Fri Mar 05 20:29:44 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.700295	93.797254	0.000000
-1.601433	97.071025	0.005005
-2.710633	72.674430	0.010010
-4.291825	22.926579	0.015014
-7.839599	-2.922799	0.020019
-12.827316	-2.978769	0.025024
-18.116404	-6.894305	0.030029
-23.103881	-1.803176	0.035034
-26.809291	-8.559049	0.040038
-30.959156	0.437021	0.045043
-34.586760	-8.083226	0.050048
-38.199776	-10.223937	0.055053
-41.637998	-1.137941	0.060058
-45.117713	-0.491385	0.065062
-49.074045	-11.657306	0.070067
-52.956264	-9.308098	0.075072
-56.551399	-11.921559	0.080077
-60.637764	-1.670871	0.085082
-64.288259	-6.300275	0.090086
-68.152540	-8.290473	0.095091
-72.070753	6.336215	0.100096
-75.468007	-5.921783	0.105101
-79.537552	-1.806444	0.110106
-82.972579	-0.872076	0.115110
-86.599159	-3.866826	0.120115
-90.564877	-10.022834	0.125120
-94.129940	-9.870365	0.130125
-98.399530	0.245614	0.135130
-102.234752	-6.101504	0.140134
-106.092962	-4.538201	0.145139
-109.673697	-14.481888	0.150144
-112.937126	-17.523494	0.155149
-116.872316	-5.956447	0.160154
-120.612638	-7.557911	0.165158
-124.314270	-7.301608	0.170163
-128.250273	-2.609838	0.175168
-132.117845	-7.873121	0.180173
-135.970718	-3.232449	0.185178
-139.211278	-10.404504	0.190182
-143.077008	-4.433992	0.195187
-146.952349	-9.577741	0.200192
-150.764966	-16.049804	0.205197
-154.855150	-17.783045	0.210202
-158.614573	-20.819562	0.215206
-162.539230	-12.086299	0.220211
-166.468213	-11.389960	0.225216
-169.856223	-4.451706	0.230221
-173.798753	1.102184	0.235226
-177.143992	-4.799455	0.240230
-181.090173	4.153320	0.245235
-184.809730	-1.557693	0.250240
-188.508743	-9.936990	0.255245
-192.242705	-9.498807	0.260250
-195.826474	-13.775957	0.265254
-199.845232	-12.125387	0.270259
-203.699324	-7.577456	0.275264
-207.368836	-5.723989	0.280269
-211.497467	-0.684384	0.285274
-214.919538	-11.744463	0.290278
-218.240371	-5.072328	0.295283
-222.137485	-5.874339	0.300288
-225.960427	-2.028347	0.305293
-229.927275	3.538974	0.310298
-233.620764	-5.145482	0.315302
-237.265945	5.380427	0.320307
-241.118012	2.360398	0.325312
-244.599639	-0.931631	0.330317
-248.725063	-5.139602	0.335322
-252.498525	-3.769364	0.340326
-256.182051	-3.225593	0.345331
-259.912633	4.824004	0.350336
-263.763666	-3.679143	0.355341
-267.606395	6.148220	0.360346
-271.213556	-1.394065	0.365350
-275.164762	2.204397	0.370355
-279.013904	-1.110922	0.375360
-282.612650	-4.945587	0.380365
-286.143591	2.975989	0.385370
-290.063675	-4.246662	0.390374
-293.628413	-2.597443	0.395379
-297.673965	-3.790371	0.400384
-301.270312	-6.799078	0.405389
-305.168216	5.915045	0.410394
-309.080273	4.598327	0.415398
-312.702466	-5.489811	0.420403
-316.460729	-1.020077	0.425408
-320.066721	-8.305428	0.430413
-324.088628	-1.071817	0.435418
-327.548482	-2.074341	0.440422
-331.348744	1.531654	0.445427
-335.246399	4.153430	0.450432
-339.230268	-2.529107	0.455437
-342.799972	-4.857617	0.460442
-346.101200	-10.729763	0.465446
-350.128082	-3.354971	0.470451
-354.123647	-2.691851	0.475456
-357.810901	-11.856482	0.480461
-362.038674	-5.529797	0.485466
-365.526934	-7.443927	0.490470
-369.029923	-5.332954	0.495475
-372.819697	0.170054	0.500480
-376.428518	0.744659	0.505485
-380.539801	2.257338	0.510490
-384.063911	-13.395552	0.515494
-387.866689	2.640284	0.520499
-391.960166	-11.228069	0.525504
-395.308374	-11.609663	0.530509
-399.411289	-4.681540	0.535514
-402.777908	-13.733288	0.540518
-406.812608	-10.308941	0.545523
-410.525659	-10.078759	0.550528
-414.137519	-3.328362	0.555533
-418.301803	-0.786883	0.560538
-421.616440	-6.798704	0.565542
-425.444759	-3.233816	0.570547
-429.290866	-2.022011	0.575552
-432.735437	-4.788251	0.580557
-436.824304	-3.862518	0.585562
-440.649656	-4.118975	0.590566
-444.438836	-1.295154	0.595571
-448.168242	0.770087	0.600576
-451.928254	1.480909	0.605581
-455.682137	2.890915	0.610586
-459.183648	-5.869558	0.615590
-462.960145	-5.487241	0.620595
-466.637697	-0.151819	0.625600
-470.595123	-10.154625	0.630605
-474.799818	-0.141423	0.635610
-478.204210	-4.265440	0.640614
-481.538184	-2.003102	0.645619
-485.888762	-4.902118	0.650624
-489.311498	-10.257921	0.655629
-493.460678	-4.883411	0.660634
-496.978194	3.550391	0.665638
-500.893228	-1.775661	0.670643
-504.474384	-0.949820	0.675648
-508.184788	-4.214380	0.680653
-512.291727	4.345117	0.685658
-516.078071	-1.348386	0.690662
-519.506890	1.257152	0.695667
-523.242837	-0.703918	0.700672
-526.857875	-7.747802	0.705677
-530.757481	-0.728933	0.710682
-534.772851	-7.117518	0.715686
-538.295676	-3.681668	0.720691
-542.155372	3.513770	0.725696
-546.100665	-4.220070	0.730701
-549.734587	-5.003659	0.735706
-553.194113	-6.065829	0.740710
-557.127529	-5.521107	0.745715
-560.959626	6.097961	0.750720
-564.409664	-10.115236	0.755725
-568.279563	-3.466901	0.760730
-572.391789	-9.795794	0.765734
-576.007012	-8.357288	0.770739
-580.098894	-3.431748	0.775744
-583.487026	-2.266044	0.780749
-587.296786	1.215712	0.785754
-591.022824	-0.548140	0.790758
-594.908429	-5.703693	0.795763
-598.944740	0.556543	0.800768
-602.053406	-1.490413	0.805773
-605.958031	-1.858519	0.810778
-609.690630	0.997522	0.815782
-613.637981	-2.965443	0.820787
-617.864792	-1.523787	0.825792
-620.957359	0.928831	0.830797
-625.124899	1.222491	0.835802
-628.747489	-6.029756	0.840806
-632.390838	-7.428290	0.845811
-636.081202	0.027240	0.850816
-639.794442	-5.518467	0.855821
-643.650298	-2.038721	0.860826
-647.487504	-8.250571	0.865830
-651.220818	-2.505429	0.870835
-655.238882	-0.401634	0.875840
-658.400423	-4.887454	0.880845
-662.750237	3.687439	0.885850
-666.221030	-0.266423	0.890854
-669.809256	-8.809286	0.895859
-673.782663	-3.620249	0.900864
-677.400725	-2.189021	0.905869
-681.622089	7.628499	0.910874
-685.419015	0.926157	0.915878
-688.469924	-2.143874	0.920883
-692.483499	5.937385	0.925888
-695.974600	-2.808613	0.930893
-700.297789	4.101590	0.935898
-703.668199	0.324130	0.940902
-707.691533	0.620123	0.945907
-711.513370	7.084390	0.950912
-714.965296	2.260278	0.955917
-719.001961	9.807540	0.960922
-722.397081	0.092206	0.965926
-726.647708	0.101282	0.970931
-730.363826	-0.825010	0.975936
-733.690815	-3.038749	0.980941
-738.238468	5.254084	0.985946
-741.661135	1.287914	0.990950
-745.304123	0.479267	0.995955
-749.269165	3.850476	1.000960
-752.626252	-1.026580	1.005965
-756.646564	5.573552	1.010970
-760.534867	-0.219945	1.015974
-764.551440	-2.588358	1.020979
-767.910093	4.084241	1.025984
-771.222993	-3.310310	1.030989
-775.268999	2.674227	1.035994
-778.808184	7.705733	1.040998
-782.802366	-0.779958	1.046003
-786.908377	8.486304	1.051008
-790.409020	-3.977980	1.056013
-794.274364	-6.274319	1.061018
-797.907219	9.206679	1.066022
-801.751343	6.940073	1.071027
-805.665211	10.102928	1.076032
-809.043796	-0.387607	1.081037
-813.258393	5.679132	1.086042
-816.938135	-2.503524	1.091046
-820.636788	-1.466043	1.096051
-824.205503	3.664863	1.101056
-827.330075	-0.369326	1.106061
-831.722896	1.157590	1.111066
-835.737823	0.880034	1.116070
-839.440951	-1.502083	1.121075
-843.365676	1.481222	1.126080
-846.572168	-3.823458	1.131085
-850.310914	11.508964	1.136090
-854.475524	3.865910	1.141094
-858.510371	-1.877184	1.146099
-862.151521	1.978588	1.151104
-865.547136	-3.716870	1.156109
-869.572239	4.456400	1.161114
-873.052207	-0.426065	1.166118
-876.316915	5.266587	1.171123
-880.554612	10.502945	1.176128
-884.193652	-1.355603	1.181133
-887.835327	-0.499011	1.186138
-891.772591	-0.755771	1.191142
-895.696265	-3.064693	1.196147
-899.451767	4.325949	1.201152
-903.204001	3.260629	1.206157
-907.211640	6.336140	1.211162
-910.658115	-0.026043	1.216166
-914.792844	5.085103	1.221171
-918.361269	7.614183	1.226176
-922.135380	-7.184158	1.231181
-925.909317	9.734068	1.236186
-929.822855	0.989747	1.241190
-933.280267	1.110489	1.246195
-937.087199	1.230350	1.251200
-940.802641	3.584277	1.256205
-944.737923	8.903278	1.261210
-948.337477	1.143247	1.266214
-952.097017	-13.595864	1.271219
-956.094186	-3.274431	1.276224
-959.454918	-7.903018	1.281229
-963.647527	9.008090	1.286234
-967.134563	1.581750	1.291238
-970.835542	0.464189	1.296243
-974.414984	-6.080054	1.301248
-978.139182	-10.833416	1.306253
-982.466692	1.056304	1.311258
-986.184369	1.452125	1.316262
-989.514450	-3.173436	1.321267
-993.818155	0.130909	1.326272
-997.147925	-3.441309	1.331277
-1001.212742	-7.100976	1.336282
-1005.214867	4.489175	1.341286
-1008.641880	4.430128	1.346291
-1012.199685	4.609617	1.351296
-1015.871431	-0.923187	1.356301
-1019.663727	-2.139605	1.361306
-1023.633127	3.530323	1.366310
-1027.406084	2.701901	1.371315
-1031.236833	10.145780	1.376320
-1034.811422	2.481242	1.381325
-1038.630411	-1.444751	1.386330
-1042.515746	-2.461752	1.391334
-1046.394996	-2.741723	1.396339
-1050.135760	6.119633	1.401344
-1053.685239	-4.563954	1.406349
-1057.412337	-0.195835	1.411354
-1061.372666	-4.048722	1.416358
-1064.843945	-10.526540	1.421363
-1068.984598	1.327134	1.426368
-1072.499678	-13.018789	1.431373
-1076.308770	0.322512	1.436378
-1080.039510	-10.786187	1.441382
-1083.583757	-2.471870	1.446387
-1087.568738	4.157844	1.451392
-1091.419412	-3.128133	1.456397
-1095.243155	2.720459	1.461402
-1099.096999	3.032587	1.466406
-1102.454318	-10.833909	1.471411
-1106.322210	-10.896404	1.476416
-1109.957459	2.019757	1.481421
-1113.868663	9.287404	1.486426
-1118.038414	4.115118	1.491430
-1121.483507	-4.270142	1.496435
-1124.859776	2.921410	1.501440
-1128.724280	-7.350544	1.506445
-1132.987838	0.870760	1.511450
-1136.254951	10.474898	1.516454
-1139.962485	8.401466	1.521459
-1144.165568	4.953399	1.526464
-1147.538652	-5.204755	1.531469
-1151.616703	-12.075788	1.536474
-1155.471325	-1.888801	1.541478
-1158.955978	3.577646	1.546483
-1163.117184	12.124825	1.551488
-1166.427261	0.075356	1.556493
-1170.271453	-8.523512	1.561498
-1174.130399	0.524088	1.566502
-1177.347606	-6.495664	1.571507
-1181.508820	11.524076	1.576512
-1185.370992	3.998829	1.581517
-1189.223368	7.450510	1.586522
-1192.850498	1.884048	1.591526
-1196.545780	-12.585796	1.596531
-1200.380943	-4.179036	1.601536
-1204.456876	0.524238	1.606541
-1208.111784	8.408601	1.611546
-1211.773755	14.947418	1.616550
-1215.284117	-0.547029	1.621555
-1219.228922	3.949215	1.626560
-1222.739381	-3.759969	1.631565
-1227.072992	-3.014479	1.636570
-1230.788415	12.109756	1.641574
-1234.036711	7.996579	1.646579
-1237.992124	1.380457	1.651584
-1241.705153	-4.946443	1.656589
-1245.501965	-6.202766	1.661594
-1249.487412	-2.160429	1.666598
-1252.994651	-2.491699	1.671603
-1256.972973	-1.564894	1.676608
-1260.540354	-0.755882	1.681613
-1264.198262	0.701543	1.686618
-1267.943892	7.113483	1.691622
-1271.816310	-0.409970	1.696627
-1275.881780	7.786194	1.701632
-1279.461223	-2.822843	1.706637
-1283.098224	1.949091	1.711642
-1286.980679	3.018297	1.716646
-1290.353060	-1.212129	1.721651
-1294.441511	-3.651690	1.726656
-1298.084918	-1.937920	1.731661
-1302.265911	4.472787	1.736666
-1305.695569	1.038430	1.741670
-1308.937998	-4.163643	1.746675
-1313.413104	1.989810	1.751680
-1317.103106	-9.028808	1.756685
-1320.954295	2.357918	1.761690
-1324.517481	-1.670034	1.766694
-1328.241915	-3.931260	1.771699
-1331.895780	-1.968188	1.776704
-1335.671788	1.070971	1.781709
-1339.513563	0.271419	1.786714
-1343.433881	4.025954	1.791718
-1347.093273	1.617156	1.796723
-1350.809310	3.497171	1.801728
-1354.693397	-0.777405	1.806733
-1358.280260	-2.844565	1.811738
-1362.356568	4.043063	1.816742
-1365.973329	-8.477377	1.821747
-1369.677438	2.996265	1.826752
-1373.368808	-4.667948	1.831757
-1377.193373	0.679764	1.836762
-1380.848114	4.902767	1.841766
-1384.660395	-0.704704	1.846771
-1388.798779	6.448367	1.851776
-1392.123332	3.366314	1.856781
-1395.917693	-3.275306	1.861786
-1399.892679	9.178434	1.866790
-1402.843630	-0.056599	1.871795
-1407.066574	-0.386597	1.876800
-1411.015660	1.390477	1.881805
-1414.847081	5.454166	1.886810
-1418.908478	7.148312	1.891814
-1422.399578	0.475532	1.896819
-1426.333778	7.239596	1.901824
-1429.797997	5.238066	1.906829
-1433.393539	-1.145169	1.911834
-1437.274840	7.633621	1.916838
-1440.847713	-8.403922	1.921843
-1444.803086	5.729308	1.926848
-1448.797255	-4.021436	1.931853
-1452.548124	-2.075760	1.936858
-1456.690823	8.910012	1.941862
-1459.739403	3.424813	1.946867
-1463.615373	7.796904	1.951872
-1467.444406	3.363901	1.956877
-1471.057375	7.966699	1.961882
-1475.024183	10.410599	1.966886
-1478.310887	-0.265480	1.971891
-1482.473468	8.025425	1.976896
-1486.143897	0.463699	1.981901
-1489.860494	8.205401	1.986906
-1493.965859	2.247665	1.991910
-1497.260474	6.749065	1.996915
-1501.783233	-0.573279	2.006912
-1502.407715	8.394044	2.016909
-1499.867322	4.902083	2.026906
-1497.024722	4.578013	2.036902
-1494.976731	2.173841	2.046899
-1493.258464	6.697126	2.056896
-1491.051016	0.602730	2.066893
-1489.260702	0.931897	2.076890
-1487.289348	-1.027369	2.086886
-1485.541709	-4.258165	2.096883
-1483.474830	-5.724309	2.106880
-1481.405443	-4.842986	2.116877
-1479.840489	1.735359	2.126874
-1477.803978	-3.584820	2.136870
-1476.015909	0.433095	2.146867
-1474.076732	-0.028920	2.156864
-1472.058318	6.355248	2.166861
-1470.162929	-2.074925	2.176858
-1468.394409	1.232451	2.186854
-1466.307719	-7.866234	2.196851
-1464.632275	-2.513451	2.206848
-1462.726801	-2.876904	2.216845
-1460.877240	4.667981	2.226842
-1459.146582	0.887296	2.236838
-1457.185980	-1.142854	2.246835
-1455.161994	-0.348974	2.256832
-1453.319169	-1.946584	2.266829
-1451.417274	-6.387829	2.276826
-1449.166609	-7.308638	2.286822
-1447.859518	1.401519	2.296819
-1445.766800	4.426484	2.306816
-1443.845849	3.007422	2.316813
-1441.779572	-0.165412	2.326810
-1440.031749	4.607390	2.336806
-1438.182788	6.248773	2.346803
-1436.616141	4.981178	2.356800
-1434.666156	7.369013	2.366797
-1432.458710	1.617297	2.376794
-1430.501527	2.958731	2.386790
-1428.757500	1.519061	2.396787
-1426.953079	3.786524	2.406784
-1425.122256	2.697693	2.416781
-1423.111051	5.337839	2.426778
-1421.303348	3.974821	2.436774
-1419.151327	6.898740	2.446771
-1417.542020	4.809599	2.456768
-1415.535048	4.284675	2.466765
-1414.103655	4.579784	2.476762
-1411.964809	3.245864	2.486758
-1409.999584	7.530734	2.496755
-1408.014427	1.189370	2.506752
-1406.315286	7.212612	2.516749
-1404.579202	0.009555	2.526746
-1402.515616	3.111855	2.536742
-1400.734703	3.734699	2.546739
-1398.412600	7.015091	2.556736
-1396.917036	5.575745	2.566733
-1394.900890	6.296725	2.576730
-1392.793508	9.191501	2.586726
-1391.189426	6.986373	2.596723
-1389.667343	6.995404	2.606720
-1387.128362	5.439559	2.616717
-1385.526304	5.189477	2.626714
-1383.816624	1.808516	2.636710
-1381.861815	0.571978	2.646707
-1379.919282	-2.770466	2.656704
-1378.267408	7.087693	2.666701
-1376.141485	6.726917	2.676698
-1374.246136	2.986245	2.686694
-1372.459957	6.003507	2.696691
-1370.804891	1.407625	2.706688
-1368.686306	-2.292987	2.716685
-1366.745932	4.048510	2.726682
-1365.080077	8.856600	2.736678
-1363.025206	0.508342	2.746675
-1361.054506	11.089161	2.756672
-1359.122933	5.305879	2.766669
-1357.353800	5.174334	2.776666
-1355.689147	3.445846	2.786662
-1353.567375	5.067315	2.796659
-1351.807884	7.454135	2.806656
-1349.874758	5.636889	2.816653
-1348.143993	5.228864	2.826650
-1346.070193	0.365451	2.836646
-1344.121689	-5.082634	2.846643
-1342.609261	-0.570494	2.856640
-1340.881521	-2.350121	2.866637
-1338.466492	5.893830	2.876634
-1336.655690	-0.762199	2.886630
-1334.756919	2.202335	2.896627
-1333.165793	8.536607	2.906624
-1331.156952	9.661440	2.916621
-1329.159147	1.911284	2.926618
-1327.270206	4.065827	2.936614
-1325.298354	-0.902828	2.946611
-1323.836319	3.367920	2.956608
-1321.615113	1.694062	2.966605
-1319.821681	8.288066	2.976602
-1318.139100	-2.755806	2.986598
-1316.190806	-1.127064	2.996595
-1314.126595	3.227311	3.006592
-1312.403430	-3.242570	3.016589
-1310.231022	-5.177025	3.026586
-1308.919945	-5.194170	3.036582
-1306.966003	-3.356327	3.046579
-1304.725487	1.580886	3.056576
-1302.910491	6.401470	3.066573
-1301.183731	4.489399	3.076570
-1298.927634	-0.589464	3.086566
-1297.264344	0.915961	3.096563
-1295.363201	2.408584	3.106560
-1293.644262	-2.156415	3.116557
-1291.991634	4.614881	3.126554
-1289.863571	1.995968	3.136550
-1288.004853	-5.356107	3.146547
-1286.219444	-1.762344	3.156544
-1283.817028	-0.915191	3.166541
-1282.165673	1.872670	3.176538
-1280.593636	-0.955669	3.186534
-1278.449754	-0.376607	3.196531
-1276.636333	2.517952	3.206528
-1274.653388	-0.958768	3.216525
-1273.049811	2.321478	3.226522
-1271.089728	-0.640007	3.236518
-1269.309999	0.928910	3.246515
-1267.492412	1.373885	3.256512
-1265.529032	-2.786533	3.266509
-1263.505440	-0.386645	3.276506
-1261.500588	-6.198942	3.286502
-1259.607391	0.816509	3.296499
-1257.752604	4.980243	3.306496
-1256.150269	3.137062	3.316493
-1254.251728	3.400147	3.326490
-1252.299984	3.739982	3.336486
-1250.443852	4.807219	3.346483
-1248.595216	7.497221	3.356480
-1246.549474	2.407856	3.366477
-1244.984038	1.697946	3.376474
-1243.027440	9.563790	3.386470
-1240.899924	4.132926	3.396467
-1239.131736	9.167895	3.406464
-1237.495752	8.023546	3.416461
-1235.228578	4.990845	3.426458
-1233.343018	-1.487600	3.436454
-1231.706891	4.596390	3.446451
-1229.808850	4.951154	3.456448
-1228.126008	2.653008	3.466445
-1225.926921	11.375323	3.476442
-1224.056855	7.804600	3.486438
-1222.034406	5.608432	3.496435
-1220.319987	6.957313	3.506432
-1218.780755	13.440502	3.516429
-1216.545001	5.966566	3.526426
-1214.641865	2.611611	3.536422
-1212.764662	3.146563	3.546419
-1211.006004	3.659432	3.556416
-1209.151818	8.592245	3.566413
-1207.384132	1.614787	3.576410
-1205.371889	3.061289	3.586406
-1203.345848	4.431375	3.596403
-1201.498849	2.088035	3.606400
-1199.777337	0.443716	3.616397
-1198.066816	6.931090	3.626394
-1196.024521	3.410201	3.636390
-1193.909389	-1.622327	3.646387
-1192.640078	1.124095	3.656384
-1190.360696	0.371044	3.666381
-1188.243573	2.244461	3.676378
-1186.685338	-2.356331	3.686374
-1184.490084	2.262986	3.696371
-1182.920327	3.503989	3.706368
-1180.905275	1.282198	3.716365
-1179.108844	-2.194603	3.726362
-1177.108124	1.497432	3.736358
-1175.464117	-0.808674	3.746355
-1173.495993	3.452260	3.756352
-1171.597619	2.177557	3.766349
-1169.762282	-2.582819	3.776346
-1168.046544	-5.830388	3.786342
-1166.050598	-4.422297	3.796339
-1164.108065	5.820585	3.806336
-1162.146818	-0.019396	3.816333
-1160.200729	-1.188039	3.826330
-1158.197625	-5.547355	3.836326
-1156.668977	-5.114488	3.846323
-1154.942225	0.896641	3.856320
-1152.768889	8.986840	3.866317
-1150.776429	6.258692	3.876314
-1149.150557	-7.187038	3.886310
-1147.177586	-2.314231	3.896307
-1145.264337	-5.964431	3.906304
-1143.542068	0.960049	3.916301
-1141.620960	0.161730	3.926298
-1139.557021	-0.536280	3.936294
-1137.679369	-0.220810	3.946291
-1136.035017	3.837743	3.956288
-1133.952364	1.829386	3.966285
-1132.155273	3.250371	3.976282
-1130.226170	2.829726	3.986278
-1128.408237	-1.564681	3.996275
-1126.678696	3.250772	4.006272
-1124.707027	5.733302	4.016269
-1122.837707	4.327497	4.026266
-1120.931872	2.680592	4.036262
-1118.914629	1.075866	4.046259
-1117.216672	1.344308	4.056256
-1115.361451	-5.443404	4.066253
-1113.445592	-4.984028	4.076250
-1111.677060	-2.667940	4.086246
-1109.751854	-0.383228	4.096243
-1107.555183	-3.234004	4.106240
-1105.886617	-8.359231	4.116237
-1104.176796	-5.005860	4.126234
-1102.098046	-3.980430	4.136230
-1100.123906	-5.887715	4.146227
-1098.440713	-4.890588	4.156224
-1096.613643	-10.206951	4.166221
-1094.483370	-3.867165	4.176218
-1092.708229	-8.717328	4.186214
-1090.842315	-11.592549	4.196211
-1089.234267	-5.442384	4.206208
-1087.138424	-3.028632	4.216205
-1085.012897	-3.938548	4.226202
-1083.571159	-5.078563	4.236198
-1081.438446	-5.774890	4.246195
-1079.671773	-3.638479	4.256192
-1078.185072	-1.845703	4.266189
-1075.614986	-0.677785	4.276186
-1073.779096	-4.179767	4.286182
-1072.156358	-7.723444	4.296179
-1070.331028	-6.163245	4.306176
-1068.508786	-7.225163	4.316173
-1066.041671	-7.602333	4.326170
-1064.837154	-2.642859	4.336166
-1063.044037	-5.959572	4.346163
-1060.896693	-3.828768	4.356160
-1058.889171	-1.501916	4.366157
-1057.260458	2.096569	4.376154
-1054.944110	-4.483800	4.386150
-1053.448427	1.270685	4.396147
-1051.680083	3.912113	4.406144
-1049.750141	-5.724852	4.416141
-1047.688165	-1.191451	4.426138
-1045.729770	-1.220398	4.436134
-1043.910661	0.547658	4.446131
-1041.972801	-3.772708	4.456128
-1040.526522	-2.488176	4.466125
-1038.687694	1.337243	4.476122
-1036.344309	-4.083758	4.486118
-1034.426736	-6.867726	4.496115
-1032.674459	-3.964770	4.506112
-1030.983834	-4.309299	4.516109
-1028.949567	-2.623009	4.526106
-1027.112518	-0.744125	4.536102
-1025.359691	0.254551	4.546099
-1023.137865	-1.783861	4.556096
-1021.282208	-5.937908	4.566093
-1019.619862	-7.275794	4.576090
-1017.685510	-4.499839	4.586086
-1015.976252	-5.845224	4.596083
-1013.949080	-2.839374	4.606080
-1012.347922	5.429311	4.616077
-1009.856015	-2.709085	4.626074
-1008.334483	-2.262351	4.636070
-1006.679470	-2.029592	4.646067
-1004.603427	-3.064154	4.656064
-1002.565541	-1.326314	4.666061
-1000.964438	-2.551762	4.676058
-999.094416	-5.947042	4.686054
-996.955338	-1.904342	4.696051
-995.229709	-5.595474	4.706048
-993.436529	1.043054	4.716045
-991.238152	1.089461	4.726042
-989.605847	-0.668335	4.736038
-988.053640	-1.030173	4.746035
-985.781303	0.971769	4.756032
-983.839966	3.737164	4.766029
-982.212166	-2.073040	4.776026
-980.080403	0.009806	4.786022
-977.905509	-1.975270	4.796019
-976.324252	1.621389	4.806016
-974.836203	4.421381	4.816013
-972.801222	-2.191291	4.826010
-970.798767	-2.334588	4.836006
-968.859482	-1.015160	4.846003
-966.743320	0.552302	4.856000
-965.235495	0.499154	4.865997
-963.340475	-5.690079	4.875994
-961.599925	-3.134138	4.885990
-959.687195	-3.007291	4.895987
-957.543373	0.969953	4.905984
-955.880584	-4.684777	4.915981
-953.979071	-2.130882	4.925978
-952.152275	-3.907119	4.935974
-950.100285	-8.799869	4.945971
-948.205825	-2.779074	4.955968
-946.662380	4.772578	4.965965
-944.490442	0.776436	4.975962
-942.463542	-1.437576	4.985958
-940.556243	4.900122	4.995955
-938.850863	-1.257195	5.005952
-937.113945	-1.269587	5.015949
-935.525072	2.575357	5.025946
-933.240550	3.452777	5.035942
-931.232778	1.090255	5.045939
-929.603988	-0.310099	5.055936
-927.730923	5.513613	5.065933
-925.671385	-0.424005	5.075930
-923.863116	3.205871	5.085926
-922.162327	6.789775	5.095923
-920.159654	8.741740	5.105920
-918.296275	3.721273	5.115917
-916.346036	3.125321	5.125914
-914.502121	3.177944	5.135910
-912.628459	4.755806	5.145907
-910.899780	5.513695	5.155904
-909.096093	2.924873	5.165901
-906.833268	1.858955	5.175898
-905.281999	-4.139490	5.185894
-903.285899	-0.406997	5.195891
-901.064829	-6.667258	5.205888
-899.268363	-5.457569	5.215885
-897.669166	-4.290552	5.225882
-895.767225	-3.527194	5.235878
-893.909996	-8.496129	5.245875
-892.015049	-3.177991	5.255872
-890.081532	-4.791243	5.265869
-888.326864	-1.286981	5.275866
-886.390381	0.042439	5.285862
-884.534064	-5.790024	5.295859
-882.628058	5.040013	5.305856
-880.956040	2.800680	5.315853
-878.814771	-0.838397	5.325850
-876.902729	-0.250322	5.335846
-875.061740	0.191220	5.345843
-873.105146	-0.459397	5.355840
-871.446271	-8.333434	5.365837
-869.583247	-9.295930	5.375834
-867.511352	-8.033932	5.385830
-865.769332	-5.733940	5.395827
-863.776851	-6.619232	5.405824
-861.984949	-0.154074	5.415821
-859.859781	-3.432141	5.425818
-858.506784	-4.775727	5.435814
-856.638530	-3.571165	5.445811
-854.556559	-8.681786	5.455808
-852.438695	-8.061856	5.465805
-850.624610	-11.678605	5.475802
-848.603052	-15.813251	5.485798
-846.890914	-8.301129	5.495795
-845.199796	-14.260311	5.505792
-843.572121	-11.092556	5.515789
-841.306512	-12.177803	5.525786
-839.108571	-9.971196	5.535782
-837.777868	-15.208028	5.545779
-835.921206	-8.243206	5.555776
-833.939063	-8.700507	5.565773
-831.894004	-8.815759	5.575770
-829.943362	-9.261705	5.585766
-828.037750	-11.317286	5.595763
-826.189064	-5.540121	5.605760
-824.648850	0.551616	5.615757
-822.741090	-7.090596	5.625754
-820.478120	-9.752762	5.635750
-818.774690	-12.999697	5.645747
-816.957076	-7.759135	5.655744
-815.196759	-13.753042	5.665741
-813.406141	-9.220263	5.675738
-811.047643	-14.144520	5.685734
-809.341464	-14.009800	5.695731
-807.807045	-8.640282	5.705728
-805.816114	-5.817926	5.715725
-803.989773	-8.617131	5.725722
-801.981038	-13.060741	5.735718
-799.809469	-16.477222	5.745715
-798.140323	-7.830826	5.755712
-796.411151	-9.166607	5.765709
-794.263849	-8.781854	5.775706
-792.635404	-14.388355	5.785702
-790.517569	-15.862038	5.795699
-789.050220	-5.411811	5.805696
-786.892972	-8.873361	5.815693
-784.905000	-9.663130	5.825690
-782.980116	-11.701230	5.835686
-781.306398	-14.558129	5.845683
-779.594853	-13.372671	5.855680
-777.660259	-12.835488	5.865677
-775.690858	-11.026503	5.875674
-773.518273	-18.990470	5.885670
-771.896517	-11.613843	5.895667
-769.987856	-10.857773	5.905664
-768.350678	-14.515663	5.915661
-766.293393	-10.728093	5.925658
-764.393335	-7.850126	5.935654
-762.465501	-11.442358	5.945651
-760.772799	-14.447540	5.955648
-758.724460	-10.415377	5.965645
-756.937032	-5.994147	5.975642
-754.893409	-13.124337	5.985638
-753.058109	-13.687576	5.995635
-751.448368	-8.570054	6.005632
-749.707885	-2.789742	6.015629
-747.328917	-2.617231	6.025626
-745.600069	-8.565011	6.035622
-743.809813	-9.379991	6.045619
-741.923611	-7.088736	6.055616
-740.147619	-4.615657	6.065613
-738.188424	-13.466019	6.075610
-736.317062	-13.101855	6.085606
-734.258070	-9.900315	6.095603
-732.301730	-10.610775	6.105600
-730.820442	-11.685844	6.115597
-728.657915	-5.723486	6.125594
-726.886467	-12.039638	6.135590
-725.074528	-15.867530	6.145587
-723.208975	-11.322970	6.155584
-721.287798	-18.624616	6.165581
-719.400629	-16.072973	6.175578
-717.498152	-14.587981	6.185574
-715.535112	-10.340043	6.195571
-713.829302	-13.871497	6.205568
-712.035127	-15.048656	6.215565
-709.900420	-9.407098	6.225562
-707.937128	-9.048126	6.235558
-706.015663	-15.216129	6.245555
-704.425114	-12.037605	6.255552
-702.539580	-15.226717	6.265549
-700.737162	-15.157822	6.275546
-698.961083	-13.186829	6.285542
-696.891563	-20.126899	6.295539
-695.047467	-16.816778	6.305536
-693.051019	-19.717289	6.315533
-691.129970	-17.557878	6.325530
-689.140326	-22.331501	6.335526
-687.465885	-19.535843	6.345523
-685.571854	-16.814744	6.355520
-683.598676	-13.694184	6.365517
-681.884161	-13.821229	6.375514
-679.982797	-17.178641	6.385510
-678.017655	-11.571539	6.395507
-676.138954	-8.734296	6.405504
-674.321537	-13.652497	6.415501
-672.851487	-11.424168	6.425498
-670.389156	-16.355408	6.435494
-668.592782	-16.272891	6.445491
-667.031537	-15.868596	6.455488
-665.050116	-12.533022	6.465485
-663.056359	-18.022545	6.475482
-661.092743	-10.942030	6.485478
-659.223264	-17.084324	6.495475
-657.520123	-15.450593	6.505472
-655.558693	-15.977066	6.515469
-653.843473	-21.523131	6.525466
-651.743610	-13.193330	6.535462
-649.912368	-20.125293	6.545459
-647.950808	-8.399190	6.555456
-646.493906	-11.579779	6.565453
-644.726664	-6.141553	6.575450
-642.174424	-13.896069	6.585446
-640.426084	-16.562690	6.595443
-638.954543	-16.011414	6.605440
-636.762192	-12.395305	6.615437
-635.121637	-12.482079	6.625434
-632.953005	-9.662699	6.635430
-631.095478	-10.589395	6.645427
-629.390915	-10.550602	6.655424
-627.332569	-12.387269	6.665421
-625.688201	-13.159907	6.675418
-623.836416	-11.369898	6.685414
-621.743123	-8.312683	6.695411
-619.951573	-6.039364	6.705408
-618.003235	-11.657386	6.715405
-616.194783	-12.813072	6.725402
-614.398558	-11.366284	6.735398
-612.430677	-16.998475	6.745395
-610.457828	-23.971978	6.755392
-608.736265	-12.438027	6.765389
-606.845325	-16.801084	6.775386
-604.672750	-15.556515	6.785382
-603.010543	-13.448837	6.795379
-601.471053	-5.907357	6.805376
-599.183948	-11.030010	6.815373
-597.414270	-14.446850	6.825370
-595.276050	-11.265735	6.835366
-593.697827	-13.144098	6.845363
-592.132403	-14.024102	6.855360
-590.154076	-10.408495	6.865357
-588.002730	-14.652084	6.875354
-585.894916	-14.297150	6.885350
-584.334717	-12.031059	6.895347
-582.209748	-14.241487	6.905344
-580.500565	-9.176040	6.915341
-578.850524	-10.276394	6.925338
-576.746234	-14.184037	6.935334
-574.650563	-7.438746	6.945331
-573.155429	-19.396431	6.955328
-571.212730	-9.269869	6.965325
-569.351000	-12.772446	6.975322
-567.189189	-9.010864	6.985318
-565.634561	-7.792289	6.995315
-563.818703	-3.095971	7.005312
-561.874586	-2.275920	7.015309
-559.899085	-5.967190	7.025306
-557.889107	-10.252911	7.035302
-555.928378	-3.756046	7.045299
-554.384787	-7.724112	7.055296
-552.650234	-6.142688	7.065293
-550.366389	-7.486362	7.075290
-548.498313	-1.724689	7.085286
-546.807691	-9.638335	7.095283
-545.065233	-5.138699	7.105280
-543.147907	-2.620146	7.115277
-540.953240	-6.205880	7.125274
-539.372037	-9.145736	7.135270
-537.324636	-10.674263	7.145267
-535.700551	-1.109405	7.155264
-533.399430	-7.290553	7.165261
-531.585551	-16.117555	7.175258
-529.800664	-10.468898	7.185254
-528.024626	-8.579872	7.195251
-526.191410	-8.496816	7.205248
-524.264301	-6.864020	7.215245
-522.408738	-7.381371	7.225242
-520.658133	-13.503002	7.235238
-518.512732	-15.604533	7.245235
-516.811007	-9.031533	7.255232
-514.628254	-8.642714	7.265229
-512.930753	-5.424292	7.275226
-511.470730	-12.274771	7.285222
-509.172140	-9.059189	7.295219
-507.460852	-13.102955	7.305216
-505.479699	-4.446152	7.315213
-503.628628	-10.043818	7.325210
-501.414242	-8.087410	7.335206
-499.809576	-7.751518	7.345203
-498.177189	-12.512150	7.355200
-496.096242	-1.206014	7.365197
-494.040505	-3.275837	7.375194
-492.300506	-5.044183	7.385190
-490.474230	-14.582084	7.395187
-488.619113	-12.468816	7.405184
-486.586869	-10.723306	7.415181
-485.220710	-11.353524	7.425178
-482.763120	-11.104882	7.435174
-481.036458	-9.646882	7.445171
-479.320574	-10.263473	7.455168
-477.519159	-10.134249	7.465165
-475.403653	-12.581494	7.475162
-473.482516	-14.285593	7.485158
-471.423689	-4.518533	7.495155
-469.707590	-12.644618	7.505152
-468.081428	-4.947933	7.515149
-466.043644	-12.343808	7.525146
-463.967392	-9.127412	7.535142
-462.405495	-8.453086	7.545139
-460.331252	-5.793733	7.555136
-458.683633	-7.070461	7.565133
-456.872210	-6.920713	7.575130
-454.929016	-2.290430	7.585126
-452.771577	-5.014353	7.595123
-451.134324	-10.113628	7.605120
-449.287549	-3.120050	7.615117
-446.930094	-5.054854	7.625114
-445.448428	-6.696652	7.635110
-443.530623	-6.375987	7.645107
-441.896162	-7.071128	7.655104
-439.729392	-10.082319	7.665101
-437.875146	-9.246237	7.675098
-435.884677	-11.872430	7.685094
-434.206919	-12.850796	7.695091
-432.435869	-5.123534	7.705088
-430.725542	-3.732362	7.715085
-428.595923	-5.513927	7.725082
-426.449555	-8.022901	7.735078
-424.573893	-12.294963	7.745075
-423.023237	-11.093027	7.755072
-421.266001	-6.802497	7.765069
-418.871841	-8.244188	7.775066
-417.329975	-5.921371	7.785062
-415.411519	-12.112364	7.795059
-413.525665	-2.071312	7.805056
-411.822457	-9.198988	7.815053
-409.568865	-2.794542	7.825050
-407.718525	-8.922550	7.835046
-405.921000	-7.556335	7.845043
-404.408399	-6.169889	7.855040
-402.610092	-4.690111	7.865037
-400.363890	-11.448160	7.875034
-398.480693	-8.123513	7.885030
-396.494857	-10.205777	7.895027
-394.722325	-8.870300	7.905024
-393.053530	-2.849310	7.915021
-391.044189	-3.519007	7.925018
-389.260822	-4.956308	7.935014
-387.311740	-1.574275	7.945011
-385.176142	-0.274650	7.955008
-383.377778	-3.402237	7.965005
-381.682880	-1.039091	7.975002
-379.859048	5.296634	7.984998
-377.934323	-4.643761	7.994995
-376.042227	-2.012093	8.004992
-374.547700	-12.085904	8.014989
-372.154199	-10.007969	8.024986
-370.014777	-10.437890	8.034982
-368.171100	-5.629013	8.044979
-366.682604	-1.508692	8.054976
-364.674993	-5.095988	8.064973
-362.991485	-3.564695	8.074970
-361.068213	-2.317993	8.084966
-358.964446	-5.049056	8.094963
-357.482694	-6.548709	8.104960
-355.270295	4.624481	8.114957
-353.274306	-8.159906	8.124954
-351.523552	-6.165656	8.134950
-350.050267	-3.321845	8.144947
-348.105415	-2.492262	8.154944
-345.851074	-6.638405	8.164941
-344.053488	-7.771627	8.174938
-342.204172	-6.031525	8.184934
-340.265771	-2.635115	8.194931
-338.517509	-3.986249	8.204928
-336.883562	-8.074399	8.214925
-334.596234	-8.992110	8.224922
-332.744711	-1.779716	8.234918
-331.010698	-8.463838	8.244915
-329.098443	-7.046405	8.254912
-327.204770	-5.736530	8.264909
-325.174156	-6.344832	8.274906
-323.740089	-6.398430	8.284902
-321.842699	-0.758087	8.294899
-319.738169	-4.927661	8.304896
-317.860350	-6.469987	8.314893
-315.778308	-4.779646	8.324890
-313.977098	-7.089741	8.334886
-312.096631	-11.289857	8.344883
-310.448031	-10.004007	8.354880
-308.640953	-5.092923	8.364877
-306.564678	-11.675345	8.374874
-304.684116	-10.934939	8.384870
-302.989521	-6.574318	8.394867
-300.788689	-13.410301	8.404864
-299.156247	-10.817653	8.414861
-297.338229	-11.169365	8.424858
-295.323364	-3.220380	8.434854
-293.351438	-8.949294	8.444851
-291.601508	-2.036439	8.454848
-289.560314	-4.301138	8.464845
-287.903571	-7.538684	8.474842
-285.741365	-3.483213	8.484838
-283.847361	-9.117576	8.494835
-282.221316	-11.286005	8.504832
-280.546732	-11.869021	8.514829
-278.587833	-13.531627	8.524826
-276.329630	-9.415681	8.534822
-274.730073	-14.403039	8.544819
-273.020677	-10.952654	8.554816
-271.017680	-6.619127	8.564813
-269.253076	-5.482816	8.574810
-267.038453	-6.507280	8.584807
-265.127474	-16.524343	8.594803
-263.378387	-13.920287	8.604800
-261.574894	-6.294380	8.614797
-259.700087	0.443834	8.624794
-257.727818	-4.999319	8.634791
-255.922201	-1.704803	8.644787
-254.361108	-0.987579	8.654784
-252.119038	1.111491	8.664781
-250.114277	-2.903155	8.674778
-248.329716	-4.490545	8.684775
-246.458375	-4.530202	8.694771
-244.681350	-3.244276	8.704768
-242.561671	-3.873038	8.714765
-240.927202	-6.952261	8.724762
-238.771885	-8.530920	8.734759
-237.121649	-12.029499	8.744755
-235.530695	-13.115453	8.754752
-233.381188	-6.991062	8.764749
-231.557596	-15.645732	8.774746
-229.652647	-8.361254	8.784743
-227.612781	-5.933050	8.794739
-225.982352	-3.842133	8.804736
-224.101568	-11.550663	8.814733
-222.206368	-6.574626	8.824730
-220.091855	-7.452018	8.834727
-218.298946	-1.367017	8.844723
-216.523854	-6.432881	8.854720
-214.528616	-9.981766	8.864717
-213.242958	-12.458988	8.874714
-211.096304	-12.547290	8.884711
-208.887082	-3.910820	8.894707
-207.133273	-8.565911	8.904704
-205.238182	-9.214064	8.914701
-203.295546	-14.109284	8.924698
-201.636546	-11.738701	8.934695
-199.630245	-10.768803	8.944691
-197.835405	-4.723569	8.954688
-195.763530	-5.699926	8.964685
-193.880296	-10.312503	8.974682
-192.254914	-6.104965	8.984679
-190.450212	-4.993941	8.994675
-188.056214	-1.065366	9.004672
-186.760664	-8.284166	9.014669
-184.873720	-9.699952	9.024666
-182.728550	-5.610087	9.034663
-180.929343	-8.298715	9.044659
-179.017924	-9.708929	9.054656
-177.186167	-2.499565	9.064653
-175.306710	-7.149422	9.074650
-173.385402	-9.867001	9.084647
-171.444748	-8.588183	9.094643
-169.552386	-3.096909	9.104640
-167.651669	-2.830139	9.114637
-165.764497	-4.178052	9.124634
-164.004779	-11.993538	9.134631
-162.062417	-10.628143	9.144627
-160.314947	-12.133761	9.154624
-158.729422	-15.918805	9.164621
-156.774337	-12.764906	9.174618
-154.290328	-12.438038	9.184615
-152.498469	-13.267047	9.194611
-150.986911	-5.889730	9.204608
-149.238903	-6.757529	9.214605
-147.120141	-7.378168	9.224602
-145.049357	-11.662211	9.234599
-143.416880	-8.668405	9.244595
-141.332575	-3.772998	9.254592
-139.570618	-5.861967	9.264589
-137.863655	-4.703730	9.274586
-135.926511	-7.177492	9.284583
-133.800785	-10.631869	9.294579
-132.265805	-16.234101	9.304576
-130.500267	-7.545711	9.314573
-128.429898	-15.739159	9.324570
-126.474868	-11.824170	9.334567
-124.560359	-6.868500	9.344563
-122.742244	-12.358006	9.354560
-120.945950	-9.401373	9.364557
-118.956552	-5.621333	9.374554
-116.879858	-7.102079	9.384551
-115.308795	0.717354	9.394547
-113.203280	0.032542	9.404544
-111.582034	-1.550799	9.414541
-109.519347	2.340717	9.424538
-107.755159	-2.489650	9.434535
-106.064669	2.058093	9.444531
-104.031000	-1.728944	9.454528
-101.956559	3.024391	9.464525
-100.057532	-1.311166	9.474522
-98.360355	-1.813976	9.484519
-96.407011	-4.536609	9.494515
-94.737949	-4.288087	9.504512
-92.814071	-2.968633	9.514509
-90.635918	-4.677122	9.524506
-88.909218	-9.043597	9.534503
-87.149728	-7.576334	9.544499
-85.438931	-6.273408	9.554496
-83.118726	1.371274	9.564493
-81.513442	-2.598459	9.574490
-79.345742	-5.450012	9.584487
-77.661203	-9.830280	9.594483
-75.936289	-3.838528	9.604480
-74.181729	-8.204701	9.614477
-72.120983	0.741386	9.624474
-70.109066	-8.761123	9.634471
-68.369836	-3.347967	9.644467
-66.385724	-6.397591	9.654464
-64.419809	-5.260084	9.664461
-62.630112	-4.677099	9.674458
-60.636054	-7.867252	9.684455
-58.766988	-10.309568	9.694451
-57.290744	-7.000250	9.704448
-55.142279	-1.076047	9.714445
-53.447017	-3.975373	9.724442
-51.274376	-9.920860	9.734439
-49.679251	-7.783137	9.744435
-47.554962	-5.740876	9.754432
-45.962893	-7.538994	9.764429
-43.919188	-7.874411	9.774426
-41.771556	-5.294287	9.784423
-40.438407	-13.059019	9.794419
-38.117595	-7.610716	9.804416
-36.581408	-5.972006	9.814413
-34.583219	-6.199101	9.824410
-32.477818	-4.775922	9.834407
-31.087397	-2.967113	9.844403
-28.770477	-0.008188	9.854400
-26.741273	-0.177066	9.864397
-25.292333	-3.065505	9.874394
-23.420976	-5.762372	9.884391
-21.415263	-7.220663	9.894387
-19.507007	-11.466050	9.904384
-17.593357	-5.338568	9.914381
-15.756225	-9.059448	9.924378
-13.906459	-8.446534	9.934375
-11.976954	-10.183188	9.944371
-10.192309	-4.578284	9.954368
-8.359530	-13.886382	9.964365
-6.553721	-4.498519	9.974362
-5.041207	18.755160	9.984359
-3.726373	46.696760	9.994355
-2.470995	93.188098	10.004352
-1.173307	144.679754	10.014349
0.000000	204.269585	10.019354
0.688103	246.269443	10.024359
1.773884	277.176689	10.029363
2.187641	306.068585	10.034368
2.344816	324.497253	10.039373
3.072068	338.004751	10.044378
3.166055	360.993111	10.049383
3.237100	369.453323	10.054387
3.507946	385.697173	10.059392
3.382380	395.095521	10.064397
3.913220	393.228898	10.069402
3.629623	404.254667	10.074407
3.973664	402.014130	10.079411
3.900410	409.779854	10.084416
3.758309	410.961629	10.089421
4.168819	423.835317	10.094426
4.047789	446.075922	10.099431
4.293282	444.056104	10.104435
4.347946	441.603090	10.109440
4.509112	452.756658	10.114445
4.486036	449.801944	10.119450
4.627626	448.721234	10.124455
4.469252	432.662863	10.129459
4.395379	440.133807	10.134464
4.363801	441.435154	10.139469
4.467078	440.489867	10.144474
4.529004	460.304299	10.149479
4.733440	463.812056	10.154483
5.044850	466.656188	10.159488
5.181108	467.493942	10.164493
4.580580	454.743623	10.169498
4.488426	444.321864	10.174503
4.888148	455.062064	10.179507
4.784556	466.898127	10.184512
4.738272	467.069545	10.189517
5.306046	468.396729	10.194522
5.099638	478.292159	10.199527
5.375801	475.396948	10.204531
5.491146	482.044509	10.209536
5.180550	479.756981	10.214541
5.186982	476.450617	10.219546
5.028096	488.276593	10.224551
5.075339	483.514466	10.229555
5.143684	487.441336	10.234560
4.834608	495.173754	10.239565
5.165989	486.242479	10.244570
5.009336	499.611980	10.249575
5.247320	499.113571	10.254579
5.618655	510.974850	10.259584
5.743440	515.641796	10.264589
6.023991	503.635599	10.269594
5.343813	514.216913	10.274599
5.780606	516.848664	10.279603
5.919026	531.664543	10.284608
5.652068	534.723941	10.289613
5.895194	532.597253	10.294618
5.988875	537.568796	10.299623
5.891802	534.597481	10.304627
5.871008	538.041828	10.309632
6.078996	536.169909	10.314637
6.152122	531.622841	10.319642
5.984719	542.797344	10.324647
6.160436	542.996434	10.329651
6.198361	544.960082	10.334656
5.970714	547.603193	10.339661
6.025737	543.375984	10.344666
5.942591	551.340486	10.349671
6.264146	543.748037	10.354675
6.400391	553.232466	10.359680
6.239589	553.171407	10.364685
6.823064	563.989617	10.369690
6.368322	566.924425	10.374695
6.907352	571.151572	10.379699
6.772854	569.433624	10.384704
6.579562	560.685337	10.389709
6.587067	569.308769	10.394714
6.544183	572.952196	10.399719
7.072199	576.616535	10.404723
7.435680	586.830377	10.409728
6.836338	587.052157	10.414733
7.175246	571.653144	10.419738
6.743487	577.963797	10.424743
6.890038	580.460496	10.429747
7.023404	594.308180	10.434752
7.003969	603.087321	10.439757
7.364936	594.928723	10.444762
7.204998	604.648088	10.449767
7.041216	600.474685	10.454771
7.002481	602.761236	10.459776
6.920786	596.204508	10.464781
7.777229	602.539954	10.469786
7.306684	608.465709	10.474791
7.563438	604.179498	10.479795
7.274756	617.969147	10.484800
7.159739	615.074796	10.489805
7.546189	604.041984	10.494810
7.375391	624.054612	10.499815
7.752701	628.102558	10.504819
7.780167	642.217133	10.509824
7.880382	633.593884	10.514829
8.075277	636.778342	10.519834
7.480101	639.309771	10.524839
7.791053	639.162432	10.529843
8.181506	635.621313	10.534848
8.056308	644.455195	10.539853
8.179622	640.265953	10.544858
8.091379	647.326119	10.549863
8.073448	646.431692	10.554867
8.262180	647.865082	10.559872
8.085179	653.860735	10.564877
8.308244	645.168998	10.569882
7.987976	659.988778	10.574887
8.382351	648.043159	10.579891
8.229755	645.402385	10.584896
7.925243	660.993964	10.589901
8.406829	653.688181	10.594906
8.465089	665.504899	10.599911
8.696213	660.623497	10.604915
8.655419	675.887592	10.609920
8.640973	678.337444	10.614925
9.131997	680.148417	10.619930
8.721412	672.849297	10.624935
8.480430	667.349306	10.629939
8.803181	677.668271	10.634944
8.946588	688.629304	10.639949
8.800089	673.052916	10.644954
8.618859	692.849674	10.649959
9.180452	681.386732	10.654963
8.925298	697.358421	10.659968
8.788085	698.518938	10.664973
8.966458	697.164251	10.669978
8.979632	693.501935	10.674983
8.858222	697.828147	10.679987
9.235483	699.493257	10.684992
9.253883	716.254000	10.689997
9.560675	715.022338	10.695002
9.898627	719.565462	10.700007
9.416904	710.378944	10.705011
9.242071	697.068486	10.710016
9.385293	715.703311	10.715021
9.883641	706.420408	10.720026
9.721595	725.490302	10.725031
10.022094	723.936355	10.730035
9.928471	707.107232	10.735040
9.525217	715.807303	10.740045
9.718188	703.426964	10.745050
9.668756	731.776974	10.750055
9.917231	735.112187	10.755059
9.955851	728.630831	10.760064
9.775493	742.174653	10.765069
10.357431	727.004019	10.770074
10.066499	740.496086	10.775079
9.977870	738.281927	10.780083
10.047118	730.988253	10.785088
9.911261	742.414931	10.790093
10.121433	739.708396	10.795098
9.948570	739.431632	10.800103
10.228760	740.307951	10.805107
10.273226	739.755240	10.810112
10.164086	736.579219	10.815117
10.380054	737.413739	10.820122
10.526821	754.376411	10.825127
10.899506	762.982717	10.830131
10.812791	748.008596	10.835136
10.175300	743.164775	10.840141
10.607031	746.098587	10.845146
10.721984	769.368113	10.850151
11.247137	773.698463	10.855155
11.137943	763.209803	10.860160
10.574084	751.541515	10.865165
10.924389	760.785350	10.870170
10.965968	764.607750	10.875175
10.775667	773.497827	10.880179
11.202354	759.432179	10.885184
10.856185	767.891354	10.890189
11.437351	766.220096	10.895194
11.242958	770.220488	10.900199
11.202708	774.800295	10.905203
11.409825	768.099651	10.910208
10.964890	774.634848	10.915213
11.119902	771.713168	10.920218
11.008249	778.504307	10.925223
11.363177	777.048911	10.930227
11.654751	780.397763	10.935232
11.382311	772.029417	10.940237
11.502485	768.905128	10.945242
11.304508	773.406007	10.950247
11.498131	769.899403	10.955251
11.668179	778.698894	10.960256
11.641812	780.728023	10.965261
12.156617	783.490891	10.970266
12.301205	790.203319	10.975271
11.932482	778.611123	10.980275
11.967491	767.744632	10.985280
11.960802	770.764144	10.990285
11.843907	778.103345	10.995290
11.609541	773.660439	11.000295
11.916805	786.508338	11.005299
12.188369	800.461128	11.010304
12.339053	795.472657	11.015309
12.567033	800.293556	11.020314
12.526670	805.043709	11.025319
12.264865	806.437003	11.030323
12.477090	790.767003	11.035328
12.332999	791.253658	11.040333
12.390325	798.328529	11.045338
12.501834	808.334334	11.050343
12.395674	804.336193	11.055347
12.516114	799.578058	11.060352
12.438422	804.203272	11.065357
12.607533	803.334199	11.070362
12.381498	803.518519	11.075367
12.415478	797.906812	11.080371
12.815891	802.709672	11.085376
12.467016	809.101825	11.090381
12.665497	804.397477	11.095386
12.562919	810.993210	11.100391
12.917879	826.746302	11.105395
13.130080	827.135131	11.110400
13.209930	830.889940	11.115405
13.459536	823.895475	11.120410
13.196676	828.116547	11.125415
13.394170	829.838730	11.130419
13.340376	811.809325	11.135424
13.385800	809.807174	11.140429
13.133834	798.754606	11.145434
13.420867	818.847452	11.150439
13.705603	821.473550	11.155443
13.501630	806.710467	11.160448
13.283702	813.092775	11.165453
13.635301	814.225804	11.170458
13.759324	827.454643	11.175463
13.588727	839.755879	11.180467
13.677780	832.031621	11.185472
13.629739	837.325506	11.190477
13.836020	833.129285	11.195482
13.731489	845.145586	11.200487
13.780622	830.130789	11.205491
13.955369	830.583941	11.210496
13.873434	840.404569	11.215501
14.281253	836.456914	11.220506
14.003743	836.994813	11.225511
14.156077	841.832522	11.230515
13.933915	841.071585	11.235520
13.781059	842.513741	11.240525
14.362219	829.779633	11.245530
14.218929	840.139926	11.250535
13.877829	842.138833	11.255539
14.226770	830.050494	11.260544
13.905638	837.531114	11.265549
14.208508	844.722971	11.270554
14.399859	848.362226	11.275559
14.385565	854.278392	11.280563
14.726484	855.577139	11.285568
14.418731	866.200236	11.290573
14.913179	859.157242	11.295578
14.956018	862.306075	11.300583
14.961870	856.183143	11.305587
14.932629	840.384436	11.310592
14.635492	841.081591	11.315597
14.942877	835.273292	11.320602
14.852572	849.148220	11.325607
15.130853	850.467996	11.330611
15.313329	847.839979	11.335616
14.781466	839.421502	11.340621
15.006341	845.256940	11.345626
14.809408	860.490935	11.350631
15.071296	868.164027	11.355635
14.837417	854.347152	11.360640
14.930658	861.228659	11.365645
15.322853	864.938393	11.370650
15.257664	861.708023	11.375655
15.246709	873.655804	11.380659
15.122968	866.717710	11.385664
15.281821	870.305381	11.390669
15.401410	864.377204	11.395674
15.548902	882.715082	11.400679
16.091165	887.028546	11.405683
15.926643	865.476295	11.410688
15.794453	866.408931	11.415693
15.718054	862.910677	11.420698
15.674627	872.302540	11.425703
15.815096	875.402687	11.430707
16.258914	857.587188	11.435712
15.541629	867.624289	11.440717
15.703198	864.633733	11.445722
15.982081	873.669825	11.450727
15.998183	900.076271	11.455731
16.262259	892.115898	11.460736
16.309497	895.992626	11.465741
16.702396	890.016118	11.470746
16.308563	879.481303	11.475751
16.119410	859.510022	11.480755
16.230824	858.574451	11.485760
16.296893	870.890010	11.490765
16.457317	879.493968	11.495770
16.545573	880.374098	11.500775
16.479281	882.510540	11.505779
16.756978	890.881324	11.510784
16.716512	890.857844	11.515789
16.330074	867.885382	11.520794
16.712806	893.334436	11.525799
16.388560	896.898232	11.530803
16.742891	890.207171	11.535808
16.176772	904.107573	11.540813
16.628413	899.086838	11.545818
16.719282	907.099479	11.550823
16.686756	908.599724	11.555827
17.106485	908.800907	11.560832
16.842209	906.531153	11.565837
16.815363	904.354425	11.570842
16.874582	897.472296	11.575847
17.048722	921.033840	11.580851
17.669231	920.176350	11.585856
17.218957	918.750009	11.590861
17.345796	907.999660	11.595866
17.414317	896.883287	11.600871
17.212341	902.501383	11.605875
17.502889	895.099788	11.610880
17.579053	922.928644	11.615885
17.424240	916.238345	11.620890
17.624968	910.606308	11.625895
17.612061	926.744627	11.630899
17.797663	916.920083	11.635904
17.616642	928.988079	11.640909
18.109399	918.363876	11.645914
17.888431	902.229807	11.650919
17.389265	899.708919	11.655923
17.706102	905.468210	11.660928
17.915324	912.845358	11.665933
18.137496	915.389983	11.670938
17.872821	923.579193	11.675943
17.941264	926.137299	11.680947
18.276256	921.642966	11.685952
18.101346	921.986299	11.690957
18.227209	926.271565	11.695962
18.024247	921.057164	11.700967
17.769955	927.071564	11.705971
17.976432	915.193544	11.710976
17.682365	922.321365	11.715981
17.956230	919.249807	11.720986
17.834080	935.776163	11.725991
18.091627	946.339122	11.730995
18.525184	946.545986	11.736000
18.328878	954.659650	11.741005
18.721280	954.374733	11.746010
18.873916	964.924475	11.751015
18.505608	948.979442	11.756019
18.931016	951.676174	11.761024
18.734001	946.076018	11.766029
18.810911	954.291195	11.771034
18.932967	948.324742	11.776039
18.833705	944.959431	11.781043
19.359528	953.252830	11.786048
19.096444	946.704371	11.791053
19.324519	946.470895	11.796058
19.120363	950.457123	11.801063
18.895090	943.308091	11.806067
18.971115	939.307665	11.811072
18.732379	950.091712	11.816077
19.067629	946.442624	11.821082
18.929709	956.053050	11.826087
19.168820	953.884363	11.831091
19.601588	970.079390	11.836096
19.773268	973.959948	11.841101
19.807451	952.022620	11.846106
19.640839	949.648968	11.851111
19.697782	946.217741	11.856115
19.748000	936.955700	11.861120
19.467715	945.377659	11.866125
19.734914	948.714668	11.871130
19.694061	938.183441	11.876135
19.768888	947.091266	11.881139
19.722513	941.228954	11.886144
19.563674	945.564363	11.891149
19.995412	954.695982	11.896154
20.126654	959.459820	11.901159
20.336395	966.057854	11.906163
20.223503	951.300598	11.911168
19.752800	951.238497	11.916173
20.221218	941.764667	11.921178
20.198118	951.164378	11.926183
19.992698	959.528672	11.931187
20.678927	965.099756	11.936192
20.104036	968.851787	11.941197
20.298930	968.368122	11.946202
20.371932	968.949476	11.951207
20.311131	970.157754	11.956211
20.481154	965.457893	11.961216
20.343134	966.590172	11.966221
20.556954	965.775464	11.971226
20.345400	972.341339	11.976231
20.453897	967.204988	11.981235
20.680907	968.588149	11.986240
20.321658	975.877788	11.991245
20.449753	969.391517	11.996250
21.045742	971.203136	12.001255
20.791867	963.020963	12.006259
20.965968	964.466181	12.011264
20.557357	982.465499	12.016269
20.846198	988.752868	12.021274
21.312710	1009.285736	12.026279
20.947294	997.574557	12.031283
21.469954	994.652549	12.036288
21.208146	981.235845	12.041293
20.981513	976.140323	12.046298
21.140590	975.703374	12.051303
20.961244	974.136040	12.056307
20.775645	962.325244	12.061312
21.194999	971.741140	12.066317
21.345272	959.996633	12.071322
21.428752	966.886056	12.076327
21.244289	979.232202	12.081331
21.322921	971.284015	12.086336
21.144830	976.442565	12.091341
21.080326	970.936390	12.096346
21.497927	966.988718	12.101351
21.444687	961.669994	12.106355
21.148160	951.562755	12.111360
20.816157	945.914738	12.116365
20.908440	941.929066	12.121370
20.850390	943.898612	12.126375
20.994314	947.934986	12.131379
21.035208	931.850588	12.136384
20.769402	942.976433	12.141389
20.792898	938.465540	12.146394
21.194574	946.321394	12.151399
20.874839	961.519884	12.156403
20.887808	947.078469	12.161408
21.170736	962.327507	12.166413
21.346935	959.362986	12.171418
21.197011	946.489896	12.176423
20.728035	949.966394	12.181427
21.167494	943.708034	12.186432
20.775352	950.309009	12.191437
20.823713	946.325610	12.196442
20.993952	946.229099	12.201447
20.701419	944.859603	12.206451
20.926970	960.776992	12.211456
20.805902	970.731689	12.216461
21.003594	972.171569	12.221466
21.167136	980.989568	12.226471
21.086153	983.199334	12.231475
21.304183	972.309808	12.236480
21.181539	967.397989	12.241485
21.167990	957.397010	12.246490
21.222275	954.297383	12.251495
20.867401	953.724772	12.256499
21.187928	953.905506	12.261504
20.978346	950.087830	12.266509
21.136788	951.844645	12.271514
21.213741	953.835241	12.276519
20.892007	956.040820	12.281523
21.466511	957.136734	12.286528
21.250363	948.478594	12.291533
20.948366	950.357731	12.296538
20.932268	955.309078	12.301543
20.914837	948.726170	12.306547
20.892405	948.486913	12.311552
20.749024	954.045219	12.316557
20.587528	955.009343	12.321562
21.164345	950.132639	12.326567
20.974293	953.695548	12.331571
21.198641	950.486793	12.336576
21.275554	963.628647	12.341581
21.092798	956.135341	12.346586
21.258994	958.468116	12.351591
21.002420	958.070649	12.356595
21.116206	947.385435	12.361600
21.003575	954.414945	12.366605
20.784572	959.942733	12.371610
20.923411	963.057353	12.376615
21.046217	958.421799	12.381619
21.054534	958.423656	12.386624
21.072085	962.918606	12.391629
21.064075	961.778135	12.396634
21.090604	953.902926	12.401639
21.132816	967.864071	12.406643
21.416966	956.613908	12.411648
20.972427	967.429214	12.416653
20.825026	963.057539	12.421658
21.366200	964.125651	12.426663
21.003639	960.411223	12.431667
21.400047	951.603344	12.436672
21.222180	937.935158	12.441677
21.281074	926.620014	12.446682
20.930552	931.776085	12.451687
20.834250	936.246605	12.456691
21.205794	928.141332	12.461696
20.922927	938.005111	12.466701
20.628060	943.869863	12.471706
20.725131	930.165721	12.476711
20.672644	938.494572	12.481715
20.990495	951.355125	12.486720
20.755242	965.483529	12.491725
21.320599	963.183957	12.496730
21.296620	954.197104	12.501735
21.108180	949.155428	12.506739
21.051018	930.060332	12.511744
20.881657	936.778743	12.516749
20.674159	943.361306	12.521754
20.959335	947.808837	12.526759
21.054989	959.667143	12.531763
20.953857	954.201510	12.536768
20.762535	954.760362	12.541773
21.280541	965.049970	12.546778
21.292674	955.573206	12.551783
21.005265	940.277636	12.556787
21.063138	939.134545	12.561792
20.725653	938.095512	12.566797
20.857435	935.882441	12.571802
21.380713	945.579806	12.576807
21.202571	943.419317	12.581811
21.363982	936.981365	12.586816
21.357408	943.523998	12.591821
21.535107	935.821818	12.596826
21.275086	939.414808	12.601831
20.875265	937.931529	12.606835
21.370115	934.014126	12.611840
21.099339	942.811479	12.616845
21.077845	931.293098	12.621850
21.151610	931.950026	12.626855
20.796364	933.175298	12.631859
20.853317	927.264971	12.636864
21.040771	934.358581	12.641869
21.054298	938.787929	12.646874
21.236762	932.493286	12.651879
21.090848	932.029283	12.656883
21.360511	921.779722	12.661888
21.044816	922.230668	12.666893
21.082568	921.997583	12.671898
21.060471	915.088988	12.676903
20.897472	920.795497	12.681907
20.873405	911.942732	12.686912
21.009923	916.108018	12.691917
20.825467	917.354937	12.696922
21.419195	907.807524	12.701927
20.841291	922.280710	12.706931
20.975124	920.657126	12.711936
20.646828	927.877146	12.716941
20.762702	920.189566	12.721946
20.879203	926.340381	12.726951
21.159081	941.280785	12.731955
21.100458	937.956305	12.736960
20.657061	928.556940	12.741965
20.956924	931.701069	12.746970
21.320819	935.183510	12.751975
21.144032	939.597478	12.756979
21.146548	917.580092	12.761984
20.746524	913.941041	12.766989
21.054983	923.778313	12.771994
20.928025	919.240956	12.776999
20.828237	924.063707	12.782003
21.139462	916.155728	12.787008
20.804093	924.233205	12.792013
20.797494	925.885444	12.797018
21.002256	937.562319	12.802023
20.840367	950.213940	12.807027
21.019741	948.598859	12.812032
21.085482	951.556392	12.817037
20.800506	957.222442	12.822042
20.843682	954.933608	12.827047
21.019116	955.591670	12.832051
21.003510	947.475589	12.837056
20.999410	951.502454	12.842061
20.932549	948.335412	12.847066
21.215217	955.350766	12.852071
21.065406	954.630325	12.857075
21.139347	959.952112	12.862080
21.229525	946.832559	12.867085
21.013796	944.935122	12.872090
20.923878	936.036071	12.877095
21.029678	948.542490	12.882099
21.088380	936.284298	12.887104
20.723990	939.039179	12.892109
20.874719	951.249836	12.897114
21.353971	951.247551	12.902119
20.741621	950.134077	12.907123
21.119163	950.192171	12.912128
21.021454	954.330165	12.917133
21.243683	945.704618	12.922138
21.394537	938.009873	12.927143
20.770099	936.724853	12.932147
21.080627	932.336926	12.937152
20.923094	928.528303	12.942157
20.636480	935.445196	12.947162
21.083131	919.521614	12.952167
20.889165	935.176284	12.957171
21.008539	933.277446	12.962176
21.182807	934.470308	12.967181
20.749312	938.412680	12.972186
21.145510	938.548227	12.977191
20.870810	938.503754	12.982195
21.175081	933.736759	12.987200
20.961664	933.266173	12.992205
20.855926	933.548009	12.997210
21.018086	934.600870	13.002215
21.085267	944.001948	13.007219
20.895613	940.800873	13.012224
20.919971	941.143966	13.017229
21.173861	947.397465	13.022234
21.015635	936.012856	13.027239
20.812248	943.760195	13.032243
21.175507	948.206312	13.037248
20.967839	942.721403	13.042253
20.633882	948.660203	13.047258
21.229797	956.748450	13.052263
20.647071	967.439131	13.057267
21.155143	964.435871	13.062272
21.002930	975.980465	13.067277
21.013468	971.384891	13.072282
21.208274	968.571950	13.077287
21.015449	961.547051	13.082291
21.035643	954.644309	13.087296
21.203804	949.069493	13.092301
20.928531	956.055554	13.097306
21.242013	945.959845	13.102311
20.857435	950.957343	13.107315
20.877606	949.019128	13.112320
20.977815	950.277423	13.117325
20.877520	946.010210	13.122330
21.287547	947.375219	13.127335
20.968990	944.768744	13.132339
21.051334	943.519242	13.137344
20.986560	950.747710	13.142349
20.839562	953.158822	13.147354
21.257524	942.502373	13.152359
21.127603	949.848470	13.157363
21.006008	951.973239	13.162368
20.859922	945.609559	13.167373
21.003480	955.129358	13.172378
21.383166	947.010160	13.177383
21.043216	949.705948	13.182387
20.959633	948.460831	13.187392
21.014399	952.025697	13.192397
21.192691	948.354330	13.197402
21.532586	943.837130	13.202407
21.199114	949.039376	13.207411
21.207513	946.451722	13.212416
21.331678	950.849235	13.217421
21.458352	944.052525	13.222426
21.070797	933.843115	13.227431
21.082382	927.659310	13.232435
21.048582	918.765514	13.237440
21.193190	918.069086	13.242445
20.940990	913.509125	13.247450
20.998246	916.999465	13.252455
21.037699	910.492662	13.257459
20.997675	906.099147	13.262464
21.097681	917.524617	13.267469
21.035983	910.232813	13.272474
20.982466	910.261879	13.277479
20.968255	913.588565	13.282483
21.013653	914.093890	13.287488
20.949434	909.388826	13.292493
20.765645	918.251144	13.297498
20.974198	909.397552	13.302503
20.631252	919.097426	13.307507
21.047937	912.837980	13.312512
20.882656	914.606994	13.317517
21.206645	915.703433	13.322522
21.095384	908.332797	13.327527
21.153357	924.292644	13.332531
20.835761	911.604030	13.337536
21.354701	916.782285	13.342541
20.686610	917.557531	13.347546
21.048317	909.565807	13.352551
20.967543	918.853264	13.357555
20.875602	910.553826	13.362560
21.019689	920.505625	13.367565
20.628742	925.295961	13.372570
21.001564	926.343610	13.377575
21.029908	939.133624	13.382579
21.074827	937.899554	13.387584
21.008978	930.736141	13.392589
20.809625	934.835144	13.397594
21.228134	936.905313	13.402599
20.817401	935.934735	13.407603
21.231856	924.428836	13.412608
20.908955	928.404032	13.417613
20.855294	929.885572	13.422618
21.406815	928.830917	13.427623
21.264890	937.112527	13.432627
21.215340	928.667538	13.437632
21.366523	921.704494	13.442637
21.088722	922.661933	13.447642
21.066593	925.660285	13.452647
20.942947	925.963901	13.457651
21.063709	919.496168	13.462656
20.799822	925.251887	13.467661
20.989474	925.317868	13.472666
20.977375	919.281355	13.477671
20.978640	927.502274	13.482675
21.206274	921.779204	13.487680
21.297637	924.119178	13.492685
21.366114	921.698574	13.497690
21.429396	917.290157	13.502695
20.981578	924.447232	13.507699
21.119010	927.227737	13.512704
21.182949	919.359196	13.517709
20.984862	914.147174	13.522714
20.972763	894.554480	13.527719
20.711254	901.636096	13.532723
20.850957	908.369860	13.537728
21.283612	921.048065	13.542733
20.851190	923.362760	13.547738
21.286515	919.672485	13.552743
21.041658	911.381664	13.557747
20.597338	905.846198	13.562752
20.980308	916.163616	13.567757
20.667375	921.058209	13.572762
21.064006	921.769305	13.577767
20.834333	931.140446	13.582771
21.019226	918.699709	13.587776
20.943846	929.672164	13.592781
21.076115	930.417538	13.597786
21.231370	918.519298	13.602791
21.047186	923.049564	13.607795
21.044549	926.092117	13.612800
21.063109	921.664022	13.617805
21.263044	928.332993	13.622810
20.961289	918.753341	13.627815
20.965337	916.596917	13.632819
20.909116	924.420127	13.637824
21.033602	928.331855	13.642829
20.937209	921.848290	13.647834
21.330999	926.866726	13.652839
20.894053	918.783165	13.657843
20.634230	909.755102	13.662848
21.068611	924.744968	13.667853
20.813001	931.514981	13.672858
21.167061	926.484567	13.677863
21.156670	935.112647	13.682867
20.897142	931.798132	13.687872
21.438573	932.476673	13.692877
20.908225	914.332322	13.697882
20.514978	909.052074	13.702887
20.602079	931.403738	13.707891
20.695919	932.453302	13.712896
20.829915	931.813762	13.717901
20.713653	939.416308	13.722906
21.096416	930.329904	13.727911
21.022159	932.208989	13.732915
21.066376	940.665929	13.737920
21.229828	931.135083	13.742925
21.224896	938.887039	13.747930
21.280865	930.770591	13.752935
20.978764	938.968933	13.757939
21.214211	939.893405	13.762944
21.264021	933.714541	13.767949
21.040849	939.395959	13.772954
21.133910	921.909150	13.777959
21.102479	913.123795	13.782963
20.515446	911.854890	13.787968
20.923466	918.724071	13.792973
21.096381	939.220083	13.797978
21.341599	927.805831	13.802983
20.847520	924.951372	13.807987
21.147615	917.885728	13.812992
21.023192	909.507888	13.817997
20.594209	911.544475	13.823002
21.139142	915.540538	13.828007
21.101930	937.695985	13.833011
20.740279	926.443181	13.838016
20.780277	930.201218	13.843021
21.194214	939.196888	13.848026
21.307559	929.180422	13.853031
