Fri Mar 05 20:26:32 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.267523	97.503360	0.000000
-0.195970	76.594505	0.005005
-1.101093	53.267708	0.010010
-3.648360	22.844885	0.015014
-7.982791	22.839229	0.020019
-13.082218	26.415394	0.025024
-17.269790	21.204521	0.030029
-21.773708	32.262894	0.035034
-25.849988	22.694556	0.040038
-29.546307	19.097399	0.045043
-33.500765	22.418435	0.050048
-37.037635	20.234020	0.055053
-40.484930	29.062828	0.060058
-43.885203	24.677309	0.065062
-47.820242	21.391068	0.070067
-51.800689	20.567365	0.075072
-55.550775	10.842978	0.080077
-59.501252	24.080757	0.085082
-63.131490	25.233875	0.090086
-66.956767	21.539077	0.095091
-70.593485	34.050324	0.100096
-74.299317	20.887490	0.105101
-78.157036	28.655890	0.110106
-81.847785	31.135430	0.115110
-85.442066	18.137746	0.120115
-89.575683	26.979914	0.125120
-93.106389	23.870514	0.130125
-96.887835	25.257538	0.135130
-100.581164	25.045691	0.140134
-104.318502	27.643082	0.145139
-108.612874	27.309520	0.150144
-111.988232	14.898266	0.155149
-115.951089	22.342877	0.160154
-119.674586	23.089916	0.165158
-123.028924	24.807801	0.170163
-127.094392	28.184546	0.175168
-130.527018	13.393405	0.180173
-134.880245	28.428606	0.185178
-138.485613	23.328482	0.190182
-142.305344	18.210528	0.195187
-146.295138	32.142259	0.200192
-149.116338	13.602989	0.205197
-153.074580	16.961088	0.210202
-156.803772	20.531802	0.215206
-161.085886	22.659546	0.220211
-165.416302	28.030872	0.225216
-168.804932	18.233222	0.230221
-173.093639	21.092158	0.235226
-176.470941	22.731780	0.240230
-179.766433	17.451390	0.245235
-183.917008	23.205628	0.250240
-187.194883	17.354742	0.255245
-191.160132	23.208727	0.260250
-194.362808	15.658534	0.265254
-198.250747	19.126911	0.270259
-202.462667	30.121654	0.275264
-206.222653	18.476810	0.280269
-210.154228	24.614031	0.285274
-214.107428	24.325558	0.290278
-217.290320	23.319659	0.295283
-221.144750	28.703429	0.300288
-224.461856	25.873947	0.305293
-228.718690	28.685318	0.310298
-232.540883	22.632783	0.315302
-236.083643	23.876275	0.320307
-240.171819	25.091702	0.325312
-243.716092	17.867328	0.330317
-247.354441	25.414893	0.335322
-251.322765	21.440453	0.340326
-255.113809	10.999123	0.345331
-259.287212	25.405014	0.350336
-262.619481	18.716104	0.355341
-266.525033	24.857144	0.360346
-270.126727	27.005789	0.365350
-273.482738	18.584483	0.370355
-277.807256	29.198356	0.375360
-281.433143	11.907329	0.380365
-285.400840	25.749003	0.385370
-289.126974	21.726510	0.390374
-292.494175	13.781677	0.395379
-296.478617	27.679659	0.400384
-299.751795	21.403987	0.405389
-303.666882	23.984322	0.410394
-307.510824	29.588898	0.415398
-311.586264	21.004945	0.420403
-315.828544	26.919119	0.425408
-319.070882	25.044494	0.430413
-322.912400	28.887276	0.435418
-326.667413	29.664896	0.440422
-329.907826	15.447351	0.445427
-334.041140	24.313518	0.450432
-337.724570	25.275267	0.455437
-341.759617	26.964924	0.460442
-345.356660	26.410080	0.465446
-348.914200	20.227182	0.470451
-352.975478	26.541449	0.475456
-356.410659	13.471505	0.480461
-360.377388	24.345358	0.485466
-364.091707	19.155748	0.490470
-368.005370	17.563405	0.495475
-371.493501	27.564521	0.500480
-375.009159	20.433551	0.505485
-379.445814	24.147510	0.510490
-383.166640	21.034207	0.515494
-386.749226	16.263566	0.520499
-390.761671	26.531340	0.525504
-394.198246	20.759701	0.530509
-397.897191	24.439490	0.535514
-401.805468	22.354340	0.540518
-405.289792	24.260521	0.545523
-409.477968	28.936212	0.550528
-412.835488	17.139152	0.555533
-416.888867	19.390094	0.560538
-420.721188	19.768625	0.565542
-424.233919	17.573049	0.570547
-428.055603	25.495493	0.575552
-431.670478	19.922689	0.580557
-435.513832	16.792765	0.585562
-439.516465	20.590492	0.590566
-443.106793	17.604679	0.595571
-447.140755	29.924408	0.600576
-450.612942	16.493095	0.605581
-454.526953	23.022125	0.610586
-458.056246	19.052047	0.615590
-461.561737	17.227526	0.620595
-465.619467	27.127341	0.625600
-469.293934	22.557575	0.630605
-473.350470	22.415340	0.635610
-477.001488	19.478693	0.640614
-480.878988	14.853064	0.645619
-485.057790	27.400980	0.650624
-488.416321	24.988489	0.655629
-492.079939	25.821155	0.660634
-495.797302	19.853241	0.665638
-499.488962	15.612695	0.670643
-503.427522	24.723997	0.675648
-506.936657	16.762728	0.680653
-510.682676	22.940170	0.685658
-514.746062	25.303259	0.690662
-518.537888	18.989312	0.695667
-522.385938	21.933023	0.700672
-526.092518	16.892247	0.705677
-529.557170	25.910554	0.710682
-533.057060	20.961353	0.715686
-536.770178	20.149376	0.720691
-541.015089	25.119775	0.725696
-544.775009	20.705702	0.730701
-548.524667	25.451935	0.735706
-552.254882	19.306396	0.740710
-555.722394	20.213491	0.745715
-559.521726	28.304449	0.750720
-563.317438	20.037386	0.755725
-567.182689	26.505190	0.760730
-570.972466	21.853082	0.765734
-574.737986	17.419453	0.770739
-579.086701	20.826419	0.775744
-582.577041	18.146542	0.780749
-586.491432	21.421067	0.785754
-590.205538	24.412874	0.790758
-593.242000	16.529197	0.795763
-597.255276	20.464497	0.800768
-600.921914	13.331192	0.805773
-604.919109	14.113241	0.810778
-608.602192	13.824848	0.815782
-612.075104	17.828389	0.820787
-616.263019	26.009893	0.825792
-619.954708	17.172808	0.830797
-623.924299	13.807901	0.835802
-627.868660	19.001665	0.840806
-631.080451	16.892361	0.845811
-634.612705	23.423763	0.850816
-638.587516	20.062867	0.855821
-642.517829	23.038834	0.860826
-646.512507	25.622975	0.865830
-650.132621	13.866660	0.870835
-654.235652	24.034203	0.875840
-657.577580	19.014225	0.880845
-661.180741	23.724608	0.885850
-665.000477	18.352058	0.890854
-668.810142	24.861600	0.895859
-672.635242	24.279035	0.900864
-676.293885	11.937574	0.905869
-680.093877	21.455932	0.910874
-683.951337	16.471057	0.915878
-687.261252	8.235397	0.920883
-691.428045	19.953838	0.925888
-695.552792	22.099959	0.930893
-698.963430	19.842751	0.935898
-703.214458	27.387947	0.940902
-706.591168	19.377445	0.945907
-710.485006	21.683809	0.950912
-714.175922	16.968834	0.955917
-717.308103	16.352889	0.960922
-721.329617	25.097747	0.965926
-724.789232	24.549903	0.970931
-728.654464	24.781226	0.975936
-732.809613	17.194774	0.980941
-736.921143	20.917352	0.985946
-740.508209	21.736589	0.990950
-743.920873	25.569845	0.995955
-747.903064	27.445698	1.000960
-751.783634	15.207634	1.005965
-755.194093	24.725356	1.010970
-759.229356	20.555905	1.015974
-762.678217	13.826444	1.020979
-767.042429	23.299487	1.025984
-770.382651	27.458664	1.030989
-774.014609	24.204052	1.035994
-778.155874	22.292381	1.040998
-781.461305	17.044407	1.046003
-785.557681	22.199645	1.051008
-789.169109	26.455808	1.056013
-792.950917	24.459905	1.061018
-796.814542	29.019733	1.066022
-800.333105	16.747550	1.071027
-804.092629	29.247896	1.076032
-807.957443	25.092286	1.081037
-811.947652	35.984790	1.086042
-816.015661	30.237439	1.091046
-819.489986	30.105239	1.096051
-823.201975	32.652375	1.101056
-826.656173	24.357976	1.106061
-830.521526	29.391211	1.111066
-834.434014	27.655955	1.116070
-837.835640	25.870587	1.121075
-841.833710	18.240303	1.126080
-845.871011	23.715776	1.131085
-849.284601	19.702572	1.136090
-853.269812	21.285775	1.141094
-856.636186	20.707451	1.146099
-860.437284	27.681112	1.151104
-864.374069	23.740525	1.156109
-868.373156	18.901601	1.161114
-872.375582	29.103880	1.166118
-875.826939	24.626829	1.171123
-879.328270	33.586827	1.176128
-882.822892	20.285950	1.181133
-886.880741	19.676289	1.186138
-890.990071	21.383475	1.191142
-894.398056	16.814368	1.196147
-898.884620	21.387214	1.201152
-902.085672	21.779138	1.206157
-905.755332	12.749780	1.211162
-909.686004	22.454952	1.216166
-913.083598	20.025667	1.221171
-917.263488	21.009335	1.226176
-920.834097	16.732767	1.231181
-924.477096	24.405053	1.236186
-928.431265	28.981144	1.241190
-931.890247	22.436480	1.246195
-935.881412	23.464122	1.251200
-939.449815	15.407356	1.256205
-943.059548	13.847802	1.261210
-947.218592	25.097082	1.266214
-951.022305	21.740905	1.271219
-954.899626	28.551860	1.276224
-958.733795	17.864742	1.281229
-962.258618	23.026656	1.286234
-966.145832	26.994451	1.291238
-969.378873	14.795160	1.296243
-973.668190	24.135167	1.301248
-977.396689	18.083094	1.306253
-980.931928	17.790566	1.311258
-984.747614	16.972044	1.316262
-988.179198	16.472145	1.321267
-992.187133	16.215800	1.326272
-996.090077	14.821484	1.331277
-1000.014118	15.002734	1.336282
-1004.036058	29.191636	1.341286
-1007.593120	17.837407	1.346291
-1011.449659	22.655057	1.351296
-1014.741922	15.114059	1.356301
-1018.518784	16.908643	1.361306
-1022.554237	20.663696	1.366310
-1026.117115	21.351768	1.371315
-1030.377526	20.336368	1.376320
-1033.680457	19.920037	1.381325
-1037.408528	15.872257	1.386330
-1041.165996	18.636733	1.391334
-1044.429820	14.398027	1.396339
-1048.884858	32.945481	1.401344
-1052.515014	26.672800	1.406349
-1056.494338	20.347167	1.411354
-1060.099193	27.403286	1.416358
-1063.968623	23.597348	1.421363
-1068.129408	28.764942	1.426368
-1071.276550	25.993064	1.431373
-1074.883527	29.562983	1.436378
-1078.431693	28.503135	1.441382
-1081.852788	15.924094	1.446387
-1086.237294	22.453688	1.451392
-1090.515785	21.326175	1.456397
-1094.434026	28.113935	1.461402
-1097.862738	35.059939	1.466406
-1101.207729	20.376184	1.471411
-1105.097846	20.482800	1.476416
-1108.712720	20.364049	1.481421
-1112.522851	25.467744	1.486426
-1116.809307	35.304276	1.491430
-1120.307034	28.006026	1.496435
-1124.077174	23.129350	1.501440
-1127.467987	17.838774	1.506445
-1131.022379	14.996513	1.511450
-1135.429626	21.898831	1.516454
-1138.958824	21.531461	1.521459
-1142.882948	27.276322	1.526464
-1146.688770	9.078889	1.531469
-1150.853719	18.542803	1.536474
-1154.249610	22.030187	1.541478
-1157.404906	12.857462	1.546483
-1161.374178	20.700561	1.551488
-1165.181181	19.789486	1.556493
-1169.349683	6.245252	1.561498
-1173.004382	20.388272	1.566502
-1176.486117	7.082675	1.571507
-1180.303860	19.468301	1.576512
-1184.302645	24.269563	1.581517
-1188.037029	20.601500	1.586522
-1191.692176	24.027917	1.591526
-1195.224437	14.797290	1.596531
-1199.384829	19.766355	1.601536
-1203.209291	21.398544	1.606541
-1206.975183	35.794378	1.611546
-1210.319362	30.348231	1.616550
-1214.026598	26.994401	1.621555
-1217.668227	20.838943	1.626560
-1221.595497	21.606117	1.631565
-1225.240769	11.535783	1.636570
-1229.393853	33.777244	1.641574
-1233.049706	22.991112	1.646579
-1237.330771	36.917505	1.651584
-1240.921563	31.644903	1.656589
-1244.225793	30.495814	1.661594
-1247.882605	24.252950	1.666598
-1251.737176	29.789744	1.671603
-1255.832125	31.159382	1.676608
-1259.742576	25.322969	1.681613
-1263.559281	26.506172	1.686618
-1267.220895	22.285712	1.691622
-1270.219935	21.015285	1.696627
-1274.087879	30.763036	1.701632
-1277.924915	23.140879	1.706637
-1281.986206	23.604759	1.711642
-1285.819426	31.306447	1.716646
-1289.383277	28.784481	1.721651
-1293.141670	29.594134	1.726656
-1297.092900	25.076304	1.731661
-1300.788955	31.816224	1.736666
-1304.560683	26.504876	1.741670
-1308.201033	19.926750	1.746675
-1312.300514	23.616850	1.751680
-1316.156774	23.708939	1.756685
-1319.601018	26.666571	1.761690
-1323.478403	35.928648	1.766694
-1326.938030	23.466548	1.771699
-1330.639845	31.719694	1.776704
-1334.285058	26.332955	1.781709
-1338.048052	31.260735	1.786714
-1342.202157	26.499496	1.791718
-1345.757173	25.201466	1.796723
-1349.772208	34.495077	1.801728
-1353.443099	27.393644	1.806733
-1357.114806	30.226896	1.811738
-1361.279936	30.929880	1.816742
-1364.404769	29.771172	1.821747
-1368.479295	32.558536	1.826752
-1372.555623	30.962381	1.831757
-1376.068683	24.695140	1.836762
-1379.730739	28.536105	1.841766
-1383.441894	32.561550	1.846771
-1387.244282	27.474440	1.851776
-1390.843340	26.566719	1.856781
-1394.621107	22.305138	1.861786
-1398.833444	33.029133	1.866790
-1402.551822	19.597782	1.871795
-1405.814463	26.452975	1.876800
-1409.781110	22.617461	1.881805
-1413.083349	20.279308	1.886810
-1417.612833	23.723048	1.891814
-1421.332741	18.331068	1.896819
-1425.071326	25.560517	1.901824
-1428.794514	24.253271	1.906829
-1432.044791	21.936787	1.911834
-1436.088128	35.628343	1.916838
-1439.522325	14.927736	1.921843
-1443.802029	26.424235	1.926848
-1447.610816	21.618946	1.931853
-1450.961765	16.607901	1.936858
-1455.155690	21.789356	1.941862
-1458.754125	24.104846	1.946867
-1462.565755	24.295687	1.951872
-1466.148400	26.159241	1.956877
-1469.885367	21.993754	1.961882
-1473.817080	24.338976	1.966886
-1477.477686	10.807055	1.971891
-1481.223274	18.998047	1.976896
-1485.105376	21.021539	1.981901
-1488.867101	15.027682	1.986906
-1492.456386	20.780995	1.991910
-1496.054761	22.192963	1.996915
-1500.526742	25.227920	2.006912
-1501.510453	22.038143	2.016909
-1498.738970	23.285414	2.026906
-1495.784750	19.722433	2.036902
-1493.720594	22.036644	2.046899
-1491.748361	20.980354	2.056896
-1489.876173	26.415270	2.066893
-1487.910013	18.797931	2.076890
-1486.360634	20.665634	2.086886
-1484.118895	21.268282	2.096883
-1482.273442	23.472261	2.106880
-1480.444218	22.254144	2.116877
-1478.604330	19.554867	2.126874
-1476.843247	19.200285	2.136870
-1474.705356	18.829582	2.146867
-1472.855461	23.053885	2.156864
-1470.837268	21.170790	2.166861
-1468.986445	22.854453	2.176858
-1467.170992	26.937436	2.186854
-1465.289721	26.486252	2.196851
-1463.420731	19.069225	2.206848
-1461.588024	23.968913	2.216845
-1459.835238	21.907273	2.226842
-1457.880257	23.399007	2.236838
-1455.550819	21.215042	2.246835
-1454.010720	26.771053	2.256832
-1452.018121	20.205812	2.266829
-1450.206388	18.096846	2.276826
-1448.602271	23.138932	2.286822
-1446.442932	25.164793	2.296819
-1444.186673	24.370961	2.306816
-1442.757161	17.117468	2.316813
-1440.814504	20.603797	2.326810
-1438.828267	20.333196	2.336806
-1437.135098	20.008465	2.346803
-1435.508018	29.559466	2.356800
-1433.106160	21.997148	2.366797
-1431.306966	23.436478	2.376794
-1429.515775	28.499156	2.386790
-1427.692433	26.375717	2.396787
-1425.714796	30.908029	2.406784
-1423.762063	29.291240	2.416781
-1421.932883	24.550585	2.426778
-1420.119025	25.981261	2.436774
-1418.272797	33.321430	2.446771
-1416.321140	31.068510	2.456768
-1414.618365	23.971807	2.466765
-1412.720156	28.341584	2.476762
-1410.499733	18.079944	2.486758
-1408.876271	21.434246	2.496755
-1407.014272	20.995668	2.506752
-1405.130092	21.166166	2.516749
-1403.319345	25.235745	2.526746
-1401.100978	25.663797	2.536742
-1399.441882	20.370919	2.546739
-1397.358352	20.146357	2.556736
-1395.558498	21.361402	2.566733
-1393.848358	24.280265	2.576730
-1392.001919	24.564183	2.586726
-1390.274062	19.023465	2.596723
-1387.957692	21.450555	2.606720
-1386.203498	18.810855	2.616717
-1384.175835	24.220974	2.626714
-1382.425850	20.715118	2.636710
-1380.762449	25.141457	2.646707
-1378.356207	24.724728	2.656704
-1377.063981	20.303741	2.666701
-1374.961954	20.692020	2.676698
-1373.073969	19.486687	2.686694
-1371.004022	24.634263	2.696691
-1369.498939	23.777590	2.706688
-1367.670286	28.354328	2.716685
-1365.671149	22.500205	2.726682
-1363.685288	23.377611	2.736678
-1361.987632	23.893786	2.746675
-1360.118349	25.680372	2.756672
-1358.028967	22.459677	2.766669
-1356.315838	24.066000	2.776666
-1354.099956	24.630282	2.786662
-1352.443027	33.325532	2.796659
-1350.152305	20.723765	2.806656
-1348.739344	20.625527	2.816653
-1346.891404	22.080807	2.826650
-1344.967811	23.730819	2.836646
-1343.380913	22.712647	2.846643
-1341.331611	23.246763	2.856640
-1339.223386	24.917754	2.866637
-1337.165338	17.187930	2.876634
-1335.647703	21.127639	2.886630
-1333.834262	22.634240	2.896627
-1331.733810	20.397049	2.906624
-1329.969550	22.010997	2.916621
-1327.981070	20.994877	2.926618
-1326.132704	14.939132	2.936614
-1324.194519	19.384690	2.946611
-1322.450418	22.391330	2.956608
-1320.566207	17.105107	2.966605
-1319.086679	14.356261	2.976602
-1316.875672	18.413953	2.986598
-1314.968737	16.686166	2.996595
-1312.935583	13.073462	3.006592
-1311.202733	21.148699	3.016589
-1309.188977	14.041771	3.026586
-1307.354663	19.920269	3.036582
-1305.468569	24.336288	3.046579
-1303.590244	25.908318	3.056576
-1301.660318	18.964809	3.066573
-1299.679816	23.384670	3.076570
-1298.241661	20.173515	3.086566
-1296.173700	24.086756	3.096563
-1294.498654	32.141264	3.106560
-1292.373955	19.812431	3.116557
-1290.415902	25.483250	3.126554
-1288.698725	18.684324	3.136550
-1286.746344	23.261854	3.146547
-1285.073664	22.875776	3.156544
-1283.194195	24.395535	3.166541
-1280.917834	26.900191	3.176538
-1279.240404	19.433427	3.186534
-1277.321780	20.403772	3.196531
-1275.562930	17.927617	3.206528
-1273.673529	20.497362	3.216525
-1271.789377	22.510586	3.226522
-1269.805423	18.744740	3.236518
-1267.880931	23.258856	3.246515
-1266.383100	27.923357	3.256512
-1264.297833	28.399682	3.266509
-1262.258368	18.904486	3.276506
-1260.424286	26.169366	3.286502
-1258.733326	29.160877	3.296499
-1256.893080	23.499634	3.306496
-1254.880256	21.556004	3.316493
-1252.715808	15.992886	3.326490
-1251.183173	24.406526	3.336486
-1248.999545	20.427167	3.346483
-1247.318742	26.821332	3.356480
-1245.915403	18.605826	3.366477
-1243.608615	21.241437	3.376474
-1241.507893	31.866269	3.386470
-1239.843634	26.814245	3.396467
-1237.811456	32.621674	3.406464
-1236.078601	30.034443	3.416461
-1234.102128	28.674536	3.426458
-1232.312202	33.800740	3.436454
-1230.523959	21.958418	3.446451
-1228.605247	23.915623	3.456448
-1226.640741	24.974984	3.466445
-1224.737693	21.419486	3.476442
-1223.124709	22.277731	3.486438
-1221.190480	18.005148	3.496435
-1219.283338	21.816300	3.506432
-1217.168074	17.132652	3.516429
-1215.417676	16.506824	3.526426
-1213.583762	16.500785	3.536422
-1211.606614	20.761790	3.546419
-1209.749269	17.120460	3.556416
-1208.033243	18.609591	3.566413
-1206.420925	18.354806	3.576410
-1204.057515	23.082958	3.586406
-1202.145030	21.635423	3.596403
-1200.020755	23.291343	3.606400
-1198.475503	24.561491	3.616397
-1196.770596	19.902464	3.626394
-1195.015681	20.193288	3.636390
-1193.030377	17.426753	3.646387
-1191.130455	24.261162	3.656384
-1189.209343	22.262788	3.666381
-1187.003815	22.173631	3.676378
-1185.476664	20.546183	3.686374
-1183.744253	20.936931	3.696371
-1181.778580	23.728234	3.706368
-1179.772745	17.064775	3.716365
-1177.665027	21.145448	3.726362
-1176.058429	14.245870	3.736358
-1174.288589	14.366955	3.746355
-1172.154088	26.914327	3.756352
-1170.355027	24.417604	3.766349
-1168.519291	22.638167	3.776346
-1166.763002	18.995668	3.786342
-1164.692083	15.572834	3.796339
-1162.708851	21.553947	3.806336
-1161.040607	23.033389	3.816333
-1159.046467	19.911787	3.826330
-1157.297815	21.923100	3.836326
-1155.523457	27.823955	3.846323
-1153.369874	24.168432	3.856320
-1151.736419	25.959760	3.866317
-1149.965950	23.194471	3.876314
-1147.513388	20.406906	3.886310
-1145.865986	20.748124	3.896307
-1144.500142	24.563831	3.906304
-1142.494329	23.717198	3.916301
-1140.229371	24.095416	3.926298
-1138.454150	21.711477	3.936294
-1136.650720	23.102996	3.946291
-1134.696942	20.559445	3.956288
-1132.795731	20.651651	3.966285
-1131.204461	23.157104	3.976282
-1129.028477	24.102193	3.986278
-1127.109793	24.758447	3.996275
-1125.522149	21.856633	4.006272
-1123.409765	19.009827	4.016269
-1121.411518	17.897583	4.026266
-1119.808057	30.282069	4.036262
-1118.162001	27.091444	4.046259
-1115.987450	24.428908	4.056256
-1114.370883	20.729850	4.066253
-1112.001296	26.039741	4.076250
-1110.271217	16.802573	4.086246
-1108.450855	26.174499	4.096243
-1106.564374	12.478669	4.106240
-1104.737572	25.631115	4.116237
-1102.904583	24.556373	4.126234
-1100.909384	23.656210	4.136230
-1098.855784	16.288865	4.146227
-1097.352019	16.217307	4.156224
-1095.375624	19.471176	4.166221
-1093.374548	22.080052	4.176218
-1091.540575	13.644169	4.186214
-1089.855173	16.237224	4.196211
-1087.773865	18.545905	4.206208
-1085.877601	21.078396	4.216205
-1083.822583	16.822917	4.226202
-1082.274944	15.395941	4.236198
-1080.610161	13.931282	4.246195
-1078.523149	24.956359	4.256192
-1076.749507	18.926957	4.266189
-1074.561106	14.705415	4.276186
-1072.684093	16.112057	4.286182
-1071.136595	24.892926	4.296179
-1069.100013	20.784091	4.306176
-1067.392827	23.863150	4.316173
-1065.438963	20.351754	4.326170
-1063.394335	18.875301	4.336166
-1061.219050	20.186878	4.346163
-1059.677748	17.763043	4.356160
-1057.941167	16.880596	4.366157
-1056.007313	18.205529	4.376154
-1053.826290	25.700887	4.386150
-1052.167305	21.344564	4.396147
-1050.285780	21.310513	4.406144
-1048.339393	19.732944	4.416141
-1046.670165	17.099185	4.426138
-1044.902610	19.737557	4.436134
-1042.618922	17.622893	4.446131
-1041.123283	18.629505	4.456128
-1039.009578	19.570428	4.466125
-1037.123657	11.945743	4.476122
-1035.443517	17.481237	4.486118
-1033.248063	13.438603	4.496115
-1031.686586	15.232053	4.506112
-1029.612987	18.418330	4.516109
-1027.746362	19.428778	4.526106
-1026.013913	24.242238	4.536102
-1024.042647	28.374881	4.546099
-1022.125557	22.824676	4.556096
-1020.233120	19.169983	4.566093
-1018.378065	20.779126	4.576090
-1016.612051	25.123019	4.586086
-1014.837640	19.229325	4.596083
-1012.733688	25.813373	4.606080
-1010.832868	26.807314	4.616077
-1008.862357	26.316964	4.626074
-1007.042175	24.696453	4.636070
-1005.272580	21.402465	4.646067
-1003.606303	19.195520	4.656064
-1001.446828	21.518623	4.666061
-999.573198	24.782695	4.676058
-997.504326	21.229277	4.686054
-996.132913	20.245798	4.696051
-994.331727	31.763513	4.706048
-992.119528	16.886727	4.716045
-990.127806	15.308271	4.726042
-988.377340	16.863112	4.736038
-986.333975	21.617410	4.746035
-984.824069	14.250256	4.756032
-982.647604	23.150088	4.766029
-980.655652	22.672123	4.776026
-978.881281	16.367938	4.786022
-977.290156	23.231389	4.796019
-975.263032	23.470957	4.806016
-973.187847	18.296561	4.816013
-971.524963	20.637519	4.826010
-969.841868	26.679435	4.836006
-967.966594	25.705403	4.846003
-965.748451	24.556549	4.856000
-964.032111	18.310599	4.865997
-962.065547	18.768282	4.875994
-960.146590	20.368834	4.885990
-958.651990	18.287265	4.895987
-956.493559	18.442696	4.905984
-954.456964	24.428100	4.915981
-952.660496	30.513481	4.925978
-950.859144	25.561306	4.935974
-949.203402	30.589198	4.945971
-947.029594	19.937507	4.955968
-945.216349	22.808650	4.965965
-943.111186	24.395234	4.975962
-941.521473	23.048463	4.985958
-939.672041	27.557500	4.995955
-937.853550	25.089422	5.005952
-935.928768	26.987483	5.015949
-933.910846	27.460662	5.025946
-932.139398	21.665393	5.035942
-930.244403	28.398193	5.045939
-928.458470	25.232699	5.055936
-926.272773	26.501688	5.065933
-924.590192	25.650077	5.075930
-922.648089	26.108546	5.085926
-920.789856	23.822020	5.095923
-919.019877	24.200643	5.105920
-917.191910	27.419981	5.115917
-915.036907	22.801289	5.125914
-913.312419	24.838759	5.135910
-911.745635	29.386694	5.145907
-909.569265	23.161967	5.155904
-907.578740	19.215364	5.165901
-905.710454	17.955132	5.175898
-903.979039	21.939910	5.185894
-902.011408	23.403257	5.195891
-900.280942	20.325599	5.205888
-898.379817	19.710646	5.215885
-896.327481	22.853077	5.225882
-894.518031	21.532786	5.235878
-892.680334	19.116935	5.245875
-890.824028	24.082806	5.255872
-888.951327	21.403994	5.265869
-887.062341	17.377325	5.275866
-885.379559	19.449904	5.285862
-883.360991	21.375647	5.295859
-881.481328	21.793605	5.305856
-879.267667	26.023415	5.315853
-877.722851	27.720164	5.325850
-875.848683	23.108505	5.335846
-874.051380	24.695420	5.345843
-872.097731	25.977870	5.355840
-870.207386	20.266268	5.365837
-868.033400	18.718777	5.375834
-866.072965	20.889090	5.385830
-864.551368	26.137435	5.395827
-862.896938	21.360388	5.405824
-860.975238	28.406347	5.415821
-859.044953	22.487842	5.425818
-856.896988	20.202419	5.435814
-855.127854	21.969113	5.445811
-853.550139	26.966918	5.455808
-851.621671	22.744491	5.465805
-849.328508	16.395360	5.475802
-847.382054	19.341603	5.485798
-845.788397	17.490584	5.495795
-844.133379	18.317111	5.505792
-841.973334	21.396585	5.515789
-840.152036	17.994979	5.525786
-838.327268	19.181217	5.535782
-836.036142	17.501347	5.545779
-834.665101	22.148518	5.555776
-832.919613	24.651637	5.565773
-830.512550	19.099049	5.575770
-828.942595	20.373392	5.585766
-827.092062	19.543952	5.595763
-825.041363	21.988818	5.605760
-823.174993	18.092127	5.615757
-821.364885	24.688591	5.625754
-819.580062	13.233922	5.635750
-817.543124	20.769916	5.645747
-815.592162	24.970725	5.655744
-813.937291	21.703105	5.665741
-811.816776	26.587341	5.675738
-810.169071	20.762986	5.685734
-808.224627	21.521174	5.695731
-806.569902	25.974602	5.705728
-804.680025	19.975756	5.715725
-802.743161	23.758830	5.725722
-800.640156	22.342744	5.735718
-798.907883	21.042756	5.745715
-797.037698	18.069155	5.755712
-795.143702	19.530151	5.765709
-793.159499	18.028849	5.775706
-791.409416	20.554949	5.785702
-789.414335	24.734519	5.795699
-787.730611	23.636507	5.805696
-785.713620	18.007358	5.815693
-783.760492	17.204186	5.825690
-782.002656	16.762226	5.835686
-780.250243	15.986398	5.845683
-778.371991	20.824118	5.855680
-776.289374	19.011841	5.865677
-774.224944	16.594579	5.875674
-772.627386	12.655626	5.885670
-770.771564	22.208495	5.895667
-768.885887	22.137691	5.905664
-766.950764	17.109007	5.915661
-765.323455	19.746326	5.925658
-763.062455	16.612400	5.935654
-761.581816	21.977887	5.945651
-759.324934	25.182491	5.955648
-757.408387	26.433073	5.965645
-755.484147	25.885592	5.975642
-753.955690	26.403990	5.985638
-752.391175	29.973458	5.995635
-750.053356	26.105689	6.005632
-748.156885	26.086860	6.015629
-746.221239	19.507586	6.025626
-744.358926	21.028950	6.035622
-742.664718	27.018741	6.045619
-740.700804	29.261238	6.055616
-738.787032	24.093881	6.065613
-736.851910	23.429413	6.075610
-735.199959	21.205993	6.085606
-733.193818	23.440169	6.095603
-731.109429	28.633411	6.105600
-729.537910	23.238122	6.115597
-727.873201	19.002676	6.125594
-725.822605	22.766064	6.135590
-723.673427	19.547411	6.145587
-721.917610	18.494767	6.155584
-720.176409	24.898643	6.165581
-718.048784	22.573962	6.175578
-716.008615	19.058525	6.185574
-714.631940	24.465922	6.195571
-712.749555	25.715684	6.205568
-710.704992	23.031651	6.215565
-708.704244	16.833582	6.225562
-706.926366	28.067908	6.235558
-705.036546	26.812285	6.245555
-703.297667	22.353425	6.255552
-701.478416	28.694320	6.265549
-699.396995	19.522849	6.275546
-697.325334	22.736583	6.285542
-695.699245	19.961535	6.295539
-693.813680	20.492385	6.305536
-691.971510	16.855448	6.315533
-689.971344	24.250598	6.325530
-688.264058	23.780468	6.335526
-686.247287	24.512991	6.345523
-684.370192	25.810990	6.355520
-682.446325	25.018891	6.365517
-680.646133	20.177620	6.375514
-678.747749	21.255905	6.385510
-676.907930	20.278293	6.395507
-675.120680	24.115383	6.405504
-673.201883	21.393055	6.415501
-671.187409	16.140188	6.425498
-669.572681	17.571695	6.435494
-667.527062	19.228043	6.445491
-665.504041	23.256417	6.455488
-663.735711	15.486574	6.465485
-661.702568	12.861250	6.475482
-660.116985	18.118460	6.485478
-658.364805	20.197487	6.495475
-656.146308	21.679383	6.505472
-654.368997	18.910201	6.515469
-652.545971	18.118448	6.525466
-650.689900	17.634048	6.535462
-648.852085	23.979915	6.545459
-647.157254	18.645502	6.555456
-645.073298	21.683635	6.565453
-642.907752	12.880876	6.575450
-640.975221	24.448969	6.585446
-639.424064	14.721212	6.595443
-637.665651	22.515032	6.605440
-635.731862	17.560871	6.615437
-633.666921	23.903623	6.625434
-632.048508	19.230374	6.635430
-629.883018	21.892338	6.645427
-627.916582	19.222435	6.655424
-626.300903	20.028560	6.665421
-624.095677	21.571027	6.675418
-622.533272	25.805657	6.685414
-620.799872	26.408243	6.695411
-618.995546	25.191609	6.705408
-616.974430	23.428766	6.715405
-614.838558	19.768650	6.725402
-613.034455	25.155198	6.735398
-611.300091	24.489746	6.745395
-609.486906	28.471166	6.755392
-607.311530	27.777897	6.765389
-605.788082	28.707717	6.775386
-603.535321	22.619468	6.785382
-601.801800	23.422575	6.795379
-600.071519	29.169875	6.805376
-597.938186	23.635971	6.815373
-596.352751	25.386419	6.825370
-594.630251	24.609189	6.835366
-592.461117	20.237991	6.845363
-590.664869	24.487394	6.855360
-588.523396	25.277449	6.865357
-586.775911	23.651499	6.875354
-585.031723	13.543991	6.885350
-583.207344	22.001527	6.895347
-581.328695	21.974625	6.905344
-579.494145	23.701082	6.915341
-577.526707	19.437904	6.925338
-575.378095	22.022090	6.935334
-573.624844	20.526281	6.945331
-571.844898	21.614098	6.955328
-569.812717	16.480061	6.965325
-568.234389	20.919026	6.975322
-566.406348	20.500747	6.985318
-564.318193	24.054599	6.995315
-562.290583	24.794970	7.005312
-560.435923	28.400333	7.015309
-558.727726	27.900150	7.025306
-556.965574	29.227663	7.035302
-554.777398	21.526618	7.045299
-553.188698	21.583946	7.055296
-551.287831	22.952464	7.065293
-549.309716	17.899710	7.075290
-547.543047	12.575995	7.085286
-545.442167	19.424665	7.095283
-543.838573	22.891720	7.105280
-542.040016	25.887111	7.115277
-539.926502	28.472200	7.125274
-538.085690	25.280854	7.135270
-535.912365	25.814818	7.145267
-534.490181	22.924020	7.155264
-532.427362	18.945644	7.165261
-530.405740	18.450685	7.175258
-528.682375	21.369674	7.185254
-526.697259	25.890542	7.195251
-525.053759	29.458607	7.205248
-523.114236	25.722559	7.215245
-521.147823	23.070112	7.225242
-519.275598	25.527967	7.235238
-517.143003	20.655828	7.245235
-515.778401	27.893700	7.255232
-514.090548	24.690484	7.265229
-511.820521	29.252706	7.275226
-509.695337	28.417541	7.285222
-507.820365	25.733919	7.295219
-506.022571	29.409987	7.305216
-504.474430	30.365930	7.315213
-502.490684	24.000206	7.325210
-500.527265	25.125092	7.335206
-498.567141	20.225250	7.345203
-496.677219	27.090292	7.355200
-495.009926	19.766167	7.365197
-492.963321	20.400933	7.375194
-491.031253	18.846626	7.385190
-489.258113	19.662435	7.395187
-487.678283	29.450689	7.405184
-485.749153	25.091067	7.415181
-483.488312	24.649525	7.425178
-481.509202	18.414033	7.435174
-480.012848	17.139316	7.445171
-478.023994	22.035418	7.455168
-475.796004	26.084915	7.465165
-474.308320	26.981058	7.475162
-472.623024	24.774594	7.485158
-470.665412	28.002011	7.495155
-468.704888	20.713181	7.505152
-466.453325	20.022083	7.515149
-464.873342	17.702969	7.525146
-462.919422	16.865194	7.535142
-461.238276	21.167817	7.545139
-459.527141	19.410394	7.555136
-457.340475	23.843875	7.565133
-455.337242	22.230864	7.575130
-453.707260	19.363773	7.585126
-451.710334	20.014403	7.595123
-449.910839	18.593403	7.605120
-447.932736	17.112306	7.615117
-446.063957	21.462347	7.625114
-444.103240	23.047185	7.635110
-442.505776	20.472662	7.645107
-440.449207	29.390617	7.655104
-438.542546	26.924619	7.665101
-436.734024	19.480084	7.675098
-435.121103	23.136779	7.685094
-433.041921	27.481658	7.695091
-431.392354	26.105138	7.705088
-428.999946	22.050534	7.715085
-427.426556	15.647761	7.725082
-425.266612	20.796065	7.735078
-423.360437	24.320682	7.745075
-421.950434	23.290314	7.755072
-419.882091	27.156935	7.765069
-417.993880	23.580741	7.775066
-415.964204	25.863540	7.785062
-414.247010	19.510444	7.795059
-412.153859	24.102584	7.805056
-410.429636	24.395737	7.815053
-408.739417	22.125373	7.825050
-406.989209	21.245959	7.835046
-405.088639	28.745697	7.845043
-403.113774	28.272521	7.855040
-400.976943	25.997171	7.865037
-398.980074	30.412066	7.875034
-397.155920	23.478218	7.885030
-395.301944	21.833824	7.895027
-393.842802	24.305627	7.905024
-391.834061	28.120211	7.915021
-389.541832	25.633745	7.925018
-388.088933	25.359179	7.935014
-386.012262	27.260291	7.945011
-384.248650	27.444543	7.955008
-382.331006	28.027362	7.965005
-380.530728	20.712075	7.975002
-378.639898	25.098127	7.984998
-376.964239	27.052216	7.994995
-375.055920	23.472844	8.004992
-372.615949	22.728070	8.014989
-370.754944	29.413102	8.024986
-369.349804	20.613537	8.034982
-367.426451	22.719141	8.044979
-365.426442	26.843037	8.054976
-363.589410	28.171373	8.064973
-361.525306	20.168191	8.074970
-359.673457	22.507849	8.084966
-357.911417	23.148687	8.094963
-355.834599	18.167166	8.104960
-354.061694	20.881010	8.114957
-352.613767	23.812525	8.124954
-350.833200	19.906197	8.134950
-348.435809	19.138245	8.144947
-346.571484	21.313290	8.154944
-344.814972	30.595028	8.164941
-342.845087	27.965852	8.174938
-341.106930	22.062614	8.184934
-339.246229	22.502979	8.194931
-337.189803	11.943149	8.204928
-335.350983	23.466488	8.214925
-333.403626	12.110914	8.224922
-331.895581	16.602317	8.234918
-329.774798	17.010645	8.244915
-327.730191	18.429031	8.254912
-326.308773	21.350583	8.264909
-324.303140	21.592561	8.274906
-322.505235	20.302961	8.284902
-320.187043	16.002941	8.294899
-318.273385	19.119081	8.304896
-316.632713	21.093008	8.314893
-314.951171	21.486200	8.324890
-313.082222	22.297901	8.334886
-310.918388	21.943058	8.344883
-309.112375	18.493751	8.354880
-307.290474	23.014022	8.364877
-305.280836	15.164843	8.374874
-303.501274	16.211871	8.384870
-301.583939	19.047964	8.394867
-299.700622	29.152657	8.404864
-298.058098	22.516290	8.414861
-295.963842	19.624142	8.424858
-294.065655	27.016989	8.434854
-292.413991	18.950219	8.444851
-290.519047	17.791997	8.454848
-288.454831	21.201499	8.464845
-286.524085	20.054933	8.474842
-284.558746	20.707587	8.484838
-282.861037	24.311384	8.494835
-281.266492	26.665331	8.504832
-279.032735	19.655136	8.514829
-277.230319	21.085379	8.524826
-275.179905	18.634458	8.534822
-273.688517	18.595398	8.544819
-271.911073	21.035422	8.554816
-269.693639	21.758378	8.564813
-267.634640	18.789775	8.574810
-266.257512	17.152112	8.584807
-264.077955	16.303748	8.594803
-262.104143	19.402439	8.604800
-260.105312	25.272933	8.614797
-258.625737	17.532072	8.624794
-256.734809	21.962419	8.634791
-254.655690	14.675347	8.644787
-252.857115	16.273591	8.654784
-251.153852	24.395479	8.664781
-249.084817	23.899505	8.674778
-247.081621	19.761928	8.684775
-245.060317	14.096200	8.694771
-243.280552	14.835346	8.704768
-241.541045	17.491447	8.714765
-239.766827	11.928315	8.724762
-237.914440	7.426396	8.734759
-236.169300	16.435293	8.744755
-233.811962	17.931745	8.754752
-232.129474	16.027473	8.764749
-230.519240	15.246314	8.774746
-228.607547	14.691783	8.784743
-226.447328	21.913394	8.794739
-224.863245	12.821661	8.804736
-222.788496	21.536392	8.814733
-220.850649	16.011895	8.824730
-218.927918	18.652984	8.834727
-217.179725	12.329808	8.844723
-215.765832	7.520514	8.854720
-213.308960	5.345833	8.864717
-211.742254	9.270586	8.874714
-209.661987	14.864440	8.884711
-207.649011	9.132177	8.894707
-206.004619	5.091369	8.904704
-204.102920	10.358459	8.914701
-202.235855	13.940025	8.924698
-200.246224	15.414661	8.934695
-198.614146	17.851096	8.944691
-196.981390	13.130042	8.954688
-194.606274	10.925794	8.964685
-192.598907	14.036557	8.974682
-190.781423	10.440242	8.984679
-189.330115	19.593963	8.994675
-187.578429	15.962359	9.004672
-184.942978	15.065002	9.014669
-183.411476	17.394338	9.024666
-181.694781	16.381485	9.034663
-179.775668	10.580536	9.044659
-177.709757	15.278289	9.054656
-176.041492	16.289488	9.064653
-173.997427	19.673887	9.074650
-172.275092	9.068016	9.084647
-170.053466	14.596719	9.094643
-168.409010	17.326464	9.104640
-166.616673	21.527880	9.114637
-164.735994	20.070451	9.124634
-162.798739	13.030300	9.134631
-161.331995	17.746304	9.144627
-159.144043	22.817762	9.154624
-156.890028	11.648641	9.164621
-155.189705	12.547371	9.174618
-153.639315	15.124766	9.184615
-151.478627	18.563207	9.194611
-149.646170	15.318217	9.204608
-147.740206	25.211008	9.214605
-146.133784	24.365775	9.224602
-143.866300	25.166125	9.234599
-142.237301	23.461501	9.244595
-140.455582	15.939336	9.254592
-138.222042	19.015640	9.264589
-136.497479	18.061563	9.274586
-134.843379	17.901891	9.284583
-132.776597	22.342179	9.294579
-131.040988	25.711094	9.304576
-128.996139	22.796968	9.314573
-127.083392	27.793946	9.324570
-125.022832	27.053112	9.334567
-123.135742	27.868384	9.344563
-121.763659	25.058443	9.354560
-120.037145	28.866188	9.364557
-117.857654	24.369004	9.374554
-115.687889	27.266032	9.384551
-114.000140	27.059952	9.394547
-112.168217	24.173494	9.404544
-110.474270	25.738013	9.414541
-108.516431	23.226208	9.424538
-106.664069	24.005980	9.434535
-104.555504	29.909635	9.444531
-102.802310	26.920480	9.454528
-100.911315	30.927789	9.464525
-99.188270	31.773988	9.474522
-96.977689	33.702940	9.484519
-95.029100	29.479455	9.494515
-93.500862	22.300916	9.504512
-91.726117	21.402023	9.514509
-89.282193	23.832178	9.524506
-87.827095	17.835317	9.534503
-85.947544	29.641334	9.544499
-84.184719	23.527486	9.554496
-81.931735	24.473893	9.564493
-80.240301	34.129394	9.574490
-78.460122	26.498563	9.584487
-76.357934	24.246387	9.594483
-74.799432	27.027807	9.604480
-72.868196	24.926064	9.614477
-70.896223	22.800455	9.624474
-68.742178	22.314758	9.634471
-67.056423	22.333240	9.644467
-65.105885	29.384776	9.654464
-63.615283	29.186497	9.664461
-61.738963	24.210353	9.674458
-59.375768	22.767611	9.684455
-57.699441	26.150776	9.694451
-56.025542	25.844314	9.704448
-53.969687	20.334272	9.714445
-52.416781	23.356600	9.724442
-50.156421	22.574484	9.734439
-48.413785	24.333387	9.744435
-46.417751	25.769238	9.754432
-44.654900	22.873320	9.764429
-42.447277	23.256998	9.774426
-40.802023	21.006686	9.784423
-39.095864	20.246667	9.794419
-37.163620	27.269566	9.804416
-35.428733	31.159725	9.814413
-33.038879	20.867454	9.824410
-31.503549	32.388954	9.834407
-29.320923	30.270830	9.844403
-27.500214	28.870439	9.854400
-25.876391	22.361957	9.864397
-24.293930	23.044316	9.874394
-22.264799	25.457018	9.884391
-20.244032	27.019999	9.894387
-18.418498	30.832554	9.904384
-16.240332	27.159881	9.914381
-14.399612	25.317359	9.924378
-12.802633	22.713185	9.934375
-10.779060	27.643636	9.944371
-9.309502	28.175066	9.954368
-7.099468	33.195783	9.964365
-5.315541	28.763364	9.974362
-3.467905	38.878756	9.984359
-2.406748	66.107610	9.994355
-0.970934	106.802157	10.004352
0.000000	145.702035	10.009357
0.602717	181.454741	10.014362
1.106778	191.714443	10.019367
1.640397	222.499829	10.024371
2.106808	239.287866	10.029376
2.187838	253.440787	10.034381
2.205591	274.745876	10.039386
2.641212	282.737848	10.044391
2.489857	287.940754	10.049395
2.759463	288.698866	10.054400
3.027708	303.843849	10.059405
3.329909	320.527284	10.064410
3.715456	330.459055	10.069415
3.436446	343.005785	10.074419
3.341566	332.877864	10.079424
3.309134	331.640401	10.084429
3.344562	344.649496	10.089434
3.771357	350.001489	10.094439
3.455151	354.827006	10.099443
3.659145	352.723922	10.104448
3.768283	352.632413	10.109453
3.647421	360.921345	10.114458
4.213742	358.195915	10.119463
3.915908	368.454330	10.124467
3.977698	356.309688	10.129472
3.945490	349.803526	10.134477
3.771712	345.849407	10.139482
3.891618	351.622511	10.144487
4.143976	369.894078	10.149491
4.232009	364.811662	10.154496
4.056323	369.909666	10.159501
3.909568	374.301304	10.164506
4.403134	364.744990	10.169511
4.222779	371.988423	10.174515
4.272734	365.451802	10.179520
4.083705	367.352256	10.184525
4.495901	366.485427	10.189530
4.897342	372.055939	10.194535
4.597848	372.505850	10.199539
4.438502	359.007163	10.204544
4.632761	363.029013	10.209549
4.543013	367.304323	10.214554
4.445684	370.743470	10.219559
4.400725	383.557262	10.224563
4.466547	388.716103	10.229568
4.490501	382.142620	10.234573
4.433158	381.681843	10.239578
4.713507	385.885514	10.244583
4.634530	396.022308	10.249587
4.680177	386.154216	10.254592
4.729710	395.045203	10.259597
4.804797	416.972147	10.264602
5.157882	405.856504	10.269607
5.129168	426.095305	10.274611
5.001534	423.695015	10.279616
5.088220	431.745877	10.284621
5.271636	422.623776	10.289626
5.558708	422.806667	10.294631
5.104972	427.750339	10.299635
5.393273	432.231881	10.304640
5.415936	435.008497	10.309645
5.238505	435.353785	10.314650
5.616080	427.798194	10.319655
5.107715	437.880497	10.324659
5.271266	434.211603	10.329664
5.061842	432.508765	10.334669
5.057108	444.756367	10.339674
5.566875	451.326786	10.344679
5.431135	468.600644	10.349683
5.819963	469.874350	10.354688
6.018491	483.452079	10.359693
5.319270	490.658475	10.364698
5.708663	482.449676	10.369703
5.412792	490.962141	10.374707
5.614048	480.689112	10.379712
6.065339	499.460557	10.384717
6.182441	515.647025	10.389722
6.383706	515.220693	10.394727
6.258697	524.860282	10.399731
6.645394	520.741027	10.404736
6.365727	496.072666	10.409741
6.007313	494.601746	10.414746
6.499317	505.909138	10.419751
6.813267	515.895035	10.424755
6.251961	495.278724	10.429760
6.151967	513.844795	10.434765
6.454221	519.368105	10.439770
6.575560	510.651674	10.444775
6.407643	529.851509	10.449779
6.595075	529.435268	10.454784
6.442070	527.272400	10.459789
6.474042	535.661638	10.464794
6.828932	534.140026	10.469799
6.630143	534.804120	10.474803
6.392557	531.404189	10.479808
6.819320	544.213850	10.484813
6.858323	562.898167	10.489818
7.245684	563.937143	10.494823
6.824851	575.705580	10.499827
7.293052	568.860880	10.504832
7.363098	568.854455	10.509837
7.338192	575.929689	10.514842
7.225165	571.111087	10.519847
7.214527	579.981821	10.524851
7.264749	571.809721	10.529856
7.319371	577.919766	10.534861
7.151800	585.503474	10.539866
7.235882	580.249720	10.544871
7.098491	586.467667	10.549875
7.299580	581.381337	10.554880
7.392627	577.330979	10.559885
7.154489	596.947390	10.564890
7.458506	591.177570	10.569895
7.249269	606.438450	10.574899
7.541098	615.439165	10.579904
7.563413	610.116402	10.584909
7.766146	616.094817	10.589914
8.090338	611.800209	10.594919
7.833153	623.303668	10.599923
7.738436	625.245885	10.604928
7.946131	616.313761	10.609933
7.875936	627.928542	10.614938
7.987228	612.255137	10.619943
8.143688	631.659633	10.624947
8.514427	644.333234	10.629952
8.033733	637.119434	10.634957
8.122391	648.346184	10.639962
8.482675	650.982259	10.644967
8.476985	653.588392	10.649971
8.409560	651.146920	10.654976
8.541338	653.727975	10.659981
8.259469	657.035767	10.664986
8.468339	659.878926	10.669991
8.385380	663.722717	10.674995
8.405521	664.159505	10.680000
8.671693	667.674791	10.685005
8.318578	665.559590	10.690010
8.966783	659.562954	10.695015
8.502833	667.643420	10.700019
8.624569	666.953792	10.705024
8.831970	670.790701	10.710029
8.624098	679.051112	10.715034
9.014709	689.960067	10.720039
9.434908	689.314302	10.725043
9.165387	698.555993	10.730048
9.258125	699.906908	10.735053
8.926763	693.172328	10.740058
9.370489	692.615854	10.745063
9.367793	709.170163	10.750067
8.893703	703.035528	10.755072
9.138336	704.682350	10.760077
8.972463	710.922239	10.765082
9.115775	710.814239	10.770087
9.240434	714.323721	10.775091
9.098329	707.965818	10.780096
9.304203	705.491787	10.785101
9.279321	745.802614	10.790106
9.680813	747.623126	10.795111
9.934738	774.628460	10.800115
9.840432	774.712905	10.805120
10.126282	774.296731	10.810125
10.037345	778.570454	10.815130
10.163157	744.597257	10.820135
9.737461	740.304725	10.825139
9.795146	731.918448	10.830144
9.979057	744.238720	10.835149
9.837390	756.931065	10.840154
10.174033	753.494691	10.845159
10.355526	758.389201	10.850163
10.402027	759.553522	10.855168
10.447974	756.628731	10.860173
10.258364	761.861561	10.865178
10.417707	759.648842	10.870183
10.320854	766.057527	10.875187
10.389351	763.469773	10.880192
10.508786	769.966971	10.885197
9.905136	765.423681	10.890202
10.376554	758.650924	10.895207
10.275509	761.552994	10.900211
10.281169	770.375511	10.905216
10.448658	765.679268	10.910221
10.135769	770.386116	10.915226
10.370001	769.311097	10.920231
10.371886	788.782247	10.925235
10.184467	789.463462	10.930240
10.774435	791.618212	10.935245
10.383355	795.258857	10.940250
10.823129	794.535847	10.945255
11.161488	797.129712	10.950259
10.854173	819.266493	10.955264
11.044278	816.042720	10.960269
10.877073	827.993268	10.965274
11.657223	819.274084	10.970279
11.360621	828.873430	10.975283
11.133065	834.910312	10.980288
11.072979	831.206020	10.985293
10.952008	839.651367	10.990298
11.412450	828.565590	10.995303
11.021901	836.328500	11.000307
11.119159	833.296157	11.005312
11.368133	829.605655	11.010317
11.247459	840.064813	11.015322
11.736769	845.626227	11.020327
11.534867	865.782871	11.025331
11.492947	866.595433	11.030336
11.688447	871.218075	11.035341
11.461923	871.993845	11.040346
11.704330	868.395848	11.045351
11.628093	869.445706	11.050355
11.359526	874.770021	11.055360
11.544432	868.333082	11.060365
11.450764	885.935055	11.065370
12.145466	892.080348	11.070375
12.155244	906.986474	11.075379
12.110333	900.007404	11.080384
12.113332	899.306740	11.085389
12.062803	904.536363	11.090394
12.287901	904.983049	11.095399
12.371732	909.973615	11.100403
12.183411	909.551058	11.105408
12.341510	905.529660	11.110413
12.186261	907.989373	11.115418
12.548488	904.001654	11.120423
12.285433	908.366267	11.125427
12.182026	908.682411	11.130432
12.556838	929.991441	11.135437
12.696015	932.459396	11.140442
12.913350	934.810801	11.145447
12.832779	939.961646	11.150451
12.745321	941.991061	11.155456
12.938486	943.993067	11.160461
12.620845	941.102572	11.165466
13.088660	928.712914	11.170471
12.818128	948.101562	11.175475
12.687686	938.854145	11.180480
13.209318	942.279868	11.185485
12.876340	945.371937	11.190490
12.978958	939.151530	11.195495
12.959689	945.077963	11.200499
12.913990	946.685958	11.205504
12.954746	952.859877	11.210509
13.062397	979.679175	11.215514
13.435288	978.023755	11.220519
13.141762	982.956252	11.225523
13.480331	980.312771	11.230528
13.408205	984.990750	11.235533
13.104230	989.735671	11.240538
13.339125	988.897087	11.245543
13.393347	991.921103	11.250547
13.208528	986.191244	11.255552
13.440569	999.535442	11.260557
13.583626	1026.934263	11.265562
14.023959	1024.149956	11.270567
13.660749	1033.608663	11.275571
13.711317	1028.613997	11.280576
13.989131	1030.528394	11.285581
13.790903	1032.788389	11.290586
13.772923	1028.135836	11.295591
14.191499	1018.881234	11.300595
14.127395	1026.193187	11.305600
14.312800	1027.633437	11.310605
13.991830	1032.243880	11.315610
14.203064	1019.196437	11.320615
14.178971	1034.896618	11.325619
14.271890	1033.512938	11.330624
14.099630	1032.166821	11.335629
14.488483	1055.624886	11.340634
14.588557	1056.957316	11.345639
14.667241	1054.959279	11.350643
14.811381	1061.001631	11.355648
14.925719	1049.349532	11.360653
14.147008	1043.826340	11.365658
14.811521	1050.137375	11.370663
14.693503	1068.891542	11.375667
14.786014	1071.822731	11.380672
14.917354	1077.542259	11.385677
15.165080	1089.310142	11.390682
14.721517	1067.698041	11.395687
14.996746	1064.905364	11.400691
14.869347	1068.295852	11.405696
15.157503	1059.473635	11.410701
15.016603	1064.834431	11.415706
15.106097	1060.014907	11.420711
15.075260	1066.216063	11.425715
15.029314	1071.892897	11.430720
15.079376	1061.503217	11.435725
14.824958	1062.633549	11.440730
15.029810	1064.185827	11.445735
15.282421	1066.086900	11.450739
15.314902	1077.406526	11.455744
15.411598	1092.483494	11.460749
15.269069	1100.312648	11.465754
15.195307	1095.143812	11.470759
15.475962	1102.616873	11.475763
15.217285	1102.804811	11.480768
15.209495	1098.732542	11.485773
15.218833	1100.751272	11.490778
15.541571	1114.707200	11.495783
15.663946	1134.011353	11.500787
15.812903	1132.757507	11.505792
15.767444	1126.604794	11.510797
15.629623	1133.461749	11.515802
15.940556	1130.800570	11.520807
15.753083	1143.872741	11.525811
15.805410	1137.445790	11.530816
16.021896	1133.698888	11.535821
16.298313	1143.897800	11.540826
16.330163	1152.476660	11.545831
16.446342	1140.500897	11.550835
16.017985	1138.976403	11.555840
16.420730	1147.557612	11.560845
16.254607	1156.625395	11.565850
16.639405	1165.286752	11.570855
16.620850	1162.738045	11.575859
16.472964	1170.053970	11.580864
16.646281	1161.469219	11.585869
16.411468	1167.397001	11.590874
16.837224	1169.458143	11.595879
16.701979	1172.409906	11.600883
16.627100	1175.094981	11.605888
16.843586	1166.419758	11.610893
16.734343	1175.573105	11.615898
16.942823	1175.330121	11.620903
16.854559	1162.555836	11.625907
16.819866	1173.365820	11.630912
16.585161	1165.573166	11.635917
16.785702	1176.126424	11.640922
16.976003	1162.760471	11.645927
16.585878	1179.713019	11.650931
16.709188	1190.207637	11.655936
17.194753	1199.010650	11.660941
16.998948	1213.613963	11.665946
17.150766	1205.562509	11.670951
17.177176	1203.897664	11.675955
17.390706	1210.793243	11.680960
17.371364	1210.668601	11.685965
17.214230	1213.510314	11.690970
17.384835	1217.662342	11.695975
17.212825	1228.254553	11.700979
17.481167	1239.602925	11.705984
17.586322	1238.169963	11.710989
17.540492	1248.600129	11.715994
18.028891	1239.556619	11.720999
17.997701	1243.827577	11.726003
17.624498	1247.460750	11.731008
17.774913	1247.698569	11.736013
18.035515	1242.429041	11.741018
18.132311	1238.873102	11.746023
17.950051	1244.043426	11.751027
17.835001	1242.274973	11.756032
18.292984	1232.487212	11.761037
18.012966	1251.444082	11.766042
17.980509	1241.613100	11.771047
18.265342	1241.532992	11.776051
18.233369	1242.060117	11.781056
18.622359	1235.752906	11.786061
18.113702	1244.968421	11.791066
18.401218	1251.915302	11.796071
18.181283	1250.083145	11.801075
18.476414	1267.675613	11.806080
18.898121	1268.488377	11.811085
18.415555	1265.283472	11.816090
18.561062	1272.959540	11.821095
18.929675	1280.273575	11.826099
18.708748	1282.407908	11.831104
18.594556	1276.874843	11.836109
18.663994	1287.657265	11.841114
18.977499	1273.714854	11.846119
19.154700	1281.433183	11.851123
18.896367	1283.552981	11.856128
18.964583	1281.398876	11.861133
18.715826	1285.031135	11.866138
18.732579	1281.976844	11.871143
19.035955	1284.614228	11.876147
18.789088	1285.382223	11.881152
18.836905	1287.022653	11.886157
18.938389	1287.455949	11.891162
19.354258	1297.117025	11.896167
19.352624	1312.063236	11.901171
19.068880	1318.175515	11.906176
19.610231	1311.482822	11.911181
19.476790	1304.303196	11.916186
19.563670	1320.701978	11.921191
19.559557	1315.988769	11.926195
19.662389	1319.309477	11.931200
19.642601	1316.161650	11.936205
19.660013	1323.202110	11.941210
19.902183	1315.055755	11.946215
20.000996	1318.304558	11.951219
19.485987	1314.953417	11.956224
19.759778	1316.819604	11.961229
19.569617	1315.471584	11.966234
19.539175	1312.445315	11.971239
19.638323	1318.882911	11.976243
19.663634	1326.278532	11.981248
20.238528	1331.619890	11.986253
20.036245	1348.637300	11.991258
20.367027	1351.656711	11.996263
20.649564	1350.133942	12.001267
20.390212	1340.236570	12.006272
20.230317	1323.839979	12.011277
20.236342	1324.717465	12.016282
20.375743	1333.020638	12.021287
20.242625	1325.348901	12.026291
20.236973	1327.896797	12.031296
20.851008	1329.396461	12.036301
20.269941	1331.231820	12.041306
20.272096	1320.717120	12.046311
20.231889	1328.790295	12.051315
20.140363	1324.650887	12.056320
20.461850	1322.035303	12.061325
20.170395	1317.645487	12.066330
20.235129	1323.232221	12.071335
20.364232	1323.722619	12.076339
20.473387	1324.859646	12.081344
20.521994	1320.373012	12.086349
20.382439	1329.849860	12.091354
20.341163	1323.519763	12.096359
20.625952	1328.443727	12.101363
20.465129	1329.473990	12.106368
20.405905	1320.760640	12.111373
20.262276	1337.642517	12.116378
20.509883	1336.049620	12.121383
20.612644	1329.619272	12.126387
20.343787	1341.518638	12.131392
20.673228	1339.176194	12.136397
20.561044	1340.457341	12.141402
20.257382	1331.145829	12.146407
20.373095	1327.274590	12.151411
20.320819	1328.984609	12.156416
20.799354	1327.507860	12.161421
20.336310	1310.735399	12.166426
20.407847	1303.549892	12.171431
20.436732	1293.206004	12.176435
20.355249	1292.337431	12.181440
20.421769	1289.057566	12.186445
20.117132	1294.780476	12.191450
20.167279	1302.749333	12.196455
20.221057	1295.358488	12.201459
20.038577	1295.928543	12.206464
20.485365	1303.114996	12.211469
20.330983	1307.943402	12.216474
20.263408	1314.347658	12.221479
20.365313	1303.052181	12.226483
20.092151	1314.080089	12.231488
20.488642	1316.134881	12.236493
20.326591	1315.328046	12.241498
20.492227	1308.529683	12.246503
20.374138	1303.968708	12.251507
20.125557	1302.399753	12.256512
20.226229	1297.903245	12.261517
20.077727	1313.541560	12.266522
20.268706	1317.641478	12.271527
20.478128	1333.233769	12.276531
19.948501	1329.843952	12.281536
20.396985	1330.762844	12.286541
20.609748	1347.456995	12.291546
20.277033	1335.333452	12.296551
20.573129	1319.427158	12.301555
20.218925	1316.447793	12.306560
20.367283	1308.713826	12.311565
20.278925	1309.634751	12.316570
20.511642	1310.882968	12.321575
20.748781	1305.432642	12.326579
20.389469	1312.656191	12.331584
20.647363	1305.335298	12.336589
20.294253	1308.091581	12.341594
20.408425	1301.626307	12.346599
20.473231	1298.477610	12.351603
20.434430	1308.116583	12.356608
20.227550	1306.219254	12.361613
19.998678	1312.994613	12.366618
20.428094	1309.529122	12.371623
20.410408	1309.358480	12.376627
19.949028	1320.876917	12.381632
20.176891	1313.458300	12.386637
20.245496	1320.574179	12.391642
20.125951	1313.289822	12.396647
20.539228	1304.699835	12.401651
20.593532	1310.069015	12.406656
20.411583	1303.671469	12.411661
20.372679	1309.768352	12.416666
20.165727	1316.606453	12.421671
19.985961	1309.367976	12.426675
20.199691	1319.665326	12.431680
20.587528	1310.183614	12.436685
20.573718	1313.999200	12.441690
20.347491	1321.696730	12.446695
20.514162	1321.955614	12.451699
20.494173	1322.810439	12.456704
20.425950	1319.104167	12.461709
20.186595	1330.670786	12.466714
20.484341	1328.286087	12.471719
20.719435	1328.400007	12.476723
20.412395	1326.670049	12.481728
20.551766	1322.694105	12.486733
20.278965	1313.456537	12.491738
20.349052	1312.164789	12.496743
20.356062	1293.063740	12.501747
20.055426	1296.421980	12.506752
20.327996	1306.301474	12.511757
20.274286	1315.113289	12.516762
20.364491	1317.849338	12.521767
20.501674	1323.350395	12.526771
20.344831	1308.492562	12.531776
20.296223	1298.482753	12.536781
20.426444	1303.440823	12.541786
20.205252	1296.114335	12.546791
20.195164	1302.917879	12.551795
20.358807	1306.533260	12.556800
20.358988	1291.615705	12.561805
20.558487	1300.060673	12.566810
20.144335	1302.874003	12.571815
20.604843	1300.363994	12.576819
20.491430	1297.344653	12.581824
20.358430	1290.726401	12.586829
20.293195	1292.353321	12.591834
20.281753	1296.278920	12.596839
20.260220	1289.612927	12.601843
20.051421	1299.250620	12.606848
20.445372	1292.829044	12.611853
20.440270	1299.472507	12.616858
20.467292	1298.113506	12.621863
20.530076	1294.331149	12.626867
20.426629	1294.697773	12.631872
20.420903	1296.125953	12.636877
20.472323	1299.702456	12.641882
20.302036	1306.446390	12.646887
20.571766	1292.283844	12.651891
20.313351	1296.988479	12.656896
20.532282	1285.849406	12.661901
20.273817	1305.419545	12.666906
20.484044	1301.306140	12.671911
20.717816	1289.865054	12.676915
20.650801	1300.350679	12.681920
20.440667	1291.057395	12.686925
20.044168	1285.610355	12.691930
20.116051	1288.992766	12.696935
20.505922	1288.753970	12.701939
20.367664	1295.032285	12.706944
20.277767	1279.797922	12.711949
20.249343	1284.806521	12.716954
20.310764	1290.483664	12.721959
20.411500	1283.424407	12.726963
20.072526	1282.018116	12.731968
20.430735	1285.383248	12.736973
20.502017	1298.303895	12.741978
20.132853	1283.483103	12.746983
20.116805	1279.598196	12.751987
20.182889	1296.697333	12.756992
20.701314	1297.633456	12.761997
20.225459	1306.433739	12.767002
20.044196	1305.159999	12.772007
20.458598	1304.724888	12.777011
20.058100	1306.569295	12.782016
20.692305	1298.458202	12.787021
20.514177	1303.523801	12.792026
20.316725	1289.806380	12.797031
20.057319	1277.526102	12.802035
20.105545	1297.034700	12.807040
20.516288	1294.748687	12.812045
20.350360	1310.908636	12.817050
20.163681	1309.213104	12.822055
20.595226	1304.987124	12.827059
20.318144	1297.305245	12.832064
20.307632	1291.195777	12.837069
20.358823	1290.189341	12.842074
20.199645	1271.474398	12.847079
20.100117	1275.762573	12.852083
20.368137	1292.537741	12.857088
20.388854	1298.267114	12.862093
20.576143	1299.330172	12.867098
20.062451	1289.050742	12.872103
20.232368	1288.088454	12.877107
20.321667	1302.056561	12.882112
20.364590	1307.414938	12.887117
20.071226	1304.684512	12.892122
20.026246	1305.199519	12.897127
20.416428	1297.094228	12.902131
20.249781	1308.182420	12.907136
20.418930	1305.919167	12.912141
20.729992	1311.706326	12.917146
20.261826	1302.693903	12.922151
20.500647	1287.299865	12.927155
20.226739	1288.365509	12.932160
20.284628	1280.907779	12.937165
20.268769	1289.062211	12.942170
20.459710	1291.987208	12.947175
20.585247	1279.393203	12.952179
20.139570	1278.210527	12.957184
20.328505	1281.709896	12.962189
20.260329	1281.629314	12.967194
20.197979	1278.884129	12.972199
20.259741	1274.185661	12.977203
19.959376	1286.993669	12.982208
20.179056	1294.437129	12.987213
20.493900	1314.210756	12.992218
20.356131	1317.284385	12.997223
20.240073	1318.272812	13.002227
20.294222	1327.573674	13.007232
20.203589	1313.455964	13.012237
20.428888	1311.153790	13.017242
20.317571	1327.142608	13.022247
20.395567	1321.263459	13.027251
20.381976	1322.282856	13.032256
20.484501	1302.654012	13.037261
20.037157	1300.299833	13.042266
20.376541	1308.772962	13.047271
20.640312	1312.266712	13.052275
20.344983	1298.956007	13.057280
20.564988	1292.352423	13.062285
20.044806	1289.440539	13.067290
20.283213	1291.927426	13.072295
20.486005	1286.755418	13.077299
20.156404	1297.027434	13.082304
20.251087	1288.048265	13.087309
20.278354	1296.176898	13.092314
20.173493	1297.453719	13.097319
20.402062	1295.127369	13.102323
20.063241	1299.650849	13.107328
20.507640	1306.758831	13.112333
20.279361	1297.846935	13.117338
20.017642	1305.092766	13.122343
20.429602	1308.357861	13.127347
20.453898	1316.058014	13.132352
20.355494	1308.784481	13.137357
20.354595	1305.362388	13.142362
20.330831	1308.239623	13.147367
20.326978	1298.202175	13.152371
20.165154	1299.518046	13.157376
20.286745	1300.298246	13.162381
20.468864	1298.102316	13.167386
20.244682	1299.003899	13.172391
20.488693	1292.998928	13.177395
20.259621	1303.773773	13.182400
20.386053	1304.614707	13.187405
20.318269	1311.334409	13.192410
20.291227	1304.388569	13.197415
20.530046	1302.554208	13.202419
20.215263	1302.699052	13.207424
20.337126	1311.694191	13.212429
20.210011	1303.554694	13.217434
20.418417	1304.664851	13.222439
20.361395	1297.544008	13.227443
20.292210	1301.458316	13.232448
20.405819	1288.451435	13.237453
19.992687	1303.275594	13.242458
19.915774	1307.807772	13.247463
20.047622	1309.067344	13.252467
20.217984	1329.614723	13.257472
20.862377	1320.858546	13.262477
20.553296	1314.826651	13.267482
20.238255	1305.502777	13.272487
20.338851	1304.818069	13.277491
20.270697	1308.401028	13.282496
20.441357	1297.687570	13.287501
19.922909	1297.079513	13.292506
20.116412	1314.607816	13.297511
20.510035	1318.542941	13.302515
20.335326	1327.057068	13.307520
20.609064	1312.983756	13.312525
20.445584	1306.949145	13.317530
20.239863	1313.154643	13.322535
20.540921	1302.054503	13.327539
20.272788	1309.159422	13.332544
20.495584	1295.862287	13.337549
20.320361	1302.689014	13.342554
20.193433	1309.055421	13.347559
20.449527	1301.998188	13.352563
20.246116	1309.632144	13.357568
20.547299	1303.272672	13.362573
20.410534	1307.289229	13.367578
20.755129	1314.029903	13.372583
20.411152	1306.645715	13.377587
20.212620	1315.515323	13.382592
20.278380	1309.688596	13.387597
20.152691	1315.409785	13.392602
20.109327	1312.243640	13.397607
20.379895	1301.741344	13.402611
20.203143	1314.583282	13.407616
20.157822	1314.382352	13.412621
20.321486	1313.036253	13.417626
20.317195	1314.754388	13.422631
20.436775	1303.792008	13.427635
20.578826	1317.939389	13.432640
20.702946	1311.190227	13.437645
20.366063	1314.008584	13.442650
20.048366	1319.801401	13.447655
20.316376	1313.174381	13.452659
20.445260	1313.995999	13.457664
20.199799	1320.024897	13.462669
20.508421	1318.415962	13.467674
20.358634	1315.049154	13.472679
20.732420	1308.372148	13.477683
20.427572	1309.483731	13.482688
20.466662	1315.721153	13.487693
20.654975	1314.000510	13.492698
20.434185	1286.345473	13.497703
20.173013	1275.510077	13.502707
19.967432	1287.665833	13.507712
20.337959	1289.620675	13.512717
19.882860	1296.553542	13.517722
20.183415	1305.933372	13.522727
20.146710	1306.234154	13.527731
20.325132	1315.802216	13.532736
20.560298	1314.572456	13.537741
21.050185	1323.010551	13.542746
20.156516	1307.981627	13.547751
20.273039	1290.560048	13.552755
20.245737	1293.868386	13.557760
20.125992	1288.118566	13.562765
20.379994	1289.159944	13.567770
20.433532	1308.013223	13.572775
20.320862	1306.332699	13.577779
20.033663	1293.030165	13.582784
20.348516	1302.931301	13.587789
20.720352	1306.601794	13.592794
20.294262	1296.691617	13.597799
20.428830	1282.739886	13.602803
20.302561	1284.409657	13.607808
19.806041	1283.853301	13.612813
20.015410	1295.827757	13.617818
20.164611	1315.162568	13.622823
20.390553	1316.817173	13.627827
20.156261	1319.480387	13.632832
20.637405	1318.979432	13.637837
20.484732	1319.984738	13.642842
20.281655	1320.952348	13.647847
20.446159	1322.030081	13.652851
20.324391	1323.043075	13.657856
20.522043	1318.264568	13.662861
20.199849	1298.826477	13.667866
19.898257	1303.634202	13.672871
20.237479	1314.816775	13.677875
20.064419	1322.064245	13.682880
20.099645	1321.831543	13.687885
20.360921	1324.176005	13.692890
20.335319	1331.070353	13.697895
20.692062	1320.637885	13.702899
20.289783	1332.574293	13.707904
20.230615	1327.472438	13.712909
20.150730	1321.717824	13.717914
20.518267	1328.204090	13.722919
20.621651	1322.062251	13.727923
20.602949	1312.341000	13.732928
20.348166	1314.006038	13.737933
20.270245	1295.416887	13.742938
20.004277	1298.009449	13.747943
20.415672	1309.524309	13.752947
20.346483	1319.606564	13.757952
20.560637	1312.008769	13.762957
20.483239	1303.717830	13.767962
20.599491	1302.727827	13.772967
