.221195	936.064359	15.729229
27.005289	946.395778	15.734247
27.633905	943.333573	15.739264
27.736897	943.770213	15.744282
27.798295	944.532808	15.749299
27.834607	927.985251	15.754317
27.755154	935.633364	15.759335
28.057049	934.654029	15.764352
27.786941	932.450884	15.769370
27.628713	937.753616	15.774387
27.851585	928.657556	15.779405
28.076532	931.168424	15.784423
27.913004	932.209136	15.789440
27.767898	931.151658	15.794458
27.667727	932.083165	15.799475
27.973038	941.908312	15.804493
28.098018	953.284905	15.809511
28.102675	949.049645	15.814528
28.316056	932.206430	15.819546
28.057202	938.766318	15.824563
28.334322	926.153788	15.829581
27.988417	933.072047	15.834599
27.888248	936.459027	15.839616
28.392007	935.724348	15.844634
28.019589	941.017197	15.849651
28.318258	931.404109	15.854669
28.169108	946.308640	15.859687
28.340121	940.799451	15.864704
28.435251	934.709340	15.869722
28.024387	936.786790	15.874739
28.378192	943.209642	15.879757
28.671068	955.896521	15.884775
28.336521	951.751539	15.889792
28.622453	940.539147	15.894810
28.248187	940.026300	15.899827
28.355759	943.358127	15.904845
28.696611	959.573493	15.909863
28.379868	959.185177	15.914880
28.604395	959.876138	15.919898
28.407713	968.121834	15.924915
28.612278	953.573459	15.929933
28.618240	967.029694	15.934951
28.622670	972.973455	15.939968
29.100071	967.923474	15.944986
28.633212	963.870377	15.950003
28.803826	965.112628	15.955021
28.856038	967.501615	15.960039
28.663048	955.401337	15.965056
29.077756	942.077869	15.970074
28.850159	939.386601	15.975091
28.493728	932.747170	15.980109
28.710163	945.699487	15.985127
28.780519	955.017852	15.990144
29.020444	956.964770	15.995162
28.782475	960.153511	16.000179
28.565616	964.550109	16.005197
28.566638	965.822554	16.010215
28.675164	967.708633	16.015232
28.920966	964.440066	16.020250
28.937701	967.720320	16.025267
28.654318	958.582288	16.030285
28.761085	979.116758	16.035303
29.002218	987.838475	16.040320
29.001859	985.057474	16.045338
29.253628	986.271053	16.050355
29.489585	980.709020	16.055373
29.228628	987.992853	16.060391
29.310441	979.952731	16.065408
29.291315	972.414775	16.070426
29.080475	986.128974	16.075443
29.514184	984.585922	16.080461
29.354451	987.249388	16.085479
29.505140	979.344572	16.090496
29.439614	984.330516	16.095514
29.208536	999.204123	16.100531
29.104289	986.639781	16.105549
29.040778	981.197868	16.110567
29.548871	999.719391	16.115584
29.921487	1005.920621	16.120602
29.545572	993.147918	16.125619
29.241189	991.241240	16.130637
29.339211	1010.273342	16.135655
29.695993	1013.419149	16.140672
30.127615	1010.124081	16.145690
29.765397	1014.707471	16.150707
29.891974	1016.291804	16.155725
30.068923	1015.313515	16.160743
29.685212	1018.041023	16.165760
29.726804	1014.392882	16.170778
29.563489	1023.712381	16.175795
29.700935	1017.433016	16.180813
29.998656	1008.032387	16.185831
29.683033	1009.630616	16.190848
29.785562	1016.916266	16.195866
29.969581	1013.832148	16.200883
29.863160	1013.166468	16.205901
29.787606	1006.301309	16.210919
29.981279	1010.717388	16.215936
30.426869	1007.158972	16.220954
30.150152	1013.732753	16.225971
29.993963	1011.025364	16.230989
30.377729	1008.939718	16.236007
29.965803	1011.388580	16.241024
30.399116	1010.451202	16.246042
30.352309	1017.807861	16.251059
30.493707	1009.229685	16.256077
30.393269	1005.643525	16.261095
30.376322	1004.637960	16.266112
30.670213	1001.042392	16.271130
30.239247	1001.605093	16.276147
30.404226	997.866492	16.281165
30.375815	998.248586	16.286183
30.449089	1011.752329	16.291200
30.593359	1013.574511	16.296218
30.589884	1014.284536	16.301235
30.525216	1025.345367	16.306253
30.841378	1021.198831	16.311271
30.422442	1020.745014	16.316288
30.679630	1019.898647	16.321306
31.081322	1032.453407	16.326323
30.929619	1025.405329	16.331341
30.844306	1012.425813	16.336359
30.638205	1010.352447	16.341376
30.660612	1005.038393	16.346394
30.651332	1020.689899	16.351411
30.981796	1028.066618	16.356429
31.258844	1036.469605	16.361447
30.961703	1038.335449	16.366464
31.216095	1022.058170	16.371482
30.848282	1021.591481	16.376499
30.765238	1028.532355	16.381517
31.006846	1023.018168	16.386535
30.913752	1034.121292	16.391552
31.334664	1031.078039	16.396570
30.952127	1030.793022	16.401587
30.988917	1024.586337	16.406605
31.487348	1024.566656	16.411623
31.100742	1030.443818	16.416640
31.572397	1036.574211	16.421658
31.472300	1032.470464	16.426675
31.617383	1034.292520	16.431693
31.571393	1023.199070	16.436711
31.360759	1012.009191	16.441728
31.345196	1003.989306	16.446746
31.363544	1009.743673	16.451763
31.239647	1022.031466	16.456781
31.914353	1020.470425	16.461799
31.651378	1023.428787	16.466816
31.600312	1004.044763	16.471834
31.469732	1003.101365	16.476851
31.306610	1007.207835	16.481869
31.530400	1012.710787	16.486887
31.638075	1023.265932	16.491904
31.876202	1029.175591	16.496922
31.702513	1032.081962	16.501939
31.818769	1025.947546	16.506957
31.873895	1023.922177	16.511975
31.617130	1023.618674	16.516992
31.551297	1022.921352	16.522010
31.611245	1025.883268	16.527027
31.642354	1036.891081	16.532045
31.550746	1026.072318	16.537063
31.361811	1028.719999	16.542080
31.553103	1025.683482	16.547098
31.626377	1035.500082	16.552115
31.825354	1041.719583	16.557133
32.100332	1053.261095	16.562151
32.121653	1069.263276	16.567168
32.227087	1062.317315	16.572186
32.448378	1066.691255	16.577203
32.168654	1063.062888	16.582221
32.067238	1062.187194	16.587239
31.985684	1061.951701	16.592256
32.348263	1060.012572	16.597274
32.502051	1060.939764	16.602291
32.455242	1067.069488	16.607309
32.968215	1049.942402	16.612327
32.311166	1043.907715	16.617344
32.413296	1032.131537	16.622362
32.263444	1022.276892	16.627379
32.060287	1046.472546	16.632397
32.529614	1047.528737	16.637415
32.508568	1058.879938	16.642432
32.680564	1053.118866	16.647450
32.421331	1054.093052	16.652467
32.367291	1056.426642	16.657485
32.825072	1047.931691	16.662503
32.265423	1055.367015	16.667520
32.339536	1063.914069	16.672538
32.547265	1050.727333	16.677555
32.631691	1060.858350	16.682573
32.850828	1057.433567	16.687591
32.769423	1061.888814	16.692608
32.794085	1053.159344	16.697626
32.819455	1054.421621	16.702643
32.281237	1062.578696	16.707661
32.568285	1064.439461	16.712679
32.915669	1085.527165	16.717696
32.787425	1084.729681	16.722714
33.343117	1081.557957	16.727731
33.309363	1078.971027	16.732749
33.021182	1080.777246	16.737767
33.161626	1083.482516	16.742784
33.215400	1076.131081	16.747802
33.517668	1075.834373	16.752819
33.310539	1082.686524	16.757837
33.236893	1077.843941	16.762855
33.260641	1079.104907	16.767872
33.326750	1082.569222	16.772890
33.706984	1074.785048	16.777907
33.595957	1078.634690	16.782925
33.702197	1072.928142	16.787943
33.409923	1068.639530	16.792960
33.254325	1062.572051	16.797978
33.534814	1075.603930	16.802995
33.282679	1071.968015	16.808013
33.537913	1070.403083	16.813031
33.799032	1070.985967	16.818048
33.572978	1077.007429	16.823066
33.439749	1065.322245	16.828083
33.268471	1075.635626	16.833101
33.587614	1079.276662	16.838119
33.462384	1073.912198	16.843136
33.692143	1072.835821	16.848154
33.677805	1067.875244	16.853171
33.518769	1076.851174	16.858189
33.672470	1074.223337	16.863207
34.126230	1068.140468	16.868224
33.651765	1071.897061	16.873242
33.981879	1067.521771	16.878259
33.688703	1083.040871	16.883277
34.055450	1092.005314	16.888295
34.276538	1099.149401	16.893312
34.149777	1099.792576	16.898330
34.324160	1101.482552	16.903347
33.923678	1100.096127	16.908365
34.273480	1090.479499	16.913383
34.392701	1099.525895	16.918400
34.365162	1093.669215	16.923418
34.428810	1070.128165	16.928435
34.083831	1073.160964	16.933453
34.355364	1085.012937	16.938471
34.389686	1089.923218	16.943488
34.410635	1097.884166	16.948506
34.627825	1093.725080	16.953523
34.116380	1089.581529	16.958541
34.487343	1093.388910	16.963559
34.640373	1093.010611	16.968576
34.405977	1104.293627	16.973594
34.492674	1099.920969	16.978611
34.386051	1100.785876	16.983629
34.569921	1099.166255	16.988647
34.705034	1100.116878	16.993664
34.036447	1106.633648	16.998682
34.657360	1104.228595	17.003699
34.634764	1104.405270	17.008717
34.787000	1099.081488	17.013735
34.921298	1106.185937	17.018752
34.716199	1103.813521	17.023770
34.785004	1094.586199	17.028787
34.856208	1107.542947	17.033805
35.138434	1113.030327	17.038823
35.052324	1106.171523	17.043840
34.774778	1102.923472	17.048858
35.127094	1114.087755	17.053875
35.153716	1133.123541	17.058893
35.350367	1120.745475	17.063911
35.497128	1104.049541	17.068928
34.960081	1099.351644	17.073946
35.005059	1099.180913	17.078963
35.229557	1109.767826	17.083981
35.502187	1117.503028	17.088999
35.371030	1101.446026	17.094016
35.530958	1115.203461	17.099034
35.828248	1097.870043	17.104051
35.498091	1100.568574	17.109069
35.280730	1084.810058	17.114087
35.511801	1087.897280	17.119104
35.156943	1084.995045	17.124122
35.606380	1085.469245	17.129139
35.628433	1099.133822	17.134157
35.269607	1103.472878	17.139175
35.678358	1118.876922	17.144192
35.658229	1115.314106	17.149210
35.896082	1114.274188	17.154227
35.589686	1125.228929	17.159245
35.578057	1124.769923	17.164263
35.833686	1117.694588	17.169280
35.706429	1125.234019	17.174298
35.699605	1117.494250	17.179315
35.983139	1119.774011	17.184333
35.713555	1119.211427	17.189351
35.829088	1117.865399	17.194368
35.988102	1123.175804	17.199386
35.972391	1114.147567	17.204403
36.114404	1119.399334	17.209421
35.779434	1117.096393	17.214439
36.124209	1108.956059	17.219456
35.690859	1105.728136	17.224474
36.157754	1133.847179	17.229491
36.103446	1146.418136	17.234509
36.262325	1145.785643	17.239527
36.371000	1144.997562	17.244544
36.357994	1152.772045	17.249562
36.535402	1147.423781	17.254579
36.486328	1142.229617	17.259597
36.479522	1145.527823	17.264615
36.789426	1143.507422	17.269632
36.813691	1141.527858	17.274650
36.552123	1139.881746	17.279667
36.387886	1135.832244	17.284685
36.646797	1144.686503	17.289703
36.709141	1142.792101	17.294720
36.550071	1145.667849	17.299738
36.950153	1139.788568	17.304755
36.846989	1145.244616	17.309773
36.824405	1147.861068	17.314791
36.802793	1140.397353	17.319808
36.324320	1151.442479	17.324826
36.773953	1147.936869	17.329843
37.180513	1144.538804	17.334861
37.181365	1148.527925	17.339879
37.473250	1138.159153	17.344896
37.111648	1150.384291	17.349914
37.056774	1135.537335	17.354931
36.648094	1151.477625	17.359949
37.247418	1147.380276	17.364967
37.055811	1143.000081	17.369984
36.994391	1142.987892	17.375002
36.857702	1142.687258	17.380019
36.985220	1137.936842	17.385037
36.946169	1142.144685	17.390055
37.066296	1143.676577	17.395072
36.840909	1143.761326	17.400090
37.262002	1152.767477	17.405107
37.396551	1159.494384	17.410125
37.446767	1167.370477	17.415143
37.441280	1168.670720	17.420160
37.198044	1168.752023	17.425178
37.386847	1170.727573	17.430195
37.535255	1155.226826	17.435213
37.436550	1173.596810	17.440231
37.716486	1169.039155	17.445248
37.298157	1170.090633	17.450266
37.209767	1166.684983	17.455283
37.530555	1180.141543	17.460301
37.812191	1195.138074	17.465319
38.250192	1192.052738	17.470336
38.064064	1195.351240	17.475354
38.167074	1189.626285	17.480371
38.093146	1166.764551	17.485389
38.107157	1163.109761	17.490407
38.159970	1163.364073	17.495424
37.891425	1169.824935	17.500442
38.096283	1159.772051	17.505459
38.085912	1159.864979	17.510477
38.059981	1173.699302	17.515495
38.449788	1190.772292	17.520512
38.206983	1182.821584	17.525530
38.704097	1171.314211	17.530547
38.326350	1157.591538	17.535565
38.520642	1148.795630	17.540583
38.405407	1140.572913	17.545600
38.425657	1158.200310	17.550618
38.530633	1144.578415	17.555635
38.232591	1136.719912	17.560653
38.019241	1160.365246	17.565671
38.434376	1169.797078	17.570688
38.674288	1173.021336	17.575706
38.427454	1182.237850	17.580723
38.775797	1173.620281	17.585741
38.694482	1179.162519	17.590759
38.817831	1170.897016	17.595776
38.616800	1179.563525	17.600794
38.585277	1180.970169	17.605811
38.890553	1176.133189	17.610829
38.719385	1177.664351	17.615847
38.926129	1174.590732	17.620864
38.979790	1180.935717	17.625882
38.531017	1174.015169	17.630899
38.838661	1174.197379	17.635917
38.793286	1181.838613	17.640935
39.055108	1183.830835	17.645952
38.993893	1199.490817	17.650970
39.206384	1198.774266	17.655987
39.695886	1195.117567	17.661005
39.128217	1188.843617	17.666023
39.484813	1182.475747	17.671040
39.263897	1186.846316	17.676058
39.336644	1197.468507	17.681075
39.364326	1191.541631	17.686093
39.478552	1198.328427	17.691111
39.573769	1199.494634	17.696128
39.411128	1202.857032	17.701146
39.753446	1203.370344	17.706163
39.872122	1198.498622	17.711181
39.358726	1194.820970	17.716199
39.616417	1194.468448	17.721216
39.549006	1199.844881	17.726234
39.787284	1210.464278	17.731251
39.711140	1209.400498	17.736269
39.709628	1213.283047	17.741287
39.984090	1204.732299	17.746304
39.621632	1209.639833	17.751322
39.886242	1206.181022	17.756339
40.029013	1204.143223	17.761357
39.620895	1214.300991	17.766375
39.881832	1206.571954	17.771392
40.067082	1201.643995	17.776410
39.634779	1204.185800	17.781427
39.957322	1199.009428	17.786445
39.829248	1204.091940	17.791463
40.022444	1214.171111	17.796480
40.469691	1232.741965	17.801498
40.516145	1234.026065	17.806515
40.945879	1222.579735	17.811533
40.153745	1209.698611	17.816551
40.096834	1206.541192	17.821568
40.146473	1202.998687	17.826586
40.229552	1228.703160	17.831603
40.589412	1230.918856	17.836621
40.297680	1233.162964	17.841639
40.620132	1220.750593	17.846656
40.717107	1227.859482	17.851674
40.639459	1232.762500	17.856691
40.907320	1228.069898	17.861709
40.851490	1229.420647	17.866727
40.761128	1228.999364	17.871744
40.733589	1234.202707	17.876762
40.704535	1233.098382	17.881779
40.859180	1227.822933	17.886797
40.705813	1236.802776	17.891815
40.775387	1223.957246	17.896832
40.854218	1231.509483	17.901850
40.925442	1230.917708	17.906867
41.078138	1219.990624	17.911885
41.130529	1219.656686	17.916903
41.332757	1219.742450	17.921920
40.893750	1220.141269	17.926938
41.008586	1222.318962	17.931955
41.441618	1224.320064	17.936973
41.025012	1221.514166	17.941991
41.251051	1228.552135	17.947008
41.820845	1239.721158	17.952026
41.388835	1247.958924	17.957043
42.055005	1237.278702	17.962061
41.458479	1230.450904	17.967079
41.668837	1223.137344	17.972096
41.157304	1219.086577	17.977114
41.411128	1224.597407	17.982131
41.763705	1235.393650	17.987149
41.742557	1240.750136	17.992167
41.701335	1245.785777	17.997184
41.988053	1246.949761	18.002202
41.673796	1255.041335	18.007219
41.974316	1238.979830	18.012237
41.865557	1251.677541	18.017255
41.639376	1245.577195	18.022272
41.920365	1248.044576	18.027290
41.764883	1245.472311	18.032307
41.820797	1252.095397	18.037325
41.441411	1253.135949	18.042343
41.933172	1246.070085	18.047360
41.581207	1244.905572	18.052378
41.707966	1263.442634	18.057395
42.347434	1272.321224	18.062413
42.081486	1279.753864	18.067431
41.932723	1276.837597	18.072448
42.203822	1272.160195	18.077466
41.980451	1276.554778	18.082483
42.159992	1274.133573	18.087501
42.304487	1284.239436	18.092519
42.555398	1289.250525	18.097536
43.541928	1292.344725	18.102554
42.946006	1284.591851	18.107571
42.994027	1274.897387	18.112589
42.817028	1274.189466	18.117607
42.987361	1272.197601	18.122624
42.883942	1262.049091	18.127642
42.786972	1270.408044	18.132659
43.146894	1267.621441	18.137677
42.902652	1270.441582	18.142695
42.723433	1266.949719	18.147712
42.949946	1267.127567	18.152730
42.687374	1271.901212	18.157747
42.892179	1265.626729	18.162765
42.903865	1265.495914	18.167783
42.803400	1269.314033	18.172800
42.767577	1271.086319	18.177818
42.679694	1276.741328	18.182835
43.313576	1296.550378	18.187853
43.179598	1303.195907	18.192871
43.245526	1304.483199	18.197888
43.379333	1293.901998	18.202906
43.324815	1298.181566	18.207923
43.523202	1301.632703	18.212941
43.410741	1297.807710	18.217959
43.423404	1302.343985	18.222976
43.249012	1298.914266	18.227994
43.458904	1302.146487	18.233011
43.450082	1296.203367	18.238029
43.249117	1303.529700	18.243047
43.483863	1310.906099	18.248064
43.958400	1323.800289	18.253082
44.009332	1335.514614	18.258099
44.341269	1324.727183	18.263117
43.957895	1309.668165	18.268135
43.901317	1302.315338	18.273152
44.048016	1295.562463	18.278170
44.046186	1293.778952	18.283187
44.130499	1300.405396	18.288205
43.982045	1299.477414	18.293223
43.652854	1314.206538	18.298240
44.245338	1318.060450	18.303258
44.324813	1324.640486	18.308275
44.352745	1328.170724	18.313293
44.272544	1332.021809	18.318311
44.145170	1324.971277	18.323328
44.445242	1329.269810	18.328346
44.374247	1331.466145	18.333363
44.301507	1330.157990	18.338381
44.501697	1321.044854	18.343399
44.449749	1325.117951	18.348416
44.766649	1316.214298	18.353434
44.404027	1321.349987	18.358451
44.537723	1322.005117	18.363469
44.829259	1318.335915	18.368487
44.701769	1322.526454	18.373504
44.905322	1318.153971	18.378522
44.887424	1329.651176	18.383539
44.793050	1314.402915	18.388557
44.536367	1315.165921	18.393575
44.678514	1325.146343	18.398592
45.084846	1329.506583	18.403610
45.095741	1335.491934	18.408627
45.024408	1332.052064	18.413645
45.389048	1333.192617	18.418663
44.991533	1339.554569	18.423680
45.041314	1332.112404	18.428698
45.141181	1340.992149	18.433715
45.232931	1333.892508	18.438733
45.355464	1334.248965	18.443751
45.257763	1328.958667	18.448768
45.397957	1328.374766	18.453786
45.501786	1332.481224	18.458803
45.542210	1331.839301	18.463821
45.826603	1329.160688	18.468839
45.315213	1333.475377	18.473856
45.633399	1330.003274	18.478874
45.511258	1337.153454	18.483891
45.664494	1326.644637	18.488909
45.718136	1337.941672	18.493927
45.661387	1338.224473	18.498944
45.598619	1330.413286	18.503962
45.734235	1347.832175	18.508979
45.954729	1362.053676	18.513997
46.194098	1353.826195	18.519015
46.187379	1361.909680	18.524032
46.070040	1351.947375	18.529050
45.928558	1366.270655	18.534067
46.133190	1363.955549	18.539085
46.520933	1359.602443	18.544103
46.167532	1365.513769	18.549120
46.346689	1359.993685	18.554138
46.064001	1357.122356	18.559155
46.316189	1362.668107	18.564173
46.258801	1357.770926	18.569191
46.269195	1362.055892	18.574208
46.478914	1352.033562	18.579226
46.657028	1350.553262	18.584243
46.639626	1361.298491	18.589261
46.630489	1357.062166	18.594279
46.498678	1359.191124	18.599296
46.546241	1352.650665	18.604314
46.804064	1363.183686	18.609331
46.783336	1359.296855	18.614349
46.712365	1363.914128	18.619367
47.156020	1384.274320	18.624384
47.175111	1385.218297	18.629402
47.087969	1394.664313	18.634419
47.252334	1382.050496	18.639437
47.202799	1361.564606	18.644455
46.969176	1359.349282	18.649472
47.343578	1359.231407	18.654490
47.028814	1370.530592	18.659507
47.223305	1374.974969	18.664525
47.224252	1375.132162	18.669543
47.183989	1382.401444	18.674560
47.436562	1381.219158	18.679578
47.121570	1376.880592	18.684595
47.458698	1385.288360	18.689613
47.599940	1376.974268	18.694631
47.160971	1390.808601	18.699648
47.509368	1372.307360	18.704666
47.607831	1379.628450	18.709683
47.306602	1382.714110	18.714701
47.519426	1385.201824	18.719719
47.592722	1409.753550	18.724736
47.870332	1408.752892	18.729754
48.017971	1409.188719	18.734771
47.885019	1416.732355	18.739789
48.050652	1407.116577	18.744807
47.892786	1408.146980	18.749824
48.180012	1422.085757	18.754842
48.448838	1407.345778	18.759859
48.091694	1414.003352	18.764877
48.100731	1419.114410	18.769895
48.148775	1404.469421	18.774912
48.119101	1417.824789	18.779930
48.360861	1412.127957	18.784947
48.131061	1416.411919	18.789965
48.617210	1404.360259	18.794983
48.049355	1409.376123	18.800000
48.053318	1411.110619	18.805018
48.326486	1415.611676	18.810035
48.208490	1427.543357	18.815053
48.564975	1429.987718	18.820071
48.544527	1445.347300	18.825088
48.547643	1433.611758	18.830106
48.859515	1424.963678	18.835123
48.669437	1434.224783	18.840141
48.964151	1430.673027	18.845159
48.876233	1438.834001	18.850176
48.822127	1431.420937	18.855194
48.881193	1432.042355	18.860211
48.736245	1434.399941	18.865229
49.145309	1445.706447	18.870247
49.401325	1452.838848	18.875264
49.710727	1459.001592	18.880282
49.261975	1438.469147	18.885299
49.067162	1431.542579	18.890317
49.724710	1440.130519	18.895335
49.605315	1435.737145	18.900352
49.102426	1427.148214	18.905370
49.618542	1434.863632	18.910387
49.431222	1448.550918	18.915405
49.920692	1451.147112	18.920423
49.640150	1453.620710	18.925440
49.682497	1452.525430	18.930458
49.896907	1452.615547	18.935475
49.696427	1459.193099	18.940493
49.817598	1456.700947	18.945511
49.567086	1457.936470	18.950528
49.714292	1460.260051	18.955546
50.098655	1447.519854	18.960563
50.227632	1455.333206	18.965581
50.272318	1440.858607	18.970599
50.296098	1453.140516	18.975616
50.134986	1454.166720	18.980634
50.469468	1444.464213	18.985651
50.182037	1448.766813	18.990669
50.510255	1441.177938	18.995687
50.297389	1446.848226	19.000704
50.052574	1449.286237	19.005722
50.354872	1442.854554	19.010739
50.150571	1452.759751	19.015757
50.367913	1447.180060	19.020775
50.270770	1442.267169	19.025792
50.260585	1453.143453	19.030810
50.701285	1460.785967	19.035827
50.570963	1472.947747	19.040845
50.726799	1475.721426	19.045863
50.608350	1477.270953	19.050880
50.311312	1482.603097	19.055898
50.685371	1471.954349	19.060915
50.657892	1478.295101	19.065933
50.917347	1474.072537	19.070951
51.077966	1480.666445	19.075968
50.755337	1482.968216	19.080986
51.226545	1481.275201	19.086003
50.760188	1500.932014	19.091021
51.653190	1501.972588	19.096039
51.335563	1508.988855	19.101056
51.035058	1507.275761	19.106074
51.572907	1502.975756	19.111091
51.452806	1511.945744	19.116109
51.410255	1498.089061	19.121127
51.681853	1498.831535	19.126144
51.552306	1503.669773	19.131162
51.695745	1494.491646	19.136179
51.437402	1506.356896	19.141197
51.685275	1504.930737	19.146215
51.953282	1498.819900	19.151232
51.641221	1499.861529	19.156250
51.702904	1498.979460	19.161267
51.493507	1504.307861	19.166285
51.851761	1517.609319	19.171303
52.147312	1525.096472	19.176320
52.119791	1531.499390	19.181338
52.378979	1519.079552	19.186355
52.321596	1526.465684	19.191373
52.256439	1524.728425	19.196391
52.172273	1527.201391	19.201408
52.028841	1533.404925	19.206426
52.512084	1522.089833	19.211443
52.808092	1528.886335	19.216461
52.462712	1527.536696	19.221479
52.329432	1524.504647	19.226496
52.368982	1526.419105	19.231514
52.619366	1518.732487	19.236531
52.539974	1536.104878	19.241549
52.523005	1526.520502	19.246567
52.411125	1521.803422	19.251584
52.236276	1528.885021	19.256602
52.783841	1533.231452	19.261619
52.754594	1555.774442	19.266637
52.965074	1551.991477	19.271655
52.933512	1558.370668	19.276672
53.070478	1554.083457	19.281690
52.968136	1553.356536	19.286707
52.708008	1560.545349	19.291725
53.090634	1559.057582	19.296743
53.217711	1558.688130	19.301760
52.968266	1558.295352	19.306778
54.046348	1555.584508	19.311795
53.732511	1549.471270	19.316813
53.778127	1539.736900	19.321831
53.969966	1538.378666	19.326848
53.962817	1540.965985	19.331866
54.363814	1535.010108	19.336883
54.137214	1535.658998	19.341901
54.002368	1536.226399	19.346919
53.726452	1529.218333	19.351936
54.039837	1529.361095	19.356954
53.871455	1531.560406	19.361971
54.052742	1542.500606	19.366989
53.876217	1537.364380	19.372007
54.272162	1534.143319	19.377024
53.767829	1542.471437	19.382042
54.285773	1531.459914	19.387059
53.671828	1533.727924	19.392077
53.890486	1537.227010	19.397095
53.881544	1531.464717	19.402112
53.776451	1537.365613	19.407130
54.278222	1549.628005	19.412147
54.453441	1566.075756	19.417165
54.170678	1562.063127	19.422183
54.585300	1558.824924	19.427200
54.304182	1573.221014	19.432218
54.938516	1554.313707	19.437235
54.283316	1566.214767	19.442253
54.709349	1570.278560	19.447271
54.841224	1567.560519	19.452288
54.647510	1572.482161	19.457306
54.741575	1568.031894	19.462323
54.878123	1587.742115	19.467341
55.087788	1599.952817	19.472359
55.170254	1600.782877	19.477376
55.237036	1606.931680	19.482394
55.258083	1595.077526	19.487411
55.260828	1592.509853	19.492429
54.860443	1595.799353	19.497447
55.195052	1590.840366	19.502464
54.980411	1596.729654	19.507482
55.286293	1597.179578	19.512499
55.053684	1598.324164	19.517517
55.433529	1610.896287	19.522535
55.852017	1623.938903	19.527552
55.470981	1628.648969	19.532570
55.990620	1626.145941	19.537587
55.910382	1625.122897	19.542605
55.828712	1622.581265	19.547623
56.165013	1616.292741	19.552640
56.128878	1619.761692	19.557658
55.653599	1603.729125	19.562675
56.125003	1611.602000	19.567693
55.931487	1613.762072	19.572711
56.254030	1614.792168	19.577728
56.258076	1616.401615	19.582746
56.302854	1607.938388	19.587763
56.360279	1613.511363	19.592781
56.162501	1627.044749	19.597799
56.440922	1618.695270	19.602816
56.276104	1617.947635	19.607834
56.525265	1615.813372	19.612851
56.352896	1609.292928	19.617869
56.307246	1622.260906	19.622887
56.578824	1609.525185	19.627904
56.239972	1622.860832	19.632922
56.287525	1634.783586	19.637939
56.447230	1642.772257	19.642957
56.672959	1651.551106	19.647975
56.993907	1641.476231	19.652992
56.589403	1646.080715	19.658010
56.821369	1639.261385	19.663027
56.966191	1646.439931	19.668045
56.991062	1657.071667	19.673063
57.245187	1663.402984	19.678080
57.189176	1673.626043	19.683098
57.313344	1673.981461	19.688115
57.452824	1665.892438	19.693133
57.334228	1666.425004	19.698151
57.665168	1665.805165	19.703168
57.494014	1668.507541	19.708186
57.561962	1665.514161	19.713203
57.622505	1672.511097	19.718221
57.617162	1674.820500	19.723239
57.913238	1665.547134	19.728256
57.606402	1667.255718	19.733274
57.715740	1669.179515	19.738291
57.782214	1663.501888	19.743309
57.633861	1666.084218	19.748327
58.428908	1688.963167	19.753344
58.332314	1697.965701	19.758362
58.244862	1689.426768	19.763379
58.284293	1686.606252	19.768397
58.430895	1696.007321	19.773415
58.546233	1677.774107	19.778432
58.144864	1678.851226	19.783450
58.324678	1690.804059	19.788467
58.247545	1704.747731	19.793485
58.643094	1705.836981	19.798503
58.746478	1697.107941	19.803520
58.372557	1697.173116	19.808538
58.335162	1703.779828	19.813555
58.735590	1698.705697	19.818573
58.311022	1696.814153	19.823591
58.573079	1692.361441	19.828608
58.853028	1692.769885	19.833626
58.823096	1705.284739	19.838643
58.975964	1711.341203	19.843661
58.909916	1725.703930	19.848679
59.280537	1716.611348	19.853696
59.289882	1720.028237	19.858714
59.284775	1717.061441	19.863731
59.154923	1714.972664	19.868749
59.302377	1714.478830	19.873767
59.378335	1711.646192	19.878784
59.034320	1716.809726	19.883802
59.069523	1716.707404	19.888819
59.541581	1705.163497	19.893837
59.289039	1735.268070	19.898855
59.756606	1740.367467	19.903872
59.880336	1743.847921	19.908890
59.762753	1745.302165	19.913907
60.384536	1728.237950	19.918925
60.215800	1743.254963	19.923943
60.220022	1734.761948	19.928960
60.377941	1731.938258	19.933978
60.463739	1731.412570	19.938995
60.456715	1707.987942	19.944013
60.079769	1711.399577	19.949031
60.187468	1708.429737	19.954048
60.505059	1714.520497	19.959066
60.683305	1732.542625	19.964083
60.554241	1716.963616	19.969101
60.489248	1727.266799	19.974119
60.674712	1724.515800	19.979136
60.712174	1728.368675	19.984154
60.823567	1734.558397	19.989171
60.957055	1731.865238	19.994189
60.676286	1728.498000	19.999207
61.108205	1718.756963	20.004224
60.701962	1729.665940	20.009242
61.022282	1729.164202	20.014259
60.722428	1736.269770	20.019277
60.587442	1737.040130	20.024295
60.870607	1723.974470	20.029312
60.988797	1728.473599	20.034330
60.847067	1744.380613	20.039347
61.116313	1749.945817	20.044365
61.141618	1764.841454	20.049383
61.446046	1760.138133	20.054400
61.551771	1762.621757	20.059418
61.363464	1764.254030	20.064435
61.478821	1753.373402	20.069453
61.687601	1755.874411	20.074471
61.399109	1767.895699	20.079488
61.566778	1762.597530	20.084506
61.686692	1784.159853	20.089523
62.137600	1775.164549	20.094541
62.295440	1777.382661	20.099559
62.010584	1783.892799	20.104576
61.927305	1778.865105	20.109594
61.864305	1775.081650	20.114611
62.366574	1781.718743	20.119629
61.845362	1783.602320	20.124647
61.866127	1774.635499	20.129664
61.750236	1779.673007	20.134682
62.099641	1792.899836	20.139699
62.492232	1797.256906	20.144717
62.682502	1797.066144	20.149735
62.688591	1812.795495	20.154752
63.002297	1792.810309	20.159770
62.635686	1806.373931	20.164787
62.581640	1800.090161	20.169805
62.566646	1794.887968	20.174823
62.684308	1798.961678	20.179840
62.888001	1798.106497	20.184858
62.872702	1803.204267	20.189875
62.869898	1813.963234	20.194893
62.878895	1827.744630	20.199911
62.950094	1824.748338	20.204928
63.391656	1828.690960	20.209946
63.171334	1837.019570	20.214963
63.431409	1830.665242	20.219981
63.036305	1835.753589	20.224999
63.395475	1828.041596	20.230016
63.528005	1841.557899	20.235034
63.335014	1856.432597	20.240051
64.025061	1852.777581	20.245069
63.849607	1853.375853	20.250087
63.654671	1849.060470	20.255104
63.962043	1847.284213	20.260122
63.947159	1852.983650	20.265139
64.149220	1852.144458	20.270157
64.148415	1853.727175	20.275175
64.529918	1851.530087	20.280192
64.416093	1852.203478	20.285210
64.318776	1852.457362	20.290227
64.378209	1858.681381	20.295245
64.458388	1849.459633	20.300263
64.297238	1852.976106	20.305280
64.664863	1838.606922	20.310298
64.373993	1855.451032	20.315315
64.338214	1842.392869	20.320333
64.662221	1849.844192	20.325351
64.698538	1875.108143	20.330368
64.859222	1868.103434	20.335386
65.039694	1887.681996	20.340403
64.936570	1873.369760	20.345421
65.127386	1868.668006	20.350439
64.930308	1877.434190	20.355456
65.070387	1877.055579	20.360474
65.120402	1871.728154	20.365491
65.304263	1872.645099	20.370509
65.219929	1871.671457	20.375527
65.310648	1875.991745	20.380544
65.403856	1871.622538	20.385562
65.107447	1878.411428	20.390579
65.162536	1877.692420	20.395597
65.657985	1879.925925	20.400615
65.410294	1901.435355	20.405632
65.768145	1896.961798	20.410650
65.907081	1894.627198	20.415667
66.187732	1887.847969	20.420685
66.386287	1891.097076	20.425703
66.142477	1900.575483	20.430720
66.283407	1885.383484	20.435738
66.161868	1896.511465	20.440755
66.329952	1888.135383	20.445773
66.550640	1886.132259	20.450791
66.525663	1892.367393	20.455808
66.528072	1890.309411	20.460826
66.350831	1892.379619	20.465843
66.701458	1887.786874	20.470861
66.663879	1886.062478	20.475879
66.554036	1904.063904	20.480896
66.631430	1884.305839	20.485914
66.632351	1896.798633	20.490931
66.747553	1888.618971	20.495949
66.777475	1889.141231	20.500967
66.422439	1892.530535	20.505984
66.972861	1887.719514	20.511002
67.357732	1896.417288	20.516019
67.213382	1899.068238	20.521037
67.666817	1896.109296	20.526055
67.579228	1887.769267	20.531072
67.819044	1871.543706	20.536090
67.534793	1875.889183	20.541107
67.491453	1870.597097	20.546125
67.585039	1866.886179	20.551143
67.518398	1867.385297	20.556160
67.812616	1876.945424	20.561178
67.909005	1884.973429	20.566195
67.961867	1893.778420	20.571213
68.199364	1889.675651	20.576231
68.071894	1898.721775	20.581248
68.021833	1883.936996	20.586266
68.112001	1896.472976	20.591283
68.074699	1899.246863	20.596301
67.976878	1902.719426	20.601319
68.242034	1909.586313	20.606336
68.417928	1899.217411	20.611354
68.381125	1906.153688	20.616371
68.304678	1900.604946	20.621389
68.080423	1898.893800	20.626407
68.119909	1904.602677	20.631424
68.490820	1916.013172	20.636442
68.589889	1923.671088	20.641459
68.520850	1941.329405	20.646477
68.980966	1930.714582	20.651495
69.072872	1940.616919	20.656512
68.798271	1932.796715	20.661530
68.865557	1939.423808	20.666547
68.770091	1929.489867	20.671565
69.148811	1930.301018	20.676583
69.007079	1936.359723	20.681600
69.514856	1935.924046	20.686618
69.203507	1956.727939	20.691635
69.244000	1967.058517	20.696653
69.623150	1962.302315	20.701671
69.269024	1965.529458	20.706688
69.680467	1961.030819	20.711706
69.484239	1968.499095	20.716723
69.584987	1962.546882	20.721741
69.386677	1955.954121	20.726759
69.480610	1981.231878	20.731776
70.246928	1981.345679	20.736794
70.119968	1982.237475	20.741811
70.229891	1986.977905	20.746829
70.314273	1983.688450	20.751847
70.039467	1998.310481	20.756864
70.166232	1982.451274	20.761882
70.055610	1994.250887	20.766899
69.790811	1978.952808	20.771917
69.948573	1998.519410	20.776935
70.091704	2019.350021	20.781952
70.540057	2005.660765	20.786970
70.682205	2019.373127	20.791987
70.650709	2017.037371	20.797005
70.898490	2004.739285	20.802023
70.984474	2022.387136	20.807040
71.184155	2039.927996	20.812058
71.297004	2042.696842	20.817075
71.520550	2044.983962	20.822093
71.570398	2030.075343	20.827111
70.955155	2016.972569	20.832128
71.077635	2030.972816	20.837146
71.504440	2037.638581	20.842163
71.234959	2046.647663	20.847181
71.612538	2036.901711	20.852199
71.373800	2041.139297	20.857216
71.762853	2048.440341	20.862234
71.760176	2041.791173	20.867251
71.252443	2049.020497	20.872269
71.743051	2051.246937	20.877287
71.776867	2076.613890	20.882304
71.938790	2064.056507	20.887322
71.874444	2072.142498	20.892339
71.932684	2067.883422	20.897357
72.379127	2076.772847	20.902375
72.464669	2071.727568	20.907392
72.788014	2069.145653	20.912410
72.550359	2068.050146	20.917427
72.094455	2064.381973	20.922445
72.580633	2059.797448	20.927463
72.523411	2074.305413	20.932480
72.730311	2083.371479	20.937498
73.202202	2083.220753	20.942515
73.072225	2083.760654	20.947533
73.255394	2073.446315	20.952551
73.099953	2070.755909	20.957568
73.204332	2058.076351	20.962586
73.281971	2067.465849	20.967603
73.291722	2062.892015	20.972621
73.447504	2062.100307	20.977639
73.039285	2063.648910	20.982656
73.367345	2069.911197	20.987674
73.530305	2069.311840	20.992691
73.199966	2081.982684	20.997709
73.487323	2077.363002	21.002727
73.300001	2077.477075	21.007744
73.368179	2074.146923	21.012762
73.425234	2098.738586	21.017779
73.428002	2105.974623	21.022797
73.677862	2101.600030	21.027815
73.606734	2116.273074	21.032832
73.770074	2118.786900	21.037850
74.460699	2131.555328	21.042867
74.712912	2132.227779	21.047885
74.953674	2119.506754	21.052903
74.515288	2120.026620	21.057920
74.518411	2118.115581	21.062938
74.802900	2119.074701	21.067955
74.532361	2127.217988	21.072973
74.916315	2131.190333	21.077991
75.058036	2132.029852	21.083008
75.199838	2121.680388	21.088026
75.170304	2122.519687	21.093043
75.168772	2117.823357	21.098061
75.292575	2122.447565	21.103079
75.262081	2128.429617	21.108096
75.472988	2132.661597	21.113114
75.023983	2123.443049	21.118131
74.936051	2126.682050	21.123149
75.077271	2117.212854	21.128167
75.036590	2126.332587	21.133184
75.300528	2128.918468	21.138202
75.496716	2144.382677	21.143219
75.879734	2142.400827	21.148237
75.819741	2147.578210	21.153255
75.762423	2147.472549	21.158272
75.756366	2154.551916	21.163290
75.941969	2145.474416	21.168307
75.775049	2162.631046	21.173325
76.004272	2153.869080	21.178343
75.914878	2172.850792	21.183360
75.937115	2175.183407	21.188378
76.451774	2177.887416	21.193395
76.479118	2177.400924	21.198413
76.493903	2167.658467	21.203431
76.353711	2177.522467	21.208448
76.692514	2171.209712	21.213466
76.732730	2172.125987	21.218483
76.567003	2172.717213	21.223501
77.039225	2196.682008	21.228519
77.184430	2197.165444	21.233536
77.016027	2207.958976	21.238554
77.341830	2202.899721	21.243571
77.175174	2209.815161	21.248589
77.177542	2212.739309	21.253607
77.215302	2201.390124	21.258624
77.172482	2211.292107	21.263642
77.352444	2204.614526	21.268659
77.037089	2215.473972	21.273677
77.446866	2215.997022	21.278695
77.629546	2233.487339	21.283712
77.674763	2244.043108	21.288730
77.816400	2237.635914	21.293747
77.932320	2245.598864	21.298765
77.730860	2246.218602	21.303783
77.882999	2233.737359	21.308800
77.935204	2243.545552	21.313818
77.968836	2247.059373	21.318835
77.916329	2265.488651	21.323853
78.341988	2264.087560	21.328871
78.885281	2261.544476	21.333888
78.666693	2263.518287	21.338906
79.147903	2262.807605	21.343923
79.091549	2273.537695	21.348941
79.163880	2256.541613	21.353959
79.107635	2253.578929	21.358976
79.202597	2261.322629	21.363994
79.391974	2252.682585	21.369011
79.299504	2255.413422	21.374029
79.503507	2245.519606	21.379047
79.604286	2244.451132	21.384064
79.288431	2257.290504	21.389082
79.255885	2251.624507	21.394099
79.232865	2254.889367	21.399117
79.268165	2246.040284	21.404135
79.510230	2254.723293	21.409152
79.406762	2245.833413	21.414170
79.646088	2253.746798	21.419187
79.470397	2279.267860	21.424205
79.695551	2277.911327	21.429223
80.130506	2279.651136	21.434240
79.605195	2287.639280	21.439258
80.070059	2283.415194	21.444275
80.091598	2288.036885	21.449293
80.339480	2302.666324	21.454311
80.499989	2305.792593	21.459328
80.384642	2318.589032	21.464346
80.795555	2300.189919	21.469363
80.677051	2307.930715	21.474381
81.040917	2303.013234	21.479399
80.964140	2297.953646	21.484416
80.918195	2306.438774	21.489434
81.033258	2300.946650	21.494451
81.238928	2299.599515	21.499469
81.162788	2300.952027	21.504487
81.346709	2298.124084	21.509504
81.123425	2318.274169	21.514522
81.287625	2298.592158	21.519539
81.226329	2308.199825	21.524557
81.232401	2306.741361	21.529575
81.345282	2298.406884	21.534592
80.867293	2308.475077	21.539610
81.259014	2321.616197	21.544627
81.717750	2322.995898	21.549645
81.686708	2327.349109	21.554663
81.567611	2328.607792	21.559680
81.663090	2354.018096	21.564698
82.126073	2346.506375	21.569715
82.113714	2363.135966	21.574733
82.201218	2361.276725	21.579751
82.251410	2359.379386	21.584768
81.882592	2367.597470	21.589786
82.406096	2370.464503	21.594803
82.652288	2392.580224	21.599821
82.482021	2388.971031	21.604839
82.820060	2388.759060	21.609856
83.062488	2391.982407	21.614874
83.241444	2388.071323	21.619891
83.330731	2388.430751	21.624909
82.709353	2386.998397	21.629927
83.067448	2380.995537	21.634944
82.851094	2383.263977	21.639962
83.131242	2390.827190	21.644979
83.222143	2407.188657	21.649997
83.037669	2414.035455	21.655015
83.675232	2411.349101	21.660032
83.241724	2421.651759	21.665050
83.594576	2417.445498	21.670067
84.085044	2434.710780	21.675085
83.970827	2439.641272	21.680103
84.331189	2435.127825	21.685120
84.062984	2447.083506	21.690138
84.246642	2439.740562	21.695155
84.576196	2435.173821	21.700173
84.556345	2441.015865	21.705191
84.907044	2437.617767	21.710208
84.630263	2436.738488	21.715226
84.963079	2430.920554	21.720243
84.934063	2430.970841	21.725261
84.447947	2428.738978	21.730279
84.729857	2428.719232	21.735296
84.509245	2430.054679	21.740314
84.877699	2430.500164	21.745331
84.939738	2431.561640	21.750349
84.670570	2431.447284	21.755367
84.836028	2429.542567	21.760384
84.799748	2459.047800	21.765402
85.139530	2466.042279	21.770419
85.043678	2465.282812	21.775437
85.317170	2473.100411	21.780455
85.389664	2466.929894	21.785472
85.610816	2475.341063	21.790490
85.777878	2483.307787	21.795507
85.989800	2482.337989	21.800525
85.786229	2488.596351	21.805543
86.141974	2484.936290	21.810560
85.934528	2488.458723	21.815578
86.103967	2484.214831	21.820595
86.324167	2481.771216	21.825613
85.928506	2491.289950	21.830631
86.264166	2488.546323	21.835648
86.235434	2506.614215	21.840666
86.230426	2514.564346	21.845683
86.459884	2505.472552	21.850701
86.400572	2515.761227	21.855719
86.629389	2521.169567	21.860736
86.859839	2540.093672	21.865754
87.127231	2538.710715	21.870771
87.421204	2537.641304	21.875789
87.272526	2549.275955	21.880807
87.229117	2546.536918	21.885824
87.268593	2538.741027	21.890842
87.471783	2543.625658	21.895859
87.112866	2547.890419	21.900877
87.505534	2541.176407	21.905895
87.729687	2561.033656	21.910912
87.576005	2583.939460	21.915930
87.680559	2573.471335	21.920947
87.722579	2566.740860	21.925965
87.665921	2579.156108	21.930983
88.250057	2577.511831	21.936000
88.146289	2601.041338	21.941018
88.474193	2606.368621	21.946035
88.763309	2601.592750	21.951053
88.757241	2598.849321	21.956071
88.972268	2591.952806	21.961088
88.833017	2599.140940	21.966106
88.763595	2591.538585	21.971123
88.862946	2597.563051	21.976141
88.760494	2593.272026	21.981159
88.877116	2582.967941	21.986176
88.892275	2587.417693	21.991194
88.977049	2588.472410	21.996211
89.211740	2589.907530	22.001229
89.119920	2607.632427	22.006247
89.455383	2615.038270	22.011264
89.393959	2618.686115	22.016282
89.417187	2621.979866	22.021299
89.679789	2624.173539	22.026317
89.514185	2624.553954	22.031335
89.773557	2614.422946	22.036352
89.607946	2618.503516	22.041370
89.629902	2637.254119	22.046387
90.217780	2642.251277	22.051405
89.837327	2641.008590	22.056423
90.168243	2639.318948	22.061440
90.207579	2645.265692	22.066458
90.182966	2639.873588	22.071475
90.597331	2651.954996	22.076493
90.480044	2672.597595	22.081511
90.737188	2678.144638	22.086528
90.993036	2668.437346	22.091546
90.839466	2670.259254	22.096563
91.125646	2676.089561	22.101581
90.868381	2675.139507	22.106599
91.054938	2665.876683	22.111616
91.308322	2675.893000	22.116634
91.011700	2680.457785	22.121651
91.290431	2691.425003	22.126669
91.060653	2699.252184	22.131687
91.651672	2697.041231	22.136704
91.659040	2692.388920	22.141722
91.673459	2702.881497	22.146739
91.832209	2698.856351	22.151757
91.716276	2719.905474	22.156775
92.153431	2724.522382	22.161792
91.950828	2724.380889	22.166810
92.063967	2724.277932	22.171827
92.649725	2725.125341	22.176845
92.319616	2725.076547	22.181863
92.601129	2725.684575	22.186880
92.389689	2732.782028	22.191898
92.573356	2737.739845	22.196915
92.896440	2746.698126	22.201933
92.803105	2754.414692	22.206951
92.882627	2744.982461	22.211968
93.170359	2746.007185	22.216986
93.493566	2747.401463	22.222003
93.587490	2750.585643	22.227021
93.429691	2757.580162	22.232039
93.396963	2754.643517	22.237056
93.352784	2750.608239	22.242074
93.616855	2744.437733	22.247091
93.877632	2743.259544	22.252109
93.940527	2768.859045	22.257127
94.245764	2770.423737	22.262144
94.450002	2766.357494	22.267162
94.040041	2760.609107	22.272179
94.579900	2753.526994	22.277197
94.597179	2765.836218	22.282215
94.695750	2755.830654	22.287232
94.830102	2733.430379	22.292250
94.673636	2727.334807	22.297267
94.818363	2726.112196	22.302285
94.447080	2740.472679	22.307303
94.828344	2753.530907	22.312320
94.909098	2763.140606	22.317338
94.785577	2764.936495	22.322355
95.107350	2757.439220	22.327373
95.068637	2766.029652	22.332391
95.105479	2765.916837	22.337408
95.231509	2768.424928	22.342426
94.932539	2761.774696	22.347443
95.167422	2772.774926	22.352461
95.327558	2788.793834	22.357479
95.603311	2785.838669	22.362496
95.664255	2786.108235	22.367514
95.217064	2806.012303	22.372531
95.946296	2813.346018	22.377549
96.041250	2822.352523	22.382567
96.002607	2829.605748	22.387584
96.284342	2827.429937	22.392602
96.068248	2826.810762	22.397619
96.315571	2823.885295	22.402637
96.326301	2832.589020	22.407655
96.838862	2847.202759	22.412672
96.823315	2851.441170	22.417690
96.759946	2864.180241	22.422707
96.979907	2858.435985	22.427725
96.797506	2858.423418	22.432743
96.876998	2858.878027	22.437760
96.876866	2853.290008	22.442778
97.029431	2869.714529	22.447795
97.707847	2867.960010	22.452813
97.692714	2883.870100	22.457831
97.721786	2873.392558	22.462848
97.892741	2879.174460	22.467866
97.515263	2883.230677	22.472883
97.718097	2871.458984	22.477901
97.670375	2880.168912	22.482919
97.725489	2897.881742	22.487936
98.063824	2893.591135	22.492954
98.023880	2890.515596	22.497971
98.109574	2892.644701	22.502989
98.300482	2900.174428	22.508007
98.591053	2910.445345	22.513024
98.833107	2913.051378	22.518042
98.794955	2926.940444	22.523059
98.829256	2920.839542	22.528077
98.944558	2928.537875	22.533095
98.889483	2923.789255	22.538112
99.430960	2913.055348	22.543130
99.147952	2924.025003	22.548147
99.087518	2915.096388	22.553165
98.924200	2932.903874	22.558183
99.102191	2942.786873	22.563200
99.794796	2938.000831	22.568218
99.720575	2949.959025	22.573235
99.903332	2940.322992	22.578253
100.035478	2938.491958	22.583271
99.736511	2942.890435	22.588288
100.024392	2951.093013	22.593306
100.233102	2971.013854	22.598323
100.560252	2973.839167	22.603341
100.027499	2981.911464	22.608359
100.495748	2976.357263	22.613376
100.803041	2958.839915	22.618394
100.656194	2973.829527	22.623411
100.679839	2974.035035	22.628429
100.669737	2979.863153	22.633447
100.621948	2980.063533	22.638464
100.928447	2988.349691	22.643482
101.207932	3004.356883	22.648499
101.323634	3000.382570	22.653517
101.377498	3002.773204	22.658535
101.278963	2997.450178	22.663552
101.710348	2996.098455	22.668570
101.357344	2998.724663	22.673587
101.357156	3003.061355	22.678605
102.119933	3013.741605	22.683623
101.956426	3020.761544	22.688640
101.721361	3020.581172	22.693658
102.068347	3021.648385	22.698675
102.026928	3020.805479	22.703693
102.163709	3035.324366	22.708711
102.447977	3045.320280	22.713728
102.930134	3045.767323	22.718746
102.702505	3052.767610	22.723763
102.632650	3050.730427	22.728781
103.077751	3050.743659	22.733799
102.926630	3052.524318	22.738816
102.814626	3054.077700	22.743834
103.031643	3058.959514	22.748851
103.178665	3072.722435	22.753869
103.468860	3081.121373	22.758887
103.169883	3086.753318	22.763904
103.406036	3083.551904	22.768922
103.646778	3091.847820	22.773939
103.409682	3084.901243	22.778957
103.555365	3093.315366	22.783975
103.723661	3109.286913	22.788992
103.868421	3112.949987	22.794010
103.790074	3122.546748	22.799027
104.040889	3126.653090	22.804045
104.291873	3136.654374	22.809063
104.110981	3146.638789	22.814080
104.506492	3136.924652	22.819098
104.544222	3140.391624	22.824115
104.658245	3150.035604	22.829133
104.871745	3160.250551	22.834151
104.922661	3165.878650	22.839168
105.196803	3172.775384	22.844186
105.140784	3174.372555	22.849203
105.545168	3170.897295	22.854221
105.472984	3173.616414	22.859239
104.708134	3176.612750	22.864256
105.472842	3172.095963	22.869274
105.607753	3189.454239	22.874291
105.751895	3195.285379	22.879309
106.012986	3198.588529	22.884327
106.141991	3195.375071	22.889344
105.890175	3189.812897	22.894362
106.120328	3195.709772	22.899379
106.407520	3195.138548	22.904397
106.179535	3196.520074	22.909415
106.221449	3217.017700	22.914432
106.708655	3215.986655	22.919450
106.706465	3220.896398	22.924467
106.693081	3226.777055	22.929485
107.009713	3212.352520	22.934503
106.756081	3213.229188	22.939520
107.285890	3231.294655	22.944538
107.643479	3243.379317	22.949555
107.884760	3247.180427	22.954573
107.790458	3241.587610	22.959591
107.701777	3245.929046	22.964608
107.933618	3235.742218	22.969626
108.087674	3233.938333	22.974643
107.827479	3238.605248	22.979661
107.924694	3241.739454	22.984679
107.942640	3240.741543	22.989696
107.975888	3243.620855	22.994714
108.147203	3243.956999	22.999731
107.614394	3259.448173	23.004749
108.261209	3266.294180	23.009767
107.926869	3282.438887	23.014784
108.277367	3290.509745	23.019802
108.919047	3310.061514	23.024819
108.736152	3307.081839	23.029837
108.995442	3304.511502	23.034855
109.153610	3311.238789	23.039872
109.378114	3306.023041	23.044890
109.627650	3304.701862	23.049907
109.918172	3317.547729	23.054925
109.890666	3311.612274	23.059943
109.556848	3329.419109	23.064960
109.604503	3327.690389	23.069978
109.837392	3324.531923	23.074995
109.850364	3327.381446	23.080013
110.184485	3328.291048	23.085031
110.013962	3336.084731	23.090048
110.055251	3347.692083	23.095066
110.291624	3360.167463	23.100083
110.448732	3357.432485	23.105101
110.316289	3357.963383	23.110119
110.408658	3364.751531	23.115136
110.725305	3379.839137	23.120154
111.079350	3382.546968	23.125171
110.755462	3382.844083	23.130189
111.042206	3381.736437	23.135207
110.868433	3384.611815	23.140224
111.250056	3402.119797	23.145242
111.882127	3415.341580	23.150259
111.844381	3407.699923	23.155277
112.282794	3405.591871	23.160295
111.906420	3406.683208	23.165312
111.914640	3394.589715	23.170330
112.435330	3394.520886	23.175347
112.408187	3400.335369	23.180365
112.618706	3400.326225	23.185383
112.535340	3408.909995	23.190400
112.253830	3392.966475	23.195418
112.833182	3398.734594	23.200435
112.250466	3401.247252	23.205453
112.993725	3403.462733	23.210471
113.124830	3415.529374	23.215488
112.912369	3420.435741	23.220506
113.199348	3417.747694	23.225523
113.329041	3423.343665	23.230541
113.342038	3424.925138	23.235559
113.561180	3419.231927	23.240576
113.417408	3418.471397	23.245594
113.187327	3432.850943	23.250611
113.471586	3449.047443	23.255629
113.979847	3440.756257	23.260647
113.715343	3454.396363	23.265664
113.837389	3477.730009	23.270682
114.114680	3482.343549	23.275699
114.073913	3497.728981	23.280717
114.489471	3482.287010	23.285735
114.636101	3492.975399	23.290752
114.693427	3507.350096	23.295770
115.015982	3513.502186	23.300787
114.760925	3521.435309	23.305805
114.821564	3517.258816	23.310823
114.996669	3516.787265	23.315840
115.151854	3515.743852	23.320858
115.510229	3531.591155	23.325875
115.481906	3545.343935	23.330893
115.991604	3534.888401	23.335911
115.647087	3543.050556	23.340928
115.675083	3535.438468	23.345946
115.687900	3536.061847	23.350963
116.072476	3552.808852	23.355981
116.358523	3556.463669	23.360999
116.500485	3554.546037	23.366016
116.417639	3563.569550	23.371034
116.678189	3551.731472	23.376051
116.467067	3555.828995	23.381069
116.620631	3563.396486	23.386087
116.580995	3574.607078	23.391104
116.785259	3582.854026	23.396122
116.927279	3585.769553	23.401139
117.014818	3604.804359	23.406157
117.136669	3591.533848	23.411175
117.531302	3594.278514	23.416192
117.485030	3615.544370	23.421210
117.665128	3617.353307	23.426227
117.719321	3620.485802	23.431245
118.078783	3611.324612	23.436263
118.130306	3617.271381	23.441280
118.002916	3622.434857	23.446298
118.268566	3613.946264	23.451315
118.179843	3622.031489	23.456333
118.622818	3631.495897	23.461351
118.850372	3631.523370	23.466368
118.903444	3643.736373	23.471386
118.950531	3641.643488	23.476403
118.943657	3645.039814	23.481421
119.144827	3643.218140	23.486439
119.021211	3645.122709	23.491456
119.148958	3641.372858	23.496474
119.501253	3654.148600	23.501491
119.569028	3676.068947	23.506509
120.016814	3669.639060	23.511527
119.793027	3668.315444	23.516544
119.542949	3674.842892	23.521562
120.147846	3667.789311	23.526579
119.769572	3669.264069	23.531597
119.926994	3680.832715	23.536615
120.221346	3696.521275	23.541632
120.249832	3711.540320	23.546650
120.547385	3705.158760	23.551667
120.309927	3715.935302	23.556685
120.576208	3716.338916	23.561703
120.917744	3730.659073	23.566720
120.576006	3732.131945	23.571738
120.792578	3745.112699	23.576755
120.961962	3754.551585	23.581773
121.019087	3759.393838	23.586791
121.388706	3754.539470	23.591808
121.251643	3769.434720	23.596826
121.748305	3784.914904	23.601843
121.684058	3792.816175	23.606861
121.867111	3790.157220	23.611879
122.156353	3792.682731	23.616896
122.281156	3811.851102	23.621914
122.469064	3804.297550	23.626931
122.227526	3822.482023	23.631949
122.533134	3812.513527	23.636967
122.631886	3823.175966	23.641984
122.786584	3830.266697	23.647002
123.135579	3832.063678	23.652019
122.768990	3844.115630	23.657037
123.226443	3841.509672	23.662055
123.535123	3835.500733	23.667072
123.510326	3838.988855	23.672090
123.910429	3839.626013	23.677107
123.928857	3842.820898	23.682125
124.006265	3830.465855	23.687143
124.264640	3828.097748	23.692160
124.048385	3830.113083	23.697178
123.944945	3834.656071	23.702195
123.986617	3853.072329	23.707213
124.158451	3872.337907	23.712231
124.457395	3863.860382	23.717248
124.407574	3864.666828	23.722266
124.550433	3879.855822	23.727283
124.537877	3895.551839	23.732301
124.572220	3894.316842	23.737319
124.996864	3898.372874	23.742336
125.170105	3931.501728	23.747354
125.278024	3924.588630	23.752371
125.530897	3924.408320	23.757389
125.167867	3938.439037	23.762407
125.656185	3937.059278	23.767424
125.401720	3960.057244	23.772442
125.897518	3954.726424	23.777459
125.883532	3956.596245	23.782477
126.220472	3963.138780	23.787495
126.535915	3975.189864	23.792512
126.700404	3984.674520	23.797530
127.010520	3975.272386	23.802547
126.838317	3986.809657	23.807565
127.138347	3985.308088	23.812583
127.093173	3972.920551	23.817600
126.902026	3987.326683	23.822618
127.019893	3985.025008	23.827635
127.399332	4007.145529	23.832653
127.134601	4013.708503	23.837671
127.794789	4015.203367	23.842688
127.526126	4020.339947	23.847706
127.871050	4018.483507	23.852723