20.872197	929.789233	13.858035
21.099207	926.244150	13.863040
20.944231	916.095435	13.868045
21.007754	924.878887	13.873050
21.142273	920.982684	13.878055
20.600375	921.572214	13.883059
20.884835	934.498005	13.888064
20.795621	933.157587	13.893069
20.863839	953.312329	13.898074
21.469694	938.946684	13.903079
20.929725	950.166726	13.908083
21.099685	941.866502	13.913088
21.229334	940.420211	13.918093
20.980949	930.079793	13.923098
20.884367	912.791984	13.928103
20.975733	922.520369	13.933107
20.804102	940.073387	13.938112
21.127964	935.199182	13.943117
20.997351	941.129204	13.948122
21.096673	941.267943	13.953127
21.020211	945.254304	13.958131
20.970841	941.466276	13.963136
21.038486	930.447792	13.968141
20.624928	931.294413	13.973146
20.943479	933.233858	13.978151
21.037734	938.585515	13.983155
20.726743	945.465297	13.988160
21.075236	943.939946	13.993165
21.273652	941.818754	13.998170
21.350016	941.003892	14.003175
20.935518	934.648330	14.008179
20.887095	934.353291	14.013184
21.366697	936.285976	14.018189
20.664047	931.517812	14.023207
20.723605	925.145501	14.028224
21.398521	942.737450	14.033242
21.277312	937.367660	14.038259
21.108123	928.485119	14.043277
20.810469	924.947723	14.048295
20.960293	925.625421	14.053312
20.995768	944.678439	14.058330
20.783365	938.582303	14.063347
21.339625	940.511794	14.068365
21.073302	944.817171	14.073383
20.899164	943.433978	14.078400
21.082959	946.725331	14.083418
20.849696	946.421218	14.088435
20.918504	943.242220	14.093453
20.830777	960.896048	14.098471
20.934630	943.952283	14.103488
21.015982	959.872422	14.108506
21.235763	966.412613	14.113523
21.599914	971.783051	14.118541
21.072355	982.239709	14.123559
21.326021	984.149826	14.128576
21.405666	979.301691	14.133594
21.501447	984.422354	14.138611
21.809596	986.141312	14.143629
21.465563	982.807925	14.148647
21.880624	977.420232	14.153664
21.309359	968.051237	14.158682
21.079996	963.066773	14.163699
21.554224	971.284121	14.168717
21.463829	985.605179	14.173735
21.743743	984.623045	14.178752
21.604808	992.590560	14.183770
21.838648	987.664346	14.188787
21.860788	990.045544	14.193805
21.524941	974.309164	14.198823
21.443130	954.727158	14.203840
21.423086	960.792792	14.208858
21.811012	981.766930	14.213875
21.835146	986.044871	14.218893
21.720266	980.919447	14.223911
21.768969	994.681929	14.228928
21.851002	987.443991	14.233946
21.538795	988.745938	14.238963
21.919824	985.753088	14.243981
21.684137	994.036481	14.248999
21.661584	984.235470	14.254016
21.882569	988.953922	14.259034
21.480596	995.967668	14.264051
21.788830	976.661624	14.269069
21.601213	995.698380	14.274087
21.903162	990.832089	14.279104
21.815555	984.947264	14.284122
21.836164	992.107542	14.289139
21.408031	990.818336	14.294157
21.521576	1007.129794	14.299175
21.927476	1008.248000	14.304192
22.102334	1015.248408	14.309210
21.855537	1030.531976	14.314227
22.027879	1014.302371	14.319245
22.077735	1025.086965	14.324263
22.451018	1016.624367	14.329280
22.664562	1020.327843	14.334298
22.157977	1005.144050	14.339315
22.411952	991.838283	14.344333
22.169830	991.433336	14.349351
22.192749	985.258751	14.354368
22.082537	990.269125	14.359386
21.928414	995.434367	14.364403
22.146336	987.584874	14.369421
22.179552	1001.456798	14.374439
22.423894	1000.288428	14.379456
22.468261	988.659902	14.384474
22.183506	995.076080	14.389491
22.397146	996.173039	14.394509
22.111206	1000.697065	14.399527
22.092091	1011.500514	14.404544
22.597306	1019.484859	14.409562
22.350098	1020.638016	14.414579
22.958577	1013.523743	14.419597
22.394314	1011.977821	14.424615
22.222493	1013.225920	14.429632
22.535072	1015.611137	14.434650
22.416363	1021.203322	14.439667
22.749741	1012.972032	14.444685
22.922802	1022.697207	14.449703
22.790042	1016.388562	14.454720
22.574757	996.215881	14.459738
22.301447	1002.499677	14.464755
22.592307	1004.603639	14.469773
22.447943	1024.481393	14.474791
22.409163	1015.911481	14.479808
22.617862	1023.266718	14.484826
22.742619	1021.363941	14.489843
22.770437	1020.060216	14.494861
22.920763	1022.438278	14.499879
22.963864	1022.563568	14.504896
22.877691	1016.963218	14.509914
22.693685	1023.152556	14.514931
22.838853	1013.678707	14.519949
22.915082	1020.152154	14.524967
22.496184	1022.075161	14.529984
22.750859	1015.084954	14.535002
22.864756	1022.260256	14.540019
22.838004	1013.905505	14.545037
22.632346	1016.022590	14.550055
22.519893	1015.823477	14.555072
22.875676	1011.752408	14.560090
22.899074	1007.311209	14.565107
22.769242	1015.005151	14.570125
22.729130	1008.452071	14.575143
23.134409	1033.872026	14.580160
23.653030	1019.092574	14.585178
23.479176	1017.272027	14.590195
23.348946	1015.733961	14.595213
23.394187	1010.158273	14.600231
23.186785	1014.916742	14.605248
23.396137	999.157876	14.610266
23.184125	1007.214131	14.615283
23.534942	1000.836234	14.620301
23.587415	1011.345123	14.625319
23.456647	1013.080603	14.630336
23.577953	1015.178575	14.635354
23.287047	1011.242105	14.640371
23.550365	1003.451430	14.645389
23.209286	1007.927623	14.650407
23.100753	1006.705420	14.655424
23.681446	999.902325	14.660442
23.503293	1013.200784	14.665459
23.307718	1013.560767	14.670477
23.372731	1000.152996	14.675495
23.492227	1001.305869	14.680512
23.527511	1016.961285	14.685530
23.185277	1004.749464	14.690547
23.201750	1018.175763	14.695565
23.517078	1012.711155	14.700583
23.058370	1023.322028	14.705600
23.187401	1006.337995	14.710618
23.328021	1016.047890	14.715635
23.397835	1012.576134	14.720653
23.326707	1022.286771	14.725671
23.563302	1034.087651	14.730688
23.474399	1036.311960	14.735706
23.530082	1046.875418	14.740723
23.815849	1046.866051	14.745741
24.114065	1041.515847	14.750759
23.859331	1046.692435	14.755776
24.101610	1033.904447	14.760794
23.594814	1037.471129	14.765811
23.658728	1036.792429	14.770829
23.956900	1037.655686	14.775847
23.854592	1038.063715	14.780864
23.975433	1042.095014	14.785882
23.621536	1042.634405	14.790899
23.940768	1039.860613	14.795917
23.997148	1041.992539	14.800935
23.889465	1048.086344	14.805952
23.985191	1047.147740	14.810970
24.018397	1048.743815	14.815987
23.821358	1043.944504	14.821005
24.336042	1037.592366	14.826023
24.064694	1054.419867	14.831040
24.039558	1046.072704	14.836058
23.986622	1045.428370	14.841075
24.093427	1039.997009	14.846093
24.355074	1044.573714	14.851111
23.961093	1048.072069	14.856128
24.342136	1046.298301	14.861146
23.969039	1040.279660	14.866163
23.753918	1044.440047	14.871181
24.256317	1049.324423	14.876199
24.007252	1050.828663	14.881216
24.298951	1046.748929	14.886234
24.006846	1039.710634	14.891251
24.216614	1045.450215	14.896269
24.190608	1045.797312	14.901287
24.163817	1038.729288	14.906304
24.650792	1051.006202	14.911322
24.427132	1050.894038	14.916339
24.338951	1040.960311	14.921357
24.486407	1050.148467	14.926375
24.050651	1051.791021	14.931392
24.156142	1054.495563	14.936410
24.397130	1075.623833	14.941427
24.466386	1066.851043	14.946445
24.528963	1076.803088	14.951463
24.667971	1066.831536	14.956480
24.653790	1076.305038	14.961498
24.852974	1067.351077	14.966515
24.424791	1068.581864	14.971533
24.947601	1065.899869	14.976551
25.051396	1068.717943	14.981568
25.238799	1061.634623	14.986586
25.126046	1063.115551	14.991603
24.712567	1051.899769	14.996621
25.088368	1042.091816	15.001639
24.129885	1042.880213	15.006656
24.566437	1050.425641	15.011674
24.924954	1060.657666	15.016691
24.641409	1071.379064	15.021709
24.836850	1064.409292	15.026727
24.785530	1069.919962	15.031744
24.566512	1067.691333	15.036762
24.660307	1073.366050	15.041779
24.997375	1073.074794	15.046797
25.079715	1067.834515	15.051815
24.702350	1075.654484	15.056832
24.716513	1065.539249	15.061850
24.854793	1071.420803	15.066867
24.936505	1078.195424	15.071885
25.112711	1073.325565	15.076903
24.976758	1093.979148	15.081920
25.318967	1092.044827	15.086938
25.204425	1088.860432	15.091955
25.212932	1099.607632	15.096973
25.885413	1087.734132	15.101991
25.109472	1082.371181	15.107008
25.441822	1067.102288	15.112026
25.317111	1060.888295	15.117043
24.924827	1067.955585	15.122061
25.056797	1064.961542	15.127079
25.252069	1084.061617	15.132096
25.271895	1091.179596	15.137114
25.627748	1094.388486	15.142131
25.402497	1091.767589	15.147149
25.722941	1083.475402	15.152167
25.241977	1076.166761	15.157184
25.748771	1065.796778	15.162202
25.630080	1059.064299	15.167219
25.519693	1066.794493	15.172237
25.306752	1061.502208	15.177255
25.424813	1064.830813	15.182272
25.771299	1077.315774	15.187290
25.581778	1079.560856	15.192307
25.395752	1074.053488	15.197325
26.065135	1074.251928	15.202343
25.774139	1075.361735	15.207360
25.478089	1068.147876	15.212378
25.839662	1059.002854	15.217395
25.607711	1071.449500	15.222413
25.992667	1064.984333	15.227431
25.618527	1066.684702	15.232448
25.954670	1065.339664	15.237466
26.019320	1073.381720	15.242483
25.706904	1061.462397	15.247501
25.975586	1057.844083	15.252519
25.609413	1059.766550	15.257536
25.647420	1071.298684	15.262554
26.188240	1084.359847	15.267571
26.290828	1098.842147	15.272589
26.008440	1090.595762	15.277607
26.081679	1080.705476	15.282624
25.950102	1072.600217	15.287642
26.243869	1075.229119	15.292659
25.885004	1075.910875	15.297677
26.200114	1067.098875	15.302695
25.787310	1076.982018	15.307712
26.255279	1083.644702	15.312730
26.443070	1088.269380	15.317747
26.154413	1089.520388	15.322765
26.437473	1092.391674	15.327783
26.086218	1084.002119	15.332800
26.243884	1088.787332	15.337818
26.517947	1089.309944	15.342835
26.258668	1082.927066	15.347853
26.519521	1085.026388	15.352871
26.225347	1077.428406	15.357888
26.217844	1081.700409	15.362906
26.442140	1081.412981	15.367923
26.065499	1083.214425	15.372941
26.337189	1082.414496	15.377959
26.433155	1094.637404	15.382976
26.443535	1093.940497	15.387994
26.771020	1089.737067	15.393011
26.649056	1100.254964	15.398029
26.377071	1092.225570	15.403047
26.566128	1098.619711	15.408064
26.530493	1098.804749	15.413082
26.709560	1090.832408	15.418099
26.595173	1100.933817	15.423117
26.796679	1100.758563	15.428135
26.207137	1111.675084	15.433152
26.575855	1095.395193	15.438170
26.490678	1099.346107	15.443187
26.239642	1101.371340	15.448205
26.586302	1090.238790	15.453223
26.661582	1093.239169	15.458240
26.596524	1110.960350	15.463258
27.024471	1118.033703	15.468275
26.674208	1119.201730	15.473293
26.861425	1123.466286	15.478311
27.027151	1123.416289	15.483328
26.975556	1117.052184	15.488346
27.397792	1109.423298	15.493363
26.996966	1115.903659	15.498381
26.995298	1108.875639	15.503399
26.999142	1110.707640	15.508416
26.839901	1115.013291	15.513434
27.130100	1110.757599	15.518451
27.343967	1115.211386	15.523469
27.114079	1107.318416	15.528487
27.305919	1111.956613	15.533504
27.268658	1113.375170	15.538522
27.484468	1107.509545	15.543539
27.328620	1094.380731	15.548557
26.907241	1092.665719	15.553575
27.088578	1102.152100	15.558592
26.994349	1113.672324	15.563610
27.615607	1121.647658	15.568627
27.341229	1113.552566	15.573645
27.652284	1112.118717	15.578663
27.631949	1114.936147	15.583680
27.264437	1115.192992	15.588698
27.749988	1105.059179	15.593715
27.445517	1120.433837	15.598733
27.326414	1114.322746	15.603751
27.686088	1117.897549	15.608768
27.463603	1122.142503	15.613786
27.828781	1110.001815	15.618803
27.541516	1107.911479	15.623821
27.726237	1111.043846	15.628839
27.633955	1115.923987	15.633856
27.362359	1117.136097	15.638874
27.455286	1108.150294	15.643891
27.346699	1109.462248	15.648909
27.656176	1109.189549	15.653927
28.040216	1105.349904	15.658944
27.656996	1110.965432	15.663962
27.767493	1103.631661	15.668979
27.446143	1110.160692	15.673997
27.605401	1110.077120	15.679015
27.712827	1108.625410	15.684032
27.888847	1112.647929	15.689050
27.681874	1109.371304	15.694067
27.511715	1126.530391	15.699085
27.865093	1132.269125	15.704103
28.418030	1134.361197	15.709120
28.077590	1147.684089	15.714138
28.088089	1138.203322	15.719155
28.263293	1148.379702	15.724173
28.197861	1129.789006	15.729191
28.319945	1131.943501	15.734208
27.948388	1118.657157	15.739226
28.245892	1118.089064	15.744243
28.208250	1129.918029	15.749261
28.197196	1133.424546	15.754279
28.219449	1136.865976	15.759296
27.998877	1136.982981	15.764314
28.486991	1137.721570	15.769331
28.266425	1142.744876	15.774349
28.471252	1142.458980	15.779367
28.489066	1147.710114	15.784384
28.505959	1139.603161	15.789402
28.693331	1137.492179	15.794419
28.706063	1133.231969	15.799437
28.448679	1121.513033	15.804455
28.488312	1112.144041	15.809472
28.425402	1109.399722	15.814490
28.420379	1119.747971	15.819507
28.468282	1135.955211	15.824525
28.655358	1134.292593	15.829543
28.886559	1141.988798	15.834560
28.455544	1142.573524	15.839578
28.767084	1139.178018	15.844595
28.478770	1148.508096	15.849613
28.564441	1135.765445	15.854631
28.973606	1130.738863	15.859648
28.453089	1137.858098	15.864666
28.713414	1133.386939	15.869683
28.636772	1133.010652	15.874701
28.487989	1142.365664	15.879719
28.778888	1146.888973	15.884736
28.292176	1147.042131	15.889754
28.816987	1140.123614	15.894771
28.938373	1151.941392	15.899789
29.035596	1162.262354	15.904807
29.175997	1155.103114	15.909824
29.100896	1160.995140	15.914842
29.180278	1147.946739	15.919859
29.022235	1144.287920	15.924877
29.121681	1151.240647	15.929895
29.270169	1152.727111	15.934912
29.207143	1162.450707	15.939930
29.426860	1154.358590	15.944947
29.226404	1132.597730	15.949965
29.026292	1142.278681	15.954983
29.428435	1145.436156	15.960000
29.546667	1138.676865	15.965018
29.295282	1132.616751	15.970035
29.557276	1129.307801	15.975053
29.364514	1122.934745	15.980071
29.467615	1123.119680	15.985088
29.263453	1125.414295	15.990106
29.370118	1117.741352	15.995123
29.530413	1129.612682	16.000141
29.013571	1125.013786	16.005159
29.815607	1140.605253	16.010176
29.496115	1161.521014	16.015194
29.722893	1164.857473	16.020211
29.679720	1167.857882	16.025229
29.546831	1158.046036	16.030247
30.003612	1162.012780	16.035264
29.387997	1152.175678	16.040282
29.477543	1155.689751	16.045299
30.049983	1156.517140	16.050317
29.845336	1164.462195	16.055335
29.724177	1165.151662	16.060352
29.436523	1153.808765	16.065370
29.756950	1156.620622	16.070387
29.644316	1159.146038	16.075405
29.629700	1159.444130	16.080423
29.741475	1163.697135	16.085440
29.574738	1162.145998	16.090458
29.683613	1168.334305	16.095475
29.727343	1168.739496	16.100493
29.692062	1174.532368	16.105511
30.196742	1185.829716	16.110528
30.189608	1190.771809	16.115546
30.259515	1185.934596	16.120563
30.258812	1199.573017	16.125581
30.167591	1202.843795	16.130599
30.411916	1189.430847	16.135616
30.322781	1172.330402	16.140634
30.234000	1175.591347	16.145651
30.283212	1171.377217	16.150669
30.146622	1168.402389	16.155687
30.541088	1179.509669	16.160704
30.709475	1181.581280	16.165722
30.024143	1172.880007	16.170739
30.345633	1171.626961	16.175757
30.569169	1186.023992	16.180775
30.690393	1174.732274	16.185792
30.199254	1175.436703	16.190810
30.492756	1187.087059	16.195827
30.326212	1185.241730	16.200845
30.327443	1184.884482	16.205863
30.668156	1186.467710	16.210880
30.634949	1189.118893	16.215898
30.817429	1189.506676	16.220915
30.861379	1188.348229	16.225933
30.570287	1184.669719	16.230951
31.022729	1185.380966	16.235968
31.077301	1184.110713	16.240986
31.223061	1183.587269	16.246003
30.877688	1166.266572	16.251021
30.508189	1159.685731	16.256039
30.974479	1164.000175	16.261056
31.014201	1174.166719	16.266074
30.888538	1166.927209	16.271091
31.054732	1171.092885	16.276109
30.474408	1175.388631	16.281127
31.040407	1177.376380	16.286144
31.088969	1182.751612	16.291162
31.048208	1188.243339	16.296179
31.120617	1182.073361	16.301197
31.043744	1186.960507	16.306215
31.153457	1178.360525	16.311232
30.910220	1183.307236	16.316250
31.049757	1182.377366	16.321267
31.171501	1176.446491	16.326285
31.030474	1190.027057	16.331303
31.232695	1181.402881	16.336320
30.985230	1182.921036	16.341338
30.980658	1191.358019	16.346355
31.553117	1184.788963	16.351373
30.978576	1185.237703	16.356391
31.366261	1178.347330	16.361408
31.461953	1197.137816	16.366426
31.312217	1212.849694	16.371443
31.485471	1211.236463	16.376461
31.427391	1224.528550	16.381479
31.848166	1214.217800	16.386496
31.718268	1218.311160	16.391514
31.775351	1213.235308	16.396531
31.838297	1211.570455	16.401549
31.745975	1210.361380	16.406567
31.690249	1194.271768	16.411584
31.467375	1197.867138	16.416602
31.459127	1213.101841	16.421619
31.609580	1212.845065	16.426637
31.729929	1220.091797	16.431655
31.815951	1214.194918	16.436672
31.837232	1220.340587	16.441690
31.883268	1214.793009	16.446707
32.100360	1213.142899	16.451725
31.874082	1212.060581	16.456743
32.161992	1212.518068	16.461760
32.122645	1217.095641	16.466778
31.902465	1216.608535	16.471795
31.981335	1203.108702	16.476813
31.859700	1220.497690	16.481831
32.103340	1209.356311	16.486848
32.174227	1216.557446	16.491866
31.921500	1208.836378	16.496883
32.033528	1211.480132	16.501901
31.965033	1215.966398	16.506919
32.069629	1229.871203	16.511936
32.296122	1231.187931	16.516954
32.234897	1239.409031	16.521971
32.563969	1235.280813	16.526989
32.270020	1243.301501	16.532007
32.528192	1245.792964	16.537024
32.525381	1230.662297	16.542042
32.714405	1238.349550	16.547059
32.931469	1233.054691	16.552077
32.524747	1222.627366	16.557095
32.432797	1204.872945	16.562112
32.643215	1194.896209	16.567130
32.638287	1217.394701	16.572147
32.688482	1215.381092	16.577165
32.576295	1228.288551	16.582183
33.061261	1220.298815	16.587200
32.643849	1217.463145	16.592218
32.400020	1220.843210	16.597235
32.953609	1234.270566	16.602253
32.543653	1229.972345	16.607271
32.866947	1234.599056	16.612288
32.707927	1232.412742	16.617306
32.795075	1240.792654	16.622323
32.911457	1231.924158	16.627341
32.603031	1240.979072	16.632359
32.713819	1231.980905	16.637376
32.972439	1231.335639	16.642394
32.437331	1250.703430	16.647411
33.082518	1243.361394	16.652429
33.273365	1260.579469	16.657447
33.252705	1261.429094	16.662464
33.034259	1241.102416	16.667482
33.144040	1254.528211	16.672499
33.447208	1258.917463	16.677517
33.449125	1267.356601	16.682535
33.246985	1264.120070	16.687552
33.248753	1253.114761	16.692570
33.305425	1269.563002	16.697587
33.366215	1265.018231	16.702605
33.632825	1265.792154	16.707623
33.515945	1271.056948	16.712640
33.596481	1263.639784	16.717658
33.543356	1270.653081	16.722675
33.603561	1262.078248	16.727693
33.462538	1271.960650	16.732711
33.405743	1266.094392	16.737728
33.560800	1261.322227	16.742746
33.500324	1265.950377	16.747763
33.768562	1261.798819	16.752781
33.607452	1272.612525	16.757799
33.484301	1265.251440	16.762816
33.799020	1258.287722	16.767834
33.222583	1267.740905	16.772851
33.647553	1259.688356	16.777869
33.563407	1270.675405	16.782887
33.725664	1284.498706	16.787904
34.137749	1291.053994	16.792922
33.933511	1298.369835	16.797939
34.197026	1290.313130	16.802957
34.185887	1275.507794	16.807975
34.135168	1280.102931	16.812992
34.171721	1265.568429	16.818010
33.938336	1274.018356	16.823027
34.192679	1272.481850	16.828045
34.058057	1276.354180	16.833063
34.074653	1289.596663	16.838080
34.243401	1297.276170	16.843098
33.962401	1300.423077	16.848115
34.096991	1288.553401	16.853133
34.227587	1295.030886	16.858151
34.537894	1302.129385	16.863168
34.280359	1288.162443	16.868186
34.474810	1296.235832	16.873203
34.366921	1296.482734	16.878221
34.527987	1305.966190	16.883239
34.501229	1304.990474	16.888256
34.797732	1293.667564	16.893274
34.702935	1301.123257	16.898291
34.538047	1293.071951	16.903309
34.564520	1288.892876	16.908327
34.543110	1288.419684	16.913344
34.475677	1291.294998	16.918362
34.238274	1293.539883	16.923379
34.433969	1287.435144	16.928397
34.723658	1303.646484	16.933415
34.959035	1308.719830	16.938432
35.360262	1312.063109	16.943450
34.748199	1311.558271	16.948467
35.128081	1305.444600	16.953485
34.742571	1305.893083	16.958503
35.050932	1306.108208	16.963520
35.129385	1315.372033	16.968538
35.015625	1318.366427	16.973555
35.337926	1315.901987	16.978573
35.259032	1318.930148	16.983591
34.972904	1318.779177	16.988608
35.261795	1312.845185	16.993626
35.117891	1328.318725	16.998643
35.279783	1311.966184	17.003661
35.519878	1317.268447	17.008679
35.176156	1322.014148	17.013696
35.521230	1317.008736	17.018714
35.226453	1328.732577	17.023731
35.479409	1320.696416	17.028749
35.493824	1312.657403	17.033767
35.155720	1316.268033	17.038784
35.461162	1322.137188	17.043802
35.346177	1320.840480	17.048819
35.259098	1315.370723	17.053837
35.196852	1322.679661	17.058855
34.955340	1331.148221	17.063872
35.338603	1326.059635	17.068890
35.110424	1348.748095	17.073907
35.575838	1343.350666	17.078925
35.663496	1336.209188	17.083943
35.610019	1347.441520	17.088960
35.940210	1331.795161	17.093978
35.664195	1339.677758	17.098995
35.730311	1344.276306	17.104013
36.317542	1338.714730	17.109031
35.819617	1344.751343	17.114048
36.024369	1344.597593	17.119066
35.850309	1349.212423	17.124083
36.302867	1337.482338	17.129101
36.030261	1340.198469	17.134119
35.608977	1349.361113	17.139136
36.314334	1339.387144	17.144154
36.224239	1344.633535	17.149171
36.194827	1336.615657	17.154189
36.072310	1335.666221	17.159207
36.090427	1342.916734	17.164224
36.319516	1363.668216	17.169242
36.260422	1371.118251	17.174259
36.220169	1370.920202	17.179277
36.233402	1368.360322	17.184295
36.079614	1379.139905	17.189312
36.669483	1372.042587	17.194330
36.739282	1369.832344	17.199347
36.434046	1371.583106	17.204365
36.816362	1374.081535	17.209383
36.815592	1368.151244	17.214400
36.964672	1363.837760	17.219418
37.220996	1372.831003	17.224435
36.773632	1358.806176	17.229453
36.940736	1357.915945	17.234471
36.590390	1354.253134	17.239488
36.715523	1354.258376	17.244506
36.779427	1359.750779	17.249523
36.551146	1366.608008	17.254541
37.120511	1356.158628	17.259559
36.822461	1369.147764	17.264576
36.981801	1361.581126	17.269594
37.034996	1356.254154	17.274611
36.731183	1366.911359	17.279629
36.909593	1356.267920	17.284647
36.862964	1365.729482	17.289664
36.929102	1356.772966	17.294682
36.974420	1367.067744	17.299699
36.739042	1372.384507	17.304717
37.398887	1383.432318	17.309735
37.615266	1392.711950	17.314752
37.402399	1388.506520	17.319770
37.508353	1396.672732	17.324787
37.508103	1387.497118	17.329805
37.675064	1363.467161	17.334823
37.334869	1376.384372	17.339840
37.060976	1367.522978	17.344858
37.496826	1377.426711	17.349875
37.385279	1393.046173	17.354893
37.422676	1396.903685	17.359911
37.186705	1403.117201	17.364928
37.442845	1396.408158	17.369946
37.719996	1392.288177	17.374963
37.574443	1402.880842	17.379981
37.677598	1395.618883	17.384999
37.417250	1401.885051	17.390016
37.487976	1382.289151	17.395034
37.884079	1392.178784	17.400051
37.837482	1394.215498	17.405069
38.254242	1394.937167	17.410087
38.269519	1394.198566	17.415104
38.017245	1396.835958	17.420122
38.090834	1385.196162	17.425139
38.002079	1393.328929	17.430157
38.186476	1384.680733	17.435175
38.410020	1386.792343	17.440192
37.997049	1385.807427	17.445210
38.331423	1384.731639	17.450227
38.036837	1401.074023	17.455245
38.426851	1378.392766	17.460263
38.180644	1391.507364	17.465280
38.520666	1391.709576	17.470298
38.491886	1390.108097	17.475315
38.120841	1393.212753	17.480333
38.877163	1390.867851	17.485351
38.359980	1402.710593	17.490368
38.641524	1396.854819	17.495386
38.803097	1403.119768	17.500403
38.462406	1393.425848	17.505421
38.958972	1398.627463	17.510439
38.508678	1392.721660	17.515456
38.579505	1407.394956	17.520474
38.714904	1412.748559	17.525491
39.038253	1417.313971	17.530509
39.167945	1406.727031	17.535527
38.915604	1392.252633	17.540544
38.785971	1388.557759	17.545562
38.539956	1380.481589	17.550579
38.700344	1403.293786	17.555597
39.031394	1402.339653	17.560615
38.640341	1413.629019	17.565632
38.958089	1413.158365	17.570650
39.025659	1411.868715	17.575667
39.104803	1406.565902	17.580685
39.262743	1407.270645	17.585703
38.980265	1418.788098	17.590720
39.186980	1414.437092	17.595738
39.265296	1409.159579	17.600755
39.079214	1413.541959	17.605773
39.154758	1407.547570	17.610791
39.419705	1417.005093	17.615808
39.412638	1418.157735	17.620826
39.366596	1414.435366	17.625843
39.509871	1429.984341	17.630861
39.993781	1421.175096	17.635879
39.806177	1409.421202	17.640896
39.764935	1403.343190	17.645914
39.662686	1397.496713	17.650931
39.512093	1407.118030	17.655949
39.672692	1391.501800	17.660967
39.442723	1410.744058	17.665984
39.751798	1402.518000	17.671002
39.875377	1415.946463	17.676019
39.587547	1428.194680	17.681037
40.067550	1421.618243	17.686055
40.012096	1427.238249	17.691072
40.059457	1434.440097	17.696090
40.275926	1420.230688	17.701107
39.992496	1413.516451	17.706125
39.977415	1423.122460	17.711143
39.833849	1422.096149	17.716160
40.057255	1430.569274	17.721178
40.301906	1421.606272	17.726195
39.991209	1436.535504	17.731213
39.986931	1424.856183	17.736231
40.252558	1425.910278	17.741248
40.146204	1433.658900	17.746266
40.371813	1426.501669	17.751283
40.026941	1432.970098	17.756301
40.231660	1434.106269	17.761319
40.275142	1432.431911	17.766336
40.520625	1445.567246	17.771354
40.780256	1453.248072	17.776371
40.370565	1444.823579	17.781389
40.783278	1452.917304	17.786407
41.009847	1451.682521	17.791424
40.738538	1448.730692	17.796442
40.986960	1425.450581	17.801459
40.537671	1425.386979	17.806477
40.650277	1438.230458	17.811495
40.657602	1440.934999	17.816512
40.751899	1463.079837	17.821530
41.053707	1444.969734	17.826547
40.789370	1459.729569	17.831565
41.052756	1455.575586	17.836583
40.611258	1452.312688	17.841600
40.346605	1463.865087	17.846618
41.083355	1446.934636	17.851635
40.824036	1462.697293	17.856653
41.105835	1461.379767	17.861671
41.128404	1484.016649	17.866688
41.358608	1489.569886	17.871706
41.400878	1481.127563	17.876723
41.329976	1495.399608	17.881741
41.798538	1484.037313	17.886759
41.725058	1483.775346	17.891776
41.388023	1467.300059	17.896794
41.654699	1458.163630	17.901811
41.454733	1450.383680	17.906829
41.336757	1456.068725	17.911847
41.626032	1469.244290	17.916864
41.535232	1478.012165	17.921882
41.660486	1479.070561	17.926899
41.593183	1495.266688	17.931917
41.705704	1484.881423	17.936935
41.605953	1488.771056	17.941952
41.729081	1480.757086	17.946970
41.807457	1479.078731	17.951987
41.709657	1481.241603	17.957005
41.908089	1489.447391	17.962023
41.941118	1493.776761	17.967040
41.983101	1485.768650	17.972058
42.182446	1476.609913	17.977075
42.121238	1486.029046	17.982093
42.018521	1480.888919	17.987111
42.165596	1474.703765	17.992128
41.916389	1491.124744	17.997146
42.074951	1473.681624	18.002163
42.236713	1489.500643	18.007181
42.003981	1498.170825	18.012199
42.357867	1509.346182	18.017216
42.247970	1502.790637	18.022234
42.268484	1507.641123	18.027251
42.623987	1507.762214	18.032269
42.376867	1512.413129	18.037287
42.562176	1498.704133	18.042304
42.495233	1506.976634	18.047322
42.829367	1505.052989	18.052339
42.832420	1503.165626	18.057357
42.615700	1507.243811	18.062375
42.881666	1505.333396	18.067392
42.374288	1524.426556	18.072410
42.833389	1500.356862	18.077427
42.784259	1511.147380	18.082445
42.402667	1520.378521	18.087463
42.804633	1520.177587	18.092480
42.640252	1542.078285	18.097498
43.064859	1538.310714	18.102515
42.815267	1545.476603	18.107533
42.916760	1533.361100	18.112551
43.173997	1529.925401	18.117568
43.088045	1544.870026	18.122586
43.447336	1533.106680	18.127603
43.391886	1542.407736	18.132621
43.149163	1535.476944	18.137639
43.377420	1539.067307	18.142656
43.223487	1541.449146	18.147674
43.225484	1536.243535	18.152691
43.425407	1544.652830	18.157709
43.288055	1558.793956	18.162727
43.984842	1554.490600	18.167744
43.887866	1562.778934	18.172762
43.902823	1542.855860	18.177779
43.870998	1534.802075	18.182797
43.584004	1526.099981	18.187815
43.695665	1537.920411	18.192832
43.262181	1545.860480	18.197850
43.729341	1551.386176	18.202867
43.916295	1557.316011	18.207885
44.203141	1565.573810	18.212903
44.058032	1555.813982	18.217920
44.086948	1560.228188	18.222938
44.141643	1562.468216	18.227955
44.150447	1556.784868	18.232973
44.289042	1568.368998	18.237991
44.327354	1559.777818	18.243008
44.371823	1554.151707	18.248026
44.360156	1541.372313	18.253043
43.943958	1540.330482	18.258061
43.703855	1541.723225	18.263079
44.103648	1549.738053	18.268096
44.144666	1564.093780	18.273114
44.423644	1551.079256	18.278131
44.331412	1558.326238	18.283149
44.058033	1558.500432	18.288167
44.587892	1569.843620	18.293184
44.662059	1584.380491	18.298202
44.875602	1578.304247	18.303219
44.610000	1580.217032	18.308237
44.761941	1580.187324	18.313255
45.067411	1573.752702	18.318272
45.045994	1590.499275	18.323290
44.987008	1583.027904	18.328307
45.097517	1567.089127	18.333325
44.710863	1554.475707	18.338343
44.978137	1566.571016	18.343360
44.692166	1585.821649	18.348378
45.043435	1581.303604	18.353395
45.186484	1582.451982	18.358413
44.872688	1584.847524	18.363431
45.336837	1580.191136	18.368448
45.255042	1586.376209	18.373466
45.102810	1581.259674	18.378483
45.184754	1590.159736	18.383501
45.197611	1589.401847	18.388519
45.586932	1594.848735	18.393536
45.325424	1588.097099	18.398554
45.271471	1585.293056	18.403571
45.504869	1597.082322	18.408589
45.546206	1588.825710	18.413607
45.518865	1588.730209	18.418624
45.780920	1613.654121	18.423642
45.781650	1615.286899	18.428659
45.751286	1622.231452	18.433677
45.799172	1615.116630	18.438695
45.894371	1616.230168	18.443712
45.826023	1621.712301	18.448730
45.862526	1619.550590	18.453747
45.676515	1611.516633	18.458765
45.788315	1612.065931	18.463783
45.887722	1610.490391	18.468800
45.912194	1608.116661	18.473818
45.969587	1613.645593	18.478835
46.078132	1608.061941	18.483853
45.993203	1611.618895	18.488871
46.234991	1608.238339	18.493888
45.918598	1607.188452	18.498906
46.191635	1619.164118	18.503923
46.663169	1641.437837	18.508941
46.576536	1636.510604	18.513959
46.740263	1630.920502	18.518976
46.263514	1620.796650	18.523994
46.539595	1639.225446	18.529011
46.646422	1639.932848	18.534029
46.536451	1647.007303	18.539047
46.751610	1638.486192	18.544064
46.738266	1639.314222	18.549082
46.910690	1641.447394	18.554099
46.997712	1635.279614	18.559117
47.045230	1637.330455	18.564135
47.262973	1621.206983	18.569152
46.965875	1632.720643	18.574170
47.025984	1642.740326	18.579187
47.223485	1631.468339	18.584205
47.189323	1642.936929	18.589223
47.144575	1636.020921	18.594240
46.937622	1633.895675	18.599258
46.774679	1631.481041	18.604275
46.998706	1634.113304	18.609293
47.089751	1635.373803	18.614311
47.373985	1626.699318	18.619328
47.220942	1627.724240	18.624346
47.439713	1645.698909	18.629363
47.443365	1630.609269	18.634381
47.115942	1636.432397	18.639399
47.399226	1637.803030	18.644416
47.475356	1653.056986	18.649434
47.616549	1664.398523	18.654451
47.803817	1660.026950	18.659469
47.582222	1671.479047	18.664487
47.946414	1667.061952	18.669504
47.645761	1661.829053	18.674522
47.507804	1670.733558	18.679539
47.797673	1659.669411	18.684557
47.354231	1653.170138	18.689575
47.709792	1658.141854	18.694592
47.917367	1683.245255	18.699610
48.119864	1680.388497	18.704627
48.269436	1680.264782	18.709645
48.243818	1680.016415	18.714663
48.442451	1689.162208	18.719680
48.121164	1684.455647	18.724698
48.573537	1685.362785	18.729715
48.879802	1686.344351	18.734733
48.167780	1687.202792	18.739751
48.680182	1678.302331	18.744768
48.561939	1695.449088	18.749786
48.513878	1680.026281	18.754803
48.619530	1686.205886	18.759821
48.536029	1698.662426	18.764839
48.649202	1679.920628	18.769856
48.764466	1683.831082	18.774874
48.766189	1688.877328	18.779891
48.906086	1693.579057	18.784909
48.818586	1678.897964	18.789927
48.805868	1688.612315	18.794944
49.000806	1682.456407	18.799962
48.739523	1688.878582	18.804979
48.999924	1683.123599	18.809997
48.732605	1701.149114	18.815015
49.037866	1682.751076	18.820032
49.087731	1693.540099	18.825050
48.692844	1689.693172	18.830067
49.246849	1697.677984	18.835085
49.452141	1700.424150	18.840103
49.485708	1705.171155	18.845120
49.541897	1697.773384	18.850138
49.378931	1717.518190	18.855155
49.478583	1700.822764	18.860173
49.365429	1706.570062	18.865191
49.451931	1706.110323	18.870208
49.775739	1711.251511	18.875226
49.726474	1703.798978	18.880243
49.957176	1711.079483	18.885261
49.866651	1708.357544	18.890279
49.756164	1705.145623	18.895296
49.649944	1707.762136	18.900314
49.774546	1697.525025	18.905331
50.016892	1699.457497	18.910349
50.089880	1708.409398	18.915367
50.037260	1702.352740	18.920384
49.656267	1706.957422	18.925402
49.520465	1713.822088	18.930419
49.991841	1721.599856	18.935437
50.026129	1727.713777	18.940455
50.107411	1735.164422	18.945472
50.220033	1735.702582	18.950490
50.363971	1728.135851	18.955507
50.600699	1723.828734	18.960525
50.332951	1736.351657	18.965543
50.009813	1738.130485	18.970560
50.494427	1735.689645	18.975578
50.582068	1761.782912	18.980595
50.628813	1761.318500	18.985613
50.888594	1765.113902	18.990631
50.643865	1758.742560	18.995648
51.061438	1752.146044	19.000666
50.890077	1763.706612	19.005683
51.134653	1763.493809	19.010701
51.021956	1762.397267	19.015719
50.864317	1761.773530	19.020736
51.252558	1756.588045	19.025754
50.970061	1766.867742	19.030771
50.873228	1758.948476	19.035789
50.934784	1770.467972	19.040807
50.851047	1751.313082	19.045824
50.924050	1762.701751	19.050842
51.091248	1754.318789	19.055859
51.474798	1768.537505	19.060877
51.366034	1779.924500	19.065895
51.627346	1777.714329	19.070912
51.739937	1780.761601	19.075930
51.377038	1780.073851	19.080947
51.763892	1792.975374	19.085965
51.589007	1792.661142	19.090983
51.664536	1787.929019	19.096000
51.807843	1785.009318	19.101018
51.336631	1792.286965	19.106035
51.847503	1768.509824	19.111053
51.910406	1782.907897	19.116071
52.083026	1784.755541	19.121088
52.032493	1781.681913	19.126106
51.904782	1779.973466	19.131123
52.092984	1785.261368	19.136141
51.648969	1778.377504	19.141159
52.279338	1793.627381	19.146176
52.494084	1782.057570	19.151194
52.037955	1792.298118	19.156211
52.269927	1802.579169	19.161229
52.490757	1802.693427	19.166247
52.262536	1822.943525	19.171264
52.794835	1807.281731	19.176282
52.468067	1804.714646	19.181299
53.022023	1786.977636	19.186317
52.913938	1801.022303	19.191335
53.102556	1788.467169	19.196352
53.378696	1774.862198	19.201370
52.808143	1780.190086	19.206387
53.194985	1758.689361	19.211405
53.166460	1760.385813	19.216423
52.913522	1759.069378	19.221440
53.002527	1746.213185	19.226458
52.948652	1756.811150	19.231475
52.911644	1757.836452	19.236493
53.114915	1768.571964	19.241511
53.113402	1779.749936	19.246528
53.208071	1784.134061	19.251546
53.165800	1793.132712	19.256563
53.390981	1782.966807	19.261581
53.459557	1780.164424	19.266599
53.509023	1790.331419	19.271616
53.743455	1780.905761	19.276634
53.447701	1794.049071	19.281651
53.706398	1787.201010	19.286669
53.667740	1793.185012	19.291687
53.506600	1790.484544	19.296704
53.647723	1789.647198	19.301722
53.301077	1790.146125	19.306739
53.386127	1793.119922	19.311757
53.862298	1792.424210	19.316775
53.646161	1795.591552	19.321792
53.809010	1804.869761	19.326810
53.952714	1824.712892	19.331827
53.778303	1826.135298	19.336845
53.897074	1823.509742	19.341863
54.157551	1822.573132	19.346880
53.887494	1823.830670	19.351898
53.663027	1821.177263	19.356915
54.093681	1824.283152	19.361933
54.332338	1834.276067	19.366951
54.446663	1840.846060	19.371968
54.808376	1831.606936	19.376986
54.507257	1850.417502	19.382003
54.502223	1847.259522	19.387021
54.835185	1843.467949	19.392039
54.692013	1839.360603	19.397056
54.844122	1842.780705	19.402074
54.779769	1840.974052	19.407091
54.907412	1843.349577	19.412109
55.077616	1842.716028	19.417127
54.841305	1835.872948	19.422144
55.134571	1843.047583	19.427162
55.006230	1829.993157	19.432179
55.069627	1833.808884	19.437197
55.222352	1843.674716	19.442215
55.193498	1836.031660	19.447232
54.997094	1832.658796	19.452250
55.038100	1840.892248	19.457267
55.169780	1851.906669	19.462285
55.767400	1852.865380	19.467303
55.635320	1866.377505	19.472320
55.853154	1872.267936	19.477338
55.488360	1865.828386	19.482355
55.756021	1867.536608	19.487373
55.607044	1862.387992	19.492391
55.860099	1861.635045	19.497408
56.117079	1862.314579	19.502426
55.470117	1875.196202	19.507443
55.660479	1864.922529	19.512461
56.119840	1863.888916	19.517479
56.080629	1868.250369	19.522496
56.405939	1861.304342	19.527514
56.072839	1875.694869	19.532531
55.908081	1862.487336	19.537549
56.061256	1860.607449	19.542567
55.982668	1864.382902	19.547584
56.160981	1860.070903	19.552602
56.051441	1871.399101	19.557619
56.225893	1881.544655	19.562637
56.500080	1886.892819	19.567655
56.113685	1895.966076	19.572672
56.686755	1898.471935	19.577690
56.820939	1884.792754	19.582707
56.566853	1892.580909	19.587725
56.751841	1883.074976	19.592743
56.511637	1890.733494	19.597760
56.610241	1881.781704	19.602778
56.928916	1886.118337	19.607795
56.626189	1890.145059	19.612813
56.822200	1903.283980	19.617831
56.829775	1915.447740	19.622848
57.215806	1917.324292	19.627866
57.482593	1908.067223	19.632883
57.238409	1910.687683	19.637901
57.359550	1910.622774	19.642919
57.339652	1911.543106	19.647936
57.404992	1914.875596	19.652954
57.667897	1912.728864	19.657971
57.413744	1914.469967	19.662989
57.675488	1910.393988	19.668007
57.332488	1917.648104	19.673024
57.777735	1923.253737	19.678042
57.705415	1918.759879	19.683059
57.601055	1909.941906	19.688077
57.649834	1913.776503	19.693095
57.445886	1908.303135	19.698112
57.798052	1930.755223	19.703130
58.060501	1931.761098	19.708147
57.790530	1941.482034	19.713165
58.221576	1934.179316	19.718183
58.091701	1941.887124	19.723200
58.153428	1935.940342	19.728218
58.443933	1938.700495	19.733235
58.182021	1947.276489	19.738253
58.436202	1936.219399	19.743271
58.045301	1937.356996	19.748288
58.197196	1944.797274	19.753306
58.242350	1951.665442	19.758323
58.353594	1965.367745	19.763341
58.420170	1971.746411	19.768359
58.374755	1980.587579	19.773376
58.625198	1966.587740	19.778394
58.650641	1968.893848	19.783411
58.756910	1963.084680	19.788429
59.334023	1968.088818	19.793447
59.083325	1964.590866	19.798464
59.041987	1956.189131	19.803482
58.937066	1970.350655	19.808499
59.073562	1982.681113	19.813517
59.426813	1978.904361	19.818535
59.591673	1983.918402	19.823552
59.374739	1994.427705	19.828570
59.396034	1977.196222	19.833587
59.393554	1993.530439	19.838605
59.822791	1995.123242	19.843623
59.838033	1994.441249	19.848640
59.561305	1966.442045	19.853658
59.853804	1964.957592	19.858675
59.660612	1970.232447	19.863693
60.051793	1966.778433	19.868711
59.706689	1977.211415	19.873728
59.926160	1988.010578	19.878746
60.130233	1976.646036	19.883763
60.199206	1980.623731	19.888781
60.284468	1978.365311	19.893799
59.709976	1977.318798	19.898816
59.994312	1975.907222	19.903834
60.124343	1985.739802	19.908851
60.061635	1991.272300	19.913869
60.252575	1987.510418	19.918887
60.273987	1984.857885	19.923904
60.327292	1985.525072	19.928922
60.611769	1985.130501	19.933939
60.371216	1990.848673	19.938957
60.517279	1983.765995	19.943975
60.469741	1978.609813	19.948992
60.541749	1998.892506	19.954010
61.002175	2008.567013	19.959027
60.880670	2013.426157	19.964045
61.262443	2013.165517	19.969063
60.985301	2017.758453	19.974080
60.927820	2015.370983	19.979098
60.895552	2014.128664	19.984115
60.724691	2021.225596	19.989133
61.058125	2015.511537	19.994151
60.886375	2012.888229	19.999168
61.019424	2013.230434	20.004186
61.451855	2021.057838	20.009203
61.171565	2042.715059	20.014221
61.450345	2042.349712	20.019239
61.559031	2048.866424	20.024256
61.565146	2036.192307	20.029274
61.611814	2045.686626	20.034291
61.608109	2045.431612	20.039309
61.669144	2036.845966	20.044327
61.592943	2039.460111	20.049344
61.633804	2049.144920	20.054362
62.039372	2052.182496	20.059379
62.122192	2081.906330	20.064397
62.236255	2077.818461	20.069415
62.342493	2083.125836	20.074432
62.149333	2087.117833	20.079450
62.219635	2078.017842	20.084467
62.308122	2079.482510	20.089485
62.444676	2070.826595	20.094503
62.259579	2077.357135	20.099520
61.952597	2077.974808	20.104538
62.440794	2070.169731	20.109555
62.318675	2075.957144	20.114573
62.401630	2083.343989	20.119591
62.698748	2077.329722	20.124608
62.363018	2088.305594	20.129626
62.443078	2080.405137	20.134643
62.439994	2098.882182	20.139661
62.630499	2094.555586	20.144679
62.716982	2090.450087	20.149696
62.535536	2106.202591	20.154714
63.037944	2114.987155	20.159731
63.053857	2118.208016	20.164749
63.167457	2120.970460	20.169767
63.311194	2121.106455	20.174784
63.152812	2125.274614	20.179802
63.499312	2123.136545	20.184819
63.452021	2126.211746	20.189837
63.326665	2124.606709	20.194855
63.729278	2111.225881	20.199872
63.581975	2119.509971	20.204890
63.736119	2127.242589	20.209907
63.467743	2139.448181	20.214925
63.897055	2144.637200	20.219943
64.353590	2146.698397	20.224960
64.302782	2150.183182	20.229978
64.466414	2144.769879	20.234995
64.008298	2141.973547	20.240013
64.152360	2146.537895	20.245031
64.603448	2140.868738	20.250048
64.276732	2148.014968	20.255066
64.517404	2140.228876	20.260083
64.276410	2146.603180	20.265101
64.424808	2138.450316	20.270119
64.618307	2134.508651	20.275136
64.446474	2135.693130	20.280154
64.614947	2132.781933	20.285171
64.738245	2138.066944	20.290189
64.636821	2137.088133	20.295207
64.709960	2137.215722	20.300224
64.777902	2139.070667	20.305242
64.807749	2134.705966	20.310259
64.742532	2152.644748	20.315277
64.938607	2165.704453	20.320295
65.434749	2159.405924	20.325312
65.355701	2160.181536	20.330330
65.548262	2172.419838	20.335347
65.737213	2172.912807	20.340365
65.473142	2166.293451	20.345383
65.561265	2164.624477	20.350400
65.568502	2167.464457	20.355418
65.704186	2165.050878	20.360435
65.760016	2169.272985	20.365453
65.828293	2171.851529	20.370471
66.041034	2155.973676	20.375488
66.029279	2162.996536	20.380506
66.226886	2160.213619	20.385523
65.901732	2167.446919	20.390541
65.951405	2161.323415	20.395559
65.955711	2156.308352	20.400576
65.710816	2167.360253	20.405594
65.796674	2158.055582	20.410611
65.963273	2166.594832	20.415629
65.855028	2162.422830	20.420647
65.989801	2171.226728	20.425664
66.209605	2191.374427	20.430682
66.380749	2195.486123	20.435699
66.140171	2191.388704	20.440717
65.920104	2190.644332	20.445735
66.625733	2208.783538	20.450752
66.956728	2219.086064	20.455770
67.104491	2216.816853	20.460787
67.082192	2216.453107	20.465805
66.979095	2213.087298	20.470823
66.826889	2217.729591	20.475840
66.687036	2219.638920	20.480858
66.831890	2211.940436	20.485875
66.980317	2222.191847	20.490893
66.746661	2207.605106	20.495911
67.127525	2224.733458	20.500928
67.082417	2234.336924	20.505946
67.405854	2231.497745	20.510963
67.552740	2242.856131	20.515981
67.699410	2237.325152	20.520999
67.992320	2231.556120	20.526016
67.628190	2247.422072	20.531034
68.232457	2226.099940	20.536051
68.049480	2241.702598	20.541069
68.128070	2231.116131	20.546087
68.330028	2235.270906	20.551104
67.911912	2233.331053	20.556122
67.931065	2236.562435	20.561139
68.225536	2232.117750	20.566157
68.054433	2235.877376	20.571175
68.000561	2232.934757	20.576192
68.126220	2251.863413	20.581210
68.297827	2260.195836	20.586227
68.569708	2262.928346	20.591245
68.397180	2267.616370	20.596263
68.782148	2261.319796	20.601280
68.795731	2265.611595	20.606298
68.801540	2262.008166	20.611315
68.808492	2260.362350	20.616333
68.499773	2268.507870	20.621351
69.009249	2273.997211	20.626368
68.870135	2280.932676	20.631386
69.506452	2284.838073	20.636403
69.511822	2292.966556	20.641421
69.329501	2279.289496	20.646439
69.293675	2267.450135	20.651456
69.058516	2272.348726	20.656474
69.163411	2285.848619	20.661491
69.478145	2285.138518	20.666509
69.370996	2301.435496	20.671527
69.365898	2288.534839	20.676544
69.266967	2289.920868	20.681562
69.646875	2296.213527	20.686579
69.556215	2299.822690	20.691597
69.353740	2312.994064	20.696615
69.922486	2315.991518	20.701632
69.745396	2321.440911	20.706650
69.614267	2327.343915	20.711667
70.022608	2311.461446	20.716685
70.221953	2318.350035	20.721703
70.515335	2313.103186	20.726720
70.456600	2313.840170	20.731738
70.714666	2315.375356	20.736755
70.664898	2307.444352	20.741773
70.594404	2316.159151	20.746791
70.951848	2308.535262	20.751808
70.647243	2314.128481	20.756826
70.499543	2314.395904	20.761843
71.269098	2323.023155	20.766861
70.836940	2339.886430	20.771879
71.121325	2329.828694	20.776896
70.864547	2331.817250	20.781914
71.080998	2332.465516	20.786931
71.030645	2332.796861	20.791949
70.969412	2338.547138	20.796967
71.208705	2326.719704	20.801984
71.370348	2335.399855	20.807002
71.575858	2335.410375	20.812019
71.442742	2330.794725	20.817037
71.112301	2341.100560	20.822055
71.170348	2350.575958	20.827072
71.514009	2366.296919	20.832090
71.648790	2359.112817	20.837107
71.792619	2362.812814	20.842125
71.854332	2367.962211	20.847143
72.074338	2365.684604	20.852160
72.004149	2371.478012	20.857178
71.827097	2373.176195	20.862195
72.257412	2384.265317	20.867213
72.125299	2390.424930	20.872231
72.394616	2392.134526	20.877248
72.434073	2396.574835	20.882266
72.380947	2388.811079	20.887283
72.871473	2393.523195	20.892301
72.835042	2388.745804	20.897319
72.825523	2387.462857	20.902336
72.808504	2391.393811	20.907354
72.945635	2381.880241	20.912371
73.331161	2380.905566	20.917389
73.038531	2383.104359	20.922407
73.271022	2377.898660	20.927424
73.248149	2383.321911	20.932442
73.329126	2383.878516	20.937459
73.564294	2375.849336	20.942477
73.011808	2383.182706	20.947495
73.201111	2377.010889	20.952512
73.077590	2391.056225	20.957530
73.379702	2387.348093	20.962547
73.351780	2377.057744	20.967565
73.176872	2406.247557	20.972583
73.367823	2412.335211	20.977600
73.324484	2410.647056	20.982618
73.436535	2418.228437	20.987635
73.629595	2422.351649	20.992653
73.765438	2445.532799	20.997671
73.881572	2439.551180	21.002688
74.089759	2446.579218	21.007706
74.149158	2445.399331	21.012723
74.323997	2442.697864	21.017741
73.824661	2451.887796	21.022759
74.126561	2449.733983	21.027776
74.509302	2470.200611	21.032794
74.467235	2469.043195	21.037811
74.688001	2466.850403	21.042829
74.563565	2473.673495	21.047847
74.874425	2473.931510	21.052864
74.982327	2470.587055	21.057882
74.858266	2471.922047	21.062899
74.906138	2470.991772	21.067917
75.044347	2470.914701	21.072935
75.038089	2472.068870	21.077952
75.194545	2473.857827	21.082970
75.420340	2477.574674	21.087987
75.828778	2477.558341	21.093005
75.711728	2480.566080	21.098023
75.902115	2466.608378	21.103040
75.747513	2462.567964	21.108058
75.427542	2466.831994	21.113075
75.858285	2464.993507	21.118093
76.005369	2485.903618	21.123111
75.795536	2477.006155	21.128128
75.955927	2490.050604	21.133146
75.869457	2487.306633	21.138163
75.938121	2481.928016	21.143181
76.113279	2483.666797	21.148199
76.114901	2481.488497	21.153216
76.368726	2484.548006	21.158234
76.512784	2490.369436	21.163251
76.597242	2479.506546	21.168269
76.375013	2485.700234	21.173287
76.428491	2489.804035	21.178304
76.551746	2505.009680	21.183322
76.532144	2506.704795	21.188339
77.163800	2510.350637	21.193357
76.881115	2518.372581	21.198375
76.860987	2506.108123	21.203392
77.044867	2510.620614	21.208410
76.925463	2515.963343	21.213427
77.282108	2510.806234	21.218445
76.896049	2514.360297	21.223463
77.007613	2510.387548	21.228480
77.283282	2520.934303	21.233498
77.029694	2532.829520	21.238515
77.641431	2523.617741	21.243533
77.414866	2532.688711	21.248551
77.721036	2526.537525	21.253568
77.904651	2524.075341	21.258586
77.961942	2526.091713	21.263603
78.107705	2523.182487	21.268621
77.983353	2531.102891	21.273639
78.030940	2525.687502	21.278656
78.090643	2527.738099	21.283674
77.893365	2533.016166	21.288691
78.353920	2540.128288	21.293709
78.212616	2544.218329	21.298727
78.305827	2559.446914	21.303744
78.638352	2552.718873	21.308762
78.653524	2564.443829	21.313779
78.530551	2565.353894	21.318797
78.450488	2567.656470	21.323815
78.297741	2557.111377	21.328832
78.667388	2569.151083	21.333850
78.901270	2581.530234	21.338867
79.184551	2573.171557	21.343885
79.293869	2587.360869	21.348903
79.256982	2582.043095	21.353920
79.187146	2579.917079	21.358938
79.328363	2582.668128	21.363955
79.534687	2576.544642	21.368973
79.316333	2581.778105	21.373991
79.512268	2576.639521	21.379008
79.632643	2598.671805	21.384026
79.606315	2619.166905	21.389043
79.764815	2600.651104	21.394061
79.757501	2609.554225	21.399079
79.840677	2612.933587	21.404096
79.906519	2603.225154	21.409114
79.772211	2612.699932	21.414131
79.946639	2620.472841	21.419149
80.128297	2629.588112	21.424167
80.220557	2640.110712	21.429184
80.420433	2643.758581	21.434202
80.699850	2644.949015	21.439219
80.565733	2633.228076	21.444237
80.435638	2635.088706	21.449255
80.668148	2628.644809	21.454272
80.893680	2626.624286	21.459290
80.967264	2637.161661	21.464307
80.992546	2647.095558	21.469325
81.233998	2656.619782	21.474343
81.145888	2660.042988	21.479360
81.676168	2658.681805	21.484378
81.090701	2669.203161	21.489395
81.586084	2657.996154	21.494413
81.606501	2664.234604	21.499431
81.536590	2670.828845	21.504448
81.924959	2658.206503	21.509466
81.588508	2661.593010	21.514483
81.689212	2663.011740	21.519501
81.559740	2659.008954	21.524519
81.776571	2657.876313	21.529536
81.989688	2657.454564	21.534554
81.493882	2663.710044	21.539571
81.635447	2662.248019	21.544589
82.284104	2673.375701	21.549607
82.251077	2688.033812	21.554624
82.744238	2681.428765	21.559642
82.344389	2678.798445	21.564659
82.563113	2676.030156	21.569677
82.587477	2679.976613	21.574695
82.642631	2676.627151	21.579712
82.839327	2674.030708	21.584730
82.749017	2678.327396	21.589747
82.882424	2667.092365	21.594765
83.027630	2678.562270	21.599783
82.955281	2702.376419	21.604800
83.401889	2704.823147	21.609818
83.200804	2712.167505	21.614835
83.256294	2707.078015	21.619853
83.439120	2709.511746	21.624871
83.440927	2713.201443	21.629888
83.517666	2706.662788	21.634906
83.356624	2719.744541	21.639923
83.387103	2710.737033	21.644941
83.612853	2729.301097	21.649959
83.522086	2741.668439	21.654976
83.750387	2731.771187	21.659994
83.601751	2737.123377	21.665011
83.734243	2742.034291	21.670029
84.049304	2751.948009	21.675047
84.385595	2769.050288	21.680064
84.516686	2763.786683	21.685082
84.522075	2768.198714	21.690099
84.714101	2762.844372	21.695117
84.821278	2765.528516	21.700135
84.816690	2770.300831	21.705152
84.858411	2767.627612	21.710170
85.095109	2762.229176	21.715187
84.676375	2761.144386	21.720205
84.570011	2777.464581	21.725223
84.837616	2791.646157	21.730240
85.000167	2778.069382	21.735258
85.158424	2791.907342	21.740275
85.300892	2784.164102	21.745293
85.732160	2790.186061	21.750311
85.378459	2795.098222	21.755328
85.907448	2792.028722	21.760346
85.787961	2791.335925	21.765363
85.563408	2785.041145	21.770381
86.114311	2791.811757	21.775399
85.847001	2797.416516	21.780416
85.981516	2807.874290	21.785434
85.987342	2815.314708	21.790451
85.866179	2829.459988	21.795469
86.225231	2817.001867	21.800487
86.169438	2825.568314	21.805504
86.213195	2816.121270	21.810522
86.012044	2826.019814	21.815539
86.533781	2838.859859	21.820557
86.726787	2840.634382	21.825575
86.658559	2852.053504	21.830592
86.748984	2839.537513	21.835610
86.858245	2846.445437	21.840627
86.998567	2854.256161	21.845645
87.197285	2844.916538	21.850663
87.046162	2842.963127	21.855680
87.132735	2843.662807	21.860698
86.923287	2877.198011	21.865715
87.422127	2879.233696	21.870733
87.656502	2874.901449	21.875751
87.478586	2880.337808	21.880768
87.763442	2874.539919	21.885786
87.850347	2873.508215	21.890803
87.725213	2881.368362	21.895821
87.783459	2888.094081	21.900839
88.127840	2896.643168	21.905856
88.053059	2895.852777	21.910874
88.237160	2901.284119	21.915891
88.321851	2892.538450	21.920909
88.460098	2893.656237	21.925927
88.369643	2901.856189	21.930944
88.361080	2896.662002	21.935962
88.519551	2895.423018	21.940979
88.308753	2891.647094	21.945997
89.021649	2903.880914	21.951015
88.995989	2915.982372	21.956032
89.414822	2923.647248	21.961050
89.054033	2914.685487	21.966067
89.127952	2917.342712	21.971085
89.226884	2910.388242	21.976103
89.379205	2920.928999	21.981120
89.407024	2915.953976	21.986138
89.645211	2912.000258	21.991155
89.460498	2924.040557	21.996173
89.554606	2917.016845	22.001191
89.407039	2921.969332	22.006208
89.454825	2933.475424	22.011226
89.694190	2946.185963	22.016243
89.686355	2937.429850	22.021261
90.111739	2941.320297	22.026279
89.897545	2948.834412	22.031296
89.788545	2953.155400	22.036314
89.855586	2963.775075	22.041331
90.369714	2973.410203	22.046349
90.606266	2968.246914	22.051367
90.353017	2977.130479	22.056384
90.621659	2970.081270	22.061402
90.871877	2966.350592	22.066419
90.720827	2975.349224	22.071437
91.248003	2977.518063	22.076455
91.171645	2996.332802	22.081472
91.327456	2991.750318	22.086490
91.422139	2992.464445	22.091507
91.424341	2990.637595	22.096525
91.552695	2988.302140	22.101543
91.488835	2996.788952	22.106560
91.496545	2997.684498	22.111578
91.766126	2995.365852	22.116595
91.563031	2999.587012	22.121613
91.739979	2996.185804	22.126631
91.701210	3001.092650	22.131648
91.598518	2998.313412	22.136666
91.996957	3003.683870	22.141683
91.892546	3019.497440	22.146701
92.312712	3023.926004	22.151719
92.204602	3030.584707	22.156736
92.030651	3022.625133	22.161754
92.356361	3034.883047	22.166771
92.337793	3055.917143	22.171789
92.766737	3045.817776	22.176807
92.391379	3058.916699	22.181824
92.898142	3051.440103	22.186842
92.959808	3049.296982	22.191859
93.032218	3072.692192	22.196877
93.505395	3074.290703	22.201895
93.394823	3083.448137	22.206912
93.728922	3076.851760	22.211930
93.787844	3078.867162	22.216947
93.587208	3080.588851	22.221965
93.966288	3067.333622	22.226983
94.157194	3061.237566	22.232000
94.320046	3074.279000	22.237018
94.389176	3076.818237	22.242035
94.167314	3057.812661	22.247053
94.016063	3052.351695	22.252071
94.262031	3059.989146	22.257088
94.032045	3069.282820	22.262106
94.006527	3065.179962	22.267123
94.211949	3069.066188	22.272141
94.557308	3068.780667	22.277159
94.537124	3077.503629	22.282176
94.524933	3091.336014	22.287194
95.073536	3099.190320	22.292211
94.739058	3104.455857	22.297229
94.989589	3097.802000	22.302247
94.810549	3111.076548	22.307264
95.061879	3104.443013	22.312282
94.893976	3099.611625	22.317299
94.844643	3121.751995	22.322317
95.038648	3128.180857	22.327335
94.757516	3138.712226	22.332352
94.811235	3138.773700	22.337370
95.607910	3155.723573	22.342387
95.191749	3169.138245	22.347405
95.576379	3173.309001	22.352423
95.934152	3175.128089	22.357440
95.898653	3189.837441	22.362458
96.453304	3190.997408	22.367475
96.116104	3194.231548	22.372493
96.415406	3192.401350	22.377511
96.464479	3188.434450	22.382528
96.448571	3198.058278	22.387546
96.724341	3191.296520	22.392563
96.402082	3192.800840	22.397581
96.482145	3197.223905	22.402599
96.713588	3210.887760	22.407616
97.169767	3205.052984	22.412634
97.022333	3206.100715	22.417651
97.275930	3205.879382	22.422669
97.452302	3200.901814	22.427687
97.660616	3200.415527	22.432704
97.605878	3202.456150	22.437722
97.845105	3204.328756	22.442739
97.474863	3201.046220	22.447757
98.190224	3219.460467	22.452775
98.207634	3220.419769	22.457792
98.189296	3236.185236	22.462810
98.309164	3228.266801	22.467827
98.205282	3230.972887	22.472845
98.478427	3225.733663	22.477863
98.223785	3225.635850	22.482880
98.322072	3231.968320	22.487898
98.652618	3227.084153	22.492915
98.543323	3231.840276	22.497933
98.634294	3228.348103	22.502951
98.825426	3225.609285	22.507968
98.971755	3244.015969	22.512986
99.427555	3248.606474	22.518003
99.306155	3248.334021	22.523021
99.302130	3251.022614	22.528039
99.506512	3244.198272	22.533056
99.391115	3255.740078	22.538074
99.476934	3247.755478	22.543091
99.439906	3246.331314	22.548109
99.395693	3247.183237	22.553127
99.613975	3254.967585	22.558144
99.576011	3270.950183	22.563162
99.701419	3286.618053	22.568179
99.818069	3286.038612	22.573197
100.005840	3281.014361	22.578215
100.087667	3285.228714	22.583232
100.173969	3306.031695	22.588250
100.716103	3307.734874	22.593267
100.662775	3307.636425	22.598285
100.828967	3305.791253	22.603303
100.919563	3309.020134	22.608320
100.980125	3303.636214	22.613338
101.083200	3300.256157	22.618355
101.098827	3300.227735	22.623373
101.106148	3302.945208	22.628391
101.528911	3304.714619	22.633408
101.448344	3292.998769	22.638426
101.354259	3294.386478	22.643443
101.302520	3295.570777	22.648461
101.389378	3316.763856	22.653479
101.596982	3323.511585	22.658496
101.587955	3326.399222	22.663514
101.999269	3313.538244	22.668531
101.772160	3328.291661	22.673549
101.882661	3327.191659	22.678567
101.895536	3347.322821	22.683584
101.971898	3353.669066	22.688602
102.482953	3350.812348	22.693619
102.431314	3356.766020	22.698637
102.151731	3352.626503	22.703655
102.633031	3370.255441	22.708672
102.475382	3380.623337	22.713690
102.976583	3380.401853	22.718707
102.753779	3384.940133	22.723725
102.714765	3392.671972	22.728743
103.304000	3398.055420	22.733760
102.917750	3409.162258	22.738778
103.255813	3410.126295	22.743795
103.464419	3409.210450	22.748813
103.682220	3412.814751	22.753831
103.567530	3418.359222	22.758848
103.644111	3432.984869	22.763866
104.003175	3440.261510	22.768883
103.832543	3453.077986	22.773901
104.116994	3441.796252	22.778919
104.481905	3435.294708	22.783936
104.329649	3432.568127	22.788954
104.413878	3434.377376	22.793971
104.507109	3443.456125	22.798989
104.548593	3458.370585	22.804007
105.138239	3455.762481	22.809024
104.785609	3460.203489	22.814042
105.151157	3460.119271	22.819059
105.076106	3464.643456	22.824077
105.515008	3460.428675	22.829095
105.488808	3454.896486	22.834112
105.231861	3460.730329	22.839130
105.778700	3454.106157	22.844147
105.780026	3458.526910	22.849165
105.639986	3452.047663	22.854183
105.779445	3457.505999	22.859200
105.776027	3478.955207	22.864218
106.128004	3483.448279	22.869235
105.844147	3490.692158	22.874253
106.039715	3494.777518	22.879271
106.536191	3495.585719	22.884288
106.130446	3496.857160	22.889306
105.947636	3499.829967	22.894323
105.759760	3501.869833	22.899341
106.339751	3511.439755	22.904359
106.803122	3511.977909	22.909376
106.864561	3521.259224	22.914394
107.161841	3506.539323	22.919411
107.257157	3510.001917	22.924429
107.353124	3523.549217	22.929447
107.602067	3529.178918	22.934464
107.345322	3548.231588	22.939482
107.655368	3548.610903	22.944499
107.683126	3544.963539	22.949517
107.584038	3544.084163	22.954535
107.866235	3541.150624	22.959552
107.634553	3551.747560	22.964570
108.215170	3538.240300	22.969587
108.004637	3551.233139	22.974605
108.033298	3573.279157	22.979623
108.216214	3570.709142	22.984640
108.214734	3576.921579	22.989658
108.185814	3573.047250	22.994675
108.513744	3582.004491	22.999693
108.714928	3599.727930	23.004711
109.335560	3600.631193	23.009728
108.965385	3599.656587	23.014746
109.197665	3589.946922	23.019763
109.578314	3596.522441	23.024781
109.285732	3604.675563	23.029799
109.624823	3586.885695	23.034816
109.376864	3591.389503	23.039834
109.294272	3598.724847	23.044851
109.586294	3601.820984	23.049869
109.991408	3609.460880	23.054887
109.913303	3616.148890	23.059904
109.816100	3621.021208	23.064922
109.851131	3619.885233	23.069939
109.950590	3633.065498	23.074957
109.816460	3642.226250	23.079975
110.183982	3637.942563	23.084992
110.440340	3648.335099	23.090010
110.758745	3664.352554	23.095027
111.235144	3674.696650	23.100045
111.006540	3678.161374	23.105063
111.531327	3687.764601	23.110080
111.373093	3681.782172	23.115098
111.504128	3675.411427	23.120115
111.701164	3677.286104	23.125133
111.683965	3667.952856	23.130151
111.832950	3666.368407	23.135168
111.867294	3671.195380	23.140186
111.988133	3666.744129	23.145203
112.069444	3677.901693	23.150221
112.119975	3670.503828	23.155239
112.029130	3659.590138	23.160256
111.903057	3668.840087	23.165274
112.217708	3664.719794	23.170291
111.946368	3672.660315	23.175309
112.200231	3692.988736	23.180327
112.440208	3692.535933	23.185344
112.486972	3709.296088	23.190362
112.386476	3709.315288	23.195379
112.731999	3712.542157	23.200397
112.553511	3720.025010	23.205415
112.704490	3728.951557	23.210432
112.550367	3737.649068	23.215450
113.030324	3751.221884	23.220467
113.489594	3754.318920	23.225485
113.442990	3761.246624	23.230503
113.336454	3764.265534	23.235520
113.525365	3790.755341	23.240538
113.834062	3788.281659	23.245555
114.131139	3794.803728	23.250573
114.037305	3793.337436	23.255591
114.264938	3793.141477	23.260608
114.347139	3810.333480	23.265626
114.304941	3821.655593	23.270643
114.684399	3814.068329	23.275661
114.876601	3822.043579	23.280679
114.811348	3831.395638	23.285696
114.891793	3826.646340	23.290714
115.129955	3837.562684	23.295731
115.081307	3838.975452	23.300749
115.123465	3854.104965	23.305767
115.241455	3842.905321	23.310784
115.491455	3842.034771	23.315802
115.963113	3847.286885	23.320819
115.951357	3848.157266	23.325837
115.651514	3863.600920	23.330855
115.955549	3868.198517	23.335872
115.901365	3876.768468	23.340890
116.031548	3880.308190	23.345907
116.188520	3876.469434	23.350925
116.445744	3886.799855	23.355943
116.719016	3892.495831	23.360960
116.658197	3907.428632	23.365978
116.475498	3904.061749	23.370995
116.780252	3901.422691	23.376013
116.796096	3913.368887	23.381031
116.911532	3919.571480	23.386048
117.306658	3933.769234	23.391066
117.242500	3936.539915	23.396083
117.510701	3936.390980	23.401101
117.016090	3939.404937	23.406119
117.544091	3938.024346	23.411136
117.591760	3955.877322	23.416154
117.644319	3961.399262	23.421171
118.322419	3949.101718	23.426189