20.509729	1298.379971	13.777971
20.096944	1292.960759	13.782976
20.186228	1285.999529	13.787981
20.170910	1297.030459	13.792986
20.367449	1298.867961	13.797991
20.512629	1299.647553	13.802995
20.048019	1296.340421	13.808000
20.205530	1295.689218	13.813005
20.471534	1288.404889	13.818010
20.126975	1286.833895	13.823015
20.314529	1289.959721	13.828019
20.192392	1291.532632	13.833024
20.194942	1293.976704	13.838029
20.449335	1288.263416	13.843034
20.035863	1294.976738	13.848039
20.418296	1296.147454	13.853043
20.026370	1305.954718	13.858048
20.375077	1315.090312	13.863053
20.420852	1323.523538	13.868058
20.527198	1321.521054	13.873063
20.389107	1296.735704	13.878067
20.193747	1295.869521	13.883072
20.193148	1287.064834	13.888077
20.441762	1293.803458	13.893082
20.567433	1293.332387	13.898087
20.686248	1292.155881	13.903091
20.538962	1296.092106	13.908096
20.483408	1289.212326	13.913101
20.276687	1300.630204	13.918106
19.901960	1301.633074	13.923111
20.472146	1285.763533	13.928115
20.211230	1297.954933	13.933120
20.191452	1297.257882	13.938125
20.280054	1293.794706	13.943130
20.186653	1302.355781	13.948135
20.220660	1299.040094	13.953139
20.309936	1298.253105	13.958144
20.217516	1297.933520	13.963149
20.242990	1297.688181	13.968154
19.793810	1301.814492	13.973159
20.358605	1301.506793	13.978163
20.433464	1329.957931	13.983168
20.314256	1320.930847	13.988173
20.577338	1315.608854	13.993178
20.181959	1305.999725	13.998183
20.372877	1302.796218	14.003187
20.235630	1307.544615	14.008192
19.956421	1302.592029	14.013210
20.471086	1323.200317	14.018227
20.391260	1334.889844	14.023245
20.656974	1330.724505	14.028263
20.727638	1316.000483	14.033280
20.184081	1308.728451	14.038298
20.330445	1308.379501	14.043315
20.092798	1314.568052	14.048333
20.575028	1319.167843	14.053351
20.496035	1336.971696	14.058368
20.463448	1338.549964	14.063386
21.264250	1330.053612	14.068403
20.636675	1327.150757	14.073421
20.532079	1311.218271	14.078439
20.351556	1316.902200	14.083456
20.383486	1322.758319	14.088474
20.360335	1313.727984	14.093491
20.382849	1319.099530	14.098509
20.466688	1326.207386	14.103527
20.311603	1343.749672	14.108544
20.680156	1344.803058	14.113562
20.663887	1354.848059	14.118579
20.202122	1352.722587	14.123597
20.535113	1343.734536	14.128615
20.618131	1357.005771	14.133632
20.483267	1356.201441	14.138650
20.668086	1344.301698	14.143667
20.484022	1347.975839	14.148685
20.560774	1348.611713	14.153703
20.839125	1351.115686	14.158720
20.938121	1353.698602	14.163738
21.034504	1349.178012	14.168755
20.510450	1359.064896	14.173773
21.027646	1356.172946	14.178791
21.094723	1373.928379	14.183808
20.666415	1367.820876	14.188826
21.167989	1367.701571	14.193843
21.086072	1365.348772	14.198861
21.147476	1365.883272	14.203879
21.106704	1355.277945	14.208896
21.112415	1352.919038	14.213914
21.100013	1350.957856	14.218931
20.906451	1345.665521	14.223949
20.966977	1337.696223	14.228967
21.029886	1353.161928	14.233984
20.994380	1370.227414	14.239002
21.009540	1371.988410	14.244019
21.085650	1382.204318	14.249037
21.486457	1381.103764	14.254055
21.434370	1377.807088	14.259072
21.421370	1369.377582	14.264090
21.640295	1353.745817	14.269107
20.867037	1352.760152	14.274125
21.115983	1351.875733	14.279143
20.830421	1355.673031	14.284160
20.858132	1371.608421	14.289178
21.154951	1373.175056	14.294195
20.861983	1377.130847	14.299213
20.960525	1377.942575	14.304231
20.791341	1379.968932	14.309248
21.120238	1388.248991	14.314266
21.562680	1397.822879	14.319283
21.389560	1410.727591	14.324301
21.767607	1404.776194	14.329319
21.774051	1391.471801	14.334336
21.445364	1390.537929	14.339354
21.666406	1381.533102	14.344371
21.335180	1383.218780	14.349389
21.449665	1384.460557	14.354407
21.084166	1388.904557	14.359424
21.117107	1412.897948	14.364442
21.381610	1403.194029	14.369459
21.406352	1417.482946	14.374477
21.321356	1405.042579	14.379495
21.605914	1411.666996	14.384512
21.706639	1415.319330	14.389530
21.835298	1408.608590	14.394547
21.529937	1414.128419	14.399565
21.679958	1413.159097	14.404583
21.576259	1416.763808	14.409600
21.568622	1421.106697	14.414618
21.502705	1411.721318	14.419635
21.502275	1423.582301	14.424653
21.860238	1430.850987	14.429671
22.343019	1437.086717	14.434688
22.304439	1440.369581	14.439706
21.998065	1419.149050	14.444723
22.137737	1420.338048	14.449741
21.970319	1411.080545	14.454759
22.033899	1414.465090	14.459776
22.020301	1416.776531	14.464794
22.252879	1416.108655	14.469811
22.229528	1417.215112	14.474829
22.029983	1418.525853	14.479847
22.168700	1408.870307	14.484864
22.036460	1413.923641	14.489882
22.252541	1403.831032	14.494899
22.119203	1414.236099	14.499917
22.199735	1409.146997	14.504935
21.954963	1411.372607	14.509952
21.984291	1417.484015	14.514970
22.314642	1412.502937	14.519987
22.028057	1416.616600	14.525005
22.013013	1414.972018	14.530023
22.365933	1412.674132	14.535040
21.984441	1413.071626	14.540058
22.126078	1406.366682	14.545075
22.279618	1416.046434	14.550093
22.366701	1409.638060	14.555111
22.629028	1421.674218	14.560128
22.445013	1419.122183	14.565146
22.508382	1404.388224	14.570163
22.121252	1407.182390	14.575181
22.248160	1415.417599	14.580199
22.391123	1412.851171	14.585216
22.119835	1420.832131	14.590234
22.333887	1411.356482	14.595251
22.151044	1424.239161	14.600269
22.659048	1437.743145	14.605287
22.989303	1440.286048	14.610304
22.595537	1435.920684	14.615322
22.480444	1418.680964	14.620339
22.647669	1415.003229	14.625357
22.366457	1419.580090	14.630375
22.275644	1427.017878	14.635392
22.692838	1445.348358	14.640410
22.792411	1442.142314	14.645427
22.850858	1448.389094	14.650445
22.728487	1454.468080	14.655463
23.076388	1448.714961	14.660480
22.725638	1439.409598	14.665498
22.543255	1430.697177	14.670515
22.490371	1434.754696	14.675533
22.517332	1435.846838	14.680551
22.713954	1441.717638	14.685568
22.509057	1454.824090	14.690586
22.624385	1453.561416	14.695603
22.926892	1453.892295	14.700621
22.673196	1457.344755	14.705639
22.899458	1449.039070	14.710656
22.755464	1451.001642	14.715674
22.982246	1452.971149	14.720691
22.914746	1455.818171	14.725709
22.892019	1454.748979	14.730727
22.944136	1446.000722	14.735744
23.073114	1456.019481	14.740762
22.975574	1441.685537	14.745779
23.093988	1456.646983	14.750797
22.847666	1471.053118	14.755815
23.422762	1476.333447	14.760832
23.230531	1486.228845	14.765850
23.381444	1471.617712	14.770867
23.283431	1461.688418	14.775885
22.953259	1453.164726	14.780903
23.233883	1459.608890	14.785920
23.089147	1471.299439	14.790938
23.029192	1481.153287	14.795955
23.003486	1480.910431	14.800973
23.115949	1481.531176	14.805991
23.354358	1479.408851	14.811008
23.348705	1481.973872	14.816026
23.517271	1483.641201	14.821043
23.664412	1477.204342	14.826061
23.310206	1475.591821	14.831079
23.555040	1477.256423	14.836096
23.472258	1483.587092	14.841114
23.763614	1476.230583	14.846131
23.644212	1482.727544	14.851149
23.587501	1482.749189	14.856167
24.017711	1477.676655	14.861184
23.713917	1464.833818	14.866202
23.472623	1450.722571	14.871219
23.622117	1450.555595	14.876237
23.330381	1452.634541	14.881255
23.697876	1463.909901	14.886272
23.759983	1476.904574	14.891290
23.920773	1470.685771	14.896307
23.648882	1454.989027	14.901325
23.601332	1453.423558	14.906343
23.694691	1465.779291	14.911360
23.685145	1479.159785	14.916378
23.593526	1480.440734	14.921395
23.622619	1474.615750	14.926413
23.937471	1480.831089	14.931431
23.825549	1475.994460	14.936448
23.871611	1486.256133	14.941466
23.766283	1484.951567	14.946483
24.059229	1483.791128	14.951501
23.908845	1485.598990	14.956519
24.034931	1480.331133	14.961536
23.883093	1480.654247	14.966554
23.927304	1482.656023	14.971571
24.077263	1476.868393	14.976589
24.136016	1476.505097	14.981607
23.861994	1481.247575	14.986624
24.070506	1474.022260	14.991642
24.143389	1492.818284	14.996659
23.896820	1492.843466	15.001677
23.839372	1486.605978	15.006695
24.256840	1478.713387	15.011712
23.936506	1494.617900	15.016730
23.732756	1482.627428	15.021747
24.158136	1481.187884	15.026765
24.267833	1498.293285	15.031783
24.372753	1505.427756	15.036800
24.177237	1501.858189	15.041818
24.097787	1505.599059	15.046835
24.121025	1504.956700	15.051853
24.114415	1506.514326	15.056871
24.254019	1491.828683	15.061888
24.450527	1502.793132	15.066906
24.389241	1497.452902	15.071923
24.594559	1492.609719	15.076941
24.517663	1506.003338	15.081959
24.871760	1493.326907	15.086976
24.609799	1497.002497	15.091994
24.663079	1501.244457	15.097011
24.664301	1494.623216	15.102029
24.496743	1499.093883	15.107047
24.495776	1500.706452	15.112064
24.686341	1505.923846	15.117082
24.588541	1500.587079	15.122099
24.837546	1489.789930	15.127117
24.501790	1504.473064	15.132135
24.707768	1501.089584	15.137152
24.944263	1494.495317	15.142170
24.818596	1500.647996	15.147187
24.908301	1501.331363	15.152205
24.869090	1503.112058	15.157223
24.752607	1492.891523	15.162240
25.064080	1496.853983	15.167258
24.415824	1496.984915	15.172275
24.956252	1494.565874	15.177293
24.661212	1505.335006	15.182311
24.849292	1493.420464	15.187328
24.891560	1503.283193	15.192346
24.985942	1504.256046	15.197363
24.933341	1494.361960	15.202381
24.717921	1504.967378	15.207399
24.757663	1500.217454	15.212416
24.793768	1492.373880	15.217434
24.526368	1501.832952	15.222451
25.198147	1515.527974	15.227469
25.318792	1517.277670	15.232487
25.531280	1526.160771	15.237504
25.114329	1522.492018	15.242522
25.290337	1536.244104	15.247539
25.231982	1528.920533	15.252557
25.207018	1533.699602	15.257575
25.312114	1527.045263	15.262592
25.423645	1529.081927	15.267610
25.164332	1537.349700	15.272627
25.502513	1526.662574	15.277645
25.177387	1533.843622	15.282663
25.396078	1528.409963	15.287680
25.425605	1530.532067	15.292698
25.436365	1529.127183	15.297715
25.616987	1526.055278	15.302733
25.625188	1523.610213	15.307751
25.506088	1518.584373	15.312768
25.846230	1515.991985	15.317786
25.346170	1525.146820	15.322803
25.454989	1522.686495	15.327821
25.510247	1531.308376	15.332839
25.769979	1526.387287	15.337856
25.795709	1520.740579	15.342874
25.476358	1526.545835	15.347891
25.923769	1524.925016	15.352909
25.742104	1526.182576	15.357927
25.828619	1528.012438	15.362944
25.741728	1527.044712	15.367962
25.779268	1534.237921	15.372979
25.936051	1530.406089	15.377997
25.852656	1522.911116	15.383015
25.711825	1523.764962	15.388032
25.892122	1526.102914	15.393050
25.751260	1527.003957	15.398067
26.094226	1520.134714	15.403085
25.624017	1534.461784	15.408103
25.627526	1526.832609	15.413120
26.180398	1525.236657	15.418138
25.656892	1526.887733	15.423155
25.638898	1526.023067	15.428173
25.458438	1527.913598	15.433191
25.509702	1526.605291	15.438208
25.844690	1541.657344	15.443226
25.702167	1553.679525	15.448243
25.919584	1546.489721	15.453261
25.867082	1556.112763	15.458279
26.282207	1555.467679	15.463296
26.302237	1548.623184	15.468314
26.032037	1553.714299	15.473331
26.514389	1553.246477	15.478349
26.403402	1561.743087	15.483367
26.813566	1562.470519	15.488384
27.106754	1556.036289	15.493402
27.050362	1546.967065	15.498419
26.712714	1533.774050	15.503437
26.579102	1526.147081	15.508455
26.521353	1532.657041	15.513472
26.562201	1528.690324	15.518490
26.265532	1530.858946	15.523507
26.548789	1525.948264	15.528525
26.637466	1518.356635	15.533543
26.518608	1537.548250	15.538560
26.759965	1540.802222	15.543578
26.496803	1546.292561	15.548595
26.689192	1538.917196	15.553613
26.542169	1536.857120	15.558631
26.615190	1534.547225	15.563648
26.805548	1537.623707	15.568666
26.512500	1539.223086	15.573683
26.665025	1529.551100	15.578701
26.573684	1539.012791	15.583719
26.591712	1546.264963	15.588736
26.882134	1536.645701	15.593754
26.346261	1537.361983	15.598771
26.953178	1543.624368	15.603789
26.973685	1552.038651	15.608807
26.803057	1550.092453	15.613824
26.966174	1552.647875	15.618842
26.701554	1557.887544	15.623859
26.882205	1557.233449	15.628877
26.925314	1547.383053	15.633895
27.124563	1546.825097	15.638912
26.952176	1553.689989	15.643930
26.800324	1558.947068	15.648947
27.110482	1551.388528	15.653965
27.164382	1557.150785	15.658983
27.003851	1562.034070	15.664000
27.225860	1550.349246	15.669018
26.672704	1556.350682	15.674035
26.686199	1556.947888	15.679053
27.262329	1558.228531	15.684071
27.024006	1576.485965	15.689088
27.537683	1585.110274	15.694106
27.539138	1594.115953	15.699123
27.455507	1577.143956	15.704141
27.128307	1567.789135	15.709159
27.255971	1583.493304	15.714176
27.775624	1578.146913	15.719194
27.659778	1586.627009	15.724211
27.597851	1566.274157	15.729229
27.571957	1556.479593	15.734247
27.486101	1549.025112	15.739264
27.816912	1554.431736	15.744282
27.675067	1566.652815	15.749299
27.594632	1554.672504	15.754317
27.763114	1562.622732	15.759335
27.441282	1558.657217	15.764352
27.716183	1544.281076	15.769370
27.354281	1556.772417	15.774387
27.512404	1552.141241	15.779405
27.613459	1557.759120	15.784423
27.872150	1579.009514	15.789440
27.989997	1585.002265	15.794458
27.613377	1586.598459	15.799475
27.867909	1580.957711	15.804493
28.125702	1574.064272	15.809511
27.849879	1582.752357	15.814528
28.099002	1580.390773	15.819546
28.184992	1581.788128	15.824563
27.868156	1564.104553	15.829581
28.138973	1563.294501	15.834599
27.730913	1562.124729	15.839616
28.222217	1566.541463	15.844634
28.120222	1579.851061	15.849651
28.269610	1578.622271	15.854669
28.077121	1568.000085	15.859687
27.732802	1575.975473	15.864704
28.091196	1577.701417	15.869722
28.349132	1581.655135	15.874739
28.210093	1579.789628	15.879757
28.210012	1573.913413	15.884775
28.116585	1577.927886	15.889792
28.256310	1579.047674	15.894810
28.075583	1582.565607	15.899827
28.143099	1582.451031	15.904845
28.340142	1582.779857	15.909863
28.161930	1587.405626	15.914880
28.583044	1585.074029	15.919898
28.266908	1590.914191	15.924915
28.116567	1584.044939	15.929933
28.049961	1594.138246	15.934951
28.420088	1603.903923	15.939968
28.313140	1612.424301	15.944986
28.283311	1619.655826	15.950003
28.464844	1616.439033	15.955021
28.817917	1604.100096	15.960039
28.757690	1613.133714	15.965056
28.852030	1603.109936	15.970074
29.214828	1605.543856	15.975091
28.796896	1595.968310	15.980109
29.145604	1597.620294	15.985127
28.810336	1575.896821	15.990144
29.076839	1565.645044	15.995162
28.757237	1565.670861	16.000179
28.668398	1565.192671	16.005197
28.990962	1568.347966	16.010215
28.599320	1569.343278	16.015232
28.853166	1579.496371	16.020250
29.116967	1597.925443	16.025267
29.357210	1594.269054	16.030285
29.218355	1583.517962	16.035303
28.671821	1575.785354	16.040320
29.099613	1583.006801	16.045338
29.391524	1592.037731	16.050355
29.158741	1588.371836	16.055373
29.048556	1584.585712	16.060391
28.798295	1596.338024	16.065408
29.119130	1594.736598	16.070426
29.202470	1595.233788	16.075443
29.129569	1602.571278	16.080461
29.239065	1596.630386	16.085479
29.137159	1607.345981	16.090496
29.257362	1595.017448	16.095514
28.943645	1594.731643	16.100531
28.866862	1603.033266	16.105549
29.193641	1594.884506	16.110567
28.972841	1606.256947	16.115584
29.496875	1613.952290	16.120602
29.668568	1620.730090	16.125619
29.329912	1617.659967	16.130637
29.649844	1630.951087	16.135655
29.309553	1631.588988	16.140672
29.392283	1624.404896	16.145690
29.281228	1630.541928	16.150707
29.021834	1632.773836	16.155725
29.376533	1621.662419	16.160743
29.442241	1643.957539	16.165760
29.824183	1649.350539	16.170778
30.280868	1657.059005	16.175795
29.982503	1653.178601	16.180813
30.089746	1632.212702	16.185831
29.742153	1634.077989	16.190848
30.047111	1623.343393	16.195866
29.921530	1629.358468	16.200883
29.813270	1627.572205	16.205901
30.118269	1622.922302	16.210919
30.018284	1624.578992	16.215936
29.796343	1624.153489	16.220954
30.089686	1624.871241	16.225971
29.975001	1629.129800	16.230989
30.260642	1630.453633	16.236007
30.189025	1638.302189	16.241024
29.967969	1627.929917	16.246042
29.962162	1639.334952	16.251059
30.122600	1642.265212	16.256077
30.446863	1646.539505	16.261095
30.450516	1658.363061	16.266112
30.504979	1647.292428	16.271130
30.273999	1639.662051	16.276147
30.433033	1650.868552	16.281165
30.612238	1632.743186	16.286183
30.166508	1629.627214	16.291200
30.526914	1634.460477	16.296218
30.555289	1633.413011	16.301235
30.010015	1640.972939	16.306253
30.741443	1647.932841	16.311271
30.641163	1653.723658	16.316288
30.828537	1658.871614	16.321306
30.773276	1645.627169	16.326323
30.289398	1642.529863	16.331341
30.602774	1652.234621	16.336359
30.850307	1658.436391	16.341376
30.888234	1665.045987	16.346394
30.850715	1659.340883	16.351411
30.557371	1663.833234	16.356429
30.878519	1662.993914	16.361447
30.735465	1683.188491	16.366464
30.495572	1675.539853	16.371482
30.412597	1677.240242	16.376499
30.673056	1667.544659	16.381517
30.905679	1669.290673	16.386535
30.841514	1674.454368	16.391552
30.780239	1669.092050	16.396570
30.830900	1662.553301	16.401587
30.727169	1669.884730	16.406605
30.922685	1668.844426	16.411623
30.935457	1688.978766	16.416640
31.019334	1699.729296	16.421658
31.199875	1699.249827	16.426675
31.019732	1704.336857	16.431693
31.466721	1688.631394	16.436711
31.363383	1697.824530	16.441728
31.335267	1679.102146	16.446746
31.571805	1683.524940	16.451763
31.502841	1684.893533	16.456781
31.394810	1683.986585	16.461799
31.097366	1687.313149	16.466816
31.405598	1685.145838	16.471834
31.631786	1680.662649	16.476851
31.648274	1690.249606	16.481869
31.645077	1686.634378	16.486887
31.684232	1688.924864	16.491904
31.739960	1684.543581	16.496922
31.416385	1673.369618	16.501939
31.107039	1677.518445	16.506957
31.762848	1673.663620	16.511975
31.746701	1679.833516	16.516992
31.508342	1680.923158	16.522010
31.707353	1679.506327	16.527027
31.567190	1678.108980	16.532045
31.779125	1687.844099	16.537063
32.048189	1677.408570	16.542080
31.825375	1688.135641	16.547098
31.869738	1673.929853	16.552115
31.737967	1680.715964	16.557133
31.633040	1682.481992	16.562151
31.596552	1683.821809	16.567168
31.555905	1681.626764	16.572186
31.990597	1678.408124	16.577203
31.978871	1686.486264	16.582221
31.747440	1683.223627	16.587239
32.063715	1694.689029	16.592256
31.898259	1703.339133	16.597274
32.112795	1710.363410	16.602291
32.034931	1712.923471	16.607309
32.249346	1705.380909	16.612327
32.320410	1707.269102	16.617344
32.502420	1713.173019	16.622362
32.739613	1706.771250	16.627379
32.586953	1715.700904	16.632397
32.563269	1708.702849	16.637415
32.812890	1711.746321	16.642432
32.143912	1695.269465	16.647450
32.676063	1699.293533	16.652467
32.119954	1710.963360	16.657485
32.559892	1710.864898	16.662503
32.434406	1704.439956	16.667520
32.394897	1712.813565	16.672538
32.501887	1714.362534	16.677555
32.433489	1713.645114	16.682573
32.545861	1709.497046	16.687591
32.516418	1718.602115	16.692608
32.251590	1713.077180	16.697626
32.707275	1705.101293	16.702643
32.592482	1710.749722	16.707661
32.794336	1722.240473	16.712679
33.069642	1730.626022	16.717696
32.829752	1726.653684	16.722714
33.117391	1732.334687	16.727731
32.776158	1723.321791	16.732749
32.860802	1725.535026	16.737767
32.997520	1739.822919	16.742784
32.905322	1740.742170	16.747802
33.102179	1737.674711	16.752819
33.235751	1749.354132	16.757837
33.031435	1749.263244	16.762855
33.282251	1748.038715	16.767872
33.367512	1740.711796	16.772890
33.453258	1744.944717	16.777907
33.362593	1749.687141	16.782925
33.498469	1743.123754	16.787943
33.170218	1723.044403	16.792960
32.920398	1737.806878	16.797978
33.321084	1738.172447	16.802995
33.053683	1741.460410	16.808013
33.016199	1745.536797	16.813031
33.409876	1736.853448	16.818048
33.289487	1748.521459	16.823066
33.405545	1744.938323	16.828083
33.201853	1748.818624	16.833101
33.174416	1742.590397	16.838119
33.457235	1754.346698	16.843136
33.436595	1771.013863	16.848154
33.629211	1765.767541	16.853171
33.507181	1772.545063	16.858189
33.377921	1765.689666	16.863207
33.931120	1764.875470	16.868224
33.902501	1771.502807	16.873242
34.209472	1766.337353	16.878259
33.985549	1773.823290	16.883277
34.085205	1772.962656	16.888295
34.390939	1763.526430	16.893312
33.744466	1770.720300	16.898330
34.118035	1759.312386	16.903347
34.230074	1764.278117	16.908365
34.071511	1769.854895	16.913383
34.134212	1763.517897	16.918400
34.185682	1769.278266	16.923418
34.513764	1766.551686	16.928435
34.204718	1765.317338	16.933453
33.729449	1768.827231	16.938471
34.146696	1762.546953	16.943488
34.251402	1770.016659	16.948506
34.228830	1767.482075	16.953523
33.718056	1759.628041	16.958541
33.737164	1757.870216	16.963559
33.805068	1758.402122	16.968576
34.311654	1777.811286	16.973594
34.519051	1785.823860	16.978611
34.615913	1792.885822	16.983629
34.630173	1796.014040	16.988647
34.606806	1797.141765	16.993664
34.376148	1800.077798	16.998682
34.672494	1799.948751	17.003699
34.616746	1803.420848	17.008717
34.623453	1804.469841	17.013735
34.880508	1799.943152	17.018752
34.758513	1802.978266	17.023770
34.983430	1799.200781	17.028787
35.032678	1803.410437	17.033805
34.917111	1800.393577	17.038823
35.027864	1798.702932	17.043840
34.759658	1801.976879	17.048858
34.940993	1792.924647	17.053875
35.104255	1785.439754	17.058893
34.857125	1792.432300	17.063911
35.113769	1794.676319	17.068928
34.861956	1812.453256	17.073946
35.048941	1800.988546	17.078963
34.888055	1796.559974	17.083981
34.766673	1810.960676	17.088999
35.025620	1798.650745	17.094016
35.039965	1805.339675	17.099034
34.827065	1799.807998	17.104051
35.177960	1809.236305	17.109069
35.372499	1826.898027	17.114087
35.388312	1833.821916	17.119104
35.549554	1828.168422	17.124122
35.315695	1821.198325	17.129139
35.740711	1826.512946	17.134157
35.412794	1830.507466	17.139175
35.569467	1821.942094	17.144192
35.796073	1829.129680	17.149210
35.788903	1824.157459	17.154227
35.673700	1810.752527	17.159245
35.430842	1807.582924	17.164263
35.584077	1817.749870	17.169280
35.548820	1817.222226	17.174298
35.516590	1820.713386	17.179315
35.744476	1823.502358	17.184333
35.589533	1822.363772	17.189351
36.105802	1823.424314	17.194368
35.766099	1820.687027	17.199386
36.031004	1814.104604	17.204403
36.070936	1815.219876	17.209421
35.764756	1821.930829	17.214439
35.906600	1812.475088	17.219456
36.109761	1813.386567	17.224474
36.048001	1817.361447	17.229491
36.286989	1809.479054	17.234509
36.065762	1814.102315	17.239527
36.319383	1814.783939	17.244544
35.941531	1819.440832	17.249562
36.000202	1814.292937	17.254579
36.361612	1816.399123	17.259597
36.344503	1822.798907	17.264615
36.641761	1820.063861	17.269632
36.359075	1821.913314	17.274650
36.205553	1821.077323	17.279667
36.360919	1832.935030	17.284685
36.421727	1847.907640	17.289703
36.609466	1841.452349	17.294720
36.500023	1845.137523	17.299738
36.354344	1842.254451	17.304755
36.525737	1851.957605	17.309773
36.128957	1852.098768	17.314791
36.447394	1845.551054	17.319808
36.548818	1855.538303	17.324826
36.751312	1848.856486	17.329843
36.713616	1845.875964	17.334861
36.367682	1859.953857	17.339879
37.275193	1866.959721	17.344896
36.961796	1860.014090	17.349914
36.737623	1861.722860	17.354931
37.145102	1861.650812	17.359949
36.829315	1864.473012	17.364967
36.981719	1867.296054	17.369984
37.246471	1884.309539	17.375002
37.024573	1883.801432	17.380019
37.267052	1874.319377	17.385037
37.135860	1880.221398	17.390055
37.226890	1867.845375	17.395072
37.066648	1884.567969	17.400090
37.157538	1883.468827	17.405107
37.514420	1877.688940	17.410125
37.373026	1883.064023	17.415143
37.534324	1876.100098	17.420160
37.423879	1880.074107	17.425178
37.253102	1877.103004	17.430195
37.338284	1880.964799	17.435213
37.400831	1890.845008	17.440231
37.795899	1869.009341	17.445248
37.728270	1875.727894	17.450266
37.684886	1877.676837	17.455283
37.529555	1877.121932	17.460301
37.707387	1875.842962	17.465319
37.924543	1875.225507	17.470336
37.847659	1877.524304	17.475354
37.782698	1880.200320	17.480371
37.909116	1874.449323	17.485389
37.528646	1880.608189	17.490407
37.867564	1877.457480	17.495424
37.591009	1879.848686	17.500442
37.569543	1886.700676	17.505459
37.808834	1879.592955	17.510477
37.783010	1899.194950	17.515495
38.086245	1900.933665	17.520512
38.230308	1910.249510	17.525530
37.936089	1911.125480	17.530547
38.220631	1905.533307	17.535565
38.063666	1911.142133	17.540583
38.473193	1917.808205	17.545600
38.505416	1926.916155	17.550618
38.362396	1918.770563	17.555635
38.602275	1909.544532	17.560653
38.334357	1916.058292	17.565671
38.366089	1911.156133	17.570688
38.668554	1904.228673	17.575706
38.556841	1906.432349	17.580723
38.519662	1897.749975	17.585741
38.430523	1905.093353	17.590759
38.345720	1910.785843	17.595776
38.628443	1910.410416	17.600794
38.319671	1906.286196	17.605811
38.790892	1898.163000	17.610829
38.773986	1904.252883	17.615847
38.544002	1895.092356	17.620864
38.485350	1904.191187	17.625882
38.538844	1905.659041	17.630899
38.998407	1907.822737	17.635917
38.730781	1931.105102	17.640935
38.977998	1924.285550	17.645952
39.042841	1919.622728	17.650970
39.047390	1922.712408	17.655987
39.313150	1914.846139	17.661005
39.290097	1922.874304	17.666023
39.272862	1915.938046	17.671040
39.464462	1919.621636	17.676058
39.272259	1919.604324	17.681075
39.390864	1917.086526	17.686093
39.434059	1930.472395	17.691111
39.455347	1909.428565	17.696128
39.470434	1900.240749	17.701146
39.239739	1904.447885	17.706163
39.373133	1902.884187	17.711181
39.211797	1913.882420	17.716199
39.210053	1916.671064	17.721216
39.311268	1908.537654	17.726234
39.157841	1917.388898	17.731251
39.376489	1912.055785	17.736269
39.385482	1919.476334	17.741287
39.434367	1915.633292	17.746304
39.794502	1929.523139	17.751322
39.813560	1943.824492	17.756339
40.053583	1945.449017	17.761357
39.865478	1946.597520	17.766375
39.773811	1951.623331	17.771392
39.832900	1942.154748	17.776410
39.910164	1950.639653	17.781427
40.073423	1955.462778	17.786445
40.362758	1946.304347	17.791463
40.074403	1953.040832	17.796480
40.051242	1939.101973	17.801498
39.810905	1948.082720	17.806515
39.926789	1936.164387	17.811533
39.840106	1944.703750	17.816551
39.835204	1948.589369	17.821568
39.954579	1949.823337	17.826586
40.124093	1968.529056	17.831603
40.710414	1960.605348	17.836621
40.581749	1971.279070	17.841639
40.654310	1977.054249	17.846656
40.746266	1969.427255	17.851674
40.825427	1970.120191	17.856691
40.551235	1946.790488	17.861709
40.360728	1950.348609	17.866727
40.386120	1966.118269	17.871744
40.611606	1963.951529	17.876762
40.752560	1976.752380	17.881779
40.841040	1970.702209	17.886797
41.017365	1974.171944	17.891815
40.739638	1984.476168	17.896832
41.142814	1960.205448	17.901850
40.927746	1969.009921	17.906867
41.245524	1968.396079	17.911885
40.877425	1973.008204	17.916903
40.938946	1970.921885	17.921920
40.732821	1958.799254	17.926938
40.942704	1970.438368	17.931955
41.136516	1962.167457	17.936973
41.105991	1974.137514	17.941991
41.066857	1973.335185	17.947008
41.139855	1969.841450	17.952026
41.013845	1967.885719	17.957043
41.070248	1961.259399	17.962061
41.402991	1961.332199	17.967079
41.077915	1975.754536	17.972096
41.388874	1973.178524	17.977114
41.068288	1999.240500	17.982131
41.313145	2000.920107	17.987149
41.611201	1999.452842	17.992167
41.522733	2010.695947	17.997184
41.955287	1994.784020	18.002202
41.528525	2005.900949	18.007219
41.791241	1997.735440	18.012237
41.605434	1999.088087	18.017255
41.562369	1991.945900	18.022272
41.856623	1991.322437	18.027290
41.812520	1994.358540	18.032307
42.092564	1993.135623	18.037325
42.202891	1994.558240	18.042343
42.201596	1996.668024	18.047360
42.084229	1992.680006	18.052378
42.143669	2003.583319	18.057395
42.056561	1994.322073	18.062413
42.001175	1991.092642	18.067431
41.987726	1991.945863	18.072448
42.369096	1998.260938	18.077466
42.090120	2000.617153	18.082483
42.230090	1997.697934	18.087501
42.667467	2003.989921	18.092519
42.173189	2011.665395	18.097536
42.195179	2021.526204	18.102554
42.361323	2018.294474	18.107571
42.413938	2021.096492	18.112589
42.732188	2025.920881	18.117607
42.766288	2030.955765	18.122624
42.778291	2020.293556	18.127642
42.445272	2029.532182	18.132659
42.648595	2021.608169	18.137677
42.576235	2034.260606	18.142695
42.340178	2023.225008	18.147712
42.566772	2027.990864	18.152730
42.846843	2026.729398	18.157747
42.799277	2027.636043	18.162765
42.977364	2014.916441	18.167783
42.730148	2028.163872	18.172800
43.049266	2039.050182	18.177818
43.106182	2052.549600	18.182835
43.318683	2058.997818	18.187853
43.220820	2052.506178	18.192871
43.173763	2055.099141	18.197888
43.429713	2048.584113	18.202906
43.200161	2049.821823	18.207923
43.612194	2040.420380	18.212941
43.283821	2041.387540	18.217959
43.270219	2048.619049	18.222976
43.534759	2040.154332	18.227994
43.527105	2051.897421	18.233011
42.773344	2061.748256	18.238029
43.402407	2048.097774	18.243047
43.632022	2049.517104	18.248064
43.753406	2047.714617	18.253082
43.844835	2045.806001	18.258099
43.746484	2044.969851	18.263117
43.764660	2050.773396	18.268135
43.584831	2054.129265	18.273152
43.842004	2048.221271	18.278170
43.535257	2052.077185	18.283187
43.350174	2044.951328	18.288205
43.973363	2056.187160	18.293223
43.842704	2071.107945	18.298240
44.030499	2071.958180	18.303258
44.145481	2083.544875	18.308275
44.138644	2082.984371	18.313293
44.172175	2076.587391	18.318311
44.093659	2082.584920	18.323328
44.350160	2074.007413	18.328346
44.439598	2084.952410	18.333363
43.902863	2080.718193	18.338381
44.216219	2073.291020	18.343399
44.269048	2081.917547	18.348416
44.483633	2080.294475	18.353434
44.210899	2076.873155	18.358451
44.296031	2082.047007	18.363469
44.577538	2094.599801	18.368487
44.719265	2118.531386	18.373504
44.925192	2102.977191	18.378522
44.742756	2112.740093	18.383539
44.867454	2118.212050	18.388557
44.845258	2107.726703	18.393575
44.547541	2115.109742	18.398592
44.690824	2113.322632	18.403610
44.829564	2114.732078	18.408627
45.022216	2118.061595	18.413645
45.160779	2109.903239	18.418663
45.190949	2119.666062	18.423680
45.343481	2110.014929	18.428698
45.172135	2102.973375	18.433715
45.170821	2101.421699	18.438733
45.451045	2108.543455	18.443751
45.273164	2111.404274	18.448768
45.296161	2104.984578	18.453786
45.592081	2111.686163	18.458803
45.723870	2108.873627	18.463821
45.609442	2107.804853	18.468839
45.068368	2110.139172	18.473856
45.254004	2106.886222	18.478874
45.035592	2108.452519	18.483891
45.162528	2115.451636	18.488909
45.736589	2107.694198	18.493927
45.303911	2111.774718	18.498944
45.525196	2124.590418	18.503962
45.750674	2132.285673	18.508979
45.649028	2140.129062	18.513997
45.400373	2130.959564	18.519015
45.577861	2143.742937	18.524032
45.809566	2133.395632	18.529050
45.763204	2132.475675	18.534067
45.711880	2139.073763	18.539085
46.187147	2148.220529	18.544103
46.317019	2155.690353	18.549120
46.204384	2154.364867	18.554138
46.532466	2156.601484	18.559155
46.413759	2144.801409	18.564173
46.647253	2130.517034	18.569191
46.078242	2124.761217	18.574208
46.261597	2117.591511	18.579226
46.392855	2131.567607	18.584243
46.484076	2157.026963	18.589261
46.901927	2152.350245	18.594279
46.948842	2145.348587	18.599296
46.992037	2146.442127	18.604314
47.004657	2129.926865	18.609331
46.802928	2123.425014	18.614349
46.409644	2119.451072	18.619367
46.497087	2123.584725	18.624384
46.777332	2133.137777	18.629402
47.176832	2142.743396	18.634419
47.157436	2146.457546	18.639437
46.814675	2127.407210	18.644455
46.938145	2144.578821	18.649472
46.891336	2152.942835	18.654490
46.994552	2155.308915	18.659507
46.913754	2157.383420	18.664525
47.139134	2154.165024	18.669543
47.178955	2165.288680	18.674560
47.321119	2151.677997	18.679578
47.449552	2153.952746	18.684595
47.353701	2157.931581	18.689613
47.426032	2151.766712	18.694631
47.579464	2154.280525	18.699648
47.366945	2155.517887	18.704666
47.858682	2144.638285	18.709683
47.389430	2154.940921	18.714701
47.409353	2147.032717	18.719719
47.584484	2147.406741	18.724736
47.240996	2156.506319	18.729754
47.713122	2164.272377	18.734771
47.535942	2182.049659	18.739789
47.625915	2174.974261	18.744807
47.829601	2182.495253	18.749824
47.746394	2189.448474	18.754842
47.696912	2179.728830	18.759859
47.902805	2182.677122	18.764877
48.053720	2174.250899	18.769895
48.068697	2177.524601	18.774912
48.214417	2179.428481	18.779930
48.065299	2173.129806	18.784947
47.888030	2186.123173	18.789965
48.460859	2192.546237	18.794983
48.436871	2206.906627	18.800000
48.043427	2213.003200	18.805018
48.253021	2220.180323	18.810035
48.309267	2215.024808	18.815053
48.608006	2211.318037	18.820071
48.758409	2208.585890	18.825088
48.993246	2202.108771	18.830106
49.107040	2197.058139	18.835123
48.667385	2211.690904	18.840141
49.135606	2193.414924	18.845159
48.922471	2206.648428	18.850176
48.718718	2210.585492	18.855194
48.910305	2199.553926	18.860211
48.633539	2200.999754	18.865229
49.039435	2194.773805	18.870247
48.946967	2207.151152	18.875264
48.926147	2195.809729	18.880282
49.354021	2199.320421	18.885299
49.371682	2204.675763	18.890317
49.402079	2193.194030	18.895335
49.020350	2197.520511	18.900352
49.081334	2198.712686	18.905370
49.325414	2195.444104	18.910387
49.322682	2203.418843	18.915405
49.593595	2195.152810	18.920423
49.629988	2196.717809	18.925440
49.363628	2206.984980	18.930458
49.795194	2212.280609	18.935475
49.486530	2222.707919	18.940493
49.788342	2219.266518	18.945511
49.773681	2230.560947	18.950528
49.509039	2229.617587	18.955546
49.697799	2224.101136	18.960563
49.655573	2220.601333	18.965581
49.629697	2237.822042	18.970599
49.844135	2235.204744	18.975616
49.834896	2223.528732	18.980634
50.075248	2214.845170	18.985651
49.618562	2223.310772	18.990669
49.807085	2237.826866	18.995687
50.421507	2243.949928	19.000704
50.279192	2237.175048	19.005722
50.749310	2246.771047	19.010739
50.520522	2248.060565	19.015757
50.710876	2243.820466	19.020775
50.672250	2238.553434	19.025792
50.413835	2230.632152	19.030810
50.702734	2224.627786	19.035827
50.921604	2228.821527	19.040845
50.506329	2221.261920	19.045863
50.619529	2230.638740	19.050880
50.705078	2233.957047	19.055898
50.619104	2238.952159	19.060915
50.786069	2244.329327	19.065933
50.964551	2237.174498	19.070951
51.141237	2236.428980	19.075968
51.079652	2241.357277	19.080986
51.251523	2240.530722	19.086003
50.856825	2242.368197	19.091021
50.924231	2239.978857	19.096039
51.126716	2235.801325	19.101056
51.131443	2245.999334	19.106074
51.169106	2232.114994	19.111091
50.671374	2248.666077	19.116109
50.942714	2243.445574	19.121127
51.454441	2253.938719	19.126144
51.366945	2266.156434	19.131162
51.865813	2267.856131	19.136179
51.348353	2276.176499	19.141197
51.688736	2272.090233	19.146215
51.941375	2284.141240	19.151232
51.256501	2280.533105	19.156250
51.747827	2276.445577	19.161267
51.741038	2273.352277	19.166285
51.586556	2272.715416	19.171303
51.927143	2274.468673	19.176320
51.689151	2271.257289	19.181338
52.019664	2262.453133	19.186355
51.934767	2278.111720	19.191373
51.992229	2290.789298	19.196391
52.382632	2294.528591	19.201408
52.243745	2297.313221	19.206426
52.289154	2306.120405	19.211443
52.005450	2308.231222	19.216461
52.524393	2304.108606	19.221479
52.960274	2295.504724	19.226496
52.275739	2306.130472	19.231514
52.412760	2301.548047	19.236531
52.873749	2302.855781	19.241549
52.733401	2302.934025	19.246567
52.626894	2302.149501	19.251584
52.344850	2306.663054	19.256602
52.723513	2294.992770	19.261619
52.540224	2302.342709	19.266637
52.734031	2303.941610	19.271655
52.563150	2290.032265	19.276672
52.780888	2299.636298	19.281690
52.718471	2295.987100	19.286707
52.922106	2309.744955	19.291725
52.874875	2319.974112	19.296743
53.351168	2315.310835	19.301760
53.585736	2314.171444	19.306778
53.814209	2314.890141	19.311795
53.564033	2314.148192	19.316813
53.402921	2300.191658	19.321831
53.498326	2279.972393	19.326848
53.399078	2295.241571	19.331866
53.688967	2282.827191	19.336883
53.824186	2278.518791	19.341901
53.486904	2279.421312	19.346919
53.715997	2286.578053	19.351936
53.897767	2287.971216	19.356954
53.930085	2288.335769	19.361971
53.736167	2295.803027	19.366989
53.746727	2299.622561	19.372007
54.184328	2292.108605	19.377024
53.697479	2299.529763	19.382042
53.667377	2301.019641	19.387059
53.997086	2302.049410	19.392077
53.974610	2298.132698	19.397095
53.936745	2295.401456	19.402112
53.960219	2303.015750	19.407130
53.876597	2295.837405	19.412147
54.061086	2318.933446	19.417165
54.240047	2324.584821	19.422183
54.373966	2324.706637	19.427200
54.551418	2342.481047	19.432218
54.487039	2331.968443	19.437235
54.828098	2325.640299	19.442253
54.974725	2338.476746	19.447271
54.944779	2331.123856	19.452288
54.620969	2331.282485	19.457306
54.809458	2336.024630	19.462323
54.592017	2329.948372	19.467341
54.447327	2335.372915	19.472359
54.733351	2327.588145	19.477376
54.487657	2336.039041	19.482394
54.675369	2360.401817	19.487411
54.727968	2354.628581	19.492429
54.953519	2367.154353	19.497447
55.029851	2365.998504	19.502464
55.066514	2358.549239	19.507482
55.340377	2375.341604	19.512499
55.649136	2384.757343	19.517517
55.454803	2384.243247	19.522535
55.582393	2376.740930	19.527552
55.352374	2398.327673	19.532570
55.408408	2397.186071	19.537587
55.617395	2396.694180	19.542605
55.542077	2403.982902	19.547623
55.913416	2388.668677	19.552640
55.658991	2400.508035	19.557658
55.809674	2394.905562	19.562675
55.915073	2389.057819	19.567693
55.916628	2394.224659	19.572711
56.181919	2385.890196	19.577728
55.814693	2389.116348	19.582746
55.683097	2389.455130	19.587763
56.023547	2385.283871	19.592781
55.945908	2393.630128	19.597799
56.115530	2402.369580	19.602816
56.223911	2414.135359	19.607834
56.563868	2407.024703	19.612851
56.770718	2407.315018	19.617869
56.300673	2420.000532	19.622887
56.396163	2414.410787	19.627904
56.509476	2417.476148	19.632922
56.683535	2409.656489	19.637939
57.003775	2417.666364	19.642957
56.819448	2409.365833	19.647975
56.847643	2402.452775	19.652992
57.039792	2411.489902	19.658010
57.051812	2411.867922	19.663027
57.157537	2405.527718	19.668045
56.965236	2414.228144	19.673063
56.985503	2408.259463	19.678080
57.026429	2418.944223	19.683098
57.003101	2413.858749	19.688115
56.995276	2419.712997	19.693133
56.854967	2419.725162	19.698151
57.087159	2435.720351	19.703168
57.200571	2443.554778	19.708186
57.352348	2451.053511	19.713203
57.307905	2441.071742	19.718221
56.829857	2442.518227	19.723239
57.254377	2458.526819	19.728256
57.357541	2467.133749	19.733274
57.420037	2469.728979	19.738291
57.898663	2468.932939	19.743309
57.744148	2473.253156	19.748327
57.864625	2474.072462	19.753344
57.615663	2466.562503	19.758362
57.938519	2481.678037	19.763379
58.245701	2493.493195	19.768397
58.261162	2508.332916	19.773415
58.542807	2501.048239	19.778432
58.195265	2487.965266	19.783450
58.406592	2503.609106	19.788467
58.394978	2501.677534	19.793485
58.370459	2509.463986	19.798503
58.484413	2500.493643	19.803520
58.391714	2507.063099	19.808538
58.419149	2509.908557	19.813555
58.455733	2506.267903	19.818573
58.174719	2511.660762	19.823591
58.931391	2505.202550	19.828608
58.613799	2499.614146	19.833626
58.740410	2507.127146	19.838643
58.725265	2495.790878	19.843661
58.597433	2511.325201	19.848679
59.195241	2518.089744	19.853696
58.940348	2529.399116	19.858714
58.951956	2535.321891	19.863731
59.380883	2532.366712	19.868749
59.132482	2537.528628	19.873767
59.476401	2534.263716	19.878784
59.336458	2539.865347	19.883802
59.252303	2537.177625	19.888819
59.515935	2539.973623	19.893837
59.491752	2547.249543	19.898855
59.617985	2529.513797	19.903872
59.555159	2536.316053	19.908890
59.689693	2540.433663	19.913907
59.916640	2532.413577	19.918925
59.552769	2539.148213	19.923943
59.515612	2539.029085	19.928960
59.774208	2548.226392	19.933978
59.823191	2557.771768	19.938995
60.083188	2559.928850	19.944013
60.091043	2561.700595	19.949031
60.130872	2560.523807	19.954048
60.402749	2560.666102	19.959066
59.926915	2567.349386	19.964083
60.096377	2555.434590	19.969101
59.891845	2564.214927	19.974119
60.365428	2579.680946	19.979136
60.652091	2589.392168	19.984154
60.574682	2588.779185	19.989171
60.777962	2594.486568	19.994189
60.578364	2589.640736	19.999207
60.980448	2586.788939	20.004224
60.865555	2577.796835	20.009242
61.005106	2590.298757	20.014259
61.193118	2573.643327	20.019277
61.176201	2585.895676	20.024295
60.674641	2584.825674	20.029312
60.906038	2583.592378	20.034330
61.008936	2583.999172	20.039347
61.136205	2580.679914	20.044365
61.030016	2586.782746	20.049383
61.112863	2584.368863	20.054400
61.176776	2603.266076	20.059418
61.223971	2610.602225	20.064435
61.646782	2600.940704	20.069453
61.776991	2612.843963	20.074471
62.152443	2599.931128	20.079488
62.453353	2591.751335	20.084506
62.340337	2574.995241	20.089523
62.641593	2566.292321	20.094541
62.160626	2568.444071	20.099559
62.386130	2556.468421	20.104576
62.570158	2542.163216	20.109594
62.453638	2555.309261	20.114611
62.570103	2531.471894	20.119629
62.803677	2517.106897	20.124647
62.311098	2515.947369	20.129664
62.477203	2516.501400	20.134682
62.435895	2510.374954	20.139699
62.661827	2510.047901	20.144717
62.334421	2515.625929	20.149735
62.173505	2506.273083	20.154752
62.466955	2500.789389	20.159770
62.359182	2509.290756	20.164787
62.657974	2516.618200	20.169805
62.518037	2535.732683	20.174823
62.465785	2548.645868	20.179840
62.724974	2548.345761	20.184858
62.504826	2546.351474	20.189875
62.823187	2532.636039	20.194893
62.871943	2541.298098	20.199911
62.710333	2547.751920	20.204928
62.985749	2558.527603	20.209946
62.959986	2568.195816	20.214963
63.318129	2572.906265	20.219981
63.221437	2578.143113	20.224999
63.077439	2581.275500	20.230016
63.491122	2575.616072	20.235034
63.316156	2578.940606	20.240051
63.607254	2590.550749	20.245069
63.558616	2597.988699	20.250087
63.784310	2605.404145	20.255104
63.909362	2594.381319	20.260122
63.617949	2608.134235	20.265139
63.987513	2599.231620	20.270157
63.814924	2600.184194	20.275175
63.715590	2603.274853	20.280192
64.191936	2598.590242	20.285210
63.798057	2611.424240	20.290227
64.190156	2601.579620	20.295245
64.013551	2608.616368	20.300263
64.367334	2637.153547	20.305280
64.524892	2627.297543	20.310298
64.346798	2640.278859	20.315315
64.512883	2642.096961	20.320333
64.677598	2642.301182	20.325351
64.617363	2634.108950	20.330368
64.835406	2634.673581	20.335386
64.811780	2638.644963	20.340403
64.950485	2636.450276	20.345421
64.739051	2637.230490	20.350439
64.820363	2633.457603	20.355456
64.784357	2629.133142	20.360474
64.568327	2644.256908	20.365491
64.868591	2660.428700	20.370509
64.918402	2658.885331	20.375527
64.991235	2661.810892	20.380544
65.258499	2666.499681	20.385562
65.424156	2670.197040	20.390579
65.129765	2663.863896	20.395597
65.206111	2666.384585	20.400615
65.226936	2687.855453	20.405632
65.539981	2688.353021	20.410650
65.477830	2691.670602	20.415667
65.512432	2704.562994	20.420685
65.707332	2698.385429	20.425703
65.483578	2698.156828	20.430720
65.670806	2687.618003	20.435738
65.683666	2705.170537	20.440755
66.182877	2705.201855	20.445773
66.398046	2719.962748	20.450791
66.110026	2727.336680	20.455808
66.423807	2715.655958	20.460826
66.421920	2719.891339	20.465843
66.269605	2724.551877	20.470861
66.591599	2713.954572	20.475879
66.413850	2722.719720	20.480896
66.575643	2718.748339	20.485914
66.060972	2723.985032	20.490931
66.545182	2713.546710	20.495949
66.605050	2725.049885	20.500967
66.854059	2747.563671	20.505984
67.405095	2751.470973	20.511002
67.442917	2763.175132	20.516019
67.276150	2756.528978	20.521037
67.324118	2746.712395	20.526055
66.932754	2745.884386	20.531072
66.978108	2756.014131	20.536090
67.448651	2772.435777	20.541107
67.777092	2774.209914	20.546125
67.944361	2775.470141	20.551143
67.673842	2769.848954	20.556160
67.782554	2766.372932	20.561178
67.772119	2771.263360	20.566195
67.764879	2761.473663	20.571213
68.000430	2756.423874	20.576231
67.981320	2764.620207	20.581248
67.691442	2762.507219	20.586266
67.743695	2765.873435	20.591283
68.085376	2768.491846	20.596301
68.175020	2763.165626	20.601319
67.645889	2774.315975	20.606336
67.593180	2762.095840	20.611354
67.816921	2768.791937	20.616371
67.830228	2790.585875	20.621389
68.076478	2798.839810	20.626407
68.103884	2798.042556	20.631424
67.999724	2793.684078	20.636442
68.114804	2813.763539	20.641459
68.445794	2830.122552	20.646477
68.648784	2820.302437	20.651495
68.683062	2828.767964	20.656512
69.004651	2815.103667	20.661530
69.033489	2821.974818	20.666547
69.170682	2813.469396	20.671565
69.203601	2808.009830	20.676583
69.116185	2816.401937	20.681600
69.100528	2807.068211	20.686618
68.915535	2818.196751	20.691635
69.326676	2810.267492	20.696653
69.848403	2826.623616	20.701671
69.592528	2829.552859	20.706688
69.561883	2813.415002	20.711706
69.545770	2823.217928	20.716723
69.565229	2835.691229	20.721741
70.166471	2839.789562	20.726759
70.140430	2846.189645	20.731776
69.827515	2834.703946	20.736794
69.535286	2834.915750	20.741811
69.959538	2837.868687	20.746829
70.271060	2833.311760	20.751847
69.972529	2849.220556	20.756864
70.069268	2838.065193	20.761882
70.260845	2836.931833	20.766899
70.237922	2841.066772	20.771917
70.277740	2839.909629	20.776935
70.095062	2842.609312	20.781952
70.621137	2864.681071	20.786970
70.521263	2875.960484	20.791987
70.502592	2878.572664	20.797005
70.467730	2874.970843	20.802023
70.356427	2883.893039	20.807040
70.523218	2863.746539	20.812058
70.929276	2856.147655	20.817075
70.725264	2870.264451	20.822093
71.315737	2864.862262	20.827111
71.009099	2878.294562	20.832128
71.291421	2872.484489	20.837146
71.411911	2872.073558	20.842163
71.360208	2873.083173	20.847181
71.388169	2860.378126	20.852199
71.263387	2868.814765	20.857216
71.539097	2864.416141	20.862234
71.559405	2879.294010	20.867251
71.281577	2901.951829	20.872269
71.759475	2903.563705	20.877287
71.645188	2904.707587	20.882304
71.621769	2908.364364	20.887322
71.947833	2906.375744	20.892339
71.928119	2929.013683	20.897357
71.970860	2918.509532	20.902375
71.752324	2933.725243	20.907392
72.273271	2942.670152	20.912410
72.628276	2947.254579	20.917427
72.919500	2958.706886	20.922445
73.053366	2941.719855	20.927463
72.855054	2931.209298	20.932480
72.978038	2930.709867	20.937498
72.820101	2922.971983	20.942515
72.763202	2919.556946	20.947533
72.921799	2911.830733	20.952551
72.770772	2923.136431	20.957568
72.653824	2916.012652	20.962586
73.054511	2921.481019	20.967603
73.246295	2943.407193	20.972621
73.207902	2945.154895	20.977639
73.452606	2944.698196	20.982656
73.144251	2944.737157	20.987674
73.315419	2943.789539	20.992691
73.121796	2951.998073	20.997709
73.404042	2952.458086	21.002727
73.161494	2953.631078	21.007744
73.102334	2959.790282	21.012762
73.443730	2971.469796	21.017779
73.426841	2977.529446	21.022797
73.583826	2975.936702	21.027815
73.781037	2987.181411	21.032832
74.084384	2982.727215	21.037850
74.191612	2995.036412	21.042867
74.164488	3011.683215	21.047885
74.702629	3005.660813	21.052903
74.610092	3016.887247	21.057920
74.615957	3006.917520	21.062938
74.602014	2988.836221	21.067955
74.238134	2995.524655	21.072973
74.463133	2997.871454	21.077991
74.647136	2998.385679	21.083008
74.450597	3008.550240	21.088026
74.671971	3009.012096	21.093043
74.771073	3021.335197	21.098061
74.841989	3006.267252	21.103079
75.060754	3020.521294	21.108096
75.044337	3040.622036	21.113114
75.362207	3038.764499	21.118131
75.318609	3042.249110	21.123149
75.409502	3035.037066	21.128167
75.295730	3036.623742	21.133184
75.300513	3050.429739	21.138202
75.599021	3042.245360	21.143219
75.339587	3050.550972	21.148237
75.879575	3040.505488	21.153255
75.687515	3050.029055	21.158272
75.589366	3040.244229	21.163290
75.543260	3036.460092	21.168307
75.737779	3059.167904	21.173325
76.301690	3058.381050	21.178343
75.872923	3061.301723	21.183360
76.281684	3057.011619	21.188378
76.323700	3052.526706	21.193395
76.267095	3060.961236	21.198413
76.518046	3062.116897	21.203431
76.272293	3061.987765	21.208448
76.176547	3059.627454	21.213466
76.618237	3076.774592	21.218483
76.457475	3095.447111	21.223501
76.667812	3085.580024	21.228519
76.638259	3086.231355	21.233536
76.836309	3083.913866	21.238554
77.045087	3065.343076	21.243571
76.558271	3065.208333	21.248589
76.608838	3074.823805	21.253607
76.893612	3087.453240	21.258624
76.721368	3092.777048	21.263642
76.862516	3081.979410	21.268659
77.015938	3103.008113	21.273677
77.311461	3114.109810	21.278695
77.177159	3127.123903	21.283712
77.163101	3121.515173	21.288730
77.552073	3117.698608	21.293747
77.668791	3132.849265	21.298765
77.759405	3140.820642	21.303783
78.088962	3145.860714	21.308800
77.852055	3144.621815	21.313818
78.016323	3140.610595	21.318835
78.789960	3129.527207	21.323853
79.333586	3117.681296	21.328871
79.392913	3111.566081	21.333888
79.299881	3105.092079	21.338906
79.450992	3090.271631	21.343923
79.480243	3092.831370	21.348941
79.459764	3082.192444	21.353959
79.434844	3064.754684	21.358976
79.193242	3048.488950	21.363994
79.514960	3040.816894	21.369011
79.097136	3049.278340	21.374029
79.313914	3034.578056	21.379047
79.376356	3038.502783	21.384064
79.089840	3041.095560	21.389082
79.555030	3037.409239	21.394099
79.264138	3049.091316	21.399117
79.292682	3035.505009	21.404135
79.263870	3038.722958	21.409152
79.234751	3065.770824	21.414170
79.335919	3076.199460	21.419187
79.429320	3076.258523	21.424205
79.361621	3084.282647	21.429223
79.691168	3079.506449	21.434240
80.013527	3090.540920	21.439258
80.112646	3091.777432	21.444275
80.105462	3105.267594	21.449293
80.087024	3100.145704	21.454311
80.122163	3097.473465	21.459328
79.987600	3104.730293	21.464346
80.073051	3094.699831	21.469363
80.226039	3109.013221	21.474381
80.559401	3123.056368	21.479399
80.731133	3129.877347	21.484416
80.755823	3129.510005	21.489434
80.930435	3128.277855	21.494451
80.940382	3140.409964	21.499469
80.658715	3124.582391	21.504487
81.228809	3123.068496	21.509504
80.811098	3131.350621	21.514522
81.155975	3124.259290	21.519539
80.989846	3131.378785	21.524557
81.089144	3150.791810	21.529575
81.038055	3158.244595	21.534592
81.040568	3164.422368	21.539610
81.459639	3150.684005	21.544627
81.481826	3165.177206	21.549645
81.388385	3181.456410	21.554663
81.786901	3175.496323	21.559680
81.740041	3186.380500	21.564698
81.983438	3186.698832	21.569715
81.726405	3186.427544	21.574733
81.894974	3190.663412	21.579751
82.014140	3194.734101	21.584768
82.067572	3218.458956	21.589786
82.605359	3213.020993	21.594803
82.347445	3215.311894	21.599821
82.336399	3230.965230	21.604839
82.519672	3223.993230	21.609856
82.623733	3228.812848	21.614874
82.686732	3241.733437	21.619891
82.989623	3247.840535	21.624909
82.935386	3253.912548	21.629927
83.147069	3245.712010	21.634944
83.001903	3257.960987	21.639962
83.430920	3246.379465	21.644979
83.360568	3249.811754	21.649997
83.605208	3245.791623	21.655015
83.759466	3252.038058	21.660032
83.304862	3255.943817	21.665050
83.147254	3245.227524	21.670067
83.545356	3265.730521	21.675085
83.742936	3272.748822	21.680103
84.056624	3277.260495	21.685120
83.733421	3276.390116	21.690138
83.989138	3282.644771	21.695155
83.765074	3287.757442	21.700173
83.802538	3288.944805	21.705191
83.868898	3288.164912	21.710208
84.069733	3303.781392	21.715226
84.419083	3303.454311	21.720243
84.411197	3304.480568	21.725261
84.341217	3302.428403	21.730279
84.912514	3304.036447	21.735296
84.678539	3316.784201	21.740314
84.792186	3303.393320	21.745331
84.940269	3310.388067	21.750349
84.738756	3330.525802	21.755367
85.340595	3335.055262	21.760384
85.114257	3335.000906	21.765402
85.098656	3335.417966	21.770419
85.278003	3340.549710	21.775437
85.275587	3343.127129	21.780455
85.372601	3332.798886	21.785472
85.161007	3339.922585	21.790490
85.536473	3336.927006	21.795507
85.771221	3357.739369	21.800525
85.938056	3364.612370	21.805543
86.023991	3356.312253	21.810560
85.903750	3360.309462	21.815578
85.967910	3362.864469	21.820595
85.970282	3360.646577	21.825613
85.721069	3360.812981	21.830631
86.282753	3358.546020	21.835648
85.913487	3374.575219	21.840666
86.188562	3378.563674	21.845683
86.359043	3384.831965	21.850701
86.009646	3399.044822	21.855719
86.381214	3392.119808	21.860736
86.599383	3422.065418	21.865754
86.797542	3426.984947	21.870771
86.960632	3428.464585	21.875789
86.931436	3427.340427	21.880807
87.298418	3415.070129	21.885824
87.270451	3432.992687	21.890842
87.309116	3432.361158	21.895859
87.800285	3445.931854	21.900877
87.449642	3453.416036	21.905895
87.857997	3449.796104	21.910912
87.806436	3449.350449	21.915930
87.972308	3451.536836	21.920947
87.851442	3450.328178	21.925965
87.895709	3449.818471	21.930983
88.086557	3447.368345	21.936000
87.911778	3462.661010	21.941018
87.807179	3439.264112	21.946035
88.349035	3453.524484	21.951053
88.124109	3473.462408	21.956071
88.648155	3472.891141	21.961088
88.903676	3472.077929	21.966106
89.025580	3465.858978	21.971123
89.200055	3456.242794	21.976141
89.135052	3456.485234	21.981159
89.319352	3447.971934	21.986176
89.029236	3452.295966	21.991194
89.231805	3451.769669	21.996211
89.212789	3451.210268	22.001229
89.029709	3466.778799	22.006247
89.315106	3456.367725	22.011264
89.633470	3461.192580	22.016282
89.415099	3458.895023	22.021299
89.470412	3458.868913	22.026317
89.502639	3459.383759	22.031335
89.792194	3448.822566	22.036352
89.623648	3458.358380	22.041370
89.594357	3463.526583	22.046387
90.280105	3465.178542	22.051405
90.399604	3477.364259	22.056423
90.723877	3467.090148	22.061440
90.583984	3460.268685	22.066458
90.196535	3442.333701	22.071475
90.224864	3451.214310	22.076493
90.459586	3469.620502	22.081511
90.686612	3462.788515	22.086528
90.786419	3482.673097	22.091546
90.732173	3476.455484	22.096563
90.991688	3473.286427	22.101581
90.887306	3481.535303	22.106599
90.973560	3470.297747	22.111616
90.852422	3465.806472	22.116634
91.067026	3487.637002	22.121651
91.275561	3501.443973	22.126669
91.454998	3510.143194	22.131687
91.423072	3505.774558	22.136704
91.360451	3501.175610	22.141722
91.303604	3509.968360	22.146739
91.964649	3512.163116	22.151757
91.625827	3520.170138	22.156775
91.985116	3519.574011	22.161792
92.418619	3520.919289	22.166810
92.298619	3523.311747	22.171827
92.559511	3513.140535	22.176845
92.469973	3528.415742	22.181863
92.374198	3522.391953	22.186880
92.587186	3524.535440	22.191898
92.533542	3523.555197	22.196915
92.650871	3523.042490	22.201933
92.415661	3527.802243	22.206951
92.461275	3535.094270	22.211968
92.680487	3541.336766	22.216986
92.987082	3545.557808	22.222003
92.668712	3549.631500	22.227021
92.890672	3555.401576	22.232039
93.116896	3559.630719	22.237056
93.230140	3573.919435	22.242074
93.028436	3582.028130	22.247091
93.362638	3576.399879	22.252109
93.567342	3573.879085	22.257127
93.583358	3591.576136	22.262144
93.628543	3597.058970	22.267162
93.519016	3611.870968	22.272179
93.762441	3609.719226	22.277197
93.718756	3615.786559	22.282215
94.287999	3621.797851	22.287232
94.529541	3634.801236	22.292250
94.449153	3637.440698	22.297267
94.690941	3626.702918	22.302285
94.625861	3635.667759	22.307303
94.604661	3629.806671	22.312320
94.953467	3642.645855	22.317338
94.844182	3638.640361	22.322355
94.801155	3633.869904	22.327373
94.713871	3633.429153	22.332391
94.670405	3631.784919	22.337408
95.011710	3652.299876	22.342426
94.609383	3660.575909	22.347443
94.998846	3663.473996	22.352461
95.068811	3668.310210	22.357479
95.284465	3682.410425	22.362496
95.934661	3691.233712	22.367514
95.856542	3687.975277	22.372531
95.823022	3688.479375	22.377549
95.862829	3698.421861	22.382567
96.252827	3691.903616	22.387584
96.398626	3679.009938	22.392602
96.387915	3679.394762	22.397619
96.487200	3689.008376	22.402637
96.546964	3683.472617	22.407655
96.426788	3682.435319	22.412672
96.452874	3704.556615	22.417690
96.621050	3715.568160	22.422707
96.973694	3716.451998	22.427725
96.691776	3721.859598	22.432743
96.755621	3718.750796	22.437760
96.995490	3714.617234	22.442778
96.452244	3730.990010	22.447795
96.846568	3742.520107	22.452813
96.863542	3745.239250	22.457831
97.327642	3759.288910	22.462848
97.780273	3772.268197	22.467866
97.541614	3793.310853	22.472883
98.064550	3774.799206	22.477901
97.889434	3780.742819	22.482919
98.075293	3769.884054	22.487936
98.244916	3778.706932	22.492954
98.152714	3774.643611	22.497971
98.361002	3769.162803	22.502989
98.288145	3776.377869	22.508007
98.347861	3777.066128	22.513024
98.476020	3789.673161	22.518042
98.368725	3802.327975	22.523059
98.234219	3807.010400	22.528077
98.205070	3808.272147	22.533095
98.497818	3817.501785	22.538112
98.787393	3825.391464	22.543130
98.708425	3836.945972	22.548147
98.914889	3837.919993	22.553165
99.418887	3846.879967	22.558183
99.482316	3855.472812	22.563200
99.583754	3864.288521	22.568218
99.570779	3866.874009	22.573235
99.629211	3859.667523	22.578253
99.268816	3867.120428	22.583271
99.449068	3870.910954	22.588288
99.863277	3865.856687	22.593306
99.859479	3877.908212	22.598323
100.156258	3885.957255	22.603341
99.934552	3892.376407	22.608359
99.813267	3902.854476	22.613376
100.108225	3900.132010	22.618394
100.523889	3917.477022	22.623411
100.831237	3914.434764	22.628429
100.899158	3926.062680	22.633447
100.889164	3927.821702	22.638464
101.436894	3925.884927	22.643482
100.942838	3930.432776	22.648499
100.807709	3929.904458	22.653517
101.036588	3921.523017	22.658535
100.880574	3924.349229	22.663552
101.612191	3940.233394	22.668570
101.319497	3961.954360	22.673587
101.737973	3956.592582	22.678605
101.670790	3962.589071	22.683623
101.610865	3967.428789	22.688640
101.836005	3956.104209	22.693658
102.146907	3958.751350	22.698675
101.900950	3966.238763	22.703693
102.254221	3979.724174	22.708711
102.171263	3972.719539	22.713728
102.280916	3978.930131	22.718746
102.183472	3975.425339	22.723763
102.248101	3980.971296	22.728781
102.658257	4004.211806	22.733799
102.679265	4006.969687	22.738816
103.029272	4002.031812	22.743834
102.872917	4018.902538	22.748851
103.061867	4009.522048	22.753869
102.963745	4024.261842	22.758887
103.222506	4037.032343	22.763904
103.342215	4039.079073	22.768922
103.430431	4037.180941	22.773939
103.604217	4028.636730	22.778957
103.569309	4028.781552	22.783975
103.763781	4047.937508	22.788992
104.158520	4050.262134	22.794010
104.130841	4068.976029	22.799027
104.515074	4058.927949	22.804045
104.747921	4058.075056	22.809063
104.433692	4058.291951	22.814080
104.790843	4060.988376	22.819098
104.718812	4069.406278	22.824115
104.747365	4060.732591	22.829133
104.875444	4059.940457	22.834151
104.584038	4061.248762	22.839168
105.163782	4063.722467	22.844186
104.882373	4065.873281	22.849203
104.867121	4080.517317	22.854221
104.869104	4077.659026	22.859239
104.950745	4088.185110	22.864256
105.248479	4088.653711	22.869274
105.056420	4103.034104	22.874291
105.344962	4118.661070	22.879309
105.624371	4116.144007	22.884327
105.400315	4121.190095	22.889344
105.940649	4124.337984	22.894362
105.919644	4139.088410	22.899379
105.894203	4153.180321	22.904397
105.973444	4153.812778	22.909415
106.280555	4154.838428	22.914432
106.406239	4144.146319	22.919450
106.308833	4166.409936	22.924467
106.868616	4179.458249	22.929485
106.804880	4180.227573	22.934503
106.899955	4190.081337	22.939520
107.170558	4175.080262	22.944538
107.200633	4178.862560	22.949555
107.088669	4182.589627	22.954573
107.365713	4178.742654	22.959591
107.459383	4199.336412	22.964608
107.503867	4204.657528	22.969626
107.628388	4209.261017	22.974643
107.828624	4198.781973	22.979661
107.956146	4203.757869	22.984679
107.703172	4210.789462	22.989696
108.166519	4202.667842	22.994714
107.886215	4210.515649	22.999731
108.056303	4228.494132	23.004749
108.291256	4239.220870	23.009767
108.320349	4234.648763	23.014784
108.760232	4232.560010	23.019802
108.700472	4235.915318	23.024819
108.568499	4251.506421	23.029837
109.181460	4257.801297	23.034855
109.094296	4268.234851	23.039872
109.219014	4268.851408	23.044890
109.097873	4266.798611	23.049907
109.127902	4274.340509	23.054925
109.166360	4283.873743	23.059943
109.280229	4289.856443	23.064960
109.712641	4292.942122	23.069978
109.682444	4305.628342	23.074995
109.593821	4308.429721	23.080013
109.747121	4313.714646	23.085031
110.024669	4330.024862	23.090048
110.293309	4318.007864	23.095066
110.406196	4326.710315	23.100083
110.171711	4318.022563	23.105101
110.221239	4334.155949	23.110119
110.493008	4348.151882	23.115136
111.123587	4344.989557	23.120154
111.221222	4353.430129	23.125171
111.043256	4356.284310	23.130189
111.193295	4345.601547	23.135207
111.100685	4345.831881	23.140224
111.519367	4345.126347	23.145242
111.461457	4348.136815	23.150259
111.339169	4355.198774	23.155277
111.313941	4343.134997	23.160295
111.237131	4357.559410	23.165312
111.355851	4368.496729	23.170330
111.423063	4386.129931	23.175347
111.533378	4390.119763	23.180365
111.781196	4405.965149	23.185383
111.735836	4421.944622	23.190400
112.010547	4422.876334	23.195418
112.290436	4422.115044	23.200435
112.197896	4440.690281	23.205453
112.448096	4429.556444	23.210471
112.661195	4441.423588	23.215488
112.802432	4463.760526	23.220506
113.212698	4465.974182	23.225523
112.976906	4470.329967	23.230541
113.417169	4463.998472	23.235559
113.409943	4466.482451	23.240576
113.172858	4475.258100	23.245594
113.851967	4474.854822	23.250611
113.630028	4476.672092	23.255629
113.710844	4487.226128	23.260647
113.847417	4501.870762	23.265664
114.069842	4499.610532	23.270682
113.962711	4499.696072	23.275699
114.060853	4501.220792	23.280717
114.826634	4519.582175	23.285735
114.659238	4524.867962	23.290752
114.577366	4527.276529	23.295770
115.125744	4520.754698	23.300787
115.064873	4515.946678	23.305805
115.309924	4511.391973	23.310823
115.112367	4511.938776	23.315840
115.334259	4514.179329	23.320858
115.356284	4512.939143	23.325875
115.350277	4518.496566	23.330893
115.945887	4504.385014	23.335911
115.595869	4513.269949	23.340928
115.584969	4525.011604	23.345946
115.971748	4534.530369	23.350963