127.792746	4037.837960	23.857741
127.708023	4046.003807	23.862759
128.615983	4033.785205	23.867776
128.317457	4046.029431	23.872794
128.326176	4044.252556	23.877811
128.272239	4068.515156	23.882829
128.579356	4069.814586	23.887847
128.547419	4075.506593	23.892864
128.708717	4083.679647	23.897882
129.158637	4097.438503	23.902899
129.251538	4105.903319	23.907917
129.086065	4114.620953	23.912935
129.505198	4098.752963	23.917952
129.778208	4128.358561	23.922970
129.911073	4135.324693	23.927987
130.089076	4131.722468	23.933005
130.081992	4135.436759	23.938023
130.134811	4132.046444	23.943040
130.086363	4139.379760	23.948058
130.185577	4133.359259	23.953075
130.433506	4155.448265	23.958093
130.413617	4163.799723	23.963111
130.491469	4154.468337	23.968128
130.652040	4158.824579	23.973146
131.270775	4172.711565	23.978163
131.616492	4174.589354	23.983181
131.851378	4177.075613	23.988199
131.990043	4174.027180	23.993216
131.864437	4165.396120	23.998234
132.070029	4172.898203	24.003251
132.242691	4167.551177	24.008269
131.874741	4171.784010	24.013287
132.254246	4175.372163	24.018304
132.293954	4186.927723	24.023322
132.314138	4183.774671	24.028339
132.367906	4180.178083	24.033357
132.262900	4177.241663	24.038375
132.444280	4189.443315	24.043392
132.398794	4197.208075	24.048410
132.406304	4197.264343	24.053427
132.550486	4206.772835	24.058445
132.779895	4234.783128	24.063463
133.148560	4228.963498	24.068480
133.116057	4246.584938	24.073498
133.184878	4260.781535	24.078515
133.232893	4260.981602	24.083533
133.266791	4281.339602	24.088551
133.602584	4294.570881	24.093568
133.745507	4301.066622	24.098586
134.287568	4297.046007	24.103603
134.674623	4312.581990	24.108621
134.522033	4315.303125	24.113639
134.939561	4308.044687	24.118656
134.971459	4308.059307	24.123674
135.222172	4311.179496	24.128691
135.341465	4298.117229	24.133709
135.449846	4315.123126	24.138727
135.796822	4331.103705	24.143744
135.940050	4339.602326	24.148762
136.038873	4339.102006	24.153779
136.046811	4334.818828	24.158797
135.808089	4335.165311	24.163815
136.120245	4336.238183	24.168832
136.195876	4335.197959	24.173850
136.278357	4339.772820	24.178867
136.560493	4345.729529	24.183885
136.971649	4338.293514	24.188903
137.606400	4336.571765	24.193920
137.447566	4319.219953	24.198938
137.203701	4313.823644	24.203955
137.342083	4318.594124	24.208973
137.283417	4341.404914	24.213991
137.538044	4345.985370	24.219008
137.821145	4345.563445	24.224026
137.282212	4346.777526	24.229043
137.873384	4343.419329	24.234061
137.679246	4346.338260	24.239079
137.675076	4345.637235	24.244096
137.730588	4368.929411	24.249114
137.440669	4381.635903	24.254131
138.009572	4378.798891	24.259149
137.954064	4401.746943	24.264167
138.190521	4408.022492	24.269184
138.523176	4418.644922	24.274202
138.389960	4438.759163	24.279219
138.928535	4433.896518	24.284237
138.901343	4457.002986	24.289255
139.215078	4461.847037	24.294272
139.415098	4466.735969	24.299290
139.269828	4478.043547	24.304307
139.746854	4475.396601	24.309325
139.646706	4495.850220	24.314343
139.837117	4502.996160	24.319360
140.135402	4501.722962	24.324378
140.312488	4501.991350	24.329395
140.492466	4512.642913	24.334413
140.502897	4523.039091	24.339431
140.810708	4519.637138	24.344448
140.599464	4530.014383	24.349466
141.040107	4540.668460	24.354483
141.582158	4542.859570	24.359501
141.340355	4552.780696	24.364519
141.368417	4557.379249	24.369536
141.617836	4558.788623	24.374554
141.511244	4557.013551	24.379571
141.959063	4570.333422	24.384589
141.764199	4590.338907	24.389607
141.957507	4580.796887	24.394624
142.225143	4589.057113	24.399642
142.079955	4608.850159	24.404659
142.462165	4615.767324	24.409677
142.514759	4618.876686	24.414695
142.556963	4616.812762	24.419712
142.931536	4637.763609	24.424730
143.042757	4635.712280	24.429747
143.051158	4635.648829	24.434765
143.230204	4653.870324	24.439783
143.576866	4655.594620	24.444800
143.824507	4659.705051	24.449818
143.545880	4672.506756	24.454835
143.759583	4657.906053	24.459853
143.974586	4685.629208	24.464871
144.045156	4698.416167	24.469888
144.369974	4695.098002	24.474906
144.264490	4702.714465	24.479923
144.741291	4710.279002	24.484941
144.771775	4729.664220	24.489959
145.101917	4721.974237	24.494976
145.422509	4718.910060	24.499994
145.491932	4726.053371	24.505011
145.805722	4714.842323	24.510029
145.778664	4724.210097	24.515047
145.769622	4722.277057	24.520064
146.083072	4726.346333	24.525082
146.138348	4741.390480	24.530099
146.325426	4742.526596	24.535117
146.198669	4749.152073	24.540135
146.254024	4748.080438	24.545152
146.379399	4743.043628	24.550170
146.267702	4769.914313	24.555187
146.656755	4786.168749	24.560205
146.569936	4787.649850	24.565223
146.603626	4792.336478	24.570240
146.929441	4810.895081	24.575258
147.301310	4818.737594	24.580275
147.417821	4812.367118	24.585293
147.571296	4828.737834	24.590311
147.629988	4849.680343	24.595328
147.905694	4851.884073	24.600346
147.806510	4857.332993	24.605363
147.857030	4863.589607	24.610381
148.338247	4873.096718	24.615399
148.616056	4875.805975	24.620416
148.716881	4884.591745	24.625434
148.483829	4907.074043	24.630451
148.750390	4908.370578	24.635469
148.983892	4919.152364	24.640487
149.000278	4929.140358	24.645504
149.513207	4933.671161	24.650522
149.289987	4943.715462	24.655539
149.502961	4947.457809	24.660557
149.585652	4975.105837	24.665575
149.813840	4971.794363	24.670592
150.255007	4966.936851	24.675610
149.963049	4992.534654	24.680627
150.566722	5002.313412	24.685645
150.783595	5002.612444	24.690663
151.012435	4997.085443	24.695680
151.317946	4984.901547	24.700698
150.865488	4997.743048	24.705715
151.552514	5007.974262	24.710733
151.677645	5018.078721	24.715751
151.602826	5016.139608	24.720768
151.996887	5008.834222	24.725786
152.063034	5017.255839	24.730803
151.910799	5018.177803	24.735821
151.953688	5038.459103	24.740839
152.369772	5034.702266	24.745856
152.638407	5046.403735	24.750874
152.546720	5050.333147	24.755891
152.898050	5043.792176	24.760909
153.000137	5058.051897	24.765927
153.233368	5068.026653	24.770944
153.855581	5058.349857	24.775962
153.542580	5070.293558	24.780979
153.952036	5061.819760	24.785997
153.980118	5065.162063	24.791015
153.803042	5068.034357	24.796032
154.042964	5067.872626	24.801050
154.130963	5075.179145	24.806067
154.058171	5075.087727	24.811085
154.218905	5082.934936	24.816103
154.031690	5095.015948	24.821120
154.322053	5098.412422	24.826138
154.569873	5115.817913	24.831155
154.710461	5125.886938	24.836173
154.788831	5135.478117	24.841191
154.898095	5137.637622	24.846208
155.175346	5147.366247	24.851226
155.099228	5164.618893	24.856243
155.188702	5170.921351	24.861261
155.528911	5181.241025	24.866279
155.164758	5198.080180	24.871296
155.653554	5213.372744	24.876314
155.823221	5233.527103	24.881331
155.830785	5233.503119	24.886349
156.102446	5262.780000	24.891367
156.351293	5273.713800	24.896384
156.876011	5283.805084	24.901402
157.152596	5289.629320	24.906419
157.148561	5296.104875	24.911437
157.968161	5307.322191	24.916455
157.942195	5328.569184	24.921472
158.058321	5316.642580	24.926490
158.364748	5324.015100	24.931507
158.480572	5319.930788	24.936525
158.486726	5322.043034	24.941543
158.451571	5325.217674	24.946560
158.581025	5328.783831	24.951578
158.599699	5338.999106	24.956595
158.752760	5352.326561	24.961613
158.933611	5358.004804	24.966631
158.724454	5356.561471	24.971648
159.408070	5362.178440	24.976666
159.310541	5374.951089	24.981683
159.454877	5376.890257	24.986701
159.758320	5378.943311	24.991719
159.877094	5401.153911	24.996736
160.046727	5397.989360	25.001754
160.313378	5406.569624	25.006771
160.333529	5417.008153	25.011789
160.684519	5431.931903	25.016807
160.780517	5443.122290	25.021824
160.853320	5442.696891	25.026842
161.066727	5440.889574	25.031859
161.269205	5447.029372	25.036877
161.548220	5462.721481	25.041895
161.188124	5472.158561	25.046912
161.650673	5469.417771	25.051930
161.595061	5474.053552	25.056947
161.913818	5491.059522	25.061965
162.036806	5499.504608	25.066983
161.913346	5506.034699	25.072000
162.224476	5517.370223	25.077018
162.065559	5532.090566	25.082035
162.163873	5536.082651	25.087053
162.564690	5554.276196	25.092071
162.729097	5566.417183	25.097088
163.114455	5564.965586	25.102106
163.128926	5587.703700	25.107123
163.364629	5589.037475	25.112141
163.637395	5588.362260	25.117159
163.795439	5608.917869	25.122176
163.659505	5623.268797	25.127194
163.725467	5625.827084	25.132211
164.106849	5641.478673	25.137229
164.605159	5648.561133	25.142247
164.629236	5660.435043	25.147264
165.006269	5655.607992	25.152282
165.198223	5677.701913	25.157299
165.000482	5678.636679	25.162317
165.757711	5672.447705	25.167335
165.553417	5679.618595	25.172352
165.744585	5693.059870	25.177370
165.857225	5702.423300	25.182387
166.010646	5710.297186	25.187405
166.177986	5699.542252	25.192423
166.103995	5717.256245	25.197440
166.448633	5720.908564	25.202458
166.490091	5737.213964	25.207475
166.549180	5730.497419	25.212493
166.612324	5755.787372	25.217511
166.671045	5759.474271	25.222528
167.181312	5782.910176	25.227546
167.354421	5804.027766	25.232563
167.531200	5804.818646	25.237581
167.921344	5818.288106	25.242599
167.937704	5838.164039	25.247616
167.881697	5844.625304	25.252634
168.362447	5832.801440	25.257651
168.287409	5871.790037	25.262669
168.943353	5868.954615	25.267687
168.878332	5873.074325	25.272704
168.926754	5881.291553	25.277722
169.061288	5883.329124	25.282739
169.348652	5896.242272	25.287757
169.667756	5894.292166	25.292775
169.557305	5914.327678	25.297792
170.290042	5916.982698	25.302810
170.352022	5926.809889	25.307827
170.105318	5930.541591	25.312845
170.601325	5921.457134	25.317863
170.591207	5930.996848	25.322880
170.802973	5939.084998	25.327898
171.210447	5948.462947	25.332915
171.021311	5969.573224	25.337933
171.154990	5960.603944	25.342951
170.995855	5974.409741	25.347968
171.180557	5960.741564	25.352986
171.665668	5974.324271	25.358003
172.009054	5998.356751	25.363021
171.803717	5992.324256	25.368039
172.041837	6007.250849	25.373056
172.055853	6019.604225	25.378074
172.016409	6023.119587	25.383091
172.200666	6038.431666	25.388109
172.624847	6047.117008	25.393127
172.536423	6060.849455	25.398144
173.004321	6063.602589	25.403162
173.448102	6078.284821	25.408179
173.299979	6081.553951	25.413197
173.761150	6089.578818	25.418215
173.742434	6110.914683	25.423232
174.205155	6120.286294	25.428250
174.027480	6110.488511	25.433267
174.194303	6133.761003	25.438285
174.594323	6139.682342	25.443303
174.500513	6155.420465	25.448320
174.415180	6160.775600	25.453338
174.806606	6173.564611	25.458355
174.878393	6194.381050	25.463373
175.312992	6199.602954	25.468391
175.481250	6210.857933	25.473408
175.477550	6215.595032	25.478426
176.137521	6223.941547	25.483443
176.236810	6238.780357	25.488461
176.289814	6231.444565	25.493479
176.382195	6249.364770	25.498496
176.425453	6259.258110	25.503514
176.920022	6267.156584	25.508531
176.726515	6286.264048	25.513549
177.000201	6300.236394	25.518567
176.880343	6309.901637	25.523584
177.173843	6313.544950	25.528602
177.675734	6326.354248	25.533619
177.814881	6332.493498	25.538637
178.021962	6353.850364	25.543655
178.194914	6360.461821	25.548672
177.824116	6368.815392	25.553690
178.572440	6371.307509	25.558707
178.610867	6390.982391	25.563725
178.779959	6396.057862	25.568743
179.089829	6403.211646	25.573760
179.415320	6416.234830	25.578778
179.508155	6429.779787	25.583795
179.556840	6435.142766	25.588813
180.110283	6442.470960	25.593831
180.250448	6453.224689	25.598848
180.357497	6453.849691	25.603866
180.866578	6448.397858	25.608883
180.863433	6448.602966	25.613901
180.774409	6444.775244	25.618919
180.822339	6459.898631	25.623936
180.988153	6474.867908	25.628954
181.210110	6483.540901	25.633971
180.961219	6496.709230	25.638989
180.933927	6503.962450	25.644007
181.684200	6512.144454	25.649024
181.459468	6528.090316	25.654042
182.156881	6532.676401	25.659059
182.223493	6547.802406	25.664077
182.321182	6558.918621	25.669095
182.663048	6554.528060	25.674112
182.821485	6569.602468	25.679130
183.176057	6570.578271	25.684148
183.061956	6577.666760	25.689165
183.296890	6597.452214	25.694183
183.403178	6602.926453	25.699200
183.528941	6605.969493	25.704218
183.908796	6627.717792	25.709236
184.113124	6632.339245	25.714253
184.201468	6634.232430	25.719271
184.296450	6651.914304	25.724288
184.423516	6668.983663	25.729306
184.880815	6669.398621	25.734324
184.550364	6678.130683	25.739341
184.925135	6692.817448	25.744359
185.540704	6695.896507	25.749376
185.207794	6725.584245	25.754394
185.810830	6735.346171	25.759412
185.972581	6733.097665	25.764429
186.197024	6750.325480	25.769447
186.489015	6753.825156	25.774464
186.495770	6757.490689	25.779482
186.914290	6744.055184	25.784500
187.022660	6770.993549	25.789517
187.106294	6792.334533	25.794535
187.520745	6787.528695	25.799552
187.366717	6802.182636	25.804570
187.678925	6802.132114	25.809588
188.029477	6819.065304	25.814605
187.922569	6818.942332	25.819623
187.964690	6823.179770	25.824640
188.047159	6852.439601	25.829658
188.365568	6845.457754	25.834676
188.374890	6866.158415	25.839693
188.624711	6892.942263	25.844711
188.711385	6889.986544	25.849728
189.035216	6911.716653	25.854746
189.471607	6915.525388	25.859764
189.537957	6926.131502	25.864781
190.080867	6933.480506	25.869799
190.251767	6938.301730	25.874816
190.453828	6941.449913	25.879834
190.872560	6933.865845	25.884852
190.636389	6952.351502	25.889869
190.606412	6961.208929	25.894887
191.205126	6967.711081	25.899904
190.929160	6981.257111	25.904922
190.948942	6979.954939	25.909940
191.566447	7004.760507	25.914957
191.624920	7010.071777	25.919975
191.676788	7010.620623	25.924992
191.699396	7037.038884	25.930010
192.043525	7041.566576	25.935028
192.235175	7045.722801	25.940045
191.991220	7064.921136	25.945063
192.792767	7063.208706	25.950080
193.248097	7087.576036	25.955098
193.374004	7081.799513	25.960116
193.781990	7088.048865	25.965133
193.755080	7083.642193	25.970151
193.918239	7095.275551	25.975168
194.146441	7111.751759	25.980186
194.553540	7119.349117	25.985204
194.530088	7123.242231	25.990221
194.793809	7126.523042	25.995239
194.901460	7134.870005	26.000256
194.811612	7151.968992	26.005274
194.606910	7148.612748	26.010292
195.058763	7178.257324	26.015309
195.163900	7181.797907	26.020327
195.585538	7195.681417	26.025344
195.593380	7217.395074	26.030362
195.908901	7220.971369	26.035380
196.222038	7244.161689	26.040397
196.399083	7251.993289	26.045415
196.859344	7247.984158	26.050432
196.996373	7268.441555	26.055450
197.470178	7264.839420	26.060468
197.710409	7274.178782	26.065485
197.984627	7278.797952	26.070503
198.253189	7268.599362	26.075520
198.340698	7287.774255	26.080538
198.614847	7288.806995	26.085556
198.495291	7296.755144	26.090573
198.535748	7302.288134	26.095591
199.068357	7292.068679	26.100608
198.721757	7311.676331	26.105626
198.533108	7325.838230	26.110644
198.950288	7342.800740	26.115661
199.067985	7361.780498	26.120679
199.056822	7365.515920	26.125696
199.155470	7396.124476	26.130714
199.758626	7399.650239	26.135732
199.860756	7426.215457	26.140749
199.999242	7437.085834	26.145767
200.223636	7465.503556	26.150784
200.620341	7469.184212	26.155802
200.932359	7484.241360	26.160820
201.874526	7480.042037	26.165837
202.156637	7475.176820	26.170855
202.370946	7480.722291	26.175872
202.117550	7479.731157	26.180890
202.174965	7474.343880	26.185908
202.340105	7482.992682	26.190925
202.480974	7482.869545	26.195943
203.060031	7492.158178	26.200960
203.277499	7499.073070	26.205978
203.321057	7509.757986	26.210996
203.490832	7505.230920	26.216013
203.440826	7509.964010	26.221031
203.957573	7510.267231	26.226048
203.660380	7528.854605	26.231066
203.958181	7530.996997	26.236084
204.153681	7531.807808	26.241101
204.303241	7552.987510	26.246119
204.146369	7562.075615	26.251136
204.583794	7589.014150	26.256154
204.712681	7597.202188	26.261172
204.695080	7599.613619	26.266189
204.695231	7631.750711	26.271207
205.110449	7639.406845	26.276224
205.316959	7662.931924	26.281242
205.468796	7691.743275	26.286260
205.910369	7695.168972	26.291277
205.726751	7718.927869	26.296295
206.312125	7733.437309	26.301312
206.872518	7752.566530	26.306330
206.777169	7753.370999	26.311348
207.407919	7775.457897	26.316365
207.464068	7795.381249	26.321383
207.730500	7798.287227	26.326400
207.717923	7800.470482	26.331418
208.205990	7824.558398	26.336436
208.598109	7827.837783	26.341453
208.561044	7832.657043	26.346471
208.694037	7848.171159	26.351488
208.906924	7860.810686	26.356506
208.667643	7865.497735	26.361524
209.019489	7884.251195	26.366541
209.100957	7902.742471	26.371559
209.530225	7922.370449	26.376576
209.589960	7940.554420	26.381594
209.583387	7964.416104	26.386612
210.243081	7972.215208	26.391629
210.251125	7983.778777	26.396647
210.744327	8000.100413	26.401664
210.720908	8013.787312	26.406682
211.019981	8030.031338	26.411700
211.393795	8024.127589	26.416717
212.238561	8032.205681	26.421735
212.806487	8031.342463	26.426752
212.947132	8035.269459	26.431770
213.044166	8032.642356	26.436788
213.359956	8024.795594	26.441805
213.082625	8032.955777	26.446823
213.245683	8027.545165	26.451840
213.298522	8036.484454	26.456858
213.364221	8035.786281	26.461876
213.765029	8037.002688	26.466893
213.814494	8053.516302	26.471911
213.911558	8058.231629	26.476928
213.878659	8057.967403	26.481946
213.881721	8078.310351	26.486964
214.767418	8084.718467	26.491981
214.645145	8097.994315	26.496999
214.943737	8118.672634	26.502016
214.801505	8128.950493	26.507034
214.935279	8139.598658	26.512052
215.339238	8154.515533	26.517069
215.229075	8177.755116	26.522087
215.503681	8190.461019	26.527104
215.879840	8201.950731	26.532122
216.164199	8219.577916	26.537140
216.515996	8227.357385	26.542157
217.081796	8246.979372	26.547175
217.557751	8242.691280	26.552192
217.576774	8251.161983	26.557210
217.575349	8267.225578	26.562228
218.037659	8273.765796	26.567245
217.864151	8280.950727	26.572263
218.148678	8299.561210	26.577280
218.064221	8317.088743	26.582298
218.326148	8323.161245	26.587316
218.931013	8334.079508	26.592333
219.073514	8352.441216	26.597351
219.077575	8366.347930	26.602368
219.417052	8379.264774	26.607386
219.200228	8399.139591	26.612404
219.773032	8398.317677	26.617421
220.057748	8421.573381	26.622439
220.360540	8439.601178	26.627456
220.451767	8444.549695	26.632474
220.236168	8467.490985	26.637492
220.543621	8484.613542	26.642509
220.802109	8508.215473	26.647527
220.938552	8520.985389	26.652544
221.401985	8538.153177	26.657562
221.604785	8545.179490	26.662580
222.463154	8558.602777	26.667597
222.159364	8571.118311	26.672615
222.935537	8589.664554	26.677632
222.957613	8597.206406	26.682650
223.195906	8603.398860	26.687668
223.609561	8608.589554	26.692685
223.557402	8622.728559	26.697703
223.591751	8638.759307	26.702720
223.928589	8637.226246	26.707738
224.010694	8660.924604	26.712756
224.455910	8658.927295	26.717773
224.169360	8672.401780	26.722791
224.630384	8690.774901	26.727808
224.564647	8702.094250	26.732826
224.806321	8716.712167	26.737844
225.570453	8719.054642	26.742861
225.337367	8731.543300	26.747879
225.793034	8760.503042	26.752896
225.967552	8769.762537	26.757914
226.148605	8785.127926	26.762932
226.312811	8790.315167	26.767949
226.360192	8806.299949	26.772967
226.607731	8826.810330	26.777984
227.082076	8833.632959	26.783002
226.962637	8861.065862	26.788020
227.232718	8870.815394	26.793037
227.979655	8886.919713	26.798055
228.223591	8894.426349	26.803072
228.846141	8895.857729	26.808090
228.557918	8914.313575	26.813108
228.945756	8918.016865	26.818125
229.130745	8927.425486	26.823143
229.537041	8947.487750	26.828160
229.896024	8945.666653	26.833178
229.706109	8956.756530	26.838196
230.229157	8963.675725	26.843213
230.614105	8986.540176	26.848231
230.372456	8992.291888	26.853248
230.880915	8993.000565	26.858266
230.790940	9015.186487	26.863284
230.701152	9022.312783	26.868301
230.939338	9033.614625	26.873319
231.154794	9052.268534	26.878336
231.706276	9070.288534	26.883354
231.536321	9095.457235	26.888372
232.177985	9112.276596	26.893389
232.245858	9119.379380	26.898407
232.253061	9143.301734	26.903424
232.544884	9147.214762	26.908442
232.565437	9185.383469	26.913460
232.936873	9188.101432	26.918477
233.247480	9217.729298	26.923495
233.253723	9241.875849	26.928512
233.868210	9246.940715	26.933530
234.042644	9277.276625	26.938548
234.097316	9294.534051	26.943565
234.614113	9313.414109	26.948583
234.621966	9322.808326	26.953600
235.132535	9348.666943	26.958618
235.214643	9360.060803	26.963636
235.460446	9370.915089	26.968653
235.957445	9390.250900	26.973671
236.074134	9402.195657	26.978688
236.822993	9406.846861	26.983706
236.709499	9422.797348	26.988724
237.281812	9420.374401	26.993741
237.420845	9421.860482	26.998759
237.431660	9444.004607	27.003776
237.655307	9447.804636	27.008794
237.617152	9454.262253	27.013812
237.922949	9465.339592	27.018829
238.062220	9481.242373	27.023847
238.171237	9496.193835	27.028864
238.629319	9506.790098	27.033882
238.647148	9518.308040	27.038900
238.895089	9534.552411	27.043917
239.384839	9541.497253	27.048935
239.543123	9565.532341	27.053952
239.939394	9565.127277	27.058970
240.300783	9595.411994	27.063988
240.568364	9595.448863	27.069005
240.735058	9607.976040	27.074023
240.937612	9624.041625	27.079040
241.161517	9623.763585	27.084058
241.083703	9631.207376	27.089076
241.555684	9657.699894	27.094093
242.129829	9654.994883	27.099111
242.275681	9681.864841	27.104128
242.562126	9685.340132	27.109146
242.488839	9683.460758	27.114164
242.732853	9711.822961	27.119181
243.214392	9717.685925	27.124199
243.096268	9734.487018	27.129216
243.833318	9739.854392	27.134234
243.879187	9748.291756	27.139252
243.917016	9771.374066	27.144269
244.217121	9787.404996	27.149287
244.357351	9784.625506	27.154304
244.984593	9809.847365	27.159322
244.980815	9825.784725	27.164340
245.485777	9841.731118	27.169357
245.783949	9850.844475	27.174375
245.306025	9864.841603	27.179392
245.659892	9872.068750	27.184410
246.055549	9902.174308	27.189428
246.078511	9926.851295	27.194445
246.455227	9938.866783	27.199463
246.575774	9960.987095	27.204480
246.733696	9981.891881	27.209498
247.062186	9994.328664	27.214516
246.889781	10025.645295	27.219533
247.508059	10039.840885	27.224551
247.673515	10069.033572	27.229568
248.124157	10078.640212	27.234586
248.168659	10101.465404	27.239604
248.437455	10128.006879	27.244621
249.261381	10148.325670	27.249639
249.567201	10154.484790	27.254656
250.033358	10145.519039	27.259674
250.248306	10174.844128	27.264692
250.335009	10186.680568	27.269709
250.773436	10187.717636	27.274727
250.592918	10199.303130	27.279744
251.021858	10197.475066	27.284762
251.210713	10219.545914	27.289780
251.462043	10229.460657	27.294797
251.739052	10230.025286	27.299815
251.589792	10253.355368	27.304832
251.938118	10252.995315	27.309850
252.171383	10276.740203	27.314868
252.456771	10284.313336	27.319885
252.964919	10301.633819	27.324903
253.014332	10315.789704	27.329920
253.535046	10316.536246	27.334938
253.458469	10344.261719	27.339956
253.568802	10363.397954	27.344973
254.029261	10374.169958	27.349991
254.009009	10389.207840	27.355008
254.228949	10406.056138	27.360026
254.507834	10432.109382	27.365044
254.788530	10452.956296	27.370061
255.459884	10460.678130	27.375079
255.417591	10479.557483	27.380096
255.865590	10495.671842	27.385114
256.562991	10515.658522	27.390132
256.255152	10520.645757	27.395149
256.770246	10537.317299	27.400167
257.078434	10553.461875	27.405184
257.233585	10557.650088	27.410202
257.187440	10577.439576	27.415220
257.319776	10596.493111	27.420237
257.429926	10604.830595	27.425255
257.547456	10632.770814	27.430272
257.892698	10656.813261	27.435290
258.591378	10667.489660	27.440308
258.873674	10692.084456	27.445325
258.907656	10713.616022	27.450343
259.418365	10724.632511	27.455360
259.893276	10741.862784	27.460378
259.829079	10754.520981	27.465396
260.186964	10780.350918	27.470413
260.523679	10785.303974	27.475431
260.509059	10817.669816	27.480448
260.761434	10822.335681	27.485466
261.341013	10847.239871	27.490484
261.333312	10864.195798	27.495501
261.762812	10873.888171	27.500519
261.916893	10895.716848	27.505536
262.054541	10912.887741	27.510554
262.462303	10934.584743	27.515572
262.924985	10950.657899	27.520589
263.452201	10942.845585	27.525607
263.367012	10972.528190	27.530624
263.822332	10978.823590	27.535642
264.359866	10983.708106	27.540660
264.597104	11001.469246	27.545677
265.134293	11003.185985	27.550695
265.102865	11021.609767	27.555712
265.245964	11019.443094	27.560730
265.394319	11010.545594	27.565748
265.309189	11041.368354	27.570765
265.737225	11036.057282	27.575783
265.992430	11054.924172	27.580800
266.442117	11073.464158	27.585818
266.863097	11077.617622	27.590836
266.591159	11100.835947	27.595853
266.889973	11111.513830	27.600871
267.338558	11123.107582	27.605888
267.376890	11134.358255	27.610906
267.801088	11138.566711	27.615924
267.826887	11171.270021	27.620941
268.256153	11169.034104	27.625959
268.197218	11203.271569	27.630976
268.336025	11217.464815	27.635994
269.061529	11233.154802	27.641012
269.088722	11253.893296	27.646029
269.081436	11278.841762	27.651047
269.641266	11305.399133	27.656064
269.902765	11334.447522	27.661082
270.248404	11345.623398	27.666100
270.236147	11373.178764	27.671117
270.837729	11393.136039	27.676135
270.751029	11416.481160	27.681152
271.051231	11443.546489	27.686170
271.496454	11462.718891	27.691188
271.526981	11483.334385	27.696205
271.787616	11500.150462	27.701223
272.327065	11525.585373	27.706240
272.507251	11546.060416	27.711258
273.117415	11562.886179	27.716276
273.053388	11582.666844	27.721293
273.887613	11602.400388	27.726311
274.180036	11614.166198	27.731328
274.345399	11639.863794	27.736346
274.964538	11648.029231	27.741364
275.037029	11653.098871	27.746381
275.327761	11669.893615	27.751399
275.739807	11672.849561	27.756416
276.192271	11688.464695	27.761434
276.466883	11708.751752	27.766452
276.576985	11717.185685	27.771469
276.604784	11722.230398	27.776487
277.022719	11737.206862	27.781504
277.050471	11752.176268	27.786522
277.478277	11768.210599	27.791540
277.753204	11781.866158	27.796557
277.556710	11794.200780	27.801575
278.451959	11812.661608	27.806592
278.224362	11836.401334	27.811610
278.850724	11839.810952	27.816628
278.965301	11853.785519	27.821645
279.295357	11867.670068	27.826663
279.633643	11871.550043	27.831680
279.591900	11904.367431	27.836698
280.053997	11904.176935	27.841716
280.218878	11925.688574	27.846733
280.440983	11941.790508	27.851751
280.542370	11954.812924	27.856768
280.858142	11969.408225	27.861786
281.422605	11979.171695	27.866804
281.854485	11997.676302	27.871821
282.237838	12004.722686	27.876839
282.694396	12021.561049	27.881856
282.616736	12027.503823	27.886874
283.181626	12044.021323	27.891892
283.282308	12064.275185	27.896909
283.130082	12062.489559	27.901927
283.566237	12091.769535	27.906944
283.361765	12118.643583	27.911962
284.082237	12132.231398	27.916980
283.794716	12159.300377	27.921997
284.071912	12183.087108	27.927015
284.533853	12199.170176	27.932032
284.747075	12229.974166	27.937050
285.260960	12244.955322	27.942068
285.173541	12274.304932	27.947085
285.953575	12298.665787	27.952103
285.915712	12315.749162	27.957120
286.257205	12351.749519	27.962138
286.738922	12369.904638	27.967156
287.218044	12398.154129	27.972173
287.331282	12422.792459	27.977191
287.979209	12442.863380	27.982208
288.031655	12469.693754	27.987226
288.688783	12477.060964	27.992244
288.807431	12492.271834	27.997261
288.820712	12520.550146	28.002279
289.668903	12536.523212	28.007296
289.860926	12541.567211	28.012314
290.739735	12553.039382	28.017332
290.879582	12574.319204	28.022349
290.972929	12577.365877	28.027367
291.162262	12581.561800	28.032384
291.189439	12609.726489	28.037402
291.476394	12613.824607	28.042420
291.811963	12632.956740	28.047437
292.329596	12643.533730	28.052455
292.180252	12668.159996	28.057472
292.287429	12687.207578	28.062490
292.861740	12703.066258	28.067508
293.062980	12723.716050	28.072525
292.874476	12742.387546	28.077543
293.499562	12755.227611	28.082560
293.590106	12773.609676	28.087578
294.068051	12802.450851	28.092596
294.383068	12817.009504	28.097613
294.397110	12841.672194	28.102631
294.878187	12855.917506	28.107648
295.110075	12883.104919	28.112666
295.608740	12900.270115	28.117684
295.303444	12923.439072	28.122701
295.826959	12948.531197	28.127719
296.262831	12975.843693	28.132736
296.317273	12995.960740	28.137754
296.441654	13011.119461	28.142772
297.287139	13034.965036	28.147789
297.446835	13059.442417	28.152807
297.760916	13082.823627	28.157824
298.044543	13108.000985	28.162842
298.788118	13117.505916	28.167860
299.351343	13137.887130	28.172877
299.255048	13152.340944	28.177895
299.955285	13163.464211	28.182912
299.813107	13185.843636	28.187930
300.290800	13195.391780	28.192948
300.415181	13213.021088	28.197965
300.989772	13232.206798	28.202983
301.502743	13253.599899	28.208000
301.367512	13264.219485	28.213018
301.924378	13280.702718	28.218036
301.822409	13291.432537	28.223053
302.348025	13318.309231	28.228071
302.757714	13327.429356	28.233088
302.996111	13346.008953	28.238106
302.990327	13358.830428	28.243124
303.522758	13387.708135	28.248141
303.902762	13401.157914	28.253159
303.974995	13418.962650	28.258176
304.531544	13456.885685	28.263194
304.358938	13463.766218	28.268212
304.959652	13488.979472	28.273229
304.778853	13511.967616	28.278247
305.572281	13529.767647	28.283264
305.687850	13561.989683	28.288282
305.631414	13580.103711	28.293300
305.882241	13618.048812	28.298317
306.306911	13627.893982	28.303335
306.777799	13663.804401	28.308352
306.944004	13689.526580	28.313370
307.277060	13717.456133	28.318388
307.591577	13741.446579	28.323405
307.824574	13769.453178	28.328423
308.669172	13787.364812	28.333440
308.738109	13820.023940	28.338458
309.197748	13836.035216	28.343476
309.484803	13847.435115	28.348493
309.784966	13861.150909	28.353511
310.257199	13880.261060	28.358528
310.170559	13912.106131	28.363546
310.452835	13933.214403	28.368564
311.171567	13948.436968	28.373581
310.972637	13971.781747	28.378599
311.608741	13985.309405	28.383616
311.831020	14012.319897	28.388634
312.155134	14032.874243	28.393652
311.995844	14055.291613	28.398669
312.037291	14086.485693	28.403687
312.496842	14107.576188	28.408704
312.633131	14150.301365	28.413722
312.950339	14175.162612	28.418740
313.728709	14202.302871	28.423757
314.239985	14237.432190	28.428775
314.793771	14236.491327	28.433792
315.106335	14259.772935	28.438810
315.513163	14293.002297	28.443828
316.167585	14302.217536	28.448845
316.411626	14317.213047	28.453863
316.960215	14325.392468	28.458880
317.266783	14341.751822	28.463898
317.402058	14361.381126	28.468916
318.105639	14368.819112	28.473933
318.002513	14377.587250	28.478951
318.469786	14383.314301	28.483968
318.493143	14411.121488	28.488986
318.785792	14421.469105	28.494004
318.813512	14434.041119	28.499021
318.991714	14456.396729	28.504039
319.799972	14480.197077	28.509056
319.878955	14505.040344	28.514074
319.750402	14525.225762	28.519092
320.186118	14544.277915	28.524109
320.369552	14579.655229	28.529127
320.868782	14605.969825	28.534144
321.220388	14626.795823	28.539162
321.452872	14649.460316	28.544180
322.166610	14667.415396	28.549197
322.864673	14694.342215	28.554215
323.148180	14705.003914	28.559232
323.259806	14728.442150	28.564250
323.371940	14740.020955	28.569268
324.157201	14759.281492	28.574285
323.965051	14777.253538	28.579303
324.668942	14797.829376	28.584320
324.505538	14817.833370	28.589338
324.928403	14834.203452	28.594356
325.409244	14857.605186	28.599373
325.688374	14888.462196	28.604391
325.843814	14896.034933	28.609408
326.074120	14923.245221	28.614426
326.018701	14955.825916	28.619444
327.083305	14968.323067	28.624461
327.064130	15000.203336	28.629479
327.764742	15014.682073	28.634496
327.692235	15041.118744	28.639514
328.025820	15058.475055	28.644532
328.417306	15080.512994	28.649549
328.736706	15099.650504	28.654567
329.020875	15114.257994	28.659584
329.379880	15142.389616	28.664602
329.268455	15169.880545	28.669620
330.098619	15188.930374	28.674637
329.935913	15215.259693	28.679655
330.209828	15238.015385	28.684672
330.552095	15274.263608	28.689690
331.011805	15291.517618	28.694708
331.432934	15326.570044	28.699725
331.983702	15348.795153	28.704743
332.418672	15375.201614	28.709760
332.711692	15391.197285	28.714778
332.975895	15417.587536	28.719796
333.499589	15435.253487	28.724813
334.298717	15445.919050	28.729831
334.445044	15463.619586	28.734848
335.002123	15467.677403	28.739866
335.146505	15496.952749	28.744884
335.631526	15493.132998	28.749901
335.836248	15522.167121	28.754919
335.976974	15524.945853	28.759936
336.353262	15552.798747	28.764954
336.612592	15566.868784	28.769972
337.122251	15586.105597	28.774989
337.205267	15606.088862	28.780007
337.603426	15629.149594	28.785024
337.892050	15643.199681	28.790042
338.072427	15679.553191	28.795060
338.199370	15688.431845	28.800077
338.341320	15714.002648	28.805095
338.539390	15749.428051	28.810112
339.529029	15773.387312	28.815130
339.806944	15814.759902	28.820148
340.218870	15824.367715	28.825165
339.977566	15850.240533	28.830183
340.367501	15882.080262	28.835200
341.439097	15896.485859	28.840218
342.414705	15903.538094	28.845236
343.041218	15913.349333	28.850253
343.602044	15926.572354	28.855271
343.873350	15926.215815	28.860288
344.034384	15919.185240	28.865306
343.949363	15933.765348	28.870324
344.695566	15955.708063	28.875341
344.639875	15968.977407	28.880359
344.784538	15980.593001	28.885376
345.062678	16000.692121	28.890394
345.338175	16005.081533	28.895412
345.592839	16022.551500	28.900429
345.822696	16049.266575	28.905447
345.866830	16059.161070	28.910464
346.115663	16084.235989	28.915482
346.118972	16120.251086	28.920500
346.531867	16135.815686	28.925517
346.952956	16172.240057	28.930535
346.787002	16203.463019	28.935552
347.457985	16224.795345	28.940570
347.656352	16249.935064	28.945588
348.240764	16281.675150	28.950605
348.642112	16315.978641	28.955623
348.963102	16350.037167	28.960640
349.019495	16373.400892	28.965658
349.159889	16417.370951	28.970676
349.701597	16434.954878	28.975693
349.926446	16470.501477	28.980711
350.219051	16517.995830	28.985728
350.974215	16532.581577	28.990746
351.090155	16569.241518	28.995764
351.664770	16607.224388	29.000781
351.998999	16629.861611	29.005799
352.374741	16661.080466	29.010816
353.274895	16691.386557	29.015834
353.165164	16729.840562	29.020852
353.891548	16738.761885	29.025869
354.270676	16758.697487	29.030887
354.605306	16793.063453	29.035904
355.242432	16811.531943	29.040922
356.101654	16816.385614	29.045940
356.749931	16829.062057	29.050957
357.176626	16837.326920	29.055975
357.305796	16860.114866	29.060992
357.910041	16856.942866	29.066010
357.742632	16870.632722	29.071028
357.955460	16881.280921	29.076045
358.331419	16901.106394	29.081063
358.323577	16926.907392	29.086080
358.721129	16942.363451	29.091098
358.975315	16969.225837	29.096116
359.100774	16991.477203	29.101133
359.606875	17015.009196	29.106151
359.679332	17041.156226	29.111168
360.329076	17071.356917	29.116186
360.750113	17105.466123	29.121204
360.799610	17122.033667	29.126221
361.633644	17140.457594	29.131239
362.052417	17161.982584	29.136256
362.424258	17184.368973	29.141274
362.480041	17209.899687	29.146292
363.008842	17240.963048	29.151309
363.111392	17269.584281	29.156327
363.043260	17296.763544	29.161344
363.954125	17306.025078	29.166362
363.911789	17337.256016	29.171380
364.384564	17368.173842	29.176397
364.699366	17404.276929	29.181415
365.199377	17438.303027	29.186432
365.959608	17452.739244	29.191450
366.251427	17478.068227	29.196468
367.175583	17486.945091	29.201485
367.294802	17511.269385	29.206503
367.067674	17532.847028	29.211520
367.840541	17546.641577	29.216538
367.974696	17571.754506	29.221556
368.124746	17590.038365	29.226573
368.338488	17614.118237	29.231591
368.949152	17634.576722	29.236608
369.640448	17654.889711	29.241626
370.201120	17675.918802	29.246644
370.309319	17681.200690	29.251661
370.836014	17706.875682	29.256679
371.009722	17726.297247	29.261696
371.522331	17740.041317	29.266714
371.594091	17778.349316	29.271732
372.044458	17798.891435	29.276749
372.667623	17816.458056	29.281767
372.516094	17843.037005	29.286784
373.401772	17869.607416	29.291802
373.177190	17902.104343	29.296820
373.848057	17923.823292	29.301837
374.148281	17947.539511	29.306855
374.197422	17985.609499	29.311872
374.860720	18002.780963	29.316890
374.863858	18043.993851	29.321908
375.209239	18072.015665	29.326925
375.925780	18097.272077	29.331943
376.223611	18144.341447	29.336960
376.644628	18160.074909	29.341978
376.853716	18193.695083	29.346996
377.081143	18221.716276	29.352013
377.506729	18252.718585	29.357031
377.870746	18283.330365	29.362048
378.819134	18313.553023	29.367066
378.749689	18346.410020	29.372084
379.315663	18371.791267	29.377101
380.055359	18388.500977	29.382119
380.026788	18427.838001	29.387136
380.791369	18445.061142	29.392154
380.761770	18481.640519	29.397172
381.269885	18504.102379	29.402189
381.953139	18526.225331	29.407207
382.311475	18563.615949	29.412224
382.392941	18580.450435	29.417242
382.835104	18619.644035	29.422260
383.095932	18652.545905	29.427277
383.467283	18678.850433	29.432295
383.227021	18718.438859	29.437312
383.928709	18752.709338	29.442330
384.448973	18795.612368	29.447348
384.905752	18823.150045	29.452365
385.141205	18854.441735	29.457383
385.381240	18885.572907	29.462400
386.016914	18920.034599	29.467418
386.543096	18950.286401	29.472436
386.410745	18977.985944	29.477453
387.248133	19005.757410	29.482471
387.847434	19023.230774	29.487488
388.190921	19048.630466	29.492506
388.366457	19083.193792	29.497524
388.903238	19110.961767	29.502541
389.202609	19128.628719	29.507559
389.385232	19162.934775	29.512576
390.085307	19184.907944	29.517594
390.204174	19221.511857	29.522612
390.571546	19255.726863	29.527629
391.122456	19284.906393	29.532647
391.116573	19318.836495	29.537664
391.551070	19345.039559	29.542682
391.989006	19388.223107	29.547700
392.149248	19425.628062	29.552717
392.910937	19449.191535	29.557735
392.995925	19485.356935	29.562752
393.553853	19518.712944	29.567770
394.022050	19557.971296	29.572788
394.633982	19589.641129	29.577805
395.091034	19614.973250	29.582823
395.352348	19650.259275	29.587840
395.734610	19678.580101	29.592858
396.540644	19710.803173	29.597876
396.734330	19752.404030	29.602893
397.368770	19765.399698	29.607911
397.586291	19801.091904	29.612928
397.817609	19825.127506	29.617946
398.269483	19855.240129	29.622964
398.576047	19886.699742	29.627981
399.112505	19915.638631	29.632999
399.292324	19959.148381	29.638016
399.855554	19989.444726	29.643034
400.479287	20024.233636	29.648052
400.420906	20056.342364	29.653069
401.136686	20082.967263	29.658087
401.452226	20113.166287	29.663104
401.936846	20145.463912	29.668122
402.485779	20170.934284	29.673140
402.360564	20203.828871	29.678157
403.110360	20230.093434	29.683175
403.766916	20271.271868	29.688192
404.893065	20289.504564	29.693210
405.143045	20318.572140	29.698228
405.323516	20326.587118	29.703245
405.720161	20359.052373	29.708263
405.615104	20385.441984	29.713280
405.899542	20415.315394	29.718298
406.495007	20433.802131	29.723316
406.406747	20484.672134	29.728333
407.318607	20517.548619	29.733351
407.398759	20551.812221	29.738368
407.608484	20574.688053	29.743386
408.238640	20609.666641	29.748404
408.327427	20638.247022	29.753421
408.803475	20665.079641	29.758439
409.357992	20696.313152	29.763456
409.303847	20742.958940	29.768474
409.833580	20766.745648	29.773492
410.197096	20812.440690	29.778509
410.522373	20845.798794	29.783527
410.752591	20892.498160	29.788544
411.491249	20924.002052	29.793562
411.943139	20956.016351	29.798580
412.098058	21000.912738	29.803597
412.816162	21036.446089	29.808615
413.290687	21078.558968	29.813632
413.442238	21118.081167	29.818650
414.164908	21149.174592	29.823668
414.195083	21188.274485	29.828685
414.819267	21223.721629	29.833703
414.797810	21267.074902	29.838720
415.393839	21305.732102	29.843738
416.009073	21356.599153	29.848756
416.209833	21398.628921	29.853773
416.883648	21435.339773	29.858791
417.362021	21482.125785	29.863808
417.680781	21523.537740	29.868826
418.244772	21555.890596	29.873844
418.806417	21596.732431	29.878861
419.370209	21628.778312	29.883879
419.744838	21669.393380	29.888896
420.394880	21698.379287	29.893914
420.740159	21737.231077	29.898932
420.758056	21778.292329	29.903949
421.365101	21808.317032	29.908967
421.930115	21839.144744	29.913984
422.199451	21873.463773	29.919002
422.890367	21901.574827	29.924020
423.057267	21948.070818	29.929037
423.628159	21983.566756	29.934055
424.060540	22023.628515	29.939072
424.058058	22051.796754	29.944090
424.860266	22087.626246	29.949108
425.046328	22139.001320	29.954125
425.478748	22166.683042	29.959143
425.660494	22220.900761	29.964160
426.464446	22249.787551	29.969178
426.948084	22296.052950	29.974196
427.172863	22338.711482	29.979213
427.860214	22361.168046	29.984231
428.461871	22396.326061	29.989248
428.802349	22435.087392	29.994266
429.307847	22464.892450	29.999284
429.403961	22500.276950	30.004301
430.213647	22533.460631	30.009319
430.698684	22562.214500	30.014336
430.933021	22599.650238	30.019354
431.455519	22630.839917	30.024372
431.669491	22661.525106	30.029389
431.815005	22694.201375	30.034407
431.909927	22732.011710	30.039424
432.927643	22781.118721	30.044442
433.526889	22795.919913	30.049460
433.520980	22839.146628	30.054477
434.385317	22852.455591	30.059495
434.600787	22895.060394	30.064512
434.824886	22933.839124	30.069530
435.383275	22963.082979	30.074548
436.102909	22996.500946	30.079565
436.436146	23020.987931	30.084583
436.869082	23057.811824	30.089600
437.180465	23089.517297	30.094618
437.597872	23113.494792	30.099636
438.316399	23158.474492	30.104653
438.905548	23187.379894	30.109671
439.205065	23222.889557	30.114688
439.504461	23259.200371	30.119706
440.049078	23288.376919	30.124724
439.988091	23332.432133	30.129741
440.778253	23370.019012	30.134759
441.097914	23412.011550	30.139776
441.776285	23446.338925	30.144794
442.042222	23480.325641	30.149812
442.350820	23527.369236	30.154829
442.538294	23561.852260	30.159847
443.137790	23596.692701	30.164864
443.570750	23645.232327	30.169882
444.188439	23685.193935	30.174900
444.511100	23731.905068	30.179917
444.716388	23762.217253	30.184935
445.358033	23806.589552	30.189952
445.761923	23854.171890	30.194970
446.296814	23890.727047	30.199988
446.809658	23942.807354	30.205005
446.885994	23989.067749	30.210023
447.807734	24033.317288	30.215040
447.797734	24078.429048	30.220058
448.162748	24123.881346	30.225076
448.775897	24173.840892	30.230093
449.384745	24217.989553	30.235111
449.822889	24251.925274	30.240128
450.168131	24294.661240	30.245146
450.938004	24331.021642	30.250164
451.328681	24380.152365	30.255181
451.826869	24421.172285	30.260199
452.953639	24440.957597	30.265216
453.436068	24465.782240	30.270234
453.811182	24499.656060	30.275252
454.403888	24528.831952	30.280269
454.870730	24565.564134	30.285287
455.620782	24588.214744	30.290304
455.964005	24624.167998	30.295322
456.135965	24633.472884	30.300340
456.293858	24665.324897	30.305357
456.569697	24705.942205	30.310375
457.036650	24725.867650	30.315392
457.127891	24764.356909	30.320410
457.451768	24795.711672	30.325428
458.211841	24839.586675	30.330445
458.715406	24861.400186	30.335463
459.075925	24905.079855	30.340480
459.194042	24940.468634	30.345498
459.795288	24980.794538	30.350516
460.385300	25020.878919	30.355533
460.456639	25066.710753	30.360551
460.854706	25107.159148	30.365568
460.953165	25163.701971	30.370586
461.641563	25207.052940	30.375604
461.814170	25267.809069	30.380621
462.555826	25312.494973	30.385639
463.123116	25358.040661	30.390656
463.574162	25412.589499	30.395674
464.227990	25447.285109	30.400692
465.177370	25484.386047	30.405709
465.761591	25514.166163	30.410727
466.932933	25544.928116	30.415744
467.017503	25578.737857	30.420762
467.593715	25605.863035	30.425780
468.433009	25632.179053	30.430797
468.697790	25673.558422	30.435815
468.987846	25693.295828	30.440832
469.187848	25736.614959	30.445850
469.868000	25758.607177	30.450868
469.876067	25789.918876	30.455885
470.316266	25846.753929	30.460903
470.908317	25870.257137	30.465920
471.331912	25925.119332	30.470938
471.450690	25975.562677	30.475956
471.919181	26007.426962	30.480973
472.283868	26048.551103	30.485991
473.035070	26094.903081	30.491008
472.989107	26146.403651	30.496026
473.581400	26187.445408	30.501044
474.222623	26235.767498	30.506061
474.333703	26291.095113	30.511079
474.882242	26338.614528	30.516096
475.256500	26386.837793	30.521114
475.592427	26445.649298	30.526132
476.161762	26498.056655	30.531149
476.701512	26555.204511	30.536167
477.375668	26603.612271	30.541184
477.813271	26666.891912	30.546202
478.391668	26704.352575	30.551220
478.857714	26753.530562	30.556237
479.502148	26796.413828	30.561255
480.048847	26838.737655	30.566272
480.444320	26894.315899	30.571290
480.852858	26928.251765	30.576308
481.515656	26964.914111	30.581325
482.266116	27004.456336	30.586343
483.046348	27029.120915	30.591360
483.098405	27073.969636	30.596378
483.644177	27100.452215	30.601396
484.157749	27137.483017	30.606413
484.140247	27192.118833	30.611431
484.890690	27235.413399	30.616448
485.040184	27276.968097	30.621466
485.512647	27318.929989	30.626484
485.936806	27362.530564	30.631501
486.409830	27406.115594	30.636519
486.852355	27450.268138	30.641536
487.307216	27512.741568	30.646554
487.855493	27558.278397	30.651572
488.479551	27612.983616	30.656589
488.542987	27662.803657	30.661607
489.177538	27709.633472	30.666624
490.166298	27758.291617	30.671642
490.598741	27807.254407	30.676660
491.148054	27855.562115	30.681677
491.362018	27899.993389	30.686695
492.096711	27938.226216	30.691712
492.429184	27984.455723	30.696730
492.747413	28036.231273	30.701748
493.447158	28092.265481	30.706765
493.380242	28145.900720	30.711783
494.184496	28202.744384	30.716800
494.526806	28255.052572	30.721818
494.990701	28301.416478	30.726836
496.066414	28359.660902	30.731853
496.717520	28403.056364	30.736871
497.448911	28434.002678	30.741888
497.769202	28481.439479	30.746906
498.505788	28526.113840	30.751924
499.352654	28562.243859	30.756941
499.519504	28600.355964	30.761959
499.993094	28640.078669	30.766976
500.275628	28684.278973	30.771994
500.861262	28726.355706	30.777012
501.380691	28776.212111	30.782029
501.471750	28829.227186	30.787047
502.237503	28869.839982	30.792064
502.435119	28920.565969	30.797082
502.715548	28977.220009	30.802100
503.242954	29021.788802	30.807117
503.906869	29081.615846	30.812135
504.290908	29133.048743	30.817152
505.143770	29176.809687	30.822170
505.855590	29208.487090	30.827188
506.387708	29255.807309	30.832205
507.123014	29300.647901	30.837223
507.928146	29331.002670	30.842240
508.486797	29372.683516	30.847258
508.433559	29409.289743	30.852276
509.382505	29437.683413	30.857293
509.718312	29475.234837	30.862311
509.803873	29519.317493	30.867328
510.373788	29549.497386	30.872346
510.747127	29593.113627	30.877364
511.309613	29635.788957	30.882381
511.310152	29697.028814	30.887399
511.923038	29739.228328	30.892416
512.567226	29771.640967	30.897434
512.646324	29827.988049	30.902452
513.405984	29879.171201	30.907469
513.524146	29938.643899	30.912487
514.349144	29994.486628	30.917504
514.606925	30052.183430	30.922522
515.195898	30112.131785	30.927540
515.933581	30151.600201	30.932557
516.286377	30206.007486	30.937575
517.413486	30248.354930	30.942592
517.734119	30304.611596	30.947610
518.213469	30352.989875	30.952628
518.807401	30398.664505	30.957645
519.362946	30442.659028	30.962663
519.964501	30481.727551	30.967680
520.387693	30538.699963	30.972698
520.617599	30589.293602	30.977716
521.567025	30627.588389	30.982733
522.144746	30689.211259	30.987751
522.411529	30736.997263	30.992768
523.382512	30784.606623	30.997786
523.478460	30837.033256	31.002804
524.506860	30876.636790	31.007821
524.871748	30930.656844	31.012839
525.344513	30985.969614	31.017856
526.116730	31018.862379	31.022874
526.055573	31066.227176	31.027892
526.925635	31113.768459	31.032909
527.338384	31168.708415	31.037927
527.461120	31217.574747	31.042944
527.994193	31275.315538	31.047962
528.161259	31325.505363	31.052980
529.275629	31393.485391	31.057997
529.465657	31455.165008	31.063015
530.164290	31508.266934	31.068032
530.780602	31558.994302	31.073050
531.096213	31617.979828	31.078068
531.634023	31673.503635	31.083085
532.005790	31731.326885	31.088103
532.580158	31778.360810	31.093120
533.839055	31820.558941	31.098138
534.130777	31891.687252	31.103156
534.825547	31935.873235	31.108173
535.428423	31989.099146	31.113191
535.591707	32040.718191	31.118208
536.132855	32090.596999	31.123226
536.877177	32134.386306	31.128244
537.821645	32169.889332	31.133261
538.065504	32212.972039	31.138279
538.279829	32261.309886	31.143296
539.029004	32305.169803	31.148314
539.444888	32354.806137	31.153332
539.930804	32397.686847	31.158349
540.243652	32457.194389	31.163367
540.917537	32489.262487	31.168384
541.772687	32533.638897	31.173402
542.464130	32578.610519	31.178420
542.728390	32624.736330	31.183437
543.154456	32681.181360	31.188455
543.758928	32722.176186	31.193472
544.374577	32769.075537	31.198490
544.536575	32825.747541	31.203508
545.713395	32865.360611	31.208525
546.237033	32921.474094	31.213543
546.456080	32970.703851	31.218560
547.210717	33012.534548	31.223578
547.520979	33067.966884	31.228596
548.088870	33115.051367	31.233613
548.390354	33171.446980	31.238631
549.043109	33232.510986	31.243648
549.533624	33282.057827	31.248666
549.904931	33343.748723	31.253684
550.656407	33400.891548	31.258701
551.445188	33459.529280	31.263719
551.780273	33514.396411	31.268736
552.293791	33576.010350	31.273754
552.770947	33623.599391	31.278772
553.375891	33678.762996	31.283789
553.802195	33741.077145	31.288807
554.394293	33813.860443	31.293824
554.827096	33873.120666	31.298842
555.036037	33937.688100	31.303860
555.651397	34008.562727	31.308877
556.518517	34058.409740	31.313895
557.143165	34125.096543	31.318912
557.829388	34179.342449	31.323930
558.571473	34229.187820	31.328948
559.108262	34291.380816	31.333965
559.976097	34352.523460	31.338983
560.237806	34402.576699	31.344000
561.038751	34445.346328	31.349018
562.112106	34508.028490	31.354036
562.379687	34555.979896	31.359053
563.002582	34605.619951	31.364071
563.305926	34653.083555	31.369088
563.704628	34698.022428	31.374106
564.160651	34758.566897	31.379124
564.546100	34822.972500	31.384141
565.520374	34879.671900	31.389159
566.120932	34931.701651	31.394176
566.304987	34985.249816	31.399194
566.593133	35045.262419	31.404212
567.138621	35099.267314	31.409229
567.787025	35155.967530	31.414247
567.972530	35213.495218	31.419264
568.508219	35283.593411	31.424282
568.967977	35348.383326	31.429300
569.662199	35406.040330	31.434317
570.462459	35454.261038	31.439335
570.857982	35530.594012	31.444352
571.299020	35587.344482	31.449370
571.697354	35651.398084	31.454388
572.676699	35707.905579	31.459405
573.307741	35765.651136	31.464423
574.063251	35826.776084	31.469440
574.909480	35890.570085	31.474458
575.117645	35953.286688	31.479476
575.788094	36008.130683	31.484493
576.800573	36076.209217	31.489511
576.947407	36138.652499	31.494528
577.906849	36179.701794	31.499546
578.390782	36239.398982	31.504564
578.910661	36291.548290	31.509581
579.872794	36339.652754	31.514599
580.178070	36407.096381	31.519616
581.076390	36465.484448	31.524634
581.324384	36516.637200	31.529652
582.286559	36569.029099	31.534669
582.959156	36616.355902	31.539687
583.520820	36672.507487	31.544704
583.972217	36716.103261	31.549722
584.705853	36779.604829	31.554740
584.908379	36832.375519	31.559757
585.537815	36875.364728	31.564775
585.758822	36945.816391	31.569792
586.407270	36996.427528	31.574810
586.768969	37063.596770	31.579828
587.307541	37125.749560	31.584845
588.117817	37199.093054	31.589863
588.255056	37275.481394	31.594880
589.414553	37330.849385	31.599898
589.891789	37407.554697	31.604916
590.206614	37475.387368	31.609933
590.917665	37529.952366	31.614951
591.362480	37599.614301	31.619968
591.938852	37661.938061	31.624986