118.096045	3954.089929	23.431207
118.532977	3951.695681	23.436224
118.348194	3945.331909	23.441242
118.695008	3947.856916	23.446259
119.041578	3954.444326	23.451277
118.490669	3955.410907	23.456295
118.880499	3949.348061	23.461312
119.129302	3963.833496	23.466330
119.184247	3978.043054	23.471347
119.383614	3975.172986	23.476365
119.487631	3981.459240	23.481383
119.289020	3982.512824	23.486400
119.611217	3975.596986	23.491418
119.623932	3981.213394	23.496435
119.901529	3972.986995	23.501453
119.390496	3992.258571	23.506471
119.862534	3998.186431	23.511488
119.845760	3999.277890	23.516506
119.740894	4021.900475	23.521523
120.404834	4007.700604	23.526541
119.816356	4023.757638	23.531559
120.219329	4038.380620	23.536576
120.452010	4042.854342	23.541594
120.597837	4048.529005	23.546611
120.681803	4056.903178	23.551629
121.041780	4065.327748	23.556647
121.403797	4065.743634	23.561664
121.162519	4068.702276	23.566682
121.078308	4069.869000	23.571699
121.292164	4081.955255	23.576717
121.701901	4101.099041	23.581735
121.662162	4107.462551	23.586752
121.416922	4096.741503	23.591770
121.500759	4095.470268	23.596787
122.154250	4108.186590	23.601805
122.106546	4125.388661	23.606823
122.032954	4123.996989	23.611840
122.115429	4135.862727	23.616858
122.329956	4156.775486	23.621875
122.592543	4145.466022	23.626893
122.641798	4153.538192	23.631911
122.447191	4155.898613	23.636928
122.875687	4173.689558	23.641946
123.041215	4188.884707	23.646963
123.347038	4183.417306	23.651981
123.429216	4190.812421	23.656999
123.870066	4196.041254	23.662016
124.172275	4207.125452	23.667034
123.713409	4214.989960	23.672051
124.158544	4216.187936	23.677069
123.928471	4223.073522	23.682087
124.217478	4216.025195	23.687104
124.454643	4212.485880	23.692122
124.277871	4207.502920	23.697139
124.433467	4203.303998	23.702157
124.181304	4217.825507	23.707175
124.752615	4232.059968	23.712192
124.986608	4238.248513	23.717210
125.022192	4244.891933	23.722227
125.421305	4229.712958	23.727245
125.289865	4234.775809	23.732263
125.422204	4228.911242	23.737280
125.582475	4225.012869	23.742298
125.225408	4237.323234	23.747315
125.365025	4245.034118	23.752333
125.454532	4262.240433	23.757351
125.409590	4264.184450	23.762368
126.070610	4270.444166	23.767386
126.212461	4285.844582	23.772403
126.168485	4285.093257	23.777421
126.401341	4293.008786	23.782439
126.031068	4290.878501	23.787456
126.777466	4306.794591	23.792474
127.048855	4311.687036	23.797491
127.248600	4319.334091	23.802509
127.020182	4316.325266	23.807527
127.589216	4314.344152	23.812544
127.535115	4320.322993	23.817562
127.391322	4328.105858	23.822579
127.582895	4313.689149	23.827597
127.747865	4324.818919	23.832615
127.932993	4334.930653	23.837632
128.030492	4337.571004	23.842650
127.951376	4345.773098	23.847667
128.086878	4346.192856	23.852685
127.985725	4355.800352	23.857703
128.209754	4362.331177	23.862720
128.461427	4370.036061	23.867738
128.402189	4383.796922	23.872755
128.592441	4378.766398	23.877773
128.855933	4393.168100	23.882791
128.775562	4395.891890	23.887808
128.772119	4397.697143	23.892826
128.815397	4407.447637	23.897843
129.237233	4424.289623	23.902861
129.322174	4431.195881	23.907879
129.533828	4436.796477	23.912896
129.784631	4439.672013	23.917914
129.739113	4458.479771	23.922931
130.203859	4458.290055	23.927949
130.138583	4455.362967	23.932967
130.029529	4470.789422	23.937984
130.728700	4483.250979	23.943002
130.507634	4496.158218	23.948019
130.770366	4488.343774	23.953037
130.752884	4490.507652	23.958055
130.852861	4498.007861	23.963072
131.549467	4487.298417	23.968090
131.379388	4490.612390	23.973107
131.303697	4488.703370	23.978125
131.393953	4504.780936	23.983143
131.798217	4508.892310	23.988160
131.926546	4504.191803	23.993178
131.989879	4511.853629	23.998195
132.034191	4506.506476	24.003213
131.816631	4509.177424	24.008231
132.053336	4522.347619	24.013248
132.552816	4528.595443	24.018266
132.310842	4539.960187	24.023283
132.246620	4548.967961	24.028301
132.497560	4552.874077	24.033319
132.529341	4564.052798	24.038336
132.930850	4569.882787	24.043354
132.865734	4572.863003	24.048371
133.283858	4571.974261	24.053389
133.444965	4581.586505	24.058407
133.531546	4598.315363	24.063424
133.908329	4596.093454	24.068442
134.159035	4606.510388	24.073459
134.042141	4598.132557	24.078477
134.306944	4599.492273	24.083495
133.907392	4596.171605	24.088512
134.437666	4598.831899	24.093530
134.866910	4618.010225	24.098547
134.668625	4618.535134	24.103565
134.836901	4622.208996	24.108583
134.479816	4623.436578	24.113600
135.024985	4614.605454	24.118618
134.815294	4625.030510	24.123635
134.687616	4641.601623	24.128653
135.207557	4646.389254	24.133671
135.084693	4659.358076	24.138688
135.322721	4666.842654	24.143706
135.354669	4682.691339	24.148723
135.733437	4686.082270	24.153741
136.211711	4699.876517	24.158759
135.849094	4710.709931	24.163776
136.680676	4697.299281	24.168794
136.473004	4703.430209	24.173811
136.477687	4716.300073	24.178829
136.923101	4715.910468	24.183847
136.919673	4736.147616	24.188864
137.071328	4744.093645	24.193882
136.908618	4752.225901	24.198899
137.122098	4740.316471	24.203917
137.430143	4741.374290	24.208935
137.344744	4764.011431	24.213952
137.797626	4768.305512	24.218970
137.577761	4773.222154	24.223987
137.892380	4779.084962	24.229005
138.547421	4784.658269	24.234023
138.533008	4794.473287	24.239040
138.605416	4793.310808	24.244058
138.705836	4798.919052	24.249075
138.973505	4794.720976	24.254093
139.166054	4792.383658	24.259111
138.920492	4799.324690	24.264128
139.388794	4792.566123	24.269146
138.957810	4797.474738	24.274163
139.168074	4797.824374	24.279181
138.974602	4794.737499	24.284199
138.862334	4810.101883	24.289216
139.152002	4818.094391	24.294234
139.361681	4826.713296	24.299251
139.621289	4839.651977	24.304269
139.775812	4846.948562	24.309287
139.679720	4856.257411	24.314304
140.122109	4867.849220	24.319322
140.484316	4874.208767	24.324339
140.152019	4888.298426	24.329357
140.618592	4889.087097	24.334375
140.681420	4911.054146	24.339392
140.802611	4906.109980	24.344410
141.042579	4910.670920	24.349427
141.314006	4920.471918	24.354445
141.261335	4939.039118	24.359463
141.435969	4942.936264	24.364480
141.556498	4935.303962	24.369498
141.733168	4945.958730	24.374515
141.587053	4963.389098	24.379533
141.959683	4971.185156	24.384551
142.151166	4968.010119	24.389568
142.419964	4985.489221	24.394586
142.657609	4992.344648	24.399603
142.686435	4995.701759	24.404621
142.867482	5002.187799	24.409639
142.805208	5009.467106	24.414656
143.038787	5022.483263	24.419674
143.021694	5028.976517	24.424691
143.229820	5038.727108	24.429709
143.394711	5042.625047	24.434727
143.531778	5062.844176	24.439744
143.932652	5065.997228	24.444762
144.260530	5075.170959	24.449779
144.214702	5066.143492	24.454797
145.067894	5050.829131	24.459815
145.007006	5052.316344	24.464832
145.050323	5047.253163	24.469850
145.304498	5040.143129	24.474867
145.151639	5043.178338	24.479885
145.374051	5043.592129	24.484903
145.265311	5046.219859	24.489920
145.639059	5057.261040	24.494938
145.818986	5062.988879	24.499955
145.835955	5065.857765	24.504973
146.188717	5054.560767	24.509991
146.001120	5068.394655	24.515008
145.735299	5061.716824	24.520026
146.144086	5061.504560	24.525043
145.773792	5070.394664	24.530061
146.091759	5073.676585	24.535079
146.281098	5094.674154	24.540096
146.481724	5096.110237	24.545114
146.595532	5098.667878	24.550131
146.692484	5124.305412	24.555149
146.997395	5127.685409	24.560167
146.832945	5138.435613	24.565184
146.797067	5148.782188	24.570202
147.374883	5159.464415	24.575219
147.295578	5167.938418	24.580237
147.666659	5174.415478	24.585255
147.631989	5185.392847	24.590272
147.718946	5186.802217	24.595290
148.169697	5193.148573	24.600307
148.370221	5207.047374	24.605325
148.868973	5213.263355	24.610343
148.858304	5227.246985	24.615360
148.885299	5223.537175	24.620378
149.136879	5216.680013	24.625395
149.165620	5223.859948	24.630413
149.484562	5234.288477	24.635431
149.748730	5246.502203	24.640448
149.709187	5240.253964	24.645466
150.047338	5246.188736	24.650483
149.830466	5253.923158	24.655501
150.067085	5245.128269	24.660519
150.061527	5255.060193	24.665536
150.351201	5268.003112	24.670554
150.607148	5271.758356	24.675571
150.502257	5277.161920	24.680589
150.651984	5278.211192	24.685607
150.840749	5291.475475	24.690624
150.588981	5297.942536	24.695642
150.645459	5307.392559	24.700659
150.852279	5328.984026	24.705677
151.200147	5338.658251	24.710695
151.107779	5357.076531	24.715712
151.215000	5372.083152	24.720730
151.457605	5388.673953	24.725747
151.809117	5407.592704	24.730765
152.092966	5405.990505	24.735783
152.291458	5410.673866	24.740800
152.533210	5427.329360	24.745818
152.719218	5431.242132	24.750835
152.814251	5436.415618	24.755853
153.046641	5432.805184	24.760871
153.211600	5431.697920	24.765888
153.422446	5454.578410	24.770906
153.763916	5464.113697	24.775923
153.699789	5463.119270	24.780941
153.794042	5462.093298	24.785959
153.514961	5464.408384	24.790976
153.795547	5477.598402	24.795994
154.203441	5478.776467	24.801011
154.223365	5500.547464	24.806029
154.558793	5493.400657	24.811047
154.321379	5494.104130	24.816064
154.536032	5513.680533	24.821082
154.814450	5522.777461	24.826099
154.968926	5524.020322	24.831117
155.041522	5526.278562	24.836135
155.078307	5533.576951	24.841152
154.940376	5543.508144	24.846170
155.400425	5557.953605	24.851187
155.440683	5567.373337	24.856205
155.711896	5576.315669	24.861223
156.272675	5573.496248	24.866240
157.015924	5575.991385	24.871258
156.837224	5557.865510	24.876275
157.122310	5575.323048	24.881293
157.152978	5584.508293	24.886311
157.319798	5586.740505	24.891328
157.438458	5581.961737	24.896346
157.923177	5583.652330	24.901363
157.472971	5591.752992	24.906381
157.673254	5588.814022	24.911399
157.534067	5579.725598	24.916416
157.597452	5587.328181	24.921434
157.921177	5600.385550	24.926451
157.717642	5616.195678	24.931469
157.939513	5629.765757	24.936487
158.359990	5643.891108	24.941504
158.198038	5643.453556	24.946522
158.503195	5648.962608	24.951539
158.454064	5678.156160	24.956557
158.650131	5679.144574	24.961575
158.940895	5696.618659	24.966592
158.916421	5708.140803	24.971610
159.436890	5714.735903	24.976627
159.620661	5739.280436	24.981645
159.913968	5744.291817	24.986663
160.197222	5759.613797	24.991680
160.331635	5753.118886	24.996698
160.758673	5747.471877	25.001715
160.495580	5772.300135	25.006733
160.788078	5772.386495	25.011751
160.735674	5769.621526	25.016768
160.800941	5778.068108	25.021786
161.146511	5791.263782	25.026803
161.235647	5810.305132	25.031821
161.614719	5802.273972	25.036839
161.688144	5811.896279	25.041856
161.770105	5811.044545	25.046874
162.361727	5832.904270	25.051891
162.085219	5847.291209	25.056909
162.283786	5843.269079	25.061927
162.695555	5837.386080	25.066944
162.153498	5841.889458	25.071962
162.751789	5852.415509	25.076979
162.978786	5859.464225	25.081997
163.294353	5852.908918	25.087015
163.641093	5849.575979	25.092032
163.823580	5851.464276	25.097050
164.287063	5838.604601	25.102067
163.715075	5850.302264	25.107085
163.714343	5847.998744	25.112103
164.262671	5845.638374	25.117120
164.442360	5867.764451	25.122138
164.695829	5860.549498	25.127155
164.708234	5872.798376	25.132173
164.684925	5870.246685	25.137191
164.745571	5870.930192	25.142208
164.874569	5878.800982	25.147226
165.353312	5890.818173	25.152243
165.451237	5894.085795	25.157261
165.176506	5907.000455	25.162279
165.666770	5904.023061	25.167296
165.785504	5910.219676	25.172314
166.055638	5924.519539	25.177331
166.057546	5939.137551	25.182349
166.093392	5926.943141	25.187367
166.426370	5945.704249	25.192384
166.356294	5967.250315	25.197402
166.733625	5964.341268	25.202419
166.664900	5973.995784	25.207437
166.849681	5985.950555	25.212455
167.120934	5986.252735	25.217472
166.801303	5999.512162	25.222490
167.401021	6010.369334	25.227507
167.455889	6024.731938	25.232525
167.781697	6032.211088	25.237543
168.425154	6038.334330	25.242560
168.239363	6048.155472	25.247578
168.295183	6053.692627	25.252595
168.143926	6064.105441	25.257613
168.100774	6085.464853	25.262631
168.567209	6089.075814	25.267648
168.645530	6120.819555	25.272666
168.972969	6103.680774	25.277683
168.966014	6129.265805	25.282701
169.723302	6140.134145	25.287719
169.698587	6147.095668	25.292736
169.789384	6150.093042	25.297754
170.243788	6165.789420	25.302771
170.484937	6171.105096	25.307789
170.438224	6172.017379	25.312807
170.663639	6172.868182	25.317824
171.095358	6194.636705	25.322842
171.212922	6205.072852	25.327859
171.110635	6200.352714	25.332877
171.481912	6218.943625	25.337895
171.659864	6205.568962	25.342912
171.307242	6208.496205	25.347930
171.642957	6229.283222	25.352947
171.816760	6239.423248	25.357965
171.463691	6241.797454	25.362983
172.193975	6248.069809	25.368000
172.219203	6267.964589	25.373018
172.457941	6272.017096	25.378035
172.340182	6283.353140	25.383053
172.524778	6296.832213	25.388071
172.773391	6309.304222	25.393088
172.468835	6328.006162	25.398106
172.805633	6333.619792	25.403123
173.314368	6349.465850	25.408141
173.365667	6361.855275	25.413159
173.919108	6367.808109	25.418176
174.102950	6381.201618	25.423194
174.046482	6400.584019	25.428211
174.304440	6397.671890	25.433229
174.443063	6406.971829	25.438247
174.907715	6424.395450	25.443264
174.878907	6440.018089	25.448282
175.179925	6439.552337	25.453299
175.571748	6444.260284	25.458317
175.317061	6472.307965	25.463335
175.699443	6465.477374	25.468352
175.496140	6484.585881	25.473370
175.871102	6484.076081	25.478387
175.992443	6494.950079	25.483405
176.136091	6501.562338	25.488423
176.643577	6508.244057	25.493440
176.287415	6537.437106	25.498458
176.985994	6519.178849	25.503475
176.742451	6527.875726	25.508493
176.815576	6544.120325	25.513511
177.228109	6554.376723	25.518528
176.892191	6572.585132	25.523546
177.135552	6578.260174	25.528563
177.731532	6602.238437	25.533581
177.679783	6610.777323	25.538599
178.058665	6622.798443	25.543616
178.362115	6643.270952	25.548634
178.349822	6646.178642	25.553651
178.659440	6657.308358	25.558669
178.762929	6690.312140	25.563687
179.415700	6687.329932	25.568704
179.348981	6686.550635	25.573722
179.474949	6707.649508	25.578739
179.767633	6717.364912	25.583757
180.038225	6724.865020	25.588775
180.512603	6714.043862	25.593792
180.473047	6712.722051	25.598810
180.614201	6720.659017	25.603827
181.070579	6718.653868	25.608845
180.877316	6727.462441	25.613863
181.386245	6725.832093	25.618880
181.393342	6737.512087	25.623898
181.523762	6732.177156	25.628915
181.447856	6741.624808	25.633933
181.340050	6760.022897	25.638951
181.777892	6756.569016	25.643968
181.526816	6774.205504	25.648986
181.758008	6782.331936	25.654003
182.123699	6787.281780	25.659021
182.051648	6803.194950	25.664039
182.408976	6814.662593	25.669056
182.575604	6823.389457	25.674074
182.467788	6844.262995	25.679092
183.170656	6855.246765	25.684109
183.171157	6865.843667	25.689127
183.603010	6875.164821	25.694144
183.894770	6877.680241	25.699162
184.038487	6880.509602	25.704180
184.695533	6876.011251	25.709197
184.519658	6880.621004	25.714215
184.995823	6901.577773	25.719232
185.309268	6902.010158	25.724250
185.473661	6904.282301	25.729268
185.479965	6908.548289	25.734285
185.631992	6907.405214	25.739303
185.944863	6897.631760	25.744320
186.024487	6901.575260	25.749338
185.616276	6906.210257	25.754356
185.961407	6916.481587	25.759373
185.809264	6935.591171	25.764391
186.065699	6939.943971	25.769408
186.437944	6968.212093	25.774426
186.423569	6971.810229	25.779444
186.678487	6979.693791	25.784461
186.696082	6991.469091	25.789479
187.190391	6998.485179	25.794496
187.190134	7011.463260	25.799514
187.171236	7029.299085	25.804532
187.553358	7041.375108	25.809549
187.692456	7075.824205	25.814567
187.839661	7069.683119	25.819584
188.199185	7080.309491	25.824602
188.395605	7098.062289	25.829620
188.714739	7109.580313	25.834637
188.747234	7134.471515	25.839655
189.027711	7129.483910	25.844672
189.263319	7148.172366	25.849690
189.089194	7168.581678	25.854708
189.692369	7166.974029	25.859725
189.965791	7181.295042	25.864743
190.133689	7185.651013	25.869760
190.138864	7205.167446	25.874778
190.656773	7207.215682	25.879796
190.818618	7204.745190	25.884813
190.887574	7227.318204	25.889831
190.934454	7232.877682	25.894848
191.244566	7230.996501	25.899866
191.074724	7237.528448	25.904884
191.621319	7249.044940	25.909901
191.797494	7259.324559	25.914919
191.718983	7256.710614	25.919936
191.654237	7271.395640	25.924954
192.128928	7288.471680	25.929972
192.504170	7287.610879	25.934989
192.227887	7305.253586	25.940007
192.750449	7321.189758	25.945024
192.888025	7329.646155	25.950042
192.864921	7340.315614	25.955060
193.121651	7351.628177	25.960077
193.417228	7361.931322	25.965095
193.975563	7375.368319	25.970112
194.059827	7380.905369	25.975130
194.372268	7373.045299	25.980148
195.442272	7371.893549	25.985165
195.215474	7384.708208	25.990183
195.373252	7371.175986	25.995200
195.672308	7371.291220	26.000218
195.391677	7368.434865	26.005236
196.037112	7379.155147	26.010253
196.020701	7383.374532	26.015271
196.353604	7378.982003	26.020288
196.496819	7389.977494	26.025306
196.334926	7388.148720	26.030324
196.982297	7386.094155	26.035341
196.602422	7394.517411	26.040359
196.582589	7394.074457	26.045376
197.178093	7412.758593	26.050394
196.884086	7421.549013	26.055412
197.294996	7420.821793	26.060429
197.160586	7435.200984	26.065447
197.421294	7433.112843	26.070464
197.879894	7456.140267	26.075482
197.769628	7480.709376	26.080500
198.312867	7473.965994	26.085517
198.203885	7495.357594	26.090535
197.985510	7497.866318	26.095552
198.971863	7517.648109	26.100570
199.064703	7539.737019	26.105588
199.584638	7530.153613	26.110605
199.575851	7541.285181	26.115623
199.614402	7559.468931	26.120640
199.724982	7566.990254	26.125658
199.953919	7578.583611	26.130676
200.343726	7586.459370	26.135693
200.423201	7594.335033	26.140711
200.309243	7594.953605	26.145728
200.805267	7619.144594	26.150746
200.588152	7635.739597	26.155764
200.902302	7652.393136	26.160781
201.116434	7674.111967	26.165799
201.229918	7679.696403	26.170816
201.563297	7693.066471	26.175834
201.725185	7701.627005	26.180852
202.022182	7715.963661	26.185869
202.010608	7735.010942	26.190887
202.027110	7750.907072	26.195904
202.250138	7754.227555	26.200922
202.723449	7780.841272	26.205940
202.952575	7778.616482	26.210957
203.539071	7792.529363	26.215975
203.492530	7805.473808	26.220992
203.719647	7803.832409	26.226010
203.675559	7827.830497	26.231028
204.203232	7829.937858	26.236045
204.350099	7834.184064	26.241063
204.568442	7859.378911	26.246080
204.651182	7858.620578	26.251098
204.724222	7872.557943	26.256116
204.908333	7878.227194	26.261133
205.119105	7891.507610	26.266151
205.468607	7906.314502	26.271168
205.468780	7921.103129	26.276186
205.547035	7940.680087	26.281204
206.180023	7948.178915	26.286221
206.097462	7960.303797	26.291239
206.190881	7981.524550	26.296256
206.790293	7977.122413	26.301274
206.714609	7999.752702	26.306292
207.319679	8007.707683	26.311309
207.665895	8004.113900	26.316327
207.622950	8018.992120	26.321344
208.433181	8023.843978	26.326362
208.647945	8038.471431	26.331380
208.564589	8033.334969	26.336397
208.771364	8039.140341	26.341415
208.756629	8060.515759	26.346432
209.232732	8060.777074	26.351450
209.415898	8070.349908	26.356468
209.306718	8067.411002	26.361485
209.597787	8084.601429	26.366503
209.648645	8097.684044	26.371520
209.805911	8099.723016	26.376538
209.909585	8128.799441	26.381556
209.923768	8138.364239	26.386573
210.171293	8156.291138	26.391591
210.506449	8163.310335	26.396608
210.562263	8181.196611	26.401626
210.984593	8202.623741	26.406644
211.157880	8209.934735	26.411661
211.476602	8214.777663	26.416679
211.692161	8223.284301	26.421696
212.105991	8240.362091	26.426714
212.216747	8261.173258	26.431732
212.249026	8264.248063	26.436749
212.675033	8275.188898	26.441767
212.715944	8302.114840	26.446784
212.835269	8303.788471	26.451802
213.251641	8314.558540	26.456820
213.623628	8334.723434	26.461837
213.711796	8326.979669	26.466855
214.019030	8340.619674	26.471872
213.932125	8350.702373	26.476890
213.833504	8361.303154	26.481908
214.075081	8375.943582	26.486925
214.690481	8389.225648	26.491943
214.714297	8395.275543	26.496960
215.227702	8395.680433	26.501978
215.252235	8424.033898	26.506996
215.347711	8423.683092	26.512013
215.569883	8438.183851	26.517031
215.628465	8443.261902	26.522048
215.949219	8458.582662	26.527066
216.069252	8480.117005	26.532084
216.335285	8494.638762	26.537101
216.486326	8503.660649	26.542119
216.635686	8532.464206	26.547136
216.839897	8547.098955	26.552154
217.248974	8556.631368	26.557172
217.422027	8566.771923	26.562189
217.900898	8576.429753	26.567207
218.109912	8596.100828	26.572224
218.610791	8605.656410	26.577242
218.621554	8615.480954	26.582260
218.529542	8633.296904	26.587277
218.821937	8637.431613	26.592295
218.844650	8659.926816	26.597312
219.129777	8677.535941	26.602330
219.596502	8674.828930	26.607348
219.389808	8705.135543	26.612365
219.759085	8707.274186	26.617383
219.673326	8741.467481	26.622400
220.435456	8740.526836	26.627418
220.643830	8767.328554	26.632436
220.573814	8772.744346	26.637453
221.323499	8786.974068	26.642471
221.432924	8795.041141	26.647488
222.075955	8794.828499	26.652506
222.545444	8799.029849	26.657524
222.877183	8813.738568	26.662541
223.271350	8813.881154	26.667559
223.187131	8822.348179	26.672576
223.710762	8814.696856	26.677594
223.576795	8813.592147	26.682612
223.565257	8817.811554	26.687629
224.021249	8810.462572	26.692647
223.603401	8817.207467	26.697664
223.972678	8831.675717	26.702682
223.932222	8847.702492	26.707700
224.360256	8848.244161	26.712717
224.681929	8872.054596	26.717735
224.765808	8888.055299	26.722752
225.124063	8884.756458	26.727770
224.588692	8891.049928	26.732788
224.843795	8911.080781	26.737805
225.228656	8919.177594	26.742823
225.290892	8937.193987	26.747840
225.297156	8952.604733	26.752858
225.905609	8966.645062	26.757876
225.932781	8987.313175	26.762893
226.273230	9001.149159	26.767911
226.390859	9023.878057	26.772928
226.686019	9038.623914	26.777946
226.844453	9058.622370	26.782964
227.159027	9077.194815	26.787981
227.379539	9081.931313	26.792999
227.699571	9116.858738	26.798016
227.987080	9119.809225	26.803034
228.203465	9143.111982	26.808052
228.448810	9155.778131	26.813069
228.627132	9171.500848	26.818087
228.862898	9186.370425	26.823104
229.179178	9202.365109	26.828122
229.573668	9209.435546	26.833140
230.058520	9232.262433	26.838157
230.543582	9242.460345	26.843175
230.586243	9244.586208	26.848192
230.639930	9239.854407	26.853210
230.831619	9259.952889	26.858228
231.223664	9263.349469	26.863245
231.212934	9272.498730	26.868263
231.193314	9302.506409	26.873280
231.771279	9304.918002	26.878298
231.970398	9314.992347	26.883316
232.176717	9333.858588	26.888333
232.785888	9327.162509	26.893351
232.515890	9346.240439	26.898368
232.617196	9361.699805	26.903386
232.853211	9377.434397	26.908404
233.255895	9394.268968	26.913421
233.570186	9403.444016	26.918439
233.453824	9419.973382	26.923456
233.920364	9433.631095	26.928474
234.375896	9446.731441	26.933492
234.377931	9467.321984	26.938509
234.585602	9468.140010	26.943527
234.795166	9493.176108	26.948544
234.848316	9497.879214	26.953562
235.223987	9513.790396	26.958580
235.515578	9537.667674	26.963597
235.823033	9539.973296	26.968615
235.959777	9560.841935	26.973632
236.299346	9561.278118	26.978650
236.325895	9579.199057	26.983668
236.141438	9602.864290	26.988685
236.453671	9617.630817	26.993703
236.909246	9638.069423	26.998720
237.533209	9648.393423	27.003738
237.672100	9663.549240	27.008756
237.891947	9670.552118	27.013773
238.276987	9687.056549	27.018791
238.064266	9699.365698	27.023808
238.419969	9707.376300	27.028826
238.596782	9714.327035	27.033844
238.653830	9735.289677	27.038861
239.503307	9751.154707	27.043879
239.574341	9765.701306	27.048896
239.397711	9772.575013	27.053914
240.133926	9785.216178	27.058932
240.131572	9793.988246	27.063949
240.480208	9811.484307	27.068967
240.576747	9834.177264	27.073984
241.373394	9841.453441	27.079002
241.379765	9860.399827	27.084020
241.247849	9862.317117	27.089037
241.766699	9878.024466	27.094055
241.788879	9895.181137	27.099072
241.803556	9900.311537	27.104090
242.284810	9916.346795	27.109108
242.182775	9943.170187	27.114125
242.598974	9959.273310	27.119143
242.794530	9980.929589	27.124160
242.991732	10000.092847	27.129178
243.615227	10014.864455	27.134196
243.465908	10030.832323	27.139213
243.890915	10044.677044	27.144231
243.716494	10065.433074	27.149248
243.925239	10088.042027	27.154266
244.521728	10101.874813	27.159284
244.917428	10123.189712	27.164301
245.660054	10123.702148	27.169319
245.875854	10144.246165	27.174336
245.971842	10165.318101	27.179354
246.264821	10160.041436	27.184372
246.377890	10184.785170	27.189389
246.767075	10187.661428	27.194407
246.578309	10194.437705	27.199424
247.055462	10203.168995	27.204442
247.258203	10225.032641	27.209460
247.192457	10251.047268	27.214477
247.496805	10254.407688	27.219495
248.064354	10275.173235	27.224512
248.188423	10294.335933	27.229530
248.454455	10305.268346	27.234548
248.582293	10322.414564	27.239565
249.021945	10341.186640	27.244583
249.215817	10353.095853	27.249600
249.319694	10372.071019	27.254618
249.650412	10382.275425	27.259636
249.746034	10397.750535	27.264653
250.005346	10416.407426	27.269671
250.195079	10430.897578	27.274688
250.387175	10449.195328	27.279706
250.810948	10455.093764	27.284724
250.867904	10482.362815	27.289741
250.809908	10496.633194	27.294759
251.277902	10509.414925	27.299776
251.779417	10523.127873	27.304794
252.556115	10522.563374	27.309812
252.789089	10544.193643	27.314829
253.467009	10512.285800	27.319847
253.838437	10521.164380	27.324864
254.066520	10524.349315	27.329882
254.396516	10515.963814	27.334900
254.172422	10530.690017	27.339917
254.785169	10543.357805	27.344935
254.904342	10545.320551	27.349952
254.712359	10554.491216	27.354970
255.268917	10550.091643	27.359988
254.924971	10559.234589	27.365005
255.180578	10568.745139	27.370023
255.212146	10586.459884	27.375040
255.203631	10611.955234	27.380058
255.658261	10621.612749	27.385076
255.858650	10653.217579	27.390093
255.942848	10666.305382	27.395111
256.765728	10674.615877	27.400128
256.714486	10699.584583	27.405146
257.141477	10714.184365	27.410164
257.214105	10737.416097	27.415181
257.417200	10752.611573	27.420199
257.768183	10775.243748	27.425216
257.962456	10793.955548	27.430234
258.566021	10800.858836	27.435252
258.732657	10825.735176	27.440269
259.206344	10837.322745	27.445287
259.446164	10842.442766	27.450304
259.658618	10850.851049	27.455322
259.895904	10867.200886	27.460340
259.980353	10878.682102	27.465357
260.595819	10898.355160	27.470375
260.853981	10902.780080	27.475392
260.901162	10922.702336	27.480410
261.319331	10946.994548	27.485428
261.543307	10953.960771	27.490445
261.598658	10975.049760	27.495463
261.875364	10987.093056	27.500480
261.954092	11001.087118	27.505498
262.140426	11013.366391	27.510516
262.332477	11047.768951	27.515533
262.342432	11055.131767	27.520551
262.665246	11077.364738	27.525568
262.716744	11111.681232	27.530586
263.344145	11120.680320	27.535604
263.384923	11146.611035	27.540621
263.653921	11175.266393	27.545639
264.244377	11187.294472	27.550656
264.358821	11213.676347	27.555674
264.735944	11228.752480	27.560692
264.971289	11238.204112	27.565709
265.290906	11259.133319	27.570727
265.717404	11272.061623	27.575744
265.743482	11283.320268	27.580762
266.434757	11285.463854	27.585780
266.623102	11308.252615	27.590797
266.637366	11326.329096	27.595815
266.943125	11339.935274	27.600832
267.313368	11351.898824	27.605850
267.911391	11361.108556	27.610868
267.959548	11385.714276	27.615885
268.151557	11391.871976	27.620903
268.502896	11409.083369	27.625920
268.285240	11425.103936	27.630938
268.786906	11438.689407	27.635956
268.877941	11457.443080	27.640973
269.087213	11480.549494	27.645991
269.451352	11499.307898	27.651008
269.774253	11530.057595	27.656026
270.550890	11514.967728	27.661044
271.111534	11536.499577	27.666061
271.289540	11541.710955	27.671079
271.641701	11531.828489	27.676096
271.410002	11556.802971	27.681114
271.802115	11575.060762	27.686132
271.899736	11589.996450	27.691149
272.148551	11603.692027	27.696167
272.506861	11611.590487	27.701184
272.408240	11647.991304	27.706202
273.104416	11648.919708	27.711220
272.966145	11675.195679	27.716237
273.075514	11698.196155	27.721255
273.324413	11711.768245	27.726272
273.319840	11738.682392	27.731290
274.050380	11762.678594	27.736308
274.077181	11783.930676	27.741325
274.390285	11808.604652	27.746343
274.734428	11829.357581	27.751360
274.743141	11857.078156	27.756378
275.294932	11884.661851	27.761396
275.252112	11901.787869	27.766413
275.776888	11925.969230	27.771431
276.629796	11937.007835	27.776448
276.930548	11961.932750	27.781466
277.193839	11983.268040	27.786484
277.460363	11988.621702	27.791501
277.811350	12008.870834	27.796519
278.211269	12019.025575	27.801536
278.281139	12037.836271	27.806554
278.242168	12051.592879	27.811572
278.575564	12061.549080	27.816589
278.709307	12082.113141	27.821607
279.394588	12090.980213	27.826624
279.159150	12114.210224	27.831642
279.492107	12117.444114	27.836660
279.744616	12137.881686	27.841677
280.108459	12153.442172	27.846695
280.436783	12176.015712	27.851712
280.311835	12204.264921	27.856730
280.688583	12213.821548	27.861748
280.890086	12237.645833	27.866765
281.419207	12265.132693	27.871783
281.379164	12281.744124	27.876800
281.477939	12317.113487	27.881818
281.951731	12340.987022	27.886836
282.167904	12362.293952	27.891853
282.469666	12389.403448	27.896871
283.201142	12409.599755	27.901888
283.460099	12436.291312	27.906906
283.972762	12449.316303	27.911924
284.266732	12459.911106	27.916941
284.500703	12477.658181	27.921959
285.321221	12486.128478	27.926976
285.433043	12502.968219	27.931994
285.689678	12513.477113	27.937012
286.396707	12517.776660	27.942029
286.268396	12540.029172	27.947047
286.640859	12551.178650	27.952064
286.671661	12563.910197	27.957082
287.536436	12569.394033	27.962100
287.655079	12582.060039	27.967117
287.533055	12589.857480	27.972135
288.293223	12591.257081	27.977152
288.145499	12608.431704	27.982170
288.530734	12611.323630	27.987188
288.706770	12629.410906	27.992205
288.872724	12646.761878	27.997223
288.945697	12660.881181	28.002240
288.648620	12690.027123	28.007258
289.117471	12716.501336	28.012276
289.802240	12729.921632	28.017293
289.534711	12761.100489	28.022311
290.153062	12786.473610	28.027328
290.020014	12820.823772	28.032346
290.525930	12837.953121	28.037364
291.634067	12845.505243	28.042381
292.056314	12869.934691	28.047399
292.600427	12872.312337	28.052416
292.562317	12894.614748	28.057434
293.058690	12915.130801	28.062452
293.376631	12916.536172	28.067469
292.962621	12934.378789	28.072487
293.341132	12941.320318	28.077504
293.715296	12974.559031	28.082522
293.748134	12995.295378	28.087540
294.106834	13016.244595	28.092557
294.170713	13034.293454	28.097575
294.725795	13050.861156	28.102592
294.525036	13076.937760	28.107610
295.133459	13089.058465	28.112628
295.555188	13100.740777	28.117645
296.008730	13127.045662	28.122663
296.604517	13126.295533	28.127680
296.586381	13146.662180	28.132698
296.810872	13159.100939	28.137716
297.336792	13171.829751	28.142733
297.475318	13190.105701	28.147751
297.957610	13203.656592	28.152768
297.878416	13225.382162	28.157786
298.196488	13246.315049	28.162804
298.596761	13258.494745	28.167821
298.438138	13288.470384	28.172839
299.149817	13303.076499	28.177856
299.541405	13312.405936	28.182874
299.485250	13339.872406	28.187892
299.873751	13356.344881	28.192909
300.146026	13385.083616	28.197927
300.497751	13415.397236	28.202944
300.580599	13423.187738	28.207962
300.899413	13459.022666	28.212980
301.498074	13481.052060	28.217997
301.750863	13497.437885	28.223015
302.551746	13514.883089	28.228032
302.658895	13536.363324	28.233050
302.779217	13561.288427	28.238068
303.035737	13572.025370	28.243085
303.185599	13597.773834	28.248103
303.427287	13624.825835	28.253120
303.555249	13649.263781	28.258138
303.985777	13672.294481	28.263156
304.357269	13680.066173	28.268173
304.614249	13706.124624	28.273191
304.967003	13734.897906	28.278208
305.344590	13751.917672	28.283226
305.447723	13778.254534	28.288244
305.869845	13791.857556	28.293261
305.882706	13821.926760	28.298279
306.324977	13848.118184	28.303296
307.079257	13870.926472	28.308314
307.458241	13900.620342	28.313332
308.058553	13909.109914	28.318349
308.228795	13939.714649	28.323367
308.391153	13945.307202	28.328384
309.016396	13967.769664	28.333402
309.329617	13978.849832	28.338420
309.901047	13996.616731	28.343437
309.902076	14008.889487	28.348455
309.977431	14024.347809	28.353472
310.103830	14043.773956	28.358490
310.313025	14063.409219	28.363508
310.865429	14071.821007	28.368525
310.939966	14111.925926	28.373543
310.988341	14122.682555	28.378560
311.338054	14148.699923	28.383578
311.484845	14169.261572	28.388596
311.893238	14191.377103	28.393613
312.151160	14213.568233	28.398631
312.505940	14226.986559	28.403648
312.594472	14258.208151	28.408666
312.633153	14281.190040	28.413684
313.434172	14302.226895	28.418701
313.382749	14338.533912	28.423719
313.837062	14369.928092	28.428736
314.332326	14388.556894	28.433754
314.444275	14421.260466	28.438772
314.783820	14446.683741	28.443789
314.900204	14480.059411	28.448807
315.413992	14510.052003	28.453824
315.977990	14542.818802	28.458842
316.275592	14568.966816	28.463860
316.737078	14585.812074	28.468877
316.917865	14614.011793	28.473895
317.171434	14630.495440	28.478912
317.810950	14654.804660	28.483930
317.770296	14688.346428	28.488948
318.214805	14705.050754	28.493965
318.414821	14746.008014	28.498983
318.943893	14759.024307	28.504000
319.618537	14775.707191	28.509018
319.614861	14802.501325	28.514036
320.425159	14812.012150	28.519053
320.903031	14828.693976	28.524071
321.329915	14837.622745	28.529088
321.517324	14847.175095	28.534106
321.653738	14863.766129	28.539124
322.159082	14865.937234	28.544141
322.684172	14889.937178	28.549159
322.856479	14900.197927	28.554176
323.125610	14916.529432	28.559194
323.256639	14941.282274	28.564212
323.601679	14944.864292	28.569229
323.665049	14966.173918	28.574247
323.948575	14987.803244	28.579264
324.602894	15011.912779	28.584282
324.491958	15034.894251	28.589300
324.793092	15052.024386	28.594317
325.088153	15086.982435	28.599335
325.409617	15105.346065	28.604352
325.616275	15133.793259	28.609370
326.054720	15144.943279	28.614388
326.821679	15168.431976	28.619405
327.078296	15191.415923	28.624423
327.076523	15210.399886	28.629440
327.533872	15226.180463	28.634458
327.811467	15258.042146	28.639476
328.448979	15280.541293	28.644493
328.434056	15305.896520	28.649511
328.692924	15314.386481	28.654528
329.377112	15335.168037	28.659546
329.109153	15344.706861	28.664564
329.780196	15361.999813	28.669581
329.799317	15389.984932	28.674599
329.964271	15413.865363	28.679616
330.616340	15435.269884	28.684634
330.990861	15458.283958	28.689652
331.322914	15471.715856	28.694669
331.246968	15508.208646	28.699687
331.347395	15525.128912	28.704704
332.142068	15551.031403	28.709722
331.852552	15585.829551	28.714740
333.187166	15590.845410	28.719757
333.910394	15609.191282	28.724775
334.166754	15630.123589	28.729792
334.450446	15635.519895	28.734810
334.722341	15664.953192	28.739828
334.725637	15671.328304	28.744845
334.864172	15697.050803	28.749863
335.419910	15719.053072	28.754880
335.707875	15743.854332	28.759898
335.629738	15772.576011	28.764916
335.986794	15798.661831	28.769933
336.307144	15822.452689	28.774951
336.515982	15859.947434	28.779968
336.862177	15881.547168	28.784986
336.986464	15919.003766	28.790004
337.450098	15946.264029	28.795021
337.949993	15980.194848	28.800039
337.964856	16013.404122	28.805056
338.538581	16037.747773	28.810074
338.697515	16073.232349	28.815092
339.166580	16102.130991	28.820109
339.263021	16141.119147	28.825127
339.463867	16177.177528	28.830144
340.418867	16210.377944	28.835162
340.392354	16252.061450	28.840180
341.184749	16279.037853	28.845197
341.233380	16309.141154	28.850215
341.137418	16338.988255	28.855232
342.158356	16363.487510	28.860250
342.361040	16401.696680	28.865268
342.975442	16428.517082	28.870285
343.318739	16460.695356	28.875303
343.785135	16483.806548	28.880320
344.398096	16501.730750	28.885338
344.567547	16521.292425	28.890356
345.004961	16540.263248	28.895373
345.446719	16566.211685	28.900391
345.485622	16587.644665	28.905408
345.793225	16614.766620	28.910426
346.181147	16637.261668	28.915444
346.230846	16650.963980	28.920461
346.669714	16677.599422	28.925479
346.732531	16707.163095	28.930496
347.397872	16736.932361	28.935514
347.495010	16758.857438	28.940532
347.788924	16785.779332	28.945549
347.935663	16818.811459	28.950567
348.208281	16848.427593	28.955584
348.844385	16873.216331	28.960602
349.076180	16909.234285	28.965620
349.434810	16940.388353	28.970637
350.017363	16955.133505	28.975655
350.072981	16994.374198	28.980672
350.742100	17012.285125	28.985690
351.202654	17043.058222	28.990708
351.591884	17063.595734	28.995725
352.219643	17075.175922	29.000743
352.495185	17109.000889	29.005760
353.134417	17119.224833	29.010778
353.250588	17148.057069	29.015796
353.556151	17167.208918	29.020813
354.140343	17180.730864	29.025831
354.018556	17213.957205	29.030848
354.522052	17230.210418	29.035866
354.686634	17259.635510	29.040884
354.868677	17289.716899	29.045901
355.512455	17311.555062	29.050919
355.522046	17344.134003	29.055936
356.137897	17366.390849	29.060954
356.292561	17393.593853	29.065972
356.645831	17424.274178	29.070989
357.388852	17447.341159	29.076007
357.750428	17476.534886	29.081024
358.216056	17498.425716	29.086042
358.396077	17518.022792	29.091060
358.786245	17534.708938	29.096077
359.305513	17560.368356	29.101095
359.192729	17597.201850	29.106112
360.119535	17608.029493	29.111130
360.417557	17637.399393	29.116148
360.307001	17667.158070	29.121165
361.224990	17688.891656	29.126183
361.587150	17702.428182	29.131200
362.017018	17729.224938	29.136218
362.590552	17756.489785	29.141236
363.026127	17775.877965	29.146253
363.258717	17787.317135	29.151271
363.228937	17810.534573	29.156288
363.831235	17825.035291	29.161306
364.314439	17853.607599	29.166324
364.075483	17877.018308	29.171341
364.701074	17891.974428	29.176359
365.124973	17924.134634	29.181376
365.366163	17945.966979	29.186394
365.706622	17973.914227	29.191412
365.631047	18008.591196	29.196429
366.152950	18029.069874	29.201447
366.603445	18059.146593	29.206464
366.805903	18076.811268	29.211482
367.185819	18099.210308	29.216500
367.495451	18122.108378	29.221517
368.052248	18135.330803	29.226535
368.471522	18168.353282	29.231552
368.658291	18186.377277	29.236570
369.075188	18215.609644	29.241588
369.430124	18243.822397	29.246605
369.750886	18265.887004	29.251623
369.668993	18296.577763	29.256640
370.328096	18326.122931	29.261658
370.654265	18343.697723	29.266676
370.972719	18384.054989	29.271693
371.579804	18408.613999	29.276711
371.751201	18437.610698	29.281728
372.058653	18461.364757	29.286746
372.432247	18493.366829	29.291764
373.128081	18525.208957	29.296781
373.541878	18560.393448	29.301799
373.739279	18598.064164	29.306816
373.964297	18624.702974	29.311834
374.847713	18649.667565	29.316852
375.023810	18667.851305	29.321869
375.847774	18692.927806	29.326887
376.278425	18721.079752	29.331904
376.657944	18747.820538	29.336922
376.662688	18765.564351	29.341940
376.889903	18790.115199	29.346957
377.566799	18814.945239	29.351975
377.447976	18847.351320	29.356992
377.654058	18871.878103	29.362010
377.981526	18906.001481	29.367028
378.569302	18943.844702	29.372045
379.244053	18971.938520	29.377063
379.730887	19016.053896	29.382080
380.061155	19029.919520	29.387098
380.480068	19056.155707	29.392116
380.442006	19086.988682	29.397133
381.101633	19110.894324	29.402151
381.396883	19143.310243	29.407168
381.775347	19177.837537	29.412186
382.464039	19207.021372	29.417204
382.611266	19241.847484	29.422221
382.944263	19267.613426	29.427239
383.159159	19309.000298	29.432256
383.796243	19324.557204	29.437274
384.033583	19349.197089	29.442292
384.208656	19384.361236	29.447309
384.723905	19408.874644	29.452327
385.175267	19446.985726	29.457344
385.527491	19481.226113	29.462362
385.985263	19510.246504	29.467380
386.310149	19550.164774	29.472397
386.922071	19574.903615	29.477415
387.102710	19602.874525	29.482432
387.299219	19620.975407	29.487450
387.402392	19665.240370	29.492468
387.721864	19694.261876	29.497485
388.289684	19719.884445	29.502503
388.691288	19758.829109	29.507520
389.173116	19796.411327	29.512538
389.583427	19826.482112	29.517556
389.759820	19861.509703	29.522573
390.200669	19886.608617	29.527591
390.702407	19924.851043	29.532608
391.322388	19952.819120	29.537626
391.594280	19978.753078	29.542644
391.436035	20016.016889	29.547661
392.067563	20043.137904	29.552679
392.554368	20084.294106	29.557696
393.040351	20118.069239	29.562714
393.354358	20155.393587	29.567732
393.522219	20199.040611	29.572749
393.807604	20237.204476	29.577767
394.259823	20278.999860	29.582784
394.413410	20315.924891	29.587802
395.248035	20357.091360	29.592820
395.382344	20401.037248	29.597837
396.326105	20429.102250	29.602855
396.681613	20468.894340	29.607872
397.006366	20515.223968	29.612890
398.020979	20532.727369	29.617908
398.153772	20561.099801	29.622925
398.682607	20586.689051	29.627943
398.757629	20616.301697	29.632960
399.007393	20646.816635	29.637978
399.534801	20673.339481	29.642996
399.820249	20718.827797	29.648013
400.557470	20747.983154	29.653031
400.802051	20781.426461	29.658048
400.845530	20819.383783	29.663066
401.495314	20854.050315	29.668084
401.507095	20899.969441	29.673101
401.953805	20934.744899	29.678119
402.360712	20978.668657	29.683136
402.658865	21012.312619	29.688154
403.259632	21047.292958	29.693172
403.633272	21088.616308	29.698189
404.539409	21116.453846	29.703207
404.864497	21143.815394	29.708224
405.307689	21177.774465	29.713242
406.206104	21201.918941	29.718260
406.299573	21236.875783	29.723277
406.875523	21257.704891	29.728295
407.280748	21294.338530	29.733312
407.678109	21324.397318	29.738330
408.248132	21343.119953	29.743348
408.106945	21383.484936	29.748365
408.304713	21409.592155	29.753383
408.727202	21441.651533	29.758400
409.051379	21478.424525	29.763418
409.452133	21500.884584	29.768436
409.600579	21541.314874	29.773453
410.107998	21577.234307	29.778471
410.535795	21614.204540	29.783488
410.968776	21647.021893	29.788506
411.335126	21675.385110	29.793524
411.649032	21717.867927	29.798541
411.820605	21746.070920	29.803559
412.301317	21787.947683	29.808576
412.713608	21836.711145	29.813594
413.033633	21873.010012	29.818612
413.462518	21919.444530	29.823629
413.795063	21958.352483	29.828647
414.623723	21998.890584	29.833664
414.877013	22038.292585	29.838682
415.719191	22076.237517	29.843700
415.638483	22120.510717	29.848717
416.169232	22153.175715	29.853735
416.869315	22196.826175	29.858752
417.029622	22234.096451	29.863770
417.639656	22263.772657	29.868788
418.073360	22299.232910	29.873805
418.352067	22341.439468	29.878823
418.792195	22378.265392	29.883840
419.280856	22421.086924	29.888858
419.930171	22447.363354	29.893876
420.122213	22489.575451	29.898893
420.781310	22535.560810	29.903911
421.341242	22553.634339	29.908928
421.778814	22590.033481	29.913946
422.315193	22619.139244	29.918964
422.650262	22657.960301	29.923981
423.247084	22683.034894	29.928999
423.758074	22722.876425	29.934016
424.036000	22749.641002	29.939034
424.599506	22782.665972	29.944052
424.761992	22812.952472	29.949069
425.201584	22840.144340	29.954087
426.240817	22868.157539	29.959104
426.264190	22913.787660	29.964122
426.437867	22932.053121	29.969140
426.969152	22970.757831	29.974157
427.091989	22992.688519	29.979175
427.396873	23033.490732	29.984192
427.559583	23082.556145	29.989210
428.225313	23110.536337	29.994228
428.548139	23156.217902	29.999245
428.651101	23205.182940	30.004263
429.445273	23243.252536	30.009280
429.669668	23280.243316	30.014298
430.447682	23319.376653	30.019316
430.552220	23356.709649	30.024333
431.178648	23391.856508	30.029351
431.946208	23424.647876	30.034368
432.582861	23451.094980	30.039386
433.029887	23484.944973	30.044404
433.482545	23521.363542	30.049421
433.397802	23550.159591	30.054439
434.214447	23569.023597	30.059456
434.509684	23605.972342	30.064474
434.810196	23631.231126	30.069492
435.169597	23668.997648	30.074509
435.528300	23697.342077	30.079527
436.224302	23731.928013	30.084544
436.367100	23766.173656	30.089562
437.667292	23783.057827	30.094580
438.135894	23817.540758	30.099597
438.085776	23849.979631	30.104615
439.230818	23871.363499	30.109632
439.178173	23897.765986	30.114650
439.498099	23927.538794	30.119668
439.917536	23956.984662	30.124685
440.143124	23992.814267	30.129703
440.515999	24013.888897	30.134720
440.860246	24053.677625	30.139738
441.356784	24086.546623	30.144756
441.772623	24127.004706	30.149773
442.020797	24158.831900	30.154791
442.975275	24182.282774	30.159808
443.304524	24227.541817	30.164826
443.557651	24253.102166	30.169844
443.810558	24289.479484	30.174861
444.492055	24336.863903	30.179879
444.971436	24372.318361	30.184896
445.118699	24416.463952	30.189914
445.805757	24441.868037	30.194932
445.849951	24492.960640	30.199949
446.338965	24527.393017	30.204967
447.790186	24559.163266	30.209984
448.076398	24595.038131	30.215002
448.743424	24634.786341	30.220020
449.100053	24652.150250	30.225037
449.723866	24676.599814	30.230055
450.423293	24701.799109	30.235072
450.702819	24730.547920	30.240090
451.059143	24757.015076	30.245108
451.495463	24776.973050	30.250125
451.405290	24805.349998	30.255143
451.902805	24833.719238	30.260160
452.318455	24873.900385	30.265178
452.739454	24905.978034	30.270196
453.115007	24945.251965	30.275213
453.444822	24978.596016	30.280231
454.065800	25007.375218	30.285248
454.432259	25059.816549	30.290266
454.350453	25091.546921	30.295284
455.002535	25131.787157	30.300301
455.161168	25184.625947	30.305319
455.865001	25217.378388	30.310336
455.987018	25262.798630	30.315354
456.306739	25302.815738	30.320372
456.990790	25344.583619	30.325389
457.158471	25387.417792	30.330407
457.475448	25422.964264	30.335424
457.402256	25470.007486	30.340442
458.490224	25526.328623	30.345460
459.159705	25571.074055	30.350477
459.324729	25621.022120	30.355495
460.188379	25671.286813	30.360512
460.359913	25716.924181	30.365530
460.888111	25761.143566	30.370548
461.602836	25817.527550	30.375565
461.543757	25863.536095	30.380583
462.187894	25906.005055	30.385600
462.534353	25965.970453	30.390618
463.136604	26016.408643	30.395636
463.653776	26058.235692	30.400653
463.950208	26111.369123	30.405671
464.322270	26157.836081	30.410688
465.007568	26214.433339	30.415706
465.688281	26264.417060	30.420724
466.372100	26313.399130	30.425741
466.364547	26362.125939	30.430759
466.819703	26404.813036	30.435776
467.155568	26461.117036	30.440794
467.795678	26503.566159	30.445812
468.684340	26561.659832	30.450829
468.893927	26607.634793	30.455847
469.741664	26650.657069	30.460864
469.877454	26702.987669	30.465882
470.535483	26744.826367	30.470900
471.026620	26787.910544	30.475917
471.406746	26835.143949	30.480935
472.277717	26876.911253	30.485952
472.331973	26929.433627	30.490970
473.150984	26974.695672	30.495988
473.781835	27007.166378	30.501005
474.363268	27056.544400	30.506023
475.189366	27082.452879	30.511040
475.171738	27118.076096	30.516058
476.266063	27161.917644	30.521076
476.372714	27195.501173	30.526093
476.884376	27233.425960	30.531111
477.522346	27256.988507	30.536128
478.219275	27291.141584	30.541146
478.421450	27329.252985	30.546164
478.995204	27356.992131	30.551181
479.149907	27400.421472	30.556199
479.902554	27433.431447	30.561216
480.249756	27473.849026	30.566234
480.636587	27499.864394	30.571252
480.931034	27546.820442	30.576269
481.472099	27578.463578	30.581287
482.135428	27598.797024	30.586304
482.674071	27640.902097	30.591322
482.928787	27673.432487	30.596340
483.899647	27696.583378	30.601357
483.846340	27736.923595	30.606375
484.309605	27771.740491	30.611392
484.484434	27806.274072	30.616410
485.029928	27838.632413	30.621428
485.715024	27874.740999	30.626445
485.773221	27915.754090	30.631463
486.557868	27951.534985	30.636480
486.741037	27997.493683	30.641498
487.174344	28050.577814	30.646516
487.723996	28088.990208	30.651533
487.870511	28137.441755	30.656551
488.278945	28179.491756	30.661568
488.687599	28237.246398	30.666586
489.308449	28289.924818	30.671604
490.358119	28335.610928	30.676621
490.720763	28383.518214	30.681639
491.473456	28416.563285	30.686656
492.073423	28450.322968	30.691674
492.172764	28495.005818	30.696692
493.320750	28525.618082	30.701709
493.529380	28568.792980	30.706727
494.125298	28615.488211	30.711744
494.755512	28652.784437	30.716762
495.358837	28681.479268	30.721780
495.977695	28715.636763	30.726797
496.318430	28757.286171	30.731815
496.738241	28785.225636	30.736832
497.234236	28830.976125	30.741850
497.357944	28876.376316	30.746868
497.870103	28916.147169	30.751885
498.257484	28966.704444	30.756903
498.561337	29014.280988	30.761920
499.074186	29056.097579	30.766938
499.971431	29098.442435	30.771956
500.149354	29146.832103	30.776973
500.556070	29200.182676	30.781991
501.120719	29241.871725	30.787008
501.785624	29286.498179	30.792026
501.673658	29349.086360	30.797044
502.563312	29391.857113	30.802061
502.827278	29448.684093	30.807079
503.093017	29503.441782	30.812096
503.674570	29555.315805	30.817114
504.459929	29606.226145	30.822132
505.251119	29643.374504	30.827149
505.834037	29700.597552	30.832167
506.606280	29730.069492	30.837184
507.289056	29779.742251	30.842202
507.595579	29825.776293	30.847220
508.734979	29859.122028	30.852237
508.915528	29891.832574	30.857255
509.335362	29932.139111	30.862272
509.914261	29966.486836	30.867290
510.203656	29998.999021	30.872308
510.939023	30022.690348	30.877325
511.139386	30071.654419	30.882343
511.635247	30105.360051	30.887360
511.978598	30141.879563	30.892378
512.046148	30181.087620	30.897396
512.431770	30222.659549	30.902413
512.872280	30274.225786	30.907431
513.404678	30315.509803	30.912448
513.800738	30370.886352	30.917466
514.250890	30426.976292	30.922484
514.951472	30471.945459	30.927501
515.584845	30524.358038	30.932519
516.045407	30573.323140	30.937536
516.874857	30623.561391	30.942554
517.230029	30675.509704	30.947572
518.122266	30710.215707	30.952589
518.634219	30759.067584	30.957607
519.219362	30800.678549	30.962624
519.317345	30843.757305	30.967642
519.803066	30894.111026	30.972660
520.755443	30932.120824	30.977677
521.125049	30985.661233	30.982695
521.618395	31017.684316	30.987712
522.651889	31066.077355	30.992730
522.544344	31110.844440	30.997748
523.091052	31149.020226	31.002765
523.471239	31208.752158	31.007783
524.248519	31261.604397	31.012800
525.138425	31312.873789	31.017818
525.083266	31360.325207	31.022836
525.952795	31411.629675	31.027853
526.343458	31457.970126	31.032871
526.570572	31512.718617	31.037888
527.270742	31552.864706	31.042906
527.387029	31612.646442	31.047924
528.367886	31653.250859	31.052941
529.008453	31699.188097	31.057959
529.841496	31749.049375	31.062976
530.472993	31790.847759	31.067994
530.948147	31841.853870	31.073012
531.288713	31880.209197	31.078029
532.372988	31927.058352	31.083047
532.352460	31971.399381	31.088064
533.172616	32005.649913	31.093082
533.493411	32054.841869	31.098100
534.222224	32101.628348	31.103117
534.670926	32143.371629	31.108135
535.234299	32177.973928	31.113152
535.871014	32228.567760	31.118170
535.861749	32280.525598	31.123188
536.671102	32313.284250	31.128205
537.022887	32372.922476	31.133223
537.564339	32414.222940	31.138240
538.118925	32451.669133	31.143258
538.263476	32502.584931	31.148276
538.832222	32551.286499	31.153293
539.093859	32600.661313	31.158311
539.514977	32642.266812	31.163328
540.284686	32691.934546	31.168346
540.685220	32757.945454	31.173364
541.170534	32798.554390	31.178381
541.693626	32846.720293	31.183399
542.334813	32908.484865	31.188416
542.919063	32948.533025	31.193434
543.120104	33020.623317	31.198452
543.957142	33071.362794	31.203469
544.130863	33121.290674	31.208487
544.852658	33186.208623	31.213504
545.395734	33241.145812	31.218522
545.601756	33312.483110	31.223540
546.154266	33370.409470	31.228557
546.724757	33441.206924	31.233575
547.338014	33507.070289	31.238592
548.113527	33557.890414	31.243610
548.560009	33629.611657	31.248628
549.053704	33689.042860	31.253645
549.709371	33756.081136	31.258663
550.387002	33810.209032	31.263680
551.126684	33859.809390	31.268698
551.631551	33930.717117	31.273716
552.477512	33981.601410	31.278733
553.242995	34035.943046	31.283751
553.523586	34086.274545	31.288768
554.061684	34143.256919	31.293786
554.719479	34200.322891	31.298804
555.379564	34248.370159	31.303821
556.123596	34305.618230	31.308839
556.378429	34370.917852	31.313856
557.164016	34412.116632	31.318874
558.061135	34470.095987	31.323892
558.632726	34517.095625	31.328909
559.434116	34566.462838	31.333927
559.846541	34609.621126	31.338944
560.892354	34637.975303	31.343962
561.306215	34684.519724	31.348980
561.544029	34726.867462	31.353997
562.011943	34777.302060	31.359015
562.396221	34829.793204	31.364032
563.252269	34864.270955	31.369050
563.404717	34913.149803	31.374068
563.840390	34968.625308	31.379085
564.660957	35014.292424	31.384103
565.274450	35062.037323	31.389120
565.944304	35113.884822	31.394138
566.390359	35162.902088	31.399156
566.783317	35210.903242	31.404173
567.239213	35254.890235	31.409191
567.619622	35308.330967	31.414208
568.401457	35352.234779	31.419226
568.482094	35407.473478	31.424244
568.748362	35454.874368	31.429261
569.511590	35509.698855	31.434279
569.962749	35567.051503	31.439296
570.716349	35623.514319	31.444314
570.999781	35682.566763	31.449332
571.521668	35737.072560	31.454349
572.455669	35797.346087	31.459367
572.644167	35868.159508	31.464384
573.267075	35919.599198	31.469402
573.818563	35992.228274	31.474420
574.203824	36054.396849	31.479437
574.936480	36117.945005	31.484455
575.129373	36187.042189	31.489472
575.972091	36251.725800	31.494490
576.909915	36315.517933	31.499508
577.516322	36370.389132	31.504525
578.192700	36438.377685	31.509543
578.880581	36493.263113	31.514560
579.654722	36546.463780	31.519578
580.053391	36605.630401	31.524596
580.751680	36654.638665	31.529613
581.770704	36706.561620	31.534631
582.112865	36761.236532	31.539648
582.634351	36813.954842	31.544666
583.073371	36880.516717	31.549684
583.490751	36939.128131	31.554701
583.997587	36994.299443	31.559719
584.623995	37057.808164	31.564736
585.266663	37109.030775	31.569754
585.594325	37181.987587	31.574772
586.085910	37254.106623	31.579789
586.779251	37311.280028	31.584807
587.096102	37375.313823	31.589824
588.037081	37447.417303	31.594842
588.195149	37508.823319	31.599860
588.929142	37584.052249	31.604877
589.405617	37648.840552	31.609895
590.140512	37724.566628	31.614912
591.226660	37789.107015	31.619930
591.820657	37854.247921	31.624948
592.139285	37913.758261	31.629965
593.326476	37965.361895	31.634983
593.911383	38026.388046	31.640000
594.344929	38074.144939	31.645018
595.248049	38133.936664	31.650036
595.683818	38190.679463	31.655053
596.478534	38249.288945	31.660071
596.905788	38312.767877	31.665088
597.800279	38353.560087	31.670106
598.407239	38420.098131	31.675124
598.869575	38478.584738	31.680141
599.449777	38517.765460	31.685159
599.668879	38575.002895	31.690176
600.236394	38620.447333	31.695194
600.811730	38670.715671	31.700212
601.319416	38717.918575	31.705229
601.988859	38768.834478	31.710247
602.423545	38835.281748	31.715264
603.084840	38886.205608	31.720282
603.543067	38949.093834	31.725300
603.888949	39016.131495	31.730317
604.884653	39070.955789	31.735335
605.490322	39125.304666	31.740352
606.080740	39184.244786	31.745370
606.538217	39245.817557	31.750388
607.282343	39305.246099	31.755405
607.795437	39357.879064	31.760423
608.186728	39426.517941	31.765440
609.134874	39488.007147	31.770458
609.459784	39558.445309	31.775476
609.740700	39619.604443	31.780493
610.571491	39682.346169	31.785511
610.850451	39763.759831	31.790528
611.546820	39836.934270	31.795546
612.372898	39909.304640	31.800564
612.645439	39970.198287	31.805581
613.483580	40046.528555	31.810599
613.768231	40116.861893	31.815616
614.578772	40186.865776	31.820634
614.999562	40263.324972	31.825652
615.928140	40340.958911	31.830669
616.734251	40407.816794	31.835687
617.521079	40483.524824	31.840704
618.139998	40553.087629	31.845722
618.703627	40624.309048	31.850740
619.022171	40697.645112	31.855757
619.698974	40762.872287	31.860775
620.441487	40844.007535	31.865792
620.507099	40914.057319	31.870810
621.410759	40981.349782	31.875828
621.926318	41071.091764	31.880845
622.873620	41136.491764	31.885863
623.375967	41220.329068	31.890880
623.905331	41288.549711	31.895898
624.939203	41362.355065	31.900916
625.853598	41422.692749	31.905933
626.581083	41479.111439	31.910951
627.150949	41560.703377	31.915968
628.062176	41612.898239	31.920986
628.971078	41675.420362	31.926004
629.380370	41742.211011	31.931021
629.873773	41803.210054	31.936039
630.498568	41868.907074	31.941056
630.984759	41932.194517	31.946074
631.761227	41987.307542	31.951092
632.230526	42057.054827	31.956109
633.073631	42103.839902	31.961127
633.463121	42180.277926	31.966144
634.098216	42229.162502	31.971162
634.590552	42285.015661	31.976180
634.747701	42356.567639	31.981197
635.310581	42413.605457	31.986215
635.939751	42474.569488	31.991232
636.622253	42551.066591	31.996250
637.431872	42614.670944	32.001268
637.838061	42690.531325	32.006285
638.767976	42745.407848	32.011303
639.498143	42820.110032	32.016320
640.173055	42879.730757	32.021338
640.863137	42948.484403	32.026356
640.801888	43029.215382	32.031373
641.457907	43088.448689	32.036391
642.455112	43169.245214	32.041408
643.098513	43243.287993	32.046426
643.895318	43309.079823	32.051444
644.606909	43377.390124	32.056461
645.284977	43439.065838	32.061479
646.003098	43519.110351	32.066496
646.813218	43574.636329	32.071514
647.464325	43638.272842	32.076532
647.707873	43709.258303	32.081549
648.225521	43784.897532	32.086567
649.145806	43852.630741	32.091584
649.981249	43917.992866	32.096602
651.267967	43970.942654	32.101620
651.738950	44032.697618	32.106637
652.818768	44092.207576	32.111655
653.353857	44153.189348	32.116672
654.025386	44220.521956	32.121690
654.904895	44267.341800	32.126708
654.919824	44327.145147	32.131725
655.466056	44387.315221	32.136743
656.745463	44445.248830	32.141760
657.590006	44508.018592	32.146778
657.955738	44564.993938	32.151796
658.478730	44635.074299	32.156813
659.182705	44688.494475	32.161831
659.544779	44753.490300	32.166848
660.072817	44800.493731	32.171866
660.825277	44859.525292	32.176884
661.062180	44942.476476	32.181901
661.618690	45012.439445	32.186919
662.308754	45080.788266	32.191936
662.743553	45155.433958	32.196954
663.585644	45230.011965	32.201972
663.976085	45307.018855	32.206989
664.783888	45384.148924	32.212007
665.227341	45466.697437	32.217024
665.582266	45546.260156	32.222042
666.191012	45622.965515	32.227060
666.702489	45711.167363	32.232077
667.298619	45797.731396	32.237095
668.168732	45881.785081	32.242112
668.991198	45955.889761	32.247130
670.023407	46021.670142	32.252148
670.480376	46097.360610	32.257165
671.293165	46170.089016	32.262183
672.192868	46230.972670	32.267200
672.437510	46300.384684	32.272218
673.260009	46371.392903	32.277236
673.776732	46464.046274	32.282253
674.056759	46532.355620	32.287271
674.959476	46620.206328	32.292288
675.502254	46706.133394	32.297306
676.567111	46770.712461	32.302324
677.183382	46860.812228	32.307341
678.027493	46923.215273	32.312359
678.957074	46998.206508	32.317376
679.655544	47076.825409	32.322394
680.811556	47141.101052	32.327412
680.979292	47215.255339	32.332429
681.740788	47292.297050	32.337447
682.640699	47358.538921	32.342464
682.829376	47431.239393	32.347482
683.634638	47502.526273	32.352500
684.139711	47579.543804	32.357517
685.041055	47661.556440	32.362535
686.223519	47732.162610	32.367552
686.272310	47824.695697	32.372570
687.267707	47879.751498	32.377588
687.499424	47978.065144	32.382605
687.867616	48045.047394	32.387623
688.854263	48131.914128	32.392640
689.485372	48222.488628	32.397658
690.111808	48310.262374	32.402676
690.745910	48398.783159	32.407693
691.440707	48477.513006	32.412711
692.218431	48563.427482	32.417728
692.727978	48660.905518	32.422746
693.700521	48746.344950	32.427764
694.561806	48825.529464	32.432781
695.218932	48900.206117	32.437799
696.398236	48976.983544	32.442816
697.047595	49063.444688	32.447834
697.860489	49131.341600	32.452852
698.644658	49219.293528	32.457869
699.193291	49284.159617	32.462887
700.093869	49357.619265	32.467904
700.357577	49442.723652	32.472922
701.496234	49492.810587	32.477940
702.063600	49584.301519	32.482957
702.646943	49668.270575	32.487975
703.521778	49736.289316	32.492992
704.035671	49826.022857	32.498010
704.741723	49895.848854	32.503028
704.712023	49989.320834	32.508045
705.618900	50055.151975	32.513063
706.482330	50137.393520	32.518080
707.015521	50217.062476	32.523098
707.654864	50296.544479	32.528116
708.318437	50367.123830	32.533133
708.795519	50454.584798	32.538151
709.653840	50525.446188	32.543168
709.946876	50626.084168	32.548186
710.686419	50695.885869	32.553204
711.322275	50790.568882	32.558221
