Fri Mar 05 20:33:02 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-2.097293	103.413678	0.000000
-2.252023	90.619417	0.005005
-2.914809	61.701558	0.010010
-4.476148	19.529433	0.015014
-8.142376	-2.770192	0.020019
-13.341897	-1.390402	0.025024
-18.568934	3.805238	0.030029
-23.016658	-10.035588	0.035034
-27.491539	6.411351	0.040038
-31.325691	10.437087	0.045043
-34.794287	-4.761539	0.050048
-38.342804	2.750970	0.055053
-41.626773	-3.744039	0.060058
-45.512698	9.150766	0.065062
-49.446406	-1.433648	0.070067
-53.200888	-1.414961	0.075072
-56.875667	4.829363	0.080077
-60.428385	-1.334167	0.085082
-64.569723	9.073590	0.090086
-68.277344	2.759744	0.095091
-72.096926	0.033944	0.100096
-76.069158	5.923634	0.105101
-79.326010	0.381549	0.110106
-83.370119	2.244194	0.115110
-87.032972	-3.393950	0.120115
-91.248450	-2.500573	0.125120
-95.163035	10.466686	0.130125
-98.226735	-1.440729	0.135130
-101.880821	3.646044	0.140134
-105.809118	-8.910294	0.145139
-109.315279	-2.393184	0.150144
-113.075875	-1.622809	0.155149
-116.895439	-6.116279	0.160154
-120.993099	-5.071341	0.165158
-124.930213	-15.714991	0.170163
-128.674013	-12.648109	0.175168
-132.750200	-5.437624	0.180173
-136.608515	-4.501813	0.185178
-140.192865	-5.030526	0.190182
-143.803388	-1.440844	0.195187
-147.166141	3.416583	0.200192
-151.342434	-2.946919	0.205197
-154.885759	-2.278958	0.210202
-158.964866	5.655850	0.215206
-162.478568	-6.261661	0.220211
-166.082337	-16.906394	0.225216
-170.233820	-2.131917	0.230221
-173.936576	-3.952114	0.235226
-177.512833	-6.599880	0.240230
-181.265867	-2.052282	0.245235
-184.397715	-1.170827	0.250240
-188.718391	-4.716898	0.255245
-192.587015	-5.372051	0.260250
-196.261597	-0.959951	0.265254
-200.292272	0.713088	0.270259
-203.793672	-7.267148	0.275264
-208.034803	-3.693424	0.280269
-211.012888	-4.834445	0.285274
-215.043683	-1.067200	0.290278
-218.569695	-6.827898	0.295283
-222.348544	0.475624	0.300288
-226.527884	6.020144	0.305293
-230.031908	-0.617668	0.310298
-234.110988	-1.511974	0.315302
-237.436475	3.233972	0.320307
-240.949472	2.023825	0.325312
-245.350003	0.546919	0.330317
-249.073644	0.363871	0.335322
-252.826246	6.105246	0.340326
-256.617046	5.953429	0.345331
-260.189573	2.277032	0.350336
-263.966777	11.351251	0.355341
-267.636094	-5.188468	0.360346
-271.418591	2.393250	0.365350
-275.548334	5.214463	0.370355
-278.785130	0.088922	0.375360
-283.033987	1.811118	0.380365
-286.594926	-6.042794	0.385370
-290.303723	5.007470	0.390374
-294.299467	-0.102552	0.395379
-297.768298	-4.478253	0.400384
-301.761628	4.304094	0.405389
-305.720341	0.150107	0.410394
-309.232444	4.031821	0.415398
-312.775884	0.234169	0.420403
-316.546449	1.531568	0.425408
-320.279910	5.759291	0.430413
-323.952560	-5.801434	0.435418
-327.891126	2.309901	0.440422
-331.915251	5.071770	0.445427
-335.497902	-4.740298	0.450432
-339.515510	5.701759	0.455437
-342.954556	-3.906146	0.460442
-346.853499	-2.135626	0.465446
-350.294236	4.625260	0.470451
-354.057013	0.667150	0.475456
-358.428668	6.627366	0.480461
-361.879759	4.965974	0.485466