592.500284	37737.026370	31.630004
593.244891	37808.676965	31.635021
593.764884	37873.098065	31.640039
594.334980	37947.418061	31.645056
595.073765	38005.683934	31.650074
595.869501	38073.972207	31.655092
596.460668	38131.199293	31.660109
597.625513	38174.876009	31.665127
599.270323	38211.813012	31.670144
600.101803	38250.062192	31.675162
600.711443	38287.356577	31.680180
600.998609	38319.968931	31.685197
601.735503	38350.907728	31.690215
601.623479	38392.588749	31.695232
602.298474	38419.155663	31.700250
602.785244	38467.294611	31.705268
603.096820	38528.372348	31.710285
603.898055	38560.625786	31.715303
604.232693	38615.782462	31.720320
604.757085	38662.496854	31.725338
604.982170	38721.890845	31.730356
605.555709	38783.665730	31.735373
606.409475	38822.168101	31.740391
606.727735	38879.308724	31.745408
607.005242	38925.960664	31.750426
607.712272	39006.521930	31.755444
608.397403	39067.174715	31.760461
608.973578	39128.685527	31.765479
609.229926	39196.908115	31.770496
609.654329	39267.966212	31.775514
609.930490	39346.304949	31.780532
610.731283	39416.338686	31.785549
611.337514	39481.103804	31.790567
611.848835	39564.956711	31.795584
612.830362	39630.988798	31.800602
613.307296	39703.357052	31.805620
613.842988	39779.316332	31.810637
614.922697	39844.179316	31.815655
615.690316	39917.601298	31.820672
616.698344	39983.660495	31.825690
617.199601	40046.367669	31.830708
617.884395	40108.845576	31.835725
618.738215	40161.597027	31.840743
619.127876	40235.331297	31.845760
619.667579	40299.080371	31.850778
620.584103	40345.757443	31.855796
620.920890	40418.108467	31.860813
621.720622	40479.981222	31.865831
622.405676	40534.694067	31.870848
623.076553	40596.073667	31.875866
623.606986	40662.162658	31.880884
624.143251	40728.679918	31.885901
625.174994	40783.609597	31.890919
625.581778	40844.401343	31.895936
626.092954	40908.191924	31.900954
627.094266	40969.734721	31.905972
626.855552	41037.237635	31.910989
627.642896	41093.238599	31.916007
628.570258	41161.868407	31.921024
629.028367	41233.834531	31.926042
629.730430	41299.889189	31.931060
629.833661	41373.555690	31.936077
630.839440	41432.080958	31.941095
631.459647	41515.345731	31.946112
631.777674	41572.943286	31.951130
632.458791	41634.943189	31.956148
632.917407	41703.693963	31.961165
634.682658	41734.834743	31.966183
635.345097	41781.931543	31.971200
636.163751	41828.861659	31.976218
636.829578	41876.393457	31.981236
637.313884	41919.213519	31.986253
638.050487	41974.383268	31.991271
638.260858	42025.296774	31.996288
639.517353	42070.880373	32.001306
640.191906	42097.807955	32.006324
640.356201	42166.045990	32.011341
640.934381	42220.427958	32.016359
641.040642	42275.935615	32.021376
641.731565	42329.331614	32.026394
642.181023	42402.748667	32.031412
642.111018	42479.535536	32.036429
643.243963	42535.129736	32.041447
643.663829	42608.309493	32.046464
644.076418	42691.900059	32.051482
644.967966	42756.311960	32.056500
645.192583	42844.330370	32.061517
646.088502	42918.807793	32.066535
646.827387	43000.243918	32.071552
647.472867	43073.752477	32.076570
648.194456	43144.968577	32.081588
648.866210	43229.939970	32.086605
649.571243	43302.168776	32.091623
650.363160	43371.223270	32.096640
650.759149	43444.798367	32.101658
651.777604	43520.195751	32.106676
652.266085	43593.220485	32.111693
652.935334	43665.964383	32.116711
653.418270	43748.015747	32.121728
654.323694	43824.858306	32.126746
655.445097	43874.023372	32.131764
655.723945	43958.347965	32.136781
656.763005	44019.883038	32.141799
657.224322	44092.097159	32.146816
657.981449	44159.586187	32.151834
658.784246	44228.298510	32.156852
659.587967	44306.118400	32.161869
659.876847	44364.143151	32.166887
661.028087	44430.557837	32.171904
661.752723	44504.693945	32.176922
662.459563	44557.621084	32.181940
663.013894	44627.914035	32.186957
663.393623	44685.423794	32.191975
664.201252	44761.692984	32.196992
664.654459	44833.267908	32.202010
664.945141	44894.758037	32.207028
665.462160	44977.746734	32.212045
666.230532	45045.571813	32.217063
666.722733	45135.288033	32.222080
667.210220	45207.442669	32.227098
668.073996	45279.597631	32.232116
668.355516	45365.483929	32.237133
669.004966	45427.593945	32.242151
669.919440	45498.312595	32.247168
670.424225	45573.311667	32.252186
670.953222	45653.014289	32.257204
671.265185	45732.937969	32.262221
671.911383	45810.499402	32.267239
672.499907	45898.238688	32.272256
673.525356	45988.022659	32.277274
674.448776	46057.593747	32.282292
674.700037	46149.817548	32.287309
675.312708	46227.553378	32.292327
676.728966	46298.498249	32.297344
677.332483	46376.529612	32.302362
678.963786	46441.058233	32.307380
679.983504	46500.690045	32.312397
680.638799	46565.156822	32.317415
681.498970	46611.411780	32.322432
681.796817	46681.880021	32.327450
682.951065	46731.073168	32.332468
683.550800	46803.143936	32.337485
684.258201	46857.264264	32.342503
684.804020	46914.045001	32.347520
685.032613	46985.670790	32.352538
685.430708	47040.790620	32.357556
686.059666	47126.055980	32.362573
686.350810	47194.343977	32.367591
686.983386	47280.313108	32.372608
687.620414	47353.364605	32.377626
688.762470	47430.996230	32.382644
689.124241	47513.990087	32.387661
690.197228	47575.822564	32.392679
691.110298	47653.232898	32.397696
691.460501	47732.140429	32.402714
692.239075	47803.909154	32.407732
692.838723	47887.302319	32.412749
693.348734	47956.385101	32.417767
694.246729	48046.786761	32.422784
694.767407	48125.047307	32.427802
695.428592	48203.572966	32.432820
696.372991	48279.292948	32.437837
697.153511	48345.071546	32.442855
698.926208	48402.116116	32.447872
699.619346	48471.802831	32.452890
700.284841	48529.008309	32.457908
700.761510	48596.757855	32.462925
701.228901	48663.120752	32.467943
701.894248	48731.686428	32.472960
702.312091	48806.400716	32.477978
703.208862	48872.806478	32.482996
703.783772	48937.540844	32.488013
704.045915	49015.237475	32.493031
704.983370	49082.426415	32.498048
705.508195	49152.622236	32.503066
706.073954	49231.855541	32.508084
706.800971	49289.817313	32.513101
707.374880	49373.395120	32.518119
708.218671	49436.097344	32.523136
708.555944	49528.498628	32.528154
709.537351	49585.991709	32.533172
709.897118	49672.123166	32.538189
710.331873	49749.063417	32.543207
710.922499	49834.524626	32.548224
711.340292	49911.218983	32.553242
712.345707	50012.080816	32.558260
712.939526	50092.102393	32.563277
714.070422	50177.113173	32.568295
714.886444	50256.626760	32.573312
715.409399	50346.405571	32.578330
716.456434	50428.130016	32.583348
717.095279	50518.440339	32.588365
717.705405	50594.182373	32.593383
718.267492	50680.305413	32.598400
719.027977	50778.506064	32.603418
719.976069	50858.178025	32.608436
721.435802	50931.993733	32.613453
722.194283	51001.746214	32.618471
722.892871	51075.737337	32.623488
723.590455	51161.762225	32.628506
723.935371	51232.768048	32.633524
724.322089	51313.976795	32.638541
724.818255	51412.276645	32.643559
725.747914	51500.169219	32.648576
726.517062	51595.822981	32.653594
727.389960	51672.714369	32.658612
727.887093	51758.445805	32.663629
728.656428	51844.566686	32.668647
729.439442	51939.633055	32.673664
729.810489	52028.548159	32.678682
731.136382	52120.546627	32.683700
731.696292	52207.592583	32.688717
732.146400	52306.510607	32.693735
733.125095	52381.993204	32.698752
733.836820	52473.258040	32.703770
734.536685	52566.431515	32.708788
734.986409	52657.912579	32.713805
735.725787	52748.085538	32.718823
736.645121	52841.244429	32.723840
737.872083	52929.361766	32.728858
738.459343	53009.627777	32.733876
739.646920	53080.191112	32.738893
740.657397	53172.503965	32.743911
741.657201	53243.299826	32.748928
742.487064	53320.047278	32.753946
742.970054	53403.200655	32.758964
743.564801	53475.251812	32.763981
743.784036	53557.538878	32.768999
744.961470	53640.456544	32.774016
745.658865	53725.111225	32.779034
746.062175	53785.619903	32.784052
746.723890	53852.646505	32.789069
747.597031	53930.008290	32.794087
748.569346	53998.655695	32.799104
749.288156	54091.070157	32.804122
749.840347	54152.241290	32.809140
750.499540	54240.426977	32.814157
750.849520	54317.482297	32.819175
751.777802	54395.402283	32.824192
751.949896	54489.187303	32.829210
752.618480	54572.433271	32.834228
753.466362	54667.115384	32.839245
753.747852	54760.186801	32.844263
754.563336	54860.083279	32.849280
755.353376	54958.361902	32.854298
755.909763	55060.194633	32.859316
756.627586	55162.826094	32.864333
757.694745	55265.282574	32.869351
758.304808	55361.836959	32.874368
759.048272	55471.382166	32.879386
759.568656	55577.106136	32.884404
761.133519	55678.402981	32.889421
761.979954	55774.132751	32.894439
763.269430	55860.019420	32.899456
764.399722	55942.942443	32.904474
765.364607	56025.522836	32.909492
766.645374	56099.931078	32.914509
767.171428	56176.716821	32.919527
767.898593	56255.405957	32.924544
768.429132	56342.713117	32.929562
769.339511	56414.580423	32.934580
770.303657	56494.631313	32.939597
770.238857	56582.665734	32.944615
771.256687	56668.552077	32.949632
771.677718	56769.108916	32.954650
772.345483	56863.038682	32.959668
773.659866	56928.662577	32.964685
774.572357	57020.881057	32.969703
775.387816	57096.301838	32.974720
776.109360	57183.582581	32.979738
776.491140	57266.981140	32.984756
777.553330	57357.447483	32.989773
777.969677	57445.974524	32.994791
778.870976	57528.615982	32.999808
780.021943	57618.760093	33.004826
780.052090	57714.402584	33.009844
780.607507	57806.138818	33.014861
781.281564	57914.105848	33.019879
782.073243	58008.315316	33.024896
782.609950	58114.196466	33.029914
783.043066	58223.712725	33.034932
784.254704	58324.622584	33.039949
784.729757	58426.868882	33.044967
785.485603	58537.074385	33.049984
786.866122	58647.995658	33.055002
787.385248	58737.270220	33.060020
788.510571	58833.006197	33.065037
789.233278	58934.104536	33.070055
790.079072	59011.940394	33.075072
790.798841	59105.756437	33.080090
791.967083	59188.448050	33.085108
793.009093	59273.834322	33.090125
793.786487	59366.928968	33.095143
794.446541	59443.053376	33.100160
795.314617	59532.939242	33.105178
796.092078	59624.099734	33.110196
796.874004	59704.174561	33.115213
797.182357	59808.039953	33.120231
798.038890	59895.040424	33.125248
798.629319	59981.471122	33.130266
799.491095	60089.604018	33.135284
800.344467	60177.089387	33.140301
801.201138	60273.806959	33.145319
801.967213	60366.819981	33.150336
803.125054	60466.048142	33.155354
803.860015	60564.791577	33.160372
804.794786	60658.227556	33.165389
805.335669	60763.510522	33.170407
806.442289	60851.350263	33.175424
807.329453	60934.706905	33.180442
807.700213	61038.054496	33.185460
808.691487	61125.077124	33.190477
809.098386	61239.841012	33.195495
809.950513	61342.921050	33.200512
810.825828	61442.414056	33.205530
811.234281	61551.126426	33.210548
812.200882	61652.696374	33.215565
813.164925	61764.337112	33.220583
813.681411	61860.883328	33.225600
814.645080	61973.728446	33.230618
815.488510	62094.992947	33.235636
816.534239	62201.643525	33.240653
817.379853	62312.816903	33.245671
818.220607	62412.809980	33.250688
819.348982	62506.827455	33.255706
820.309517	62609.028758	33.260724
821.452258	62707.282738	33.265741
821.949764	62802.339964	33.270759
822.961039	62901.288497	33.275776
823.827018	63003.320661	33.280794
824.459009	63093.150588	33.285812
825.406477	63192.947641	33.290829
826.440694	63296.141981	33.295847
827.018685	63385.555564	33.300864
827.949070	63479.107260	33.305882
828.891623	63577.116547	33.310900
829.549582	63675.882183	33.315917
830.284312	63769.659084	33.320935
830.979697	63861.209983	33.325952
831.798928	63957.469202	33.330970
832.616635	64062.230648	33.335988
833.292163	64150.489081	33.341005
834.400694	64241.385493	33.346023
834.824507	64325.102405	33.351040
835.853066	64418.437813	33.356058
836.616198	64516.246783	33.361076
837.404815	64608.850723	33.366093
837.850885	64711.435746	33.371111
838.574884	64821.550415	33.376128
839.323022	64917.983698	33.381146
839.982081	65036.820262	33.386164
840.779095	65144.569134	33.391181
841.673495	65253.219007	33.396199
842.616625	65373.402081	33.401216
843.498015	65469.621118	33.406234
844.093948	65589.503911	33.411252
845.498636	65699.448966	33.416269
846.439688	65807.364976	33.421287
847.108887	65918.322144	33.426304
848.040181	66013.206289	33.431322
848.526297	66133.119419	33.436340
849.612597	66239.353417	33.441357
850.272234	66348.125797	33.446375
851.220542	66475.415096	33.451392
852.413209	66579.498923	33.456410
853.139294	66697.106425	33.461428
854.045556	66793.492360	33.466445
855.141566	66913.543848	33.471463
855.672809	67012.763746	33.476480
857.029873	67122.692916	33.481498
857.278432	67233.910938	33.486516
858.367325	67345.614952	33.491533
859.636730	67456.021121	33.496551
860.048359	67570.714870	33.501568
860.948043	67679.620782	33.506586
861.694713	67801.382182	33.511604
862.545143	67923.070976	33.516621
863.082848	68042.864530	33.521639
863.958637	68166.357593	33.526656
865.226626	68282.094307	33.531674
865.797303	68407.627468	33.536692
866.675636	68531.627845	33.541709
867.722416	68633.648477	33.546727
868.749559	68759.250249	33.551744
869.786210	68870.459606	33.556762
870.776113	68985.695112	33.561780
871.859519	69092.905492	33.566797
872.954613	69204.075860	33.571815
874.118571	69312.386559	33.576832
875.308511	69408.569734	33.581850
875.972832	69519.747267	33.586868
876.690770	69607.850122	33.591885
877.562692	69703.946361	33.596903
878.239510	69807.346127	33.601920
879.237008	69907.466897	33.606938
880.119764	70005.117122	33.611956
881.232374	70090.480484	33.616973
881.888981	70189.266958	33.621991
882.197963	70285.752576	33.627008
883.006207	70381.868584	33.632026
883.538843	70487.834781	33.637044
884.315449	70591.064835	33.642061
885.187648	70696.106201	33.647079
885.655150	70814.152435	33.652096
886.829418	70931.777309	33.657114
887.443762	71047.621739	33.662132
888.586465	71162.978394	33.667149
889.480091	71275.822697	33.672167
890.016577	71406.940720	33.677184
891.351255	71529.092952	33.682202
891.825438	71651.907307	33.687220
892.703274	71773.242819	33.692237
893.709357	71895.809762	33.697255
894.389586	72018.934810	33.702272
895.103658	72140.911544	33.707290
895.933418	72284.386072	33.712308
896.787705	72414.221699	33.717325
897.752208	72547.244302	33.722343
898.813490	72677.825933	33.727360
900.447846	72797.802500	33.732378
901.424055	72914.371159	33.737396
902.601177	73035.951112	33.742413
903.928968	73150.184040	33.747431
905.117837	73254.000585	33.752448
906.785682	73355.542401	33.757466
908.048179	73452.428823	33.762484
909.049668	73541.925886	33.767501
910.196563	73620.297361	33.772519
910.801562	73722.022799	33.777536
911.745761	73803.049728	33.782554
912.277556	73901.211019	33.787572
912.791800	74001.214509	33.792589
913.559711	74095.010440	33.797607
914.269851	74210.744289	33.802624
915.031878	74312.852180	33.807642
915.580626	74431.766376	33.812660
916.261308	74554.401428	33.817677
917.357122	74666.948385	33.822695
917.926124	74792.945697	33.827712
919.079757	74907.652416	33.832730
919.787856	75024.674155	33.837748
920.741303	75150.593574	33.842765
921.636577	75274.304811	33.847783
922.166293	75397.967534	33.852800
923.245609	75519.502270	33.857818
924.355107	75651.643953	33.862836
925.314893	75764.920188	33.867853
926.603868	75886.347933	33.872871
927.409465	76002.405516	33.877888
928.584676	76114.265361	33.882906
929.728975	76221.605605	33.887924
930.293923	76328.463473	33.892941
931.728324	76432.649211	33.897959
932.491423	76533.921276	33.902976
933.522386	76628.584590	33.907994
934.051035	76734.761475	33.913012
934.790926	76845.841394	33.918029
935.793457	76950.806370	33.923047
936.539321	77080.708333	33.928064
937.425338	77195.104022	33.933082
937.985935	77301.183972	33.938100
938.586284	77425.031097	33.943117
939.881294	77546.196033	33.948135
940.954752	77670.658302	33.953152
941.611616	77787.514512	33.958170
942.962888	77911.384164	33.963188
944.078286	78026.196774	33.968205
945.208791	78141.658649	33.973223
945.972965	78260.624216	33.978240
946.811453	78385.855098	33.983258
948.119317	78509.343394	33.988276
948.685813	78631.945383	33.993293
949.626378	78765.973498	33.998311
950.492315	78899.799451	34.003328
951.327036	79011.596623	34.008346
952.002048	79146.238345	34.013364
952.819667	79278.393082	34.018381
954.113112	79410.207480	34.023399
954.982606	79556.647550	34.028416
955.692943	79691.040689	34.033434
957.095073	79825.381530	34.038452
957.587255	79965.310548	34.043469
958.352177	80099.362634	34.048487
959.687765	80242.945757	34.053504
960.840248	80377.336224	34.058522
962.032348	80513.630307	34.063540
963.588868	80636.421726	34.068557
965.323875	80744.507147	34.073575
966.392804	80853.887533	34.078592
967.142338	80989.054076	34.083610
968.302395	81092.883600	34.088628
968.919597	81200.725691	34.093645
969.832529	81319.906472	34.098663
970.685717	81444.793225	34.103680
971.522813	81564.973648	34.108698
972.453217	81681.239430	34.113716
973.180853	81809.397694	34.118733
974.368848	81934.758822	34.123751
975.408420	82063.355796	34.128768
976.407283	82176.250239	34.133786
977.648854	82297.261910	34.138804
978.423899	82420.510597	34.143821
979.280821	82544.790107	34.148839
980.063567	82668.152821	34.153856
981.069456	82780.986187	34.158874
982.043056	82891.979255	34.163892
983.056726	83006.671284	34.168909
983.946017	83110.440118	34.173927
984.310330	83246.144051	34.178944
985.238001	83362.369023	34.183962
986.545702	83484.255809	34.188980
987.407911	83614.237145	34.193997
988.443651	83724.662039	34.199015
989.143273	83853.931007	34.204032
990.255924	83990.892635	34.209050
991.285657	84122.222409	34.214068
992.113941	84244.828425	34.219085
993.080383	84375.474370	34.224103
994.053542	84508.958877	34.229120
995.027817	84645.719148	34.234138
996.249952	84771.079110	34.239156
996.802866	84911.530990	34.244173
997.695530	85045.025354	34.249191
998.734360	85183.106589	34.254208
999.855828	85340.289376	34.259226
1001.201891	85453.215686	34.264244
1002.388158	85605.148498	34.269261
1003.329769	85729.572373	34.274279
1004.588614	85865.087546	34.279296
1005.515248	86006.037294	34.284314
1006.586684	86140.648228	34.289332
1007.383631	86281.171486	34.294349
1008.342151	86411.622537	34.299367
1009.345854	86548.567396	34.304384
1010.602411	86689.500783	34.309402
1011.716383	86823.527513	34.314420
1012.436106	86972.724102	34.319437
1013.714100	87099.808803	34.324455
1014.492209	87257.180450	34.329472
1015.498527	87379.712940	34.334490
1016.716774	87521.189049	34.339508
1017.474604	87659.767291	34.344525
1018.508107	87798.131837	34.349543
1019.925009	87938.447177	34.354560
1021.002506	88079.557281	34.359578
1021.923925	88210.644867	34.364596
1022.708904	88361.408955	34.369613
1023.749819	88495.426097	34.374631
1025.149073	88634.699030	34.379648
1026.246092	88772.319833	34.384666
1027.687968	88894.753700	34.389684
1028.613710	89031.758363	34.394701
1029.697238	89164.470147	34.399719
1030.653135	89297.310551	34.404736
1031.484949	89432.334311	34.409754
1032.507909	89563.319066	34.414772
1032.974508	89709.077608	34.419789
1034.181511	89841.843449	34.424807
1035.170093	89993.977789	34.429824
1035.831284	90139.164373	34.434842
1036.945864	90278.821983	34.439860
1038.073394	90415.600878	34.444877
1038.646984	90545.486690	34.449895
1039.812403	90682.495227	34.454912
1040.489388	90824.237069	34.459930
1041.499722	90958.982571	34.464948
1042.602928	91097.369675	34.469965
1043.738087	91245.593522	34.474983
1044.574593	91396.572785	34.480000
1045.268380	91557.505419	34.485018
1046.569788	91700.443813	34.490036
1047.492996	91854.524154	34.495053
1048.435029	92014.168347	34.500071
1049.638370	92173.784782	34.505088
1050.854282	92322.426791	34.510106
1051.990678	92460.222646	34.515124
1052.691107	92623.552795	34.520141
1054.173679	92783.312639	34.525159
1055.551832	92940.225018	34.530176
1056.380997	93093.165145	34.535194
1057.576580	93257.224484	34.540212
1058.337977	93414.972027	34.545229
1059.512235	93571.718894	34.550247
1060.528612	93726.676635	34.555264
1062.007587	93873.446555	34.560282
1063.041461	94019.276185	34.565300
1064.281081	94169.381611	34.570317
1065.580575	94329.782595	34.575335
1067.389872	94453.264289	34.580352
1068.088053	94609.613437	34.585370
1069.164569	94746.060347	34.590388
1070.356892	94894.805528	34.595405
1071.523159	95044.011284	34.600423
1072.560103	95188.412135	34.605440
1073.472569	95325.622437	34.610458
1074.680695	95463.501359	34.615476
1075.534814	95606.725763	34.620493
1076.594081	95760.115640	34.625511
1077.652628	95907.794439	34.630528
1078.195789	96070.459962	34.635546
1079.525744	96219.641152	34.640564
1080.542834	96373.782042	34.645581
1081.507877	96527.476786	34.650599
1082.473304	96691.136058	34.655616
1083.327377	96860.545676	34.660634
1084.293526	97012.598746	34.665652
1085.187377	97180.011683	34.670669
1086.503996	97358.195475	34.675687
1087.748410	97515.660881	34.680704
1088.493315	97690.648531	34.685722
1089.710084	97844.792955	34.690740
1091.232086	98003.141236	34.695757
1092.270135	98166.584475	34.700775
1093.450872	98315.885409	34.705792
1095.237677	98472.828307	34.710810
1096.500490	98598.836323	34.715828
1097.249938	98749.056439	34.720845
1098.147291	98890.244835	34.725863
1099.118394	99019.483872	34.730880
1099.980612	99174.883067	34.735898
1101.316367	99316.263757	34.740916
1102.076506	99465.208844	34.745933
1103.396789	99617.672129	34.750951
1104.155781	99777.672464	34.755968
1105.111695	99930.619669	34.760986
1106.654109	100071.972133	34.766004
1107.889320	100230.685091	34.771021
1108.988210	100380.265531	34.776039
1110.318731	100531.588024	34.781056
1110.779713	100695.052418	34.786074
1112.010467	100843.849295	34.791092
1113.005822	100997.879232	34.796109
1113.514648	101167.590664	34.801127
1114.850402	101337.095899	34.806144
1116.169211	101505.643301	34.811162
1117.322114	101678.881624	34.816180
1118.110520	101839.707740	34.821197
1118.989379	102019.699299	34.826215
1120.657184	102187.670945	34.831232
1121.618420	102366.234695	34.836250
1123.051923	102532.828693	34.841268
1124.319860	102696.147142	34.846285
1125.413982	102874.263345	34.851303
1126.432083	103041.736970	34.856320
1127.638086	103217.123354	34.861338
1128.677113	103376.477407	34.866356
1130.201709	103554.580930	34.871373
1131.134038	103728.090946	34.876391
1132.399861	103889.165250	34.881408
1133.824779	104057.802711	34.886426
1135.098545	104223.624087	34.891444
1136.112844	104378.388294	34.896461
1137.252812	104545.486176	34.901479
1138.622584	104704.151109	34.906496
1139.429406	104880.695445	34.911514
1140.661254	105048.123981	34.916532
1141.927923	105211.789101	34.921549
1142.631152	105390.954659	34.926567
1143.888780	105557.813120	34.931584
1144.701770	105736.849907	34.936602
1145.450307	105914.354114	34.941620
1146.683568	106096.478389	34.946637
1147.689694	106281.760198	34.951655
1148.769161	106462.576363	34.956672
1150.147012	106650.744762	34.961690
1151.316392	106827.429355	34.966708
1152.476386	107008.433017	34.971725
1153.451189	107203.429048	34.976743
1154.724566	107388.765495	34.981760
1155.956800	107562.673405	34.986778
1157.007898	107738.845522	34.991796
1158.490733	107905.127523	34.996813
1159.482783	108075.311504	35.001831
1160.593193	108242.895556	35.006848
1161.636466	108417.345987	35.011866
1162.852631	108586.567522	35.016884
1164.067577	108752.075125	35.021901
1164.918806	108934.787909	35.026919
1166.558449	109098.027719	35.031936
1167.705114	109277.752927	35.036954
1168.770723	109440.782493	35.041972
1169.810599	109628.553054	35.046989
1170.911856	109802.713022	35.052007
1172.378979	109986.861172	35.057024
1173.487656	110158.496968	35.062042
1174.239833	110338.223060	35.067060
1175.803267	110507.978691	35.072077
1178.040222	110666.266403	35.077095
1179.554127	110824.315631	35.082112
1181.082649	110985.053752	35.087130
1181.882668	111158.726858	35.092148
1183.233000	111314.754343	35.097165
1183.890164	111490.313504	35.102183
1185.318691	111643.874587	35.107200
1186.180639	111816.168839	35.112218
1187.119540	111987.857020	35.117236
1188.589059	112159.993755	35.122253
1189.447634	112331.855339	35.127271
1191.024587	112494.450317	35.132288
1192.413422	112662.381070	35.137306
1193.527991	112832.198696	35.142324
1195.007292	113007.618865	35.147341
1196.064472	113175.732414	35.152359
1197.523469	113335.445959	35.157376
1198.513730	113510.706854	35.162394
1199.454069	113677.886443	35.167412
1200.685813	113858.827882	35.172429
1201.574355	114031.943519	35.177447
1202.939450	114207.497869	35.182464
1204.221103	114387.928725	35.187482
1204.995807	114563.611078	35.192500
1206.449802	114749.056428	35.197517
1207.615938	114920.962832	35.202535
1208.894177	115090.516470	35.207552
1209.846190	115276.115137	35.212570
1210.747218	115450.890901	35.217588
1212.452237	115641.943819	35.222605
1213.223250	115830.126731	35.227623
1214.395719	116021.077235	35.232640
1215.747657	116207.486490	35.237658
1216.723548	116409.101245	35.242676
1218.208408	116585.843307	35.247693
1219.474631	116768.813402	35.252711
1221.062177	116948.833947	35.257728
1222.568955	117135.250681	35.262746
1223.164246	117311.240118	35.267764
1224.768906	117467.265306	35.272781
1225.434020	117657.213332	35.277799
1226.640148	117815.342755	35.282816
1227.667826	117993.230910	35.287834
1228.571494	118174.768062	35.292852
1230.032515	118358.693590	35.297869
1231.147387	118541.003868	35.302887
1232.273272	118729.601179	35.307904
1233.443822	118916.305865	35.312922
1234.310154	119117.876939	35.317940
1235.952403	119313.342516	35.322957
1236.972462	119510.345844	35.327975
1237.842869	119706.405647	35.332992
1239.316930	119904.251593	35.338010
1240.716814	120104.694350	35.343028
1242.208887	120308.188777	35.348045
1243.043787	120506.609475	35.353063
1244.429386	120710.149279	35.358080
1245.853483	120908.745309	35.363098
1246.843097	121116.023973	35.368116
1248.633510	121309.397556	35.373133
1249.909673	121514.417446	35.378151
1251.272846	121711.104134	35.383168
1253.121141	121898.786217	35.388186
1254.351535	122086.352551	35.393204
1256.220748	122264.750269	35.398221
1256.799946	122457.336905	35.403239
1258.333832	122639.362105	35.408256
1259.928700	122828.927565	35.413274
1261.272381	123010.022953	35.418292
1262.724430	123199.461767	35.423309
1263.879658	123385.643317	35.428327
1264.858239	123580.707759	35.433344
1266.258543	123751.805726	35.438362
1267.576284	123940.042533	35.443380
1269.181443	124121.027887	35.448397
1269.794076	124318.917112	35.453415
1271.009286	124497.484391	35.458432
1272.110533	124691.106100	35.463450
1273.051031	124901.157990	35.468468
1274.409959	125086.685622	35.473485
1275.967760	125292.399088	35.478503
1276.984786	125487.711910	35.483520
1278.831224	125676.940824	35.488538
1279.877393	125888.338941	35.493556
1281.282562	126075.297371	35.498573
1282.331068	126285.672167	35.503591
1283.870598	126476.399500	35.508608
1284.951383	126669.557229	35.513626
1286.348415	126872.660721	35.518644
1287.798572	127064.812465	35.523661
1289.043964	127260.621067	35.528679
1290.303741	127459.481716	35.533696
1291.348285	127648.053699	35.538714
1292.518133	127839.824719	35.543732
1293.867321	128030.517120	35.548749
1294.826867	128208.262603	35.553767
1295.968803	128385.270819	35.558784
1297.349711	128583.828960	35.563802
1298.194033	128777.913196	35.568820
1299.790125	128978.846960	35.573837
1301.147863	129156.091839	35.578855
1302.261777	129358.891263	35.583872
1303.790614	129545.726941	35.588890
1305.108774	129761.279592	35.593908
1306.614716	129953.062487	35.598925
1307.621289	130152.831536	35.603943
1308.789626	130359.556976	35.608960
1310.291991	130548.760025	35.613978
1311.075831	130770.068504	35.618996
1312.796382	130967.069317	35.624013
1314.364042	131164.817971	35.629031
1315.476026	131388.118936	35.634048
1316.931839	131589.625871	35.639066
1318.040141	131806.747936	35.644084
1319.615477	132019.046239	35.649101
1320.641961	132236.628046	35.654119
1321.982696	132445.583952	35.659136
1323.649268	132642.655701	35.664154
1324.825609	132857.367659	35.669172
1326.566161	133059.131186	35.674189
1327.843539	133280.368151	35.679207
1328.936298	133487.673270	35.684224
1330.755411	133701.503837	35.689242
1331.742693	133911.578305	35.694260
1333.347743	134118.869916	35.699277
1335.159993	134300.978417	35.704295
1336.788498	134507.572203	35.709312
1338.773103	134691.264990	35.714330
1339.660853	134897.637182	35.719348
1341.315663	135094.271483	35.724365
1342.552378	135281.736195	35.729383
1343.581184	135483.693203	35.734400
1345.150850	135669.080079	35.739418
1346.414824	135878.022439	35.744436
1347.779147	136059.757017	35.749453
1348.757698	136269.621887	35.754471
1350.096074	136475.186019	35.759488
1351.258945	136670.350517	35.764506
1352.529573	136884.215706	35.769524
1353.422123	137081.618154	35.774541
1354.930905	137302.937737	35.779559
1356.235577	137519.311223	35.784576
1357.410193	137729.687599	35.789594
1359.112387	137934.393081	35.794612
1360.312530	138150.851167	35.799629
1361.809356	138364.336308	35.804647
1362.751335	138593.156439	35.809664
1364.286665	138800.517673	35.814682
1365.458931	139008.368929	35.819700
1366.837319	139213.223398	35.824717
1367.998999	139409.825526	35.829735
1369.067600	139629.470857	35.834752
1370.758884	139840.401031	35.839770
1371.517753	140051.138688	35.844788
1372.805155	140270.361062	35.849805
1374.435330	140483.282516	35.854823
1375.574996	140712.112762	35.859840
1377.304732	140930.762698	35.864858
1378.087338	141155.293287	35.869876
1379.651375	141388.408320	35.874893
1380.960121	141596.547262	35.879911
1382.252050	141844.474228	35.884928
1383.737879	142073.804718	35.889946
1385.058042	142305.710788	35.894964
1386.674454	142531.665281	35.899981
1388.312001	142774.703264	35.904999
1389.361182	143004.186163	35.910016
1390.866435	143240.252495	35.915034
1392.306268	143476.077537	35.920052
1393.883278	143709.081441	35.925069
1395.427582	143951.915387	35.930087
1397.030705	144172.750681	35.935104
1399.036306	144393.840470	35.940122
1400.198094	144639.224910	35.945140
1401.543703	144858.331467	35.950157
1403.087587	145077.724942	35.955175
1404.147299	145321.901458	35.960192
1405.818639	145540.200507	35.965210
1407.039290	145783.480430	35.970228
1408.278590	146018.405925	35.975245
1409.724357	146246.189193	35.980263
1410.982601	146492.840410	35.985280
1412.531911	146726.568406	35.990298
1414.204938	146958.643244	35.995316
1415.832232	147192.324258	36.000333
1417.401805	147419.677988	36.005351
1418.737488	147670.281083	36.010368
1420.358260	147889.707253	36.015386
1421.963790	148127.911441	36.020404
1423.249207	148359.690462	36.025421
1424.703485	148590.392152	36.030439
1425.900917	148812.617431	36.035456
1427.065721	149055.715763	36.040474
1428.430597	149277.169697	36.045492
1430.122497	149518.894704	36.050509
1431.902056	149749.629070	36.055527
1432.958525	149982.977414	36.060544
1434.647320	150215.212766	36.065562
1435.953263	150459.604987	36.070580
1437.481386	150689.270353	36.075597
1438.749855	150925.241389	36.080615
1440.100114	151163.457782	36.085632
1441.640493	151390.172190	36.090650
1443.467002	151617.146971	36.095668
1444.265848	151832.090291	36.100685
1446.016915	152040.443210	36.105703
1447.129191	152265.253871	36.110720
1448.736954	152487.578450	36.115738
1450.205928	152707.682495	36.120756
1451.445657	152926.505859	36.125773
1452.807707	153159.511239	36.130791
1454.494297	153375.629411	36.135808
1455.953602	153598.061075	36.140826
1457.327523	153830.562104	36.145844
1458.903360	154049.884620	36.150861
1460.322925	154282.888689	36.155879
1461.659662	154512.763116	36.160896
1462.982836	154757.615383	36.165914
1464.736447	154986.146205	36.170932
1465.738784	155215.584054	36.175949
1467.216194	155456.790578	36.180967
1468.640137	155699.478137	36.185984
1470.363204	155947.064958	36.191002
1471.613484	156191.254448	36.196020
1473.406733	156433.888558	36.201037
1474.989200	156668.353981	36.206055
1476.236451	156905.397581	36.211072
1478.265581	157150.028079	36.216090
1479.841626	157376.295343	36.221108
1481.362034	157613.541341	36.226125
1483.384932	157857.176104	36.231143
1484.675383	158087.335534	36.236160
1485.755187	158323.997012	36.241178
1487.043871	158580.497404	36.246196
1488.299545	158821.762739	36.251213
1490.078595	159060.803538	36.256231
1491.255488	159321.397653	36.261248
1492.799285	159563.218319	36.266266
1494.121120	159810.021516	36.271284
1495.410174	160058.023673	36.276301
1497.226255	160312.614166	36.281319
1499.050212	160572.721610	36.286336
1500.392253	160810.778471	36.291354
1502.124558	161072.425902	36.296372
1503.180933	161335.514201	36.301389
1504.763156	161585.877265	36.306407
1506.343409	161842.989091	36.311424
1507.529163	162110.932327	36.316442
1509.399413	162350.881209	36.321460
1511.026611	162606.596020	36.326477
1512.971447	162864.189864	36.331495
1514.532626	163103.736290	36.336512
1516.255104	163347.012632	36.341530
1517.829464	163582.818847	36.346548
1519.591901	163827.182734	36.351565
1521.297607	164056.807472	36.356583
1522.727191	164303.142478	36.361600
1525.116952	164503.123530	36.366618
1527.213778	164709.239933	36.371636
1528.276303	164913.619369	36.376653
1530.063858	165117.669153	36.381671
1531.310328	165315.756240	36.386688
1532.311234	165520.275647	36.391706
1534.256565	165734.729232	36.396724
1535.110839	165945.045087	36.401741
1536.759059	166147.676789	36.406759
1537.670027	166367.891645	36.411776
1539.281464	166595.213385	36.416794
1540.422382	166820.911659	36.421812
1541.434776	167069.715789	36.426829
1543.008124	167290.769424	36.431847
1544.405957	167539.591530	36.436864
1545.741353	167776.692671	36.441882
1547.391522	168014.531695	36.446900
1549.049078	168274.174774	36.451917
1550.640632	168521.907096	36.456935
1552.216626	168777.697924	36.461952
1553.649930	169028.921441	36.466970
1555.351225	169276.539745	36.471988
1556.857155	169542.798671	36.477005
1558.352350	169798.609135	36.482023
1559.799839	170057.688801	36.487040
1561.293253	170318.741710	36.492058
1562.462526	170587.648968	36.497076
1564.247685	170858.299555	36.502093
1566.327249	171117.717171	36.507111
1567.904997	171379.258499	36.512128
1569.436629	171644.145070	36.517146
1571.451896	171896.613949	36.522164
1572.795264	172156.941847	36.527181
1574.832912	172415.397925	36.532199
1576.188104	172685.862996	36.537216
1577.791907	172934.877314	36.542234
1579.194196	173193.134917	36.547252
1580.932975	173475.342002	36.552269
1582.592760	173722.373377	36.557287
1584.254861	173997.657222	36.562304
1585.499357	174260.577088	36.567322
1587.412109	174521.959012	36.572340
1588.789493	174782.044876	36.577357
1590.558424	175042.425431	36.582375
1592.242908	175316.319217	36.587392
1593.536522	175579.607729	36.592410
1595.079160	175845.129250	36.597428
1596.593907	176123.698624	36.602445
1597.704330	176387.757234	36.607463
1599.830521	176670.736927	36.612480
1601.043068	176948.725537	36.617498
1602.676982	177212.363728	36.622516
1604.736731	177491.616967	36.627533
1606.161449	177764.921242	36.632551
1607.960414	178034.945349	36.637568
1609.875040	178299.015242	36.642586
1612.090310	178546.913585	36.647604
1613.023067	178787.315885	36.652621
1614.586359	179038.111865	36.657639
1616.579671	179272.727985	36.662656
1617.756837	179526.810787	36.667674
1619.332189	179770.631045	36.672692
1620.763269	180039.546429	36.677709
1622.356524	180283.683961	36.682727
1623.691903	180547.682201	36.687744
1625.227019	180806.537116	36.692762
1626.833527	181064.912792	36.697780
1627.765327	181346.159516	36.702797
1629.998106	181617.190516	36.707815
1631.597946	181890.747170	36.712832
1632.618858	182184.533793	36.717850
1634.566825	182455.323396	36.722868
1635.929258	182742.651890	36.727885
1637.757816	183025.162719	36.732903
1639.383355	183312.846485	36.737920
1640.877812	183596.276841	36.742938
1642.904832	183885.042537	36.747956
1644.611873	184168.848816	36.752973
1646.298493	184448.777321	36.757991
1648.251186	184730.797073	36.763008
1649.529433	185030.779260	36.768026
1651.431069	185320.525781	36.773044
1653.049178	185622.868864	36.778061
1654.795207	185919.407297	36.783079
1656.733756	186215.599847	36.788096
1658.367532	186506.145119	36.793114
1660.159365	186783.203470	36.798132
1661.696476	187082.713892	36.803149
1663.358902	187370.417573	36.808167
1665.468580	187649.067616	36.813184
1666.524031	187953.253857	36.818202
1668.378013	188243.407044	36.823220
1670.304618	188519.439144	36.828237
1672.030389	188815.314063	36.833255
1674.149867	189094.288398	36.838272
1675.951771	189377.616816	36.843290
1678.058210	189660.264048	36.848308
1679.888546	189926.129275	36.853325
1681.266852	190201.433355	36.858343
1683.585221	190462.579341	36.863360
1685.140416	190750.726731	36.868378
1687.272637	190997.044418	36.873396
1689.632774	191247.375531	36.878413
1691.522382	191500.282747	36.883431
1693.596359	191736.638431	36.888448
1695.313348	191974.105294	36.893466
1697.002373	192212.884926	36.898484
1698.579499	192456.239591	36.903501
1700.317055	192701.879776	36.908519
1702.268927	192934.174060	36.913536
1703.850478	193154.116163	36.918554
1705.454857	193365.032077	36.923572
1706.943033	193588.899858	36.928589
1708.228861	193806.163146	36.933607
1710.106921	194020.960033	36.938624
1711.069651	194250.815747	36.943642
1712.428858	194471.547748	36.948660
1713.880197	194720.847725	36.953677
1714.911133	194970.088760	36.958695
1716.572152	195215.601121	36.963712
1718.117133	195472.555761	36.968730
1719.620668	195740.027187	36.973748
1721.514214	196004.493541	36.978765
1723.117969	196275.251756	36.983783
1724.641319	196538.954644	36.988800
1726.222072	196820.342669	36.993818
1728.303329	197078.324384	36.998836
1729.796701	197352.050341	37.003853
1731.220909	197644.027670	37.008871
1733.447457	197914.314747	37.013888
1734.901182	198205.858960	37.018906
1736.517521	198501.427896	37.023924
1738.306542	198786.398069	37.028941
1739.862439	199072.092182	37.033959
1741.724713	199353.905951	37.038976
1743.313990	199649.510912	37.043994
1745.085965	199948.007862	37.049012
1746.996904	200250.266908	37.054029
1748.548624	200552.432347	37.059047
1751.095252	200827.214707	37.064064
1753.309567	201113.475091	37.069082
1755.466775	201389.769118	37.074100
1757.736917	201673.789533	37.079117
1759.654147	201939.411229	37.084135
1761.539997	202213.378776	37.089152
1763.207567	202484.208939	37.094170
1765.344724	202748.784086	37.099188
1767.150585	203009.516126	37.104205
1768.657748	203273.064013	37.109223
1770.634620	203537.046308	37.114240
1772.198915	203820.009112	37.119258
1773.597176	204079.198651	37.124276
1775.649653	204351.487196	37.129293
1777.207061	204633.147627	37.134311
1779.233384	204895.313082	37.139328
1780.550789	205174.335798	37.144346
1782.498051	205449.832434	37.149364
1784.324693	205726.200029	37.154381
1785.708649	206001.052412	37.159399
1787.784282	206280.315466	37.164416
1789.398089	206554.029524	37.169434
1791.680666	206830.139491	37.174452
1793.440328	207099.783368	37.179469
1795.470944	207384.517396	37.184487
1797.642287	207641.149874	37.189504
1798.508589	207916.664509	37.194522
1800.927825	208167.306055	37.199540
1802.405821	208422.731650	37.204557
1803.878280	208672.865435	37.209575
1806.041333	208909.878336	37.214592
1807.615032	209166.218564	37.219610
1808.941905	209430.761928	37.224628
1810.824615	209688.223206	37.229645
1812.402814	209943.448764	37.234663
1814.218334	210216.169724	37.239680
1815.808270	210497.928594	37.244698
1817.557500	210770.827517	37.249716
1819.473420	211042.990219	37.254733
1820.789283	211321.927110	37.259751
1822.898669	211605.804746	37.264768
1825.130095	211888.064633	37.269786
1826.804914	212164.218672	37.274804
1828.448531	212445.926826	37.279821
1830.391335	212731.219672	37.284839
1832.153432	213009.877190	37.289856
1833.926987	213304.873542	37.294874
1835.948167	213604.313539	37.299892
1837.997471	213874.905357	37.304909
1839.925169	214167.113378	37.309927
1841.906446	214454.857875	37.314944
1843.732955	214747.757375	37.319962
1845.868917	215023.139184	37.324980
1847.435260	215306.382570	37.329997
1849.260440	215612.020261	37.335015
1851.499057	215895.337133	37.340032
1853.290426	216184.972748	37.345050
1855.099685	216488.687017	37.350068
1857.389761	216754.668690	37.355085
1858.915178	217056.513323	37.360103
1860.934437	217347.653874	37.365120
1862.572363	217634.958297	37.370138
1864.420748	217928.858125	37.375156
1866.374061	218220.304747	37.380173
1867.959195	218516.013609	37.385191
1870.290633	218805.104481	37.390208
1872.076741	219100.022030	37.395226
1873.926520	219393.902220	37.400244
1876.314836	219687.393394	37.405261
1877.923738	219979.714345	37.410279
1879.677747	220286.653114	37.415296
1881.966252	220567.555457	37.420314
1883.884154	220853.850474	37.425332
1886.113123	221134.040654	37.430349
1887.930006	221425.712090	37.435367
1889.750699	221748.441612	37.440384
1891.512719	222047.247315	37.445402
1893.288080	222330.243812	37.450420
1895.700158	222616.365448	37.455437
1897.476493	222897.979845	37.460455
1899.231098	223175.141875	37.465472
1901.142982	223465.358421	37.470490
1902.892257	223722.613433	37.475508
1905.004353	223983.963835	37.480525
1906.499541	224248.358860	37.485543
1908.311170	224506.050924	37.490560
1910.242935	224762.620041	37.495578
1912.261590	225029.778862	37.500596
1914.443026	225289.217824	37.505613
1916.489815	225554.393032	37.510631
1918.009722	225816.478222	37.515648
1920.213584	226082.633340	37.520666
1921.957901	226350.309811	37.525684
1923.943821	226614.342549	37.530701
1925.428757	226891.509267	37.535719
1927.309590	227167.649009	37.540736
1928.959243	227448.550059	37.545754
1930.949639	227735.289937	37.550772
1932.882467	228016.985995	37.555789
1935.191116	228300.680459	37.560807
1937.094808	228591.068648	37.565824
1938.889138	228875.659288	37.570842
1940.616786	229167.753504	37.575860
1942.772185	229456.174438	37.580877
1944.320876	229750.635482	37.585895
1946.609926	230042.516491	37.590912
1948.561662	230338.363135	37.595930
1950.554096	230639.969466	37.600948
1952.763050	230929.859643	37.605965
1954.724065	231223.650485	37.610983
1956.497374	231528.012014	37.616000
1958.707755	231819.022231	37.621018
1960.064436	232133.331500	37.626036
1962.548970	232421.455529	37.631053
1964.512677	232728.254294	37.636071
1966.467361	233028.807578	37.641088
1968.485522	233328.691374	37.646106
1970.457785	233643.263467	37.651124
1972.728628	233934.143500	37.656141
1974.065933	234242.494108	37.661159
1976.113453	234556.117423	37.666176
1978.068901	234856.422167	37.671194
1979.587784	235173.661654	37.676212
1981.939822	235499.024464	37.681229
1983.726055	235823.106548	37.686247
1985.545805	236134.510368	37.691264
1987.749741	236451.060909	37.696282
1989.425875	236781.716315	37.701300
1991.951036	237102.789634	37.706317
1993.850914	237419.035712	37.711335
1995.591461	237745.213639	37.716352
1997.878987	238074.556850	37.721370
2000.055213	238389.745928	37.726388
2001.957915	238709.398778	37.731405
2004.078049	239031.049992	37.736423
2006.296644	239343.999887	37.741440
2008.766258	239641.163112	37.746458
2009.888721	239948.624471	37.751476
2012.395539	240230.721357	37.756493
2014.167104	240529.038990	37.761511
2015.947667	240819.380420	37.766528
2018.203090	241114.930389	37.771546
2019.937737	241413.764095	37.776564
2021.799602	241709.631958	37.781581
2023.749753	242007.848735	37.786599
2025.632384	242319.157989	37.791616
2027.846025	242632.091919	37.796634
2029.324456	242940.444226	37.801652
2031.450694	243261.064446	37.806669
2033.154797	243572.760717	37.811687
2034.648374	243903.211232	37.816704
2036.828487	244234.112478	37.821722
2038.993630	244570.274837	37.826740
2041.222881	244909.247338	37.831757
2043.573600	245245.280344	37.836775
2045.503195	245576.427844	37.841792
2047.764087	245908.844421	37.846810
2049.105262	246256.978404	37.851828
2051.395738	246595.869127	37.856845
2053.333501	246940.430217	37.861863
2055.478483	247288.235987	37.866880
2057.759671	247637.011616	37.871898
2059.644276	247994.842980	37.876916
2062.302444	248338.861235	37.881933
2064.491975	248689.965354	37.886951
2066.308130	249033.661514	37.891968
2068.877166	249382.446280	37.896986
2070.899092	249725.425469	37.902004
2073.012927	250062.827887	37.907021
2075.222959	250411.265410	37.912039
2077.609320	250749.870687	37.917056
2079.835052	251089.010161	37.922074
2082.020485	251423.076368	37.927092
2084.045544	251763.519095	37.932109
2086.463252	252094.857168	37.937127
2088.515070	252421.097327	37.942144
2091.308274	252751.310182	37.947162
2093.118900	253079.647337	37.952180
2095.722220	253414.184427	37.957197
2097.935218	253729.402293	37.962215
2099.679180	254055.846576	37.967232
2101.842195	254373.207198	37.972250
2104.104241	254694.845584	37.977268
2106.161220	255025.585590	37.982285
2108.248183	255340.927637	37.987303
2110.072856	255667.107725	37.992320
2112.637646	255992.485067	37.997338
2114.462103	256309.724574	38.002356
2116.321620	256638.847289	38.007373
2118.550222	256969.715524	38.012391
2120.601539	257294.414170	38.017408
2122.519809	257616.492521	38.022426
2124.462435	257924.824697	38.027444
2126.698191	258230.087880	38.032461
2128.395475	258543.565675	38.037479
2130.131112	258860.187707	38.042496
2132.473613	259156.925237	38.047514
2134.189732	259485.719007	38.052532
2136.849323	259793.787372	38.057549
2139.179758	260095.252785	38.062567
2140.975042	260412.324488	38.067584
2143.070231	260734.226323	38.072602
2144.988883	261070.636122	38.077620
2147.599095	261377.647159	38.082637
2149.621572	261713.050516	38.087655
2151.596117	262041.780884	38.092672
2154.119914	262346.850582	38.097690
2156.056324	262677.238848	38.102708
2158.231585	263017.547530	38.107725
2160.100225	263346.372223	38.112743
2161.968018	263694.020996	38.117760
2164.415041	264030.756552	38.122778
2166.698218	264364.622452	38.127796
2169.023390	264708.033544	38.132813
2171.500901	265045.654274	38.137831
2173.254350	265398.098521	38.142848
2175.604303	265722.276376	38.147866
2177.938903	266084.155207	38.152884
2180.290537	266421.542954	38.157901
2182.138743	266769.349882	38.162919
2184.085707	267106.929300	38.167936
2186.666068	267460.412537	38.172954
2188.832820	267820.693461	38.177972
2191.253180	268168.639217	38.182989
2193.998379	268516.965523	38.188007
2195.786998	268875.376405	38.193024
2197.869755	269205.670181	38.198042
2200.166057	269554.347661	38.203060
2202.417397	269911.212310	38.208077
2204.980801	270245.342449	38.213095
2207.283056	270597.702934	38.218112
2209.551622	270937.418023	38.223130
2212.096009	271292.458534	38.228148
2214.484950	271629.944673	38.233165
2216.656208	271958.523434	38.238183
2218.664095	272310.905759	38.243200
2221.028045	272637.066209	38.248218
2223.376462	272983.704330	38.253236
2226.194750	273309.259391	38.258253
2228.564338	273637.095744	38.263271
2230.854310	273978.103728	38.268288
2233.049357	274287.956806	38.273306
2235.229733	274618.846257	38.278324
2237.144662	274939.362410	38.283341
2239.474351	275268.576982	38.288359
2241.295148	275606.153752	38.293376
2243.588619	275933.468793	38.298394
2245.832825	276242.958428	38.303412
2247.761082	276553.539673	38.308429
2250.094554	276850.440408	38.313447
2251.993558	277161.051620	38.318464
2254.053440	277484.313571	38.323482
2255.940539	277806.180266	38.328500
2258.079361	278126.863829	38.333517
2260.463412	278449.972562	38.338535
2262.120643	278781.986014	38.343552
2264.074261	279114.562056	38.348570
2266.415867	279468.389889	38.353588
2268.485829	279814.893686	38.358605
2270.724733	280161.243543	38.363623
2272.711689	280525.440925	38.368640
2275.144831	280887.789159	38.373658
2277.275838	281253.970200	38.378676
2279.729386	281625.561607	38.383693
2282.438568	281978.263042	38.388711
2284.463591	282359.498972	38.393728
2286.772188	282719.528792	38.398746
2289.074742	283083.776262	38.403764
2291.735262	283446.721965	38.408781
2294.180722	283822.250663	38.413799
2296.055246	284197.894977	38.418816
2298.346332	284567.274571	38.423834
2301.152045	284935.708557	38.428852
2303.475543	285313.668612	38.433869
2306.272499	285669.274765	38.438887
2308.367927	286046.406567	38.443904
2311.114711	286419.395649	38.448922
2313.844619	286774.884363	38.453940
2315.883732	287138.077711	38.458957
2318.584197	287500.175114	38.463975
2320.437680	287869.493797	38.468992
2322.806242	288229.153517	38.474010
2325.247285	288606.684933	38.479028
2327.656747	288973.958147	38.484045
2330.376570	289332.138315	38.489063
2332.352600	289703.746982	38.494080
2334.705907	290079.359782	38.499098
2337.043157	290436.202031	38.504116
2339.313489	290819.422352	38.509133
2341.805848	291176.010385	38.514151
2343.901835	291549.477249	38.519168
2346.202549	291923.774785	38.524186
2348.615170	292299.400336	38.529204
2350.870925	292676.879133	38.534221
2353.290151	293053.899564	38.539239
2355.906613	293436.883063	38.544256
2357.870906	293808.766856	38.549274
2360.675152	294178.332278	38.554292
2362.717062	294560.388785	38.559309
2365.645142	294927.723277	38.564327
2367.886584	295306.088870	38.569344
2370.334071	295669.586274	38.574362
2372.624452	296010.855720	38.579380
2374.644615	296354.199561	38.584397
2377.433516	296679.995197	38.589415
2379.308494	297028.771451	38.594432
2381.334356	297380.545957	38.599450
2383.659940	297723.864281	38.604468
2386.082840	298083.779282	38.609485
2388.541159	298439.547460	38.614503
2390.901855	298808.107422	38.619520
2393.186802	299161.945670	38.624538
2395.534338	299524.917818	38.629556
2397.323364	299896.690411	38.634573
2399.961923	300265.761973	38.639591
2401.949483	300648.551012	38.644608
2404.152741	301036.334406	38.649626
2406.643457	301419.930881	38.654644
2409.203274	301810.958003	38.659661
2411.770986	302197.613879	38.664679
2413.821047	302595.552670	38.669696
2416.589544	302986.137249	38.674714
2419.092321	303390.657200	38.679732
2421.682313	303794.577975	38.684749
2424.316786	304174.385218	38.689767
2426.924237	304573.932064	38.694784
2429.129789	304968.943936	38.699802
2432.056211	305365.567659	38.704820
2434.179741	305770.420210	38.709837
2436.901874	306153.052913	38.714855
2439.277300	306543.283344	38.719872
2441.612546	306941.240645	38.724890
2444.595752	307343.691455	38.729908
2447.006965	307745.672830	38.734925
2449.492354	308133.645752	38.739943
2452.000872	308527.354173	38.744960
2454.357278	308927.435391	38.749978
2456.982107	309321.656200	38.754996
2459.394316	309726.882057	38.760013
2461.521804	310123.337984	38.765031
2463.836023	310524.995267	38.770048
2466.533120	310931.517961	38.775066
2469.676882	311333.345746	38.780084
2472.217298	311727.571740	38.785101
2475.235734	312119.714059	38.790119
2478.109059	312491.330145	38.795136
2480.541226	312877.593877	38.800154
2483.270898	313255.351260	38.805172
2485.841549	313638.009073	38.810189
2488.534737	314017.979223	38.815207
2491.387050	314386.188629	38.820224
2494.165588	314744.756986	38.825242
2496.733010	315106.964121	38.830260
2498.766008	315480.328323	38.835277
2501.654254	315840.170758	38.840295
2504.366859	316193.740990	38.845312
2506.626478	316546.543603	38.850330
2509.423216	316864.261442	38.855348
2511.905210	317185.355243	38.860365
2514.222915	317505.483496	38.865383
2516.457580	317827.452478	38.870400
2518.621629	318150.599854	38.875418
2520.820648	318470.311917	38.880436
2522.882295	318816.534208	38.885453
2524.854843	319159.975622	38.890471
2527.110113	319503.015404	38.895488
2529.383792	319875.867263	38.900506
2532.194035	320226.511741	38.905524
2534.245865	320597.922752	38.910541
2536.460609	320968.163553	38.915559
2538.914221	321362.517270	38.920576
2541.068246	321750.948482	38.925594
2543.534466	322140.750709	38.930612
2545.766961	322542.626106	38.935629
2548.063572	322952.692464	38.940647
2550.541020	323365.801131	38.945664
2552.979221	323783.307509	38.950682
2555.428943	324204.111447	38.955700
2558.367483	324630.092733	38.960717
2561.099293	325049.171559	38.965735
2563.484038	325477.801136	38.970752
2566.229272	325909.926684	38.975770
2568.860659	326330.386135	38.980788
2571.515471	326768.082922	38.985805
2574.059937	327207.597805	38.990823
2577.107989	327630.650788	38.995840
2579.376052	328079.854567	39.000858
2582.000040	328511.324754	39.005876
2584.910346	328947.191159	39.010893
2587.566433	329385.990271	39.015911
2590.221905	329828.316692	39.020928
2592.540155	330269.551182	39.025946
2595.201590	330704.888103	39.030964