712.278365	50881.389188	32.563239
712.808835	50956.571142	32.568256
713.604645	51054.221810	32.573274
714.637505	51133.177815	32.578292
715.412025	51219.850384	32.583309
716.289597	51314.756466	32.588327
716.846778	51398.308603	32.593344
717.274580	51491.283217	32.598362
718.000397	51578.242989	32.603380
718.858876	51653.290433	32.608397
719.480031	51738.800126	32.613415
720.533365	51834.391064	32.618432
720.799834	51928.365662	32.623450
721.980519	52009.602713	32.628468
722.736933	52084.232673	32.633485
723.532486	52186.699319	32.638503
724.530616	52257.845119	32.643520
726.042720	52320.845623	32.648538
726.955738	52402.947639	32.653556
727.702766	52475.159998	32.658573
727.917905	52548.678731	32.663591
728.902952	52613.127601	32.668608
729.322165	52706.207688	32.673626
730.171362	52773.809645	32.678644
730.755580	52856.048122	32.683661
731.286161	52933.040479	32.688679
732.127446	53010.798000	32.693696
732.619211	53092.847119	32.698714
733.546963	53170.004506	32.703732
734.571316	53246.035852	32.708749
734.988189	53330.951203	32.713767
736.227885	53398.998334	32.718784
736.579791	53479.767934	32.723802
737.749495	53542.644153	32.728820
738.754492	53610.356999	32.733837
739.436703	53678.295078	32.738855
740.558770	53748.495911	32.743872
741.163623	53816.232192	32.748890
741.622399	53867.361228	32.753908
742.593755	53955.189755	32.758925
742.907055	54033.297688	32.763943
744.075610	54083.171742	32.768960
744.347825	54163.584616	32.773978
745.400130	54228.921793	32.778996
746.154167	54299.956663	32.784013
746.566466	54354.165656	32.789031
747.388464	54419.275039	32.794048
747.938653	54488.304037	32.799066
748.434156	54551.193224	32.804084
749.249864	54632.651664	32.809101
749.740798	54703.707894	32.814119
750.226814	54774.803062	32.819136
750.363836	54867.238397	32.824154
751.148775	54943.419125	32.829172
752.036095	55023.330684	32.834189
752.519514	55122.479788	32.839207
753.202117	55202.304767	32.844224
753.678077	55302.873334	32.849242
754.794632	55398.927555	32.854260
755.201803	55498.037167	32.859277
755.820416	55603.758379	32.864295
756.745401	55704.535460	32.869312
757.228437	55812.331281	32.874330
757.872006	55908.690744	32.879348
758.887299	56006.175308	32.884365
759.248943	56121.748297	32.889383
760.188185	56220.126829	32.894400
760.797093	56338.120922	32.899418
761.847014	56441.281302	32.904436
762.733751	56545.686760	32.909453
763.428197	56658.343771	32.914471
764.653536	56771.447316	32.919488
765.224227	56870.730868	32.924506
766.040466	56972.577131	32.929524
766.798274	57082.603289	32.934541
767.320837	57178.792936	32.939559
768.348349	57281.993160	32.944576
769.396003	57373.235419	32.949594
770.666449	57473.102199	32.954612
771.625856	57566.408325	32.959629
771.967179	57673.274711	32.964647
773.253975	57742.845881	32.969664
774.186438	57852.899338	32.974682
774.739020	57923.437292	32.979700
775.854536	58013.942639	32.984717
776.889660	58087.791928	32.989735
777.997385	58172.203003	32.994752
778.958316	58250.304705	32.999770
779.947021	58317.248273	33.004788
780.636099	58385.025896	33.009805
781.202835	58468.166870	33.014823
782.069661	58533.097428	33.019840
782.805949	58613.443255	33.024858
783.379870	58686.948440	33.029876
783.863754	58765.194540	33.034893
784.451799	58847.601354	33.039911
785.021952	58940.430161	33.044928
785.458339	59027.591407	33.049946
786.347377	59118.883296	33.054964
787.133872	59213.462869	33.059981
787.864298	59303.356987	33.064999
788.497308	59379.491820	33.070016
789.269746	59462.623439	33.075034
789.742238	59555.076188	33.080052
790.586721	59639.112746	33.085069
791.212576	59747.132913	33.090087
792.068304	59834.550076	33.095104
792.554228	59945.621568	33.100122
793.538876	60035.570313	33.105140
794.336800	60126.509061	33.110157
794.553425	60230.751432	33.115175
795.689811	60329.480341	33.120192
796.368629	60435.819451	33.125210
797.151920	60542.774032	33.130228
797.994445	60632.331477	33.135245
799.118011	60743.732472	33.140263
800.358386	60833.363329	33.145280
800.432458	60935.349409	33.150298
801.542653	61045.402895	33.155316
802.208697	61153.835252	33.160333
802.775028	61260.007477	33.165351
804.032727	61359.309810	33.170368
804.773316	61464.880770	33.175386
805.311431	61573.013823	33.180404
806.295169	61669.446885	33.185421
806.912681	61785.907920	33.190439
807.879959	61877.620769	33.195456
809.051073	61990.085722	33.200474
809.724527	62093.539423	33.205492
810.748751	62187.429869	33.210509
811.468533	62296.144438	33.215527
812.550039	62391.694085	33.220544
813.325771	62499.753574	33.225562
814.067602	62607.241193	33.230580
815.238801	62693.696195	33.235597
815.795676	62800.071207	33.240615
816.928314	62903.544676	33.245632
817.760430	62994.858143	33.250650
818.189528	63095.109897	33.255668
819.190574	63182.794216	33.260685
819.535743	63306.943794	33.265703
820.481475	63396.204239	33.270720
821.330080	63504.008370	33.275738
822.059058	63614.968034	33.280756
822.954613	63707.929617	33.285773
823.851456	63827.396735	33.290791
824.540224	63927.567335	33.295808
825.371187	64036.169954	33.300826
826.123976	64147.580532	33.305844
827.040801	64254.743279	33.310861
828.151004	64362.065339	33.315879
828.752761	64462.378918	33.320896
829.842496	64569.812779	33.325914
830.102695	64669.382790	33.330932
831.404714	64768.755934	33.335949
832.224363	64870.454998	33.340967
833.330172	64973.991357	33.345984
834.030667	65058.952909	33.351002
834.556439	65150.126482	33.356020
835.619430	65246.208199	33.361037
835.961545	65344.764353	33.366055
837.045019	65447.558313	33.371072
837.547801	65548.228105	33.376090
838.372143	65649.684206	33.381108
838.957863	65749.018511	33.386125
839.572887	65876.322260	33.391143
840.468930	65982.967372	33.396160
841.174920	66093.067023	33.401178
842.012907	66215.947360	33.406196
842.831841	66322.552929	33.411213
843.291620	66446.976232	33.416231
844.259164	66570.274074	33.421248
845.642959	66683.288730	33.426266
846.698974	66793.800974	33.431284
847.905418	66895.370224	33.436301
848.754078	67016.996865	33.441319
849.708004	67121.405962	33.446336
850.577081	67231.912556	33.451354
851.294926	67338.988337	33.456372
852.193613	67444.235518	33.461389
853.342101	67552.665327	33.466407
853.750334	67663.089783	33.471424
855.339315	67756.731314	33.476442
856.142034	67867.631130	33.481460
857.496647	67960.729745	33.486477
857.899059	68067.006888	33.491495
858.848029	68148.723760	33.496512
859.946433	68250.241494	33.501530
860.333982	68363.585584	33.506548
862.382463	68434.812160	33.511565
863.444309	68521.863610	33.516583
864.350130	68615.201035	33.521600
865.334080	68701.526524	33.526618
865.635814	68795.213645	33.531636
866.576622	68881.344629	33.536653
866.932552	68974.581746	33.541671
867.592919	69064.346635	33.546688
868.446530	69158.269881	33.551706
868.888682	69281.725395	33.556724
869.814793	69375.935087	33.561741
870.535839	69491.330177	33.566759
871.256290	69604.540035	33.571776
872.007745	69715.325831	33.576794
873.030483	69828.969047	33.581812
873.656304	69950.093468	33.586829
874.149803	70066.311585	33.591847
875.026116	70182.829605	33.596864
876.190431	70303.491426	33.601882
876.838797	70427.603688	33.606900
877.800661	70538.885053	33.611917
878.339014	70663.888226	33.616935
879.419230	70774.671902	33.621952
880.106009	70890.725123	33.626970
881.101888	71014.855285	33.631988
881.910803	71121.583446	33.637005
882.515681	71244.197662	33.642023
883.194622	71359.161787	33.647040
884.202404	71472.722088	33.652058
884.656538	71604.726592	33.657076
885.687844	71732.779458	33.662093
886.788398	71863.583386	33.667111
887.321487	71985.493285	33.672128
888.310178	72119.368629	33.677146
889.192562	72250.980712	33.682164
890.229815	72385.551508	33.687181
890.961944	72522.711950	33.692199
891.807636	72658.591485	33.697216
893.001782	72781.949211	33.702234
893.641933	72921.749400	33.707252
895.098248	73044.542560	33.712269
896.466408	73166.655406	33.717287
897.447216	73282.271401	33.722304
898.868304	73394.152906	33.727322
899.886169	73511.198775	33.732340
900.911547	73618.114433	33.737357
901.948753	73731.872527	33.742375
902.722102	73848.150411	33.747392
904.186836	73946.593269	33.752410
904.740828	74072.228351	33.757428
905.658271	74171.328138	33.762445
906.450411	74282.689070	33.767463
906.984760	74393.548164	33.772480
907.741281	74524.854003	33.777498
908.852642	74642.687861	33.782516
909.728847	74748.622158	33.787533
910.550354	74871.843514	33.792551
910.920756	74992.261962	33.797568
912.312762	75105.124552	33.802586
912.884261	75234.619111	33.807604
913.863310	75364.864904	33.812621
914.630164	75486.771564	33.817639
915.752844	75614.784186	33.822656
916.941274	75725.502295	33.827674
918.075568	75848.325933	33.832692
918.955663	75964.561135	33.837709
919.945280	76085.058208	33.842727
920.746192	76206.173786	33.847744
921.726597	76319.607934	33.852762
922.354682	76442.041709	33.857780
923.401242	76558.620397	33.862797
924.462606	76682.490877	33.867815
925.262472	76799.666374	33.872832
926.564231	76907.162243	33.877850
927.282149	77034.641488	33.882868
928.319562	77140.385689	33.887885
929.231474	77254.948331	33.892903
930.052540	77374.095710	33.897920
930.717914	77471.665361	33.902938
931.392543	77586.166490	33.907956
932.339477	77706.502990	33.912973
933.224217	77818.955758	33.917991
933.616401	77933.105574	33.923008
934.637574	78056.731656	33.928026
935.607966	78186.130984	33.933044
936.529592	78305.248828	33.938061
937.675013	78430.684075	33.943079
938.344381	78561.265071	33.948096
939.559194	78676.912582	33.953114
940.351549	78801.293808	33.958132
941.239978	78928.056109	33.963149
942.407464	79044.888903	33.968167
942.912643	79184.728499	33.973184
944.152160	79310.678786	33.978202
945.078928	79445.010710	33.983220
946.027855	79560.016497	33.988237
946.798526	79705.556907	33.993255
947.774925	79833.435938	33.998272
948.941625	79974.458831	34.003290
949.414362	80116.452780	34.008308
950.406025	80244.142286	34.013325
951.707831	80384.166680	34.018343
952.411129	80525.368192	34.023360
953.711486	80669.478340	34.028378
954.618021	80808.582349	34.033396
955.258229	80947.590587	34.038413
956.329725	81081.922748	34.043431
957.403084	81221.496059	34.048448
958.508435	81357.183749	34.053466
959.548684	81493.710816	34.058484
960.500146	81620.530148	34.063501
961.402721	81761.999147	34.068519
961.947878	81919.406261	34.073536
962.976809	82057.652019	34.078554
963.457971	82203.072642	34.083572
964.454363	82349.158291	34.088589
966.124750	82490.642829	34.093607
967.047778	82640.193964	34.098624
968.353468	82769.037521	34.103642
969.380488	82903.451694	34.108660
970.350547	83041.839754	34.113677
971.644431	83172.527403	34.118695
973.172571	83307.408145	34.123712
974.248011	83421.150685	34.128730
975.166220	83550.857283	34.133748
976.077645	83684.662612	34.138765
977.017446	83800.869192	34.143783
977.961485	83932.957553	34.148800
978.847512	84063.791486	34.153818
979.956275	84189.659277	34.158836
980.645037	84320.336505	34.163853
981.748186	84443.589187	34.168871
982.678548	84556.210224	34.173888
983.660784	84671.358970	34.178906
984.035605	84799.711798	34.183924
984.691315	84924.157562	34.188941
985.903434	85034.068145	34.193959
986.486953	85181.838745	34.198976
987.249710	85310.683025	34.203994
988.113936	85451.746623	34.209012
988.897130	85600.417820	34.214029
990.226144	85726.480991	34.219047
991.212827	85863.474847	34.224064
992.550155	85993.079128	34.229082
993.287524	86139.396572	34.234100
994.547128	86278.429954	34.239117
995.649057	86419.209212	34.244135
996.413905	86575.939450	34.249152
997.428405	86706.781846	34.254170
998.318252	86848.154102	34.259188
998.952029	87002.239896	34.264205
1000.060729	87141.492584	34.269223
1001.127915	87292.261321	34.274240
1002.156270	87435.613597	34.279258
1003.453105	87582.168057	34.284276
1004.580527	87730.894131	34.289293
1005.772508	87866.046955	34.294311
1006.449965	88007.896942	34.299328
1007.734518	88143.403546	34.304346
1008.613102	88290.813484	34.309364
1009.895686	88447.297927	34.314381
1011.196869	88589.868277	34.319399
1011.849885	88731.638366	34.324416
1012.978793	88880.093866	34.329434
1013.974282	89020.755287	34.334452
1014.694358	89174.286347	34.339469
1015.997838	89308.500828	34.344487
1016.742636	89467.949261	34.349504
1017.982832	89610.751036	34.354522
1019.073515	89760.230478	34.359540
1019.597614	89915.303072	34.364557
1020.880965	90059.656662	34.369575
1021.641251	90212.410766	34.374592
1022.935976	90366.820103	34.379610
1024.007413	90519.514211	34.384628
1025.122540	90662.393355	34.389645
1025.799906	90813.849380	34.394663
1026.689029	90973.374383	34.399680
1027.567726	91128.266350	34.404698
1029.108395	91283.022493	34.409716
1029.999217	91446.826050	34.414733
1030.827667	91611.608415	34.419751
1032.084934	91762.219779	34.424768
1033.470969	91906.676717	34.429786
1034.618795	92057.756564	34.434804
1035.966532	92190.286638	34.439821
1037.388163	92324.241493	34.444839
1038.569852	92446.989705	34.449856
1039.744497	92580.428810	34.454874
1040.456835	92691.419134	34.459892
1041.152107	92815.265072	34.464909
1042.027922	92940.000111	34.469927
1043.083366	93070.108871	34.474944
1044.137615	93206.379215	34.479962
1044.892977	93350.104657	34.484980
1045.395287	93496.255864	34.489997
1046.914911	93633.681890	34.495015
1047.592979	93786.132251	34.500032
1048.620743	93927.281666	34.505050
1049.344953	94070.548638	34.510068
1050.254231	94228.310150	34.515085
1051.380433	94388.239518	34.520103
1052.595369	94543.841951	34.525120
1053.339596	94703.284009	34.530138
1054.282875	94858.520677	34.535156
1055.730838	95027.252883	34.540173
1056.829767	95179.019560	34.545191
1057.727014	95337.752293	34.550208
1058.786357	95493.145681	34.555226
1060.160143	95653.531774	34.560244
1061.073299	95828.472080	34.565261
1062.484845	95976.917641	34.570279
1063.215178	96141.401166	34.575296
1064.104742	96311.851247	34.580314
1065.305087	96475.509660	34.585332
1066.061837	96640.890907	34.590349
1067.355437	96802.076015	34.595367
1068.556237	96970.052327	34.600384
1070.087755	97119.024024	34.605402
1071.430142	97281.950810	34.610420
1072.672848	97441.022937	34.615437
1073.741541	97584.314386	34.620455
1074.885586	97742.335163	34.625472
1075.797569	97894.447125	34.630490
1076.943136	98050.192289	34.635508
1077.743137	98217.703805	34.640525
1079.152087	98370.378875	34.645543
1080.162266	98534.873163	34.650560
1081.167497	98678.991376	34.655578
1082.440284	98826.104739	34.660596
1083.237524	98992.281106	34.665613
1084.345162	99144.256376	34.670631
1085.243116	99300.384738	34.675648
1086.334488	99468.978893	34.680666
1087.573313	99617.437686	34.685684
1088.326882	99787.245711	34.690701
1089.902749	99941.290278	34.695719
1091.032224	100109.231378	34.700736
1091.648935	100273.250219	34.705754
1093.197534	100422.196397	34.710772
1094.071526	100588.707395	34.715789
1095.135960	100741.225206	34.720807
1096.694194	100888.654330	34.725824
1097.477015	101040.263482	34.730842
1099.085971	101162.326620	34.735860
1101.235198	101269.049293	34.740877
1102.792147	101394.367842	34.745895
1103.942791	101523.605065	34.750912
1104.581701	101643.559792	34.755930
1105.545910	101758.420418	34.760948
1106.363064	101882.891145	34.765965
1107.203368	102009.484902	34.770983
1107.800100	102151.228300	34.776000
1108.702551	102295.239842	34.781018
1109.971108	102436.808527	34.786036
1110.136041	102599.985436	34.791053
1111.507873	102746.873811	34.796071
1112.489447	102901.829791	34.801088
1113.258084	103070.754494	34.806106
1114.452561	103232.285033	34.811124
1115.371979	103406.452944	34.816141
1116.431691	103564.558485	34.821159
1117.563810	103731.981027	34.826176
1118.509303	103905.730830	34.831194
1120.284330	104073.502847	34.836212
1121.334801	104233.278620	34.841229
1122.643736	104395.077352	34.846247
1124.011631	104559.304175	34.851264
1124.587729	104734.928670	34.856282
1126.126270	104901.611403	34.861300
1127.551027	105072.110407	34.866317
1128.468655	105231.793787	34.871335
1129.449859	105404.264220	34.876352
1130.302282	105592.096621	34.881370
1131.875057	105752.894379	34.886388
1132.615876	105925.735887	34.891405
1133.843375	106092.084034	34.896423
1135.066280	106273.470971	34.901440
1135.713770	106445.786807	34.906458
1137.072563	106622.794296	34.911476
1137.769815	106810.243223	34.916493
1139.292475	106988.847525	34.921511
1140.167394	107173.707845	34.926528
1141.470333	107359.786297	34.931546
1142.972038	107533.632272	34.936564
1143.866455	107719.993647	34.941581
1144.785941	107902.479066	34.946599
1146.195688	108089.862607	34.951616
1147.120506	108280.419681	34.956634
1148.323453	108454.440030	34.961652
1149.470107	108639.369602	34.966669
1151.179815	108820.002043	34.971687
1152.778328	108996.779929	34.976704
1153.870505	109165.113879	34.981722
1155.346231	109340.116224	34.986740
1156.358785	109511.319811	34.991757
1157.488379	109677.575265	34.996775
1158.791966	109828.239710	35.001792
1159.715216	109985.364816	35.006810
1160.456613	110147.070880	35.011828
1161.600070	110303.542701	35.016845
1163.198950	110463.234578	35.021863
1164.165029	110618.768158	35.026880
1165.145170	110784.630779	35.031898
1166.154368	110946.786915	35.036916
1166.996645	111112.591374	35.041933
1168.081175	111290.233443	35.046951
1169.530087	111464.584215	35.051968
1170.460261	111639.873254	35.056986
1171.988158	111797.534119	35.062004
1173.575823	111963.263742	35.067021
1175.054139	112126.030343	35.072039
1176.393411	112293.612099	35.077056
1177.586793	112451.570857	35.082074
1179.476228	112585.605357	35.087092
1180.769327	112740.119071	35.092109
1181.982131	112898.482719	35.097127
1182.741970	113054.792370	35.102144
1183.782625	113217.888914	35.107162
1184.668894	113364.988579	35.112180
1185.822116	113536.166003	35.117197
1186.561321	113698.351362	35.122215
1187.551158	113866.556323	35.127232
1188.468677	114055.658776	35.132250
1189.796155	114230.174810	35.137268
1190.483128	114421.304509	35.142285
1191.495833	114605.768171	35.147303
1192.899124	114792.614792	35.152320
1193.619903	114992.093831	35.157338
1194.762511	115173.286898	35.162356
1195.898035	115381.977908	35.167373
1197.148918	115576.540382	35.172391
1198.539174	115785.719689	35.177408
1199.252439	115998.503148	35.182426
1200.879231	116192.333134	35.187444
1202.047990	116398.520045	35.192461
1202.885202	116613.340252	35.197479
1204.240940	116817.240538	35.202496
1205.416131	117024.900352	35.207514
1206.731802	117223.802101	35.212532
1207.992590	117442.614049	35.217549
1209.311293	117640.689117	35.222567
1210.680880	117840.467155	35.227584
1211.816907	118054.840359	35.232602
1212.988264	118258.502801	35.237620
1214.330639	118453.053584	35.242637
1215.736504	118658.125533	35.247655
1217.270004	118864.622478	35.252672
1219.072882	119064.360087	35.257690
1220.369401	119245.988030	35.262708
1221.429217	119433.917218	35.267725
1222.660042	119618.344284	35.272743
1224.454368	119800.143904	35.277760
1225.158284	119979.585291	35.282778
1226.267617	120149.629835	35.287796
1227.429359	120323.415823	35.292813
1228.373272	120511.485172	35.297831
1229.719668	120682.217365	35.302848
1230.672234	120859.687567	35.307866
1232.086464	121044.937733	35.312884
1233.348787	121237.647629	35.317901
1234.497031	121408.416040	35.322919
1235.860927	121578.796654	35.327936
1236.996476	121780.624164	35.332954
1238.299327	121962.884187	35.337972
1239.620061	122144.749998	35.342989
1240.787900	122330.592964	35.348007
1242.142141	122515.090390	35.353024
1243.275734	122715.012840	35.358042
1244.432942	122901.507434	35.363060
1245.542718	123097.218876	35.368077
1246.686027	123303.565736	35.373095
1248.122856	123484.649636	35.378112
1248.965066	123698.013672	35.383130
1250.135021	123900.649753	35.388148
1252.092755	124091.749865	35.393165
1253.181335	124288.043365	35.398183
1254.706713	124488.968100	35.403200
1255.798674	124693.205859	35.408218
1256.941898	124871.913824	35.413236
1258.170765	125090.281411	35.418253
1259.285628	125295.862758	35.423271
1260.998345	125482.996319	35.428288
1262.288243	125690.250196	35.433306
1263.258751	125894.934344	35.438324
1264.734939	126091.774679	35.443341
1265.698695	126302.999226	35.448359
1267.162146	126503.670075	35.453376
1268.531716	126719.393585	35.458394
1269.561492	126937.376964	35.463412
1270.821160	127127.900081	35.468429
1271.797024	127353.128560	35.473447
1273.316603	127542.726502	35.478464
1274.395493	127757.110923	35.483482
1275.710014	127988.105351	35.488500
1277.277202	128176.395284	35.493517
1278.252539	128409.955447	35.498535
1280.279309	128590.865588	35.503552
1282.427221	128796.195001	35.508570
1283.816626	128983.378535	35.513588
1285.218612	129173.247070	35.518605
1286.483053	129361.137116	35.523623
1287.998235	129552.713189	35.528640
1288.785530	129740.504275	35.533658
1290.252907	129925.109978	35.538676
1291.413602	130117.582424	35.543693
1292.426406	130301.388705	35.548711
1293.667793	130485.843993	35.553728
1294.776730	130666.786826	35.558746
1295.978766	130843.864548	35.563764
1297.255157	131020.032040	35.568781
1298.190638	131208.721602	35.573799
1299.440259	131396.310921	35.578816
1300.221715	131598.660044	35.583834
1301.693439	131788.687252	35.588852
1303.063073	131976.996195	35.593869
1304.171782	132188.217085	35.598887
1305.208965	132384.297563	35.603904
1306.726161	132594.290904	35.608922
1307.905608	132793.367078	35.613940
1309.120186	133006.275020	35.618957
1310.178114	133216.928777	35.623975
1311.755690	133424.308530	35.628992
1313.345905	133632.435340	35.634010
1314.271630	133845.420776	35.639028
1316.302898	134055.191093	35.644045
1317.420465	134269.948431	35.649063
1319.158768	134476.068491	35.654080
1320.214048	134676.596616	35.659098
1321.918511	134880.038680	35.664116
1322.985188	135093.137639	35.669133
1324.189661	135295.521680	35.674151
1325.811639	135504.201816	35.679168
1326.916913	135720.961281	35.684186
1328.382928	135936.904731	35.689204
1330.263425	136138.300182	35.694221
1331.423062	136354.092666	35.699239
1332.753928	136556.959580	35.704256
1333.758236	136757.915648	35.709274
1334.845382	136973.698872	35.714292
1336.371913	137181.924623	35.719309
1337.303582	137415.996334	35.724327
1338.636761	137621.670790	35.729344
1339.824438	137860.926334	35.734362
1340.970054	138082.588379	35.739380
1342.309403	138312.509174	35.744397
1343.551879	138551.381404	35.749415
1344.906019	138775.702098	35.754432
1346.292370	139021.411221	35.759450
1347.909281	139241.955156	35.764468
1349.296845	139481.534142	35.769485
1350.601394	139710.926311	35.774503
1352.367152	139940.766543	35.779520
1353.766619	140169.221980	35.784538
1355.066379	140382.968409	35.789556
1356.694681	140616.244814	35.794573
1358.277336	140833.637491	35.799591
1359.750027	141055.586413	35.804608
1361.094899	141274.363463	35.809626
1362.426994	141496.375978	35.814644
1363.867836	141700.210940	35.819661
1364.977952	141914.543299	35.824679
1366.132778	142125.118493	35.829696
1367.664427	142334.900146	35.834714
1368.909048	142537.403060	35.839732
1370.088022	142735.671801	35.844749
1371.428923	142939.530913	35.849767
1373.099161	143148.738434	35.854784
1374.413346	143363.314667	35.859802
1375.604563	143566.099017	35.864820
1376.880865	143779.112486	35.869837
1377.891926	144004.591053	35.874855
1379.107952	144220.152132	35.879872
1380.632557	144446.452232	35.884890
1381.535747	144670.824689	35.889908
1383.006548	144904.779852	35.894925
1384.095535	145145.198543	35.899943
1385.994430	145370.355785	35.904960
1387.167419	145599.077772	35.909978
1388.557557	145840.442644	35.914996
1390.456235	146064.172547	35.920013
1391.611368	146302.003725	35.925031
1393.083995	146532.142612	35.930048
1394.984617	146765.460246	35.935066
1396.551591	146988.133916	35.940084
1398.113797	147201.911164	35.945101
1399.973918	147438.941666	35.950119
1401.584293	147649.380386	35.955136
1402.739452	147855.658870	35.960154
1404.081762	148094.601951	35.965172
1405.554183	148306.651505	35.970189
1406.194322	148544.099573	35.975207
1408.143053	148757.027179	35.980224
1409.773795	148971.565993	35.985242
1411.226274	149198.405956	35.990260
1412.726851	149428.193647	35.995277
1413.740961	149645.192873	36.000295
1415.274460	149879.821245	36.005312
1416.789948	150093.929440	36.010330
1417.707838	150337.482415	36.015348
1419.749634	150565.011631	36.020365
1421.307359	150777.342746	36.025383
1422.618224	151010.822942	36.030400
1423.807890	151230.999635	36.035418
1424.870648	151469.504916	36.040436
1426.632675	151695.489023	36.045453
1428.104077	151933.742569	36.050471
1429.865063	152164.484356	36.055488
1431.239112	152388.747233	36.060506
1432.334619	152606.944906	36.065524
1434.122097	152834.923270	36.070541
1435.473117	153062.465405	36.075559
1436.944455	153294.769825	36.080576
1438.952776	153504.536520	36.085594
1440.266983	153730.149215	36.090612
1441.829686	153944.667955	36.095629
1443.258430	154169.542713	36.100647
1444.480502	154362.069515	36.105664
1445.725936	154566.448684	36.110682
1446.794539	154780.252474	36.115700
1448.302858	154987.812944	36.120717
1449.420476	155208.800809	36.125735
1450.738561	155437.416648	36.130752
1452.080083	155654.783559	36.135770
1453.091005	155883.983743	36.140788
1454.691294	156117.009856	36.145805
1455.778580	156339.303207	36.150823
1457.045509	156585.876770	36.155840
1458.425181	156830.697037	36.160858
1459.608341	157080.558891	36.165876
1461.062202	157319.297101	36.170893
1462.068482	157574.922062	36.175911
1462.855257	157842.439896	36.180928
1464.625781	158096.184716	36.185946
1466.506658	158361.148801	36.190964
1467.930547	158622.434042	36.195981
1469.778320	158895.992231	36.200999
1471.544889	159148.426546	36.206016
1473.008502	159423.584267	36.211034
1474.976652	159684.562707	36.216052
1476.459658	159928.538725	36.221069
1478.140840	160185.559241	36.226087
1479.569376	160444.993160	36.231104
1481.073455	160690.695738	36.236122
1482.726956	160941.892708	36.241140
1484.695734	161190.974272	36.246157
1486.738305	161425.893157	36.251175
1488.045852	161682.311721	36.256192
1489.728473	161911.292526	36.261210
1491.184213	162153.969217	36.266228
1492.762452	162396.945132	36.271245
1494.378597	162637.849488	36.276263
1494.980013	162884.446062	36.281280
1496.862680	163117.587849	36.286298
1497.964278	163376.625658	36.291316
1499.576819	163637.397723	36.296333
1500.847320	163897.325531	36.301351
1502.530525	164153.676549	36.306368
1504.580727	164401.118561	36.311386
1505.843889	164648.002399	36.316404
1507.108865	164892.782253	36.321421
1508.957665	165141.466105	36.326439
1510.145432	165405.045023	36.331456
1512.193430	165648.564020	36.336474
1513.208671	165902.509362	36.341492
1514.641274	166158.926786	36.346509
1516.353358	166406.017363	36.351527
1518.044194	166661.712315	36.356544
1519.341966	166919.805216	36.361562
1520.654438	167185.495036	36.366580
1521.891183	167440.341510	36.371597
1523.979279	167682.484841	36.376615
1525.216676	167933.909917	36.381632
1526.824482	168171.959678	36.386650
1528.104660	168413.956967	36.391668
1529.527316	168639.710197	36.396685
1530.930729	168889.047698	36.401703
1532.513509	169140.260969	36.406720
1534.118946	169375.832491	36.411738
1534.932980	169633.335685	36.416756
1536.487076	169879.586044	36.421773
1538.422439	170147.062149	36.426791
1539.519380	170403.827879	36.431808
1541.097631	170662.079076	36.436826
1542.904897	170928.477334	36.441844
1544.645141	171188.253836	36.446861
1546.129444	171429.121308	36.451879
1547.241386	171711.161790	36.456896
1549.202217	171975.766859	36.461914
1550.716575	172255.146850	36.466932
1551.915710	172518.341621	36.471949
1553.450492	172792.330878	36.476967
1554.848963	173068.880780	36.481984
1556.693842	173339.564364	36.487002
1558.135234	173622.048148	36.492020
1559.923349	173897.336746	36.497037
1561.703433	174162.441742	36.502055
1563.048862	174445.492044	36.507072
1564.929185	174724.247597	36.512090
1566.060100	174999.597351	36.517108
1567.669315	175288.612183	36.522125
1569.464421	175560.993149	36.527143
1570.612908	175854.576119	36.532160
1572.243551	176124.906386	36.537178
1573.994652	176428.610369	36.542196
1575.378924	176710.261982	36.547213
1577.605892	176994.103344	36.552231
1579.700793	177267.843527	36.557248
1581.676097	177544.306822	36.562266
1582.931682	177818.272736	36.567284
1584.458926	178093.110766	36.572301
1586.469166	178364.664031	36.577319
1587.680678	178639.543094	36.582336
1589.383543	178907.811930	36.587354
1591.014750	179188.882764	36.592372
1592.586265	179468.975314	36.597389
1594.008854	179730.239612	36.602407
1595.377008	180008.680556	36.607424
1597.263092	180280.735246	36.612442
1599.228011	180564.045927	36.617460
1601.233599	180826.848358	36.622477
1603.180482	181089.674402	36.627495
1604.738498	181351.891332	36.632512
1606.182292	181614.229492	36.637530
1608.025202	181877.914237	36.642548
1609.546471	182118.127580	36.647565
1610.850836	182377.142760	36.652583
1612.350827	182637.828648	36.657600
1614.142038	182874.831155	36.662618
1615.269150	183117.497992	36.667636
1616.450590	183376.183281	36.672653
1618.131953	183620.414373	36.677671
1619.396794	183892.793231	36.682688
1620.580077	184151.241641	36.687706
1622.035036	184421.233396	36.692724
1623.748722	184691.287197	36.697741
1625.370534	184967.409904	36.702759
1626.640454	185252.751761	36.707776
1629.135998	185521.925015	36.712794
1630.223865	185806.233365	36.717812
1631.975504	186098.000960	36.722829
1633.962410	186365.052011	36.727847
1635.097173	186657.416019	36.732864
1636.869913	186929.148736	36.737882
1638.868100	187212.217232	36.742900
1640.316428	187496.339200	36.747917
1642.057619	187783.005130	36.752935
1643.388851	188079.674150	36.757952
1645.029733	188362.171879	36.762970
1646.988834	188651.143487	36.767988
1648.705729	188936.183303	36.773005
1650.704140	189219.213145	36.778023
1652.322319	189495.807608	36.783040
1654.140955	189784.288135	36.788058
1655.836389	190075.861067	36.793076
1657.530862	190351.496585	36.798093
1659.304382	190630.027287	36.803111
1660.968187	190929.174031	36.808128
1662.746012	191212.466423	36.813146
1664.454150	191490.580973	36.818164
1666.592667	191756.572394	36.823181
1668.881050	192025.257340	36.828199
1670.269203	192303.389254	36.833216
1671.925031	192566.301641	36.838234
1673.981271	192850.701509	36.843252
1675.347791	193121.239435	36.848269
1677.174758	193383.938620	36.853287
1678.358504	193671.235744	36.858304
1680.003670	193941.137375	36.863322
1681.637822	194212.819024	36.868340
1682.869379	194506.192584	36.873357
1684.663315	194781.139052	36.878375
1686.612315	195066.482325	36.883392
1688.325857	195340.670389	36.888410
1690.068500	195624.970748	36.893428
1691.766205	195910.777471	36.898445
1693.507968	196187.148601	36.903463
1695.209142	196462.169599	36.908480
1697.207218	196748.136340	36.913498
1699.160107	197023.539189	36.918516
1700.932965	197285.962459	36.923533
1703.094967	197532.916723	36.928551
1704.532734	197790.674163	36.933568
1705.961278	198032.543332	36.938586
1707.940095	198272.612745	36.943604
1709.413611	198519.884024	36.948621
1711.185962	198762.755422	36.953639
1712.515388	199012.945793	36.958656
1714.083959	199268.849193	36.963674
1716.261780	199522.702384	36.968692
1717.403725	199779.297895	36.973709
1719.208493	200028.655944	36.978727
1720.684005	200293.045176	36.983744
1722.170525	200559.464837	36.988762
1723.999099	200821.439662	36.993780
1725.637367	201100.886417	36.998797
1727.266689	201369.635584	37.003815
1728.882119	201653.239462	37.008832
1730.086293	201927.846995	37.013850
1732.076349	202214.389900	37.018868
1733.350219	202511.126638	37.023885
1735.113999	202796.172526	37.028903
1736.622776	203097.038558	37.033920
1738.342915	203399.700529	37.038938
1740.073322	203701.791261	37.043956
1741.821684	204004.121923	37.048973
1744.006554	204296.013942	37.053991
1745.282068	204607.283208	37.059008
1747.311830	204900.078794	37.064026
1749.204203	205206.124946	37.069044
1750.689886	205521.707137	37.074061
1753.337956	205808.442855	37.079079
1755.879184	206103.905238	37.084096
1757.910424	206392.239654	37.089114
1759.697163	206668.592649	37.094132
1761.536420	206963.218672	37.099149
1763.414437	207245.259680	37.104167
1765.175178	207525.619550	37.109184
1766.901081	207802.114376	37.114202
1768.782203	208087.053215	37.119220
1770.413446	208376.222339	37.124237
1772.529652	208646.463984	37.129255
1774.139244	208929.266341	37.134272
1775.877688	209216.238882	37.139290
1778.230037	209483.336446	37.144308
1779.942120	209764.234792	37.149325
1781.853833	210026.809017	37.154343
1783.454505	210305.873992	37.159360
1785.070967	210583.477744	37.164378
1786.922774	210854.697705	37.169396
1788.505035	211138.707754	37.174413
1790.200346	211424.681607	37.179431
1791.757575	211721.761806	37.184448
1793.140743	212005.946953	37.189466
1794.805143	212289.009583	37.194484
1796.175407	212585.323606	37.199501
1798.203150	212876.875287	37.204519
1799.854918	213158.623342	37.209536
1801.496806	213436.057597	37.214554
1803.110761	213711.605766	37.219572
1804.905143	214010.436141	37.224589
1806.457468	214285.336279	37.229607
1808.293558	214580.252220	37.234624
1809.865340	214881.826064	37.239642
1812.037719	215166.470840	37.244660
1813.209322	215471.195983	37.249677
1815.353999	215757.396559	37.254695
1817.046139	216062.473378	37.259712
1818.962714	216370.931240	37.264730
1820.949366	216667.368543	37.269748
1822.591945	216969.130752	37.274765
1824.308511	217275.999213	37.279783
1826.469598	217588.118319	37.284800
1828.698175	217898.387076	37.289818
1830.541554	218189.013066	37.294836
1832.216867	218491.868475	37.299853
1834.576234	218786.757270	37.304871
1836.730413	219090.923136	37.309888
1838.424069	219383.571102	37.314906
1841.031022	219671.897988	37.319924
1842.876566	219961.400704	37.324941
1844.658872	220248.273605	37.329959
1846.565753	220538.429086	37.334976
1848.653923	220832.594610	37.339994
1850.556816	221120.162760	37.345012
1851.908910	221403.870582	37.350029
1854.122629	221755.436700	37.355047
1856.158108	222037.997244	37.360064
1857.812341	222326.587107	37.365082
1860.069777	222620.186683	37.370100
1861.745199	222907.302443	37.375117
1863.719607	223191.565653	37.380135
1865.688563	223482.890609	37.385152
1867.374288	223779.454918	37.390170
1869.572429	224062.162038	37.395188
1871.374330	224354.240470	37.400205
1873.531762	224634.518110	37.405223
1875.325864	224912.314824	37.410240
1876.770103	225205.862551	37.415258
1878.994180	225489.434005	37.420276
1880.923600	225779.935482	37.425293
1882.711687	226068.885860	37.430311
1884.612255	226353.933795	37.435328
1886.068972	226648.703671	37.440346
1887.940561	226938.456476	37.445364
1889.599048	227233.120183	37.450381
1891.495827	227524.699524	37.455399
1893.778941	227829.602496	37.460416
1895.317165	228128.885130	37.465434
1897.341745	228422.148794	37.470452
1899.101312	228719.138027	37.475469
1900.871988	229000.583638	37.480487
1903.194972	229285.879020	37.485504
1905.107713	229561.081623	37.490522
1906.948933	229831.191611	37.495540
1908.502566	230103.024257	37.500557
1910.589437	230368.347604	37.505575
1912.195751	230640.884621	37.510592
1913.902017	230927.908482	37.515610
1915.690566	231208.799394	37.520628
1917.722187	231498.770293	37.525645
1919.667311	231777.022126	37.530663
1921.601703	232065.968906	37.535680
1923.350748	232351.999839	37.540698
1925.050487	232647.284263	37.545716
1927.152775	232943.318451	37.550733
1929.487812	233239.799174	37.555751
1931.349200	233536.051181	37.560768
1933.152191	233835.996079	37.565786
1935.375042	234124.852439	37.570804
1937.297153	234409.084074	37.575821
1939.327474	234719.662844	37.580839
1941.253638	235014.689851	37.585856
1943.094003	235325.605400	37.590874
1944.930768	235622.680230	37.595892
1946.712080	235928.959028	37.600909
1948.410232	236245.868595	37.605927
1950.860706	236542.112105	37.610944
1952.324061	236868.001178	37.615962
1954.502375	237179.325793	37.620980
1956.105717	237498.438446	37.625997
1958.671322	237810.135212	37.631015
1960.722740	238116.123438	37.636032
1962.676728	238433.151247	37.641050
1964.615037	238744.035811	37.646068
1966.943349	239060.523421	37.651085
1968.833615	239370.680753	37.656103
1971.034142	239678.122750	37.661120
1972.698203	240001.042843	37.666138
1974.736848	240309.274189	37.671156
1976.796867	240635.714567	37.676173
1978.569735	240954.886259	37.681191
1980.500181	241268.090231	37.686208
1982.440287	241597.905045	37.691226
1984.632526	241905.176342	37.696244
1986.512519	242230.074796	37.701261
1988.593453	242548.846186	37.706279
1990.784739	242863.968651	37.711296
1992.725317	243182.713114	37.716314
1994.859444	243501.554665	37.721332
1996.851704	243820.724316	37.726349
1998.623317	244142.876207	37.731367
2000.710334	244466.477475	37.736384
2002.461210	244800.166085	37.741402
2004.663943	245115.800184	37.746420
2006.552434	245439.536889	37.751437
2008.454318	245756.134619	37.756455
2010.613648	246062.176291	37.761472
2012.111394	246358.950670	37.766490
2014.735066	246656.842493	37.771508
2016.878963	246942.745590	37.776525
2018.730911	247245.993660	37.781543
2020.750985	247541.722370	37.786560
2022.286497	247848.882843	37.791578
2024.435227	248148.885138	37.796596
2026.820788	248453.397275	37.801613
2028.518843	248753.472257	37.806631
2031.238899	249040.685032	37.811648
2033.000811	249355.839427	37.816666
2034.619079	249666.444980	37.821684
2036.899876	249981.416691	37.826701
2038.818688	250288.698975	37.831719
2040.809644	250605.953202	37.836736
2042.544540	250936.660703	37.841754
2044.708603	251241.441881	37.846772
2046.765141	251566.231801	37.851789
2048.524401	251895.743410	37.856807
2050.577626	252221.906768	37.861824
2052.624578	252559.502550	37.866842
2054.630014	252887.630640	37.871860
2056.788233	253231.560487	37.876877
2058.705304	253565.063603	37.881895
2060.960013	253895.897338	37.886912
2062.799571	254245.798246	37.891930
2065.137003	254585.028121	37.896948
2067.446028	254918.039551	37.901965
2069.480622	255267.301665	37.906983
2071.499697	255596.422854	37.912000
2073.581165	255939.709137	37.917018
2076.279274	256266.666078	37.922036
2079.710232	256579.866202	37.927053
2082.147587	256894.951741	37.932071
2084.544274	257191.170169	37.937088
2086.663702	257498.508434	37.942106
2088.966733	257793.751799	37.947124
2091.350779	258093.707555	37.952141
2093.066940	258399.586807	37.957159
2095.436043	258682.957794	37.962176
2097.236102	258980.467009	37.967194
2099.211820	259277.923309	37.972212
2101.619456	259579.909330	37.977229
2103.235165	259893.935173	37.982247
2105.286230	260195.419590	37.987264
2107.139893	260502.498853	37.992282
2108.978089	260807.447071	37.997300
2111.198157	261119.092197	38.002317
2113.036995	261445.023713	38.007335
2115.068072	261746.436727	38.012352
2116.939431	262068.781952	38.017370
2118.719838	262392.183453	38.022388
2121.059529	262712.117985	38.027405
2122.763906	263033.372930	38.032423
2124.763699	263337.459711	38.037440
2126.722718	263647.776963	38.042458
2128.996699	263954.437301	38.047476
2131.136350	264251.669265	38.052493
2133.251250	264567.093991	38.057511
2135.469578	264862.053078	38.062528
2137.062942	265176.900526	38.067546
2139.022309	265493.239760	38.072564
2141.266213	265807.705076	38.077581
2143.247755	266143.652503	38.082599
2145.452794	266457.768796	38.087616
2147.170889	266804.377012	38.092634
2149.665230	267123.858742	38.097652
2151.980843	267448.678292	38.102669
2153.883896	267796.350186	38.107687
2156.034269	268131.103616	38.112704
2158.100968	268472.729393	38.117722
2159.980322	268822.717351	38.122740
2162.370425	269162.437772	38.127757
2164.118176	269518.848597	38.132775
2166.517782	269869.288051	38.137792
2168.416740	270232.889779	38.142810
2170.980554	270597.732608	38.147828
2173.073112	270950.558314	38.152845
2175.105267	271319.347043	38.157863
2177.491417	271678.629703	38.162880
2179.921647	272046.186986	38.167898
2182.231200	272402.306575	38.172916
2184.332160	272763.946460	38.177933
2186.616162	273138.284500	38.182951
2188.972431	273500.061863	38.187968
2191.107853	273865.913439	38.192986
2193.670066	274232.027623	38.198004
2196.062151	274596.619204	38.203021
2198.011026	274953.431425	38.208039
2200.743766	275297.646277	38.213056
2203.023653	275664.313340	38.218074
2205.505018	276019.542303	38.223092
2207.973759	276358.972319	38.228109
2209.826219	276717.146120	38.233127
2212.262208	277059.451830	38.238144
2214.482623	277415.915955	38.243162
2216.593763	277777.986081	38.248180
2219.062695	278123.715818	38.253197
2220.906354	278479.858381	38.258215
2223.324901	278838.297602	38.263232
2225.667219	279179.779346	38.268250
2227.708309	279533.883394	38.273268
2230.040824	279889.719333	38.278285
2232.058677	280252.260687	38.283303
2234.574235	280607.838661	38.288320
2236.721525	280965.684942	38.293338
2238.800460	281317.749926	38.298356
2241.789607	281661.211113	38.303373
2243.508764	282010.208154	38.308391
2245.436285	282343.650567	38.313408
2248.170558	282664.618900	38.318426
2250.361551	282980.998987	38.323444
2252.706668	283305.889920	38.328461
2254.707409	283627.405811	38.333479
2257.030380	283954.713126	38.338496
2259.497946	284266.221928	38.343514
2261.546384	284588.796518	38.348532
2264.193292	284906.347779	38.353549
2265.827145	285238.132724	38.358567
2268.141533	285563.128493	38.363584
2270.320959	285897.569920	38.368602
2272.777762	286225.159065	38.373620
2275.334114	286545.822518	38.378637
2277.069287	286890.672491	38.383655
2279.292274	287227.519063	38.388672
2281.426379	287571.517611	38.393690
2283.595223	287921.098927	38.398708
2286.078092	288270.884104	38.403725
2288.084064	288635.960791	38.408743
2290.311338	288985.379224	38.413760
2292.657493	289348.622909	38.418778
2294.839450	289706.786212	38.423796
2297.136598	290069.985934	38.428813
2299.111454	290442.457435	38.433831
2301.123467	290811.848804	38.438848
2303.758020	291181.293373	38.443866
2305.613770	291579.895997	38.448884
2307.804328	291957.284600	38.453901
2310.440728	292346.668117	38.458919
2312.545999	292739.564519	38.463936
2314.956826	293125.578570	38.468954
2317.319381	293514.114448	38.473972
2320.458456	293894.118386	38.478989
2322.328640	294288.141633	38.484007
2325.000165	294671.698421	38.489024
2327.500975	295060.006367	38.494042
2329.284318	295449.392586	38.499060
2331.817423	295836.449218	38.504077
2334.318232	296234.356870	38.509095
2336.421106	296630.269220	38.514112
2339.035549	297019.444351	38.519130
2341.141375	297411.010859	38.524148
2343.723068	297803.034535	38.529165
2346.293395	298202.349459	38.534183
2348.731247	298593.479732	38.539200
2351.114232	298981.468019	38.544218
2353.703924	299384.841414	38.549236
2356.376075	299764.729773	38.554253
2358.598059	300145.958687	38.559271
2361.191084	300520.117111	38.564288
2363.756854	300904.363312	38.569306
2366.065860	301275.974042	38.574324
2368.530447	301660.361436	38.579341
2370.830918	302033.775184	38.584359
2373.058374	302392.720965	38.589376
2376.043060	302722.766500	38.594394
2378.395863	303059.033084	38.599412
2381.061396	303385.292168	38.604429
2383.518176	303720.626305	38.609447
2385.327368	304060.863043	38.614464
2387.396106	304389.678293	38.619482
2389.470802	304743.943295	38.624500
2391.949598	305088.110100	38.629517
2394.580336	305440.608730	38.634535
2396.797082	305791.394016	38.639552
2399.165666	306143.779937	38.644570
2401.366522	306504.370404	38.649588
2404.449381	306851.307144	38.654605
2406.415956	307192.679416	38.659623
2408.877261	307559.474092	38.664640
2411.340304	307913.694396	38.669658
2413.793811	308294.331178	38.674676
2416.330934	308639.749270	38.679693
2418.311757	309007.403192	38.684711
2421.186861	309384.896365	38.689728
2423.660366	309737.407915	38.694746
2425.595614	310116.698678	38.699764
2428.476130	310484.992815	38.704781
2430.737242	310854.628508	38.709799
2432.800993	311232.853856	38.714816
2435.222594	311624.914617	38.719834
2437.658662	312009.529755	38.724852
2440.268006	312384.007262	38.729869
2442.677260	312786.860463	38.734887
2444.606963	313164.998841	38.739904
2447.620222	313552.615720	38.744922
2449.978590	313942.620844	38.749940
2452.550462	314334.190799	38.754957
2455.129680	314724.107211	38.759975
2457.450690	315120.209478	38.764992
2460.333738	315512.081218	38.770010
2462.606225	315906.080044	38.775028
2465.409111	316304.361745	38.780045
2468.011323	316681.136125	38.785063
2470.489445	317072.532523	38.790080
2473.795705	317444.900144	38.795098
2476.113313	317825.397867	38.800116
2478.810030	318209.008704	38.805133
2481.372084	318588.804299	38.810151
2483.731271	318959.131868	38.815168
2486.466801	319329.906276	38.820186
2488.644008	319704.272474	38.825204
2491.172233	320076.752928	38.830221
2493.895161	320454.966120	38.835239
2496.117419	320831.428475	38.840256
2498.749138	321203.303735	38.845274
2501.165672	321592.481264	38.850292
2503.088456	321961.849792	38.855309
2506.007330	322326.716132	38.860327
2508.276393	322691.480718	38.865344
2510.431780	323032.465482	38.870362
2512.812959	323394.745862	38.875380
2515.061614	323747.395194	38.880397
2517.248562	324098.376688	38.885415
2519.747005	324473.636537	38.890432
2522.300386	324833.394601	38.895450
2524.332446	325211.874042	38.900468
2526.404275	325590.294631	38.905485
2529.205751	325982.235141	38.910503
2531.202242	326370.923708	38.915520
2533.732174	326763.436704	38.920538
2535.907646	327168.650595	38.925556
2538.141364	327575.275271	38.930573
2541.023403	327984.029837	38.935591
2543.459783	328402.045670	38.940608
2546.772180	328807.477168	38.945626
2549.457970	329219.989200	38.950644
2552.087936	329635.707477	38.955661
2555.196420	330033.978138	38.960679
2557.284644	330435.353982	38.965696
2559.991759	330848.488462	38.970714
2562.465951	331266.812404	38.975732
2565.439090	331673.754814	38.980749
2568.090501	332085.697585	38.985767
2570.529022	332503.791455	38.990784
2573.030822	332911.944180	38.995802
2576.034010	333332.025927	39.000820
2578.248995	333749.970068	39.005837
2581.169272	334169.882155	39.010855
2583.526039	334588.763688	39.015872
2586.410135	335006.645005	39.020890
2589.224321	335435.275674	39.025908
2591.677513	335848.700272	39.030925
2594.271391	336265.299398	39.035943
2596.720849	336682.655152	39.040960
2599.477858	337111.766569	39.045978
2602.006653	337541.342985	39.050996
2604.524068	337962.539317	39.056013
2607.569837	338395.735298	39.061031
2609.719077	338822.011749	39.066048
2612.350680	339247.853482	39.071066
2614.913161	339688.861385	39.076084
2617.658471	340118.132348	39.081101
2620.532015	340545.678925	39.086119
2622.791733	340985.481548	39.091136
2625.841191	341412.511880	39.096154
2628.067787	341852.491291	39.101172
2630.586559	342291.253343	39.106189
2633.198651	342728.524868	39.111207
2635.895739	343168.775655	39.116224
2638.638846	343608.990526	39.121242
2640.641557	344059.347903	39.126260
2643.397804	344501.762870	39.131277
2646.012088	344926.095193	39.136295
2648.468309	345365.504565	39.141312
2651.301429	345772.608359	39.146330
2653.817947	346192.935619	39.151348
2656.174607	346610.974854	39.156365
2658.640184	347028.993772	39.161383
2661.261938	347466.329834	39.166400
2663.724508	347892.822119	39.171418
2665.974474	348339.222611	39.176436
2668.444980	348790.839594	39.181453
2671.283512	349229.320665	39.186471
2673.631396	349679.985104	39.191488
2676.627072	350129.553181	39.196506
2679.425200	350590.648523	39.201524
2682.170320	351042.457250	39.206541
2685.260724	351504.996206	39.211559
2687.686734	351976.952663	39.216576
2690.302699	352426.510849	39.221594
2693.125477	352885.856269	39.226612
2695.588173	353351.397693	39.231629
2698.744445	353814.388239	39.236647
2701.052418	354298.729898	39.241664
2703.909079	354757.926460	39.246682
2707.727628	355210.265349	39.251700
2710.708534	355664.636603	39.256717
2713.820316	356122.206682	39.261735
2716.457081	356572.461447	39.266752
2719.162483	357029.859150	39.271770
2722.216516	357479.252787	39.276788
2724.964824	357940.848744	39.281805
2727.925315	358386.619292	39.286823
2730.615153	358849.155081	39.291840
2733.190765	359294.724458	39.296858
2736.028596	359747.177243	39.301876
2738.900131	360201.371713	39.306893
2741.684377	360666.184782	39.311911
2744.047655	361116.923117	39.316928
2747.076443	361568.465461	39.321946
2749.440096	362019.423540	39.326964
2752.212635	362483.509934	39.331981
2755.233704	362942.654134	39.336999
2757.654531	363418.309113	39.342016
2760.258840	363875.860392	39.347034
2763.117735	364349.431443	39.352052
2765.364807	364831.266273	39.357069
2768.545376	365295.894125	39.362087
2770.943458	365786.957858	39.367104
2773.625728	366257.999122	39.372122
2776.097596	366747.264213	39.377140
2778.829567	367247.369444	39.382157
2782.054077	367722.521892	39.387175
2784.971171	368207.234025	39.392192
2787.746376	368692.978293	39.397210
2790.796155	369184.636982	39.402228
2793.253108	369658.113555	39.407245
2796.220166	370134.067057	39.412263
2798.903382	370598.235465	39.417280
2801.289128	371048.642069	39.422298
2803.937028	371502.453310	39.427316
2806.385577	371966.466277	39.432333
2809.530196	372421.229315	39.437351
2811.564141	372893.924778	39.442368
2814.303857	373370.943465	39.447386
2816.984378	373847.331702	39.452404
2819.469127	374339.146669	39.457421
2822.385685	374826.015871	39.462439
2824.777167	375328.084168	39.467456
2827.747170	375828.354757	39.472474
2830.340715	376332.738184	39.477492
2832.824622	376848.854111	39.482509
2835.879733	377357.363184	39.487527
2838.694859	377884.221246	39.492544
2841.312739	378410.494637	39.497562
2844.058037	378946.635048	39.502580
2846.964117	379481.042915	39.507597
2850.060461	380012.394410	39.512615
2852.927413	380549.153114	39.517632
2855.949932	381087.706247	39.522650
2858.800818	381639.597214	39.527668
2861.525209	382192.946184	39.532685
2865.099454	382727.456858	39.537703
2868.079661	383273.418397	39.542720
2870.955949	383814.264411	39.547738
2873.960583	384358.608191	39.552756
2876.787876	384902.921351	39.557773
2879.800714	385446.360081	39.562791
2882.635360	385997.327068	39.567808
2885.709010	386543.073546	39.572826
2888.823991	387091.646122	39.577844
2891.905182	387635.624885	39.582861
2895.110965	388186.322442	39.587879
2898.042815	388731.906200	39.592896
2900.808565	389269.797645	39.597914
2903.872681	389816.231591	39.602932
2906.911394	390363.574165	39.607949
2909.942394	390899.471377	39.612967
2913.000458	391425.262354	39.617984
2915.858423	391978.517525	39.623002
2918.801566	392523.457551	39.628020
2921.501402	393072.713355	39.633037
2924.468229	393615.907912	39.638055
2927.119511	394162.262994	39.643072
2929.916319	394710.031752	39.648090
2933.119803	395266.349173	39.653108
2935.738195	395832.665016	39.658125
2938.436160	396390.362528	39.663143
2941.060688	396953.843807	39.668160
2943.704487	397524.665959	39.673178
2947.195586	398085.049552	39.678196
2949.804559	398666.735366	39.683213
2953.084450	399216.179438	39.688231
2955.905355	399768.577394	39.693248
2958.380216	400289.150085	39.698266
2961.431275	400824.252580	39.703284
2964.206832	401357.031918	39.708301
2966.873915	401903.408969	39.713319
2969.821135	402437.765817	39.718336
2972.791282	402990.921592	39.723354
2975.849293	403543.065100	39.728372
2978.446747	404099.784428	39.733389
2981.540293	404652.993007	39.738407
2984.430577	405216.947312	39.743424
2987.297904	405792.530790	39.748442
2990.158296	406350.435960	39.753460
2993.007783	406928.738940	39.758477
2995.814024	407512.944167	39.763495
2998.749048	408107.079757	39.768512
3001.770900	408708.084638	39.773530
3004.834758	409288.311570	39.778548
3007.688485	409898.444482	39.783565
3010.686665	410502.332344	39.788583
3013.969057	411103.273655	39.793600
3016.544145	411721.549548	39.798618
3019.900910	412325.115683	39.803636
3022.693965	412954.153570	39.808653
3026.048338	413575.435424	39.813671
3029.267153	414202.275696	39.818688
3032.222694	414813.102325	39.823706
3035.802924	415430.279480	39.828724
3038.703717	416047.576312	39.833741
3041.595456	416685.615560	39.838759
3045.116626	417298.986202	39.843776
3047.950745	417935.258203	39.848794
3051.241737	418556.772243	39.853812
3054.319694	419194.269704	39.858829
3057.643463	419811.671392	39.863847
3060.324068	420445.123905	39.868864
3063.431858	421069.854545	39.873882
3066.481083	421704.816316	39.878900
3069.375251	422345.235250	39.883917
3072.559180	422986.429513	39.888935
3075.697130	423638.915303	39.893952
3078.484514	424281.687371	39.898970
3081.615727	424916.308482	39.903988
3085.082292	425568.873296	39.909005
3088.408016	426204.725333	39.914023
3091.303060	426859.097182	39.919040
3094.133603	427494.287654	39.924058
3097.578625	428146.691730	39.929076
3100.712778	428787.679869	39.934093
3103.204736	429446.712388	39.939111
3106.441058	430092.313153	39.944128
3109.286493	430757.715557	39.949146
3112.622832	431414.994573	39.954164
3115.808854	432067.975189	39.959181
3119.144480	432713.393820	39.964199
3122.301889	433336.994020	39.969216
3124.986836	433959.184943	39.974234
3128.399372	434559.568157	39.979252
3130.977316	435183.620071	39.984269
3133.684211	435809.358156	39.989287
3136.698709	436431.689518	39.994304
3139.413012	437075.981451	39.999322
3142.620058	437709.518726	40.004340
3145.592548	438373.182815	40.009357
3148.494358	439021.319417	40.014375
3151.655584	439667.372468	40.019392
3154.845177	440330.367316	40.024410
3158.522216	440993.267125	40.029428
3161.352267	441653.042347	40.034445
3164.845532	442329.049022	40.039463
3168.505809	442986.327574	40.044480
3171.531719	443656.902880	40.049498
3174.580922	444327.557038	40.054516
3177.366405	445012.004583	40.059533
3180.291688	445687.449683	40.064551
3183.607971	446378.102109	40.069568
3186.434294	447079.695646	40.074586
3190.086619	447771.418429	40.079604
3193.280002	448472.406100	40.084621
3196.381075	449172.982380	40.089639
3200.140305	449868.776755	40.094656
3203.227865	450576.247223	40.099674
3206.448438	451261.759442	40.104692
3209.525140	451989.079173	40.109709
3212.795490	452696.404807	40.114727
3216.110511	453400.411862	40.119744
3218.812057	454132.935151	40.124762
3222.216316	454847.459919	40.129780
3225.105401	455588.256131	40.134797
3228.312891	456317.794481	40.139815
3231.495402	457050.045346	40.144832
3234.582281	457790.028791	40.149850
3237.929729	458536.523879	40.154868
3241.255072	459276.976360	40.159885
3244.733394	460032.051761	40.164903
3248.255130	460765.592752	40.169920
3251.704781	461522.847120	40.174938
3255.013159	462265.022101	40.179956
3258.281964	463008.088389	40.184973
3261.274252	463767.106910	40.189991
3264.741138	464516.463319	40.195008
3267.951950	465266.542033	40.200026
3271.186039	466016.135374	40.205044
3274.017911	466773.655861	40.210061
3277.497608	467533.777770	40.215079
3280.947094	468289.426430	40.220096
3283.577472	469045.784170	40.225114
3287.057096	469803.294977	40.230132
3290.539945	470571.194683	40.235149
3293.851972	471329.030133	40.240167
3297.114819	472061.967653	40.245184
3300.476070	472766.295377	40.250202
3303.724167	473487.200759	40.255220
3306.646816	474207.323111	40.260237
3309.875686	474927.371465	40.265255
3313.197702	475655.771671	40.270272
3316.370903	476390.488274	40.275290
3319.757038	477122.212267	40.280308
3322.682352	477843.316227	40.285325
3326.060236	478602.941409	40.290343
3329.161999	479340.542936	40.295360
3332.437085	480100.531253	40.300378
3335.656725	480835.632071	40.305396
3339.260924	481607.134830	40.310413
3342.562558	482368.294544	40.315431
3346.398241	483120.293991	40.320448
3349.309745	483882.871047	40.325466
3352.701572	484656.560294	40.330484
3356.300099	485438.068514	40.335501
3359.397563	486220.584123	40.340519
3362.802386	486998.976958	40.345536
3365.593922	487785.720889	40.350554
3369.181825	488581.400255	40.355572
3372.811954	489376.938364	40.360589
3375.692754	490179.482234	40.365607
3379.187463	490990.734924	40.370624
3382.467796	491799.106966	40.375642
3386.060709	492605.626544	40.380660
3389.533635	493421.979240	40.385677
3392.749706	494245.558894	40.390695
3396.472118	495061.900448	40.395712
3399.895193	495880.475018	40.400730
3403.407996	496700.715663	40.405748
3406.793985	497534.169732	40.410765
3409.888393	498366.874081	40.415783
3413.773123	499185.933381	40.420800
3416.973826	500031.924541	40.425818
3420.376531	500864.615820	40.430836
3423.890124	501704.773081	40.435853
3426.901523	502550.422197	40.440871
3430.250642	503390.323611	40.445888
3433.891936	504243.061367	40.450906
3437.287472	505083.581276	40.455924
3440.811314	505944.936681	40.460941
3443.898312	506809.498238	40.465959
3447.622633	507652.517199	40.470976
3451.142042	508523.586733	40.475994
3454.251032	509384.584323	40.481012
3458.094139	510244.312525	40.486029
3461.624427	511107.579029	40.491047
3465.412379	511963.545808	40.496064
3468.717190	512817.376249	40.501082
3472.104482	513680.130807	40.506100
3475.609159	514546.253099	40.511117
3479.027627	515394.097600	40.516122
3482.686523	516192.583819	40.521127
3485.662093	516937.282547	40.526132
3489.090591	517619.576448	40.531136
3492.168027	518263.315757	40.536141
3495.103690	518834.138621	40.541146
3497.769815	519329.494046	40.546151
3499.924743	519781.786413	40.551156
3502.289235	520176.950711	40.556160
3504.509792	520517.271528	40.561165
3506.342911	520810.425070	40.566170
3508.122183	521051.709852	40.571175
3509.638430	521255.317184	40.576180
3511.205969	521402.745687	40.581184
3512.606049	521493.273115	40.586189
3513.933087	521599.585027	40.591194
3515.243871	521615.707445	40.596199
3516.066918	521629.935253	40.601204
3516.894998	521603.009820	40.606208
3517.846403	521555.640232	40.611213
3518.701924	521467.537337	40.616218
3519.594186	521359.205520	40.621223
3520.115650	521228.686504	40.626228
3520.102302	521091.324596	40.631232
3520.734262	520918.671222	40.636237
3521.287615	520746.483476	40.641242
3521.446286	520540.835603	40.646247
3521.489446	520356.135144	40.651252
3521.783089	520132.006494	40.656256
3522.156978	519914.738409	40.661261
3521.915581	519692.963567	40.666266
3522.030021	519437.909924	40.671271
3522.059724	519205.265265	40.676276
3521.869963	518959.353667	40.681280
3521.999017	518698.926477	40.686285
3521.754010	518443.711986	40.691290
3521.821242	518196.281994	40.696295
3521.596668	517921.183606	40.701300
3521.403572	517684.760184	40.706304
3521.674720	517397.590150	40.711309
3521.144806	517152.666238	40.716314
3521.508133	516879.581574	40.721319
3521.428410	516598.875618	40.726324
3520.940727	516347.864620	40.731328
3521.215984	516077.562177	40.736333
3520.990185	515801.164556	40.741338
3520.877291	515535.921476	40.746343
3520.446218	515262.733580	40.751348
3520.180649	515020.973379	40.756352
3520.297318	514749.258397	40.761357
3519.642662	514500.066801	40.766362
3519.559697	514234.090296	40.771367
3519.147541	513980.654662	40.776372
3518.911315	513738.416145	40.781376
3519.143923	513484.011280	40.786381
3518.976570	513240.237300	40.791386
3518.627386	512998.005999	40.796391
3518.009428	512747.012290	40.801396
3518.108871	512506.776947	40.806400
3518.077368	512266.912983	40.811405
3517.620513	512051.798311	40.816410
3517.291820	511813.644207	40.821415
3517.145328	511593.314939	40.826420
3516.777815	511364.316789	40.831424
3516.630924	511133.206597	40.836429
3516.331510	510942.436237	40.841434
3516.237349	510727.601612	40.846439
3516.161006	510515.189763	40.851444
3515.907707	510308.014020	40.856448
3515.922409	510099.376873	40.861453
3515.556630	509900.662622	40.866458
3515.446182	509705.447144	40.871463
3515.307586	509500.368361	40.876468
3515.108287	509322.414596	40.881472
3514.786230	509109.973562	40.886477
3514.541619	508910.520382	40.891482
3514.467679	508747.617926	40.896487
3514.028412	508551.125838	40.901492
3514.093773	508362.849474	40.906496
3513.928267	508208.355297	40.911501
3513.896190	508028.843843	40.916506
3513.825620	507852.929018	40.921511
3513.271327	507679.517549	40.926516
3512.924171	507522.516056	40.931520
3512.994841	507360.994413	40.936525
3512.662815	507214.917069	40.941530
3512.807602	507049.282273	40.946535
3512.513212	506893.632933	40.951540
3512.192725	506746.841422	40.956544
3512.505682	506591.801797	40.961549
3512.024950	506451.510043	40.966554
3512.152154	506305.554875	40.971559
3511.859483	506147.621499	40.976564
3511.873048	506021.062577	40.981568
3511.691729	505882.945437	40.986573
3511.504063	505740.526910	40.991578
3511.570537	505596.751355	40.996583
3511.356123	505462.279596	41.001588
3511.035434	505332.884064	41.006592
3511.339119	505190.940052	41.011597
3510.755218	505079.498430	41.016602
3510.346322	504945.205247	41.021607
3510.783220	504819.684043	41.026612
3510.534580	504708.288283	41.031616
3510.365708	504589.591829	41.036621
3510.172501	504476.768847	41.041626
3510.296418	504352.558944	41.046631
3509.797958	504247.373853	41.051636
3509.818331	504128.846805	41.056640
3510.077540	504027.083218	41.061645
3509.796994	503918.167299	41.066650
3509.337240	503808.115021	41.071655
3509.565264	503720.069637	41.076660
3509.623131	503615.906247	41.081664
3509.481160	503493.149367	41.086669
3508.993656	503414.072282	41.091674
3509.301373	503303.338841	41.096679
3509.108567	503216.167220	41.101684
3508.754158	503135.347083	41.106688
3508.794647	503035.687390	41.111693
3508.465712	502951.066537	41.116698
3508.868863	502852.310112	41.121703
3508.495465	502752.815461	41.126708
3508.545961	502698.095759	41.131712
3508.708486	502593.201224	41.136717
3508.286416	502515.577535	41.141722
3508.388476	502426.381517	41.146727
3508.254837	502348.255992	41.151732
3508.323457	502273.033737	41.156736
3508.483895	502184.586478	41.161741
3507.937690	502110.321136	41.166746
3507.876278	502027.779372	41.171751
3507.780775	501946.912886	41.176756
3507.293468	501878.306074	41.181760
3507.644604	501809.009721	41.186765