-365.641226	8.125926	0.490470
-369.223980	1.095626	0.495475
-372.675059	-3.837875	0.500480
-377.100079	6.530521	0.505485
-380.720089	-6.219633	0.510490
-384.423215	-0.971656	0.515494
-388.240610	-2.982946	0.520499
-391.730194	-5.313071	0.525504
-395.918138	4.217999	0.530509
-399.447034	-5.787049	0.535514
-403.222296	-2.197491	0.540518
-407.073970	-6.702704	0.545523
-410.750596	-9.778781	0.550528
-414.602665	2.614422	0.555533
-418.120764	-0.881192	0.560538
-421.951553	5.383846	0.565542
-425.606896	5.075051	0.570547
-429.334490	-9.621113	0.575552
-433.483990	2.417498	0.580557
-437.266908	1.903593	0.585562
-441.047094	9.693353	0.590566
-444.703359	4.223453	0.595571
-448.181985	-1.380462	0.600576
-452.016470	5.679983	0.605581
-455.523290	-1.105267	0.610586
-459.714341	5.174785	0.615590
-463.791185	3.105705	0.620595
-467.130502	0.783231	0.625600
-471.032100	8.491502	0.630605
-474.524503	-3.405261	0.635610
-478.366123	2.133053	0.640614
-482.217610	6.837179	0.645619
-486.152232	-3.465627	0.650624
-490.123513	6.365304	0.655629
-492.989171	2.885446	0.660634
-497.163297	3.749273	0.665638
-501.154711	7.775623	0.670643
-504.745865	1.923265	0.675648
-508.947409	9.313656	0.680653
-512.477979	-0.886487	0.685658
-516.333102	8.399241	0.690662
-519.846680	4.658634	0.695667
-523.313773	1.795263	0.700672
-527.250621	7.790404	0.705677
-530.867451	5.124423	0.710682
-534.904081	-1.751115	0.715686
-538.633197	7.776288	0.720691
-542.634028	-3.903537	0.725696
-546.301568	4.667886	0.730701
-549.309188	4.705239	0.735706
-553.463285	2.489385	0.740710
-557.651513	4.349033	0.745715
-561.416985	0.028998	0.750720
-565.221633	-2.417695	0.755725
-568.816464	-2.472590	0.760730
-572.498540	2.255075	0.765734
-575.947172	4.209491	0.770739
-579.604299	-5.255978	0.775744
-583.774853	6.666396	0.780749
-587.569735	-3.453555	0.785754
-591.573190	4.618097	0.790758
-595.401859	4.343561	0.795763
-598.914544	6.166319	0.800768
-602.607867	5.928517	0.805773
-606.002873	-4.718901	0.810778
-610.104626	4.786139	0.815782
-614.228419	2.513513	0.820787
-617.681991	-5.987798	0.825792
-621.865346	0.206143	0.830797
-625.018821	-0.474258	0.835802
-628.277374	0.019594	0.840806
-632.156701	-0.320905	0.845811
-636.202795	3.334363	0.850816
-640.412632	5.199185	0.855821
-644.114128	-1.704475	0.860826
-647.841696	-3.266079	0.865830
-651.691238	3.633077	0.870835
-655.150025	-0.354193	0.875840
-659.267927	7.778432	0.880845
-662.869906	1.663131	0.885850
-666.597921	-2.080832	0.890854
-670.413161	7.615064	0.895859
-673.788377	3.992929	0.900864
-677.995348	4.592667	0.905869
-681.672685	3.153974	0.910874
-684.998157	3.035713	0.915878
-689.205097	1.687967	0.920883
-692.602259	-5.924973	0.925888
-696.566585	-0.768828	0.930893
-700.381990	-0.512314	0.935898
-704.180925	0.689303	0.940902
-707.770809	2.649134	0.945907
-711.836358	-5.973425	0.950912
-715.586817	0.700264	0.955917
-718.960345	1.209461	0.960922
-722.896851	8.315011	0.965926
-726.867705	2.717646	0.970931
-730.446812	-2.120741	0.975936
-734.253149	-1.838814	0.980941
-738.070955	6.189211	0.985946