115.614210	4547.427905	23.355981
115.701956	4543.794323	23.360999
116.442804	4543.359959	23.366016
116.207960	4543.809650	23.371034
116.233709	4557.840291	23.376051
116.138732	4570.262509	23.381069
116.568336	4570.256175	23.386087
116.837128	4575.250581	23.391104
116.341019	4581.591845	23.396122
117.030105	4595.620599	23.401139
116.641537	4605.092322	23.406157
116.776173	4606.684398	23.411175
116.909703	4618.564373	23.416192
116.861230	4636.796121	23.421210
117.121376	4638.900001	23.426227
117.024607	4646.655050	23.431245
117.375411	4655.331562	23.436263
117.918112	4664.809030	23.441280
117.557224	4671.703066	23.446298
117.880913	4673.486071	23.451315
118.093707	4691.980685	23.456333
118.481427	4693.934425	23.461351
118.583614	4697.947665	23.466368
118.507323	4701.737616	23.471386
118.966761	4699.596907	23.476403
118.798283	4704.053740	23.481421
119.067505	4693.642017	23.486439
119.056797	4696.479821	23.491456
119.006323	4707.901447	23.496474
118.996132	4719.798126	23.501491
119.288541	4736.996193	23.506509
119.465647	4732.062832	23.511527
119.618889	4727.613172	23.516544
119.848500	4729.242828	23.521562
120.474021	4732.581815	23.526579
120.289831	4748.538935	23.531597
120.697391	4745.045482	23.536615
120.763934	4734.175926	23.541632
120.467255	4732.347729	23.546650
120.658034	4728.843216	23.551667
120.764997	4734.234806	23.556685
121.019618	4736.109076	23.561703
120.857134	4743.782609	23.566720
120.693159	4738.951620	23.571738
121.490272	4741.884842	23.576755
120.975347	4752.103726	23.581773
121.146778	4737.320079	23.586791
121.256547	4758.143345	23.591808
121.161484	4773.150881	23.596826
121.610745	4771.680490	23.601843
121.719869	4777.489496	23.606861
121.823329	4782.038307	23.611879
122.113530	4797.668879	23.616896
122.066641	4802.427333	23.621914
122.298822	4792.787706	23.626931
122.184935	4805.561651	23.631949
122.462013	4802.939427	23.636967
122.168405	4813.676125	23.641984
122.240715	4835.897171	23.647002
122.708031	4834.140678	23.652019
122.666804	4843.852189	23.657037
123.088910	4854.009064	23.662055
123.198001	4862.330094	23.667072
123.120947	4864.812687	23.672090
123.589606	4856.106122	23.677107
123.454879	4877.078679	23.682125
123.550211	4873.029994	23.687143
123.829222	4871.175286	23.692160
123.925853	4890.994623	23.697178
123.748395	4883.212396	23.702195
123.866144	4895.638732	23.707213
123.895834	4887.707826	23.712231
124.105526	4905.996297	23.717248
124.044095	4916.792817	23.722266
124.811628	4909.214714	23.727283
124.636516	4920.019921	23.732301
124.644387	4926.694787	23.737319
124.620554	4939.577218	23.742336
124.292332	4954.772378	23.747354
124.656359	4960.665902	23.752371
124.842301	4984.184452	23.757389
125.243117	4976.169150	23.762407
125.270552	4990.108673	23.767424
125.377796	5015.993699	23.772442
125.877710	5009.153680	23.777459
125.960273	5009.692026	23.782477
125.850598	5012.387539	23.787495
126.469958	5027.566218	23.792512
126.710306	5030.169736	23.797530
126.931484	5031.062823	23.802547
127.120742	5029.877749	23.807565
127.348808	5019.104959	23.812583
127.094494	5025.650954	23.817600
126.995528	5030.572770	23.822618
127.224860	5012.960778	23.827635
127.197616	5024.858847	23.832653
127.289596	5027.123341	23.837671
127.665936	5027.907508	23.842688
127.615846	5047.355513	23.847706
128.115314	5048.585792	23.852723
128.034669	5052.814734	23.857741
128.305267	5045.266232	23.862759
128.373843	5042.393989	23.867776
128.248081	5049.776244	23.872794
128.688909	5045.125650	23.877811
128.554115	5044.047314	23.882829
128.569097	5057.173051	23.887847
128.541431	5067.249948	23.892864
128.555830	5068.955654	23.897882
129.114589	5070.167828	23.902899
129.112393	5078.563368	23.907917
129.204743	5097.493089	23.912935
129.470602	5097.129730	23.917952
129.290322	5108.374106	23.922970
130.031913	5100.778802	23.927987
129.967298	5104.093384	23.933005
129.894063	5095.863299	23.938023
130.342860	5102.523014	23.943040
130.372825	5122.474448	23.948058
130.434431	5126.472247	23.953075
130.183277	5129.451534	23.958093
130.385030	5125.336248	23.963111
130.759915	5120.956553	23.968128
130.659334	5129.552691	23.973146
130.825912	5133.211983	23.978163
130.948026	5156.260292	23.983181
131.149024	5153.289815	23.988199
131.492776	5156.714739	23.993216
131.257805	5169.619234	23.998234
131.270141	5164.608153	24.003251
131.453882	5177.943897	24.008269
131.319764	5196.752506	24.013287
131.880562	5193.662502	24.018304
131.550661	5202.762566	24.023322
132.022332	5212.913362	24.028339
132.019957	5219.119526	24.033357
131.785671	5222.373860	24.038375
132.426482	5221.088453	24.043392
132.493925	5247.001472	24.048410
132.735584	5247.634831	24.053427
133.184401	5256.740580	24.058445
133.299041	5252.975873	24.063463
133.592826	5266.908594	24.068480
133.321505	5285.671532	24.073498
133.695561	5277.637520	24.078515
133.550026	5284.213490	24.083533
133.377244	5292.702437	24.088551
133.596507	5294.052155	24.093568
133.775186	5316.293941	24.098586
133.758630	5325.529790	24.103603
133.802481	5320.752802	24.108621
134.086033	5335.427543	24.113639
134.411222	5338.691828	24.118656
134.736193	5349.668585	24.123674
134.788900	5351.158942	24.128691
135.022212	5361.985894	24.133709
135.034047	5371.267597	24.138727
135.861480	5357.924690	24.143744
135.588140	5366.204703	24.148762
135.547273	5360.601753	24.153779
135.752073	5359.263909	24.158797
135.659350	5362.100756	24.163815
136.197587	5390.761013	24.168832
135.970699	5392.638187	24.173850
135.955479	5385.086305	24.178867
136.332301	5390.098384	24.183885
136.426108	5399.448070	24.188903
136.723452	5405.537293	24.193920
136.625123	5421.789066	24.198938
136.671909	5422.408658	24.203955
136.928472	5425.079684	24.208973
137.143832	5424.969835	24.213991
137.537974	5434.505322	24.219008
137.301900	5450.296025	24.224026
137.448922	5451.609285	24.229043
137.601759	5447.803034	24.234061
137.388218	5467.594711	24.239079
137.736631	5450.447850	24.244096
138.000469	5480.241678	24.249114
137.856965	5482.502089	24.254131
138.275118	5486.419537	24.259149
138.158693	5489.483624	24.264167
138.859293	5496.086852	24.269184
138.919408	5517.114220	24.274202
139.056002	5510.853518	24.279219
139.077860	5501.258766	24.284237
139.246228	5514.528032	24.289255
139.576176	5501.987340	24.294272
139.357746	5510.726008	24.299290
139.384440	5504.878567	24.304307
139.846187	5501.810588	24.309325
139.888923	5524.562936	24.314343
140.276134	5534.768333	24.319360
140.182176	5532.087914	24.324378
140.374039	5529.446109	24.329395
140.290827	5527.711228	24.334413
140.175832	5533.527156	24.339431
140.674790	5556.520728	24.344448
140.198579	5564.565700	24.349466
140.314112	5570.531348	24.354483
141.214862	5572.882549	24.359501
141.483134	5575.052146	24.364519
142.264837	5563.385056	24.369536
142.073421	5571.790590	24.374554
142.495323	5568.817068	24.379571
142.611211	5555.791201	24.384589
142.255117	5544.245738	24.389607
142.814666	5539.428156	24.394624
142.390751	5532.208856	24.399642
142.361146	5550.141331	24.404659
142.559210	5560.257317	24.409677
142.459292	5571.526995	24.414695
142.638596	5560.849704	24.419712
142.610463	5574.091347	24.424730
142.901245	5590.145157	24.429747
143.135210	5593.853614	24.434765
142.923489	5601.030342	24.439783
143.185896	5607.169278	24.444800
143.493095	5634.033704	24.449818
143.519807	5630.621226	24.454835
143.564874	5628.927247	24.459853
143.474656	5656.259469	24.464871
143.941921	5660.848107	24.469888
143.994667	5673.359419	24.474906
144.197621	5684.681600	24.479923
144.493528	5696.667945	24.484941
144.448745	5708.066620	24.489959
144.625757	5708.249266	24.494976
144.449650	5725.446085	24.499994
144.370342	5739.938333	24.505011
144.903936	5746.159185	24.510029
144.957742	5765.678900	24.515047
145.711999	5762.404520	24.520064
145.587407	5767.989188	24.525082
145.430551	5769.549977	24.530099
145.844782	5776.985756	24.535117
146.160492	5779.890528	24.540135
146.432787	5775.980177	24.545152
146.506124	5776.981854	24.550170
146.647126	5780.049804	24.555187
147.049148	5794.915395	24.560205
146.925659	5808.670473	24.565223
147.352770	5811.364732	24.570240
147.460574	5808.132043	24.575258
147.155078	5812.186983	24.580275
147.688515	5803.898330	24.585293
147.581968	5804.289047	24.590311
147.540088	5807.597014	24.595328
147.832916	5825.491003	24.600346
147.693911	5834.454015	24.605363
148.115810	5829.051689	24.610381
147.690884	5843.024014	24.615399
147.987901	5857.031522	24.620416
148.285004	5869.680277	24.625434
148.322735	5895.099571	24.630451
148.610192	5897.754743	24.635469
148.674268	5909.098452	24.640487
149.005562	5914.241494	24.645504
148.989118	5935.612108	24.650522
149.000299	5942.196426	24.655539
149.316814	5946.354434	24.660557
149.131182	5966.899204	24.665575
149.320452	5980.511737	24.670592
149.583760	5987.767124	24.675610
149.859466	5995.925331	24.680627
150.565590	6011.481441	24.685645
151.037862	6019.597308	24.690663
151.181745	6014.614533	24.695680
151.370365	6018.142288	24.700698
151.524450	6008.777895	24.705715
151.722935	6009.662862	24.710733
151.563007	6010.945646	24.715751
151.682415	6006.133574	24.720768
151.834750	6005.574293	24.725786
151.502025	6017.646962	24.730803
151.835125	6015.142270	24.735821
151.986481	6029.602746	24.740839
152.260768	6039.919339	24.745856
152.131734	6048.534707	24.750874
152.209435	6055.232782	24.755891
152.673634	6063.283871	24.760909
152.577412	6086.170171	24.765927
152.538503	6081.282608	24.770944
152.802219	6087.930584	24.775962
152.538681	6110.839664	24.780979
153.052917	6114.448494	24.785997
153.299179	6119.240098	24.791015
153.238163	6133.082291	24.796032
153.864224	6146.921171	24.801050
153.912212	6142.037042	24.806067
153.798078	6139.148084	24.811085
153.816659	6160.363948	24.816103
153.787076	6174.569384	24.821120
154.344126	6179.764647	24.826138
154.334513	6194.476756	24.831155
154.689754	6206.427305	24.836173
154.711690	6216.406596	24.841191
154.860630	6234.532520	24.846208
155.143060	6233.751859	24.851226
155.101113	6244.539945	24.856243
155.283045	6252.057062	24.861261
155.567146	6270.893984	24.866279
155.563314	6276.847477	24.871296
156.013878	6280.965327	24.876314
156.190455	6307.671626	24.881331
156.142967	6301.015072	24.886349
156.265446	6306.322152	24.891367
156.425145	6326.607009	24.896384
156.427410	6329.474529	24.901402
156.456293	6348.616603	24.906419
156.785937	6357.520949	24.911437
156.546530	6366.006180	24.916455
157.061514	6386.966196	24.921472
157.426441	6394.097005	24.926490
157.564353	6401.864337	24.931507
157.601808	6421.555896	24.936525
158.014733	6428.568917	24.941543
158.461322	6420.263873	24.946560
158.596178	6440.046147	24.951578
158.737976	6451.772067	24.956595
159.195770	6444.953064	24.961613
159.134098	6452.402116	24.966631
158.933800	6455.769316	24.971648
159.439110	6452.022276	24.976666
159.386866	6468.566044	24.981683
159.414787	6474.401255	24.986701
159.591212	6487.808587	24.991719
159.841113	6484.645153	24.996736
160.127433	6503.828998	25.001754
160.079578	6514.953401	25.006771
160.561635	6515.679890	25.011789
160.796662	6520.287730	25.016807
160.564143	6526.940273	25.021824
161.010876	6515.967884	25.026842
161.061368	6544.211670	25.031859
161.484015	6540.202406	25.036877
161.439670	6541.085993	25.041895
161.782490	6548.505225	25.046912
161.994946	6541.783516	25.051930
161.789912	6542.475563	25.056947
161.825025	6539.875095	25.061965
161.906900	6547.642782	25.066983
161.840538	6558.504228	25.072000
162.154667	6565.094814	25.077018
162.237864	6575.781361	25.082035
162.271181	6590.670344	25.087053
162.577333	6598.273265	25.092071
162.733454	6598.149253	25.097088
163.262050	6607.136119	25.102106
162.936350	6633.134699	25.107123
163.342640	6626.843907	25.112141
163.582991	6639.390643	25.117159
163.667342	6645.869978	25.122176
164.016440	6653.631312	25.127194
164.101673	6660.005080	25.132211
164.175167	6657.091615	25.137229
164.143895	6688.621850	25.142247
164.516725	6687.501015	25.147264
164.903964	6685.470686	25.152282
164.839121	6701.411663	25.157299
164.813120	6708.958229	25.162317
165.471699	6725.298475	25.167335
165.201304	6722.872571	25.172352
165.645203	6722.371429	25.177370
165.534906	6727.190965	25.182387
166.027310	6740.574903	25.187405
166.438952	6738.496615	25.192423
166.333148	6748.812929	25.197440
166.646209	6738.578479	25.202458
166.402237	6765.029267	25.207475
166.832751	6763.893723	25.212493
167.244542	6764.053905	25.217511
167.057493	6775.635017	25.222528
167.531978	6770.643347	25.227546
167.174314	6797.061174	25.232563
167.387960	6807.008724	25.237581
167.687168	6811.613506	25.242599
168.002819	6830.686091	25.247616
168.335125	6836.832495	25.252634
167.978597	6854.141997	25.257651
168.143814	6843.938914	25.262669
168.306550	6854.724710	25.267687
167.944153	6871.079965	25.272704
168.481636	6869.096474	25.277722
168.557061	6895.257379	25.282739
169.100993	6903.196292	25.287757
169.453260	6923.407203	25.292775
169.593735	6926.081277	25.297792
169.893768	6935.597337	25.302810
169.748854	6942.403691	25.307827
170.076684	6956.568629	25.312845
170.186096	6965.696506	25.317863
170.341363	6958.265353	25.322880
170.648397	6978.098791	25.327898
170.664539	6978.400736	25.332915
170.703476	6995.854292	25.337933
170.846979	6986.558640	25.342951
170.931048	7005.780100	25.347968
171.310787	7018.833687	25.352986
171.429128	7029.202585	25.358003
171.247700	7032.256106	25.363021
171.774018	7054.593007	25.368039
171.719081	7062.905233	25.373056
171.897981	7063.975147	25.378074
172.006611	7082.904810	25.383091
172.355743	7096.802110	25.388109
172.207342	7101.503521	25.393127
172.604981	7114.516570	25.398144
172.828841	7116.387402	25.403162
172.656990	7140.617921	25.408179
173.085072	7162.891175	25.413197
173.695639	7154.815308	25.418215
173.462649	7179.376668	25.423232
173.799196	7187.733562	25.428250
173.886052	7190.428821	25.433267
174.171101	7204.201889	25.438285
174.478453	7213.722469	25.443303
174.639805	7222.925235	25.448320
175.050236	7212.876764	25.453338
175.180158	7226.625406	25.458355
175.354967	7237.593677	25.463373
175.713843	7234.279737	25.468391
175.454338	7247.319769	25.473408
175.658821	7247.786831	25.478426
175.668518	7257.855325	25.483443
176.156441	7273.165868	25.488461
176.267414	7278.704889	25.493479
176.127127	7285.874184	25.498496
176.414021	7306.706631	25.503514
176.738578	7308.626742	25.508531
176.764016	7310.846331	25.513549
177.136073	7324.488399	25.518567
177.254681	7346.768778	25.523584
177.492291	7333.971382	25.528602
177.603901	7344.701950	25.533619
177.468452	7365.460964	25.538637
177.908421	7361.132410	25.543655
177.960304	7388.512830	25.548672
178.091709	7403.711959	25.553690
178.275297	7402.615736	25.558707
177.778609	7413.174226	25.563725
178.595837	7428.007531	25.568743
178.727189	7444.517606	25.573760
178.969800	7462.301191	25.578778
179.242472	7470.230150	25.583795
179.193767	7480.172766	25.588813
179.352006	7495.330727	25.593831
179.634509	7509.288609	25.598848
180.022544	7522.120210	25.603866
180.298895	7525.709092	25.608883
180.067121	7536.103472	25.613901
180.321511	7524.966658	25.618919
180.831412	7557.466060	25.623936
180.801911	7564.155940	25.628954
180.780736	7559.463351	25.633971
180.579982	7591.779475	25.638989
181.086674	7597.141435	25.644007
181.069987	7615.187649	25.649024
181.304946	7624.878193	25.654042
181.500121	7638.232430	25.659059
181.927199	7668.225740	25.664077
182.521437	7666.491981	25.669095
182.237307	7681.128932	25.674112
182.708571	7690.948664	25.679130
182.996825	7687.588444	25.684148
183.108274	7702.263071	25.689165
183.735505	7702.240994	25.694183
183.689136	7728.335435	25.699200
183.855849	7733.124510	25.704218
184.231489	7719.215755	25.709236
184.178190	7737.347427	25.714253
184.649763	7728.246091	25.719271
184.785544	7709.748009	25.724288
185.330244	7717.857992	25.729306
185.802780	7720.843594	25.734324
185.808349	7711.320831	25.739341
185.765905	7700.696246	25.744359
185.635023	7705.908878	25.749376
185.812079	7703.646750	25.754394
186.297041	7709.962753	25.759412
186.066905	7728.937014	25.764429
186.364304	7714.194065	25.769447
186.417467	7713.794532	25.774464
186.218451	7723.773862	25.779482
186.501002	7743.835697	25.784500
186.383011	7745.516390	25.789517
186.873514	7752.054999	25.794535
186.574327	7782.107664	25.799552
187.015492	7787.090640	25.804570
187.255959	7804.454000	25.809588
187.141718	7831.221989	25.814605
187.443443	7832.082743	25.819623
187.728698	7845.590411	25.824640
187.767202	7869.864118	25.829658
188.315886	7873.186985	25.834676
188.400034	7894.770996	25.839693
188.600038	7909.441153	25.844711
188.417385	7920.470061	25.849728
188.864861	7938.055524	25.854746
189.462677	7955.565108	25.859764
189.295070	7957.335571	25.864781
189.747733	7968.297857	25.869799
189.629721	7993.392253	25.874816
190.033253	7987.712745	25.879834
190.094062	8002.810428	25.884852
190.184591	8023.343118	25.889869
190.486741	8023.569589	25.894887
190.638055	8027.088035	25.899904
190.567257	8049.574346	25.904922
191.012709	8050.543612	25.909940
190.480947	8079.707393	25.914957
190.898279	8083.896365	25.919975
191.050221	8101.233265	25.924992
191.464657	8119.658312	25.930010
192.026437	8133.935409	25.935028
192.020864	8152.373158	25.940045
192.658045	8155.803951	25.945063
192.827541	8177.320468	25.950080
192.632285	8185.279946	25.955098
193.153541	8183.418881	25.960116
193.327859	8207.477517	25.965133
193.395479	8214.719162	25.970151
193.894807	8217.775744	25.975168
194.061212	8224.283605	25.980186
194.373996	8231.798966	25.985204
194.099408	8241.789114	25.990221
194.397131	8242.583646	25.995239
194.734031	8256.643723	26.000256
194.423626	8272.894249	26.005274
195.157066	8268.358915	26.010292
195.292223	8281.595427	26.015309
195.594476	8297.686934	26.020327
195.682390	8303.723400	26.025344
195.526972	8317.786082	26.030362
195.733690	8321.071106	26.035380
195.908775	8339.049851	26.040397
196.033774	8354.136869	26.045415
196.143375	8369.167733	26.050432
196.483853	8387.660379	26.055450
197.102924	8397.639581	26.060468
197.156540	8401.483338	26.065485
197.238507	8420.226551	26.070503
197.658829	8426.070793	26.075520
197.776963	8436.792059	26.080538
198.154916	8442.826018	26.085556
198.267589	8463.051642	26.090573
199.216047	8457.737564	26.095591
199.597024	8451.810062	26.100608
199.337390	8451.435193	26.105626
199.881532	8451.866250	26.110644
199.862830	8449.575020	26.115661
200.080742	8453.141576	26.120679
200.024383	8451.282459	26.125696
199.714697	8454.115919	26.130714
200.104167	8450.094920	26.135732
199.985226	8477.815397	26.140749
200.498533	8475.731297	26.145767
200.230701	8487.774360	26.150784
200.387008	8505.902271	26.155802
200.721010	8503.451330	26.160820
200.762871	8531.263914	26.165837
200.785325	8541.703055	26.170855
200.656363	8552.601110	26.175872
200.942978	8564.093931	26.180890
201.436735	8576.865525	26.185908
201.984444	8603.911418	26.190925
202.227157	8603.143666	26.195943
202.187751	8626.066904	26.200960
202.057268	8641.730042	26.205978
202.337026	8652.536653	26.210996
202.836421	8672.777638	26.216013
203.328440	8682.039157	26.221031
203.520063	8689.748761	26.226048
203.519959	8704.823419	26.231066
204.343647	8701.499202	26.236084
204.059877	8719.213963	26.241101
204.101481	8724.030384	26.246119
204.559190	8726.195046	26.251136
204.739908	8745.505247	26.256154
204.926164	8751.501822	26.261172
205.271259	8754.418639	26.266189
205.284793	8764.834963	26.271207
205.993946	8773.799881	26.276224
205.847646	8782.647783	26.281242
205.976741	8792.775002	26.286260
205.911410	8800.812459	26.291277
206.318890	8820.002407	26.296295
206.728309	8817.791210	26.301312
206.837795	8837.935616	26.306330
206.704079	8849.872600	26.311348
206.825518	8869.140079	26.316365
207.361743	8879.152094	26.321383
207.696067	8881.163717	26.326400
207.550465	8902.492282	26.331418
207.636589	8911.255206	26.336436
207.756663	8928.897967	26.341453
207.844429	8947.483136	26.346471
208.266035	8956.359831	26.351488
207.910150	8989.768025	26.356506
208.565129	9005.745442	26.361524
208.855868	9024.557253	26.366541
209.218500	9041.543736	26.371559
209.367976	9051.574236	26.376576
209.339493	9072.717934	26.381594
209.686415	9087.656603	26.386612
209.732179	9098.481951	26.391629
209.850262	9125.302172	26.396647
210.489690	9125.461523	26.401664
210.779406	9159.372731	26.406682
210.858841	9157.345902	26.411700
211.515211	9177.392962	26.416717
211.641383	9199.343986	26.421735
212.021196	9197.697761	26.426752
211.694807	9204.867339	26.431770
212.264698	9220.530788	26.436788
212.405619	9231.217119	26.441805
212.336977	9238.112296	26.446823
212.844549	9242.329318	26.451840
213.000834	9261.746382	26.456858
213.234549	9254.944527	26.461876
213.539662	9266.768215	26.466893
213.537391	9276.511030	26.471911
213.916153	9283.852328	26.476928
214.089832	9297.845366	26.481946
214.139358	9301.742732	26.486964
214.476162	9307.409803	26.491981
214.388046	9319.186828	26.496999
214.680421	9334.309536	26.502016
214.704912	9347.824326	26.507034
215.171004	9360.735180	26.512052
215.281800	9376.443252	26.517069
215.348048	9393.170467	26.522087
215.591848	9411.721895	26.527104
215.596214	9427.413146	26.532122
216.428800	9445.193976	26.537140
216.299346	9458.046390	26.542157
216.274829	9470.716432	26.547175
216.857794	9481.375367	26.552192
217.133950	9496.460689	26.557210
217.476986	9508.701908	26.562228
217.775169	9511.343048	26.567245
217.985153	9535.585823	26.572263
218.185625	9544.695647	26.577280
218.523455	9553.748168	26.582298
218.683074	9549.658855	26.587316
219.011664	9570.251334	26.592333
219.103992	9584.400442	26.597351
219.458759	9572.718847	26.602368
219.350556	9595.228782	26.607386
219.430688	9608.158090	26.612404
219.709448	9622.997591	26.617421
220.003365	9635.803523	26.622439
220.383311	9636.454787	26.627456
220.491125	9652.995057	26.632474
220.636438	9663.197010	26.637492
221.109670	9675.172077	26.642509
220.709620	9697.884900	26.647527
221.316984	9706.078459	26.652544
221.801720	9724.020132	26.657562
221.766561	9739.270615	26.662580
222.217842	9735.264611	26.667597
222.083895	9756.147493	26.672615
222.388275	9765.420712	26.677632
222.178393	9777.007776	26.682650
222.978054	9791.797858	26.687668
223.078077	9799.217290	26.692685
222.842319	9814.305441	26.697703
223.475872	9828.387393	26.702720
223.650237	9845.054593	26.707738
223.626847	9867.096934	26.712756
224.017603	9868.622396	26.717773
224.045723	9887.722691	26.722791
224.683195	9899.570238	26.727808
224.550572	9919.674809	26.732826
224.599121	9932.445738	26.737844
225.104983	9941.789258	26.742861
225.059286	9966.849845	26.747879
225.440463	9961.964877	26.752896
225.775349	9996.438587	26.757914
225.914445	10011.144911	26.762932
226.600768	10026.556519	26.767949
226.451331	10036.427954	26.772967
226.401918	10046.188226	26.777984
226.776057	10066.746974	26.783002
226.460976	10083.814730	26.788020
226.969243	10088.295528	26.793037
226.887616	10125.933923	26.798055
227.478732	10147.709124	26.803072
227.698534	10164.490239	26.808090
228.244824	10182.777979	26.813108
228.741295	10203.909237	26.818125
228.378385	10220.795498	26.823143
229.005836	10239.240362	26.828160
229.158483	10258.045433	26.833178
229.515058	10269.522512	26.838196
229.692141	10268.542028	26.843213
229.536757	10296.037923	26.848231
230.086581	10308.984257	26.853248
230.101622	10319.584002	26.858266
230.534722	10335.781980	26.863284
230.923518	10355.082726	26.868301
231.109914	10367.081246	26.873319
231.491423	10377.725716	26.878336
231.319992	10408.601816	26.883354
231.605417	10412.152967	26.888372
232.165790	10432.523162	26.893389
231.800150	10453.530510	26.898407
232.056503	10459.269083	26.903424
232.360300	10480.543198	26.908442
232.805377	10501.998661	26.913460
233.146018	10525.320877	26.918477
233.426401	10534.055357	26.923495
233.618127	10541.678541	26.928512
233.624249	10573.180686	26.933530
234.110499	10586.437641	26.938548
234.768100	10603.570517	26.943565
234.571744	10610.640933	26.948583
234.897023	10630.157963	26.953600
235.318150	10637.432182	26.958618
235.139410	10654.749977	26.963636
235.766184	10664.420967	26.968653
235.982411	10673.095709	26.973671
236.471438	10680.927358	26.978688
236.415916	10706.095019	26.983706
236.397710	10709.200388	26.988724
237.134913	10699.321430	26.993741
237.276772	10707.397709	26.998759
237.892335	10709.443855	27.003776
237.832647	10711.371364	27.008794
238.016696	10729.405062	27.013812
238.385934	10727.890225	27.018829
238.475970	10728.296161	27.023847
238.247428	10732.409399	27.028864
238.527087	10753.339096	27.033882
238.920286	10758.618384	27.038900
239.138132	10778.392775	27.043917
239.100968	10797.909161	27.048935
239.421980	10799.282531	27.053952
239.707639	10808.662482	27.058970
240.403740	10815.527778	27.063988
240.818243	10820.550663	27.069005
240.929860	10839.978065	27.074023
241.227212	10830.414687	27.079040
241.482386	10834.273376	27.084058
241.372387	10849.628992	27.089076
241.550250	10856.108627	27.094093
241.870214	10866.466937	27.099111
241.699969	10884.445928	27.104128
242.281116	10894.339989	27.109146
242.285756	10908.389804	27.114164
242.559171	10930.173495	27.119181
242.955365	10945.709820	27.124199
242.867096	10965.079522	27.129216
243.680045	10974.709234	27.134234
243.616357	10997.470344	27.139252
244.019730	10999.671165	27.144269
244.159512	11020.757325	27.149287
244.153587	11038.501349	27.154304
244.304960	11049.414368	27.159322
244.547297	11073.962985	27.164340
245.326399	11093.024595	27.169357
245.616459	11109.301695	27.174375
245.341318	11108.885538	27.179392
245.700415	11128.925145	27.184410
245.270707	11157.058582	27.189428
246.203792	11163.239312	27.194445
246.507021	11181.731506	27.199463
246.930780	11202.314987	27.204480
247.066973	11205.447793	27.209498
246.902775	11236.419662	27.214516
247.066994	11247.577519	27.219533
247.282395	11276.004631	27.224551
247.900250	11295.584897	27.229568
248.112450	11314.086253	27.234586
248.172226	11324.640613	27.239604
248.998617	11342.275940	27.244621
249.195986	11356.161257	27.249639
249.593332	11373.677293	27.254656
249.497139	11382.881759	27.259674
249.783754	11389.617203	27.264692
250.000034	11406.868958	27.269709
250.134785	11415.885320	27.274727
250.206321	11429.556611	27.279744
250.693492	11446.438013	27.284762
250.371433	11460.446949	27.289780
250.875143	11484.289109	27.294797
251.298410	11497.020131	27.299815
251.427907	11509.073493	27.304832
251.918250	11526.082376	27.309850
252.017588	11555.509790	27.314868
252.175631	11562.487561	27.319885
252.496127	11586.858481	27.324903
252.710684	11596.875978	27.329920
252.898400	11611.850605	27.334938
252.679264	11639.849051	27.339956
253.136385	11656.711472	27.344973
253.331883	11672.210487	27.349991
253.239115	11698.387679	27.355008
254.074612	11713.360886	27.360026
254.404786	11739.083888	27.365044
254.830896	11758.608936	27.370061
255.066374	11788.656769	27.375079
255.362957	11795.084238	27.380096
255.847192	11807.824301	27.385114
256.067183	11836.710210	27.390132
256.487986	11850.738250	27.395149
256.708527	11859.088710	27.400167
256.869412	11866.695443	27.405184
257.305477	11874.843911	27.410202
257.233859	11882.519194	27.415220
257.680953	11905.977698	27.420237
257.942427	11910.193785	27.425255
258.138657	11925.824977	27.430272
258.506655	11945.980149	27.435290
258.350964	11965.275489	27.440308
258.816033	11982.441021	27.445325
258.898355	11998.250420	27.450343
259.219739	12012.680918	27.455360
259.576450	12031.469446	27.460378
259.597006	12057.121125	27.465396
260.208086	12063.657379	27.470413
260.483350	12080.237373	27.475431
260.746713	12095.144930	27.480448
261.024270	12109.484317	27.485466
261.167333	12129.324736	27.490484
261.194800	12153.126187	27.495501
261.747771	12159.046591	27.500519
261.591747	12181.304116	27.505536
261.870157	12202.975502	27.510554
262.166635	12225.595450	27.515572
262.431007	12234.054442	27.520589
262.941503	12261.235249	27.525607
262.995057	12268.910847	27.530624
263.449652	12288.425152	27.535642
263.554454	12304.663801	27.540660
264.023815	12328.902191	27.545677
264.454398	12326.920903	27.550695
264.777104	12333.212008	27.555712
264.986575	12355.893048	27.560730
265.075150	12359.771600	27.565748
265.268112	12377.910333	27.570765
265.540586	12397.502804	27.575783
265.497634	12411.001762	27.580800
266.159075	12425.023467	27.585818
266.007259	12435.971446	27.590836
266.433927	12449.784226	27.595853
266.765751	12466.899919	27.600871
266.648663	12490.502972	27.605888
266.993036	12499.690630	27.610906
267.559679	12518.185962	27.615924
267.580900	12535.444511	27.620941
267.990091	12554.807399	27.625959
268.244392	12584.700517	27.630976
268.763623	12592.524222	27.635994
268.637493	12617.507951	27.641012
268.809748	12639.934022	27.646029
269.663639	12641.969619	27.651047
269.956923	12652.215735	27.656064
270.415029	12668.911866	27.661082
270.665999	12681.691224	27.666100
270.691228	12690.414296	27.671117
271.341512	12700.442577	27.676135
271.426700	12714.387361	27.681152
271.630270	12730.016047	27.686170
271.632280	12741.896288	27.691188
271.924085	12759.316618	27.696205
272.337564	12778.363469	27.701223
272.532444	12798.539299	27.706240
273.194699	12808.919561	27.711258
273.340410	12826.001171	27.716276
273.591073	12845.412918	27.721293
273.791501	12853.490258	27.726311
273.752325	12880.971524	27.731328
274.169089	12886.427672	27.736346
274.447621	12909.187872	27.741364
274.607966	12921.343113	27.746381
274.943754	12936.180329	27.751399
274.902070	12953.911823	27.756416
275.648882	12965.520432	27.761434
275.740227	12982.457390	27.766452
276.268432	13008.752164	27.771469
276.561012	13021.320323	27.776487
276.633974	13051.330830	27.781504
276.738429	13058.258599	27.786522
277.152412	13083.954684	27.791540
277.254980	13109.754660	27.796557
277.506781	13137.307296	27.801575
277.606950	13150.730179	27.806592
278.045713	13164.750673	27.811610
278.033760	13186.703820	27.816628
277.964304	13204.635245	27.821645
278.405746	13221.990144	27.826663
278.511552	13252.738886	27.831680
279.269125	13272.709657	27.836698
279.636383	13296.541883	27.841716
279.975688	13315.925244	27.846733
280.502937	13337.536352	27.851751
280.659307	13352.031226	27.856768
280.802602	13361.703090	27.861786
280.807106	13388.280746	27.866804
281.375570	13411.501953	27.871821
281.894604	13427.094853	27.876839
281.823477	13454.945915	27.881856
282.135851	13476.958680	27.886874
282.633106	13491.064811	27.891892
282.609718	13516.793352	27.896909
282.985159	13528.242849	27.901927
283.322308	13545.979692	27.906944
283.651072	13560.408324	27.911962
283.970637	13582.617676	27.916980
283.971901	13610.411335	27.921997
284.172813	13621.476534	27.927015
284.288740	13643.057005	27.932032
284.679824	13670.229552	27.937050
285.185828	13698.194430	27.942068
285.329864	13732.617126	27.947085
285.795707	13747.529360	27.952103
286.139747	13773.312636	27.957120
286.398959	13789.664637	27.962138
287.119870	13807.360991	27.967156
287.391559	13820.825218	27.972173
288.021310	13832.530692	27.977191
287.891886	13858.786608	27.982208
288.344205	13872.030117	27.987226
288.789177	13884.091074	27.992244
289.132245	13887.955237	27.997261
289.544373	13905.439375	28.002279
289.654630	13914.678095	28.007296
289.809339	13918.157240	28.012314
289.987771	13942.356603	28.017332
290.297867	13956.764380	28.022349
290.569996	13969.571559	28.027367
290.751324	13991.848311	28.032384
291.128418	14009.452197	28.037402
291.687796	14030.496620	28.042420
291.338889	14039.457799	28.047437
291.793156	14057.159353	28.052455
291.788406	14071.893822	28.057472
292.081259	14100.116481	28.062490
292.372987	14125.118536	28.067508
292.379527	14147.383322	28.072525
293.159128	14169.826631	28.077543
293.038499	14202.457987	28.082560
293.446462	14222.576133	28.087578
293.991082	14240.127509	28.092596
294.014288	14260.546852	28.097613
294.490305	14285.961030	28.102631
294.496586	14298.764508	28.107648
294.630157	14313.336943	28.112666
294.768336	14349.261990	28.117684
295.002426	14383.995935	28.122701
295.588477	14411.463160	28.127719
295.983073	14437.064638	28.132736
295.959375	14462.029444	28.137754
296.500515	14483.639178	28.142772
296.805598	14511.827190	28.147789
297.430222	14536.297445	28.152807
297.835069	14566.085728	28.157824
298.165538	14582.917074	28.162842
298.846386	14598.588121	28.167860
298.576832	14625.260997	28.172877
299.187882	14634.587725	28.177895
299.407981	14652.344116	28.182912
299.148471	14674.884497	28.187930
299.792898	14689.079285	28.192948
299.513258	14726.103075	28.197965
300.123762	14752.278710	28.202983
300.470171	14784.387851	28.208000
300.728685	14794.451327	28.213018
301.130674	14821.195238	28.218036
301.065872	14866.553362	28.223053
301.498102	14877.045216	28.228071
301.756786	14920.117560	28.233088
302.010418	14948.668834	28.238106
302.773430	14970.467770	28.243124
303.082547	14996.262314	28.248141
303.688278	15017.377271	28.253159
303.989567	15042.717226	28.258176
304.340791	15053.996371	28.263194
305.106298	15073.266019	28.268212
305.088233	15097.088560	28.273229
305.346576	15104.960856	28.278247
305.523871	15123.526134	28.283264
305.560773	15147.838719	28.288282
306.413696	15152.941293	28.293300
306.413619	15177.843862	28.298317
306.565614	15192.857814	28.303335
306.936192	15213.015327	28.308352
307.268004	15235.239496	28.313370
307.521072	15254.808028	28.318388
307.766632	15284.520354	28.323405
308.241284	15298.530600	28.328423
308.684328	15313.617066	28.333440
308.963565	15339.124874	28.338458
309.308190	15354.263672	28.343476
309.741325	15367.122434	28.348493
310.320786	15382.502527	28.353511
310.758262	15391.252271	28.358528
310.568167	15419.467824	28.363546
311.468351	15425.701350	28.368564
311.154904	15436.295597	28.373581
311.601067	15438.048709	28.378599
312.091650	15456.278389	28.383616
312.201667	15457.287668	28.388634
312.912677	15466.797175	28.393652
313.163857	15495.404966	28.398669
313.171118	15499.333688	28.403687
313.380456	15508.791892	28.408704
313.239575	15525.268163	28.413722
313.733005	15539.193959	28.418740
313.393442	15583.190040	28.423757
313.940565	15584.757915	28.428775
314.380120	15612.554533	28.433792
314.378542	15645.893091	28.438810
314.542642	15668.453032	28.443828
314.720156	15703.956539	28.448845
315.040471	15731.311420	28.453863
315.287876	15763.180649	28.458880
315.719605	15805.304902	28.463898
316.140128	15829.912888	28.468916
316.556913	15867.580688	28.473933
316.840893	15893.319631	28.478951
317.237032	15915.453639	28.483968
317.526480	15948.927945	28.488986
318.126080	15978.204435	28.494004
317.943994	16010.285908	28.499021
318.013926	16049.860168	28.504039
318.834961	16083.688774	28.509056
319.080206	16116.379446	28.514074
319.280544	16137.023906	28.519092
319.591858	16186.659397	28.524109
320.201747	16210.218251	28.529127
321.014289	16238.455122	28.534144
320.809702	16265.196650	28.539162
321.459821	16299.271643	28.544180
321.752635	16319.037928	28.549197
322.051392	16337.192051	28.554215
322.620318	16358.763000	28.559232
322.998255	16380.164436	28.564250
323.728424	16390.308014	28.569268
324.121348	16414.880984	28.574285
323.889375	16433.824054	28.579303
324.562673	16443.893078	28.584320
324.871688	16462.532869	28.589338
325.330319	16481.199425	28.594356
325.311086	16496.933402	28.599373
325.470796	16527.401004	28.604391
325.912835	16544.103151	28.609408
326.236413	16570.254394	28.614426
326.813955	16584.959787	28.619444
326.915129	16620.334667	28.624461
326.996128	16648.079870	28.629479
327.676313	16650.202590	28.634496
327.377254	16684.529490	28.639514
327.913999	16703.143910	28.644532
328.210416	16723.635076	28.649549
328.330663	16742.434410	28.654567
328.913686	16758.707861	28.659584
329.104260	16786.777161	28.664602
329.792220	16800.549491	28.669620
329.691923	16820.816824	28.674637
329.813557	16865.857730	28.679655
330.701683	16864.688736	28.684672
330.763211	16891.134034	28.689690
331.001675	16921.812681	28.694708
331.583430	16942.490737	28.699725
331.830971	16974.204582	28.704743
332.345635	16988.106265	28.709760
332.268314	17008.059769	28.714778
332.886873	17034.593896	28.719796
333.301003	17055.422036	28.724813
333.642858	17081.019888	28.729831
334.287848	17097.090922	28.734848
334.009599	17120.813172	28.739866
334.794014	17148.671969	28.744884
334.609032	17174.021271	28.749901
335.130473	17196.153883	28.754919
335.532373	17217.039895	28.759936
335.497608	17258.770038	28.764954
335.980450	17281.475823	28.769972
336.542516	17314.768116	28.774989
336.789017	17327.126299	28.780007
337.224188	17353.062077	28.785024
337.450003	17383.209820	28.790042
337.735024	17411.141979	28.795060
338.006796	17429.575889	28.800077
338.465604	17448.046549	28.805095
338.880315	17475.416839	28.810112
339.556197	17503.870322	28.815130
340.169215	17515.440355	28.820148
340.223588	17545.342515	28.825165
340.641268	17564.525357	28.830183
341.093759	17592.581938	28.835200
341.356512	17609.904541	28.840218
341.252559	17632.000825	28.845236
341.510844	17654.861050	28.850253
341.899238	17675.292365	28.855271
342.440271	17699.826849	28.860288
342.439859	17743.728755	28.865306
343.321848	17758.151722	28.870324
343.741002	17772.651605	28.875341
343.805504	17804.463245	28.880359
344.123525	17813.226225	28.885376
344.663461	17843.133865	28.890394
345.136877	17869.084492	28.895412
345.473985	17874.812612	28.900429
345.400367	17911.328317	28.905447
346.053575	17924.896173	28.910464
346.105940	17956.613208	28.915482
346.550087	17981.321845	28.920500
347.060413	17998.188504	28.925517
346.998047	18018.886589	28.930535
347.344417	18031.539262	28.935552
347.452777	18059.752314	28.940570
347.619376	18085.991566	28.945588
347.894320	18104.581679	28.950605
348.522653	18139.836454	28.955623
348.792883	18163.107337	28.960640
349.006199	18196.205129	28.965658
349.483393	18237.406313	28.970676
349.860439	18252.886203	28.975693
349.767047	18281.156215	28.980711
350.554699	18315.350553	28.985728
351.035515	18347.376495	28.990746
351.233018	18381.022486	28.995764
351.593201	18410.968919	29.000781
351.641314	18441.739960	29.005799
352.502092	18473.606007	29.010816
352.452231	18516.025015	29.015834
352.738231	18548.691095	29.020852
353.440358	18568.303491	29.025869
353.676585	18602.440656	29.030887
353.918529	18629.148361	29.035904
354.610530	18654.254810	29.040922
354.952594	18683.322731	29.045940
355.453676	18709.317206	29.050957
355.224705	18747.045893	29.055975
355.952637	18780.576726	29.060992
356.151688	18815.588432	29.066010
356.426249	18843.414984	29.071028
356.942737	18883.050119	29.076045
357.277341	18916.036406	29.081063
357.809972	18938.612270	29.086080
358.112489	18980.779922	29.091098
358.408854	19010.086456	29.096116
359.021687	19036.863327	29.101133
359.215629	19073.461959	29.106151
359.862020	19095.000564	29.111168
360.259751	19118.627387	29.116186
360.637836	19153.534546	29.121204
360.858501	19177.993667	29.126221
360.917386	19206.007212	29.131239
361.551429	19232.711744	29.136256
361.720318	19262.906060	29.141274
362.117317	19296.278122	29.146292
363.004861	19308.651495	29.151309
363.197567	19344.669023	29.156327
363.834961	19360.150267	29.161344
364.515199	19389.603451	29.166362
364.481310	19410.283486	29.171380
365.148748	19424.623689	29.176397
364.938834	19447.015433	29.181415
365.428074	19467.594468	29.186432
365.846044	19483.999464	29.191450
365.876565	19509.389091	29.196468
366.430753	19520.310887	29.201485
366.371000	19561.691296	29.206503
367.000463	19578.120571	29.211520
367.150738	19598.320677	29.216538
367.219438	19631.189413	29.221556
367.791315	19657.225376	29.226573
367.750880	19701.381315	29.231591
368.453103	19725.905127	29.236608
368.450901	19760.201331	29.241626
368.403674	19793.694456	29.246644
369.043778	19835.924810	29.251661
369.325196	19878.056901	29.256679
369.753458	19912.169085	29.261696
369.972488	19951.457038	29.266714
370.482506	20003.446765	29.271732
371.167449	20034.453366	29.276749
371.747830	20072.284655	29.281767
372.053805	20104.337340	29.286784
372.922474	20128.157616	29.291802
373.356491	20169.592858	29.296820
373.637100	20179.686939	29.301837
373.913322	20214.916676	29.306855
374.626821	20234.733725	29.311872
375.224972	20259.223771	29.316890
375.786077	20284.380483	29.321908
375.851807	20313.129273	29.326925
376.201929	20330.694561	29.331943
376.842200	20338.834311	29.336960
377.332592	20361.436291	29.341978
377.483862	20387.544822	29.346996
377.763811	20417.141691	29.352013
377.767309	20436.640959	29.357031
378.047753	20461.175644	29.362048
378.339321	20490.426652	29.367066
378.486803	20528.439849	29.372084
379.188972	20553.135076	29.377101
379.064848	20581.102667	29.382119
379.509430	20623.203280	29.387136
380.407174	20665.914592	29.392154
380.152706	20703.386643	29.397172
381.008808	20730.307611	29.402189
381.745937	20747.665615	29.407207
382.337254	20775.781018	29.412224
383.012338	20800.867635	29.417242
383.246376	20830.398569	29.422260
383.482560	20846.817423	29.427277
383.882768	20878.515277	29.432295
383.695740	20906.865976	29.437312
384.170431	20930.493119	29.442330
384.441579	20959.887651	29.447348
385.381959	20987.361093	29.452365
385.951579	21008.313675	29.457383
386.284301	21035.027955	29.462400
386.555010	21049.685280	29.467418
386.777766	21073.515804	29.472436
387.191985	21086.465722	29.477453
387.525732	21110.398325	29.482471
387.662077	21138.183643	29.487488
387.948064	21148.805549	29.492506
388.129415	21194.077812	29.497524
388.463157	21220.487458	29.502541
388.255013	21256.783915	29.507559
388.947301	21281.740188	29.512576
389.528125	21328.888170	29.517594
389.700060	21363.774426	29.522612
390.094519	21401.748804	29.527629
390.288178	21435.773306	29.532647
390.636300	21482.317741	29.537664
391.019492	21515.178110	29.542682
391.496078	21560.015319	29.547700
391.934393	21598.736109	29.552717
392.511870	21637.415131	29.557735
392.755722	21676.761721	29.562752
393.295363	21705.586397	29.567770
393.413502	21757.267900	29.572788
394.052664	21798.656242	29.577805
394.396913	21838.141605	29.582823
394.851140	21874.344181	29.587840
395.103113	21910.638923	29.592858
395.557336	21956.712621	29.597876
396.071883	21997.072259	29.602893
396.297886	22039.432801	29.607911
396.795721	22075.530441	29.612928
397.321520	22113.025644	29.617946
397.607925	22163.733389	29.622964
398.145785	22186.041774	29.627981
399.012084	22220.505821	29.632999
399.220984	22254.884871	29.638016
399.968443	22290.039050	29.643034
400.377691	22314.901864	29.648052
401.262804	22321.498907	29.653069
401.663613	22352.990125	29.658087
402.178194	22383.473243	29.663104
402.750836	22401.810733	29.668122
402.824588	22426.446785	29.673140
403.227337	22450.691779	29.678157
403.505918	22470.123738	29.683175
403.556670	22495.086486	29.688192
403.936559	22533.629060	29.693210
404.250782	22561.320803	29.698228
404.429406	22585.489870	29.703245
405.023367	22623.324345	29.708263
405.529157	22665.298579	29.713280
406.307361	22687.830089	29.718298
406.352388	22720.854750	29.723316
406.741064	22735.616146	29.728333
407.472473	22766.181238	29.733351
407.860811	22798.103805	29.738368
408.096948	22832.542781	29.743386
408.078862	22848.996355	29.748404
408.210156	22878.923197	29.753421
408.536443	22917.943894	29.758439
408.814708	22955.133182	29.763456
409.143212	22984.634191	29.768474
409.160604	23034.254944	29.773492
409.490466	23078.959945	29.778509
410.141860	23118.585453	29.783527
410.330226	23166.845092	29.788544
411.097368	23208.649161	29.793562
411.494956	23257.400322	29.798580
412.105343	23298.757006	29.803597
412.446326	23337.720469	29.808615
412.484247	23385.832243	29.813632
413.300377	23414.465542	29.818650
413.340730	23468.754874	29.823668
413.631709	23505.193559	29.828685
414.500122	23545.863886	29.833703
414.897191	23595.418808	29.838720
415.534868	23642.923813	29.843738
415.559516	23685.869845	29.848756
416.155916	23726.256295	29.853773
416.451283	23773.318409	29.858791
416.619903	23824.387355	29.863808
417.380446	23862.069065	29.868826
417.618865	23922.671670	29.873844
418.011303	23961.996318	29.878861
419.102050	23997.533618	29.883879
419.043691	24049.112065	29.888896
419.584662	24090.274703	29.893914
420.046045	24141.671393	29.898932
420.814694	24173.885087	29.903949
421.172392	24212.839365	29.908967
421.193373	24254.564199	29.913984
422.034972	24292.784626	29.919002
422.115277	24345.120985	29.924020
422.372194	24386.343822	29.929037
423.159279	24419.624009	29.934055
423.517652	24468.047980	29.939072
424.315411	24495.030366	29.944090
424.464998	24537.961935	29.949108
424.863301	24580.149767	29.954125
426.294946	24596.210330	29.959143
426.849026	24623.724875	29.964160
427.607212	24650.274278	29.969178
428.096532	24661.855544	29.974196
428.238674	24684.013868	29.979213
428.595148	24719.305835	29.984231
428.605322	24743.498714	29.989248
429.095867	24774.191126	29.994266
429.361984	24807.047820	29.999284
429.881600	24844.257423	30.004301
429.971962	24870.267640	30.009319
429.703950	24909.631310	30.014336
430.446228	24952.294689	30.019354
430.858252	24986.669338	30.024372
431.037428	25028.560047	30.029389
431.743557	25066.197347	30.034407
432.194477	25103.921872	30.039424
432.750794	25136.718831	30.044442
432.775538	25174.598859	30.049460
433.117475	25210.358214	30.054477
433.713507	25244.030568	30.059495
433.918071	25291.856056	30.064512
434.930038	25325.494616	30.069530
435.152886	25372.751819	30.074548
435.396629	25407.465349	30.079565
435.993752	25450.600635	30.084583
436.286353	25492.681671	30.089600
436.928055	25532.406113	30.094618
437.019138	25576.448732	30.099636
437.198198	25617.297982	30.104653
437.839891	25657.660049	30.109671
438.198711	25714.723370	30.114688
439.007667	25750.779788	30.119706
439.418091	25798.722095	30.124724
439.578929	25836.354331	30.129741
440.523678	25875.097027	30.134759
440.817529	25920.850880	30.139776
441.251534	25957.739535	30.144794
441.506397	26014.470702	30.149812
441.462525	26054.575871	30.154829
442.698985	26103.348607	30.159847
442.944940	26158.166553	30.164864
443.328768	26189.079569	30.169882
444.068705	26236.030046	30.174900
444.210656	26277.623487	30.179917
445.032312	26313.612185	30.184935
445.676793	26365.228704	30.189952
446.268899	26387.675366	30.194970
446.687539	26423.206980	30.199988
447.112546	26455.877086	30.205005
447.854485	26480.712312	30.210023
447.918636	26525.493705	30.215040
448.596531	26557.955137	30.220058
449.002605	26585.405248	30.225076
449.366965	26618.709305	30.230093
449.509048	26652.096898	30.235111
450.014883	26698.599143	30.240128
450.546809	26738.874271	30.245146
451.726519	26763.381787	30.250164
452.608001	26778.484403	30.255181
453.428608	26794.561042	30.260199
453.346915	26816.113518	30.265216
454.198976	26835.109638	30.270234
454.769670	26845.655341	30.275252
454.937217	26886.723153	30.280269
455.174532	26891.151631	30.285287
455.558524	26915.706572	30.290304
455.746847	26942.564860	30.295322
456.213205	26966.897980	30.300340
456.173313	26988.635473	30.305357
456.712160	27012.296111	30.310375
457.159912	27043.856864	30.315392
457.520385	27060.886311	30.320410
457.786167	27106.063422	30.325428
458.051467	27143.336994	30.330445
458.371095	27164.901636	30.335463
458.542253	27206.057137	30.340480
458.842727	27254.794973	30.345498
459.335665	27298.078664	30.350516
459.751205	27365.510198	30.355533
460.299774	27396.048691	30.360551
460.598204	27454.675165	30.365568
460.965910	27503.313223	30.370586
461.458256	27548.124571	30.375604
461.631503	27604.006095	30.380621
461.864145	27648.838609	30.385639
462.344298	27712.128089	30.390656
462.735380	27764.828673	30.395674
463.627725	27820.944637	30.400692
464.015434	27880.612622	30.405709
464.652577	27931.163008	30.410727
464.989329	27986.016030	30.415744
465.337062	28041.502533	30.420762
466.336823	28090.933568	30.425780
466.787865	28141.000545	30.430797
467.333913	28186.509489	30.435815
467.908808	28241.971522	30.440832
468.550833	28283.923025	30.445850
468.862975	28326.740311	30.450868
468.924325	28374.553629	30.455885
470.019117	28416.348256	30.460903
470.379869	28475.567310	30.465920
470.574771	28517.165167	30.470938
471.685081	28553.355569	30.475956
472.028378	28608.190742	30.480973
472.601833	28638.114611	30.485991
472.956123	28687.399730	30.491008
473.245798	28733.436413	30.496026
474.077820	28773.127499	30.501044
474.333301	28819.168295	30.506061
474.750247	28858.645206	30.511079
475.091784	28907.526448	30.516096
475.533383	28955.298237	30.521114
476.274358	28994.799504	30.526132
476.560430	29045.691372	30.531149
476.727458	29095.614275	30.536167
477.226492	29146.425257	30.541184
478.122645	29195.696515	30.546202
478.637303	29246.899298	30.551220
478.430316	29296.668072	30.556237
478.924334	29339.670225	30.561255
479.262943	29398.557342	30.566272
479.673469	29453.340526	30.571290
480.570343	29501.547268	30.576308
480.928007	29553.158973	30.581325
481.753602	29584.779532	30.586343
482.256990	29625.941824	30.591360
482.780210	29660.497830	30.596378
483.323251	29702.035378	30.601396
483.805370	29748.291698	30.606413
484.392285	29783.810186	30.611431
484.566585	29829.518480	30.616448
485.096072	29871.247734	30.621466
485.391675	29914.517829	30.626484
485.846570	29969.959166	30.631501
486.255944	30002.464771	30.636519
486.916649	30063.138998	30.641536
487.605129	30098.389836	30.646554
488.132269	30146.780310	30.651572
488.162734	30198.846479	30.656589
489.157263	30236.127609	30.661607
489.721249	30284.834129	30.666624
489.951579	30332.640453	30.671642
490.845339	30370.870944	30.676660
491.323843	30412.163688	30.681677
492.185485	30440.470523	30.686695
493.205372	30483.176011	30.691712
493.523064	30521.383566	30.696730
494.300002	30532.466996	30.701748
494.721596	30565.006448	30.706765
495.347595	30587.650551	30.711783
495.417825	30614.636948	30.716800
495.974731	30651.906785	30.721818
496.404445	30686.339591	30.726836
496.483833	30720.424803	30.731853
496.745326	30758.047691	30.736871
496.904113	30797.679164	30.741888
497.521585	30852.999881	30.746906
497.815060	30893.989189	30.751924
497.863704	30958.617719	30.756941
498.492133	31013.385606	30.761959
498.925137	31066.290351	30.766976
499.277800	31124.330356	30.771994
499.958486	31188.149873	30.777012
500.141943	31253.952771	30.782029
500.890468	31304.447023	30.787047
501.451957	31360.104622	30.792064
501.540557	31419.103450	30.797082
502.423221	31465.636536	30.802100
503.178497	31525.664364	30.807117
503.930207	31574.445688	30.812135
504.293535	31626.220637	30.817152
504.617311	31691.038335	30.822170
505.283567	31732.964904	30.827188
505.936125	31792.567171	30.832205
506.468740	31843.269272	30.837223
507.251380	31886.553682	30.842240
507.225310	31936.687799	30.847258
508.074744	31979.955511	30.852276
508.259129	32032.650777	30.857293
508.786338	32070.584256	30.862311
509.203190	32118.403894	30.867328
509.768844	32175.214202	30.872346
510.349257	32212.133923	30.877364
510.900053	32260.615131	30.882381
511.352479	32304.520669	30.887399
511.634845	32351.905306	30.892416
511.881667	32411.191418	30.897434
512.550943	32450.452382	30.902452
513.138034	32517.376618	30.907469
513.609356	32568.450091	30.912487
514.367412	32621.285990	30.917504
514.681564	32671.112794	30.922522
515.512005	32717.938313	30.927540
516.007925	32773.094122	30.932557
516.464293	32825.865239	30.937575
516.955352	32873.583822	30.942592
517.140347	32932.782347	30.947610
517.985179	32978.189252	30.952628
518.283211	33037.647571	30.957645
518.864440	33100.539843	30.962663
519.613520	33146.046003	30.967680
520.431763	33187.340467	30.972698
520.999104	33244.759479	30.977716
521.666021	33290.753588	30.982733
522.116447	33340.220221	30.987751
522.677396	33370.313943	30.992768
523.135980	33432.722595	30.997786
523.640114	33474.245928	31.002804
523.817097	33520.302947	31.007821
524.403305	33573.840774	31.012839
525.107433	33626.420501	31.017856
525.110411	33676.971408	31.022874
525.708816	33732.399405	31.027892
526.204268	33793.265033	31.032909
526.797520	33853.424866	31.037927
527.580710	33906.558798	31.042944
527.851566	33971.442725	31.047962
528.629098	34007.860577	31.052980
529.553653	34060.940961	31.057997
530.186854	34103.789957	31.063015
531.145811	34141.170746	31.068032
531.303682	34194.605397	31.073050
531.720903	34240.134315	31.078068
532.056002	34289.765597	31.083085
532.599063	34332.221254	31.088103
533.331523	34380.203664	31.093120
533.507254	34440.521976	31.098138
534.229685	34479.642142	31.103156
534.339002	34532.603228	31.108173
534.744259	34590.721109	31.113191
535.632611	34635.781968	31.118208
536.156838	34688.284936	31.123226
536.695597	34738.520419	31.128244
537.091829	34789.961082	31.133261
537.491981	34836.698749	31.138279
537.848141	34880.363175	31.143296
538.267507	34941.189944	31.148314
539.424626	34979.562602	31.153332
540.296923	35022.462591	31.158349
540.802989	35071.657515	31.163367
541.504963	35109.748260	31.168384
541.577143	35151.106532	31.173402
542.149500	35194.904454	31.178420
542.487161	35248.102595	31.183437
542.749013	35295.210399	31.188455
543.806354	35350.293230	31.193472
543.845488	35406.547367	31.198490
544.704417	35448.766382	31.203508
545.807329	35497.772915	31.208525
545.872766	35550.586565	31.213543
546.345097	35596.006358	31.218560
546.752442	35653.492270	31.223578
547.264622	35697.167089	31.228596
547.780173	35765.361250	31.233613
548.139536	35818.411130	31.238631
548.787675	35875.801124	31.243648
549.064867	35941.036957	31.248666
549.755231	35993.703601	31.253684
550.373536	36054.343502	31.258701
550.994935	36119.556741	31.263719
551.601383	36174.100816	31.268736
552.351788	36225.306605	31.273754
552.843186	36288.162155	31.278772
553.309036	36345.910718	31.283789
553.676908	36403.375532	31.288807
554.353009	36452.388199	31.293824
554.693378	36522.522594	31.298842
555.376612	36576.164966	31.303860
556.239570	36636.471605	31.308877
556.437792	36709.677012	31.313895
557.204083	36759.693131	31.318912
557.693905	36820.646362	31.323930
558.151591	36887.708087	31.328948
558.564707	36958.731397	31.333965
558.816362	37015.791118	31.338983
559.500489	37079.842411	31.344000
560.027714	37153.266955	31.349018
560.497684	37219.629584	31.354036
561.147713	37272.404415	31.359053
561.643260	37350.014618	31.364071
562.478390	37418.604483	31.369088
562.956622	37490.980344	31.374106
563.188554	37562.508058	31.379124
564.414155	37615.975920	31.384141
564.813947	37689.938676	31.389159
565.606399	37742.369070	31.394176
566.100149	37814.707582	31.399194
566.525097	37860.440617	31.404212
567.530460	37912.492329	31.409229
567.801425	37956.372259	31.414247
568.567080	38009.312306	31.419264
569.385704	38075.206514	31.424282
569.716060	38112.436134	31.429300
570.276710	38168.616439	31.434317
570.872914	38222.162809	31.439335
571.333469	38269.524803	31.444352
572.033227	38330.369637	31.449370
572.158182	38380.686646	31.454388
573.079935	38440.974611	31.459405
573.414607	38492.050097	31.464423
574.296584	38549.656365	31.469440
574.732029	38600.515876	31.474458
575.346955	38657.827607	31.479476
575.852454	38722.303045	31.484493
576.265127	38786.686288	31.489511
576.507348	38843.901897	31.494528
576.625148	38909.389032	31.499546
577.249080	38984.551667	31.504564
578.375852	39036.734152	31.509581
579.128796	39112.737762	31.514599
579.654249	39177.867719	31.519616
580.253085	39236.139535	31.524634
580.824295	39300.469517	31.529652
581.850081	39363.729194	31.534669
582.314578	39431.725535	31.539687
582.952810	39492.674217	31.544704
583.456740	39552.785104	31.549722
583.828172	39614.878953	31.554740
584.589278	39671.775026	31.559757
585.138354	39743.745534	31.564775
585.831902	39792.514384	31.569792
586.409832	39851.025018	31.574810
586.995305	39912.925022	31.579828
587.830209	39963.601998	31.584845
588.367428	40022.692126	31.589863
589.056786	40080.924035	31.594880
589.473049	40139.939216	31.599898
590.083040	40207.311514	31.604916
590.689052	40268.369026	31.609933
591.118650	40333.734707	31.614951
591.927944	40389.919029	31.619968
592.565592	40456.150915	31.624986
593.300161	40506.418125	31.630004
594.186843	40559.581820	31.635021
594.356863	40613.891152	31.640039
595.081289	40665.961360	31.645056
595.875022	40721.067437	31.650074
596.081468	40790.570579	31.655092
597.076510	40831.458288	31.660109
597.653356	40892.308202	31.665127
598.274789	40946.111448	31.670144
598.896674	40996.145722	31.675162
599.293139	41035.202124	31.680180
599.889112	41083.758381	31.685197
600.510709	41140.416627	31.690215
601.009068	41177.593079	31.695232
601.590769	41230.498329	31.700250
601.808321	41287.514732	31.705268
602.387583	41334.860038	31.710285
602.825251	41397.323572	31.715303
603.375684	41456.252535	31.720320
604.225829	41510.551026	31.725338
604.213084	41581.871203	31.730356
605.075482	41633.666899	31.735373
605.714985	41699.663582	31.740391
606.534679	41758.140663	31.745408
607.132144	41817.454493	31.750426
607.819628	41882.390741	31.755444
608.376338	41935.548171	31.760461
609.227733	42001.587974	31.765479
610.429481	42044.338199	31.770496
610.853560	42095.328211	31.775514
611.181507	42153.052223	31.780532
612.361748	42195.689544	31.785549
612.906541	42265.081686	31.790567
613.330541	42311.883487	31.795584
613.998708	42361.065870	31.800602
614.367683	42416.532073	31.805620
615.230231	42468.207245	31.810637
615.557098	42526.967292	31.815655
616.056732	42590.090849	31.820672
616.656002	42649.211691	31.825690
616.977627	42712.215786	31.830708
617.946820	42765.966202	31.835725
618.185488	42837.964423	31.840743
618.845350	42904.710069	31.845760
619.678471	42954.088684	31.850778
620.149156	43029.608912	31.855796
620.443885	43098.183068	31.860813
621.116391	43168.019047	31.865831
621.869752	43232.678611	31.870848
622.494965	43301.935935	31.875866
623.058355	43375.947701	31.880884
623.826926	43434.252497	31.885901
624.230136	43511.996863	31.890919
624.388371	43584.234962	31.895936
625.458547	43654.886536	31.900954
625.977610	43738.036086	31.905972
626.636106	43801.359584	31.910989
627.360678	43870.168030	31.916007
627.809726	43940.231977	31.921024
628.930393	44009.148251	31.926042
629.149095	44086.116994	31.931060
629.769543	44146.596054	31.936077
630.329736	44225.504750	31.941095
630.867049	44306.972703	31.946112
631.817662	44369.280130	31.951130
632.215788	44440.565586	31.956148
632.868563	44503.961958	31.961165
633.954824	44562.705782	31.966183
634.198287	44623.170814	31.971200
634.978666	44685.922902	31.976218
635.115691	44758.210263	31.981236
635.815814	44823.382676	31.986253
636.841598	44894.746715	31.991271
637.226089	44970.661365	31.996288
638.212370	45032.728883	32.001306
638.338053	45108.622247	32.006324
639.170509	45177.737321	32.011341
639.714653	45245.210753	32.016359
640.051422	45327.983642	32.021376
640.947100	45396.433312	32.026394
641.250922	45482.193495	32.031412
642.131959	45546.901280	32.036429
643.059336	45624.782991	32.041447
643.646982	45694.926567	32.046464
644.207822	45768.633421	32.051482
644.836214	45843.749540	32.056500
645.644041	45907.015900	32.061517
646.180762	45986.400069	32.066535
647.011977	46061.181953	32.071552
647.891572	46125.668108	32.076570
648.404085	46210.247063	32.081588
648.775479	46275.802197	32.086605
649.569385	46353.405521	32.091623
650.279969	46441.765302	32.096640
651.348183	46501.524981	32.101658
651.827560	46577.040262	32.106676
652.418245	46648.821485	32.111693
653.315854	46705.835728	32.116711
653.856015	46778.209212	32.121728
654.859084	46853.336255	32.126746
655.108284	46918.149706	32.131764
655.828370	46992.779723	32.136781
656.554344	47070.848215	32.141799
657.306413	47147.063982	32.146816
657.843429	47208.787959	32.151834
658.144953	47290.070698	32.156852
658.881276	47356.805428	32.161869
659.645286	47431.010669	32.166887
659.815180	47504.818602	32.171904
660.726814	47590.078961	32.176922
661.260555	47662.965092	32.181940
662.176129	47741.037917	32.186957
663.020514	47819.504210	32.191975
663.324398	47904.029858	32.196992
663.914818	47971.358094	32.202010
664.368515	48050.651198	32.207028
665.307855	48126.724633	32.212045
666.203233	48203.322870	32.217063
666.691921	48285.826745	32.222080
667.326961	48352.287916	32.227098
667.564837	48436.154520	32.232116
668.593071	48510.388487	32.237133
669.347976	48581.804333	32.242151
669.751558	48654.286135	32.247168
670.656804	48724.631021	32.252186
671.389105	48800.046119	32.257204
671.964636	48870.226352	32.262221
672.603350	48939.809886	32.267239
673.275630	49018.463511	32.272256
673.769613	49094.842360	32.277274
674.616122	49165.889402	32.282292
675.571631	49235.499389	32.287309
676.255562	49303.938008	32.292327
676.962741	49376.077799	32.297344
677.702880	49445.233788	32.302362
678.202601	49523.450098	32.307380
679.059499	49590.540098	32.312397
680.083781	49656.698046	32.317415
680.751098	49731.196541	32.322432
681.518246	49789.118763	32.327450
682.153659	49861.309813	32.332468
682.910476	49926.249094	32.337485
683.777133	49995.282942	32.342503
684.318911	50063.564085	32.347520
685.081320	50110.165578	32.352538
686.061288	50178.670877	32.357556
686.690176	50235.455269	32.362573
687.192404	50303.134576	32.367591
687.550967	50372.872451	32.372608
688.379000	50436.842914	32.377626
688.736083	50515.007386	32.382644
689.561430	50586.148668	32.387661
690.395270	50658.021019	32.392679
690.389924	50742.877618	32.397696
691.152153	50815.140695	32.402714
691.616628	50891.241598	32.407732
691.947679	50988.476550	32.412749
692.886435	51077.495289	32.417767
693.698224	51167.986380	32.422784
694.522796	51243.441303	32.427802
695.086522	51324.880606	32.432820
695.661618	51413.810584	32.437837
696.285816	51503.727298	32.442855
696.629884	51592.382502	32.447872
697.363806	51679.174030	32.452890
698.490572	51776.261317	32.457908
699.229983	51864.640318	32.462925
700.162348	51956.631057	32.467943
700.781009	52056.827352	32.472960
701.236929	52133.591327	32.477978
702.137840	52226.304869	32.482996
702.681169	52307.193244	32.488013
703.999909	52380.415521	32.493031