3507.396418	501742.490412	41.191770
3507.640604	501686.572833	41.196775
3507.525642	501624.435542	41.201780
3507.339092	501546.770388	41.206784
3507.310653	501473.736554	41.211789
3507.303108	501415.225889	41.216794
3507.372465	501343.947622	41.221799
3507.456972	501278.183853	41.226804
3507.417309	501205.707473	41.231808
3507.512923	501140.194521	41.236813
3507.286804	501088.955512	41.241818
3507.392874	501026.578734	41.246823
3507.474424	500963.395737	41.251828
3507.553887	500892.620240	41.256832
3507.623948	500819.011364	41.261837
3507.265910	500762.679889	41.266842
3507.300711	500677.332677	41.271847
3507.253465	500622.672652	41.276852
3506.890051	500563.101834	41.281856
3507.028410	500492.922864	41.286861
3506.846122	500432.209375	41.291866
3506.957504	500375.701250	41.296871
3507.151316	500315.130398	41.301876
3506.748600	500263.866311	41.306880
3506.868551	500206.394533	41.311885
3506.726851	500162.631182	41.316890
3506.802005	500103.445092	41.321895
3506.668558	500042.115124	41.326900
3506.718408	499983.945034	41.331904
3507.211483	499936.183068	41.336909
3506.667981	499882.510374	41.341914
3506.669244	499810.021863	41.346919
3507.015650	499768.762048	41.351924
3506.642286	499707.823198	41.356928
3506.659331	499653.808122	41.361933
3506.223781	499608.014401	41.366938
3506.209943	499555.876889	41.371943
3506.202400	499515.077401	41.376948
3506.290231	499467.681964	41.381952
3506.447780	499419.667925	41.386957
3506.108789	499374.972021	41.391962
3506.221592	499323.269413	41.396967
3506.454103	499270.484676	41.401972
3506.255782	499230.271535	41.406976
3506.414468	499172.942190	41.411981
3505.920794	499131.712441	41.416986
3506.224540	499090.559057	41.421991
3506.207612	499048.798167	41.426996
3505.980064	498999.730172	41.432000
3506.405390	498953.393740	41.437005
3506.184239	498905.387557	41.442010
3506.323496	498870.536918	41.447015
3506.264361	498823.770489	41.452020
3505.999599	498777.947658	41.457024
3505.998705	498739.727151	41.462029
3506.028911	498701.197907	41.467034
3506.110348	498647.675867	41.472039
3506.443942	498603.681725	41.477044
3505.932799	498566.148980	41.482048
3506.386236	498515.807687	41.487053
3505.959359	498471.427172	41.492058
3505.799157	498426.599406	41.497063
3505.719512	498383.075033	41.502068
3505.831863	498340.279578	41.507072
3505.804631	498298.316079	41.512077
3505.854245	498264.541556	41.517082
3505.910425	498223.982195	41.522087
3505.888634	498197.812568	41.527092
3505.704947	498163.264729	41.532096
3505.490163	498112.572298	41.537101
3505.905178	498087.548481	41.542106
3505.918348	498050.792425	41.547111
3505.843630	498009.291388	41.552116
3505.734504	497971.845743	41.557120
3505.585058	497937.292060	41.562125
3505.767374	497905.520921	41.567130
3505.686996	497858.046585	41.572135
3505.573963	497818.930585	41.577140
3505.561041	497795.138398	41.582144
3505.779771	497752.476618	41.587149
3505.699959	497714.266413	41.592154
3505.464126	497689.142406	41.597159
3505.522179	497640.683718	41.602164
3505.264933	497615.107353	41.607168
3505.538864	497575.474029	41.612173
3505.325397	497546.194895	41.617178
3505.754708	497521.016157	41.622183
3505.728423	497504.819730	41.627188
3505.603317	497455.528838	41.632192
3505.607937	497414.013896	41.637197
3505.526154	497380.055980	41.642202
3505.290373	497350.425666	41.647207
3505.372241	497312.695335	41.652212
3505.432929	497283.018054	41.657216
3505.387124	497247.687260	41.662221
3505.350335	497223.999350	41.667226
3505.497293	497186.967258	41.672231
3505.320789	497160.516817	41.677236
3505.372558	497127.904274	41.682240
3505.671795	497083.456217	41.687245
3505.643994	497053.741919	41.692250
3505.257707	497023.780460	41.697255
3505.340191	497000.934089	41.702260
3505.218455	496969.310622	41.707264
3505.397331	496936.424504	41.712269
3505.394165	496909.237501	41.717274
3505.720139	496879.315119	41.722279
3505.522944	496840.564709	41.727284
3505.270595	496810.733617	41.732288
3505.453496	496777.441545	41.737293
3505.138065	496740.076590	41.742298
3505.199185	496721.131680	41.747303
3505.168530	496682.455871	41.752308
3505.346154	496647.037966	41.757312
3505.311471	496617.627819	41.762317
3504.711141	496606.432369	41.767322
3504.673417	496585.427134	41.772327
3505.202992	496553.193709	41.777332
3504.826661	496530.925558	41.782336
3505.126961	496503.841875	41.787341
3504.841008	496475.585064	41.792346
3505.068348	496462.891709	41.797351
3505.041450	496431.809246	41.802356
3504.868338	496405.914098	41.807360
3505.002201	496369.743121	41.812365
3505.045063	496361.382409	41.817370
3505.531278	496334.117201	41.822375
3505.437755	496298.336432	41.827380
3505.266712	496276.896239	41.832384
3505.136527	496246.690500	41.837389
3505.140128	496213.678888	41.842394
3505.068316	496188.020573	41.847399
3504.962396	496167.228156	41.852404
3505.132682	496151.151347	41.857408
3505.297213	496110.266353	41.862413
3504.645458	496097.914207	41.867418
3504.803736	496075.358480	41.872423
3504.970035	496041.915795	41.877428
3504.669545	496040.748172	41.882432
3505.110883	496001.135591	41.887437
3504.868103	495984.010035	41.892442
3504.975343	495948.956317	41.897447
3504.730256	495942.919330	41.902452
3504.744529	495914.614197	41.907456
3505.001989	495880.954284	41.912461
3504.874907	495862.493911	41.917466
3505.047717	495840.695070	41.922471
3504.877880	495813.634037	41.927476
3504.896792	495797.277051	41.932480
3505.244329	495763.147000	41.937485
3505.045759	495750.520465	41.942490
3504.567862	495734.748262	41.947495
3504.762268	495711.224370	41.952500
3504.948905	495695.043312	41.957504
3504.873792	495652.878738	41.962509
3505.231092	495641.278179	41.967514
3505.167532	495611.972236	41.972519
3505.333147	495578.933870	41.977524
3505.021756	495559.489674	41.982528
3505.099649	495526.515710	41.987533
3504.978881	495509.876749	41.992538
3504.968620	495477.625484	41.997543
3504.863649	495468.680137	42.002548
3505.001271	495435.038344	42.007552
3505.205719	495399.461882	42.012557
3505.005393	495397.721425	42.017562
3504.892745	495372.574746	42.022567
3505.202986	495336.120681	42.027572
3504.928206	495318.138797	42.032576
3505.031603	495290.173043	42.037581
3504.800084	495264.842471	42.042586
3505.091331	495238.821642	42.047591
3505.208254	495219.461289	42.052596
3504.986208	495189.268319	42.057600
3505.211348	495159.662857	42.062605
3505.025158	495140.299693	42.067610
3504.919257	495117.582005	42.072615
3505.105685	495078.311517	42.077620
3505.332776	495060.300693	42.082624
3505.381474	495029.811500	42.087629
3504.863996	495004.424495	42.092634
3505.080201	494976.339165	42.097639
3505.075667	494949.959603	42.102644
3504.883600	494925.584372	42.107648
3504.843193	494891.564646	42.112653
3504.936312	494881.068678	42.117658
3504.864803	494852.421021	42.122663
3504.960332	494830.683827	42.127668
3504.817769	494811.009614	42.132672
3504.853391	494774.395299	42.137677
3504.796826	494761.695002	42.142682
3504.903725	494748.665053	42.147687
3504.954982	494708.604984	42.152692
3504.939755	494694.632240	42.157696
3505.245478	494681.469550	42.162701
3505.366961	494663.424393	42.167706
3505.014222	494628.187672	42.172711
3504.722450	494585.345995	42.177716
3504.981622	494576.292024	42.182720
3504.962392	494546.876101	42.187725
3504.655911	494536.443093	42.192730
3504.930889	494509.765546	42.197735
3505.015612	494486.054877	42.202740
3504.882337	494463.695152	42.207744
3504.961716	494436.693965	42.212749
3504.771001	494417.229482	42.217754
3504.982808	494401.499025	42.222759
3505.055143	494364.928727	42.227764
3504.857311	494348.655341	42.232768
3504.982222	494318.456736	42.237773
3504.777260	494298.437385	42.242778
3504.625213	494274.156234	42.247783
3504.826199	494252.047237	42.252788
3504.686875	494240.119199	42.257792
3504.985268	494218.450490	42.262797
3505.020389	494185.126423	42.267802
3504.515789	494167.432912	42.272807
3505.009498	494145.885157	42.277812
3504.623636	494123.514303	42.282816
3504.717478	494101.168877	42.287821
3504.450467	494085.969555	42.292826
3504.669808	494063.249794	42.297831
3504.828004	494041.451126	42.302836
3504.656094	494026.388633	42.307840
3504.979772	494010.690798	42.312845
3504.676185	493991.446250	42.317850
3504.806149	493980.792035	42.322855
3504.930174	493951.301882	42.327860
3504.824191	493930.608208	42.332864
3504.763457	493900.185074	42.337869
3504.931749	493899.145767	42.342874
3504.871468	493864.874097	42.347879
3505.191272	493846.189150	42.352884
3504.940882	493824.150980	42.357888
3505.054817	493801.093095	42.362893
3505.007729	493772.136072	42.367898
3504.950785	493745.459241	42.372903
3504.831359	493719.197346	42.377908
3504.796680	493691.048432	42.382912
3505.088276	493668.924415	42.387917
3504.698992	493643.515264	42.392922
3504.738898	493632.672532	42.397927
3504.595412	493586.564280	42.402932
3504.731258	493568.262592	42.407936
3504.482063	493569.719866	42.412941
3504.688393	493547.102801	42.417946
3504.642409	493515.208201	42.422951
3504.859710	493500.640782	42.427956
3504.643022	493489.534692	42.432960
3505.238598	493463.564532	42.437965
3504.879127	493439.163149	42.442970
3504.878436	493414.553114	42.447975
3504.712493	493393.615123	42.452980
3504.582357	493376.621241	42.457984
3504.775677	493354.107273	42.462989
3504.953400	493326.126787	42.467994
3504.906827	493304.612805	42.472999
3505.012693	493286.821962	42.478004
3504.650197	493271.434504	42.483008
3505.012663	493238.715292	42.488013
3504.987396	493231.731168	42.493018
3504.452260	493193.887312	42.498023
3504.685861	493181.190702	42.503028
3504.711840	493166.146869	42.508032
3504.773659	493154.996560	42.513037
3504.879765	493122.925329	42.518042
3504.489080	493099.642489	42.523047
3504.495634	493084.297824	42.528052
3504.419546	493068.915570	42.533056
3504.529372	493045.756113	42.538061
3504.539621	493022.916202	42.543066
3504.148751	493004.342728	42.548071
3504.494807	492991.425657	42.553076
3504.204889	493000.181484	42.558080
3504.453083	492959.681373	42.563085
3504.366750	492959.188652	42.568090
3504.371080	492951.642710	42.573095
3504.762986	492931.882016	42.578100
3504.632597	492923.496482	42.583104
3504.876761	492893.529896	42.588109
3504.776004	492879.468014	42.593114
3504.753116	492854.962022	42.598119
3504.717118	492829.445273	42.603124
3504.445748	492817.689102	42.608128
3504.725349	492801.085691	42.613133
3505.069471	492782.243909	42.618138
3504.750554	492760.924258	42.623143
3504.707957	492737.180826	42.628148
3504.549683	492711.581959	42.633152
3504.778846	492687.896792	42.638157
3504.624792	492675.514307	42.643162
3504.488744	492661.153995	42.648167
3505.027516	492632.051950	42.653172
3504.735602	492621.058507	42.658176
3504.736798	492599.282953	42.663181
3504.529233	492580.680081	42.668186
3504.823567	492559.465837	42.673191
3504.873113	492542.240226	42.678196
3504.599457	492526.990028	42.683200
3504.619066	492487.436545	42.688205
3504.635705	492482.116662	42.693210
3504.437946	492459.410213	42.698215
3504.879894	492434.678275	42.703220
3504.834538	492420.809853	42.708224
3504.633826	492390.558280	42.713229
3504.800466	492385.062738	42.718234
3504.818952	492354.168769	42.723239
3504.499686	492332.747398	42.728244
3504.454881	492319.942278	42.733248
3504.772697	492298.572100	42.738253
3504.543389	492274.958868	42.743258
3504.583897	492263.203694	42.748263
3505.115953	492239.216877	42.753268
3504.668009	492226.779257	42.758272
3504.593610	492210.737683	42.763277
3504.397171	492187.929410	42.768282
3504.521077	492166.842937	42.773287
3504.627613	492144.239933	42.778292
3504.616126	492137.253218	42.783296
3504.858735	492111.539522	42.788301
3504.909693	492075.727702	42.793306
3504.643500	492067.515169	42.798311
3504.734906	492041.268213	42.803316
3504.489440	492035.179354	42.808321
3504.747563	492013.159937	42.813325
3504.355159	491994.383122	42.818330
3504.412970	491982.979531	42.823335
3504.566091	491953.684166	42.828340
3504.108012	491940.792176	42.833345
3504.373790	491944.497727	42.838349
3504.623619	491906.577816	42.843354
3504.163520	491893.584828	42.848359
3504.716044	491882.862622	42.853364
3504.723347	491874.606779	42.858369
3504.605669	491865.307192	42.863373
3504.591566	491843.938310	42.868378
3504.222890	491837.919502	42.873383
3504.832911	491809.665835	42.878388
3504.681179	491798.193963	42.883393
3504.742603	491774.989929	42.888397
3504.697187	491747.295543	42.893402
3504.431062	491740.247639	42.898407
3504.373855	491711.440921	42.903412
3504.265267	491694.695304	42.908417
3504.575413	491680.516927	42.913421
3504.483320	491677.999362	42.918426
3504.394146	491648.286025	42.923431
3504.489117	491641.940659	42.928436
3504.064139	491635.829397	42.933441
3504.602744	491600.648593	42.938445
3504.530009	491597.267023	42.943450
3504.135284	491580.110739	42.948455
3504.568391	491561.810733	42.953460
3504.565908	491551.935707	42.958465
3504.822930	491529.054955	42.963469
3504.629576	491519.919087	42.968474
3504.684244	491514.542272	42.973479
3504.583603	491469.941286	42.978484
3504.241442	491480.681181	42.983489
3504.274026	491449.935413	42.988493
3504.246023	491438.241190	42.993498
3504.172138	491429.643475	42.998503
3504.462610	491414.910925	43.003508
3504.281881	491409.419354	43.008513
3504.555889	491384.206129	43.013517
3504.710364	491388.283890	43.018522
3504.437487	491356.674658	43.023527
3504.714062	491341.488452	43.028532
3504.415892	491321.632541	43.033537
3504.201483	491300.750489	43.038541
3504.333119	491286.296163	43.043546
3504.383085	491265.270999	43.048551
3504.855694	491244.685455	43.053556
3504.512759	491233.192811	43.058561
3504.897156	491196.972091	43.063565
3504.788044	491194.305217	43.068570
3504.580747	491179.094067	43.073575
3505.051409	491145.645053	43.078580
3504.379332	491126.151896	43.083585
3504.688134	491093.133525	43.088589
3504.675982	491080.828838	43.093594
3504.384658	491064.516693	43.098599
3504.818617	491048.089903	43.103604
3504.555890	491026.404866	43.108609
3504.628522	491003.299389	43.113613
3504.296359	490993.830687	43.118618
3504.869595	490977.027308	43.123623
3504.784395	490951.414468	43.128628
3504.472648	490929.990292	43.133633
3504.383533	490917.900241	43.138637
3504.514217	490901.723835	43.143642
3504.695778	490880.576150	43.148647
3504.516887	490874.830904	43.153652
3504.495506	490848.042996	43.158657
3504.305216	490826.042406	43.163661
3504.564645	490830.508864	43.168666
3504.335208	490804.564102	43.173671
3504.661509	490781.722132	43.178676
3504.279541	490773.071516	43.183681
3504.192539	490745.128987	43.188685
3504.288329	490735.643161	43.193690
3504.258334	490733.925982	43.198695
3504.226775	490720.661859	43.203700
3504.369085	490700.786314	43.208705
3504.259993	490692.396406	43.213709
3504.195479	490682.885244	43.218714
3504.024946	490665.743328	43.223719
3504.369747	490652.824839	43.228724
3504.340927	490637.939559	43.233729
3504.121615	490637.771667	43.238733
3504.175887	490624.139389	43.243738
3503.870741	490598.408890	43.248743
3503.804616	490605.256569	43.253748
3503.521930	490589.145227	43.258753
3504.224632	490610.862584	43.263757
3504.186857	490569.693431	43.268762
3504.052768	490583.996819	43.273767
3504.351237	490539.431823	43.278772
3504.136941	490561.395462	43.283777
3504.306178	490536.147007	43.288781
3504.319235	490511.581603	43.293786
3504.293149	490509.002801	43.298791
3504.435370	490501.282133	43.303796
3504.426050	490470.136206	43.308801
3504.286791	490469.499843	43.313805
3504.244589	490462.871880	43.318810
3504.195757	490455.535914	43.323815
3504.275286	490435.264839	43.328820
3504.240642	490443.120528	43.333825
3504.353043	490417.323787	43.338829
3504.186474	490388.481665	43.343834
3504.127411	490399.177435	43.348839
3504.311021	490389.474969	43.353844
3504.172001	490377.088576	43.358849
3504.425100	490348.129418	43.363853
3504.454250	490339.666856	43.368858
3504.230881	490336.156924	43.373863
3504.259306	490309.816194	43.378868
3504.245396	490304.601811	43.383873
3504.230618	490299.438210	43.388877
3504.311363	490285.548268	43.393882
3504.167722	490264.349992	43.398887
3504.408070	490249.016687	43.403892
3504.374617	490248.110359	43.408897
3504.025744	490227.906769	43.413901
3504.227015	490202.196980	43.418906
3504.161670	490217.350781	43.423911
3504.391394	490205.463112	43.428916
3504.502711	490175.614450	43.433921
3504.584408	490160.913912	43.438925
3504.686747	490150.363166	43.443930
3504.306993	490125.707398	43.448935
3504.613157	490122.620206	43.453940
3504.448454	490103.602907	43.458945
3504.349904	490089.994394	43.463949
3504.601005	490081.142105	43.468954
3504.615476	490037.988281	43.473959
3504.506747	490039.170386	43.478964
3504.525514	490018.604580	43.483969
3504.412120	489997.755754	43.488973
3504.446395	489994.812808	43.493978
3504.694865	489970.969201	43.498983
3504.464760	489946.036307	43.503988
3504.535435	489930.324377	43.508993
3504.315777	489922.458076	43.513997
3504.546522	489905.859815	43.519002
3504.318887	489886.041877	43.524007
3504.261008	489869.641144	43.529012
3504.350298	489866.841427	43.534017
3504.630318	489843.904335	43.539021
3504.233532	489814.692533	43.544026
3504.053531	489825.812928	43.549031
3504.439467	489813.191249	43.554036
3504.190238	489791.300054	43.559041
3504.085923	489783.263520	43.564045
3504.472999	489763.854779	43.569050
3504.250066	489759.686243	43.574055
3504.583632	489735.322407	43.579060
3504.405824	489736.160910	43.584065
3504.229426	489726.008518	43.589069
3504.152464	489694.871995	43.594074
3504.191321	489681.190820	43.599079
3504.262877	489672.366716	43.604084
3503.915912	489676.473456	43.609089
3503.932545	489680.016245	43.614093
3503.973265	489650.228555	43.619098
3504.323137	489644.804546	43.624103
3504.364479	489636.846226	43.629108
3504.219784	489621.674562	43.634113
3504.420115	489603.713331	43.639117
3504.244899	489599.993055	43.644122
3503.940064	489590.873862	43.649127
3504.162666	489591.041303	43.654132
3504.020967	489563.105657	43.659137
3504.088149	489550.787426	43.664141
3504.120841	489539.487613	43.669146
3503.969730	489557.441185	43.674151
3504.217119	489524.480410	43.679156
3503.924913	489510.142352	43.684161
3504.206544	489501.842103	43.689165
3504.528688	489503.006790	43.694170
3504.224757	489488.721218	43.699175
3504.631911	489464.193453	43.704180
3504.395773	489480.033280	43.709185
3504.292731	489436.542105	43.714189
3504.556177	489422.268106	43.719194
3504.314855	489418.760839	43.724199
3504.470344	489398.527289	43.729204
3504.549386	489383.421370	43.734209
3504.263192	489368.829008	43.739213
3504.468885	489350.967986	43.744218
3504.285244	489330.281470	43.749223
3504.213781	489324.974612	43.754228
3504.190317	489321.584842	43.759233
3504.297288	489300.852362	43.764237
3504.186428	489288.815346	43.769242
3504.230914	489274.829090	43.774247
3504.432997	489261.172461	43.779252
3504.097500	489246.638446	43.784257
3504.214336	489235.629049	43.789261
3504.264914	489226.960001	43.794266
3504.015627	489222.238365	43.799271
3504.310865	489190.788933	43.804276
3504.150062	489188.636439	43.809281
3504.305377	489181.318359	43.814285
3504.349536	489153.909877	43.819290
3504.429492	489146.907593	43.824295
3504.254881	489135.944202	43.829300
3504.035853	489139.777588	43.834305
3504.284901	489097.344278	43.839309
3504.101243	489107.047476	43.844314
3503.976513	489110.967264	43.849319
3504.400170	489081.675300	43.854324
3504.062136	489065.925945	43.859329
3503.903310	489053.187259	43.864333
3504.039773	489065.574988	43.869338
3504.083263	489040.445699	43.874343
3504.358700	489026.979908	43.879348
3504.112599	489028.183787	43.884353
3504.051685	489033.461059	43.889357
3504.283897	489022.230703	43.894362
3504.049047	489005.755887	43.899367
3504.478832	488980.464164	43.904372
3504.391075	488990.354866	43.909377
3504.176086	488968.457300	43.914381
3503.892402	488950.065441	43.919386
3503.979511	488934.755286	43.924391
3504.405475	488930.433357	43.929396
3504.262940	488934.761199	43.934401
3504.130090	488914.927255	43.939405
3504.188224	488894.809853	43.944410
3504.207671	488885.233859	43.949415
3504.529240	488868.924234	43.954420
3504.408202	488870.412260	43.959425
3504.204671	488847.601032	43.964429
3504.331280	488831.271538	43.969434
3504.147035	488846.293283	43.974439
3504.465867	488798.074097	43.979444
3504.338397	488830.814644	43.984449
3504.131404	488787.946209	43.989453
3504.207292	488769.396042	43.994458
3503.824369	488774.217772	43.999463
3504.403449	488749.813860	44.004468
3504.099123	488757.003763	44.009473
3504.326453	488725.969497	44.014477
3504.098017	488708.632341	44.019482
3504.150554	488721.033561	44.024487
3504.298259	488701.205701	44.029492
3504.073142	488692.124122	44.034497
3504.083130	488664.619029	44.039501
3504.326467	488649.182648	44.044506
3504.132710	488677.983144	44.049511
3504.107141	488620.852693	44.054516
3504.166239	488636.595913	44.059521
3504.349823	488613.014101	44.064525
3504.438619	488625.510955	44.069530
3504.074926	488591.074943	44.074535
3504.250035	488549.969024	44.079540
3504.178441	488596.731589	44.084545
3504.171942	488544.865629	44.089549
3504.285567	488539.985160	44.094554
3503.869007	488516.700687	44.099559
3504.031072	488531.414690	44.104564
3504.027603	488524.931876	44.109569
3504.241810	488511.880608	44.114573
3504.279540	488483.459138	44.119578
3503.982804	488506.349932	44.124583
3504.226444	488487.924930	44.129588
3504.202475	488463.160097	44.134593
3504.388799	488465.156744	44.139597
3504.579035	488432.760264	44.144602
3504.045199	488432.186194	44.149607
3504.440307	488412.622840	44.154612
3504.496286	488393.872844	44.159617
3504.029193	488388.324341	44.164621
3503.932526	488385.148580	44.169626
3504.117988	488347.332956	44.174631
3504.358599	488336.658037	44.179636
3504.330844	488361.279314	44.184641
3504.195036	488344.028487	44.189645
3503.719855	488319.739996	44.194650
3503.714047	488313.004218	44.199655
3504.124544	488309.343071	44.204660
3503.877874	488315.207075	44.209665
3504.048352	488308.949954	44.214669
3504.107682	488300.937575	44.219674
3504.006330	488282.718856	44.224679
3503.941915	488279.386024	44.229684
3503.977046	488266.920064	44.234689
3503.861920	488269.572203	44.239693
3504.144802	488261.271214	44.244698
3503.790516	488251.804620	44.249703
3503.944232	488235.520979	44.254708
3504.088822	488229.267924	44.259713
3504.278307	488224.577993	44.264717
3504.235741	488213.441238	44.269722
3503.873600	488212.080238	44.274727
3504.270212	488190.237062	44.279732
3504.306213	488176.453943	44.284737
3503.994829	488173.464040	44.289741
3504.429544	488168.532727	44.294746
3504.099335	488168.129073	44.299751
3504.365843	488143.520521	44.304756
3504.327401	488135.624830	44.309761
3503.982475	488113.240283	44.314765
3503.959331	488106.203257	44.319770
3503.863934	488102.368763	44.324775
3504.329793	488078.083187	44.329780
3504.348195	488084.006673	44.334785
3503.950715	488079.257518	44.339789
3504.275961	488057.374816	44.344794
3504.114426	488051.271391	44.349799
3504.176610	488047.158717	44.354804
3504.201497	488044.520868	44.359809
3504.395494	488007.057786	44.364813
3504.646294	487996.127801	44.369818
3504.157373	487988.860429	44.374823
3504.375977	487969.780393	44.379828
3504.776652	487969.615789	44.384833
3504.360108	487949.471099	44.389837
3504.641964	487925.011797	44.394842
3504.326363	487908.802051	44.399847
3504.504088	487878.280768	44.404852
3503.936549	487878.167884	44.409857
3503.691228	487863.010709	44.414861
3504.570385	487867.227968	44.419866
3503.825506	487842.930836	44.424871
3504.297291	487822.949530	44.429876
3503.951132	487823.308190	44.434881
3503.852715	487815.827072	44.439885
3504.241983	487812.067878	44.444890
3504.090124	487798.263522	44.449895
3504.375349	487781.350865	44.454900
3504.013443	487778.368884	44.459905
3504.249671	487779.395300	44.464909
3504.410762	487748.775130	44.469914
3504.025460	487740.123639	44.474919
3504.091237	487731.198235	44.479924
3504.349697	487730.802839	44.484929
3504.204225	487704.789877	44.489933
3504.328657	487698.083950	44.494938
3503.815882	487700.393787	44.499943
3504.208680	487686.857842	44.504948
3503.984694	487661.515728	44.509953
3504.004070	487659.638504	44.514957
3504.183222	487643.400988	44.519962
3504.212686	487641.420860	44.524967
3504.350542	487640.943216	44.529972
3504.287167	487628.441751	44.534977
3504.315620	487613.443722	44.539981
3504.682525	487611.308950	44.544986
3504.083181	487591.699310	44.549991
3504.178197	487566.306650	44.554996
3504.221318	487570.200227	44.560001
3504.188125	487555.617128	44.565005
3504.152037	487522.647015	44.570010
3503.677526	487525.811946	44.575015
3503.961698	487509.861643	44.580020
3504.249346	487517.110415	44.585025
3504.064352	487501.639491	44.590029
3503.955127	487470.048511	44.595034
3503.743595	487480.871341	44.600039
3503.831386	487470.220089	44.605044
3503.663866	487475.717262	44.610049
3503.870740	487464.287371	44.615053
3504.230580	487459.570327	44.620058
3504.127726	487468.299159	44.625063
3504.194784	487440.985886	44.630068
3504.018371	487432.757128	44.635073
3504.104003	487428.539305	44.640077
3504.032489	487425.207444	44.645082
3503.913728	487419.451636	44.650087
3504.123067	487392.267768	44.655092
3503.541196	487399.957941	44.660097
3504.220998	487380.449839	44.665101
3504.487683	487366.325744	44.670106
3504.168108	487374.481017	44.675111
3504.036160	487358.343083	44.680116
3504.186932	487349.049484	44.685121
3504.203473	487338.814657	44.690125
3503.919081	487335.415116	44.695130
3504.088806	487304.995485	44.700135
3504.260209	487287.847105	44.705140
3503.900980	487305.481122	44.710145
3504.206560	487295.048625	44.715149
3504.419839	487272.017656	44.720154
3504.133860	487266.592159	44.725159
3504.133990	487247.697893	44.730164
3504.271797	487245.396670	44.735169
3504.221632	487235.020365	44.740173
3504.545939	487218.354306	44.745178
3504.107044	487208.039426	44.750183
3504.212891	487194.700450	44.755188
3504.504819	487169.529413	44.760193
3504.239301	487164.100654	44.765197
3504.463611	487154.086165	44.770202
3504.221380	487138.674647	44.775207
3504.042721	487116.769195	44.780212
3503.999550	487114.141974	44.785217
3504.230100	487112.383285	44.790221
3504.318857	487080.659055	44.795226
3503.963272	487068.102095	44.800231
3504.359733	487071.787962	44.805236
3504.093191	487073.603057	44.810241
3504.053356	487051.371657	44.815245
3504.339604	487027.214439	44.820250
3503.850343	487034.383566	44.825255
3504.177836	487023.643524	44.830260
3504.350801	487019.310496	44.835265
3504.152535	486995.483094	44.840269
3504.021433	486987.550915	44.845274
3504.274048	486984.623648	44.850279
3504.717511	486958.212647	44.855284
3504.342758	486934.210439	44.860289
3504.133920	486937.789378	44.865293
3504.473306	486924.210679	44.870298
3504.466465	486915.245714	44.875303
3504.202959	486896.646046	44.880308
3504.296200	486903.672500	44.885313
3504.273691	486871.003046	44.890317
3504.352599	486857.364157	44.895322
3503.863205	486864.735991	44.900327
3504.197639	486837.784841	44.905332
3503.905441	486818.379135	44.910337
3504.056546	486811.111464	44.915341
3504.334431	486804.684906	44.920346
3504.150413	486806.081734	44.925351
3503.917300	486794.569014	44.930356
3503.912088	486772.382472	44.935361
3504.314577	486751.752466	44.940365
3504.120533	486759.482911	44.945370
3504.268369	486770.451970	44.950375
3504.473130	486746.408588	44.955380
3504.197313	486731.913861	44.960385
3504.238332	486732.667251	44.965389
3504.121177	486698.543428	44.970394
3503.974896	486686.409042	44.975399
3503.930546	486673.549348	44.980404
3504.026574	486683.310892	44.985409
3504.053403	486673.935240	44.990413
3504.023479	486667.050721	44.995418
3504.039596	486643.543590	45.000423
3503.994932	486624.199876	45.005428
3503.687258	486621.918331	45.010433
3503.700349	486628.299019	45.015437
3504.112851	486617.798597	45.020442
3503.973118	486630.535511	45.025447
3504.131585	486601.990830	45.030452
3504.201107	486587.390755	45.035457
3503.948535	486579.426947	45.040461
3504.368249	486575.713358	45.045466
3503.821943	486571.899164	45.050471
3503.960132	486547.511457	45.055476
3504.331511	486543.653530	45.060481
3503.789584	486537.001857	45.065485
3504.386902	486533.665444	45.070490
3504.027119	486530.632271	45.075495
3504.052596	486495.472405	45.080500
3504.002325	486495.379065	45.085505
3504.213608	486483.593292	45.090509
3504.142847	486478.488153	45.095514
3504.100718	486465.425339	45.100519
3504.031372	486442.995265	45.105524
3503.809177	486440.244274	45.110529
3504.017227	486442.845588	45.115533
3503.889230	486437.800141	45.120538
3504.174298	486430.612466	45.125543
3504.363495	486403.582345	45.130548
3504.119940	486398.403179	45.135553
3504.203217	486394.590758	45.140557
3504.270211	486389.514479	45.145562
3504.089326	486376.676165	45.150567
3504.147933	486350.781067	45.155572
3504.250414	486350.764899	45.160577
3504.172993	486339.936499	45.165581
3504.276035	486325.786842	45.170586
3503.985868	486318.487413	45.175591
3504.409460	486308.896901	45.180596
3504.012244	486313.873479	45.185601
3503.669929	486290.067961	45.190605
3504.184965	486275.397234	45.195610
3504.286183	486267.174748	45.200615
3504.282312	486261.299115	45.205620
3504.188373	486250.827878	45.210625
3503.861858	486227.121100	45.215629
3504.100393	486222.118980	45.220634
3503.886395	486225.293605	45.225639
3504.064235	486222.428699	45.230644
3504.081726	486217.714802	45.235649
3504.029481	486197.206727	45.240653
3503.830374	486184.776425	45.245658
3503.926422	486190.080336	45.250663
3504.000364	486184.597643	45.255668
3504.335849	486182.619654	45.260673
3503.906659	486174.683591	45.265677
3504.190565	486155.338129	45.270682
3503.783490	486144.257773	45.275687
3503.972092	486132.678000	45.280692
3503.883679	486150.523569	45.285697
3503.945131	486141.192842	45.290701
3504.298251	486118.189037	45.295706
3503.919467	486109.789059	45.300711
3503.893033	486103.309048	45.305716
3503.821992	486094.201871	45.310721
3504.109707	486097.550511	45.315725
3504.045630	486088.644862	45.320730
3503.786717	486073.843014	45.325735
3503.874830	486055.744190	45.330740
3503.892861	486066.024957	45.335745
3503.957561	486045.447578	45.340749
3504.131762	486040.506237	45.345754
3503.886141	486053.006982	45.350759
3504.042623	486045.180931	45.355764
3503.862593	486027.884332	45.360769
3504.036200	486012.456836	45.365773
3504.151016	485998.811658	45.370778
3503.962351	486005.984316	45.375783
3504.174797	486003.823122	45.380788
3504.350496	485982.062993	45.385793
3504.106862	485971.311312	45.390797
3504.337905	485955.520085	45.395802
3504.604465	485952.337166	45.400807
3504.440871	485931.643772	45.405812
3504.358506	485921.981059	45.410817
3504.252649	485903.000896	45.415821
3504.289879	485875.335486	45.420826
3503.982633	485883.793395	45.425831
3504.206682	485862.785367	45.430836
3504.098947	485854.241119	45.435841
3504.020628	485838.448031	45.440845
3504.249065	485824.075550	45.445850
3504.179482	485831.736038	45.450855
3504.282443	485814.546495	45.455860
3503.898959	485791.760037	45.460865
3503.969915	485781.313140	45.465869
3504.172249	485788.778692	45.470874
3504.094621	485788.385720	45.475879
3504.120310	485762.393712	45.480884
3504.370375	485748.777638	45.485889
3504.300719	485740.733910	45.490893
3504.403691	485731.751034	45.495898
3504.387806	485711.186033	45.500903
3504.485522	485694.351824	45.505908
3504.253694	485686.587000	45.510913
3503.930968	485666.627697	45.515917
3504.182792	485645.918996	45.520922
3503.700168	485647.464420	45.525927
3504.268719	485649.755569	45.530932
3504.121854	485639.140385	45.535937
3504.025184	485618.892008	45.540941
3504.244092	485594.287691	45.545946
3504.431714	485598.108173	45.550951
3504.114813	485585.138846	45.555956
3504.234878	485564.805497	45.560961
3504.131733	485560.059846	45.565965
3504.376467	485551.358436	45.570970
3503.815802	485546.533115	45.575975
3503.970292	485521.482951	45.580980
3504.221627	485507.207933	45.585985
3504.014174	485511.850767	45.590989
3504.190030	485505.034625	45.595994
3504.222984	485503.459000	45.600999
3503.877114	485478.082586	45.606004
3503.908478	485480.813277	45.611009
3503.820538	485468.212959	45.616013
3504.077176	485463.613058	45.621018
3503.911925	485473.264537	45.626023
3504.133176	485465.985269	45.631028
3504.384532	485444.719169	45.636033
3503.771042	485437.065225	45.641037
3504.259023	485419.105239	45.646042
3504.050880	485431.752443	45.651047
3504.363085	485403.688274	45.656052
3504.406773	485385.849138	45.661057
3504.186065	485382.743139	45.666061
3503.944123	485366.266285	45.671066
3503.439865	485353.782352	45.676071
3503.552593	485341.403535	45.681076
3504.045426	485331.902914	45.686081
3503.872637	485327.674812	45.691085
3503.891679	485323.771010	45.696090
3504.144584	485333.052509	45.701095
3504.084195	485328.046742	45.706100
3504.060191	485310.927475	45.711105
3503.931553	485293.571430	45.716109
3504.069643	485290.206067	45.721114
3504.104118	485286.958400	45.726119
3504.280131	485293.820385	45.731124
3504.188171	485272.760336	45.736129
3503.869760	485246.264751	45.741133
3504.205556	485252.037632	45.746138
3503.999982	485247.510734	45.751143
3504.318253	485236.821810	45.756148
3504.310058	485207.136206	45.761153
3504.011131	485213.110738	45.766157
3504.209840	485196.969376	45.771162
3503.808901	485203.162676	45.776167
3504.019948	485170.858687	45.781172
3504.220315	485149.043053	45.786177
3503.882839	485157.759361	45.791181
3504.254340	485144.224988	45.796186
3504.190351	485152.898073	45.801191
3503.945036	485136.472215	45.806196
3504.042908	485111.177162	45.811201
3503.792531	485120.133024	45.816205
3504.195443	485111.507736	45.821210
3504.368652	485115.026629	45.826215
3503.805201	485084.060759	45.831220
3503.951826	485081.048635	45.836225
3503.929606	485068.184364	45.841229
3504.289147	485057.590140	45.846234
3504.341620	485062.495965	45.851239
3504.178258	485023.107743	45.856244
3504.082623	485027.226413	45.861249
3503.726317	485023.989804	45.866253
3504.387457	485006.812639	45.871258
3504.132613	485002.293469	45.876263
3503.941466	484979.070357	45.881268
3504.187180	484977.106436	45.886273
3503.803654	484968.301416	45.891277
3504.197610	484966.921995	45.896282
3503.821634	484958.065117	45.901287
3503.678606	484930.882784	45.906292
3503.806310	484925.543218	45.911297
3503.689593	484936.301838	45.916301
3503.943545	484927.548029	45.921306
3503.771348	484935.073110	45.926311
3503.717159	484926.368002	45.931316
3504.152433	484925.640642	45.936321
3503.903145	484928.517091	45.941325
3504.222073	484911.140622	45.946330
3503.998620	484893.849862	45.951335
3504.080785	484880.968968	45.956340
3504.413616	484876.052918	45.961345
3503.942587	484872.682432	45.966349
3504.251201	484844.364710	45.971354
3504.188188	484842.702876	45.976359
3503.973330	484835.796266	45.981364
3504.338866	484824.339724	45.986369
3504.152317	484816.922020	45.991373
3504.321921	484793.641667	45.996378
3503.942871	484786.912975	46.001383
3504.126990	484783.388264	46.006388
3504.002264	484761.370266	46.011393
3504.013494	484752.857386	46.016397
3503.914406	484751.454554	46.021402
3503.831780	484758.002978	46.026407
3503.515463	484748.579297	46.031412
3503.858065	484740.875284	46.036417
3504.160139	484747.768201	46.041421
3504.114184	484738.605754	46.046426
3503.714514	484723.267830	46.051431
3503.867475	484711.287542	46.056436
3503.805847	484710.689372	46.061441
3503.865727	484703.739292	46.066445
3503.638079	484693.440321	46.071450
3503.799574	484703.952452	46.076455
3503.784914	484699.243264	46.081460
3503.792426	484705.220182	46.086465
3503.866178	484684.842560	46.091469
3503.952430	484655.647795	46.096474
3503.742876	484657.150135	46.101479
3503.817969	484653.085353	46.106484
3504.144830	484657.846591	46.111489
3503.883405	484654.442938	46.116493
3504.100094	484649.646511	46.121498
3503.773221	484639.768488	46.126503
3504.199611	484615.180789	46.131508
3504.553696	484597.038552	46.136513
3504.264958	484601.491805	46.141517
3504.177775	484582.051426	46.146522
3503.876522	484572.574615	46.151527
3503.926750	484563.802178	46.156532
3504.178308	484563.103842	46.161537
3504.010551	484574.022717	46.166541
3504.306993	484540.741596	46.171546
3503.894522	484535.943256	46.176551
3503.957609	484529.195255	46.181556
3503.990830	484527.214211	46.186561
3503.838737	484518.828365	46.191565
3504.102510	484509.110234	46.196570
3503.958897	484483.447226	46.201575
3504.176189	484476.472185	46.206580
3503.993560	484475.133198	46.211585
3503.786208	484480.890833	46.216589
3504.086143	484467.620609	46.221594
3503.878940	484452.910659	46.226599
3503.762794	484436.869086	46.231604
3504.038176	484425.375895	46.236609
3503.676153	484430.803354	46.241613
3503.879030	484423.526598	46.246618
3503.843647	484437.565696	46.251623
3503.966222	484433.037402	46.256628
3504.337660	484414.537615	46.261633
3503.985921	484401.218356	46.266637
3503.890833	484389.327735	46.271642
3503.923806	484384.560279	46.276647
3503.890404	484384.210950	46.281652
3504.101644	484383.873617	46.286657
3504.022560	484365.444989	46.291661
3503.850234	484344.700601	46.296666
3503.952393	484350.865319	46.301671
3504.072031	484343.196388	46.306676
3504.407913	484344.409896	46.311681
3504.312172	484312.000968	46.316685
3504.288647	484302.378803	46.321690
3504.152523	484291.305210	46.326695
3504.011835	484285.247946	46.331700
3504.077316	484270.444096	46.336705
3503.883861	484253.249344	46.341709
3504.025597	484243.094402	46.346714
3503.722833	484246.030066	46.351719
3503.954202	484239.863321	46.356724
3504.273285	484237.431763	46.361729
3504.008350	484215.941930	46.366733
3504.226483	484200.100641	46.371738
3503.954607	484214.430595	46.376743
3504.167835	484190.838642	46.381748
3504.073407	484189.333705	46.386753
3504.088387	484170.079416	46.391757
3504.090469	484156.450749	46.396762
3503.819418	484162.573188	46.401767
3503.622987	484170.761017	46.406772
3504.048600	484156.204138	46.411777
3504.156727	484153.957902	46.416781
3504.050748	484122.512872	46.421786
3503.955823	484115.435058	46.426791
3504.337621	484110.967044	46.431796
3504.107300	484100.921495	46.436801
3503.986926	484088.122746	46.441805
3504.200048	484073.548727	46.446810
3504.187454	484074.564012	46.451815
3504.106109	484065.254848	46.456820
3504.229444	484051.353626	46.461825
3504.094855	484041.748885	46.466829
3504.137451	484032.521443	46.471834
3503.668896	484030.467664	46.476839
3504.174034	484024.460234	46.481844
3504.338812	484022.407682	46.486849
3503.994669	483993.786574	46.491853
3504.222283	483983.820576	46.496858
3503.865628	483981.749106	46.501863
3503.595450	483982.754445	46.506868
3504.187749	483980.684982	46.511873
3503.879191	483959.505739	46.516877
3504.190223	483934.479434	46.521882
3503.822556	483939.603941	46.526887
3504.071530	483932.066396	46.531892
3504.204208	483929.309616	46.536897
3504.156469	483917.157902	46.541901
3504.204878	483906.713551	46.546906
3504.307085	483892.562236	46.551911
3504.207294	483893.489985	46.556916
3504.076006	483869.394790	46.561921
3503.982970	483839.213850	46.566925
3504.000942	483860.337882	46.571930
3503.570741	483849.513171	46.576935
3504.016319	483846.453606	46.581940
3504.106148	483835.242711	46.586945
3503.840067	483829.407778	46.591949
3504.127380	483808.691494	46.596954
3504.109078	483805.705240	46.601959
3503.843413	483801.136832	46.606964
3503.998705	483798.275132	46.611969
3504.097312	483796.536999	46.616973
3504.017649	483772.028211	46.621978
3504.003674	483768.179977	46.626983
3503.691503	483755.006008	46.631988
3503.956961	483768.035426	46.636993
3503.505344	483764.357689	46.641997
3503.744783	483752.920444	46.647002
3503.779922	483754.992150	46.652007
3503.454040	483762.592641	46.657012
3503.942461	483753.446594	46.662017
3503.736293	483740.965160	46.667021
3504.102118	483722.110950	46.672026
3503.792294	483718.664115	46.677031
3504.026267	483714.878010	46.682036
3504.294478	483711.086493	46.687041
3503.981856	483718.836899	46.692045
3504.278245	483690.063439	46.697050
3504.187457	483667.228198	46.702055
3503.638970	483666.098972	46.707060
3503.895516	483671.124890	46.712065
3504.011876	483668.421317	46.717069
3504.356832	483640.704059	46.722074
3504.088431	483632.690862	46.727079
3503.883850	483619.702454	46.732084
3504.221081	483623.297026	46.737089
3503.834503	483613.427913	46.742093
3503.981056	483594.709564	46.747098
3504.171609	483585.863840	46.752103
3503.748409	483571.390015	46.757108
3503.812835	483580.955473	46.762113
3503.503031	483575.583354	46.767117
3504.092040	483571.538449	46.772122
3504.250701	483574.958596	46.777127
3503.787711	483548.027543	46.782132
3504.071930	483532.631245	46.787137
3503.908615	483545.677916	46.792141
3504.100777	483529.333537	46.797146
3503.897432	483515.736886	46.802151
3503.741689	483520.473354	46.807156
3504.152177	483518.077926	46.812161
3504.420669	483496.148329	46.817165
3503.998778	483494.239111	46.822170
3503.883409	483490.305517	46.827175
3503.625035	483475.957564	46.832180
3503.970214	483481.425508	46.837185
3504.223425	483457.978337	46.842189
3503.935212	483435.072696	46.847194
3504.067868	483438.040992	46.852199
3503.909670	483443.335181	46.857204
3504.202703	483433.561221	46.862209
3503.908204	483417.648320	46.867213
3504.186843	483405.647360	46.872218
3504.177590	483385.788139	46.877223
3503.909052	483381.777402	46.882228
3504.044784	483382.617285	46.887233
3503.778371	483374.755661	46.892237
3504.177964	483357.871701	46.897242
3504.254303	483341.798795	46.902247
3504.359733	483328.457202	46.907252
3504.061673	483338.181402	46.912257
3503.837101	483303.612540	46.917261
3504.287112	483312.813196	46.922266
3504.133681	483307.720279	46.927271
3504.129689	483308.987572	46.932276
3504.255382	483268.739437	46.937281
3503.696053	483272.019790	46.942285
3504.092945	483269.981139	46.947290
3503.851708	483253.705026	46.952295
3503.823443	483282.892803	46.957300
3503.876781	483249.799881	46.962305
3503.722887	483259.957324	46.967309
3503.985764	483241.473576	46.972314
3503.957685	483226.734381	46.977319
3503.888904	483212.305601	46.982324
3503.802571	483218.145814	46.987329
3503.631996	483223.847344	46.992333
3504.021208	483219.529952	46.997338
3503.524557	483225.891004	47.002343
3503.666824	483218.724707	47.007348
3503.870253	483209.978108	47.012353
3503.852556	483203.546406	47.017357
3504.143369	483170.567813	47.022362
3503.895074	483187.124087	47.027367
3503.991524	483167.146604	47.032372
3504.013877	483138.618301	47.037377
3503.960468	483178.703343	47.042381
3503.908848	483133.213723	47.047386
3503.545939	483141.884289	47.052391
3503.777983	483125.837261	47.057396
3503.895398	483120.904150	47.062401
3503.446812	483129.081606	47.067405
3504.046416	483115.307101	47.072410
3503.841468	483123.750046	47.077415
3503.632276	483136.094922	47.082420
3504.498629	483108.446494	47.087425
3504.108335	483109.268198	47.092429
3503.994811	483094.947734	47.097434
3503.932085	483090.955073	47.102439
3503.981374	483066.526342	47.107444
3503.663706	483078.128411	47.112449
3504.017536	483083.139107	47.117453
3503.743105	483057.697546	47.122458
3503.940447	483058.173045	47.127463
3503.996581	483037.289813	47.132468
3504.191588	483034.979050	47.137473
3504.050160	483037.636065	47.142477
3504.137145	483031.998417	47.147482
3503.869761	483007.265001	47.152487
3503.808447	482991.010896	47.157492
3504.049408	482998.775425	47.162497
3503.953078	482995.092052	47.167501
3503.886784	482982.588021	47.172506
3503.732794	482989.097656	47.177511
3503.861176	482989.685388	47.182516
3504.090269	482968.622747	47.187521
3504.066248	482953.426707	47.192525
3504.123414	482937.305831	47.197530
3504.174619	482939.071087	47.202535
3503.943860	482936.016945	47.207540
3504.008129	482912.294980	47.212545
3503.927578	482914.435727	47.217549
3503.942100	482904.097525	47.222554
3503.996155	482892.689075	47.227559
3503.908529	482886.572318	47.232564
3503.976576	482879.265627	47.237569
3503.880512	482877.710180	47.242573
3504.171260	482864.440312	47.247578
3503.837913	482850.458409	47.252583
3503.781965	482850.112616	47.257588
3504.084095	482846.163571	47.262593
3503.649638	482854.440241	47.267597
3503.716668	482845.512371	47.272602
3503.998415	482830.065241	47.277607
3503.822232	482831.613113	47.282612
3504.109348	482807.399800	47.287617
3503.924129	482809.354435	47.292621
3503.836055	482799.488392	47.297626
3503.987552	482800.477810	47.302631
3504.020724	482796.672598	47.307636
3504.235266	482780.577384	47.312641
3503.735568	482775.741722	47.317645
3503.865942	482771.414475	47.322650
3503.779038	482761.041561	47.327655
3503.424521	482760.793621	47.332660
3503.588729	482759.602362	47.337665
3503.579020	482767.001269	47.342669
3504.118680	482757.390657	47.347674
3503.953898	482766.334076	47.352679
3503.794037	482741.887327	47.357684
3503.953481	482725.142108	47.362689
3503.715453	482728.675769	47.367693
3503.827064	482712.292767	47.372698
3504.178474	482715.277266	47.377703
3503.933647	482719.622674	47.382708
3503.877572	482710.612864	47.387713
3504.049699	482706.279004	47.392717
3504.179932	482670.538264	47.397722
3503.879870	482679.503104	47.402727
3503.302682	482691.501090	47.407732
3503.758271	482676.431697	47.412737
3503.769199	482670.907300	47.417741
3503.953868	482667.179452	47.422746
3504.361831	482667.976340	47.427751
3503.947864	482638.249589	47.432756
3504.362939	482621.311876	47.437761
3504.492438	482624.635466	47.442765
3504.152744	482612.681080	47.447770
3503.969224	482600.043329	47.452775
3503.830505	482598.595935	47.457780
3504.070686	482578.443128	47.462785
3503.646549	482590.062315	47.467789
3504.287969	482581.246209	47.472794
3504.052534	482558.077853	47.477799
3504.071035	482542.976106	47.482804
3504.001691	482543.949774	47.487809
3503.816806	482546.664392	47.492813
3504.284954	482534.075602	47.497818
3504.216645	482515.136837	47.502823
3503.939751	482499.119063	47.507828
3504.003133	482498.247728	47.512833
3503.963713	482505.752765	47.517837
3504.055552	482507.308969	47.522842
3504.398154	482477.462394	47.527847
3504.098315	482458.256162	47.532852
3504.043767	482441.240515	47.537857
3503.749432	482452.281925	47.542861
3503.991138	482446.264981	47.547866
3503.961636	482435.578815	47.552871
3503.630351	482415.313491	47.557876
3503.830409	482402.817657	47.562881
3503.566448	482421.606435	47.567885
3503.760038	482414.482398	47.572890
3503.997150	482409.732860	47.577895
3503.611785	482411.313827	47.582900
3503.844758	482402.714199	47.587905
3503.949170	482408.625842	47.592909
3504.065574	482393.204499	47.597914
3504.210367	482381.578737	47.602919
3503.677747	482362.105195	47.607924
3503.978896	482352.684086	47.612929
3503.723194	482360.223363	47.617933
3503.904035	482360.397480	47.622938
3503.643451	482354.459896	47.627943
3503.530032	482357.061909	47.632948
3503.750745	482349.325548	47.637953
3503.516188	482356.456142	47.642957
3503.739618	482355.356833	47.647962
3503.808702	482346.479077	47.652967
3503.313180	482323.300882	47.657972
3503.523281	482324.686404	47.662977
3503.802851	482334.674484	47.667981
3503.765576	482312.994552	47.672986
3503.651807	482314.228593	47.677991
3503.794042	482305.845935	47.682996
3503.846208	482296.666823	47.688001
3503.859220	482314.550573	47.693005
3504.075609	482306.409535	47.698010
3504.103392	482296.220918	47.703015
3503.714018	482298.815886	47.708020
3503.986825	482267.814659	47.713025
3503.708671	482261.930491	47.718029
3503.695349	482256.460477	47.723034
3503.861608	482259.119635	47.728039
3503.636223	482261.840693	47.733044
3503.866170	482257.193586	47.738049
3503.715136	482263.652328	47.743053
3503.943625	482264.376265	47.748058
3503.693757	482266.239835	47.753063
3503.512623	482258.212275	47.758068
3504.037535	482247.539715	47.763073
3503.894655	482229.625819	47.768077
3503.870302	482212.402527	47.773082
3503.930736	482222.323963	47.778087
3503.549035	482216.456148	47.783092
3503.931058	482217.966510	47.788097
3503.779338	482226.097422	47.793101
3503.862216	482219.092148	47.798106
3504.092120	482206.287462	47.803111
3503.572826	482189.395718	47.808116
3503.871336	482178.910909	47.813121
3503.754755	482167.326330	47.818125
3503.890488	482165.632853	47.823130
3503.994421	482164.045738	47.828135
3503.914384	482171.101309	47.833140
3504.013034	482156.645282	47.838145
3503.850917	482154.593533	47.843149
3503.735654	482144.174103	47.848154
3504.098883	482132.412332	47.853159
3503.734998	482131.811185	47.858164
3504.151677	482112.440696	47.863169
3504.007272	482119.607795	47.868173
3503.942190	482117.287364	47.873178
3504.032493	482097.765770	47.878183
3503.824170	482089.185084	47.883188
3503.778793	482069.026216	47.888193
3503.721749	482081.094370	47.893197
3503.913229	482080.962799	47.898202
3504.033452	482073.039537	47.903207
3503.819270	482079.660326	47.908212
3504.029711	482074.205563	47.913217
3503.670920	482053.234850	47.918221
3503.882265	482043.878454	47.923226
3504.023866	482035.191769	47.928231
3503.964081	482029.273017	47.933236
3504.292726	482031.957209	47.938241
3503.992371	482032.511396	47.943245
3503.882088	481998.732847	47.948250
3503.779139	482002.549301	47.953255
3503.551129	481990.272866	47.958260
3503.825636	481982.629196	47.963265
3503.651563	481979.717949	47.968269
3503.762866	481992.266238	47.973274
3503.723843	481983.354734	47.978279
3503.803373	481986.483657	47.983284
3504.073171	481978.384710	47.988289
3503.612441	481972.073292	47.993293
3503.765290	481953.301700	47.998298
3503.866826	481942.695891	48.003303
3503.956673	481949.167333	48.008308
3504.038561	481948.090374	48.013313
3503.775449	481949.145365	48.018317
3503.906059	481941.929773	48.023322
3503.917465	481943.904085	48.028327
3503.627859	481933.866780	48.033332
3503.906151	481914.163285	48.038337
3504.000120	481905.534740	48.043341
3503.678742	481901.886728	48.048346
3503.740719	481904.410411	48.053351
3504.040847	481895.901284	48.058356
3504.060035	481898.735744	48.063361
3503.889249	481897.800055	48.068365
3503.915819	481881.227120	48.073370
3503.759714	481880.187772	48.078375
3503.589554	481871.347613	48.083380
3504.230006	481858.933833	48.088385
3504.075845	481869.497395	48.093389
3504.091245	481868.582947	48.098394
3503.893274	481842.418343	48.103399
3503.715527	481858.356566	48.108404
3503.897709	481813.485606	48.113409
3503.734016	481818.882442	48.118413
3503.747626	481801.703457	48.123418
3504.060774	481802.566039	48.128423
3503.801259	481815.882419	48.133428
3503.915313	481815.408399	48.138433
3503.846191	481810.352432	48.143437
3503.638941	481797.616572	48.148442
3503.790246	481787.509505	48.153447
3503.689110	481780.989182	48.158452
3503.732457	481772.520586	48.163457
3503.973123	481770.607813	48.168461
3504.219656	481764.235212	48.173466
3503.987594	481763.157193	48.178471
3503.736941	481765.578297	48.183476
3503.880835	481750.253440	48.188481
3503.737788	481732.592461	48.193485
3503.617267	481719.386817	48.198490
3503.884010	481710.224184	48.203495
3503.718287	481707.311576	48.208500
3503.782330	481715.560607	48.213505
3503.772588	481721.743849	48.218509
3504.079030	481712.524273	48.223514
3504.103679	481715.307226	48.228519
3503.865902	481717.827640	48.233524
3503.896741	481689.093194	48.238529
3503.743853	481696.464468	48.243533
3504.030688	481686.589275	48.248538
3504.063721	481689.320238	48.253543
3504.157493	481675.928686	48.258548
3504.166053	481666.401483	48.263553
3503.804308	481644.214726	48.268557
3504.088148	481640.775027	48.273562
3504.050952	481624.667979	48.278567
3503.735187	481639.716139	48.283572
3503.996681	481635.975953	48.288577
3503.986646	481633.748103	48.293581
3504.144200	481600.889256	48.298586
3503.966466	481601.626753	48.303591
3503.849925	481601.999890	48.308596
3503.782114	481587.367073	48.313601
3503.624824	481586.226557	48.318605
3503.613323	481579.894678	48.323610
3503.758903	481584.786669	48.328615
3503.670721	481585.205994	48.333620
3504.037589	481574.254030	48.338625
3503.752996	481561.682249	48.343629
3504.019887	481535.849121	48.348634
3503.853040	481537.800978	48.353639
3503.674280	481547.051183	48.358644
3503.877459	481536.783778	48.363649
3503.914894	481548.026610	48.368653
3503.898817	481542.303481	48.373658
3503.937333	481539.257228	48.378663
3503.478769	481520.176497	48.383668
3503.944629	481504.091180	48.388673
3503.733976	481505.999294	48.393677
3503.820907	481504.870843	48.398682
3504.209852	481495.891476	48.403687
3503.915160	481496.090092	48.408692
3504.075273	481497.939606	48.413697
3503.955521	481484.835022	48.418701
3504.001921	481460.354064	48.423706
3504.275327	481453.115723	48.428711
3503.789205	481453.648616	48.433716
3504.268307	481440.905383	48.438721
3503.939487	481429.556592	48.443725
3504.101435	481415.343364	48.448730
3504.085014	481400.651614	48.453735
3504.125224	481408.955211	48.458740
3504.236406	481386.896095	48.463745
3503.813356	481379.159759	48.468749
3503.857215	481357.263261	48.473754
3503.723841	481356.574985	48.478759
3503.507970	481367.655275	48.483764
3504.067358	481349.021531	48.488769
3503.781629	481356.515269	48.493773
3504.060261	481349.580085	48.498778
3504.404397	481340.810411	48.503783
3504.423135	481322.819468	48.508788
3504.371469	481314.720385	48.513793
3504.111354	481308.073019	48.518797
3503.752887	481280.919620	48.523802
3504.087399	481276.610449	48.528807
3504.067308	481276.968348	48.533812
3503.896685	481262.503549	48.538817
3503.864117	481263.420797	48.543821
3504.086500	481256.950507	48.548826
3503.886701	481240.514148	48.553831
3503.758434	481243.473350	48.558836
3504.108510	481222.541717	48.563841
3503.772906	481215.146189	48.568845
3503.927607	481218.871403	48.573850
3504.149469	481215.086731	48.578855
3503.981233	481201.432241	48.583860
3503.979889	481172.752795	48.588865
3504.064763	481175.374294	48.593869
3504.282338	481166.067166	48.598874
3504.087805	481163.159030	48.603879
3503.726215	481155.919600	48.608884
3504.041567	481136.361478	48.613889
3504.241531	481136.025877	48.618893
3503.954984	481142.861103	48.623898
3504.280812	481137.793210	48.628903
3503.893163	481116.268669	48.633908
3504.209830	481083.333135	48.638913
3504.452917	481101.789685	48.643917
3504.090120	481098.908134	48.648922
3504.097472	481057.052665	48.653927
3503.686083	481065.174429	48.658932
3504.206021	481049.384220	48.663937
3503.781072	481035.668846	48.668941
3503.679531	481053.166487	48.673946
3504.022772	481035.630703	48.678951
3503.904392	481038.791058	48.683956
3503.740429	481010.441104	48.688961
3503.987094	481003.865550	48.693965
3503.670439	481006.347849	48.698970
3504.017551	480993.067804	48.703975
3503.976317	480992.567637	48.708980
3504.437218	480975.773274	48.713985
3504.124781	480985.146215	48.718989
3503.924034	480965.720165	48.723994
3503.951130	480958.469900	48.728999
3503.798006	480949.119916	48.734004
3503.784727	480951.807630	48.739009
3503.847641	480969.988753	48.744013
3503.960761	480947.523465	48.749018
3504.114060	480929.966936	48.754023
3503.883779	480918.602273	48.759028
3504.065571	480899.622412	48.764033
3504.163862	480895.198479	48.769037
3503.778121	480908.738111	48.774042
3503.931399	480895.640651	48.779047
3503.950346	480886.820828	48.784052
3504.171488	480866.415910	48.789057
3504.203690	480864.079953	48.794061
3504.054746	480849.662095	48.799066
3503.979942	480831.077425	48.804071
3503.688070	480835.227996	48.809076
3504.130528	480822.338140	48.814081
3503.876959	480817.159053	48.819085
3503.832399	480819.801058	48.824090
3504.195524	480810.724116	48.829095
3503.851126	480815.389711	48.834100
3504.046407	480784.195701	48.839105
3503.931859	480778.386569	48.844109
3503.827988	480768.420652	48.849114
3504.000322	480754.914711	48.854119
3503.644005	480773.212948	48.859124
3504.081030	480766.657901	48.864129
3503.674758	480767.026173	48.869133
3503.694882	480750.098596	48.874138
3503.917227	480727.869153	48.879143
3503.896365	480730.659440	48.884148
3503.979998	480719.346390	48.889153
3503.809193	480722.869786	48.894157
3503.966966	480726.999984	48.899162
3504.098442	480722.266735	48.904167
3503.567846	480705.426162	48.909172
3504.347300	480673.430237	48.914177
3503.854515	480674.572268	48.919181
3503.773451	480671.798141	48.924186
3503.868799	480670.566968	48.929191
3503.639079	480667.208270	48.934196
3503.803735	480668.499751	48.939201
3503.475070	480673.365582	48.944205
3503.534394	480671.684053	48.949210
3503.923615	480670.507778	48.954215
3503.470225	480677.116174	48.959220
3503.682866	480674.650331	48.964225
3503.583676	480677.199645	48.969229
3503.772622	480670.785120	48.974234
3503.779831	480640.532706	48.979239
3503.851717	480636.264905	48.984244
3503.919001	480622.522115	48.989249
3503.854696	480629.778443	48.994253
3503.829369	480620.357431	48.999258
3504.049148	480611.505743	49.004263
3503.723719	480620.323516	49.009268
3503.834918	480617.214959	49.014273
3503.767376	480583.832590	49.019277
3503.787027	480591.024991	49.024282
3503.880224	480567.751660	49.029287
3503.745665	480585.305608	49.034292
3503.877435	480568.106866	49.039297
3503.519072	480577.487260	49.044301
3503.539101	480572.720917	49.049306
3503.586464	480575.247081	49.054311
3503.511335	480583.721274	49.059316
3503.579482	480577.528501	49.064321
3503.618631	480576.052842	49.069325
3503.671692	480574.372295	49.074330
3503.705822	480583.031910	49.079335
3503.503752	480568.774259	49.084340
3504.019911	480575.786846	49.089345
3503.621237	480577.927455	49.094349
3503.659609	480568.141644	49.099354
3504.022880	480563.270376	49.104359
3504.030378	480545.229823	49.109364
3503.699869	480539.606771	49.114369
3503.988938	480532.669651	49.119373
3503.645515	480530.798403	49.124378
3503.572989	480524.577174	49.129383
3503.740813	480531.188780	49.134388
3503.877866	480526.859983	49.139393
3503.777571	480533.615309	49.144397
3503.555253	480525.998925	49.149402
3503.987790	480512.958418	49.154407
3503.549600	480498.433999	49.159412
3503.613625	480487.731986	49.164417
3503.740339	480485.786427	49.169421
3503.812915	480474.779020	49.174426
3503.944943	480469.842933	49.179431
3503.882917	480486.929451	49.184436
3504.246146	480472.633055	49.189441
3503.921289	480476.788914	49.194445
3503.999824	480451.693548	49.199450
3504.116471	480425.781361	49.204455
3503.788004	480434.143641	49.209460
3504.040764	480427.820296	49.214465
3503.948790	480429.557737	49.219469
3503.799917	480429.581296	49.224474
3503.973582	480422.915741	49.229479
3503.692026	480414.599257	49.234484
3503.973439	480415.466919	49.239489
3503.855774	480403.628102	49.244493
3503.692527	480396.965115	49.249498
3504.128613	480412.706148	49.254503
3503.992979	480418.605661	49.259508
3503.890147	480403.268076	49.264513
3503.560542	480376.666262	49.269517
3503.760983	480365.486566	49.274522
3503.911088	480352.135881	49.279527
3503.554138	480368.863731	49.284532
3503.728209	480355.255895	49.289537
3503.823960	480352.149739	49.294541
3503.820236	480351.744973	49.299546
3503.729277	480357.637443	49.304551
3503.608096	480356.187109	49.309556
3503.929502	480345.799050	49.314561
3503.658380	480360.891806	49.319565
3503.584473	480347.272485	49.324570
3503.868118	480318.192036	49.329575
3503.605848	480314.179672	49.334580
3503.833541	480307.252173	49.339585
3503.941445	480309.768802	49.344589
3503.682191	480313.204904	49.349594
3503.929962	480302.423076	49.354599
3503.920778	480300.803017	49.359604
3504.056107	480302.251177	49.364609
3503.685499	480277.682635	49.369613
3503.259290	480275.368388	49.374618
3503.749676	480284.108042	49.379623
3503.611511	480281.190865	49.384628
3504.053626	480259.331544	49.389633
3503.942798	480258.639664	49.394637
3503.442719	480258.820079	49.399642
3504.104403	480254.712342	49.404647
3503.857252	480264.480692	49.409652
3503.744996	480254.566512	49.414657
3503.514353	480257.035310	49.419661
3503.527981	480257.539918	49.424666
3503.985347	480250.525426	49.429671
3503.660815	480265.576022	49.434676
3503.628116	480245.818660	49.439681
3503.998714	480245.658768	49.444685
3503.800601	480232.363039	49.449690
3503.991522	480220.424665	49.454695
3503.786530	480224.510959	49.459700
3503.776878	480205.256646	49.464705
3503.409325	480219.705997	49.469709
3503.417848	480214.029266	49.474714
3503.889801	480217.805875	49.479719
3503.595326	480219.575340	49.484724
3503.616420	480219.521362	49.489729
3503.674507	480219.714904	49.494733
3503.673752	480205.323823	49.499738
3503.748430	480197.457677	49.504743
3503.614225	480211.312745	49.509748
3503.697230	480193.361283	49.514753
3503.805641	480170.439791	49.519757
3503.617861	480163.628583	49.524762
3503.824326	480156.603040	49.529767
3503.608271	480168.596156	49.534772
3503.647122	480163.776066	49.539777
3503.750331	480168.979149	49.544781
3503.680136	480169.344986	49.549786
3503.759066	480169.585908	49.554791
3503.526123	480166.683694	49.559796
3503.463982	480162.436973	49.564801
3503.662303	480167.118289	49.569805
3503.583265	480159.377770	49.574810
3503.720241	480166.551782	49.579815
3503.678287	480167.774605	49.584820
3503.771702	480161.881748	49.589825
3503.879119	480167.033493	49.594829
3503.826461	480149.052759	49.599834
3503.915814	480129.073294	49.604839
3503.655144	480128.962503	49.609844
3503.976790	480128.962368	49.614849
3503.734100	480119.322103	49.619853
3503.685433	480119.329824	49.624858
3503.890622	480120.564262	49.629863
3503.405404	480123.529375	49.634868
3503.345268	480118.775593	49.639873
3504.061727	480118.966425	49.644877
3503.722275	480122.465909	49.649882
3503.766535	480120.837388	49.654887
3503.817783	480111.150662	49.659892
3504.028634	480093.685638	49.664897
3503.704411	480081.068496	49.669901
3503.502030	480079.935017	49.674906
3503.760645	480080.552929	49.679911
3503.827801	480080.288976	49.684916