2598.065083	331146.335688	39.035981
2600.739027	331596.749121	39.040999
2603.525963	332029.011020	39.046016
2606.709118	332458.465084	39.051034
2609.645472	332890.850451	39.056052
2612.019633	333328.807079	39.061069
2614.750128	333747.913930	39.066087
2617.400260	334180.412851	39.071104
2620.080467	334616.332268	39.076122
2623.138233	335037.029952	39.081140
2625.522491	335465.728649	39.086157
2628.007101	335898.572998	39.091175
2631.154482	336310.437566	39.096192
2633.473861	336742.997918	39.101210
2636.002082	337173.338698	39.106228
2638.441138	337591.502986	39.111245
2641.466898	338008.073588	39.116263
2644.357156	338424.383674	39.121280
2646.801057	338847.998132	39.126298
2649.487819	339244.225655	39.131316
2652.000354	339634.867017	39.136333
2654.310730	340014.569382	39.141351
2656.958815	340404.422792	39.146368
2659.475761	340799.270970	39.151386
2662.065565	341198.573699	39.156404
2664.516634	341599.317636	39.161421
2667.162313	342001.297602	39.166439
2669.938911	342406.326285	39.171456
2672.291961	342821.600380	39.176474
2675.149113	343230.190642	39.181492
2677.338963	343643.885389	39.186509
2679.870221	344069.735099	39.191527
2682.515340	344491.247676	39.196544
2685.158761	344927.965043	39.201562
2687.672679	345353.985902	39.206580
2690.574453	345792.102982	39.211597
2693.091026	346232.461075	39.216615
2696.280317	346673.623191	39.221632
2698.238516	347126.477284	39.226650
2700.983252	347574.557357	39.231668
2703.563805	348027.457974	39.236685
2706.283670	348490.817535	39.241703
2709.616391	348938.514297	39.246720
2711.958465	349409.846558	39.251738
2714.430341	349876.559347	39.256756
2717.530424	350338.269197	39.261773
2720.199601	350811.136838	39.266791
2723.258624	351280.689265	39.271808
2725.654712	351748.387898	39.276826
2728.498266	352215.199239	39.281844
2731.496276	352690.917394	39.286861
2734.267688	353159.940249	39.291879
2737.081146	353626.845342	39.296896
2739.787598	354102.241423	39.301914
2742.714092	354572.521530	39.306932
2745.700690	355037.812637	39.311949
2748.134276	355512.121976	39.316967
2751.607037	355984.028613	39.321984
2754.034121	356462.721318	39.327002
2756.733573	356915.399968	39.332020
2760.164366	357391.005841	39.337037
2762.885215	357869.207004	39.342055
2765.727211	358329.007894	39.347072
2768.142072	358809.075841	39.352090
2770.554092	359283.479463	39.357108
2773.228499	359755.197254	39.362125
2776.285187	360239.058068	39.367143
2778.938897	360710.312889	39.372160
2781.870514	361193.067083	39.377178
2784.737605	361668.237929	39.382196
2787.911024	362142.010342	39.387213
2790.305827	362616.104276	39.392231
2793.188517	363094.303712	39.397248
2795.843356	363556.240946	39.402266
2798.513624	364013.095345	39.407284
2801.349630	364459.361476	39.412301
2803.615347	364904.063942	39.417319
2806.356892	365353.000974	39.422336
2808.870818	365805.370198	39.427354
2811.592030	366263.944915	39.432372
2814.112288	366728.231244	39.437389
2816.352569	367211.209131	39.442407
2819.164592	367676.226020	39.447424
2821.812420	368159.687279	39.452442
2824.858429	368641.456081	39.457460
2828.072074	369130.552009	39.462477
2831.327848	369609.942270	39.467495
2834.348125	370080.813001	39.472512
2836.994024	370562.040087	39.477530
2839.789053	371045.978603	39.482548
2843.092580	371528.207131	39.487565
2845.785058	372023.924435	39.492583
2848.447046	372506.268698	39.497600
2851.490120	373003.517458	39.502618
2853.876947	373504.162682	39.507636
2856.748012	374000.969991	39.512653
2859.249761	374515.438369	39.517671
2862.194923	375022.015417	39.522688
2865.162707	375544.668419	39.527706
2868.283940	376050.367493	39.532724
2871.523387	376557.969730	39.537741
2874.274671	377077.973132	39.542759
2877.440987	377581.666820	39.547776
2880.082338	378104.490358	39.552794
2882.986247	378627.214675	39.557812
2886.116197	379143.629945	39.562829
2888.517776	379668.195776	39.567847
2891.522752	380186.976364	39.572864
2894.265598	380727.989066	39.577882
2897.217427	381252.750747	39.582900
2899.941022	381780.407948	39.587917
2903.249404	382320.522241	39.592935
2906.087423	382850.302732	39.597952
2909.168707	383384.172083	39.602970
2912.484404	383915.460090	39.607988
2915.426744	384435.156574	39.613005
2918.237837	384976.630429	39.618023
2921.295074	385507.809771	39.623040
2924.551253	386045.570245	39.628058
2927.006424	386573.050091	39.633076
2930.789997	387098.688734	39.638093
2933.692950	387615.886131	39.643111
2936.448609	388152.756224	39.648128
2939.717050	388669.398750	39.653146
2942.705615	389200.484217	39.658164
2945.616072	389717.421872	39.663181
2948.177419	390245.566572	39.668199
2951.205063	390771.803529	39.673216
2953.971525	391291.023491	39.678234
2956.526316	391786.632820	39.683252
2959.797647	392273.930212	39.688269
2962.424856	392763.706566	39.693287
2964.885514	393267.703884	39.698304
2968.259452	393752.605705	39.703322
2970.754189	394257.318527	39.708340
2973.466912	394766.858269	39.713357
2976.205613	395287.417162	39.718375
2978.936085	395801.680557	39.723392
2981.806371	396327.984198	39.728410
2984.166722	396866.379597	39.733428
2987.199669	397389.699355	39.738445
2989.868780	397946.386754	39.743463
2992.859501	398500.579718	39.748480
2995.675207	399056.642005	39.753498
2998.981371	399613.428607	39.758516
3002.250959	400179.871622	39.763533
3005.141295	400755.847250	39.768551
3008.237552	401319.204567	39.773568
3011.581223	401883.805891	39.778586
3014.321109	402463.603119	39.783604
3017.536025	403029.244055	39.788621
3020.630421	403604.071393	39.793639
3023.780952	404181.997627	39.798656
3026.818751	404770.502458	39.803674
3029.582776	405347.581113	39.808692
3032.753632	405929.020975	39.813709
3035.869675	406515.655286	39.818727
3039.310841	407097.182542	39.823744
3042.417449	407677.611057	39.828762
3045.308191	408272.663260	39.833780
3048.998231	408849.200331	39.838797
3051.803796	409453.418770	39.843815
3054.320834	410042.057247	39.848832
3057.703334	410642.181155	39.853850
3060.703834	411234.394949	39.858868
3063.958601	411837.733958	39.863885
3066.944283	412445.716003	39.868903
3070.184406	413041.302707	39.873920
3073.601290	413635.911677	39.878938
3076.651431	414235.913995	39.883956
3079.766903	414823.855922	39.888973
3082.545301	415431.327307	39.893991
3085.658373	416039.493228	39.899008
3088.988981	416639.654825	39.904026
3091.722863	417245.067718	39.909044
3094.925829	417831.261933	39.914061
3098.398156	418450.494663	39.919079
3101.725916	419055.496308	39.924096
3104.857757	419651.698244	39.929114
3107.601331	420256.817149	39.934132
3110.942576	420849.945258	39.939149
3114.149311	421456.358409	39.944167
3117.414558	422065.485333	39.949184
3120.646412	422638.500957	39.954202
3123.629744	423203.082055	39.959220
3127.014639	423759.050255	39.964237
3129.814879	424295.440425	39.969255
3133.084136	424841.853884	39.974272
3135.850624	425400.014364	39.979290
3138.648421	425966.214066	39.984308
3142.111668	426524.291682	39.989325
3144.939564	427091.678803	39.994343
3147.472197	427662.824199	39.999360
3150.678102	428246.769267	40.004378
3153.632480	428828.005632	40.009396
3156.602393	429405.326037	40.014413
3159.544622	430019.035335	40.019431
3162.715892	430620.688539	40.024448
3165.913078	431222.855631	40.029466
3168.814999	431843.847961	40.034484
3171.774119	432457.598364	40.039501
3175.015140	433079.950905	40.044519
3177.837373	433707.444911	40.049536
3180.978799	434351.890977	40.054554
3184.120263	434988.850226	40.059572
3187.237928	435631.773472	40.064589
3190.126472	436290.188571	40.069607
3193.455402	436962.671610	40.074624
3196.458016	437613.437419	40.079642
3199.507006	438294.791242	40.084660
3203.009733	438958.710619	40.089677
3205.882804	439647.448410	40.094695
3208.917206	440325.457106	40.099712
3212.254038	441009.424798	40.104730
3215.434183	441712.436380	40.109748
3218.527484	442402.327620	40.114765
3221.901982	443111.495680	40.119783
3224.974424	443813.096255	40.124800
3228.578700	444512.567095	40.129818
3231.865405	445234.900146	40.134836
3234.954912	445934.967568	40.139853
3238.976913	446640.587260	40.144871
3242.507512	447329.507759	40.149888
3246.025199	448025.547565	40.154906
3249.195101	448718.989498	40.159924
3252.824644	449416.539344	40.164941
3256.346106	450109.833598	40.169959
3259.406224	450798.067986	40.174976
3263.352620	451490.949854	40.179994
3266.573124	452178.965687	40.185012
3270.013727	452847.340043	40.190029
3274.190520	453520.487344	40.195047
3277.479317	454189.251083	40.200064
3280.956262	454862.873971	40.205082
3283.843378	455538.239888	40.210100
3287.455676	456196.063627	40.215117
3290.816454	456849.556097	40.220135
3293.881307	457519.976306	40.225152
3297.163114	458162.968579	40.230170
3300.156453	458807.151461	40.235188
3302.871548	459428.187073	40.240205
3306.032413	460046.857910	40.245223
3309.084631	460673.370165	40.250240
3312.047629	461314.195609	40.255258
3314.953877	461977.472590	40.260276
3318.017521	462626.084596	40.265293
3321.064288	463273.920961	40.270311
3323.742444	463945.975365	40.275328
3327.288147	464613.217880	40.280346
3330.418458	465289.862695	40.285364
3333.212206	465990.665568	40.290381
3336.850154	466679.274252	40.295399
3339.812041	467387.742592	40.300416
3343.182768	468081.304105	40.305434
3346.316153	468806.235222	40.310452
3349.635139	469516.699084	40.315469
3353.151302	470240.558869	40.320487
3356.549551	470965.473889	40.325504
3360.216078	471693.152675	40.330522
3363.671244	472420.384019	40.335540
3366.934614	473152.170416	40.340557
3369.869823	473899.049349	40.345575
3373.901675	474638.042573	40.350592
3377.383607	475383.314178	40.355610
3380.431615	476124.228575	40.360628
3383.944616	476871.260096	40.365645
3387.499621	477629.833196	40.370663
3390.912781	478379.654889	40.375680
3394.612306	479130.161184	40.380698
3398.064995	479891.646278	40.385716
3401.178671	480649.263714	40.390733
3405.155785	481410.960853	40.395751
3408.036994	482159.762465	40.400768
3412.059444	482906.080704	40.405786
3416.312633	483661.177423	40.410804
3420.005197	484403.851551	40.415821
3423.728558	485135.981653	40.420839
3427.135439	485872.277267	40.425856
3431.062494	486613.969797	40.430874
3434.576268	487339.985352	40.435892
3437.729306	488081.035674	40.440909
3441.429095	488822.576805	40.445927
3444.525830	489565.952280	40.450944
3448.084999	490296.949470	40.455962
3451.132861	491036.738141	40.460980
3454.263728	491788.708647	40.465997
3457.427312	492536.653155	40.471015
3460.301106	493301.786491	40.476032
3463.781382	494054.619974	40.481050
3467.504419	494819.556046	40.486068
3470.492366	495598.212228	40.491085
3474.314745	496364.987088	40.496103
3477.281739	497142.217101	40.501120
3481.035721	497901.120793	40.506125
3483.983562	498619.274999	40.511130
3487.524631	499288.861628	40.516135
3490.383186	499906.594862	40.521140
3493.223477	500460.378394	40.526144
3496.021213	500950.323196	40.531149
3498.373602	501399.022294	40.536154
3500.943567	501789.519260	40.541159
3503.227201	502130.603153	40.546164
3505.543201	502427.135914	40.551168
3507.373015	502640.786914	40.556173
3509.470172	502827.416940	40.561178
3510.898295	502960.806244	40.566183
3512.586514	503063.280597	40.571188
3513.418535	503133.498632	40.576192
3514.344815	503166.249423	40.581197
3515.608977	503155.876859	40.586202
3516.068962	503120.123419	40.591207
3517.373585	503051.946447	40.596212
3517.452758	502983.912280	40.601216
3518.355535	502873.891784	40.606221
3519.050275	502758.943498	40.611226
3519.260871	502616.740242	40.616231
3519.641906	502456.085790	40.621236
3519.710287	502285.457831	40.626240
3520.143334	502092.500441	40.631245
3520.482685	501894.089388	40.636250
3520.570865	501691.565373	40.641255
3520.472645	501475.047945	40.646260
3520.882605	501263.610437	40.651264
3521.312754	501039.614215	40.656269
3521.139402	500792.679514	40.661274
3521.002937	500535.409406	40.666279
3521.370776	500291.621824	40.671284
3520.886614	500055.963508	40.676288
3520.726429	499793.826980	40.681293
3520.712020	499533.840296	40.686298
3520.717309	499283.869888	40.691303
3520.612960	499021.915750	40.696308
3520.696523	498768.179721	40.701312
3520.602144	498500.293476	40.706317
3520.535039	498234.423938	40.711322
3520.146480	497986.472145	40.716327
3520.258730	497713.630885	40.721332
3519.847095	497451.297502	40.726336
3519.686941	497189.123086	40.731341
3519.496128	496934.493384	40.736346
3519.017603	496679.247404	40.741351
3518.852230	496424.353388	40.746356
3518.888132	496188.106708	40.751360
3518.725697	495929.711792	40.756365
3518.395602	495679.238318	40.761370
3517.943074	495448.831316	40.766375
3518.153904	495207.886100	40.771380
3517.657511	494967.707732	40.776384
3517.646835	494723.905021	40.781389
3517.628773	494495.088301	40.786394
3517.498532	494257.830255	40.791399
3517.190411	494027.534479	40.796404
3516.969325	493806.134220	40.801408
3516.608897	493567.789643	40.806413
3516.231221	493341.344763	40.811418
3515.727316	493124.589126	40.816423
3515.777398	492914.630385	40.821428
3515.257800	492713.114938	40.826432
3515.119483	492509.612688	40.831437
3515.194666	492303.694318	40.836442
3515.361579	492114.420342	40.841447
3515.153030	491907.884084	40.846452
3514.603958	491718.769884	40.851456
3514.697286	491514.460477	40.856461
3514.682431	491320.649243	40.861466
3513.826640	491136.338141	40.866471
3513.970940	490939.256541	40.871476
3513.731599	490760.719124	40.876480
3513.280147	490577.756677	40.881485
3513.009933	490418.162473	40.886490
3513.138432	490247.868042	40.891495
3513.201159	490069.681467	40.896500
3512.553993	489909.332149	40.901504
3512.574177	489734.238631	40.906509
3512.637982	489577.825975	40.911514
3512.179016	489418.911538	40.916519
3512.087485	489259.988333	40.921524
3511.865734	489111.113067	40.926528
3511.995335	488956.862802	40.931533
3511.901850	488802.798488	40.936538
3511.593967	488650.944805	40.941543
3511.436544	488501.396094	40.946548
3510.943834	488373.375636	40.951552
3511.035967	488230.977920	40.956557
3511.118292	488096.482506	40.961562
3510.690864	487960.648418	40.966567
3511.062238	487816.481248	40.971572
3510.625734	487696.298610	40.976576
3510.194853	487560.006313	40.981581
3510.188091	487449.783707	40.986586
3510.002640	487318.668292	40.991591
3510.413561	487185.431510	40.996596
3510.150479	487078.945090	41.001600
3509.981644	486956.182692	41.006605
3509.909774	486823.779521	41.011610
3509.407378	486720.570910	41.016615
3509.445441	486597.469562	41.021620
3509.335873	486496.882456	41.026624
3509.087969	486380.055708	41.031629
3509.147700	486277.262424	41.036634
3508.885104	486179.534656	41.041639
3509.199101	486071.684956	41.046644
3509.022510	485969.535266	41.051648
3508.695577	485871.866752	41.056653
3509.123157	485757.665003	41.061658
3508.583734	485663.119202	41.066663
3508.323998	485565.489163	41.071668
3508.306506	485479.117446	41.076672
3508.335620	485384.125792	41.081677
3508.235522	485293.865484	41.086682
3507.912492	485213.062815	41.091687
3508.470780	485104.510479	41.096692
3508.043764	485042.721262	41.101696
3508.168916	484951.511849	41.106701
3508.345111	484857.608888	41.111706
3507.743524	484773.758059	41.116711
3507.735921	484690.116954	41.121716
3507.788766	484602.818270	41.126720
3507.682367	484522.738390	41.131725
3507.835557	484440.286679	41.136730
3507.596024	484361.392406	41.141735
3507.847859	484276.239283	41.146740
3507.545929	484219.139293	41.151744
3507.489780	484127.448004	41.156749
3507.331305	484047.830352	41.161754
3507.016093	483975.431380	41.166759
3507.085097	483902.870080	41.171764
3507.081350	483826.672200	41.176768
3507.100469	483749.355792	41.181773
3507.194522	483683.122734	41.186778
3507.152844	483608.095268	41.191783
3507.220505	483546.425725	41.196788
3506.867541	483483.150526	41.201792
3506.694896	483416.148069	41.206797
3507.119041	483340.032638	41.211802
3506.868510	483280.337820	41.216807
3506.907234	483208.741349	41.221812
3506.682162	483142.100890	41.226816
3506.866440	483077.067479	41.231821
3506.621641	483014.381645	41.236826
3506.378808	482958.839242	41.241831
3506.888297	482886.255182	41.246836
3506.366272	482831.161873	41.251840
3506.265486	482760.295131	41.256845
3506.582253	482684.295436	41.261850
3506.377000	482628.746149	41.266855
3506.331486	482572.816786	41.271860
3505.950907	482525.452346	41.276864
3506.231112	482451.078875	41.281869
3506.196132	482401.328800	41.286874
3505.917740	482349.691691	41.291879
3506.175655	482287.582738	41.296884
3505.978361	482244.647430	41.301888
3505.903468	482189.582967	41.306893
3506.372699	482144.464692	41.311898
3505.943087	482094.218853	41.316903
3505.927304	482037.523225	41.321908
3505.687158	481989.932611	41.326912
3505.663340	481955.532272	41.331917
3505.628821	481894.329658	41.336922
3505.458278	481860.205687	41.341927
3505.649626	481809.759630	41.346932
3505.533460	481780.541843	41.351936
3505.754478	481721.831766	41.356941
3505.694378	481674.718621	41.361946
3505.426384	481635.796046	41.366951
3505.742745	481586.343049	41.371956
3505.590361	481548.111404	41.376960
3505.697465	481498.792600	41.381965
3505.657737	481456.236013	41.386970
3505.698293	481397.046784	41.391975
3505.843710	481349.140316	41.396980
3505.548071	481314.781811	41.401984
3505.461631	481270.256052	41.406989
3505.731889	481228.663389	41.411994
3505.287326	481189.058442	41.416999
3505.720937	481135.278750	41.422004
3505.600834	481101.905547	41.427008
3505.319812	481045.400979	41.432013
3505.442692	481005.705973	41.437018
3505.067737	480971.967459	41.442023
3505.461316	480916.217308	41.447028
3505.291788	480887.513336	41.452032
3505.164215	480841.422283	41.457037
3505.415707	480809.915378	41.462042
3505.219558	480761.453398	41.467047
3505.219635	480735.762716	41.472052
3505.094883	480691.089681	41.477056
3504.908376	480655.851345	41.482061
3505.682703	480620.359735	41.487066
3505.022542	480597.458860	41.492071
3505.384593	480535.074526	41.497076
3505.274342	480505.752556	41.502080
3505.207073	480466.339877	41.507085
3505.238752	480437.046045	41.512090
3505.218051	480394.129437	41.517095
3505.401216	480344.694364	41.522100
3505.462720	480320.817660	41.527104
3505.061688	480277.251487	41.532109
3505.265205	480236.832758	41.537114
3505.163180	480197.577054	41.542119
3505.430991	480146.405208	41.547124
3505.071236	480114.943128	41.552128
3505.102083	480083.115218	41.557133
3505.357089	480045.018948	41.562138
3505.160046	480008.666293	41.567143
3505.210546	479963.507841	41.572148
3504.914251	479939.636553	41.577152
3504.753866	479906.571731	41.582157
3505.064960	479863.196130	41.587162
3504.574551	479830.436714	41.592167
3505.085223	479794.630573	41.597172
3504.903733	479773.933430	41.602176
3504.951690	479733.892978	41.607181
3505.047644	479698.304235	41.612186
3504.797190	479661.908707	41.617191
3504.992735	479627.875015	41.622196
3504.791274	479602.012008	41.627200
3504.952815	479566.361985	41.632205
3505.150956	479542.310717	41.637210
3504.785647	479504.716851	41.642215
3505.134751	479465.743113	41.647220
3504.861067	479427.222461	41.652224
3504.902372	479393.466120	41.657229
3504.985890	479369.128706	41.662234
3504.695834	479337.705044	41.667239
3505.163086	479296.837300	41.672244
3504.752060	479264.621830	41.677248
3504.796115	479237.452644	41.682253
3504.901531	479210.932511	41.687258
3504.789160	479181.659582	41.692263
3504.907708	479150.424420	41.697268
3505.021197	479117.365665	41.702272
3504.747580	479080.009878	41.707277
3505.040073	479050.267354	41.712282
3504.915094	479020.489416	41.717287
3505.060073	478979.570603	41.722292
3504.698889	478962.296339	41.727296
3504.685957	478918.361763	41.732301
3504.888657	478894.359664	41.737306
3504.614122	478857.763754	41.742311
3504.767043	478825.053017	41.747316
3504.746645	478800.021851	41.752320
3504.712967	478758.421341	41.757325
3504.828884	478736.865270	41.762330
3504.470231	478711.330006	41.767335
3504.793063	478689.386439	41.772340
3505.058766	478642.670637	41.777344
3504.803142	478618.537936	41.782349
3504.974806	478581.465572	41.787354
3504.673849	478564.029408	41.792359
3504.977285	478530.990331	41.797364
3504.623666	478497.193529	41.802368
3504.576615	478469.530913	41.807373
3504.602367	478423.916757	41.812378
3504.699262	478418.529614	41.817383
3504.735862	478380.515341	41.822388
3504.634977	478357.878208	41.827392
3504.322084	478318.043963	41.832397
3504.413577	478303.130131	41.837402
3504.302404	478263.821356	41.842407
3504.252135	478248.625819	41.847412
3504.437699	478224.017478	41.852416
3504.191122	478207.687332	41.857421
3504.619881	478178.327393	41.862426
3504.133105	478161.579067	41.867431
3504.452478	478122.100603	41.872436
3504.597261	478111.840649	41.877440
3504.693811	478082.938507	41.882445
3504.891123	478052.550709	41.887450
3504.663215	478021.216493	41.892455
3504.227418	477980.995567	41.897460
3504.649416	477965.674490	41.902464
3504.214054	477940.606470	41.907469
3504.550617	477915.568448	41.912474
3504.363642	477905.715579	41.917479
3504.346104	477859.904255	41.922484
3504.401921	477845.907948	41.927488
3504.326614	477833.858177	41.932493
3504.489031	477808.898226	41.937498
3504.533054	477780.510743	41.942503
3504.457308	477755.841767	41.947508
3504.466832	477739.876196	41.952512
3504.387323	477703.196653	41.957517
3504.650220	477674.014227	41.962522
3504.442168	477663.201651	41.967527
3504.702634	477626.316192	41.972532
3504.500584	477592.493894	41.977536
3504.418251	477575.275707	41.982541
3504.424824	477553.026115	41.987546
3504.698358	477526.071720	41.992551
3504.681126	477491.814598	41.997556
3504.636366	477479.658423	42.002560
3504.522805	477442.071536	42.007565
3504.659122	477411.743083	42.012570
3504.092288	477388.519647	42.017575
3504.481023	477365.398552	42.022580
3504.706016	477327.859300	42.027584
3504.444279	477325.011904	42.032589
3504.694294	477283.718237	42.037594
3504.356903	477260.762472	42.042599
3504.534715	477239.042955	42.047604
3504.597993	477213.743163	42.052608
3504.620128	477178.668384	42.057613
3504.433746	477160.959474	42.062618
3504.049714	477132.131914	42.067623
3504.339642	477110.698625	42.072628
3504.441528	477091.423651	42.077632
3504.370136	477072.176046	42.082637
3504.647838	477035.742906	42.087642
3504.599955	477006.811353	42.092647
3504.367764	476985.764544	42.097652
3504.546880	476963.334979	42.102656
3504.127212	476947.385929	42.107661
3504.334807	476904.577733	42.112666
3504.019280	476897.836275	42.117671
3504.202535	476860.910926	42.122676
3504.739916	476851.044409	42.127680
3504.082067	476821.499450	42.132685
3504.384221	476799.252983	42.137690
3503.955466	476785.687298	42.142695
3504.348414	476757.445941	42.147700
3504.353149	476736.716197	42.152704
3504.213430	476720.418624	42.157709
3504.669717	476686.034596	42.162714
3504.098374	476680.397828	42.167719
3504.366727	476639.150616	42.172724
3504.783305	476614.959923	42.177728
3504.277565	476592.790238	42.182733
3504.550160	476568.520881	42.187738
3504.610645	476546.819158	42.192743
3504.665821	476507.227217	42.197748
3504.347530	476492.022022	42.202752
3504.174875	476460.473892	42.207757
3504.357465	476437.840458	42.212762
3504.172164	476425.452442	42.217767
3504.401310	476409.451096	42.222772
3504.575399	476370.600336	42.227776
3504.160389	476357.082871	42.232781
3504.210522	476333.355224	42.237786
3504.256640	476315.710184	42.242791
3504.690223	476287.259010	42.247796
3504.320022	476258.985523	42.252800
3504.479056	476242.944443	42.257805
3504.727177	476208.947285	42.262810
3504.262253	476189.456931	42.267815
3504.526476	476153.835259	42.272820
3504.473197	476127.386793	42.277824
3504.317235	476104.705127	42.282829
3504.399653	476079.502246	42.287834
3504.287533	476055.546497	42.292839
3504.082325	476027.145237	42.297844
3504.154041	476014.361555	42.302848
3504.202734	475994.080253	42.307853
3504.379839	475961.411689	42.312858
3503.846698	475952.930359	42.317863
3503.818493	475922.017446	42.322868
3504.249285	475910.444051	42.327872
3503.728407	475898.564908	42.332877
3503.906522	475873.853488	42.337882
3503.797947	475878.685707	42.342887
3504.194790	475846.438386	42.347892
3504.334355	475841.550651	42.352896
3504.067422	475810.523245	42.357901
3504.203757	475780.800539	42.362906
3503.950551	475783.374831	42.367911
3503.934508	475749.215911	42.372916
3504.454280	475741.987244	42.377920
3504.328992	475725.331789	42.382925
3504.256272	475700.507748	42.387930
3504.137560	475671.990945	42.392935
3504.307800	475656.048995	42.397940
3504.417480	475626.228904	42.402944
3503.869880	475614.353816	42.407949
3503.979131	475578.856992	42.412954
3504.026458	475571.398826	42.417959
3503.811826	475548.421695	42.422964
3504.074922	475534.745810	42.427968
3503.903839	475519.161813	42.432973
3504.047206	475504.085642	42.437978
3504.076729	475481.221899	42.442983
3504.241023	475465.432796	42.447988
3504.134779	475445.226116	42.452992
3503.857091	475431.128780	42.457997
3504.106794	475400.424569	42.463002
3503.864130	475400.310904	42.468007
3503.726601	475383.859844	42.473012
3503.789968	475353.995984	42.478016
3503.571119	475355.753928	42.483021
3503.411957	475343.614541	42.488026
3503.433186	475330.787719	42.493031
3503.837578	475297.220496	42.498036
3504.066699	475304.026913	42.503040
3503.795285	475295.605307	42.508045
3503.884939	475266.396080	42.513050
3503.925573	475270.343200	42.518055
3504.192593	475241.866192	42.523060
3504.247819	475219.910440	42.528064
3503.706083	475207.375265	42.533069
3504.243776	475181.845871	42.538074
3504.093190	475178.220305	42.543079
3503.701130	475150.810379	42.548084
3503.775624	475132.551583	42.553088
3503.930876	475123.504918	42.558093
3504.224557	475105.870375	42.563098
3504.362082	475086.993338	42.568103
3504.186435	475060.613499	42.573108
3503.973175	475051.371616	42.578112
3503.870099	475036.486108	42.583117
3504.079040	475016.938793	42.588122
3504.038126	475001.485881	42.593127
3504.056064	474973.402671	42.598132
3504.356064	474965.802972	42.603136
3504.028753	474939.599006	42.608141
3504.212000	474911.540269	42.613146
3504.090427	474889.257294	42.618151
3503.952861	474876.658030	42.623156
3504.097232	474874.607771	42.628160
3503.988093	474844.871799	42.633165
3503.997587	474826.420252	42.638170
3504.037309	474808.977652	42.643175
3503.909474	474786.695553	42.648180
3504.123352	474772.317312	42.653184
3503.799286	474758.277524	42.658189
3503.846519	474744.635224	42.663194
3504.071874	474727.416649	42.668199
3503.940726	474710.153034	42.673204
3503.973873	474688.757756	42.678208
3503.731303	474679.013460	42.683213
3504.146753	474659.686597	42.688218
3503.806956	474644.179278	42.693223
3504.005157	474625.089470	42.698228
3504.216310	474598.394453	42.703232
3503.801456	474599.828628	42.708237
3504.191519	474566.465209	42.713242
3503.957307	474550.383565	42.718247
3503.960556	474531.273795	42.723252
3504.074197	474514.427511	42.728256
3503.698071	474502.727414	42.733261
3504.283507	474466.849245	42.738266
3503.973985	474469.990171	42.743271
3503.804100	474444.368936	42.748276
3503.906097	474430.616393	42.753280
3503.574050	474430.567537	42.758285
3503.540416	474402.187558	42.763290
3503.911063	474391.281749	42.768295
3504.011652	474382.192706	42.773300
3504.002132	474356.495325	42.778304
3503.579563	474358.234865	42.783309
3503.665086	474334.651339	42.788314
3503.726704	474332.107223	42.793319
3503.671989	474307.836196	42.798324
3503.756313	474311.371091	42.803329
3503.793055	474300.974205	42.808333
3503.727674	474270.723590	42.813338
3503.607682	474270.083643	42.818343
3503.649629	474264.450631	42.823348
3503.924228	474238.404062	42.828353
3503.920925	474224.161137	42.833357
3504.212015	474207.286552	42.838362
3503.985978	474184.512426	42.843367
3503.933957	474171.341626	42.848372
3504.029558	474156.525446	42.853377
3503.654524	474140.009535	42.858381
3503.862515	474133.285777	42.863386
3503.797997	474108.052973	42.868391
3503.524068	474095.221332	42.873396
3503.925756	474075.237133	42.878401
3503.864180	474078.440307	42.883405
3503.867679	474045.035753	42.888410
3504.056658	474043.079738	42.893415
3503.819366	474019.648249	42.898420
3503.989496	473996.912673	42.903425
3503.530685	474000.432091	42.908429
3503.812844	473964.195457	42.913434
3504.104784	473963.743838	42.918439
3503.959511	473943.845962	42.923444
3504.012244	473926.299168	42.928449
3503.874491	473917.146210	42.933453
3503.960252	473890.672839	42.938458
3504.044286	473884.526175	42.943463
3503.899411	473867.821596	42.948468
3504.238481	473837.709166	42.953473
3503.850136	473821.752684	42.958477
3503.725189	473816.602133	42.963482
3503.886202	473792.499151	42.968487
3503.917348	473782.356332	42.973492
3504.358152	473761.301160	42.978497
3504.152685	473744.048469	42.983501
3504.126927	473722.712172	42.988506
3503.910229	473697.807051	42.993511
3503.580620	473699.126433	42.998516
3504.022818	473670.264703	43.003521
3503.804466	473660.516089	43.008525
3503.825015	473644.292079	43.013530
3503.894823	473635.663777	43.018535
3503.986614	473622.824722	43.023540
3504.124647	473598.116861	43.028545
3503.738568	473587.583680	43.033549
3503.928977	473576.503164	43.038554
3503.881872	473558.414241	43.043559
3504.025206	473542.120051	43.048564
3503.721559	473521.182298	43.053569
3503.779266	473506.219563	43.058573
3503.644077	473490.020045	43.063578
3503.577899	473486.279452	43.068583
3503.764101	473473.982975	43.073588
3503.835613	473449.488210	43.078593
3503.632266	473449.266935	43.083597
3503.648306	473432.283111	43.088602
3503.766884	473436.421031	43.093607
3503.542713	473403.862458	43.098612
3503.848531	473388.708349	43.103617
3503.626621	473395.738771	43.108621
3503.646567	473365.878847	43.113626
3503.637376	473359.290543	43.118631
3503.796622	473347.353086	43.123636
3504.296238	473333.334191	43.128641
3503.573575	473315.351830	43.133645
3503.832312	473300.053024	43.138650
3503.743816	473302.297447	43.143655
3503.798052	473269.187746	43.148660
3503.766978	473267.925421	43.153665
3503.769950	473258.090941	43.158669
3503.829114	473224.473479	43.163674
3503.835282	473223.712175	43.168679
3503.722999	473214.554875	43.173684
3503.784571	473178.554475	43.178689
3503.342046	473180.804178	43.183693
3503.610782	473169.964517	43.188698
3503.955827	473157.997581	43.193703
3503.930435	473138.637573	43.198708
3503.801368	473128.975974	43.203713
3503.625711	473128.547554	43.208717
3503.724891	473095.024936	43.213722
3503.795185	473085.027658	43.218727
3503.833852	473085.629881	43.223732
3504.100426	473052.131426	43.228737
3503.543354	473035.643388	43.233741
3504.087414	473032.718706	43.238746
3504.108294	473003.973319	43.243751
3503.694876	472993.748301	43.248756
3503.673408	472975.401351	43.253761
3503.375798	472948.480434	43.258765
3503.726124	472946.853655	43.263770
3503.626776	472945.297951	43.268775
3503.658182	472942.352903	43.273780
3504.048271	472914.005259	43.278785
3503.638078	472917.872018	43.283789
3503.705983	472893.782691	43.288794
3503.959409	472878.940636	43.293799
3503.640683	472857.446972	43.298804
3503.838260	472857.010245	43.303809
3503.591416	472835.403813	43.308813
3503.996066	472823.579337	43.313818
3503.779495	472820.622774	43.318823
3503.744489	472795.586448	43.323828
3503.753864	472765.930086	43.328833
3503.496415	472772.408724	43.333837
3503.842827	472762.164876	43.338842
3504.021706	472741.352823	43.343847
3503.648015	472736.089237	43.348852
3503.841048	472722.929460	43.353857
3503.619463	472694.678192	43.358861
3503.704192	472680.521659	43.363866
3503.872112	472676.946686	43.368871
3503.705012	472657.862082	43.373876
3504.141577	472631.838555	43.378881
3503.531731	472643.442186	43.383885
3503.841516	472620.378849	43.388890
3503.844902	472598.529844	43.393895
3503.438038	472597.985879	43.398900
3503.618119	472577.883166	43.403905
3503.512270	472565.936460	43.408909
3503.681767	472556.176707	43.413914
3503.516406	472550.271831	43.418919
3503.214482	472557.720729	43.423924
3503.875657	472517.771746	43.428929
3503.469506	472507.291870	43.433933
3503.527359	472496.535878	43.438938
3503.597243	472493.483297	43.443943
3503.306551	472494.036210	43.448948
3503.869980	472464.291838	43.453953
3503.678067	472470.151898	43.458957
3503.939172	472457.589506	43.463962
3504.003186	472433.703024	43.468967
3503.751282	472426.088229	43.473972
3504.252981	472400.054113	43.478977
3503.513955	472381.566580	43.483981
3503.935400	472374.656428	43.488986
3503.843329	472362.707426	43.493991
3503.814226	472346.439539	43.498996
3503.807909	472324.743856	43.504001
3503.673458	472321.977013	43.509005
3504.030870	472301.389761	43.514010
3504.197991	472281.947820	43.519015
3503.670288	472273.464079	43.524020
3503.963136	472237.476161	43.529025
3503.882675	472237.032674	43.534029
3504.046039	472230.872975	43.539034
3503.699266	472215.821146	43.544039
3503.848162	472213.871293	43.549044
3503.985966	472185.714599	43.554049
3503.924867	472180.604236	43.559053
3503.771133	472157.715028	43.564058
3503.984820	472134.767722	43.569063
3503.589085	472128.747056	43.574068
3503.844665	472113.802720	43.579073
3503.742199	472094.200436	43.584077
3503.929726	472076.732136	43.589082
3503.930945	472066.390421	43.594087
3503.867023	472047.846573	43.599092
3504.018099	472024.250018	43.604097
3503.769262	472022.109542	43.609101
3503.909658	471990.657058	43.614106
3503.859085	471982.249863	43.619111
3503.799614	471971.512139	43.624116
3504.392284	471944.905433	43.629121
3503.831587	471944.030903	43.634125
3503.822021	471916.505463	43.639130
3503.513656	471905.249407	43.644135
3503.875834	471893.887360	43.649140
3503.990666	471886.619953	43.654145
3503.630488	471867.210269	43.659149
3504.036698	471848.591933	43.664154
3503.947584	471836.591462	43.669159
3503.580845	471828.386261	43.674164
3504.034673	471806.566605	43.679169
3503.871249	471786.973663	43.684173
3503.628975	471771.093876	43.689178
3503.624070	471756.748094	43.694183
3503.281908	471755.585540	43.699188
3503.897190	471714.324188	43.704193
3503.394604	471722.818999	43.709197
3503.584755	471716.553523	43.714202
3503.356199	471710.252835	43.719207
3503.312925	471701.540202	43.724212
3503.628184	471680.299958	43.729217
3503.468146	471678.348191	43.734221
3503.757099	471672.928897	43.739226
3503.438569	471672.016078	43.744231
3503.611044	471643.194127	43.749236
3504.006151	471636.338586	43.754241
3503.509154	471635.099108	43.759245
3503.579297	471625.962957	43.764250
3503.904444	471603.656476	43.769255
3503.597370	471588.547216	43.774260
3503.536904	471586.275530	43.779265
3503.508891	471566.458194	43.784269
3503.616281	471539.471411	43.789274
3503.875756	471549.620176	43.794279
3503.581837	471538.615111	43.799284
3503.967002	471521.520663	43.804289
3503.204334	471515.456422	43.809293
3503.801901	471511.154299	43.814298
3504.082726	471502.238270	43.819303
3503.516005	471485.192855	43.824308
3503.881173	471459.179130	43.829313
3503.755799	471462.899750	43.834317
3503.558355	471430.333813	43.839322
3503.674362	471417.489548	43.844327
3503.693433	471408.564155	43.849332
3503.945447	471400.920025	43.854337
3504.101775	471370.630072	43.859341
3504.180942	471356.676288	43.864346
3504.147546	471341.219414	43.869351
3503.702387	471327.855442	43.874356
3504.184720	471309.021805	43.879361
3503.820045	471293.262386	43.884365
3504.010320	471282.383436	43.889370
3504.047587	471252.213520	43.894375
3503.788146	471235.778377	43.899380
3503.917739	471230.181372	43.904385
3503.898594	471211.477605	43.909389
3503.632905	471196.919172	43.914394
3504.348681	471179.873578	43.919399
3503.696627	471170.040236	43.924404
3503.942816	471144.653274	43.929409
3503.691962	471126.594407	43.934413
3503.754864	471097.434138	43.939418
3503.663806	471090.908741	43.944423
3503.433205	471091.502887	43.949428
3503.705901	471049.990177	43.954433
3503.646173	471058.618048	43.959437
3503.350807	471044.114894	43.964442
3503.300836	471049.344564	43.969447
3503.391171	471039.343122	43.974452
3503.482010	471012.763837	43.979457
3503.455333	471008.002616	43.984461
3503.528970	470995.468965	43.989466
3503.744673	471002.988697	43.994471
3503.273541	470994.191302	43.999476
3503.937530	470959.460600	44.004481
3503.571777	470966.210406	44.009485
3503.733273	470957.819970	44.014490
3503.594426	470944.001759	44.019495
3503.305253	470918.851228	44.024500
3503.649330	470903.283666	44.029505
3503.919161	470911.656722	44.034509
3503.846820	470895.749399	44.039514
3503.748328	470877.716929	44.044519
3503.609636	470873.784532	44.049524
3503.757917	470855.053978	44.054529
3503.708312	470834.428200	44.059533
3503.815384	470821.838462	44.064538
3503.831482	470813.623040	44.069543
3503.734928	470808.467242	44.074548
3503.607536	470782.986792	44.079553
3503.740091	470786.818857	44.084557
3503.586555	470767.426170	44.089562
3503.926637	470741.466203	44.094567
3503.467129	470746.050920	44.099572
3503.680419	470733.190853	44.104577
3503.624434	470712.109686	44.109581
3503.389782	470693.540907	44.114586
3503.742744	470691.710750	44.119591
3503.603930	470692.391793	44.124596
3503.686636	470666.117531	44.129601
3503.622939	470656.089553	44.134605
3503.503263	470658.136403	44.139610
3503.678411	470642.341859	44.144615
3503.433519	470639.288060	44.149620
3503.596433	470617.361038	44.154625
3503.457911	470611.907639	44.159629
3503.554931	470598.102614	44.164634
3504.222520	470597.135275	44.169639
3503.576616	470585.576963	44.174644
3503.831720	470563.128337	44.179649
3503.783281	470559.080220	44.184653
3503.695922	470533.035460	44.189658
3503.936760	470513.225315	44.194663
3503.501838	470515.981077	44.199668
3503.763405	470493.227167	44.204673
3503.973067	470470.684228	44.209677
3503.400682	470472.346370	44.214682
3503.824958	470455.447652	44.219687
3503.580299	470438.756046	44.224692
3503.846155	470418.992555	44.229697
3503.910056	470419.945755	44.234701
3503.853595	470392.628485	44.239706
3504.086472	470369.067804	44.244711
3503.593648	470371.629944	44.249716
3503.788234	470344.729214	44.254721
3504.012074	470336.125879	44.259725
3503.922059	470324.226066	44.264730
3503.972695	470300.998303	44.269735
3503.718115	470298.706458	44.274740
3503.989316	470278.435006	44.279745
3503.700810	470268.087484	44.284749
3503.578329	470256.040668	44.289754
3503.776062	470236.389167	44.294759
3503.399967	470221.492607	44.299764
3503.923201	470212.791200	44.304769
3503.954269	470199.604715	44.309773
3503.606082	470183.537650	44.314778
3503.843648	470162.358826	44.319783
3503.627217	470169.947165	44.324788
3503.815444	470139.396874	44.329793
3503.944741	470130.453507	44.334797
3503.947832	470119.806327	44.339802
3504.417512	470094.839042	44.344807
3503.698148	470092.113649	44.349812
3503.964112	470065.860359	44.354817
3503.843547	470044.585925	44.359821
3503.801226	470035.061255	44.364826
3503.903531	470029.062648	44.369831
3503.778009	470004.544224	44.374836
3503.777307	469981.932605	44.379841
3503.813513	469986.895427	44.384845
3503.697919	469956.190091	44.389850
3503.856584	469940.701813	44.394855
3503.586349	469943.786513	44.399860
3503.646191	469918.630299	44.404865
3503.458835	469913.792825	44.409869
3503.813368	469897.563767	44.414874
3503.712541	469891.293031	44.419879
3503.682442	469871.474399	44.424884
3503.721120	469861.936848	44.429889
3503.403695	469860.618175	44.434893
3503.361753	469856.213998	44.439898
3503.794516	469823.292419	44.444903
3503.607947	469816.629618	44.449908
3503.491814	469817.104307	44.454913
3503.731355	469806.216795	44.459917
3503.718148	469780.412866	44.464922
3504.090451	469777.109287	44.469927
3503.532081	469763.863592	44.474932
3503.521956	469730.859770	44.479937
3503.325747	469728.051639	44.484941
3503.542663	469726.141503	44.489946
3503.790590	469713.934427	44.494951
3503.606155	469697.080605	44.499956
3503.510430	469684.978528	44.504961
3503.351656	469675.421401	44.509965
3503.631345	469664.426070	44.514970
3504.087436	469660.044532	44.519975
3503.519493	469637.268697	44.524980
3503.719302	469626.488771	44.529985
3503.688781	469623.755837	44.534989
3503.711677	469601.444274	44.539994
3503.607415	469578.240185	44.544999
3503.574196	469582.757776	44.550004
3503.746613	469574.263655	44.555009
3503.530975	469549.657536	44.560013
3503.681660	469544.360944	44.565018
3503.586408	469541.029829	44.570023
3503.762563	469534.461705	44.575028
3504.098690	469506.270013	44.580033
3503.810155	469493.437797	44.585037
3503.465457	469479.042741	44.590042
3503.717216	469447.112483	44.595047
3503.525923	469452.669095	44.600052
3503.657941	469444.029205	44.605057
3503.490692	469440.354550	44.610061
3503.377458	469419.990923	44.615066
3503.650711	469414.320022	44.620071
3503.611298	469404.186199	44.625076
3503.765642	469397.773581	44.630081
3503.664667	469389.829602	44.635085
3503.390894	469378.668098	44.640090
3503.535833	469361.204237	44.645095
3503.451293	469365.679287	44.650100
3503.554784	469358.514186	44.655105
3503.642523	469341.059350	44.660109
3503.234265	469325.558820	44.665114
3503.549061	469325.255598	44.670119
3503.272844	469319.063112	44.675124
3503.555949	469313.644131	44.680129
3503.444887	469292.519525	44.685133
3503.206113	469286.523914	44.690138
3503.465976	469277.103237	44.695143
3503.503284	469268.376842	44.700148
3503.493342	469275.577963	44.705153
3503.288690	469267.853127	44.710157
3503.287480	469237.787761	44.715162
3503.231639	469236.731906	44.720167
3503.285463	469228.915500	44.725172
3503.370921	469231.994785	44.730177
3503.336421	469219.477153	44.735181
3503.202913	469224.771187	44.740186
3503.607303	469216.493759	44.745191
3503.554840	469198.300450	44.750196
3503.471124	469198.364420	44.755201
3503.576720	469190.539817	44.760205
3503.340577	469177.394918	44.765210
3503.458480	469183.815349	44.770215
3503.635495	469158.234086	44.775220
3503.653548	469135.669284	44.780225
3503.287305	469136.842634	44.785229
3503.109163	469137.022932	44.790234
3503.206656	469131.988149	44.795239
3503.426239	469133.626617	44.800244
3503.221489	469110.235084	44.805249
3503.156098	469107.203386	44.810253
3503.136651	469090.221592	44.815258
3503.363034	469089.780238	44.820263
3503.445840	469089.919291	44.825268
3503.365450	469088.106790	44.830273
3503.705757	469081.411176	44.835277
3503.025670	469059.666457	44.840282
3503.122072	469046.164705	44.845287
3503.262180	469044.875064	44.850292
3503.230247	469049.341867	44.855297
3503.110730	469045.456792	44.860301
3503.149365	469043.574774	44.865306
3503.349011	469042.529229	44.870311
3503.069552	469050.736353	44.875316
3503.273413	469044.569307	44.880321
3503.382442	469042.929668	44.885325
3503.099108	469038.664875	44.890330
3503.448175	469011.738003	44.895335
3503.562199	469008.221619	44.900340
3503.737960	468997.191663	44.905345
3503.606659	469000.406645	44.910349
3503.490219	468979.840289	44.915354
3503.470720	468964.835759	44.920359
3503.473942	468956.520234	44.925364
3503.593914	468951.583257	44.930369
3503.468114	468949.625817	44.935373
3503.413985	468928.897457	44.940378
3503.456057	468917.381573	44.945383
3503.481589	468910.684956	44.950388
3503.380832	468915.061262	44.955393
3503.693798	468909.941666	44.960397
3503.294860	468894.236535	44.965402
3503.472357	468883.104840	44.970407
3503.604362	468871.321208	44.975412
3503.220867	468872.700106	44.980417
3503.339928	468874.202378	44.985421
3503.033675	468875.569067	44.990426
3503.116475	468854.210568	44.995431
3503.419153	468848.230653	45.000436
3503.628258	468816.407574	45.005441
3503.566585	468830.512483	45.010445
3502.934015	468833.553212	45.015450
3503.445353	468826.424869	45.020455
3503.508056	468822.865864	45.025460
3503.266808	468806.071002	45.030465
3503.302569	468792.730777	45.035469
3503.576994	468784.017404	45.040474
3503.620357	468780.664257	45.045479
3503.289481	468773.161995	45.050484
3503.549925	468766.022586	45.055489
3503.332215	468756.575755	45.060493
3503.163126	468743.673494	45.065498
3503.375248	468728.784291	45.070503
3503.488091	468734.647936	45.075508
3503.259508	468725.861937	45.080513
3503.599709	468723.120991	45.085517
3503.321617	468707.751532	45.090522
3503.349275	468697.201146	45.095527
3503.103891	468701.853868	45.100532
3503.264484	468692.296511	45.105537
3503.465478	468694.901294	45.110541
3503.098385	468695.466376	45.115546
3503.432915	468686.135035	45.120551
3503.375221	468684.724530	45.125556
3503.348134	468673.625060	45.130561
3503.284951	468655.230162	45.135565
3503.320117	468649.748793	45.140570
3503.564342	468645.045617	45.145575
3503.376443	468660.640958	45.150580
3503.626096	468642.652922	45.155585
3503.708021	468614.398800	45.160589
3503.310233	468613.396962	45.165594
3503.315196	468602.444496	45.170599
3503.320581	468599.705752	45.175604
3503.166197	468592.986768	45.180609
3503.401194	468569.373015	45.185613
3503.286666	468568.681319	45.190618
3503.445256	468558.363681	45.195623
3503.196382	468575.895419	45.200628
3503.596191	468557.477957	45.205633
3503.592503	468571.016147	45.210637
3503.307577	468545.760661	45.215642
3503.743642	468528.706412	45.220647
3503.515444	468518.703402	45.225652
3503.305973	468518.280225	45.230657
3503.462548	468504.058776	45.235661
3503.404709	468498.439960	45.240666
3503.808175	468480.173960	45.245671
3503.446298	468476.631303	45.250676
3503.497268	468467.446090	45.255681
3503.767492	468452.446101	45.260685
3503.089884	468440.232462	45.265690
3503.186125	468433.930138	45.270695
3503.290818	468427.474368	45.275700
3503.152696	468423.947038	45.280705
3503.143366	468422.630277	45.285709
3503.187844	468423.282421	45.290714
3503.347385	468426.705035	45.295719
3503.233533	468433.213031	45.300724
3503.587010	468404.662190	45.305729
3503.472066	468390.686392	45.310733
3503.354310	468380.970077	45.315738
3503.544468	468368.365723	45.320743
3503.757297	468375.177022	45.325748
3503.507789	468352.552258	45.330753
3503.518551	468338.505853	45.335757
3503.532539	468334.751653	45.340762
3503.460845	468323.557642	45.345767
3503.598686	468344.679072	45.350772
3503.383909	468302.325272	45.355777
3503.322573	468301.371644	45.360781
3503.115310	468298.869284	45.365786
3503.604794	468298.284923	45.370791
3503.359518	468296.447712	45.375796
3503.368450	468289.601410	45.380801
3503.384353	468264.602254	45.385805
3503.239159	468254.078965	45.390810
3503.413226	468247.510768	45.395815
3503.246108	468247.435814	45.400820
3502.897638	468246.983898	45.405825
3503.336508	468241.489317	45.410829
3503.470986	468241.772319	45.415834
3503.363353	468230.634642	45.420839
3503.549918	468219.044831	45.425844
3503.464874	468200.247361	45.430849
3503.609130	468207.221665	45.435853
3503.210980	468202.974846	45.440858
3503.649888	468194.894374	45.445863
3503.573214	468174.168828	45.450868
3503.485444	468170.887014	45.455873
3503.495917	468160.440481	45.460877
3503.506663	468157.802238	45.465882
3503.568101	468151.099703	45.470887
3503.739368	468127.901153	45.475892
3503.715487	468118.271285	45.480897
3503.754596	468111.876488	45.485901
3503.654775	468090.799593	45.490906
3503.821753	468077.894506	45.495911
3503.371091	468077.306627	45.500916
3503.351727	468074.115392	45.505921
3503.859243	468052.536834	45.510925
3503.386092	468034.155485	45.515930
3503.805507	468028.410405	45.520935
3503.638449	468020.020014	45.525940
3503.758486	468004.232182	45.530945
3503.652566	467985.437819	45.535949
3503.429243	467978.171790	45.540954
3503.879987	467973.030190	45.545959
3503.726977	467962.964326	45.550964
3503.375912	467941.774880	45.555969
3503.786325	467936.386126	45.560973
3503.615987	467946.249666	45.565978
3503.759739	467916.666526	45.570983
3503.664556	467899.949257	45.575988
3503.761884	467892.632516	45.580993
3503.716196	467892.639775	45.585997
3503.697741	467870.992053	45.591002
3503.884531	467854.635812	45.596007
3503.761676	467836.198921	45.601012
3503.501921	467822.144223	45.606017
3503.814670	467803.435635	45.611021
3503.868166	467816.356823	45.616026
3503.513129	467793.596021	45.621031
3503.824217	467767.282006	45.626036
3503.476515	467766.931365	45.631041
3503.941918	467752.863412	45.636045
3503.304875	467741.809153	45.641050
3503.624984	467726.496534	45.646055
3503.815841	467715.362109	45.651060
3503.583336	467705.562208	45.656065
3504.071646	467683.986308	45.661069
3503.678881	467674.110314	45.666074
3503.623585	467652.620303	45.671079
3503.536877	467642.036758	45.676084
3503.768609	467637.284627	45.681089
3503.793350	467634.948335	45.686093
3503.569061	467613.332881	45.691098
3503.931427	467594.717674	45.696103
3503.779423	467593.879755	45.701108
3503.395319	467577.207894	45.706113
3503.667279	467550.088513	45.711117
3503.349223	467548.465559	45.716122
3504.007067	467546.434829	45.721127
3503.771147	467529.790214	45.726132
3503.910773	467502.032523	45.731137
3503.511564	467490.534898	45.736141
3503.459358	467482.075433	45.741146
3503.870519	467478.714649	45.746151
3503.760095	467456.624690	45.751156
3503.622550	467459.181727	45.756161
3503.679610	467442.034387	45.761165
3503.508800	467429.841461	45.766170
3503.397697	467416.371458	45.771175
3503.187892	467416.455362	45.776180
3503.136286	467408.350710	45.781185
3503.700209	467403.140377	45.786189
3503.258461	467382.725279	45.791194
3503.402499	467364.093673	45.796199
3503.380630	467360.902726	45.801204
3503.171236	467366.057107	45.806209
3503.272123	467357.776215	45.811213
3503.248452	467353.520738	45.816218
3503.538659	467356.314410	45.821223
3503.649152	467345.496724	45.826228
3503.452833	467326.411826	45.831233
3503.549890	467310.018639	45.836237
3503.629116	467314.316125	45.841242
3503.489670	467302.675928	45.846247
3503.529770	467279.598585	45.851252
3503.360793	467270.954669	45.856257
3503.882368	467262.860775	45.861261
3503.501953	467272.859247	45.866266
3503.274766	467245.514135	45.871271
3503.376582	467242.151503	45.876276
3503.366287	467238.502357	45.881281
3503.360065	467224.255068	45.886285
3503.170437	467234.882577	45.891290
3503.601276	467227.005833	45.896295
3503.595410	467221.074225	45.901300
3503.642000	467190.694129	45.906305
3503.929015	467183.144337	45.911309
3503.592464	467174.121222	45.916314
3503.206910	467156.485844	45.921319
3503.437547	467145.801183	45.926324
3503.416363	467142.204447	45.931329
3503.717802	467138.100363	45.936333
3503.347414	467131.009403	45.941338
3503.424474	467118.979942	45.946343
3503.360177	467097.845729	45.951348
3503.261718	467095.579556	45.956353
3503.183127	467085.349390	45.961357
3503.295589	467088.627547	45.966362
3503.176673	467085.096955	45.971367
3503.030169	467093.638769	45.976372
3503.084711	467086.632748	45.981377
3503.382444	467092.569043	45.986381
3502.935196	467077.326535	45.991386
3503.259264	467072.458270	45.996391
3503.245660	467058.009211	46.001396
3503.332966	467039.944052	46.006401
3503.414209	467046.877996	46.011405
3503.369672	467048.304846	46.016410
3503.360110	467046.075323	46.021415
3503.379333	467048.303394	46.026420
3503.163856	467032.314333	46.031425
3503.353732	467004.953694	46.036429
3503.184836	467011.369417	46.041434
3503.056705	466993.338270	46.046439
3503.626226	466997.355500	46.051444
3503.573681	467003.955660	46.056449
3503.446919	466998.398042	46.061453
3503.388980	466980.913560	46.066458
3503.498340	466955.999487	46.071463
3503.060547	466963.116910	46.076468
3503.157282	466950.374353	46.081473
3503.261209	466941.281515	46.086477
3503.005047	466951.514031	46.091482
3503.308962	466943.657245	46.096487
3503.269451	466957.709202	46.101492
3502.948854	466958.672628	46.106497
3503.142404	466944.089335	46.111501
3503.101546	466953.222985	46.116506
3503.173187	466922.838543	46.121511
3503.327218	466912.470111	46.126516
3503.222044	466911.523349	46.131521
3503.214080	466901.180517	46.136525
3503.418595	466904.139914	46.141530
3503.447421	466906.366482	46.146535
3503.545453	466897.984448	46.151540
3503.450928	466901.143231	46.156545
3503.343420	466872.105402	46.161549
3503.212748	466868.678045	46.166554
3503.502011	466864.677246	46.171559
3503.468866	466864.023337	46.176564
3503.032747	466868.605196	46.181569
3503.493334	466844.751022	46.186573
3503.229943	466840.634744	46.191578
3503.081368	466812.465337	46.196583
3503.288394	466811.621345	46.201588
3503.424954	466814.439375	46.206593
3503.172393	466805.301412	46.211597
3503.299176	466813.445196	46.216602
3503.332571	466809.383416	46.221607
3503.314724	466808.321433	46.226612
3503.285399	466786.065831	46.231617
3503.748002	466766.115673	46.236621
3503.177526	466771.225858	46.241626
3503.004395	466772.673052	46.246631
3503.131136	466763.170877	46.251636
3503.100382	466772.810077	46.256641
3503.477717	466773.257541	46.261645
3503.141937	466776.353062	46.266650