704.442847	52472.543619	32.498048
705.121256	52545.272005	32.503066
705.615086	52627.649908	32.508084
706.366747	52706.184004	32.513101
707.386589	52779.414456	32.518119
707.935057	52846.373220	32.523136
708.701363	52923.132169	32.528154
709.634882	53002.364520	32.533172
710.257450	53073.235461	32.538189
711.106706	53152.863785	32.543207
711.225217	53226.179569	32.548224
712.031395	53304.350930	32.553242
712.672241	53386.478478	32.558260
712.722481	53471.784088	32.563277
714.061200	53544.559719	32.568295
715.095325	53632.086129	32.573312
716.027788	53708.048663	32.578330
716.182679	53789.286410	32.583348
717.035946	53867.225447	32.588365
717.870573	53949.933869	32.593383
718.802118	54031.645611	32.598400
719.407371	54109.666203	32.603418
720.403832	54202.418847	32.608436
720.863145	54282.811769	32.613453
721.773795	54356.665697	32.618471
722.354879	54435.486951	32.623488
723.199103	54509.273164	32.628506
723.875581	54608.571620	32.633524
724.439853	54686.307656	32.638541
725.309253	54769.554025	32.643559
725.626738	54858.456703	32.648576
726.341188	54941.030933	32.653594
727.111037	55029.903470	32.658612
727.423494	55120.869441	32.663629
728.583262	55208.547575	32.668647
728.906503	55309.137130	32.673664
729.910211	55399.063254	32.678682
730.757070	55485.005892	32.683700
731.107775	55586.018739	32.688717
732.133247	55682.549616	32.693735
732.720719	55775.255406	32.698752
733.325226	55873.056987	32.703770
734.352583	55965.526412	32.708788
734.821987	56059.761333	32.713805
736.031766	56149.030151	32.718823
736.925901	56249.316170	32.723840
737.160534	56330.921850	32.728858
738.107753	56414.450577	32.733876
738.510526	56514.484798	32.738893
739.710348	56609.622753	32.743911
740.476642	56704.631332	32.748928
741.106878	56799.977742	32.753946
742.256647	56890.642411	32.758964
742.743562	56978.792841	32.763981
743.485748	57052.258285	32.768999
744.164783	57150.951350	32.774016
745.262418	57231.647048	32.779034
745.934330	57326.313967	32.784052
746.329868	57410.774773	32.789069
747.092829	57486.792606	32.794087
747.666910	57580.740831	32.799104
748.284941	57663.734111	32.804122
748.920995	57755.274049	32.809140
749.617700	57850.113338	32.814157
750.440297	57930.376003	32.819175
751.106179	58028.043494	32.824192
751.766438	58113.838685	32.829210
752.901214	58208.212286	32.834228
753.483515	58300.259134	32.839245
754.379299	58389.591940	32.844263
755.055618	58485.697412	32.849280
756.137374	58570.818299	32.854298
756.455377	58664.017175	32.859316
757.299867	58760.015211	32.864333
758.259886	58851.587921	32.869351
758.753395	58958.904537	32.874368
759.178504	59051.172714	32.879386
760.621496	59142.281640	32.884404
761.132456	59239.863342	32.889421
762.605802	59319.014951	32.894439
762.972214	59412.459291	32.899456
763.641204	59504.908746	32.904474
764.770243	59588.978545	32.909492
766.078536	59674.706204	32.914509
766.876419	59754.257653	32.919527
767.464981	59844.340959	32.924544
768.051432	59918.464539	32.929562
768.754002	60002.733537	32.934580
769.250209	60107.887210	32.939597
769.918514	60190.299641	32.944615
770.724463	60284.868723	32.949632
771.541087	60380.582736	32.954650
772.231299	60468.771031	32.959668
772.696292	60581.674420	32.964685
773.492896	60676.212232	32.969703
774.167921	60778.155289	32.974720
774.677051	60880.456846	32.979738
775.536939	60977.430028	32.984756
776.165688	61104.993085	32.989773
777.005128	61208.854212	32.994791
777.703708	61312.233116	32.999808
778.390010	61416.293429	33.004826
779.235058	61521.573159	33.009844
780.192897	61631.553059	33.014861
781.025026	61737.878080	33.019879
781.790613	61849.203441	33.024896
782.612584	61944.968773	33.029914
784.079229	62045.791702	33.034932
784.984265	62140.619594	33.039949
786.153751	62222.443292	33.044967
787.169480	62313.424080	33.049984
787.903639	62393.903129	33.055002
789.146339	62469.331212	33.060020
789.444513	62545.730958	33.065037
790.354993	62610.728567	33.070055
791.331591	62697.984894	33.075072
791.473736	62772.749370	33.080090
792.474615	62842.397524	33.085108
792.721171	62923.439583	33.090125
793.335091	63016.110847	33.095143
794.262999	63100.503102	33.100160
794.868428	63193.685006	33.105178
795.510659	63281.196184	33.110196
796.204542	63378.255483	33.115213
796.850346	63473.968165	33.120231
797.388273	63568.037402	33.125248
797.787427	63683.158271	33.130266
798.995708	63789.245457	33.135284
799.399411	63902.431065	33.140301
800.126936	64013.481491	33.145319
800.974990	64112.585360	33.150336
801.884615	64233.426515	33.155354
802.541495	64338.995009	33.160372
803.566346	64459.032886	33.165389
804.407080	64566.174543	33.170407
805.304163	64681.942240	33.175424
806.342537	64793.895178	33.180442
807.123924	64903.792628	33.185460
807.677291	65030.197099	33.190477
808.082543	65136.757506	33.195495
809.096613	65244.756519	33.200512
809.884281	65374.849550	33.205530
810.847833	65493.245570	33.210548
811.456943	65616.849940	33.215565
812.196460	65738.292998	33.220583
813.467550	65860.751330	33.225600
814.002796	65963.331894	33.230618
815.506862	66066.778976	33.235636
816.583765	66180.477299	33.240653
817.540763	66299.608916	33.245671
818.649733	66396.908030	33.250688
819.332187	66499.742806	33.255706
820.313478	66593.851081	33.260724
820.940700	66685.761004	33.265741
821.860047	66791.487552	33.270759
822.759764	66891.096585	33.275776
823.416504	66997.674635	33.280794
824.253640	67102.443137	33.285812
825.139438	67216.983409	33.290829
825.756825	67309.608539	33.295847
826.650853	67412.316579	33.300864
827.415776	67509.019055	33.305882
828.187479	67610.300962	33.310900
829.379267	67721.428408	33.315917
830.606222	67812.070051	33.320935
831.872174	67894.979765	33.325952
832.878250	67984.469700	33.330970
833.781305	68048.220298	33.335988
834.697207	68122.203320	33.341005
835.477071	68201.293837	33.346023
836.399670	68265.149434	33.351040
836.676177	68344.882897	33.356058
837.194604	68427.338953	33.361076
838.013317	68504.497668	33.366093
838.444124	68604.051130	33.371111
839.459247	68679.915764	33.376128
840.046962	68786.066057	33.381146
840.735920	68877.379509	33.386164
841.630808	68970.909724	33.391181
842.257258	69071.584259	33.396199
842.946639	69172.173484	33.401216
843.722573	69287.608964	33.406234
844.596111	69385.067926	33.411252
845.006409	69492.848705	33.416269
845.691683	69609.583041	33.421287
846.568557	69718.093184	33.426304
847.355414	69844.851997	33.431322
848.535314	69952.626553	33.436340
849.539015	70067.575480	33.441357
849.980573	70188.642014	33.446375
850.868957	70295.845670	33.451392
851.715959	70410.701494	33.456410
853.175820	70519.963612	33.461428
854.288386	70633.957111	33.466445
855.051850	70747.368678	33.471463
856.055265	70849.843600	33.476480
856.403750	70970.304234	33.481498
857.631953	71076.169114	33.486516
858.695721	71189.307970	33.491533
859.338274	71294.799654	33.496551
860.468544	71404.327633	33.501568
861.284725	71515.258368	33.506586
862.407511	71612.644470	33.511604
862.826948	71719.671425	33.516621
863.952528	71822.125632	33.521639
865.025161	71936.764869	33.526656
865.715428	72052.299683	33.531674
867.132556	72128.808720	33.536692
867.921030	72227.344184	33.541709
868.845801	72328.493386	33.546727
870.505061	72421.779345	33.551744
870.778743	72524.486480	33.556762
871.709061	72611.077597	33.561780
872.489579	72717.382667	33.566797
873.100908	72819.563676	33.571815
873.797396	72920.796449	33.576832
874.208275	73026.624874	33.581850
875.149795	73127.219397	33.586868
876.826489	73222.060825	33.591885
877.406417	73326.069320	33.596903
878.620960	73428.201695	33.601920
879.110529	73538.576414	33.606938
880.119152	73617.993499	33.611956
880.631501	73717.995773	33.616973
880.970187	73826.203313	33.621991
881.861311	73922.797126	33.627008
882.330945	74023.180558	33.632026
883.176286	74126.045094	33.637044
884.071486	74242.476289	33.642061
884.648659	74360.614457	33.647079
885.425461	74480.724827	33.652096
886.494147	74599.778348	33.657114
887.786326	74708.173854	33.662132
888.740086	74818.848286	33.667149
889.677126	74947.442104	33.672167
890.674362	75058.477474	33.677184
891.384992	75175.569087	33.682202
892.032236	75293.410873	33.687220
893.059569	75406.522561	33.692237
893.903686	75524.972670	33.697255
894.402913	75644.950873	33.702272
895.459284	75777.834806	33.707290
896.167165	75894.804626	33.712308
897.365807	76012.651348	33.717325
898.056520	76154.412272	33.722343
899.308366	76270.886911	33.727360
900.240135	76393.979704	33.732378
901.306092	76513.038622	33.737396
902.437818	76633.952217	33.742413
903.017807	76757.867926	33.747431
904.200976	76872.650499	33.752448
905.228405	76998.152376	33.757466
906.349572	77109.748102	33.762484
906.979106	77236.604099	33.767501
907.589383	77359.222980	33.772519
908.718030	77467.564484	33.777536
909.508254	77599.143793	33.782554
910.592619	77730.664508	33.787572
911.463904	77853.320672	33.792589
912.273941	77977.807639	33.797607
913.014571	78099.778167	33.802624
914.094947	78224.394276	33.807642
914.997169	78349.728444	33.812660
916.375026	78473.597144	33.817677
916.849711	78590.682749	33.822695
918.145982	78704.509512	33.827712
919.413824	78815.629798	33.832730
920.316167	78919.179569	33.837748
921.677741	79039.957063	33.842765
922.689190	79151.524497	33.847783
923.694827	79258.295855	33.852800
924.117771	79367.790008	33.857818
925.017787	79480.489448	33.862836
925.972567	79588.831904	33.867853
926.501214	79724.492969	33.872871
927.164646	79839.153624	33.877888
927.828926	79958.106855	33.882906
928.481554	80080.482396	33.887924
929.418189	80194.696998	33.892941
930.121091	80319.524917	33.897959
931.349114	80436.697103	33.902976
932.712885	80553.096113	33.907994
933.545288	80671.773841	33.913012
934.647584	80785.124597	33.918029
934.998017	80909.841469	33.923047
936.119389	81020.927395	33.928064
937.065595	81149.824250	33.933082
937.742159	81285.535208	33.938100
938.534510	81398.097850	33.943117
939.425460	81537.082539	33.948135
940.418785	81657.769541	33.953152
942.179568	81773.878326	33.958170
943.246147	81888.226965	33.963188
944.676183	82005.331603	33.968205
945.408432	82126.075494	33.973223
946.451826	82239.690092	33.978240
947.299374	82347.330665	33.983258
948.074822	82478.791655	33.988276
949.191536	82589.071149	33.993293
949.631059	82722.502668	33.998311
950.629790	82840.698445	34.003328
951.455206	82968.917672	34.008346
952.245003	83091.681036	34.013364
953.234243	83209.431528	34.018381
954.299697	83351.017870	34.023399
954.851018	83473.581159	34.028416
955.826824	83619.767190	34.033434
956.455907	83763.821872	34.038452
957.245952	83904.216570	34.043469
957.938655	84047.852114	34.048487
959.120956	84197.581455	34.053504
959.846619	84346.398193	34.058522
961.015137	84499.084466	34.063540
961.871653	84640.971922	34.068557
962.246404	84797.706627	34.073575
963.553062	84951.638709	34.078592
965.425793	85106.670526	34.083610
965.981773	85258.789506	34.088628
967.160055	85390.583909	34.093645
968.621706	85533.278896	34.098663
969.887615	85667.324653	34.103680
971.006357	85810.132954	34.108698
972.196856	85938.350028	34.113716
973.482899	86063.618798	34.118733
974.460666	86189.114391	34.123751
975.224728	86313.955502	34.128768
976.299171	86440.366684	34.133786
976.990409	86572.157346	34.138804
978.173804	86693.272856	34.143821
979.228431	86821.263914	34.148839
980.069856	86945.350258	34.153856
981.152021	87066.939258	34.158874
981.622142	87189.505255	34.163892
982.650019	87305.438533	34.168909
983.373426	87433.131821	34.173927
984.289885	87556.899913	34.178944
985.311182	87687.171549	34.183962
986.111285	87811.389611	34.188980
987.549943	87935.392984	34.193997
988.580936	88046.681947	34.199015
989.779935	88174.670741	34.204032
990.643763	88297.749536	34.209050
991.274361	88431.755544	34.214068
992.313183	88545.474132	34.219085
993.574578	88676.826525	34.224103
994.522696	88798.573094	34.229120
995.316490	88918.201112	34.234138
996.398437	89052.094892	34.239156
997.805452	89184.590793	34.244173
998.805670	89309.196676	34.249191
999.810818	89427.586006	34.254208
1000.470730	89558.748515	34.259226
1001.113856	89696.769774	34.264244
1002.355055	89825.419305	34.269261
1003.082937	89967.577410	34.274279
1004.407459	90100.692808	34.279296
1005.461535	90234.825970	34.284314
1006.561837	90367.061647	34.289332
1007.712899	90503.539981	34.294349
1008.447838	90644.347965	34.299367
1009.672365	90769.261700	34.304384
1011.162899	90902.418820	34.309402
1011.672488	91041.563934	34.314420
1012.947398	91152.127973	34.319437
1013.945893	91293.163829	34.324455
1014.395950	91429.620296	34.329472
1015.694672	91567.947515	34.334490
1016.511388	91713.144948	34.339508
1017.279929	91853.917392	34.344525
1017.927111	92000.187256	34.349543
1018.932775	92153.345669	34.354560
1020.390718	92303.226521	34.359578
1021.328246	92448.776416	34.364596
1022.960895	92581.149457	34.369613
1024.276034	92719.519237	34.374631
1024.899691	92867.424087	34.379648
1026.185899	92997.008482	34.384666
1027.154324	93141.033682	34.389684
1028.107821	93264.948387	34.394701
1029.012549	93402.679300	34.399719
1030.283447	93536.323688	34.404736
1031.186476	93682.848594	34.409754
1031.915221	93828.314240	34.414772
1033.168649	93971.749190	34.419789
1034.162610	94114.960669	34.424807
1034.880597	94265.605001	34.429824
1036.139728	94401.685395	34.434842
1036.515789	94550.659194	34.439860
1037.795331	94680.621323	34.444877
1038.570841	94814.769646	34.449895
1039.316789	94957.165691	34.454912
1040.390305	95100.105146	34.459930
1041.015656	95250.536784	34.464948
1042.166334	95402.353436	34.469965
1043.415117	95561.664162	34.474983
1044.146471	95716.927576	34.480000
1045.110899	95864.140166	34.485018
1045.863991	96018.700034	34.490036
1047.183926	96187.979768	34.495053
1048.048270	96358.623731	34.500071
1048.834413	96523.853700	34.505088
1050.201146	96684.235338	34.510106
1050.883659	96853.469609	34.515124
1052.430946	97024.705838	34.520141
1053.701804	97189.148707	34.525159
1054.528590	97358.534603	34.530176
1056.117588	97505.677505	34.535194
1057.206606	97679.269017	34.540212
1058.194179	97837.428971	34.545229
1059.234574	97993.019421	34.550247
1060.234691	98160.700883	34.555264
1061.728616	98315.689976	34.560282
1062.354966	98482.762636	34.565300
1063.850834	98642.283447	34.570317
1065.116242	98802.778367	34.575335
1065.684578	98962.974040	34.580352
1067.148968	99123.161181	34.585370
1068.216931	99291.630970	34.590388
1069.521489	99456.084793	34.595405
1070.673946	99618.020581	34.600423
1071.378119	99781.895242	34.605440
1072.799466	99935.521224	34.610458
1073.316995	100101.496751	34.615476
1074.497682	100272.151246	34.620493
1075.829015	100422.169384	34.625511
1077.025688	100590.330812	34.630528
1077.982391	100750.901050	34.635546
1079.247134	100915.112177	34.640564
1080.447735	101069.318609	34.645581
1081.475625	101225.565615	34.650599
1082.698986	101384.984222	34.655616
1084.144173	101538.015942	34.660634
1084.894697	101701.820869	34.665652
1086.306711	101837.604925	34.670669
1088.344983	101970.271955	34.675687
1089.760397	102110.258525	34.680704
1091.168850	102245.324183	34.685722
1091.901327	102379.523670	34.690740
1093.184551	102509.757488	34.695757
1094.218259	102644.960982	34.700775
1094.738801	102786.694818	34.705792
1096.159578	102918.668142	34.710810
1097.233980	103027.581855	34.715828
1097.671296	103153.505336	34.720845
1099.087070	103278.236117	34.725863
1099.581990	103414.200474	34.730880
1100.510624	103547.540157	34.735898
1101.320221	103680.886869	34.740916
1102.325458	103827.106024	34.745933
1103.490586	103974.667516	34.750951
1104.337351	104114.952635	34.755968
1106.012421	104244.861637	34.760986
1106.812021	104402.090010	34.766004
1107.820935	104545.288160	34.771021
1109.049336	104690.040658	34.776039
1109.777739	104838.025034	34.781056
1110.847993	104996.176199	34.786074
1111.922944	105158.384149	34.791092
1112.929030	105317.712074	34.796109
1113.754269	105493.814897	34.801127
1114.571261	105653.909239	34.806144
1116.305527	105813.358832	34.811162
1116.784155	105983.426005	34.816180
1117.823470	106161.898240	34.821197
1119.237181	106328.547265	34.826215
1119.735345	106506.228432	34.831232
1121.028803	106697.036882	34.836250
1122.030422	106870.691533	34.841268
1123.540944	107040.753996	34.846285
1124.729894	107225.070859	34.851303
1125.912134	107419.573490	34.856320
1127.550261	107588.549934	34.861338
1128.642355	107762.835855	34.866356
1129.769768	107933.218694	34.871373
1131.139934	108089.184336	34.876391
1131.905286	108279.975358	34.881408
1132.954847	108449.329889	34.886426
1134.338882	108633.316328	34.891444
1135.989855	108786.102479	34.896461
1137.569185	108947.034205	34.901479
1138.808554	109121.515334	34.906496
1140.021318	109279.906165	34.911514
1141.436917	109437.272042	34.916532
1142.236673	109594.021623	34.921549
1143.370398	109748.218927	34.926567
1144.620323	109906.797799	34.931584
1145.559063	110068.148928	34.936602
1147.144203	110233.487312	34.941620
1147.912039	110391.538326	34.946637
1149.100404	110541.775852	34.951655
1150.188849	110696.473708	34.956672
1151.687268	110857.506824	34.961690
1152.675047	111027.730901	34.966708
1153.319980	111193.478434	34.971725
1154.608191	111345.673595	34.976743
1155.908811	111508.850295	34.981760
1156.993128	111669.277240	34.986778
1158.108834	111826.187029	34.991796
1159.036377	111974.904884	34.996813
1160.232357	112119.972750	35.001831
1161.026746	112280.715617	35.006848
1162.573704	112432.281271	35.011866
1163.283175	112589.627630	35.016884
1163.852955	112762.677426	35.021901
1165.365174	112927.247796	35.026919
1166.160750	113093.066344	35.031936
1167.304846	113259.185082	35.036954
1168.505112	113446.876683	35.041972
1169.438360	113622.425831	35.046989
1170.695683	113791.296546	35.052007
1171.921405	113987.604087	35.057024
1173.149903	114154.918162	35.062042
1174.474242	114343.242467	35.067060
1175.376099	114532.319079	35.072077
1176.477081	114704.981269	35.077095
1177.614718	114899.024490	35.082112
1178.543753	115085.410298	35.087130
1179.818991	115276.902172	35.092148
1181.128380	115464.426848	35.097165
1182.562914	115650.901050	35.102183
1183.465281	115851.085777	35.107200
1184.641617	116034.976439	35.112218
1186.521835	116210.494301	35.117236
1188.344490	116401.945606	35.122253
1189.576335	116576.233182	35.127271
1190.946526	116761.731737	35.132288
1192.339609	116929.316528	35.137306
1193.729873	117099.954608	35.142324
1195.167804	117256.080873	35.147341
1196.655983	117418.594912	35.152359
1197.742526	117586.144093	35.157376
1198.826653	117751.788944	35.162394
1200.236628	117906.321718	35.167412
1200.829306	118075.991386	35.172429
1202.419768	118243.673674	35.177447
1202.962586	118420.672978	35.182464
1204.245642	118594.516549	35.187482
1205.346084	118768.409316	35.192500
1206.045410	118944.019640	35.197517
1207.441766	119120.558768	35.202535
1208.853806	119316.162132	35.207552
1209.936659	119498.161164	35.212570
1210.890130	119673.976628	35.217588
1211.954338	119866.884988	35.222605
1213.388146	120053.783801	35.227623
1214.173871	120248.068999	35.232640
1215.862311	120435.069365	35.237658
1217.051875	120618.642297	35.242676
1218.180945	120807.038695	35.247693
1219.605575	120979.419231	35.252711
1220.828817	121180.265429	35.257728
1222.082462	121357.399604	35.262746
1223.329145	121519.046795	35.267764
1224.658099	121692.549065	35.272781
1225.860530	121849.937189	35.277799
1227.131259	122026.085257	35.282816
1228.477955	122196.966315	35.287834
1229.402002	122361.139682	35.292852
1231.302203	122514.874525	35.297869
1232.704527	122669.170699	35.302887
1233.771426	122827.903394	35.307904
1235.181831	122999.780078	35.312922
1236.282517	123163.816330	35.317940
1237.287537	123332.593162	35.322957
1238.509168	123501.412621	35.327975
1239.497103	123675.007386	35.332992
1240.236860	123848.009424	35.338010
1241.804193	124023.604247	35.343028
1242.664267	124206.063769	35.348045
1244.090125	124387.573278	35.353063
1245.418151	124578.346062	35.358080
1246.296496	124767.291703	35.363098
1247.506168	124947.547368	35.368116
1248.503491	125148.611381	35.373133
1249.575410	125342.153620	35.378151
1250.762600	125541.632355	35.383168
1252.290656	125735.370898	35.388186
1253.687523	125931.817099	35.393204
1254.774012	126149.278220	35.398221
1256.279353	126345.241478	35.403239
1257.557435	126536.187998	35.408256
1258.728699	126746.268008	35.413274
1260.002149	126942.411759	35.418292
1260.956026	127146.791007	35.423309
1262.292253	127358.318937	35.428327
1263.557904	127571.924573	35.433344
1264.639299	127768.079422	35.438362
1266.011982	127984.014809	35.443380
1267.314705	128197.366045	35.448397
1268.201872	128414.788142	35.453415
1269.134642	128636.359906	35.458432
1270.363183	128857.899096	35.463450
1271.928929	129079.323111	35.468468
1273.367966	129302.846688	35.473485
1274.558191	129516.099272	35.478503
1275.776803	129732.908914	35.483520
1277.077311	129965.923438	35.488538
1279.080671	130171.792492	35.493556
1280.074324	130393.735963	35.498573
1281.705200	130611.639777	35.503591
1283.133381	130822.001254	35.508608
1283.960043	131041.290493	35.513626
1285.833384	131245.705776	35.518644
1287.669210	131441.829924	35.523661
1288.744093	131637.024805	35.528679
1290.204219	131855.598870	35.533696
1291.454771	132043.508854	35.538714
1293.062050	132233.466592	35.543732
1293.841270	132424.811553	35.548749
1295.305816	132604.506401	35.553767
1296.849150	132788.383694	35.558784
1298.435394	132950.728573	35.563802
1300.143354	133112.434185	35.568820
1301.218396	133289.559834	35.573837
1302.405888	133462.690174	35.578855
1303.672526	133648.150113	35.583872
1304.700977	133828.872274	35.588890
1306.020941	134010.550226	35.593908
1306.948648	134205.507329	35.598925
1308.211108	134393.646285	35.603943
1309.381547	134584.652065	35.608960
1310.402040	134786.199927	35.613978
1311.726097	134961.154883	35.618996
1312.685726	135171.762302	35.624013
1313.918244	135385.495710	35.629031
1315.478766	135585.911581	35.634048
1316.335780	135799.935803	35.639066
1317.800746	136010.456310	35.644084
1318.677999	136232.336882	35.649101
1319.975486	136450.794322	35.654119
1321.745703	136667.644962	35.659136
1323.067811	136896.036571	35.664154
1324.270004	137114.286006	35.669172
1325.371248	137340.219769	35.674189
1326.754687	137567.022819	35.679207
1328.035496	137799.090284	35.684224
1329.592848	138012.043555	35.689242
1331.034182	138235.649074	35.694260
1332.919414	138463.519778	35.699277
1334.600447	138667.384482	35.704295
1336.193873	138878.589404	35.709312
1337.249636	139080.465293	35.714330
1338.908978	139295.553281	35.719348
1340.374000	139510.762411	35.724365
1342.341976	139714.702731	35.729383
1344.084794	139905.880220	35.734400
1344.931000	140109.291799	35.739418
1346.475688	140306.992087	35.744436
1347.511228	140512.328009	35.749453
1348.252915	140715.785640	35.754471
1350.252670	140916.484618	35.759488
1351.292943	141119.669387	35.764506
1352.395750	141325.000138	35.769524
1353.914838	141531.825017	35.774541
1355.442922	141743.681467	35.779559
1356.455723	141951.299405	35.784576
1357.552761	142165.445261	35.789594
1359.308381	142375.444856	35.794612
1360.333588	142586.677316	35.799629
1361.809009	142802.681334	35.804647
1362.944120	143015.116029	35.809664
1364.199844	143237.976938	35.814682
1365.561535	143441.290841	35.819700
1366.533330	143637.265951	35.824717
1367.845683	143841.464894	35.829735
1369.188052	144041.819894	35.834752
1370.311485	144273.924015	35.839770
1371.793425	144479.621224	35.844788
1373.097609	144702.497656	35.849805
1374.199213	144906.863852	35.854823
1375.990577	145132.023550	35.859840
1376.973527	145364.652465	35.864858
1378.517272	145569.383701	35.869876
1379.572219	145807.252161	35.874893
1380.927837	146035.567795	35.879911
1382.275688	146260.768052	35.884928
1383.715724	146497.883363	35.889946
1385.757256	146718.793587	35.894964
1387.030727	146946.824645	35.899981
1388.270228	147176.650093	35.904999
1390.174579	147388.726093	35.910016
1391.460505	147614.731756	35.915034
1393.211321	147845.190665	35.920052
1394.559221	148066.182456	35.925069
1395.599182	148276.043869	35.930087
1397.146985	148518.481333	35.935104
1398.290532	148746.000800	35.940122
1400.121464	148954.625398	35.945140
1402.187592	149181.557654	35.950157
1403.496899	149402.780288	35.955175
1405.559146	149620.145015	35.960192
1406.686374	149832.132475	35.965210
1407.749270	150049.658882	35.970228
1409.337763	150271.692471	35.975245
1410.674278	150481.635197	35.980263
1411.947862	150704.938823	35.985280
1413.354846	150928.691856	35.990298
1414.916174	151139.186263	35.995316
1416.425965	151361.315836	36.000333
1417.675278	151596.635364	36.005351
1419.503680	151808.296035	36.010368
1420.332837	152039.032637	36.015386
1421.617243	152268.468724	36.020404
1423.258304	152499.371133	36.025421
1424.918293	152717.162664	36.030439
1427.237009	152910.001122	36.035456
1429.030760	153114.106603	36.040474
1430.751006	153299.752242	36.045492
1431.914441	153509.450144	36.050509
1433.612647	153721.093001	36.055527
1435.375262	153912.859175	36.060544
1436.298196	154117.895244	36.065562
1437.312357	154322.677167	36.070580
1438.622918	154518.360369	36.075597
1439.989096	154719.285046	36.080615
1441.489134	154931.195237	36.085632
1442.493018	155149.753479	36.090650
1443.652169	155356.179625	36.095668
1445.150816	155550.380785	36.100685
1445.792761	155768.620132	36.105703
1447.452333	155968.250321	36.110720
1448.472182	156184.454264	36.115738
1449.740544	156398.274329	36.120756
1451.128080	156622.347492	36.125773
1452.311670	156850.296550	36.130791
1453.904388	157065.590836	36.135808
1455.623745	157300.355697	36.140826
1457.450833	157515.501438	36.145844
1458.816404	157748.131878	36.150861
1459.973475	157970.386420	36.155879
1461.924829	158186.302772	36.160896
1463.219446	158412.152217	36.165914
1464.465985	158647.470503	36.170932
1465.888058	158876.041716	36.175949
1467.166442	159111.637045	36.180967
1468.992059	159334.871935	36.185984
1470.205734	159575.946116	36.191002
1471.698682	159819.069951	36.196020
1473.826467	160048.297541	36.201037
1475.321482	160274.685110	36.206055
1477.125805	160496.180737	36.211072
1478.756851	160725.390183	36.216090
1480.033584	160960.592314	36.221108
1481.610427	161181.849364	36.226125
1483.077951	161410.252217	36.231143
1485.120773	161621.799945	36.236160
1486.507621	161863.090416	36.241178
1487.842181	162085.406085	36.246196
1489.427246	162308.038427	36.251213
1490.599517	162548.758852	36.256231
1492.135608	162769.803890	36.261248
1493.446355	162999.078757	36.266266
1494.652525	163241.345626	36.271284
1496.255697	163482.688642	36.276301
1497.491434	163726.831031	36.281319
1499.068602	163958.517325	36.286336
1500.183423	164209.961904	36.291354
1501.866535	164454.025392	36.296372
1504.026694	164692.827473	36.301389
1505.131281	164936.846558	36.306407
1507.144248	165166.213695	36.311424
1508.516805	165412.146520	36.316442
1510.416350	165645.567840	36.321460
1511.823727	165886.678708	36.326477
1513.050993	166125.879213	36.331495
1514.984447	166360.263556	36.336512
1516.202783	166603.717452	36.341530
1517.896790	166845.296311	36.346548
1519.506985	167074.612347	36.351565
1520.827852	167315.758845	36.356583
1522.540710	167553.128284	36.361600
1524.287027	167776.529034	36.366618
1525.880834	168004.064903	36.371636
1526.844690	168215.999475	36.376653
1528.548542	168431.698989	36.381671
1530.223436	168635.963278	36.386688
1531.424018	168851.212376	36.391706
1532.617890	169077.270713	36.396724
1534.225707	169295.565256	36.401741
1535.579510	169528.729426	36.406759
1536.974563	169760.987857	36.411776
1538.355783	169994.328068	36.416794
1539.511903	170237.891184	36.421812
1541.008598	170489.114023	36.426829
1542.416243	170736.597937	36.431847
1544.231517	170990.297678	36.436864
1545.451954	171233.526998	36.441882
1546.720827	171491.705769	36.446900
1548.490645	171745.963081	36.451917
1549.886558	172003.896705	36.456935
1551.517006	172267.249426	36.461952
1553.261180	172525.638549	36.466970
1554.930676	172792.718055	36.471988
1556.212151	173053.733880	36.477005
1557.460670	173321.162878	36.482023
1559.220034	173594.614340	36.487040
1560.803856	173855.409776	36.492058
1562.397607	174142.249396	36.497076
1564.214376	174404.102372	36.502093
1565.873670	174683.146257	36.507111
1567.067071	174957.737117	36.512128
1568.834109	175222.888989	36.517146
1570.093500	175503.917643	36.522164
1571.552587	175783.482951	36.527181
1573.036271	176067.486520	36.532199
1575.081529	176347.317789	36.537216
1576.521120	176634.744958	36.542234
1577.974590	176924.189110	36.547252
1579.968061	177199.873134	36.552269
1582.071007	177477.711059	36.557287
1584.184419	177750.322141	36.562304
1586.135726	178011.656579	36.567322
1587.849458	178277.128326	36.572340
1589.658913	178536.344437	36.577357
1591.015677	178791.510670	36.582375
1592.791774	179040.369661	36.587392
1594.455578	179290.174132	36.592410
1596.051705	179550.470709	36.597428
1597.842746	179791.110217	36.602445
1599.331984	180052.898597	36.607463
1600.823386	180314.548669	36.612480
1602.296693	180575.023241	36.617498
1603.783373	180826.463484	36.622516
1605.713983	181075.462038	36.627533
1607.233855	181340.146237	36.632551
1608.881170	181586.617047	36.637568
1610.858764	181816.821300	36.642586
1612.701265	182050.765881	36.647604
1614.645738	182276.486179	36.652621
1616.250327	182500.104593	36.657639
1617.864916	182716.071425	36.662656
1619.350082	182926.540370	36.667674
1620.370072	183158.553249	36.672692
1622.396618	183374.610144	36.677709
1623.603136	183608.448295	36.682727
1624.655590	183843.606395	36.687744
1626.162149	184083.401176	36.692762
1627.241914	184331.982296	36.697780
1628.712795	184577.343127	36.702797
1630.235819	184842.682262	36.707815
1631.827080	185108.595820	36.712832
1633.138596	185378.298679	36.717850
1634.469817	185656.755610	36.722868
1636.434931	185927.664932	36.727885
1637.941567	186218.609139	36.732903
1639.258414	186499.014970	36.737920
1641.494134	186772.068910	36.742938
1643.130418	187054.026284	36.747956
1644.514491	187335.987358	36.752973
1645.981376	187615.119856	36.757991
1647.298416	187902.843498	36.763008
1649.268361	188185.427316	36.768026
1650.981848	188478.180221	36.773044
1652.945384	188768.078034	36.778061
1654.357718	189062.176784	36.783079
1656.107738	189357.581598	36.788096
1657.941542	189648.710984	36.793114
1659.361034	189950.111052	36.798132
1661.309642	190238.560813	36.803149
1663.204958	190518.784576	36.808167
1664.405738	190815.503908	36.813184
1666.681944	191108.856226	36.818202
1668.145098	191400.296202	36.823220
1669.883630	191692.252595	36.828237
1671.668075	191981.919068	36.833255
1673.308379	192275.861644	36.838272
1675.406176	192561.496794	36.843290
1676.951263	192852.856251	36.848308
1679.105071	193139.640749	36.853325
1681.409238	193420.933060	36.858343
1683.209135	193693.676869	36.863360
1684.978352	193965.627474	36.868378
1686.324827	194239.321960	36.873396
1688.232839	194507.763284	36.878413
1690.021904	194787.736279	36.883431
1691.785843	195060.366283	36.888448
1693.773915	195317.846203	36.893466
1695.169703	195586.095338	36.898484
1696.625266	195858.448579	36.903501
1698.352257	196129.922493	36.908519
1699.791112	196408.348080	36.913536
1702.149044	196658.592275	36.918554
1703.311805	196923.877327	36.923572
1705.286285	197168.612979	36.928589
1706.833675	197412.871818	36.933607
1708.355222	197668.292511	36.938624
1710.417648	197915.657708	36.943642
1711.879444	198162.040564	36.948660
1713.465582	198398.161921	36.953677
1715.167969	198660.577689	36.958695
1716.705108	198918.070836	36.963712
1718.229456	199184.388717	36.968730
1719.932529	199445.868967	36.973748
1721.850784	199699.599054	36.978765
1723.632043	199974.105037	36.983783
1724.825220	200253.427575	36.988800
1726.876423	200518.843342	36.993818
1728.402887	200786.514234	36.998836
1730.132828	201062.315851	37.003853
1731.968534	201329.254860	37.008871
1733.399617	201618.218838	37.013888
1735.102324	201892.416872	37.018906
1736.740797	202171.170709	37.023924
1739.332101	202445.116149	37.028941
1740.959945	202721.373794	37.033959
1742.823822	202997.582629	37.038976
1745.013728	203259.486038	37.043994
1746.737821	203538.283830	37.049012
1748.447183	203813.899179	37.054029
1749.965209	204084.811417	37.059047
1751.823202	204358.933304	37.064064
1753.825210	204628.565347	37.069082
1755.512912	204913.481412	37.074100
1757.339503	205179.868804	37.079117
1759.381835	205462.052800	37.084135
1760.594244	205743.328981	37.089152
1762.284785	206012.877241	37.094170
1764.162795	206287.487408	37.099188
1765.776010	206575.838157	37.104205
1767.682883	206856.641252	37.109223
1769.493577	207134.312691	37.114240
1771.389322	207409.636111	37.119258
1773.545977	207690.923942	37.124276
1775.215348	207972.265048	37.129293
1777.220205	208246.267404	37.134311
1778.970715	208513.786230	37.139328
1780.803109	208781.267838	37.144346
1782.387313	209064.696761	37.149364
1784.452954	209346.476383	37.154381
1786.196220	209619.523485	37.159399
1788.050594	209893.125429	37.164416
1789.559603	210157.909477	37.169434
1791.146498	210448.656688	37.174452
1793.389342	210708.311957	37.179469
1794.934751	210991.578044	37.184487
1796.584237	211275.463641	37.189504
1798.538906	211550.021693	37.194522
1799.940806	211808.418438	37.199540
1801.656231	212076.630886	37.204557
1803.418828	212333.233189	37.209575
1805.116603	212606.452696	37.214592
1806.963931	212864.376688	37.219610
1808.616013	213133.365289	37.224628
1810.546594	213401.714083	37.229645
1812.312661	213667.588998	37.234663
1813.911753	213947.799762	37.239680
1815.913488	214205.069688	37.244698
1817.418285	214485.500810	37.249716
1819.081767	214768.599478	37.254733
1820.986804	215051.597512	37.259751
1822.839692	215336.991881	37.264768
1824.484534	215607.311972	37.269786
1826.264905	215898.573151	37.274804
1828.147292	216182.404719	37.279821
1830.321903	216486.632230	37.284839
1831.875191	216791.734171	37.289856
1833.997907	217067.481673	37.294874
1835.672285	217368.707177	37.299892
1837.279214	217667.443443	37.304909
1839.417746	217959.265801	37.309927
1841.410472	218263.859973	37.314944
1843.025653	218566.420398	37.319962
1844.764677	218864.023382	37.324980
1847.028506	219164.439176	37.329997
1849.057741	219461.287522	37.335015
1851.078724	219760.715863	37.340032
1853.177876	220048.985046	37.345050
1854.879518	220337.991384	37.350068
1857.029599	220624.007340	37.355085
1859.597767	220916.268520	37.360103
1861.087662	221197.058636	37.365120
1863.131650	221532.385422	37.370138
1865.128318	221822.874312	37.375156
1866.903211	222104.651028	37.380173
1868.837694	222381.591137	37.385191
1870.752016	222671.042416	37.390208
1873.206821	222943.457852	37.395226
1875.070954	223224.259468	37.400244
1876.811438	223502.897727	37.405261
1879.000767	223769.314116	37.410279
1880.946392	224040.887233	37.415296
1882.594672	224308.457895	37.420314
1884.659548	224580.890062	37.425332
1886.486902	224862.185808	37.430349
1888.711247	225130.683601	37.435367
1889.801317	225414.815598	37.440384
1891.798832	225692.214350	37.445402
1893.982514	225968.213112	37.450420
1895.267777	226251.021819	37.455437
1896.839260	226537.341515	37.460455
1898.284003	226827.390143	37.465472
1900.223680	227104.078975	37.470490
1902.268628	227387.202677	37.475508
1903.470903	227664.924619	37.480525
1905.553948	227949.034593	37.485543
1906.992869	228231.850904	37.490560
1908.573674	228514.264668	37.495578
1910.717726	228799.002655	37.500596
1912.188352	229093.753197	37.505613
1913.976718	229388.606680	37.510631
1915.916801	229691.259344	37.515648
1918.114331	229990.595948	37.520666
1920.243968	230289.944319	37.525684
1922.177481	230599.585294	37.530701
1924.317568	230890.070328	37.535719
1926.323256	231194.622385	37.540736
1927.967049	231499.258264	37.545754
1930.504986	231797.149878	37.550772
1932.365644	232094.540361	37.555789
1934.152435	232397.226231	37.560807
1936.025204	232707.544168	37.565824
1938.005894	233004.105706	37.570842
1940.012813	233308.384982	37.575860
1942.170325	233628.464315	37.580877
1944.360926	233919.052178	37.585895
1946.382613	234232.932478	37.590912
1948.481688	234539.410576	37.595930
1950.729776	234835.401830	37.600948
1952.719317	235127.650603	37.605965
1954.970578	235430.805454	37.610983
1956.837337	235741.362408	37.616000
1958.892937	236020.395962	37.621018
1960.808237	236318.019010	37.626036
1962.482178	236628.863186	37.631053
1964.912400	236913.833796	37.636071
1966.901201	237210.050750	37.641088
1969.049366	237521.304861	37.646106
1971.431043	237803.898025	37.651124
1973.223360	238104.085457	37.656141
1975.242994	238378.127224	37.661159
1977.386527	238679.149467	37.666176
1979.403233	238965.841998	37.671194
1981.842453	239257.649707	37.676212
1983.611192	239545.119630	37.681229
1985.687708	239826.216953	37.686247
1987.354569	240114.618847	37.691264
1989.438619	240403.742655	37.696282
1991.397905	240691.616981	37.701300
1992.959086	240987.987905	37.706317
1994.820627	241273.643964	37.711335
1996.642034	241584.579999	37.716352
1998.818026	241885.046575	37.721370
2000.813675	242187.955503	37.726388
2002.208376	242496.472339	37.731405
2004.525072	242791.737167	37.736423
2006.328327	243101.689282	37.741440
2007.882737	243404.874349	37.746458
2009.697525	243696.182252	37.751476
2011.197482	244000.799774	37.756493
2013.308117	244293.332097	37.761511
2015.091431	244597.499637	37.766528
2017.096217	244904.452200	37.771546
2019.308361	245211.245561	37.776564
2020.580632	245522.710041	37.781581
2022.857226	245834.320706	37.786599
2024.598564	246152.367187	37.791616
2026.672975	246485.779879	37.796634
2028.517479	246808.028010	37.801652
2030.532684	247134.491748	37.806669
2032.499167	247474.274096	37.811687
2034.228446	247810.183085	37.816704
2036.296877	248156.656713	37.821722
2038.636388	248488.253818	37.826740
2040.244468	248846.867625	37.831757
2042.621562	249194.056672	37.836775
2044.899209	249544.031012	37.841792
2046.571459	249898.572811	37.846810
2048.711990	250243.515537	37.851828
2050.673526	250608.732424	37.856845
2052.900639	250961.207177	37.861863
2055.222350	251315.267965	37.866880
2057.593638	251666.705242	37.871898
2060.351957	252007.489301	37.876916
2062.201790	252365.538951	37.881933
2064.109973	252713.901948	37.886951
2066.714266	253059.742010	37.891968
2068.718774	253404.636378	37.896986
2071.180707	253740.898346	37.902004
2073.471550	254092.302265	37.907021
2076.008656	254406.606104	37.912039
2078.387777	254737.421489	37.917056
2080.584842	255056.886125	37.922074
2083.218288	255378.441233	37.927092
2085.065381	255708.707532	37.932109
2087.248343	256033.484985	37.937127
2089.345827	256351.062229	37.942144
2091.284903	256663.889417	37.947162
2093.443690	256997.359753	37.952180
2095.105584	257325.549482	37.957197
2097.140721	257644.738808	37.962215
2099.321450	257965.734459	37.967232
2101.475844	258299.207369	37.972250
2104.001101	258616.719903	37.977268
2106.027296	258945.311329	37.982285
2108.144754	259264.972381	37.987303
2110.401854	259576.736854	37.992320
2112.239081	259892.607321	37.997338
2114.401712	260208.324939	38.002356
2116.593863	260526.222877	38.007373
2118.835734	260851.302280	38.012391
2120.982496	261174.999982	38.017408
2122.892925	261494.518653	38.022426
2125.101370	261782.338423	38.027444
2126.878026	262087.246883	38.032461
2128.948612	262384.767581	38.037479
2131.515352	262659.016982	38.042496
2133.470289	262951.958611	38.047514
2135.421156	263247.365231	38.052532
2137.266732	263553.661290	38.057549
2139.445762	263847.076202	38.062567
2141.700664	264155.543327	38.067584
2143.241828	264469.001290	38.072602
2145.396108	264771.337334	38.077620
2147.285897	265097.721492	38.082637
2149.202050	265417.319095	38.087655
2151.720250	265743.248460	38.092672
2153.435689	266069.025942	38.097690
2155.737755	266393.897726	38.102708
2157.686500	266729.926967	38.107725
2160.058228	267072.468794	38.112743
2162.115089	267402.257555	38.117760
2164.101081	267750.119472	38.122778
2166.282012	268086.366803	38.127796
2168.311513	268448.397270	38.132813
2170.468921	268792.904796	38.137831
2172.739570	269142.119564	38.142848
2174.538044	269498.776350	38.147866
2176.997737	269851.644973	38.152884
2178.970347	270218.283399	38.157901
2181.100596	270582.356653	38.162919
2183.509622	270940.949527	38.167936
2185.428577	271307.800131	38.172954
2187.996803	271670.305538	38.177972
2190.297534	272038.188186	38.182989
2192.622488	272402.561426	38.188007
2195.281043	272767.186696	38.193024
2197.072413	273128.875740	38.198042
2199.472897	273496.514273	38.203060
2201.932272	273866.252003	38.208077
2204.370106	274220.573320	38.213095
2206.645411	274574.945839	38.218112
2208.700873	274945.560613	38.223130
2211.589628	275294.475763	38.228148
2213.853838	275644.607688	38.233165
2216.210990	275995.258332	38.238183
2218.700387	276333.770554	38.243200
2221.096848	276678.140262	38.248218
2223.828249	277015.216847	38.253236
2226.109306	277355.794245	38.258253
2228.400397	277686.234034	38.263271
2230.796797	278006.597315	38.268288
2232.707585	278353.838089	38.273306
2234.836252	278686.107037	38.278324
2237.292706	279013.827520	38.283341
2239.825069	279339.147950	38.288359
2242.436593	279660.899251	38.293376
2244.453115	279971.389482	38.298394
2246.593906	280263.086834	38.303412
2248.641677	280562.597647	38.308429
2250.554236	280854.432574	38.313447
2252.773758	281142.052572	38.318464
2254.321641	281464.403617	38.323482
2256.489005	281770.499802	38.328500
2258.753010	282077.799868	38.333517
2260.282014	282395.733248	38.338535
2262.758091	282716.996539	38.343552
2265.212873	283044.334384	38.348570
2267.518455	283363.922295	38.353588
2269.503223	283681.249173	38.358605
2271.681238	284018.512091	38.363623
2274.148089	284350.343502	38.368640
2275.930573	284691.021838	38.373658
2278.632560	285036.329910	38.378676
2280.795466	285371.714342	38.383693
2282.789916	285721.604942	38.388711
2285.352387	286066.502387	38.393728
2287.562570	286425.503230	38.398746
2290.235419	286762.177350	38.403764
2292.539198	287105.844665	38.408781
2294.806443	287449.263396	38.413799
2297.389934	287789.583286	38.418816
2299.530195	288145.392633	38.423834
2301.939485	288497.094470	38.428852
2304.137969	288855.510262	38.433869
2306.027813	289205.591628	38.438887
2308.410378	289560.446389	38.443904
2310.831494	289923.271050	38.448922
2313.429029	290280.351660	38.453940
2315.592518	290642.682746	38.458957
2318.019572	291012.363715	38.463975
2320.054194	291371.132442	38.468992
2322.349095	291750.994318	38.474010
2324.756463	292108.788399	38.479028
2327.184437	292484.233399	38.484045
2329.344579	292864.521314	38.489063
2332.010359	293235.786808	38.494080
2334.147358	293601.216762	38.499098
2336.273038	293979.476068	38.504116
2338.674574	294345.269282	38.509133
2340.997785	294726.569631	38.514151
2344.117078	295095.600858	38.519168
2347.568225	295446.873540	38.524186
2350.207481	295803.227705	38.529204
2352.627100	296143.282533	38.534221
2354.388715	296497.945598	38.539239
2356.797235	296846.180382	38.544256
2359.771086	297190.235210	38.549274
2362.559824	297527.003007	38.554292
2365.226567	297862.214608	38.559309
2367.426733	298199.150649	38.564327
2369.681096	298517.864437	38.569344
2371.715467	298848.906912	38.574362
2373.642322	299172.675530	38.579380
2375.734517	299489.431895	38.584397
2377.430317	299812.270646	38.589415
2379.734123	300136.460282	38.594432
2381.818536	300465.789730	38.599450
2383.953277	300801.537069	38.604468
2386.414004	301139.137130	38.609485
2388.431770	301476.984479	38.614503
2391.148534	301824.245751	38.619520
2392.983278	302176.624645	38.624538
2395.128948	302536.167341	38.629556
2397.468446	302894.408398	38.634573
2399.318297	303265.985475	38.639591
2401.807105	303650.389378	38.644608
2403.968985	304030.678328	38.649626
2406.131333	304414.700087	38.654644
2408.805189	304805.650304	38.659661
2410.975337	305208.033301	38.664679
2413.305709	305592.456948	38.669696
2415.443379	306007.238154	38.674714
2417.844925	306415.422946	38.679732
2420.398916	306826.223929	38.684749
2422.713685	307246.459582	38.689767
2425.530593	307650.358197	38.694784
2427.725958	308076.350433	38.699802
2430.114357	308504.825206	38.704820
2432.514377	308918.894919	38.709837
2435.072052	309338.983371	38.714855
2437.762891	309770.275893	38.719872
2440.349479	310195.563656	38.724890
2443.157357	310603.111356	38.729908
2446.545283	311018.566500	38.734925
2449.242038	311425.620889	38.739943
2452.049417	311826.712858	38.744960
2454.691043	312220.413102	38.749978
2457.059309	312631.350395	38.754996
2459.689695	313018.445801	38.760013
2462.147032	313420.450955	38.765031
2464.953708	313820.545127	38.770048
2467.569806	314210.127541	38.775066
2470.104721	314608.814046	38.780084
2472.633263	314990.305269	38.785101
2474.564895	315391.928958	38.790119
2477.580770	315776.743391	38.795136
2480.088805	316173.878730	38.800154
2482.542794	316567.795492	38.805172
2484.966570	316948.686314	38.810189
2487.277505	317350.292778	38.815207
2490.047450	317731.735223	38.820224
2492.764734	318120.397424	38.825242
2495.158419	318508.347379	38.830260
2497.621041	318895.903849	38.835277
2499.750382	319296.133986	38.840295
2502.492570	319674.322086	38.845312
2504.773385	320061.927865	38.850330
2507.440846	320422.575294	38.855348
2509.959218	320781.162352	38.860365
2512.493245	321131.770893	38.865383
2514.733291	321481.815104	38.870400
2516.912891	321835.169058	38.875418
2519.152205	322197.096138	38.880436
2521.824806	322563.575201	38.885453
2524.479577	322945.877411	38.890471
2526.587293	323308.785717	38.895488
2529.047363	323682.988681	38.900506
2531.389925	324064.878170	38.905524
2534.095479	324435.712005	38.910541
2536.502674	324829.472982	38.915559
2539.049495	325208.505903	38.920576
2541.611520	325605.311478	38.925594
2544.112958	325994.988610	38.930612
2546.822988	326383.894340	38.935629
2549.495166	326781.362312	38.940647
2551.827654	327174.717323	38.945664
2554.496111	327583.000085	38.950682
2556.946702	327976.789448	38.955700
2560.067144	328377.251032	38.960717
2561.975600	328791.056843	38.965735
2564.827525	329197.448166	38.970752
2567.528686	329601.728073	38.975770
2569.688503	330016.553891	38.980788
2572.611502	330417.061312	38.985805
2574.889073	330839.761355	38.990823
2577.646550	331251.184360	38.995840
2580.614365	331664.298467	39.000858
2583.275507	332073.319680	39.005876
2585.964683	332473.802014	39.010893
2588.661513	332892.233738	39.015911
2591.344312	333295.658023	39.020928
2594.031612	333704.259385	39.025946
2596.681402	334122.767390	39.030964
2599.311528	334530.408024	39.035981
2602.145846	334937.810751	39.040999
2605.394195	335335.496458	39.046016
2607.596649	335742.537390	39.051034
2610.174932	336150.709741	39.056052
2613.183769	336550.482936	39.061069
2615.431965	336960.530806	39.066087
2618.105092	337361.926544	39.071104
2620.781851	337777.969956	39.076122
2622.961251	338187.132350	39.081140
2625.624240	338591.594418	39.086157
2628.034752	339011.252173	39.091175
2630.814132	339422.622211	39.096192
2633.313143	339841.904999	39.101210
2636.034062	340274.936716	39.106228
2638.570626	340688.901348	39.111245
2641.101238	341104.438336	39.116263
2643.962464	341525.810566	39.121280
2646.809887	341936.213826	39.126298
2649.355647	342332.190185	39.131316
2651.809863	342717.692731	39.136333
2654.509583	343093.150658	39.141351
2656.782338	343479.057897	39.146368
2659.543344	343870.318485	39.151386
2661.774377	344261.254212	39.156404
2664.438455	344650.900119	39.161421
2666.575523	345067.055988	39.166439
2668.901771	345475.740242	39.171456
2671.558635	345882.820594	39.176474
2674.272577	346319.541769	39.181492
2676.890114	346741.220137	39.186509
2679.300209	347174.327101	39.191527
2682.049340	347593.744212	39.196544
2684.841194	348035.085665	39.201562
2687.307626	348475.281998	39.206580
2690.402774	348906.413856	39.211597
2693.287673	349345.699244	39.216615
2696.177647	349784.294888	39.221632
2699.207451	350227.561241	39.226650
2701.667831	350666.700135	39.231668
2704.282866	351104.338607	39.236685
2706.866090	351550.736441	39.241703
2709.691560	351997.828338	39.246720
2712.392353	352448.210842	39.251738
2714.869887	352903.168688	39.256756
2718.116576	353349.167028	39.261773
2721.052641	353794.093835	39.266791
2723.851653	354244.115303	39.271808
2726.728551	354695.440454	39.276826
2729.548849	355150.425806	39.281844
2732.268337	355602.630898	39.286861
2735.064898	356045.453417	39.291879
2737.948006	356489.019818	39.296896
2740.837588	356937.936981	39.301914
2743.263890	357396.086473	39.306932
2746.491357	357848.470039	39.311949
2749.078572	358301.458466	39.316967
2751.550100	358764.131414	39.321984
2754.725149	359215.926866	39.327002
2757.196003	359671.636776	39.332020
2760.061783	360126.543796	39.337037
2762.936805	360580.099857	39.342055
2765.659869	361040.553752	39.347072
2768.647320	361489.032633	39.352090
2771.503906	361958.897861	39.357108
2774.221839	362404.187438	39.362125
2777.118351	362864.596006	39.367143
2779.484817	363327.875638	39.372160
2782.279491	363784.585819	39.377178
2784.971090	364255.697476	39.382196
2787.596846	364711.156228	39.387213
2790.301093	365178.348068	39.392231
2793.081847	365647.730841	39.397248
2796.276007	366090.371386	39.402266
2798.622367	366538.851689	39.407284
2801.417285	366970.735954	39.412301
2803.688027	367405.236688	39.417319
2806.184315	367852.791767	39.422336
2809.208852	368294.269829	39.427354
2811.294717	368745.408079	39.432372
2814.039135	369197.731552	39.437389
2816.813349	369668.417485	39.442407
2820.123576	370115.693524	39.447424
2823.144552	370566.842315	39.452442
2825.582621	371041.042763	39.457460
2828.340976	371506.636012	39.462477
2831.100204	371975.395761	39.467495
2833.384045	372463.103714	39.472512
2836.343381	372934.662929	39.477530
2839.078478	373443.398807	39.482548
2841.713363	373941.411526	39.487565
2844.467678	374446.960371	39.492583
2847.256844	374955.694377	39.497600
2849.939480	375455.736289	39.502618
2852.887466	375980.264481	39.507636
2855.487006	376493.347776	39.512653
2858.398085	377016.219167	39.517671
2861.462511	377547.406402	39.522688
2864.584038	378070.078417	39.527706
2867.594156	378595.222049	39.532724
2870.514222	379119.358133	39.537741
2873.307555	379649.063147	39.542759
2876.657500	380173.472193	39.547776
2880.227386	380691.421045	39.552794
2883.081481	381225.509024	39.557812
2885.724834	381739.150962	39.562829
2889.099271	382257.109598	39.567847
2891.970670	382781.000636	39.572864
2895.132257	383298.801145	39.577882
2898.323233	383817.426967	39.582900
2901.225765	384327.771129	39.587917
2904.511664	384848.574461	39.592935
2907.165121	385364.575032	39.597952
2910.446802	385866.873208	39.602970
2912.796607	386392.013537	39.607988
2915.493082	386918.511861	39.613005
2918.876869	387422.268998	39.618023
2921.416218	387961.459111	39.623040
2924.330123	388471.109649	39.628058
2927.325430	389003.313132	39.633076
2929.614754	389531.993567	39.638093
2932.793316	390068.894933	39.643111
2935.425103	390614.269457	39.648128
2938.124838	391139.107361	39.653146
2941.021425	391693.198286	39.658164
2943.325419	392243.417934	39.663181
2946.568478	392795.635859	39.668199
2949.382274	393354.176775	39.673216
2952.343007	393905.762236	39.678234
2955.286212	394436.876838	39.683252
2958.183000	394957.973839	39.688269
2960.941913	395475.001972	39.693287
2963.547104	395997.498460	39.698304
2966.664911	396519.043548	39.703322
2969.419992	397052.226100	39.708340
2972.188073	397587.806948	39.713357
2975.139740	398125.682873	39.718375
2978.349818	398673.195076	39.723392
2980.896022	399209.570774	39.728410
2983.805715	399770.499863	39.733428
2986.943166	400319.010235	39.738445
2989.589812	400882.649353	39.743463
2991.909476	401455.204168	39.748480
2995.165398	402027.600629	39.753498
2998.426988	402609.772121	39.758516
3001.431382	403186.294763	39.763533
3005.175213	403756.706882	39.768551
3007.832723	404346.623691	39.773568
3011.167248	404918.144305	39.778586
3014.117732	405510.173045	39.783604
3017.265933	406088.216779	39.788621
3020.746349	406667.337894	39.793639
3023.848285	407257.256006	39.798656
3026.924126	407830.234120	39.803674
3029.917868	408415.787121	39.808692
3032.878918	409000.675003	39.813709
3036.033678	409587.751495	39.818727
3039.040196	410188.248354	39.823744
3042.266341	410773.693608	39.828762
3045.480860	411364.933380	39.833780
3048.299847	411953.689499	39.838797
3051.812128	412544.351802	39.843815
3054.612247	413143.681255	39.848832
3057.973378	413735.306677	39.853850
3061.373219	414316.852846	39.858868
3064.442134	414912.454176	39.863885
3068.032862	415494.402769	39.868903
3070.746100	416080.000945	39.873920
3073.881686	416663.011634	39.878938
3076.250430	417266.885606	39.883956
3079.658271	417857.836442	39.888973
3083.217259	418450.170083	39.893991
3086.267289	419051.313748	39.899008
3089.262319	419642.165949	39.904026
3092.059733	420242.513301	39.909044
3094.704328	420850.523775	39.914061
3098.134826	421445.044218	39.919079
3100.772042	422065.697591	39.924096
3103.933670	422675.233094	39.929114
3106.808829	423296.733168	39.934132
3109.459900	423915.569139	39.939149
3112.702968	424534.196073	39.944167
3115.814910	425157.820297	39.949184
3118.933575	425776.413206	39.954202
3122.164642	426368.299443	39.959220
3124.918930	426964.047765	39.964237
3128.060165	427548.170665	39.969255
3130.485752	428138.067960	39.974272
3133.817765	428731.658870	39.979290
3136.613527	429332.945366	39.984308
3139.751597	429944.979303	39.989325
3142.756967	430553.018089	39.994343
3145.499348	431177.597818	39.999360
3148.349564	431808.198590	40.004378
3151.609892	432436.870302	40.009396
3154.343399	433092.201895	40.014413
3157.133688	433738.390786	40.019431
3160.664446	434386.345530	40.024448
3163.938813	435027.613555	40.029466
3167.626753	435683.841808	40.034484
3170.344372	436346.182552	40.039501
3173.587448	437006.928748	40.044519
3176.825744	437688.269551	40.049536
3180.230633	438349.005283	40.054554
3183.636302	439007.444530	40.059572
3186.875162	439686.451617	40.064589
3190.277848	440354.729754	40.069607
3193.712129	441031.947092	40.074624
3196.628143	441696.822350	40.079642
3199.849568	442380.111923	40.084660
3202.609191	443068.720864	40.089677
3206.447455	443748.937570	40.094695
3209.201659	444436.546264	40.099712
3212.216129	445136.700029	40.104730
3215.791283	445840.085781	40.109748
3218.582791	446543.928972	40.114765
3222.326130	447241.526007	40.119783
3225.551472	447943.233910	40.124800
3228.656791	448641.143347	40.129818
3232.343657	449356.757268	40.134836
3235.004810	450061.578328	40.139853
3238.830921	450759.866883	40.144871
3242.090539	451477.709786	40.149888
3245.125518	452192.782140	40.154906
3248.755084	452897.717377	40.159924
3251.790058	453602.977847	40.164941
3255.122946	454323.098168	40.169959
3258.449182	455045.878622	40.174976
3261.643401	455757.169785	40.179994
3265.154306	456466.263001	40.185012
3268.317100	457195.831113	40.190029
3271.747808	457905.144161	40.195047
3275.104637	458629.523965	40.200064
3278.200113	459345.573102	40.205082
3281.652925	460067.815948	40.210100
3284.694955	460797.688639	40.215117
3287.957457	461516.220430	40.220135
3291.410407	462241.831250	40.225152
3294.390964	462953.075202	40.230170
3298.120266	463633.269808	40.235188
3301.091352	464309.971296	40.240205
3304.669993	464972.999337	40.245223
3307.736250	465643.118397	40.250240
3310.630190	466317.340400	40.255258
3313.968351	466994.151233	40.260276
3316.875249	467692.452464	40.265293
3319.916057	468385.854201	40.270311
3323.174469	469086.834898	40.275328
3326.149876	469796.383120	40.280346
3329.047374	470510.015442	40.285364
3332.147205	471243.666134	40.290381
3335.325787	471964.636998	40.295399
3338.473770	472711.930755	40.300416
3341.607497	473467.086989	40.305434
3344.986654	474217.979974	40.310452
3347.869087	474985.405419	40.315469
3351.686405	475744.008897	40.320487
3354.698768	476517.169366	40.325504
3358.025450	477298.338574	40.330522
3361.273155	478078.276502	40.335540
3364.821661	478864.050353	40.340557
3368.483581	479648.359811	40.345575
3372.066353	480431.083740	40.350592
3375.566309	481224.706563	40.355610
3379.413766	482016.523918	40.360628
3382.908827	482804.018591	40.365645
3386.417707	483596.583220	40.370663
3389.905723	484386.238267	40.375680
3393.616114	485161.323306	40.380698
3397.546520	485946.245998	40.385716
3400.934494	486724.653679	40.390733
3404.534121	487512.949539	40.395751
3408.043835	488285.665771	40.400768
3411.233194	489091.138627	40.405786
3414.830961	489866.958995	40.410804
3418.515917	490652.735804	40.415821
3421.701118	491433.406092	40.420839
3425.529059	492210.355669	40.425856
3428.832289	492995.386796	40.430874
3432.307986	493784.145436	40.435892
3435.340985	494573.344322	40.440909
3439.033206	495349.072049	40.445927
3442.843154	496141.817824	40.450944
3445.873325	496938.237813	40.455962
3449.268925	497728.000452	40.460980
3452.609131	498524.251214	40.465997
3455.801853	499324.580013	40.471015
3459.524414	500122.163875	40.476032
3462.660534	500940.404067	40.481050
3466.073489	501742.457919	40.486068
3469.502090	502552.499964	40.491085
3472.373282	503368.145960	40.496103
3475.794039	504177.105082	40.501120
3479.191340	504992.793868	40.506125
3483.268426	505734.469386	40.511130
3486.670668	506441.153172	40.516135
3489.475307	507075.444065	40.521140
3492.486532	507662.521842	40.526144
3495.133425	508200.103452	40.531149
3498.232715	508667.876992	40.536154
3500.745193	509092.978864	40.541159
3502.733188	509435.332937	40.546164
3504.904550	509735.255247	40.551168
3506.437642	509997.936978	40.556173
3508.243223	510208.412898	40.561178
3509.884312	510363.516230	40.566183
3511.251386	510490.938352	40.571188
3512.569988	510573.190903	40.576192
3513.618037	510630.090037	40.581197
3514.836832	510646.895408	40.586202
3515.567629	510632.463182	40.591207
3516.345027	510590.452404	40.596212
3517.235989	510517.159251	40.601216
3517.376228	510446.868046	40.606221
3518.157612	510317.841333	40.611226
3518.807484	510207.755285	40.616231
3519.470158	510061.190494	40.621236
3519.737638	509897.131700	40.626240
3519.923534	509722.864666	40.631245
3520.408835	509534.382658	40.636250
3520.771911	509323.555766	40.641255
3520.950427	509125.353286	40.646260
3521.348919	508900.096403	40.651264
3521.047821	508664.878728	40.656269
3521.280533	508426.638926	40.661274
3521.070359	508181.787098	40.666279
3521.353767	507941.711119	40.671284
3521.359224	507683.662890	40.676288
3521.216205	507432.920483	40.681293
3521.143205	507159.292451	40.686298
3520.924104	506900.762055	40.691303
3521.010041	506636.562895	40.696308
3520.935133	506377.850126	40.701312
3520.662683	506115.369547	40.706317
3520.244072	505848.151407	40.711322
3520.132561	505575.617819	40.716327
3519.954760	505318.423711	40.721332
3520.013283	505050.207068	40.726336
3519.429910	504803.595441	40.731341
3519.401488	504533.613410	40.736346
3519.414843	504285.432583	40.741351
3519.040220	504025.922655	40.746356
3518.820793	503772.963572	40.751360
3518.527166	503524.871138	40.756365
3517.940936	503268.369471	40.761370
3517.659989	503040.613704	40.766375
3517.946396	502806.742506	40.771380
3517.885290	502559.713224	40.776384
3517.249329	502325.424698	40.781389
3517.466216	502090.593374	40.786394
3516.984256	501863.714672	40.791399
3516.599689	501624.669989	40.796404
3516.470442	501402.436882	40.801408
3516.324066	501186.227088	40.806413
3516.355773	500956.117393	40.811418
3515.924019	500754.727707	40.816423
3515.801170	500544.631174	40.821428
3515.709402	500323.188588	40.826432
3515.491482	500129.654635	40.831437
3515.439484	499914.072576	40.836442
3515.110426	499703.239449	40.841447
3514.605797	499511.363995	40.846452
3514.845956	499303.271004	40.851456
3514.476887	499123.013022	40.856461
3514.137958	498923.663597	40.861466
3513.976772	498734.965447	40.866471
3513.886923	498553.645162	40.871476
3513.642446	498356.704489	40.876480
3513.380995	498193.075684	40.881485
3513.117611	498008.334838	40.886490
3513.128926	497845.824167	40.891495
3512.993012	497676.095712	40.896500
3512.913493	497510.761302	40.901504
3512.438750	497332.780351	40.906509
3512.363699	497180.605365	40.911514
3512.237252	497020.893601	40.916519
3512.039673	496861.090417	40.921524
3512.098183	496704.890659	40.926528
3511.446439	496561.965522	40.931533
3511.584272	496393.447548	40.936538
3511.385975	496255.612609	40.941543
3511.209320	496113.773367	40.946548
3511.200800	495967.400266	40.951552
3510.916520	495843.752557	40.956557
3510.662438	495700.605918	40.961562
3510.865805	495565.335148	40.966567
3510.700562	495428.349487	40.971572
3510.838043	495287.568102	40.976576
3510.408367	495178.926287	40.981581
3510.066369	495044.041657	40.986586
3510.076222	494920.442486	40.991591
3510.139036	494796.631574	40.996596
3510.254751	494667.950517	41.001600
3509.773249	494558.756233	41.006605
3509.637225	494435.075578	41.011610
3509.684392	494328.328145	41.016615
3509.788734	494201.063419	41.021620
3509.726104	494087.647968	41.026624
3509.241759	493978.653231	41.031629
3509.406476	493856.389621	41.036634
3509.428865	493752.073345	41.041639
3509.004380	493644.434379	41.046644
3508.838893	493531.234309	41.051648
3508.935768	493440.272926	41.056653
3508.772640	493320.336301	41.061658
3508.744097	493231.824365	41.066663
3508.667678	493130.761078	41.071668
3508.790499	493028.956799	41.076672
3508.475848	492934.260012	41.081677
3508.289549	492832.351587	41.086682
3508.428025	492740.671229	41.091687
3508.218900	492643.930672	41.096692
3508.107755	492553.099085	41.101696
3508.136852	492457.282077	41.106701
3508.145788	492363.544049	41.111706
3507.782283	492294.476144	41.116711
3507.723588	492203.887765	41.121716
3507.759918	492111.663384	41.126720
3507.504754	492035.335600	41.131725
3507.663652	491944.660925	41.136730
3507.662209	491871.077695	41.141735