3504.086323	480074.724713	49.689921
3504.123051	480072.489294	49.694925
3503.936539	480066.285935	49.699930
3504.040403	480048.989803	49.704935
3503.517149	480041.268773	49.709940
3503.957568	480028.936134	49.714945
3504.007628	480021.681894	49.719949
3503.794578	480034.181355	49.724954
3504.011384	480024.772462	49.729959
3503.554621	480031.432280	49.734964
3503.921969	480022.911721	49.739969
3503.964864	479997.416018	49.744973
3503.997335	479993.407676	49.749978
3504.010493	479978.811536	49.754983
3503.993643	479978.054119	49.759988
3504.139677	479979.095220	49.764993
3503.931267	479976.341122	49.769997
3503.948306	479954.599322	49.775002
3503.936940	479928.453343	49.780007
3503.914867	479940.669309	49.785012
3504.070903	479943.634444	49.790017
3503.909925	479939.859363	49.795021
3504.059721	479935.832467	49.800026
3503.902992	479907.277081	49.805031
3503.568714	479895.978936	49.810036
3503.915081	479892.681074	49.815041
3504.003309	479897.177159	49.820045
3503.759195	479891.590939	49.825050
3504.216714	479881.181123	49.830055
3504.064199	479882.928180	49.835060
3504.184558	479871.000748	49.840065
3504.128086	479860.064068	49.845069
3504.146236	479846.125806	49.850074
3504.323427	479837.280502	49.855079
3503.903941	479824.779600	49.860084
3504.016935	479813.258692	49.865089
3504.148040	479793.272288	49.870093
3503.691935	479811.587189	49.875098
3504.031580	479798.864939	49.880103
3503.995189	479798.617347	49.885108
3503.577916	479777.704112	49.890113
3503.854564	479765.549217	49.895117
3503.507139	479758.357704	49.900122
3503.579547	479748.870153	49.905127
3503.841302	479768.135799	49.910132
3504.019993	479762.077321	49.915137
3503.737455	479750.821589	49.920141
3503.511248	479760.485529	49.925146
3503.744164	479757.661648	49.930151
3504.072099	479765.211021	49.935156
3503.747005	479756.445068	49.940161
3503.854643	479756.833481	49.945165
3503.868482	479728.554924	49.950170
3503.809336	479719.138826	49.955175
3503.772259	479720.563605	49.960180
3503.540948	479722.779201	49.965185
3503.951758	479724.943983	49.970189
3503.416045	479719.657175	49.975194
3503.758645	479706.883724	49.980199
3503.640351	479708.017292	49.985204
3504.204198	479705.394472	49.990209
3503.802006	479721.724623	49.995213
3503.860932	479698.506356	50.000218
3503.763950	479679.366682	50.005223
3503.664053	479689.314741	50.010228
3503.719932	479674.508924	50.015233
3503.999109	479672.437839	50.020237
3503.640582	479679.538321	50.025242
3503.988458	479687.236597	50.030247
3503.610663	479688.107132	50.035252
3503.773396	479673.335101	50.040257
3503.854473	479681.075547	50.045261
3503.631211	479665.401698	50.050266
3503.710767	479638.126120	50.055271
3503.295198	479636.772936	50.060276
3503.471076	479637.505289	50.065281
3503.453657	479655.953697	50.070285
3503.723318	479667.667649	50.075290
3503.672812	479652.118509	50.080295
3503.860722	479646.007864	50.085300
3503.852246	479636.989116	50.090305
3503.835438	479627.312909	50.095309
3503.532129	479629.185171	50.100314
3504.087232	479618.303720	50.105319
3503.987254	479625.211332	50.110324
3503.875397	479636.833578	50.115329
3503.978761	479617.763528	50.120333
3503.599232	479597.857634	50.125338
3504.055498	479587.447863	50.130343
3503.805433	479588.348889	50.135348
3504.033657	479584.410876	50.140353
3504.146959	479581.909924	50.145357
3503.602363	479573.634658	50.150362
3504.051743	479568.597512	50.155367
3503.630240	479571.806010	50.160372
3503.697924	479541.643701	50.165377
3503.846083	479537.566307	50.170381
3503.690006	479526.999911	50.175386
3503.684141	479531.105550	50.180391
3503.532497	479547.345570	50.185396
3503.810979	479538.737499	50.190401
3503.917165	479519.818933	50.195405
3503.897072	479522.710620	50.200410
3503.933310	479526.910956	50.205415
3503.643260	479530.200034	50.210420
3503.976963	479495.485525	50.215425
3504.112188	479481.275125	50.220429
3503.900739	479479.332240	50.225434
3503.852492	479495.150559	50.230439
3503.866688	479494.793618	50.235444
3503.970050	479478.257193	50.240449
3504.093590	479458.981100	50.245453
3503.512369	479468.245216	50.250458
3503.912419	479439.905204	50.255463
3503.574747	479434.384317	50.260468
3503.649020	479430.926683	50.265473
3503.849325	479438.293653	50.270477
3503.533037	479444.019309	50.275482
3503.877652	479437.681130	50.280487
3503.528360	479445.337664	50.285492
3503.724476	479432.485839	50.290497
3503.930162	479455.105225	50.295501
3503.728706	479446.877021	50.300506
3504.138062	479432.268531	50.305511
3503.845794	479414.882428	50.310516
3503.780863	479394.622553	50.315521
3503.838494	479417.012006	50.320525
3503.618008	479381.320704	50.325530
3503.982915	479410.654814	50.330535
3503.770275	479396.600685	50.335540
3503.842457	479378.599517	50.340545
3504.016219	479409.737480	50.345549
3503.641594	479362.161783	50.350554
3503.901140	479366.428209	50.355559
3503.075639	479354.903339	50.360564
3503.698677	479346.088700	50.365569
3503.713059	479361.897226	50.370573
3503.709751	479328.603929	50.375578
3503.987196	479338.644551	50.380583
3503.465292	479354.183117	50.385588
3503.770182	479340.351204	50.390593
3503.983814	479349.033666	50.395597
3503.238038	479360.300187	50.400602
3503.855597	479353.462762	50.405607
3503.803275	479333.707587	50.410612
3503.667665	479349.691857	50.415617
3504.062094	479349.477519	50.420621
3504.053753	479321.911343	50.425626
3504.033781	479301.846970	50.430631
3503.574062	479309.825064	50.435636
3503.414777	479300.323242	50.440641
3503.589914	479290.160450	50.445645
3503.593158	479304.501188	50.450650
3503.995809	479298.153792	50.455655
3503.933609	479304.751491	50.460660
3503.596276	479293.656185	50.465665
3503.682679	479302.814858	50.470669
3503.612997	479291.018464	50.475674
3503.631395	479298.211534	50.480679
3503.162420	479311.360010	50.485684
3503.683205	479296.176376	50.490689
3503.807082	479289.670336	50.495693
3503.333589	479293.849934	50.500698
3503.683186	479299.571738	50.505703
3503.883103	479276.533394	50.510708
3503.682970	479264.402872	50.515713
3503.782177	479243.407439	50.520717
3503.809723	479255.717337	50.525722
3504.010261	479246.918756	50.530727
3503.563582	479240.198822	50.535732
3503.441689	479215.792348	50.540737
3503.549853	479171.737874	50.545741
3503.173744	479140.327519	50.550746
3503.422521	479087.534343	50.555751
3503.272851	479031.205981	50.560756
3503.418033	478960.793455	50.565761
3503.324096	478867.461899	50.570765
3503.073663	478783.529886	50.575770
3503.139747	478681.151652	50.580775
3502.608848	478572.431196	50.585780
3502.377794	478450.283803	50.590785
3502.465314	478323.017489	50.595789
3501.975700	478184.641624	50.600794
3501.886911	478041.133554	50.605799
3502.029572	477885.982312	50.610804
3501.595448	477709.078067	50.615809
3501.004039	477582.623841	50.620813
3500.740066	477388.914750	50.625818
3500.863848	477211.765871	50.630823
3500.335557	477053.571979	50.635828
3499.960447	476829.010021	50.640833
3499.970760	476628.965647	50.645837
3499.441697	476418.817243	50.650842
3499.167238	476204.318294	50.655847
3498.715137	475993.950541	50.660852
3498.392690	475761.715012	50.665857
3498.023649	475533.032134	50.670861
3497.603145	475301.364331	50.675866
3497.524268	475048.604998	50.680871
3497.049371	474809.539922	50.685876
3496.468669	474554.319370	50.690881
3496.225712	474297.166749	50.695885
3495.635709	474035.807844	50.700890
3495.268785	473760.926862	50.705895
3494.965802	473490.999714	50.710900
3494.904071	473217.330410	50.715905
3494.349717	472933.596949	50.720909
3493.588713	472649.892208	50.725914
3493.411002	472345.763372	50.730919
3492.772052	472060.561065	50.735924
3492.470516	471749.244412	50.740929
3491.753321	471442.196463	50.745933
3491.202161	471143.533253	50.750938
3490.691932	470823.972111	50.755943
3490.196412	470523.871618	50.760948
3489.793127	470197.236897	50.765953
3489.442801	469869.422570	50.770957
3488.838899	469550.769159	50.775962
3488.300392	469222.213857	50.780967
3487.508692	468893.389179	50.785972
3486.742426	468558.927320	50.790977
3486.281107	468229.178012	50.795981
3485.661417	467895.899255	50.800986
3485.131710	467547.085273	50.805991
3484.611921	467215.503884	50.810996
3483.908997	466871.117461	50.816001
3483.528573	466524.443309	50.821005
3482.896145	466181.403582	50.826010
3482.354096	465836.772025	50.831015
3481.847648	465485.638374	50.836020
3481.188579	465131.125421	50.841025
3480.582732	464777.561667	50.846029
3480.084289	464425.699293	50.851034
3479.708459	464054.388560	50.856039
3478.644623	463694.692247	50.861044
3478.551622	463326.164177	50.866049
3477.868318	462955.288730	50.871053
3477.219469	462595.457697	50.876058
3476.458312	462223.669060	50.881063
3475.658887	461867.501360	50.886068
3475.297440	461483.920865	50.891073
3474.686867	461101.539534	50.896077
3473.900799	460733.381127	50.901082
3473.485374	460342.434470	50.906087
3472.719600	459980.854009	50.911092
3471.817659	459611.224030	50.916097
3471.162804	459239.063257	50.921101
3470.342165	458867.683266	50.926106
3469.716218	458483.990474	50.931111
3468.889248	458117.164198	50.936116
3468.320071	457750.544723	50.941121
3467.998597	457376.017058	50.946125
3466.707489	456994.432730	50.951130
3466.720591	456628.970931	50.956135
3465.680384	456255.197501	50.961140
3464.891928	455878.131156	50.966145
3464.360614	455487.066207	50.971149
3463.659057	455128.846229	50.976154
3462.889097	454759.824853	50.981159
3462.326048	454382.088934	50.986164
3461.564515	454016.757762	50.991169
3461.292797	453626.329783	50.996173
3460.262996	453254.585082	51.001178
3459.705598	452881.592624	51.006183
3459.112372	452505.352371	51.011188
3458.285321	452127.417694	51.016193
3457.508501	451747.997325	51.021197
3456.962729	451372.593536	51.026202
3456.543214	451001.273847	51.031207
3455.550314	450624.913666	51.036212
3454.809658	450246.376186	51.041217
3454.248500	449869.022027	51.046221
3453.197934	449496.610745	51.051226
3452.960639	449116.046858	51.056231
3452.081452	448752.071345	51.061236
3451.597627	448371.382020	51.066241
3451.301723	447991.113535	51.071245
3450.069087	447620.223551	51.076250
3449.243724	447243.020909	51.081255
3448.698155	446868.660860	51.086260
3447.981769	446490.109375	51.091265
3447.520615	446115.571778	51.096269
3446.752559	445740.721492	51.101274
3446.216350	445368.011115	51.106279
3445.246574	444998.510319	51.111284
3444.771589	444620.296897	51.116289
3444.091185	444233.430385	51.121293
3443.207629	443875.572874	51.126298
3442.718180	443497.800837	51.131303
3441.678249	443122.749416	51.136308
3440.726574	442744.226465	51.141313
3440.155021	442383.404083	51.146317
3439.588084	442021.915684	51.151322
3439.026957	441649.100791	51.156327
3437.997609	441291.583392	51.161332
3437.229973	440921.277434	51.166337
3436.980795	440549.970125	51.171341
3435.796420	440192.207317	51.176346
3435.559154	439821.191686	51.181351
3434.831203	439467.915206	51.186356
3433.938345	439099.632266	51.191361
3433.206369	438729.084557	51.196365
3432.291091	438377.725948	51.201370
3432.003228	438022.709230	51.206375
3430.968074	437661.459157	51.211380
3430.215414	437307.749625	51.216385
3429.727705	436933.785594	51.221389
3428.845848	436592.525730	51.226394
3428.096543	436229.965837	51.231399
3427.554533	435874.451066	51.236404
3426.831704	435522.361843	51.241409
3426.141665	435163.585426	51.246413
3425.221438	434822.358439	51.251418
3424.840839	434463.777084	51.256423
3423.826310	434107.423594	51.261428
3423.089617	433770.698165	51.266433
3422.448056	433417.525950	51.271437
3422.010236	433066.652564	51.276442
3421.036392	432720.759522	51.281447
3420.288659	432375.511638	51.286452
3419.572274	432037.135227	51.291457
3418.925958	431692.471564	51.296461
3418.377776	431342.607827	51.301466
3417.899038	430988.030808	51.306471
3416.849007	430653.345581	51.311476
3415.858126	430309.327466	51.316481
3415.404766	429970.679412	51.321485
3414.740192	429631.603285	51.326490
3414.072530	429283.940088	51.331495
3413.283463	428945.154117	51.336500
3412.730936	428601.298250	51.341505
3412.250286	428275.583967	51.346509
3411.230274	427930.269585	51.351514
3410.701777	427587.945875	51.356519
3409.683280	427256.793265	51.361524
3408.955563	426922.441429	51.366529
3408.393396	426580.592635	51.371533
3407.568695	426256.685812	51.376538
3406.950707	425915.370695	51.381543
3406.077121	425584.022100	51.386548
3405.499328	425260.191227	51.391553
3404.469393	424933.176992	51.396557
3403.477830	424606.813099	51.401562
3403.035197	424279.825120	51.406567
3402.397443	423978.618708	51.411572
3401.694576	423659.157136	51.416577
3401.303481	423323.615354	51.421581
3400.420196	423005.774850	51.426586
3399.843934	422680.312847	51.431591
3399.206835	422356.660049	51.436596
3398.099145	422036.329160	51.441601
3397.523769	421712.074821	51.446605
3396.618363	421407.580374	51.451610
3396.389588	421089.665110	51.456615
3395.838410	420769.841230	51.461620
3394.860510	420450.716202	51.466625
3394.713489	420122.692265	51.471629
3393.765184	419804.876118	51.476634
3392.929224	419478.630156	51.481639
3392.373442	419158.864800	51.486644
3391.659775	418845.141468	51.491649
3391.073722	418530.810180	51.496653
3390.098800	418203.453658	51.501658
3389.779165	417893.696766	51.506663
3389.101309	417571.875006	51.511668
3387.955975	417261.987738	51.516673
3387.454882	416942.188743	51.521677
3386.596555	416622.112381	51.526682
3385.790004	416317.750582	51.531687
3385.017362	415999.305119	51.536692
3384.193298	415698.750484	51.541697
3383.885617	415379.767348	51.546701
3382.901427	415087.412671	51.551706
3382.415216	414771.017176	51.556711
3381.486549	414469.119730	51.561716
3380.548359	414174.080790	51.566721
3380.190726	413863.194023	51.571725
3379.078005	413565.966028	51.576730
3378.529570	413257.948747	51.581735
3378.123928	412959.789738	51.586740
3377.329639	412659.072014	51.591745
3376.768570	412367.055202	51.596749
3375.941651	412070.300518	51.601754
3375.420027	411765.287174	51.606759
3374.784162	411470.986465	51.611764
3373.834026	411180.874443	51.616769
3373.451303	410870.773293	51.621773
3372.447326	410582.646010	51.626778
3371.661066	410283.732586	51.631783
3370.792277	409983.507841	51.636788
3370.240988	409696.952229	51.641793
3369.856254	409401.295491	51.646797
3368.739362	409106.132812	51.651802
3368.338453	408807.194654	51.656807
3367.449778	408518.190809	51.661812
3366.419670	408233.730087	51.666817
3366.555138	407951.674558	51.671821
3365.248997	407650.784307	51.676826
3364.625318	407375.400166	51.681831
3363.860478	407089.616182	51.686836
3363.104085	406808.733133	51.691841
3362.745947	406516.424336	51.696845
3361.922619	406246.627417	51.701850
3361.590838	405947.243821	51.706855
3360.705061	405666.574180	51.711860
3359.797873	405377.924990	51.716865
3359.119476	405095.158769	51.721869
3358.443642	404819.887230	51.726874
3357.879784	404532.904216	51.731879
3357.368988	404250.815517	51.736884
3356.673602	403972.337194	51.741889
3356.019022	403685.106626	51.746893
3355.178615	403407.154579	51.751898
3354.406368	403112.490267	51.756903
3354.073643	402846.805751	51.761908
3352.875655	402562.955192	51.766913
3352.209721	402270.223418	51.771917
3351.385773	402012.234957	51.776922
3351.107436	401721.648239	51.781927
3350.257504	401461.981854	51.786932
3349.333627	401180.439605	51.791937
3349.163879	400895.267842	51.796941
3348.161529	400629.670831	51.801946
3347.676699	400346.857193	51.806951
3346.867298	400074.463581	51.811956
3346.213952	399797.467458	51.816961
3345.679535	399519.052075	51.821965
3344.658919	399260.335573	51.826970
3344.119711	398973.400546	51.831975
3343.564662	398703.522737	51.836980
3342.797812	398436.192864	51.841985
3342.187616	398150.710868	51.846989
3341.006350	397899.838732	51.851994
3340.659014	397617.844117	51.856999
3340.064654	397346.919159	51.862004
3339.521415	397088.872781	51.867009
3338.925731	396809.859516	51.872013
3338.091447	396555.693766	51.877018
3337.304357	396271.087954	51.882023
3336.541811	396006.152989	51.887028
3335.489278	395739.710997	51.892033
3335.003785	395463.058851	51.897037
3334.437033	395205.942358	51.902042
3334.022706	394946.537120	51.907047
3333.389076	394680.223921	51.912052
3332.611937	394408.388928	51.917057
3332.002635	394141.864277	51.922061
3331.127412	393871.489686	51.927066
3330.485775	393603.440495	51.932071
3329.834510	393342.407935	51.937076
3328.992581	393083.513806	51.942081
3328.823544	392816.934663	51.947085
3327.534675	392561.310844	51.952090
3326.958532	392298.910970	51.957095
3326.356467	392031.580642	51.962100
3325.700356	391769.087708	51.967105
3325.151941	391499.431060	51.972109
3324.309727	391244.184589	51.977114
3323.595653	390985.534285	51.982119
3323.273357	390727.608342	51.987124
3322.124280	390461.750973	51.992129
3321.640988	390197.032232	51.997133
3320.609851	389948.290097	52.002138
3320.523438	389687.293420	52.007143
3319.487151	389425.529644	52.012148
3318.812732	389168.741398	52.017153
3318.140915	388905.492211	52.022157
3317.123403	388653.840088	52.027162
3316.622070	388396.917209	52.032167
3315.895492	388145.927501	52.037172
3315.352253	387895.669906	52.042177
3314.983112	387638.669849	52.047181
3314.127992	387383.524843	52.052186
3313.291896	387122.933197	52.057191
3312.771111	386870.884922	52.062196
3311.899806	386608.082803	52.067201
3311.527508	386364.729856	52.072205
3310.619699	386109.889404	52.077210
3310.082522	385858.701346	52.082215
3309.374213	385603.469804	52.087220
3308.340252	385349.712092	52.092225
3307.582635	385094.688265	52.097229
3307.226576	384853.280894	52.102234
3306.378971	384605.159644	52.107239
3305.725216	384353.191423	52.112244
3305.042719	384113.204142	52.117249
3304.496629	383858.519842	52.122253
3303.704249	383618.953664	52.127258
3302.955507	383357.482349	52.132263
3302.486830	383113.080585	52.137268
3301.382620	382874.296496	52.142273
3300.738610	382614.558269	52.147277
3299.796473	382394.819677	52.152282
3299.382986	382142.595168	52.157287
3298.940257	381913.212173	52.162292
3298.080627	381665.098852	52.167297
3297.742584	381418.554576	52.172301
3296.728357	381179.898202	52.177306
3296.094426	380948.504998	52.182311
3295.615637	380701.164501	52.187316
3294.506947	380460.433050	52.192321
3294.080168	380220.177231	52.197325
3293.396956	379985.810287	52.202330
3292.536477	379741.576088	52.207335
3291.875595	379515.697771	52.212340
3291.034799	379279.545657	52.217345
3290.599459	379038.393681	52.222349
3289.902826	378806.717831	52.227354
3289.475842	378569.961860	52.232359
3289.100668	378331.110595	52.237364
3288.158299	378092.932596	52.242369
3287.374044	377851.345251	52.247373
3286.721998	377619.706241	52.252378
3286.034741	377378.914612	52.257383
3285.260315	377146.452820	52.262388
3284.819050	376918.108476	52.267393
3284.333043	376672.320740	52.272397
3283.375768	376430.904757	52.277402
3282.763653	376197.521510	52.282407
3282.076045	375956.670502	52.287412
3281.147062	375729.871854	52.292417
3280.588351	375497.671636	52.297421
3279.943098	375264.644354	52.302426
3279.111266	375017.578503	52.307431
3278.604234	374784.119612	52.312436
3277.595951	374558.191830	52.317441
3277.257126	374320.531947	52.322445
3276.276254	374102.966281	52.327450
3275.772879	373861.463232	52.332455
3274.825133	373639.183868	52.337460
3273.933915	373414.604934	52.342465
3273.569270	373187.677492	52.347469
3272.773802	372964.505518	52.352474
3272.347703	372727.791491	52.357479
3271.777588	372508.524407	52.362484
3271.056985	372280.529015	52.367489
3270.587375	372054.197095	52.372493
3269.765820	371826.393271	52.377498
3269.225222	371590.835686	52.382503
3268.773774	371357.832062	52.387508
3268.162250	371131.263234	52.392513
3267.359222	370899.406592	52.397517
3266.531155	370666.356974	52.402522
3265.821676	370418.404954	52.407527
3265.226130	370197.323651	52.412532
3264.332592	369968.172907	52.417537
3263.916843	369731.618548	52.422541
3262.950276	369513.390840	52.427546
3262.425842	369291.276005	52.432551
3261.927370	369060.760474	52.437556
3260.702195	368832.902742	52.442561
3260.047453	368607.497693	52.447565
3259.332487	368384.339824	52.452570
3258.995192	368169.720232	52.457575
3258.458100	367944.089617	52.462580
3257.293561	367724.154219	52.467585
3257.086559	367489.513636	52.472589
3256.102051	367279.622440	52.477594
3255.308804	367045.708264	52.482599
3254.769060	366828.544514	52.487604
3254.187402	366625.023334	52.492609
3253.210592	366397.826064	52.497613
3252.422709	366179.171851	52.502618
3251.924282	365961.921011	52.507623
3251.419792	365741.235315	52.512628
3250.672751	365526.998482	52.517633
3250.233536	365312.203082	52.522637
3249.336369	365089.998841	52.527642
3248.927314	364868.021621	52.532647
3247.938771	364647.941445	52.537652
3247.428407	364433.661997	52.542657
3246.936789	364207.394673	52.547661
3246.170279	363991.143621	52.552666
3245.709048	363771.866340	52.557671
3244.679378	363547.869024	52.562676
3243.765750	363338.050026	52.567681
3243.219527	363118.172416	52.572685
3242.756941	362909.806778	52.577690
3242.139461	362681.134651	52.582695
3241.210373	362461.950595	52.587700
3240.656692	362247.082603	52.592705
3240.099972	362037.455716	52.597709
3238.730320	361836.353272	52.602714
3238.165901	361609.372306	52.607719
3237.816777	361400.803873	52.612724
3236.896817	361183.622554	52.617729
3236.559264	360978.358299	52.622733
3235.784076	360777.259087	52.627738
3235.139385	360554.535136	52.632743
3234.399045	360351.774655	52.637748
3233.588205	360142.866593	52.642753
3233.025430	359920.381184	52.647757
3232.178882	359716.362516	52.652762
3231.724990	359507.522456	52.657767
3231.133824	359299.670161	52.662772
3230.410917	359098.937328	52.667777
3229.706710	358879.344917	52.672781
3229.199722	358674.606534	52.677786
3228.471582	358467.306716	52.682791
3227.873227	358258.382344	52.687796
3227.315018	358042.910890	52.692801
3226.629743	357827.484036	52.697805
3225.810139	357627.523856	52.702810
3224.947054	357408.255340	52.707815
3224.695152	357193.189767	52.712820
3223.801870	356992.551596	52.717825
3223.463244	356780.780668	52.722829
3222.437941	356570.669761	52.727834
3221.827375	356356.318943	52.732839
3221.511370	356141.208074	52.737844
3220.547495	355939.024521	52.742849
3220.160605	355725.933475	52.747853
3218.815387	355523.503200	52.752858
3218.315894	355309.384835	52.757863
3217.781048	355098.350410	52.762868
3216.919147	354898.207883	52.767873
3216.603533	354688.842129	52.772877
3215.766935	354473.093969	52.777882
3214.938425	354266.556074	52.782887
3214.177264	354072.832922	52.787892
3213.535567	353864.075260	52.792897
3213.360803	353664.073717	52.797901
3212.343960	353460.845317	52.802906
3211.653345	353242.294960	52.807911
3211.111427	353043.290728	52.812916
3210.004198	352841.372126	52.817921
3209.519190	352626.196894	52.822925
3209.071994	352431.349081	52.827930
3208.420049	352226.174884	52.832935
3207.643312	352013.842770	52.837940
3206.993213	351823.554885	52.842945
3206.801204	351606.165900	52.847949
3205.768558	351401.099630	52.852954
3204.835817	351201.793975	52.857959
3204.321240	350988.550989	52.862964
3203.476741	350792.487497	52.867969
3203.130618	350588.403884	52.872973
3202.252290	350389.977376	52.877978
3201.445691	350175.632087	52.882983
3200.925325	349985.698918	52.887988
3199.784279	349796.677700	52.892993
3199.643823	349581.970183	52.897997
3198.915865	349394.256579	52.903002
3198.238591	349190.958186	52.908007
3197.710302	348990.969590	52.913012
3196.765997	348799.190519	52.918017
3196.169273	348588.699872	52.923021
3195.462439	348399.299738	52.928026
3194.879286	348188.449104	52.933031
3194.357861	347991.968143	52.938036
3193.527689	347801.440158	52.943041
3193.100934	347591.504246	52.948045
3191.979229	347396.006971	52.953050
3191.475536	347201.073007	52.958055
3190.846248	347005.267411	52.963060
3189.727168	346800.146729	52.968065
3189.318034	346596.974638	52.973069
3188.561369	346405.539479	52.978074
3188.176045	346214.248555	52.983079
3187.492369	346028.323788	52.988084
3186.686486	345838.294412	52.993089
3186.408140	345624.357134	52.998093
3185.465780	345430.402818	53.003098
3184.510737	345236.118970	53.008103
3183.902173	345044.935839	53.013108
3183.390010	344853.431392	53.018113
3183.020905	344649.584322	53.023117
3182.147369	344458.644814	53.028122
3181.613610	344264.545618	53.033127
3180.615751	344068.941085	53.038132
3179.930564	343876.544497	53.043137
3179.349756	343671.734841	53.048141
3178.520886	343490.126624	53.053146
3177.698990	343301.746034	53.058151
3177.233069	343103.941502	53.063156
3176.466652	342926.776122	53.068161
3175.992778	342728.411621	53.073165
3175.298255	342540.110303	53.078170
3174.701880	342345.047503	53.083175
3174.105224	342156.093151	53.088180
3173.423669	341962.671672	53.093185
3172.872704	341765.690748	53.098189
3172.048152	341580.767014	53.103194
3171.118148	341389.088475	53.108199
3170.661946	341195.527099	53.113204
3169.867584	341000.211322	53.118209
3169.233036	340804.996920	53.123213
3168.209816	340628.425493	53.128218
3168.017149	340446.249342	53.133223
3167.359036	340247.015022	53.138228
3166.228399	340063.535204	53.143233
3165.964532	339873.808465	53.148237
3165.422035	339688.656279	53.153242
3164.753143	339498.839754	53.158247
3164.186784	339305.697227	53.163252
3163.407304	339114.395172	53.168257
3162.808544	338926.831382	53.173261
3161.817778	338741.543704	53.178266
3161.455994	338546.915536	53.183271
3160.788270	338355.364425	53.188276
3159.617679	338171.961827	53.193281
3159.311746	337977.246732	53.198285
3158.605600	337788.423808	53.203290
3158.088612	337605.679883	53.208295
3157.353466	337413.500247	53.213300
3156.599126	337226.439797	53.218305
3156.119842	337042.720993	53.223309
3155.175526	336855.893192	53.228314
3154.718343	336664.558362	53.233319
3154.093011	336476.329827	53.238324
3153.059536	336300.359063	53.243329
3152.611975	336105.813561	53.248333
3151.737201	335927.194662	53.253338
3150.972263	335739.851663	53.258343
3150.692648	335541.255765	53.263348
3149.731578	335365.372915	53.268353
3149.369241	335177.328230	53.273357
3148.517877	334995.444649	53.278362
3148.022687	334810.653023	53.283367
3147.453668	334624.828829	53.288372
3146.516133	334441.709997	53.293377
3145.940023	334254.027532	53.298381
3145.428465	334071.349466	53.303386
3144.631035	333878.431294	53.308391
3143.754337	333687.052584	53.313396
3143.260883	333502.817239	53.318401
3142.778035	333319.547123	53.323405
3142.230828	333139.188902	53.328410
3141.316342	332960.313967	53.333415
3140.940125	332763.074603	53.338420
3139.949070	332578.508230	53.343425
3139.258589	332387.580213	53.348429
3138.514848	332204.195725	53.353434
3137.993668	332022.277589	53.358439
3137.028562	331832.486238	53.363444
3136.113542	331658.266976	53.368449
3135.818629	331479.137540	53.373453
3134.841872	331300.090080	53.378458
3134.321716	331119.798842	53.383463
3134.135515	330931.103895	53.388468
3133.045063	330763.529475	53.393473
3132.586722	330575.360381	53.398477
3131.865787	330395.328249	53.403482
3131.020443	330212.718557	53.408487
3130.438935	330029.557492	53.413492
3129.418075	329863.166579	53.418497
3129.139252	329676.086985	53.423501
3128.465404	329499.787706	53.428506
3127.795868	329318.853761	53.433511
3127.325000	329133.305286	53.438516
3126.309809	328962.150597	53.443521
3126.054272	328780.793426	53.448525
3125.769989	328598.218318	53.453530
3124.823853	328406.327487	53.458535
3124.282909	328225.446961	53.463540
3123.143354	328038.448580	53.468545
3122.543357	327850.575125	53.473549
3121.795155	327672.857629	53.478554
3121.191327	327502.780273	53.483559
3120.556796	327309.233439	53.488564
3119.928265	327136.867806	53.493569
3119.370482	326950.640387	53.498573
3118.702314	326770.871375	53.503578
3117.773394	326585.771135	53.508583
3117.448541	326415.519978	53.513588
3116.480643	326240.940129	53.518593
3116.115859	326059.313825	53.523597
3115.492737	325878.160808	53.528602
3114.352231	325697.776675	53.533607
3114.066883	325513.717832	53.538612
3113.072574	325339.471183	53.543617
3112.339224	325161.414712	53.548621
3111.793621	324985.797820	53.553626
3110.880442	324795.216937	53.558631
3110.630489	324626.274100	53.563636
3109.588058	324461.300879	53.568641
3109.194688	324276.365210	53.573645
3108.514276	324100.105774	53.578650
3107.788010	323928.385261	53.583655
3107.347493	323734.188075	53.588660
3106.383899	323572.128624	53.593665
3105.739736	323387.001514	53.598669
3105.150963	323215.054095	53.603674
3104.342258	323033.975103	53.608679
3103.744711	322852.633163	53.613684
3102.870441	322693.358628	53.618689
3102.493517	322513.177737	53.623693
3101.999911	322342.079182	53.628698
3100.859778	322171.413586	53.633703
3100.511163	321983.028526	53.638708
3099.808618	321825.252903	53.643713
3098.934540	321645.556253	53.648717
3098.481647	321475.213394	53.653722
3097.672182	321301.030987	53.658727
3097.147861	321123.544015	53.663732
3096.047939	320961.373912	53.668737
3095.669923	320789.821178	53.673741
3094.989848	320618.850608	53.678746
3094.194074	320442.245470	53.683751
3093.786969	320270.645417	53.688756
3092.971054	320100.611985	53.693761
3092.120044	319935.217885	53.698765
3091.649641	319766.860575	53.703770
3090.931638	319590.979869	53.708775
3090.500991	319417.243106	53.713780
3089.396949	319253.211842	53.718785
3089.004340	319077.329588	53.723789
3088.310713	318921.278882	53.728794
3087.572786	318756.705021	53.733799
3087.332417	318570.816455	53.738804
3086.324954	318405.495289	53.743809
3085.668077	318234.134659	53.748813
3084.814360	318068.508485	53.753818
3084.379402	317893.776523	53.758823
3083.954304	317721.130619	53.763828
3083.095591	317558.050613	53.768833
3082.502384	317378.504831	53.773837
3081.963315	317210.866745	53.778842
3081.013161	317041.994812	53.783847
3080.571760	316862.551364	53.788852
3080.091817	316695.488678	53.793857
3079.524581	316512.550610	53.798861
3078.568505	316343.856647	53.803866
3077.848426	316178.180621	53.808871
3077.215944	316000.191766	53.813876
3076.338158	315832.044731	53.818881
3075.759026	315643.836064	53.823885
3075.400942	315488.847088	53.828890
3074.707554	315314.278727	53.833895
3074.036853	315140.012034	53.838900
3073.235730	314964.798072	53.843905
3072.422396	314789.814912	53.848909
3071.689686	314630.096781	53.853914
3071.238880	314454.877439	53.858919
3070.470182	314289.817137	53.863924
3069.615274	314120.492330	53.868929
3068.948193	313937.005203	53.873933
3068.687854	313777.669356	53.878938
3067.474839	313612.016237	53.883943
3066.925704	313448.396759	53.888948
3066.418698	313281.460068	53.893953
3065.693676	313110.152369	53.898957
3064.851790	312940.059693	53.903962
3064.143135	312776.744531	53.908967
3063.814406	312613.267145	53.913972
3063.076266	312460.600107	53.918977
3062.512822	312282.135605	53.923981
3061.771029	312114.215700	53.928986
3061.020869	311941.331360	53.933991
3060.351692	311778.746917	53.938996
3059.768004	311621.521651	53.944001
3058.840547	311448.155314	53.949005
3058.109415	311295.001734	53.954010
3057.450879	311133.967987	53.959015
3056.999894	310957.851740	53.964020
3056.081399	310804.345179	53.969025
3055.522771	310650.781461	53.974029
3054.824921	310483.157731	53.979034
3053.984309	310316.294818	53.984039
3053.505328	310151.106022	53.989044
3052.708946	310006.109684	53.994049
3051.902854	309838.018321	53.999053
3051.560835	309682.763841	54.004058
3050.726332	309521.806616	54.009063
3050.310810	309355.027845	54.014068
3049.439598	309200.544024	54.019073
3048.655397	309042.175589	54.024077
3048.449098	308882.977011	54.029082
3047.486125	308721.962641	54.034087
3046.947355	308551.611715	54.039092
3046.519696	308395.681564	54.044097
3045.716678	308237.493307	54.049101
3045.240026	308080.806560	54.054106
3044.129706	307914.314011	54.059111
3043.943299	307740.748536	54.064116
3043.060615	307582.291932	54.069121
3042.462130	307412.330858	54.074125
3041.854496	307260.018337	54.079130
3040.881215	307098.315924	54.084135
3040.160420	306937.235443	54.089140
3039.878872	306779.905029	54.094145
3039.203929	306610.489751	54.099149
3038.087094	306448.911096	54.104154
3037.426795	306293.244342	54.109159
3037.403430	306127.264994	54.114164
3036.431741	305972.029116	54.119169
3035.626829	305801.691136	54.124173
3034.894152	305635.976216	54.129178
3034.112362	305477.883040	54.134183
3033.608906	305321.553680	54.139188
3032.930916	305170.675919	54.144193
3032.568449	305008.059360	54.149197
3031.710877	304839.409218	54.154202
3030.784989	304686.685697	54.159207
3030.390831	304517.274246	54.164212
3029.700494	304371.898139	54.169217
3028.967061	304215.578444	54.174221
3028.207343	304059.390061	54.179226
3027.548286	303888.695549	54.184231
3026.997335	303736.319100	54.189236
3025.979587	303589.873504	54.194241
3025.601884	303423.284834	54.199245
3025.095880	303268.354185	54.204250
3024.235787	303111.798659	54.209255
3023.953257	302947.206183	54.214260
3023.418500	302789.223660	54.219265
3022.510954	302632.751527	54.224269
3021.874024	302469.538836	54.229274
3021.100027	302299.140765	54.234279
3020.644981	302137.605149	54.239284
3019.696016	301985.951980	54.244289
3019.575783	301812.393956	54.249293
3018.538200	301661.442073	54.254298
3017.809907	301496.180027	54.259303
3017.340290	301334.060140	54.264308
3016.509008	301171.742660	54.269313
3015.862965	300998.445199	54.274317
3015.382863	300855.375242	54.279322
3014.717487	300693.107408	54.284327
3013.765780	300526.147984	54.289332
3013.086373	300366.250407	54.294337
3012.426281	300194.736936	54.299341
3011.990065	300031.820970	54.304346
3011.485576	299876.581047	54.309351
3010.998030	299710.795175	54.314356
3010.001281	299552.271280	54.319361
3009.386287	299393.101084	54.324365
3008.844299	299218.460986	54.329370
3007.934000	299053.097900	54.334375
3007.408513	298886.858817	54.339380
3006.469184	298742.815565	54.344385
3005.874340	298568.896231	54.349389
3005.181449	298417.530243	54.354394
3004.266440	298254.306332	54.359399
3003.813048	298092.893746	54.364404
3003.206510	297940.495010	54.369409
3002.723105	297777.940884	54.374413
3001.971685	297616.371300	54.379418
3001.473381	297461.281013	54.384423
3000.526418	297285.404269	54.389428
3000.007552	297138.797416	54.394433
2999.273788	296976.333130	54.399437
2998.656075	296815.072744	54.404442
2997.690625	296660.310387	54.409447
2997.401792	296485.856735	54.414452
2996.859348	296337.826836	54.419457
2995.805156	296180.837040	54.424461
2995.240140	296029.219631	54.429466
2994.517931	295860.003803	54.434471
2994.084031	295693.059697	54.439476
2993.585760	295536.083261	54.444481
2992.981933	295367.688685	54.449485
2992.221965	295215.388426	54.454490
2991.371461	295049.706673	54.459495
2990.894219	294884.194910	54.464500
2989.832086	294721.678846	54.469505
2989.598358	294550.703765	54.474509
2988.894224	294394.472111	54.479514
2988.421470	294233.517749	54.484519
2987.537614	294062.976245	54.489524
2986.571572	293918.067685	54.494529
2986.101257	293742.723561	54.499533
2985.361983	293584.332156	54.504538
2984.727327	293428.700017	54.509543
2984.113573	293267.232439	54.514548
2983.567014	293112.935903	54.519553
2983.032971	292943.458723	54.524557
2981.890305	292777.082903	54.529562
2981.343373	292618.329295	54.534567
2980.915448	292456.271443	54.539572
2980.130383	292301.171685	54.544577
2979.661827	292135.172587	54.549581
2979.274976	291975.145300	54.554586
2978.477400	291805.632603	54.559591
2977.724952	291645.230016	54.564596
2977.109449	291480.170556	54.569601
2976.433763	291314.967707	54.574605
2975.693216	291147.890415	54.579610
2974.911456	290989.096500	54.584615
2974.505739	290813.587153	54.589620
2973.336282	290653.912095	54.594625
2972.847328	290493.670810	54.599629
2972.133708	290327.403686	54.604634
2971.489947	290171.821821	54.609639
2971.086058	290005.530939	54.614644
2970.021932	289851.339745	54.619649
2969.398452	289691.501288	54.624653
2969.395142	289536.810927	54.629658
2968.406548	289377.794114	54.634663
2967.885845	289207.115323	54.639668
2967.132394	289033.850091	54.644673
2966.463016	288878.704510	54.649677
2965.828691	288715.174393	54.654682
2964.907146	288546.570619	54.659687
2964.282032	288386.731697	54.664692
2963.970900	288224.805564	54.669697
2963.131161	288055.093451	54.674701
2962.462539	287890.651476	54.679706
2961.377210	287730.910530	54.684711
2961.171233	287569.018348	54.689716
2960.316471	287403.204852	54.694721
2959.654825	287235.144996	54.699725
2958.962082	287077.047937	54.704730
2958.146354	286912.577817	54.709735
2957.805196	286745.791319	54.714740
2956.959588	286593.856010	54.719745
2956.283089	286424.397367	54.724749
2956.047861	286262.127170	54.729754
2955.161401	286102.201169	54.734759
2954.330768	285937.682019	54.739764
2953.588655	285775.084354	54.744769
2953.124598	285617.561679	54.749773
2952.396671	285451.115957	54.754778
2952.089297	285292.371349	54.759783
2951.486534	285135.303392	54.764788
2950.358366	284971.976991	54.769793
2949.852032	284799.179836	54.774797
2949.476941	284633.467432	54.779802
2948.419517	284471.301168	54.784807
2947.830970	284293.983496	54.789812
2947.269118	284136.679474	54.794817
2946.692849	283975.404650	54.799821
2946.148447	283808.674541	54.804826
2945.327294	283641.224135	54.809831
2944.997421	283460.554329	54.814836
2944.238200	283306.337446	54.819841
2943.504706	283131.410812	54.824845
2942.905115	282965.198508	54.829850
2941.931209	282799.376489	54.834855
2941.140250	282617.709702	54.839860
2940.518070	282466.221438	54.844865
2939.855999	282306.538679	54.849869
2939.532033	282137.098957	54.854874
2938.957553	281980.101872	54.859879
2938.421370	281804.124840	54.864884
2937.811359	281641.148251	54.869889
2937.140191	281461.270377	54.874893
2936.644741	281293.487529	54.879898
2935.498908	281125.654783	54.884903
2935.028350	280940.320265	54.889908
2934.266844	280766.365140	54.894913
2933.516824	280602.722811	54.899917
2933.038935	280443.621660	54.904922
2932.159037	280276.536129	54.909927
2931.880168	280097.996554	54.914932
2931.121727	279937.691762	54.919937
2930.212909	279757.774671	54.924941
2929.768369	279580.279941	54.929946
2928.994476	279402.480756	54.934951
2928.664263	279241.929767	54.939956
2927.520728	279075.140418	54.944961
2926.924311	278896.065094	54.949965
2926.140185	278728.760362	54.954970
2925.306766	278562.482141	54.959975
2924.986676	278394.798279	54.964980
2924.315939	278225.718206	54.969985
2923.579524	278061.080002	54.974989
2923.039846	277884.847995	54.979994
2922.107897	277723.704401	54.984999
2921.857199	277554.786964	54.990004
2921.026133	277382.472218	54.995009
2920.176084	277213.114790	55.000013
2919.592064	277042.390877	55.005018
2918.870818	276876.222043	55.010023
2918.229625	276711.543159	55.015028
2917.406815	276552.572463	55.020033
2916.779616	276384.962476	55.025037
2916.462593	276206.377439	55.030042
2915.409887	276041.916469	55.035047
2914.848518	275877.836141	55.040052
2914.129991	275718.925300	55.045057
2913.855065	275549.604062	55.050061
2912.992809	275372.378724	55.055066
2912.367523	275205.685251	55.060071
2911.747308	275032.572939	55.065076
2910.861267	274870.632395	55.070081
2910.468960	274706.041382	55.075085
2909.978501	274532.144478	55.080090
2908.918619	274363.533273	55.085095
2908.411031	274191.676559	55.090100
2907.675748	274016.035638	55.095105
2906.709285	273843.156440	55.100109
2906.066977	273674.606495	55.105114
2905.647062	273503.398107	55.110119
2905.049716	273333.465770	55.115124
2904.235848	273164.866610	55.120129
2903.487475	273014.135896	55.125133
2903.280131	272838.156784	55.130138
2902.400875	272671.070649	55.135143
2902.080014	272496.484832	55.140148
2901.409687	272317.548330	55.145153
2900.488425	272161.878726	55.150157
2899.737463	271984.890625	55.155162
2898.902449	271810.615500	55.160167
2898.482396	271648.474046	55.165172
2897.768414	271484.723705	55.170177
2896.931445	271307.138073	55.175181
2896.392166	271139.947363	55.180186
2895.480330	270975.719052	55.185191
2895.038422	270806.424575	55.190196
2894.370589	270630.696938	55.195201
2893.939782	270471.027793	55.200205
2893.026891	270312.835755	55.205210
2892.680655	270139.604130	55.210215
2892.157064	269964.414090	55.215220
2891.310242	269798.673067	55.220225
2890.676222	269627.142551	55.225229
2889.907663	269451.736724	55.230234
2889.227361	269287.395673	55.235239
2888.631596	269115.833750	55.240244
2888.124573	268941.379904	55.245249
2887.253140	268765.761318	55.250253
2886.569132	268601.395548	55.255258
2885.922242	268429.892831	55.260263
2885.193331	268248.597868	55.265268
2884.609274	268092.060629	55.270273
2883.824031	267913.041360	55.275277
2883.250114	267746.187971	55.280282
2882.367841	267582.643383	55.285287
2881.921375	267419.080782	55.290292
2881.317241	267253.964164	55.295297
2880.724060	267076.035357	55.300301
2880.087317	266909.981686	55.305306
2879.269733	266739.728982	55.310311
2878.885752	266569.000196	55.315316
2878.293965	266395.273658	55.320321
2877.296388	266226.475847	55.325325
2876.961140	266044.864629	55.330330
2875.988425	265877.438289	55.335335
2875.387712	265697.117178	55.340340
2874.437151	265546.496419	55.345345
2873.983915	265374.989528	55.350349
2873.697080	265200.603933	55.355354
2872.864515	265037.383432	55.360359
2872.497632	264848.341040	55.365364
2871.757369	264678.713581	55.370369
2870.979807	264506.443422	55.375373
2870.511959	264328.776014	55.380378
2869.667325	264151.779576	55.385383
2869.185048	263977.731076	55.390388
2868.260739	263801.256778	55.395393
2867.870757	263614.510769	55.400397
2867.527146	263439.956677	55.405402
2866.518745	263260.006844	55.410407
2865.748419	263085.011130	55.415412
2864.849380	262901.758802	55.420417
2864.231797	262730.100853	55.425421
2863.659099	262562.816368	55.430426
2863.076262	262378.801161	55.435431
2862.850080	262206.342945	55.440436
2861.880206	262030.386132	55.445441
2860.880899	261851.836356	55.450445
2860.635511	261673.243717	55.455450
2859.562799	261517.193864	55.460455
2859.279459	261321.849606	55.465460
2858.292790	261140.547720	55.470465
2857.605068	260967.602981	55.475469
2857.324927	260791.333937	55.480474
2856.658801	260624.065296	55.485479
2855.862831	260443.344877	55.490484
2854.924277	260264.073343	55.495489
2854.638015	260083.246985	55.500493
2853.900264	259902.441296	55.505498
2853.200644	259737.496051	55.510503
2852.600759	259563.035679	55.515508
2852.010024	259381.010084	55.520513
2851.131145	259200.099877	55.525517
2850.343728	259014.030860	55.530522
2849.842211	258838.434822	55.535527
2849.156821	258662.664279	55.540532
2848.479625	258491.476720	55.545537
2847.729272	258314.723474	55.550541
2847.519207	258129.862539	55.555546
2846.504903	257957.862834	55.560551
2845.893019	257782.132217	55.565556
2845.333231	257601.096249	55.570561
2844.872713	257426.971845	55.575565
2844.094820	257246.047088	55.580570
2842.998329	257068.993029	55.585575
2842.577296	256894.837307	55.590580
2841.571763	256724.085024	55.595585
2840.838076	256548.578370	55.600589
2840.619928	256358.371982	55.605594
2839.682047	256194.001693	55.610599
2839.388912	256014.223604	55.615604
2838.796620	255832.150044	55.620609
2837.852532	255660.217369	55.625613
2837.189748	255488.062021	55.630618
2836.554764	255313.432095	55.635623
2835.916388	255133.251008	55.640628
2835.424508	254963.921356	55.645633
2834.264150	254783.084680	55.650637
2834.146524	254595.385208	55.655642
2833.085218	254428.081668	55.660647
2832.435816	254252.054245	55.665652
2831.964354	254084.530261	55.670657
2831.468329	253905.779355	55.675661
2830.921015	253721.688666	55.680666
2829.925568	253546.506151	55.685671
2829.556729	253360.044587	55.690676
2828.690228	253190.215508	55.695681
2827.932571	253016.549312	55.700685
2827.986499	252830.046798	55.705690
2826.840918	252648.955112	55.710695
2826.235649	252465.256833	55.715700
2825.427038	252283.882950	55.720705
2824.892093	252113.187427	55.725709
2823.999890	251933.278740	55.730714
2823.378685	251763.055613	55.735719
2823.029819	251570.276965	55.740724
2822.167151	251385.907490	55.745729
2821.428020	251219.472631	55.750733
2820.899872	251031.587099	55.755738
2820.162429	250856.315410	55.760743
2819.587006	250671.493753	55.765748
2819.054863	250492.191682	55.770753
2818.284770	250309.158440	55.775757
2817.454739	250133.902167	55.780762
2816.600475	249956.994599	55.785767
2816.353753	249779.354357	55.790772
2815.743047	249595.176150	55.795777
2814.605088	249410.266720	55.800781
2814.239440	249232.900575	55.805786
2813.586151	249057.897611	55.810791
2812.618412	248875.559412	55.815796
2812.427245	248699.948876	55.820801
2811.311644	248518.958754	55.825805
2810.864008	248336.869888	55.830810
2810.349548	248172.363472	55.835815
2809.715996	247980.703726	55.840820
2808.846601	247811.084282	55.845825
2807.965293	247623.666129	55.850829
2807.539424	247450.768132	55.855834
2807.033458	247274.674303	55.860839
2806.238331	247093.838869	55.865844
2805.655503	246917.834035	55.870849
2804.908880	246733.349735	55.875853
2804.708200	246538.210875	55.880858
2803.786523	246379.297032	55.885863
2803.539597	246187.552930	55.890868
2802.450233	245994.618270	55.895873
2801.832779	245820.784858	55.900877
2801.167275	245634.837585	55.905882
2800.365273	245456.933868	55.910887
2800.146997	245268.344230	55.915892
2799.210823	245077.984078	55.920897
2798.176310	244890.695634	55.925901
2798.307192	244706.507954	55.930906
2797.210918	244536.699148	55.935911
2796.506830	244352.644176	55.940916
2796.255559	244162.482439	55.945921
2795.158896	243970.646805	55.950925
2794.564163	243786.982747	55.955930
2793.787258	243608.237139	55.960935
2793.428052	243419.341369	55.965940
2792.465401	243238.359273	55.970945
2791.946673	243055.295378	55.975949
2791.217503	242863.377718	55.980954
2790.604084	242691.075652	55.985959
2790.020147	242508.073800	55.990964
2789.252363	242318.072964	55.995969
2788.481416	242136.018013	56.000973
2787.640877	241949.339716	56.005978
2787.208480	241770.109233	56.010983
2786.974493	241587.766333	56.015988
2785.926195	241410.212737	56.020993
2785.235640	241218.342426	56.025997
2784.692886	241032.738822	56.031002
2783.811841	240845.839444	56.036007
2783.361567	240665.416576	56.041012
2782.812398	240483.889197	56.046017
2781.898681	240301.859603	56.051021
2781.282385	240111.354401	56.056026
2780.428869	239928.068087	56.061031
2779.853034	239741.682341	56.066036
2779.036202	239572.014307	56.071041
2778.278580	239391.260104	56.076045
2778.375945	239205.023256	56.081050
2777.255811	239024.479828	56.086055
2777.171702	238841.506289	56.091060
2776.146857	238653.079880	56.096065
2775.555319	238466.622307	56.101069
2774.881526	238292.222643	56.106074
2774.030892	238103.387608	56.111079
2773.693262	237913.987832	56.116084
2772.897105	237728.786179	56.121089
2772.023431	237542.807730	56.126093
2771.969771	237350.817549	56.131098
2770.708118	237160.903348	56.136103
2770.017938	236971.128152	56.141108
2769.578083	236790.735277	56.146113
2768.789684	236606.400085	56.151117
2768.327875	236422.802866	56.156122
2767.615628	236236.928428	56.161127
2767.111058	236033.858902	56.166132
2766.499806	235862.254258	56.171137
2765.159272	235674.977961	56.176141
2765.061100	235473.092879	56.181146
2764.139096	235283.713923	56.186151
2763.767929	235104.306142	56.191156
2763.269064	234914.631681	56.196161
2762.493701	234716.904013	56.201165
2761.762091	234527.725474	56.206170
2760.929818	234334.489108	56.211175
2760.582004	234149.273691	56.216180
2759.844951	233963.330903	56.221185
2759.115057	233781.639670	56.226189
2758.445563	233580.128933	56.231194
2757.667899	233397.885782	56.236199
2756.818153	233200.987711	56.241204
2756.355344	233022.132895	56.246209
2755.623354	232835.478471	56.251213
2755.128302	232647.004484	56.256218
2754.461621	232462.020984	56.261223
2753.884385	232272.313069	56.266228
2752.981678	232080.874689	56.271233
2752.358941	231893.466374	56.276237
2751.616654	231704.218594	56.281242
2750.757646	231512.621666	56.286247
2750.281581	231327.482870	56.291252
2749.891010	231145.488241	56.296257
2749.134417	230959.707119	56.301261
2748.514232	230773.497366	56.306266
2747.611284	230594.436747	56.311271
2746.969452	230392.622819	56.316276
2746.220858	230213.614882	56.321281
2745.526143	230032.205324	56.326285
2744.983418	229842.471421	56.331290
2744.001312	229658.892927	56.336295
2743.774369	229476.748382	56.341300
2743.156462	229283.361041	56.346305
2741.999275	229096.603226	56.351309
2741.762953	228906.670000	56.356314
2740.983532	228729.783226	56.361319
2740.958174	228544.018553	56.366324
2740.093254	228352.072756	56.371329
2738.800859	228158.336389	56.376333
2738.464697	227970.050538	56.381338
2737.842361	227792.224162	56.386343
2737.130274	227605.780943	56.391348
2736.566845	227409.130037	56.396353
2736.041095	227219.526395	56.401357
2735.682740	227032.188173	56.406362
2734.656268	226841.137002	56.411367
2734.124121	226643.006155	56.416372
2733.599135	226446.605992	56.421377
2732.531925	226260.094658	56.426381
2732.192933	226062.927563	56.431386
2731.410219	225880.445768	56.436391
2730.845880	225683.964513	56.441396
2730.222723	225488.587853	56.446401
2729.222495	225293.054962	56.451405
2728.978435	225099.185015	56.456410
2728.201771	224905.056166	56.461415
2727.468241	224715.363811	56.466420
2727.041107	224523.522880	56.471425
2726.118192	224324.682932	56.476429
2725.627248	224132.089223	56.481434
2724.939747	223944.351835	56.486439
2724.107452	223740.254158	56.491444
2723.438079	223553.355005	56.496449
2722.424159	223355.397524	56.501453
2721.866150	223168.889000	56.506458
2721.139960	222985.742814	56.511463
2720.824222	222791.125993	56.516468
2720.208492	222596.531713	56.521473
2719.248317	222408.968460	56.526477
2718.974763	222208.910742	56.531482
2718.368128	222015.640380	56.536487
2717.759658	221823.898371	56.541492
2717.029036	221623.621779	56.546497
2716.172807	221432.620128	56.551501
2715.770384	221232.330766	56.556506
2714.677895	221047.286818	56.561511
2714.224803	220851.487333	56.566516
2713.551782	220658.892864	56.571521
2712.673065	220469.946669	56.576525
2712.066103	220270.939754	56.581530
2711.265472	220085.648271	56.586535
2710.224801	219905.130638	56.591540
2710.128978	219715.553169	56.596545
2709.098795	219527.333479	56.601549
2708.941651	219326.322977	56.606554
2708.178267	219148.118211	56.611559
2707.459353	218960.372574	56.616564
2706.777864	218759.930395	56.621569
2706.328990	218574.765212	56.626573
2705.733944	218375.990662	56.631578
2705.158296	218194.970798	56.636583
2704.499164	217999.020588	56.641588
2703.682666	217803.910504	56.646593
2702.882015	217611.827965	56.651597
2702.310831	217408.355286	56.656602
2701.553677	217216.381487	56.661607
2700.755542	217026.795018	56.666612
2700.205741	216833.681993	56.671617
2699.625730	216649.891844	56.676621
2699.048638	216458.540764	56.681626
2698.117927	216271.866790	56.686631
2697.595710	216075.951144	56.691636
2697.142686	215883.309112	56.696641
2696.267387	215684.981119	56.701645
2695.886632	215487.186338	56.706650
2694.870839	215297.473587	56.711655
2693.981659	215113.290987	56.716660
2693.578113	214919.243672	56.721665
2692.844965	214726.814733	56.726669
2692.193586	214539.973936	56.731674
2691.757050	214348.784667	56.736679
2690.931062	214153.113576	56.741684
2690.411325	213960.411177	56.746689
2689.519602	213775.736217	56.751693
2689.117730	213582.952594	56.756698
2688.434070	213397.291100	56.761703
2687.419088	213211.478957	56.766708
2687.076907	213008.084904	56.771713
2686.377986	212824.196660	56.776717
2685.520190	212615.819676	56.781722
2684.963111	212437.001309	56.786727
2684.202195	212240.854621	56.791732
2683.858264	212042.644169	56.796737
2682.784391	211853.739566	56.801741
2682.375148	211663.368341	56.806746
2681.691158	211465.073517	56.811751
2680.712419	211286.656045	56.816756
2680.383594	211090.088023	56.821761
2679.481057	210901.808197	56.826765
2679.088780	210710.889815	56.831770
2678.456626	210518.928147	56.836775
2677.692637	210339.448362	56.841780
2676.758132	210149.992155	56.846785
2675.952627	209963.048881	56.851789
2675.940138	209760.414704	56.856794
2675.265408	209572.662767	56.861799
2674.514894	209382.225168	56.866804
2674.064890	209190.824169	56.871809
2673.164289	208994.035074	56.876813
2672.740368	208800.200211	56.881818
2671.570617	208616.589619	56.886823
2670.814266	208420.581325	56.891828
2670.079077	208230.221212	56.896833
2669.647260	208042.715442	56.901837
2669.047038	207854.613293	56.906842
2668.097400	207665.574360	56.911847
2667.882666	207490.381240	56.916852
2667.407246	207291.035754	56.921857
2666.770251	207100.230906	56.926861
2666.246779	206903.948799	56.931866
2665.139855	206708.192479	56.936871
2664.572145	206498.517233	56.941876
2664.130571	206315.778238	56.946881
2663.248723	206125.257099	56.951885
2663.071551	205927.103411	56.956890
2662.198737	205730.447802	56.961895
2661.230434	205537.104191	56.966900
2660.378416	205341.006564	56.971905
2659.993960	205153.438714	56.976909
2659.382979	204950.304573	56.981914
2658.553968	204753.301686	56.986919
2658.193190	204556.887067	56.991924
2657.482621	204368.940704	56.996929
2656.490536	204175.249038	57.001933
2656.190187	203978.394112	57.006938
2655.670074	203778.991233	57.011943
2654.651949	203588.334532	57.016948
2653.885205	203389.404774	57.021953
2653.198408	203207.579762	57.026957
2652.967602	203012.816962	57.031962
2651.738601	202812.473494	57.036967
2651.469662	202611.405970	57.041972
2650.978257	202419.435323	57.046977
2650.094755	202230.950732	57.051981
2649.401634	202032.357684	57.056986
2648.616602	201837.317694	57.061991
2648.065572	201641.465039	57.066996
2647.468529	201447.478328	57.072001
2646.921120	201258.714712	57.077005
2646.037111	201059.111865	57.082010
2645.339399	200873.796587	57.087015
2644.594151	200676.323779	57.092020
2644.082495	200475.506027	57.097025
2643.352316	200284.115063	57.102029
2642.583629	200100.187998	57.107034
2642.131968	199902.722371	57.112039
2641.448971	199707.088390	57.117044
2640.729192	199515.673029	57.122049
2640.087599	199327.681788	57.127053
2639.490595	199129.936597	57.132058
2638.734584	198942.550188	57.137063
2637.956059	198741.539356	57.142068
2637.477441	198546.627993	57.147073
2636.993141	198354.046928	57.152077
2636.040153	198165.472842	57.157082
2635.089875	197975.944624	57.162087
2634.357573	197772.156083	57.167092
2634.112789	197586.716713	57.172097
2633.542616	197404.281708	57.177101
2633.026809	197204.812954	57.182106
2632.176891	197012.778239	57.187111
2631.648232	196817.715754	57.192116
2631.550330	196620.817027	57.197121
2630.414369	196430.623946	57.202125
2629.905990	196231.234080	57.207130
2628.932404	196021.191930	57.212135
2628.389830	195825.880883	57.217140
2627.707825	195632.017798	57.222145
2626.914856	195437.307768	57.227149
2626.452182	195230.254470	57.232154
2625.605927	195044.054212	57.237159
2625.309540	194840.729801	57.242164
2624.646664	194639.271095	57.247169
2623.860042	194445.658120	57.252173
2623.181788	194255.578727	57.257178
2622.775821	194051.206019	57.262183
2621.639471	193849.800022	57.267188
2621.082923	193643.684194	57.272193
2620.295510	193458.218435	57.277197
2619.915377	193243.614937	57.282202
2618.950711	193053.483680	57.287207
2618.523824	192862.619037	57.292212
2617.957211	192662.985217	57.297217
2617.003792	192473.426963	57.302221
2616.615282	192268.397155	57.307226
2616.079985	192063.416901	57.312231
2615.045962	191862.219041	57.317236
2614.586363	191671.949459	57.322241
2613.635019	191470.498363	57.327245
2613.447165	191262.959907	57.332250
2612.453007	191076.772451	57.337255
2611.374999	190878.830038	57.342260
2610.996030	190681.362943	57.347265
2610.301621	190489.506622	57.352269
2609.744843	190289.486512	57.357274
2608.960793	190100.305056	57.362279
2608.753519	189900.854612	57.367284
2608.042189	189701.370353	57.372289
2607.040993	189503.306918	57.377293
2606.421960	189303.428012	57.382298
2605.882533	189119.860588	57.387303
2604.975951	188916.021210	57.392308
2604.591514	188715.573255	57.397313
2603.794328	188523.741110	57.402317
2603.360934	188335.299906	57.407322
2602.316517	188145.633132	57.412327
2601.895412	187939.838127	57.417332
2601.280663	187740.423161	57.422337
2600.349623	187543.552730	57.427341
2599.656207	187345.271478	57.432346
2598.965967	187157.257378	57.437351
2598.228106	186968.551866	57.442356
2597.708860	186764.520532	57.447361
2597.259599	186572.526775	57.452365
2596.597574	186371.305926	57.457370
2596.135679	186179.621134	57.462375
2595.199014	185986.943730	57.467380
2594.636371	185780.862686	57.472385
2593.764670	185587.744128	57.477389
2593.423084	185392.150711	57.482394
2592.974278	185191.333801	57.487399
2592.126873	185000.987201	57.492404
2591.783279	184800.282567	57.497409
2590.782725	184605.865559	57.502413
2590.247774	184389.265770	57.507418
2589.550218	184199.242284	57.512423
2588.829774	183991.782304	57.517428
2588.325526	183789.593791	57.522433
2587.639461	183597.879107	57.527437
2587.155882	183388.247233	57.532442
2586.359751	183183.080084	57.537447
2585.413002	182988.852390	57.542452
2584.792018	182780.822560	57.547457
2584.045300	182586.844795	57.552461
2583.432698	182371.780898	57.557466
2582.846124	182188.872093	57.562471
2582.371877	181980.835507	57.567476
2581.711952	181772.180573	57.572481
2580.687710	181588.046114	57.577485
2580.463050	181365.445955	57.582490
2579.745904	181179.458242	57.587495
2578.853217	180971.848939	57.592500
2578.533525	180766.401345	57.597505
2577.554543	180579.669028	57.602509
2576.824883	180365.574874	57.607514
2576.268898	180167.774288	57.612519
2575.587686	179961.917159	57.617524
2575.176283	179754.161133	57.622529
2574.482498	179561.714890	57.627533
2573.726422	179350.631911	57.632538
2572.847024	179160.010405	57.637543
2572.191988	178954.713656	57.642548
2571.477685	178750.686550	57.647553
2570.357881	178554.509151	57.652557
2570.077130	178357.919878	57.657562
2569.574524	178164.063232	57.662567
2568.769058	177961.936882	57.667572
2568.017886	177764.203844	57.672577
2567.116656	177575.335520	57.677581
2566.715735	177379.380396	57.682586
2566.098567	177174.531502	57.687591
2565.463057	176983.664974	57.692596
2565.166309	176787.479897	57.697601
2564.338917	176584.091770	57.702605
2563.609077	176367.270573	57.707610
2563.175993	176178.003716	57.712615
2562.607732	175968.777689	57.717620
2561.891225	175769.446064	57.722625
2560.909614	175574.990564	57.727629
2560.169427	175368.860070	57.732634
2559.605483	175164.419710	57.737639
2558.935385	174977.676087	57.742644
2558.078884	174776.400095	57.747649
2557.484979	174587.865587	57.752653
2556.886152	174379.797199	57.757658
2556.173143	174178.361530	57.762663
2555.483367	173988.191615	57.767668
2555.326420	173787.420161	57.772673
2554.337382	173585.471588	57.777677
2553.840025	173383.153600	57.782682
2553.191733	173187.283174	57.787687
2552.266490	172979.108410	57.792692
2551.680305	172784.578222	57.797697
2550.868562	172592.793634	57.802701
2550.658898	172372.719170	57.807706
2549.901958	172176.387647	57.812711
2549.013329	171976.186355	57.817716
2548.399463	171781.563723	57.822721
2547.447094	171587.555263	57.827725
2547.353396	171381.380941	57.832730
2546.574244	171176.677084	57.837735
2545.679139	170978.796456	57.842740
2545.638719	170776.025120	57.847745
2544.566443	170577.284387	57.852749
2544.064764	170370.289827	57.857754
2543.305634	170164.163775	57.862759
2542.337038	169969.072239	57.867764
2542.182781	169752.971384	57.872769
2541.148477	169562.661167	57.877773
2540.538266	169346.876455	57.882778
2539.972641	169150.173737	57.887783
2539.146608	168955.064729	57.892788
2538.462464	168748.997923	57.897793
2537.613212	168552.050731	57.902797
2537.217164	168350.785423	57.907802
2536.392060	168149.907078	57.912807
2535.623664	167955.391702	57.917812
2535.127798	167757.235420	57.922817
2534.444241	167562.873919	57.927821
2534.009207	167353.532535	57.932826
2533.663324	167150.981291	57.937831
2532.579224	166935.806662	57.942836
2532.142261	166736.934287	57.947841
2531.126299	166547.221147	57.952845
2530.621100	166338.761194	57.957850
2530.103184	166135.136400	57.962855
2529.302667	165941.653751	57.967860
2528.865738	165735.220849	57.972865
2528.063381	165533.869640	57.977869
2527.265201	165326.199267	57.982874
2526.583042	165120.380832	57.987879
2525.826427	164929.465000	57.992884
2525.538907	164730.172739	57.997889
2524.184855	164531.215870	58.002893
2524.045046	164329.066874	58.007898
2523.359541	164125.212644	58.012903
2522.419800	163920.560645	58.017908
2522.149632	163713.197118	58.022913
2521.733751	163468.018486	58.027917
2521.412929	163255.185488	58.032922
2520.378738	163042.403210	58.037927
2519.170291	162834.443204	58.042932
2518.784748	162639.348239	58.047937
2518.292638	162441.906320	58.052941
2517.758442	162223.506095	58.057946
2517.264798	162022.748248	58.062951
2515.943059	161812.014921	58.067956
2515.678500	161611.248491	58.072961
2514.948093	161403.335393	58.077965
2514.235224	161202.121020	58.082970
2513.446575	160990.837612	58.087975
2512.858278	160787.291889	58.092980
2512.149228	160579.685329	58.097985
2511.404365	160391.830104	58.102989
2511.008802	160183.095507	58.107994
2510.278423	159975.190730	58.112999
2509.315833	159768.302916	58.118004
2509.000274	159563.881888	58.123009
2508.305164	159369.082659	58.128013
2507.402985	159153.531063	58.133018
2507.082588	158961.471632	58.138023
2506.380846	158742.852327	58.143028
2505.730236	158537.765712	58.148033
2504.673747	158338.910436	58.153037
2504.258930	158133.661693	58.158042
2503.723543	157930.988553	58.163047
2502.798916	157723.776253	58.168052
2502.262803	157518.448660	58.173057
2501.599859	157322.676862	58.178061
2501.142018	157112.978833	58.183066