3503.436128	466758.559203	46.271655
3503.392361	466733.516950	46.276660
3503.116243	466730.974577	46.281665
3503.215127	466721.933149	46.286669
3503.157632	466733.503457	46.291674
3503.125669	466723.468573	46.296679
3503.333947	466722.624379	46.301684
3503.339625	466725.767350	46.306689
3503.358012	466729.263261	46.311693
3503.382140	466711.410634	46.316698
3503.437967	466692.336014	46.321703
3503.457196	466678.743524	46.326708
3503.054848	466693.512200	46.331713
3503.700574	466684.536443	46.336717
3503.416973	466681.944540	46.341722
3503.447499	466662.620356	46.346727
3503.444705	466645.076172	46.351732
3503.554505	466641.002283	46.356737
3503.413671	466642.850038	46.361741
3503.308638	466648.647291	46.366746
3503.426595	466626.520363	46.371751
3503.557176	466605.506975	46.376756
3503.234860	466605.912909	46.381761
3503.746533	466595.741329	46.386765
3503.707310	466594.175641	46.391770
3503.839098	466570.068885	46.396775
3503.549742	466550.896574	46.401780
3503.495710	466545.834415	46.406785
3503.625490	466536.788024	46.411789
3503.159312	466528.089363	46.416794
3503.195280	466522.658021	46.421799
3503.330967	466517.312330	46.426804
3503.127870	466522.415214	46.431809
3503.419711	466513.241783	46.436813
3503.443281	466524.697977	46.441818
3503.403558	466510.607623	46.446823
3503.347482	466497.888947	46.451828
3503.058339	466482.823847	46.456833
3503.472314	466459.382267	46.461837
3503.111101	466473.181150	46.466842
3503.074283	466459.749501	46.471847
3502.998104	466468.635405	46.476852
3503.122592	466470.136993	46.481857
3503.011272	466469.647550	46.486861
3503.443195	466462.023890	46.491866
3503.317808	466465.136909	46.496871
3503.389118	466468.776620	46.501876
3503.354371	466442.718445	46.506881
3503.342567	466431.868914	46.511885
3503.257125	466424.428430	46.516890
3503.211992	466421.697387	46.521895
3503.444832	466423.486098	46.526900
3503.139031	466426.069854	46.531905
3503.593080	466419.710373	46.536909
3503.442681	466394.938112	46.541914
3503.502982	466376.673823	46.546919
3503.242017	466382.800043	46.551924
3503.131272	466376.377696	46.556929
3503.499499	466369.119025	46.561933
3503.030768	466371.880664	46.566938
3503.394331	466379.277282	46.571943
3503.670429	466354.741808	46.576948
3503.689862	466338.309428	46.581953
3503.660295	466334.764587	46.586957
3503.677202	466333.544963	46.591962
3503.270044	466299.939291	46.596967
3503.467429	466289.665117	46.601972
3503.388014	466283.846287	46.606977
3503.441483	466267.712721	46.611981
3503.507471	466267.398080	46.616986
3503.342966	466262.099774	46.621991
3503.367066	466240.494357	46.626996
3503.414915	466242.363032	46.632001
3503.497134	466244.023442	46.637005
3503.377935	466240.289920	46.642010
3503.585651	466223.219193	46.647015
3503.398574	466200.886493	46.652020
3503.052087	466205.657159	46.657025
3503.448683	466189.570715	46.662029
3503.056570	466195.159927	46.667034
3503.260613	466188.079269	46.672039
3503.600104	466188.938395	46.677044
3502.952916	466188.837894	46.682049
3503.325712	466198.058613	46.687053
3503.373909	466177.260655	46.692058
3503.302439	466162.566587	46.697063
3503.524709	466151.274248	46.702068
3503.118702	466156.409291	46.707073
3503.631142	466145.071083	46.712077
3503.370066	466146.937887	46.717082
3503.265258	466134.683070	46.722087
3503.445655	466114.726197	46.727092
3503.302791	466112.061269	46.732097
3503.441959	466101.441248	46.737101
3503.347533	466105.715719	46.742106
3503.383652	466099.422201	46.747111
3503.387469	466096.531254	46.752116
3502.921498	466083.724990	46.757121
3503.340069	466069.764739	46.762125
3503.030334	466066.923347	46.767130
3503.297795	466055.471688	46.772135
3503.403768	466064.785348	46.777140
3503.313603	466055.012887	46.782145
3503.302012	466059.020733	46.787149
3503.198658	466058.479313	46.792154
3503.332365	466047.910836	46.797159
3503.444327	466037.396499	46.802164
3503.121832	466022.894138	46.807169
3503.672159	466004.754910	46.812173
3503.288477	466012.117640	46.817178
3503.394154	466006.066643	46.822183
3503.537560	466009.897873	46.827188
3503.255377	465985.551631	46.832193
3503.601440	465979.614757	46.837197
3503.719091	465973.764693	46.842202
3503.619207	465975.555325	46.847207
3503.489064	465952.351314	46.852212
3503.420864	465940.293433	46.857217
3503.474704	465933.084306	46.862221
3503.585852	465931.393383	46.867226
3503.484237	465917.464543	46.872231
3503.722536	465908.451440	46.877236
3503.258186	465895.087008	46.882241
3503.300799	465878.954862	46.887245
3503.296452	465885.902715	46.892250
3503.470321	465877.102619	46.897255
3503.606673	465873.277931	46.902260
3503.400231	465870.166641	46.907265
3503.651522	465837.673176	46.912269
3503.613915	465827.334503	46.917274
3503.421791	465831.624472	46.922279
3503.541785	465834.242416	46.927284
3503.361785	465815.102862	46.932289
3503.352426	465799.283124	46.937293
3503.570384	465802.747644	46.942298
3503.401459	465793.393185	46.947303
3503.467719	465790.137362	46.952308
3503.393586	465769.358339	46.957313
3503.367960	465754.149649	46.962317
3503.509992	465737.291751	46.967322
3503.321014	465748.832670	46.972327
3503.545886	465739.923037	46.977332
3503.549572	465746.717539	46.982337
3503.451248	465708.194019	46.987341
3503.403871	465710.128502	46.992346
3503.462210	465697.999772	46.997351
3503.601397	465709.488843	47.002356
3503.430082	465689.840709	47.007361
3503.119568	465659.717694	47.012365
3503.254938	465664.970123	47.017370
3503.153438	465652.765213	47.022375
3503.247424	465658.734118	47.027380
3503.210837	465659.500581	47.032385
3503.403358	465652.168019	47.037389
3503.343924	465653.394480	47.042394
3503.218673	465643.018861	47.047399
3503.316665	465626.472093	47.052404
3503.185160	465621.776924	47.057409
3503.367347	465623.776549	47.062413
3503.407601	465622.603904	47.067418
3503.397495	465615.506195	47.072423
3503.610539	465609.336695	47.077428
3503.407450	465609.368833	47.082433
3503.410805	465578.080481	47.087437
3503.358563	465570.938707	47.092442
3503.368246	465576.870250	47.097447
3503.621280	465564.507833	47.102452
3503.464468	465575.384535	47.107457
3503.566247	465538.553209	47.112461
3503.732627	465522.756198	47.117466
3503.532347	465531.814239	47.122471
3503.650128	465528.296683	47.127476
3503.167132	465509.661133	47.132481
3503.548579	465482.369667	47.137485
3503.286950	465473.688948	47.142490
3503.556907	465480.593578	47.147495
3503.332291	465468.965832	47.152500
3503.370161	465476.464956	47.157505
3503.225173	465452.349965	47.162509
3503.491265	465440.441802	47.167514
3503.603369	465436.671578	47.172519
3503.525083	465435.466949	47.177524
3503.438120	465441.718066	47.182529
3503.538744	465418.020605	47.187533
3503.396349	465402.627280	47.192538
3503.383617	465386.858478	47.197543
3503.355864	465387.522134	47.202548
3503.317795	465396.858855	47.207553
3503.643201	465365.924968	47.212557
3503.637746	465353.045472	47.217562
3503.477824	465343.334420	47.222567
3503.526053	465335.771005	47.227572
3503.470210	465337.250467	47.232577
3503.702292	465307.294740	47.237581
3503.700020	465299.080060	47.242586
3503.384090	465296.138122	47.247591
3503.565796	465283.685395	47.252596
3503.258049	465293.014076	47.257601
3503.566703	465262.792632	47.262605
3503.412285	465258.658819	47.267610
3503.314261	465244.982522	47.272615
3503.619456	465251.628105	47.277620
3503.529251	465246.977036	47.282625
3503.440428	465221.889407	47.287629
3503.273777	465211.621542	47.292634
3503.097860	465211.598675	47.297639
3503.451085	465194.808386	47.302644
3503.338423	465198.883080	47.307649
3503.224464	465198.596866	47.312653
3503.167310	465193.839141	47.317658
3503.112402	465195.166333	47.322663
3503.231743	465174.102594	47.327668
3503.385145	465159.625841	47.332673
3503.049112	465166.271382	47.337677
3503.363739	465151.667720	47.342682
3503.309885	465162.781913	47.347687
3503.607562	465147.927374	47.352692
3503.385086	465158.358272	47.357697
3503.144132	465149.978417	47.362701
3503.288747	465125.411595	47.367706
3503.155331	465114.124214	47.372711
3503.287429	465107.257413	47.377716
3503.076363	465114.948144	47.382721
3503.275893	465110.910490	47.387725
3503.318395	465114.554988	47.392730
3503.129508	465109.513800	47.397735
3503.502378	465112.294707	47.402740
3503.011823	465102.585094	47.407745
3503.323809	465089.452421	47.412749
3503.145653	465078.273514	47.417754
3503.134170	465065.039821	47.422759
3503.356227	465073.676326	47.427764
3503.137225	465071.885386	47.432769
3503.459411	465073.660092	47.437773
3503.585424	465070.952534	47.442778
3502.941547	465069.634437	47.447783
3503.263150	465070.395017	47.452788
3503.529964	465043.476084	47.457793
3503.017482	465033.465639	47.462797
3503.112421	465038.623191	47.467802
3503.059785	465027.018730	47.472807
3503.386518	465025.699349	47.477812
3502.684536	465028.295182	47.482817
3503.332401	465025.555845	47.487821
3503.402642	465017.532439	47.492826
3503.231284	465029.578073	47.497831
3503.759255	465017.476148	47.502836
3503.533452	465007.014689	47.507841
3503.427710	464994.911494	47.512845
3503.377090	464975.192910	47.517850
3503.240779	464979.677073	47.522855
3503.701956	464962.514561	47.527860
3503.213645	464948.139094	47.532865
3503.568975	464930.689020	47.537869
3503.391291	464928.283003	47.542874
3503.180238	464927.099330	47.547879
3503.367741	464924.838436	47.552884
3503.309286	464930.273816	47.557889
3503.443974	464910.627306	47.562893
3503.516563	464895.250344	47.567898
3503.046573	464892.332700	47.572903
3503.629386	464881.895504	47.577908
3503.150173	464893.584183	47.582913
3503.292943	464874.342052	47.587917
3503.370105	464884.928569	47.592922
3503.190281	464860.463433	47.597927
3503.351595	464859.930860	47.602932
3503.127390	464853.373851	47.607937
3502.950297	464834.892202	47.612941
3503.112490	464838.720675	47.617946
3503.151911	464836.280331	47.622951
3503.708257	464823.565274	47.627956
3503.370172	464839.643576	47.632961
3503.383579	464821.588208	47.637965
3503.397066	464806.575505	47.642970
3503.387075	464789.183058	47.647975
3503.408819	464804.038146	47.652980
3503.218821	464805.741695	47.657985
3503.459711	464782.680607	47.662989
3503.373695	464791.923748	47.667994
3503.090060	464769.148398	47.672999
3503.584349	464743.562346	47.678004
3503.261311	464748.228206	47.683009
3503.346968	464738.985178	47.688013
3503.715272	464746.787313	47.693018
3503.330552	464744.971827	47.698023
3503.476714	464713.000379	47.703028
3503.496413	464709.447479	47.708033
3503.321909	464702.223315	47.713037
3503.412032	464712.148616	47.718042
3503.383843	464702.720719	47.723047
3503.460748	464694.087597	47.728052
3503.211493	464675.515792	47.733057
3503.158656	464653.464516	47.738061
3503.564546	464653.653958	47.743066
3503.184844	464646.766480	47.748071
3503.478307	464658.536006	47.753076
3503.156255	464651.588706	47.758081
3503.137251	464654.178054	47.763085
3503.127500	464655.396718	47.768090
3503.236237	464646.606409	47.773095
3503.328113	464620.982392	47.778100
3503.206373	464609.084354	47.783105
3503.189654	464601.885928	47.788109
3503.387502	464605.455247	47.793114
3503.451205	464614.928361	47.798119
3503.565871	464605.376418	47.803124
3503.576508	464609.228887	47.808129
3503.322926	464568.750075	47.813133
3503.304988	464561.501117	47.818138
3503.053422	464570.466248	47.823143
3503.273699	464562.824653	47.828148
3503.210042	464562.226206	47.833153
3503.010271	464566.720486	47.838157
3503.398668	464548.504192	47.843162
3503.326615	464556.832409	47.848167
3503.523554	464530.785980	47.853172
3503.414328	464526.492745	47.858177
3503.556440	464523.427588	47.863181
3503.496258	464510.606946	47.868186
3503.450378	464516.598278	47.873191
3503.554014	464489.603015	47.878196
3503.565989	464480.675795	47.883201
3503.532112	464466.583160	47.888205
3503.504489	464481.598413	47.893210
3503.467366	464460.406563	47.898215
3503.437256	464427.955425	47.903220
3503.494541	464440.827363	47.908225
3503.330063	464429.798091	47.913229
3503.526335	464426.267948	47.918234
3503.120378	464433.229042	47.923239
3503.795451	464405.078389	47.928244
3503.358493	464391.962241	47.933249
3503.471852	464385.656008	47.938253
3503.668510	464368.889818	47.943258
3503.516437	464371.956647	47.948263
3503.589103	464350.138784	47.953268
3503.520408	464345.788393	47.958273
3503.552995	464334.727924	47.963277
3503.784777	464327.997255	47.968282
3503.307662	464309.309008	47.973287
3503.413310	464299.504790	47.978292
3503.220118	464293.399122	47.983297
3503.177818	464295.231504	47.988301
3503.521043	464298.017206	47.993306
3503.293645	464294.401868	47.998311
3503.323205	464274.010697	48.003316
3502.951214	464259.869943	48.008321
3503.230235	464244.814874	48.013325
3503.351984	464245.404223	48.018330
3502.865385	464249.943904	48.023335
3503.426505	464237.582736	48.028340
3503.206043	464241.167522	48.033345
3503.243654	464242.733714	48.038349
3503.309450	464248.403193	48.043354
3503.221393	464248.721426	48.048359
3503.234799	464231.933381	48.053364
3503.166632	464221.091630	48.058369
3503.228736	464203.890163	48.063373
3503.387986	464198.895158	48.068378
3503.327001	464210.061687	48.073383
3503.365048	464198.949572	48.078388
3503.094687	464202.237973	48.083393
3503.184193	464199.181085	48.088397
3503.300206	464193.280079	48.093402
3503.319838	464189.828530	48.098407
3503.399592	464163.597325	48.103412
3502.940709	464160.931388	48.108417
3503.069133	464153.304165	48.113421
3503.335076	464151.740775	48.118426
3503.032498	464144.384526	48.123431
3503.219330	464155.156922	48.128436
3503.298590	464146.117501	48.133441
3503.392133	464157.817478	48.138445
3503.649820	464149.155560	48.143450
3503.408286	464138.493309	48.148455
3503.377745	464116.184389	48.153460
3503.186105	464121.641026	48.158465
3503.218940	464112.101797	48.163469
3503.616088	464105.294207	48.168474
3503.349235	464107.060672	48.173479
3503.421366	464074.034993	48.178484
3503.315906	464075.420958	48.183489
3503.348711	464063.396761	48.188493
3503.465258	464057.952054	48.193498
3503.313692	464068.473701	48.198503
3503.391832	464060.499400	48.203508
3503.321057	464040.326719	48.208513
3503.625749	464023.695324	48.213517
3503.519297	464006.976761	48.218522
3503.284916	464015.837980	48.223527
3503.407215	464005.473149	48.228532
3503.606224	464014.874428	48.233537
3503.566059	463995.761849	48.238541
3503.477627	463966.919886	48.243546
3503.217164	463973.553850	48.248551
3503.394432	463957.703247	48.253556
3503.353860	463976.524416	48.258561
3503.318904	463958.374536	48.263565
3503.436217	463931.528547	48.268570
3503.245814	463925.625187	48.273575
3503.066964	463921.190694	48.278580
3503.330787	463930.429625	48.283585
3503.031532	463923.732051	48.288589
3503.000577	463921.657723	48.293594
3503.189938	463915.947902	48.298599
3503.126033	463913.828067	48.303604
3503.300689	463913.952639	48.308609
3503.294581	463925.465639	48.313613
3503.566526	463896.465192	48.318618
3503.057601	463888.025769	48.323623
3503.423219	463880.918809	48.328628
3503.415204	463883.303659	48.333633
3502.916010	463878.463367	48.338637
3503.285060	463865.523779	48.343642
3503.270369	463876.125314	48.348647
3503.641324	463862.830427	48.353652
3503.408656	463842.531007	48.358657
3503.641274	463834.532206	48.363661
3503.315115	463827.483857	48.368666
3503.151435	463831.059736	48.373671
3503.009064	463823.221629	48.378676
3502.786654	463824.068243	48.383681
3503.342438	463827.378261	48.388685
3503.190836	463828.467252	48.393690
3502.996101	463815.211035	48.398695
3503.094691	463801.553450	48.403700
3502.840825	463796.927933	48.408705
3503.105317	463793.133333	48.413709
3502.960969	463789.555497	48.418714
3503.021344	463790.154559	48.423719
3503.256738	463791.233097	48.428724
3503.251444	463793.921810	48.433729
3503.004512	463787.013067	48.438733
3503.408898	463774.929977	48.443738
3502.914923	463776.732368	48.448743
3503.331653	463773.775840	48.453748
3503.406616	463780.103276	48.458753
3503.532868	463785.256183	48.463757
3503.638788	463760.491053	48.468762
3503.401067	463746.582306	48.473767
3503.484447	463730.036378	48.478772
3503.301170	463738.636063	48.483777
3503.321403	463735.539345	48.488781
3503.207428	463735.912396	48.493786
3502.791924	463728.878137	48.498791
3503.136632	463721.825144	48.503796
3503.198664	463708.528276	48.508801
3502.979786	463703.390067	48.513805
3502.926919	463690.872062	48.518810
3503.007899	463693.141437	48.523815
3503.029512	463682.893793	48.528820
3502.998629	463688.933701	48.533825
3502.987378	463688.631232	48.538829
3503.123097	463683.234113	48.543834
3502.908230	463698.583796	48.548839
3502.995061	463686.297278	48.553844
3503.384974	463680.961409	48.558849
3503.065182	463683.243418	48.563853
3503.014583	463684.367166	48.568858
3502.881574	463681.953945	48.573863
3503.016645	463685.127628	48.578868
3502.782060	463686.077600	48.583873
3502.991236	463685.131720	48.588877
3503.089171	463685.116278	48.593882
3502.913364	463690.621236	48.598887
3503.008079	463665.756339	48.603892
3502.833430	463678.361110	48.608897
3503.016436	463678.484364	48.613901
3503.187087	463665.068873	48.618906
3503.009317	463676.710567	48.623911
3503.308836	463668.548987	48.628916
3503.300721	463681.837432	48.633921
3503.133629	463677.299602	48.638925
3503.511629	463676.732751	48.643930
3503.145076	463667.002880	48.648935
3503.149902	463648.035022	48.653940
3503.513930	463642.703235	48.658945
3503.145480	463640.276509	48.663949
3503.350192	463632.180615	48.668954
3503.385615	463633.899340	48.673959
3503.348547	463632.231664	48.678964
3503.297310	463635.586945	48.683969
3503.341736	463614.178511	48.688973
3503.573577	463600.398307	48.693978
3503.336694	463607.992230	48.698983
3503.337309	463601.095014	48.703988
3503.389567	463602.608223	48.708993
3503.411086	463599.460567	48.713997
3503.587525	463579.806236	48.719002
3503.238421	463572.102142	48.724007
3503.581184	463547.755761	48.729012
3503.285018	463564.842683	48.734017
3503.204739	463556.538233	48.739021
3503.563740	463551.866507	48.744026
3503.094603	463538.805635	48.749031
3503.218312	463523.774609	48.754036
3503.151603	463520.843745	48.759041
3503.022448	463520.813483	48.764045
3503.463278	463517.396680	48.769050
3503.172812	463507.502567	48.774055
3503.207637	463507.598529	48.779060
3503.191816	463502.833893	48.784065
3502.860721	463514.652054	48.789069
3503.443882	463503.047700	48.794074
3503.235849	463516.266418	48.799079
3503.110302	463481.039628	48.804084
3503.170432	463466.830047	48.809089
3503.304616	463471.981775	48.814093
3503.310290	463454.890056	48.819098
3503.033020	463477.501966	48.824103
3503.377090	463461.928920	48.829108
3503.334721	463465.130682	48.834113
3502.868465	463469.210878	48.839117
3503.362230	463446.311242	48.844122
3503.365216	463451.635857	48.849127
3503.142746	463435.493048	48.854132
3503.581979	463428.171444	48.859137
3503.032125	463429.881266	48.864141
3503.551638	463420.467664	48.869146
3503.230870	463416.004783	48.874151
3503.419960	463423.987875	48.879156
3503.477077	463414.343068	48.884161
3503.117020	463405.524919	48.889165
3503.515264	463368.592278	48.894170
3503.364731	463369.326118	48.899175
3503.161004	463372.857688	48.904180
3502.930174	463375.074952	48.909185
3502.735162	463369.831461	48.914189
3503.213440	463372.291648	48.919194
3503.019225	463369.634492	48.924199
3503.032093	463366.944604	48.929204
3503.270891	463369.189069	48.934209
3502.951018	463369.696101	48.939213
3503.385430	463357.658746	48.944218
3503.214057	463369.096736	48.949223
3503.348038	463353.049669	48.954228
3503.407062	463329.762189	48.959233
3502.912233	463333.491922	48.964237
3503.160402	463322.802576	48.969242
3502.967981	463326.281651	48.974247
3503.114309	463328.845027	48.979252
3503.099170	463326.210275	48.984257
3502.863267	463338.013487	48.989261
3503.058475	463319.015245	48.994266
3503.354075	463318.055689	48.999271
3503.092029	463322.661501	49.004276
3503.543682	463318.025795	49.009281
3503.286064	463309.597135	49.014285
3503.123474	463288.119666	49.019290
3503.277812	463294.992566	49.024295
3503.296039	463281.651643	49.029300
3503.300750	463283.730257	49.034305
3503.340686	463294.424875	49.039309
3503.577761	463275.876414	49.044314
3503.244593	463277.551998	49.049319
3503.446611	463272.905025	49.054324
3503.250343	463246.158459	49.059329
3503.247895	463244.535996	49.064333
3503.379209	463236.958707	49.069338
3502.953355	463249.400573	49.074343
3503.429860	463231.777820	49.079348
3503.754396	463235.682351	49.084353
3503.077196	463230.464325	49.089357
3503.588174	463199.193684	49.094362
3503.556180	463199.959509	49.099367
3503.534007	463199.760190	49.104372
3503.969827	463196.344129	49.109377
3503.549637	463161.619825	49.114381
3503.496274	463156.810330	49.119386
3503.384073	463154.495192	49.124391
3503.454432	463145.659619	49.129396
3503.789635	463140.991566	49.134401
3503.390501	463119.906326	49.139405
3503.788503	463111.171098	49.144410
3503.172930	463103.661100	49.149415
3503.626172	463097.250051	49.154420
3503.324583	463077.011515	49.159425
3503.365642	463073.353537	49.164429
3503.607614	463053.079779	49.169434
3503.299603	463061.547303	49.174439
3503.512037	463060.093725	49.179444
3503.387906	463039.167801	49.184449
3503.356622	463033.796916	49.189453
3503.549324	463016.066698	49.194458
3503.487021	463015.315846	49.199463
3503.555330	463003.894034	49.204468
3503.365171	463002.047644	49.209473
3503.425285	462987.229159	49.214477
3503.514917	462978.289040	49.219482
3503.324813	462973.196822	49.224487
3503.109805	462971.050062	49.229492
3503.335400	462968.630795	49.234497
3503.104260	462966.892311	49.239501
3503.435250	462975.563163	49.244506
3503.040613	462952.093401	49.249511
3502.978765	462925.984498	49.254516
3503.081895	462925.055347	49.259521
3503.476597	462921.950038	49.264525
3503.631039	462915.383300	49.269530
3503.322230	462921.264489	49.274535
3503.287672	462917.060560	49.279540
3503.286366	462911.177747	49.284545
3503.160194	462914.849280	49.289549
3503.422581	462888.942663	49.294554
3503.170620	462883.961634	49.299559
3503.220258	462872.999149	49.304564
3503.371687	462892.500945	49.309569
3503.083708	462884.533361	49.314573
3503.348816	462881.702111	49.319578
3503.082717	462894.981104	49.324583
3503.019548	462880.993489	49.329588
3503.497268	462888.728295	49.334593
3503.239748	462859.911571	49.339597
3503.211595	462849.164234	49.344602
3503.011103	462833.879674	49.349607
3503.198565	462835.472999	49.354612
3503.200192	462834.002010	49.359617
3502.907925	462845.814400	49.364621
3503.114571	462827.828241	49.369626
3502.809496	462839.439794	49.374631
3503.229581	462837.091204	49.379636
3503.424307	462827.677965	49.384641
3503.099999	462846.291390	49.389645
3503.500026	462833.853449	49.394650
3503.318596	462835.860096	49.399655
3503.353481	462818.154659	49.404660
3503.113912	462790.602911	49.409665
3502.719071	462792.744726	49.414669
3503.253728	462783.784901	49.419674
3502.923620	462794.741122	49.424679
3503.136939	462781.825499	49.429684
3503.245617	462789.567956	49.434689
3503.450267	462777.769460	49.439693
3503.633834	462782.102087	49.444698
3503.553958	462783.940538	49.449703
3503.362150	462746.643649	49.454708
3503.579779	462744.276333	49.459713
3503.588452	462743.514253	49.464717
3503.260456	462748.739208	49.469722
3503.203614	462737.184887	49.474727
3503.228891	462722.016711	49.479732
3503.063224	462703.937148	49.484737
3502.693131	462695.779607	49.489741
3503.248929	462699.698401	49.494746
3502.670096	462694.718277	49.499751
3502.856702	462687.487070	49.504756
3502.892844	462699.501214	49.509761
3502.863960	462698.085755	49.514765
3503.375406	462710.379781	49.519770
3503.100057	462699.722157	49.524775
3503.124399	462684.706253	49.529780
3503.517948	462693.468764	49.534785
3503.284029	462695.940169	49.539789
3503.402816	462688.364667	49.544794
3503.261344	462694.980216	49.549799
3503.282201	462687.775208	49.554804
3503.302920	462683.308914	49.559809
3502.940657	462665.818276	49.564813
3503.481889	462650.061331	49.569818
3503.352561	462654.088425	49.574823
3502.922993	462649.388997	49.579828
3503.437747	462649.713405	49.584833
3503.213214	462651.879031	49.589837
3503.425027	462651.997739	49.594842
3503.130048	462646.414855	49.599847
3503.525654	462641.940014	49.604852
3503.465008	462616.540579	49.609857
3503.103486	462616.902059	49.614861
3503.262233	462589.895697	49.619866
3503.204903	462602.482553	49.624871
3503.524760	462607.148691	49.629876
3503.419729	462600.927170	49.634881
3503.441994	462579.571926	49.639885
3503.631188	462562.095473	49.644890
3503.184948	462561.151707	49.649895
3503.085824	462558.631570	49.654900
3503.649381	462555.854538	49.659905
3503.296263	462552.968812	49.664909
3503.308601	462536.534629	49.669914
3503.471662	462528.292754	49.674919
3503.145322	462510.136990	49.679924
3503.510818	462505.108994	49.684929
3503.145805	462517.085212	49.689933
3503.371837	462500.718660	49.694938
3502.864462	462508.913610	49.699943
3503.011992	462500.167009	49.704948
3503.451568	462507.502246	49.709953
3503.285215	462500.580351	49.714957
3502.964628	462477.504103	49.719962
3503.190840	462474.780382	49.724967
3502.918430	462464.730782	49.729972
3502.945180	462459.350581	49.734977
3503.211420	462469.350517	49.739981
3503.089012	462458.465732	49.744986
3503.125678	462466.523989	49.749991
3503.024693	462468.720823	49.754996
3503.172044	462467.835380	49.760001
3503.073037	462465.771667	49.765005
3503.416190	462459.174963	49.770010
3503.326596	462460.558523	49.775015
3503.202593	462466.004887	49.780020
3503.372919	462457.508251	49.785025
3503.298019	462437.892606	49.790029
3503.092817	462423.419973	49.795034
3502.932988	462421.163000	49.800039
3503.143835	462418.948873	49.805044
3503.222665	462418.784299	49.810049
3502.850023	462418.285348	49.815053
3503.352696	462422.364741	49.820058
3503.425929	462412.970525	49.825063
3503.051819	462421.651615	49.830068
3503.689288	462420.739419	49.835073
3503.380028	462394.415392	49.840077
3503.363833	462383.260195	49.845082
3503.325836	462377.940925	49.850087
3503.400751	462371.690896	49.855092
3503.609752	462376.070303	49.860097
3503.406282	462364.031785	49.865101
3503.538593	462337.232155	49.870106
3503.650512	462333.106395	49.875111
3503.652965	462325.954893	49.880116
3503.635906	462323.066735	49.885121
3503.419579	462299.517361	49.890125
3503.544099	462288.948482	49.895130
3503.385775	462273.656859	49.900135
3503.212697	462286.414348	49.905140
3503.484604	462270.750415	49.910145
3503.412559	462274.007762	49.915149
3503.362231	462250.685683	49.920154
3503.407652	462244.846020	49.925159
3503.530514	462237.421869	49.930164
3503.137461	462227.999839	49.935169
3503.222778	462244.571049	49.940173
3503.617292	462232.894398	49.945178
3503.022066	462212.904333	49.950183
3502.970006	462208.652315	49.955188
3503.572433	462188.726514	49.960193
3503.397376	462194.992500	49.965197
3503.188632	462192.844670	49.970202
3503.319133	462191.556138	49.975207
3503.229047	462198.112999	49.980212
3503.188488	462186.555809	49.985217
3502.837884	462201.370116	49.990221
3503.200194	462182.192310	49.995226
3503.494466	462186.406124	50.000231
3502.909449	462162.965593	50.005236
3503.429854	462158.521645	50.010241
3503.199748	462157.746569	50.015245
3503.066503	462156.956183	50.020250
3503.069743	462159.998776	50.025255
3502.930251	462159.817991	50.030260
3503.341243	462162.390391	50.035265
3502.860409	462167.690361	50.040269
3503.105301	462147.415292	50.045274
3503.357647	462156.961108	50.050279
3502.833775	462163.586544	50.055284
3503.274076	462154.641374	50.060289
3502.919739	462163.725185	50.065293
3503.032298	462156.099764	50.070298
3502.921053	462162.457108	50.075303
3503.220606	462152.976289	50.080308
3503.193823	462119.912528	50.085313
3503.079047	462120.235014	50.090317
3503.034620	462104.418090	50.095322
3503.055907	462111.109527	50.100327
3503.026410	462106.194590	50.105332
3503.059721	462101.624750	50.110337
3503.058325	462111.058540	50.115341
3503.204635	462103.529201	50.120346
3502.866061	462114.030642	50.125351
3503.246415	462111.789692	50.130356
3503.367145	462112.024236	50.135361
3503.041761	462113.292934	50.140365
3503.255773	462105.651459	50.145370
3503.233283	462116.052221	50.150375
3503.231360	462121.225787	50.155380
3503.475860	462084.467404	50.160385
3503.376264	462085.193236	50.165389
3503.149882	462073.716075	50.170394
3503.218211	462071.118695	50.175399
3503.153612	462075.744280	50.180404
3503.384111	462065.259978	50.185409
3503.086033	462055.518552	50.190413
3503.161255	462066.512510	50.195418
3503.194619	462059.964651	50.200423
3502.870345	462057.023580	50.205428
3503.280383	462049.655410	50.210433
3503.208609	462028.466639	50.215437
3503.314444	462016.480475	50.220442
3503.394776	462016.569251	50.225447
3503.236246	462016.137883	50.230452
3503.365724	462007.546091	50.235457
3503.240788	462011.876918	50.240461
3503.325362	462022.615829	50.245466
3503.410091	461997.699869	50.250471
3502.972402	461997.718370	50.255476
3503.191533	461972.831856	50.260481
3503.334460	461982.445763	50.265485
3503.404722	461971.225969	50.270490
3503.212985	461975.567362	50.275495
3503.136962	461970.304721	50.280500
3503.241811	461969.933158	50.285505
3503.278315	461974.441348	50.290509
3503.504342	461961.878255	50.295514
3503.009438	461939.792631	50.300519
3503.120279	461930.341543	50.305524
3503.305129	461935.891378	50.310529
3503.021839	461931.574418	50.315533
3503.126845	461926.536744	50.320538
3503.023912	461924.727191	50.325543
3503.090648	461915.688814	50.330548
3503.499622	461915.624209	50.335553
3503.114180	461931.357137	50.340557
3503.253805	461915.612420	50.345562
3503.534086	461916.988270	50.350567
3503.457418	461896.256609	50.355572
3503.159068	461889.456818	50.360577
3503.251100	461883.203943	50.365581
3503.106390	461888.400133	50.370586
3502.874817	461875.300698	50.375591
3502.991405	461886.237491	50.380596
3503.312103	461875.079500	50.385601
3502.900780	461877.528319	50.390605
3503.246833	461874.126242	50.395610
3503.293014	461873.459640	50.400615
3502.967238	461881.017501	50.405620
3503.034280	461867.718706	50.410625
3503.047896	461877.809565	50.415629
3503.607229	461862.454936	50.420634
3503.350824	461837.643430	50.425639
3503.139721	461838.437613	50.430644
3503.272847	461824.316850	50.435649
3503.067374	461834.290203	50.440653
3503.263030	461839.280451	50.445658
3503.111354	461824.038178	50.450663
3502.949983	461836.134739	50.455668
3503.173509	461821.036033	50.460673
3503.193813	461826.054000	50.465677
3503.118396	461828.094701	50.470682
3502.952521	461815.390593	50.475687
3502.933622	461826.044520	50.480692
3503.600808	461818.686345	50.485697
3503.376523	461800.868884	50.490701
3503.309819	461795.401853	50.495706
3503.585811	461784.301601	50.500711
3503.172407	461792.431248	50.505716
3503.247987	461787.702504	50.510721
3503.633512	461778.258652	50.515725
3503.387125	461754.713434	50.520730
3503.256722	461741.395052	50.525735
3503.392768	461707.036954	50.530740
3503.516668	461665.782946	50.535745
3503.270441	461636.303458	50.540749
3503.421796	461550.919306	50.545754
3503.188097	461486.644227	50.550759
3502.999145	461407.703940	50.555764
3503.196286	461315.565925	50.560769
3502.577140	461226.193982	50.565773
3502.512505	461115.127217	50.570778
3502.573929	461009.771374	50.575783
3502.326852	460884.175486	50.580788
3502.359925	460743.977643	50.585793
3501.894237	460604.263504	50.590797
3501.613752	460455.287837	50.595802
3501.357099	460295.503574	50.600807
3501.052620	460134.812695	50.605812
3500.684841	459970.732208	50.610817
3500.170085	459788.362613	50.615821
3500.110692	459599.781950	50.620826
3500.117011	459422.957287	50.625831
3499.380110	459229.306664	50.630836
3498.922170	459031.704411	50.635841
3498.580412	458822.516596	50.640845
3498.570089	458604.498802	50.645850
3498.287480	458388.550954	50.650855
3497.832493	458168.772984	50.655860
3497.633192	457929.067205	50.660865
3497.028910	457705.909484	50.665869
3496.662052	457458.869524	50.670874
3496.326662	457219.177576	50.675879
3495.723912	456967.147237	50.680884
3495.363505	456704.016513	50.685889
3495.042171	456454.421676	50.690893
3494.602720	456181.404739	50.695898
3494.197196	455913.908913	50.700903
3493.789327	455643.011163	50.705908
3493.428055	455352.113800	50.710913
3492.618108	455082.642640	50.715917
3492.452737	454799.773875	50.720922
3491.832805	454508.043988	50.725927
3491.414239	454209.733550	50.730932
3491.104207	453908.256343	50.735937
3490.349991	453606.236483	50.740941
3489.888546	453306.500273	50.745946
3489.427466	452993.567977	50.750951
3488.543007	452675.776574	50.755956
3488.050548	452371.821577	50.760961
3487.678293	452054.600178	50.765965
3487.270677	451729.616513	50.770970
3486.718563	451422.461614	50.775975
3486.140280	451086.028060	50.780980
3485.406737	450757.174940	50.785985
3484.922623	450439.339984	50.790989
3484.531444	450092.003039	50.795994
3483.670729	449769.296116	50.800999
3483.047695	449427.973873	50.806004
3482.581535	449095.604099	50.811009
3481.739459	448767.450341	50.816013
3481.323629	448415.118905	50.821018
3481.008387	448070.378694	50.826023
3480.180031	447732.210558	50.831028
3479.980903	447374.703430	50.836033
3479.374488	447031.008995	50.841037
3478.734985	446681.173715	50.846042
3477.780208	446325.901726	50.851047
3477.115710	445969.055891	50.856052
3476.740756	445609.215132	50.861057
3475.963456	445261.410852	50.866061
3475.101606	444903.869632	50.871066
3474.815789	444546.841081	50.876071
3473.961547	444192.333433	50.881076
3473.543303	443831.711337	50.886081
3472.640683	443468.317868	50.891085
3472.133551	443103.587386	50.896090
3471.498568	442737.501054	50.901095
3470.800909	442383.551132	50.906100
3470.308796	442013.471846	50.911105
3469.594223	441652.914810	50.916109
3468.956983	441281.425948	50.921114
3468.702201	440916.622681	50.926119
3467.450467	440546.691952	50.931124
3466.766627	440181.336360	50.936129
3465.989901	439811.928649	50.941133
3465.304531	439438.160303	50.946138
3464.436800	439078.300322	50.951143
3463.723284	438719.375338	50.956148
3463.562114	438356.930861	50.961153
3462.697936	437989.185139	50.966157
3461.929038	437623.145150	50.971162
3461.551721	437258.154877	50.976167
3460.955830	436896.189436	50.981172
3460.216844	436528.478565	50.986177
3459.519883	436162.228127	50.991181
3458.674407	435789.598156	50.996186
3458.260751	435417.732222	51.001191
3457.149092	435055.796458	51.006196
3456.823206	434684.362867	51.011201
3455.906762	434323.198230	51.016205
3455.062908	433956.380537	51.021210
3454.508327	433587.531435	51.026215
3453.720034	433225.696262	51.031220
3452.998110	432861.941200	51.036225
3452.503989	432502.664557	51.041229
3451.904276	432137.102566	51.046234
3451.340473	431773.408703	51.051239
3450.182567	431419.706513	51.056244
3449.805855	431036.192385	51.061249
3449.028326	430687.193844	51.066253
3448.321963	430320.785162	51.071258
3447.676194	429962.462249	51.076263
3446.928292	429599.579709	51.081268
3446.258033	429224.643083	51.086273
3445.217534	428877.744315	51.091277
3444.688315	428505.339991	51.096282
3444.333458	428158.297985	51.101287
3443.302900	427800.793748	51.106292
3442.615462	427437.389421	51.111297
3441.658983	427087.152472	51.116301
3441.130791	426731.560753	51.121306
3440.585072	426372.817873	51.126311
3439.465038	426027.672272	51.131316
3439.025280	425677.817749	51.136321
3437.878106	425323.879884	51.141325
3437.849254	424967.169970	51.146330
3436.882579	424611.594162	51.151335
3436.232423	424276.485881	51.156340
3435.501717	423921.828892	51.161345
3434.781901	423573.439231	51.166349
3433.927839	423219.224406	51.171354
3433.294770	422884.807531	51.176359
3432.426607	422525.429757	51.181364
3431.880036	422187.028255	51.186369
3430.518900	421843.239356	51.191373
3430.226164	421498.261217	51.196378
3429.494395	421171.205565	51.201383
3428.594654	420839.498659	51.206388
3427.992180	420500.501158	51.211393
3427.299594	420171.624010	51.216397
3426.722412	419829.718481	51.221402
3426.019045	419495.068640	51.226407
3425.270629	419154.096470	51.231412
3424.340861	418819.906253	51.236417
3423.691301	418487.192025	51.241421
3422.799417	418164.521524	51.246426
3422.167546	417826.512632	51.251431
3421.463163	417517.472848	51.256436
3421.036089	417184.581163	51.261441
3420.433824	416857.988466	51.266445
3419.392627	416539.743739	51.271450
3419.021893	416206.831781	51.276455
3418.300869	415889.545477	51.281460
3417.600901	415554.899589	51.286465
3416.966297	415233.730598	51.291469
3416.220367	414910.593881	51.296474
3415.577066	414574.174606	51.301479
3414.325166	414263.662018	51.306484
3413.995105	413931.733802	51.311489
3413.183157	413609.431561	51.316493
3412.328438	413285.582611	51.321498
3411.853165	412968.911647	51.326503
3411.186547	412667.868785	51.331508
3410.149808	412346.807891	51.336513
3409.586748	412030.445653	51.341517
3409.161245	411718.022255	51.346522
3408.584240	411388.670865	51.351527
3407.477175	411095.838384	51.356532
3406.888763	410769.251708	51.361537
3406.238297	410463.381318	51.366541
3405.080584	410151.895868	51.371546
3404.835257	409835.104379	51.376551
3404.015809	409526.811665	51.381556
3403.217417	409211.905322	51.386561
3402.653949	408902.549288	51.391565
3401.665029	408600.169609	51.396570
3401.223632	408289.771531	51.401575
3400.272825	407991.598327	51.406580
3400.061785	407684.817171	51.411585
3399.134318	407382.263232	51.416589
3398.393652	407074.746477	51.421594
3397.734972	406761.190528	51.426599
3397.067492	406465.397466	51.431604
3396.270471	406166.826444	51.436609
3395.542819	405858.583911	51.441613
3394.710230	405558.945237	51.446618
3394.462671	405260.761518	51.451623
3393.363525	404961.845466	51.456628
3392.603542	404665.338271	51.461633
3392.034386	404368.493107	51.466637
3390.962908	404071.927894	51.471642
3390.307462	403783.249504	51.476647
3389.475551	403487.072994	51.481652
3388.982681	403199.786912	51.486657
3388.792189	402918.169309	51.491661
3388.034971	402627.005580	51.496666
3387.724939	402324.940518	51.501671
3386.533593	402038.821943	51.506676
3385.959812	401735.140842	51.511681
3385.229278	401432.015440	51.516685
3384.160119	401150.368690	51.521690
3383.775210	400860.045111	51.526695
3383.179874	400567.566149	51.531700
3382.591183	400270.711361	51.536705
3381.251657	399981.725562	51.541709
3380.611929	399694.609292	51.546714
3380.219433	399410.120508	51.551719
3379.584639	399131.336283	51.556724
3379.152420	398840.697125	51.561729
3378.486079	398551.592237	51.566733
3377.676845	398266.701860	51.571738
3377.365555	397971.663507	51.576743
3376.165740	397699.184680	51.581748
3375.626688	397403.007891	51.586753
3374.807684	397119.685329	51.591757
3373.803831	396834.025336	51.596762
3373.752887	396550.805293	51.601767
3372.521206	396270.438913	51.606772
3371.575640	395978.000019	51.611777
3371.106578	395705.338521	51.616781
3370.282424	395424.188803	51.621786
3369.721432	395153.723770	51.626791
3368.804979	394885.448360	51.631796
3368.427835	394603.687251	51.636801
3367.643736	394324.428856	51.641805
3366.709816	394070.641416	51.646810
3366.318124	393788.825026	51.651815
3365.330252	393519.507760	51.656820
3364.946157	393246.406323	51.661825
3364.241824	392975.844999	51.666829
3363.476912	392709.893080	51.671834
3362.894794	392430.434787	51.676839
3361.968975	392161.910716	51.681844
3361.412133	391892.182066	51.686849
3360.940582	391626.531412	51.691853
3360.082910	391360.914365	51.696858
3359.508646	391084.749421	51.701863
3358.485120	390816.484707	51.706868
3357.871021	390552.679155	51.711873
3357.249268	390285.313072	51.716877
3356.729164	390030.718710	51.721882
3355.956562	389758.185369	51.726887
3355.089608	389494.691602	51.731892
3354.509906	389224.284993	51.736897
3354.033328	388971.990072	51.741901
3353.123387	388698.478646	51.746906
3352.855864	388428.245497	51.751911
3351.657126	388170.973483	51.756916
3351.459346	387896.148191	51.761921
3350.673015	387644.477774	51.766925
3349.552536	387372.896715	51.771930
3349.442254	387115.851921	51.776935
3348.463102	386861.358489	51.781940
3348.114487	386589.573225	51.786945
3347.443306	386320.761360	51.791949
3346.396554	386060.703927	51.796954
3346.164807	385790.623475	51.801959
3345.245051	385531.457690	51.806964
3344.712897	385276.272225	51.811969
3344.102872	385010.848779	51.816973
3342.944763	384740.169635	51.821978
3342.451756	384468.010067	51.826983
3341.552126	384222.615516	51.831988
3340.805556	383964.504920	51.836993
3340.330939	383704.925371	51.841997
3339.369389	383452.313007	51.847002
3338.974886	383187.580010	51.852007
3337.990064	382928.558980	51.857012
3337.233396	382664.311923	51.862017
3336.381772	382428.358824	51.867021
3335.487803	382179.516666	51.872026
3335.277520	381921.815915	51.877031
3334.291601	381685.981171	51.882036
3333.898949	381424.796167	51.887041
3333.293145	381182.133017	51.892045
3332.311478	380936.094269	51.897050
3331.791568	380685.835260	51.902055
3331.448017	380438.064670	51.907060
3331.017306	380182.142011	51.912065
3329.948074	379938.069149	51.917069
3329.360284	379682.676712	51.922074
3328.666598	379429.206921	51.927079
3327.621720	379193.111912	51.932084
3327.136000	378934.035863	51.937089
3326.525970	378693.418005	51.942093
3325.468906	378442.975163	51.947098
3325.213453	378191.233941	51.952103
3324.489788	377959.862525	51.957108
3323.533635	377701.183416	51.962113
3323.294190	377462.457976	51.967117
3322.423504	377227.137578	51.972122
3321.837963	376973.456837	51.977127
3321.063932	376731.911867	51.982132
3320.384292	376485.034339	51.987137
3319.866880	376235.509689	51.992141
3318.671780	375999.165047	51.997146
3318.210213	375751.561744	52.002151
3317.698574	375515.411424	52.007156
3316.830918	375274.304942	52.012161
3316.096299	375028.673615	52.017165
3315.238546	374798.475280	52.022170
3314.980475	374550.120226	52.027175
3313.722083	374322.602627	52.032180
3313.141842	374086.861880	52.037185
3312.814041	373848.179940	52.042189
3312.086649	373615.639500	52.047194
3311.353764	373378.799569	52.052199
3311.033310	373139.730801	52.057204
3309.891398	372897.458130	52.062209
3309.568788	372675.557993	52.067213
3308.599560	372433.102679	52.072218
3307.996225	372191.351259	52.077223
3307.378230	371962.345721	52.082228
3306.674325	371722.693507	52.087233
3305.836943	371483.213674	52.092237
3305.160374	371265.305152	52.097242
3304.676370	371027.802007	52.102247
3304.009643	370793.099363	52.107252
3303.322291	370556.185415	52.112257
3302.694890	370324.424993	52.117261
3301.808966	370094.764853	52.122266
3301.224118	369853.480531	52.127271
3300.198363	369634.270560	52.132276
3299.659565	369405.315045	52.137281
3298.999255	369175.461667	52.142285
3298.522172	368952.777846	52.147290
3297.787371	368714.563770	52.152295
3297.067405	368492.399378	52.157300
3296.232134	368254.885586	52.162305
3295.707352	368025.564401	52.167309
3294.941944	367812.918810	52.172314
3294.434706	367570.286567	52.177319
3293.714366	367348.090986	52.182324
3293.330025	367128.258125	52.187329
3292.533790	366902.993840	52.192333
3291.634437	366670.442822	52.197338
3291.203268	366435.704832	52.202343
3290.281776	366212.721221	52.207348
3289.451012	365979.824998	52.212353
3289.248020	365749.169004	52.217357
3288.480057	365527.836916	52.222362
3287.894952	365304.108628	52.227367
3287.138521	365089.311394	52.232372
3286.468952	364849.615977	52.237377
3286.128237	364620.553473	52.242381
3285.180514	364392.552670	52.247386
3284.667348	364161.505099	52.252391
3283.792808	363935.653142	52.257396
3283.060620	363699.320146	52.262401
3282.406401	363476.815111	52.267405
3281.478847	363266.285499	52.272410
3281.202461	363035.118480	52.277415
3280.265294	362815.810090	52.282420
3279.238320	362589.899315	52.287425
3278.759232	362368.506253	52.292429
3278.107167	362144.671364	52.297434
3277.580067	361922.164213	52.302439
3276.953616	361708.144877	52.307444
3276.174859	361478.678075	52.312449
3275.859356	361261.350561	52.317453
3274.952856	361032.894156	52.322458
3274.075675	360816.213230	52.327463
3273.295554	360597.683887	52.332468
3272.531718	360370.270441	52.337473
3271.871921	360155.053415	52.342477
3271.161006	359943.431373	52.347482
3270.955342	359734.578432	52.352487
3269.947377	359522.925182	52.357492
3269.772551	359301.444228	52.362497
3269.143489	359083.876497	52.367501
3267.789120	358862.401974	52.372506
3267.473424	358637.835804	52.377511
3266.772699	358415.237999	52.382516
3266.140897	358206.267748	52.387521
3265.727356	357981.612251	52.392525
3264.782902	357765.335422	52.397530
3264.196478	357537.498919	52.402535
3263.082510	357329.364619	52.407540
3262.566571	357113.424311	52.412545
3262.232265	356898.777603	52.417549
3261.170663	356685.186565	52.422554
3260.702357	356468.421603	52.427559
3259.896222	356264.203992	52.432564
3259.150931	356046.081385	52.437569
3258.669876	355841.072647	52.442573
3257.858397	355632.349021	52.447578
3257.172075	355406.961618	52.452583
3256.516745	355203.428406	52.457588
3255.934470	354989.576219	52.462593
3255.324492	354777.305324	52.467597
3254.433746	354565.001611	52.472602
3253.704452	354352.366096	52.477607
3253.323560	354140.183570	52.482612
3252.288297	353932.888073	52.487617
3251.665599	353722.879787	52.492621
3251.343188	353518.676454	52.497626
3250.668611	353293.863236	52.502631
3249.753702	353095.503488	52.507636
3249.026789	352883.726842	52.512641
3248.567392	352678.167613	52.517645
3247.604004	352476.911939	52.522650
3247.003475	352256.078145	52.527655
3246.406140	352056.289948	52.532660
3245.654268	351841.968072	52.537665
3245.288608	351633.895852	52.542669
3244.484645	351430.345924	52.547674
3244.155398	351229.596007	52.552679
3243.320504	351015.487539	52.557684
3242.740358	350796.629588	52.562689
3241.893085	350587.407856	52.567693
3240.852486	350376.994262	52.572698
3240.297714	350171.465896	52.577703
3239.430669	349964.459096	52.582708
3238.661336	349769.092579	52.587713
3238.178302	349565.968415	52.592717
3237.654706	349366.871189	52.597722
3236.778418	349160.015507	52.602727
3235.888146	348961.102067	52.607732
3235.296612	348764.609439	52.612737
3235.006382	348566.643168	52.617741
3234.096625	348365.719999	52.622746
3233.533199	348153.160808	52.627751
3232.841518	347947.493073	52.632756
3231.924078	347753.186369	52.637761
3231.331195	347558.140450	52.642765
3230.457354	347361.534819	52.647770
3230.249104	347158.027498	52.652775
3229.417587	346975.565207	52.657780
3228.598440	346774.367482	52.662785
3228.202826	346567.604331	52.667789
3227.533833	346373.049961	52.672794
3226.925755	346170.773164	52.677799
3226.368347	345981.341229	52.682804
3225.576068	345771.023668	52.687809
3224.911494	345572.953406	52.692813
3223.965611	345379.559395	52.697818
3223.736791	345169.379589	52.702823
3222.801081	344970.052052	52.707828
3222.052354	344771.406943	52.712833
3221.836746	344562.673690	52.717837
3220.844215	344382.570357	52.722842
3220.205867	344171.942678	52.727847
3219.731872	343976.713088	52.732852
3218.869460	343779.966173	52.737857
3218.175057	343579.195796	52.742861
3217.525296	343383.992059	52.747866
3217.071090	343173.942595	52.752871
3216.071457	342981.312820	52.757876
3215.304353	342791.649219	52.762881
3215.046457	342587.701070	52.767885
3213.961289	342392.181169	52.772890
3213.435903	342198.506610	52.777895
3212.962740	342000.801381	52.782900
3212.188736	341803.957642	52.787905
3211.609432	341609.958831	52.792909
3210.579305	341412.492530	52.797914
3210.354170	341204.360006	52.802919
3209.751872	341009.879297	52.807924
3208.656863	340811.046773	52.812929
3208.370885	340616.234783	52.817933
3207.317451	340421.314493	52.822938
3206.854154	340225.740226	52.827943
3205.892240	340029.098742	52.832948
3205.710117	339833.427859	52.837953
3204.928500	339634.312912	52.842957
3204.045308	339451.555782	52.847962
3203.326845	339252.047808	52.852967
3202.943252	339056.253656	52.857972
3201.953210	338866.944208	52.862977
3201.544597	338663.006999	52.867981
3200.702839	338469.880013	52.872986
3199.923362	338264.421946	52.877991
3198.890641	338088.710394	52.882996
3198.378581	337898.304237	52.888001
3197.981719	337704.977301	52.893005
3196.979861	337521.647953	52.898010
3196.166893	337334.164295	52.903015
3195.662545	337152.282580	52.908020
3194.831926	336968.211814	52.913025
3194.673600	336782.583159	52.918029
3193.722406	336588.780580	52.923034
3193.179705	336404.459041	52.928039
3192.542436	336220.839281	52.933044
3191.741097	336030.295278	52.938049
3191.420950	335841.278386	52.943053
3190.504718	335658.897685	52.948058
3189.668428	335471.488819	52.953063
3189.259144	335284.419193	52.958068
3188.567508	335098.666573	52.963073
3187.872728	334904.436702	52.968077
3187.103993	334721.953768	52.973082
3186.333280	334536.797641	52.978087
3185.431897	334354.691114	52.983092
3184.911038	334168.883489	52.988097
3184.624404	333984.642133	52.993101
3183.634481	333797.914873	52.998106
3183.239889	333618.271986	53.003111
3182.461914	333432.172112	53.008116
3181.640620	333254.937904	53.013121
3181.046546	333062.748998	53.018125
3180.405357	332887.700203	53.023130
3180.176646	332693.314020	53.028135
3179.051402	332508.539537	53.033140
3178.323905	332326.120168	53.038145
3177.995553	332130.678966	53.043149
3177.274729	331962.132322	53.048154
3176.602377	331779.448248	53.053159
3176.226677	331584.471296	53.058164
3175.206417	331400.288339	53.063169
3174.589872	331212.553226	53.068173
3173.698234	331029.698279	53.073178
3173.271910	330843.943347	53.078183
3172.361932	330666.182119	53.083188
3171.201722	330492.864415	53.088193
3171.164991	330307.275614	53.093197
3170.405532	330134.250087	53.098202
3169.801670	329944.371170	53.103207
3168.738254	329770.781868	53.108212
3168.189267	329582.930067	53.113217
3167.689496	329401.256579	53.118221
3167.035941	329227.397497	53.123226
3166.469607	329039.979886	53.128231
3165.964025	328865.230942	53.133236
3165.115330	328676.074949	53.138241
3164.759390	328496.642413	53.143245
3164.050419	328315.941414	53.148250
3163.070891	328123.189497	53.153255
3162.568202	327940.927403	53.158260
3161.583163	327755.915166	53.163265
3161.195992	327573.990364	53.168269
3160.261058	327397.600198	53.173274
3159.716739	327219.773000	53.178279
3159.242311	327043.283715	53.183284
3158.497683	326866.200281	53.188289
3157.776983	326673.683878	53.193293
3157.019843	326504.850666	53.198298
3156.349153	326328.034388	53.203303
3155.825900	326145.440382	53.208308
3155.009793	325956.221699	53.213313
3154.526177	325777.286860	53.218317
3153.612407	325602.340578	53.223322
3153.218728	325417.076531	53.228327
3152.422651	325237.273353	53.233332
3151.654840	325065.739985	53.238337
3150.952053	324890.300495	53.243341
3150.098189	324721.758910	53.248346
3149.792135	324539.356058	53.253351
3149.010808	324358.682949	53.258356
3148.450642	324179.094729	53.263361
3147.667651	324005.371918	53.268365
3146.915839	323831.720194	53.273370
3146.330292	323657.176129	53.278375
3145.605544	323475.957470	53.283380
3144.989998	323301.468335	53.288385
3144.443203	323119.940683	53.293389
3143.559006	322961.482953	53.298394
3143.098155	322777.776769	53.303399
3142.470048	322590.175612	53.308404
3141.683988	322421.796903	53.313409
3141.111257	322244.905461	53.318413
3140.367213	322069.008298	53.323418
3139.785493	321887.458099	53.328423
3139.217794	321719.985550	53.333428
3138.363310	321542.424332	53.338433
3137.861572	321367.098493	53.343437
3137.059800	321194.824259	53.348442
3136.362401	321014.512716	53.353447
3135.820179	320836.213201	53.358452
3135.220261	320653.262934	53.363457
3134.551804	320485.243824	53.368461
3133.751798	320314.113391	53.373466
3133.176309	320132.634990	53.378471
3132.669150	319963.036201	53.383476
3131.668289	319789.135726	53.388481
3131.228455	319595.107423	53.393485
3130.267383	319434.720390	53.398490
3129.484893	319260.427886	53.403495
3128.821905	319086.065220	53.408500
3128.083985	318913.623758	53.413505
3127.719250	318734.477240	53.418509
3126.899320	318578.471386	53.423514
3126.449559	318402.036704	53.428519
3125.838996	318231.508981	53.433524
3124.764181	318058.762775	53.438529
3124.254831	317878.669928	53.443533
3123.664094	317713.434365	53.448538
3122.879358	317546.395896	53.453543
3122.233261	317369.201014	53.458548
3121.093933	317201.556019	53.463553
3120.792020	317023.109289	53.468557
3120.405661	316864.154721	53.473562
3119.587430	316689.888604	53.478567
3119.182452	316521.948001	53.483572
3117.991825	316343.793428	53.488577
3117.589075	316169.333330	53.493581