3507.568517	491792.393836	41.146740
3507.606535	491700.774864	41.151744
3507.317880	491634.072895	41.156749
3507.150763	491552.766182	41.161754
3507.237045	491482.915165	41.166759
3507.147425	491415.775808	41.171764
3507.398872	491332.274940	41.176768
3507.050073	491261.175111	41.181773
3507.275028	491182.387670	41.186778
3507.254061	491109.918697	41.191783
3506.848207	491036.699957	41.196788
3506.839132	490966.456919	41.201792
3506.532686	490912.163200	41.206797
3506.608552	490828.991703	41.211802
3506.503029	490773.298400	41.216807
3506.631246	490717.719925	41.221812
3506.694945	490650.452293	41.226816
3506.557253	490592.889640	41.231821
3506.603181	490524.712736	41.236826
3506.514936	490454.227056	41.241831
3506.538480	490390.864609	41.246836
3506.404902	490323.272455	41.251840
3506.085360	490279.969310	41.256845
3506.161785	490218.725092	41.261850
3506.178415	490154.451292	41.266855
3506.254735	490104.754276	41.271860
3506.366087	490041.832597	41.276864
3506.034004	489992.858250	41.281869
3505.996815	489934.214088	41.286874
3505.853407	489889.109530	41.291879
3505.798630	489831.176897	41.296884
3506.049815	489775.272305	41.301888
3505.684827	489731.873781	41.306893
3505.973547	489667.808553	41.311898
3505.949400	489617.872885	41.316903
3505.466157	489572.719980	41.321908
3505.881814	489518.763934	41.326912
3505.631673	489478.486904	41.331917
3505.383945	489425.699068	41.336922
3505.671251	489382.753783	41.341927
3505.485255	489332.589692	41.346932
3505.703745	489290.161566	41.351936
3505.171731	489249.320802	41.356941
3505.565757	489193.341257	41.361946
3505.769332	489151.371025	41.366951
3505.595944	489106.775827	41.371956
3505.846211	489051.628983	41.376960
3505.554312	489015.156324	41.381965
3505.518572	488970.133846	41.386970
3505.599285	488923.269436	41.391975
3505.542768	488875.565538	41.396980
3505.752004	488835.771687	41.401984
3505.270966	488797.403772	41.406989
3505.560751	488743.110845	41.411994
3505.358366	488701.963541	41.416999
3505.381055	488651.916608	41.422004
3505.871901	488610.558237	41.427008
3505.273127	488570.283716	41.432013
3505.128704	488524.821490	41.437018
3505.257084	488481.646016	41.442023
3505.144444	488439.268314	41.447028
3505.267998	488396.447971	41.452032
3504.925994	488361.248265	41.457037
3505.301487	488322.592054	41.462042
3504.939641	488285.825127	41.467047
3505.106150	488250.038322	41.472052
3505.004370	488203.859452	41.477056
3504.721489	488177.767497	41.482061
3504.981784	488138.419982	41.487066
3504.868599	488117.113122	41.492071
3505.271582	488083.618651	41.497076
3505.388758	488035.277347	41.502080
3504.908354	488004.809570	41.507085
3504.821736	487967.289383	41.512090
3505.165961	487930.460825	41.517095
3504.891370	487894.337838	41.522100
3505.178777	487851.237100	41.527104
3505.204679	487822.259263	41.532109
3505.038228	487775.380421	41.537114
3504.859091	487743.294346	41.542119
3504.912877	487701.800456	41.547124
3504.989169	487675.549735	41.552128
3504.716871	487635.322929	41.557133
3504.934809	487595.626406	41.562138
3504.985498	487567.049494	41.567143
3504.907082	487527.855554	41.572148
3505.256211	487501.308199	41.577152
3504.894230	487471.074118	41.582157
3504.764057	487426.164201	41.587162
3504.771723	487393.186883	41.592167
3504.952211	487358.358625	41.597172
3505.096669	487329.411952	41.602176
3504.781472	487299.778061	41.607181
3504.726254	487265.290815	41.612186
3504.944638	487234.407426	41.617191
3504.644056	487206.037455	41.622196
3504.820606	487164.522989	41.627200
3504.784976	487137.681351	41.632205
3504.814620	487108.093970	41.637210
3504.805681	487080.032304	41.642215
3504.821738	487036.871296	41.647220
3504.773723	486997.164902	41.652224
3504.455063	486978.472677	41.657229
3504.842698	486941.027474	41.662234
3505.011827	486908.226420	41.667239
3504.462949	486876.501255	41.672244
3504.885556	486841.735097	41.677248
3504.941585	486821.514471	41.682253
3504.620021	486774.961614	41.687258
3504.636565	486755.101753	41.692263
3504.537198	486728.674863	41.697268
3504.797695	486687.753967	41.702272
3504.315790	486663.363050	41.707277
3504.686829	486641.572750	41.712282
3504.899391	486598.632975	41.717287
3504.218695	486573.057599	41.722292
3504.348750	486550.748059	41.727296
3504.243789	486523.308631	41.732301
3504.350417	486491.580535	41.737306
3504.282514	486471.885697	41.742311
3504.279302	486447.165559	41.747316
3504.612345	486420.315300	41.752320
3504.306767	486400.151380	41.757325
3504.544826	486369.820712	41.762330
3504.605955	486339.973876	41.767335
3504.214527	486318.303716	41.772340
3504.275975	486287.342283	41.777344
3504.401887	486267.515286	41.782349
3504.640581	486236.221811	41.787354
3504.562363	486204.319822	41.792359
3504.154163	486187.819256	41.797364
3504.547487	486158.831474	41.802368
3504.771434	486126.476335	41.807373
3504.535893	486099.512858	41.812378
3504.599289	486077.618566	41.817383
3504.052542	486036.975836	41.822388
3504.287691	486011.052323	41.827392
3504.031640	485986.067601	41.832397
3504.153723	485971.408053	41.837402
3503.947744	485948.998946	41.842407
3503.942256	485932.789120	41.847412
3504.376005	485894.422727	41.852416
3504.132819	485887.267657	41.857421
3504.486137	485862.591731	41.862426
3504.536022	485839.027565	41.867431
3504.152887	485806.058611	41.872436
3504.455729	485784.480751	41.877440
3504.243570	485761.312517	41.882445
3504.159240	485729.815974	41.887450
3504.261603	485707.712464	41.892455
3503.880210	485695.513257	41.897460
3504.295950	485661.657905	41.902464
3504.417095	485652.216159	41.907469
3504.270050	485616.423307	41.912474
3504.345740	485593.614650	41.917479
3504.254907	485571.338880	41.922484
3504.552578	485539.882968	41.927488
3504.396582	485527.141434	41.932493
3504.116770	485493.243739	41.937498
3504.555921	485469.465616	41.942503
3504.012519	485449.692899	41.947508
3504.271053	485422.498401	41.952512
3504.030200	485399.790203	41.957517
3504.195511	485381.627840	41.962522
3504.542300	485354.824576	41.967527
3504.428562	485341.316339	41.972532
3504.469267	485310.153966	41.977536
3504.244145	485291.445303	41.982541
3504.119712	485261.879417	41.987546
3504.246278	485237.897111	41.992551
3504.166972	485213.339388	41.997556
3504.408120	485184.019564	42.002560
3504.292678	485171.828649	42.007565
3504.288621	485138.899954	42.012570
3504.184550	485108.216080	42.017575
3503.962479	485098.169718	42.022580
3503.947711	485073.246992	42.027584
3503.994000	485058.294762	42.032589
3504.316682	485038.283413	42.037594
3504.439003	485018.202389	42.042599
3504.149749	484992.917653	42.047604
3504.053226	484964.714744	42.052608
3504.081527	484948.549407	42.057613
3504.086741	484914.858947	42.062618
3504.168386	484903.903241	42.067623
3504.048150	484892.016874	42.072628
3504.410702	484870.428551	42.077632
3504.050602	484838.619502	42.082637
3504.125323	484816.012721	42.087642
3504.366847	484798.141730	42.092647
3504.233429	484769.539074	42.097652
3504.467827	484742.854045	42.102656
3504.534917	484718.525861	42.107661
3504.013356	484686.539432	42.112666
3504.353092	484665.359780	42.117671
3504.078945	484653.244281	42.122676
3504.467805	484629.118438	42.127680
3504.141273	484603.383124	42.132685
3504.228852	484585.333619	42.137690
3504.496438	484558.339118	42.142695
3503.874808	484535.639418	42.147700
3504.117057	484508.446202	42.152704
3504.082041	484490.162673	42.157709
3504.008130	484466.920365	42.162714
3504.245160	484450.164334	42.167719
3504.092610	484432.203300	42.172724
3504.412661	484400.995304	42.177728
3504.160620	484377.527728	42.182733
3504.114671	484351.139780	42.187738
3504.348002	484344.415445	42.192743
3504.284035	484311.798780	42.197748
3504.554980	484282.878178	42.202752
3504.459152	484263.742778	42.207757
3504.396333	484238.877229	42.212762
3504.598013	484210.524758	42.217767
3504.343084	484184.473589	42.222772
3504.383455	484153.816027	42.227776
3504.267028	484142.485890	42.232781
3504.396412	484102.846789	42.237786
3504.371607	484077.316401	42.242791
3504.322076	484061.415938	42.247796
3504.361617	484024.425374	42.252800
3504.032826	484006.542463	42.257805
3503.810486	483978.560650	42.262810
3504.143851	483965.132772	42.267815
3503.791620	483958.095543	42.272820
3504.397047	483923.396540	42.277824
3503.910257	483922.865528	42.282829
3503.836507	483886.095260	42.287834
3503.972619	483872.951814	42.292839
3503.533845	483855.339465	42.297844
3504.020805	483839.455355	42.302848
3503.990963	483828.516660	42.307853
3503.773457	483791.312956	42.312858
3504.179352	483788.816941	42.317863
3503.812349	483768.102656	42.322868
3503.932476	483757.038890	42.327872
3503.875667	483735.718238	42.332877
3503.983375	483714.371560	42.337882
3504.282746	483707.535238	42.342887
3504.194495	483676.289276	42.347892
3504.220167	483647.659812	42.352896
3504.080681	483627.618721	42.357901
3504.478002	483611.545934	42.362906
3504.300015	483594.804092	42.367911
3504.092012	483557.750431	42.372916
3504.174985	483535.292841	42.377920
3504.070143	483510.838315	42.382925
3504.116985	483494.415506	42.387930
3504.187537	483464.208065	42.392935
3504.109468	483441.573160	42.397940
3504.028071	483423.346617	42.402944
3504.037244	483414.022804	42.407949
3504.227814	483389.217444	42.412954
3504.471983	483362.275640	42.417959
3504.015688	483345.273577	42.422964
3504.034108	483321.305983	42.427968
3504.289509	483305.812693	42.432973
3504.257908	483279.826338	42.437978
3504.573806	483262.499495	42.442983
3504.176650	483250.149228	42.447988
3504.030745	483216.429024	42.452992
3504.399394	483191.291272	42.457997
3504.040844	483170.423013	42.463002
3504.485992	483141.979833	42.468007
3504.177101	483116.087750	42.473012
3504.316629	483091.442074	42.478016
3504.106751	483062.291649	42.483021
3504.208257	483048.443790	42.488026
3504.465087	483021.296848	42.493031
3504.166369	482993.275016	42.498036
3504.361130	482970.343108	42.503040
3504.197767	482943.465134	42.508045
3504.008290	482926.420532	42.513050
3504.040553	482907.415545	42.518055
3504.217370	482891.427680	42.523060
3504.336983	482854.574227	42.528064
3503.805794	482840.978218	42.533069
3504.039307	482813.733339	42.538074
3504.109667	482795.836887	42.543079
3503.944056	482781.220388	42.548084
3503.789898	482751.148687	42.553088
3503.780301	482738.635505	42.558093
3503.865673	482723.928628	42.563098
3504.059870	482695.524458	42.568103
3503.721098	482694.666011	42.573108
3504.202939	482665.658998	42.578112
3504.081612	482664.918183	42.583117
3503.908119	482627.451954	42.588122
3503.960875	482608.392767	42.593127
3504.064440	482589.528202	42.598132
3504.112125	482561.704333	42.603136
3504.121146	482555.774843	42.608141
3504.029112	482535.319784	42.613146
3504.078464	482513.829007	42.618151
3503.882155	482498.913143	42.623156
3503.839094	482476.372914	42.628160
3503.878089	482456.657076	42.633165
3503.443727	482439.954757	42.638170
3503.755490	482432.052010	42.643175
3503.771404	482410.617072	42.648180
3503.812109	482381.983366	42.653184
3503.660928	482390.418129	42.658189
3503.780099	482363.089356	42.663194
3504.174329	482344.735959	42.668199
3503.827710	482340.585322	42.673204
3503.775869	482311.104784	42.678208
3504.050105	482301.231864	42.683213
3503.736752	482281.470201	42.688218
3504.113427	482265.044891	42.693223
3503.891972	482241.417887	42.698228
3504.016888	482215.506707	42.703232
3503.758276	482206.427312	42.708237
3503.964776	482186.583390	42.713242
3503.965675	482164.491867	42.718247
3503.987607	482157.344174	42.723252
3504.108166	482127.278758	42.728256
3503.776808	482108.229124	42.733261
3503.954604	482079.370632	42.738266
3504.092918	482070.481781	42.743271
3503.960454	482043.597680	42.748276
3504.121033	482033.235902	42.753280
3503.802267	482016.616286	42.758285
3503.819484	481994.471322	42.763290
3504.074584	481978.166324	42.768295
3503.617941	481963.595208	42.773300
3503.736135	481945.335733	42.778304
3503.836135	481935.034146	42.783309
3503.970799	481915.859999	42.788314
3503.855782	481898.600052	42.793319
3503.901444	481874.474363	42.798324
3503.857678	481858.064493	42.803329
3503.798521	481851.689542	42.808333
3503.854504	481828.372872	42.813338
3503.733606	481813.697910	42.818343
3503.685347	481797.136691	42.823348
3503.669760	481776.618083	42.828353
3503.957585	481773.988469	42.833357
3503.874731	481742.789215	42.838362
3503.811639	481728.459738	42.843367
3503.684688	481721.690104	42.848372
3503.753599	481699.029940	42.853377
3503.695514	481688.499861	42.858381
3503.727867	481682.009052	42.863386
3504.190541	481644.085697	42.868391
3503.649675	481644.525885	42.873396
3503.797621	481619.775679	42.878401
3504.008124	481606.517606	42.883405
3503.883071	481587.384186	42.888410
3503.924255	481566.248347	42.893415
3503.729633	481553.206278	42.898420
3504.034324	481533.244834	42.903425
3503.879758	481515.180078	42.908429
3503.710436	481507.454335	42.913434
3504.000818	481481.972062	42.918439
3503.458096	481484.591362	42.923444
3503.535686	481469.023377	42.928449
3503.592071	481445.098144	42.933453
3503.528232	481426.208242	42.938458
3503.633604	481421.681947	42.943463
3503.536746	481421.190568	42.948468
3504.082072	481390.246159	42.953473
3503.824490	481370.120065	42.958477
3503.602319	481366.557594	42.963482
3504.043270	481340.037929	42.968487
3503.934457	481334.886750	42.973492
3503.955192	481301.086222	42.978497
3503.851658	481294.262068	42.983501
3503.775141	481274.968659	42.988506
3503.948199	481260.246820	42.993511
3503.931151	481230.556470	42.998516
3503.897787	481217.995398	43.003521
3503.990676	481202.019416	43.008525
3503.667802	481186.565172	43.013530
3503.865188	481160.286444	43.018535
3503.775844	481162.327419	43.023540
3503.908884	481147.510479	43.028545
3503.836389	481132.878027	43.033549
3504.016835	481110.756935	43.038554
3504.327803	481095.202439	43.043559
3503.817548	481080.892491	43.048564
3503.848705	481046.481823	43.053569
3504.079949	481037.223117	43.058573
3503.856553	481020.334222	43.063578
3503.988170	480989.961283	43.068583
3503.664122	480980.080915	43.073588
3503.880046	480954.812411	43.078593
3503.876014	480939.560935	43.083597
3503.874498	480929.984266	43.088602
3503.963012	480893.436057	43.093607
3503.521304	480898.623722	43.098612
3503.833177	480877.900402	43.103617
3504.258111	480850.977236	43.108621
3503.823575	480847.194875	43.113626
3504.103043	480810.413644	43.118631
3503.725681	480802.872520	43.123636
3503.732138	480786.909861	43.128641
3503.962018	480769.594405	43.133645
3504.049617	480748.349004	43.138650
3503.739025	480727.571891	43.143655
3503.705392	480716.682719	43.148660
3503.883279	480700.338191	43.153665
3503.841302	480681.849493	43.158669
3503.997352	480672.653173	43.163674
3504.025948	480646.552452	43.168679
3503.852674	480631.530175	43.173684
3504.257331	480606.231393	43.178689
3503.887256	480592.709691	43.183693
3503.905056	480574.110099	43.188698
3503.964868	480546.889518	43.193703
3503.421547	480532.077669	43.198708
3503.714383	480506.036343	43.203713
3504.009429	480494.993755	43.208717
3503.748048	480485.052560	43.213722
3503.736408	480459.819386	43.218727
3503.659301	480448.379537	43.223732
3503.695332	480438.847367	43.228737
3503.515408	480427.575774	43.233741
3503.981732	480417.012801	43.238746
3504.106513	480392.568746	43.243751
3503.865933	480374.516532	43.248756
3503.796030	480356.589346	43.253761
3504.037399	480342.109389	43.258765
3503.643579	480324.081349	43.263770
3503.772204	480315.953332	43.268775
3503.635628	480296.567107	43.273780
3504.007147	480272.134579	43.278785
3503.866582	480268.913721	43.283789
3504.029445	480242.436530	43.288794
3504.256900	480229.428217	43.293799
3503.621217	480214.123991	43.298804
3503.485844	480195.446904	43.303809
3503.532778	480189.003971	43.308813
3503.546387	480150.185913	43.313818
3503.907024	480135.281565	43.318823
3503.866085	480133.565148	43.323828
3504.095180	480116.806653	43.328833
3503.732874	480102.269911	43.333837
3503.518532	480085.581474	43.338842
3503.897113	480063.731933	43.343847
3503.849932	480057.557200	43.348852
3503.919526	480037.023310	43.353857
3503.562225	480010.475999	43.358861
3503.633658	480008.032375	43.363866
3503.721256	479988.053001	43.368871
3503.587700	479973.581357	43.373876
3503.303226	479958.778837	43.378881
3503.525159	479956.666139	43.383885
3503.797593	479941.927608	43.388890
3503.663576	479919.297463	43.393895
3503.422529	479921.565240	43.398900
3503.656356	479897.001987	43.403905
3503.728677	479871.704116	43.408909
3503.540720	479880.196443	43.413914
3503.860160	479857.494558	43.418919
3503.399424	479831.419422	43.423924
3503.667973	479827.627087	43.428929
3503.779701	479813.471279	43.433933
3503.601180	479802.604501	43.438938
3503.590904	479784.160624	43.443943
3503.617166	479791.960363	43.448948
3503.529724	479758.224954	43.453953
3503.758755	479737.766902	43.458957
3503.438107	479739.185812	43.463962
3503.726222	479726.623651	43.468967
3503.373023	479709.044699	43.473972
3503.989891	479703.170299	43.478977
3503.909474	479696.747333	43.483981
3503.683086	479685.026585	43.488986
3503.487559	479660.074825	43.493991
3503.273197	479667.456571	43.498996
3503.546942	479643.140067	43.504001
3503.600581	479628.435884	43.509005
3503.450974	479614.878662	43.514010
3503.526160	479617.501892	43.519015
3503.737605	479595.222174	43.524020
3503.592048	479571.731979	43.529025
3503.429314	479576.166444	43.534029
3503.407676	479563.551788	43.539034
3503.966913	479550.743964	43.544039
3503.817223	479536.679951	43.549044
3503.308858	479525.206375	43.554049
3503.431662	479507.552010	43.559053
3503.793677	479481.701100	43.564058
3503.881407	479483.663585	43.569063
3503.608168	479456.899540	43.574068
3503.827574	479440.902134	43.579073
3504.183999	479429.849251	43.584077
3503.720619	479410.311104	43.589082
3503.943188	479387.623990	43.594087
3503.410607	479393.231814	43.599092
3503.443134	479360.540950	43.604097
3503.509090	479356.273789	43.609101
3503.361731	479350.063993	43.614106
3503.450376	479355.066885	43.619111
3503.344509	479325.843778	43.624116
3503.482037	479316.244349	43.629121
3503.708840	479302.323365	43.634125
3503.667139	479294.171173	43.639130
3503.940018	479267.371232	43.644135
3503.722952	479254.179155	43.649140
3503.560407	479252.633909	43.654145
3503.656637	479218.311113	43.659149
3503.892886	479212.851459	43.664154
3503.982076	479206.908287	43.669159
3503.405022	479190.073716	43.674164
3503.668594	479166.619728	43.679169
3503.740105	479169.750359	43.684173
3503.530343	479151.185392	43.689178
3503.578159	479130.755355	43.694183
3503.555652	479136.536012	43.699188
3503.583230	479110.078686	43.704193
3503.785225	479102.749394	43.709197
3503.720782	479088.570236	43.714202
3503.727195	479066.981121	43.719207
3503.310944	479053.212275	43.724212
3503.689115	479039.571242	43.729217
3503.706021	479031.815090	43.734221
3503.385506	479017.220265	43.739226
3503.697557	479000.650419	43.744231
3503.764554	478991.011303	43.749236
3503.807066	478980.514550	43.754241
3503.833184	478961.962801	43.759245
3503.396504	478950.680267	43.764250
3503.562749	478951.971600	43.769255
3503.637094	478924.239717	43.774260
3503.468734	478908.100461	43.779265
3503.571466	478905.043634	43.784269
3503.271156	478895.259817	43.789274
3503.700745	478870.765704	43.794279
3503.324944	478860.233649	43.799284
3503.596730	478859.126494	43.804289
3504.067986	478857.531719	43.809293
3503.882883	478831.969143	43.814298
3503.883568	478809.569822	43.819303
3503.646764	478793.390613	43.824308
3503.589843	478771.608479	43.829313
3503.820841	478772.838912	43.834317
3503.655713	478747.374424	43.839322
3503.414204	478726.939021	43.844327
3503.308583	478721.381234	43.849332
3503.299358	478724.119278	43.854337
3503.709255	478699.729421	43.859341
3503.525626	478687.747937	43.864346
3503.635767	478674.098338	43.869351
3503.642114	478669.688420	43.874356
3503.722124	478656.144926	43.879361
3503.740363	478633.083825	43.884365
3503.478384	478641.132284	43.889370
3503.659545	478605.274680	43.894375
3503.442839	478601.660163	43.899380
3503.456494	478586.809494	43.904385
3503.665930	478587.181828	43.909389
3503.290385	478571.835208	43.914394
3503.629365	478548.621959	43.919399
3503.423865	478563.452332	43.924404
3503.255908	478546.704586	43.929409
3503.538103	478522.233339	43.934413
3503.373805	478503.103124	43.939418
3502.997004	478509.902839	43.944423
3503.326921	478514.969166	43.949428
3503.316878	478498.703198	43.954433
3503.489393	478492.391898	43.959437
3503.209815	478478.398338	43.964442
3503.739991	478461.540179	43.969447
3503.360906	478462.309600	43.974452
3503.332987	478469.966390	43.979457
3503.562264	478435.215787	43.984461
3503.248244	478424.065599	43.989466
3503.362823	478415.077497	43.994471
3503.224012	478413.629789	43.999476
3503.367916	478408.285866	44.004481
3503.167315	478400.513167	44.009485
3503.087793	478383.244525	44.014490
3503.573248	478377.846612	44.019495
3503.209047	478375.674352	44.024500
3503.114719	478386.534392	44.029505
3503.461434	478361.089866	44.034509
3503.414676	478366.925259	44.039514
3503.160967	478337.774740	44.044519
3503.390189	478325.879819	44.049524
3503.515012	478327.937914	44.054529
3503.564507	478315.716646	44.059533
3503.378692	478320.965891	44.064538
3503.855197	478295.602125	44.069543
3503.460146	478295.259152	44.074548
3503.473326	478288.719579	44.079553
3503.527940	478267.476724	44.084557
3503.367192	478257.518499	44.089562
3503.299403	478249.674071	44.094567
3503.183649	478239.860761	44.099572
3503.377723	478235.674467	44.104577
3503.647997	478224.837246	44.109581
3503.265881	478217.549270	44.114586
3503.333835	478202.030910	44.119591
3503.043633	478207.296684	44.124596
3502.761523	478205.364824	44.129601
3503.356601	478205.929607	44.134605
3503.031850	478204.713986	44.139610
3503.237306	478174.426406	44.144615
3503.239925	478155.421509	44.149620
3503.651534	478157.535652	44.154625
3503.508642	478145.192650	44.159629
3503.260387	478159.016507	44.164634
3503.517417	478130.291747	44.169639
3503.429144	478130.711144	44.174644
3503.374150	478121.192245	44.179649
3503.184937	478116.407681	44.184653
3503.058398	478119.772496	44.189658
3503.618018	478103.213453	44.194663
3503.464478	478082.966198	44.199668
3503.267416	478077.422683	44.204673
3503.603630	478064.091687	44.209677
3503.311257	478070.118024	44.214682
3503.545847	478033.642798	44.219687
3503.280841	478029.833094	44.224692
3503.461151	478027.524056	44.229697
3503.680132	478019.127422	44.234701
3503.332763	478003.471834	44.239706
3503.729832	477980.806213	44.244711
3503.459635	477989.920495	44.249716
3503.656276	477973.621431	44.254721
3503.598470	477953.815026	44.259725
3503.548845	477953.873564	44.264730
3503.401252	477932.206198	44.269735
3503.574525	477936.131809	44.274740
3503.512365	477910.903370	44.279745
3503.444694	477902.247917	44.284749
3503.336970	477896.082079	44.289754
3503.499142	477876.342188	44.294759
3503.445129	477872.296388	44.299764
3503.622986	477850.932251	44.304769
3503.863483	477837.768271	44.309773
3503.412473	477829.224054	44.314778
3503.472269	477803.925524	44.319783
3503.582511	477807.202288	44.324788
3503.715827	477800.187450	44.329793
3503.723564	477774.694393	44.334797
3503.353640	477767.911122	44.339802
3503.568981	477757.437087	44.344807
3503.588887	477756.521721	44.349812
3503.515999	477737.427001	44.354817
3503.479414	477724.053340	44.359821
3503.229281	477711.625659	44.364826
3503.629808	477703.960397	44.369831
3503.692271	477684.742873	44.374836
3503.720148	477678.707576	44.379841
3503.664486	477670.202164	44.384845
3503.605642	477651.966700	44.389850
3503.896340	477626.631451	44.394855
3503.861439	477634.745786	44.399860
3503.631281	477604.070069	44.404865
3503.692503	477589.261817	44.409869
3503.600854	477592.266445	44.414874
3503.339203	477573.252081	44.419879
3503.448165	477551.898514	44.424884
3503.656025	477541.374868	44.429889
3503.450295	477535.680531	44.434893
3503.246498	477517.569215	44.439898
3503.317602	477508.030092	44.444903
3503.262133	477506.822546	44.449908
3503.117442	477507.960398	44.454913
3503.248472	477498.715881	44.459917
3503.262224	477504.592643	44.464922
3503.582527	477485.638257	44.469927
3503.392876	477468.234186	44.474932
3503.294461	477456.187810	44.479937
3503.524616	477463.753517	44.484941
3503.106990	477459.663742	44.489946
3503.533655	477435.168328	44.494951
3503.252872	477425.532741	44.499956
3503.442019	477420.586848	44.504961
3503.363977	477411.831460	44.509965
3503.252302	477415.447446	44.514970
3503.552039	477402.983345	44.519975
3503.386177	477379.899209	44.524980
3503.181082	477357.429416	44.529985
3503.212895	477356.816234	44.534989
3503.066094	477363.681347	44.539994
3503.735857	477350.398519	44.544999
3503.614434	477331.463123	44.550004
3503.437112	477327.639425	44.555009
3503.703226	477317.410539	44.560013
3503.461863	477303.714197	44.565018
3503.446971	477293.529712	44.570023
3503.423294	477284.005463	44.575028
3503.523719	477281.911689	44.580033
3503.344706	477265.468696	44.585037
3503.222760	477251.753444	44.590042
3502.971014	477233.548087	44.595047
3503.352307	477235.413717	44.600052
3503.210786	477239.338538	44.605057
3503.640828	477228.070077	44.610061
3502.974937	477237.044518	44.615066
3503.072315	477207.938217	44.620071
3503.280894	477195.691118	44.625076
3503.269988	477191.486324	44.630081
3503.671585	477182.198897	44.635085
3503.172273	477194.339942	44.640090
3502.954671	477187.025585	44.645095
3503.069002	477191.062021	44.650100
3503.109083	477174.128195	44.655105
3503.517511	477146.898527	44.660109
3503.203614	477149.482216	44.665114
3503.254994	477140.098079	44.670119
3503.299159	477147.338534	44.675124
3503.271431	477146.481350	44.680129
3503.233437	477123.224664	44.685133
3503.090454	477119.243454	44.690138
3503.497311	477094.395985	44.695143
3503.514810	477094.595960	44.700148
3503.070967	477104.295586	44.705153
3503.554863	477101.887777	44.710157
3503.370646	477078.147336	44.715162
3503.402513	477074.290526	44.720167
3503.239954	477055.057281	44.725172
3503.337265	477061.478463	44.730177
3503.656395	477045.564734	44.735181
3503.608675	477028.188528	44.740186
3503.553151	477015.678973	44.745191
3503.407531	477009.366805	44.750196
3503.362599	477010.539599	44.755201
3503.500555	476989.535619	44.760205
3503.567662	476969.607132	44.765210
3503.541287	476968.597681	44.770215
3503.585696	476965.347049	44.775220
3503.526720	476930.233931	44.780225
3503.650880	476926.970688	44.785229
3503.307911	476923.629229	44.790234
3503.537500	476911.175909	44.795239
3503.192890	476895.772422	44.800244
3503.168598	476882.751028	44.805249
3503.672122	476876.538947	44.810253
3503.282641	476888.003953	44.815258
3503.417307	476883.370630	44.820263
3503.093289	476851.948363	44.825268
3503.591337	476843.912586	44.830273
3503.336023	476835.539738	44.835277
3503.212144	476851.321439	44.840282
3503.091704	476852.404813	44.845287
3503.486239	476839.266512	44.850292
3503.271587	476821.156280	44.855297
3503.364340	476809.180663	44.860301
3503.263599	476801.290190	44.865306
3503.552116	476801.396651	44.870311
3503.678394	476784.803647	44.875316
3503.413640	476762.900118	44.880321
3503.626440	476755.010754	44.885325
3503.168822	476760.911554	44.890330
3503.462214	476746.674170	44.895335
3503.441843	476737.199820	44.900340
3503.437067	476716.116748	44.905345
3503.669755	476711.619940	44.910349
3503.055962	476715.670190	44.915354
3503.832220	476696.642994	44.920359
3503.691968	476684.095941	44.925364
3503.382648	476668.990796	44.930369
3503.764118	476660.466546	44.935373
3503.631322	476641.684342	44.940378
3503.538615	476633.640486	44.945383
3503.543384	476620.867742	44.950388
3503.365993	476603.866441	44.955393
3503.482961	476593.153933	44.960397
3503.224808	476585.288255	44.965402
3503.426639	476573.143209	44.970407
3503.429846	476585.509292	44.975412
3503.508877	476566.490807	44.980417
3503.574568	476543.014328	44.985421
3503.476898	476538.062868	44.990426
3503.652557	476525.719198	44.995431
3503.548294	476517.474391	45.000436
3503.441894	476490.325202	45.005441
3503.726170	476489.266629	45.010445
3503.405655	476479.738230	45.015450
3503.711402	476452.473166	45.020455
3503.291672	476450.309468	45.025460
3503.256124	476436.630685	45.030465
3503.671981	476429.773443	45.035469
3503.449281	476409.940887	45.040474
3503.404217	476408.782313	45.045479
3503.485494	476398.379441	45.050484
3503.541521	476401.563639	45.055489
3503.495917	476373.391020	45.060493
3503.198118	476362.338478	45.065498
3503.876497	476349.915245	45.070503
3503.265761	476353.762350	45.075508
3503.406041	476329.868367	45.080513
3503.380762	476318.975462	45.085517
3503.324584	476309.354519	45.090522
3503.391720	476310.256224	45.095527
3503.409063	476299.305888	45.100532
3503.439244	476277.760680	45.105537
3503.431128	476273.757986	45.110541
3503.296283	476265.669959	45.115546
3503.499141	476262.090069	45.120551
3503.668250	476253.345794	45.125556
3503.470222	476229.657213	45.130561
3503.753949	476210.453987	45.135565
3503.621389	476221.676030	45.140570
3503.736116	476198.546183	45.145575
3503.458004	476191.190341	45.150580
3503.523524	476187.581460	45.155585
3503.544430	476171.866226	45.160589
3503.263314	476146.923587	45.165594
3503.399986	476140.515844	45.170599
3503.392065	476141.277368	45.175604
3503.110330	476133.719342	45.180609
3503.299209	476129.178645	45.185613
3503.160800	476111.309140	45.190618
3503.288526	476099.479623	45.195623
3503.321966	476091.973135	45.200628
3503.414623	476092.161242	45.205633
3503.628043	476097.246600	45.210637
3503.324175	476076.412864	45.215642
3503.272800	476057.617244	45.220647
3503.676551	476046.960486	45.225652
3503.305508	476043.775368	45.230657
3503.608842	476041.041186	45.235661
3503.307458	476024.667199	45.240666
3503.240623	476016.010798	45.245671
3503.504616	476004.565161	45.250676
3503.209220	475996.198297	45.255681
3503.357464	475991.866728	45.260685
3503.326423	475981.481392	45.265690
3503.126372	475960.225654	45.270695
3503.450505	475951.912905	45.275700
3503.426638	475964.182281	45.280705
3503.284575	475960.707538	45.285709
3503.144581	475942.077868	45.290714
3503.327291	475926.640975	45.295719
3503.057757	475910.718020	45.300724
3502.980803	475916.761638	45.305729
3503.598064	475909.010754	45.310733
3503.275896	475915.904078	45.315738
3503.437873	475907.211465	45.320743
3503.526489	475890.116831	45.325748
3503.179729	475872.280044	45.330753
3503.299280	475867.142032	45.335757
3503.044917	475861.759009	45.340762
3502.953726	475875.458247	45.345767
3503.298401	475866.381949	45.350772
3503.001345	475864.959065	45.355777
3503.396682	475850.603566	45.360781
3503.114105	475833.567552	45.365786
3503.256221	475827.767064	45.370791
3503.388697	475824.553012	45.375796
3503.178218	475827.323262	45.380801
3503.357264	475818.070382	45.385805
3503.362172	475817.106614	45.390810
3503.356234	475788.926907	45.395815
3503.469743	475780.292585	45.400820
3503.217413	475779.420157	45.405825
3503.655618	475770.329033	45.410829
3503.429930	475766.411310	45.415834
3503.553259	475742.265885	45.420839
3503.692021	475733.323443	45.425844
3503.377883	475728.051202	45.430849
3503.513843	475698.683190	45.435853
3503.486034	475696.051985	45.440858
3503.583605	475692.590005	45.445863
3503.434773	475692.410803	45.450868
3503.191686	475668.677997	45.455873
3503.491330	475647.495005	45.460877
3503.479653	475646.990016	45.465882
3503.416128	475651.663094	45.470887
3503.659469	475632.921866	45.475892
3503.125878	475622.362349	45.480897
3503.313125	475596.888835	45.485901
3503.121502	475599.554765	45.490906
3503.540198	475590.922811	45.495911
3503.634317	475581.936672	45.500916
3503.354300	475560.389039	45.505921
3503.521121	475551.948934	45.510925
3503.611248	475559.132012	45.515930
3503.487490	475538.674734	45.520935
3503.280908	475519.092176	45.525940
3503.470415	475505.377189	45.530945
3503.495182	475502.788334	45.535949
3503.456214	475501.882171	45.540954
3503.298913	475487.968559	45.545959
3503.413299	475487.494326	45.550964
3503.457877	475465.641861	45.555969
3503.714383	475459.214962	45.560973
3503.199480	475465.885474	45.565978
3503.217512	475436.180920	45.570983
3503.178583	475430.155504	45.575988
3503.153832	475426.053899	45.580993
3503.305744	475427.550472	45.585997
3503.080012	475433.820491	45.591002
3503.384244	475417.705089	45.596007
3503.566276	475412.151601	45.601012
3502.981556	475391.767030	45.606017
3503.144428	475373.494451	45.611021
3503.104553	475377.758369	45.616026
3502.986402	475378.537344	45.621031
3503.359253	475369.152256	45.626036
3503.242472	475384.933986	45.631041
3503.179416	475373.083512	45.636045
3502.992966	475363.482706	45.641050
3503.183979	475346.219369	45.646055
3503.350495	475340.769686	45.651060
3502.855191	475341.152100	45.656065
3503.189247	475329.188150	45.661069
3502.941423	475331.609568	45.666074
3503.307581	475333.629830	45.671079
3503.504965	475325.691658	45.676084
3503.133172	475321.746254	45.681089
3503.330569	475301.136604	45.686093
3502.810358	475305.729885	45.691098
3503.466839	475291.687516	45.696103
3503.392662	475293.523948	45.701108
3503.103585	475296.458751	45.706113
3503.593248	475285.940072	45.711117
3503.233151	475261.110188	45.716122
3503.222915	475255.891162	45.721127
3503.406206	475244.001676	45.726132
3503.086900	475247.194693	45.731137
3503.491577	475243.988213	45.736141
3503.276268	475233.834361	45.741146
3503.121232	475210.796703	45.746151
3503.109237	475194.325615	45.751156
3502.894742	475204.446078	45.756161
3503.248606	475191.566564	45.761165
3503.216038	475203.736406	45.766170
3503.222668	475200.795577	45.771175
3503.061297	475198.742965	45.776180
3503.059142	475195.195289	45.781185
3503.303018	475191.456668	45.786189
3503.246249	475172.610388	45.791194
3503.323875	475155.719614	45.796199
3503.399080	475153.883037	45.801204
3503.172135	475155.034020	45.806209
3503.485957	475150.321297	45.811213
3503.435271	475128.584896	45.816218
3503.216760	475113.160109	45.821223
3502.993167	475119.987437	45.826228
3503.151619	475110.940234	45.831233
3503.275953	475099.820277	45.836237
3502.937993	475117.360512	45.841242
3503.222442	475108.445453	45.846247
3503.723228	475097.519428	45.851252
3503.137889	475078.705916	45.856257
3503.260275	475062.314854	45.861261
3503.659202	475064.025845	45.866266
3503.449703	475055.188833	45.871271
3503.277584	475045.382864	45.876276
3503.367399	475031.531252	45.881281
3503.425986	475014.389936	45.886285
3503.436981	475021.281593	45.891290
3503.342981	475005.076745	45.896295
3503.132919	474993.299969	45.901300
3503.138721	474982.756235	45.906305
3503.486434	474975.402407	45.911309
3503.022379	474975.881261	45.916314
3503.151346	474974.188231	45.921319
3503.249996	474976.048063	45.926324
3502.764747	474976.378207	45.931329
3503.388972	474966.294275	45.936333
3503.042335	474959.658426	45.941338
3502.897462	474944.627365	45.946343
3503.274979	474928.804112	45.951348
3503.036467	474938.624382	45.956353
3503.252429	474924.043143	45.961357
3503.405956	474930.050628	45.966362
3503.091813	474931.114031	45.971367
3503.011196	474926.260851	45.976372
3502.995034	474949.630043	45.981377
3503.381189	474914.392365	45.986381
3503.254981	474906.505174	45.991386
3503.247547	474888.816630	45.996391
3503.571639	474885.622831	46.001396
3503.105327	474887.622652	46.006401
3503.354853	474879.118508	46.011405
3503.610906	474874.009357	46.016410
3503.472222	474849.600154	46.021415
3503.685782	474848.147178	46.026420
3503.622501	474843.595361	46.031425
3503.549618	474806.149130	46.036429
3503.412883	474802.825405	46.041434
3503.346463	474796.702771	46.046439
3503.624049	474787.433846	46.051444
3503.258755	474781.865318	46.056449
3503.304398	474764.725836	46.061453
3503.150927	474762.722618	46.066458
3503.181386	474763.528815	46.071463
3503.294070	474744.756728	46.076468
3503.329904	474748.806063	46.081473
3503.599782	474715.157723	46.086477
3503.372900	474704.194434	46.091482
3503.142754	474700.074457	46.096487
3503.414594	474690.654334	46.101492
3503.332537	474689.248070	46.106497
3503.466410	474675.693376	46.111501
3503.314145	474654.783520	46.116506
3503.329033	474644.390237	46.121511
3503.571177	474651.498924	46.126516
3503.245111	474650.384662	46.131521
3503.329783	474635.469153	46.136525
3502.883406	474629.406523	46.141530
3503.088494	474615.485719	46.146535
3502.826708	474618.821806	46.151540
3503.320196	474621.480955	46.156545
3503.175535	474611.822499	46.161549
3503.015781	474627.560923	46.166554
3503.148716	474616.692780	46.171559
3503.233872	474617.490338	46.176564
3502.897160	474608.470486	46.181569
3503.066429	474589.993438	46.186573
3502.961610	474587.019446	46.191578
3502.991857	474582.452788	46.196583
3503.351619	474567.595126	46.201588
3502.798753	474578.022821	46.206593
3503.245569	474572.325878	46.211597
3503.058370	474576.511874	46.216602
3503.173474	474575.581318	46.221607
3503.145821	474568.286670	46.226612
3503.286609	474568.923374	46.231617
3503.310372	474553.307803	46.236621
3503.359992	474533.937235	46.241626
3503.256508	474532.737099	46.246631
3503.403420	474538.644369	46.251636
3503.323453	474535.970569	46.256641
3503.190805	474521.393452	46.261645
3503.313328	474500.997572	46.266650
3503.151022	474499.097100	46.271655
3503.134311	474488.505980	46.276660
3503.037808	474486.848545	46.281665
3503.235358	474494.471215	46.286669
3503.280068	474490.763945	46.291674
3503.153976	474483.332762	46.296679
3503.385626	474479.139751	46.301684
3503.046066	474462.415712	46.306689
3503.198537	474440.291646	46.311693
3502.954437	474445.297671	46.316698
3502.944146	474444.589681	46.321703
3503.060201	474444.115160	46.326708
3502.701706	474454.816325	46.331713
3503.290073	474442.760969	46.336717
3503.207908	474449.109977	46.341722
3502.737644	474431.798314	46.346727
3503.375315	474434.231947	46.351732
3503.254956	474438.356719	46.356737
3503.490097	474418.753967	46.361741
3503.119721	474403.808834	46.366746
3503.196484	474397.714137	46.371751
3503.376415	474403.565540	46.376756
3503.136542	474406.594069	46.381761
3503.153501	474396.859277	46.386765
3503.027513	474370.926846	46.391770
3502.974327	474359.935917	46.396775
3503.122673	474352.917505	46.401780
3503.101844	474351.096034	46.406785
3502.959589	474340.321925	46.411789
3503.155535	474347.843528	46.416794
3503.155515	474347.387351	46.421799
3503.486757	474342.215494	46.426804
3503.439634	474346.075268	46.431809
3503.320705	474325.261180	46.436813
3503.355340	474310.251964	46.441818
3503.395715	474315.010306	46.446823
3503.382012	474303.658288	46.451828
3503.172665	474309.773999	46.456833
3503.586443	474291.511475	46.461837
3503.601867	474280.306906	46.466842
3503.219583	474265.059421	46.471847
3503.488249	474256.653369	46.476852
3503.421819	474260.668277	46.481857
3503.182273	474239.163524	46.486861
3503.063307	474236.749291	46.491866
3503.164124	474227.102542	46.496871
3503.141574	474225.990972	46.501876
3503.241325	474228.712405	46.506881
3503.329609	474225.403708	46.511885
3503.238153	474221.160336	46.516890
3503.374508	474197.517894	46.521895
3503.335192	474179.428261	46.526900
3503.011998	474180.290377	46.531905
3503.392229	474171.106325	46.536909
3503.315105	474165.390703	46.541914
3503.124860	474175.457156	46.546919
3503.246922	474149.434548	46.551924
3503.245895	474138.485944	46.556929
3503.276003	474139.190844	46.561933
3503.372064	474125.996581	46.566938
3502.951734	474127.279563	46.571943
3503.577464	474129.461677	46.576948
3503.225398	474125.360852	46.581953
3503.209844	474095.304817	46.586957
3503.229407	474086.684621	46.591962
3503.234869	474082.983480	46.596967
3503.430006	474082.243008	46.601972
3503.274408	474085.359642	46.606977
3503.504832	474071.637217	46.611981
3503.437460	474051.777790	46.616986
3503.441877	474055.984296	46.621991
3503.450922	474044.324404	46.626996
3503.309672	474061.124813	46.632001
3503.218887	474024.237545	46.637005
3503.242934	474007.557038	46.642010
3503.393384	474001.146442	46.647015
3503.651480	473990.410249	46.652020
3503.276983	474002.584166	46.657025
3503.441113	473979.241216	46.662029
3503.208976	473978.771029	46.667034
3503.298244	473961.319838	46.672039
3503.850879	473957.228055	46.677044
3503.392949	473947.162592	46.682049
3503.415949	473926.376351	46.687053
3503.656056	473916.960886	46.692058
3503.412460	473902.857063	46.697063
3503.469669	473908.677317	46.702068
3503.302176	473885.538741	46.707073
3503.591457	473871.198606	46.712077
3503.250727	473870.796269	46.717082
3503.345552	473872.758187	46.722087
3503.549551	473862.385303	46.727092
3503.162254	473835.124871	46.732097
3503.380282	473825.003199	46.737101
3503.142351	473823.824269	46.742106
3503.302145	473824.762131	46.747111
3503.364696	473818.061232	46.752116
3502.963986	473823.142852	46.757121
3503.462792	473803.193695	46.762125
3503.418488	473780.643805	46.767130
3503.244017	473784.523814	46.772135
3503.787487	473775.972750	46.777140
3503.437294	473770.300176	46.782145
3503.139030	473745.407968	46.787149
3503.389929	473732.290356	46.792154
3503.387541	473729.097290	46.797159
3503.439160	473730.102943	46.802164
3503.383915	473724.130289	46.807169
3503.137092	473698.469545	46.812173
3503.384900	473686.873090	46.817178
3502.958233	473695.861970	46.822183
3503.134454	473687.723744	46.827188
3503.143048	473690.662417	46.832193
3503.231096	473674.427731	46.837197
3502.921443	473693.992318	46.842202
3503.145634	473682.754423	46.847207
3503.306828	473672.084068	46.852212
3503.302511	473660.426067	46.857217
3503.395803	473643.835698	46.862221
3503.451807	473636.933014	46.867226
3503.204388	473652.027079	46.872231
3503.402995	473639.069742	46.877236
3503.377297	473616.161899	46.882241
3503.548702	473599.508457	46.887245
3503.629240	473607.302026	46.892250
3503.545573	473597.582756	46.897255
3503.595352	473571.013240	46.902260
3503.510766	473562.054452	46.907265
3503.386480	473553.152625	46.912269
3503.379671	473544.637748	46.917274
3502.999672	473534.154239	46.922279
3503.409611	473512.850206	46.927284
3503.205843	473519.370795	46.932289
3503.502238	473505.637562	46.937293
3503.280513	473514.695510	46.942298
3503.362300	473495.927153	46.947303
3503.633335	473473.175010	46.952308
3503.099222	473471.637349	46.957313
3503.248503	473449.918234	46.962317
3503.304311	473468.614226	46.967322
3503.246363	473460.411540	46.972327
3503.326212	473442.048963	46.977332
3503.203406	473424.580141	46.982337
3503.221878	473420.775442	46.987341
3502.984940	473428.213732	46.992346
3503.100110	473412.633529	46.997351
3503.055905	473405.746605	47.002356
3503.094905	473415.118223	47.007361
3503.213496	473417.127119	47.012365
3503.487717	473397.770660	47.017370
3503.238116	473393.400037	47.022375
3503.565268	473370.385457	47.027380
3503.072585	473375.025508	47.032385
3503.215855	473366.841672	47.037389
3502.962803	473371.494539	47.042394
3503.252989	473369.066226	47.047399
3503.365826	473348.163814	47.052404
3503.081017	473345.268778	47.057409
3503.226783	473330.139893	47.062413
3503.201568	473322.945795	47.067418
3503.023248	473333.923214	47.072423
3503.394180	473320.482221	47.077428
3503.178860	473337.548388	47.082433
3503.130010	473318.090844	47.087437
3502.985713	473297.127639	47.092442
3502.969960	473281.922865	47.097447
3503.184387	473280.418952	47.102452
3503.076492	473280.841548	47.107457
3502.900804	473283.403879	47.112461
3503.026457	473272.181332	47.117466
3503.123593	473282.659023	47.122471
3503.066679	473275.419227	47.127476
3502.999483	473278.065793	47.132481
3503.139635	473279.665767	47.137485
3503.217925	473266.828593	47.142490
3503.036230	473264.576231	47.147495
3503.219768	473239.657945	47.152500
3503.304383	473231.787472	47.157505
3503.301505	473232.497617	47.162509
3503.361923	473235.985766	47.167514
3503.005863	473221.493718	47.172519
3503.332896	473229.654001	47.177524
3503.304832	473216.022547	47.182529
3503.278023	473201.123606	47.187533
3503.336603	473190.317145	47.192538
3503.111810	473195.168351	47.197543
3503.037239	473191.276932	47.202548
3503.017550	473186.464397	47.207553
3503.112836	473194.053029	47.212557
3503.192252	473189.630360	47.217562
3502.828411	473173.010477	47.222567
3503.242104	473154.240038	47.227572
3502.972741	473153.877097	47.232577
3502.913453	473148.969429	47.237581
3503.233239	473140.909677	47.242586
3503.126251	473151.977303	47.247591
3503.365154	473143.119275	47.252596
3503.269998	473146.378573	47.257601
3503.483029	473139.400210	47.262605
3503.313384	473113.827914	47.267610
3503.210524	473107.254308	47.272615
3503.182045	473092.355552	47.277620
3503.184539	473098.843674	47.282625
3503.439468	473096.066061	47.287629
3503.410114	473086.287271	47.292634
3503.220417	473070.856375	47.297639
3503.364252	473049.796684	47.302644
3503.027275	473055.730176	47.307649
3502.806130	473055.055463	47.312653
3503.016452	473049.648935	47.317658
3502.908035	473054.025556	47.322663
3502.963214	473052.800254	47.327668
3502.920959	473049.917531	47.332673
3503.195845	473062.445594	47.337677
3503.195924	473048.556123	47.342682
3503.075836	473049.741023	47.347687
3503.389743	473012.635885	47.352692
3503.420437	473011.819983	47.357697
3503.258348	473010.223485	47.362701
3503.364989	473005.036099	47.367706
3503.034593	473009.853348	47.372711
3503.260127	473007.333827	47.377716
3503.286781	472990.500001	47.382721
3503.119080	472975.268323	47.387725
3503.160855	472967.151060	47.392730
3503.296191	472974.784135	47.397735
3503.262131	472962.015218	47.402740
3503.401279	472965.136128	47.407745
3503.305452	472957.395452	47.412749
3503.404001	472929.043180	47.417754
3503.237519	472928.410515	47.422759
3503.451511	472913.017079	47.427764
3503.190445	472930.445659	47.432769
3503.339391	472909.232940	47.437773
3503.446018	472886.354054	47.442778
3503.173895	472889.539978	47.447783
3503.260498	472866.005240	47.452788
3502.990349	472882.015921	47.457793
3503.561944	472871.330975	47.462797
3503.257796	472867.374396	47.467802
3503.229777	472859.369506	47.472807
3503.359275	472830.302517	47.477812
3503.218546	472829.868547	47.482817
3503.018213	472826.757316	47.487821
3503.385217	472816.104678	47.492826
3503.247466	472825.707271	47.497831
3503.449770	472822.329634	47.502836
3503.355480	472798.975485	47.507841
3503.131326	472785.780274	47.512845
3502.962935	472789.304664	47.517850
3503.283773	472781.548758	47.522855
3503.500591	472777.053591	47.527860
3502.972631	472785.805417	47.532865
3503.381067	472778.796047	47.537869
3503.565111	472750.582092	47.542874
3503.344346	472752.492614	47.547879
3503.534903	472739.079749	47.552884
3503.502156	472732.545633	47.557889
3503.487286	472704.616514	47.562893
3503.332613	472703.170897	47.567898
3503.216484	472704.051038	47.572903
3503.544555	472694.823877	47.577908
3503.011273	472698.355262	47.582913
3503.236523	472666.535518	47.587917
3503.440868	472660.065290	47.592922
3503.250629	472651.781803	47.597927
3503.292932	472649.189813	47.602932
3503.462450	472646.780487	47.607937
3503.538245	472639.620875	47.612941
3503.375497	472630.167106	47.617946
3503.084208	472628.236150	47.622951
3503.430269	472616.420789	47.627956
3503.220287	472624.767578	47.632961
3503.254110	472618.577751	47.637965
3503.063103	472581.095401	47.642970
3503.066048	472587.532921	47.647975
3503.601156	472572.037782	47.652980
3503.365267	472567.766200	47.657985
3503.277979	472571.125731	47.662989
3503.329631	472572.080744	47.667994
3503.258584	472553.994683	47.672999
3503.391083	472529.235676	47.678004
3503.070862	472531.922330	47.683009
3503.297824	472521.545137	47.688013
3503.149144	472523.038744	47.693018
3503.171521	472522.173444	47.698023
3503.263831	472517.190971	47.703028
3503.246510	472500.566464	47.708033
3503.475723	472479.188534	47.713037
3503.103024	472484.215363	47.718042
3503.289104	472471.259267	47.723047
3503.409619	472469.719446	47.728052
3503.375581	472467.038113	47.733057
3503.087715	472451.064642	47.738061
3503.503954	472425.905814	47.743066
3503.306240	472425.784999	47.748071
3503.294097	472423.455052	47.753076
3503.104642	472430.429962	47.758081
3503.287522	472426.751172	47.763085
3503.589879	472397.656248	47.768090
3503.377639	472394.242675	47.773095
3503.566991	472382.654721	47.778100
3503.065523	472389.222721	47.783105
3503.163831	472382.110154	47.788109
3503.285223	472358.366560	47.793114
3502.900398	472349.505386	47.798119
3503.226147	472340.633286	47.803124
3503.052369	472337.771251	47.808129
3503.036547	472339.750805	47.813133
3503.373467	472346.845321	47.818138
3502.949758	472341.234658	47.823143
3503.387020	472333.561568	47.828148
3503.157546	472328.427136	47.833153
3502.904685	472299.267747	47.838157
3503.140643	472293.603501	47.843162
3502.777449	472297.513619	47.848167
3503.128463	472291.476334	47.853172
3503.086792	472289.607280	47.858177
3503.094660	472284.790177	47.863181
3503.285238	472281.464998	47.868186
3502.912449	472292.321631	47.873191
3502.975651	472285.265273	47.878196
3503.474019	472281.790060	47.883201
3503.242706	472292.725719	47.888205
3503.335976	472251.497216	47.893210
3503.064138	472254.885967	47.898215
3503.411434	472243.729212	47.903220
3503.414074	472254.425141	47.908225
3503.231593	472252.730419	47.913229
3503.664177	472232.536733	47.918234
3503.215747	472228.957688	47.923239
3503.661180	472203.844667	47.928244
3503.396250	472197.397771	47.933249
3503.253840	472192.553705	47.938253
3503.350228	472170.638817	47.943258
3503.105095	472160.133284	47.948263
3503.090662	472159.375174	47.953268
3502.986838	472163.751260	47.958273
3503.103012	472146.649122	47.963277
3503.679577	472155.632191	47.968282
3503.084379	472163.786582	47.973287
3503.193572	472131.325332	47.978292
3503.199788	472125.849434	47.983297
3502.919142	472121.077893	47.988301
3503.513106	472118.246563	47.993306
3503.393711	472112.689127	47.998311
3503.442146	472107.764183	48.003316
3503.424942	472106.144714	48.008321
3503.355112	472076.094283	48.013325
3503.295711	472068.195431	48.018330
3503.121572	472074.103468	48.023335
3503.622087	472062.314071	48.028340
3503.615632	472065.914378	48.033345
3503.468840	472037.346180	48.038349
3503.531662	472027.704397	48.043354
3503.448899	472031.164689	48.048359
3503.563674	472009.855052	48.053364
3503.366600	471991.687025	48.058369
3503.056611	471985.196490	48.063373
3503.276603	471979.686764	48.068378
3503.082346	471980.021647	48.073383
3503.040972	471981.498333	48.078388
3503.078757	471972.468812	48.083393
3502.843111	471961.505429	48.088397
3503.026328	471940.235597	48.093402
3503.022746	471929.995932	48.098407
3503.014109	471928.679261	48.103412
3502.757582	471936.070494	48.108417
3502.999346	471920.976089	48.113421
3503.209688	471926.924788	48.118426
3503.060352	471932.575474	48.123431
3503.358479	471935.823498	48.128436
3503.317527	471932.230691	48.133441
3503.177074	471925.054314	48.138445
3502.974034	471924.782255	48.143450
3502.967888	471921.589500	48.148455
3502.956629	471905.267717	48.153460
3503.042739	471903.986764	48.158465
3503.028511	471899.122368	48.163469
3503.329861	471888.631710	48.168474
3503.181943	471895.296070	48.173479
3503.182281	471888.604372	48.178484
3503.311561	471889.597842	48.183489
3503.143064	471898.343923	48.188493
3503.112585	471894.698761	48.193498
3503.322489	471874.742696	48.198503
3503.221686	471852.402386	48.203508
3503.373141	471856.484717	48.208513
3503.173118	471846.580226	48.213517
3503.299980	471844.278937	48.218522
3502.849752	471851.650121	48.223527
3503.060057	471845.634946	48.228532
3503.221815	471851.185789	48.233537
3503.208973	471818.287082	48.238541
3503.287161	471806.868457	48.243546
3502.909038	471809.361577	48.248551
3503.172276	471798.420646	48.253556
3503.105166	471799.039603	48.258561
3502.781528	471810.699836	48.263565
3503.335141	471793.731044	48.268570
3502.862364	471802.373175	48.273575
3502.950743	471802.714084	48.278580
3503.065624	471805.281367	48.283585
3503.017817	471794.997930	48.288589
3503.209507	471783.662742	48.293594
3503.131727	471767.554143	48.298599
3503.364743	471750.534598	48.303604
3503.099966	471743.225723	48.308609
3503.379270	471746.527447	48.313613
3503.537648	471743.916998	48.318618
3503.206598	471738.342218	48.323623
3503.406092	471708.857019	48.328628
3503.044238	471709.471870	48.333633
3503.081713	471708.502761	48.338637
3503.342105	471703.138660	48.343642
3502.962377	471706.798028	48.348647
3503.215220	471701.485815	48.353652
3502.995678	471715.461612	48.358657
3502.775431	471705.205386	48.363661
3503.252985	471702.899348	48.368666
3502.856207	471677.361156	48.373671
3502.803083	471671.336871	48.378676
3502.694292	471668.058910	48.383681
3502.942951	471669.084218	48.388685
3503.131769	471671.589137	48.393690
3503.206311	471664.429383	48.398695
3502.914860	471658.949712	48.403700
3503.048143	471663.998158	48.408705
3502.893504	471662.501766	48.413709
3503.183309	471654.953121	48.418714
3503.067994	471660.294334	48.423719
3503.120462	471663.175669	48.428724
3503.039935	471655.026523	48.433729
3502.874754	471670.768082	48.438733
3503.089258	471659.023660	48.443738
3502.962790	471661.020768	48.448743
3503.043021	471645.241963	48.453748
3502.866993	471625.549435	48.458753
3502.473205	471627.740882	48.463757
3503.075622	471635.503414	48.468762
3503.181510	471644.104845	48.473767
3503.088807	471622.776905	48.478772
3503.048936	471623.239477	48.483777
3503.091119	471609.443766	48.488781
3503.588675	471613.522137	48.493786
3502.989050	471623.958719	48.498791
3503.040287	471609.096980	48.503796
3503.132652	471614.151905	48.508801
3503.027791	471605.550329	48.513805
3503.484296	471594.021096	48.518810
3502.955546	471567.286943	48.523815
3503.076661	471566.101826	48.528820
3502.827596	471562.186982	48.533825
3502.869553	471570.240901	48.538829
3502.807376	471565.282615	48.543834
3502.679094	471576.354456	48.548839
3502.795426	471566.602610	48.553844
3502.831472	471573.491473	48.558849
3502.663470	471574.531945	48.563853
3502.717269	471567.172655	48.568858
3502.730069	471572.595033	48.573863
3502.933587	471557.252931	48.578868
3502.841297	471567.558660	48.583873
3502.950186	471567.186598	48.588877
3502.962801	471558.971997	48.593882
3503.388554	471566.204829	48.598887
3503.278173	471564.701435	48.603892
3503.063336	471555.103316	48.608897
3503.019595	471565.857629	48.613901
3503.235365	471557.256051	48.618906
3503.263161	471563.994136	48.623911
3502.928150	471561.258864	48.628916
3503.011122	471558.406834	48.633921
3502.955438	471542.345261	48.638925
3503.113730	471527.213066	48.643930
3503.042514	471539.746070	48.648935
3503.232317	471528.106869	48.653940
3503.277302	471532.206092	48.658945
3502.885956	471530.696407	48.663949
3503.128993	471526.957253	48.668954
3502.994646	471525.711120	48.673959
3503.084266	471521.641347	48.678964
3503.092289	471526.709624	48.683969
3503.331888	471521.855716	48.688973
3503.641512	471504.519688	48.693978
3503.060050	471493.762798	48.698983
3502.990482	471482.924996	48.703988
3502.863176	471487.457023	48.708993
3502.836450	471487.613348	48.713997
3503.288345	471476.743819	48.719002
3503.208004	471479.696866	48.724007
3503.646501	471472.682304	48.729012
3503.614213	471458.492698	48.734017
3503.568529	471446.890670	48.739021
3503.923741	471436.391269	48.744026
3503.374371	471416.858941	48.749031
3503.641610	471397.957960	48.754036
3503.586905	471387.371236	48.759041
3503.292403	471391.574840	48.764045
3503.386648	471360.889083	48.769050
3503.541353	471356.251338	48.774055
3503.427251	471352.163034	48.779060
3503.472823	471340.191652	48.784065
3503.390163	471327.682878	48.789069
3503.468847	471306.023346	48.794074
3503.136489	471306.227979	48.799079
3503.420528	471301.721867	48.804084
3503.265362	471294.699683	48.809089
3503.220897	471296.430386	48.814093
3503.155364	471263.032160	48.819098
3503.354373	471262.747241	48.824103
3503.353134	471247.690752	48.829108
3503.278684	471255.002754	48.834113
3502.853590	471264.144532	48.839117
3503.261640	471242.534268	48.844122
3503.288139	471258.195151	48.849127
3502.941316	471217.693180	48.854132
3503.263318	471211.964343	48.859137
3503.239634	471210.041650	48.864141
3503.086154	471203.627522	48.869146
3502.678552	471208.406696	48.874151
3502.995827	471202.881387	48.879156
3503.374442	471201.199286	48.884161
3503.113259	471206.158103	48.889165
3503.324825	471207.087905	48.894170
3503.107300	471210.417546	48.899175
3503.036390	471190.860076	48.904180
3503.210117	471187.131816	48.909185
3503.210672	471180.744030	48.914189
3503.242460	471172.576940	48.919194
3503.278064	471171.912278	48.924199
3503.322615	471175.403287	48.929204
3503.319309	471171.703005	48.934209
3502.962217	471157.513832	48.939213
3503.290350	471136.169569	48.944218
3502.831434	471147.851557	48.949223
3502.837833	471128.180416	48.954228
3503.027625	471125.412834	48.959233
3502.922398	471130.651198	48.964237
3502.992102	471132.718743	48.969242
3502.768997	471124.896098	48.974247
3502.939165	471122.131619	48.979252
3503.222099	471119.298619	48.984257
3503.145344	471127.574260	48.989261
3503.127263	471119.060157	48.994266
3503.351047	471140.063754	48.999271
3503.195924	471110.836534	49.004276
3502.974183	471092.722307	49.009281
3503.198641	471081.077376	49.014285
3503.087993	471079.979559	49.019290
3503.163957	471084.580939	49.024295
3503.264201	471078.329454	49.029300
3503.435031	471067.605527	49.034305
3503.064028	471080.186193	49.039309
3503.207023	471049.644357	49.044314
3503.441610	471044.791130	49.049319
3503.063327	471042.468200	49.054324
3503.471360	471034.799250	49.059329
3503.169883	471034.390646	49.064333
3503.329591	471036.089100	49.069338
3502.994968	471016.319663	49.074343
3502.826866	470989.679845	49.079348
3503.023619	471002.931272	49.084353
3503.055137	470997.704557	49.089357
3502.999924	470979.665303	49.094362
3502.839475	470991.401598	49.099367
3502.776022	470992.172092	49.104372
3503.315371	470988.588794	49.109377
3503.001817	470990.666233	49.114381
3503.224764	470985.105079	49.119386
3503.077018	470987.713974	49.124391
3503.296965	470991.126595	49.129396
3503.172095	470983.744640	49.134401
3503.105954	470984.160682	49.139405
3503.403708	470949.386417	49.144410
3503.347835	470952.589156	49.149415
3503.244321	470948.904672	49.154420
3503.268041	470942.208971	49.159425
3503.224864	470942.621385	49.164429
3503.114044	470932.296780	49.169434
3502.878710	470913.272002	49.174439
3503.142458	470893.965537	49.179444
3503.407606	470890.881834	49.184449
3503.328734	470895.406335	49.189453
3503.443318	470894.627787	49.194458
3503.617259	470893.738464	49.199463
3503.407181	470870.603209	49.204468
3503.522600	470856.541934	49.209473
3503.285140	470854.652997	49.214477
3503.514012	470838.850082	49.219482
3503.176542	470840.475042	49.224487
3503.039696	470820.876946	49.229492
3503.325564	470809.171459	49.234497
3502.866782	470806.100769	49.239501
3503.157629	470806.460391	49.244506
3503.354015	470805.719608	49.249511
3503.561965	470800.110078	49.254516
3503.482146	470800.376194	49.259521
3503.309628	470779.161390	49.264525
3503.164958	470765.090463	49.269530
3502.963317	470769.026030	49.274535
3502.834397	470754.496333	49.279540
3503.111269	470765.910149	49.284545
3502.709769	470765.872229	49.289549
3503.079150	470761.099025	49.294554
3502.955206	470762.436757	49.299559
3503.164688	470759.564621	49.304564
3503.242914	470758.842512	49.309569
3502.986216	470742.457206	49.314573
3503.209591	470728.023900	49.319578
3502.941090	470721.931984	49.324583
3503.192689	470722.297811	49.329588
3503.086627	470712.986290	49.334593
3503.059536	470711.165485	49.339597
3503.304768	470715.486707	49.344602
3503.091697	470709.538118	49.349607
3503.154975	470709.325343	49.354612
3503.237496	470705.256531	49.359617
3503.016666	470680.703238	49.364621
3503.122095	470667.860151	49.369626
3503.012468	470679.132314	49.374631
3503.253542	470668.244985	49.379636
3503.069331	470662.849493	49.384641
3502.889342	470673.828595	49.389645
3503.414538	470662.592172	49.394650
3503.090574	470668.422896	49.399655
3503.129410	470674.246973	49.404660
3503.215566	470661.508323	49.409665
3503.051719	470637.909224	49.414669
3503.073812	470623.558356	49.419674
3503.109350	470621.727644	49.424679
3503.269442	470623.476769	49.429684
3503.210295	470626.578681	49.434689
3503.022760	470621.792073	49.439693
3503.199511	470616.643702	49.444698
3503.177593	470618.370898	49.449703
3503.146510	470616.905597	49.454708
3503.512443	470592.056669	49.459713
3503.172608	470588.409472	49.464717
3503.405399	470577.422010	49.469722
3503.309626	470580.985996	49.474727
3503.117249	470574.679214	49.479732
3503.435498	470565.148469	49.484737
3503.107196	470554.148282	49.489741
3503.129417	470543.396874	49.494746
3502.883066	470534.107445	49.499751
3503.402425	470528.550018	49.504756
3503.194337	470532.131764	49.509761
3503.200682	470530.254960	49.514765
3503.531677	470518.491479	49.519770
3503.145649	470512.722263	49.524775
3502.830047	470496.396770	49.529780
3503.284115	470482.231018	49.534785
3503.211057	470484.270494	49.539789
3503.139369	470486.766035	49.544794
3503.123867	470486.362917	49.549799
3503.199454	470485.844007	49.554804
3503.381059	470485.359038	49.559809
3503.196011	470467.948233	49.564813
3503.300253	470456.271254	49.569818
3503.125987	470458.580219	49.574823
3503.224333	470460.896794	49.579828
3502.969451	470448.718894	49.584833
3502.917776	470447.459628	49.589837
3503.108519	470458.430947	49.594842
3503.267646	470456.580686	49.599847
3503.067985	470439.172166	49.604852
3503.448606	470421.164936	49.609857
3503.322805	470410.132665	49.614861
3503.112616	470397.288597	49.619866
3503.375739	470411.188988	49.624871
3503.272229	470404.969505	49.629876
3503.107784	470393.030768	49.634881
3503.185006	470379.279395	49.639885
3503.050540	470366.828924	49.644890
3503.278443	470364.511502	49.649895
3503.079716	470361.501037	49.654900