2500.182604	156905.166741	58.188071
2499.645224	156701.153588	58.193076
2499.179478	156498.426949	58.198081
2498.269623	156304.034861	58.203085
2497.877669	156088.662958	58.208090
2497.319285	155885.115620	58.213095
2495.979838	155671.447386	58.218100
2495.719131	155470.588426	58.223105
2494.912795	155271.253568	58.228109
2494.205398	155056.306816	58.233114
2493.802090	154856.910513	58.238119
2493.088958	154651.920514	58.243124
2492.541801	154449.600305	58.248129
2491.617804	154252.247671	58.253133
2491.145636	154042.367389	58.258138
2490.468248	153835.330147	58.263143
2489.515951	153626.291238	58.268148
2488.952057	153415.476064	58.273153
2488.396335	153228.049356	58.278157
2487.530324	153019.445449	58.283162
2486.806568	152809.282275	58.288167
2486.119523	152613.782955	58.293172
2485.960710	152403.532802	58.298177
2484.965759	152207.728770	58.303181
2484.252505	152000.505221	58.308186
2483.460420	151798.532217	58.313191
2482.662421	151609.920107	58.318196
2482.259264	151399.702344	58.323201
2481.371412	151206.696271	58.328205
2480.750494	151001.409045	58.333210
2480.411181	150808.038748	58.338215
2479.474599	150606.693339	58.343220
2479.117584	150405.015820	58.348225
2478.360225	150211.346715	58.353229
2477.847354	150007.395854	58.358234
2477.296168	149799.385209	58.363239
2475.974328	149604.576333	58.368244
2475.704127	149398.747918	58.373249
2475.287867	149199.019125	58.378253
2474.554304	148998.198004	58.383258
2473.615677	148788.107358	58.388263
2472.655233	148587.871255	58.393268
2472.294806	148376.344463	58.398273
2471.474052	148191.593950	58.403277
2470.911442	147985.261696	58.408282
2470.230420	147785.812396	58.413287
2469.675092	147601.709501	58.418292
2469.458136	147379.859609	58.423297
2468.263051	147180.724326	58.428301
2467.770729	146981.478900	58.433306
2466.983601	146780.337036	58.438311
2465.869985	146585.157655	58.443316
2466.083642	146375.268776	58.448321
2464.776342	146179.957383	58.453325
2464.308615	145988.644315	58.458330
2463.534764	145786.871249	58.463335
2462.896342	145587.568800	58.468340
2462.298772	145392.874156	58.473345
2461.396583	145182.941333	58.478349
2461.342684	144991.988096	58.483354
2460.432804	144797.486439	58.488359
2459.686529	144590.989395	58.493364
2459.306760	144388.146252	58.498369
2458.426011	144185.917553	58.503373
2457.860697	143988.812110	58.508378
2457.348526	143788.980114	58.513383
2456.557087	143583.195826	58.518388
2456.018593	143380.600444	58.523393
2455.223328	143178.745983	58.528397
2454.575470	142985.662757	58.533402
2453.951444	142780.314736	58.538407
2452.979038	142583.409850	58.543412
2452.611250	142376.257654	58.548417
2451.688408	142181.431408	58.553421
2450.941187	141975.206122	58.558426
2450.570405	141775.110649	58.563431
2449.638904	141577.748311	58.568436
2449.032598	141379.471671	58.573441
2448.361127	141179.567538	58.578445
2447.663688	140980.126260	58.583450
2447.518900	140783.266981	58.588455
2446.480614	140590.921491	58.593460
2446.044529	140379.397398	58.598465
2445.343431	140179.250440	58.603469
2445.004695	139975.172102	58.608474
2444.137614	139771.229718	58.613479
2443.625256	139572.416386	58.618484
2442.796713	139364.671669	58.623489
2442.298216	139163.686199	58.628493
2441.511468	138953.472851	58.633498
2441.036756	138749.703916	58.638503
2440.054455	138544.759018	58.643508
2439.334229	138338.528887	58.648513
2438.905266	138135.709781	58.653517
2438.244621	137918.877132	58.658522
2437.559540	137723.394068	58.663527
2436.893304	137524.453613	58.668532
2436.318380	137318.258360	58.673537
2435.431874	137109.357044	58.678541
2434.910175	136900.932968	58.683546
2434.156986	136695.151464	58.688551
2433.099099	136498.198381	58.693556
2432.772024	136288.439251	58.698561
2432.234252	136089.335677	58.703565
2431.571314	135885.451168	58.708570
2430.971934	135673.706959	58.713575
2430.289175	135485.441551	58.718580
2429.552293	135267.548005	58.723585
2428.627023	135061.017643	58.728589
2427.979377	134865.357135	58.733594
2427.539192	134660.175533	58.738599
2426.364341	134461.793845	58.743604
2425.899827	134262.754673	58.748609
2425.238739	134066.161650	58.753613
2424.597363	133867.305680	58.758618
2423.854146	133665.342268	58.763623
2423.138169	133476.675988	58.768628
2423.208876	133266.342114	58.773633
2422.418539	133068.683948	58.778637
2421.300345	132851.643956	58.783642
2420.707930	132660.168866	58.788647
2420.104922	132461.545206	58.793652
2419.623099	132254.913877	58.798657
2418.976286	132049.923400	58.803661
2418.377504	131846.794021	58.808666
2417.651188	131643.749823	58.813671
2416.648643	131448.473737	58.818676
2416.158374	131238.358068	58.823681
2415.512534	131036.944022	58.828685
2415.047504	130838.767117	58.833690
2414.321055	130637.838666	58.838695
2413.872152	130432.168047	58.843700
2413.127431	130223.192619	58.848705
2412.427582	130021.489563	58.853709
2411.589912	129812.265202	58.858714
2410.815111	129599.349074	58.863719
2410.209271	129408.241085	58.868724
2410.056504	129199.141359	58.873729
2409.023605	129001.677114	58.878733
2408.118069	128798.123053	58.883738
2407.591027	128584.845175	58.888743
2406.776121	128389.471756	58.893748
2406.356983	128187.038936	58.898753
2405.455500	127991.174027	58.903757
2404.744496	127783.875325	58.908762
2404.190028	127578.318711	58.913767
2403.469361	127378.149477	58.918772
2403.015726	127175.335837	58.923777
2402.358889	126988.202376	58.928781
2401.654110	126770.877271	58.933786
2401.146074	126567.733845	58.938791
2400.344753	126370.035824	58.943796
2399.552211	126165.314918	58.948801
2399.153127	125963.898563	58.953805
2398.798395	125763.632317	58.958810
2398.083764	125556.884410	58.963815
2397.227158	125358.338933	58.968820
2396.680078	125137.890509	58.973825
2395.728566	124938.944074	58.978829
2394.918729	124731.011141	58.983834
2394.735086	124533.634923	58.988839
2393.673333	124326.811748	58.993844
2393.224491	124121.823198	58.998849
2392.479791	123917.429154	59.003853
2391.674384	123714.735192	59.008858
2391.129202	123499.607837	59.013863
2390.562143	123306.974422	59.018868
2390.233233	123091.460503	59.023873
2389.205769	122903.601329	59.028877
2388.600860	122688.705831	59.033882
2388.051357	122480.152251	59.038887
2387.134438	122283.454853	59.043892
2386.807480	122059.987409	59.048897
2385.867906	121859.385838	59.053901
2385.198274	121649.169038	59.058906
2384.662096	121447.414643	59.063911
2383.809308	121240.112451	59.068916
2383.124456	121031.033041	59.073921
2382.423144	120836.242195	59.078925
2381.559243	120636.399742	59.083930
2381.046416	120430.015001	59.088935
2380.451130	120231.961399	59.093940
2379.907952	120025.178352	59.098945
2378.988097	119833.032430	59.103949
2378.664975	119618.847287	59.108954
2378.161122	119418.950684	59.113959
2376.992147	119214.336440	59.118964
2376.587070	119012.745022	59.123969
2375.819048	118812.520412	59.128973
2375.488767	118614.214880	59.133978
2374.980568	118405.255404	59.138983
2373.883157	118184.418822	59.143988
2373.309667	117980.361034	59.148993
2372.511543	117788.794923	59.153997
2371.723365	117578.407468	59.159002
2371.461050	117378.075688	59.164007
2370.822056	117175.494629	59.169012
2370.280204	116957.379799	59.174017
2369.586683	116759.691990	59.179021
2368.851676	116550.897754	59.184026
2368.487579	116334.911847	59.189031
2367.731744	116135.118680	59.194036
2366.935404	115920.855132	59.199041
2366.122252	115715.145893	59.204045
2365.873832	115501.313133	59.209050
2365.324971	115291.979201	59.214055
2363.977301	115090.028455	59.219060
2363.708826	114868.352753	59.224065
2363.250700	114660.095004	59.229069
2362.412475	114461.705361	59.234074
2361.744226	114245.239576	59.239079
2361.050851	114027.357925	59.244084
2360.672301	113807.619390	59.249089
2359.767393	113593.703726	59.254093
2359.046853	113385.034791	59.259098
2358.968505	113163.654907	59.264103
2358.022802	112960.800682	59.269108
2357.471859	112728.989546	59.274113
2356.260263	112520.964163	59.279117
2355.869096	112303.449396	59.284122
2355.428491	112088.133875	59.289127
2354.490816	111876.922616	59.294132
2354.057679	111664.719288	59.299137
2352.913196	111455.353098	59.304141
2352.412827	111242.231143	59.309146
2351.876244	111031.959833	59.314151
2350.945336	110817.437492	59.319156
2350.584788	110598.067060	59.324161
2349.773497	110399.134279	59.329165
2349.192396	110189.270653	59.334170
2348.365209	109970.563617	59.339175
2347.703091	109754.351642	59.344180
2347.300418	109543.043780	59.349185
2346.291846	109330.304492	59.354189
2345.841824	109123.684536	59.359194
2345.179239	108903.190488	59.364199
2344.239591	108695.731672	59.369204
2343.805470	108481.956858	59.374209
2343.091936	108282.898852	59.379213
2342.289214	108078.589953	59.384218
2341.840288	107865.324188	59.389223
2341.053827	107651.434873	59.394228
2341.080927	107432.659542	59.399233
2340.401140	107228.877652	59.404237
2339.381820	107019.986404	59.409242
2338.706390	106794.577052	59.414247
2337.576681	106577.483970	59.419252
2337.418570	106365.460665	59.424257
2336.783153	106152.772559	59.429261
2336.020332	105939.472056	59.434266
2335.647793	105721.441826	59.439271
2334.782519	105513.605160	59.444276
2334.047755	105282.883510	59.449281
2333.439470	105076.120212	59.454285
2332.862737	104862.292240	59.459290
2332.479846	104634.274593	59.464295
2331.654971	104420.413800	59.469300
2330.704301	104200.382789	59.474305
2330.080892	103999.645688	59.479309
2329.268721	103782.857559	59.484314
2328.699845	103559.669625	59.489319
2327.896774	103354.176627	59.494324
2327.497365	103132.418659	59.499329
2326.991494	102917.810322	59.504333
2326.075607	102702.793156	59.509338
2325.649251	102485.530723	59.514343
2324.968540	102267.010144	59.519348
2324.104478	102047.442230	59.524353
2323.858466	101833.297406	59.529357
2322.981865	101615.822610	59.534362
2322.395965	101398.430614	59.539367
2321.688317	101175.014556	59.544372
2321.087795	100957.857350	59.549377
2320.227482	100742.684450	59.554381
2319.271305	100523.633919	59.559386
2319.307203	100298.452756	59.564391
2318.485160	100087.980237	59.569396
2317.806871	99856.465536	59.574401
2316.957673	99651.437396	59.579405
2316.205076	99440.414248	59.584410
2315.981044	99214.308013	59.589415
2314.962162	98998.840285	59.594420
2314.628834	98771.036792	59.599425
2313.917315	98546.676245	59.604429
2312.939133	98332.229505	59.609434
2312.236981	98113.745101	59.614439
2311.601834	97897.757498	59.619444
2311.068920	97679.764153	59.624449
2310.358642	97461.077965	59.629453
2309.712164	97237.214655	59.634458
2309.218778	97017.616725	59.639463
2308.335749	96803.803484	59.644468
2308.027479	96586.945613	59.649473
2307.377762	96365.507800	59.654477
2306.518614	96142.475426	59.659482
2305.992927	95909.815822	59.664487
2305.204067	95697.469444	59.669492
2304.507772	95475.832091	59.674497
2304.206167	95258.922463	59.679501
2303.358698	95035.778667	59.684506
2302.949621	94793.123690	59.689511
2301.620495	94583.023347	59.694516
2301.380863	94359.320593	59.699521
2300.743887	94136.811879	59.704525
2299.855963	93912.981744	59.709530
2299.579945	93681.764140	59.714535
2298.665056	93479.383095	59.719540
2298.269262	93241.695449	59.724545
2297.222974	93025.407464	59.729549
2296.446260	92794.760392	59.734554
2296.133971	92567.770655	59.739559
2295.042618	92352.758250	59.744564
2294.690779	92128.689831	59.749569
2293.899163	91900.603505	59.754573
2292.828355	91681.434703	59.759578
2292.591504	91458.572286	59.764583
2291.838491	91249.077862	59.769588
2291.272285	91026.563714	59.774593
2290.768097	90813.457823	59.779597
2290.088439	90585.557566	59.784602
2289.672275	90356.242000	59.789607
2288.570578	90137.581694	59.794612
2288.223311	89904.747322	59.799617
2287.731697	89680.757685	59.804621
2286.695040	89459.430917	59.809626
2286.247257	89236.700593	59.814631
2285.286745	89021.554211	59.819636
2284.783128	88798.234914	59.824641
2284.280472	88572.210584	59.829645
2283.475823	88343.947786	59.834650
2283.009406	88103.118889	59.839655
2282.117181	87893.551925	59.844660
2281.600853	87668.845178	59.849665
2280.850286	87450.130852	59.854669
2279.814608	87218.651644	59.859674
2279.470112	86986.684941	59.864679
2278.659852	86778.256925	59.869684
2278.384109	86551.748621	59.874689
2277.344607	86330.486001	59.879693
2276.907481	86108.591300	59.884698
2276.382787	85877.184973	59.889703
2275.207869	85658.175832	59.894708
2275.047545	85442.221940	59.899713
2274.419685	85209.292473	59.904718
2273.353971	84978.945204	59.909722
2273.271844	84760.399532	59.914727
2272.061913	84538.117584	59.919732
2271.739648	84306.341229	59.924737
2270.952721	84075.179880	59.929742
2270.205097	83858.390742	59.934746
2269.881532	83625.462074	59.939751
2268.830710	83407.698799	59.944756
2268.449624	83174.866620	59.949761
2267.711572	82947.360764	59.954766
2266.995032	82729.234566	59.959770
2266.551384	82513.539245	59.964775
2265.768506	82283.195495	59.969780
2265.099071	82055.726433	59.974785
2264.305942	81823.392872	59.979790
2263.527283	81605.472007	59.984794
2263.045763	81373.277825	59.989799
2262.271372	81153.288522	59.994804
2261.863354	80919.344842	59.999809
2261.070428	80696.137410	60.004814
2260.107365	80479.569441	60.009818
2259.433368	80246.543751	60.014823
2258.532631	80023.873974	60.019828
2258.292009	79801.253995	60.024833
2257.482740	79583.435202	60.029838
2257.058025	79367.306790	60.034842
2256.157322	79138.981041	60.039847
2255.199559	78917.580635	60.044852
2254.807134	78696.384450	60.049857
2253.844300	78470.160843	60.054862
2253.424302	78253.175195	60.059866
2253.100981	78034.383183	60.064871
2252.224928	77818.862215	60.069876
2251.548413	77594.117334	60.074881
2250.889393	77373.560648	60.079886
2250.401879	77159.315689	60.084890
2250.125427	76922.760433	60.089895
2249.403583	76690.314846	60.094900
2248.512138	76469.982200	60.099905
2247.815523	76248.803660	60.104910
2247.131541	76024.146949	60.109914
2246.897321	75800.023322	60.114919
2245.820247	75569.775821	60.119924
2245.130386	75342.149646	60.124929
2244.340593	75116.271585	60.129934
2243.759495	74902.344033	60.134938
2243.101579	74667.668587	60.139943
2242.349287	74441.354958	60.144948
2241.665684	74216.806954	60.149953
2240.934296	73995.158050	60.154958
2240.198562	73779.473980	60.159962
2239.897688	73558.686592	60.164967
2239.323700	73332.148099	60.169972
2238.735282	73108.066211	60.174977
2237.837216	72878.492632	60.179982
2236.916660	72656.704809	60.184986
2236.708015	72425.189903	60.189991
2235.858395	72204.897261	60.194996
2235.152091	71977.242145	60.200001
2234.352186	71754.279601	60.205006
2233.599748	71546.445831	60.210010
2233.154643	71315.044686	60.215015
2232.362720	71095.040256	60.220020
2231.860212	70872.977972	60.225025
2230.977265	70650.015675	60.230030
2230.271696	70428.186961	60.235034
2229.986659	70196.608808	60.240039
2228.964353	69980.067546	60.245044
2228.462396	69747.179873	60.250049
2227.964171	69541.828872	60.255054
2226.945801	69316.223799	60.260058
2226.438739	69079.816764	60.265063
2225.471939	68878.157401	60.270068
2224.994399	68647.122074	60.275073
2224.476023	68434.761613	60.280078
2223.741286	68217.750824	60.285082
2222.964935	67992.420303	60.290087
2222.020415	67780.843912	60.295092
2221.339262	67559.056437	60.300097
2220.489814	67348.711029	60.305102
2220.225620	67142.581757	60.310106
2219.933095	66921.151584	60.315111
2218.799226	66716.013443	60.320116
2218.421348	66483.040504	60.325121
2218.103723	66269.598359	60.330126
2216.951321	66050.622930	60.335130
2216.627042	65812.209511	60.340135
2215.698827	65602.310367	60.345140
2214.761917	65388.067426	60.350145
2214.474852	65175.924414	60.355150
2213.774988	64958.149830	60.360154
2213.291235	64735.369193	60.365159
2212.083672	64524.921355	60.370164
2211.727663	64295.796218	60.375169
2210.698976	64093.572741	60.380174
2210.022199	63880.923281	60.385178
2209.903524	63658.458198	60.390183
2209.029773	63441.880895	60.395188
2208.389514	63224.629476	60.400193
2207.679109	63015.376321	60.405198
2206.697415	62795.223744	60.410202
2206.522344	62576.832666	60.415207
2205.702125	62373.720572	60.420212
2205.119991	62154.825886	60.425217
2204.130538	61932.693215	60.430222
2203.846888	61726.701189	60.435226
2203.547057	61508.918369	60.440231
2202.444371	61288.096525	60.445236
2201.838109	61071.985029	60.450241
2201.345644	60846.221742	60.455246
2200.334516	60638.204345	60.460250
2199.771225	60416.474600	60.465255
2198.944107	60208.246002	60.470260
2198.652205	59980.979813	60.475265
2197.996742	59769.965370	60.480270
2197.220361	59559.377657	60.485274
2196.827923	59333.585027	60.490279
2195.511515	59118.064474	60.495284
2194.951777	58894.123765	60.500289
2194.236972	58687.299668	60.505294
2193.683071	58479.566073	60.510298
2193.271672	58266.250922	60.515303
2192.273869	58052.556457	60.520308
2191.584001	57837.397625	60.525313
2191.136778	57623.291588	60.530318
2190.367366	57413.489806	60.535322
2189.714285	57205.206983	60.540327
2188.864454	56987.696954	60.545332
2188.444661	56773.988839	60.550337
2187.574543	56567.826994	60.555342
2186.698717	56365.944113	60.560346
2186.355318	56151.674064	60.565351
2185.145433	55945.196461	60.570356
2184.368293	55735.902343	60.575361
2183.874993	55530.948745	60.580366
2183.163318	55343.909489	60.585370
2182.441479	55134.721048	60.590375
2181.793898	54933.830380	60.595380
2180.988229	54728.368829	60.600385
2180.230513	54532.253267	60.605390
2179.505040	54344.251722	60.610394
2179.129616	54142.244304	60.615399
2178.210658	53953.242687	60.620404
2177.549441	53751.145698	60.625409
2176.861297	53564.193697	60.630414
2175.945052	53364.850176	60.635418
2175.586472	53178.027069	60.640423
2174.747482	52982.441042	60.645428
2174.316587	52789.406067	60.650433
2173.595504	52594.188398	60.655438
2173.029761	52415.838671	60.660442
2172.416968	52201.132431	60.665447
2171.484582	52014.412337	60.670452
2170.640597	51830.198770	60.675457
2170.165368	51646.786047	60.680462
2169.193048	51450.503668	60.685466
2168.710787	51253.974832	60.690471
2168.058042	51077.936526	60.695476
2167.260042	50891.054879	60.700481
2166.801053	50709.344992	60.705486
2165.507375	50526.260191	60.710490
2165.120988	50338.448935	60.715495
2164.412081	50159.922780	60.720500
2163.965491	49979.474348	60.725505
2163.037888	49796.253513	60.730510
2162.414904	49627.744923	60.735514
2161.526505	49442.091771	60.740519
2160.669017	49273.446559	60.745524
2160.303398	49093.623790	60.750529
2159.206340	48917.503206	60.755534
2158.466501	48752.735464	60.760538
2157.742963	48578.922150	60.765543
2157.082279	48415.014947	60.770548
2156.021693	48252.517169	60.775553
2155.860395	48089.175933	60.780558
2155.068081	47930.108836	60.785562
2154.492131	47762.996007	60.790567
2153.729161	47605.164053	60.795572
2152.730273	47445.599472	60.800577
2151.936829	47293.282475	60.805582
2151.413750	47134.945328	60.810586
2151.097552	46981.669591	60.815591
2149.984511	46821.764982	60.820596
2149.157311	46673.691058	60.825601
2148.493642	46521.268403	60.830606
2147.736382	46364.857395	60.835610
2147.146774	46217.872520	60.840615
2145.833152	46073.470933	60.845620
2145.402727	45928.098536	60.850625
2145.078168	45781.261882	60.855630
2143.898687	45655.156359	60.860634
2143.418655	45514.878193	60.865639
2142.728028	45381.450713	60.870644
2142.125312	45234.969566	60.875649
2141.192712	45099.011170	60.880654
2140.697124	44972.934904	60.885658
2140.211736	44830.154910	60.890663
2139.262732	44695.296601	60.895668
2138.811667	44554.332039	60.900673
2138.149376	44424.943094	60.905678
2137.179361	44292.536058	60.910682
2136.387665	44151.499118	60.915687
2135.751973	44029.380000	60.920692
2135.007888	43903.815797	60.925697
2134.288071	43773.397131	60.930702
2133.616818	43651.994738	60.935706
2133.037265	43518.668243	60.940711
2132.331413	43400.271254	60.945716
2131.275690	43263.903945	60.950721
2131.029916	43137.288989	60.955726
2130.344274	43022.699072	60.960730
2129.616009	42901.371061	60.965735
2129.182907	42770.791101	60.970740
2128.376566	42663.287682	60.975745
2127.757658	42539.579339	60.980750
2126.949370	42415.645770	60.985754
2126.477403	42287.659311	60.990759
2125.428681	42168.917188	60.995764
2124.957715	42056.317202	61.000769
2124.460781	41933.640580	61.005774
2123.635299	41809.514864	61.010778
2122.855373	41680.813323	61.015783
2122.564557	41564.918167	61.020788
2121.890372	41444.306479	61.025793
2121.123325	41328.640257	61.030798
2120.313942	41215.818016	61.035802
2119.954213	41092.363527	61.040807
2118.926154	40971.175705	61.045812
2118.267847	40854.689073	61.050817
2117.845616	40733.356218	61.055822
2117.038541	40627.705961	61.060826
2116.634922	40506.330650	61.065831
2115.489758	40396.836637	61.070836
2115.189983	40269.524026	61.075841
2114.576989	40156.981142	61.080846
2113.909396	40043.340969	61.085850
2113.427730	39917.623428	61.090855
2112.534724	39803.339213	61.095860
2111.921848	39683.131746	61.100865
2111.360790	39568.869157	61.105870
2110.752535	39447.299844	61.110874
2110.089078	39327.425417	61.115879
2109.192630	39207.759537	61.120884
2108.760480	39095.251868	61.125889
2107.834700	38975.628634	61.130894
2106.991318	38859.407864	61.135898
2106.768087	38738.138217	61.140903
2105.720826	38634.327945	61.145908
2105.443457	38525.655193	61.150913
2104.872255	38393.031084	61.155918
2103.924162	38276.609595	61.160922
2103.672686	38157.485845	61.165927
2102.759597	38042.464171	61.170932
2102.055463	37935.499037	61.175937
2101.494082	37807.411659	61.180942
2100.736215	37699.304152	61.185946
2100.203666	37572.579761	61.190951
2099.189105	37461.844599	61.195956
2098.414935	37357.818611	61.200961
2098.208325	37226.407211	61.205966
2097.331209	37111.986830	61.210970
2096.783673	36997.984402	61.215975
2095.893961	36897.661043	61.220980
2095.678096	36781.531998	61.225985
2095.257649	36660.128310	61.230990
2094.279101	36544.929630	61.235994
2093.476463	36424.038773	61.240999
2092.912913	36314.938780	61.246004
2092.287815	36185.885907	61.251009
2091.737394	36061.907019	61.256014
2091.045412	35955.393496	61.261018
2090.168834	35840.237205	61.266023
2089.611619	35732.820156	61.271028
2088.934012	35612.677138	61.276033
2088.482973	35496.384055	61.281038
2087.570638	35384.144805	61.286042
2087.125877	35262.100718	61.291047
2086.227044	35151.936133	61.296052
2085.520279	35033.470933	61.301057
2084.914647	34913.762469	61.306062
2083.891070	34803.120534	61.311066
2083.658439	34688.043840	61.316071
2082.996723	34577.647854	61.321076
2082.526865	34461.760062	61.326081
2081.813842	34347.182343	61.331086
2081.065978	34234.113943	61.336090
2080.595017	34106.151040	61.341095
2079.666742	33989.384685	61.346100
2078.999360	33881.353774	61.351105
2078.479028	33764.415218	61.356110
2077.706919	33654.967390	61.361114
2077.026348	33542.545707	61.366119
2076.074629	33423.817889	61.371124
2075.490288	33308.823902	61.376129
2075.019939	33191.225597	61.381134
2074.001890	33088.593887	61.386138
2073.501221	32966.913653	61.391143
2072.976606	32865.259106	61.396148
2072.051559	32752.445398	61.401153
2071.759088	32641.774520	61.406158
2071.042826	32535.327770	61.411162
2070.702385	32411.042427	61.416167
2069.795044	32302.696401	61.421172
2069.267806	32189.406218	61.426177
2068.752092	32063.664279	61.431182
2067.782529	31952.059332	61.436186
2067.189665	31831.906443	61.441191
2066.675712	31723.520756	61.446196
2065.610005	31605.653672	61.451201
2065.136954	31493.462639	61.456206
2064.113092	31389.132645	61.461210
2063.765637	31280.510127	61.466215
2062.951817	31174.996221	61.471220
2062.627177	31052.447281	61.476225
2061.765559	30930.570688	61.481230
2061.132384	30822.766050	61.486234
2060.628932	30711.642267	61.491239
2059.566605	30599.990100	61.496244
2058.656037	30495.407626	61.501249
2058.089505	30384.828554	61.506254
2057.615189	30280.228789	61.511258
2057.038949	30169.358816	61.516263
2056.465876	30064.949901	61.521268
2055.991640	29955.239165	61.526273
2055.368919	29838.520033	61.531278
2054.383171	29726.586742	61.536282
2054.167164	29610.188642	61.541287
2053.111280	29496.362573	61.546292
2052.475687	29389.164984	61.551297
2052.044994	29274.157387	61.556302
2051.304924	29166.445388	61.561306
2050.720574	29048.526617	61.566311
2049.830168	28954.139889	61.571316
2049.146395	28841.810837	61.576321
2048.775532	28712.453538	61.581326
2047.897696	28610.296782	61.586330
2047.425445	28495.756280	61.591335
2046.605133	28387.739861	61.596340
2046.053981	28278.957867	61.601345
2045.299370	28153.942619	61.606350
2044.508350	28056.589404	61.611354
2044.053497	27934.466803	61.616359
2043.142167	27829.964724	61.621364
2042.234410	27711.304408	61.626369
2041.936871	27608.439415	61.631374
2040.898526	27501.961148	61.636378
2040.736894	27395.131185	61.641383
2040.067655	27285.869050	61.646388
2039.125427	27186.962115	61.651393
2038.565635	27069.440847	61.656398
2037.661670	26972.597052	61.661402
2037.267440	26847.444643	61.666407
2036.403449	26755.071198	61.671412
2035.572927	26638.255561	61.676417
2035.195785	26532.237971	61.681422
2034.247229	26437.973848	61.686426
2033.865294	26321.093268	61.691431
2032.917732	26230.339468	61.696436
2032.120893	26126.920993	61.701441
2031.568372	26020.940912	61.706446
2030.750312	25927.180355	61.711450
2030.375191	25815.623392	61.716455
2029.347334	25725.285620	61.721460
2028.815521	25621.083543	61.726465
2028.510683	25514.953755	61.731470
2027.499516	25416.855264	61.736474
2027.026176	25298.465194	61.741479
2026.281469	25206.139361	61.746484
2025.546411	25116.080784	61.751489
2025.115023	25014.784948	61.756494
2024.077000	24915.533602	61.761498
2023.591382	24820.770332	61.766503
2023.149730	24725.034764	61.771508
2022.380192	24632.233632	61.776513
2021.698640	24515.527449	61.781518
2020.527024	24426.815899	61.786522
2020.121331	24320.373584	61.791527
2019.535597	24232.920594	61.796532
2018.846968	24129.462280	61.801537
2018.009016	24039.714341	61.806542
2017.235826	23948.744400	61.811546
2016.510155	23853.920709	61.816551
2015.924650	23762.394512	61.821556
2014.726318	23670.484373	61.826561
2014.426731	23583.964029	61.831566
2013.727461	23502.297132	61.836570
2013.147793	23401.324079	61.841575
2012.770384	23313.327394	61.846580
2011.821157	23223.464303	61.851585
2011.156485	23134.404683	61.856590
2010.255505	23044.593383	61.861594
2009.960381	22963.830100	61.866599
2009.003811	22885.123480	61.871604
2008.059901	22800.372699	61.876609
2008.145505	22715.954893	61.881614
2007.032858	22624.345172	61.886618
2006.209533	22535.682067	61.891623
2005.653182	22453.815465	61.896628
2004.764086	22365.433811	61.901633
2004.315731	22285.588225	61.906638
2003.727412	22207.790677	61.911642
2003.381204	22118.195059	61.916647
2002.523958	22037.211425	61.921652
2001.346509	21950.728742	61.926657
2001.091087	21861.724230	61.931662
2000.633980	21787.034037	61.936666
2000.185948	21700.471703	61.941671
1999.474368	21606.951785	61.946676
1998.550602	21533.664972	61.951681
1998.076940	21438.444594	61.956686
1997.044650	21354.595984	61.961690
1996.662490	21270.752813	61.966695
1995.867794	21185.067916	61.971700
1995.122112	21105.753962	61.976705
1994.515461	21012.673342	61.981710
1993.832408	20944.730467	61.986714
1993.154567	20855.146473	61.991719
1992.550127	20771.856821	61.996724
1991.777753	20698.013750	62.001729
1991.419653	20605.867248	62.006734
1990.365690	20541.812760	62.011738
1989.663143	20451.567020	62.016743
1989.069545	20374.373875	62.021748
1988.698323	20296.496810	62.026753
1988.069294	20211.120949	62.031758
1987.260658	20135.389803	62.036762
1986.205309	20047.236615	62.041767
1985.620547	19968.556585	62.046772
1985.035167	19880.191973	62.051777
1984.313573	19803.851734	62.056782
1983.564051	19744.209017	62.061786
1983.199390	19661.415773	62.066791
1982.360043	19587.265644	62.071796
1981.639421	19508.850677	62.076801
1981.107980	19426.282915	62.081806
1980.613457	19362.149983	62.086810
1979.865105	19267.020683	62.091815
1979.198644	19200.930919	62.096820
1978.497534	19119.227773	62.101825
1978.012981	19036.880809	62.106830
1977.239346	18962.583867	62.111834
1976.358647	18880.531918	62.116839
1976.061416	18797.470037	62.121844
1974.943861	18725.593266	62.126849
1974.189793	18642.299984	62.131854
1973.591281	18578.289402	62.136858
1973.007769	18516.552302	62.141863
1972.543784	18446.818684	62.146868
1971.929458	18366.160802	62.151873
1971.088767	18282.912003	62.156878
1970.486845	18214.091809	62.161882
1969.816060	18132.132447	62.166887
1969.243215	18063.008320	62.171892
1968.854166	17986.614308	62.176897
1967.954887	17898.432682	62.181902
1967.273899	17828.203019	62.186906
1966.578568	17743.468476	62.191911
1965.939466	17673.524947	62.196916
1965.159074	17597.079311	62.201921
1964.725496	17521.312756	62.206926
1963.981064	17449.132419	62.211930
1963.044457	17381.941906	62.216935
1962.483256	17306.469785	62.221940
1961.601707	17235.856650	62.226945
1961.176055	17150.599035	62.231950
1960.057649	17093.327646	62.236954
1960.166144	17010.451653	62.241959
1959.246754	16945.960757	62.246964
1958.301883	16863.850296	62.251969
1958.189107	16778.814040	62.256974
1957.314485	16725.244546	62.261978
1956.648379	16644.425024	62.266983
1956.219205	16569.529131	62.271988
1955.480501	16489.370397	62.276993
1954.828384	16429.234734	62.281998
1954.057297	16354.414674	62.287002
1953.463860	16276.611885	62.292007
1952.488379	16209.704163	62.297012
1951.817751	16137.025284	62.302017
1951.337814	16057.842797	62.307022
1950.604790	15979.117847	62.312026
1949.834482	15916.277402	62.317031
1949.068805	15838.929796	62.322036
1948.687800	15771.065710	62.327041
1947.926813	15698.493613	62.332046
1947.080590	15634.488518	62.337050
1946.551430	15564.935859	62.342055
1945.885095	15490.173215	62.347060
1945.093964	15428.936592	62.352065
1944.747680	15360.965794	62.357070
1943.850399	15296.880621	62.362074
1943.172405	15214.189001	62.367079
1942.746302	15151.580393	62.372084
1942.137912	15085.268669	62.377089
1941.672922	15009.737435	62.382094
1941.155792	14938.235891	62.387098
1940.332787	14861.610664	62.392103
1939.519137	14778.942323	62.397108
1938.583936	14711.764297	62.402113
1938.125778	14640.895950	62.407118
1937.413361	14564.174938	62.412122
1936.756990	14500.004732	62.417127
1936.043209	14422.239483	62.422132
1935.095130	14361.491664	62.427137
1934.519202	14282.910473	62.432142
1933.845023	14223.877059	62.437146
1933.333026	14158.392500	62.442151
1932.565921	14090.230710	62.447156
1931.337557	14030.633022	62.452161
1931.130525	13954.769281	62.457166
1930.529420	13899.994538	62.462170
1929.757752	13828.775331	62.467175
1929.232813	13766.058333	62.472180
1928.751583	13696.465485	62.477185
1928.266873	13630.898646	62.482190
1927.488605	13562.829763	62.487194
1926.556323	13498.233043	62.492199
1926.092080	13419.159907	62.497204
1925.507155	13349.900181	62.502209
1924.880777	13284.106848	62.507214
1923.836541	13222.371816	62.512218
1923.221420	13159.525031	62.517223
1923.047625	13095.169854	62.522228
1922.059396	13027.933753	62.527233
1921.322927	12952.185360	62.532238
1920.524499	12882.868029	62.537242
1920.093302	12816.226871	62.542247
1919.326585	12754.469314	62.547252
1918.450303	12693.189576	62.552257
1918.119804	12620.782905	62.557262
1917.351985	12558.214083	62.562266
1916.900696	12492.673065	62.567271
1916.080627	12415.583970	62.572276
1915.248601	12362.241156	62.577281
1915.016174	12301.163919	62.582286
1914.145482	12237.080641	62.587290
1913.525257	12162.673748	62.592295
1912.826830	12096.822109	62.597300
1912.014806	12036.940543	62.602305
1911.675317	11963.192183	62.607310
1910.736707	11900.859336	62.612314
1910.010537	11828.344651	62.617319
1909.722317	11769.367972	62.622324
1908.900035	11698.200589	62.627329
1908.650268	11625.938329	62.632334
1907.251800	11568.319171	62.637338
1906.798213	11493.824592	62.642343
1906.546629	11434.316481	62.647348
1905.508385	11359.977905	62.652353
1905.200433	11294.688970	62.657358
1904.377794	11242.843324	62.662362
1903.690623	11158.138499	62.667367
1903.029403	11108.447711	62.672372
1902.037855	11028.981865	62.677377
1901.450712	10967.000282	62.682382
1901.016207	10900.475756	62.687386
1900.121717	10833.869099	62.692391
1899.792806	10771.625992	62.697396
1898.858538	10710.961870	62.702401
1898.155249	10636.984378	62.707406
1897.576540	10580.987980	62.712410
1896.750696	10513.460884	62.717415
1896.292828	10458.626954	62.722420
1895.390533	10392.652742	62.727425
1894.977583	10317.859833	62.732430
1894.273773	10272.184083	62.737434
1893.915563	10200.021388	62.742439
1893.514785	10136.771697	62.747444
1892.937952	10066.099110	62.752449
1891.890735	9991.156811	62.757454
1891.153884	9934.363791	62.762458
1890.273901	9856.496386	62.767463
1889.810762	9788.449837	62.772468
1889.021040	9737.464353	62.777473
1888.411981	9651.948225	62.782478
1887.628316	9591.796880	62.787482
1887.024419	9531.569503	62.792487
1886.634020	9458.873230	62.797492
1885.638550	9397.407117	62.802497
1884.952146	9331.055341	62.807502
1883.986710	9264.070818	62.812506
1883.542012	9197.470998	62.817511
1882.648184	9139.411193	62.822516
1881.838966	9086.179686	62.827521
1881.572470	9015.000037	62.832526
1880.728772	8947.825604	62.837530
1879.994023	8896.062646	62.842535
1879.702706	8830.647602	62.847540
1879.012149	8783.751787	62.852545
1878.468465	8714.160364	62.857550
1877.665294	8649.309023	62.862554
1877.037190	8588.361864	62.867559
1876.518172	8529.494635	62.872564
1875.451725	8466.402615	62.877569
1875.004531	8392.391555	62.882574
1874.292302	8342.775196	62.887578
1873.738854	8281.763784	62.892583
1872.914601	8221.423991	62.897588
1872.286490	8160.522359	62.902593
1872.138479	8092.816876	62.907598
1871.169597	8031.821552	62.912602
1870.544389	7967.781553	62.917607
1869.918010	7897.404337	62.922612
1869.036170	7830.063472	62.927617
1868.633847	7778.645660	62.932622
1867.670560	7719.202491	62.937626
1867.172814	7646.896509	62.942631
1866.565620	7583.692311	62.947636
1865.773502	7527.807839	62.952641
1865.452730	7459.618687	62.957646
1864.666575	7400.329716	62.962650
1863.939265	7336.183992	62.967655
1863.537664	7269.957853	62.972660
1862.605515	7206.477884	62.977665
1862.532429	7138.289531	62.982670
1861.237557	7075.550864	62.987674
1860.248190	7010.123648	62.992679
1859.728145	6946.674023	62.997684
1859.224018	6890.328521	63.002689
1858.823541	6824.295873	63.007694
1857.957730	6768.373886	63.012698
1857.227859	6701.923135	63.017703
1856.674386	6627.326732	63.022708
1855.857669	6569.468199	63.027713
1855.418032	6515.958812	63.032718
1854.703432	6446.995131	63.037722
1853.810382	6388.680068	63.042727
1853.418245	6329.394336	63.047732
1852.434264	6272.130681	63.052737
1852.129529	6199.676442	63.057742
1851.167588	6146.495842	63.062746
1850.729737	6082.188091	63.067751
1850.177714	6026.666334	63.072756
1849.206207	5962.402022	63.077761
1848.669362	5894.507546	63.082766
1848.027066	5826.558342	63.087770
1847.207389	5773.892086	63.092775
1846.500027	5710.888437	63.097780
1845.912117	5644.837149	63.102785
1845.631116	5583.272932	63.107790
1844.670013	5532.016672	63.112794
1844.004217	5462.868399	63.117799
1843.455838	5402.493478	63.122804
1842.339116	5351.055895	63.127809
1842.022632	5287.078592	63.132814
1841.557975	5226.600388	63.137818
1840.807686	5168.127064	63.142823
1840.337142	5109.708151	63.147828
1839.768104	5040.079545	63.152833
1838.992753	4967.153128	63.157838
1838.128196	4908.281726	63.162842
1837.453826	4840.940798	63.167847
1836.946778	4786.033350	63.172852
1836.181555	4714.643040	63.177857
1835.292271	4648.317513	63.182862
1834.675107	4591.084946	63.187866
1834.192794	4529.307837	63.192871
1833.382792	4467.732083	63.197876
1832.586277	4422.562216	63.202881
1832.515354	4349.261996	63.207886
1831.430588	4300.736530	63.212890
1830.716728	4233.976460	63.217895
1830.295020	4173.409779	63.222900
1829.254753	4114.920419	63.227905
1828.466895	4052.301007	63.232910
1827.978966	3994.699263	63.237914
1827.211955	3933.590560	63.242919
1826.499997	3882.086743	63.247924
1825.997404	3825.489630	63.252929
1825.395064	3755.853445	63.257934
1824.906226	3700.271246	63.262938
1824.078672	3651.020144	63.267943
1823.574007	3580.098717	63.272948
1822.867549	3529.031403	63.277953
1822.230061	3467.103569	63.282958
1821.151089	3416.169141	63.287962
1820.625950	3355.686918	63.292967
1819.782733	3301.494550	63.297972
1818.778737	3246.226943	63.302977
1818.642508	3188.873781	63.307982
1817.905042	3147.999788	63.312986
1817.167818	3088.041307	63.317991
1816.856801	3033.981515	63.322996
1815.855467	2986.573340	63.328001
1815.498980	2915.898942	63.333006
1814.946712	2859.730629	63.338010
1814.253387	2796.325543	63.343015
1813.628117	2728.435232	63.348020
1812.632996	2682.884281	63.353025
1811.819152	2614.227139	63.358030
1810.877754	2574.059038	63.363034
1810.561784	2525.030957	63.368039
1810.111257	2463.294547	63.373044
1809.392682	2415.717148	63.378049
1809.220851	2373.002417	63.383054
1808.301804	2312.104414	63.388058
1807.609448	2249.781937	63.393063
1807.058128	2186.611664	63.398068
1806.266800	2126.956705	63.403073
1805.781872	2076.172356	63.408078
1805.007449	2020.251517	63.413082
1804.075316	1966.118433	63.418087
1803.371631	1907.888842	63.423092
1802.260795	1853.663109	63.428097
1802.149042	1791.087160	63.433102
1801.015873	1749.493697	63.438106
1800.640540	1700.574801	63.443111
1800.391145	1647.455057	63.448116
1799.359180	1602.958190	63.453121
1799.139770	1534.993205	63.458126
1798.257836	1483.501951	63.463130
1797.501032	1441.520777	63.468135
1796.770666	1375.090989	63.473140
1796.045088	1327.000959	63.478145
1795.438061	1275.913899	63.483150
1794.474554	1224.486194	63.488154
1793.968074	1172.097408	63.493159
1793.271149	1119.934609	63.498164
1792.502974	1070.886224	63.503169
1792.079807	1023.959587	63.508174
1791.617732	970.458155	63.513178
1790.921218	922.059686	63.518183
1790.221866	856.749423	63.523188
1789.243945	817.232260	63.528193
1788.568906	765.646826	63.533198
1788.011244	715.954315	63.538202
1787.035104	662.530914	63.543207
1786.523410	618.710640	63.548212
1785.464365	581.706603	63.553217
1785.139714	525.336870	63.558222
1784.521863	489.478895	63.563226
1783.492244	444.733674	63.568231
1782.714204	400.732417	63.573236
1782.101640	366.865672	63.578241
1781.468464	323.672729	63.583246
1781.037243	302.108716	63.588250
1780.663262	266.832329	63.593255
1779.911021	213.720392	63.598260
1778.815607	170.744812	63.603265
1778.226768	132.784146	63.608270
1777.226464	104.223054	63.613274
1776.406246	72.389582	63.618279
1775.600010	36.228328	63.623284
1774.231774	19.163609	63.628289
1773.648312	-3.201315	63.633294
1772.595543	-1.515489	63.638298
1771.477311	-6.710614	63.643303
1768.896861	42.728741	63.648308
1767.611104	68.642345	63.653313
1767.787636	54.784279	63.658318
1768.149601	66.339664	63.663322
1767.862699	67.653141	63.668327
1768.193736	53.688537	63.673332
1767.727242	61.921907	63.678337
1766.554054	61.430140	63.683342
1765.377031	68.634616	63.688346
1764.575317	65.652164	63.693351
1763.927284	61.314343	63.698356
1762.969409	72.822277	63.703361
1762.758734	69.096254	63.708366
1762.413207	65.659732	63.713370
1761.461873	71.639333	63.718375
1760.680914	69.063599	63.723380
1760.295121	78.599360	63.728385
1760.290819	72.293748	63.733390
1759.431124	65.483726	63.738394
1758.544107	65.138908	63.743399
1757.922011	69.587023	63.748404
1756.488570	71.087307	63.753409
1755.799213	70.769449	63.758414
1755.981508	64.380591	63.763418
1755.453588	67.785564	63.768423
1755.368232	70.110992	63.773428
1754.027919	65.313822	63.778433
1753.373498	66.983712	63.783438
1752.548162	61.835100	63.788442
1751.841254	64.427969	63.793447
1751.325818	67.034589	63.798452
1750.144023	76.666796	63.803457
1749.280665	77.371643	63.808462
1749.077686	73.245424	63.813466
1748.649864	72.889188	63.818471
1748.276260	65.251335	63.823476
1747.345323	72.910333	63.828481
1746.506062	77.683105	63.833486
1745.819787	70.894431	63.838490
1744.628070	71.298183	63.843495
1744.750971	68.159439	63.848500
1744.182349	77.147062	63.853505
1744.027078	71.869960	63.858510
1743.461945	70.584615	63.863514
1741.806632	76.576673	63.868519
1741.204539	68.919913	63.873524
1740.990549	81.494031	63.878529
1740.558493	73.863881	63.883534
1739.939416	70.112831	63.888538
1738.771175	75.570216	63.893543
1738.431124	77.024603	63.898548
1737.403660	71.952248	63.903553
1736.651194	83.172105	63.908558
1736.112640	73.475686	63.913562
1735.411692	70.904600	63.918567
1734.695388	72.267351	63.923572
1733.745178	81.186266	63.928577
1733.030705	76.043704	63.933582
1732.950555	76.116388	63.938586
1732.764887	73.245847	63.943591
1732.246493	72.951307	63.948596
1730.801281	76.454655	63.953601
1730.027042	75.178867	63.958606
1729.273131	69.309279	63.963610
1729.465477	69.474306	63.968615
1728.845223	68.202449	63.973620
1727.458167	78.461784	63.978625
1726.783769	85.630614	63.983630
1726.812702	73.885467	63.988634
1725.825947	70.885106	63.993639
1724.972797	77.554034	63.998644
1724.028554	75.034206	64.003649
1723.976110	69.939475	64.008654
1723.469273	75.261861	64.013658
1722.514185	76.714579	64.018663
1721.506843	66.901806	64.023668
1720.478426	72.188754	64.028673
1720.871555	71.897686	64.033678
1720.352495	76.419334	64.038682
1719.327563	75.815731	64.043687
1718.302807	76.828500	64.048692
1717.448023	81.048650	64.053697
1717.357383	65.840541	64.058702
1716.567521	67.137707	64.063706
1715.656833	74.989043	64.068711
1715.775979	71.265837	64.073716
1714.565595	77.250326	64.078721
1713.650173	76.700297	64.083726
1713.131111	75.027591	64.088730
1711.956602	80.954345	64.093735
1712.402462	67.472972	64.098740
1712.249355	77.681417	64.103745
1710.791494	71.963061	64.108750
1710.087525	82.888211	64.113754
1709.262192	79.983644	64.118759
1708.762334	70.445094	64.123764
1708.016877	76.261127	64.128769
1707.793665	74.189769	64.133774
1707.082724	78.861745	64.138778
1705.969684	77.176144	64.143783
1705.111526	73.522999	64.148788
1704.515079	76.880518	64.153793
1704.434472	71.432288	64.158798
1703.334543	80.474339	64.163802
1702.205053	76.315502	64.168807
1702.221014	77.358530	64.173812
1701.308967	71.813692	64.178817
1700.505995	76.892952	64.183822
1700.363493	74.794584	64.188826
1699.573142	74.478588	64.193831
1698.921722	61.999408	64.198836
1697.960109	77.950289	64.203841
1697.281174	74.740197	64.208846
1696.806519	76.971337	64.213850
1696.025371	83.947390	64.218855
1695.926180	74.857721	64.223860
1695.052875	76.781590	64.228865
1694.423132	74.520909	64.233870
1694.322306	74.147440	64.238874
1693.242261	78.125826	64.243879
1692.341264	70.268969	64.248884
1691.080537	73.626340	64.253889
1690.597147	71.662541	64.258894
1690.115993	78.162007	64.263898
1689.566964	72.132156	64.268903
1688.824441	71.158854	64.273908
1688.293663	74.277284	64.278913
1687.832778	71.904629	64.283918
1687.285784	66.546248	64.288922
1686.498554	74.084666	64.293927
1686.194448	62.422393	64.298932
1685.171017	77.375409	64.303937
1684.083022	74.794849	64.308942
1683.359866	71.336316	64.313946
1682.349612	84.439033	64.318951
1682.669512	73.338393	64.323956
1681.589028	76.244511	64.328961
1680.822846	73.139746	64.333966
1680.280726	71.663101	64.338970
1679.366225	78.155703	64.343975
1679.237214	71.860443	64.348980
1678.659249	82.298799	64.353985
1677.980256	76.821032	64.358990
1677.758309	75.399190	64.363994
1676.777380	74.684535	64.368999
1675.850659	73.535487	64.374004
1674.450843	73.967593	64.379009
1674.521618	74.889950	64.384014
1673.816673	73.842873	64.389018
1672.746898	82.448056	64.394023
1672.748326	73.080632	64.399028
1671.780901	81.265852	64.404033
1671.426605	78.977195	64.409038
1671.092100	79.752610	64.414042
1669.993569	88.931652	64.419047
1669.678349	81.070067	64.424052
1668.244289	72.995111	64.429057
1667.394264	77.936772	64.434062
1666.661704	71.395177	64.439066
1666.510355	81.505571	64.444071
1666.756693	72.067708	64.449076
1665.909385	76.024906	64.454081
1665.423389	75.021903	64.459086
1664.764108	79.054894	64.464090
1663.603017	80.836825	64.469095
1662.932485	73.870633	64.474100
1661.515882	77.483015	64.479105
1661.235652	78.361775	64.484110
1660.222172	67.905024	64.489114
1658.636563	78.848792	64.494119
1658.821215	81.175490	64.499124
1658.523936	81.708448	64.504129
1657.903118	71.156208	64.509134
1657.648321	67.804641	64.514138
1656.871431	73.638293	64.519143
1656.091184	68.976144	64.524148
1654.917968	78.014081	64.529153
1654.305448	73.618607	64.534158
1654.044481	70.895655	64.539162
1653.467163	70.530065	64.544167
1653.133807	64.016532	64.549172
1652.383381	71.561726	64.554177
1651.662537	69.206717	64.559182
1651.205610	71.616400	64.564186
1649.894008	70.306145	64.569191
1649.079734	67.382498	64.574196
1648.589167	70.896675	64.579201
1648.013657	69.695004	64.584206
1647.638348	71.278005	64.589210
1646.612877	77.266265	64.594215
1646.202078	69.659573	64.599220
1645.536907	68.410643	64.604225
1645.018434	62.478457	64.609230
1644.719657	61.582917	64.614234
1643.320716	69.254781	64.619239
1642.667091	61.131572	64.624244
1641.888511	64.037055	64.629249
1641.496119	64.720742	64.634254
1641.399237	68.402622	64.639258
1640.476709	76.833032	64.644263
1639.487246	69.486998	64.649268
1638.468290	66.315167	64.654273
1637.740557	62.035775	64.659278
1637.359099	67.989544	64.664282
1636.805527	74.762295	64.669287
1636.532558	58.479292	64.674292
1635.626760	70.284915	64.679297
1635.242844	65.632358	64.684302
1634.893104	65.306317	64.689306
1633.646394	70.009796	64.694311
1633.082939	62.477825	64.699316
1631.928192	69.998938	64.704321
1631.556978	65.442137	64.709326
1630.914874	72.359841	64.714330
1630.361070	64.561404	64.719335
1630.139311	59.225495	64.724340
1629.326840	58.104049	64.729345
1628.135208	62.959630	64.734350
1627.520724	63.585558	64.739354
1626.637915	74.307309	64.744359
1627.024677	64.572751	64.749364
1626.119572	64.197735	64.754369
1624.991643	74.182554	64.759374
1623.835926	69.557985	64.764378
1623.684364	71.329376	64.769383
1622.936749	71.732022	64.774388
1621.859252	64.559258	64.779393
1621.565224	77.111387	64.784398
1621.793333	68.999503	64.789402
1620.723544	74.471255	64.794407
1620.192306	69.941453	64.799412
1619.318291	70.523454	64.804417
1618.270030	74.570936	64.809422
1617.596473	77.499169	64.814426
1616.884562	70.602647	64.819431
1616.729227	63.141466	64.824436
1615.813740	72.363978	64.829441
1615.440152	74.583807	64.834446
1614.674792	68.902161	64.839450
1613.580808	78.078916	64.844455
1613.104863	72.087939	64.849460
1612.296332	71.998788	64.854465
1612.008883	67.756694	64.859470
1611.894260	64.065894	64.864474
1610.648194	63.732433	64.869479
1609.735440	65.755636	64.874484
1608.827657	64.619374	64.879489
1608.283755	73.735550	64.884494
1607.916074	65.787702	64.889498
1607.363054	76.881274	64.894503
1607.505165	57.551862	64.899508
1606.046557	61.439025	64.904513
1605.227286	67.711509	64.909518
1604.349421	64.293350	64.914522
1603.626390	70.605740	64.919527
1603.690274	54.491591	64.924532
1602.875510	60.810665	64.929537
1602.139469	62.539288	64.934542
1601.234101	63.425900	64.939546
1600.337141	68.409726	64.944551
1600.037801	63.522966	64.949556
1599.580743	61.394153	64.954561
1599.299862	74.661713	64.959566
1598.063312	65.684939	64.964570
1596.900809	69.804194	64.969575
1596.588678	58.755086	64.974580
1595.961973	65.637229	64.979585
1595.448407	71.242978	64.984590
1595.074658	56.336926	64.989594
1594.225542	73.022165	64.994599
1593.603413	62.392891	64.999604
1592.444820	60.017558	65.004609
1591.875573	62.757333	65.009614
1591.412235	65.819331	65.014618
1590.847911	64.846135	65.019623
1590.534285	63.561871	65.024628
1589.161716	60.119808	65.029633
1587.785002	64.225786	65.034638
1588.231721	65.071066	65.039642
1587.253448	66.871293	65.044647
1586.793840	61.189972	65.049652
1586.454706	64.292164	65.054657
1586.009899	61.738780	65.059662
1585.738689	67.870581	65.064666
1584.279421	73.095136	65.069671
1583.589084	64.298104	65.074676
1582.830286	78.223495	65.079681
1582.351424	71.200072	65.084686
1581.281964	64.779844	65.089690
1580.205270	68.707274	65.094695
1579.880681	67.244978	65.099700
1579.268132	62.759646	65.104705
1578.769108	63.870295	65.109710
1578.726034	64.604151	65.114714
1577.811014	76.600494	65.119719
1577.349497	60.148762	65.124724
1576.218065	61.687893	65.129729
1575.212834	64.575786	65.134734
1574.993513	64.404076	65.139738
1574.380081	72.504693	65.144743
1574.156644	57.382376	65.149748
1572.506049	64.166992	65.154753
1571.643397	71.029856	65.159758
1571.441652	57.943117	65.164762
1570.531538	73.169891	65.169767
1570.516175	66.815589	65.174772
1569.965341	70.452894	65.179777
1569.420874	66.314720	65.184782
1569.007032	58.050940	65.189786
1567.779824	62.112674	65.194791
1567.119870	60.367768	65.199796
1566.588515	62.549588	65.204801
1565.454982	61.792988	65.209806
1564.925137	54.219431	65.214810
1563.782472	68.565352	65.219815
1563.318200	57.603504	65.224820
1562.735377	62.395502	65.229825
1562.507058	59.061821	65.234830
1562.743609	56.712429	65.239834
1561.226085	67.687998	65.244839
1560.556465	60.073567	65.249844
1559.594924	68.585887	65.254849
1559.108928	61.275023	65.259854
1558.841904	54.910248	65.264858
1557.677591	64.746320	65.269863
1556.824299	61.300620	65.274868
1556.364529	63.489992	65.279873
1555.791049	64.760710	65.284878
1555.241555	53.992182	65.289882
1554.717492	66.998745	65.294887
1554.656252	67.230857	65.299892
1554.232268	65.677123	65.304897
1553.083234	68.617835	65.309902
1552.034200	61.487894	65.314906
1551.170349	67.239188	65.319911
1550.902914	63.389745	65.324916
1549.694446	69.198949	65.329921
1548.654884	70.184172	65.334926
1548.030892	64.549477	65.339930
1547.570193	58.844685	65.344935
1547.319916	53.928064	65.349940
1546.946204	59.100006	65.354945
1546.238523	59.412749	65.359950
1545.413910	59.345099	65.364954
1544.037226	70.895972	65.369959
1543.662091	53.938520	65.374964
1543.183591	63.388084	65.379969
1542.988981	62.606894	65.384974
1542.908681	64.313348	65.389978
1541.414283	71.718148	65.394983
1540.772370	65.250508	65.399988
1540.171920	65.740183	65.404993
1539.559538	57.522149	65.409998
1538.468063	64.386683	65.415002
1537.704112	67.789770	65.420007
1537.330877	63.553434	65.425012
1536.726179	64.893772	65.430017
1536.149998	59.163176	65.435022
1535.547719	65.566781	65.440026
1534.126337	72.098957	65.445031
1533.701904	60.728658	65.450036
1533.254470	68.635745	65.455041
1532.821668	64.963968	65.460046
1532.400184	58.475502	65.465050
1531.290344	67.085509	65.470055
1530.507823	56.943800	65.475060
1530.069476	62.933422	65.480065
1529.431225	65.945950	65.485070
1529.066121	60.637562	65.490074
1528.405668	68.641575	65.495079
1527.497620	65.575174	65.500084
1526.921854	67.369815	65.505089
1526.126656	62.147112	65.510094
1525.665435	54.226768	65.515098
1524.454444	64.805136	65.520103
1523.554825	58.972970	65.525108
1522.922501	61.770089	65.530113
1522.178409	65.731425	65.535118
1522.382759	52.893993	65.540122
1521.701617	65.506042	65.545127
1521.255458	67.177588	65.550132
1520.925830	59.849774	65.555137
1519.323358	68.151704	65.560142
1518.704938	64.859511	65.565146
1518.065247	69.509166	65.570151
1517.723527	54.352044	65.575156
1517.238266	52.998868	65.580161
1516.024243	59.558024	65.585166
1515.345152	59.765308	65.590170
1514.509999	65.970950	65.595175
1514.244113	64.862039	65.600180
1514.142619	66.939296	65.605185
1513.170899	69.545917	65.610190
1512.287474	55.479400	65.615194
1511.755975	65.662795	65.620199
1511.011178	57.700780	65.625204
1510.195433	56.961519	65.630209
1508.956460	64.667947	65.635214
1508.650796	59.067842	65.640218
1508.065388	65.621736	65.645223
1507.570992	59.474448	65.650228
1507.271221	52.424174	65.655233
1506.490554	65.212890	65.660238
1505.923505	52.682539	65.665242
1505.113096	60.096938	65.670247
1504.143452	55.291477	65.675252
1503.979847	57.440103	65.680257
1503.231518	57.382422	65.685262
1502.067809	57.644637	65.690266
1501.083872	62.692774	65.695271
1500.766318	60.809899	65.700276
1500.442795	61.742862	65.705281
1499.580279	65.320894	65.710286
1499.405342	55.997294	65.715290
1498.388324	63.239521	65.720295
1497.626712	54.081688	65.725300
1496.763018	61.337398	65.730305
1496.228000	56.387182	65.735310
1496.595114	55.966172	65.740314
1495.399567	60.956472	65.745319
1494.613608	63.800088	65.750324
1493.943344	58.883978	65.755329
1493.072873	68.345372	65.760334
1492.115461	64.436842	65.765338
1491.070137	70.429882	65.770343
1490.553322	66.579073	65.775348
1490.421435	73.628616	65.780353
1489.772877	63.255894	65.785358
1488.764970	53.684612	65.790362
1487.846005	58.824930	65.795367
1487.357122	60.000216	65.800372
1486.884301	61.751698	65.805377
1486.232018	66.389167	65.810382
1486.061560	65.250902	65.815386
1485.348528	72.886384	65.820391
1484.922167	57.810528	65.825396
1484.146685	47.979965	65.830401
1483.176347	61.257719	65.835406
1482.896608	55.071598	65.840410
1481.912960	56.147310	65.845415
1481.556194	50.222593	65.850420
1480.555097	52.217296	65.855425
1479.856533	54.162348	65.860430
1478.851241	59.417313	65.865434
1477.592557	65.641382	65.870439
1477.711066	52.625204	65.875444
1477.016434	58.598785	65.880449
1476.707758	54.554057	65.885454
1476.557770	48.571250	65.890458
1475.714653	55.356911	65.895463
1474.720137	49.932514	65.900468
1473.957055	53.157278	65.905473
1473.386831	61.205306	65.910478
1473.154052	53.016859	65.915482
1471.541935	56.198350	65.920487
1470.978678	54.949043	65.925492
1469.931634	56.310803	65.930497
1469.651020	66.435410	65.935502
1469.440135	54.349948	65.940506
1468.883250	64.630422	65.945511
1468.482351	58.375246	65.950516
1467.743221	54.626007	65.955521
1466.380990	60.354019	65.960526
1466.128263	58.123376	65.965530
1465.740992	59.252556	65.970535
1464.907418	59.768256	65.975540
1463.903382	60.788868	65.980545
1462.883464	59.110656	65.985550
1462.682552	54.345477	65.990554
1462.236870	67.404245	65.995559
1461.839597	54.438494	66.000564
1460.559441	57.933094	66.005569
1459.781432	65.211469	66.010574
1459.660650	61.080111	66.015578
1459.073148	59.902468	66.020583
1458.413333	59.333988	66.025588
1457.322944	56.153089	66.030593
1456.542769	54.286969	66.035598
1456.493318	59.759051	66.040602
1455.965100	65.281989	66.045607
1454.659654	59.856547	66.050612
1453.967888	50.449511	66.055617
1453.091451	63.092602	66.060622
1453.072261	55.090991	66.065626
1452.542626	65.272518	66.070631
1451.523189	54.895678	66.075636
1450.628071	59.754671	66.080641
1449.765672	62.366017	66.085646
1449.665253	56.657611	66.090650
1449.070181	62.654802	66.095655
1448.237762	54.720929	66.100660
1447.526457	63.136737	66.105665
1446.688751	58.247253	66.110670
1446.467916	50.706625	66.115674
1445.922667	53.453651	66.120679
1445.357973	54.536913	66.125684
1444.024455	60.664076	66.130689
1443.654374	60.117364	66.135694
1442.968682	57.775758	66.140698
1441.899898	60.639104	66.145703
1441.248583	57.273314	66.150708
1440.804953	55.494064	66.155713
1440.151457	60.420317	66.160718
1439.636414	49.187458	66.165722
1439.316393	54.986392	66.170727
1438.801607	55.195969	66.175732
1437.535627	49.354257	66.180737
1436.649011	61.387105	66.185742
1436.556165	51.066444	66.190746
1436.034051	52.433102	66.195751
1434.915736	55.096162	66.200756
1434.315921	50.318690	66.205761
1433.521890	58.433829	66.210766
1433.210237	55.931855	66.215770
1432.490747	58.810656	66.220775
1431.391779	53.989509	66.225780
1430.559059	49.782068	66.230785
1429.935734	53.265333	66.235790
1430.075138	42.149247	66.240794
1429.755603	49.111903	66.245799
1429.006490	50.834764	66.250804
1428.262379	51.210100	66.255809
1427.231298	59.985817	66.260814
1426.167734	53.873818	66.265818
1425.090768	71.192961	66.270823
1424.929432	63.814764	66.275828
1424.364062	56.710521	66.280833
1423.840807	54.895043	66.285838
1423.779396	54.849639	66.290842
1422.497729	59.907271	66.295847
1421.862696	55.039203	66.300852
1420.931399	60.843828	66.305857
1420.488501	61.164986	66.310862
1419.877035	57.327663	66.315866
1418.852635	60.429971	66.320871
1418.208636	58.589529	66.325876
1417.931930	54.851969	66.330881
1416.992074	59.347495	66.335886
1416.928480	53.899748	66.340890
1416.243928	62.476891	66.345895
1415.319747	56.311203	66.350900
1414.270942	62.205470	66.355905
1413.761777	69.597249	66.360910
1413.506036	55.271747	66.365914
1411.902672	69.244651	66.370919
1411.397410	59.530436	66.375924
1411.010105	64.671436	66.380929
1410.469919	61.819429	66.385934
1410.311815	57.039567	66.390938
1409.775941	59.483909	66.395943
1408.920870	60.081893	66.400948
1408.063216	58.999239	66.405953
1407.593666	69.887167	66.410958
1406.879581	55.435817	66.415962
1405.573642	66.380982	66.420967
1404.782754	58.150362	66.425972
1404.703846	46.662116	66.430977
1403.900416	56.196447	66.435982
1403.810762	50.410642	66.440986
1402.527984	52.445413	66.445991
1401.751574	52.800659	66.450996
1401.299789	56.718717	66.456001
1400.725869	58.979872	66.461006
1400.557090	52.963790	66.466010
1398.959145	55.212661	66.471015
1398.508854	59.370181	66.476020
1397.951065	58.367605	66.481025
1397.380486	54.342439	66.486030
1397.108012	56.081015	66.491034
1396.141111	55.085117	66.496039
1395.504080	52.179122	66.501044
1394.879508	45.959519	66.506049
1394.298703	48.111381	66.511054
1393.501915	41.447640	66.516058
1392.258251	58.417953	66.521063
1392.019628	46.221805	66.526068
1391.653290	47.055928	66.531073
1390.653020	46.890090	66.536078
1390.249617	49.747044	66.541082
1389.002956	52.009472	66.546087
1388.484995	52.949698	66.551092
1388.400557	54.835008	66.556097
1387.454071	48.512030	66.561102
1387.140423	47.320840	66.566106
1385.581002	47.436268	66.571111
1385.016589	58.414961	66.576116
1384.991695	45.382168	66.581121
1384.426509	50.690211	66.586126
1384.076112	43.581780	66.591130
1382.861770	54.209608	66.596135
1382.152136	45.029372	66.601140
1381.905189	44.228130	66.606145
1380.651259	47.658671	66.611150
1379.834173	47.597762	66.616154
1379.096588	52.788129	66.621159
1378.441114	58.030102	66.626164
1378.417174	49.155616	66.631169
1378.057131	54.817411	66.636174
1377.857482	47.079463	66.641178
1376.534938	59.317232	66.646183
1375.918956	58.877425	66.651188
1374.908310	55.933050	66.656193
1373.887598	55.183835	66.661198
1373.388479	60.017754	66.666202
1373.076239	59.228468	66.671207
1372.618103	64.819126	66.676212
1371.587063	64.186672	66.681217
1370.562428	59.462548	66.686222
1370.317704	61.545226	66.691226
1369.808082	60.531846	66.696231
1369.071473	65.567521	66.701236
1368.158914	62.793638	66.706241
1367.287771	70.078955	66.711246
1367.055617	58.725451	66.716250
1366.607631	71.988022	66.721255
1366.651910	68.644148	66.726260
1365.946287	57.244479	66.731265
1364.636346	57.400689	66.736270
1363.604604	53.563955	66.741274
1363.011464	60.289411	66.746279
1362.098920	63.774509	66.751284
1362.251325	60.243139	66.756289
1361.108020	69.918245	66.761294
1360.348054	68.722307	66.766298
1359.531398	61.344208	66.771303
1359.258668	57.979765	66.776308
1359.054300	59.299084	66.781313
1357.576933	62.486033	66.786318
1356.991684	51.070392	66.791322
1356.238591	70.604168	66.796327
1356.027342	56.225876	66.801332
1355.027211	50.630535	66.806337
1353.950640	70.028071	66.811342
1354.054664	61.393439	66.816346
1353.544783	67.706692	66.821351
1352.471630	63.277296	66.826356
1351.562202	59.654513	66.831361
1350.445916	57.141682	66.836366
1350.240174	55.584835	66.841370
1349.661485	58.540623	66.846375
1349.403953	63.285681	66.851380
1349.462887	54.528909	66.856385
1348.216750	59.030566	66.861390
1347.475979	50.009831	66.866394
1346.104065	59.090490	66.871399
1345.128346	48.965381	66.876404
1344.577539	46.413128	66.881409
1344.242284	58.817245	66.886414
1344.039528	42.174673	66.891418
1343.435529	58.631731	66.896423
1343.211431	57.530391	66.901428
1342.502105	56.897272	66.906433
1341.382344	64.111726	66.911438
1340.720592	55.488441	66.916442
1339.736678	47.261729	66.921447
1338.714567	57.103651	66.926452
1338.157601	60.188454	66.931457
1337.924793	59.853327	66.936462
1337.473138	57.039306	66.941466
1337.168710	58.221567	66.946471
1336.111602	60.152688	66.951476
1335.563207	56.486714	66.956481
1334.561468	69.100867	66.961486
1334.168920	61.349427	66.966490
1333.142741	67.464057	66.971495
1332.362381	59.450990	66.976500
1331.807681	52.296194	66.981505
1331.468357	59.091693	66.986510
1331.314726	53.891657	66.991514
1330.414328	56.080145	66.996519
1329.657115	60.295927	67.001524
1328.934645	59.152387	67.006529
1327.762217	59.862348	67.011534
1326.986295	57.612391	67.016538
1326.281410	54.728241	67.021543
1325.798865	55.229183	67.026548
1325.820892	45.771806	67.031553
1324.911446	56.745428	67.036558
1324.124173	60.519709	67.041562
1323.170559	57.566289	67.046567
1322.702453	57.356880	67.051572
1322.380474	50.344866	67.056577
1321.522998	52.898697	67.061582
1320.827020	52.733398	67.066586
1320.177015	51.338642	67.071591
1319.690801	51.210960	67.076596
1318.870827	59.792300	67.081601
1317.709590	57.357594	67.086606
1317.385918	57.281344	67.091610
1317.073924	62.528651	67.096615
1316.258065	61.786318	67.101620
1315.099474	54.752760	67.106625
1314.074158	63.500789	67.111630
1313.892754	53.760355	67.116634
1313.374875	58.724998	67.121639
1312.809937	56.624433	67.126644
1312.732642	57.704356	67.131649
1311.856268	60.368428	67.136654
1310.818599	59.257656	67.141658
1310.036691	60.619907	67.146663
1309.688907	62.274269	67.151668
1309.523817	52.703132	67.156673
1308.066429	61.854167	67.161678
1307.481604	61.928246	67.166682
1306.901835	63.053358	67.171687
1306.520286	64.878670	67.176692
1305.805302	57.547509	67.181697
1304.898820	68.577445	67.186702
1304.452130	63.999591	67.191706
1303.520690	59.369492	67.196711
1302.593691	55.484594	67.201716
1302.183231	55.728074	67.206721
1301.342186	55.339836	67.211726
1300.948193	56.761846	67.216730
1300.565901	58.492658	67.221735