-741.928529	8.499375	0.990950
-745.616893	5.701660	0.995955
-749.028787	-6.735794	1.000960
-753.364032	4.535100	1.005965
-756.895084	-0.965349	1.010970
-760.491214	-3.243202	1.015974
-764.387422	2.283781	1.020979
-768.184736	1.432091	1.025984
-771.959481	9.417018	1.030989
-775.550890	-4.276895	1.035994
-779.587450	3.972234	1.040998
-783.206335	5.293430	1.046003
-786.557867	-6.480268	1.051008
-790.241083	3.224664	1.056013
-794.625150	6.079528	1.061018
-798.420468	-8.688747	1.066022
-801.934882	4.102059	1.071027
-805.273769	-1.602491	1.076032
-809.515167	6.228430	1.081037
-813.147231	0.635408	1.086042
-816.930520	6.420388	1.091046
-820.969004	6.080410	1.096051
-824.606031	1.152083	1.101056
-828.111944	3.368325	1.106061
-832.221609	2.470478	1.111066
-835.999031	0.215414	1.116070
-839.993111	8.166121	1.121075
-843.431264	3.817876	1.126080
-846.908241	8.252976	1.131085
-850.652305	0.169040	1.136090
-854.581087	1.661309	1.141094
-858.554014	7.806246	1.146099
-862.032170	2.411042	1.151104
-866.094499	2.410839	1.156109
-869.702762	-7.451459	1.161114
-873.099625	1.488739	1.166118
-876.930876	6.751635	1.171123
-880.538975	1.996963	1.176128
-884.928459	6.712046	1.181133
-888.462182	0.945730	1.186138
-892.244675	-4.575805	1.191142
-896.221141	-2.314192	1.196147
-899.770909	-4.093051	1.201152
-903.483983	11.716344	1.206157
-907.250411	9.439137	1.211162
-911.289219	5.330532	1.216166
-914.976268	4.231220	1.221171
-918.572651	4.143991	1.226176
-922.456485	3.065117	1.231181
-925.975392	-2.785507	1.236186
-929.688243	5.271760	1.241190
-933.619958	6.312054	1.246195
-937.066090	0.736808	1.251200
-940.743043	-3.527373	1.256205
-944.674663	-2.116500	1.261210
-948.658650	-1.890973	1.266214
-952.374486	-2.990353	1.271219
-956.111896	3.082388	1.276224
-960.079270	3.133394	1.281229
-963.945570	3.075205	1.286234
-967.550939	-3.321333	1.291238
-971.338672	7.529653	1.296243
-974.729269	-3.620932	1.301248
-978.732494	1.496163	1.306253
-982.491908	-8.051623	1.311258
-986.507704	-3.080736	1.316262
-990.440491	7.121709	1.321267
-993.595334	-7.158880	1.326272
-997.770008	-2.982561	1.331277
-1001.384496	-1.448852	1.336282
-1004.935774	-1.409124	1.341286
-1008.852416	-2.586682	1.346291
-1012.660841	-4.979997	1.351296
-1016.402751	5.691843	1.356301
-1020.092888	-4.467766	1.361306
-1024.076133	5.528340	1.366310
-1027.744293	1.516776	1.371315
-1031.095957	-2.796131	1.376320
-1035.084972	3.020513	1.381325
-1039.194219	6.664482	1.386330
-1042.707046	8.697647	1.391334
-1046.561304	6.406332	1.396339
-1049.797652	-3.247083	1.401344
-1053.704449	-1.366924	1.406349
-1057.937406	2.454555	1.411354
-1061.824238	7.452250	1.416358
-1065.626414	2.877148	1.421363
-1068.877589	0.543020	1.426368
-1072.587298	10.126454	1.431373
-1076.444227	-2.630369	1.436378
-1080.183066	0.113923	1.441382
-1084.563861	11.816869	1.446387
-1087.856501	-2.698576	1.451392
-1091.281597	0.372427	1.456397
-1095.232794	-12.831308	1.461402
-1099.375195	-4.873807	1.466406
-1103.074214	0.852403	1.471411
-1106.447905	2.385599	1.476416