3503.491067	470357.025297	49.659905
3502.972666	470365.218953	49.664909
3503.266873	470362.384069	49.669914
3502.973120	470343.317301	49.674919
3502.752063	470327.331618	49.679924
3502.846256	470325.187420	49.684929
3502.908936	470348.650801	49.689933
3503.399450	470331.133105	49.694938
3503.192154	470329.087257	49.699943
3502.862705	470314.132661	49.704948
3503.042077	470309.440084	49.709953
3502.980524	470313.657785	49.714957
3503.317932	470315.581704	49.719962
3502.875787	470311.342249	49.724967
3502.698984	470312.434872	49.729972
3503.010011	470307.518693	49.734977
3502.856766	470314.032309	49.739981
3503.039130	470307.970406	49.744986
3502.921256	470316.557060	49.749991
3502.936230	470318.684036	49.754996
3503.270198	470306.210189	49.760001
3502.972582	470317.664356	49.765005
3503.056904	470302.644352	49.770010
3503.048304	470285.458997	49.775015
3503.115338	470271.962654	49.780020
3503.273995	470272.089688	49.785025
3503.166315	470275.351418	49.790029
3503.195374	470273.217509	49.795034
3502.967541	470280.148511	49.800039
3503.044979	470281.251651	49.805044
3502.916736	470260.637696	49.810049
3502.797286	470274.142361	49.815053
3502.997004	470266.455355	49.820058
3503.116580	470266.335074	49.825063
3503.121085	470267.246949	49.830068
3503.327460	470237.454372	49.835073
3503.042480	470227.866720	49.840077
3503.251728	470225.349437	49.845082
3503.326025	470227.416347	49.850087
3503.207186	470219.120593	49.855092
3503.423865	470217.362612	49.860097
3502.995885	470211.904133	49.865101
3503.139137	470189.827638	49.870106
3503.221357	470186.215059	49.875111
3502.999869	470181.636510	49.880116
3503.096164	470181.367812	49.885121
3503.146251	470178.368694	49.890125
3503.235752	470175.109852	49.895130
3502.922488	470186.870756	49.900135
3503.224393	470171.106487	49.905140
3503.445239	470162.402131	49.910145
3503.192726	470152.961409	49.915149
3503.305978	470134.590599	49.920154
3503.136641	470135.124366	49.925159
3502.837535	470122.902565	49.930164
3503.219570	470136.277359	49.935169
3502.955541	470120.247610	49.940173
3503.240269	470124.816208	49.945178
3503.116895	470124.024543	49.950183
3502.540840	470121.529971	49.955188
3503.350126	470131.491122	49.960193
3503.118612	470117.433481	49.965197
3503.110360	470088.333696	49.970202
3502.933101	470093.279513	49.975207
3503.209342	470087.304106	49.980212
3503.250354	470088.565109	49.985217
3503.075353	470090.722135	49.990221
3503.415227	470083.215704	49.995226
3503.409829	470083.317970	50.000231
3503.015285	470063.252897	50.005236
3503.425742	470052.541270	50.010241
3503.319666	470041.353588	50.015245
3503.117252	470035.707314	50.020250
3503.169582	470041.326641	50.025255
3503.043169	470040.079163	50.030260
3503.175064	470032.047898	50.035265
3503.110130	470029.371131	50.040269
3503.109676	470001.740262	50.045274
3502.743997	470004.992114	50.050279
3502.838026	470000.566451	50.055284
3502.846854	469989.867572	50.060289
3503.038003	469996.428252	50.065293
3503.137504	469996.361842	50.070298
3503.079664	469982.935747	50.075303
3503.026882	469999.167804	50.080308
3503.270333	469996.695787	50.085313
3502.924549	469997.003950	50.090317
3503.093153	469989.017565	50.095322
3503.051427	469991.660526	50.100327
3502.973962	469992.788164	50.105332
3503.211310	469983.117843	50.110337
3502.999526	469963.834973	50.115341
3503.375273	469956.373526	50.120346
3502.952737	469951.522507	50.125351
3503.165429	469946.317591	50.130356
3503.432114	469942.168822	50.135361
3503.238756	469946.204633	50.140365
3503.239510	469940.779717	50.145370
3503.375801	469930.516953	50.150375
3503.078809	469910.030720	50.155380
3503.493624	469899.673220	50.160385
3503.435227	469904.803092	50.165389
3503.490973	469903.983108	50.170394
3503.493609	469889.381311	50.175399
3503.269961	469875.423660	50.180404
3503.240954	469856.263900	50.185409
3503.103691	469864.498910	50.190413
3503.452536	469854.151814	50.195418
3503.426035	469861.558128	50.200423
3503.189240	469837.158455	50.205428
3503.318812	469816.199113	50.210433
3503.057371	469815.226461	50.215437
3503.320594	469814.424380	50.220442
3503.129818	469810.753485	50.225447
3502.951330	469809.970519	50.230452
3503.578594	469804.750742	50.235457
3503.162700	469790.468523	50.240461
3503.399568	469763.813819	50.245466
3503.117877	469768.218523	50.250471
3502.969476	469774.985040	50.255476
3503.418333	469759.856328	50.260481
3503.498664	469758.474757	50.265485
3503.192943	469747.419871	50.270490
3503.121202	469738.609483	50.275495
3503.036722	469726.961922	50.280500
3502.988527	469720.429292	50.285505
3502.898101	469735.501411	50.290509
3502.969181	469732.955207	50.295514
3503.121604	469722.284194	50.300519
3502.963860	469734.984066	50.305524
3503.360407	469721.942282	50.310529
3503.363722	469725.287954	50.315533
3503.471474	469712.089010	50.320538
3503.052034	469688.630626	50.325543
3503.278687	469683.778336	50.330548
3503.423900	469683.400501	50.335553
3503.152342	469692.062404	50.340557
3503.164475	469682.681038	50.345562
3503.055506	469675.245402	50.350567
3503.003991	469665.519190	50.355572
3503.178733	469636.846148	50.360577
3502.848940	469644.553976	50.365581
3503.180600	469634.310887	50.370586
3503.204852	469642.621856	50.375591
3502.838160	469641.716530	50.380596
3503.373073	469630.934316	50.385601
3503.116525	469642.787962	50.390605
3502.856118	469642.778436	50.395610
3503.022197	469636.718911	50.400615
3503.121068	469633.813404	50.405620
3503.344032	469627.592786	50.410625
3503.057175	469610.095950	50.415629
3503.148080	469592.691493	50.420634
3502.993481	469587.341739	50.425639
3503.002894	469589.672469	50.430644
3503.160559	469581.180656	50.435649
3503.062211	469587.381622	50.440653
3502.931480	469593.942605	50.445658
3503.370474	469586.166829	50.450663
3503.236723	469590.345388	50.455668
3503.390732	469567.151131	50.460673
3503.366604	469546.925612	50.465677
3503.024186	469553.520065	50.470682
3503.194675	469547.104917	50.475687
3503.113467	469550.109075	50.480692
3503.329525	469536.639401	50.485697
3503.236092	469539.189192	50.490701
3503.212311	469521.600002	50.495706
3503.112649	469510.816622	50.500711
3503.061508	469496.730051	50.505716
3503.392437	469495.815857	50.510721
3503.472103	469491.645858	50.515725
3503.404630	469475.736644	50.520730
3503.127394	469470.862546	50.525735
3502.824380	469446.219378	50.530740
3503.279688	469401.074734	50.535745
3503.081822	469351.216671	50.540749
3503.054067	469293.472984	50.545754
3503.065027	469233.999187	50.550759
3502.805435	469157.481721	50.555764
3502.802361	469062.975169	50.560769
3502.551534	468976.974505	50.565773
3502.339196	468857.960543	50.570778
3502.492234	468744.516085	50.575783
3501.971492	468629.757839	50.580788
3501.841436	468489.180247	50.585793
3501.770718	468362.434262	50.590797
3501.538217	468211.983907	50.595802
3501.263895	468050.891289	50.600807
3500.802866	467886.784692	50.605812
3500.631335	467717.966232	50.610817
3500.393974	467546.418749	50.615821
3500.185156	467351.236619	50.620826
3499.835013	467172.199496	50.625831
3499.517702	466984.535583	50.630836
3499.456301	466767.774532	50.635841
3498.892460	466556.414942	50.640845
3498.434529	466351.577814	50.645850
3498.398112	466126.692972	50.650855
3497.870079	465897.776019	50.655860
3497.474921	465666.147986	50.660865
3497.099009	465431.928169	50.665869
3496.516672	465185.364998	50.670874
3496.340572	464924.180627	50.675879
3495.774775	464679.130316	50.680884
3495.616449	464418.849756	50.685889
3495.016229	464159.548707	50.690893
3494.624825	463891.894457	50.695898
3494.427016	463619.337684	50.700903
3493.611739	463346.875044	50.705908
3493.508837	463055.125820	50.710913
3492.976605	462777.590371	50.715917
3492.418267	462484.586778	50.720922
3492.045983	462180.391893	50.725927
3491.644576	461890.601374	50.730932
3491.278586	461583.201836	50.735937
3490.441881	461278.104018	50.740941
3489.864772	460962.968923	50.745946
3489.168947	460653.782426	50.750951
3488.731041	460346.579658	50.755956
3488.251740	460021.778306	50.760961
3487.727295	459705.297928	50.765965
3487.277932	459379.417121	50.770970
3486.753470	459050.956369	50.775975
3485.986685	458732.319092	50.780980
3485.683374	458393.871325	50.785985
3485.026327	458067.090839	50.790989
3484.463481	457722.180710	50.795994
3483.893840	457380.614392	50.800999
3483.283388	457053.456487	50.806004
3483.001303	456711.327131	50.811009
3482.276736	456364.189345	50.816013
3481.673489	456007.793761	50.821018
3480.879847	455659.083247	50.826023
3480.108916	455315.183406	50.831028
3479.704503	454954.782430	50.836033
3478.936445	454610.972830	50.841037
3478.330662	454266.675712	50.846042
3477.832688	453903.228561	50.851047
3477.465113	453555.331388	50.856052
3477.100624	453186.321249	50.861057
3476.215909	452834.638662	50.866061
3475.169468	452463.035412	50.871066
3474.891868	452106.577552	50.876071
3474.227368	451736.830264	50.881076
3473.701498	451380.907767	50.886081
3472.952174	451005.631186	50.891085
3472.245336	450638.714530	50.896090
3471.846070	450273.113529	50.901095
3470.755391	449902.845950	50.906100
3470.350343	449530.840187	50.911105
3469.493545	449171.738920	50.916109
3468.859694	448791.028960	50.921114
3468.562893	448434.618949	50.926119
3467.372420	448053.731204	50.931124
3466.806424	447692.277468	50.936129
3466.159490	447318.143156	50.941133
3465.662974	446948.496044	50.946138
3464.801027	446586.513823	50.951143
3464.347685	446212.483615	50.956148
3463.533154	445836.220643	50.961153
3462.853954	445471.807029	50.966157
3462.233483	445106.312670	50.971162
3461.626486	444721.675273	50.976167
3460.507176	444355.131608	50.981172
3460.188125	443988.861894	50.986177
3459.499746	443621.325233	50.991181
3458.590840	443240.163398	50.996186
3458.256246	442882.914558	51.001191
3457.281699	442517.132151	51.006196
3456.795119	442137.256705	51.011201
3455.710688	441775.490687	51.016205
3455.097203	441402.019937	51.021210
3454.710131	441035.157826	51.026215
3453.809147	440667.356138	51.031220
3453.168143	440300.827742	51.036225
3452.713763	439935.432005	51.041229
3451.486397	439562.690198	51.046234
3450.631864	439195.366794	51.051239
3449.596952	438836.443340	51.056244
3449.250985	438468.673362	51.061249
3448.818779	438124.088326	51.066253
3448.280320	437755.881289	51.071258
3447.728482	437387.087050	51.076263
3446.817419	437039.719484	51.081268
3446.195620	436665.036016	51.086273
3445.324917	436307.116412	51.091277
3444.847531	435943.772779	51.096282
3444.078635	435587.146994	51.101287
3443.275156	435219.706267	51.106292
3442.734720	434853.919659	51.111297
3441.921920	434496.193738	51.116301
3440.860267	434146.322024	51.121306
3440.612275	433789.487070	51.126311
3439.853824	433430.366561	51.131316
3439.033123	433070.743050	51.136321
3438.135916	432724.634442	51.141325
3437.458495	432366.679602	51.146330
3436.752432	432011.669722	51.151335
3436.129313	431670.708871	51.156340
3435.365709	431306.176509	51.161345
3434.777871	430966.140323	51.166349
3434.056749	430613.119677	51.171354
3433.453582	430257.130005	51.176359
3432.566716	429917.559103	51.181364
3432.066013	429567.536701	51.186369
3431.460779	429219.125988	51.191373
3430.520655	428871.144521	51.196378
3429.889712	428518.716289	51.201383
3429.047110	428177.871596	51.206388
3428.504393	427825.166230	51.211393
3427.654797	427485.456542	51.216397
3426.806922	427136.828215	51.221402
3426.227997	426794.755887	51.226407
3425.358469	426449.245770	51.231412
3425.045135	426104.278196	51.236417
3424.228193	425777.087796	51.241421
3423.290679	425432.845224	51.246426
3422.771639	425096.786463	51.251431
3421.831946	424767.876167	51.256436
3421.330316	424413.036792	51.261441
3420.739608	424085.713970	51.266445
3419.804848	423746.199152	51.271450
3419.217896	423406.879120	51.276455
3418.093414	423075.463035	51.281460
3417.466991	422742.236988	51.286465
3416.605495	422416.283215	51.291469
3416.182240	422087.487611	51.296474
3415.383130	421770.686041	51.301479
3414.826785	421440.659130	51.306484
3414.340341	421114.706917	51.311489
3413.154017	420789.217159	51.316493
3412.631990	420463.466160	51.321498
3412.221518	420141.250089	51.326503
3411.224429	419811.603793	51.331508
3410.461772	419479.452448	51.336513
3409.851527	419164.776091	51.341517
3409.180538	418831.535660	51.346522
3408.736053	418519.798145	51.351527
3407.780671	418203.488973	51.356532
3407.137418	417876.914262	51.361537
3406.396924	417548.522017	51.366541
3405.661417	417234.072668	51.371546
3404.925182	416920.102675	51.376551
3404.023900	416602.776365	51.381556
3403.677846	416285.409574	51.386561
3402.910962	415971.764328	51.391565
3402.495541	415657.755222	51.396570
3401.858688	415340.500224	51.401575
3400.706224	415025.863985	51.406580
3400.536663	414705.911222	51.411585
3399.363988	414378.313365	51.416589
3398.633328	414064.819611	51.421594
3397.924918	413751.115708	51.426599
3397.005552	413453.703264	51.431604
3396.650910	413141.181921	51.436609
3395.952706	412825.941989	51.441613
3395.021962	412515.461590	51.446618
3394.366673	412209.787612	51.451623
3393.327359	411904.577754	51.456628
3392.842579	411602.834500	51.461633
3391.944800	411294.902529	51.466637
3391.435618	410999.179278	51.471642
3391.021368	410682.219992	51.476647
3390.056195	410391.746658	51.481652
3389.496727	410090.711458	51.486657
3388.671314	409793.247515	51.491661
3387.822904	409499.672295	51.496666
3387.641423	409199.737386	51.501671
3386.524815	408899.261224	51.506676
3386.049717	408603.127874	51.511681
3385.230727	408307.350970	51.516685
3384.586885	408009.713757	51.521690
3383.835443	407715.241920	51.526695
3382.937372	407421.146226	51.531700
3382.533650	407123.055813	51.536705
3381.744782	406840.449784	51.541709
3381.087022	406543.715466	51.546714
3380.466297	406245.218836	51.551719
3379.817107	405944.360249	51.556724
3379.180198	405653.967825	51.561729
3378.209296	405359.076155	51.566733
3377.558925	405072.035258	51.571738
3377.035139	404779.608977	51.576743
3376.098195	404489.532736	51.581748
3375.545546	404191.564840	51.586753
3374.528554	403916.008655	51.591757
3373.830618	403639.154195	51.596762
3373.300980	403344.885503	51.601767
3372.644948	403062.681812	51.606772
3372.128250	402772.828358	51.611777
3371.362273	402500.524435	51.616781
3370.259771	402211.165178	51.621786
3370.077602	401930.045751	51.626791
3369.246104	401648.365653	51.631796
3368.698102	401363.638870	51.636801
3367.817498	401079.928072	51.641805
3367.261388	400811.923236	51.646810
3366.811701	400515.989077	51.651815
3366.059842	400238.783275	51.656820
3365.127858	399950.190168	51.661825
3364.696977	399670.005505	51.666829
3363.719419	399394.251709	51.671834
3362.878415	399111.890139	51.676839
3361.983263	398836.398237	51.681844
3361.874500	398547.077906	51.686849
3360.767677	398285.265788	51.691853
3360.067280	398005.338313	51.696858
3359.579644	397727.789857	51.701863
3359.000360	397460.854365	51.706868
3358.242049	397185.301631	51.711873
3357.551784	396914.057596	51.716877
3356.505077	396640.198386	51.721882
3356.024467	396368.459170	51.726887
3355.249205	396100.933650	51.731892
3354.851850	395821.829709	51.736897
3354.061800	395555.878407	51.741901
3353.326579	395290.882420	51.746906
3352.725669	395013.812418	51.751911
3351.713051	394759.762785	51.756916
3351.409282	394479.132974	51.761921
3350.624798	394214.263489	51.766925
3349.856278	393946.694457	51.771930
3349.399767	393671.344971	51.776935
3348.383247	393409.989094	51.781940
3347.763857	393130.643937	51.786945
3347.256966	392873.525619	51.791949
3346.335930	392614.716534	51.796954
3345.905892	392344.767825	51.801959
3345.289056	392090.635847	51.806964
3344.353775	391821.220620	51.811969
3343.719858	391558.239280	51.816973
3343.231894	391297.114416	51.821978
3342.575363	391024.191001	51.826983
3341.631719	390767.482153	51.831988
3341.219367	390491.617360	51.836993
3340.515013	390232.425802	51.841997
3339.816391	389972.138070	51.847002
3339.647022	389707.136962	51.852007
3338.507922	389448.466102	51.857012
3337.528184	389171.333084	51.862017
3337.091666	388913.793196	51.867021
3336.118775	388654.098600	51.872026
3335.651674	388386.057957	51.877031
3334.731244	388131.538643	51.882036
3334.401391	387875.372994	51.887041
3333.515439	387614.741707	51.892045
3332.700751	387355.419579	51.897050
3332.043607	387094.900939	51.902055
3331.480147	386845.300234	51.907060
3330.985232	386576.487690	51.912065
3330.172717	386329.694655	51.917069
3329.503814	386078.808465	51.922074
3328.834572	385810.755325	51.927079
3327.583516	385557.033168	51.932084
3327.337645	385302.514546	51.937089
3326.857055	385040.452972	51.942093
3325.659722	384794.422543	51.947098
3325.160784	384543.753334	51.952103
3324.366733	384285.474341	51.957108
3323.627804	384038.425464	51.962113
3323.040319	383798.141199	51.967117
3322.282763	383550.278236	51.972122
3321.678550	383286.087614	51.977127
3320.938247	383061.361612	51.982132
3320.609787	382809.483957	51.987137
3319.913311	382551.838829	51.992141
3318.987286	382313.582339	51.997146
3318.701947	382057.013290	52.002151
3317.923519	381805.454447	52.007156
3317.113172	381556.162523	52.012161
3316.393856	381315.476401	52.017165
3315.495643	381074.282959	52.022170
3314.943217	380819.477299	52.027175
3314.300049	380580.275098	52.032180
3313.592804	380333.960096	52.037185
3312.930740	380086.771626	52.042189
3312.059210	379841.191617	52.047194
3311.479687	379603.473924	52.052199
3310.837737	379366.247905	52.057204
3310.386627	379118.384058	52.062209
3309.264700	378878.992744	52.067213
3308.614147	378645.350006	52.072218
3308.291471	378390.466660	52.077223
3307.210765	378159.381693	52.082228
3306.526377	377922.713233	52.087233
3305.858419	377693.366175	52.092237
3305.386813	377449.437563	52.097242
3304.579719	377202.940625	52.102247
3303.858431	376967.900199	52.107252
3303.289724	376740.388776	52.112257
3302.610979	376494.579377	52.117261
3301.962081	376264.178202	52.122266
3301.393658	376024.885632	52.127271
3300.574707	375786.928532	52.132276
3299.857730	375549.818756	52.137281
3299.465864	375322.780093	52.142285
3298.336396	375089.929963	52.147290
3297.665977	374844.185519	52.152295
3297.009808	374614.742726	52.157300
3296.525015	374386.441671	52.162305
3295.991489	374147.997409	52.167309
3294.989368	373922.421108	52.172314
3294.790229	373673.033812	52.177319
3293.780576	373453.205121	52.182324
3293.241266	373225.440451	52.187329
3292.499042	372991.932102	52.192333
3291.957464	372762.562632	52.197338
3291.356135	372520.176736	52.202343
3290.512337	372299.145530	52.207348
3289.792809	372051.484332	52.212353
3289.121508	371826.734701	52.217357
3288.391679	371598.482509	52.222362
3287.790996	371355.148529	52.227367
3287.149865	371134.587940	52.232372
3286.679239	370909.521855	52.237377
3285.664084	370672.253266	52.242381
3285.031806	370440.824872	52.247386
3283.912885	370208.632664	52.252391
3283.369275	369994.410769	52.257396
3282.950442	369760.350034	52.262401
3282.165069	369531.713939	52.267405
3281.204520	369312.161200	52.272410
3280.845099	369087.856615	52.277415
3280.124249	368878.287419	52.282420
3279.472457	368643.646896	52.287425
3279.047860	368427.185037	52.292429
3278.166704	368194.715427	52.297434
3277.705500	367966.172463	52.302439
3276.793675	367742.304496	52.307444
3276.251026	367514.687958	52.312449
3275.608135	367293.115805	52.317453
3274.923487	367065.366754	52.322458
3274.240695	366841.127243	52.327463
3273.401630	366627.647916	52.332468
3272.522722	366399.417327	52.337473
3272.093493	366176.762670	52.342477
3271.207629	365962.244417	52.347482
3270.538376	365752.881185	52.352487
3270.043954	365529.266799	52.357492
3269.243290	365303.740632	52.362497
3268.634485	365092.456547	52.367501
3267.854427	364878.654244	52.372506
3267.479409	364650.284191	52.377511
3266.654710	364432.161484	52.382516
3265.932065	364213.461834	52.387521
3265.332174	363987.439388	52.392525
3264.864163	363778.773078	52.397530
3264.158382	363550.322621	52.402535
3262.946538	363344.341820	52.407540
3262.595027	363126.468831	52.412545
3261.936639	362907.040364	52.417549
3260.886857	362692.278196	52.422554
3260.625423	362475.558343	52.427559
3259.593661	362266.338260	52.432564
3259.143286	362056.872616	52.437569
3258.542496	361839.847261	52.442573
3257.992217	361625.204741	52.447578
3257.447101	361405.267847	52.452583
3256.584829	361195.583615	52.457588
3255.837190	360974.455378	52.462593
3255.141693	360756.396759	52.467597
3254.573382	360548.902370	52.472602
3253.785685	360329.151524	52.477607
3253.169827	360129.321973	52.482612
3252.440513	359912.028216	52.487617
3252.135497	359702.045703	52.492621
3251.276800	359483.218265	52.497626
3250.770750	359252.119867	52.502631
3249.708536	359050.040827	52.507636
3249.254206	358829.594247	52.512641
3248.591071	358625.058349	52.517645
3247.602295	358415.890913	52.522650
3247.087324	358196.443481	52.527655
3246.317896	357994.542775	52.532660
3245.518797	357782.059982	52.537665
3245.150541	357570.093409	52.542669
3244.339904	357363.743390	52.547674
3243.833783	357141.643347	52.552679
3243.334674	356946.795402	52.557684
3242.602019	356729.615254	52.562689
3241.926808	356513.773799	52.567693
3240.833774	356297.921157	52.572698
3240.452517	356084.219862	52.577703
3239.780531	355879.292299	52.582708
3239.080712	355662.891222	52.587713
3238.148728	355461.845748	52.592717
3237.530199	355260.520860	52.597722
3236.869004	355051.262028	52.602727
3236.082408	354859.072656	52.607732
3235.544220	354643.964993	52.612737
3235.061287	354439.816072	52.617741
3234.149095	354243.547015	52.622746
3233.414222	354033.608558	52.627751
3232.639599	353825.838699	52.632756
3232.085921	353622.868384	52.637761
3231.495350	353432.882197	52.642765
3230.825778	353230.692156	52.647770
3230.307213	353010.510178	52.652775
3229.294946	352811.299398	52.657780
3228.648658	352614.244085	52.662785
3228.254012	352410.175016	52.667789
3227.429067	352216.225882	52.672794
3226.941201	351998.783383	52.677799
3226.295295	351804.957119	52.682804
3225.593606	351598.464838	52.687809
3225.033806	351401.671275	52.692813
3223.989391	351194.442685	52.697818
3223.506670	350984.375803	52.702823
3222.836220	350785.485097	52.707828
3222.081816	350592.002452	52.712833
3221.821687	350381.694403	52.717837
3220.816820	350172.648623	52.722842
3219.949452	349977.425546	52.727847
3219.577813	349782.097903	52.732852
3218.957723	349577.621040	52.737857
3218.260098	349378.296803	52.742861
3217.374479	349176.049238	52.747866
3216.839980	348977.588535	52.752871
3216.057343	348778.351924	52.757876
3215.260668	348575.782670	52.762881
3214.854018	348372.947367	52.767885
3214.245711	348182.843607	52.772890
3213.639313	347973.446462	52.777895
3212.894059	347773.767655	52.782900
3212.351942	347571.739876	52.787905
3211.717056	347370.184182	52.792909
3210.599655	347179.699412	52.797914
3210.425270	346970.153833	52.802919
3209.517727	346767.773745	52.807924
3208.997348	346573.221934	52.812929
3208.341545	346368.051743	52.817933
3207.605877	346165.260539	52.822938
3206.582753	345971.447974	52.827943
3206.032784	345776.949042	52.832948
3205.483640	345578.682303	52.837953
3204.673455	345375.874650	52.842957
3203.787159	345187.433827	52.847962
3203.454102	344981.698583	52.852967
3202.860069	344793.413876	52.857972
3202.026251	344604.988319	52.862977
3201.457384	344404.455358	52.867981
3200.701379	344200.998717	52.872986
3200.351737	344005.265869	52.877991
3199.327910	343809.460847	52.882996
3198.606697	343619.563470	52.888001
3197.972835	343417.841119	52.893005
3197.077061	343227.435576	52.898010
3196.697590	343023.915334	52.903015
3196.027631	342835.890948	52.908020
3195.195829	342645.117078	52.913025
3194.541961	342444.081875	52.918029
3193.599684	342257.295110	52.923034
3193.196984	342063.753373	52.928039
3192.578952	341876.583236	52.933044
3191.548363	341678.506897	52.938049
3191.236865	341487.494354	52.943053
3190.344876	341297.743961	52.948058
3190.201583	341109.936378	52.953063
3189.257059	340914.618527	52.958068
3188.402577	340734.940579	52.963073
3188.042336	340534.514484	52.968077
3187.276010	340350.621407	52.973082
3186.612314	340158.871371	52.978087
3185.726068	339973.723399	52.983092
3185.033702	339786.940527	52.988097
3184.573975	339595.945618	52.993101
3183.952455	339413.503298	52.998106
3183.521036	339219.371756	53.003111
3182.914293	339029.060238	53.008116
3181.995857	338827.113310	53.013121
3181.328528	338639.024856	53.018125
3180.574861	338454.946072	53.023130
3180.009416	338258.236319	53.028135
3179.123727	338060.965683	53.033140
3178.627630	337862.029082	53.038145
3177.825995	337680.628564	53.043149
3177.088988	337503.519413	53.048154
3176.947482	337309.259877	53.053159
3176.035109	337116.496358	53.058164
3175.461885	336930.348200	53.063169
3174.859553	336740.360191	53.068173
3173.852842	336544.198751	53.073178
3173.222232	336352.279403	53.078183
3172.681902	336163.629134	53.083188
3171.606617	335967.935063	53.088193
3171.236185	335785.570129	53.093197
3170.152636	335604.310336	53.098202
3169.604142	335421.743472	53.103207
3168.931383	335233.162451	53.108212
3168.178443	335051.263357	53.113217
3167.791350	334860.726822	53.118221
3167.053723	334687.810725	53.123226
3166.554488	334498.131008	53.128231
3165.982616	334318.212444	53.133236
3165.125259	334123.598698	53.138241
3164.705620	333941.389351	53.143245
3163.799152	333756.227086	53.148250
3163.276743	333565.097387	53.153255
3162.520940	333381.285002	53.158260
3161.409878	333200.201409	53.163265
3160.953469	333020.108466	53.168269
3160.249257	332845.833218	53.173274
3159.524774	332661.275713	53.178279
3158.884011	332472.249318	53.183284
3158.114183	332305.315044	53.188289
3157.857665	332118.849107	53.193293
3157.107476	331944.247962	53.198298
3156.459268	331760.847134	53.203303
3155.605815	331572.412090	53.208308
3155.086131	331389.830110	53.213313
3154.480377	331210.876397	53.218317
3153.681325	331040.328698	53.223322
3152.997155	330855.938381	53.228327
3152.691408	330675.331992	53.233332
3151.650935	330494.663188	53.238337
3150.968864	330303.957374	53.243341
3150.118631	330135.936091	53.248346
3149.876972	329950.327841	53.253351
3149.224871	329757.120898	53.258356
3148.379495	329581.128916	53.263361
3147.645742	329403.794983	53.268365
3146.769674	329232.695194	53.273370
3146.360339	329040.033552	53.278375
3145.579646	328858.785034	53.283380
3144.906117	328686.098942	53.288385
3144.563689	328501.190457	53.293389
3143.790139	328336.259067	53.298394
3143.096819	328141.857913	53.303399
3142.407122	327963.418881	53.308404
3141.670807	327792.548339	53.313409
3141.362853	327606.512018	53.318413
3140.381327	327426.870391	53.323418
3139.849130	327236.871474	53.328423
3139.255958	327060.426422	53.333428
3138.376594	326891.893387	53.338433
3137.881242	326699.061279	53.343437
3137.103233	326522.033222	53.348442
3136.422140	326342.596181	53.353447
3135.871885	326157.282184	53.358452
3135.250643	325981.144687	53.363457
3134.341033	325799.833059	53.368461
3133.388797	325627.617124	53.373466
3133.175927	325448.282218	53.378471
3132.432975	325264.855262	53.383476
3131.575273	325086.283553	53.388481
3131.395746	324917.610171	53.393485
3130.226092	324734.300453	53.398490
3129.482198	324561.158171	53.403495
3128.896096	324387.328578	53.408500
3128.350696	324215.529047	53.413505
3127.728056	324030.221653	53.418509
3127.103012	323863.067873	53.423514
3126.587138	323673.032521	53.428519
3125.887981	323498.989811	53.433524
3124.830035	323330.019345	53.438529
3124.530314	323147.357782	53.443533
3123.702629	322973.843549	53.448538
3123.062839	322793.119159	53.453543
3122.425802	322617.689902	53.458548
3121.589804	322444.812441	53.463553
3121.005433	322270.316212	53.468557
3120.148316	322102.966531	53.473562
3119.638053	321921.506894	53.478567
3118.922124	321736.998569	53.483572
3118.139134	321568.974132	53.488577
3117.539577	321400.487500	53.493581
3116.556746	321228.802089	53.498586
3115.789506	321052.702810	53.503591
3115.165042	320899.903608	53.508596
3114.569558	320718.964208	53.513601
3114.055761	320553.619666	53.518605
3113.398676	320395.401375	53.523610
3112.956885	320228.160656	53.528615
3112.310850	320055.732223	53.533620
3111.536120	319884.087689	53.538625
3110.876797	319713.519441	53.543629
3110.102802	319545.820784	53.548634
3109.518647	319373.610429	53.553639
3109.009936	319203.119249	53.558644
3108.123256	319036.557833	53.563649
3107.954439	318860.563302	53.568653
3107.045075	318696.856652	53.573658
3106.156192	318509.695539	53.578663
3105.947877	318338.696919	53.583668
3105.135842	318160.587607	53.588673
3104.587493	317990.915288	53.593677
3103.762639	317827.830320	53.598682
3103.183663	317645.303587	53.603687
3102.238641	317479.563454	53.608692
3101.650619	317299.405529	53.613697
3101.109566	317121.225937	53.618701
3100.259096	316964.203713	53.623706
3099.709712	316791.091948	53.628711
3099.041155	316620.748734	53.633716
3098.270705	316447.798656	53.638721
3097.758226	316268.594466	53.643725
3097.112769	316116.860226	53.648730
3096.135910	315939.536801	53.653735
3095.653611	315775.146498	53.658740
3095.005486	315599.731119	53.663745
3094.380236	315421.816413	53.668749
3093.484928	315255.886425	53.673754
3092.819791	315095.547149	53.678759
3092.079958	314923.557199	53.683764
3091.458507	314758.194188	53.688769
3090.922466	314585.738544	53.693773
3090.475535	314420.754791	53.698778
3089.884382	314259.307569	53.703783
3089.164246	314089.655759	53.708788
3088.111226	313916.236799	53.713793
3087.845589	313731.285222	53.718797
3086.794514	313570.699088	53.723802
3086.225805	313411.207716	53.728807
3085.667284	313244.482769	53.733812
3085.199460	313078.405269	53.738817
3084.410486	312899.620917	53.743821
3083.513582	312727.397579	53.748826
3082.928831	312565.131917	53.753831
3082.117071	312393.785815	53.758836
3081.477529	312226.919331	53.763841
3080.984515	312064.994905	53.768845
3080.214711	311904.489103	53.773850
3079.465397	311736.900786	53.778855
3078.735292	311567.322969	53.783860
3078.077774	311413.852275	53.788865
3077.377633	311242.384869	53.793869
3076.786834	311083.657524	53.798874
3075.957760	310912.133625	53.803879
3075.261621	310762.360489	53.808884
3074.583062	310607.389631	53.813889
3074.322500	310434.349043	53.818893
3073.626518	310282.461704	53.823898
3072.985689	310116.356228	53.828903
3072.252075	309942.702219	53.833908
3071.346893	309786.314642	53.838913
3070.395534	309616.692549	53.843917
3069.900241	309457.667743	53.848922
3069.637225	309306.016198	53.853927
3069.002505	309140.774176	53.858932
3068.044928	308996.362276	53.863937
3067.658732	308820.818180	53.868941
3066.643490	308664.828516	53.873946
3066.214629	308499.094670	53.878951
3065.642992	308333.485051	53.883956
3064.687487	308166.433522	53.888961
3064.237033	308003.172521	53.893965
3063.645663	307851.087282	53.898970
3062.932826	307685.753787	53.903975
3062.431403	307520.310223	53.908980
3061.429347	307360.166013	53.913985
3061.301591	307193.338701	53.918989
3060.331880	307033.367214	53.923994
3059.705800	306860.786797	53.928999
3059.268519	306699.661098	53.934004
3058.261502	306528.795758	53.939009
3057.697690	306358.955064	53.944013
3056.650516	306202.941928	53.949018
3056.330008	306048.952702	53.954023
3055.539537	305880.929832	53.959028
3054.613637	305729.022337	53.964033
3054.216195	305558.619507	53.969037
3053.397885	305405.064826	53.974042
3052.872437	305248.356829	53.979047
3052.176718	305091.853855	53.984052
3051.445973	304935.483570	53.989057
3050.901947	304768.489861	53.994061
3050.073770	304618.577435	53.999066
3049.919137	304450.273900	54.004071
3049.104733	304297.150269	54.009076
3048.012475	304125.735112	54.014081
3047.841652	303965.582589	54.019085
3046.848546	303802.147596	54.024090
3046.061359	303643.110880	54.029095
3045.460843	303484.859353	54.034100
3044.902657	303332.432638	54.039105
3044.325843	303174.202483	54.044109
3043.756709	303015.054166	54.049114
3043.061568	302847.674644	54.054119
3042.457648	302685.781149	54.059124
3041.605471	302530.726192	54.064129
3040.926505	302365.329912	54.069133
3040.488719	302214.538272	54.074138
3039.893523	302058.983765	54.079143
3039.021520	301893.031793	54.084148
3038.031032	301725.112030	54.089153
3037.615482	301565.224806	54.094157
3036.816190	301419.582823	54.099162
3036.108293	301260.250873	54.104167
3035.724481	301088.210740	54.109172
3034.845944	300941.027407	54.114177
3034.575725	300774.597001	54.119181
3033.697845	300622.651068	54.124186
3032.618658	300461.263362	54.129191
3032.250768	300303.557416	54.134196
3031.502299	300154.697457	54.139201
3030.838033	299982.242117	54.144205
3030.187100	299831.812974	54.149210
3029.714231	299676.898878	54.154215
3029.028189	299515.397082	54.159220
3027.947077	299359.509357	54.164225
3027.710818	299198.369002	54.169229
3026.775055	299044.087841	54.174234
3026.121281	298891.697374	54.179239
3025.565813	298733.408421	54.184244
3024.683492	298576.317051	54.189249
3024.245901	298424.070222	54.194253
3023.585830	298277.461142	54.199258
3022.729897	298117.589312	54.204263
3022.685133	297961.230702	54.209268
3021.787255	297810.100324	54.214273
3021.437159	297639.986771	54.219277
3020.577122	297479.427415	54.224282
3019.748814	297319.321298	54.229287
3019.143778	297164.349475	54.234292
3018.303946	297014.788192	54.239297
3017.885417	296842.520042	54.244301
3017.075569	296693.539494	54.249306
3016.352858	296531.633300	54.254311
3016.179317	296365.616273	54.259316
3014.962452	296217.107239	54.264321
3014.146308	296060.054158	54.269325
3013.716057	295891.708919	54.274330
3013.088200	295741.119872	54.279335
3012.400505	295573.451780	54.284340
3011.523411	295413.631918	54.289345
3011.064370	295260.570947	54.294349
3010.195264	295113.865139	54.299354
3009.453766	294959.065945	54.304359
3009.497933	294798.412176	54.309364
3008.203810	294642.936192	54.314369
3008.043544	294482.034393	54.319373
3006.980659	294335.358700	54.324378
3006.638297	294175.656979	54.329383
3006.064562	294017.468858	54.334388
3005.106603	293862.422973	54.339393
3004.609704	293688.636476	54.344397
3004.144445	293527.400220	54.349402
3003.368700	293375.406694	54.354407
3002.898418	293212.337355	54.359412
3001.872787	293054.016321	54.364417
3001.268528	292889.821921	54.369421
3000.601812	292727.649213	54.374426
2999.814740	292559.459661	54.379431
2999.070506	292410.796733	54.384436
2998.496473	292260.680596	54.389441
2998.508810	292097.228470	54.394445
2997.530252	291935.053634	54.399450
2996.823509	291776.859534	54.404455
2996.377436	291612.435465	54.409460
2995.208926	291459.000270	54.414465
2994.878310	291280.932571	54.419469
2994.063377	291130.446383	54.424474
2993.479632	290959.804117	54.429479
2992.549158	290801.695744	54.434484
2991.771161	290645.040262	54.439489
2991.420193	290479.556230	54.444493
2990.749715	290323.800374	54.449498
2990.053181	290172.250716	54.454503
2989.643107	289999.313713	54.459508
2988.533122	289844.238367	54.464513
2988.001774	289677.407136	54.469517
2987.433715	289518.323804	54.474522
2986.728468	289359.847854	54.479527
2986.107754	289198.658853	54.484532
2985.027642	289048.137068	54.489537
2985.015702	288883.056837	54.494541
2984.285811	288732.963344	54.499546
2983.494403	288558.914302	54.504551
2982.954986	288391.115826	54.509556
2982.108384	288243.383602	54.514561
2981.830373	288077.020714	54.519565
2981.080896	287919.467839	54.524570
2980.400292	287748.278668	54.529575
2979.638641	287589.657905	54.534580
2978.850166	287428.851070	54.539585
2978.819198	287252.923653	54.544589
2977.881690	287092.420391	54.549594
2976.986713	286932.368743	54.554599
2976.495438	286767.898101	54.559604
2975.679198	286606.356697	54.564609
2975.069954	286436.072406	54.569613
2974.406551	286276.671438	54.574618
2973.377322	286104.645239	54.579623
2972.847355	285945.910642	54.584628
2972.342662	285795.500020	54.589633
2971.656783	285622.935359	54.594637
2971.225628	285464.414131	54.599642
2970.634943	285300.060437	54.604647
2969.886400	285133.643279	54.609652
2968.989410	284963.505742	54.614657
2968.408696	284787.842433	54.619661
2967.690184	284635.784321	54.624666
2966.876798	284467.492518	54.629671
2966.397518	284301.923790	54.634676
2965.615493	284156.675549	54.639681
2965.105203	283986.450944	54.644685
2964.256968	283826.899984	54.649690
2963.423708	283662.303903	54.654695
2962.675253	283506.531794	54.659700
2961.896612	283351.783139	54.664705
2961.206279	283194.881130	54.669709
2960.772041	283038.575239	54.674714
2960.337506	282884.612420	54.679719
2959.881925	282722.859617	54.684724
2958.996525	282563.619748	54.689729
2958.352148	282403.246547	54.694733
2957.934308	282239.119080	54.699738
2957.106586	282083.206280	54.704743
2956.330003	281913.430620	54.709748
2955.602195	281751.007514	54.714753
2954.950058	281594.863044	54.719757
2954.232845	281447.260703	54.724762
2953.590925	281281.945965	54.729767
2953.113012	281121.953560	54.734772
2952.288982	280956.718502	54.739777
2951.899251	280790.344991	54.744781
2951.260918	280625.284206	54.749786
2950.233458	280466.626585	54.754791
2949.955280	280304.437571	54.759796
2949.010253	280139.297884	54.764801
2948.615344	279973.230628	54.769805
2947.958497	279821.135971	54.774810
2947.027010	279657.547611	54.779815
2946.740963	279483.364099	54.784820
2945.884537	279327.608041	54.789825
2945.427033	279164.453928	54.794829
2944.707789	279002.385423	54.799834
2944.034540	278833.611436	54.804839
2943.599276	278665.742079	54.809844
2942.585603	278502.039192	54.814849
2942.294057	278340.615998	54.819853
2941.522979	278170.838664	54.824858
2940.641407	277995.934188	54.829863
2940.202038	277834.305114	54.834868
2939.284147	277682.327877	54.839873
2938.637358	277510.034887	54.844877
2937.937181	277329.218424	54.849882
2937.373083	277166.412011	54.854887
2936.925384	277006.719769	54.859892
2936.197442	276847.835927	54.864897
2935.508263	276668.010928	54.869901
2935.108258	276510.374038	54.874906
2933.964216	276336.504216	54.879911
2933.660011	276159.037737	54.884916
2932.704318	276006.480590	54.889921
2932.166012	275837.379316	54.894925
2931.433755	275672.485555	54.899930
2930.719124	275512.377056	54.904935
2930.017827	275334.591380	54.909940
2929.552419	275172.813446	54.914945
2929.143657	275003.920861	54.919949
2928.140626	274838.764331	54.924954
2927.359407	274670.643823	54.929959
2926.888911	274505.886893	54.934964
2926.093510	274343.524492	54.939969
2925.859990	274174.858860	54.944973
2924.952410	274008.057258	54.949978
2924.012004	273850.072921	54.954983
2923.687729	273679.766230	54.959988
2922.884071	273512.948199	54.964993
2922.189214	273338.701656	54.969997
2921.636059	273179.586379	54.975002
2920.809269	273008.798976	54.980007
2920.168138	272836.912525	54.985012
2919.353814	272672.439335	54.990017
2918.473177	272510.854585	54.995021
2917.943946	272353.925869	55.000026
2917.778890	272187.337942	55.005031
2917.013804	272023.213581	55.010036
2916.219559	271859.832438	55.015041
2915.881086	271686.522908	55.020045
2915.127797	271515.876844	55.025050
2914.312266	271346.361264	55.030055
2913.842673	271157.027508	55.035060
2912.695457	270992.683629	55.040065
2911.948917	270818.139948	55.045069
2911.347081	270653.531508	55.050074
2910.676414	270497.516820	55.055079
2910.183844	270337.984804	55.060084
2909.309433	270177.774685	55.065089
2908.690175	270006.216270	55.070093
2908.416908	269834.883268	55.075098
2907.688889	269672.612607	55.080103
2907.225198	269500.825926	55.085108
2906.412299	269342.516359	55.090113
2905.665760	269171.182026	55.095117
2905.191423	269006.095307	55.100122
2904.698673	268836.172570	55.105127
2903.982588	268661.522667	55.110132
2903.103809	268500.447683	55.115137
2902.737912	268317.134162	55.120141
2902.038078	268144.952250	55.125146
2901.254585	267986.842100	55.130151
2900.767871	267803.395054	55.135156
2900.331959	267637.411225	55.140161
2899.427539	267456.679115	55.145165
2898.755046	267280.876649	55.150170
2898.064667	267110.145243	55.155175
2897.633165	266929.312974	55.160180
2897.035686	266756.962483	55.165185
2896.485802	266581.752080	55.170189
2895.664073	266407.348823	55.175194
2894.642324	266229.437222	55.180199
2894.320975	266049.810311	55.185204
2893.449743	265880.559653	55.190209
2892.530753	265706.248463	55.195213
2891.945198	265536.647090	55.200218
2891.345950	265353.804537	55.205223
2890.692791	265177.108408	55.210228
2889.808213	265013.641459	55.215233
2888.996687	264841.478397	55.220237
2888.925295	264677.220671	55.225242
2887.928680	264511.046581	55.230247
2887.226819	264333.263405	55.235252
2886.508127	264166.510633	55.240257
2886.267869	263996.880707	55.245261
2885.451624	263816.798294	55.250266
2884.901275	263640.494071	55.255271
2884.620483	263471.227357	55.260276
2883.617515	263292.702846	55.265281
2882.918467	263111.328834	55.270285
2882.277715	262942.348576	55.275290
2881.267676	262772.051600	55.280295
2880.865193	262600.232318	55.285300
2880.196771	262421.578895	55.290305
2879.490633	262250.979395	55.295309
2878.976014	262076.605885	55.300314
2878.125726	261902.234680	55.305319
2877.594732	261724.986089	55.310324
2876.459182	261556.084893	55.315329
2875.849569	261372.711206	55.320333
2875.239393	261220.408440	55.325338
2874.626778	261046.000095	55.330343
2874.001164	260872.408881	55.335348
2873.440041	260713.145909	55.340353
2872.929317	260537.321011	55.345357
2872.259516	260349.500640	55.350362
2871.678386	260184.689168	55.355367
2871.193568	260008.020066	55.360372
2870.479790	259828.942432	55.365377
2869.614886	259657.299933	55.370381
2869.401134	259467.090406	55.375386
2868.320094	259303.835745	55.380391
2867.732006	259130.086884	55.385396
2867.148987	258956.846690	55.390401
2866.244920	258774.718324	55.395405
2866.037295	258606.079499	55.400410
2864.860935	258427.432618	55.405415
2864.466356	258244.994764	55.410420
2863.469751	258078.493152	55.415425
2862.788731	257902.722458	55.420429
2862.356924	257724.467559	55.425434
2861.538151	257556.028095	55.430439
2860.854214	257380.920403	55.435444
2860.154288	257211.163532	55.440449
2859.855065	257032.175080	55.445453
2858.905092	256861.159222	55.450458
2858.266042	256696.104560	55.455463
2857.933558	256512.766868	55.460468
2856.982467	256342.209996	55.465473
2856.119282	256163.082327	55.470477
2855.564542	255989.254096	55.475482
2854.919352	255814.650842	55.480487
2854.480328	255639.200137	55.485492
2854.001527	255472.414726	55.490497
2853.119911	255296.703309	55.495501
2852.633389	255112.678122	55.500506
2851.729434	254939.364460	55.505511
2851.369314	254750.735497	55.510516
2850.354246	254585.945749	55.515521
2849.732951	254408.538517	55.520525
2849.239585	254239.311581	55.525530
2848.783746	254056.021045	55.530535
2847.899778	253888.970020	55.535540
2847.025182	253705.211312	55.540545
2846.358905	253528.652412	55.545549
2845.695862	253353.493845	55.550554
2844.810303	253188.888511	55.555559
2844.626487	253005.021103	55.560564
2843.790234	252844.381101	55.565569
2842.937839	252664.159788	55.570573
2842.542410	252484.401100	55.575578
2841.513944	252312.968600	55.580583
2841.333020	252138.575252	55.585588
2840.780445	251971.651744	55.590593
2839.764569	251787.458913	55.595597
2839.350092	251603.858650	55.600602
2838.467225	251434.619547	55.605607
2837.978761	251256.786832	55.610612
2836.973610	251089.732094	55.615617
2836.368334	250902.011728	55.620621
2835.906224	250737.749074	55.625626
2835.136633	250571.217811	55.630631
2834.523768	250399.415796	55.635636
2834.004825	250218.711281	55.640641
2833.371231	250038.687246	55.645645
2832.872407	249856.451956	55.650650
2831.903140	249688.578014	55.655655
2831.711934	249505.886945	55.660660
2830.648322	249330.592134	55.665665
2830.126793	249149.430825	55.670669
2829.777748	248963.021822	55.675674
2828.621698	248790.645403	55.680679
2828.123761	248603.954808	55.685684
2827.170411	248436.563534	55.690689
2826.696352	248252.085143	55.695693
2826.140056	248070.777798	55.700698
2825.321999	247902.907294	55.705703
2824.781938	247724.068006	55.710708
2824.023487	247557.130695	55.715713
2823.408192	247374.636626	55.720717
2822.870271	247199.490202	55.725722
2821.965971	247014.470276	55.730727
2821.556459	246836.044310	55.735732
2820.612427	246669.086461	55.740737
2820.148290	246483.462729	55.745741
2819.654607	246297.309133	55.750746
2818.583578	246122.095634	55.755751
2818.152628	245952.892782	55.760756
2817.556908	245773.504462	55.765761
2816.933185	245596.285391	55.770765
2816.265472	245411.484740	55.775770
2815.708391	245239.628830	55.780775
2815.005071	245052.797046	55.785780
2813.986407	244877.576825	55.790785
2813.568527	244696.149965	55.795789
2813.169695	244515.433366	55.800794
2812.355738	244338.347913	55.805799
2811.821711	244154.240836	55.810804
2810.932795	243969.324389	55.815809
2810.282119	243793.996386	55.820813
2809.855515	243617.003353	55.825818
2809.257027	243436.217983	55.830823
2808.504039	243244.176219	55.835828
2807.420499	243071.718914	55.840833
2806.831717	242887.571368	55.845837
2806.450433	242704.842743	55.850842
2805.336737	242531.550595	55.855847
2805.022728	242348.811832	55.860852
2804.346140	242169.390277	55.865857
2803.556898	241995.843772	55.870861
2803.324027	241811.590512	55.875866
2802.389352	241630.682708	55.880871
2801.869221	241445.100379	55.885876
2800.901241	241272.525402	55.890881
2800.259151	241091.826714	55.895885
2800.054553	240903.750624	55.900890
2798.900680	240729.779833	55.905895
2798.544737	240547.075867	55.910900
2797.822220	240360.559602	55.915905
2797.207145	240176.700403	55.920909
2796.524596	239998.836356	55.925914
2795.805992	239818.992054	55.930919
2795.405262	239624.277348	55.935924
2794.807676	239444.134353	55.940929
2793.995458	239267.132290	55.945933
2793.681431	239076.300838	55.950938
2792.435111	238894.046042	55.955943
2791.911375	238703.935962	55.960948
2791.295185	238522.447765	55.965953
2790.439064	238345.326774	55.970957
2789.692430	238161.466183	55.975962
2788.876930	237983.830052	55.980967
2788.770416	237790.599760	55.985972
2787.962510	237626.000620	55.990977
2787.081976	237439.361392	55.995981
2786.771368	237245.273143	56.000986
2785.897034	237067.495034	56.005991
2784.979751	236882.466813	56.010996
2784.144897	236701.500072	56.016001
2783.563964	236525.153301	56.021005
2782.991674	236348.296178	56.026010
2782.079890	236182.646220	56.031015
2781.911213	235995.565750	56.036020
2781.068689	235814.932768	56.041025
2780.509503	235647.801854	56.046029
2779.733370	235466.598764	56.051034
2778.962170	235294.281970	56.056039
2778.386516	235106.834670	56.061044
2777.888119	234933.787766	56.066049
2777.365620	234751.348990	56.071053
2776.800851	234561.889362	56.076058
2775.986147	234389.479133	56.081063
2775.389600	234195.976565	56.086068
2774.779766	234015.691861	56.091073
2774.024993	233832.374861	56.096077
2773.662877	233640.924219	56.101082
2773.051209	233462.805172	56.106087
2772.201939	233276.143049	56.111092
2771.531601	233086.932113	56.116097
2770.771121	232909.779767	56.121101
2770.119305	232716.416168	56.126106
2769.312409	232541.054245	56.131111
2768.752062	232351.878252	56.136116
2768.337321	232171.642440	56.141121
2767.423731	231979.976855	56.146125
2767.085700	231790.435751	56.151130
2766.165213	231609.237135	56.156135
2765.744967	231421.008383	56.161140
2765.143065	231239.479937	56.166145
2764.046851	231045.960955	56.171149
2763.994716	230855.307042	56.176154
2763.211756	230675.819895	56.181159
2762.498242	230485.449725	56.186164
2761.938292	230300.759157	56.191169
2761.085532	230103.791664	56.196173
2760.549173	229907.894820	56.201178
2759.599403	229723.980098	56.206183
2759.028538	229531.323210	56.211188
2758.441297	229350.279963	56.216193
2757.609764	229165.838419	56.221197
2757.156196	228960.866102	56.226202
2756.244647	228784.483953	56.231207
2755.689337	228598.472135	56.236212
2754.902626	228415.323602	56.241217
2754.319608	228229.800724	56.246221
2753.668148	228026.618772	56.251226
2752.911979	227848.151513	56.256231
2752.148838	227663.905982	56.261236
2751.361250	227483.382076	56.266241
2750.809388	227307.276948	56.271245
2750.469097	227114.334235	56.276250
2749.596859	226928.147044	56.281255
2749.395916	226743.534379	56.286260
2748.817261	226555.850221	56.291265
2747.684203	226371.233229	56.296269
2746.842864	226172.846970	56.301274
2746.066255	225990.835034	56.306279
2745.740003	225806.829873	56.311284
2744.972052	225629.947722	56.316289
2744.550888	225443.246822	56.321293
2743.993769	225251.895839	56.326298
2743.010297	225067.067100	56.331303
2742.341078	224879.579297	56.336308
2741.736169	224688.975556	56.341313
2740.732003	224508.492381	56.346317
2740.659817	224319.345493	56.351322
2739.795693	224135.442008	56.356327
2738.870767	223938.041889	56.361332
2738.067314	223764.721126	56.366337
2737.648545	223577.578587	56.371341
2737.283135	223385.043223	56.376346
2735.999829	223208.184340	56.381351
2735.396363	223016.705980	56.386356
2734.885483	222841.507780	56.391361
2734.190864	222658.000963	56.396365
2733.608166	222480.969104	56.401370
2732.865315	222307.680139	56.406375
2732.247870	222112.259948	56.411380
2731.803052	221929.415430	56.416385
2730.915558	221747.074272	56.421389
2730.312359	221554.606550	56.426394
2729.709429	221378.713375	56.431399
2728.867956	221196.455349	56.436404
2728.370081	221008.516827	56.441409
2727.225805	220831.768666	56.446413
2727.134262	220640.546103	56.451418
2726.393949	220462.220004	56.456423
2725.635008	220278.805463	56.461428
2725.133138	220095.057876	56.466433
2724.168755	219918.016059	56.471437
2724.169488	219732.216694	56.476442
2723.348696	219552.008835	56.481447
2722.884154	219357.615374	56.486452
2722.267643	219165.270464	56.491457
2721.274962	218976.448015	56.496461
2721.122815	218785.278028	56.501466
2720.352832	218597.274151	56.506471
2719.820428	218406.394517	56.511476
2719.157146	218206.358376	56.516481
2718.423431	218020.005053	56.521485
2717.841751	217818.302279	56.526490
2716.848732	217622.507873	56.531495
2715.947470	217427.259551	56.536500
2715.282025	217233.680102	56.541505
2714.754176	217051.026307	56.546509
2714.012133	216854.074123	56.551514
2713.147892	216673.803986	56.556519
2712.716248	216490.614524	56.561524
2712.405628	216295.046669	56.566529
2711.245829	216110.000573	56.571533
2710.798015	215909.834977	56.576538
2710.040631	215733.025306	56.581543
2709.236496	215544.080311	56.586548
2708.924458	215347.535250	56.591553
2707.843158	215163.039326	56.596557
2707.289391	214977.594797	56.601562
2706.763115	214790.733548	56.606567
2706.132255	214595.755853	56.611572
2705.051787	214418.211595	56.616577
2704.387853	214228.102483	56.621581
2704.154963	214043.666150	56.626586
2703.308382	213861.898665	56.631591
2702.708459	213669.108040	56.636596
2702.053508	213489.296839	56.641601
2701.200839	213307.977322	56.646605
2700.738465	213115.484723	56.651610
2700.112883	212937.706887	56.656615
2699.412461	212738.188941	56.661620
2698.885186	212547.872071	56.666625
2698.053274	212375.996109	56.671629
2697.558081	212169.765138	56.676634
2696.780073	211991.657632	56.681639
2696.378575	211796.842770	56.686644
2695.854862	211608.068172	56.691649
2694.904069	211418.356273	56.696653
2694.487913	211218.734330	56.701658
2693.636954	211031.769708	56.706663
2693.207601	210838.324042	56.711668
2692.383835	210654.169064	56.716673
2691.637905	210463.969352	56.721677
2690.706141	210268.734030	56.726682
2689.953520	210076.118286	56.731687
2689.564683	209885.418285	56.736692
2688.874042	209695.695783	56.741697
2688.206656	209507.828392	56.746701
2687.486052	209308.209799	56.751706
2686.549944	209135.951814	56.756711
2685.956549	208942.843427	56.761716
2685.337719	208763.765238	56.766721
2684.686186	208582.707284	56.771725
2684.222319	208388.192837	56.776730
2683.546296	208201.514422	56.781735
2682.687000	208022.909211	56.786740
2682.480343	207836.526651	56.791745
2681.642885	207642.442847	56.796749
2681.025288	207448.337564	56.801754
2680.051491	207263.503721	56.806759
2679.523106	207068.736446	56.811764
2679.084260	206894.166065	56.816769
2678.602007	206703.668933	56.821773
2677.986025	206502.744806	56.826778
2676.987738	206311.694325	56.831783
2676.447327	206128.258924	56.836788
2675.709672	205929.455934	56.841793
2674.944577	205748.984460	56.846797
2674.587307	205549.511609	56.851802
2673.718019	205362.898104	56.856807
2673.189800	205168.557016	56.861812
2672.572681	204981.344810	56.866817
2671.484701	204796.180406	56.871821
2670.907393	204600.194540	56.876826
2670.309616	204413.859224	56.881831
2669.372839	204227.120060	56.886836
2669.003277	204045.674899	56.891841
2668.261446	203862.074901	56.896845
2667.777714	203665.097460	56.901850
2667.144659	203476.314596	56.906855
2666.348736	203285.458335	56.911860
2665.871839	203087.565518	56.916865
2664.977023	202910.826760	56.921869
2664.409113	202713.853218	56.926874
2663.853463	202535.382063	56.931879
2662.939797	202342.613276	56.936884
2662.478591	202147.991843	56.941889
2661.428094	201965.248619	56.946893
2660.967084	201769.712205	56.951898
2660.391670	201589.796445	56.956903
2659.537133	201404.249791	56.961908
2658.977163	201217.282715	56.966913
2657.945836	201038.217239	56.971917
2657.743190	200845.226468	56.976922
2657.086600	200660.147254	56.981927
2656.747140	200469.610064	56.986932
2655.866257	200291.350350	56.991937
2655.145769	200097.540732	56.996941
2654.399270	199902.934223	57.001946
2653.881327	199721.450246	57.006951
2652.852509	199532.997972	57.011956
2652.518203	199331.532885	57.016961
2651.581336	199148.297481	57.021965
2651.430414	198966.185261	57.026970
2650.739495	198784.795463	57.031975
2650.002997	198588.906869	57.036980
2649.509647	198399.724759	57.041985
2648.837136	198212.455007	57.046989
2648.473858	198010.299602	57.051994
2647.515368	197824.692595	57.056999
2646.703181	197627.279819	57.062004
2646.051981	197431.623755	57.067009
2645.163957	197243.577187	57.072013
2644.588853	197039.448543	57.077018
2644.135703	196850.341962	57.082023
2643.430792	196655.040872	57.087028
2642.780263	196466.565010	57.092033
2642.157087	196278.747175	57.097037
2641.520602	196080.943390	57.102042
2640.625410	195893.131874	57.107047
2640.160230	195708.459470	57.112052
2639.722457	195507.394402	57.117057
2638.771381	195308.154672	57.122061
2637.999254	195114.855048	57.127066
2637.576440	194923.180413	57.132071
2636.968466	194733.737115	57.137076
2636.147708	194534.352520	57.142081
2635.252577	194349.027870	57.147085
2635.100785	194155.722684	57.152090
2634.291821	193964.876288	57.157095
2633.042726	193771.199289	57.162100
2632.805212	193570.199229	57.167105
2632.272440	193378.051642	57.172109
2631.651021	193182.012636	57.177114
2631.079378	192998.512116	57.182119
2630.289393	192803.455586	57.187124
2629.552135	192608.302404	57.192129
2628.873450	192418.013844	57.197133
2628.417453	192214.483708	57.202138
2627.453457	192026.799289	57.207143
2626.820550	191824.965567	57.212148
2626.534895	191628.459649	57.217153
2625.660145	191438.129604	57.222157
2625.154544	191237.537745	57.227162
2624.595228	191057.401452	57.232167
2623.924519	190852.562331	57.237172
2623.024507	190649.656151	57.242177
2622.464607	190459.114658	57.247181
2621.929918	190256.762956	57.252186
2621.239972	190066.650754	57.257191
2620.198717	189864.202840	57.262196
2619.825680	189661.929816	57.267201
2618.872242	189467.154279	57.272205
2618.219631	189273.896776	57.277210
2617.388714	189086.978773	57.282215
2616.762631	188890.601561	57.287220
2616.529319	188704.035677	57.292225
2615.484062	188507.090339	57.297229
2615.091732	188315.233157	57.302234
2614.281153	188125.173277	57.307239
2613.631509	187923.066001	57.312244
2613.053533	187731.724067	57.317249
2612.555826	187535.599339	57.322253
2611.784108	187338.195736	57.327258
2611.080223	187151.087194	57.332263
2610.707414	186951.662813	57.337268
2609.978591	186752.728247	57.342273
2608.864870	186564.134916	57.347277
2608.400163	186356.356572	57.352282
2607.788300	186166.782094	57.357287
2607.062009	185976.603158	57.362292
2606.612893	185780.389123	57.367297
2605.618288	185585.979795	57.372301
2605.017930	185391.559717	57.377306
2604.242676	185203.363623	57.382311
2603.530181	185016.812172	57.387316
2603.193927	184821.716609	57.392321
2602.123779	184629.384235	57.397325
2601.739054	184426.716051	57.402330
2601.454688	184242.199001	57.407335
2600.433074	184047.329870	57.412340
2599.873466	183840.201413	57.417345
2599.186626	183655.648774	57.422349
2598.592698	183456.567339	57.427354
2597.865839	183260.433707	57.432359
2597.329579	183073.849687	57.437364
2596.447048	182871.165660	57.442369
2595.630801	182681.739989	57.447373
2595.101931	182482.092897	57.452378
2594.497115	182287.610673	57.457383
2593.803178	182095.649421	57.462388
2593.344221	181904.389576	57.467393
2592.424906	181712.898213	57.472397
2592.003393	181510.134692	57.477402
2590.816602	181324.500725	57.482407
2590.330590	181130.920696	57.487412
2590.295661	180925.872558	57.492417
2589.327362	180736.415800	57.497421
2588.490050	180537.538809	57.502426
2588.149126	180345.834626	57.507431
2587.250452	180151.395787	57.512436
2586.843783	179951.295730	57.517441
2586.006756	179762.064142	57.522445
2585.180644	179551.907229	57.527450
2584.777271	179358.131270	57.532455
2583.738631	179168.565378	57.537460
2583.183636	178973.428725	57.542465
2582.411208	178789.978746	57.547469
2581.898310	178585.704398	57.552474
2581.260348	178384.414536	57.557479
2580.464287	178202.255538	57.562484
2579.797218	178011.796458	57.567489
2579.170697	177827.729723	57.572493
2578.712948	177626.580284	57.577498
2577.769032	177434.870308	57.582503
2577.259345	177239.581874	57.587508
2576.686058	177046.466707	57.592513
2575.824196	176855.420514	57.597517
2575.287454	176664.717978	57.602522
2574.557622	176475.840305	57.607527
2573.962761	176270.852541	57.612532
2573.418716	176081.184091	57.617537
2572.476398	175891.516028	57.622541
2572.098471	175688.150245	57.627546
2571.610476	175498.971634	57.632551
2570.616431	175301.047287	57.637556
2570.084806	175103.890058	57.642561
2569.426912	174913.443773	57.647565
2569.001288	174718.319306	57.652570
2568.136903	174521.141314	57.657575
2567.610079	174317.984009	57.662580
2566.928216	174116.785480	57.667585
2566.434014	173933.910713	57.672589
2565.793994	173719.556818	57.677594
2564.985420	173527.016988	57.682599
2563.662133	173325.720559	57.687604
2563.624612	173131.559710	57.692609
2562.635287	172936.011748	57.697613
2562.145364	172737.892898	57.702618
2561.337293	172546.515038	57.707623
2560.703832	172346.131668	57.712628
2560.345611	172153.794170	57.717633
2559.434385	171963.020484	57.722637
2558.677157	171771.867223	57.727642
2558.149399	171568.317074	57.732647
2557.272703	171373.598328	57.737652
2557.067827	171168.689179	57.742657
2556.203450	170983.572062	57.747661
2555.909090	170786.169612	57.752666
2554.833074	170590.227329	57.757671
2554.066253	170389.798747	57.762676
2553.693520	170205.675650	57.767681
2552.553517	170013.167310	57.772685
2552.448291	169812.369808	57.777690
2551.835533	169614.604092	57.782695
2550.872122	169417.619813	57.787700
2550.191812	169219.256418	57.792705
2549.558770	169022.107357	57.797709
2548.655198	168827.405623	57.802714
2548.021388	168633.946504	57.807719
2547.665036	168437.595895	57.812724
2547.369900	168238.273660	57.817729
2546.212290	168056.218110	57.822733
2545.403355	167850.633843	57.827738
2544.809261	167651.018714	57.832743
2543.882300	167463.563194	57.837748
2543.345153	167270.591612	57.842753
2542.707121	167074.788603	57.847757
2542.210767	166880.286622	57.852762
2541.636638	166694.393938	57.857767
2540.903343	166500.440103	57.862772
2540.406560	166296.556899	57.867777
2539.481323	166104.034269	57.872781
2539.145011	165912.525567	57.877786
2538.571791	165705.822101	57.882791
2537.849766	165523.073989	57.887796
2537.376343	165320.858144	57.892801
2536.472557	165121.610709	57.897805
2535.879698	164920.204328	57.902810
2535.096285	164736.961203	57.907815
2533.984141	164533.286898	57.912820
2533.976226	164323.831360	57.917825
2533.153115	164140.495770	57.922829
2532.795806	163943.800111	57.927834
2531.990266	163747.036673	57.932839
2531.122100	163525.274108	57.937844
2530.589943	163280.903648	57.942849
2529.895926	163085.931593	57.947853
2529.410068	162876.877938	57.952858
2528.771800	162692.236148	57.957863
2527.980010	162485.356560	57.962868
2527.715402	162282.564937	57.967873
2526.511739	162087.106870	57.972877
2526.005240	161888.640527	57.977882
2525.618783	161680.913029	57.982887
2524.241539	161485.485739	57.987892
2524.057000	161280.029817	57.992897
2523.074673	161095.755869	57.997901
2522.699414	160891.794509	58.002906
2522.195071	160686.952088	58.007911
2521.348389	160483.601754	58.012916
2520.936366	160276.979847	58.017921
2519.975252	160075.671461	58.022925
2519.291154	159877.702124	58.027930
2518.677397	159681.121231	58.032935
2517.619640	159486.302681	58.037940
2517.249669	159280.010480	58.042945
2516.593573	159085.461040	58.047949
2516.300768	158881.510902	58.052954
2515.275158	158691.370120	58.057959
2514.440026	158495.708144	58.062964
2514.218712	158288.266753	58.067969
2513.375956	158093.498147	58.072973
2512.651603	157886.291424	58.077978
2512.237161	157695.944795	58.082983
2511.211474	157492.169775	58.087988
2510.664215	157293.443316	58.092993
2509.799436	157095.683624	58.097997
2509.240305	156893.617946	58.103002
2508.815079	156700.176661	58.108007
2507.816999	156513.615635	58.113012
2507.458331	156304.695124	58.118017
2506.587950	156113.577760	58.123021
2506.023938	155911.404222	58.128026
2505.563623	155718.431669	58.133031
2504.694585	155522.791911	58.138036
2504.360250	155315.932921	58.143041
2503.258285	155103.578227	58.148045
2502.558192	154911.182147	58.153050
2502.104094	154716.345668	58.158055
2501.236289	154525.783413	58.163060
2500.992469	154318.611082	58.168065
2499.824355	154121.183645	58.173069