3116.628199	316014.491461	53.498586
3116.059935	315843.010702	53.503591
3115.425413	315682.387463	53.508596
3114.669588	315515.137250	53.513601
3114.062685	315350.511379	53.518605
3113.431479	315188.664589	53.523610
3112.794061	315022.362432	53.528615
3112.242696	314859.356632	53.533620
3111.290138	314691.346825	53.538625
3111.101673	314508.778031	53.543629
3110.356053	314348.806852	53.548634
3109.612519	314186.314201	53.553639
3109.199837	314013.710812	53.558644
3108.552284	313845.778690	53.563649
3107.729796	313666.109746	53.568653
3107.225629	313504.138362	53.573658
3106.191108	313331.122974	53.578663
3105.486242	313165.566973	53.583668
3104.799032	313001.637610	53.588673
3104.472926	312827.770858	53.593677
3103.760017	312661.807930	53.598682
3103.212052	312489.936465	53.603687
3102.402691	312333.308117	53.608692
3101.328333	312159.558696	53.613697
3100.992272	311985.030106	53.618701
3100.268252	311826.477723	53.623706
3099.694908	311659.039734	53.628711
3099.071732	311488.299029	53.633716
3098.201416	311314.999815	53.638721
3098.078287	311148.228283	53.643725
3096.910270	310979.635627	53.648730
3096.371571	310806.385015	53.653735
3095.726268	310639.568041	53.658740
3094.751426	310484.720333	53.663745
3094.473531	310307.837208	53.668749
3093.387314	310141.445784	53.673754
3092.691220	309983.523016	53.678759
3092.179307	309815.741555	53.683764
3091.443309	309657.137117	53.688769
3090.692124	309490.029669	53.693773
3090.039467	309330.622198	53.698778
3089.801285	309166.718062	53.703783
3089.274120	308999.370757	53.708788
3088.105592	308843.660266	53.713793
3087.840770	308671.585466	53.718797
3087.077088	308502.645148	53.723802
3086.543339	308338.990376	53.728807
3085.853406	308169.273979	53.733812
3084.863458	308002.762480	53.738817
3084.337001	307848.247829	53.743821
3083.889713	307674.647138	53.748826
3083.269174	307514.544650	53.753831
3082.085849	307342.256830	53.758836
3081.054251	307176.489308	53.763841
3080.925395	307017.810826	53.768845
3080.090265	306860.746359	53.773850
3079.689003	306699.385811	53.778855
3079.100871	306534.973333	53.783860
3078.405837	306373.684331	53.788865
3077.843277	306198.902999	53.793869
3077.096065	306039.149760	53.798874
3076.356798	305863.581052	53.803879
3075.885847	305700.040269	53.808884
3074.984820	305539.495873	53.813889
3074.322466	305362.768386	53.818893
3073.502867	305204.935511	53.823898
3072.528861	305047.203283	53.828903
3072.327053	304886.878510	53.833908
3071.331472	304729.072931	53.838913
3070.791069	304564.268481	53.843917
3070.147818	304414.734054	53.848922
3069.611078	304248.171516	53.853927
3068.958537	304095.073015	53.858932
3067.960568	303932.734005	53.863937
3067.258307	303764.847401	53.868941
3067.035941	303609.846759	53.873946
3066.207372	303457.488467	53.878951
3065.673127	303294.107641	53.883956
3065.058722	303138.098963	53.888961
3064.981091	302968.661019	53.893965
3063.900708	302804.551158	53.898970
3063.411655	302636.374839	53.903975
3062.714203	302470.701512	53.908980
3061.433609	302309.322182	53.913985
3061.072731	302142.347389	53.918989
3060.356987	301979.197553	53.923994
3059.311836	301810.930045	53.928999
3058.955362	301668.808980	53.934004
3058.192032	301506.557484	53.939009
3057.638459	301345.418600	53.944013
3056.788080	301199.733596	53.949018
3056.168266	301031.194193	53.954023
3055.637252	300862.360426	53.959028
3054.915710	300720.652795	53.964033
3054.566488	300551.178735	53.969037
3053.880327	300387.385885	53.974042
3052.586123	300237.313617	53.979047
3052.439149	300066.457319	53.984052
3051.439378	299910.837405	53.989057
3051.247645	299757.381448	53.994061
3050.328059	299603.811337	53.999066
3049.225581	299439.344893	54.004071
3048.859138	299277.715921	54.009076
3048.069789	299129.778335	54.014081
3047.513865	298969.757982	54.019085
3046.583644	298810.917246	54.024090
3046.054143	298664.440662	54.029095
3045.550639	298500.005845	54.034100
3044.757224	298351.329697	54.039105
3044.203946	298191.104468	54.044109
3043.515053	298042.258716	54.049114
3042.964924	297884.834050	54.054119
3042.578064	297724.556594	54.059124
3041.366011	297571.820428	54.064129
3040.937896	297408.518672	54.069133
3040.359590	297259.145431	54.074138
3039.290203	297106.437230	54.079143
3038.813452	296946.886386	54.084148
3037.894332	296800.317135	54.089153
3037.705904	296642.528550	54.094157
3036.750684	296498.995341	54.099162
3036.111912	296338.552812	54.104167
3035.647128	296187.989269	54.109172
3034.383200	296037.704886	54.114177
3034.280467	295877.380873	54.119181
3033.826484	295732.519879	54.124186
3033.032553	295583.485048	54.129191
3032.246320	295411.452112	54.134196
3031.757860	295268.429866	54.139201
3031.179020	295111.745978	54.144205
3030.231177	294957.743485	54.149210
3029.786820	294789.501449	54.154215
3029.288089	294634.332546	54.159220
3028.357092	294476.252278	54.164225
3027.807562	294318.035115	54.169229
3027.154258	294158.891969	54.174234
3026.016734	294004.995194	54.179239
3025.476048	293839.696378	54.184244
3024.881487	293694.907134	54.189249
3024.517482	293540.429193	54.194253
3023.654795	293392.957183	54.199258
3022.636627	293230.916893	54.204263
3022.261929	293079.420003	54.209268
3021.571703	292923.337886	54.214273
3020.831593	292769.122677	54.219277
3020.065742	292621.150955	54.224282
3019.586715	292473.999635	54.229287
3019.058330	292317.203872	54.234292
3018.257730	292172.751873	54.239297
3017.623010	292004.435970	54.244301
3017.130541	291863.806072	54.249306
3016.507305	291710.233826	54.254311
3016.000009	291544.189511	54.259316
3015.005743	291399.589429	54.264321
3014.576788	291238.982564	54.269325
3013.929795	291077.951689	54.274330
3013.665483	290922.437547	54.279335
3012.858699	290765.990465	54.284340
3012.067905	290607.376009	54.289345
3011.632114	290431.310870	54.294349
3011.048702	290267.850002	54.299354
3009.875461	290114.745860	54.304359
3009.661893	289945.368693	54.309364
3008.747585	289789.956760	54.314369
3008.235169	289636.136532	54.319373
3007.451343	289475.202744	54.324378
3006.602406	289305.823878	54.329383
3006.107491	289150.701760	54.334388
3005.144757	288994.991440	54.339393
3004.862068	288837.747206	54.344397
3004.275788	288678.055094	54.349402
3003.427364	288526.834235	54.354407
3002.905963	288360.204439	54.359412
3002.053810	288198.898746	54.364417
3001.580957	288029.281349	54.369421
3000.782118	287881.082998	54.374426
2999.918003	287712.724347	54.379431
2999.395813	287544.795379	54.384436
2998.581736	287396.395472	54.389441
2998.253672	287241.780804	54.394445
2997.459707	287082.451836	54.399450
2996.587201	286921.174192	54.404455
2996.240604	286765.670861	54.409460
2995.258872	286612.407298	54.414465
2994.521968	286447.287776	54.419469
2993.805150	286295.841307	54.424474
2993.212419	286144.120454	54.429479
2992.907634	285976.309115	54.434484
2991.836491	285823.747005	54.439489
2991.689712	285657.183914	54.444493
2990.913315	285508.471633	54.449498
2990.212313	285353.253008	54.454503
2989.615729	285191.650779	54.459508
2988.631032	285037.291912	54.464513
2988.287038	284870.326745	54.469517
2987.604782	284710.036756	54.474522
2986.927648	284545.772871	54.479527
2986.276859	284386.954929	54.484532
2985.316486	284232.948469	54.489537
2985.041532	284069.741341	54.494541
2984.111709	283912.928441	54.499546
2983.383289	283750.811701	54.504551
2982.775941	283585.415816	54.509556
2981.846694	283446.022886	54.514561
2981.224126	283289.212078	54.519565
2980.825066	283135.167342	54.524570
2980.199948	282965.851959	54.529575
2979.904773	282806.849851	54.534580
2978.691564	282649.877653	54.539585
2978.348971	282496.587834	54.544589
2977.841175	282335.352568	54.549594
2976.996521	282174.297917	54.554599
2976.762650	282006.830418	54.559604
2975.549015	281851.182410	54.564609
2974.780607	281686.117041	54.569613
2974.106006	281531.988127	54.574618
2973.301920	281376.275171	54.579623
2972.987411	281214.474170	54.584628
2972.369915	281067.059728	54.589633
2971.657316	280900.610033	54.594637
2971.023285	280752.434091	54.599642
2970.240316	280593.101113	54.604647
2969.821980	280424.236176	54.609652
2969.221387	280268.872782	54.614657
2968.535383	280093.020888	54.619661
2967.681622	279945.236123	54.624666
2966.981407	279788.411243	54.629671
2966.337996	279616.067133	54.634676
2965.780670	279461.307976	54.639681
2965.385523	279293.865360	54.644685
2964.664567	279125.659301	54.649690
2963.886963	278970.858528	54.654695
2963.243686	278810.306090	54.659700
2962.613509	278650.693883	54.664705
2962.027248	278479.970499	54.669709
2961.202519	278315.983017	54.674714
2960.258813	278157.184422	54.679719
2959.869460	277984.774356	54.684724
2959.119555	277832.770566	54.689729
2958.569024	277667.771800	54.694733
2958.061950	277513.768472	54.699738
2957.376749	277344.359493	54.704743
2956.778193	277180.972786	54.709748
2956.151875	277019.347777	54.714753
2955.557523	276836.375193	54.719757
2954.751500	276678.751671	54.724762
2953.804378	276511.981857	54.729767
2953.498294	276355.145101	54.734772
2952.659110	276204.963569	54.739777
2951.947393	276034.845573	54.744781
2951.294272	275862.859101	54.749786
2950.546809	275702.832232	54.754791
2950.081328	275534.356151	54.759796
2949.059086	275372.513578	54.764801
2948.862275	275213.239986	54.769805
2948.019026	275050.375807	54.774810
2947.481500	274883.388288	54.779815
2947.034357	274714.858359	54.784820
2945.820701	274545.838530	54.789825
2945.114459	274390.160221	54.794829
2944.612571	274222.097397	54.799834
2944.046575	274060.488228	54.804839
2943.895949	273901.156403	54.809844
2942.942173	273737.673036	54.814849
2942.191594	273558.519921	54.819853
2941.636475	273400.601977	54.824858
2940.805716	273239.671470	54.829863
2940.567322	273067.237366	54.834868
2939.468173	272906.807801	54.839873
2939.351332	272734.711039	54.844877
2938.556595	272570.234778	54.849882
2937.810073	272395.054183	54.854887
2937.264049	272217.091284	54.859892
2936.600726	272056.287186	54.864897
2935.821315	271867.358942	54.869901
2934.717267	271703.084552	54.874906
2933.873034	271531.790724	54.879911
2933.858014	271369.152232	54.884916
2933.155776	271208.150655	54.889921
2931.985702	271041.314507	54.894925
2931.590205	270871.452374	54.899930
2931.046736	270705.408478	54.904935
2930.466956	270533.308895	54.909940
2929.558341	270374.606805	54.914945
2929.144371	270194.967880	54.919949
2928.522915	270037.544744	54.924954
2927.684414	269863.932683	54.929959
2927.056156	269682.825162	54.934964
2925.780759	269509.435154	54.939969
2925.257081	269346.189904	54.944973
2924.752772	269180.674947	54.949978
2923.838355	269007.533531	54.954983
2923.425635	268855.629682	54.959988
2922.408401	268697.250755	54.964993
2922.215357	268540.549635	54.969997
2921.559030	268380.611023	54.975002
2920.567766	268223.832602	54.980007
2920.162961	268064.363618	54.985012
2919.524721	267894.667933	54.990017
2918.716222	267727.953566	54.995021
2918.197883	267566.745384	55.000026
2917.530672	267398.149568	55.005031
2917.081756	267236.905024	55.010036
2915.900019	267074.757818	55.015041
2915.648193	266915.850714	55.020045
2915.047621	266749.562161	55.025050
2914.223228	266587.460411	55.030055
2913.726198	266417.921119	55.035060
2912.553011	266250.424514	55.040065
2912.212063	266093.722047	55.045069
2911.623639	265930.462565	55.050074
2910.909166	265769.948187	55.055079
2910.594064	265603.054547	55.060084
2909.353619	265442.445281	55.065089
2908.835908	265269.649775	55.070093
2908.080687	265112.351073	55.075098
2907.059311	264958.558227	55.080103
2906.911090	264798.209248	55.085108
2906.290109	264644.658748	55.090113
2905.835936	264476.972598	55.095117
2905.314871	264310.545044	55.100122
2904.764553	264141.855539	55.105127
2904.141605	263970.528933	55.110132
2903.205966	263805.236893	55.115137
2902.779224	263631.892878	55.120141
2902.209691	263453.936379	55.125146
2901.246554	263293.818927	55.130151
2900.832487	263120.167538	55.135156
2900.194728	262954.319374	55.140161
2899.464818	262782.679191	55.145165
2899.135551	262598.903873	55.150170
2898.213333	262433.483021	55.155175
2897.757688	262260.526292	55.160180
2897.108648	262089.765044	55.165185
2896.396058	261909.539904	55.170189
2895.548251	261733.385663	55.175194
2894.720657	261564.384785	55.180199
2894.141403	261387.373254	55.185204
2893.398128	261219.046849	55.190209
2892.456948	261041.507065	55.195213
2892.525867	260869.461311	55.200218
2891.468149	260697.288419	55.205223
2890.869832	260520.229493	55.210228
2889.969210	260362.472144	55.215233
2889.396449	260193.915599	55.220237
2888.958808	260007.586777	55.225242
2888.117113	259843.657212	55.230247
2887.457981	259667.499829	55.235252
2886.678753	259503.356839	55.240257
2886.174316	259330.129435	55.245261
2885.388078	259164.663450	55.250266
2885.157457	258990.119538	55.255271
2884.287089	258806.101223	55.260276
2883.539755	258649.059181	55.265281
2882.919989	258463.651659	55.270285
2882.211026	258292.545681	55.275290
2881.380977	258122.375825	55.280295
2880.947856	257949.392753	55.285300
2880.136363	257776.928127	55.290305
2879.374898	257608.606902	55.295309
2878.735877	257445.487235	55.300314
2878.054429	257280.566213	55.305319
2877.646982	257100.805364	55.310324
2876.950772	256933.085514	55.315329
2875.998932	256763.088732	55.320333
2875.603742	256587.426595	55.325338
2874.496827	256429.602544	55.330343
2874.197183	256253.314328	55.335348
2873.565035	256081.713946	55.340353
2872.898951	255917.479113	55.345357
2872.410160	255742.672894	55.350362
2871.540693	255573.173341	55.355367
2871.267948	255396.423159	55.360372
2870.295834	255228.264432	55.365377
2869.653670	255052.362516	55.370381
2869.118952	254879.194189	55.375386
2868.432330	254714.021270	55.380391
2867.578717	254526.209210	55.385396
2867.032062	254366.107834	55.390401
2866.216747	254188.884331	55.395405
2865.682503	254027.609780	55.400410
2864.783680	253861.758092	55.405415
2864.333314	253684.171659	55.410420
2863.542813	253510.917695	55.415425
2863.056760	253346.503647	55.420429
2862.279258	253164.894784	55.425434
2861.809153	252999.612638	55.430439
2861.361897	252821.109714	55.435444
2860.517546	252650.182558	55.440449
2859.814045	252476.049906	55.445453
2859.200606	252297.624739	55.450458
2858.116425	252130.759799	55.455463
2857.814680	251953.329759	55.460468
2856.998084	251786.957573	55.465473
2856.455861	251614.557427	55.470477
2855.985346	251432.315960	55.475482
2855.116645	251271.911717	55.480487
2854.617682	251090.617380	55.485492
2853.443782	250924.455396	55.490497
2853.023549	250745.339087	55.495501
2852.475936	250578.619878	55.500506
2851.646835	250405.451444	55.505511
2851.316944	250228.536969	55.510516
2850.614530	250056.622163	55.515521
2849.639773	249888.952624	55.520525
2849.055100	249710.449198	55.525530
2848.434222	249543.386107	55.530535
2848.048221	249370.326872	55.535540
2847.168471	249200.325566	55.540545
2846.624136	249028.055764	55.545549
2846.185167	248845.277361	55.550554
2844.875564	248674.682564	55.555559
2844.448521	248493.354260	55.560564
2843.893828	248327.988216	55.565569
2843.034256	248165.217241	55.570573
2842.749605	247985.242163	55.575578
2841.909892	247816.305614	55.580583
2841.341131	247637.038057	55.585588
2840.694752	247460.227745	55.590593
2839.819269	247286.993697	55.595597
2839.315849	247113.191618	55.600602
2838.699669	246938.465359	55.605607
2838.501310	246755.498589	55.610612
2837.432159	246585.657540	55.615617
2836.834033	246406.243341	55.620621
2836.296066	246226.921703	55.625626
2835.403890	246048.827807	55.630631
2835.177309	245866.477820	55.635636
2834.289676	245688.434591	55.640641
2833.495437	245507.320917	55.645645
2833.006435	245326.821253	55.650650
2832.491809	245156.206547	55.655655
2831.870644	244960.779966	55.660660
2831.277284	244785.517986	55.665665
2830.403417	244599.248612	55.670669
2829.467343	244421.673079	55.675674
2828.862184	244252.983759	55.680679
2828.274058	244055.974401	55.685684
2827.353939	243888.226708	55.690689
2826.725814	243702.760035	55.695693
2826.296252	243527.881219	55.700698
2825.377944	243359.930196	55.705703
2824.949657	243175.578567	55.710708
2824.181967	243002.154595	55.715713
2823.190822	242825.048326	55.720717
2823.156969	242650.209904	55.725722
2821.984508	242477.309117	55.730727
2821.619831	242296.004503	55.735732
2820.958112	242121.851936	55.740737
2820.143579	241943.318365	55.745741
2819.700038	241764.497119	55.750746
2818.903691	241598.057027	55.755751
2818.453625	241404.595003	55.760756
2817.956693	241229.297148	55.765761
2816.686922	241051.040687	55.770765
2816.233442	240874.717873	55.775770
2815.615522	240702.826759	55.780775
2815.022849	240522.885047	55.785780
2814.237666	240349.645837	55.790785
2813.395422	240173.538413	55.795789
2813.086535	239985.760404	55.800794
2812.216242	239820.709584	55.805799
2811.684462	239632.203505	55.810804
2811.002812	239456.886597	55.815809
2810.176891	239273.698829	55.820813
2809.654203	239100.368983	55.825818
2808.932098	238925.976013	55.830823
2808.303704	238745.482500	55.835828
2807.636474	238576.658064	55.840833
2806.847794	238398.100311	55.845837
2806.040064	238207.526761	55.850842
2805.485205	238040.824332	55.855847
2804.706424	237864.277537	55.860852
2804.349561	237693.877445	55.865857
2803.462391	237516.126098	55.870861
2803.315789	237340.422204	55.875866
2802.445922	237157.856009	55.880871
2801.997524	236982.735230	55.885876
2801.159520	236806.632416	55.890881
2800.407008	236628.071826	55.895885
2800.041642	236446.674674	55.900890
2799.006930	236270.476579	55.905895
2798.507539	236083.321006	55.910900
2797.602770	235908.401587	55.915905
2796.936797	235728.963049	55.920909
2796.549616	235556.737785	55.925914
2795.886969	235375.415028	55.930919
2795.238941	235187.673478	55.935924
2794.748132	235015.847479	55.940929
2793.688562	234830.208833	55.945933
2793.203528	234653.417170	55.950938
2792.310929	234477.734355	55.955943
2791.754510	234298.408289	55.960948
2791.291864	234114.127830	55.965953
2790.894744	233947.559692	55.970957
2790.211031	233762.983869	55.975962
2789.252244	233578.808436	55.980967
2788.589473	233393.338780	55.985972
2788.204974	233213.325406	55.990977
2787.467805	233034.921453	55.995981
2786.917229	232850.555425	56.000986
2786.099136	232667.097851	56.005991
2785.397857	232481.508714	56.010996
2784.855369	232296.225804	56.016001
2784.049893	232115.058930	56.021005
2783.519334	231936.242350	56.026010
2782.497891	231759.031603	56.031015
2782.242187	231565.047419	56.036020
2781.550698	231379.127869	56.041025
2780.727632	231201.377506	56.046029
2780.147426	231013.531376	56.051034
2779.430830	230841.773960	56.056039
2778.844800	230645.781549	56.061044
2778.193890	230475.771309	56.066049
2777.419589	230282.661259	56.071053
2777.011217	230098.634569	56.076058
2776.050800	229924.014802	56.081063
2775.424982	229730.475014	56.086068
2775.056505	229548.276389	56.091073
2774.144188	229363.694455	56.096077
2773.747038	229175.262955	56.101082
2772.951018	228994.355337	56.106087
2772.321293	228809.908027	56.111092
2771.481181	228631.045075	56.116097
2770.728953	228442.925984	56.121101
2770.628896	228263.462800	56.126106
2769.477639	228083.759085	56.131111
2768.922347	227889.702912	56.136116
2768.386857	227700.863633	56.141121
2767.397223	227519.684187	56.146125
2766.927345	227332.694004	56.151130
2766.065360	227159.362655	56.156135
2765.530909	226981.549528	56.161140
2764.745976	226791.478696	56.166145
2764.296302	226610.368428	56.171149
2763.689851	226424.063860	56.176154
2762.878322	226243.495450	56.181159
2762.252084	226054.483238	56.186164
2761.617349	225869.546543	56.191169
2760.846784	225695.478089	56.196173
2760.381750	225506.225174	56.201178
2759.690703	225329.280559	56.206183
2758.701047	225140.073383	56.211188
2758.091977	224959.042875	56.216193
2757.550477	224781.910261	56.221197
2757.247416	224584.333678	56.226202
2756.037206	224413.036393	56.231207
2755.432690	224228.900616	56.236212
2754.960073	224046.144688	56.241217
2754.196416	223864.822857	56.246221
2753.645667	223674.696673	56.251226
2753.004415	223500.968885	56.256231
2752.255065	223315.597873	56.261236
2751.808464	223134.316602	56.266241
2750.948593	222949.154906	56.271245
2750.704455	222759.797079	56.276250
2749.836766	222579.576718	56.281255
2749.115832	222396.456574	56.286260
2748.505513	222209.856817	56.291265
2747.511589	222024.120247	56.296269
2747.138358	221834.823309	56.301274
2746.192331	221656.386949	56.306279
2745.672625	221473.364422	56.311284
2745.166520	221289.856450	56.316289
2744.707432	221110.567728	56.321293
2743.838814	220912.962676	56.326298
2742.956299	220728.879197	56.331303
2742.788832	220545.994062	56.336308
2741.947941	220364.247128	56.341313
2740.850088	220168.818906	56.346317
2740.630213	219985.497908	56.351322
2740.017843	219807.738656	56.356327
2739.248201	219626.211371	56.361332
2738.332918	219435.873396	56.366337
2737.663097	219257.157136	56.371341
2737.466282	219067.202765	56.376346
2736.709200	218882.391160	56.381351
2735.945256	218694.780672	56.386356
2735.185603	218502.562006	56.391361
2734.689001	218322.967744	56.396365
2733.698683	218126.293206	56.401370
2733.042538	217947.017923	56.406375
2732.507441	217749.063047	56.411380
2731.903548	217571.104258	56.416385
2731.267897	217389.714102	56.421389
2730.830124	217209.031351	56.426394
2729.846799	217026.958912	56.431399
2729.140103	216840.069774	56.436404
2728.727199	216647.495694	56.441409
2728.108816	216467.632645	56.446413
2727.484132	216282.234013	56.451418
2726.687308	216093.617296	56.456423
2726.043449	215898.306988	56.461428
2725.085484	215722.509219	56.466433
2724.094684	215539.894515	56.471437
2724.088512	215347.806951	56.476442
2723.067790	215161.506681	56.481447
2722.545436	214983.299740	56.486452
2721.991469	214790.129482	56.491457
2721.108703	214612.973428	56.496461
2720.529437	214430.487439	56.501466
2719.645218	214250.519568	56.506471
2719.639846	214060.370245	56.511476
2718.843648	213869.633935	56.516481
2717.993446	213698.495661	56.521485
2717.522248	213506.308791	56.526490
2716.728971	213322.485063	56.531495
2716.013232	213127.423248	56.536500
2715.599362	212938.283724	56.541505
2714.535442	212763.490540	56.546509
2713.913243	212576.332467	56.551514
2713.377148	212393.870690	56.556519
2712.768776	212193.945235	56.561524
2712.010544	212006.733977	56.566529
2711.134384	211827.229646	56.571533
2711.006821	211648.740024	56.576538
2710.233290	211461.469127	56.581543
2709.725298	211272.285715	56.586548
2708.857979	211075.013959	56.591553
2708.015316	210895.710570	56.596557
2707.287292	210708.663768	56.601562
2707.058410	210529.696931	56.606567
2705.938805	210338.194903	56.611572
2705.682496	210148.618589	56.616577
2704.709669	209964.171026	56.621581
2704.511204	209774.955775	56.626586
2703.648055	209592.171975	56.631591
2702.943439	209402.388923	56.636596
2702.231251	209209.629421	56.641601
2701.574080	209027.171020	56.646605
2701.233196	208831.248385	56.651610
2700.095929	208652.138081	56.656615
2699.555827	208453.855460	56.661620
2699.135990	208263.178065	56.666625
2698.075058	208083.459148	56.671629
2697.727072	207888.889731	56.676634
2696.919924	207700.528159	56.681639
2695.992705	207511.829834	56.686644
2695.460074	207324.889563	56.691649
2694.345971	207145.334573	56.696653
2694.014468	206959.750822	56.701658
2693.433502	206784.465092	56.706663
2692.655702	206594.422370	56.711668
2691.986487	206403.904884	56.716673
2691.124796	206235.397756	56.721677
2691.028009	206043.645331	56.726682
2690.526444	205861.210003	56.731687
2689.543236	205672.577261	56.736692
2689.115045	205488.336996	56.741697
2688.021661	205301.364640	56.746701
2687.889653	205113.337000	56.751706
2687.041080	204930.030492	56.756711
2686.692192	204739.404013	56.761716
2686.167762	204552.051220	56.766721
2684.882025	204361.816193	56.771725
2684.391516	204162.674606	56.776730
2683.738560	203965.824730	56.781735
2682.940262	203789.347922	56.786740
2682.405198	203601.796281	56.791745
2681.486099	203422.972653	56.796749
2680.843204	203220.333312	56.801754
2680.285048	203044.533430	56.806759
2679.687894	202860.582838	56.811764
2679.300413	202670.656556	56.816769
2678.487027	202478.125919	56.821773
2678.045047	202287.827780	56.826778
2676.930204	202096.453365	56.831783
2676.414134	201904.679329	56.836788
2675.836972	201721.263783	56.841793
2675.036684	201537.833285	56.846797
2674.466329	201343.486441	56.851802
2673.790130	201159.324894	56.856807
2673.075565	200969.201696	56.861812
2672.902800	200779.502348	56.866817
2671.462007	200588.146597	56.871821
2671.151036	200406.767513	56.876826
2670.482192	200212.122124	56.881831
2669.730036	200026.831111	56.886836
2669.356872	199842.295116	56.891841
2668.343194	199647.324612	56.896845
2667.854303	199454.651309	56.901850
2666.765601	199273.462838	56.906855
2666.298014	199077.428033	56.911860
2666.105986	198892.433927	56.916865
2665.269946	198716.780938	56.921869
2664.584872	198526.674343	56.926874
2664.072292	198321.538258	56.931879
2663.303536	198141.359111	56.936884
2662.733350	197950.625571	56.941889
2661.866144	197768.821766	56.946893
2661.306062	197577.871646	56.951898
2660.631127	197388.149270	56.956903
2660.020335	197199.269978	56.961908
2659.381480	197010.815728	56.966913
2658.669832	196826.471039	56.971917
2658.219326	196629.119216	56.976922
2657.477093	196432.692354	56.981927
2656.894348	196233.390669	56.986932
2656.203733	196051.132222	56.991937
2655.147453	195860.572379	56.996941
2654.545203	195655.028307	57.001946
2654.187260	195473.279072	57.006951
2653.137913	195281.040663	57.011956
2652.684533	195083.682476	57.016961
2651.632839	194905.073541	57.021965
2651.370813	194719.380005	57.026970
2650.878841	194527.730514	57.031975
2649.988333	194335.508682	57.036980
2649.716284	194146.790499	57.041985
2648.595875	193956.731444	57.046989
2648.320047	193761.805998	57.051994
2647.569212	193579.146043	57.056999
2646.846485	193377.778261	57.062004
2646.356075	193193.220776	57.067009
2645.487090	193002.998268	57.072013
2644.798115	192805.800834	57.077018
2643.832692	192613.444793	57.082023
2643.258574	192420.035065	57.087028
2642.793692	192228.237400	57.092033
2641.861965	192050.192197	57.097037
2641.486346	191856.346080	57.102042
2640.836755	191667.366299	57.107047
2640.204876	191484.224457	57.112052
2639.533307	191288.977011	57.117057
2638.818365	191097.884996	57.122061
2638.151849	190896.251255	57.127066
2637.480744	190716.655563	57.132071
2636.957397	190523.016274	57.137076
2636.358794	190325.929017	57.142081
2635.483994	190139.611807	57.147085
2634.947261	189946.167802	57.152090
2634.008384	189763.348291	57.157095
2633.217028	189566.218352	57.162100
2632.890281	189368.735716	57.167105
2632.088293	189184.586286	57.172109
2631.488361	188987.670144	57.177114
2630.580086	188815.065743	57.182119
2630.021253	188621.223492	57.187124
2629.624079	188431.211353	57.192129
2628.486539	188249.192500	57.197133
2628.115515	188063.541515	57.202138
2627.652914	187870.908460	57.207143
2626.594673	187692.517806	57.212148
2626.264199	187493.809537	57.217153
2625.539325	187307.848667	57.222157
2624.966584	187120.045165	57.227162
2624.193759	186931.370852	57.232167
2623.410021	186742.279209	57.237172
2623.486908	186545.113438	57.242177
2622.328927	186357.723805	57.247181
2621.777207	186155.685006	57.252186
2621.218074	185973.049111	57.257191
2620.126274	185783.412289	57.262196
2619.909435	185582.162599	57.267201
2619.265250	185395.242534	57.272205
2618.504541	185200.835923	57.277210
2617.884273	185011.611027	57.282215
2617.103173	184814.194286	57.287220
2616.435364	184615.984446	57.292225
2615.624681	184429.489109	57.297229
2615.204460	184226.751086	57.302234
2614.717420	184035.435589	57.307239
2613.781642	183847.550421	57.312244
2613.377932	183649.328442	57.317249
2612.471276	183455.652157	57.322253
2611.930561	183250.838655	57.327258
2611.348188	183061.412437	57.332263
2610.700630	182867.748545	57.337268
2610.221705	182672.964781	57.342273
2609.280840	182472.746928	57.347277
2608.521400	182267.730932	57.352282
2607.778092	182084.758414	57.357287
2607.143802	181894.264167	57.362292
2606.169147	181698.176708	57.367297
2605.325512	181498.914663	57.372301
2605.134726	181304.104037	57.377306
2604.250248	181125.915383	57.382311
2603.845683	180939.726589	57.387316
2603.400300	180738.763989	57.392321
2602.590067	180557.385815	57.397325
2602.044629	180358.552408	57.402330
2601.219806	180160.985326	57.407335
2600.789269	179969.576828	57.412340
2600.221363	179774.654765	57.417345
2599.128650	179583.569153	57.422349
2598.460675	179378.247050	57.427354
2597.783250	179187.250050	57.432359
2596.756197	179004.106577	57.437364
2596.745816	178802.270056	57.442369
2595.724716	178615.146023	57.447373
2595.100976	178427.616425	57.452378
2594.476092	178230.522683	57.457383
2593.796334	178052.517908	57.462388
2593.344312	177859.799482	57.467393
2592.506104	177673.820847	57.472397
2592.174276	177474.839893	57.477402
2591.121945	177282.346438	57.482407
2590.715844	177087.894460	57.487412
2590.096714	176890.284620	57.492417
2589.096522	176699.833392	57.497421
2588.586130	176502.017383	57.502426
2588.243518	176316.258822	57.507431
2587.216230	176117.903322	57.512436
2586.977485	175926.749926	57.517441
2585.878144	175735.225029	57.522445
2585.729786	175535.232242	57.527450
2584.990113	175334.431096	57.532455
2584.037986	175145.950843	57.537460
2583.924747	174937.968079	57.542465
2582.997146	174744.996122	57.547469
2582.264718	174550.200847	57.552474
2581.602598	174348.730909	57.557479
2580.881271	174152.829281	57.562484
2580.405824	173956.762458	57.567489
2579.606596	173763.991045	57.572493
2579.051294	173554.546522	57.577498
2578.072220	173354.225538	57.582503
2577.258797	173159.755046	57.587508
2577.198635	172968.701741	57.592513
2576.117963	172773.525115	57.597517
2575.738650	172577.513389	57.602522
2574.748218	172382.515148	57.607527
2574.283052	172175.937791	57.612532
2573.697969	171987.172544	57.617537
2572.675882	171789.931205	57.622541
2572.330500	171587.738233	57.627546
2571.547970	171392.991712	57.632551
2570.629985	171200.048059	57.637556
2570.345467	170999.832382	57.642561
2569.360711	170806.354400	57.647565
2568.770950	170619.694808	57.652570
2568.128918	170422.450985	57.657575
2567.397214	170222.946008	57.662580
2566.936540	170025.942514	57.667585
2566.086774	169850.874887	57.672589
2565.504292	169648.818533	57.677594
2564.851800	169453.641430	57.682599
2563.837691	169260.760772	57.687604
2563.353187	169067.237621	57.692609
2562.555549	168887.944147	57.697613
2561.791544	168686.582869	57.702618
2561.249907	168501.159384	57.707623
2560.656750	168307.784445	57.712628
2560.255001	168114.469169	57.717633
2559.166798	167931.576612	57.722637
2559.102610	167733.479294	57.727642
2558.025060	167542.626527	57.732647
2557.535516	167347.993856	57.737652
2556.714512	167141.385291	57.742657
2556.258987	166961.766918	57.747661
2555.561325	166770.450936	57.752666
2554.872140	166575.714007	57.757671
2554.201412	166387.549248	57.762676
2553.641623	166188.254271	57.767681
2552.906649	165997.622076	57.772685
2552.048935	165809.019374	57.777690
2551.403152	165623.893540	57.782695
2550.483302	165435.912920	57.787700
2550.291848	165237.302151	57.792705
2549.593793	165050.407294	57.797709
2548.797690	164859.523593	57.802714
2548.248264	164669.682582	57.807719
2547.933218	164474.401453	57.812724
2547.109016	164273.378525	57.817729
2546.528966	164086.635141	57.822733
2545.830039	163878.499525	57.827738
2545.264222	163689.034905	57.832743
2544.142899	163494.395355	57.837748
2543.952200	163290.899745	57.842753
2542.986188	163100.764140	57.847757
2542.492597	162903.587042	57.852762
2541.683531	162712.335137	57.857767
2541.257412	162524.049604	57.862772
2540.482607	162318.566825	57.867777
2539.582789	162148.082236	57.872781
2539.442942	161876.971548	57.877786
2538.938642	161669.682312	57.882791
2537.851093	161477.324090	57.887796
2537.533518	161278.398848	57.892801
2536.360190	161081.695421	57.897805
2535.670367	160883.721345	57.902810
2535.659747	160684.865183	57.907815
2534.659969	160480.089703	57.912820
2534.293118	160275.494800	57.917825
2533.242969	160088.681314	57.922829
2532.521632	159883.877861	57.927834
2531.899175	159681.793324	57.932839
2530.994334	159498.939248	57.937844
2530.519870	159294.214511	57.942849
2529.674874	159102.301105	57.947853
2529.340037	158901.955318	57.952858
2528.278107	158707.955343	57.957863
2527.496543	158519.760022	57.962868
2527.377458	158322.688754	57.967873
2526.562122	158132.949883	57.972877
2526.311673	157928.413745	57.977882
2525.594109	157728.008216	57.982887
2524.602817	157541.898173	57.987892
2524.060868	157326.491558	57.992897
2523.443449	157139.447254	57.997901
2522.696387	156936.063529	58.002906
2522.284201	156746.878553	58.007911
2521.418734	156550.304303	58.012916
2520.925718	156337.985206	58.017921
2519.969984	156145.762463	58.022925
2519.447932	155940.416714	58.027930
2518.611388	155748.380708	58.032935
2517.750676	155549.040224	58.037940
2517.157929	155356.052527	58.042945
2516.485092	155157.637952	58.047949
2516.009107	154964.112788	58.052954
2515.405773	154770.863145	58.057959
2514.460562	154579.715357	58.062964
2513.902071	154380.041474	58.067969
2513.264797	154185.516690	58.072973
2512.443630	153988.454473	58.077978
2511.853685	153794.407481	58.082983
2511.137861	153602.809407	58.087988
2510.773777	153412.364244	58.092993
2509.678873	153227.171275	58.097997
2509.087950	153024.587035	58.103002
2508.453572	152836.386999	58.108007
2507.779884	152654.409878	58.113012
2507.441153	152451.928969	58.118017
2506.772205	152263.407171	58.123021
2505.794076	152068.275061	58.128026
2505.625842	151872.939477	58.133031
2504.480156	151680.670670	58.138036
2503.719826	151486.295528	58.143041
2503.254484	151293.679652	58.148045
2503.093114	151099.249995	58.153050
2502.362531	150901.238453	58.158055
2501.279732	150701.593481	58.163060
2500.981621	150500.986497	58.168065
2499.890651	150311.233629	58.173069
2499.251589	150108.878274	58.178074
2498.926908	149912.142930	58.183079
2497.935402	149716.048271	58.188084
2497.596515	149524.528521	58.193089
2496.345160	149340.627768	58.198093
2496.178774	149140.643771	58.203098
2495.525379	148953.765382	58.208103
2494.728953	148762.093890	58.213108
2494.409901	148561.248020	58.218113
2493.687860	148367.953004	58.223117
2492.634958	148163.298782	58.228122
2492.068506	147960.182816	58.233127
2491.609116	147771.183555	58.238132
2491.131434	147573.508127	58.243137
2490.156024	147380.742165	58.248141
2489.437043	147180.972330	58.253146
2488.963083	146982.067230	58.258151
2488.222109	146786.141379	58.263156
2487.655886	146582.716436	58.268161
2486.945619	146396.751598	58.273165
2486.227468	146197.013243	58.278170
2486.003452	145996.537000	58.283175
2484.918603	145798.358866	58.288180
2483.965377	145589.003394	58.293185
2483.633529	145418.272206	58.298189
2483.223515	145212.874299	58.303194
2482.404061	145015.446933	58.308199
2481.432497	144809.441745	58.313204
2480.931714	144609.196135	58.318209
2480.545082	144416.075406	58.323213
2479.613278	144219.496877	58.328218
2478.819490	144023.380599	58.333223
2478.151202	143829.113654	58.338228
2477.510566	143616.799163	58.343233
2476.943278	143430.765750	58.348237
2476.065338	143237.323597	58.353242
2475.674685	143043.424208	58.358247
2474.502751	142853.741525	58.363252
2474.248196	142653.787195	58.368257
2473.075862	142464.106981	58.373261
2473.008563	142272.181585	58.378266
2472.157506	142081.347328	58.383271
2471.546179	141896.206936	58.388276
2471.011273	141689.390945	58.393281
2469.947811	141507.336021	58.398285
2469.851431	141311.799931	58.403290
2468.957077	141116.963361	58.408295
2467.915034	140926.954392	58.413300
2467.693502	140722.166413	58.418305
2466.885101	140533.266428	58.423309
2465.886305	140345.515926	58.428314
2465.544350	140151.296837	58.433319
2464.880145	139958.502303	58.438324
2464.331827	139766.414859	58.443329
2463.400122	139579.306489	58.448333
2462.517822	139384.479188	58.453338
2462.421124	139193.835780	58.458343
2461.354746	139012.558691	58.463348
2460.796963	138809.120267	58.468353
2460.243005	138621.221101	58.473357
2459.858620	138421.061194	58.478362
2459.154698	138231.409538	58.483367
2458.705146	138038.402775	58.488372
2457.811283	137844.845154	58.493377
2457.451591	137646.808264	58.498381
2456.504207	137447.785953	58.503386
2456.037876	137243.835561	58.508391
2454.757019	137055.769326	58.513396
2454.401102	136858.931346	58.518401
2453.468872	136675.881358	58.523405
2452.878960	136472.260803	58.528410
2452.510765	136279.608361	58.533415
2451.265997	136087.731341	58.538420
2450.608515	135894.924020	58.543425
2450.228165	135706.901548	58.548429
2449.486544	135518.010170	58.553434
2449.100777	135319.383314	58.558439
2448.057507	135144.059019	58.563444
2447.758037	134948.927240	58.568449
2447.123732	134764.317574	58.573453
2446.452125	134571.622886	58.578458
2445.864533	134369.566474	58.583463
2445.224615	134185.952250	58.588468
2444.272120	133986.052409	58.593473
2443.591408	133789.616934	58.598477
2443.092220	133594.144863	58.603482
2442.654247	133394.370819	58.608487
2441.909756	133212.418062	58.613492
2441.319683	133015.414588	58.618497
2440.530913	132829.685853	58.623501
2439.773998	132628.316358	58.628506
2439.291507	132430.156628	58.633511
2438.292657	132237.847033	58.638516
2437.964529	132044.162181	58.643521
2437.362312	131849.912387	58.648525
2436.690202	131649.920916	58.653530
2436.422399	131458.300950	58.658535
2435.526643	131259.732214	58.663540
2434.820430	131052.472125	58.668545
2434.269574	130860.088160	58.673549
2433.621006	130657.699332	58.678554
2433.224150	130449.632531	58.683559
2432.233758	130256.509463	58.688564
2431.539145	130057.421956	58.693569
2430.927748	129861.459910	58.698573
2429.960052	129662.202579	58.703578
2429.676163	129453.591807	58.708583
2428.659059	129255.831246	58.713588
2428.039578	129060.854081	58.718593
2427.620948	128875.778559	58.723597
2427.042971	128672.491136	58.728602
2426.044850	128467.328591	58.733607
2425.190325	128276.661637	58.738612
2424.982069	128068.252475	58.743617
2423.470810	127879.229137	58.748621
2422.927051	127681.201558	58.753626
2422.856291	127488.993350	58.758631
2422.179146	127299.282947	58.763636
2421.396029	127104.574110	58.768641
2420.410222	126903.409077	58.773645
2419.992202	126715.579330	58.778650
2419.554318	126523.982166	58.783655
2418.589874	126331.237944	58.788660
2418.156062	126127.209864	58.793665
2417.461804	125933.371547	58.798669
2416.673456	125740.997265	58.803674
2416.247444	125544.604695	58.808679
2415.330292	125347.351656	58.813684
2414.688802	125151.351669	58.818689
2414.102915	124956.398310	58.823693
2413.412455	124761.234351	58.828698
2413.071129	124565.737076	58.833703
2411.883765	124379.099438	58.838708
2411.760371	124171.976432	58.843713
2410.463773	123982.806411	58.848717
2410.037527	123788.064761	58.853722
2409.485574	123589.395229	58.858727
2408.648135	123401.883502	58.863732
2408.350590	123195.887689	58.868737
2407.159775	123009.539483	58.873741
2406.637368	122813.156701	58.878746
2406.189510	122618.579360	58.883751
2405.432751	122435.531323	58.888756
2404.845263	122233.677629	58.893761
2404.284367	122037.941556	58.898765
2403.658647	121843.233012	58.903770
2403.119052	121647.839275	58.908775
2402.131608	121456.301819	58.913780
2401.715485	121252.549205	58.918785
2401.159815	121053.937278	58.923789
2400.046514	120848.076296	58.928794
2399.892519	120646.597687	58.933799
2398.657999	120464.527824	58.938804
2398.381321	120265.217375	58.943809
2397.838975	120064.630093	58.948813
2396.928680	119871.644507	58.953818
2396.314299	119660.450968	58.958823
2395.540966	119477.540361	58.963828
2395.198335	119270.953804	58.968833
2394.268349	119073.977873	58.973837
2393.351695	118875.623782	58.978842
2393.069428	118679.792374	58.983847
2392.467793	118493.839785	58.988852
2391.805230	118291.736288	58.993857
2390.937113	118094.485018	58.998861
2390.212553	117907.330982	59.003866
2389.809994	117700.036423	59.008871
2388.958864	117507.166934	59.013876
2388.547465	117303.869703	59.018881
2387.869583	117108.087527	59.023885
2387.145208	116911.279551	59.028890
2386.960113	116702.422423	59.033895
2385.901726	116508.247606	59.038900
2385.552393	116306.230631	59.043905
2384.683909	116093.938577	59.048909
2383.868920	115906.559559	59.053914
2383.594625	115691.174346	59.058919
2382.651759	115501.952467	59.063924
2382.216373	115297.424563	59.068929
2381.817026	115097.856073	59.073933
2380.497820	114882.021355	59.078938
2380.272165	114669.442511	59.083943
2379.389438	114481.304057	59.088948
2378.844250	114282.044385	59.093953
2378.359932	114068.927679	59.098957
2377.292337	113876.919692	59.103962
2376.457750	113662.897231	59.108967
2375.757543	113462.818143	59.113972
2375.296052	113267.799205	59.118977
2374.794746	113066.657227	59.123981
2373.983506	112863.681060	59.128986
2373.497890	112655.076295	59.133991
2372.794789	112449.382716	59.138996
2372.236850	112252.571882	59.144001
2371.318003	112054.690165	59.149005
2370.650604	111851.344027	59.154010
2369.865686	111652.416168	59.159015
2369.409080	111451.292818	59.164020
2368.865767	111242.379030	59.169025
2368.353320	111046.884193	59.174029
2367.630434	110841.130909	59.179034
2367.019185	110638.001589	59.184039
2366.163113	110431.581117	59.189044
2365.406303	110223.966293	59.194049
2365.055461	110023.104324	59.199053
2363.688449	109821.078835	59.204058
2363.404446	109619.251350	59.209063
2362.697865	109418.933005	59.214068
2362.339692	109216.657356	59.219073
2361.746681	109021.045437	59.224077
2360.921835	108819.405481	59.229082
2360.184715	108602.701730	59.234087
2359.433560	108406.643898	59.239092
2359.201796	108190.250762	59.244097
2358.130204	108003.327258	59.249101
2357.318491	107803.768565	59.254106
2356.840496	107591.893238	59.259111
2356.125029	107383.794734	59.264116
2355.922007	107178.402283	59.269121
2355.024973	106979.022545	59.274125
2354.058675	106779.293770	59.279130
2353.904112	106571.316372	59.284135
2353.088374	106363.490018	59.289140
2352.344418	106152.215162	59.294145
2351.952631	105952.668642	59.299149
2351.247581	105743.256592	59.304154
2350.880010	105534.604984	59.309159
2349.945039	105335.105321	59.314164
2349.434104	105110.517010	59.319169
2348.735878	104910.222008	59.324173
2347.822753	104692.064980	59.329178
2347.210067	104481.266255	59.334183
2346.442059	104275.785230	59.339188
2345.367032	104061.034870	59.344193
2344.803498	103875.439692	59.349197
2344.377203	103674.325302	59.354202
2343.943649	103459.770515	59.359207
2343.137460	103263.915711	59.364212
2342.503688	103040.609905	59.369217
2342.232754	102835.386119	59.374221
2341.273971	102631.967017	59.379226
2340.662469	102415.673646	59.384231
2339.702873	102207.240351	59.389236
2339.086082	101998.976584	59.394241
2338.534999	101798.329378	59.399245
2338.056189	101587.205415	59.404250
2337.409685	101371.333229	59.409255
2336.393444	101173.562666	59.414260
2335.805768	100966.965484	59.419265
2335.562113	100752.405341	59.424269
2334.367050	100547.348150	59.429274
2333.868384	100345.658478	59.434279
2332.963807	100141.066282	59.439284
2332.462807	99920.363620	59.444289
2331.670535	99726.743685	59.449293
2331.318559	99523.414070	59.454298
2330.537463	99307.233548	59.459303
2329.880612	99114.003231	59.464308
2329.381895	98903.027360	59.469313
2328.711159	98685.725162	59.474317
2327.692578	98487.863754	59.479322
2327.405577	98278.858022	59.484327
2326.833422	98068.878239	59.489332
2325.854424	97860.575920	59.494337
2325.325485	97654.062505	59.499341
2324.655849	97447.668405	59.504346
2324.051798	97236.534304	59.509351
2323.321325	97044.626973	59.514356
2322.720045	96829.931775	59.519361
2322.192946	96605.618294	59.524365
2321.108799	96407.556997	59.529370
2320.598890	96199.195493	59.534375
2320.020056	95998.768121	59.539380
2319.480449	95780.895678	59.544385
2319.191256	95566.480058	59.549389
2318.377551	95367.262454	59.554394
2317.614947	95148.277246	59.559399
2316.645209	94938.605075	59.564404
2316.288459	94722.546643	59.569409
2315.908279	94514.421110	59.574413
2314.857448	94311.718140	59.579418
2314.198875	94094.305775	59.584423
2313.425742	93884.428375	59.589428
2312.891465	93671.693123	59.594433
2311.957166	93459.143818	59.599437
2311.297765	93256.172742	59.604442
2310.853099	93047.411589	59.609447
2309.830468	92839.023058	59.614452
2309.299432	92620.780472	59.619457
2309.019974	92409.215349	59.624461
2308.135358	92211.666769	59.629466
2307.891790	92000.239359	59.634471
2307.039260	91792.937015	59.639476
2306.526641	91577.517151	59.644481
2306.035876	91361.569637	59.649485
2304.660268	91150.482057	59.654490
2304.492431	90930.841636	59.659495
2303.464761	90728.300874	59.664500
2302.940662	90512.132379	59.669505
2302.347370	90300.561153	59.674509
2301.256546	90102.265289	59.679514
2300.906567	89888.573458	59.684519
2300.208243	89675.141845	59.689524
2299.645828	89463.174380	59.694529
2299.273520	89256.384114	59.699533
2298.217309	89050.173434	59.704538
2297.798290	88833.973169	59.709543
2296.855231	88619.861596	59.714548
2296.242884	88406.517541	59.719553
2295.763152	88188.970239	59.724557
2294.962500	87989.043621	59.729562
2294.467811	87774.121200	59.734567
2293.823941	87574.103817	59.739572
2293.095054	87350.042888	59.744577
2292.400603	87142.100325	59.749581
2291.417151	86942.903397	59.754586
2291.015910	86722.366177	59.759591
2290.310826	86511.762489	59.764596
2289.824826	86303.756939	59.769601
2289.014136	86088.413329	59.774605
2288.538480	85889.177347	59.779610
2287.801998	85671.043263	59.784615
2286.740214	85456.531887	59.789620
2286.562124	85246.231080	59.794625
2285.896987	85032.155510	59.799629
2284.932668	84833.501313	59.804634
2284.781903	84609.371030	59.809639
2283.797315	84398.845180	59.814644
2283.094641	84192.808872	59.819649
2282.696007	83980.907491	59.824653
2282.011123	83771.107320	59.829658
2281.517367	83549.235775	59.834663
2280.671427	83336.657504	59.839668
2279.761260	83120.548414	59.844673
2279.100872	82904.357559	59.849677
2278.387731	82700.448118	59.854682
2277.784704	82485.057431	59.859687
2277.549181	82279.751645	59.864692
2276.416621	82066.141510	59.869697
2276.194171	81849.803319	59.874701
2275.596769	81639.066167	59.879706
2274.716751	81418.685381	59.884711
2273.871783	81210.983274	59.889716
2273.509398	80993.079016	59.894721
2273.053343	80771.154804	59.899725
2272.106540	80555.534298	59.904730
2271.482571	80340.612657	59.909735
2270.548938	80125.102267	59.914740
2270.003095	79917.099463	59.919745
2269.232839	79688.956284	59.924750
2268.487322	79484.722174	59.929754
2267.877006	79272.325338	59.934759
2267.252001	79070.915269	59.939764
2266.703719	78845.338086	59.944769
2265.772436	78633.220530	59.949774
2265.057151	78433.326543	59.954778
2264.382669	78214.835634	59.959783
2263.846481	78006.660448	59.964788
2262.904006	77801.517406	59.969793
2262.720451	77584.558544	59.974798
2261.503643	77386.718663	59.979802
2260.973995	77171.789753	59.984807
2260.364899	76963.250207	59.989812
2259.756725	76753.945938	59.994817
2259.469643	76544.795657	59.999822
2258.321380	76339.604888	60.004826
2257.764247	76118.747996	60.009831
2257.351772	75924.856258	60.014836
2256.310893	75714.199340	60.019841
2255.705337	75500.966501	60.024846
2254.711566	75297.244402	60.029850
2254.655596	75098.070522	60.034855
2253.725704	74894.025558	60.039860
2252.913496	74679.528971	60.044865
2252.594573	74464.170802	60.049870
2251.939664	74270.010254	60.054874
2251.751286	74057.898579	60.059879
2250.811377	73852.161485	60.064884
2250.033019	73634.008744	60.069889
2249.409870	73421.187152	60.074894
2248.848814	73225.140211	60.079898
2248.574807	72998.741838	60.084903
2247.327256	72792.608278	60.089908
2246.629010	72579.617490	60.094913
2246.196808	72363.710670	60.099918
2245.066607	72155.164105	60.104922
2244.707114	71949.969017	60.109927
2243.839796	71733.909979	60.114932
2243.111438	71523.994985	60.119937
2242.588847	71319.820495	60.124942
2241.826343	71107.172398	60.129946
2241.480984	70903.753243	60.134951
2240.577335	70697.694553	60.139956
2239.958741	70494.969059	60.144961
2239.581849	70278.594730	60.149966
2238.737019	70077.999745	60.154970
2238.049774	69862.832047	60.159975
2237.171875	69656.628127	60.164980
2236.373101	69453.283171	60.169985
2235.800444	69247.370839	60.174990
2235.080024	69038.665483	60.179994
2234.692909	68835.933031	60.184999
2233.930305	68636.676177	60.190004
2233.178058	68428.622088	60.195009
2232.794959	68212.930211	60.200014
2231.957163	68016.161756	60.205018
2230.926731	67801.318139	60.210023
2230.638475	67603.491315	60.215028
2229.897315	67392.450768	60.220033
2229.437709	67186.250886	60.225038
2228.389105	66986.454592	60.230042
2228.048993	66778.922752	60.235047
2227.275560	66584.248549	60.240052
2226.736472	66372.639220	60.245057
2226.626819	66163.449809	60.250062
2225.169860	65950.635414	60.255066
2224.761989	65739.968476	60.260071
2224.121305	65537.674776	60.265076
2223.270756	65337.791277	60.270081
2223.044582	65125.458880	60.275086
2222.080431	64924.277329	60.280090
2221.596063	64700.553842	60.285095
2221.025022	64496.081651	60.290100
2219.877692	64299.482437	60.295105
2219.662766	64083.898573	60.300110
2218.679604	63879.007581	60.305114
2218.050179	63667.227046	60.310119
2217.392971	63464.989485	60.315124
2216.585524	63265.624171	60.320129
2216.019558	63049.123027	60.325134
2215.309975	62856.765510	60.330138
2214.411966	62645.627800	60.335143
2213.825061	62447.724066	60.340148
2213.411499	62247.008930	60.345153
2212.709701	62044.761884	60.350158
2211.994419	61851.680980	60.355162
2211.159007	61631.515752	60.360167
2210.489034	61436.165212	60.365172
2209.900583	61237.508261	60.370177
2209.377404	61046.390010	60.375182
2208.512774	60846.109514	60.380186
2208.163192	60635.511884	60.385191
2207.251495	60439.573726	60.390196
2206.251961	60240.878533	60.395201
2205.631702	60040.368426	60.400206
2204.851719	59846.479473	60.405210
2204.352906	59651.038011	60.410215
2203.787422	59457.701496	60.415220
2202.857204	59258.578392	60.420225
2202.492289	59057.474867	60.425230
2201.685515	58877.293462	60.430234
2201.079551	58675.200400	60.435239
2200.176167	58488.039665	60.440244
2199.426839	58285.324699	60.445249
2198.924037	58088.456892	60.450254
2197.915227	57908.940444	60.455258
2197.305915	57721.341970	60.460263
2196.436313	57532.498495	60.465268
2195.761459	57350.946804	60.470273
2195.147703	57156.955021	60.475278
2193.887617	56980.741060	60.480282
2194.000643	56801.712537	60.485287
2192.939574	56618.814563	60.490292
2192.235336	56450.518412	60.495297
2191.671865	56270.510462	60.500302
2190.646117	56091.090304	60.505306
2190.151887	55911.973686	60.510311
2189.347886	55747.133597	60.515316
2188.689991	55575.008724	60.520321
2187.991899	55399.945492	60.525326
2187.023586	55228.072490	60.530330
2186.420590	55063.551605	60.535335
2185.749871	54890.226292	60.540340
2184.776546	54729.105837	60.545345
2184.364807	54568.385058	60.550350
2183.342643	54409.923908	60.555354
2182.513142	54247.490586	60.560359
2181.892004	54095.471626	60.565364
2181.178132	53936.247346	60.570369
2180.278052	53785.009380	60.575374
2179.444615	53644.847019	60.580378
2178.934999	53492.252136	60.585383
2178.376507	53347.994874	60.590388
2177.123283	53204.219192	60.595393
2176.506480	53067.583627	60.600398
2175.769245	52930.664425	60.605402
2174.928062	52789.142926	60.610407
2174.369088	52655.035868	60.615412
2173.645663	52520.370512	60.620417
2173.125812	52375.814250	60.625422
2171.967671	52258.920278	60.630426
2171.489451	52123.899393	60.635431
2170.755069	51995.849579	60.640436
2170.249341	51870.596268	60.645441
2169.660084	51732.963390	60.650446
2168.636643	51604.168028	60.655450
2167.823938	51479.032581	60.660455
2167.148285	51360.292872	60.665460
2166.538125	51235.579438	60.670465
2165.997469	51102.569417	60.675470
2165.198075	50994.843367	60.680474
2164.904583	50868.490777	60.685479
2164.138356	50748.700070	60.690484
2163.082349	50623.004873	60.695489
2162.530530	50500.049571	60.700494
2161.946843	50390.960941	60.705498
2161.450507	50272.190487	60.710503
2160.741350	50145.443849	60.715508
2159.936479	50021.035502	60.720513
2159.617929	49895.124018	60.725518
2158.622031	49788.559526	60.730522
2157.969092	49671.782579	60.735527
2157.385828	49552.075254	60.740532
2156.800955	49437.940211	60.745537
2155.990342	49312.259589	60.750542
2155.832053	49202.003450	60.755546
2155.087168	49076.247628	60.760551