1299.823967	57.834773	67.226740
1298.359710	50.802512	67.231745
1297.307239	57.342378	67.236750
1296.851534	56.508101	67.241754
1296.566725	61.680124	67.246759
1295.686028	53.632563	67.251764
1295.556276	55.846779	67.256769
1294.663665	55.908291	67.261774
1294.711253	47.519188	67.266778
1294.250547	58.006736	67.271783
1293.366302	53.492143	67.276788
1292.676052	49.832965	67.281793
1291.828404	59.535201	67.286798
1291.340358	60.465960	67.291802
1290.023008	59.834902	67.296807
1289.425801	60.125421	67.301812
1289.186164	49.738234	67.306817
1289.023941	54.518603	67.311822
1288.101869	58.237052	67.316826
1287.184355	51.329188	67.321831
1286.248485	52.340606	67.326836
1285.851636	53.178017	67.331841
1284.374875	58.470156	67.336846
1283.942076	54.087222	67.341850
1283.654324	55.050793	67.346855
1282.863212	55.662304	67.351860
1282.781839	54.863133	67.356865
1282.223160	58.388191	67.361870
1281.519273	50.601113	67.366874
1280.349764	57.433984	67.371879
1279.868191	57.322919	67.376884
1279.378649	56.230671	67.381889
1278.390682	65.367015	67.386894
1277.765761	57.977391	67.391898
1276.976552	65.703868	67.396903
1276.672000	61.674285	67.401908
1276.472914	62.633222	67.406913
1275.248014	58.316299	67.411918
1274.833925	51.743143	67.416922
1273.998646	59.655139	67.421927
1272.889849	55.430147	67.426932
1272.233390	47.984042	67.431937
1271.292067	56.165212	67.436942
1271.014503	56.032751	67.441946
1270.865806	64.600419	67.446951
1270.365317	64.596442	67.451956
1269.945197	56.612859	67.456961
1268.638380	57.113977	67.461966
1268.286354	59.133296	67.466970
1267.050297	63.124027	67.471975
1266.183660	67.630039	67.476980
1265.845109	57.946135	67.481985
1264.971811	58.255325	67.486990
1264.934364	62.421341	67.491994
1264.515664	58.528182	67.496999
1263.017668	64.000330	67.502004
1262.628467	55.836791	67.507009
1262.073456	68.226969	67.512014
1261.577187	51.304643	67.517018
1260.521794	61.443621	67.522023
1259.569281	53.122064	67.527028
1259.280786	57.774275	67.532033
1258.823827	57.160979	67.537038
1258.649886	52.391539	67.542042
1257.498479	58.819416	67.547047
1256.763693	55.758690	67.552052
1256.241094	58.864851	67.557057
1255.420114	59.577314	67.562062
1254.642788	61.299978	67.567066
1253.870712	60.050806	67.572071
1253.060721	59.055245	67.577076
1252.932492	58.397568	67.582081
1252.470671	59.587517	67.587086
1251.784342	52.158782	67.592090
1250.694184	57.261734	67.597095
1249.919105	56.864602	67.602100
1250.067839	56.848867	67.607105
1248.484078	61.320670	67.612110
1247.987525	54.850518	67.617114
1247.592316	55.853256	67.622119
1246.816848	60.423624	67.627124
1246.457831	51.977746	67.632129
1245.123221	50.780173	67.637134
1244.559852	52.312701	67.642138
1244.058507	52.504409	67.647143
1243.503369	58.356509	67.652148
1243.188865	60.191669	67.657153
1241.860985	58.789599	67.662158
1241.640204	52.907963	67.667162
1241.056169	55.932431	67.672167
1240.252668	55.784251	67.677172
1239.705039	50.282595	67.682177
1238.525920	62.253183	67.687182
1238.331815	60.719727	67.692186
1238.094223	58.559246	67.697191
1236.930746	58.040946	67.702196
1235.867420	54.989888	67.707201
1235.261806	54.690395	67.712206
1234.966232	50.872284	67.717210
1234.635525	53.041182	67.722215
1233.403511	42.649377	67.727220
1233.112409	46.980301	67.732225
1232.332745	60.514801	67.737230
1231.890488	56.407773	67.742234
1230.740583	63.999223	67.747239
1230.146104	53.078684	67.752244
1229.701479	53.191989	67.757249
1228.946147	54.130565	67.762254
1228.506558	47.862677	67.767258
1227.588976	49.107752	67.772263
1226.856822	62.809743	67.777268
1226.616312	55.775331	67.782273
1225.749038	59.136578	67.787278
1224.953942	56.952782	67.792282
1224.101055	52.827471	67.797287
1223.638877	62.160924	67.802292
1223.160485	52.551309	67.807297
1222.598561	62.592909	67.812302
1221.528473	58.762334	67.817306
1221.186118	53.142886	67.822311
1220.760425	54.450098	67.827316
1220.181120	49.817660	67.832321
1218.879816	58.205898	67.837326
1217.992897	52.867008	67.842330
1217.852504	64.473739	67.847335
1217.023415	59.165076	67.852340
1216.758868	50.038705	67.857345
1215.426365	60.992895	67.862350
1214.695988	58.423493	67.867354
1214.242671	53.755253	67.872359
1213.624651	58.098742	67.877364
1213.655457	57.075154	67.882369
1212.541087	59.531095	67.887374
1211.690168	51.295910	67.892378
1211.461897	58.076910	67.897383
1210.377096	59.886326	67.902388
1209.704903	46.890256	67.907393
1208.411633	53.818527	67.912398
1208.435428	51.607024	67.917402
1208.129493	58.600649	67.922407
1207.598788	54.994974	67.927412
1206.970350	55.277862	67.932417
1205.912921	55.444462	67.937422
1205.421943	55.052630	67.942426
1204.831422	61.295143	67.947431
1203.521825	61.331531	67.952436
1203.142189	52.600357	67.957441
1202.348036	56.640693	67.962446
1201.899152	52.774425	67.967450
1201.401688	47.315267	67.972455
1200.301995	58.133091	67.977460
1199.845434	49.750045	67.982465
1199.221145	59.337936	67.987470
1199.121801	51.036858	67.992474
1197.849314	53.346059	67.997479
1196.928251	50.844834	68.002484
1196.317738	42.065226	68.007489
1196.073516	50.058289	68.012494
1195.705913	52.956885	68.017498
1194.599289	51.970668	68.022503
1193.889016	62.606722	68.027508
1193.267845	47.623455	68.032513
1193.092468	51.368274	68.037518
1192.235754	56.443587	68.042522
1191.182721	63.166509	68.047527
1190.449544	60.059815	68.052532
1190.060857	58.260837	68.057537
1189.381962	62.404276	68.062542
1188.557711	53.748540	68.067546
1187.705056	58.930443	68.072551
1187.116084	58.587313	68.077556
1187.033125	50.953841	68.082561
1186.321512	51.871285	68.087566
1185.894161	46.528715	68.092570
1184.797365	57.489586	68.097575
1184.246124	50.954032	68.102580
1183.628858	49.383795	68.107585
1182.586052	61.837353	68.112590
1182.495131	50.114504	68.117594
1181.730029	58.162020	68.122599
1180.155657	57.650741	68.127604
1179.476235	58.936808	68.132609
1178.909808	67.985646	68.137614
1178.473681	59.197225	68.142618
1178.332735	62.378326	68.147623
1177.560498	52.686143	68.152628
1177.557628	46.750943	68.157633
1176.194484	54.980295	68.162638
1175.692920	56.493546	68.167642
1175.326911	49.602107	68.172647
1173.891772	48.264440	68.177652
1172.904748	47.766995	68.182657
1172.429746	58.141706	68.187662
1172.123507	52.043436	68.192666
1171.720287	53.078998	68.197671
1170.929829	58.623177	68.202676
1170.262201	49.564072	68.207681
1169.231055	59.412213	68.212686
1169.258555	54.063541	68.217690
1168.875864	46.376815	68.222695
1167.648162	49.591968	68.227700
1167.085310	53.295906	68.232705
1166.172625	57.670495	68.237710
1164.768505	53.591870	68.242714
1164.391456	53.528859	68.247719
1163.605134	56.596551	68.252724
1163.566447	46.525944	68.257729
1163.380807	58.420561	68.262734
1163.143265	53.270160	68.267738
1162.202690	57.068863	68.272743
1160.804090	48.414595	68.277748
1160.728800	45.340484	68.282753
1159.535689	52.172422	68.287758
1158.750263	46.467332	68.292762
1158.181279	51.440124	68.297767
1157.722036	54.164062	68.302772
1157.668614	52.131998	68.307777
1156.472629	55.900359	68.312782
1155.901244	57.689647	68.317786
1154.936686	50.682089	68.322791
1153.691805	62.715204	68.327796
1153.285809	48.777951	68.332801
1152.475681	51.975589	68.337806
1152.273246	47.090845	68.342810
1151.650536	52.117914	68.347815
1150.998610	54.820458	68.352820
1151.079879	40.066125	68.357825
1150.248524	43.760726	68.362830
1149.251835	45.734349	68.367834
1148.861470	56.592343	68.372839
1147.474365	56.816130	68.377844
1146.900537	44.968241	68.382849
1146.004964	57.781591	68.387854
1145.604080	47.937324	68.392858
1145.712131	42.299879	68.397863
1143.970722	58.171436	68.402868
1143.667841	50.188168	68.407873
1143.026909	47.470524	68.412878
1142.687738	48.502211	68.417882
1142.149748	49.477209	68.422887
1140.819742	53.366239	68.427892
1140.725407	48.104757	68.432897
1139.961212	45.802536	68.437902
1139.227134	48.814615	68.442906
1138.178856	44.586374	68.447911
1137.456320	50.004638	68.452916
1137.337254	46.806602	68.457921
1136.809337	51.807559	68.462926
1136.261429	54.799494	68.467930
1135.594327	56.376927	68.472935
1135.207795	61.483135	68.477940
1134.009834	51.764061	68.482945
1132.780191	59.625271	68.487950
1132.262549	50.947604	68.492954
1132.299935	52.351491	68.497959
1131.129959	56.175650	68.502964
1129.907080	56.311826	68.507969
1129.571208	61.088276	68.512974
1129.176665	45.436631	68.517978
1129.016332	56.324272	68.522983
1128.047738	58.197242	68.527988
1127.443550	52.094327	68.532993
1126.210549	58.918433	68.537998
1125.917602	51.471331	68.543002
1125.385375	41.326263	68.548007
1124.794353	53.182846	68.553012
1123.699517	49.471373	68.558017
1123.094090	53.970572	68.563022
1122.692070	58.371187	68.568026
1122.537362	53.292773	68.573031
1121.456053	61.411096	68.578036
1120.974984	47.075785	68.583041
1120.050760	52.614442	68.588046
1119.247789	47.743216	68.593050
1118.204923	53.554635	68.598055
1117.129376	48.646338	68.603060
1117.183979	51.286977	68.608065
1116.856208	45.699926	68.613070
1116.382510	53.139706	68.618074
1116.223131	47.696183	68.623079
1114.479680	46.718249	68.628084
1114.389074	45.149421	68.633089
1113.614721	47.898253	68.638094
1112.847516	43.549624	68.643098
1112.007282	45.510992	68.648103
1111.178309	61.473988	68.653108
1111.047734	37.241124	68.658113
1110.232728	46.335802	68.663118
1109.291451	41.175919	68.668122
1108.855712	47.660330	68.673127
1108.046257	55.815839	68.678132
1107.684360	51.659788	68.683137
1106.616360	50.965513	68.688142
1105.848245	51.158678	68.693146
1105.540514	46.924628	68.698151
1105.115929	50.188689	68.703156
1104.355374	51.361522	68.708161
1103.122190	49.454030	68.713166
1102.695141	46.525759	68.718170
1102.599265	43.018108	68.723175
1101.318843	42.527934	68.728180
1100.445903	40.739766	68.733185
1100.163608	53.255301	68.738190
1099.549091	40.628578	68.743194
1099.071736	43.139361	68.748199
1098.334294	45.984828	68.753204
1097.585911	41.812984	68.758209
1096.774003	42.604478	68.763214
1096.011153	46.081616	68.768218
1096.035243	48.985729	68.773223
1094.662023	53.184432	68.778228
1093.939916	44.007866	68.783233
1093.583378	44.829432	68.788238
1093.185689	42.174038	68.793242
1092.534076	49.161146	68.798247
1091.195792	45.191944	68.803252
1090.856651	42.021034	68.808257
1090.265844	42.592856	68.813262
1089.917377	40.514686	68.818266
1089.345955	50.843233	68.823271
1088.190979	53.597421	68.828276
1088.040362	42.379256	68.833281
1087.200592	54.420491	68.838286
1086.117346	44.773090	68.843290
1085.352651	46.785529	68.848295
1084.572603	55.921966	68.853300
1084.909475	49.404449	68.858305
1083.615154	47.863085	68.863310
1082.828057	44.719274	68.868314
1082.162122	39.946116	68.873319
1081.330043	39.766262	68.878324
1081.647976	32.747137	68.883329
1080.682396	41.726997	68.888334
1079.764893	41.210645	68.893338
1078.919724	36.048105	68.898343
1078.389144	33.618859	68.903348
1077.796622	43.698445	68.908353
1077.146987	45.312537	68.913358
1076.445322	37.589842	68.918362
1076.349783	45.396826	68.923367
1074.850043	38.539096	68.928372
1074.070691	43.605286	68.933377
1073.709992	40.251727	68.938382
1073.412933	42.929377	68.943386
1072.802619	43.363957	68.948391
1071.571021	51.894130	68.953396
1071.418481	44.859949	68.958401
1070.610168	53.474179	68.963406
1069.868475	49.326510	68.968410
1069.148696	51.719742	68.973415
1068.264123	53.580945	68.978420
1067.857205	43.907972	68.983425
1067.546521	48.622070	68.988430
1066.407199	52.144911	68.993434
1065.622252	51.478168	68.998439
1065.101249	55.724250	69.003444
1064.973127	46.473709	69.008449
1063.571406	47.751698	69.013454
1062.592318	37.029606	69.018458
1061.780657	40.238549	69.023463
1061.535021	45.134688	69.028468
1061.329814	31.614974	69.033473
1060.774073	41.953639	69.038478
1060.443228	43.709413	69.043482
1059.405599	40.386267	69.048487
1058.718300	40.213351	69.053492
1058.490009	35.599244	69.058497
1057.368828	40.927971	69.063502
1056.508243	42.566163	69.068506
1056.130284	26.941886	69.073511
1055.141037	44.729677	69.078516
1054.528380	43.868374	69.083521
1053.741203	42.334662	69.088526
1053.145064	45.014159	69.093530
1053.028512	38.119340	69.098535
1052.076210	35.970074	69.103540
1051.068347	35.444454	69.108545
1050.223333	46.453616	69.113550
1049.714333	31.357962	69.118554
1049.780708	35.988421	69.123559
1048.997656	40.662543	69.128564
1047.973929	37.512233	69.133569
1047.301612	43.903395	69.138574
1046.887606	41.960238	69.143578
1046.445533	44.053830	69.148583
1045.263940	55.390932	69.153588
1044.487229	36.217266	69.158593
1043.870967	43.993543	69.163598
1043.679199	44.296892	69.168602
1042.836879	48.185658	69.173607
1041.787757	47.575141	69.178612
1041.788388	43.795098	69.183617
1041.531825	41.087301	69.188622
1040.123838	43.525365	69.193626
1039.276868	37.732342	69.198631
1038.653767	46.593080	69.203636
1038.137740	45.934028	69.208641
1037.160892	42.643800	69.213646
1035.970159	39.392330	69.218650
1036.028209	43.590451	69.223655
1035.509578	48.134203	69.228660
1035.531664	41.020210	69.233665
1034.381469	35.341660	69.238670
1033.217204	40.442284	69.243674
1032.754372	39.913545	69.248679
1032.245758	43.575760	69.253684
1032.197425	40.114169	69.258689
1030.987416	46.269173	69.263694
1030.381672	47.508862	69.268698
1029.346971	40.709646	69.273703
1028.163605	54.330472	69.278708
1027.857466	43.599107	69.283713
1027.449575	46.133544	69.288718
1026.759416	41.222331	69.293722
1026.557203	36.903701	69.298727
1025.812050	44.561713	69.303732
1024.891609	40.973934	69.308737
1023.803583	57.306158	69.313742
1023.471541	40.524968	69.318746
1023.520037	36.844546	69.323751
1022.260559	49.168603	69.328756
1021.732386	43.419486	69.333761
1020.940460	51.223716	69.338766
1020.239184	35.273984	69.343770
1019.698341	33.836714	69.348775
1018.554959	44.101715	69.353780
1018.221853	42.607741	69.358785
1017.758717	33.926178	69.363790
1017.503719	43.811726	69.368794
1016.391569	35.955661	69.373799
1015.524670	38.231961	69.378804
1015.103959	45.349503	69.383809
1014.218343	42.483165	69.388814
1013.184303	45.415264	69.393818
1012.631792	41.215442	69.398823
1012.166619	41.234283	69.403828
1011.915872	37.866397	69.408833
1011.734535	43.534479	69.413838
1010.699135	54.140280	69.418842
1009.708764	49.909191	69.423847
1009.076372	47.598659	69.428852
1008.262745	49.912219	69.433857
1007.790869	49.558388	69.438862
1006.766851	47.928330	69.443866
1006.462562	35.709610	69.448871
1005.907105	48.426292	69.453876
1005.181673	47.470978	69.458881
1004.294665	48.670266	69.463886
1003.470531	54.535235	69.468890
1003.197709	39.953952	69.473895
1002.619325	39.020976	69.478900
1001.814744	44.442860	69.483905
1000.939086	50.199331	69.488910
1000.327294	50.249385	69.493914
999.997808	45.198796	69.498919
999.082945	52.036991	69.503924
998.341340	40.266315	69.508929
997.862784	48.222543	69.513934
997.215942	46.168204	69.518938
996.827923	50.378945	69.523943
995.843371	46.169015	69.528948
995.101910	52.823505	69.533953
994.641615	51.745586	69.538958
994.143980	42.085491	69.543962
993.604176	44.812808	69.548967
992.599911	45.682247	69.553972
991.959464	43.283115	69.558977
990.868377	46.020870	69.563982
990.134842	50.636669	69.568986
989.762183	45.257058	69.573991
989.330911	49.255484	69.578996
989.070595	42.452929	69.584001
987.883034	46.809802	69.589006
986.803636	46.779715	69.594010
986.730689	42.162977	69.599015
985.849148	58.216354	69.604020
985.466543	45.584312	69.609025
984.541234	46.676159	69.614030
983.460256	44.113729	69.619034
983.549525	44.411793	69.624039
983.024939	47.723320	69.629044
982.212843	45.466618	69.634049
981.099692	42.037250	69.639054
980.339885	46.203066	69.644058
980.221622	50.683128	69.649063
979.285362	47.321810	69.654068
978.455870	41.049788	69.659073
977.833750	60.001343	69.664078
977.346586	48.218572	69.669082
977.067123	48.745615	69.674087
976.150451	51.105543	69.679092
975.359785	49.946150	69.684097
974.876251	55.014188	69.689102
974.236873	50.500188	69.694106
973.212427	52.374214	69.699111
972.259737	57.846484	69.704116
971.902353	42.427102	69.709121
971.655308	51.554449	69.714126
971.187979	51.324481	69.719130
970.073827	45.201832	69.724135
968.919331	48.722395	69.729140
968.460976	30.565724	69.734145
968.291849	45.118017	69.739150
967.630193	47.724378	69.744154
967.019486	45.732106	69.749159
965.787077	55.039891	69.754164
965.678104	45.461466	69.759169
965.046050	37.980049	69.764174
963.670671	47.400464	69.769178
963.303506	44.353883	69.774183
962.668186	48.041001	69.779188
962.167450	40.772079	69.784193
961.946251	42.407916	69.789198
961.005823	45.549068	69.794202
960.224283	43.721175	69.799207
959.486918	53.142583	69.804212
958.706696	48.710922	69.809217
957.880871	43.274112	69.814222
957.045153	44.769607	69.819226
956.807060	39.132049	69.824231
956.252753	44.820053	69.829236
956.014034	42.615632	69.834241
955.265068	44.210864	69.839246
954.425081	42.890593	69.844250
954.171003	34.803412	69.849255
952.628025	37.138420	69.854260
951.977655	37.025890	69.859265
951.522438	49.564202	69.864270
951.026961	50.519858	69.869274
950.787634	41.184530	69.874279
949.284019	57.139775	69.879284
949.287390	44.247633	69.884289
948.882168	47.428208	69.889294
947.629157	52.211831	69.894298
947.368324	50.655904	69.899303
946.969330	53.094320	69.904308
945.907545	44.848649	69.909313
945.695951	36.932905	69.914318
944.200816	38.262092	69.919322
942.703478	38.610763	69.924327
941.831225	49.695247	69.929332
941.883471	44.634390	69.934337
941.937419	45.679243	69.939342
940.766096	42.790585	69.944346
940.492384	44.020040	69.949351
939.960518	49.300775	69.954356
939.163828	43.313709	69.959361
938.182184	49.585380	69.964366
937.794433	48.675703	69.969370
937.588267	45.581430	69.974375
935.888944	56.184088	69.979380
935.304929	45.597886	69.984385
934.935073	49.223847	69.989390
934.497300	54.644155	69.994394
934.346632	49.970400	69.999399
933.297206	46.097251	70.004404
932.538114	40.269786	70.009409
932.098010	43.030135	70.014414
931.503709	49.913534	70.019418
930.587498	40.244371	70.024423
929.472262	49.285939	70.029428
929.321632	41.462997	70.034433
928.067303	46.029215	70.039438
927.163878	49.896199	70.044442
927.074924	44.151334	70.049447
926.340432	48.863494	70.054452
925.945129	56.344438	70.059457
925.995199	44.648087	70.064462
925.034719	50.626235	70.069466
924.190329	49.432831	70.074471
922.566440	50.192737	70.079476
921.808334	48.542478	70.084481
921.625999	36.668650	70.089486
920.988248	50.529114	70.094490
920.799911	44.650253	70.099495
920.215235	52.530337	70.104500
919.434317	54.450788	70.109505
918.646002	46.495929	70.114510
918.046336	46.709654	70.119514
917.868851	54.786719	70.124519
916.138274	57.906967	70.129524
915.401591	45.558372	70.134529
915.126619	54.974017	70.139534
914.457349	57.094323	70.144538
914.596530	48.066198	70.149543
913.587891	58.907469	70.154548
912.674245	47.392860	70.159553
912.087323	47.563558	70.164558
911.288178	46.779275	70.169562
910.430048	39.242388	70.174567
909.735972	41.149020	70.179572
909.369580	41.489629	70.184577
908.920694	42.781655	70.189582
908.006457	42.133961	70.194586
907.213641	36.136831	70.199591
906.453652	43.048174	70.204596
906.310915	48.732194	70.209601
905.592320	54.950979	70.214606
904.350131	48.268417	70.219610
904.176669	40.972662	70.224615
903.391043	42.100656	70.229620
902.956685	44.357045	70.234625
902.606629	41.058594	70.239630
901.643389	39.679107	70.244634
900.916426	28.226274	70.249639
899.515853	43.288340	70.254644
898.506476	41.769539	70.259649
898.449401	42.325855	70.264654
897.846718	46.622807	70.269658
897.632489	35.991971	70.274663
897.367386	50.971122	70.279668
896.334155	52.751958	70.284673
895.710401	45.578323	70.289678
894.653386	50.546821	70.294682
894.587727	45.506306	70.299687
893.364386	51.344945	70.304692
892.699514	49.441738	70.309697
892.111396	46.591180	70.314702
891.494180	48.144964	70.319706
890.835455	43.142060	70.324711
889.627777	51.963387	70.329716
889.386508	42.014944	70.334721
889.021821	34.891552	70.339726
888.325450	57.802044	70.344730
887.634333	46.710929	70.349735
886.332707	55.298052	70.354740
886.191032	45.761113	70.359745
885.794544	52.109991	70.364750
884.840836	48.246862	70.369754
884.341578	44.130062	70.374759
883.493552	48.201132	70.379764
882.974374	43.269063	70.384769
882.839003	47.750269	70.389774
881.403976	47.081384	70.394778
880.984327	42.657025	70.399783
880.472414	47.195002	70.404788
879.619682	42.309708	70.409793
878.731853	47.207131	70.414798
877.718699	43.578972	70.419802
877.739811	39.153856	70.424807
877.045314	49.386895	70.429812
876.530239	45.095995	70.434817
875.751810	41.756911	70.439822
874.841738	48.149676	70.444826
874.629164	44.367301	70.449831
873.604374	39.195579	70.454836
872.678361	31.321008	70.459841
872.245560	46.243262	70.464846
871.573650	51.437487	70.469850
871.546231	43.038278	70.474855
870.385070	52.315835	70.479860
869.592330	42.191809	70.484865
868.881598	46.083338	70.489870
868.369104	50.328095	70.494874
867.577456	37.947274	70.499879
866.291384	50.532664	70.504884
865.947460	48.624117	70.509889
865.933144	43.313659	70.514894
865.326965	46.300722	70.519898
865.064669	35.417346	70.524903
863.895848	45.842567	70.529908
863.162826	40.772648	70.534913
862.812262	40.256035	70.539918
861.483814	39.615932	70.544922
860.938642	40.715132	70.549927
860.142951	41.964589	70.554932
859.957265	45.215892	70.559937
859.498156	46.121622	70.564942
858.563666	46.894852	70.569946
858.291362	39.414562	70.574951
857.427132	33.561283	70.579956
856.219795	41.685549	70.584961
855.550470	38.119374	70.589966
854.850183	44.273751	70.594970
854.897932	38.540255	70.599975
853.867602	40.744846	70.604980
853.083316	40.273608	70.609985
852.593905	36.290870	70.614990
851.862364	41.466200	70.619994
851.587083	38.516980	70.624999
850.501695	36.149280	70.630004
849.718648	40.649987	70.635009
849.447898	35.181649	70.640014
848.695671	48.787525	70.645018
847.868999	36.331863	70.650023
846.966934	47.608769	70.655028
846.548502	39.019485	70.660033
846.291425	38.880657	70.665038
844.872250	48.245017	70.670042
844.518748	44.191761	70.675047
843.839528	47.646195	70.680052
843.213515	41.157338	70.685057
842.926104	36.776597	70.690062
841.659310	44.673791	70.695066
841.123136	44.035334	70.700071
840.640871	45.406801	70.705076
840.262367	45.777733	70.710081
839.470148	46.285475	70.715086
838.327401	56.583561	70.720090
838.235020	49.921459	70.725095
837.459859	54.356262	70.730100
836.648651	51.426108	70.735105
835.820429	51.967967	70.740110
834.844043	50.756178	70.745114
834.942205	51.071745	70.750119
834.437737	50.784635	70.755124
833.521197	46.931382	70.760129
832.487727	45.455867	70.765134
831.813710	54.132355	70.770138
831.438794	50.964027	70.775143
830.817333	50.679769	70.780148
829.544225	48.475996	70.785153
829.073338	50.643594	70.790158
828.667006	47.978586	70.795162
828.527862	45.857679	70.800167
827.750969	43.701084	70.805172
826.714130	51.733575	70.810177
826.444753	44.875720	70.815182
825.643645	47.195226	70.820186
824.414466	44.203871	70.825191
823.913933	52.887440	70.830196
823.093479	54.170813	70.835201
823.115608	52.532017	70.840206
822.495547	53.282022	70.845210
821.636702	47.047848	70.850215
820.671395	44.075996	70.855220
820.190788	51.720334	70.860225
819.685213	41.413427	70.865230
818.493799	46.362343	70.870234
817.744963	43.307152	70.875239
817.407602	47.752699	70.880244
816.997836	47.243939	70.885249
816.751760	46.635007	70.890254
815.472928	51.440144	70.895258
814.820727	48.259184	70.900263
814.447551	46.243339	70.905268
813.531580	38.630544	70.910273
812.917473	32.286462	70.915278
811.819563	45.012229	70.920282
811.677948	36.744747	70.925287
811.058727	48.077566	70.930292
810.574904	49.487134	70.935297
809.822700	36.726323	70.940302
808.802265	43.658644	70.945306
808.923079	31.936864	70.950311
807.490433	39.978739	70.955316
806.770459	48.440192	70.960321
806.629695	38.272344	70.965326
805.412425	41.044451	70.970330
804.850611	38.565046	70.975335
803.882820	37.676756	70.980340
802.997219	43.650906	70.985345
803.257415	46.315573	70.990350
802.697881	45.974157	70.995354
802.023462	42.464002	71.000359
801.114338	43.195368	71.005364
800.545979	48.180735	71.010369
799.752434	42.366687	71.015374
798.302841	45.245164	71.020378
797.936527	42.195324	71.025383
797.406775	49.435900	71.030388
797.099761	47.016863	71.035393
796.991662	43.143751	71.040398
795.859486	49.728012	71.045402
795.343336	39.470107	71.050407
794.631307	39.706477	71.055412
793.523148	45.872175	71.060417
793.205965	40.283503	71.065422
792.440620	35.184063	71.070426
792.119527	43.578869	71.075431
790.910685	40.592180	71.080436
789.900537	42.061876	71.085441
789.505829	34.973248	71.090446
788.876857	44.497276	71.095450
789.202131	40.228751	71.100455
787.869618	38.764588	71.105460
786.901445	41.113852	71.110465
786.635456	37.297414	71.115470
785.906468	42.229503	71.120474
785.398194	35.586307	71.125479
784.473450	39.701155	71.130484
783.595712	37.666285	71.135489
783.437625	38.292298	71.140494
782.446740	42.879724	71.145498
781.661525	41.952917	71.150503
780.795342	50.940699	71.155508
780.435599	48.537943	71.160513
780.421033	42.385436	71.165518
779.232817	44.858040	71.170522
778.720626	33.654918	71.175527
777.928286	48.511406	71.180532
777.408002	53.914904	71.185537
776.458410	38.135696	71.190542
775.292404	39.229661	71.195546
774.935326	39.627154	71.200551
774.921554	43.423528	71.205556
774.180189	42.418780	71.210561
773.221006	48.641197	71.215566
772.336816	49.056368	71.220570
772.081740	42.997340	71.225575
771.615252	45.610525	71.230580
770.622659	39.903869	71.235585
770.105320	38.407721	71.240590
769.291037	44.455683	71.245594
769.012248	47.073683	71.250599
768.033922	47.038638	71.255604
767.139855	48.218629	71.260609
767.011397	43.013079	71.265614
765.639536	50.069169	71.270618
764.934021	48.721249	71.275623
764.055695	49.006178	71.280628
763.942683	48.281452	71.285633
763.788004	44.396834	71.290638
763.153115	45.713763	71.295642
762.585814	43.757215	71.300647
761.520063	49.868867	71.305652
760.616243	48.543054	71.310657
759.721336	39.297936	71.315662
758.764454	47.141098	71.320666
758.394137	40.404983	71.325671
758.011924	42.400780	71.330676
757.667508	44.745376	71.335681
757.304098	35.600154	71.340686
756.165206	44.178766	71.345690
755.679752	40.917664	71.350695
755.031732	36.168568	71.355700
753.941779	42.487499	71.360705
753.231404	42.400343	71.365710
752.452557	40.750287	71.370714
752.322250	44.562058	71.375719
751.648096	57.132084	71.380724
750.426880	55.465717	71.385729
750.086486	40.594060	71.390734
749.115303	43.569868	71.395738
749.187100	38.518523	71.400743
748.413786	45.865687	71.405748
747.116735	46.400208	71.410753
746.662066	44.862549	71.415758
746.428608	46.388389	71.420762
746.119472	38.065583	71.425767
744.929140	41.095203	71.430772
743.993301	40.129310	71.435777
743.663989	41.323479	71.440782
742.515116	42.894126	71.445786
741.935065	28.172601	71.450791
741.432589	41.487991	71.455796
740.833437	41.466710	71.460801
740.730799	37.441347	71.465806
739.969675	46.212138	71.470810
738.745816	39.416369	71.475815
738.338231	42.770811	71.480820
737.581080	40.585873	71.485825
737.474362	32.216655	71.490830
736.170250	45.464127	71.495834
735.426913	32.277741	71.500839
735.172647	37.485924	71.505844
734.313934	35.594700	71.510849
734.079756	38.243446	71.515854
733.524493	44.862038	71.520858
733.059793	41.867297	71.525863
732.114854	36.850087	71.530868
731.210265	46.272924	71.535873
730.543109	39.103102	71.540878
729.536595	47.506109	71.545882
729.076592	46.705740	71.550887
728.145363	38.920370	71.555892
727.186792	44.078258	71.560897
727.093469	34.008530	71.565902
726.532893	44.384271	71.570906
726.177448	35.067479	71.575911
724.854159	40.370164	71.580916
724.365379	41.696956	71.585921
724.140923	37.072824	71.590926
723.101961	42.063739	71.595930
722.100317	36.976713	71.600935
721.240206	42.281353	71.605940
721.127278	39.624848	71.610945
721.165157	41.970084	71.615950
719.901870	39.425762	71.620954
719.176100	36.299124	71.625959
718.641866	38.397977	71.630964
717.863804	44.526918	71.635969
716.781319	29.445423	71.640974
715.849158	39.919746	71.645978
715.633108	39.922633	71.650983
715.274461	36.119382	71.655988
714.518276	40.713618	71.660993
713.921617	35.855432	71.665998
713.030728	46.996549	71.671002
712.392910	43.816485	71.676007
712.126292	43.031062	71.681012
711.424097	39.547435	71.686017
710.371982	35.504508	71.691022
709.773959	39.551593	71.696026
709.581083	31.705453	71.701031
708.667613	41.183323	71.706036
707.448691	45.289840	71.711041
706.907219	39.225961	71.716046
706.209056	45.156104	71.721050
706.090267	37.774405	71.726055
705.320962	41.888185	71.731060
704.119164	47.961593	71.736065
704.009388	39.931908	71.741070
703.477529	43.476451	71.746074
703.018619	36.817534	71.751079
702.132534	38.926677	71.756084
701.151070	41.271780	71.761089
700.774276	38.392361	71.766094
699.824945	47.798676	71.771098
699.046801	43.064004	71.776103
698.434660	41.330654	71.781108
697.915097	44.854318	71.786113
697.633246	39.324693	71.791118
696.697726	40.840891	71.796122
696.025782	40.563128	71.801127
695.256576	40.277197	71.806132
694.607035	40.741767	71.811137
694.277969	38.644803	71.816142
693.162698	43.182678	71.821146
692.410852	37.051374	71.826151
691.965307	35.587968	71.831156
691.659241	43.236063	71.836161
690.921976	32.363697	71.841166
689.973453	44.362393	71.846170
689.769097	39.093245	71.851175
688.713201	44.126293	71.856180
687.757823	45.481652	71.861185
687.237931	37.801120	71.866190
686.561771	43.360334	71.871194
686.373013	34.898528	71.876199
685.612439	46.383177	71.881204
684.454486	45.108896	71.886209
684.178794	37.100901	71.891214
683.640706	53.913347	71.896218
683.018895	38.452585	71.901223
682.150016	44.408338	71.906228
681.220069	48.167658	71.911233
681.212366	38.445423	71.916238
680.052410	52.646103	71.921242
679.380013	47.604440	71.926247
678.988306	43.883728	71.931252
678.443437	42.519717	71.936257
677.552964	34.182258	71.941262
676.482204	53.829723	71.946266
675.698643	34.595842	71.951271
675.413945	39.023552	71.956276
674.932953	41.817256	71.961281
674.452981	37.497166	71.966286
673.598933	45.210438	71.971290
672.867829	38.154898	71.976295
672.417931	40.286063	71.981300
671.386781	40.841363	71.986305
670.233773	35.351108	71.991310
669.937127	44.896355	71.996314
669.749910	40.326224	72.001319
669.182636	38.294001	72.006324
668.173404	38.489421	72.011329
667.755511	40.443602	72.016334
667.120808	41.530290	72.021338
666.766726	33.479589	72.026343
665.769155	34.608285	72.031348
664.792803	42.601230	72.036353
664.535746	33.659871	72.041358
663.639157	40.298129	72.046362
662.702728	42.923081	72.051367
662.222395	47.263674	72.056372
661.493341	39.050328	72.061377
661.453530	37.121776	72.066382
660.361808	38.572972	72.071386
659.563566	29.962218	72.076391
659.206459	30.239884	72.081396
658.247700	39.505781	72.086401
657.435328	36.227373	72.091406
656.598985	51.322700	72.096410
655.275585	40.471135	72.101415
654.623405	37.793270	72.106420
654.578064	38.674150	72.111425
654.616947	34.517451	72.116430
653.535822	34.852058	72.121434
652.724837	27.038121	72.126439
652.451779	38.661183	72.131444
652.100916	45.602056	72.136449
651.421495	32.840768	72.141454
650.421484	46.500319	72.146458
649.889343	44.594970	72.151463
649.152273	39.961010	72.156468
647.689154	34.162180	72.161473
647.439391	30.313219	72.166478
646.639804	34.378219	72.171482
646.347250	36.561602	72.176487
646.277981	41.513252	72.181492
645.774044	42.085535	72.186497
644.982186	30.122748	72.191502
643.965738	45.855454	72.196506
643.013025	41.167525	72.201511
642.508907	34.605709	72.206516
641.598729	45.336751	72.211521
641.324749	39.201911	72.216526
640.415690	38.345333	72.221530
639.354581	29.568289	72.226535
638.923505	38.010573	72.231540
638.400572	35.838833	72.236545
638.049030	37.052324	72.241550
637.621906	45.702141	72.246554
636.556404	42.375738	72.251559
636.052237	32.210598	72.256564
635.445473	33.896816	72.261569
634.477950	24.504056	72.266574
633.491137	48.682926	72.271578
633.037785	38.293648	72.276583
633.035883	42.072357	72.281588
632.313856	38.304908	72.286593
631.584075	32.054998	72.291598
630.825499	43.444719	72.296602
630.034617	31.991137	72.301607
628.890068	34.636625	72.306612
628.316676	37.180123	72.311617
627.801526	39.987159	72.316622
627.446920	42.170965	72.321626
626.937395	29.653871	72.326631
625.735651	36.063188	72.331636
625.303476	37.568641	72.336641
625.206021	23.968799	72.341646
623.809135	30.227841	72.346650
623.132044	37.051928	72.351655
622.494280	30.091933	72.356660
621.825516	34.829964	72.361665
621.685033	24.535956	72.366670
620.413979	41.957121	72.371674
619.494139	29.795530	72.376679
619.328231	43.175601	72.381684
618.706533	34.800098	72.386689
618.730672	38.114188	72.391694
617.451114	35.041080	72.396698
616.368439	37.548988	72.401703
616.367186	31.681383	72.406708
615.557945	48.790896	72.411713
614.673289	34.119500	72.416718
613.720808	28.770809	72.421722
613.635120	38.200456	72.426727
613.230207	37.448107	72.431732
612.065108	30.597324	72.436737
611.532627	26.957395	72.441742
610.680194	30.958280	72.446746
610.470369	37.250641	72.451751
609.551441	34.329841	72.456756
608.706704	35.352220	72.461761
608.054094	20.665965	72.466766
607.708220	41.875863	72.471770
606.531272	42.530102	72.476775
606.059293	40.697184	72.481780
605.426003	37.601587	72.486785
604.970240	31.626592	72.491790
604.119821	44.393430	72.496794
603.289476	36.655132	72.501799
602.484659	39.132988	72.506804
602.242232	37.290323	72.511809
602.034164	29.801434	72.516814
600.909350	33.840969	72.521818
600.063168	27.232719	72.526823
599.385162	36.237877	72.531828
599.226191	36.047181	72.536833
598.549183	29.314218	72.541838
597.326741	37.138213	72.546842
596.895913	34.264265	72.551847
596.526618	37.167926	72.556852
595.416130	31.945330	72.561857
594.836934	26.166616	72.566862
594.214644	37.422671	72.571866
593.754542	41.171848	72.576871
593.106563	34.429530	72.581876
591.896225	34.507198	72.586881
591.539753	34.709078	72.591886
590.575285	34.154656	72.596890
590.525995	33.006631	72.601895
589.942468	23.303581	72.606900
588.968498	38.401902	72.611905
588.463836	32.967708	72.616910
588.014337	29.344531	72.621914
587.203023	30.044626	72.626919
586.493707	36.466998	72.631924
586.096005	35.428077	72.636929
585.256728	25.921877	72.641934
583.877694	44.729046	72.646938
583.147072	30.865769	72.651943
583.029553	26.059049	72.656948
582.620863	34.877815	72.661953
582.410194	26.425829	72.666958
580.770459	33.778549	72.671962
580.279988	32.874253	72.676967
579.854327	31.533858	72.681972
579.169221	34.123542	72.686977
578.343299	30.432584	72.691982
577.301304	37.354219	72.696986
577.067944	33.598849	72.701991
576.900226	28.759123	72.706996
575.524524	33.363750	72.712001
575.034690	38.946926	72.717006
574.319209	39.956615	72.722010
574.256888	33.814887	72.727015
573.391681	36.483719	72.732020
572.191495	44.953888	72.737025
571.535225	32.368719	72.742030
571.019796	36.541447	72.747034
570.751495	32.536177	72.752039
569.813206	27.803409	72.757044
568.968587	45.103061	72.762049
568.457414	34.180543	72.767054
567.976849	45.555961	72.772058
567.169290	39.510847	72.777063
566.725271	33.258024	72.782068
565.800530	41.447782	72.787073
565.533217	32.867622	72.792078
564.415098	37.115841	72.797082
563.604788	37.125080	72.802087
562.942309	36.486302	72.807092
562.583448	41.659114	72.812097
562.468035	28.122064	72.817102
561.028511	40.563266	72.822106
560.263777	30.937968	72.827111
560.476311	30.882069	72.832116
559.503780	32.360055	72.837121
558.600282	33.800239	72.842126
557.735611	38.282483	72.847130
557.353420	33.664574	72.852135
557.115647	29.842102	72.857140
555.548803	31.755368	72.862145
555.191330	36.710339	72.867150
554.523514	32.465929	72.872154
554.144271	28.962456	72.877159
553.058188	28.731771	72.882164
552.145147	38.510809	72.887169
551.632297	25.276762	72.892174
551.093664	32.551892	72.897178
550.770028	33.268941	72.902183
550.550135	31.446348	72.907188
549.489363	32.498423	72.912193
549.043263	24.538105	72.917198
548.362416	32.660631	72.922202
547.404153	39.248820	72.927207
546.634800	35.501554	72.932212
546.081747	36.821270	72.937217
545.562105	28.345962	72.942222
544.436414	30.704631	72.947226
543.884681	26.944784	72.952231
543.440979	22.183715	72.957236
542.857096	26.936627	72.962241
542.642914	30.706563	72.967246
541.217580	37.425917	72.972250
540.731962	28.766996	72.977255
540.489252	30.612868	72.982260
539.188518	33.519814	72.987265
538.270602	29.174898	72.992270
537.871333	35.052734	72.997274
537.364690	31.672058	73.002279
537.039559	30.372429	73.007284
536.670926	37.464368	73.012289
535.739682	36.639748	73.017294
534.916817	37.374816	73.022298
534.351359	42.717733	73.027303
533.378885	38.204887	73.032308
532.449200	40.000911	73.037313
532.216593	41.405206	73.042318
531.361605	37.652662	73.047322
530.872166	34.218784	73.052327
529.922029	34.865316	73.057332
529.024839	36.940016	73.062337
528.933409	27.931306	73.067342
528.304245	38.299066	73.072346
527.720867	33.106084	73.077351
527.122605	39.955482	73.082356
525.738613	41.798641	73.087361
525.625315	33.146649	73.092366
525.027818	36.376825	73.097370
524.475074	39.833263	73.102375
523.538618	37.754226	73.107380
522.579350	39.944472	73.112385
522.563087	38.270795	73.117390
521.863675	38.232421	73.122394
520.878265	37.375434	73.127399
520.593613	32.939115	73.132404
519.733092	42.627797	73.137409
519.144897	31.802721	73.142414
518.007996	37.252431	73.147418
517.532535	42.396512	73.152423
517.224368	35.256316	73.157428
516.502291	38.060062	73.162433
515.181245	30.653856	73.167438
514.760889	41.373135	73.172442
514.985336	34.911344	73.177447
515.022831	38.366804	73.182452
513.697134	41.121622	73.187457
512.956838	35.688711	73.192462
511.688900	41.247608	73.197466
511.250319	30.742478	73.202471
510.302923	38.574737	73.207476
508.990091	38.604117	73.212481
508.769309	35.756652	73.217486
508.196143	41.192263	73.222490
507.775536	45.521787	73.227495
507.957969	38.387021	73.232500
506.556021	39.283727	73.237505
505.758815	33.564996	73.242510
505.092154	27.937435	73.247514
504.320118	30.473175	73.252519
503.845027	32.037523	73.257524
502.998466	41.758677	73.262529
502.496155	41.285212	73.267534
501.987658	38.439425	73.272538
500.897890	38.855898	73.277543
500.416971	35.663520	73.282548
499.998054	37.469656	73.287553
499.436424	35.991663	73.292558
498.709793	32.852619	73.297562
498.066311	36.061741	73.302567
497.601142	29.425954	73.307572
496.410023	39.384921	73.312577
495.688828	39.780532	73.317582
495.185459	44.662557	73.322586
494.376903	42.019110	73.327591
494.202834	37.685027	73.332596
492.895247	45.459555	73.337601
492.489274	38.197748	73.342606
492.154598	45.341055	73.347610
491.195287	44.219726	73.352615
490.552250	35.678932	73.357620
489.604319	40.210730	73.362625
489.379901	34.263565	73.367630
488.872527	36.591570	73.372634
488.074111	39.046364	73.377639
487.382917	41.662273	73.382644
486.322533	42.870431	73.387649
486.037548	38.431016	73.392654
484.853602	52.512575	73.397658
484.070545	52.752464	73.402663
483.803647	43.792203	73.407668
483.263785	45.294334	73.412673
483.118031	45.068424	73.417678
482.374672	44.530861	73.422682
481.227629	47.880132	73.427687
480.615995	38.818675	73.432692
479.960668	45.265590	73.437697
479.284301	46.499308	73.442702
478.356609	35.321474	73.447706
477.404235	45.477385	73.452711
477.542882	39.708925	73.457716
476.846442	47.881265	73.462721
476.790501	42.036569	73.467726
475.739523	41.481782	73.472730
474.951125	47.421619	73.477735
473.706129	29.882464	73.482740
472.716969	40.799591	73.487745
472.353316	28.860130	73.492750
471.700905	37.131106	73.497754
471.453725	36.042995	73.502759
471.366451	38.110115	73.507764
470.080638	46.608158	73.512769
469.559153	33.951094	73.517774
468.990967	43.834491	73.522778
468.360719	41.422844	73.527783
467.566299	44.186089	73.532788
466.634238	34.186939	73.537793
466.160977	46.158864	73.542798
465.645040	40.573532	73.547802
464.610597	45.387203	73.552807
463.953543	36.638917	73.557812
463.455959	49.004226	73.562817
463.192659	27.237005	73.567822
461.903158	31.548836	73.572826
460.777971	40.989536	73.577831
460.613897	31.467283	73.582836
459.819983	42.805894	73.587841
459.775611	37.370943	73.592846
459.709193	38.138488	73.597850
458.509848	48.696450	73.602855
457.740112	34.547721	73.607860
456.948447	33.230965	73.612865
456.055612	33.761163	73.617870
455.433440	38.983817	73.622874
454.485957	37.643000	73.627879
454.586947	29.552968	73.632884
453.612160	36.211626	73.637889
452.792871	37.841857	73.642894
452.245518	39.755194	73.647898
451.821998	38.250479	73.652903
451.406758	40.273655	73.657908
450.166831	45.672000	73.662913
449.660157	31.706872	73.667918
449.115200	38.043166	73.672922
448.075089	34.946196	73.677927
447.571823	33.755383	73.682932
446.600316	44.791133	73.687937
446.519406	36.003104	73.692942
445.993318	44.675008	73.697946
444.659294	36.338933	73.702951
444.694423	37.167572	73.707956
443.641559	34.283947	73.712961
443.262405	39.150919	73.717966
442.170228	41.456986	73.722970
441.323653	42.506521	73.727975
441.070402	42.665169	73.732980
440.324900	51.903467	73.737985
439.928162	32.745279	73.742990
438.883031	44.160189	73.747994
438.249645	33.735001	73.752999
438.039166	38.321212	73.758004
437.333854	42.934222	73.763009
436.315385	41.795532	73.768014
435.667109	42.824514	73.773018
435.020899	37.636837	73.778023
434.867543	47.154529	73.783028
433.428689	45.157147	73.788033
432.875110	30.663336	73.793038
432.315706	36.123574	73.798042
431.798203	42.994814	73.803047
431.572494	18.138695	73.808052
430.443804	32.646686	73.813057
430.237142	39.503094	73.818062
429.314872	44.106518	73.823066
428.385690	33.234876	73.828071
427.770034	40.519145	73.833076
426.683639	36.108076	73.838081
426.075429	31.504129	73.843086
425.269232	36.417064	73.848090
424.472325	28.496899	73.853095
424.113206	34.608045	73.858100
423.553824	41.941696	73.863105
423.020680	32.393096	73.868110
422.281020	37.252853	73.873114
421.413679	35.344195	73.878119
421.385416	30.860736	73.883124
420.758291	42.592248	73.888129
420.383809	33.679111	73.893134
419.318230	36.132335	73.898138
418.605724	36.342081	73.903143
418.129388	30.975959	73.908148
417.105739	36.666284	73.913153
416.275083	34.843246	73.918158
415.638805	33.905445	73.923162
415.510353	42.799425	73.928167
415.024378	37.838536	73.933172
413.638132	35.552088	73.938177
412.982839	33.163372	73.943182
412.654626	33.895360	73.948186
412.088701	45.035231	73.953191
411.474893	34.799320	73.958196
410.462157	37.009164	73.963201
410.191808	35.355473	73.968206
409.787723	41.678791	73.973210
408.712549	36.550008	73.978215
407.930693	28.837186	73.983220
407.174295	50.531955	73.988225
407.048567	32.447079	73.993230
406.038082	39.947224	73.998234
405.350849	43.369920	74.003239
404.898264	33.601909	74.008244
403.970434	43.799659	74.013249
403.206718	38.922450	74.018254
402.627477	35.693721	74.023258
401.914279	46.354013	74.028263
401.796092	34.151530	74.033268
400.752418	40.710797	74.038273
399.996611	44.885586	74.043278
399.401082	38.551289	74.048282
398.898939	40.258737	74.053287
398.403820	46.771604	74.058292
397.362007	37.575293	74.063297
396.643061	32.888073	74.068302
396.217521	29.764167	74.073306
395.287543	43.923552	74.078311
394.700635	38.152429	74.083316
393.725009	44.257736	74.088321
393.730693	37.160596	74.093326
393.155118	35.852007	74.098330
392.024670	42.382527	74.103335
391.463506	31.608383	74.108340
390.536924	43.761352	74.113345
390.415698	33.708735	74.118350
389.743750	40.043196	74.123354
388.584837	49.585495	74.128359
388.481754	37.995614	74.133364
387.730583	45.134328	74.138369
386.869871	37.224341	74.143374
386.051267	35.956056	74.148378
385.292274	39.521076	74.153383
385.338455	35.319068	74.158388
384.100327	42.611068	74.163393
383.564759	43.149019	74.168398
382.960079	41.521796	74.173402
382.027564	42.364271	74.178407
382.003871	36.530218	74.183412
380.518101	37.891357	74.188417
379.912654	34.357729	74.193422
379.554414	37.459926	74.198426
379.076511	35.293687	74.203431
378.740931	34.956107	74.208436
377.560541	35.787618	74.213441
376.817668	38.478021	74.218446
376.495946	39.391905	74.223450
375.623583	43.064880	74.228455
374.992410	38.388911	74.233460
373.879662	40.568974	74.238465
373.412222	38.642342	74.243470
373.239433	37.548696	74.248474
372.351750	42.225474	74.253479
371.851686	36.609254	74.258484
370.874925	34.180312	74.263489
370.782987	35.379278	74.268494
369.863881	34.563827	74.273498
368.790674	36.201430	74.278503
368.458662	29.262185	74.283508
368.002713	40.840270	74.288513
367.000776	39.533396	74.293518
366.117647	34.902311	74.298522
365.371659	37.463903	74.303527
365.587904	33.796189	74.308532
364.448151	43.652406	74.313537
363.657539	32.299824	74.318542
362.908156	38.790131	74.323546
362.317562	41.905702	74.328551
362.218394	40.478628	74.333556
360.889629	43.957831	74.338561
360.229521	42.456140	74.343566
359.811649	33.447431	74.348570
359.421700	42.668505	74.353575
358.828634	39.669070	74.358580
357.761467	47.113612	74.363585
356.992174	43.051012	74.368590
356.691602	42.876589	74.373594
355.591793	42.976183	74.378599
355.031085	34.212585	74.383604
354.435587	46.046300	74.388609
353.977836	38.188808	74.393614
353.787146	39.548590	74.398618
352.340155	43.155447	74.403623
352.137557	35.381876	74.408628
351.143876	39.039497	74.413633
350.346201	45.919127	74.418638
349.626411	42.272840	74.423642
349.099976	40.915430	74.428647
348.788210	40.432133	74.433652
348.147619	41.568722	74.438657
347.183393	38.935942	74.443662
346.744791	36.692485	74.448666
345.910632	38.358236	74.453671
345.301654	38.557812	74.458676
344.180314	35.596835	74.463681
343.734804	35.186891	74.468686
343.185195	36.857759	74.473690
342.539276	38.695362	74.478695
342.445526	30.316248	74.483700
341.339404	38.919747	74.488705
340.495505	40.571282	74.493710
339.972863	33.522072	74.498714
339.501703	43.585563	74.503719
338.769024	39.791524	74.508724
337.832861	42.914862	74.513729
337.377627	35.034897	74.518734
336.982377	40.033756	74.523738
335.821982	35.823757	74.528743
335.432420	33.446333	74.533748
334.468742	43.708161	74.538753
334.265089	35.105287	74.543758
333.279260	36.945021	74.548762
332.252319	41.798544	74.553767
331.986132	39.015106	74.558772
331.388130	38.736699	74.563777
331.194672	40.633086	74.568782
330.096987	34.121794	74.573786
329.191430	42.839993	74.578791
328.613412	25.886932	74.583796
328.556772	39.110790	74.588801
327.543375	34.612444	74.593806
326.797392	41.193681	74.598810
326.099281	50.590028	74.603815
325.451215	33.570852	74.608820
324.651877	39.493545	74.613825
323.745751	42.952721	74.618830
323.232085	33.517742	74.623834
322.570628	46.689762	74.628839
322.547980	33.114317	74.633844
321.768734	43.203254	74.638849
320.959108	38.808052	74.643854
320.420623	36.116897	74.648858
319.167352	43.162180	74.653863
318.857956	26.844399	74.658868
317.625036	32.719496	74.663873
317.135090	41.721543	74.668878
317.356004	29.629040	74.673882
316.199633	36.870189	74.678887
315.598140	39.517576	74.683892
315.031007	39.507065	74.688897
314.583988	35.355275	74.693902
313.813679	41.850507	74.698906
312.555372	46.739335	74.703911
312.310271	35.533223	74.708916
311.750746	41.307314	74.713921
310.945279	38.113087	74.718926
310.062836	37.936786	74.723930
309.348563	37.372564	74.728935
309.038545	45.494388	74.733940
308.540912	37.786767	74.738945
307.616962	42.481960	74.743950
306.879684	36.039397	74.748954
306.094983	42.177381	74.753959
305.947582	34.857066	74.758964
304.714194	47.793811	74.763969
303.988037	39.343599	74.768974
303.590006	43.761012	74.773978
303.004632	43.064285	74.778983
302.818359	35.368545	74.783988
301.894240	39.144407	74.788993
301.023185	42.796696	74.793998
300.740827	39.911761	74.799002
299.534663	43.778308	74.804007
299.066074	39.043334	74.809012
298.071481	42.201229	74.814017
297.953677	44.385180	74.819022
296.945181	40.218801	74.824026
295.685102	45.560502	74.829031
295.570756	32.628878	74.834036
295.181417	32.558496	74.839041
294.847819	35.707237	74.844046
293.783849	44.007571	74.849050
292.743399	35.206913	74.854055
292.375101	31.670207	74.859060
292.040727	32.300690	74.864065
291.059744	44.552239	74.869070
290.403993	33.261774	74.874074
289.321417	50.049045	74.879079
289.406408	33.920719	74.884084
288.964319	34.774950	74.889089
287.974624	34.328748	74.894094
287.212186	32.830773	74.899098
286.483210	41.143948	74.904103
285.539062	35.921804	74.909108
284.571569	31.509202	74.914113
283.665495	36.531134	74.919118
283.546111	32.483250	74.924122
283.216225	39.930153	74.929127
283.165108	37.401024	74.934132
282.170647	38.067330	74.939137
281.262963	36.909472	74.944142
280.789729	33.135605	74.949146
280.011063	40.236146	74.954151
279.277123	25.261793	74.959156
278.375620	33.288652	74.964161
277.896982	34.013093	74.969166
277.515696	35.400104	74.974170
276.249747	28.920393	74.979175
275.840193	33.636109	74.984180
275.247980	38.543364	74.989185
275.129617	36.665194	74.994190
274.022149	38.260989	74.999194
273.353098	36.137855	75.004199
272.865917	27.610149	75.009204
271.979320	30.402334	75.014209
271.262319	28.102342	75.019214
270.558571	20.544287	75.024218
269.820607	30.263948	75.029223
269.687548	29.670178	75.034228
268.492805	35.171784	75.039233
267.950315	41.334249	75.044238
267.557154	33.595797	75.049242
266.350318	35.224780	75.054247
265.740910	30.446030	75.059252
265.070371	28.170174	75.064257
264.513626	32.496192	75.069262
264.202467	28.920422	75.074266
263.567564	43.032803	75.079271
262.720944	35.961136	75.084276
262.093506	38.773519	75.089281
261.577342	42.123250	75.094286
260.711107	33.928774	75.099290
259.665936	37.607250	75.104295
259.212452	37.356288	75.109300
258.704229	38.567993	75.114305
258.325996	39.114009	75.119310
257.620962	34.840933	75.124314
256.895321	40.810243	75.129319
256.498613	21.212167	75.134324
255.320422	33.906732	75.139329
254.076731	35.991024	75.144334
253.501351	35.289563	75.149338
252.943115	38.243880	75.154343
252.569314	30.865045	75.159348
252.122783	31.224830	75.164353
251.949031	31.826562	75.169358
251.406143	30.052332	75.174362
250.194252	39.558964	75.179367
249.816323	22.399007	75.184372
248.711407	32.787442	75.189377
247.985965	29.886410	75.194382
247.800906	21.706371	75.199386
246.909362	35.944809	75.204391
246.438731	27.176354	75.209396
245.342015	30.120310	75.214401
244.659064	40.632302	75.219406
244.503522	32.173164	75.224410
243.580223	37.778169	75.229415
242.891432	27.527469	75.234420
242.051407	29.176840	75.239425
241.536256	33.578234	75.244430
240.955271	36.512525	75.249434
239.832056	43.877732	75.254439
239.385675	36.668161	75.259444
238.694994	33.017273	75.264449
238.377275	33.301335	75.269454
238.009320	30.704443	75.274458
236.899967	31.915779	75.279463
236.405549	40.726160	75.284468
236.119223	32.951763	75.289473
234.996783	35.500859	75.294478
234.305465	32.848280	75.299482
233.582299	36.491207	75.304487
233.072565	22.857812	75.309492
232.403627	27.044024	75.314497
231.392014	33.281271	75.319502
230.770648	22.176167	75.324506
230.188696	42.691959	75.329511
229.944710	31.263343	75.334516
229.204850	35.550749	75.339521
227.740265	34.508492	75.344526
227.666774	30.120563	75.349530
227.040959	34.421329	75.354535
226.578908	30.038569	75.359540
226.000770	32.459902	75.364545
225.249265	39.612896	75.369550
225.140832	35.098073	75.374554
223.902213	34.857156	75.379559
223.438977	35.987580	75.384564
222.242107	31.753495	75.389569
221.000723	30.804972	75.394574
220.616641	32.968293	75.399578
219.946465	40.357481	75.404583
219.813490	33.541078	75.409588
219.460856	34.959800	75.414593
218.713370	33.609273	75.419598
217.775761	38.948488	75.424602
216.832043	36.274648	75.429607
216.415160	36.322209	75.434612
216.306213	33.830688	75.439617
215.267833	46.252257	75.444622
214.576702	36.066590	75.449626
213.753811	33.002909	75.454631
213.454877	33.298171	75.459636
212.427333	31.803058	75.464641
211.420185	36.439004	75.469646
211.271343	30.229103	75.474650
210.645884	31.637701	75.479655
209.936197	32.326447	75.484660
209.141898	37.814706	75.489665
208.316865	39.281928	75.494670
208.072936	25.360163	75.499674
207.405603	37.173801	75.504679
206.610773	32.382049	75.509684
205.703546	39.941492	75.514689
205.005812	42.304627	75.519694
204.997631	34.000197	75.524698
203.639176	39.144733	75.529703
203.038090	35.763423	75.534708
202.990158	28.455654	75.539713
202.105908	38.258578	75.544718
201.035705	38.596371	75.549722
200.220424	43.871938	75.554727
200.020334	36.355033	75.559732
199.599056	34.503081	75.564737
198.737153	32.691410	75.569742
197.884571	30.338940	75.574746
197.062127	41.559147	75.579751
196.732246	34.506057	75.584756
196.474942	34.714261	75.589761
195.000204	34.788542	75.594766
194.898525	29.949373	75.599770
194.142778	41.324528	75.604775
193.196357	31.892349	75.609780
192.447840	34.793434	75.614785
191.637695	34.834307	75.619790
191.392799	40.933572	75.624794
190.887222	40.990546	75.629799
189.974792	29.447732	75.634804
189.132127	33.130221	75.639809
188.270228	38.816918	75.644814
188.116297	34.187928	75.649818
187.627204	32.731563	75.654823
187.188007	30.943971	75.659828
186.533776	36.632254	75.664833
185.658712	36.380706	75.669838
184.797082	33.056708	75.674842
183.933529	38.824095	75.679847
183.254150	30.820638	75.684852
182.543314	33.468138	75.689857
182.234772	37.322520	75.694862
181.540700	34.318738	75.699866
180.585954	38.870648	75.704871
180.243913	30.562678	75.709876
179.978933	39.981456	75.714881
178.622893	41.848731	75.719886
177.744535	31.861663	75.724890
177.174131	29.049478	75.729895
176.904865	30.166333	75.734900
176.689744	25.737912	75.739905
175.754380	34.285858	75.744910
174.704113	33.111350	75.749914
174.027435	37.123770	75.754919
174.028794	23.006794	75.759924
172.865719	32.388976	75.764929
172.126332	29.031303	75.769934
171.993467	25.822937	75.774938
170.561957	40.999029	75.779943
169.759197	31.282186	75.784948
169.181973	40.090005	75.789953
168.628744	40.919399	75.794958
168.758467	34.636705	75.799962
167.757010	29.909451	75.804967
166.760284	31.596445	75.809972
165.977436	33.690885	75.814977
165.555840	34.948721	75.819982
165.409096	25.639801	75.824986
164.243033	34.727576	75.829991
163.595444	28.054730	75.834996
162.743777	39.456220	75.840001
162.494820	32.051193	75.845006
162.068169	31.116309	75.850010
160.789455	35.757723	75.855015
160.224576	34.553142	75.860020
160.013953	31.986373	75.865025
158.896257	32.008483	75.870030
158.263610	26.173767	75.875034
157.477214	41.119280	75.880039
157.237034	26.597692	75.885044
156.374461	28.679613	75.890049
155.761032	34.451283	75.895054
155.014090	31.582094	75.900058
154.533909	40.241981	75.905063
153.643641	34.971882	75.910068
152.795256	27.927356	75.915073
152.215422	34.631950	75.920078
151.840132	34.873162	75.925082
151.119818	42.264050	75.930087
150.818350	28.107046	75.935092
149.352587	31.376384	75.940097
149.107538	42.758433	75.945102
148.476358	31.069872	75.950106
147.791439	36.666863	75.955111
146.758692	38.881576	75.960116
146.657714	34.272533	75.965121
145.763464	41.281149	75.970126
145.615064	30.815016	75.975130
144.110605	34.828537	75.980135
143.393066	43.012187	75.985140
142.933364	44.142063	75.990145
142.584917	33.354590	75.995150
142.390101	36.482796	76.000154
141.376999	38.596609	76.005159
140.921765	32.968574	76.010164
139.982245	30.920143	76.015169
138.626236	43.218910	76.020174
138.208999	33.070030	76.025178
137.568921	41.108866	76.030183
137.344797	34.384277	76.035188
137.087655	36.986260	76.040193
136.067171	33.078909	76.045198
135.352156	22.703127	76.050202
134.836012	30.455695	76.055207
133.984636	40.458398	76.060212
133.313904	34.538297	76.065217
132.585998	33.850146	76.070222
132.137293	30.707911	76.075226
130.819789	35.352369	76.080231
130.362883	29.844452	76.085236
129.910954	38.998149	76.090241
129.540433	38.275092	76.095246
128.822860	34.294216	76.100250
127.486321	33.296259	76.105255
127.127763	28.023396	76.110260
127.120508	28.194892	76.115265
126.130221	39.082332	76.120270
125.328872	27.633803	76.125274
124.374227	30.168806	76.130279
124.219414	33.156593	76.135284
123.733665	33.153650	76.140289
122.456146	32.836986	76.145294
122.077668	29.401283	76.150298
121.301064	43.392770	76.155303
120.603454	30.197793	76.160308
119.612801	36.778665	76.165313
118.902590	41.455609	76.170318
118.394078	34.041513	76.175322
117.913446	41.115072	76.180327
117.538944	32.908485	76.185332
117.346411	26.465869	76.190337
116.076193	43.543291	76.195342
115.685205	24.559359	76.200346
114.839827	33.056705	76.205351
114.054376	34.618569	76.210356
113.309307	25.564333	76.215361
112.751227	39.025814	76.220366
112.741901	23.838229	76.225370
111.437967	35.340227	76.230375
110.469132	29.929713	76.235380
109.978816	30.755395	76.240385
109.385961	34.036955	76.245390
108.824637	21.610309	76.250394
107.689512	31.421716	76.255399
107.455426	21.371380	76.260404
106.983901	25.803683	76.265409
106.309398	29.503536	76.270414
105.710141	28.944689	76.275418
104.938158	32.377815	76.280423
104.492856	31.619379	76.285428
103.474623	29.610322	76.290433
102.436673	36.526746	76.295438
102.251717	24.801747	76.300442
101.582196	38.251036	76.305447
101.086700	28.478922	76.310452
100.239342	27.784598	76.315457
99.340641	30.906773	76.320462
98.937854	22.479203	76.325466
98.467085	25.810682	76.330471
97.540877	26.239098	76.335476
96.833643	27.815303	76.340481
95.673620	31.116343	76.345486
95.703515	30.488714	76.350490
95.301889	28.949037	76.355495
94.402055	31.372810	76.360500
93.534950	29.836396	76.365505
93.048763	31.897744	76.370510
92.466740	16.413566	76.375514
91.728013	31.223746	76.380519
90.560675	33.344827	76.385524
90.711841	30.217331	76.390529
89.835112	33.435353	76.395534
88.947939	32.759997	76.400538
88.062124	36.198664	76.405543
87.753409	25.844842	76.410548
87.417272	26.218591	76.415553
86.090086	24.004922	76.420558
85.455600	22.712113	76.425562
84.747680	31.588089	76.430567
84.594385	36.043768	76.435572
83.996396	25.081645	76.440577
82.946484	28.156975	76.445582
82.700337	19.187197	76.450586
81.711344	32.305808	76.455591
80.724182	38.963408	76.460596
80.058985	34.925310	76.465601
79.410918	39.459890	76.470606
79.042453	34.600196	76.475610
78.526501	32.525246	76.480615
78.084188	31.069331	76.485620
77.100003	34.488995	76.490625
76.149200	31.721728	76.495630
76.102358	27.771106	76.500634
75.288131	38.758217	76.505639
74.258985	35.129817	76.510644
74.135190	26.958957	76.515649
73.466749	34.049851	76.520654
72.486639	20.251832	76.525658
71.623873	33.314048	76.530663
71.022950	33.048786	76.535668
70.658414	32.133975	76.540673
69.897953	38.140419	76.545678
69.061608	28.454208	76.550682
68.308794	27.817357	76.555687
67.990541	29.520772	76.560692
67.355967	24.793406	76.565697
66.199293	30.803108	76.570702
65.803889	21.204281	76.575706
65.321175	25.553219	76.580711
64.638883	30.276182	76.585716
63.863737	32.695851	76.590721
63.233553	28.742062	76.595726
62.725723	31.712031	76.600730
62.126649	25.009407	76.605735
60.898456	27.274245	76.610740
60.303152	28.430490	76.615745
59.470728	26.454900	76.620750
59.637698	25.215635	76.625754
58.997502	32.765648	76.630759
58.140164	36.500979	76.635764
57.333823	30.772841	76.640769
56.393746	29.226001	76.645774
56.237174	33.764203	76.650778
54.875106	35.564697	76.655783
54.244541	27.323271	76.660788
53.901451	28.497642	76.665793
53.386436	39.941662	76.670798
53.077289	24.204242	76.675802
51.789425	33.186904	76.680807
51.233680	27.469267	76.685812
50.931056	25.275150	76.690817
49.909823	30.895832	76.695822
49.441082	21.554707	76.700826
48.452272	24.905732	76.705831
48.325593	32.235082	76.710836
47.812805	25.547086	76.715841
46.709558	29.745833	76.720846
46.515732	26.652855	76.725850
45.689903	38.233175	76.730855
44.200084	30.388979	76.735860
44.076155	26.163650	76.740865
43.248557	29.354928	76.745870
43.103766	22.228204	76.750874
42.110362	26.447281	76.755879
41.068016	23.484897	76.760884
40.703331	25.384952	76.765889
40.004988	21.339542	76.770894
39.818555	29.244540	76.775898
38.696357	26.514085	76.780903
37.854584	29.048465	76.785908
37.578579	26.008018	76.790913
37.213463	26.110431	76.795918
36.473170	19.099182	76.800922
35.520497	25.767059	76.805927
34.780699	29.113070	76.810932
34.233847	27.282755	76.815937
33.242189	32.654301	76.820942
32.791062	15.201752	76.825946
32.170167	22.045371	76.830951
31.420939	26.151394	76.835956
31.098339	22.249486	76.840961
29.948229	21.251814	76.845966
29.385279	21.658590	76.850970
28.845001	27.155265	76.855975
28.234130	21.304505	76.860980
27.461554	18.917263	76.865985
26.568459	31.538050	76.870990
26.362044	17.987245	76.875994
25.485912	32.029303	76.880999
25.121025	29.370460	76.886004
24.036067	25.858219	76.891009
23.136295	33.842296	76.896014
22.937342	22.550053	76.901018
22.547056	28.808123	76.906023
22.073262	24.805752	76.911028
21.271109	22.923119	76.916033
20.561060	25.676189	76.921038
19.758625	24.235144	76.926042
18.733058	33.084524	76.931047
17.662038	30.714921	76.936052
17.292479	17.915530	76.941057
17.146936	26.760168	76.946062
16.937401	13.030097	76.951066
15.646411	22.346000	76.956071
14.792967	21.834025	76.961076
14.605485	17.825416	76.966081
13.484149	26.433028	76.971086
12.776866	22.595631	76.976090
12.124122	33.474995	76.981095
11.697891	32.629957	76.986100
11.521889	32.183399	76.991105
10.397901	37.454636	76.996110
9.693726	27.700065	77.001114
9.095619	32.215650	77.006119
8.565303	36.296227	77.011124
7.697747	26.430522	77.016129
6.545320	29.249423	77.021134
6.281283	31.586012	77.026139
5.965796	29.321413	77.031143
5.477354	34.048165	77.036148
4.488379	22.121846	77.041153
3.798956	28.260473	77.046158