2499.452930	153921.597283	58.178074
2498.851213	153728.289847	58.183079
2497.754498	153535.049263	58.188084
2497.239798	153325.383738	58.193089
2496.576598	153143.669265	58.198093
2495.980605	152939.205162	58.203098
2495.287832	152742.066425	58.208103
2494.439418	152555.465389	58.213108
2493.922280	152352.657510	58.218113
2492.984099	152170.928374	58.223117
2492.406721	151968.412028	58.228122
2491.779695	151770.213663	58.233127
2490.976009	151596.207090	58.238132
2490.556740	151395.118194	58.243137
2489.431887	151210.119229	58.248141
2489.114940	151009.003765	58.253146
2488.726709	150826.788148	58.258151
2487.775190	150640.862498	58.263156
2487.358673	150443.782675	58.268161
2486.765767	150256.683891	58.273165
2486.122259	150056.528442	58.278170
2485.658402	149850.867826	58.283175
2484.801525	149664.653127	58.288180
2483.899756	149470.541208	58.293185
2483.233344	149274.995097	58.298189
2482.427134	149077.299000	58.303194
2482.256192	148888.425439	58.308199
2481.053806	148694.276861	58.313204
2480.708087	148501.035837	58.318209
2479.844357	148317.104950	58.323213
2479.093832	148123.549079	58.328218
2478.627464	147928.017564	58.333223
2477.858781	147739.398000	58.338228
2477.303502	147546.195943	58.343233
2476.689013	147350.475385	58.348237
2476.432157	147159.401577	58.353242
2475.635536	146962.314311	58.358247
2474.921486	146773.145334	58.363252
2474.353960	146564.014622	58.368257
2473.628332	146378.598841	58.373261
2472.785787	146185.869963	58.378266
2472.460140	145979.831029	58.383271
2471.602814	145780.651171	58.388276
2471.377068	145583.875965	58.393281
2470.275450	145385.296488	58.398285
2469.444658	145182.329227	58.403290
2468.822015	144974.564842	58.408295
2468.255110	144779.602439	58.413300
2467.937281	144578.057310	58.418305
2467.438367	144386.746400	58.423309
2466.624990	144184.405535	58.428314
2465.770965	143978.412684	58.433319
2464.772234	143778.365770	58.438324
2464.275776	143583.984229	58.443329
2463.706302	143381.660771	58.448333
2463.027262	143183.485819	58.453338
2462.660436	142980.294199	58.458343
2461.337832	142786.671269	58.463348
2460.894623	142592.567086	58.468353
2460.503062	142398.633838	58.473357
2459.769535	142203.370987	58.478362
2458.987404	142002.081431	58.483367
2458.369343	141798.136939	58.488372
2457.885699	141599.445687	58.493377
2456.964729	141409.668694	58.498381
2456.497268	141214.700358	58.503386
2455.898405	141019.957400	58.508391
2455.066948	140817.539930	58.513396
2454.225997	140613.206703	58.518401
2453.597071	140423.885120	58.523405
2452.911647	140227.953908	58.528410
2452.190163	140042.753390	58.533415
2451.530580	139843.440834	58.538420
2451.207757	139649.552353	58.543425
2450.179544	139447.327732	58.548429
2449.808669	139257.248364	58.553434
2449.079812	139059.413124	58.558439
2448.325164	138867.415022	58.563444
2447.585634	138656.281676	58.568449
2447.268332	138455.933089	58.573453
2446.518055	138257.331548	58.578458
2445.704794	138077.011074	58.583463
2445.038441	137879.237287	58.588468
2444.617428	137677.334980	58.593473
2443.595827	137484.003301	58.598477
2442.995671	137280.671053	58.603482
2442.935577	137084.572422	58.608487
2441.971154	136898.095979	58.613492
2441.475359	136690.965322	58.618497
2440.622203	136487.094253	58.623501
2439.824918	136283.889068	58.628506
2439.475001	136080.309479	58.633511
2438.464877	135885.970159	58.638516
2437.712843	135675.698581	58.643521
2437.234672	135485.177719	58.648525
2436.229200	135295.110096	58.653530
2436.022287	135088.770739	58.658535
2435.224214	134901.238962	58.663540
2434.716478	134702.216499	58.668545
2433.938964	134506.757020	58.673549
2433.303038	134307.528929	58.678554
2432.634532	134114.392239	58.683559
2431.883417	133917.217623	58.688564
2431.321062	133715.047528	58.693569
2430.579579	133514.584044	58.698573
2429.834087	133327.727414	58.703578
2429.294459	133121.874045	58.708583
2428.263941	132937.250029	58.713588
2427.950371	132734.488486	58.718593
2427.035640	132535.012020	58.723597
2426.624716	132337.387863	58.728602
2426.121096	132140.351378	58.733607
2425.145593	131950.186790	58.738612
2424.823678	131748.170322	58.743617
2423.656901	131571.871303	58.748621
2423.064346	131383.542429	58.753626
2422.916378	131182.023206	58.758631
2421.921483	130993.062103	58.763636
2421.310810	130795.823304	58.768641
2420.477816	130604.921170	58.773645
2419.893732	130413.193374	58.778650
2419.094153	130214.324686	58.783655
2418.175242	130016.276514	58.788660
2417.927648	129824.613710	58.793665
2417.263470	129638.238474	58.798669
2416.759145	129440.458889	58.803674
2416.012347	129246.948603	58.808679
2415.364074	129056.561187	58.813684
2414.912720	128857.558044	58.818689
2414.215321	128664.475807	58.823693
2413.480700	128458.814394	58.828698
2413.006442	128250.001578	58.833703
2412.092266	128059.282136	58.838708
2411.625883	127849.836065	58.843713
2411.078064	127660.305944	58.848717
2410.048409	127465.849603	58.853722
2409.596308	127261.117539	58.858727
2408.767051	127062.809528	58.863732
2407.938738	126863.080401	58.868737
2407.517087	126666.158439	58.873741
2406.944527	126467.115549	58.878746
2406.412389	126264.524479	58.883751
2405.432647	126065.371269	58.888756
2405.069811	125857.740031	58.893761
2404.765835	125658.127081	58.898765
2403.889765	125464.333691	58.903770
2403.126166	125256.910263	58.908775
2402.301955	125047.897939	58.913780
2401.752953	124847.694835	58.918785
2400.796279	124661.310814	58.923789
2399.952096	124463.773336	58.928794
2399.562624	124256.399861	58.933799
2398.605396	124065.867546	58.938804
2398.428088	123858.095242	58.943809
2397.566947	123668.096552	58.948813
2396.959779	123473.919265	58.953818
2396.654251	123269.803584	58.958823
2395.640655	123071.287337	58.963828
2394.643655	122859.551198	58.968833
2393.914271	122672.497351	58.973837
2393.240278	122474.261857	58.978842
2392.908683	122278.309958	58.983847
2391.850617	122087.655352	58.988852
2391.466623	121893.352608	58.993857
2390.868754	121692.038050	58.998861
2390.285719	121502.112292	59.003866
2389.548385	121308.339662	59.008871
2388.565885	121111.712341	59.013876
2388.288283	120912.981279	59.018881
2387.454387	120719.444135	59.023885
2386.700808	120518.963125	59.028890
2386.226282	120320.788329	59.033895
2385.381422	120134.481765	59.038900
2385.203476	119934.624980	59.043905
2384.410840	119734.410093	59.048909
2383.599758	119536.446946	59.053914
2383.184124	119336.841903	59.058919
2381.933119	119142.100205	59.063924
2381.872504	118936.899997	59.068929
2380.957588	118746.443737	59.073933
2380.434342	118546.893552	59.078938
2380.001849	118342.759978	59.083943
2378.778291	118154.134431	59.088948
2378.512047	117945.140520	59.093953
2377.649297	117746.532681	59.098957
2376.780055	117557.772794	59.103962
2376.372047	117356.690057	59.108967
2375.414863	117165.769716	59.113972
2375.031107	116962.432789	59.118977
2374.497246	116772.743170	59.123981
2373.621785	116577.770838	59.128986
2373.134754	116371.681096	59.133991
2372.473009	116177.661788	59.138996
2372.130947	115976.998339	59.144001
2371.318983	115770.482560	59.149005
2370.585236	115570.220819	59.154010
2369.853829	115360.153813	59.159015
2368.794425	115180.010373	59.164020
2368.828848	114973.779439	59.169025
2368.292568	114777.148590	59.174029
2367.430095	114577.619614	59.179034
2366.792970	114362.652363	59.184039
2366.068775	114169.908644	59.189044
2365.264430	113968.217311	59.194049
2364.733160	113765.278400	59.199053
2364.088086	113557.992586	59.204058
2363.510678	113351.624375	59.209063
2362.832768	113156.488367	59.214068
2362.178865	112956.329891	59.219073
2361.512885	112753.788619	59.224077
2360.903437	112550.852887	59.229082
2360.407996	112330.022731	59.234087
2359.192823	112138.419634	59.239092
2358.679612	111931.989498	59.244097
2358.147915	111717.840545	59.249101
2357.077276	111520.412425	59.254106
2356.820924	111313.464385	59.259111
2356.211713	111117.108634	59.264116
2355.617857	110908.148645	59.269121
2354.920920	110710.578886	59.274125
2354.282817	110505.989052	59.279130
2354.056728	110303.347254	59.284135
2353.173257	110096.318458	59.289140
2352.349239	109885.093726	59.294145
2351.637376	109674.443186	59.299149
2350.811521	109466.020843	59.304154
2350.662079	109258.210087	59.309159
2349.607846	109060.481799	59.314164
2349.398570	108842.416843	59.319169
2348.568464	108629.179675	59.324173
2347.654748	108427.303310	59.329178
2347.430077	108215.020774	59.334183
2346.714882	108002.576742	59.339188
2345.829884	107803.594483	59.344193
2345.222685	107584.233307	59.349197
2344.297473	107374.746886	59.354202
2343.952429	107154.948287	59.359207
2342.813282	106958.113515	59.364212
2342.267476	106752.937741	59.369217
2341.847383	106542.191935	59.374221
2340.730358	106338.195255	59.379226
2340.473298	106119.864164	59.384231
2339.958651	105911.372269	59.389236
2339.409419	105713.293053	59.394241
2338.852987	105501.683386	59.399245
2337.882095	105283.149520	59.404250
2337.265408	105076.984173	59.409255
2336.465014	104868.388062	59.414260
2335.900872	104656.577739	59.419265
2335.327767	104452.085828	59.424269
2334.470629	104246.130755	59.429274
2333.887844	104024.355694	59.434279
2332.973489	103818.622768	59.439284
2332.188825	103614.444425	59.444289
2331.699143	103407.049005	59.449293
2331.042207	103197.372682	59.454298
2330.587802	102988.554272	59.459303
2329.781279	102788.694127	59.464308
2329.270339	102565.271940	59.469313
2328.574124	102361.236335	59.474317
2327.876208	102166.052371	59.479322
2327.345272	101945.367086	59.484327
2326.757476	101735.635745	59.489332
2325.982332	101522.117128	59.494337
2325.186055	101317.440404	59.499341
2324.708563	101110.431263	59.504346
2324.285809	100890.677625	59.509351
2323.372007	100691.753170	59.514356
2322.710297	100474.978343	59.519361
2322.360251	100260.382611	59.524365
2321.128020	100055.151794	59.529370
2320.996286	99830.014710	59.534375
2319.992780	99624.795845	59.539380
2319.411797	99416.086560	59.544385
2318.760882	99198.662296	59.549389
2317.799540	98988.494875	59.554394
2317.398439	98777.967795	59.559399
2316.766626	98564.206333	59.564404
2316.142565	98354.371797	59.569409
2315.820247	98151.068713	59.574413
2315.064321	97939.888858	59.579418
2314.317409	97715.060288	59.584423
2313.811936	97506.039258	59.589428
2313.013479	97287.261154	59.594433
2312.556983	97066.705793	59.599437
2311.465089	96855.164309	59.604442
2310.817430	96638.524924	59.609447
2309.652334	96433.905716	59.614452
2309.596586	96214.614259	59.619457
2308.774319	96005.016701	59.624461
2308.203512	95799.161070	59.629466
2308.005333	95574.488634	59.634471
2306.956894	95361.717523	59.639476
2306.341105	95151.974644	59.644481
2305.726316	94942.601384	59.649485
2304.801658	94732.169405	59.654490
2304.597604	94500.748310	59.659495
2303.713330	94287.415949	59.664500
2302.889962	94071.412507	59.669505
2302.489834	93856.377699	59.674509
2301.497865	93645.218305	59.679514
2301.059094	93424.835264	59.684519
2300.193615	93221.916290	59.689524
2299.810243	93002.815923	59.694529
2298.941675	92787.675463	59.699533
2298.184852	92571.777454	59.704538
2297.687279	92351.541189	59.709543
2296.589495	92150.406294	59.714548
2295.805457	91937.549782	59.719553
2295.485939	91730.119208	59.724557
2294.697006	91514.040038	59.729562
2294.021133	91293.950372	59.734567
2293.457081	91099.918155	59.739572
2293.131364	90888.736436	59.744577
2292.433234	90681.084102	59.749581
2291.809042	90472.306074	59.754586
2291.041987	90244.423503	59.759591
2290.052709	90036.240122	59.764596
2289.391561	89832.730243	59.769601
2289.334067	89616.135292	59.774605
2288.329914	89404.200505	59.779610
2287.752422	89181.713500	59.784615
2286.966651	88973.463602	59.789620
2286.601057	88757.585407	59.794625
2285.724820	88541.701575	59.799629
2285.166752	88336.166882	59.804634
2284.479697	88108.059385	59.809639
2283.539130	87896.953398	59.814644
2282.803552	87692.264458	59.819649
2282.547157	87474.467131	59.824653
2281.820010	87268.291054	59.829658
2281.600560	87046.517262	59.834663
2280.346575	86836.098971	59.839668
2279.698326	86630.055963	59.844673
2279.383618	86404.779184	59.849677
2278.290467	86191.267128	59.854682
2277.823186	85976.662690	59.859687
2277.246262	85769.697452	59.864692
2276.485411	85552.627180	59.869697
2276.009049	85332.376182	59.874701
2275.231819	85122.596420	59.879706
2274.882105	84904.656154	59.884711
2273.958931	84688.000762	59.889716
2273.331396	84471.307033	59.894721
2272.874859	84245.473347	59.899725
2271.945402	84033.351464	59.904730
2271.181635	83801.340355	59.909735
2270.527184	83594.136021	59.914740
2269.821436	83373.206455	59.919745
2269.242233	83165.379566	59.924750
2268.284211	82959.630386	59.929754
2267.975093	82744.114475	59.934759
2267.402555	82532.470810	59.939764
2266.565758	82312.821773	59.944769
2266.080046	82094.913025	59.949774
2265.274092	81884.922773	59.954778
2264.743067	81663.020093	59.959783
2263.851720	81452.768851	59.964788
2263.372843	81240.185381	59.969793
2262.761079	81020.368451	59.974798
2261.868189	80804.337643	59.979802
2261.393351	80592.539668	59.984807
2260.366652	80385.723946	59.989812
2259.838053	80164.571983	59.994817
2259.368967	79955.973668	59.999822
2258.409113	79748.748101	60.004826
2258.020693	79527.549014	60.009831
2257.423558	79312.551494	60.014836
2256.584299	79098.006525	60.019841
2256.256062	78881.462608	60.024846
2255.023700	78670.038905	60.029850
2254.733143	78439.628284	60.034855
2254.080277	78235.195506	60.039860
2253.418303	78013.878609	60.044865
2252.928838	77791.738311	60.049870
2251.929247	77583.431902	60.054874
2251.528872	77366.611226	60.059879
2250.643993	77156.751173	60.064884
2249.955163	76939.207721	60.069889
2249.321568	76722.532252	60.074894
2248.528379	76515.319209	60.079898
2248.133491	76281.439091	60.084903
2247.326556	76083.166771	60.089908
2246.707755	75869.780191	60.094913
2246.150709	75648.003433	60.099918
2245.395952	75441.466872	60.104922
2244.803264	75219.846182	60.109927
2244.100105	75007.166346	60.114932
2243.416807	74798.844633	60.119937
2242.809644	74575.376915	60.124942
2242.256661	74358.751938	60.129946
2241.551044	74119.136276	60.134951
2240.891300	73909.597251	60.139956
2240.232452	73688.688121	60.144961
2239.365708	73469.030790	60.149966
2238.577681	73250.978887	60.154970
2238.155474	73033.511199	60.159975
2237.238084	72829.244577	60.164980
2236.648393	72618.814679	60.169985
2235.867825	72401.391702	60.174990
2235.554017	72189.408499	60.179994
2234.999481	71968.311782	60.184999
2234.148664	71764.666331	60.190004
2233.260383	71545.153950	60.195009
2233.037919	71320.027201	60.200014
2231.965373	71115.460703	60.205018
2231.468626	70897.008294	60.210023
2230.864030	70686.670895	60.215028
2230.081350	70475.021079	60.220033
2229.648263	70259.067723	60.225038
2228.704876	70059.236114	60.230042
2228.035672	69834.102122	60.235047
2227.386556	69627.380921	60.240052
2226.831726	69419.950188	60.245057
2226.447757	69195.348336	60.250062
2225.450636	68985.553745	60.255066
2224.684484	68769.587231	60.260071
2224.080756	68561.128245	60.265076
2223.377793	68352.750559	60.270081
2222.685013	68139.597882	60.275086
2221.820228	67928.463570	60.280090
2221.461810	67714.648143	60.285095
2220.852034	67494.718794	60.290100
2220.263032	67295.916872	60.295105
2219.536958	67075.637037	60.300110
2218.659409	66873.237207	60.305114
2218.252032	66658.484836	60.310119
2217.592389	66440.259970	60.315124
2216.658952	66233.027684	60.320129
2216.197785	66023.401670	60.325134
2214.990962	65818.421076	60.330138
2214.957101	65600.641565	60.335143
2214.193456	65404.160267	60.340148
2213.286308	65188.445930	60.345153
2212.954801	64970.223637	60.350158
2211.761976	64768.506985	60.355162
2211.387131	64554.599275	60.360167
2210.828234	64352.216524	60.365172
2209.995156	64145.782353	60.370177
2209.533935	63931.904793	60.375182
2208.736971	63726.488920	60.380186
2208.264858	63505.959509	60.385191
2207.699964	63302.673820	60.390196
2206.980956	63088.102580	60.395201
2206.491991	62878.094267	60.400206
2205.247324	62673.017205	60.405210
2204.577337	62458.698566	60.410215
2204.229288	62244.305953	60.415220
2203.308962	62041.175608	60.420225
2202.748792	61835.156920	60.425230
2201.985936	61637.615731	60.430234
2201.618660	61416.685559	60.435239
2201.008257	61211.666174	60.440244
2200.125763	61011.358366	60.445249
2199.528656	60801.858747	60.450254
2198.973761	60600.401705	60.455258
2198.101473	60377.142137	60.460263
2197.133656	60169.674172	60.465268
2196.362788	59969.309106	60.470273
2196.279681	59764.209192	60.475278
2195.278135	59565.926747	60.480282
2194.780026	59357.969093	60.485287
2194.194939	59154.095024	60.490292
2193.085460	58948.476806	60.495297
2192.810596	58745.963384	60.500302
2192.163780	58543.612448	60.505306
2191.455209	58345.318650	60.510311
2190.938842	58133.756529	60.515316
2190.168394	57917.176055	60.520321
2189.515005	57712.917122	60.525326
2188.619419	57518.817594	60.530330
2188.273573	57301.183124	60.535335
2187.363235	57101.282468	60.540340
2186.757770	56900.180399	60.545345
2186.137960	56685.764756	60.550350
2185.387196	56493.248141	60.555354
2184.760433	56286.250436	60.560359
2184.208364	56081.889002	60.565364
2183.189790	55867.637906	60.570369
2182.599161	55666.002597	60.575374
2181.924131	55483.966198	60.580378
2181.651812	55276.401448	60.585383
2180.800363	55069.984742	60.590388
2179.910455	54876.155823	60.595393
2179.565904	54671.008167	60.600398
2178.610635	54469.193859	60.605402
2177.646722	54264.838881	60.610407
2177.287883	54063.826833	60.615412
2176.709837	53870.095188	60.620417
2176.249079	53662.651424	60.625422
2175.550498	53470.667750	60.630426
2174.836509	53270.116342	60.635431
2174.592335	53068.138297	60.640436
2173.231450	52863.191193	60.645441
2172.809426	52658.423389	60.650446
2172.147100	52457.233593	60.655450
2171.308191	52256.342999	60.660455
2170.654388	52063.534939	60.665460
2169.780169	51859.831947	60.670465
2169.411518	51658.088709	60.675470
2168.640989	51471.915206	60.680474
2167.988634	51260.666057	60.685479
2167.526751	51070.638295	60.690484
2166.634359	50866.971557	60.695489
2166.206002	50666.210731	60.700494
2164.975087	50477.912158	60.705498
2164.363092	50275.644036	60.710503
2164.109908	50085.489184	60.715508
2163.309123	49889.516498	60.720513
2163.029849	49690.081218	60.725518
2161.759445	49504.089682	60.730522
2160.989854	49293.423292	60.735527
2160.740495	49104.372885	60.740532
2159.697141	48906.725298	60.745537
2159.381790	48714.405705	60.750542
2158.224512	48523.544097	60.755546
2157.653438	48332.556746	60.760551
2156.802297	48142.862273	60.765556
2156.096304	47949.790428	60.770561
2155.763714	47767.964175	60.775566
2154.806779	47587.140385	60.780570
2154.290342	47396.632108	60.785575
2153.843197	47201.268758	60.790580
2153.144017	47017.929892	60.795585
2152.410514	46822.144838	60.800590
2151.730633	46643.997612	60.805594
2151.075847	46454.119288	60.810599
2150.526044	46267.259772	60.815604
2149.748159	46081.175418	60.820609
2148.902847	45884.621429	60.825614
2148.487170	45704.822321	60.830618
2147.286637	45522.097300	60.835623
2147.194164	45328.191381	60.840628
2146.085115	45151.427333	60.845633
2145.739937	44954.314176	60.850638
2144.983504	44770.821221	60.855642
2144.184816	44588.159224	60.860647
2143.406497	44414.067010	60.865652
2142.418797	44233.712739	60.870657
2141.876058	44044.981322	60.875662
2140.966846	43876.506900	60.880666
2140.366586	43696.722932	60.885671
2139.909681	43526.883457	60.890676
2138.968955	43355.496831	60.895681
2138.408908	43188.637196	60.900686
2137.841313	43016.951201	60.905690
2137.383104	42838.466022	60.910695
2136.349121	42665.121299	60.915700
2135.383938	42491.416368	60.920705
2135.279134	42310.594132	60.925710
2134.056048	42156.619351	60.930714
2133.678015	41994.963395	60.935719
2133.224682	41819.131665	60.940724
2132.490539	41643.295681	60.945729
2131.772297	41474.033251	60.950734
2130.945761	41316.192571	60.955738
2130.125426	41145.210359	60.960743
2129.769661	40983.623597	60.965748
2128.573308	40820.517928	60.970753
2128.042470	40644.523926	60.975758
2127.421981	40491.122995	60.980762
2126.652124	40324.409718	60.985767
2125.809485	40164.745043	60.990772
2124.918167	40011.900451	60.995777
2124.380866	39866.999179	61.000782
2123.485584	39722.679226	61.005786
2122.605821	39555.481811	61.010791
2122.013419	39412.125068	61.015796
2120.766417	39269.570569	61.020801
2120.432863	39118.803425	61.025806
2119.611104	38981.375545	61.030810
2118.952970	38851.925201	61.035815
2118.590003	38719.455409	61.040820
2117.135413	38584.298502	61.045825
2116.680352	38448.106724	61.050830
2115.578288	38317.510476	61.055834
2114.964038	38184.790685	61.060839
2114.375082	38061.296634	61.065844
2113.672230	37938.335311	61.070849
2112.803998	37813.837728	61.075854
2111.970348	37694.507844	61.080858
2111.305403	37578.569629	61.085863
2110.501181	37463.463649	61.090868
2109.748268	37353.827559	61.095873
2109.353449	37239.638202	61.100878
2108.674097	37132.413548	61.105882
2107.915150	37004.412787	61.110887
2107.755000	36888.125756	61.115892
2106.796816	36779.248341	61.120897
2106.156944	36658.519836	61.125902
2105.474244	36547.012656	61.130906
2104.649162	36441.051595	61.135911
2104.133040	36314.255195	61.140916
2103.264802	36206.761335	61.145921
2102.824436	36094.056944	61.150926
2101.831666	35987.595839	61.155930
2101.219350	35873.949714	61.160935
2100.918689	35768.526118	61.165940
2099.871614	35654.289774	61.170945
2099.296057	35544.390754	61.175950
2098.522376	35445.059875	61.180954
2097.882969	35336.831931	61.185959
2097.389921	35218.908585	61.190964
2096.760279	35125.919981	61.195969
2096.177872	35004.530424	61.200974
2095.352329	34914.376331	61.205978
2095.010942	34802.501000	61.210983
2094.282343	34701.835022	61.215988
2093.500855	34596.868082	61.220993
2093.088905	34479.948581	61.225998
2092.330256	34380.420922	61.231002
2091.532098	34263.199132	61.236007
2091.179711	34152.371413	61.241012
2090.261749	34052.177180	61.246017
2089.807843	33942.550701	61.251022
2088.919653	33836.044031	61.256026
2088.355701	33726.782542	61.261031
2087.701436	33614.879475	61.266036
2087.290822	33520.362121	61.271041
2086.624590	33400.329791	61.276046
2086.046372	33280.176899	61.281050
2085.427087	33172.836894	61.286055
2084.562081	33058.771175	61.291060
2083.589109	32961.315157	61.296065
2083.006821	32844.848210	61.301070
2082.398904	32741.573751	61.306074
2081.792218	32643.318743	61.311079
2081.110374	32536.356251	61.316084
2080.297792	32438.599731	61.321089
2079.831777	32325.490287	61.326094
2078.862329	32220.248970	61.331098
2078.298685	32113.096632	61.336103
2077.837118	32015.151019	61.341108
2077.048152	31912.292879	61.346113
2076.471216	31794.645729	61.351118
2076.054191	31697.394965	61.356122
2075.227867	31589.865789	61.361127
2074.803256	31480.974665	61.366132
2073.791107	31376.699934	61.371137
2073.260278	31274.899868	61.376142
2072.694112	31171.609636	61.381146
2072.135961	31061.807023	61.386151
2071.259017	30957.842161	61.391156
2070.355486	30849.141817	61.396161
2069.773766	30735.040881	61.401166
2069.292681	30647.957099	61.406170
2068.858806	30543.129767	61.411175
2068.026109	30439.703135	61.416180
2067.137684	30337.542155	61.421185
2066.753142	30228.649803	61.426190
2066.002878	30134.802981	61.431194
2065.619564	30027.182133	61.436199
2064.690124	29916.524931	61.441204
2064.187376	29807.262287	61.446209
2063.592028	29703.225937	61.451214
2062.594363	29591.527893	61.456218
2062.014516	29495.910215	61.461223
2061.517136	29381.032706	61.466228
2060.850729	29293.380400	61.471233
2059.973156	29176.107810	61.476238
2059.400631	29081.922836	61.481242
2058.816642	28975.094389	61.486247
2058.001929	28870.161250	61.491252
2057.237761	28766.195577	61.496257
2056.761839	28656.358125	61.501262
2056.007903	28568.791541	61.506266
2055.120869	28464.656121	61.511271
2054.499653	28354.233927	61.516276
2053.635517	28263.570952	61.521281
2053.166608	28174.395612	61.526286
2052.328558	28077.989900	61.531290
2051.776013	27977.973751	61.536295
2051.038527	27877.410926	61.541300
2050.013503	27791.060628	61.546305
2049.506641	27691.253852	61.551310
2048.605336	27602.557860	61.556314
2047.983974	27515.543069	61.561319
2047.445872	27414.935676	61.566324
2046.504704	27338.512930	61.571329
2046.211866	27247.104635	61.576334
2045.554684	27173.111527	61.581338
2044.798900	27080.321095	61.586343
2044.361382	26984.280126	61.591348
2043.473074	26910.337535	61.596353
2042.924840	26813.857024	61.601358
2042.267321	26715.390557	61.606362
2041.430840	26632.975301	61.611367
2041.032060	26538.284648	61.616372
2040.166993	26452.925545	61.621377
2039.719234	26364.923416	61.626382
2038.647643	26274.237373	61.631386
2037.997059	26187.181454	61.636391
2037.653519	26101.350485	61.641396
2036.408565	26028.890229	61.646401
2035.662421	25941.584630	61.651406
2035.020063	25860.221420	61.656410
2034.508680	25789.244425	61.661415
2034.088337	25697.876192	61.666420
2033.090161	25624.197835	61.671425
2032.588789	25541.190024	61.676430
2031.840741	25454.929120	61.681434
2030.964362	25379.925441	61.686439
2030.678460	25299.952244	61.691444
2029.673658	25221.973221	61.696449
2029.398018	25133.332901	61.701454
2028.651911	25059.789309	61.706458
2027.930555	24980.636306	61.711463
2027.168338	24908.382508	61.716468
2026.441446	24830.127518	61.721473
2026.114564	24747.866144	61.726478
2025.326581	24672.155180	61.731482
2024.768847	24592.694606	61.736487
2024.198596	24506.569331	61.741492
2022.851945	24444.599748	61.746497
2022.770750	24353.330665	61.751502
2022.232759	24272.105842	61.756506
2021.713392	24193.926856	61.761511
2020.940648	24115.173262	61.766516
2020.039973	24040.210520	61.771521
2019.536248	23948.346640	61.776526
2018.724008	23879.442805	61.781530
2017.956490	23802.176180	61.786535
2017.521816	23718.856083	61.791540
2016.378508	23652.717642	61.796545
2015.908698	23568.254882	61.801550
2015.111077	23504.117010	61.806554
2014.576555	23430.189609	61.811559
2013.976606	23344.748929	61.816564
2012.973361	23276.486081	61.821569
2012.476433	23198.123629	61.826574
2011.899927	23125.938455	61.831578
2011.011507	23052.507246	61.836583
2010.644745	22977.600602	61.841588
2010.018842	22912.757954	61.846593
2009.479142	22828.582648	61.851598
2008.590986	22756.651556	61.856602
2007.852756	22694.487217	61.861607
2007.589456	22614.736294	61.866612
2006.834779	22541.870569	61.871617
2006.350156	22468.029744	61.876622
2005.392437	22387.136996	61.881626
2004.704156	22314.330480	61.886631
2004.570925	22235.048821	61.891636
2003.496467	22166.029000	61.896641
2002.918662	22082.122702	61.901646
2002.131838	22001.122683	61.906650
2001.359789	21932.746810	61.911655
2000.905568	21852.256980	61.916660
2000.024424	21784.792910	61.921665
1999.785640	21703.555043	61.926670
1998.905717	21642.379860	61.931674
1998.591112	21571.637557	61.936679
1998.079526	21482.444628	61.941684
1996.945458	21418.191725	61.946689
1996.334101	21332.037270	61.951694
1995.425412	21253.227072	61.956698
1994.830572	21190.812958	61.961703
1994.513525	21106.286161	61.966708
1993.637726	21041.417411	61.971713
1993.058768	20959.326972	61.976718
1992.093178	20887.385094	61.981722
1991.282042	20820.197498	61.986727
1990.901898	20741.281499	61.991732
1990.099247	20679.374552	61.996737
1989.325679	20601.536280	62.001742
1989.039676	20541.873912	62.006746
1988.154044	20453.832592	62.011751
1987.311989	20394.776978	62.016756
1986.708224	20318.442510	62.021761
1986.354393	20250.306798	62.026766
1985.592021	20175.539377	62.031770
1985.105726	20108.111017	62.036775
1984.315498	20031.184991	62.041780
1983.566016	19963.780862	62.046785
1983.037378	19881.143687	62.051790
1982.346465	19821.885047	62.056794
1981.612378	19750.545618	62.061799
1981.005451	19678.420112	62.066804
1980.335240	19605.309809	62.071809
1979.634565	19527.738461	62.076814
1978.932780	19465.604366	62.081818
1978.154401	19392.033394	62.086823
1977.874177	19313.030944	62.091828
1976.913087	19251.316627	62.096833
1976.238978	19181.020690	62.101838
1976.014299	19110.361629	62.106842
1974.949422	19036.555955	62.111847
1974.629370	18962.291363	62.116852
1973.876820	18892.121279	62.121857
1972.915661	18822.432249	62.126862
1972.348016	18752.720152	62.131866
1971.742568	18680.919927	62.136871
1971.271810	18608.155254	62.141876
1970.391648	18547.634797	62.146881
1969.613958	18476.222448	62.151886
1968.763191	18401.803181	62.156890
1968.144799	18349.640475	62.161895
1967.634751	18265.183690	62.166900
1966.884661	18196.348921	62.171905
1966.351445	18138.880629	62.176910
1965.689488	18064.005530	62.181914
1964.784461	18001.221536	62.186919
1964.359031	17926.682561	62.191924
1963.816795	17859.150416	62.196929
1963.154804	17796.845348	62.201934
1962.657971	17719.894004	62.206938
1961.757575	17657.624176	62.211943
1961.046680	17576.322354	62.216948
1960.092192	17520.414792	62.221953
1959.483097	17458.603559	62.226958
1959.017584	17391.085347	62.231962
1958.164165	17330.787994	62.236967
1957.734538	17255.770187	62.241972
1957.091899	17184.810834	62.246977
1956.354588	17127.951373	62.251982
1956.159191	17049.853132	62.256986
1954.960511	16987.191289	62.261991
1954.848017	16919.708294	62.266996
1953.942344	16851.768145	62.272001
1953.347577	16768.917393	62.277006
1952.797270	16703.688999	62.282010
1952.040224	16638.650775	62.287015
1951.366090	16566.092913	62.292020
1950.826615	16505.084309	62.297025
1950.000554	16424.662066	62.302030
1949.075673	16354.010224	62.307034
1948.441174	16292.654443	62.312039
1948.007446	16224.527686	62.317044
1946.916370	16157.648127	62.322049
1946.614259	16081.933384	62.327054
1945.970008	16021.625496	62.332058
1945.111564	15960.323354	62.337063
1944.563513	15889.856737	62.342068
1943.820322	15815.145498	62.347073
1943.322704	15745.750133	62.352078
1942.562829	15681.334816	62.357082
1941.899843	15614.454979	62.362087
1941.512048	15536.749110	62.367092
1940.766871	15486.318099	62.372097
1940.071001	15417.418011	62.377102
1939.381662	15338.003051	62.382106
1938.611079	15275.477141	62.387111
1937.701249	15206.510338	62.392116
1937.224897	15143.668129	62.397121
1936.395379	15079.861994	62.402126
1935.962817	15018.155332	62.407130
1935.198502	14963.655236	62.412135
1934.725907	14883.889152	62.417140
1933.898128	14820.597039	62.422145
1932.946418	14753.282167	62.427150
1932.908471	14682.221659	62.432154
1932.005975	14617.198776	62.437159
1931.428136	14545.719475	62.442164
1930.638045	14489.080764	62.447169
1930.103081	14417.622384	62.452174
1929.237958	14358.478379	62.457178
1928.716942	14287.762643	62.462183
1928.180034	14208.641071	62.467188
1926.902774	14149.849784	62.472193
1926.324669	14091.927864	62.477198
1926.071026	14028.444793	62.482202
1924.952852	13964.793295	62.487207
1924.369393	13898.754077	62.492212
1923.630993	13840.702287	62.497217
1922.945901	13787.473410	62.502222
1922.423429	13724.001127	62.507226
1921.752494	13673.695401	62.512231
1921.453167	13590.112660	62.517236
1920.645810	13542.234012	62.522241
1920.006943	13475.215739	62.527246
1919.628536	13413.378199	62.532250
1918.919467	13354.031892	62.537255
1918.147122	13286.862010	62.542260
1917.535820	13225.575466	62.547265
1916.908277	13152.042411	62.552270
1916.223537	13086.466445	62.557274
1915.448421	13027.893050	62.562279
1915.132179	12956.219839	62.567284
1914.461965	12890.511926	62.572289
1913.936605	12817.100888	62.577294
1913.147040	12746.709437	62.582298
1912.189591	12684.572878	62.587303
1911.686006	12605.668764	62.592308
1910.862609	12549.079427	62.597313
1910.211972	12477.479796	62.602318
1909.466390	12413.567987	62.607322
1908.931617	12356.948148	62.612327
1908.651837	12278.155602	62.617332
1907.344495	12220.253267	62.622337
1906.972137	12144.311849	62.627342
1906.214166	12078.585860	62.632346
1905.491175	12016.083680	62.637351
1904.947454	11948.061248	62.642356
1904.059082	11886.918472	62.647361
1903.786293	11826.907854	62.652366
1903.123500	11766.286077	62.657370
1901.856916	11696.057776	62.662375
1901.658022	11621.534899	62.667380
1900.685488	11570.515124	62.672385
1899.942003	11509.754098	62.677390
1899.756628	11445.983112	62.682394
1898.830310	11378.675558	62.687399
1898.317664	11321.079180	62.692404
1897.608842	11251.542040	62.697409
1896.915911	11184.790503	62.702414
1896.190200	11127.112888	62.707418
1895.266435	11070.966365	62.712423
1894.910740	11008.560547	62.717428
1894.060304	10948.127674	62.722433
1893.346766	10893.890717	62.727438
1893.068967	10823.396073	62.732442
1892.303743	10761.912412	62.737447
1891.828274	10692.371768	62.742452
1891.017840	10638.813911	62.747457
1890.320684	10572.897205	62.752462
1890.008739	10500.436875	62.757466
1889.116212	10445.118185	62.762471
1888.490347	10372.380458	62.767476
1887.969815	10309.307765	62.772481
1886.862985	10250.193856	62.777486
1886.584306	10181.055726	62.782490
1885.948966	10112.074935	62.787495
1884.908671	10047.732678	62.792500
1884.257366	9988.590089	62.797505
1883.291305	9931.702985	62.802510
1882.723143	9864.011772	62.807514
1882.019021	9813.713564	62.812519
1881.622269	9744.250003	62.817524
1880.969405	9686.870687	62.822529
1880.230742	9632.714843	62.827534
1879.666971	9569.631990	62.832538
1879.014391	9525.575777	62.837543
1878.630672	9442.625735	62.842548
1878.019449	9385.875694	62.847553
1877.139774	9316.203979	62.852558
1876.658090	9243.053536	62.857562
1875.689141	9190.627802	62.862567
1875.356791	9117.916993	62.867572
1874.406926	9066.567182	62.872577
1873.596149	9000.579933	62.877582
1872.950034	8935.533701	62.882586
1872.583484	8879.055216	62.887591
1871.968099	8808.048436	62.892596
1871.287512	8754.653401	62.897601
1870.435246	8694.104821	62.902606
1869.521567	8620.454007	62.907610
1868.826725	8565.571992	62.912615
1868.154246	8503.038283	62.917620
1867.620194	8448.712615	62.922625
1867.023154	8386.789094	62.927630
1866.707705	8324.102807	62.932634
1865.634198	8259.730889	62.937639
1865.135463	8200.618850	62.942644
1864.291174	8139.284695	62.947649
1863.907330	8086.569948	62.952654
1863.349796	8017.268492	62.957658
1862.134105	7953.561457	62.962663
1861.560966	7896.676106	62.967668
1861.211903	7836.859340	62.972673
1860.409294	7772.358947	62.977678
1859.893830	7719.890830	62.982682
1858.846688	7661.241136	62.987687
1858.356676	7595.820547	62.992692
1857.629452	7530.147595	62.997697
1857.292254	7473.600328	63.002702
1856.670317	7415.130227	63.007706
1855.622436	7361.385504	63.012711
1854.921459	7307.793373	63.017716
1854.884688	7243.140944	63.022721
1853.999170	7186.931888	63.027726
1853.402565	7125.695500	63.032730
1852.573127	7065.702497	63.037735
1851.925591	6989.233979	63.042740
1851.393343	6934.775087	63.047745
1850.679869	6872.678722	63.052750
1850.300507	6806.991592	63.057754
1849.033208	6745.486972	63.062759
1848.500160	6690.384221	63.067764
1848.150690	6636.860180	63.072769
1847.463416	6574.430377	63.077774
1846.400251	6505.242650	63.082778
1845.851067	6453.377546	63.087783
1845.044116	6388.731197	63.092788
1844.413909	6332.892659	63.097793
1843.691112	6276.239982	63.102798
1843.429754	6219.722507	63.107802
1842.242016	6162.015289	63.112807
1842.032720	6098.423038	63.117812
1841.200180	6046.985337	63.122817
1840.462655	5992.696980	63.127822
1840.099840	5926.335897	63.132826
1839.289989	5877.376748	63.137831
1838.692308	5800.392134	63.142836
1838.257922	5743.835316	63.147841
1837.171588	5693.632577	63.152846
1837.025553	5625.980303	63.157850
1836.096660	5571.367343	63.162855
1835.237161	5504.646077	63.167860
1834.621390	5443.863747	63.172865
1833.910421	5389.350162	63.177870
1833.385975	5332.548919	63.182874
1832.837409	5281.704538	63.187879
1832.283574	5210.128542	63.192884
1831.574774	5154.847223	63.197889
1830.841088	5095.448022	63.202894
1830.416846	5019.193192	63.207898
1829.390193	4963.565525	63.212903
1828.763370	4898.969644	63.217908
1827.982030	4841.253539	63.222913
1827.223510	4791.420644	63.227918
1826.993452	4735.604258	63.232922
1826.186138	4672.311048	63.237927
1825.676156	4608.000763	63.242932
1824.891374	4539.297013	63.247937
1824.095567	4490.425415	63.252942
1823.512533	4436.306749	63.257946
1822.644577	4369.415282	63.262951
1822.338076	4310.826100	63.267956
1821.890483	4247.522555	63.272961
1820.683759	4193.281394	63.277966
1820.327873	4125.874360	63.282970
1819.006306	4079.609093	63.287975
1818.410593	4014.147731	63.292980
1817.836866	3959.075017	63.297985
1816.743757	3917.518779	63.302990
1816.566453	3849.844103	63.307994
1816.013845	3810.850767	63.312999
1815.572022	3763.184125	63.318004
1814.728344	3705.157433	63.323009
1813.928362	3645.851104	63.328014
1813.643470	3575.153628	63.333018
1812.685449	3529.968065	63.338023
1812.205899	3470.192782	63.343028
1811.652840	3413.185802	63.348033
1810.414817	3367.806232	63.353038
1810.221537	3311.869521	63.358042
1809.607753	3255.124379	63.363047
1808.597773	3193.206489	63.368052
1807.901655	3141.376349	63.373057
1807.190012	3087.481809	63.378062
1806.902089	3031.387690	63.383066
1806.369834	2986.586516	63.388071
1805.670698	2923.117256	63.393076
1805.262003	2864.009844	63.398081
1804.162297	2807.013943	63.403086
1803.756852	2740.493359	63.408090
1802.926748	2685.110459	63.413095
1802.213388	2633.235172	63.418100
1801.855536	2575.754879	63.423105
1800.929072	2520.335066	63.428110
1800.387541	2456.545494	63.433114
1799.258968	2414.637186	63.438119
1798.872478	2356.245934	63.443124
1798.186796	2294.924645	63.448129
1797.361862	2249.861489	63.453134
1796.864960	2189.002758	63.458138
1796.033894	2138.262999	63.463143
1795.211976	2082.409503	63.468148
1794.857456	2039.884126	63.473153
1793.822840	1983.009647	63.478158
1793.415207	1924.849801	63.483162
1792.591726	1894.480458	63.488167
1792.408244	1834.354135	63.493172
1791.778841	1775.813725	63.498177
1790.914868	1734.414999	63.503182
1790.050187	1677.868799	63.508186
1789.169676	1623.473396	63.513191
1788.670259	1574.588122	63.518196
1788.033395	1522.386843	63.523201
1787.049736	1472.015871	63.528206
1786.598960	1418.718490	63.533210
1785.969930	1373.384850	63.538215
1785.043210	1321.643521	63.543220
1784.687214	1268.291424	63.548225
1783.670944	1232.419243	63.553230
1783.548114	1179.024139	63.558234
1782.695163	1133.487086	63.563239
1782.090147	1079.880306	63.568244
1781.511399	1028.291363	63.573249
1780.520068	980.258175	63.578254
1780.110339	930.954724	63.583258
1779.506280	897.134338	63.588263
1778.550220	846.854987	63.593268
1777.711098	799.760231	63.598273
1777.096240	757.980934	63.603278
1776.336085	709.197533	63.608282
1775.526538	664.115557	63.613287
1775.076465	633.529491	63.618292
1774.208239	588.129047	63.623297
1773.419348	553.580263	63.628302
1772.994345	503.741345	63.633306
1772.222969	472.618412	63.638311
1771.696505	438.602264	63.643316
1770.859075	395.873722	63.648321
1770.247778	361.850724	63.653326
1769.530641	309.102772	63.658330
1768.898564	279.741719	63.663335
1767.934730	249.468289	63.668340
1767.344461	209.814029	63.673345
1766.445921	186.082747	63.678350
1765.799875	152.948870	63.683354
1765.073371	123.789213	63.688359
1764.160841	98.190002	63.693364
1763.725194	73.259439	63.698369
1762.871013	46.626023	63.703374
1761.517974	41.411397	63.708378
1761.184517	35.128107	63.713383
1760.444877	14.677201	63.718388
1758.898093	6.662704	63.723393
1756.955800	38.857422	63.728398
1755.544343	64.836648	63.733402
1755.201977	82.054794	63.738407
1755.232684	86.216296	63.743412
1755.600136	84.317631	63.748417
1755.330038	85.008674	63.753422
1755.134344	77.793577	63.758426
1754.061413	76.938945	63.763431
1752.952748	85.316856	63.768436
1752.056666	89.821081	63.773441
1750.976178	96.709015	63.778446
1751.088316	86.054534	63.783450
1750.310176	91.571371	63.788455
1749.452039	94.762261	63.793460
1748.957143	90.417457	63.798465
1748.528258	102.732364	63.803470
1748.339282	98.454095	63.808474
1747.597320	88.485613	63.813479
1746.752860	100.928016	63.818484
1746.061209	95.228296	63.823489
1744.747243	102.803026	63.828494
1744.207423	91.679636	63.833498
1743.397220	102.159576	63.838503
1743.192043	99.978103	63.843508
1742.996706	98.485782	63.848513
1742.281273	103.267258	63.853518
1741.567601	99.148011	63.858522
1740.880022	102.289741	63.863527
1739.667091	106.587247	63.868532
1739.162091	93.893967	63.873537
1738.324626	102.049048	63.878542
1737.735595	99.393940	63.883546
1737.657545	104.873722	63.888551
1737.307935	108.800733	63.893556
1736.755784	95.190833	63.898561
1734.995594	107.080072	63.903566
1734.803311	99.730382	63.908570
1734.325481	100.173717	63.913575
1733.708328	105.215559	63.918580
1733.258955	98.731456	63.923585
1732.031593	107.520903	63.928590
1731.828513	94.702405	63.933594
1731.029009	104.048383	63.938599
1730.136089	105.841298	63.943604
1729.587973	101.132781	63.948609
1728.392032	113.517476	63.953614
1728.153748	97.899126	63.958618
1727.589276	102.388546	63.963623
1726.402435	97.891857	63.968628
1725.994748	103.141711	63.973633
1725.543154	102.555847	63.978638
1725.657139	97.183933	63.983642
1723.944447	103.437412	63.988647
1723.780038	100.039926	63.993652
1723.769749	102.675123	63.998657
1722.439952	103.351538	64.003662
1721.517213	104.242431	64.008666
1720.463492	101.487660	64.013671
1720.256961	103.278802	64.018676
1720.297233	106.035282	64.023681
1719.458405	106.441333	64.028686
1718.172767	101.403666	64.033690
1717.921790	100.678709	64.038695
1717.066737	103.232023	64.043700
1716.517402	98.575744	64.048705
1715.978786	105.126896	64.053710
1715.144997	100.432213	64.058714
1714.408176	94.164083	64.063719
1714.089971	107.980043	64.068724
1713.362869	93.855459	64.073729
1712.025439	98.759380	64.078734
1711.995797	98.281549	64.083738
1711.524779	103.487845	64.088743
1710.150710	105.297257	64.093748
1709.821354	98.596978	64.098753
1709.626132	100.118239	64.103758
1708.664014	94.680686	64.108762
1707.772443	99.630495	64.113767
1706.976315	97.825159	64.118772
1706.695677	95.288240	64.123777
1706.033749	100.360851	64.128782
1705.505339	94.627334	64.133786
1704.737076	98.649222	64.138791
1703.618409	101.547187	64.143796
1703.036825	101.544952	64.148801
1702.700539	102.251245	64.153806
1702.582635	107.018256	64.158810
1701.883590	102.242252	64.163815
1700.918993	100.640296	64.168820
1700.508552	100.191406	64.173825
1699.484450	95.829736	64.178830
1698.854415	95.664885	64.183834
1698.298105	102.307159	64.188839
1697.114188	98.112799	64.193844
1697.261908	92.738683	64.198849
1695.548436	106.922903	64.203854
1695.480060	98.402349	64.208858
1694.958608	100.273473	64.213863
1693.871337	99.373833	64.218868
1693.208187	92.042168	64.223873
1692.903417	101.162917	64.228878
1692.567970	97.515053	64.233882
1691.307999	90.751273	64.238887
1690.678581	100.932847	64.243892
1690.251434	95.905504	64.248897
1689.557715	90.010589	64.253902
1688.883490	92.629807	64.258906
1688.357337	88.562799	64.263911
1687.713823	97.669538	64.268916
1687.097413	89.412654	64.273921
1686.525590	98.422851	64.278926
1685.962265	97.055215	64.283930
1685.095715	96.735542	64.288935
1683.777525	98.455666	64.293940
1683.373798	96.640054	64.298945
1682.809080	101.142135	64.303950
1682.738974	101.490758	64.308954
1681.538315	106.644212	64.313959
1680.866766	99.652931	64.318964
1680.220607	97.850593	64.323969
1679.358057	102.125587	64.328974
1678.803527	103.688150	64.333978
1678.638473	103.217634	64.338983
1677.851244	104.389798	64.343988
1677.390959	97.868018	64.348993
1676.787760	101.467876	64.353998
1676.309890	93.532769	64.359002
1675.121472	92.693359	64.364007
1674.035494	97.546320	64.369012
1673.521414	94.600200	64.374017
1672.704804	102.291508	64.379022
1672.468382	98.963814	64.384026
1671.682283	99.721055	64.389031
1670.915400	103.796351	64.394036
1670.675403	97.785217	64.399041
1670.076220	100.953924	64.404046
1669.475679	105.562626	64.409050
1669.221816	98.736821	64.414055
1667.920035	102.006088	64.419060
1666.990487	95.036870	64.424065
1666.144084	98.038262	64.429070
1665.428464	100.563136	64.434074
1664.868158	96.616675	64.439079
1664.287485	94.225191	64.444084
1664.053926	93.442279	64.449089
1663.265576	101.420839	64.454094
1662.819536	96.459582	64.459098
1662.450835	101.525050	64.464103
1661.857353	107.955614	64.469108
1660.840485	104.275639	64.474113
1659.488685	105.502791	64.479118
1659.174381	96.127161	64.484122
1658.528608	92.017657	64.489127
1658.033052	105.984788	64.494132
1657.386744	96.458464	64.499137
1656.806389	102.984714	64.504142
1656.406656	97.727516	64.509146
1655.976190	103.495087	64.514151
1654.451605	102.213913	64.519156
1653.876340	96.681819	64.524161
1652.801704	100.181522	64.529166
1652.451790	98.642798	64.534170
1652.160730	93.355725	64.539175
1651.274931	103.805114	64.544180
1651.036190	95.317936	64.549185
1650.396966	108.151969	64.554190
1649.777128	98.476361	64.559194
1648.750580	96.499485	64.564199
1647.254462	97.716449	64.569204
1646.816085	96.185471	64.574209
1646.738341	95.038761	64.579214
1646.530645	91.897323	64.584218
1645.732491	98.041847	64.589223
1644.853079	91.392687	64.594228
1644.730569	89.492988	64.599233
1643.532645	93.477482	64.604238
1642.526053	98.115992	64.609242
1642.175276	99.794432	64.614247
1640.908695	99.978293	64.619252
1640.851598	99.350280	64.624257
1639.925443	99.353908	64.629262
1639.523034	105.703659	64.634266
1639.203984	93.611665	64.639271
1638.203958	96.452962	64.644276
1638.007231	87.933885	64.649281
1636.879443	99.826796	64.654286
1635.919559	94.240685	64.659290
1635.736157	91.719870	64.664295
1634.740027	95.552464	64.669300
1634.603886	90.628721	64.674305
1633.806484	95.733904	64.679310
1633.467036	99.605690	64.684314
1632.467400	87.577658	64.689319
1631.638899	98.675544	64.694324
1630.574477	96.302563	64.699329
1630.177250	101.699000	64.704334
1629.730083	101.095103	64.709338
1629.576338	94.174555	64.714343
1628.292110	97.575094	64.719348
1627.338429	93.899292	64.724353
1626.672260	92.858671	64.729358
1626.089062	94.528301	64.734362
1625.643531	89.595359	64.739367
1624.776245	94.061932	64.744372
1624.843225	89.348778	64.749377
1624.216606	86.999297	64.754382
1622.953485	94.025096	64.759386
1621.796386	93.157081	64.764391
1621.217476	94.594215	64.769396
1621.483078	90.027707	64.774401
1620.459230	94.864509	64.779406
1619.819159	96.718218	64.784410
1619.512598	91.954014	64.789415
1618.737180	101.901745	64.794420
1617.784368	96.382327	64.799425
1616.805129	99.745461	64.804430
1616.294085	99.992241	64.809434
1615.332435	97.915182	64.814439
1614.665280	97.830366	64.819444
1614.907259	94.753116	64.824449
1614.232038	100.658921	64.829454
1613.600155	100.746700	64.834458
1612.522468	101.222269	64.839463
1611.556094	102.599531	64.844468
1611.125887	100.075346	64.849473
1610.413498	104.976219	64.854478
1610.120530	103.333837	64.859482
1609.994874	106.245981	64.864487
1608.313784	112.205926	64.869492
1607.564715	101.645677	64.874497
1606.652157	101.943628	64.879502
1606.446982	106.290834	64.884506
1605.754224	98.312609	64.889511
1605.211731	100.144513	64.894516
1604.930270	98.534998	64.899521
1604.202176	104.215814	64.904526
1603.379729	104.516797	64.909530
1602.557584	102.496429	64.914535
1601.831109	110.105628	64.919540
1601.355792	99.309504	64.924545
1600.791856	113.710135	64.929550
1600.025723	106.626669	64.934554
1599.788410	97.976844	64.939559
1598.471451	108.991490	64.944564
1598.014100	104.648638	64.949569
1597.229369	102.704331	64.954574
1597.087278	97.502411	64.959578
1596.381368	103.911419	64.964583
1594.604493	100.051010	64.969588
1594.342714	97.944777	64.974593
1593.671230	102.697227	64.979598
1592.930036	100.266605	64.984602
1592.503740	96.264180	64.989607
1592.068512	106.419651	64.994612
1592.027120	96.983333	64.999617
1591.140824	113.109920	65.004622
1590.641296	98.539219	65.009626
1589.652906	94.235004	65.014631
1588.683830	105.550779	65.019636
1588.354749	103.225001	65.024641
1587.362099	109.761569	65.029646
1586.119936	106.090610	65.034650
1585.657367	107.220684	65.039655
1585.196066	103.938188	65.044660
1585.028175	98.582671	65.049665
1584.191748	104.028386	65.054670
1583.513391	96.830061	65.059674
1583.332249	89.119080	65.064679
1582.315687	102.025677	65.069684
1581.237504	99.870949	65.074689
1580.592311	97.909210	65.079694
1579.860900	103.817642	65.084698
1579.709303	99.957660	65.089703
1579.006971	103.566979	65.094708
1578.773710	98.180847	65.099713
1577.471570	101.991114	65.104718
1576.707058	107.597298	65.109722
1576.008137	100.452703	65.114727
1575.770647	103.973980	65.119732
1575.582536	105.590314	65.124737
1574.400410	104.585945	65.129742
1573.397334	100.269876	65.134746
1572.970443	102.865598	65.139751
1571.981438	105.287271	65.144756
1571.664630	98.134012	65.149761
1571.202371	102.604065	65.154766
1570.336739	108.177429	65.159770
1569.629077	95.629944	65.164775
1568.540806	107.035627	65.169780
1568.081069	97.105951	65.174785
1567.775883	99.773802	65.179790
1567.259666	108.748376	65.184794
1566.675276	105.113274	65.189799
1565.361909	102.420323	65.194804
1564.897929	90.833929	65.199809
1564.344992	100.001992	65.204814
1563.644657	104.438907	65.209818
1563.417454	96.765206	65.214823
1562.415850	102.798571	65.219828
1561.752916	95.446414	65.224833
1561.297325	104.192154	65.229838
1560.625467	105.383869	65.234842
1560.116087	94.068042	65.239847
1558.701524	112.073156	65.244852
1558.189831	106.141473	65.249857
1557.434714	100.161734	65.254862
1556.800054	99.229667	65.259866
1556.764665	104.393578	65.264871
1555.977869	107.792393	65.269876
1555.308303	101.810100	65.274881
1554.408603	104.938267	65.279886
1553.242574	113.456262	65.284890
1553.062439	103.034303	65.289895
1552.462451	109.412301	65.294900
1552.313357	101.182134	65.299905
1551.466643	113.156582	65.304910
1549.912351	99.382688	65.309914
1549.560973	96.084314	65.314919
1548.705373	104.101970	65.319924
1548.486362	97.762665	65.324929
1547.970324	97.223343	65.329934
1547.518153	107.083462	65.334938
1547.343489	96.482441	65.339943
1545.551209	100.689146	65.344948
1545.363175	101.627372	65.349953
1545.086308	98.843868	65.354958
1543.863919	113.122035	65.359962
1542.862736	98.787176	65.364967
1541.987432	108.682986	65.369972
1541.334309	100.316858	65.374977
1541.004415	98.765509	65.379982
1540.836861	107.309369	65.384986
1540.458093	99.440553	65.389991
1539.904031	117.307382	65.394996
1538.991010	95.909452	65.400001
1538.286339	99.003481	65.405006
1537.539896	108.077717	65.410010
1536.471683	101.920647	65.415015
1535.371407	103.861690	65.420020
1534.972711	104.404452	65.425025
1534.535130	105.303480	65.430030
1533.895469	112.725433	65.435034
1533.854629	96.254164	65.440039
1533.184575	98.645673	65.445044
1532.184522	95.795725	65.450049
1531.486941	103.774085	65.455054
1530.716077	105.670675	65.460058
1530.277119	99.331626	65.465063
1528.779214	105.134773	65.470068
1528.149231	97.931934	65.475073
1527.885194	101.925791	65.480078
1527.451211	103.636388	65.485082
1527.048618	107.002550	65.490087
1526.249187	108.611941	65.495092
1525.966727	98.786574	65.500097
1525.156002	97.582866	65.505102
1523.890756	102.920111	65.510106
1523.576701	97.989954	65.515111
1522.911322	98.354316	65.520116
1521.832993	102.707795	65.525121
1521.090402	106.697267	65.530126
1520.391651	97.841652	65.535130
1520.059951	90.378533	65.540135
1519.347403	98.075417	65.545140
1518.936147	94.668289	65.550145
1518.519778	92.157694	65.555150
1517.397410	89.781356	65.560154
1516.535194	85.688941	65.565159
1515.760283	98.823663	65.570164
1515.644665	99.110134	65.575169
1514.988829	97.530154	65.580174
1514.466441	99.321033	65.585178
1513.871135	96.357894	65.590183
1512.609334	101.611018	65.595188
1512.150845	96.296954	65.600193
1511.836263	95.941674	65.605198
1511.259388	103.066641	65.610202
1509.964049	101.241343	65.615207
1509.319422	99.535003	65.620212
1508.819454	98.532660	65.625217
1508.178695	97.825504	65.630222
1507.561385	102.082080	65.635226
1507.589029	94.601287	65.640231
1506.043048	104.468052	65.645236
1505.482427	101.950416	65.650241
1504.978725	98.528018	65.655246
1504.308615	93.736444	65.660250
1504.108829	97.612858	65.665255
1503.063394	104.662469	65.670260
1502.559319	100.573071	65.675265
1502.197745	91.100911	65.680270
1500.843346	104.141638	65.685274
1500.098015	101.859938	65.690279
1499.473759	94.271419	65.695284
1498.685433	94.237426	65.700289
1498.326885	93.275693	65.705294
1497.762307	101.158806	65.710298
1497.493507	98.128019	65.715303
1496.377132	102.495439	65.720308
1495.558619	100.890850	65.725313
1494.983220	103.387178	65.730318
1494.493653	102.272797	65.735322
1494.142946	95.050824	65.740327
1492.702858	96.038196	65.745332
1492.149848	96.394172	65.750337
1491.519896	94.373265	65.755342
1491.289460	102.988614	65.760346
1491.148012	95.107333	65.765351
1489.599735	110.590064	65.770356
1488.792925	92.557896	65.775361
1488.425893	90.164048	65.780366
1487.861855	102.271778	65.785370
1487.825500	89.616081	65.790375
1486.331987	100.026454	65.795380
1485.327227	95.467838	65.800385
1484.787387	100.199391	65.805390
1483.944996	97.507338	65.810394
1483.960000	89.867706	65.815399
1483.340669	98.589006	65.820404
1482.990782	93.282925	65.825409
1482.276051	103.941713	65.830414
1481.114212	97.036297	65.835418
1480.840856	96.598775	65.840423
1479.701633	97.169334	65.845428
1478.761897	100.027915	65.850433
1478.490350	94.364029	65.855438
1477.567341	101.782126	65.860442
1477.288381	87.425587	65.865447
1476.868113	96.611999	65.870452
1476.151645	95.626720	65.875457
1475.089371	93.627209	65.880462
1474.250776	102.085309	65.885466
1473.684231	96.900390	65.890471
1473.325527	100.007267	65.895476
1473.150283	88.559525	65.900481
1472.177002	96.228463	65.905486
1471.120785	95.681957	65.910490
1470.827769	93.301580	65.915495
1470.153104	98.146024	65.920500
1469.396742	91.649272	65.925505
1468.571368	98.184521	65.930510
1467.623957	105.932934	65.935514
1467.317954	91.482919	65.940519
1466.383284	106.715180	65.945524
1466.212106	92.857180	65.950529
1465.644427	94.421873	65.955534
1464.699384	94.876425	65.960538
1463.935682	90.205395	65.965543
1463.455746	99.566873	65.970548
1463.143881	97.749317	65.975553
1462.038987	97.581137	65.980558
1460.913625	96.058440	65.985562
1460.521553	89.371335	65.990567
1459.864329	94.638790	65.995572
1459.436825	93.073003	66.000577
1459.317749	91.817750	66.005582
1458.054893	99.400247	66.010586
1457.652457	93.484349	66.015591
1456.484776	103.209017	66.020596
1456.182576	89.261456	66.025601
1455.595053	99.783335	66.030606
1454.240789	103.948876	66.035610
1453.623445	94.911615	66.040615
1453.236485	96.698330	66.045620
1453.000454	90.844299	66.050625
1452.675620	94.390500	66.055630
1451.504704	97.870884	66.060634
1450.737521	89.242221	66.065639
1450.190454	93.292097	66.070644
1449.781897	92.325703	66.075649
1449.474338	87.765117	66.080654
1448.007776	95.305871	66.085658
1447.779291	101.068173	66.090663
1447.202768	94.976514	66.095668
1446.473437	93.783551	66.100673
1445.243787	94.185567	66.105678
1444.272806	96.166023	66.110682
1443.910234	95.283786	66.115687
1443.209606	101.679368	66.120692
1443.370913	85.292699	66.125697
1442.993238	92.354474	66.130702
1441.260407	95.637155	66.135706
1440.706103	88.294588	66.140711
1440.011220	92.235492	66.145716
1439.917709	92.739229	66.150721
1439.201167	92.771118	66.155726
1438.104055	87.941771	66.160730
1437.427538	84.620974	66.165735
1436.873732	79.036651	66.170740
1436.635283	89.339044	66.175745
1436.074382	88.906224	66.180750
1434.445229	89.001149	66.185754
1434.324003	95.394536	66.190759
1433.561752	90.639707	66.195764
1433.285161	89.016825	66.200769
1432.882318	85.691959	66.205774
1431.484008	93.422148	66.210778
1431.245573	85.663527	66.215783
1430.251945	90.974988	66.220788
1429.692084	86.514428	66.225793
1428.694896	82.919743	66.230798
1427.868418	97.709026	66.235802
1427.796770	83.152398	66.240807
1427.318915	88.921211	66.245812
1426.632577	95.577877	66.250817
1426.121849	88.285159	66.255822
1424.991537	94.695415	66.260826
1424.537013	89.407553	66.265831
1423.854034	91.616636	66.270836
1422.792111	104.618795	66.275841
1422.262248	85.877172	66.280846
1421.735072	97.927006	66.285850
1421.020880	95.159407	66.290855
1420.582689	96.268286	66.295860
1420.070395	95.741012	66.300865
1419.302475	95.957692	66.305870
1418.183510	87.746077	66.310874
1417.749401	92.020859	66.315879
1417.195140	94.091214	66.320884
1416.361009	102.524963	66.325889
1415.589574	88.178901	66.330894
1414.661537	90.759673	66.335898
1414.505274	94.241238	66.340903
1413.853777	96.131503	66.345908
1413.404378	90.601553	66.350913
1413.037352	92.230561	66.355918
1412.203514	89.051470	66.360922
1411.736311	81.873268	66.365927
1410.611886	90.739506	66.370932
1409.466394	88.590823	66.375937
1408.955339	92.470978	66.380942
1408.093947	93.730701	66.385946
1408.068016	98.932525	66.390951
1407.500979	93.651509	66.395956
1406.657857	95.253685	66.400961
1405.962328	97.934703	66.405966
1404.841962	98.231059	66.410970
1404.672388	88.908183	66.415975
1404.173540	91.745601	66.420980
1403.280151	93.603350	66.425985
1402.375482	87.664788	66.430990
1401.265541	94.615869	66.435994
1401.190915	88.950662	66.440999
1400.702816	99.794215	66.446004
1400.196705	91.251810	66.451009
1400.066321	89.154681	66.456014
1398.853456	92.121355	66.461018
1398.305330	90.607867	66.466023
1397.846152	97.480749	66.471028
1396.559311	102.397278	66.476033
1396.245730	94.688450	66.481038
1395.791825	101.051135	66.486042
1394.858972	93.697782	66.491047
1393.551488	91.965940	66.496052
1392.885563	92.212149	66.501057
1392.497352	98.635356	66.506062
1392.057388	100.074109	66.511066
1392.006020	92.785658	66.516071
1390.973862	100.877145	66.521076
1389.877069	96.132925	66.526081
1389.489312	93.788118	66.531086
1388.798236	92.962834	66.536090
1388.271762	91.065858	66.541095
1387.276505	88.098514	66.546100
1386.501377	97.016480	66.551105
1386.354974	85.605175	66.556110
1385.794146	99.677302	66.561114
1384.762524	94.578946	66.566119
1383.916720	91.736083	66.571124
1383.288133	97.711791	66.576129
1383.209494	90.673684	66.581134
1382.466310	96.656568	66.586138
1381.544141	90.673485	66.591143
1380.516806	95.930397	66.596148
1380.302041	92.269714	66.601153
1380.208852	83.008822	66.606158
1378.479884	94.044875	66.611162
1377.948292	88.759812	66.616167
1377.256323	89.372867	66.621172
1376.605073	88.036627	66.626177
1376.424206	92.764752	66.631182
1375.708018	97.101724	66.636186
1375.057021	95.393278	66.641191
1374.034034	92.889245	66.646196
1373.646686	97.457802	66.651201
1373.256261	83.667797	66.656206
1371.998351	94.245776	66.661210
1371.600634	89.642762	66.666215
1370.868522	89.519448	66.671220
1370.187788	98.676306	66.676225
1369.949675	93.699412	66.681230
1368.759294	99.702920	66.686234
1367.964031	90.121532	66.691239
1367.621734	90.551274	66.696244
1366.978828	91.574429	66.701249
1367.021509	85.545225	66.706254
1365.217702	95.099794	66.711258
1364.695292	92.777973	66.716263
1364.462810	91.729988	66.721268
1363.867619	92.660404	66.726273
1363.453302	93.954734	66.731278
1362.169274	89.479989	66.736282
1361.710933	89.037191	66.741287
1361.047492	101.925561	66.746292
1360.562332	94.833799	66.751297
1359.791169	81.164246	66.756302
1358.501809	97.886360	66.761306
1358.219141	94.491941	66.766311
1357.767395	88.432517	66.771316
1357.106118	96.203283	66.776321
1357.130532	96.068529	66.781326
1355.565886	97.487364	66.786330
1354.967386	97.265545	66.791335
1354.471088	95.259699	66.796340
1353.792031	97.015586	66.801345
1353.090458	97.426746	66.806350
1351.997576	95.290226	66.811354
1351.782514	101.477754	66.816359
1351.407997	96.030531	66.821364
1350.626780	94.560414	66.826369
1349.755903	87.085267	66.831374
1348.818795	95.973794	66.836378
1348.517681	89.448876	66.841383
1348.102569	92.637272	66.846388
1347.325453	92.447001	66.851393
1346.780405	84.707173	66.856398
1345.869304	95.283650	66.861402
1345.522887	93.326522	66.866407
1344.300942	97.068954	66.871412
1343.188815	96.818396	66.876417
1342.932840	98.445531	66.881422
1342.378997	98.457892	66.886426
1341.862677	93.258719	66.891431
1341.544986	86.365853	66.896436
1340.925145	98.660659	66.901441
1339.898731	84.924452	66.906446
1339.003674	98.631815	66.911450
1338.747194	94.192438	66.916455
1338.366157	97.432189	66.921460
1337.293120	92.152781	66.926465
1336.851690	84.874305	66.931470
1335.951739	95.450589	66.936474
1335.212990	93.842838	66.941479
1334.147278	98.651700	66.946484
1333.496091	96.899141	66.951489
1333.372744	87.346578	66.956494
1332.586387	96.925511	66.961498
1332.264811	90.350232	66.966503
1331.899584	93.303616	66.971508
1330.775221	95.567117	66.976513
1330.370292	90.870640	66.981518
1329.175046	90.439335	66.986522
1328.307386	95.087403	66.991527
1327.587959	93.503391	66.996532
1327.265342	100.964860	67.001537
1327.101691	92.144106	67.006542
1326.443696	96.400874	67.011546
1325.129726	90.525832	67.016551
1324.718868	89.238124	67.021556
1324.113788	94.208731	67.026561
1323.836900	89.004619	67.031566
1322.684443	93.497688	67.036570
1321.917993	93.531235	67.041575
1321.573326	90.876814	67.046580
1320.943626	90.869699	67.051585
1320.309242	95.475955	67.056590
1319.080322	100.162534	67.061594
1318.368968	92.636807	67.066599
1318.317632	94.053215	67.071604
1317.652063	89.320904	67.076609
1316.665084	91.982043	67.081614
1315.579429	97.983115	67.086618
1315.268773	91.097018	67.091623
1314.775698	89.395023	67.096628
1314.166245	92.967558	67.101633
1314.305123	86.719634	67.106638
1312.800263	105.880904	67.111642
1312.189978	88.957736	67.116647
1311.764678	89.082134	67.121652
1310.704573	97.482442	67.126657
1310.200143	83.153911	67.131662
1309.305343	93.644225	67.136666
1308.568844	89.460939	67.141671
1308.067153	87.787125	67.146676
1307.713537	98.744923	67.151681
1307.215248	77.615544	67.156686
1305.929703	90.520806	67.161690
1305.328517	87.845667	67.166695
1305.259312	87.730527	67.171700
1304.608834	91.326932	67.176705
1303.569078	85.769436	67.181710
1302.710606	100.369861	67.186714
1302.215462	91.917205	67.191719