2154.461580	48968.749805	60.765556
2153.575036	48852.382260	60.770561
2153.286835	48716.812741	60.775566
2152.563333	48604.992269	60.780570
2151.638858	48471.648286	60.785575
2151.129428	48350.883875	60.790580
2150.375684	48225.454986	60.795585
2149.729895	48111.056570	60.800590
2148.904904	48000.976912	60.805594
2148.661164	47873.153984	60.810599
2147.854203	47762.051175	60.815604
2147.168482	47644.973235	60.820609
2146.753572	47514.314054	60.825614
2145.834357	47407.485958	60.830618
2145.052097	47274.628225	60.835623
2144.331540	47159.672101	60.840628
2144.048144	47038.763735	60.845633
2143.221833	46916.977548	60.850638
2142.657148	46796.140777	60.855642
2142.183777	46674.616589	60.860647
2141.212607	46548.946239	60.865652
2140.618009	46439.032716	60.870657
2140.217963	46313.422105	60.875662
2139.311550	46200.412245	60.880666
2138.617057	46076.678307	60.885671
2137.998962	45954.830949	60.890676
2137.648034	45836.781965	60.895681
2137.098044	45706.236690	60.900686
2135.923040	45594.759954	60.905690
2135.357261	45470.004042	60.910695
2134.901758	45340.850852	60.915700
2134.218515	45228.893569	60.920705
2134.009037	45104.276670	60.925710
2133.051104	44987.433559	60.930714
2132.438203	44854.633667	60.935719
2131.591094	44735.699826	60.940724
2130.835984	44610.028072	60.945729
2130.331922	44481.271631	60.950734
2129.835469	44368.521669	60.955738
2129.139996	44237.599275	60.960743
2128.305265	44108.705120	60.965748
2127.489429	43994.363637	60.970753
2126.772642	43866.350770	60.975758
2126.358526	43747.743982	60.980762
2125.549476	43627.521306	60.985767
2124.867317	43503.367186	60.990772
2124.131665	43387.695003	60.995777
2123.624920	43266.803831	61.000782
2122.425268	43161.586307	61.005786
2122.341843	43039.342401	61.010791
2121.918356	42923.073509	61.015796
2120.960267	42812.867303	61.020801
2120.517091	42680.142464	61.025806
2119.866990	42554.383525	61.030810
2118.993530	42428.588202	61.035815
2118.383571	42308.962917	61.040820
2117.764023	42184.476263	61.045825
2117.243855	42068.326486	61.050830
2116.137612	41958.683671	61.055834
2115.641105	41832.968860	61.060839
2115.027145	41703.791932	61.065844
2114.358592	41589.771836	61.070849
2113.855245	41457.543438	61.075854
2112.791613	41349.070932	61.080858
2112.311572	41222.203757	61.085863
2111.895887	41104.807481	61.090868
2111.072228	40988.099680	61.095873
2110.517864	40863.751362	61.100878
2109.654669	40750.659431	61.105882
2109.307604	40625.647526	61.110887
2108.386434	40512.202727	61.115892
2107.561527	40401.175013	61.120897
2107.036508	40268.048542	61.125902
2106.228417	40152.200866	61.130906
2105.583645	40034.127331	61.135911
2105.010582	39920.635963	61.140916
2104.191765	39803.544962	61.145921
2103.970008	39685.748202	61.150926
2102.968149	39563.255738	61.155930
2102.416565	39449.142783	61.160935
2102.020856	39330.312108	61.165940
2101.013970	39214.834325	61.170945
2100.654785	39096.344123	61.175950
2100.049674	38976.399826	61.180954
2098.985105	38864.525348	61.185959
2098.866138	38739.881517	61.190964
2097.940984	38622.584694	61.195969
2097.484433	38499.006358	61.200974
2096.676811	38386.299095	61.205978
2096.073268	38257.130725	61.210983
2095.298014	38128.547027	61.215988
2094.466295	38014.217826	61.220993
2093.637620	37897.784886	61.225998
2093.182862	37779.023423	61.231002
2092.401842	37666.710335	61.236007
2092.280776	37541.508136	61.241012
2091.340175	37426.427192	61.246017
2090.765747	37299.474542	61.251022
2089.893187	37184.521972	61.256026
2089.304702	37061.991450	61.261031
2088.662696	36942.370889	61.266036
2088.018158	36837.851883	61.271041
2087.354510	36706.624698	61.276046
2086.777097	36592.354861	61.281050
2085.926426	36468.050909	61.286055
2085.405970	36346.301957	61.291060
2084.667928	36237.124395	61.296065
2084.364396	36110.700412	61.301070
2083.360226	35985.702037	61.306074
2082.682581	35868.843433	61.311079
2082.177251	35746.715496	61.316084
2081.254011	35634.218817	61.321089
2080.576588	35519.543802	61.326094
2079.846432	35398.462475	61.331098
2079.251441	35283.363471	61.336103
2078.665313	35166.100105	61.341108
2077.796970	35047.393491	61.346113
2077.561572	34920.962914	61.351118
2076.742442	34810.884485	61.356122
2076.032505	34696.730765	61.361127
2075.600280	34578.960302	61.366132
2074.645033	34465.626261	61.371137
2074.107728	34342.593806	61.376142
2073.620849	34227.590804	61.381146
2072.979301	34107.408777	61.386151
2071.854467	33989.640164	61.391156
2071.126511	33874.063072	61.396161
2070.688221	33753.626925	61.401166
2070.039682	33639.058218	61.406170
2069.164661	33528.063119	61.411175
2068.703743	33413.783847	61.416180
2067.603688	33299.804323	61.421185
2067.276445	33188.119297	61.426190
2066.506400	33073.192908	61.431194
2065.793013	32963.108333	61.436199
2065.581771	32850.150816	61.441204
2064.520765	32743.963014	61.446209
2064.246873	32619.623039	61.451214
2063.171699	32511.781252	61.456218
2062.266210	32399.497970	61.461223
2062.015475	32281.978875	61.466228
2061.303570	32175.943176	61.471233
2060.454448	32056.444193	61.476238
2059.831464	31952.642912	61.481242
2059.344286	31834.434453	61.486247
2058.833116	31719.436879	61.491252
2057.897106	31613.426132	61.496257
2057.337562	31497.319006	61.501262
2056.762460	31386.028368	61.506266
2055.990890	31279.769290	61.511271
2055.207707	31164.223032	61.516276
2054.491831	31054.884755	61.521281
2054.276001	30941.413242	61.526286
2053.256645	30825.418582	61.531290
2052.571275	30716.774544	61.536295
2052.031044	30603.334721	61.541300
2051.224016	30500.821651	61.546305
2050.672312	30385.389504	61.551310
2049.867241	30284.301126	61.556314
2048.606974	30167.584596	61.561319
2048.421593	30053.643525	61.566324
2047.622452	29969.228779	61.571329
2046.766622	29858.789374	61.576334
2046.269256	29754.226785	61.581338
2045.911362	29645.937619	61.586343
2045.137804	29537.166874	61.591348
2044.570876	29443.595109	61.596353
2044.027473	29330.016086	61.601358
2043.258410	29226.959879	61.606362
2042.445182	29110.792980	61.611367
2041.677299	29006.587773	61.616372
2041.248870	28901.400362	61.621377
2040.524068	28796.958988	61.626382
2039.658955	28698.785944	61.631386
2039.079694	28582.048514	61.636391
2038.534697	28477.800258	61.641396
2037.811429	28387.942089	61.646401
2037.625991	28280.996470	61.651406
2036.828629	28163.356630	61.656410
2036.030769	28062.111826	61.661415
2035.357408	27954.179388	61.666420
2034.374318	27849.121557	61.671425
2033.672433	27732.528173	61.676430
2032.860196	27640.593418	61.681434
2032.428923	27537.263658	61.686439
2031.768390	27435.558628	61.691444
2030.768686	27351.966539	61.696449
2030.385558	27249.476157	61.701454
2029.737507	27141.380817	61.706458
2029.074938	27036.531732	61.711463
2028.287679	26939.306411	61.716468
2027.330348	26844.694686	61.721473
2026.534732	26744.518553	61.726478
2026.167635	26655.272212	61.731482
2025.082286	26563.972994	61.736487
2024.891800	26460.336239	61.741492
2024.069200	26377.312686	61.746497
2023.368581	26277.647252	61.751502
2022.826111	26188.435272	61.756506
2022.091283	26108.104359	61.761511
2021.189185	26001.147727	61.766516
2020.303346	25923.328071	61.771521
2020.087755	25824.612074	61.776526
2019.147821	25739.369724	61.781530
2018.397033	25651.371391	61.786535
2018.094311	25565.273781	61.791540
2017.198513	25473.821929	61.796545
2016.644603	25386.356930	61.801550
2015.859151	25294.013497	61.806554
2015.331704	25207.096548	61.811559
2014.644150	25119.594188	61.816564
2013.805598	25033.960400	61.821569
2013.240943	24941.544466	61.826574
2012.493056	24860.456576	61.831578
2011.702159	24778.279729	61.836583
2011.241881	24683.386233	61.841588
2010.657183	24603.228567	61.846593
2009.608778	24513.664711	61.851598
2008.951309	24430.633705	61.856602
2008.445176	24347.723637	61.861607
2007.949138	24260.148194	61.866612
2007.371211	24183.509057	61.871617
2007.000530	24087.282068	61.876622
2005.716573	24009.612287	61.881626
2005.091277	23915.996512	61.886631
2004.708238	23834.754836	61.891636
2003.710978	23754.033554	61.896641
2002.833220	23672.282885	61.901646
2002.347750	23591.231653	61.906650
2001.775340	23509.397032	61.911655
2001.102988	23425.852413	61.916660
2000.169628	23355.241416	61.921665
1999.576854	23267.397747	61.926670
1999.481169	23191.465476	61.931674
1998.787104	23112.711448	61.936679
1998.494283	23023.567502	61.941684
1997.621168	22950.462835	61.946689
1997.014591	22857.925054	61.951694
1996.120115	22764.696747	61.956698
1995.560045	22687.335481	61.961703
1994.921460	22591.433268	61.966708
1994.060201	22506.025919	61.971713
1993.612581	22416.433786	61.976718
1992.644831	22334.258922	61.981722
1991.786946	22257.515564	61.986727
1991.038994	22169.843149	61.991732
1990.315381	22094.678282	61.996737
1989.960786	22011.039347	62.001742
1989.193175	21942.545067	62.006746
1988.594387	21860.770505	62.011751
1987.933943	21778.041240	62.016756
1987.116896	21705.094504	62.021761
1986.774430	21622.466401	62.026766
1986.219415	21541.885955	62.031770
1985.085329	21458.698184	62.036775
1984.808980	21385.277045	62.041780
1983.795641	21304.153092	62.046785
1983.088310	21217.506770	62.051790
1982.220450	21147.222905	62.056794
1981.359991	21075.734067	62.061799
1981.213359	21005.151602	62.066804
1980.394352	20937.115164	62.071809
1979.660969	20856.845247	62.076814
1978.977164	20784.585917	62.081818
1978.482623	20727.422546	62.086823
1978.061598	20645.745288	62.091828
1977.518591	20571.403839	62.096833
1976.898474	20473.909532	62.101838
1975.953749	20407.035453	62.106842
1975.266171	20323.648588	62.111847
1974.872942	20246.119623	62.116852
1974.174026	20181.171076	62.121857
1973.325768	20094.403292	62.126862
1972.529155	20022.508421	62.131866
1971.697013	19954.459374	62.136871
1971.198546	19872.667756	62.141876
1970.459865	19803.006147	62.146881
1969.777877	19732.443698	62.151886
1969.112544	19661.647597	62.156890
1968.448461	19592.086800	62.161895
1968.132771	19517.716231	62.166900
1967.309651	19442.289282	62.171905
1966.625835	19357.648887	62.176910
1966.006921	19290.285742	62.181914
1965.205909	19220.126607	62.186919
1964.511497	19136.559635	62.191924
1964.145650	19068.837535	62.196929
1963.517625	18992.799939	62.201934
1962.680691	18920.227317	62.206938
1962.043287	18846.539025	62.211943
1961.601710	18764.218773	62.216948
1960.257490	18704.801221	62.221953
1960.008921	18626.871256	62.226958
1959.322680	18562.212805	62.231962
1958.334952	18493.204047	62.236967
1957.795211	18415.294119	62.241972
1957.002408	18351.520269	62.246977
1956.661030	18273.001693	62.251982
1956.056548	18201.341663	62.256986
1955.247705	18136.892718	62.261991
1954.800894	18057.542531	62.266996
1953.954214	17996.073166	62.272001
1953.320009	17923.853902	62.277006
1952.644061	17849.901324	62.282010
1951.837577	17777.537597	62.287015
1951.366787	17703.921017	62.292020
1951.030544	17638.892712	62.297025
1950.245119	17567.752569	62.302030
1949.422654	17493.382088	62.307034
1948.766649	17428.609873	62.312039
1948.260240	17345.247246	62.317044
1947.260483	17287.093993	62.322049
1946.469531	17204.994130	62.327054
1946.126373	17134.217567	62.332058
1945.382748	17068.518635	62.337063
1944.733546	16999.718534	62.342068
1943.806261	16931.767250	62.347073
1943.456089	16856.010946	62.352078
1942.480207	16785.480666	62.357082
1941.949202	16714.432325	62.362087
1941.679897	16655.486647	62.367092
1940.842188	16584.928835	62.372097
1940.084027	16510.060308	62.377102
1939.255769	16437.694647	62.382106
1938.571472	16375.882496	62.387111
1938.211606	16304.839061	62.392116
1936.864427	16242.768187	62.397121
1936.771609	16168.217800	62.402126
1935.955864	16108.162343	62.407130
1934.902826	16043.413362	62.412135
1934.964227	15980.107050	62.417140
1933.997871	15912.109225	62.422145
1933.589026	15845.949728	62.427150
1932.907030	15774.449769	62.432154
1932.473779	15705.291017	62.437159
1931.768171	15627.717012	62.442164
1931.156517	15567.104403	62.447169
1930.234719	15494.111378	62.452174
1929.489606	15420.187502	62.457178
1928.609591	15368.244092	62.462183
1928.444083	15288.266725	62.467188
1927.368010	15227.274545	62.472193
1926.807437	15148.647742	62.477198
1926.159970	15076.112669	62.482202
1925.359581	15007.261190	62.487207
1924.747453	14952.409425	62.492212
1923.946440	14882.642160	62.497217
1923.396185	14812.768615	62.502222
1922.686555	14747.612842	62.507226
1921.746689	14692.716656	62.512231
1921.535730	14631.644466	62.517236
1920.730880	14574.593125	62.522241
1920.208939	14503.694804	62.527246
1919.822142	14430.436135	62.532250
1918.689300	14369.360092	62.537255
1918.250115	14298.648569	62.542260
1917.483867	14231.864825	62.547265
1916.846480	14163.494491	62.552270
1916.225084	14101.509043	62.557274
1915.626009	14044.438158	62.562279
1915.098406	13968.407430	62.567284
1914.476491	13902.849301	62.572289
1913.676205	13821.458226	62.577294
1913.172063	13760.492275	62.582298
1912.571154	13691.853772	62.587303
1911.986994	13625.328771	62.592308
1911.320664	13563.374831	62.597313
1910.430864	13484.589913	62.602318
1909.878114	13419.836116	62.607322
1909.065425	13357.281009	62.612327
1908.652035	13285.017143	62.617332
1907.666800	13217.812397	62.622337
1907.308109	13145.754966	62.627342
1906.633422	13078.384022	62.632346
1905.632213	13006.673792	62.637351
1904.941165	12937.872265	62.642356
1904.146915	12878.656346	62.647361
1903.699919	12807.991225	62.652366
1903.229098	12744.069916	62.657370
1902.243213	12680.410567	62.662375
1901.735185	12614.783834	62.667380
1901.296143	12548.319601	62.672385
1900.199089	12481.979847	62.677390
1899.815904	12412.714953	62.682394
1898.971570	12352.606156	62.687399
1898.645956	12277.316750	62.692404
1897.732900	12220.161277	62.697409
1897.032224	12147.274984	62.702414
1896.338004	12079.602937	62.707418
1895.753390	12021.998154	62.712423
1895.235624	11958.049522	62.717428
1894.417407	11887.770846	62.722433
1893.614768	11824.500081	62.727438
1892.856311	11764.872383	62.732442
1892.101165	11689.616593	62.737447
1891.821059	11631.592887	62.742452
1890.958409	11573.708243	62.747457
1890.538809	11509.697386	62.752462
1889.997519	11446.448060	62.757466
1888.829782	11389.291962	62.762471
1888.684575	11318.624417	62.767476
1887.672156	11251.615751	62.772481
1887.280485	11194.019187	62.777486
1886.619677	11132.636192	62.782490
1885.884926	11058.387157	62.787495
1885.294688	10996.885406	62.792500
1884.362552	10930.059530	62.797505
1883.509425	10869.062031	62.802510
1883.179653	10805.758129	62.807514
1882.278280	10754.171161	62.812519
1881.540809	10679.707822	62.817524
1881.290964	10632.703217	62.822529
1880.460362	10560.714712	62.827534
1879.917405	10503.803251	62.832538
1879.034058	10434.931754	62.837543
1878.630486	10375.424807	62.842548
1877.759079	10312.829533	62.847553
1877.384731	10247.144282	62.852558
1876.856005	10186.800865	62.857562
1875.959664	10115.167359	62.862567
1875.443809	10047.197162	62.867572
1874.529648	9984.467622	62.872577
1873.792542	9913.266241	62.877582
1873.071521	9850.174031	62.882586
1872.420598	9793.282391	62.887591
1872.072380	9727.997248	62.892596
1871.353884	9677.953467	62.897601
1870.493622	9612.285399	62.902606
1870.143160	9550.408263	62.907610
1869.283659	9486.720992	62.912615
1868.797986	9416.149922	62.917620
1868.158702	9361.639617	62.922625
1867.243453	9287.522633	62.927630
1866.863837	9221.125508	62.932634
1866.240903	9153.097449	62.937639
1865.796546	9080.515830	62.942644
1864.728068	9016.913434	62.947649
1864.154906	8956.539203	62.952654
1863.676603	8881.701196	62.957658
1862.723512	8818.136551	62.962663
1861.905173	8764.590962	62.967668
1861.233915	8697.384076	62.972673
1860.785484	8629.129900	62.977678
1859.991813	8561.330444	62.982682
1858.881730	8502.142675	62.987687
1858.575101	8435.094454	62.992692
1857.734774	8383.060189	62.997697
1857.166894	8319.724461	63.002702
1857.201537	8258.854186	63.007706
1856.186652	8197.203296	63.012711
1855.483008	8127.287066	63.017716
1854.803881	8065.811407	63.022721
1854.073967	7998.246971	63.027726
1853.282606	7938.873165	63.032730
1852.533851	7881.760930	63.037735
1852.046018	7812.064754	63.042740
1851.396582	7758.076652	63.047745
1850.646445	7702.451605	63.052750
1850.379583	7635.746579	63.057754
1849.509386	7572.231659	63.062759
1848.821244	7513.848199	63.067764
1848.118581	7446.253138	63.072769
1847.396838	7382.599490	63.077774
1846.848332	7317.451303	63.082778
1846.048294	7258.804979	63.087783
1845.575999	7193.075669	63.092788
1844.712991	7131.827902	63.097793
1843.834684	7073.164759	63.102798
1843.397909	7016.689457	63.107802
1842.873649	6954.165906	63.112807
1842.296155	6889.265976	63.117812
1841.693702	6829.097466	63.122817
1841.007583	6771.458111	63.127822
1840.133376	6705.995919	63.132826
1839.132638	6651.828189	63.137831
1838.805769	6589.303228	63.142836
1838.062341	6531.738587	63.147841
1837.408620	6473.737112	63.152846
1837.104218	6414.012032	63.157850
1836.302877	6348.065763	63.162855
1835.790442	6274.537535	63.167860
1835.126331	6212.942502	63.172865
1834.462249	6153.806449	63.177870
1833.647030	6085.188687	63.182874
1832.828656	6029.476607	63.187879
1832.263533	5960.885181	63.192884
1831.685490	5906.253926	63.197889
1830.699619	5852.757235	63.202894
1830.375256	5791.463389	63.207898
1829.492758	5737.425365	63.212903
1828.972020	5669.027017	63.217908
1828.244785	5614.482052	63.222913
1827.271046	5553.879150	63.227918
1827.138444	5497.328985	63.232922
1826.109681	5438.954123	63.237927
1825.491234	5377.540673	63.242932
1824.915602	5313.060259	63.247937
1824.010041	5255.941208	63.252942
1823.555143	5188.949667	63.257946
1822.754423	5141.541421	63.262951
1822.315162	5072.713270	63.267956
1821.524348	5020.295245	63.272961
1820.535959	4963.237803	63.277966
1820.234673	4899.480718	63.282970
1819.240099	4855.554147	63.287975
1819.134096	4783.687454	63.292980
1818.449430	4726.525123	63.297985
1817.403435	4671.890701	63.302990
1817.083058	4616.472421	63.307994
1816.355509	4561.254664	63.312999
1815.904385	4491.084746	63.318004
1815.110050	4429.703164	63.323009
1814.241397	4374.193813	63.328014
1813.510840	4309.824404	63.333018
1812.510600	4259.578966	63.338023
1812.118038	4193.704378	63.343028
1811.410538	4143.107625	63.348033
1811.060367	4089.160683	63.353038
1810.484718	4034.168434	63.358042
1809.733381	3975.726135	63.363047
1809.152435	3912.540624	63.368052
1808.362796	3864.704890	63.373057
1807.757906	3803.477237	63.378062
1807.110626	3741.567260	63.383066
1806.059888	3681.147543	63.388071
1805.389277	3625.887975	63.393076
1804.766267	3571.539862	63.398081
1804.067206	3519.450165	63.403086
1803.753592	3458.830717	63.408090
1802.932993	3405.524089	63.413095
1802.649126	3349.771171	63.418100
1802.057647	3288.236745	63.423105
1801.335573	3226.724102	63.428110
1800.612208	3168.422531	63.433114
1799.630260	3116.198584	63.438119
1799.264814	3052.367404	63.443124
1798.580151	2995.984673	63.448129
1797.764619	2938.171839	63.453134
1797.217692	2885.936418	63.458138
1796.291918	2834.144617	63.463143
1795.977338	2764.409198	63.468148
1794.661603	2718.058202	63.473153
1793.977954	2667.040045	63.478158
1793.771516	2611.335206	63.483162
1792.915965	2556.158719	63.488167
1792.395064	2495.103782	63.493172
1791.847218	2436.807220	63.498177
1791.058503	2384.608827	63.503182
1790.282092	2334.371514	63.508186
1789.500683	2281.727554	63.513191
1788.527060	2212.022922	63.518196
1787.736295	2173.569374	63.523201
1787.184222	2126.076181	63.528206
1787.087949	2072.598668	63.533210
1786.332941	2023.668093	63.538215
1785.594562	1970.142298	63.543220
1784.902712	1932.246195	63.548225
1784.108948	1877.152363	63.553230
1784.085161	1823.064927	63.558234
1783.158296	1774.313098	63.563239
1782.482282	1718.683069	63.568244
1781.496813	1670.751550	63.573249
1780.799031	1616.289302	63.578254
1780.474795	1560.622152	63.583258
1779.612074	1520.185104	63.588263
1778.627955	1454.639131	63.593268
1778.085033	1407.067970	63.598273
1777.312288	1353.263651	63.603278
1776.924623	1311.965554	63.608282
1775.990699	1272.113783	63.613287
1775.678262	1225.421334	63.618292
1774.975120	1171.015225	63.623297
1774.261362	1121.467642	63.628302
1773.876379	1063.640388	63.633306
1773.060801	1019.233258	63.638311
1772.516361	974.622345	63.643316
1771.618722	918.528271	63.648321
1770.917092	869.353387	63.653326
1770.392014	819.756368	63.658330
1769.341140	776.833505	63.663335
1768.965205	719.047186	63.668340
1768.374648	673.200236	63.673345
1767.297002	627.186342	63.678350
1766.699317	580.295244	63.683354
1766.184544	543.189178	63.688359
1765.448933	495.000290	63.693364
1764.657558	442.081493	63.698369
1763.739513	409.498028	63.703374
1763.444306	357.338139	63.708378
1762.366904	319.748753	63.713383
1761.763246	280.069620	63.718388
1761.330268	248.846129	63.723393
1760.158991	210.006401	63.728398
1759.753793	161.034431	63.733402
1759.257208	131.352544	63.738407
1758.762640	92.378858	63.743412
1757.764600	50.656147	63.748417
1756.677119	32.775737	63.753422
1755.721277	-4.227341	63.758426
1754.095678	2.094287	63.763431
1749.887879	83.126514	63.768436
1749.632362	85.054769	63.773441
1749.887050	95.088074	63.778446
1750.539553	74.504324	63.783450
1750.508399	83.384517	63.788455
1750.289453	72.951376	63.793460
1749.741983	76.122917	63.798465
1748.447461	76.298576	63.803470
1747.635747	81.174214	63.808474
1746.629469	93.230755	63.813479
1746.323875	85.566342	63.818484
1746.017945	84.028530	63.823489
1744.826035	90.995693	63.828494
1744.637406	82.055858	63.833498
1743.886331	90.541025	63.838503
1743.370959	88.164407	63.843508
1743.133015	81.577366	63.848513
1741.875178	95.511035	63.853518
1741.141933	81.370097	63.858522
1740.097831	92.782933	63.863527
1740.117069	83.959898	63.868532
1740.005716	88.334800	63.873537
1738.841147	96.373123	63.878542
1738.261406	89.862439	63.883546
1737.534007	88.727458	63.888551
1736.814742	90.246810	63.893556
1736.080770	86.603908	63.898561
1734.991389	93.687259	63.903566
1734.511050	82.571796	63.908570
1734.150815	87.243271	63.913575
1733.920474	87.249928	63.918580
1733.370848	80.682427	63.923585
1732.495868	86.719308	63.928590
1732.078491	80.657513	63.933594
1730.961191	90.162798	63.938599
1730.193127	87.689119	63.943604
1729.709877	90.990818	63.948609
1728.852750	89.349734	63.953614
1728.062175	86.691970	63.958618
1727.212080	91.878068	63.963623
1726.591297	84.618537	63.968628
1726.157333	86.871606	63.973633
1725.571433	91.642002	63.978638
1725.723082	82.438389	63.983642
1724.503175	87.164395	63.988647
1723.074626	81.782021	63.993652
1723.107691	78.829444	63.998657
1722.600025	90.466173	64.003662
1721.895761	84.964036	64.008666
1721.250499	89.253421	64.013671
1720.481260	88.016279	64.018676
1720.014427	72.106260	64.023681
1719.091678	87.640955	64.028686
1718.852101	81.095178	64.033690
1717.758946	92.222494	64.038695
1716.922482	88.075474	64.043700
1716.453472	76.729560	64.048705
1715.647529	85.608225	64.053710
1715.034210	74.600628	64.058714
1714.325110	72.116015	64.063719
1713.637288	85.427713	64.068724
1713.184254	82.326833	64.073729
1712.426186	92.298626	64.078734
1712.539459	78.220377	64.083738
1711.483652	88.345113	64.088743
1710.667939	78.386809	64.093748
1709.832963	79.533456	64.098753
1708.999698	86.826874	64.103758
1708.693875	80.258504	64.108762
1708.189093	81.363747	64.113767
1707.148038	78.540769	64.118772
1706.792005	82.561864	64.123777
1706.133347	82.300657	64.128782
1705.102458	84.057172	64.133786
1705.241429	79.061364	64.138791
1704.198968	82.144374	64.143796
1703.558684	77.139869	64.148801
1702.681823	88.171331	64.153806
1702.149031	83.099288	64.158810
1701.208257	93.060678	64.163815
1700.520102	91.999901	64.168820
1700.287579	85.416734	64.173825
1699.578262	90.231968	64.178830
1698.914940	86.486392	64.183834
1698.395745	85.157502	64.188839
1697.281347	85.045954	64.193844
1697.027977	75.130806	64.198849
1696.074194	82.400789	64.203854
1695.906085	81.763622	64.208858
1695.058536	84.626441	64.213863
1694.430244	77.106339	64.218868
1694.109414	82.720894	64.223873
1692.888670	92.239470	64.228878
1692.023115	76.260321	64.233882
1691.160672	84.886187	64.238887
1691.123629	89.608836	64.243892
1690.944464	81.408685	64.248897
1689.257162	84.412770	64.253902
1688.662875	82.785147	64.258906
1687.753456	89.027787	64.263911
1688.037895	84.371576	64.268916
1687.356263	77.265231	64.273921
1686.169064	94.043595	64.278926
1685.509531	82.779988	64.283930
1684.733349	85.492701	64.288935
1684.179756	90.210663	64.293940
1683.697677	87.606417	64.298945
1682.901471	86.373570	64.303950
1682.540336	83.873119	64.308954
1682.062703	81.399058	64.313959
1681.317482	82.130906	64.318964
1680.877299	83.411976	64.323969
1680.128355	87.922844	64.328974
1679.369462	80.697883	64.333978
1678.095837	88.212644	64.338983
1677.093395	88.330907	64.343988
1677.530492	81.827467	64.348993
1676.558551	88.119465	64.353998
1675.765481	81.573301	64.359002
1674.894166	87.574923	64.364007
1674.255455	81.633453	64.369012
1673.822887	78.893613	64.374017
1672.796740	80.051713	64.379022
1672.442777	76.700138	64.384026
1671.928846	85.623893	64.389031
1671.215469	80.590005	64.394036
1671.130067	77.526936	64.399041
1670.369268	83.239763	64.404046
1669.803497	81.550844	64.409050
1668.414124	83.111998	64.414055
1667.559919	83.834354	64.419060
1666.944132	78.753427	64.424065
1666.182583	88.129683	64.429070
1666.198450	80.038908	64.434074
1665.496766	83.520394	64.439079
1664.626931	84.256271	64.444084
1664.236944	73.162756	64.449089
1663.520748	86.176189	64.454094
1662.996985	81.362923	64.459098
1662.588083	84.592896	64.464103
1661.295887	84.306177	64.469108
1660.326696	80.984518	64.474113
1659.379696	92.063404	64.479118
1658.972905	76.522338	64.484122
1658.643886	87.181355	64.489127
1658.084965	86.405994	64.494132
1657.909364	85.963987	64.499137
1656.576992	79.274836	64.504142
1656.399133	80.384929	64.509146
1655.748496	80.792674	64.514151
1655.042698	86.843704	64.519156
1654.070016	81.395266	64.524161
1652.875847	85.454885	64.529166
1652.535277	83.706542	64.534170
1652.011840	80.955908	64.539175
1651.519823	86.089875	64.544180
1650.917324	85.919110	64.549185
1650.437184	89.898425	64.554190
1649.927315	89.045887	64.559194
1649.606979	84.708095	64.564199
1648.278080	85.343433	64.569204
1647.359526	73.392432	64.574209
1646.397138	76.740289	64.579214
1645.921671	84.885221	64.584218
1645.524150	84.661396	64.589223
1644.839481	86.831297	64.594228
1644.488281	80.643890	64.599233
1643.893588	93.628569	64.604238
1643.238089	80.292197	64.609242
1641.620588	76.892181	64.614247
1641.188911	87.289958	64.619252
1641.371471	78.502493	64.624257
1640.178946	87.089342	64.629262
1639.736365	85.961186	64.634266
1639.062844	89.360933	64.639271
1638.482102	87.475700	64.644276
1638.173404	75.519289	64.649281
1637.180696	83.754271	64.654286
1636.190490	83.220893	64.659290
1635.348536	86.869750	64.664295
1634.690339	76.432289	64.669300
1634.377922	77.604759	64.674305
1633.666956	86.034687	64.679310
1633.498082	73.575090	64.684314
1632.588419	72.609445	64.689319
1631.725364	80.831716	64.694324
1631.210794	76.605210	64.699329
1629.947569	86.463294	64.704334
1629.665287	76.901263	64.709338
1629.241818	84.268373	64.714343
1628.675709	85.208329	64.719348
1628.469612	74.921405	64.724353
1626.561742	77.854910	64.729358
1625.660424	76.780708	64.734362
1625.629551	80.283372	64.739367
1625.415054	87.718214	64.744372
1624.590443	68.301113	64.749377
1623.397786	83.531764	64.754382
1623.198896	78.545474	64.759386
1622.861620	75.654886	64.764391
1622.296248	81.749845	64.769396
1621.422094	81.324195	64.774401
1620.266878	80.383370	64.779406
1619.629494	73.426140	64.784410
1619.337685	80.201470	64.789415
1618.593578	81.609680	64.794420
1618.293399	68.030800	64.799425
1617.445098	87.065598	64.804430
1616.407731	78.408855	64.809434
1615.606486	78.521987	64.814439
1614.699267	79.013081	64.819444
1614.451229	69.973903	64.824449
1613.727398	74.980693	64.829454
1613.388956	73.268289	64.834458
1612.813776	81.189363	64.839463
1612.544159	83.657615	64.844468
1611.471075	75.566375	64.849473
1610.375987	85.244788	64.854478
1609.815056	74.088556	64.859482
1609.348517	78.860506	64.864487
1608.574720	77.961596	64.869492
1608.481161	80.458650	64.874497
1607.284533	80.716600	64.879502
1606.332589	76.127494	64.884506
1605.623214	79.862529	64.889511
1604.786685	84.912460	64.894516
1604.618178	73.820045	64.899521
1603.937057	83.998826	64.904526
1603.871071	81.497232	64.909530
1603.074855	84.069644	64.914535
1602.146514	83.028128	64.919540
1601.252988	82.223936	64.924545
1600.054116	95.944855	64.929550
1600.033032	85.869814	64.934554
1599.265669	79.037318	64.939559
1599.057279	80.393541	64.944564
1598.971915	76.092548	64.949569
1597.519562	84.995083	64.954574
1596.532934	80.080326	64.959578
1595.893341	81.617019	64.964583
1595.217554	83.153155	64.969588
1594.939266	74.501988	64.974593
1594.385612	88.561948	64.979598
1594.273912	78.048718	64.984602
1593.030806	79.105698	64.989607
1591.804685	84.980780	64.994612
1591.336764	71.370206	64.999617
1590.607443	80.509537	65.004622
1590.096048	88.524563	65.009626
1589.958528	72.890282	65.014631
1588.642845	77.398166	65.019636
1587.758826	76.650816	65.024641
1587.077113	85.353651	65.029646
1587.033960	81.299844	65.034650
1586.189809	76.871818	65.039655
1585.907700	79.646412	65.044660
1585.850966	79.343223	65.049665
1584.805343	86.660947	65.054670
1583.839211	83.854503	65.059674
1582.903031	84.285554	65.064679
1581.868120	88.491790	65.069684
1581.628798	83.160263	65.074689
1580.491415	79.991517	65.079694
1579.792349	77.025950	65.084698
1579.319061	72.229921	65.089703
1578.700668	84.761042	65.094708
1578.453544	75.056241	65.099713
1577.748340	81.405237	65.104718
1577.698558	75.557892	65.109722
1576.827207	78.153287	65.114727
1575.723251	84.843185	65.119732
1574.897450	75.771223	65.124737
1574.285146	80.974773	65.129742
1573.740234	85.024313	65.134746
1573.106209	86.380352	65.139751
1571.590654	92.359779	65.144756
1571.394325	79.865127	65.149761
1570.640672	88.636168	65.154766
1570.735475	84.316012	65.159770
1570.178668	89.583288	65.164775
1569.198355	94.082058	65.169780
1568.958148	82.023313	65.174785
1567.785266	86.060662	65.179790
1567.045013	81.411128	65.184794
1566.469115	82.601814	65.189799
1565.716930	82.333425	65.194804
1565.520636	85.999568	65.199809
1563.855483	84.475883	65.204814
1563.119374	77.941213	65.209818
1563.061882	76.930086	65.214823
1562.478703	82.322978	65.219828
1562.096888	79.215546	65.224833
1561.314882	84.911268	65.229838
1560.984078	82.406018	65.234842
1560.025285	79.317718	65.239847
1559.068957	81.850926	65.244852
1558.480437	77.289254	65.249857
1557.912012	90.886360	65.254862
1557.680540	78.706382	65.259866
1556.546146	78.153366	65.264871
1555.327357	85.855008	65.269876
1554.897455	79.621776	65.274881
1554.447185	84.313879	65.279886
1554.125212	80.914662	65.284890
1553.666022	81.679949	65.289895
1552.567343	88.742760	65.294900
1551.847663	82.326909	65.299905
1551.131453	81.250130	65.304910
1550.583504	82.557805	65.309914
1550.055165	89.047444	65.314919
1549.563739	80.731349	65.319924
1548.865239	81.498389	65.324929
1547.806251	82.060930	65.329934
1547.068430	77.623909	65.334938
1546.591309	78.800481	65.339943
1546.212419	91.263594	65.344948
1545.798941	77.633340	65.349953
1544.616799	82.282455	65.354958
1543.821616	81.297075	65.359962
1543.229631	85.197980	65.364967
1542.466280	83.343362	65.369972
1542.532923	78.051539	65.374977
1541.378995	86.717447	65.379982
1540.339737	85.505918	65.384986
1539.871983	82.492570	65.389991
1539.324825	86.405277	65.394996
1538.989944	80.186913	65.400001
1538.372695	86.263321	65.405006
1537.341699	77.550411	65.410010
1536.224602	79.691274	65.415015
1535.690973	80.569318	65.420020
1535.468902	74.139066	65.425025
1534.700781	82.690056	65.430030
1534.356431	78.376602	65.435034
1534.027883	84.385059	65.440039
1532.559090	92.405561	65.445044
1531.981375	74.754902	65.450049
1531.424499	81.600739	65.455054
1530.908839	78.330075	65.460058
1530.869336	81.231706	65.465063
1529.381535	79.478012	65.470068
1528.872067	69.950528	65.475073
1528.071590	77.120502	65.480078
1527.638365	76.049229	65.485082
1527.128360	76.690128	65.490087
1525.547197	80.029113	65.495092
1525.186895	69.394551	65.500097
1524.734156	74.853453	65.505102
1523.783746	79.990886	65.510106
1523.784587	67.242573	65.515111
1522.854261	72.480892	65.520116
1522.939233	71.797216	65.525121
1521.522393	73.533123	65.530126
1520.713632	72.759645	65.535130
1520.326692	74.473831	65.540135
1519.820822	70.758487	65.545140
1518.862074	68.644765	65.550145
1517.720521	82.520595	65.555150
1517.030294	72.859408	65.560154
1516.678535	77.345046	65.565159
1515.931478	71.573812	65.570164
1515.661136	65.449284	65.575169
1515.043441	75.466606	65.580174
1514.966469	68.496058	65.585178
1514.451136	60.461329	65.590183
1513.072215	74.010590	65.595188
1512.859003	69.783539	65.600193
1511.466877	76.580747	65.605198
1510.373104	84.175807	65.610202
1509.874783	74.059922	65.615207
1509.423378	78.193962	65.620212
1509.226885	68.574174	65.625217
1508.362944	78.015610	65.630222
1508.071689	77.439027	65.635226
1507.532912	71.328768	65.640231
1506.293977	81.536276	65.645236
1505.824286	76.022171	65.650241
1505.197602	87.266235	65.655246
1504.697443	77.470767	65.660250
1503.508124	64.857964	65.665255
1502.714315	72.728633	65.670260
1502.311939	65.516479	65.675265
1501.725660	75.356921	65.680270
1501.121390	76.336084	65.685274
1500.911697	73.032577	65.690279
1500.032048	83.927326	65.695284
1499.226803	71.783350	65.700289
1498.793063	80.967192	65.705294
1497.766145	75.855453	65.710298
1496.904627	73.010344	65.715303
1496.033078	76.651325	65.720308
1495.630082	72.900716	65.725313
1495.158224	82.557399	65.730318
1494.612296	81.750047	65.735322
1494.349569	78.473892	65.740327
1493.029080	82.880082	65.745332
1492.350716	73.486680	65.750337
1491.663648	77.287584	65.755342
1490.975110	70.865233	65.760346
1491.009999	71.924181	65.765351
1489.664962	74.957578	65.770356
1489.280088	64.326934	65.775361
1488.417402	73.293504	65.780366
1488.073946	71.533031	65.785370
1487.723219	78.300381	65.790375
1486.880453	85.123847	65.795380
1485.992844	74.580972	65.800385
1485.218910	86.113368	65.805390
1484.709807	81.258394	65.810394
1483.914785	74.931815	65.815399
1482.723941	80.463863	65.820404
1482.301120	77.538006	65.825409
1481.574743	83.056170	65.830414
1481.243596	78.239152	65.835418
1481.225729	77.647512	65.840423
1480.307363	76.396297	65.845428
1479.642245	73.803838	65.850433
1478.645163	81.610625	65.855438
1477.862287	78.104891	65.860442
1477.594279	78.519684	65.865447
1476.969189	77.570374	65.870452
1476.024528	70.119546	65.875457
1475.214662	73.903696	65.880462
1474.630582	76.220079	65.885466
1474.382092	70.111008	65.890471
1473.028506	72.013508	65.895476
1472.494625	71.141169	65.900481
1471.789648	77.936431	65.905486
1471.514293	75.799280	65.910490
1471.016208	73.006814	65.915495
1470.442331	80.440416	65.920500
1469.259276	71.849480	65.925505
1468.643409	74.418499	65.930510
1467.945940	72.980795	65.935514
1467.723070	76.640124	65.940519
1466.951695	72.613745	65.945524
1466.027870	67.941383	65.950529
1465.276156	71.500250	65.955534
1464.533541	78.713083	65.960538
1464.317326	67.316042	65.965543
1463.707937	81.272896	65.970548
1462.913598	66.618250	65.975553
1461.973864	74.259804	65.980558
1461.551047	70.176457	65.985562
1461.414725	61.646267	65.990567
1460.018934	75.379582	65.995572
1459.151668	71.628645	66.000577
1458.510348	79.828334	66.005582
1457.690092	72.110159	66.010586
1457.451232	73.247304	66.015591
1456.798186	74.942286	66.020596
1457.005052	68.831815	66.025601
1455.747368	67.639266	66.030606
1454.649501	69.009122	66.035610
1454.179264	67.696161	66.040615
1453.685979	82.628055	66.045620
1453.324380	73.617992	66.050625
1452.057316	68.008273	66.055630
1451.636895	77.150574	66.060634
1451.206384	66.714851	66.065639
1450.474388	74.760213	66.070644
1449.416913	66.668156	66.075649
1448.437853	75.504998	66.080654
1447.969956	70.055279	66.085658
1447.847305	69.470831	66.090663
1447.288085	71.647649	66.095668
1446.681798	73.541785	66.100673
1445.899146	73.077998	66.105678
1445.236155	73.112440	66.110682
1444.673623	67.247252	66.115687
1443.384288	73.708030	66.120692
1442.698592	73.919547	66.125697
1442.233640	71.508179	66.130702
1441.774572	75.124622	66.135706
1441.435965	71.169823	66.140711
1440.343413	75.859934	66.145716
1439.681618	72.875871	66.150721
1439.044254	69.611957	66.155726
1438.354100	82.834168	66.160730
1438.038020	67.171535	66.165735
1436.791603	72.819665	66.170740
1435.675414	69.799010	66.175745
1435.500052	64.430539	66.180750
1434.831709	76.382974	66.185754
1434.806263	59.269081	66.190759
1433.833507	68.667898	66.195764
1433.484956	71.714838	66.200769
1432.423396	74.985487	66.205774
1431.847881	78.286122	66.210778
1431.625578	69.343816	66.215783
1430.804868	76.868691	66.220788
1429.467072	69.169705	66.225793
1428.644792	82.826081	66.230798
1428.091737	79.510921	66.235802
1428.210663	80.832481	66.240807
1427.273020	79.426652	66.245812
1426.832042	73.759768	66.250817
1425.964729	76.613190	66.255822
1424.987195	79.023656	66.260826
1424.569707	78.862965	66.265831
1423.946878	73.597149	66.270836
1422.859558	69.942702	66.275841
1422.304234	66.364553	66.280846
1421.586936	71.660509	66.285850
1421.579935	66.445054	66.290855
1420.826647	72.120470	66.295860
1420.245867	66.040568	66.300865
1419.173410	71.031846	66.305870
1418.211554	74.035916	66.310874
1418.398229	59.840395	66.315879
1417.213041	76.306253	66.320884
1416.291598	63.537386	66.325889
1415.552465	80.799685	66.330894
1414.936543	69.486682	66.335898
1414.861120	77.063419	66.340903
1414.388299	73.640893	66.345908
1413.854939	64.844227	66.350913
1412.546694	69.880868	66.355918
1411.789087	79.683899	66.360922
1411.414379	68.914460	66.365927
1410.811523	70.822251	66.370932
1410.187324	71.459245	66.375937
1409.198908	68.738419	66.380942
1408.802353	73.652235	66.385946
1408.479084	70.231174	66.390951
1407.049548	71.144405	66.395956
1406.316564	69.203004	66.400961
1405.812061	75.237855	66.405966
1405.378997	74.486703	66.410970
1405.182085	70.708087	66.415975
1403.797238	81.139099	66.420980
1403.148703	70.771155	66.425985
1402.638733	75.147907	66.430990
1401.830813	74.126751	66.435994
1402.013991	69.556010	66.440999
1400.790270	77.392532	66.446004
1400.005058	68.743132	66.451009
1399.114621	69.537565	66.456014
1398.835944	73.271999	66.461018
1398.592455	76.593984	66.466023
1397.881772	73.915750	66.471028
1396.796065	70.609568	66.476033
1396.243873	76.756081	66.481038
1395.408483	81.935197	66.486042
1394.947857	75.071371	66.491047
1393.667088	79.816649	66.496052
1393.379673	74.401334	66.501057
1393.151191	76.159736	66.506062
1392.508199	78.006102	66.511066
1391.892350	72.338637	66.516071
1390.589805	75.267557	66.521076
1390.188821	73.902599	66.526081
1389.560723	70.627764	66.531086
1388.971194	81.733466	66.536090
1388.003262	68.114129	66.541095
1386.939823	78.481443	66.546100
1386.870614	66.083333	66.551105
1386.453682	75.206159	66.556110
1385.662831	75.845995	66.561114
1385.278987	79.026285	66.566119
1384.141692	73.750792	66.571124
1383.502212	69.091615	66.576129
1382.795472	70.511295	66.581134
1382.412258	78.972747	66.586138
1381.918466	73.262229	66.591143
1380.822265	77.330041	66.596148
1380.134594	77.879359	66.601153
1379.886634	77.445721	66.606158
1379.112603	75.679587	66.611162
1378.045567	74.172919	66.616167
1377.514838	77.157360	66.621172
1376.631826	68.782137	66.626177
1376.086026	71.586045	66.631182
1375.700425	73.110800	66.636186
1375.445888	64.607297	66.641191
1374.412216	74.818492	66.646196
1373.783039	73.284803	66.651201
1373.327702	77.182940	66.656206
1372.168500	76.621334	66.661210
1371.497016	70.756137	66.666215
1370.942784	77.653615	66.671220
1370.215877	74.254140	66.676225
1369.841885	81.860990	66.681230
1369.409328	70.553549	66.686234
1368.673763	64.728504	66.691239
1367.678151	78.950184	66.696244
1367.200370	77.682594	66.701249
1366.612754	65.494626	66.706254
1365.392513	72.876441	66.711258
1364.611832	78.195102	66.716263
1364.058934	80.000345	66.721268
1363.924531	69.954395	66.726273
1363.140479	76.038420	66.731278
1362.847811	74.321931	66.736282
1361.889704	70.978136	66.741287
1360.983363	68.854569	66.746292
1360.615290	71.262795	66.751297
1360.149290	67.736695	66.756302
1358.853564	68.242326	66.761306
1358.796310	65.755129	66.766311
1357.690479	70.373263	66.771316
1357.122799	64.750195	66.776321
1356.853657	72.827655	66.781326
1355.847398	72.194436	66.786330
1355.100454	68.164213	66.791335
1354.554295	79.725075	66.796340
1354.085161	71.645195	66.801345
1353.030150	75.846819	66.806350
1352.132909	71.220741	66.811354
1351.662573	66.842195	66.816359
1350.918660	75.050321	66.821364
1350.801427	73.851577	66.826369
1350.382223	72.265593	66.831374
1349.339606	80.128542	66.836378
1348.698481	71.981386	66.841383
1347.761774	70.578594	66.846388
1347.638876	70.500396	66.851393
1346.678415	67.770422	66.856398
1345.650124	72.010378	66.861402
1345.400056	62.419643	66.866407
1344.832467	64.198837	66.871412
1344.326978	70.812597	66.876417
1343.237972	67.529043	66.881422
1342.731786	72.718916	66.886426
1342.475734	57.893610	66.891431
1341.111116	66.596224	66.896436
1340.171939	72.744337	66.901441
1339.733440	69.958197	66.906446
1339.019809	75.305629	66.911450
1338.859435	67.943078	66.916455
1338.250488	70.214554	66.921460
1337.417516	69.137477	66.926465
1336.700127	74.597471	66.931470
1335.914854	74.048979	66.936474
1335.823351	66.233930	66.941479
1334.816203	72.774476	66.946484
1333.983553	66.884450	66.951489
1333.400860	66.735843	66.956494
1332.437841	75.492896	66.961498
1332.560299	66.363338	66.966503
1331.379126	74.715098	66.971508
1330.801459	72.564523	66.976513
1330.631514	62.300305	66.981518
1329.583460	70.533129	66.986522
1328.594619	71.176071	66.991527
1327.867756	74.885564	66.996532
1327.504724	75.383288	67.001537
1327.161722	69.795472	67.006542
1326.164896	73.230912	67.011546
1325.449545	59.516268	67.016551
1324.352091	70.497711	67.021556
1324.415152	75.463050	67.026561
1323.827058	67.383169	67.031566
1322.663538	72.735891	67.036570
1321.979295	63.545345	67.041575
1321.514236	68.739720	67.046580
1320.789661	70.903425	67.051585
1320.705239	70.413832	67.056590
1319.393675	75.559856	67.061594
1318.620345	65.147132	67.066599
1318.106735	79.230696	67.071604
1317.705000	67.497322	67.076609
1317.195230	71.412004	67.081614
1315.829787	75.513182	67.086618
1315.247847	68.116728	67.091623
1314.641326	70.599137	67.096628
1314.108041	65.997216	67.101633
1314.030309	72.793715	67.106638
1313.157502	68.222116	67.111642
1312.491444	70.734491	67.116647
1311.449557	70.449155	67.121652
1311.131077	63.220557	67.126657
1310.581326	60.573538	67.131662
1309.246667	72.242407	67.136666
1308.913366	63.220002	67.141671
1308.080016	72.306531	67.146676
1307.853383	72.093438	67.151681
1307.474037	72.508602	67.156686
1306.019690	71.511398	67.161690
1305.625896	71.433692	67.166695
1305.033042	78.149660	67.171700
1304.622020	69.970669	67.176705
1303.632562	72.435113	67.181710
1302.772161	75.908797	67.186714
1302.263498	70.142318	67.191719
1301.898339	72.097498	67.196724
1301.421680	68.845921	67.201729
1300.391737	65.515150	67.206734
1299.592523	77.687107	67.211738
1299.322143	62.925587	67.216743
1298.459787	70.023446	67.221748
1297.306160	63.189402	67.226753
1296.853398	66.044764	67.231758
1296.242306	79.304882	67.236762
1296.251198	74.899042	67.241767
1295.689591	75.377877	67.246772
1294.564263	65.505254	67.251777
1294.256347	63.474231	67.256782
1293.230946	68.888584	67.261786
1292.356662	62.396487	67.266791
1291.476003	69.926192	67.271796
1290.957377	74.963508	67.276801
1290.843398	72.643028	67.281806
1289.892415	78.526529	67.286810
1288.893447	65.703817	67.291815
1288.314857	69.571096	67.296820
1287.864972	67.488527	67.301825
1287.739109	62.654681	67.306830
1286.120741	77.894760	67.311834
1285.934764	62.777623	67.316839
1285.255895	68.103768	67.321844
1284.692516	63.249595	67.326849
1284.221720	65.505426	67.331854
1282.835248	73.345790	67.336858
1282.336076	67.612501	67.341863
1281.806790	75.171502	67.346868
1281.373381	74.898247	67.351873
1280.860040	63.900151	67.356878
1279.547413	73.703135	67.361882
1279.317442	67.423994	67.366887
1278.605119	76.226360	67.371892
1277.808810	76.099113	67.376897
1277.729085	67.910035	67.381902
1276.622585	68.283118	67.386906
1276.132625	67.280836	67.391911
1275.612230	67.622235	67.396916
1274.446022	67.698882	67.401921
1273.686749	64.970066	67.406926
1272.794607	75.770651	67.411930
1272.935164	68.992625	67.416935
1272.365978	71.145830	67.421940
1271.316970	74.636895	67.426945
1270.509161	69.610274	67.431950
1269.941049	75.125397	67.436954
1269.479112	68.387972	67.441959
1268.886364	69.575090	67.446964
1267.725313	59.433774	67.451969
1267.264644	55.137292	67.456974
1266.637872	62.498899	67.461978
1266.541710	58.705861	67.466983
1265.276840	69.102077	67.471988
1264.097559	65.487558	67.476993
1263.816496	57.070301	67.481998
1263.043626	67.568064	67.487002
1263.235024	66.441680	67.492007
1262.552000	70.767119	67.497012
1261.506068	77.790100	67.502017
1260.829859	69.315814	67.507022
1260.165156	73.258293	67.512026
1259.775373	55.483274	67.517031
1258.821596	66.538084	67.522036
1257.910665	71.131575	67.527041
1257.749409	62.140175	67.532046
1257.046770	69.490195	67.537050
1255.946132	64.956421	67.542055
1255.128512	69.956125	67.547060
1254.528595	69.040717	67.552065
1254.640986	63.254353	67.557070
1253.789369	71.279347	67.562074
1252.673967	64.906029	67.567079
1251.955543	63.258831	67.572084
1251.379708	65.045663	67.577089
1251.033706	63.042779	67.582094
1250.171734	68.137846	67.587098
1249.401571	62.212688	67.592103
1248.752426	65.666989	67.597108
1248.419177	69.220874	67.602113
1248.074320	62.385993	67.607118
1246.606207	70.740828	67.612122
1246.315674	66.157097	67.617127
1245.530636	64.149905	67.622132
1245.109150	73.336542	67.627137
1244.205370	71.578467	67.632142
1242.977459	75.392882	67.637146
1242.909250	64.085898	67.642151
1242.565617	71.582266	67.647156
1241.830346	71.913683	67.652161
1241.009770	64.730242	67.657166
1239.946453	72.225927	67.662170
1240.054362	61.401877	67.667175
1239.511020	62.521221	67.672180
1238.242772	67.209380	67.677185
1237.815556	65.839158	67.682190
1236.859524	69.343836	67.687194
1236.553782	66.697460	67.692199
1235.484697	71.793925	67.697204
1234.498378	71.479284	67.702209
1233.935257	67.164405	67.707214
1233.531046	77.581483	67.712218
1233.460676	75.153147	67.717223
1232.703722	71.110364	67.722228
1231.326034	82.568492	67.727233
1230.956371	76.707385	67.732238
1230.305089	63.012554	67.737242
1230.140681	67.550426	67.742247
1229.156246	69.411697	67.747252
1228.056187	78.009220	67.752257
1227.851506	64.000522	67.757262
1227.188630	72.247826	67.762266
1226.472470	63.016659	67.767271
1225.424256	70.793799	67.772276
1225.032177	73.432941	67.777281
1224.520891	69.582910	67.782286
1223.938385	73.565943	67.787290
1223.319023	68.747496	67.792295
1222.180081	72.301766	67.797300
1221.815570	68.614478	67.802305
1221.528355	55.975102	67.807310
1220.615143	70.603178	67.812314
1219.713128	64.546031	67.817319
1218.612494	70.396576	67.822324
1218.092360	72.529376	67.827329
1218.118702	64.058510	67.832334
1217.612420	66.961818	67.837338
1216.668602	65.221160	67.842343
1215.618394	72.400953	67.847348
1215.140195	70.062701	67.852353
1215.043155	64.547762	67.857358
1213.780861	71.736048	67.862362
1212.744628	70.207207	67.867367
1212.440573	67.570027	67.872372
1212.193146	64.289904	67.877377
1211.872758	62.782850	67.882382
1210.376026	71.561727	67.887386
1209.834805	70.883002	67.892391
1209.206491	67.912606	67.897396
1208.725577	72.828818	67.902401
1207.796088	63.764046	67.907406
1207.153516	69.358827	67.912410
1206.793319	67.897528	67.917415
1206.242151	70.503622	67.922420
1205.006598	78.938196	67.927425
1204.309658	69.347583	67.932430
1203.499739	78.670112	67.937434
1203.148968	71.642209	67.942439
1203.085595	72.929665	67.947444
1202.359431	73.448881	67.952449
1201.546385	65.773822	67.957454
1200.849792	76.193241	67.962458
1200.143334	71.734005	67.967463
1199.154155	71.777804	67.972468
1198.384249	72.725026	67.977473
1198.146426	72.953696	67.982478
1197.482893	81.163267	67.987482
1197.084014	69.363241	67.992487
1195.871051	58.607320	67.997492
1195.365093	65.492409	68.002497
1194.971035	62.554153	68.007502
1194.191763	65.918771	68.012506
1193.373754	68.321296	68.017511
1192.354749	68.882353	68.022516
1191.877069	70.849133	68.027521
1191.821582	70.761800	68.032526
1190.858467	74.906292	68.037530
1189.995063	68.434582	68.042535
1189.434471	69.260211	68.047540
1188.650915	68.597951	68.052545
1188.648973	61.957710	68.057550
1187.506130	78.683407	68.062554
1186.398226	72.315235	68.067559
1186.069585	74.080117	68.072564
1185.666492	77.414880	68.077569
1184.992644	70.892526	68.082574
1183.890707	72.912851	68.087578
1182.841643	66.921681	68.092583
1182.581780	74.485157	68.097588
1182.347685	75.941690	68.102593
1181.944050	68.305608	68.107598
1180.634557	78.480300	68.112602
1180.211086	67.972570	68.117607
1179.611143	73.172645	68.122612
1179.123979	75.282862	68.127617
1178.555871	67.056346	68.132622
1177.360778	72.967661	68.137626
1176.827223	70.188787	68.142631
1176.459708	68.747580	68.147636
1175.560761	68.415913	68.152641
1174.853277	67.568094	68.157646
1173.926536	69.595253	68.162650
1173.914845	64.057283	68.167655
1173.279575	62.549848	68.172660
1172.025226	72.561228	68.177665
1171.545090	67.790041	68.182670
1170.966787	75.057229	68.187674
1170.463741	68.963459	68.192679
1169.777779	69.722297	68.197684
1168.612541	72.763527	68.202689
1168.029661	73.313583	68.207694
1167.835904	80.174262	68.212698
1167.313896	64.926087	68.217703
1166.173574	73.121599	68.222708
1165.367149	66.297061	68.227713
1165.105562	66.578399	68.232718
1164.574556	76.162507	68.237722
1163.895301	68.045136	68.242727
1163.317461	69.065902	68.247732
1162.299734	79.826563	68.252737
1161.912495	65.455825	68.257742
1160.861593	67.471196	68.262746
1159.983314	68.905599	68.267751
1159.386018	75.198092	68.272756
1158.599950	73.003433	68.277761
1158.579949	70.117657	68.282766
1158.398173	70.649656	68.287770
1157.177494	73.338584	68.292775
1156.552955	71.840485	68.297780
1155.948249	76.334844	68.302785
1155.225492	70.197173	68.307790
1154.204364	74.395058	68.312794
1153.673842	69.018450	68.317799
1153.574492	68.933363	68.322804
1152.556841	70.366281	68.327809
1151.952212	65.449318	68.332814
1151.332990	73.326991	68.337818
1150.585877	67.473896	68.342823
1149.593761	66.284997	68.347828
1148.678940	68.520005	68.352833
1148.230742	65.804834	68.357838
1147.593196	72.270887	68.362842
1147.294613	70.878646	68.367847
1147.021884	66.348871	68.372852
1145.879106	80.377966	68.377857
1145.374661	65.981719	68.382862
1144.778207	74.197974	68.387866
1143.707904	68.525593	68.392871
1143.033892	64.422342	68.397876
1142.238181	75.114578	68.402881
1141.849790	60.091173	68.407886
1141.307829	74.601874	68.412890
1140.847416	69.928483	68.417895
1139.739754	67.480626	68.422900
1139.414411	66.278724	68.427905
1138.960020	70.506325	68.432910
1137.825535	68.963180	68.437914
1136.758486	61.549322	68.442919
1136.231192	69.398182	68.447924
1135.688037	67.735757	68.452929
1135.439860	62.692721	68.457934
1135.138983	70.406222	68.462938
1134.093356	66.595468	68.467943
1133.654119	73.357992	68.472948
1132.718135	73.029077	68.477953
1132.077216	63.592013	68.482958
1131.159156	71.529834	68.487962
1130.457368	63.633681	68.492967
1130.208422	65.360662	68.497972
1129.525722	78.867151	68.502977
1128.762099	69.009628	68.507982
1127.550720	79.118274	68.512986
1127.012629	75.423917	68.517991
1126.767272	72.965071	68.522996
1126.158081	77.614692	68.528001
1125.689036	71.187517	68.533006
1124.588495	74.283132	68.538010
1124.261929	78.093012	68.543015
1123.734947	66.283422	68.548020
1122.403702	73.586794	68.553025
1121.993148	64.896841	68.558030
1121.386496	71.321715	68.563034
1121.085171	66.714490	68.568039
1120.277207	66.964463	68.573044
1119.376339	61.392882	68.578049
1118.895034	58.668792	68.583054
1118.402782	65.701521	68.588058
1117.395406	69.345294	68.593063
1116.354638	72.038740	68.598068
1115.890602	74.222561	68.603073
1115.559112	65.647768	68.608078
1115.175070	64.646018	68.613082
1114.014288	68.456119	68.618087
1113.422000	67.455953	68.623092
1112.730450	68.406507	68.628097
1112.388380	64.693594	68.633102
1111.516646	65.368454	68.638106
1110.867521	68.512121	68.643111
1110.200060	59.071404	68.648116
1109.503618	68.700750	68.653121
1109.434691	67.909079	68.658126
1107.940502	67.650037	68.663130
1107.357314	65.943524	68.668135
1106.856602	62.874014	68.673140
1106.465052	72.664604	68.678145
1105.846398	65.699836	68.683150
1105.057626	68.058312	68.688154
1104.470650	60.929234	68.693159
1103.476195	68.748325	68.698164
1102.496071	67.284723	68.703169
1102.326840	56.373883	68.708174
1101.492703	69.737297	68.713178
1101.090908	61.534817	68.718183
1100.634411	57.340213	68.723188
1099.573537	72.676202	68.728193
1099.007031	64.998239	68.733198
1098.208620	57.798718	68.738202
1097.763250	62.223584	68.743207
1096.898608	64.089503	68.748212
1096.005455	60.721295	68.753217
1095.616205	64.588453	68.758222
1095.098082	60.637041	68.763226
1094.523407	70.333756	68.768231
1093.741129	61.707672	68.773236
1092.971203	65.424070	68.778241
1092.672571	62.420191	68.783246
1091.788810	66.597823	68.788250
1090.793580	76.348822	68.793255
1090.226724	65.529611	68.798260
1089.626131	71.054658	68.803265
1089.323631	70.815806	68.808270
1087.877816	68.385492	68.813274
1087.393917	73.481969	68.818279
1087.326204	65.899711	68.823284
1086.384937	74.044665	68.828289
1086.151773	65.638743	68.833294
1085.264390	72.884143	68.838298
1084.475981	64.311076	68.843303
1084.240031	63.858212	68.848308
1082.627053	72.598871	68.853313
1082.139182	62.006799	68.858318
1081.276784	69.934202	68.863322
1081.073796	66.120322	68.868327
1080.826864	64.306711	68.873332
1080.300406	76.173544	68.878337
1079.169978	68.583711	68.883342
1078.597362	65.322217	68.888346
1078.123743	64.206989	68.893351
1076.970426	64.623876	68.898356
1076.209701	71.305079	68.903361
1076.031125	68.392491	68.908366
1075.166801	75.569572	68.913370
1074.655549	65.670351	68.918375
1073.805282	67.084557	68.923380
1072.936897	66.153552	68.928385
1072.474947	66.015761	68.933390
1072.039656	72.678314	68.938394
1071.548932	67.706984	68.943399
1070.661212	77.464542	68.948404
1069.734924	75.501953	68.953409
1069.807283	66.199029	68.958414
1068.726687	65.197703	68.963418
1067.554350	65.986628	68.968423
1067.010870	58.391749	68.973428
1066.272421	64.932212	68.978433
1066.320424	66.451112	68.983438
1065.419500	64.598033	68.988442
1064.542401	70.739506	68.993447
1063.923185	64.288931	68.998452
1063.098086	68.028307	69.003457
1063.298429	62.250033	69.008462
1061.840606	74.075788	69.013466
1061.124939	62.282045	69.018471
1061.160896	62.801490	69.023476
1059.856626	71.111429	69.028481
1059.652320	64.375654	69.033486
1059.077843	70.885307	69.038490
1057.983322	68.757097	69.043495
1057.009165	65.567370	69.048500
1056.355282	60.159953	69.053505
1055.905868	69.669587	69.058510
1055.422437	69.878994	69.063514
1054.744045	55.674465	69.068519
1054.087323	61.415026	69.073524
1053.210456	60.483800	69.078529
1052.961180	66.642096	69.083534
1052.329114	71.047784	69.088538
1051.397724	63.341151	69.093543
1050.598394	64.777223	69.098548
1049.834649	78.735010	69.103553
1049.702160	61.300751	69.108558
1049.005627	69.037772	69.113562
1047.921965	66.097282	69.118567
1047.450391	58.935672	69.123572
1046.735207	65.149162	69.128577
1046.379998	60.482714	69.133582
1045.215274	71.129591	69.138586
1044.216187	64.252172	69.143591
1044.183096	59.498211	69.148596
1043.773936	75.124779	69.153601
1043.243029	60.415815	69.158606
1042.004910	67.458400	69.163610
1041.476089	69.464879	69.168615
1040.987115	62.627737	69.173620
1040.239338	63.024280	69.178625
1039.367124	56.415267	69.183630
1038.586724	63.418150	69.188634
1038.126090	58.975058	69.193639
1037.843379	55.616994	69.198644
1036.944005	64.110108	69.203649
1036.338392	62.066557	69.208654
1035.622519	61.339962	69.213658
1035.023991	59.743141	69.218663
1034.649516	66.310864	69.223668
1033.121960	72.503786	69.228673
1032.818003	67.211017	69.233678
1032.446663	66.552614	69.238682
1031.580183	71.817195	69.243687
1030.828542	62.623287	69.248692
1030.016254	67.112844	69.253697
1029.619256	58.165296	69.258702
1029.010842	61.654164	69.263706
1028.493139	61.788603	69.268711
1028.028485	59.142309	69.273716
1026.895831	61.156544	69.278721
1026.516484	58.378407	69.283726
1025.244284	68.864191	69.288730
1024.505306	64.746080	69.293735
1024.164202	59.899197	69.298740
1023.407867	71.536095	69.303745
1023.368225	61.197586	69.308750
1022.980002	68.778329	69.313754
1021.677601	64.863397	69.318759
1021.191131	63.649299	69.323764
1020.614919	71.163756	69.328769
1019.339606	67.826413	69.333774
1018.437379	71.511841	69.338778
1017.947543	68.587277	69.343783
1017.577716	67.559627	69.348788
1017.325749	64.236098	69.353793
1016.852795	64.910625	69.358798
1016.094657	61.338040	69.363802
1015.175740	69.239758	69.368807
1014.630187	58.270532	69.373812
1013.798798	65.773545	69.378817
1013.309145	67.560908	69.383822
1012.743152	67.710918	69.388826
1011.983263	66.825751	69.393831
1011.115609	63.508713	69.398836
1010.356695	72.952475	69.403841
1010.066526	69.187166	69.408846
1009.268856	67.226217	69.413850
1007.882332	69.315545	69.418855
1007.561000	65.605658	69.423860
1006.914518	66.096482	69.428865
1006.675991	61.058239	69.433870
1006.221046	69.878049	69.438874
1005.139226	65.893339	69.443879
1004.674909	56.026103	69.448884
1003.744688	63.169526	69.453889
1003.491511	54.270068	69.458894
1002.365271	65.486422	69.463898
1001.459049	71.047495	69.468903
1001.376572	66.041193	69.473908
1000.850565	66.500236	69.478913
999.964676	66.713759	69.483918
998.845955	62.236605	69.488922
998.220037	57.695239	69.493927
998.300635	61.922895	69.498932
997.589972	70.975781	69.503937
996.574540	69.524146	69.508942
995.687750	61.212776	69.513946
995.226721	56.963723	69.518951
994.624779	56.460287	69.523956
994.063732	68.468241	69.528961
993.190940	66.899297	69.533966
992.680086	59.961572	69.538970
992.384662	64.215938	69.543975
991.295875	57.917369	69.548980
990.273643	60.011823	69.553985
989.877753	56.386344	69.558990
989.412489	48.652892	69.563994
988.958400	63.707853	69.568999
987.989529	55.102042	69.574004
987.013538	61.639314	69.579009
986.743957	55.301873	69.584014
986.256770	60.323188	69.589018
985.728830	65.038751	69.594023
984.980020	56.899400	69.599028
983.924376	59.423373	69.604033
983.559033	50.499191	69.609038
982.643605	50.955541	69.614042
981.463857	58.484023	69.619047
981.590047	58.774643	69.624052
980.732703	60.601591	69.629057
980.176221	52.125714	69.634062
979.080042	49.105249	69.639066
978.651227	64.388001	69.644071
978.259304	53.561505	69.649076
977.859658	63.124723	69.654081
976.806244	60.491692	69.659086
975.923576	56.675585	69.664090
975.362907	57.676313	69.669095
975.287289	57.816116	69.674100
974.137071	52.962364	69.679105
973.538690	57.750636	69.684110
972.892396	55.092255	69.689114
972.216356	63.382692	69.694119
971.527148	55.019398	69.699124
970.819413	53.014192	69.704129
969.988317	55.504018	69.709134
969.577454	58.519917	69.714138
969.048362	61.974099	69.719143
967.895946	58.047950	69.724148
967.210006	64.001336	69.729153
967.057643	61.917224	69.734158
966.738636	51.725683	69.739162
965.705617	53.064922	69.744167
965.064712	51.604173	69.749172
964.215972	61.024382	69.754177
963.368850	54.349908	69.759182
962.393756	57.927096	69.764186
961.513309	63.294842	69.769191
961.530494	54.991041	69.774196
960.997282	59.768946	69.779201
961.049105	59.166226	69.784206
960.325321	57.983594	69.789210
958.875387	60.720126	69.794215
958.438205	53.407990	69.799220
957.215577	64.172915	69.804225
956.423081	55.452322	69.809230
956.348884	63.382069	69.814234
955.766826	58.442652	69.819239
955.805052	64.168848	69.824244
953.983494	62.982698	69.829249
953.313685	57.626734	69.834254
953.163126	59.656619	69.839258
952.390910	66.155172	69.844263
951.753448	55.848723	69.849268
950.467403	61.044466	69.854273
949.886223	64.119009	69.859278
949.625160	56.151220	69.864282
949.009219	68.472266	69.869287
949.251134	62.744146	69.874292
948.032990	68.698644	69.879297
947.242907	67.569142	69.884302
946.750885	56.550421	69.889306
945.381092	63.390068	69.894311
945.162622	65.347181	69.899316
944.072779	58.108937	69.904321
943.940180	60.238466	69.909326
943.175093	62.216326	69.914330
942.061316	63.968973	69.919335
941.439902	62.298547	69.924340
940.833960	57.662556	69.929345
940.584877	61.967898	69.934350
940.219692	62.283090	69.939354
939.102407	70.627981	69.944359
938.764846	52.048405	69.949364
938.284863	53.231844	69.954369
937.239834	51.996258	69.959374
936.200131	55.109072	69.964378
935.307792	57.654386	69.969383
935.116664	49.844210	69.974388
934.538435	55.988618	69.979393
933.931970	57.774082	69.984398
932.994029	65.541652	69.989402
932.328400	58.967619	69.994407
931.790895	58.635295	69.999412
931.498172	55.269379	70.004417
930.512036	61.647434	70.009422
930.021877	60.303055	70.014426
929.155033	59.636785	70.019431
928.740862	64.124517	70.024436
927.577281	62.116167	70.029441
926.756166	61.658664	70.034446
926.607722	57.426117	70.039450
925.888664	62.380259	70.044455
925.649318	58.797691	70.049460
924.609401	64.227095	70.054465
923.990364	59.694117	70.059470
923.599785	57.613224	70.064474
922.714326	65.362984	70.069479
922.087667	61.227036	70.074484
921.323618	64.294415	70.079489
921.052592	64.682935	70.084494
919.984851	53.397871	70.089498
919.148230	54.794185	70.094503
918.866265	62.458947	70.099508
918.073940	58.775143	70.104513
917.022193	53.683399	70.109518
916.255362	61.628747	70.114522
915.661679	62.775091	70.119527
915.224540	54.365397	70.124532
915.180334	61.541314	70.129537
914.304859	64.169108	70.134542
913.380947	52.121568	70.139546
912.392711	64.356779	70.144551
912.482541	54.518082	70.149556
911.829898	58.810375	70.154561
911.064269	61.256686	70.159566
910.309549	56.483531	70.164570
909.258214	66.361775	70.169575
908.508970	53.305572	70.174580
907.745513	58.069664	70.179585
907.324824	65.709196	70.184590
906.836147	59.141704	70.189594
906.074255	67.751748	70.194599
905.482391	58.144535	70.199604
904.688278	60.387222	70.204609
903.836871	65.100658	70.209614
903.682482	64.332055	70.214618
902.948145	64.086255	70.219623
902.087012	58.125242	70.224628
901.370655	58.557826	70.229633
900.662274	56.835018	70.234638
900.540076	58.772082	70.239642
899.589200	61.672078	70.244647
898.807834	55.815067	70.249652
898.153919	62.132378	70.254657
897.849098	69.762935	70.259662
896.863431	60.286203	70.264666
895.669903	58.785684	70.269671
895.156911	59.975961	70.274676
894.843759	58.534034	70.279681
894.659536	67.635622	70.284686
893.604853	59.199629	70.289690
892.708109	60.771100	70.294695
892.048886	66.491592	70.299700
891.679881	58.526799	70.304705
891.016577	61.756349	70.309710
890.546661	56.617754	70.314714
889.371011	66.559942	70.319719
889.257532	56.542289	70.324724
888.302104	72.656335	70.329729
887.409280	60.279000	70.334734
887.200838	54.620976	70.339738
886.425534	68.210031	70.344743
885.704376	53.096172	70.349748
884.394788	57.062511	70.354753
883.683311	57.060660	70.359758
883.678166	53.436096	70.364762
883.132053	58.988775	70.369767
883.118434	58.281350	70.374772
881.793565	60.012423	70.379777
881.134110	52.521216	70.384782
880.786741	50.264721	70.389786
879.284856	52.979601	70.394791
878.711411	57.186756	70.399796
878.123704	64.403438	70.404801
877.710773	57.320851	70.409806
877.572573	54.390822	70.414810
876.415240	59.067796	70.419815
875.952570	54.807993	70.424820
875.367732	59.556282	70.429825
874.464140	59.280656	70.434830
873.224077	56.033980	70.439834
872.361003	60.113766	70.444839
872.416620	51.852744	70.449844
871.612610	63.796871	70.454849
871.323070	59.522130	70.459854
871.000942	63.082163	70.464858
869.720375	67.928566	70.469863
869.327116	57.740976	70.474868
868.237906	66.570277	70.479873
867.444680	61.591952	70.484878
866.954539	59.318756	70.489882
866.286252	58.496327	70.494887
866.020231	61.385109	70.499892
865.732116	66.130331	70.504897
864.781818	69.134328	70.509902
863.988258	60.972181	70.514906
863.129129	66.601492	70.519911
861.916506	57.894186	70.524916
861.325277	55.673350	70.529921
860.960082	59.421587	70.534926
860.776196	61.258083	70.539930
860.192554	66.769433	70.544935
859.682327	52.809462	70.549940
858.580864	62.339305	70.554945
858.179658	64.240352	70.559950
857.696816	60.877896	70.564954
856.251756	65.911335	70.569959
855.960613	55.434684	70.574964
855.329522	60.333841	70.579969
854.659800	71.690477	70.584974
853.863900	65.920948	70.589978
852.872135	74.841983	70.594983
852.585636	66.640136	70.599988
852.249688	70.125101	70.604993
851.168776	72.784037	70.609998
850.044802	61.347106	70.615002
849.308236	71.730362	70.620007
849.231646	61.667416	70.625012
848.976732	65.756072	70.630017
848.474287	66.105739	70.635022
847.605495	59.865268	70.640026
846.896893	57.653655	70.645031
846.514099	54.647442	70.650036
845.115565	56.316141	70.655041
844.470950	67.520545	70.660046
843.766730	61.175034	70.665050
843.409808	63.616238	70.670055
843.034962	57.880625	70.675060
841.897940	67.554909	70.680065
841.049393	65.416034	70.685070
840.930075	61.210399	70.690074
840.215405	63.285919	70.695079
839.184400	61.139816	70.700084
838.462225	58.482511	70.705089
838.138577	57.641506	70.710094
837.762695	52.877466	70.715098
837.083116	57.599839	70.720103
836.003713	54.433267	70.725108
835.677211	66.602599	70.730113
834.662744	58.666438	70.735118
833.906869	59.374990	70.740122
832.907009	67.138253	70.745127
832.770807	55.671849	70.750132
832.117690	58.149159	70.755137
831.718711	61.131645	70.760142
831.458799	59.823179	70.765146
830.336587	60.219457	70.770151
829.831715	57.530721	70.775156
828.625101	58.757296	70.780161
828.223239	63.023884	70.785166
827.734550	51.323430	70.790170
827.002929	61.830475	70.795175
826.273959	61.508149	70.800180
825.179440	70.835053	70.805185
824.812428	60.742644	70.810190
824.425523	60.339064	70.815194
823.395042	56.958129	70.820199
822.490400	55.069465	70.825204
822.009319	60.384721	70.830209
821.514982	53.556381	70.835214
821.723273	56.293974	70.840218
820.101737	61.524254	70.845223
819.545744	58.872043	70.850228
818.979739	67.053531	70.855233
818.286636	66.375414	70.860238
817.501075	58.894837	70.865242
816.518315	63.241273	70.870247
816.191101	59.204351	70.875252
815.772263	68.172970	70.880257
815.268602	60.012008	70.885262
814.334320	59.107354	70.890266
813.616971	57.393885	70.895271
813.252412	57.887191	70.900276
812.409695	62.058373	70.905281
811.201385	53.689457	70.910286
810.573689	55.610791	70.915290
810.421265	61.320013	70.920295
810.111066	57.554773	70.925300
809.212883	62.745613	70.930305
808.316513	62.098278	70.935310
807.744347	60.472087	70.940314
807.025310	63.846145	70.945319
806.695115	53.823579	70.950324
805.806492	52.619924	70.955329
805.039494	55.547453	70.960334
804.881954	54.762013	70.965338
803.667501	66.957569	70.970343
802.659588	59.983900	70.975348
802.096436	58.370469	70.980353
801.711786	62.702129	70.985358
801.277326	51.406213	70.990362
799.891242	60.932495	70.995367
799.236818	58.188724	71.000372
798.781510	53.082521	71.005377
798.448950	60.307484	71.010382
798.224418	52.587802	71.015386
797.475333	64.381274	71.020391
796.786575	58.522175	71.025396
795.993529	61.950595	71.030401
795.131704	59.908468	71.035406
794.091362	58.165995	71.040410
793.525096	56.985147	71.045415
793.061916	55.160262	71.050420
792.765645	52.040938	71.055425
791.972003	55.786420	71.060430
791.053172	50.301418	71.065434
790.178142	60.878606	71.070439
789.839270	58.488307	71.075444
789.680406	60.975260	71.080449
788.456042	59.883402	71.085454
788.066164	50.505856	71.090458
786.922431	58.016064	71.095463
787.065964	60.265645	71.100468
786.269370	69.773794	71.105473
785.230046	59.154483	71.110478
784.812007	56.518167	71.115482
783.837255	61.476775	71.120487
783.019096	58.451567	71.125492
782.470242	55.124870	71.130497
781.754201	68.409617	71.135502
782.023196	51.578578	71.140506
780.531209	70.044138	71.145511
779.907727	54.019066	71.150516
779.135446	62.689134	71.155521
778.424996	63.191775	71.160526
778.146671	57.715202	71.165530
777.153999	60.153538	71.170535
776.510335	55.522024	71.175540
775.971338	60.225186	71.180545
775.676737	59.587723	71.185550
774.721895	55.541910	71.190554
773.461596	63.867044	71.195559
773.243007	65.174482	71.200564
772.932414	61.513389	71.205569
772.298068	63.240249	71.210574
771.406958	53.748531	71.215578
770.671038	69.357721	71.220583
770.188289	61.981921	71.225588
769.569976	58.644206	71.230593
768.606074	66.531074	71.235598
768.183691	63.739333	71.240602
767.450858	68.501742	71.245607
766.727005	57.803835	71.250612
765.837060	56.515249	71.255617
764.909449	58.402337	71.260622
764.972076	58.048630	71.265626
764.686633	63.397405	71.270631
763.605268	47.333276	71.275636
762.734619	57.728420	71.280641
762.052084	60.672478	71.285646
761.858051	58.255972	71.290650
760.427283	58.638323	71.295655
759.619996	62.275601	71.300660
759.097954	59.356225	71.305665
758.699436	60.719116	71.310670
758.645635	60.817605	71.315674
757.635232	64.931920	71.320679
756.668714	60.801240	71.325684
756.383816	53.580031	71.330689
755.907768	59.670355	71.335694
755.048054	55.429634	71.340698
754.078739	56.802970	71.345703
753.596935	54.900634	71.350708
753.051762	48.651265	71.355713
752.060745	51.953516	71.360718
751.592025	52.539107	71.365722
750.778881	62.030970	71.370727
750.647938	52.637441	71.375732
749.386239	53.503816	71.380737
748.371315	57.756047	71.385742
747.967258	47.116054	71.390746
747.316376	56.105842	71.395751
747.422577	57.863046	71.400756
746.372935	61.464793	71.405761
745.450306	61.577022	71.410766
745.184911	58.291939	71.415770
744.889624	60.652378	71.420775
743.953914	56.439529	71.425780
742.774395	49.343404	71.430785
742.337228	61.637581	71.435790
741.892053	57.572143	71.440794
740.793206	63.935088	71.445799
740.531268	56.044750	71.450804
739.751956	57.736349	71.455809
739.143768	68.378304	71.460814
738.417228	53.307946	71.465818
737.412668	58.704976	71.470823
737.345442	59.955202	71.475828
736.611112	58.559851	71.480833
735.164955	62.835011	71.485838
735.175131	52.733043	71.490842
734.475732	60.994123	71.495847
733.659760	54.481942	71.500852
732.888932	52.048460	71.505857
732.041622	58.965871	71.510862
731.698906	45.892340	71.515866
731.361484	53.912862	71.520871
730.804552	68.093225	71.525876
729.809289	61.964400	71.530881
728.929482	66.116281	71.535886
728.755662	57.923333	71.540890
727.416572	63.001468	71.545895
726.844724	51.492481	71.550900
726.311222	49.401264	71.555905
725.511261	63.300194	71.560910
725.529182	48.895067	71.565914
724.676620	59.501807	71.570919
723.457758	55.283585	71.575924
723.146236	56.918059	71.580929
722.480232	59.266559	71.585934
722.398785	55.441260	71.590938
721.090952	59.087278	71.595943
720.131656	55.553130	71.600948
719.947444	58.167123	71.605953
719.438976	59.063400	71.610958
718.859683	52.073573	71.615962
717.878824	55.219678	71.620967
717.623953	55.891076	71.625972
716.677313	42.506851	71.630977
715.135729	51.094405	71.635982
714.872263	53.027156	71.640986
714.371794	65.987429	71.645991
714.258190	57.628778	71.650996
713.874338	54.308944	71.656001
712.494085	53.227752	71.661006
712.176880	48.646785	71.666010
711.280887	54.578471	71.671015
709.994207	55.442534	71.676020
709.547225	52.416604	71.681025
708.861274	53.503567	71.686030
708.783677	46.952685	71.691034
708.132484	61.646368	71.696039
707.863787	54.186045	71.701044
706.899710	57.416215	71.706049
705.892761	53.154802	71.711054
705.370743	49.890085	71.716058
704.208183	55.376936	71.721063
703.486435	50.051405	71.726068
703.205743	50.868840	71.731073
702.544510	49.231627	71.736078
702.401774	52.204868	71.741082
701.757225	50.684847	71.746087
700.804715	54.413070	71.751092
699.932453	55.465045	71.756097
699.491093	47.067124	71.761102
699.091244	46.372312	71.766106
698.096500	50.334341	71.771111
697.518510	47.699857	71.776116
697.047864	52.723307	71.781121
695.567168	57.322530	71.786126
695.048406	50.420845	71.791130
694.330069	51.765280	71.796135
694.236579	54.446830	71.801140
693.966676	51.331207	71.806145
692.801200	61.383807	71.811150
692.298328	53.334723	71.816154
691.364479	53.656916	71.821159
691.069080	54.503503	71.826164
690.160090	48.135462	71.831169
689.202337	54.356108	71.836174
689.088975	46.901021	71.841178
687.889498	54.041671	71.846183
687.307553	53.748016	71.851188
686.677394	42.916963	71.856193
685.972748	53.306191	71.861198
686.035622	46.950565	71.866202
685.098818	52.434593	71.871207
684.240482	52.350527	71.876212
683.543551	53.544900	71.881217
682.594914	60.883735	71.886222
682.293141	47.887276	71.891226
681.230007	49.773894	71.896231
680.707558	54.733055	71.901236
680.446109	55.567930	71.906241
679.550168	56.160058	71.911246
679.118594	51.611499	71.916250
678.217272	56.654643	71.921255
677.321070	57.664705	71.926260
677.227903	46.871151	71.931265
676.252805	54.121158	71.936270
675.167879	47.612404	71.941274
674.669650	54.917367	71.946279
674.392945	49.784332	71.951284
674.262785	53.559817	71.956289
673.447534	60.120479	71.961294
672.753988	47.601143	71.966298
671.298485	51.573471	71.971303
669.972108	53.095156	71.976308
669.904782	57.021486	71.981313
669.153711	56.153947	71.986318
669.029597	47.681864	71.991322
668.529033	61.652976	71.996327
668.373643	45.466694	72.001332
667.613271	48.178738	72.006337
666.519482	60.774592	72.011342
665.898726	45.129190	72.016346
664.667496	48.679456	72.021351
663.812309	42.160937	72.026356
663.858536	46.774079	72.031361
663.257939	52.608278	72.036366
662.882322	48.791981	72.041370
661.324769	55.243763	72.046375
660.788822	57.243562	72.051380
660.718017	50.970722	72.056385
659.951585	46.213717	72.061390
659.034586	51.674099	72.066394
658.215747	55.759520	72.071399
657.618427	56.047061	72.076404
657.603842	50.648363	72.081409
656.418239	48.325110	72.086414
655.930860	47.959633	72.091418
655.217321	51.629318	72.096423
654.303143	53.482766	72.101428
653.847529	50.191718	72.106433
652.554274	54.404725	72.111438
652.464892	47.808417	72.116442
652.225113	51.177157	72.121447
651.468888	51.456888	72.126452
650.663926	43.870664	72.131457
650.048371	52.026941	72.136462
649.610554	50.269011	72.141466
648.389864	64.069371	72.146471
647.870564	50.208695	72.151476
647.460675	43.288113	72.156481
646.425953	50.199116	72.161486
645.421475	44.106499	72.166490
645.004953	50.961637	72.171495
644.680470	52.694376	72.176500
644.495591	53.375135	72.181505
643.285294	55.830829	72.186510
642.437674	56.620279	72.191514
641.865255	52.091003	72.196519
641.242974	49.450971	72.201524
640.639915	47.403966	72.206529
639.517857	59.204815	72.211534
638.872301	52.850037	72.216538
638.263528	55.142135	72.221543
637.970834	57.634635	72.226548
637.623047	55.704674	72.231553
636.291943	56.834469	72.236558
635.835205	45.433346	72.241562
635.357818	57.275036	72.246567
635.000956	59.202167	72.251572
634.248782	56.581244	72.256577
633.106122	52.634788	72.261582
632.700321	46.396376	72.266586
632.426436	49.499313	72.271591
631.281308	53.647741	72.276596
630.165116	46.155242	72.281601
629.406202	56.881129	72.286606
629.533200	48.651336	72.291610
629.435082	47.269821	72.296615
628.581122	55.938731	72.301620
628.012693	54.116449	72.306625
626.253737	62.421705	72.311630
625.428849	50.591930	72.316634
625.159281	55.222247	72.321639
624.372243	47.946990	72.326644
624.367140	48.613314	72.331649
623.548668	48.742117	72.336654
623.310395	40.001220	72.341658
622.209259	56.214199	72.346663
621.323144	54.254853	72.351668
621.123471	45.214493	72.356673
619.906360	52.736446	72.361678
619.248516	53.380564	72.366682
618.766885	50.076320	72.371687
618.405298	47.467319	72.376692
617.490593	49.253054	72.381697
616.478682	54.126170	72.386702
616.290593	49.825855	72.391706
615.867904	51.304578	72.396711
615.011074	50.833944	72.401716
614.266306	47.680417	72.406721
613.824411	45.465828	72.411726
612.972128	52.358827	72.416730
611.957907	51.500098	72.421735
611.353276	54.505900	72.426740
611.110963	50.062834	72.431745
610.408143	55.791898	72.436750
609.118419	44.753676	72.441754
608.561477	45.452690	72.446759
607.976432	50.368213	72.451764
607.920054	48.272001	72.456769
607.204071	52.309517	72.461774
606.968979	49.314519	72.466778
605.709255	55.993290	72.471783
604.786636	58.759577	72.476788
603.683225	43.985853	72.481793
602.958446	52.102762	72.486798
602.849622	45.930602	72.491802
603.022287	47.683518	72.496807
601.868933	53.528489	72.501812
600.747190	48.621510	72.506817
600.080492	57.251143	72.511822
599.412506	52.366516	72.516826
599.218465	53.406705	72.521831
598.557173	57.569554	72.526836
597.879715	42.295914	72.531841
597.058471	48.102185	72.536846
596.533695	44.694433	72.541850
595.535274	52.257260	72.546855
594.528656	66.062971	72.551860
594.379255	44.031572	72.556865
593.604709	58.320709	72.561870
593.066577	47.323644	72.566874
592.140891	51.771452	72.571879
591.385300	57.780160	72.576884
590.837046	51.613330	72.581889
590.177196	61.695824	72.586894
590.354669	51.190337	72.591898
589.173977	57.159517	72.596903
588.056131	61.357235	72.601908
587.739544	60.611334	72.606913
587.340117	62.247207	72.611918
586.743000	52.175744	72.616922
586.087628	56.741352	72.621927
585.042090	50.420335	72.626932
584.718662	53.862326	72.631937
583.285443	62.609315	72.636942
583.010984	58.067292	72.641946
582.445174	54.421649	72.646951
582.256341	61.220034	72.651956
581.092437	51.139496	72.656961
579.993605	58.801902	72.661966
579.794171	51.351074	72.666970
579.372543	53.247526	72.671975
578.468219	51.455099	72.676980
577.752056	48.572995	72.681985
576.824519	54.124967	72.686990
576.294527	51.314136	72.691994
575.800207	55.710594	72.696999
575.444661	51.545764	72.702004
575.410704	47.673491	72.707009
573.901698	55.079528	72.712014
573.365880	50.594905	72.717018
572.432348	53.519059	72.722023
571.613256	59.389653	72.727028
571.355472	53.747420	72.732033
570.465234	56.059130	72.737038
570.175685	47.198673	72.742042
569.284525	49.682417	72.747047
568.318111	50.501851	72.752052
568.248042	53.707949	72.757057
567.521325	58.855781	72.762062
566.339300	53.531066	72.767066
565.777112	45.739052	72.772071
565.528040	51.042617	72.777076
565.160911	47.147717	72.782081
563.752095	63.772423	72.787086
563.381375	50.476316	72.792090
562.958368	52.065484	72.797095
561.837580	58.569182	72.802100
561.023094	54.463259	72.807105
560.256811	59.607933	72.812110
560.094572	46.573514	72.817114
559.811494	48.976179	72.822119
558.946775	49.855112	72.827124
558.239069	41.739351	72.832129
557.559882	56.610967	72.837134
556.408788	58.372874	72.842138
555.584356	48.969987	72.847143
555.126535	55.710289	72.852148
554.789599	48.793876	72.857153
554.284317	52.595995	72.862158
554.193508	54.449220	72.867162
552.952630	50.628835	72.872167
552.254891	59.626120	72.877172
551.455504	54.998980	72.882177
550.456613	59.439539	72.887182
549.817982	51.273350	72.892186
549.440308	46.099650	72.897191
548.868431	50.618849	72.902196
548.626939	48.815476	72.907201
547.181050	49.493669	72.912206
546.579462	52.032223	72.917210
546.380162	51.258185	72.922215
545.348490	62.123731	72.927220
544.439883	56.645089	72.932225
543.581564	52.923046	72.937230
543.262124	54.800072	72.942234
543.187954	54.960157	72.947239
542.690516	50.653932	72.952244
541.835302	52.140060	72.957249
540.699986	54.938670	72.962254
540.643266	45.981210	72.967258
539.671696	50.589307	72.972263
538.358209	55.542026	72.977268
537.995618	44.263133	72.982273
537.830926	52.924776	72.987278
537.177171	47.353507	72.992282
536.279934	48.236051	72.997287
534.918652	55.140762	73.002292
534.756399	53.308998	73.007297
534.473458	52.491514	73.012302
533.754975	51.618826	73.017306
532.896205	50.536672	73.022311
532.378478	49.195192	73.027316
531.789306	51.575654	73.032321
530.896843	51.463961	73.037326
530.094574	42.734070	73.042330
529.654579	44.858957	73.047335
529.125108	56.379367	73.052340
528.610061	44.194361	73.057345
527.693798	51.105458	73.062350
526.960059	51.755381	73.067354
526.669669	39.982447	73.072359
525.202327	45.686650	73.077364
524.708063	36.669584	73.082369
524.117868	42.505300	73.087374
523.496590	44.726874	73.092378
523.098921	50.167651	73.097383
522.894537	50.343747	73.102388
521.909852	37.907129	73.107393
520.828872	52.636166	73.112398
520.479571	49.741374	73.117402
519.611528	49.849722	73.122407
518.770358	53.158149	73.127412
518.260122	51.061698	73.132417
517.904305	53.720380	73.137422
517.359745	52.302753	73.142426
516.291594	53.832270	73.147431
515.055283	56.602825	73.152436
515.125392	42.884858	73.157441
514.873259	56.057887	73.162446
514.094724	57.274767	73.167450
512.928937	53.406172	73.172455
512.076911	50.343881	73.177460
512.153047	55.322834	73.182465
511.565137	54.686395	73.187470
510.483305	49.803066	73.192474
509.702174	54.374531	73.197479
509.100425	58.024868	73.202484
508.609059	52.128119	73.207489
507.615513	60.694718	73.212494
507.005228	53.175308	73.217498
506.701351	55.100322	73.222503
505.804460	58.854446	73.227508
505.746851	50.649333	73.232513
504.512278	57.732572	73.237518
503.698084	56.176550	73.242522
503.303219	54.364497	73.247527
502.476157	61.803868	73.252532
501.828884	59.035391	73.257537
501.075745	57.753495	73.262542
500.830728	56.471081	73.267546
499.919250	57.031054	73.272551
498.917267	58.070646	73.277556
498.731416	52.483198	73.282561
498.240835	59.676579	73.287566
497.326882	54.738127	73.292570
496.603206	47.807641	73.297575
495.847904	52.319801	73.302580
495.597222	47.269384	73.307585
494.452657	55.388534	73.312590
493.514960	53.073179	73.317594
493.202469	57.584185	73.322599
492.500917	62.305405	73.327604
492.284728	48.284538	73.332609
491.743181	54.205555	73.337614
490.685271	56.599196	73.342618
490.045057	50.641009	73.347623
489.245845	56.814385	73.352628
488.392230	45.873923	73.357633
487.509201	51.683759	73.362638
487.081213	56.847099	73.367642
486.739739	49.026255	73.372647
486.283986	49.269207	73.377652
485.586722	39.510209	73.382657
484.695476	48.522556	73.387662
483.883976	52.340353	73.392666
483.807804	48.780738	73.397671
482.814437	55.494400	73.402676
482.145130	47.301584	73.407681
481.671359	51.991247	73.412686
480.855621	50.508020	73.417690
479.841023	47.378601	73.422695
478.969359	58.928300	73.427700
479.063543	39.005944	73.432705
478.255073	51.884398	73.437710
477.367163	50.969333	73.442714
476.413424	50.880037	73.447719
476.103787	57.926323	73.452724
475.879954	53.056133	73.457729
474.990508	56.965198	73.462734
473.895924	55.151082	73.467738
473.309358	47.784025	73.472743
472.649951	59.284141	73.477748
472.653736	50.200353	73.482753
471.610798	53.626094	73.487758
470.763425	51.326321	73.492762
470.618812	41.431975	73.497767
469.374582	51.880392	73.502772
468.794935	44.569005	73.507777
467.799751	50.491332	73.512782
467.437805	45.942768	73.517786
467.061447	51.487389	73.522791
466.151678	46.090971	73.527796
465.563298	47.086760	73.532801
464.894310	57.087148	73.537806
464.419140	55.950214	73.542810
463.905856	45.179471	73.547815
462.715184	59.265265	73.552820
462.203781	51.837349	73.557825
461.458705	52.888065	73.562830
460.811774	54.225920	73.567834
460.145004	51.627719	73.572839
459.386752	53.495817	73.577844
458.726658	45.120194	73.582849
458.410708	58.082617	73.587854
457.937477	50.333232	73.592858
457.084512	49.217065	73.597863
456.362670	59.615383	73.602868
455.705727	47.724240	73.607873
455.108050	49.893185	73.612878
454.246207	49.273595	73.617882
453.358494	51.387823	73.622887
452.913928	47.213546	73.627892
452.766690	48.744604	73.632897
451.579617	53.815995	73.637902
450.841647	51.606031	73.642906
450.599726	51.333953	73.647911
449.828306	60.871273	73.652916
449.106818	46.684919	73.657921
448.078523	55.395841	73.662926
447.654161	52.159782	73.667930
447.462456	48.134454	73.672935
446.492333	51.553334	73.677940
445.660707	46.647521	73.682945
444.943446	55.141733	73.687950
444.455104	54.907339	73.692954
444.102844	48.759789	73.697959
442.553406	53.482064	73.702964
442.398286	52.754612	73.707969
441.709425	57.185238	73.712974
441.246367	58.217837	73.717978
440.492163	49.166509	73.722983
439.347763	49.080796	73.727988
439.198600	44.279142	73.732993
438.689609	48.783611	73.737998
437.988669	51.147206	73.743002
437.023632	45.726491	73.748007
436.341233	57.714397	73.753012
436.168582	48.329142	73.758017
435.288505	54.504377	73.763022
434.182431	58.840630	73.768026
433.654349	50.888679	73.773031
432.907661	54.000731	73.778036
432.941756	47.821588	73.783041
431.959060	55.615352	73.788046
431.102256	50.672554	73.793050
430.740049	49.760479	73.798055
430.148806	51.617745	73.803060
429.495119	47.347483	73.808065
428.305602	47.776740	73.813070
427.897627	58.743218	73.818074
427.632145	48.497550	73.823079
426.422062	56.007425	73.828084
426.053874	51.198089	73.833089
425.363354	53.323486	73.838094
425.006610	51.573182	73.843098
424.072980	46.912287	73.848103
423.284775	49.971031	73.853108
423.100105	48.316314	73.858113
421.747767	53.883979	73.863118
420.686016	56.122143	73.868122
420.469290	43.714601	73.873127
419.720556	49.417904	73.878132
419.506568	44.606080	73.883137
419.159411	47.512550	73.888142
417.976996	54.004042	73.893146
417.288307	42.293019	73.898151
416.768137	50.880410	73.903156
415.972486	46.126571	73.908161
414.726063	46.438747	73.913166
414.221399	47.615173	73.918170
414.143818	52.432529	73.923175
413.596775	58.496360	73.928180
413.509861	49.646226	73.933185
412.399573	51.365425	73.938190
411.454761	52.037975	73.943194
410.708408	44.939248	73.948199
409.572976	49.567190	73.953204
408.862414	52.523682	73.958209
408.579742	56.022274	73.963214
408.052717	47.237537	73.968218
407.760847	46.754227	73.973223
406.769685	50.963369	73.978228
406.086416	39.778189	73.983233
405.661627	52.220209	73.988238
404.985357	58.866026	73.993242
404.432862	49.145486	73.998247
403.389877	58.995744	74.003252
403.325461	48.818968	74.008257
401.961748	49.673385	74.013262
400.833889	46.027463	74.018266
400.789382	45.851667	74.023271
400.099626	53.810073	74.028276
400.154574	45.684812	74.033281
398.961149	41.920030	74.038286
397.935524	48.392853	74.043290
397.538662	50.690660	74.048295
397.029850	46.507710	74.053300
396.305453	42.720233	74.058305
395.189028	46.536178	74.063310
394.720760	49.523451	74.068314
394.369320	38.006283	74.073319
393.906912	58.069373	74.078324
392.826360	48.961256	74.083329
392.379226	50.215252	74.088334
391.600580	46.483728	74.093338
391.156481	49.941811	74.098343
389.825248	51.817651	74.103348
389.589647	44.606009	74.108353
388.849577	47.325934	74.113358
388.511330	41.174588	74.118362
387.742018	51.137354	74.123367
386.416463	49.402661	74.128372
386.054454	44.664891	74.133377
385.928290	44.648763	74.138382
385.293539	51.554468	74.143386
384.193517	30.655493	74.148391
383.412666	57.520224	74.153396
382.914253	41.369752	74.158401
382.834111	47.004372	74.163406
381.732451	51.477134	74.168410
381.203467	37.789998	74.173415
380.539767	50.285856	74.178420
379.407271	53.317475	74.183425
378.856011	51.153475	74.188430
378.139323	54.367993	74.193434
377.890746	43.990336	74.198439
377.508078	50.199863	74.203444
376.580496	45.520679	74.208449
375.621406	51.524018	74.213454
374.939115	46.510858	74.218458
374.631439	41.046923	74.223463
373.422337	48.402118	74.228468
373.005270	49.296513	74.233473
372.725889	52.862391	74.238478
371.810371	63.931830	74.243482
370.992820	43.957655	74.248487
369.993657	49.574720	74.253492
369.784725	45.254105	74.258497
369.548473	46.496577	74.263502
368.360601	50.170955	74.268506
367.721060	43.454193	74.273511
366.985315	54.009279	74.278516
366.818711	44.867502	74.283521
366.165604	45.126155	74.288526
365.072886	47.992168	74.293530
364.279693	50.477716	74.298535
363.773275	50.889613	74.303540
363.321679	49.782059	74.308545
362.477610	54.002471	74.313550
361.280331	51.020486	74.318554
361.278491	41.814609	74.323559
360.701771	52.394816	74.328564
360.433808	46.110849	74.333569
359.446222	56.543645	74.338574
358.532465	50.256932	74.343578
357.863699	44.650269	74.348583
356.640895	45.811837	74.353588
356.201620	50.781447	74.358593
355.793639	49.107128	74.363598
355.235089	49.487911	74.368602
355.344527	42.167675	74.373607
353.931435	52.475890	74.378612
353.522154	50.311349	74.383617
352.824497	39.100098	74.388622
351.599191	49.062998	74.393626
350.919619	52.468726	74.398631
350.153209	50.326405	74.403636
350.138581	44.437306	74.408641
349.799925	47.701973	74.413646
348.628806	50.962108	74.418650
347.883529	50.172593	74.423655
347.207141	54.959219	74.428660
347.057021	51.764634	74.433665
346.226727	51.326134	74.438670
345.045697	59.766543	74.443674
344.571387	54.874787	74.448679
343.988497	50.202185	74.453684
343.793287	42.446377	74.458689
342.478820	51.742251	74.463694
341.856575	47.416543	74.468698
341.366095	54.688771	74.473703
340.682370	61.994954	74.478708
340.440467	47.169249	74.483713
339.653420	49.207549	74.488718
338.774250	56.188486	74.493722
338.400068	45.383001	74.498727
337.322651	61.228006	74.503732
336.630743	47.610996	74.508737
336.042708	56.961417	74.513742
335.614458	51.504085	74.518746
334.924974	47.815142	74.523751
333.857805	56.820878	74.528756
333.467580	50.580052	74.533761
333.140664	57.118168	74.538766
332.067437	56.795659	74.543770
331.590057	51.683624	74.548775
330.673650	53.403499	74.553780
330.394798	47.652703	74.558785
329.620119	50.802358	74.563790
328.579502	56.695704	74.568794
328.105410	52.797395	74.573799
327.797354	53.012106	74.578804
326.884300	57.101599	74.583809
326.444338	50.904971	74.588814
325.299898	63.455386	74.593818
325.292641	55.048303	74.598823
323.992391	57.895370	74.603828
323.480214	47.498231	74.608833
323.022364	56.070973	74.613838
322.084836	56.531084	74.618842
321.254460	56.448995	74.623847
320.566557	59.122780	74.628852
320.027106	60.426194	74.633857
319.644092	54.438109	74.638862
319.169650	56.057590	74.643866
318.641856	52.059032	74.648871
317.648537	59.286826	74.653876
317.306947	59.708732	74.658881
316.487360	49.499358	74.663886
315.144082	52.209784	74.668890
314.568862	48.460059	74.673895
314.266774	53.264309	74.678900
313.839510	51.358106	74.683905
313.187507	51.566136	74.688910
311.918301	49.543384	74.693914
311.506739	47.322445	74.698919
311.214844	56.455362	74.703924
310.771471	51.799958	74.708929
309.690423	50.012146	74.713934
308.875403	50.244581	74.718938
308.541384	47.874089	74.723943
307.574899	61.484238	74.728948
306.441314	52.887665	74.733953
305.843658	56.018576	74.738958
305.322082	57.497338	74.743962
305.145907	51.862644	74.748967
304.844380	57.083119	74.753972
304.189374	49.556713	74.758977
303.400459	55.980807	74.763982
302.608776	62.898928	74.768986
302.183450	49.468101	74.773991
301.086465	50.936071	74.778996
300.301939	50.736296	74.784001
299.734638	53.606904	74.789006
298.598515	53.895251	74.794010
298.179125	42.603399	74.799015
297.442376	50.309118	74.804020
297.094150	48.513323	74.809025
296.724002	44.123796	74.814030
296.151631	49.759596	74.819034
295.094358	44.232221	74.824039
294.363367	54.352903	74.829044
294.072227	52.516472	74.834049
293.488777	41.615045	74.839054
292.851013	50.033536	74.844058
292.365235	49.213717	74.849063
291.363080	50.362227	74.854068
290.204891	50.849635	74.859073
289.991283	47.628905	74.864078
289.335186	54.213181	74.869082
288.729499	41.225849	74.874087
287.672802	49.731612	74.879092
286.956089	44.452734	74.884097
286.797017	46.278996	74.889102
285.883332	52.976867	74.894106
285.028556	48.219885	74.899111
284.612645	46.538960	74.904116
284.165497	55.146268	74.909121
283.531996	47.294746	74.914126
282.168699	56.136387	74.919130
281.755720	48.792185	74.924135
281.276421	51.798580	74.929140
280.948773	50.991407	74.934145
279.510637	43.618219	74.939150
278.617812	53.356269	74.944154
278.489360	45.846871	74.949159
277.632318	54.472205	74.954164
277.420918	52.875377	74.959169
277.323904	49.591910	74.964174
276.109688	52.425286	74.969178
275.385845	43.225689	74.974183
274.716094	50.849771	74.979188
274.263330	48.260093	74.984193
273.198042	50.199260	74.989198
271.978607	54.823303	74.994202
272.187463	47.402066	74.999207
271.649610	53.986421	75.004212
271.051368	50.830155	75.009217
270.241189	46.550193	75.014222
269.446880	51.566942	75.019226
268.880312	41.176918	75.024231
267.662175	51.301134	75.029236
266.882665	40.091926	75.034241
266.787991	39.447892	75.039246
265.899499	45.217661	75.044250
265.750012	47.375131	75.049255
264.824888	48.161291	75.054260
264.376097	47.010733	75.059265
263.933790	47.149081	75.064270
262.435803	52.956080	75.069274
262.051906	42.382400	75.074279
261.233168	43.744535	75.079284
260.743018	47.252553	75.084289
260.461214	42.492562	75.089294
259.065614	51.247897	75.094298
258.697959	51.882123	75.099303
258.180339	51.346506	75.104308
257.668362	43.497701	75.109313
257.267398	45.223750	75.114318
255.882138	49.473687	75.119322
255.515876	45.540862	75.124327
255.124018	48.293627	75.129332
254.299877	56.672451	75.134337
253.411565	52.417564	75.139342
252.671782	53.975273	75.144346
252.174409	52.425608	75.149351
251.915528	51.230588	75.154356
250.936596	52.212986	75.159361
250.584799	46.134789	75.164366
249.664515	53.325729	75.169370
248.937369	43.175771	75.174375
248.142546	56.567757	75.179380
247.601923	50.210577	75.184385
247.308079	45.217542	75.189390
245.955349	39.836637	75.194394
245.534999	42.595521	75.199399
244.956522	40.528935	75.204404
244.510744	38.616238	75.209409
243.943175	39.779069	75.214414
242.636590	39.829686	75.219418
242.428164	30.107984	75.224423
241.588575	43.492902	75.229428
241.352159	40.384625	75.234433
240.326897	41.320796	75.239438
239.201428	38.567126	75.244442
239.092959	40.339591	75.249447
238.622875	51.830056	75.254452
237.512627	45.786031	75.259457
236.923959	45.633903	75.264462
236.151781	45.805916	75.269466
236.341955	43.156336	75.274471
235.090291	41.572375	75.279476
234.317953	43.236202	75.284481
233.790973	42.211654	75.289486
233.023103	46.992386	75.294490
232.266927	36.530101	75.299495
231.493445	47.357726	75.304500
230.991254	49.522536	75.309505
230.685988	47.081242	75.314510
229.971774	52.053695	75.319514
229.152103	40.313168	75.324519
228.507484	44.763595	75.329524
227.839549	45.049880	75.334529
227.088265	35.859412	75.339534
225.933498	41.871910	75.344538
225.794618	39.132861	75.349543
225.199701	46.057473	75.354548
224.924032	41.990366	75.359553
223.756533	35.231662	75.364558
222.695404	45.048590	75.369562
222.649819	36.721754	75.374567
222.172752	36.663802	75.379572
221.148205	35.504111	75.384577
220.376348	30.388593	75.389582
219.486498	38.676965	75.394586
219.263146	35.580801	75.399591
218.690213	36.392835	75.404596
217.625518	35.629050	75.409601
216.928809	31.461911	75.414606
216.356584	41.088937	75.419610
216.181730	33.631105	75.424615
215.931048	41.098502	75.429620
214.472974	30.432734	75.434625
214.144505	33.585402	75.439630
212.794299	43.396376	75.444634
212.238689	31.579075	75.449639
211.611811	41.358316	75.454644
210.988669	44.247305	75.459649
210.878006	37.036281	75.464654
210.250588	43.940845	75.469658
209.788924	44.058635	75.474663
208.690674	44.878722	75.479668
207.852633	43.892729	75.484673
207.749567	32.580447	75.489678
206.147095	47.085197	75.494682
205.997353	42.324662	75.499687
205.634655	48.007476	75.504692
204.760687	38.549569	75.509697
204.026892	31.439465	75.514702
203.281906	49.931221	75.519706
202.662053	44.192233	75.524711
202.063618	45.495612	75.529716
201.167390	47.587628	75.534721
200.618816	36.289597	75.539726
199.973168	42.504792	75.544730
199.564805	40.892065	75.549735
198.676739	40.514865	75.554740
197.325964	40.317087	75.559745
197.135930	39.856992	75.564750
196.802292	48.436747	75.569754
196.621060	38.343285	75.574759
195.866891	41.193241	75.579764
194.912998	34.469885	75.584769
194.403015	31.372113	75.589774
193.042285	51.258281	75.594778
192.431393	41.886169	75.599783
191.781457	42.319404	75.604788
191.414639	45.664269	75.609793
191.295726	44.809639	75.614798
190.232160	50.066452	75.619802
189.411375	45.319860	75.624807
188.830734	48.131116	75.629812
188.527105	47.056777	75.634817
187.839155	42.186508	75.639822
186.709796	47.226732	75.644826
186.179701	47.503668	75.649831
185.767226	42.315094	75.654836
184.650712	45.192859	75.659841
183.849440	46.716235	75.664846
183.338202	56.688365	75.669850
182.975018	44.692154	75.674855
182.515654	50.103377	75.679860
181.495419	41.633887	75.684865
180.757332	43.688082	75.689870
180.307003	52.694872	75.694874
179.985837	41.206049	75.699879
178.441813	45.381989	75.704884
177.953367	47.997200	75.709889
177.918688	49.081395	75.714894
176.867678	57.682487	75.719898
175.953037	50.913451	75.724903
175.035302	56.244793	75.729908
174.514352	50.138386	75.734913
174.477152	45.173832	75.739918
174.045948	54.846198	75.744922
173.228461	41.552059	75.749927
172.141503	52.857028	75.754932
171.723481	53.671183	75.759937
171.374120	51.623279	75.764942
170.273661	55.031499	75.769946
169.527295	51.216060	75.774951
169.120356	45.119864	75.779956
168.185374	43.343524	75.784961
167.594523	46.959075	75.789966
166.603412	51.284989	75.794970
166.343712	44.178153	75.799975
165.969260	51.791444	75.804980
165.131977	51.295775	75.809985
164.248687	44.026589	75.814990
163.549624	46.312685	75.819994
163.308661	41.667624	75.824999
162.722149	44.910326	75.830004
161.716277	56.852074	75.835009
161.107906	38.943583	75.840014
160.593867	43.420513	75.845018
159.961988	38.932397	75.850023
158.947891	44.862572	75.855028
158.147359	44.261698	75.860033
157.832889	46.147434	75.865038
157.100544	49.567930	75.870042
156.599919	34.977500	75.875047
155.551170	37.937512	75.880052
154.834899	47.861904	75.885057
155.098957	53.987262	75.890062
153.911565	49.918873	75.895066
153.155443	46.221690	75.900071
152.519181	38.559892	75.905076
151.659072	49.336690	75.910081
150.720522	43.281105	75.915086
149.424392	49.833413	75.920090
149.753147	49.199143	75.925095
149.764042	45.389129	75.930100
149.285260	47.086601	75.935105
148.475211	47.423951	75.940110
147.429186	54.986628	75.945114
146.664018	44.081111	75.950119
145.524456	51.535699	75.955124
144.794890	50.846244	75.960129
144.229835	46.369553	75.965134
143.523740	52.067702	75.970138
143.212690	47.589934	75.975143
142.916971	54.422705	75.980148
142.031030	47.693264	75.985153
141.566864	45.788249	75.990158
140.794162	50.050963	75.995162
140.276138	47.113753	76.000167
139.427615	44.155125	76.005172
138.704445	47.394391	76.010177
138.120369	36.005849	76.015182
136.736522	53.536622	76.020186
136.489205	47.492252	76.025191
136.257007	48.142743	76.030196
135.381602	50.184154	76.035201
134.485433	42.992729	76.040206
133.736807	55.238816	76.045210
133.242575	53.297595	76.050215
132.789556	44.417568	76.055220
132.042872	47.569122	76.060225
131.173542	42.913871	76.065230
130.168600	45.168324	76.070234
129.702572	46.147835	76.075239
129.653667	40.439259	76.080244
129.355732	49.440675	76.085249
128.598578	36.417638	76.090254
127.414993	36.803516	76.095258
126.917662	40.826782	76.100263
125.973136	45.321898	76.105268
124.929403	39.809796	76.110273
124.751360	44.770895	76.115278
124.060932	42.917731	76.120282
123.340910	36.578160	76.125287
122.278661	45.586329	76.130292
121.488563	45.540463	76.135297
121.645213	39.177798	76.140302
121.210163	49.997213	76.145306
120.754639	43.743197	76.150311
119.917832	44.185747	76.155316
118.990664	49.587994	76.160321
118.087169	41.330156	76.165326
117.085452	32.679557	76.170330
116.478023	39.554141	76.175335
116.283599	37.287579	76.180340
115.730024	47.663849	76.185345
115.178467	47.586256	76.190350
114.125141	48.104334	76.195354
113.961589	40.994794	76.200359
113.012924	43.268664	76.205364
112.001506	51.841384	76.210369
111.377544	41.872148	76.215374
110.684913	45.928137	76.220378
110.211866	50.245577	76.225383
109.077456	35.562263	76.230388
108.267190	42.762505	76.235393
107.917461	43.989977	76.240398
107.486569	48.575083	76.245402
107.135845	51.311847	76.250407
106.923297	39.531337	76.255412
105.474356	50.122923	76.260417
105.293191	38.887761	76.265422
104.528184	41.671662	76.270426
103.573546	49.394820	76.275431
102.925222	43.103744	76.280436
102.215752	44.379120	76.285441
101.860453	31.872333	76.290446
100.427149	44.749563	76.295450
99.718603	44.644969	76.300455
99.621925	29.953883	76.305460
98.971885	42.321438	76.310465
98.567614	43.608070	76.315470
97.768791	49.595403	76.320474
96.771703	42.795399	76.325479
96.669221	35.668241	76.330484
96.081925	47.935910	76.335489
95.394396	40.682849	76.340494
94.275321	44.879382	76.345498
93.794931	49.313113	76.350503
92.968320	41.960805	76.355508
91.895174	48.113308	76.360513
91.610653	44.314136	76.365518
91.148100	43.930622	76.370522
90.698110	47.941616	76.375527
89.729937	49.195172	76.380532
89.094728	46.562088	76.385537
88.792085	40.636938	76.390542
88.004716	49.085626	76.395546
86.810058	35.968374	76.400551
86.157248	41.530303	76.405556
85.540294	44.552372	76.410561
85.437659	42.603909	76.415566
84.334589	44.869297	76.420570
83.603395	42.219984	76.425575
83.168195	38.654576	76.430580
82.527086	49.940512	76.435585
81.965624	37.953877	76.440590
80.857041	47.382607	76.445594
80.484787	49.558263	76.450599
80.188743	41.061648	76.455604
79.185592	47.344917	76.460609
78.399104	42.214435	76.465614
77.385113	43.983076	76.470618
76.968908	47.422562	76.475623
76.963968	42.940147	76.480628
76.324994	39.938665	76.485633
75.406727	43.406176	76.490638
74.320950	51.650147	76.495642
73.995909	51.356670	76.500647
73.336541	41.058783	76.505652
72.162110	46.807978	76.510657
72.101824	41.116992	76.515662
71.442876	41.293077	76.520666
70.355007	49.056414	76.525671
70.125816	50.255207	76.530676
69.136274	47.128284	76.535681
69.256733	36.335459	76.540686
67.704279	46.582449	76.545690
66.704501	47.896247	76.550695
66.687896	49.993110	76.555700
65.778804	50.753133	76.560705
65.737099	44.035748	76.565710
64.534128	42.584460	76.570714
64.119246	50.243629	76.575719
63.913126	39.925503	76.580724
62.500861	43.725687	76.585729
61.718454	39.958614	76.590734
60.916582	44.733774	76.595738
60.667384	46.684804	76.600743
60.410146	39.863024	76.605748
59.342595	49.026601	76.610753
58.328301	47.775459	76.615758
57.798185	42.689253	76.620762
57.413241	50.629074	76.625767
57.113531	41.603197	76.630772
55.858727	47.308447	76.635777
55.470091	36.196271	76.640782
54.948296	45.638660	76.645786
54.171130	38.928185	76.650791
53.113244	40.919877	76.655796
52.295775	41.053439	76.660801
52.095595	45.183868	76.665806
51.666595	45.941447	76.670810
50.945467	41.869716	76.675815
50.008648	41.661195	76.680820
49.509096	44.552586	76.685825
49.161203	35.834016	76.690830
48.428386	43.331001	76.695834
47.287133	38.583537	76.700839
47.106609	38.828406	76.705844
45.924028	53.575356	76.710849
45.153867	42.492485	76.715854
44.547151	47.545607	76.720858
43.895554	44.185027	76.725863
43.880583	43.810565	76.730868
43.017400	47.967887	76.735873
42.036339	43.388839	76.740878
41.266109	29.980006	76.745882
40.891104	41.420618	76.750887
40.405895	36.188486	76.755892
39.491312	45.538982	76.760897
38.801563	38.395105	76.765902
37.946920	39.523342	76.770906
37.549088	44.890076	76.775911
37.264148	33.274094	76.780916
36.103816	36.625683	76.785921
35.500287	33.214865	76.790926
34.810987	43.909252	76.795930
34.522396	37.835217	76.800935
33.460993	42.924586	76.805940
32.447394	45.847503	76.810945
32.392940	39.977396	76.815950
31.726393	38.405878	76.820954
30.882499	40.570029	76.825959
30.162070	43.006223	76.830964
29.768179	54.760515	76.835969
29.191227	41.935857	76.840974
28.432203	52.332291	76.845978
27.526763	41.791396	76.850983
26.925085	43.029100	76.855988
26.341703	51.057343	76.860993
26.044635	43.065522	76.865998
24.959200	41.535584	76.871002
24.574288	39.707840	76.876007
24.244889	40.039533	76.881012
22.827935	47.882182	76.886017
22.525055	37.617345	76.891022
21.744451	48.726842	76.896026
20.963501	49.275634	76.901031
20.098523	40.355691	76.906036
19.301821	42.603782	76.911041
18.773267	44.014327	76.916046
18.520159	50.777228	76.921050
18.273405	51.609823	76.926055
17.689078	35.246122	76.931060
16.395266	42.695396	76.936065
15.847382	38.905126	76.941070
14.670660	50.120383	76.946074
13.986041	47.722281	76.951079
13.878918	40.334099	76.956084
13.298507	42.713272	76.961089
12.867578	35.491855	76.966094
11.541184	41.853510	76.971098
10.865814	46.416121	76.976103
10.726434	42.311540	76.981108
10.056152	53.956953	76.986113
9.171855	43.609810	76.991118
8.156359	49.686918	76.996122
7.500340	47.134448	77.001127
7.425590	37.528658	77.006132
6.438883	46.830744	77.011137
5.895858	41.902728	77.016142
5.080425	45.550979	77.021147
4.877574	46.441227	77.026151
4.398858	40.195672	77.031156
3.074541	41.073985	77.036161