1301.801469	88.639868	67.196724
1300.784971	90.168713	67.201729
1300.199561	83.526577	67.206734
1299.472570	94.242530	67.211738
1299.271303	98.306846	67.216743
1298.766200	98.120654	67.221748
1298.099722	94.905534	67.226753
1297.593009	87.837720	67.231758
1296.093162	98.427385	67.236762
1295.619710	88.242929	67.241767
1294.848292	91.051156	67.246772
1294.285272	89.082741	67.251777
1294.023939	85.278084	67.256782
1292.517203	93.924445	67.261786
1292.144423	93.550060	67.266791
1291.269284	84.996972	67.271796
1291.113697	99.474614	67.276801
1290.625938	91.090174	67.281806
1290.134085	91.400199	67.286810
1288.946132	94.738278	67.291815
1288.364279	90.867883	67.296820
1287.668347	93.173676	67.301825
1287.356761	82.813680	67.306830
1286.441704	94.986689	67.311834
1285.620223	87.278210	67.316839
1285.127418	90.922092	67.321844
1284.633986	90.544812	67.326849
1283.742628	86.113340	67.331854
1282.379312	95.285689	67.336858
1282.054313	94.072648	67.341863
1281.495006	92.775432	67.346868
1280.823965	94.110589	67.351873
1280.768816	85.775648	67.356878
1280.338699	88.990091	67.361882
1279.295308	91.699636	67.366887
1278.853404	87.904766	67.371892
1278.018286	93.463892	67.376897
1277.164827	90.130272	67.381902
1275.990091	99.105486	67.386906
1275.745209	99.032469	67.391911
1275.593271	89.970164	67.396916
1274.659374	97.222888	67.401921
1273.864681	88.830482	67.406926
1273.090125	92.219538	67.411930
1272.610695	97.430378	67.416935
1271.937435	86.643757	67.421940
1270.848347	102.097722	67.426945
1270.576058	84.490054	67.431950
1269.667097	91.942240	67.436954
1268.883699	95.083543	67.441959
1269.159294	83.095808	67.446964
1268.185173	107.207962	67.451969
1267.528436	86.964801	67.456974
1266.555929	96.833543	67.461978
1266.151674	92.641601	67.466983
1265.230895	86.328763	67.471988
1264.319821	90.816593	67.476993
1263.999556	79.385650	67.481998
1263.683665	88.687939	67.487002
1262.775247	97.871552	67.492007
1262.004780	88.939130	67.497012
1261.145252	90.595999	67.502017
1260.870467	86.747754	67.507022
1260.100445	92.080490	67.512026
1258.787844	98.127127	67.517031
1258.204609	87.212656	67.522036
1257.603241	94.448783	67.527041
1257.655469	86.965680	67.532046
1257.098603	88.957631	67.537050
1256.060215	94.916514	67.542055
1255.307455	87.192391	67.547060
1254.273209	94.978319	67.552065
1254.133512	91.655802	67.557070
1253.491232	89.403529	67.562074
1253.005801	91.992831	67.567079
1252.109160	94.005690	67.572084
1250.980921	94.397982	67.577089
1250.820102	80.803324	67.582094
1250.577192	84.648752	67.587098
1249.333732	91.144871	67.592103
1248.976511	95.347525	67.597108
1248.252268	89.238413	67.602113
1247.394791	88.535821	67.607118
1246.374601	91.899283	67.612122
1245.902580	93.481928	67.617127
1245.623372	88.920023	67.622132
1244.828346	95.581390	67.627137
1244.572608	95.874382	67.632142
1243.207116	95.236795	67.637146
1242.803729	94.182880	67.642151
1242.160494	87.860616	67.647156
1241.610333	95.949627	67.652161
1241.296516	90.371351	67.657166
1239.994863	87.553713	67.662170
1239.570741	96.794369	67.667175
1239.306928	86.955069	67.672180
1237.764023	96.577042	67.677185
1237.176552	90.348414	67.682190
1236.556736	93.343866	67.687194
1236.322999	95.139362	67.692199
1236.171606	93.400403	67.697204
1235.158783	97.536989	67.702209
1234.075933	85.315816	67.707214
1233.464520	94.871682	67.712218
1233.230257	94.363316	67.717223
1232.130813	89.900294	67.722228
1230.865102	93.678119	67.727233
1230.780629	88.777744	67.732238
1230.298776	88.550023	67.737242
1230.061551	94.403604	67.742247
1229.492733	92.909214	67.747252
1228.348267	95.163338	67.752257
1227.861478	81.290930	67.757262
1227.091523	91.767719	67.762266
1226.129707	91.452311	67.767271
1225.399764	90.428247	67.772276
1224.378782	95.234767	67.777281
1224.166019	88.281083	67.782286
1224.265934	93.693123	67.787290
1223.274381	97.435244	67.792295
1222.499065	97.424499	67.797300
1221.277081	95.999277	67.802305
1221.301746	89.233346	67.807310
1220.404252	99.060212	67.812314
1219.218550	92.417352	67.817319
1218.830669	91.595945	67.822324
1218.104641	97.752757	67.827329
1217.989799	91.013740	67.832334
1217.714312	93.952867	67.837338
1216.439560	91.112040	67.842343
1215.736080	85.499537	67.847348
1214.892840	91.498366	67.852353
1214.674995	92.889210	67.857358
1213.349259	90.884398	67.862362
1212.443565	93.942660	67.867367
1212.325611	89.440274	67.872372
1211.570866	101.240881	67.877377
1211.720450	82.973210	67.882382
1211.149276	97.594197	67.887386
1210.003292	100.507742	67.892391
1209.444126	91.350928	67.897396
1208.238207	94.969444	67.902401
1207.500843	78.604286	67.907406
1206.802301	86.089259	67.912410
1206.152958	100.460903	67.917415
1205.868004	87.944131	67.922420
1205.660191	96.532223	67.927425
1204.953396	91.675614	67.932430
1204.194608	81.691105	67.937434
1203.463990	90.565756	67.942439
1202.629597	85.134925	67.947444
1201.774946	84.922335	67.952449
1201.230164	93.798976	67.957454
1200.987622	89.135052	67.962458
1199.791217	87.149106	67.967463
1199.171874	80.976025	67.972468
1198.024302	89.551123	67.977473
1197.729631	86.188601	67.982478
1197.350747	97.308115	67.987482
1196.841102	83.426735	67.992487
1196.120650	84.413376	67.997492
1194.904736	86.568487	68.002497
1194.775507	86.120694	68.007502
1194.052433	88.609022	68.012506
1192.920155	90.854914	68.017511
1192.412839	85.900358	68.022516
1191.831234	90.960295	68.027521
1191.391616	87.849483	68.032526
1191.123860	92.826397	68.037530
1190.433438	97.454206	68.042535
1189.512845	89.748910	68.047540
1188.833530	93.097612	68.052545
1187.714342	90.489107	68.057550
1186.870400	94.696625	68.062554
1186.146552	92.205027	68.067559
1186.005151	81.625604	68.072564
1185.139316	93.540069	68.077569
1184.885456	94.879873	68.082574
1184.564901	85.412311	68.087578
1183.514692	87.096372	68.092583
1183.020876	74.168128	68.097588
1182.237930	94.753746	68.102593
1181.314028	86.552238	68.107598
1180.765546	90.589769	68.112602
1179.791533	86.863769	68.117607
1179.693777	85.978884	68.122612
1178.649042	89.989675	68.127617
1177.778614	88.423413	68.132622
1177.201577	82.926435	68.137626
1176.629746	85.701377	68.142631
1176.769046	75.507832	68.147636
1175.421928	84.068937	68.152641
1174.791043	77.525537	68.157646
1173.961502	81.781228	68.162650
1173.371143	87.791891	68.167655
1173.428757	81.427584	68.172660
1172.121860	83.781678	68.177665
1171.783820	80.965379	68.182670
1171.183970	90.186672	68.187674
1169.817467	82.839309	68.192679
1169.276730	81.424049	68.197684
1168.624416	94.340626	68.202689
1168.232867	76.919122	68.207694
1168.005974	85.292620	68.212698
1166.747057	84.620780	68.217703
1166.282270	76.267424	68.222708
1165.466841	97.119987	68.227713
1165.043678	85.358496	68.232718
1164.278296	85.694697	68.237722
1163.090441	86.763564	68.242727
1162.774340	84.293863	68.247732
1162.034294	77.950754	68.252737
1161.739148	79.773366	68.257742
1161.389829	79.172918	68.262746
1160.141780	90.706622	68.267751
1159.735243	82.359770	68.272756
1159.033694	88.545815	68.277761
1158.640738	83.860088	68.282766
1157.714384	73.397625	68.287770
1156.591221	87.130250	68.292775
1156.329053	78.147003	68.297780
1155.965331	79.505856	68.302785
1155.112697	79.775512	68.307790
1154.487599	77.030100	68.312794
1153.878934	84.805143	68.317799
1153.059951	74.492763	68.322804
1151.886456	82.527945	68.327809
1151.427858	81.027085	68.332814
1151.121255	85.330506	68.337818
1150.117203	83.317148	68.342823
1150.027992	75.109072	68.347828
1148.585741	85.301704	68.352833
1148.133731	80.048204	68.357838
1147.676132	80.157264	68.362842
1147.240244	83.410489	68.367847
1146.841365	81.535854	68.372852
1145.778544	81.011035	68.377857
1144.952128	77.062882	68.382862
1144.495352	78.427074	68.387866
1143.895962	82.155736	68.392871
1142.704548	83.908002	68.397876
1142.093118	83.524286	68.402881
1141.903842	84.667739	68.407886
1141.527193	82.061013	68.412890
1140.725857	92.959128	68.417895
1140.148162	81.234839	68.422900
1139.361816	93.040477	68.427905
1138.732746	90.205812	68.432910
1137.415643	84.905394	68.437914
1136.605960	79.907479	68.442919
1136.426955	85.379636	68.447924
1135.742475	90.728759	68.452929
1135.421461	84.613906	68.457934
1135.059391	86.658478	68.462938
1133.517455	92.812606	68.467943
1133.308716	82.461522	68.472948
1132.874360	93.399044	68.477953
1132.102396	87.201368	68.482958
1131.114627	83.709392	68.487962
1130.136455	79.974615	68.492967
1129.983226	79.328791	68.497972
1129.537333	86.641133	68.502977
1128.306037	86.262965	68.507982
1127.519739	78.216221	68.512986
1126.927981	91.610451	68.517991
1126.887851	89.817534	68.522996
1126.174615	83.520635	68.528001
1125.187645	90.062744	68.533006
1124.520328	81.913497	68.538010
1124.003779	86.977290	68.543015
1123.440755	80.462536	68.548020
1122.325032	85.199001	68.553025
1121.494127	83.913481	68.558030
1121.350211	84.079889	68.563034
1120.554098	84.130830	68.568039
1120.284881	79.100579	68.573044
1119.512097	87.915717	68.578049
1118.635152	88.085172	68.583054
1117.893397	82.202822	68.588058
1117.277625	95.394294	68.593063
1117.093340	80.330514	68.598068
1115.915178	84.088156	68.603073
1115.365224	80.182775	68.608078
1114.795717	76.091270	68.613082
1114.145501	90.556092	68.618087
1113.418609	78.961202	68.623092
1112.678281	84.621986	68.628097
1112.072110	80.817011	68.633102
1111.789161	81.710435	68.638106
1110.015119	83.397688	68.643111
1109.652516	78.896381	68.648116
1109.420730	85.507614	68.653121
1108.759614	86.090601	68.658126
1108.791836	83.999171	68.663130
1107.549605	84.316616	68.668135
1107.143495	75.558126	68.673140
1106.510026	88.306128	68.678145
1105.410606	82.207856	68.683150
1104.797952	80.198496	68.688154
1104.105039	84.273203	68.693159
1103.665493	75.259834	68.698164
1102.618373	85.604106	68.703169
1101.924344	77.099571	68.708174
1101.355697	77.999014	68.713178
1100.602055	75.359219	68.718183
1100.433960	69.959650	68.723188
1099.761671	75.114447	68.728193
1098.680492	82.450564	68.733198
1098.489506	75.715795	68.738202
1097.864201	78.636452	68.743207
1096.653833	78.024735	68.748212
1095.643842	84.359199	68.753217
1095.411218	76.749531	68.758222
1095.124449	84.101220	68.763226
1094.595474	86.418351	68.768231
1093.521363	75.652987	68.773236
1092.805543	82.224514	68.778241
1092.247842	87.089853	68.783246
1091.897432	81.572623	68.788250
1090.674307	89.811269	68.793255
1090.346803	79.404969	68.798260
1089.649454	89.065982	68.803265
1088.979445	84.634074	68.808270
1088.553005	87.508910	68.813274
1087.279055	90.822907	68.818279
1087.000735	76.083181	68.823284
1086.383084	85.493395	68.828289
1085.813022	83.043600	68.833294
1084.982553	76.457858	68.838298
1084.013968	87.253272	68.843303
1083.598678	71.395195	68.848308
1083.520015	81.429306	68.853313
1082.577529	76.914586	68.858318
1081.366618	72.980307	68.863322
1081.195434	80.990125	68.868327
1080.844517	81.252541	68.873332
1079.464473	89.550844	68.878337
1078.638711	91.416866	68.883342
1078.275899	81.145495	68.888346
1077.551033	86.015349	68.893351
1077.421579	74.274983	68.898356
1076.257584	86.880292	68.903361
1075.287049	77.744809	68.908366
1075.066242	84.573494	68.913370
1074.340793	93.456810	68.918375
1073.946280	83.420718	68.923380
1073.056847	91.144242	68.928385
1072.246291	80.584547	68.933390
1072.223063	72.457450	68.938394
1071.421715	79.000007	68.943399
1070.312727	81.609677	68.948404
1069.408701	89.747110	68.953409
1068.626436	85.407181	68.958414
1068.503351	79.554173	68.963418
1068.034656	83.829766	68.968423
1067.887254	82.531735	68.973428
1066.527309	84.787086	68.978433
1066.049272	80.253686	68.983438
1065.254505	82.468021	68.988442
1064.449042	83.507644	68.993447
1063.623279	82.404253	68.998452
1063.080452	87.260923	69.003457
1062.607428	88.190896	69.008462
1061.519464	82.024591	69.013466
1060.831243	93.593860	69.018471
1060.372035	81.672555	69.023476
1060.289058	77.150432	69.028481
1059.773103	83.534055	69.033486
1058.899521	71.103084	69.038490
1057.889191	84.573358	69.043495
1057.490014	76.086593	69.048500
1056.289954	81.497243	69.053505
1055.665182	88.241956	69.058510
1055.234574	86.408655	69.063514
1054.478579	90.816686	69.068519
1054.375315	82.889976	69.073524
1053.365211	84.269663	69.078529
1052.158619	89.695550	69.083534
1051.631030	80.224686	69.088538
1051.242150	87.207843	69.093543
1051.185691	76.042498	69.098548
1050.068886	85.771818	69.103553
1049.407223	88.229914	69.108558
1049.288401	90.842932	69.113562
1047.859904	86.105913	69.118567
1047.306207	83.312902	69.123572
1046.515111	90.680167	69.128577
1046.014128	86.249768	69.133582
1045.612543	90.156721	69.138586
1044.573985	88.180434	69.143591
1043.824137	86.465728	69.148596
1043.436755	81.898988	69.153601
1042.720984	90.025405	69.158606
1041.753291	85.629827	69.163610
1041.037172	86.224735	69.168615
1040.366469	79.474822	69.173620
1039.978689	82.975875	69.178625
1039.630145	89.110520	69.183630
1039.361014	84.189076	69.188634
1038.235815	88.775693	69.193639
1037.529348	88.430775	69.198644
1037.147099	87.288378	69.203649
1035.988392	88.661749	69.208654
1035.419146	84.045094	69.213658
1034.550928	81.723168	69.218663
1034.246491	89.337871	69.223668
1033.579035	76.475145	69.228673
1032.494730	81.250800	69.233678
1032.052742	79.387775	69.238682
1031.348780	85.227298	69.243687
1031.202174	75.331558	69.248692
1030.392223	81.607412	69.253697
1029.468555	74.579201	69.258702
1029.088505	75.724624	69.263706
1028.078217	88.212457	69.268711
1027.304747	72.141718	69.273716
1026.437130	75.193979	69.278721
1026.047016	82.910618	69.283726
1025.855938	75.847866	69.288730
1024.841495	81.009803	69.293735
1024.526650	79.594910	69.298740
1023.304830	81.159678	69.303745
1022.538618	74.615779	69.308750
1022.220340	73.445862	69.313754
1021.578086	90.768454	69.318759
1021.175586	78.164780	69.323764
1020.368639	84.321888	69.328769
1019.737073	89.186375	69.333774
1019.300604	80.885322	69.338778
1018.245293	82.243829	69.343783
1017.407622	83.458903	69.348788
1016.864897	83.466411	69.353793
1016.223698	76.880548	69.358798
1016.091785	80.750908	69.363802
1014.845890	86.006442	69.368807
1014.440071	77.840866	69.373812
1013.974703	87.282058	69.378817
1012.874676	81.969255	69.383822
1012.343286	84.692064	69.388826
1011.512072	83.624251	69.393831
1011.294333	75.401947	69.398836
1010.372000	83.301029	69.403841
1009.557262	87.701070	69.408846
1008.965733	77.287910	69.413850
1008.098845	85.614992	69.418855
1007.993380	82.318593	69.423860
1006.971486	78.485168	69.428865
1006.279749	72.199088	69.433870
1005.691321	66.418549	69.438874
1005.246160	78.802279	69.443879
1004.549232	82.877647	69.448884
1003.518806	85.802854	69.453889
1002.783572	77.175600	69.458894
1002.768638	74.503469	69.463898
1001.877125	91.648098	69.468903
1001.412009	76.564373	69.473908
1000.596187	78.342104	69.478913
999.749355	81.805807	69.483918
999.026536	75.501019	69.488922
997.833173	74.626446	69.493927
997.528658	73.790235	69.498932
997.097177	82.863334	69.503937
996.606752	85.669514	69.508942
996.333814	82.298835	69.513946
995.175086	79.252011	69.518951
994.388349	76.737365	69.523956
993.882128	75.564236	69.528961
993.158157	77.877715	69.533966
992.675203	75.592283	69.538970
991.685612	83.804848	69.543975
991.281948	83.648311	69.548980
990.904286	78.231632	69.553985
989.600149	84.568775	69.558990
989.211296	76.253850	69.563994
988.257116	81.738950	69.568999
988.151513	68.745859	69.574004
987.545351	75.678428	69.579009
986.444608	73.630061	69.584014
985.811344	76.955709	69.589018
984.900803	72.205713	69.594023
984.897608	70.367504	69.599028
983.944051	82.398461	69.604033
982.636609	82.051403	69.609038
982.429780	80.329170	69.614042
981.973512	89.794149	69.619047
981.287680	69.786017	69.624052
981.309801	79.233224	69.629057
979.833689	72.611477	69.634062
979.510314	67.522060	69.639066
978.825516	76.993429	69.644071
977.998908	72.974407	69.649076
977.115482	79.345542	69.654081
976.264727	84.624957	69.659086
976.350980	76.329060	69.664090
975.694794	81.566479	69.669095
974.457237	80.318901	69.674100
974.008778	79.852526	69.679105
973.219797	80.917940	69.684110
972.935486	74.371504	69.689114
972.241128	81.002719	69.694119
971.310667	76.166011	69.699124
970.971651	84.875893	69.704129
969.975966	85.799154	69.709134
969.213201	76.963404	69.714138
968.548388	76.706495	69.719143
968.134410	76.767647	69.724148
968.049735	76.145621	69.729153
966.630573	77.144146	69.734158
966.229378	73.358640	69.739162
965.559607	81.256973	69.744167
965.001930	78.163417	69.749172
963.716713	70.472093	69.754177
962.990820	76.554814	69.759182
963.065049	77.159609	69.764186
962.559088	75.145928	69.769191
961.281960	83.153515	69.774196
960.439970	85.845327	69.779201
959.803576	81.684080	69.784206
959.484566	78.737055	69.789210
959.075217	83.613503	69.794215
958.400962	82.847165	69.799220
957.601332	83.428575	69.804225
956.906858	85.387286	69.809230
956.678252	77.630345	69.814234
955.531381	94.347259	69.819239
954.768565	81.985437	69.824244
954.066937	78.052192	69.829249
953.509628	87.501711	69.834254
953.293037	84.505273	69.839258
951.799472	88.647486	69.844263
951.292439	88.319745	69.849268
950.939214	79.544994	69.854273
950.345672	86.213792	69.859278
949.547304	76.888550	69.864282
948.646194	83.027541	69.869287
948.380897	78.149659	69.874292
947.600399	84.573813	69.879297
947.161176	86.994962	69.884302
946.070488	79.502927	69.889306
945.762638	82.029328	69.894311
945.177170	78.358301	69.899316
944.722247	77.902422	69.904321
943.327325	85.340555	69.909326
942.888782	78.687776	69.914330
942.333398	77.842604	69.919335
941.915206	70.137914	69.924340
940.839353	75.593502	69.929345
939.839926	78.170021	69.934350
939.661055	75.129738	69.939354
938.954334	80.890870	69.944359
938.634552	79.186614	69.949364
938.152391	82.811507	69.954369
937.006975	85.766074	69.959374
936.483293	80.968731	69.964378
935.657160	89.639433	69.969383
934.759211	85.541888	69.974388
934.086911	83.851147	69.979393
933.651750	75.220328	69.984398
933.508664	75.664159	69.989402
932.608617	82.829585	69.994407
931.620924	73.301089	69.999412
931.072748	80.834726	70.004417
930.212057	78.640953	70.009422
930.161523	80.913521	70.014426
928.937008	86.574123	70.019431
928.322115	81.690370	70.024436
928.247128	74.490889	70.029441
926.876859	80.803889	70.034446
926.382507	70.704883	70.039450
925.524555	83.013956	70.044455
925.005058	77.525243	70.049460
924.934897	76.043044	70.054465
923.880078	81.460600	70.059470
923.370441	85.233371	70.064474
922.660655	87.699154	70.069479
922.457081	79.320067	70.074484
921.245609	85.789153	70.079489
920.486638	80.297546	70.084494
920.123737	75.138733	70.089498
919.024478	79.714959	70.094503
917.978059	84.878868	70.099508
917.510914	75.165042	70.104513
916.948089	82.645819	70.109518
917.157015	73.272268	70.114522
916.398216	83.058203	70.119527
915.175534	80.541991	70.124532
914.498862	83.139701	70.129537
913.865234	88.752015	70.134542
913.648770	76.973483	70.139546
912.510025	87.493243	70.144551
911.830374	79.738698	70.149556
911.481221	78.594209	70.154561
910.792618	78.826804	70.159566
909.972482	80.502747	70.164570
909.271339	87.343216	70.169575
908.615502	83.226078	70.174580
908.255355	76.422061	70.179585
906.979434	91.416983	70.184590
906.442673	73.736406	70.189594
905.853261	83.736663	70.194599
905.405932	78.793137	70.199604
904.952632	77.936459	70.204609
903.928202	88.397031	70.209614
903.601354	78.295026	70.214618
902.990591	86.551414	70.219623
901.994592	81.865511	70.224628
901.289753	73.900515	70.229633
900.146973	83.864253	70.234638
900.329988	76.500714	70.239642
899.844412	71.235272	70.244647
898.468661	85.657872	70.249652
897.953973	79.857740	70.254657
897.426016	81.763158	70.259662
897.004496	71.245716	70.264666
895.864125	81.333650	70.269671
895.314167	80.615358	70.274676
894.592492	72.783932	70.279681
894.396040	77.864626	70.284686
893.719552	67.312068	70.289690
892.613768	72.788205	70.294695
892.088234	82.836646	70.299700
891.701697	71.432118	70.304705
890.869911	80.387577	70.309710
890.042492	74.671909	70.314714
889.250444	87.307974	70.319719
888.719138	85.033411	70.324724
888.779223	82.202687	70.329729
887.275877	92.291625	70.334734
886.818002	82.953220	70.339738
886.115993	83.840816	70.344743
885.284778	83.919495	70.349748
885.066596	81.636104	70.354753
884.098151	77.565570	70.359758
883.449330	77.261984	70.364762
882.986567	77.209488	70.369767
882.253378	79.480307	70.374772
881.503846	71.792091	70.379777
880.687229	82.661142	70.384782
880.380012	73.284576	70.389786
879.946582	83.373554	70.394791
878.762176	81.020003	70.399796
878.294785	76.841347	70.404801
877.461291	91.605020	70.409806
877.103799	82.764732	70.414810
876.507584	79.074934	70.419815
875.298715	85.926825	70.424820
874.648185	78.971907	70.429825
873.768880	85.670425	70.434830
873.934144	82.827693	70.439834
873.289963	86.106219	70.444839
872.391617	78.883234	70.449844
871.898918	76.498454	70.454849
871.141365	85.390066	70.459854
870.274337	80.341453	70.464858
869.406835	73.537765	70.469863
868.658536	81.450190	70.474868
868.436623	67.497919	70.479873
867.803837	83.932756	70.484878
867.242837	83.370770	70.489882
866.339593	78.668545	70.494887
865.943285	79.699884	70.499892
865.278347	75.421783	70.504897
863.948543	80.887855	70.509902
863.251090	84.346749	70.514906
862.796077	83.815205	70.519911
861.981062	82.500436	70.524916
862.155444	78.842544	70.529921
861.545907	85.515478	70.534926
860.738236	81.144975	70.539930
859.920313	87.975655	70.544935
859.151997	76.072074	70.549940
858.096504	78.927206	70.554945
857.456830	84.168329	70.559950
857.298743	77.698019	70.564954
856.734929	77.746765	70.569959
855.694792	73.482650	70.574964
855.120897	74.553292	70.579969
854.286961	87.716425	70.584974
853.988173	84.879738	70.589978
853.622386	75.681233	70.594983
852.479764	87.236113	70.599988
852.088157	81.824836	70.604993
851.313320	79.868163	70.609998
850.616552	79.286788	70.615002
849.259801	73.716884	70.620007
848.798647	86.278213	70.625012
848.492218	78.918455	70.630017
848.283849	81.074217	70.635022
847.338406	72.300709	70.640026
846.112634	80.970376	70.645031
845.520640	79.147031	70.650036
845.641096	72.850013	70.655041
844.779715	73.125894	70.660046
844.158636	71.363951	70.665050
843.622273	84.454491	70.670055
842.580757	76.230862	70.675060
841.706445	71.331656	70.680065
840.716856	76.820860	70.685070
840.081007	80.727272	70.690074
839.704599	81.477903	70.695079
839.327553	86.295607	70.700084
838.852525	82.733188	70.705089
838.455800	75.835660	70.710094
837.727665	80.725011	70.715098
837.131492	75.988119	70.720103
835.711855	84.073634	70.725108
834.746904	74.614105	70.730113
834.247748	76.018210	70.735118
834.068295	65.388145	70.740122
833.834632	70.566224	70.745127
832.772486	80.074024	70.750132
832.179949	76.681699	70.755137
831.578986	85.438009	70.760142
831.115082	73.120138	70.765146
829.933041	79.594036	70.770151
829.172530	78.434607	70.775156
828.918545	71.025509	70.780161
828.223783	80.593109	70.785166
827.239758	83.376954	70.790170
826.414416	79.431901	70.795175
825.823022	84.264799	70.800180
825.676550	73.891256	70.805185
824.993355	87.031978	70.810190
824.110087	77.895343	70.815194
823.344709	79.819640	70.820199
822.630299	86.346847	70.825204
822.342333	84.574466	70.830209
821.118503	92.493208	70.835214
820.762912	77.896740	70.840218
820.193672	82.052752	70.845223
819.746889	81.042088	70.850228
818.680728	65.185203	70.855233
817.754309	82.441063	70.860238
817.400370	62.875359	70.865242
816.936220	77.655935	70.870247
816.435707	78.114085	70.875252
815.842963	59.644533	70.880257
814.849354	73.984252	70.885262
814.660775	67.304340	70.890266
813.926346	75.101024	70.895271
812.836219	82.607399	70.900276
812.419684	72.371462	70.905281
811.394102	79.410245	70.910286
810.438984	72.666259	70.915290
809.808948	77.891663	70.920295
809.413121	80.298039	70.925300
809.511659	68.737479	70.930305
808.384354	76.847436	70.935310
807.372864	70.635975	70.940314
806.769854	69.642297	70.945319
806.261359	79.150289	70.950324
805.999386	70.894064	70.955329
804.860715	78.294625	70.960334
804.028793	63.450719	70.965338
803.702403	70.373477	70.970343
802.855020	71.527085	70.975348
802.818240	69.143869	70.980353
801.757740	78.375449	70.985358
801.066213	68.992267	70.990362
800.324783	75.109035	70.995367
799.536576	78.356884	71.000372
798.964823	67.238912	71.005377
797.959706	76.267711	71.010382
797.616275	72.466737	71.015386
797.268326	60.018467	71.020391
796.468478	74.114459	71.025396
795.686749	69.438657	71.030401
794.942730	81.381112	71.035406
794.354886	78.560484	71.040410
793.611460	76.600408	71.045415
792.641551	75.102162	71.050420
792.519302	70.841781	71.055425
791.524063	72.410013	71.060430
791.548803	73.492612	71.065434
790.692878	73.449099	71.070439
789.639455	77.057712	71.075444
789.298130	67.618791	71.080449
788.196632	77.774688	71.085454
787.617575	79.035401	71.090458
787.007729	72.417817	71.095463
786.500831	75.278691	71.100468
786.308275	70.346681	71.105473
785.163048	76.772157	71.110478
784.304302	75.486455	71.115482
783.861203	75.266843	71.120487
783.313373	86.250825	71.125492
782.611243	73.243914	71.130497
781.588317	74.732979	71.135502
780.876735	80.398724	71.140506
780.553435	69.709563	71.145511
780.112698	73.365730	71.150516
779.325319	73.674009	71.155521
778.579617	82.721448	71.160526
777.994503	78.348665	71.165530
777.379673	78.107506	71.170535
776.204351	84.389546	71.175540
775.824016	76.481748	71.180545
775.248412	76.306885	71.185550
774.469036	72.586349	71.190554
773.376273	72.165804	71.195559
772.418317	73.838495	71.200564
772.741128	71.281343	71.205569
771.762510	76.385624	71.210574
771.482566	75.630686	71.215578
771.423509	76.031187	71.220583
770.188234	76.568463	71.225588
769.483356	70.926378	71.230593
768.528756	81.806376	71.235598
767.761929	75.858760	71.240602
766.943143	72.434660	71.245607
766.194069	75.539094	71.250612
766.019521	70.008130	71.255617
765.716123	75.068004	71.260622
764.865660	71.948569	71.265626
764.254777	70.771651	71.270631
763.530601	68.392205	71.275636
762.878266	61.259425	71.280641
761.703801	73.243594	71.285646
761.192122	66.140460	71.290650
760.632386	64.939632	71.295655
759.887887	78.512737	71.300660
759.666032	67.846858	71.305665
758.537800	74.876765	71.310670
757.809077	71.378407	71.315674
757.609589	71.435411	71.320679
756.835949	71.566467	71.325684
755.839727	69.438490	71.330689
755.212643	74.283386	71.335694
755.001424	72.915114	71.340698
754.623593	63.780060	71.345703
753.200188	68.940958	71.350708
753.001912	72.128022	71.355713
752.202733	75.681983	71.360718
751.378491	75.087813	71.365722
750.519748	70.399055	71.370727
749.917132	72.901435	71.375732
749.510775	68.599555	71.380737
749.215488	69.477633	71.385742
748.362735	70.602151	71.390746
747.368383	71.307665	71.395751
747.132296	82.235712	71.400756
746.263402	63.231406	71.405761
745.353619	64.681972	71.410766
744.450876	68.484233	71.415770
744.062187	73.988194	71.420775
743.635748	75.360238	71.425780
743.549118	66.759145	71.430785
742.233462	74.858109	71.435790
741.485985	73.267702	71.440794
741.396738	64.917764	71.445799
740.089874	74.593858	71.450804
739.486538	64.627383	71.455809
738.833089	73.603367	71.460814
738.142775	69.677854	71.465818
737.286379	76.424797	71.470823
736.459581	74.265124	71.475828
736.006810	72.206756	71.480833
735.523341	75.161680	71.485838
735.120886	74.304825	71.490842
734.488131	67.441748	71.495847
733.514628	75.115660	71.500852
732.905329	74.228657	71.505857
732.313222	78.888219	71.510862
731.944406	76.633558	71.515866
730.923300	77.173027	71.520871
730.161282	82.840506	71.525876
729.702305	79.068976	71.530881
729.407198	76.640155	71.535886
727.938725	79.245694	71.540890
727.640315	71.917803	71.545895
726.675096	79.500514	71.550900
726.628431	84.074820	71.555905
725.998676	80.158590	71.560910
724.928471	82.686534	71.565914
724.590509	71.496671	71.570919
723.930210	78.568791	71.575924
722.725527	70.562014	71.580929
722.174795	78.255357	71.585934
721.651635	72.048193	71.590938
721.349774	68.729471	71.595943
720.296213	75.824776	71.600948
719.518465	68.871246	71.605953
718.867043	74.298767	71.610958
718.401035	75.043179	71.615962
718.130120	68.824244	71.620967
716.950593	84.098766	71.625972
716.334514	68.819988	71.630977
715.810876	68.944371	71.635982
715.422999	67.146912	71.640986
714.771089	68.386122	71.645991
713.581232	70.245566	71.650996
713.317503	66.160684	71.656001
712.540907	73.625057	71.661006
711.723635	71.501723	71.666010
711.096175	64.831777	71.671015
710.422872	76.840254	71.676020
709.906842	72.904349	71.681025
709.190281	78.619787	71.686030
708.128335	73.786778	71.691034
707.771961	64.545817	71.696039
707.270745	73.480222	71.701044
707.000954	71.167223	71.706049
706.092283	66.989481	71.711054
704.876669	75.783739	71.716058
704.259121	67.148909	71.721063
703.650820	70.519527	71.726068
703.985146	63.898306	71.731073
702.475690	73.272357	71.736078
701.640768	76.305320	71.741082
701.336769	71.340601	71.746087
700.713777	74.074894	71.751092
699.867715	70.470658	71.756097
698.789719	79.536323	71.761102
698.386820	68.987590	71.766106
698.074802	59.462029	71.771111
697.501852	67.524759	71.776116
697.113316	72.375841	71.781121
696.092599	71.478658	71.786126
695.438157	73.598217	71.791130
694.761514	62.914877	71.796135
693.897423	73.677977	71.801140
693.328309	67.903917	71.806145
692.890176	66.795706	71.811150
692.035889	69.533710	71.816154
691.203858	68.902954	71.821159
690.494957	72.448866	71.826164
690.337143	70.816630	71.831169
689.316321	64.581482	71.836174
688.251752	70.147328	71.841178
687.680663	72.356119	71.846183
687.106207	62.331449	71.851188
687.023236	69.915622	71.856193
686.528697	68.847933	71.861198
685.215774	69.913277	71.866202
684.879464	65.660182	71.871207
683.994142	75.247105	71.876212
683.643836	64.338345	71.881217
682.302284	68.574768	71.886222
681.464426	71.288083	71.891226
681.419178	72.496941	71.896231
680.813143	65.156542	71.901236
680.785082	64.475051	71.906241
679.378574	70.574737	71.911246
678.784547	67.964861	71.916250
678.458234	76.451954	71.921255
677.199585	77.754665	71.926260
676.586795	65.197205	71.931265
675.940229	69.764521	71.936270
675.330304	73.927034	71.941274
675.070572	70.090679	71.946279
674.301098	73.900128	71.951284
673.712802	69.450614	71.956289
673.296903	68.185903	71.961294
672.348554	67.501134	71.966298
671.341928	67.204113	71.971303
670.463146	73.822174	71.976308
670.105148	63.477615	71.981313
669.782816	70.916974	71.986318
668.936582	62.909928	71.991322
668.082708	65.247328	71.996327
667.442098	74.472015	72.001332
667.075589	72.699546	72.006337
666.422893	73.620350	72.011342
665.497152	67.854197	72.016346
664.674007	70.099973	72.021351
664.107208	78.338353	72.026356
664.197318	73.211539	72.031361
663.063816	68.976573	72.036366
662.149840	66.468110	72.041370
661.837370	72.612799	72.046375
660.831010	75.124293	72.051380
659.993258	71.684329	72.056385
659.117016	73.946446	72.061390
658.668569	72.533956	72.066394
658.477495	67.489764	72.071399
658.024104	71.715665	72.076404
657.262574	74.158213	72.081409
656.515627	77.418456	72.086414
655.577041	78.832640	72.091418
655.267018	63.957744	72.096423
653.768139	75.447982	72.101428
653.493985	74.332591	72.106433
652.863042	73.346553	72.111438
652.551948	75.581761	72.116442
651.830444	66.331144	72.121447
651.157495	67.094327	72.126452
650.789315	68.540687	72.131457
650.288276	66.994647	72.136462
648.917660	75.520295	72.141466
648.410044	74.662854	72.146471
648.071725	74.828705	72.151476
647.213080	70.352861	72.156481
646.248559	72.159107	72.161486
645.308825	72.324531	72.166490
645.348003	67.585875	72.171495
644.546264	70.391220	72.176500
643.490177	72.915369	72.181505
642.601833	73.862664	72.186510
642.369090	65.131888	72.191514
642.154337	66.285736	72.196519
641.529807	72.995782	72.201524
640.622544	70.437371	72.206529
640.017471	70.581046	72.211534
639.279407	66.095467	72.216538
638.576027	69.109078	72.221543
637.189407	73.584513	72.226548
636.952286	69.643638	72.231553
636.535770	65.149435	72.236558
636.093141	69.272699	72.241562
636.052835	61.159411	72.246567
634.713714	77.269917	72.251572
634.194488	63.134817	72.256577
633.033935	61.884614	72.261582
631.904527	72.882364	72.266586
631.841493	61.450057	72.271591
630.956086	67.346938	72.276596
630.973298	69.268093	72.281601
629.801706	73.024893	72.286606
628.922536	65.776891	72.291610
628.408273	62.725397	72.296615
627.874027	70.764630	72.301620
627.555466	62.735075	72.306625
626.601454	68.015255	72.311630
625.544372	74.732685	72.316634
625.139571	63.682808	72.321639
624.585778	67.934162	72.326644
624.398985	59.571390	72.331649
623.541627	75.034324	72.336654
622.530695	73.757145	72.341658
622.470097	67.924204	72.346663
621.228182	61.360023	72.351668
620.447088	60.949837	72.356673
620.160778	72.784733	72.361678
619.572418	66.308863	72.366682
618.809152	67.371865	72.371687
617.822781	69.164255	72.376692
617.269350	71.674600	72.381697
616.778749	66.878385	72.386702
616.382302	72.300015	72.391706
615.681567	72.102538	72.396711
614.439255	74.897628	72.401716
614.063859	62.669820	72.406721
613.439433	69.412968	72.411726
612.083962	69.781805	72.416730
611.629991	65.214725	72.421735
611.555237	70.317043	72.426740
611.076715	68.910928	72.431745
610.597092	72.890278	72.436750
609.137898	72.640122	72.441754
608.870958	60.112772	72.446759
608.401411	73.591646	72.451764
607.474125	61.476961	72.456769
606.828912	68.198189	72.461774
606.107754	64.362788	72.466778
605.489452	60.025307	72.471783
604.792904	70.895784	72.476788
603.549350	64.584184	72.481793
603.163454	68.310488	72.486798
602.881312	71.406836	72.491802
602.491620	66.654479	72.496807
601.720766	68.836753	72.501812
601.070352	66.772042	72.506817
600.414008	67.505785	72.511822
599.510478	78.272036	72.516826
599.172753	71.532328	72.521831
597.980598	67.868131	72.526836
597.403534	64.845568	72.531841
597.255022	56.708518	72.536846
596.206067	78.063496	72.541850
595.546444	61.523841	72.546855
594.560911	75.294626	72.551860
594.220411	72.160272	72.556865
594.046835	64.257444	72.561870
592.645992	69.924187	72.566874
592.308339	69.290425	72.571879
591.197952	74.250170	72.576884
591.240321	80.127045	72.581889
590.546960	68.951242	72.586894
589.468034	74.530450	72.591898
589.006393	70.560682	72.596903
588.551901	74.324722	72.601908
587.558906	67.919610	72.606913
586.969173	68.070316	72.611918
586.115024	69.120993	72.616922
586.375012	64.561640	72.621927
584.827233	73.311072	72.626932
583.968505	68.325912	72.631937
583.623106	67.084682	72.636942
582.989833	71.971599	72.641946
582.621333	71.085708	72.646951
581.573810	74.349685	72.651956
580.884517	57.704380	72.656961
580.397740	67.112733	72.661966
579.896029	69.450845	72.666970
578.798416	56.447097	72.671975
578.069601	63.817154	72.676980
577.557668	68.044503	72.681985
577.347390	65.665274	72.686990
576.602250	71.795298	72.691994
575.651749	64.866185	72.696999
574.936414	69.162200	72.702004
574.665053	59.723232	72.707009
574.270792	67.585634	72.712014
573.074544	77.876540	72.717018
572.236743	65.425920	72.722023
571.635129	71.304429	72.727028
571.461562	69.619519	72.732033
570.106403	68.908117	72.737038
569.093245	67.888358	72.742042
568.922848	68.830143	72.747047
568.366577	82.128874	72.752052
567.921119	66.740984	72.757057
567.890026	71.306492	72.762062
566.744733	74.390505	72.767066
566.270573	67.852307	72.772071
565.251123	73.934560	72.777076
563.952869	74.948745	72.782081
563.588774	69.940006	72.787086
562.858459	79.705701	72.792090
563.124833	62.928691	72.797095
562.245987	75.640128	72.802100
561.557542	72.089688	72.807105
561.081220	69.472135	72.812110
559.904384	78.365930	72.817114
559.015697	72.611267	72.822119
558.550818	76.178270	72.827124
558.159317	70.647195	72.832129
557.275387	65.125166	72.837134
556.264806	72.100140	72.842138
555.821501	63.409226	72.847143
554.944413	72.909713	72.852148
554.704457	74.100698	72.857153
554.170686	68.242201	72.862158
553.114364	70.320146	72.867162
552.482253	63.144792	72.872167
552.140311	71.632799	72.877172
551.578891	76.751129	72.882177
550.529912	71.446200	72.887182
549.450961	74.447113	72.892186
549.295456	66.472027	72.897191
548.828121	73.191745	72.902196
548.323404	71.599005	72.907201
548.121669	64.386643	72.912206
546.809720	82.066654	72.917210
545.869798	73.033790	72.922215
545.096748	78.408179	72.927220
544.334398	76.238309	72.932225
543.911049	65.823765	72.937230
543.516878	68.732957	72.942234
543.207659	62.316730	72.947239
542.141206	65.027072	72.952244
541.475907	64.912281	72.957249
540.918181	67.592058	72.962254
539.657866	69.000757	72.967258
538.866216	61.784587	72.972263
538.404663	73.404545	72.977268
538.337222	68.104134	72.982273
538.209434	68.256967	72.987278
537.088232	74.185126	72.992282
536.123913	64.487531	72.997287
535.730459	70.053770	73.002292
534.664265	63.800692	73.007297
534.114713	62.796991	73.012302
533.329322	64.084315	73.017306
533.187006	62.134236	73.022311
532.028823	59.828725	73.027316
531.317544	63.890714	73.032321
530.773800	65.858638	73.037326
530.123544	72.725765	73.042330
529.783052	62.400532	73.047335
529.244582	61.336720	73.052340
527.902464	71.188826	73.057345
527.370158	67.599336	73.062350
526.923324	68.728657	73.067354
526.474036	66.775433	73.072359
525.163647	68.177923	73.077364
524.493239	67.270745	73.082369
524.341099	67.848503	73.087374
523.740742	73.994902	73.092378
523.064596	68.184324	73.097383
522.166674	71.839232	73.102388
521.653083	71.471624	73.107393
521.445328	63.545867	73.112398
520.270560	66.729210	73.117402
519.498148	61.459093	73.122407
518.922019	67.418706	73.127412
518.473604	72.840738	73.132417
517.417544	72.464921	73.137422
516.503913	78.949807	73.142426
516.324775	67.878205	73.147431
515.631133	71.934237	73.152436
515.170196	70.987387	73.157441
514.388253	65.360822	73.162446
513.276652	74.972792	73.167450
513.082502	68.098270	73.172455
512.663126	70.368086	73.177460
511.550381	65.037065	73.182465
511.006252	70.181030	73.187470
510.111774	73.067419	73.192474
510.170161	69.473728	73.197479
509.083451	78.529804	73.202484
508.079799	75.543676	73.207489
507.596696	71.735040	73.212494
506.993624	75.301986	73.217498
506.612580	68.996552	73.222503
505.594695	69.669640	73.227508
504.513907	81.556978	73.232513
504.535504	68.769219	73.237518
503.968706	77.382934	73.242522
503.297150	70.333725	73.247527
502.514948	70.767421	73.252532
501.341350	75.516498	73.257537
501.221468	71.782470	73.262542
500.456962	70.776747	73.267546
499.850160	71.385930	73.272551
499.059946	68.529811	73.277556
498.266121	73.007082	73.282561
498.114524	66.622523	73.287566
496.979606	66.620399	73.292570
496.249077	65.495725	73.297575
495.871102	65.716799	73.302580
495.255404	66.849371	73.307585
495.236875	63.532861	73.312590
493.784597	75.695416	73.317594
493.376660	63.196860	73.322599
492.671223	67.368315	73.327604
491.483796	70.318722	73.332609
490.844710	69.198406	73.337614
490.053831	67.428914	73.342618
489.982593	69.155998	73.347623
489.776671	67.184514	73.352628
488.980294	73.754805	73.357633
488.062916	69.509154	73.362638
487.397814	75.678489	73.367642
486.602463	65.256990	73.372647
485.548479	67.675210	73.377652
484.817528	60.480933	73.382657
484.699801	63.398133	73.387662
483.978273	65.429080	73.392666
483.738717	70.532417	73.397671
482.448690	72.002647	73.402676
481.798885	69.258207	73.407681
481.550770	76.822950	73.412686
480.678562	66.043113	73.417690
479.514590	71.948145	73.422695
479.238044	71.897598	73.427700
478.362050	73.677188	73.432705
478.466633	73.029763	73.437710
477.006635	74.281069	73.442714
476.756900	68.856740	73.447719
476.105549	69.113481	73.452724
475.370177	69.314222	73.457729
475.153011	65.245612	73.462734
473.824071	84.992584	73.467738
473.341622	66.775263	73.472743
472.812746	56.457982	73.477748
472.169465	78.521062	73.482753
471.514834	65.233912	73.487758
470.763791	73.140545	73.492762
470.399807	68.961283	73.497767
469.280307	71.915072	73.502772
468.501188	75.393377	73.507777
468.203328	73.665198	73.512782
467.470677	74.135166	73.517786
466.782766	67.410274	73.522791
465.965718	74.590990	73.527796
465.058308	72.169866	73.532801
464.901300	66.621957	73.537806
464.202006	79.019386	73.542810
463.577429	72.185055	73.547815
462.443969	75.973700	73.552820
461.974816	72.911904	73.557825
461.934216	62.859033	73.562830
460.984894	72.669093	73.567834
460.182450	72.612443	73.572839
459.117035	79.060024	73.577844
458.661412	83.951784	73.582849
458.480732	63.590632	73.587854
457.497129	70.976077	73.592858
456.538310	71.731237	73.597863
456.381561	71.988036	73.602868
455.727928	67.195757	73.607873
455.093106	76.561482	73.612878
454.100047	76.057384	73.617882
453.833173	68.229365	73.622887
453.132498	69.821761	73.627892
451.997583	66.673645	73.632897
451.604310	76.040311	73.637902
451.042010	73.841755	73.642906
450.583651	67.466650	73.647911
449.346811	75.988424	73.652916
448.655728	74.209353	73.657921
448.396255	78.055885	73.662926
448.077614	71.409362	73.667930
447.116979	75.017516	73.672935
446.227628	72.003743	73.677940
445.267835	71.264116	73.682945
445.103973	77.374106	73.687950
444.075231	79.739437	73.692954
443.311093	73.099235	73.697959
442.777312	77.811059	73.702964
441.974139	74.693672	73.707969
442.178441	61.993514	73.712974
441.209410	80.240242	73.717978
440.407722	74.268341	73.722983
439.742111	74.142589	73.727988
439.313610	79.452651	73.732993
438.534339	79.710859	73.737998
437.460518	77.516530	73.743002
437.150514	71.422143	73.748007
436.610866	76.406137	73.753012
435.362433	81.668636	73.758017
434.855881	71.749922	73.763022
434.030196	71.290130	73.768026
433.852700	80.770655	73.773031
433.309391	72.778521	73.778036
432.107189	69.847715	73.783041
431.677872	71.486770	73.788046
431.280554	74.090551	73.793050
430.823186	75.585842	73.798055
430.072725	72.441139	73.803060
428.683729	73.826240	73.808065
428.831171	61.955155	73.813070
428.050026	68.234450	73.818074
427.534262	72.933943	73.823079
426.899222	66.139141	73.828084
425.755596	72.813658	73.833089
424.594055	68.327814	73.838094
423.714173	81.476265	73.843098
423.400320	71.373889	73.848103
422.985488	77.063395	73.853108
422.737750	74.947193	73.858113
422.689401	69.240051	73.863118
421.648626	74.024769	73.868122
420.544634	68.302892	73.873127
420.085606	70.514384	73.878132
418.825428	72.788865	73.883137
418.475363	68.128004	73.888142
417.536828	77.501123	73.893146
417.569123	71.358510	73.898151
416.510914	70.481610	73.903156
415.237276	78.367443	73.908161
414.960548	71.373629	73.913166
414.628231	75.681198	73.918170
414.391961	66.716061	73.923175
413.719021	68.617861	73.928180
412.766033	63.477479	73.933185
412.345706	65.801077	73.938190
411.390740	66.144057	73.943194
410.100015	61.059065	73.948199
409.408674	64.299472	73.953204
408.772047	65.600978	73.958209
408.964367	62.331301	73.963214
408.287063	71.503526	73.968218
407.489198	63.744351	73.973223
406.881231	64.274895	73.978228
405.883060	71.430866	73.983233
405.990877	63.327117	73.988238
404.436460	62.358974	73.993242
404.053800	60.794127	73.998247
403.510525	61.585599	74.003252
402.683290	62.526394	74.008257
401.855398	59.528081	74.013262
401.037458	66.175942	74.018266
400.772299	63.944249	74.023271
400.515678	59.899284	74.028276
399.093975	64.334696	74.033281
398.529014	60.318359	74.038286
397.710305	63.217942	74.043290
397.641112	56.974812	74.048295
397.416100	63.132386	74.053300
396.461439	63.170972	74.058305
395.627349	70.239302	74.063310
394.659859	68.108476	74.068314
393.329276	61.247895	74.073319
393.150414	64.841886	74.078324
392.380485	74.210222	74.083329
392.083482	62.168683	74.088334
391.605457	66.739164	74.093338
391.127570	68.631968	74.098343
390.537768	73.264416	74.103348
389.515698	77.267155	74.108353
389.208258	61.895189	74.113358
388.176272	64.254749	74.118362
387.335742	65.708598	74.123367
386.693991	64.426310	74.128372
386.154918	72.549921	74.133377
385.977603	66.399710	74.138382
384.687517	65.037802	74.143386
384.016475	67.376121	74.148391
383.779323	62.303040	74.153396
382.937793	74.582793	74.158401
382.192774	68.537232	74.163406
381.572342	68.971998	74.168410
381.150453	65.158371	74.173415
380.413313	65.107110	74.178420
379.113244	65.360013	74.183425
378.717807	61.020203	74.188430
378.384888	68.844460	74.193434
377.864561	65.295677	74.198439
376.969777	63.170621	74.203444
375.788869	67.039400	74.208449
375.544310	57.146776	74.213454
375.436102	66.788137	74.218458
374.491363	67.473276	74.223463
373.643779	53.797455	74.228468
372.889220	62.901566	74.233473
372.733501	63.598173	74.238478
371.306878	62.953463	74.243482
370.698786	70.097750	74.248487
370.292801	67.568380	74.253492
369.842777	60.100724	74.258497
369.613401	60.581988	74.263502
368.092863	60.190363	74.268506
367.732747	57.366682	74.273511
367.486565	64.784457	74.278516
366.109445	59.647026	74.283521
365.726844	60.009205	74.288526
364.839379	59.273854	74.293530
364.534517	56.763066	74.298535
363.826144	58.978028	74.303540
362.298511	68.199025	74.308545
362.115711	62.377698	74.313550
361.740382	57.917995	74.318554
361.355127	64.791807	74.323559
360.934437	57.404636	74.328564
359.910639	59.420704	74.333569
359.386238	64.623050	74.338574
358.528819	66.609454	74.343578
357.340348	61.175463	74.348583
357.210343	63.091684	74.353588
356.634464	56.117172	74.358593
355.895961	68.216505	74.363598
355.134548	75.500346	74.368602
354.368545	69.978532	74.373607
354.023848	67.321128	74.378612
353.436906	59.832717	74.383617
352.435013	64.573415	74.388622
351.288289	65.151978	74.393626
350.836244	64.550672	74.398631
350.798022	62.073089	74.403636
349.925599	65.872220	74.408641
349.251654	69.161909	74.413646
348.495913	72.849409	74.418650
347.865146	66.322033	74.423655
347.512678	71.758758	74.428660
346.209547	74.658283	74.433665
345.877620	68.744026	74.438670
344.710946	72.457588	74.443674
344.496880	64.630637	74.448679
344.222488	64.201295	74.453684
343.251060	69.829695	74.458689
342.614739	74.225138	74.463694
341.958941	69.840092	74.468698
341.745313	62.591813	74.473703
340.773153	68.120982	74.478708
339.685437	70.858449	74.483713
339.175665	62.659156	74.488718
338.736205	62.815935	74.493722
338.348951	70.346080	74.498727
337.250921	62.798771	74.503732
336.762790	66.296970	74.508737
336.037854	67.885379	74.513742
335.118871	68.257347	74.518746
334.287295	65.907769	74.523751
334.085916	61.119153	74.528756
333.464712	68.615617	74.533761
333.031182	62.285473	74.538766
331.758537	72.320558	74.543770
331.318677	65.707572	74.548775
330.917942	62.814676	74.553780
329.776721	63.978996	74.558785
329.045774	53.733390	74.563790
328.896001	64.642926	74.568794
327.970502	60.138442	74.573799
327.832563	59.294697	74.578804
326.740337	71.492985	74.583809
326.182040	57.838891	74.588814
325.335857	72.763932	74.593818
324.869106	66.166271	74.598823
323.934585	69.196296	74.603828
322.655001	62.699789	74.608833
322.488341	55.975463	74.613838
322.005178	64.377171	74.618842
322.003916	65.200553	74.623847
321.365173	53.653469	74.628852
320.174068	62.589042	74.633857
319.473323	59.772345	74.638862
319.129079	61.505091	74.643866
318.147019	66.223718	74.648871
317.407440	61.741648	74.653876
316.527551	63.592874	74.658881
316.375780	55.317616	74.663886
315.481247	50.958015	74.668890
314.601275	52.954333	74.673895
314.045066	52.270288	74.678900
313.350398	64.996571	74.683905
313.196492	52.552211	74.688910
312.080030	64.596666	74.693914
311.369064	61.273824	74.698919
311.170611	54.575066	74.703924
310.518259	58.786988	74.708929
309.767162	55.763855	74.713934
308.845242	65.796665	74.718938
308.383237	55.799940	74.723943
307.841079	51.155527	74.728948
306.586344	64.051493	74.733953
306.033691	55.559428	74.738958
305.412915	58.895845	74.743962
305.126403	64.601178	74.748967
304.574404	57.597645	74.753972
303.394456	68.374899	74.758977
302.679408	68.837379	74.763982
302.459500	65.026271	74.768986
301.528258	64.558117	74.773991
300.842329	55.494363	74.778996
300.076792	62.083435	74.784001
299.902069	62.678997	74.789006
299.508718	67.264382	74.794010
297.934052	64.866091	74.799015
297.196305	68.891356	74.804020
296.612026	62.683017	74.809025
296.236317	68.956076	74.814030
296.162599	70.886984	74.819034
295.620042	61.981727	74.824039
294.866460	60.381399	74.829044
293.917722	67.977378	74.834049
292.915511	67.690848	74.839054
292.269046	64.349846	74.844058
291.827224	70.786407	74.849063
291.423854	62.183819	74.854068
290.335534	66.436846	74.859073
289.498682	58.915747	74.864078
289.001714	61.243691	74.869082
288.370275	63.566260	74.874087
288.064842	58.478846	74.879092
286.752876	64.516349	74.884097
286.245604	56.540604	74.889102
285.762290	56.721728	74.894106
285.451676	66.901542	74.899111
284.759587	59.887226	74.904116
283.805581	70.634785	74.909121
283.506313	62.395651	74.914126
282.494404	59.631713	74.919130
281.454114	62.837881	74.924135
281.280769	57.677377	74.929140
280.500452	70.775287	74.934145
279.967654	60.763041	74.939150
278.846945	62.368813	74.944154
278.104752	59.705392	74.949159
278.031838	65.371952	74.954164
277.516582	64.604117	74.959169
276.900957	61.568864	74.964174
275.662805	69.526367	74.969178
274.867653	64.403467	74.974183
274.483049	55.845204	74.979188
273.981070	62.144695	74.984193
273.483856	55.055171	74.989198
272.478171	56.557457	74.994202
271.705539	59.322000	74.999207
271.889820	56.827880	75.004212
270.717429	65.229061	75.009217
270.281504	56.661633	75.014222
269.462245	64.653294	75.019226
268.360382	63.764495	75.024231
267.614667	56.646770	75.029236
266.815702	58.608117	75.034241
266.361093	53.676949	75.039246
266.028615	61.245672	75.044250
265.667356	60.566834	75.049255
264.746925	52.745259	75.054260
263.864863	59.641492	75.059265
263.518408	60.001079	75.064270
262.949091	54.802767	75.069274
261.841387	60.375641	75.074279
261.135510	53.448689	75.079284
260.548489	60.275819	75.084289
260.255108	65.419281	75.089294
259.454556	67.382461	75.094298
258.523426	65.958676	75.099303
258.051910	63.230039	75.104308
257.692717	66.860663	75.109313
256.927782	59.324961	75.114318
255.799003	59.867592	75.119322
255.487309	65.613212	75.124327
255.280899	53.812740	75.129332
253.873148	57.315606	75.134337
253.159382	61.169901	75.139342
252.466908	59.930429	75.144346
251.840615	68.295037	75.149351
252.095591	52.470778	75.154356
250.767564	66.088072	75.159361
250.028307	60.445344	75.164366
249.766160	55.335269	75.169370
248.843269	56.343400	75.174375
248.311523	54.805498	75.179380
247.639951	58.968458	75.184385
247.266092	57.703432	75.189390
245.915419	58.793943	75.194394
245.166761	60.029768	75.199399
244.885926	54.854864	75.204404
244.198123	61.415789	75.209409
243.818034	64.668125	75.214414
242.949557	56.125497	75.219418
241.827992	57.023373	75.224423
241.534283	55.319798	75.229428
241.050018	58.418428	75.234433
240.103776	51.692224	75.239438
239.473097	59.382596	75.244442
238.786944	61.015311	75.249447
238.375997	61.669031	75.254452
237.708404	56.174157	75.259457
236.753941	55.769653	75.264462
236.005105	58.585606	75.269466
235.538486	67.071419	75.274471
235.210170	52.399846	75.279476
233.832039	59.480816	75.284481
233.255296	59.553842	75.289486
232.797554	59.541667	75.294490
232.274475	63.482266	75.299495
232.131029	51.383184	75.304500
230.982737	58.351825	75.309505
230.394403	51.319417	75.314510
229.812140	56.076844	75.319514
228.950148	57.594088	75.324519
227.992218	57.598568	75.329524
227.497380	65.682029	75.334529
226.883307	60.642247	75.339534
226.767270	65.035201	75.344538
225.526415	61.736929	75.349543
224.946971	61.020339	75.354548
224.440860	70.154266	75.359553
224.121090	57.387855	75.364558
222.911795	66.788413	75.369562
222.068502	65.960918	75.374567
221.915727	63.075825	75.379572
221.110382	66.473222	75.384577
220.451403	65.337228	75.389582
219.567663	65.337769	75.394586
218.645305	64.619073	75.399591
218.667384	57.230742	75.404596
218.612656	61.307996	75.409601
217.318659	55.949251	75.414606
216.370652	57.089130	75.419610
215.910566	58.247423	75.424615
215.037437	57.027298	75.429620
214.182701	63.739420	75.434625
213.463158	64.322489	75.439630
212.939283	59.709877	75.444634
212.539415	63.441606	75.449639
211.957528	64.042156	75.454644
210.987586	67.620335	75.459649
210.225684	62.064808	75.464654
210.160692	53.312112	75.469658
209.400887	64.333079	75.474663
208.777792	57.044443	75.479668
208.027873	66.672973	75.484673
207.410935	63.641102	75.489678
206.593916	56.471690	75.494682
205.647738	67.295290	75.499687
205.443875	56.692898	75.504692
204.952938	65.160513	75.509697
203.643005	65.635853	75.514702
203.455780	60.680996	75.519706
202.690023	70.903408	75.524711
202.077082	63.086453	75.529716
200.882074	69.647823	75.534721
200.353246	66.444213	75.539726
200.106076	64.703262	75.544730
199.483647	68.812669	75.549735
198.583607	59.166500	75.554740
197.478972	73.227600	75.559745
197.280873	63.783340	75.564750
196.950382	63.659423	75.569754
195.987301	58.238476	75.574759
195.220319	62.976473	75.579764
194.422088	60.773018	75.584769
194.036257	59.361677	75.589774
193.592334	62.059648	75.594778
192.572414	71.225028	75.599783
192.077749	57.029411	75.604788
191.212558	66.228468	75.609793
190.782525	56.532608	75.614798
190.100081	64.026241	75.619802
188.993280	67.900634	75.624807
188.845002	59.493949	75.629812
188.257193	55.648470	75.634817
187.612452	55.394881	75.639822
186.534048	56.993948	75.644826
185.750751	61.854396	75.649831
185.532057	57.729301	75.654836
184.707575	67.005448	75.659841
183.774575	63.030497	75.664846
183.168550	59.673621	75.669850
182.920161	65.997353	75.674855
182.391212	55.680180	75.679860
181.381460	70.543012	75.684865
180.574275	68.457682	75.689870
180.289093	63.906372	75.694874
179.702681	66.639678	75.699879
178.992840	62.673306	75.704884
177.983470	68.358271	75.709889
177.326149	67.497990	75.714894
177.087665	50.192812	75.719898
176.209576	61.806647	75.724903
175.430696	62.533227	75.729908
174.595642	60.777194	75.734913
174.288213	57.874185	75.739918
173.797066	52.024777	75.744922
172.518528	59.678098	75.749927
172.160574	59.307829	75.754932
171.379294	62.472747	75.759937
170.797523	56.998905	75.764942
170.169854	55.679740	75.769946
169.300200	54.578925	75.774951
168.778173	57.298813	75.779956
168.327241	64.572616	75.784961
168.064117	56.252055	75.789966
167.043261	52.321082	75.794970
166.095463	64.783391	75.799975
166.030635	54.584617	75.804980
164.617331	64.210108	75.809985
163.590313	62.254449	75.814990
163.308968	61.815198	75.819994
162.615150	68.246215	75.824999
162.447768	54.287014	75.830004
161.988066	57.610397	75.835009
161.270353	59.544629	75.840014
160.762261	58.468174	75.845018
160.012615	59.450293	75.850023
159.019798	51.372228	75.855028
158.162770	65.794399	75.860033
157.539891	59.775184	75.865038
157.335986	59.219509	75.870042
155.974417	62.147367	75.875047
155.394358	57.881194	75.880052
154.799400	63.858060	75.885057
154.446295	61.146838	75.890062
153.937763	63.243263	75.895066
152.921013	69.292111	75.900071
151.942765	61.426184	75.905076
151.738757	63.505597	75.910081
151.126575	63.529099	75.915086
150.643340	56.923078	75.920090
149.671468	65.327029	75.925095
149.018859	50.134757	75.930100
148.635462	58.804423	75.935105
147.930650	52.402465	75.940110
146.967278	51.657220	75.945114
146.087658	60.950048	75.950119
145.726009	52.716165	75.955124
145.048983	69.615403	75.960129
144.198307	63.444854	75.965134
143.712716	60.447254	75.970138
142.922564	67.436103	75.975143
142.556259	53.934396	75.980148
142.309157	68.287712	75.985153
140.987794	62.335713	75.990158
140.192221	62.760615	75.995162
139.677678	64.178339	76.000167
139.769633	49.583291	76.005172
138.394263	61.356845	76.010177
137.821149	65.185591	76.015182
137.459187	64.860120	76.020186
136.813429	62.815300	76.025191
135.601952	56.968787	76.030196
134.888489	63.779830	76.035201
134.446026	64.560017	76.040206
134.156985	56.137939	76.045210
133.062924	58.674652	76.050215
132.587405	61.443902	76.055220
132.008087	59.910458	76.060225
131.401753	62.309484	76.065230
130.613718	56.332382	76.070234
129.359753	55.743863	76.075239
129.286461	54.699013	76.080244
128.931360	60.047863	76.085249
128.016773	68.229801	76.090254
127.069533	60.526099	76.095258
126.147258	66.809048	76.100263
126.345306	67.826153	76.105268
125.656310	66.005847	76.110273
124.488430	64.556786	76.115278
124.272168	66.767464	76.120282
123.362768	67.137982	76.125287
122.548694	51.351728	76.130292
121.501018	58.984030	76.135297
120.595123	60.240232	76.140302
120.488990	58.394802	76.145306
119.934192	66.653414	76.150311
119.724782	64.658872	76.155316
119.009820	71.400775	76.160321
118.157285	70.764023	76.165326
117.845960	57.928486	76.170330
117.169908	57.528521	76.175335
116.161099	61.832015	76.180340
115.276803	56.314965	76.185345
114.754198	58.993955	76.190350
113.908949	65.857555	76.195354
113.267749	68.178568	76.200359
112.654844	59.697747	76.205364
112.160921	59.631440	76.210369
111.948198	62.674179	76.215374
110.949957	59.657404	76.220378
110.009143	69.532435	76.225383
109.656890	57.077161	76.230388
108.508950	65.091309	76.235393
107.703346	61.274272	76.240398
107.169605	59.905454	76.245402
106.301869	60.217295	76.250407
106.639073	63.689584	76.255412
106.012960	64.167901	76.260417
104.853826	62.059871	76.265422
104.553634	54.601513	76.270426
103.070948	65.507533	76.275431
102.632841	56.147298	76.280436
101.917272	61.479512	76.285441
100.943509	60.948829	76.290446
101.204692	61.202086	76.295450
100.446948	70.022915	76.300455
99.910757	60.079080	76.305460
99.053074	53.862363	76.310465
98.310987	63.642626	76.315470
97.691410	61.674067	76.320474
96.451947	59.309193	76.325479
96.079794	56.097976	76.330484
95.944232	58.180669	76.335489
94.770440	63.615915	76.340494
94.383088	53.847046	76.345498
93.107411	63.239313	76.350503
92.908662	58.719969	76.355508
92.521888	65.346465	76.360513
91.698473	65.233355	76.365518
91.004777	53.542160	76.370522
90.010806	59.089080	76.375527
90.075976	55.437547	76.380532
89.115702	54.327558	76.385537
87.866147	63.673085	76.390542
87.662261	58.317205	76.395546
86.825872	61.878861	76.400551
86.393488	61.190893	76.405556
85.345445	56.242435	76.410561
84.597624	58.794918	76.415566
84.605826	58.842511	76.420570
83.997513	68.263983	76.425575
83.406786	58.442390	76.430580
82.339254	62.096099	76.435585
81.677090	60.653149	76.440590
81.414057	57.388264	76.445594
80.170694	69.790498	76.450599
79.305168	60.853236	76.455604
78.932455	61.029379	76.460609
78.481450	62.703486	76.465614
78.273021	65.485347	76.470618
76.944595	67.494913	76.475623
76.367014	63.693564	76.480628
75.903062	67.735148	76.485633
74.781683	71.695491	76.490638
73.997199	57.145590	76.495642
73.567268	63.900394	76.500647
73.214138	70.182486	76.505652
72.705986	63.539456	76.510657
71.820274	60.604102	76.515662
70.988341	47.700219	76.520666
70.693455	63.141350	76.525671
70.325947	65.330418	76.530676
69.239089	57.738896	76.535681
68.499718	64.885243	76.540686
68.001824	61.219422	76.545690
67.351063	56.166617	76.550695
66.134279	58.082691	76.555700
65.666864	56.329571	76.560705
65.126873	57.287747	76.565710
65.040078	48.401355	76.570714
63.702145	57.617480	76.575719
62.964247	61.343208	76.580724
62.467006	61.651175	76.585729
62.088554	60.730686	76.590734
61.431787	57.426091	76.595738
60.206010	66.884533	76.600743
59.885717	64.149171	76.605748
59.375730	62.828615	76.610753
58.528306	63.652894	76.615758
57.847379	62.463676	76.620762
57.030826	65.837677	76.625767
56.742939	67.020577	76.630772
56.401537	64.228658	76.635777
54.878791	66.371726	76.640782
54.714873	69.567534	76.645786
54.021013	67.047864	76.650791
53.536675	62.646606	76.655796
52.321853	70.408095	76.660801
51.519722	65.541858	76.665806
51.088140	57.648727	76.670810
50.504572	72.949826	76.675815
50.471326	64.299312	76.680820
49.263265	66.789587	76.685825
48.650969	67.694643	76.690830
48.399875	58.766641	76.695834
47.597046	66.087115	76.700839
46.659727	60.241082	76.705844
45.816815	62.979052	76.710849
45.240819	63.143465	76.715854
45.362645	69.762973	76.720858
43.863513	68.365203	76.725863
43.090430	61.471122	76.730868
42.792577	61.775680	76.735873
42.448798	61.407901	76.740878
41.695547	63.921839	76.745882
40.511686	70.539845	76.750887
40.017637	55.044787	76.755892
39.693718	56.643439	76.760897
38.478277	60.601449	76.765902
38.117691	61.064244	76.770906
37.343310	61.118373	76.775911
36.920805	61.728238	76.780916
36.118086	61.589769	76.785921
35.031060	62.072226	76.790926
34.738267	64.597887	76.795930
33.978068	65.379878	76.800935
34.059762	55.138832	76.805940
32.798128	55.213901	76.810945
31.745916	67.079468	76.815950
31.426641	62.904202	76.820954
30.684344	64.937007	76.825959
30.545383	56.246591	76.830964
29.525494	64.767045	76.835969
28.529448	67.983602	76.840974
28.474819	58.466033	76.845978
27.742298	61.733601	76.850983
26.370374	63.855785	76.855988
26.211689	55.477595	76.860993
25.442168	54.434980	76.865998
25.329529	52.704134	76.871002
24.642263	57.678617	76.876007
23.819414	69.666880	76.881012
23.137848	58.621897	76.886017
22.192467	56.626474	76.891022
21.623658	59.612468	76.896026
20.774956	63.967732	76.901031
20.721210	54.349102	76.906036
19.431419	55.374833	76.911041
18.303266	64.152251	76.916046
17.912739	57.071014	76.921050
17.437562	52.545306	76.926055
17.451288	56.542250	76.931060
17.027141	59.735407	76.936065
15.355975	59.450027	76.941070
14.934778	55.718372	76.946074
14.497951	60.883149	76.951079
13.858880	58.233330	76.956084
13.105477	55.059280	76.961089
12.530207	62.963205	76.966094
11.857534	59.482968	76.971098
10.504191	59.577406	76.976103
10.085025	71.275786	76.981108
9.678779	67.098624	76.986113
9.076081	72.220475	76.991118
8.940688	68.017461	76.996122
7.618348	68.009185	77.001127
7.093297	59.008191	77.006132
6.779926	63.230770	77.011137
5.402168	68.356390	77.016142
4.528990	59.429845	77.021147
4.081696	58.323227	77.026151
3.421556	61.795298	77.031156
3.431783	58.767535	77.036161