-1110.812560	1.995803	1.481421
-1113.896303	-5.560977	1.486426
-1117.600784	-3.132775	1.491430
-1121.668330	-6.123105	1.496435
-1125.179909	-11.078897	1.501440
-1129.338385	1.954159	1.506445
-1133.374094	-3.521729	1.511450
-1136.840041	1.027136	1.516454
-1140.621444	0.129355	1.521459
-1143.786391	-7.840157	1.526464
-1147.908755	5.124079	1.531469
-1151.810513	-0.948782	1.536474
-1155.518510	6.040477	1.541478
-1159.231656	13.669219	1.546483
-1162.784946	-3.426813	1.551488
-1167.151890	-7.179691	1.556493
-1170.507785	-6.833513	1.561498
-1174.056996	2.110969	1.566502
-1178.147880	5.487318	1.571507
-1181.821416	2.933932	1.576512
-1185.647512	10.752669	1.581517
-1189.462409	-1.882946	1.586522
-1193.015277	-9.784006	1.591526
-1196.999030	4.296659	1.596531
-1200.546360	4.190978	1.601536
-1204.666089	-1.132570	1.606541
-1208.159637	-1.850804	1.611546
-1211.663048	-5.785930	1.616550
-1215.828398	-4.895430	1.621555
-1219.309834	-5.192972	1.626560
-1223.495075	4.250743	1.631565
-1227.043710	3.587083	1.636570
-1230.760152	3.522703	1.641574
-1234.538086	0.397920	1.646579
-1237.823986	-6.210147	1.651584
-1241.933951	3.577934	1.656589
-1245.976236	-8.453497	1.661594
-1249.800302	-0.772181	1.666598
-1253.563796	5.587459	1.671603
-1257.098830	-3.423347	1.676608
-1260.575127	-2.464851	1.681613
-1264.583736	-8.498333	1.686618
-1268.568975	2.704819	1.691622
-1272.227279	0.571754	1.696627
-1276.024273	-5.946574	1.701632
-1279.997457	0.956008	1.706637
-1283.452579	-1.159097	1.711642
-1286.726120	-5.045744	1.716646
-1290.683779	-0.422689	1.721651
-1294.312018	-5.670197	1.726656
-1298.892576	-2.060729	1.731661
-1302.238718	-2.657337	1.736666
-1305.832326	-3.774133	1.741670
-1309.870759	-7.557240	1.746675
-1313.395602	-8.883722	1.751680
-1317.787465	-7.229828	1.756685
-1321.038488	-2.423371	1.761690
-1324.604325	-2.128518	1.766694
-1328.567407	-3.337521	1.771699
-1332.041317	-12.763249	1.776704
-1336.095840	0.573619	1.781709
-1339.818279	-6.262453	1.786714
-1343.370979	-3.121776	1.791718
-1347.526467	5.260858	1.796723
-1350.660848	-7.022941	1.801728
-1355.181449	-2.164588	1.806733
-1358.827140	-2.530239	1.811738
-1362.653993	-2.508926	1.816742
-1366.092740	-1.617782	1.821747
-1369.339883	0.417490	1.826752
-1373.714414	-0.511108	1.831757
-1377.159124	-5.970784	1.836762
-1380.880387	-6.649145	1.841766
-1384.987888	4.026580	1.846771
-1388.889770	-1.714693	1.851776
-1392.839959	2.549379	1.856781
-1396.242702	-1.114580	1.861786
-1399.815214	-8.189013	1.866790
-1403.525772	-9.446200	1.871795
-1407.310706	-7.512426	1.876800
-1411.346138	6.157393	1.881805
-1415.277527	-4.808139	1.886810
-1419.007496	-7.639101	1.891814
-1422.583283	-6.331705	1.896819
-1426.064105	-6.211152	1.901824
-1429.989036	1.759402	1.906829
-1433.990174	-2.534066	1.911834
-1437.491559	3.640394	1.916838
-1441.436933	4.146004	1.921843
-1445.141433	4.103710	1.926848
-1449.045490	5.714438	1.931853
-1452.872104	-0.202774	1.936858
-1456.410829	-2.427227	1.941862
-1460.223962	-1.632109	1.946867
-1463.566336	-3.861184	1.951872
-1467.892432	1.100277	1.956877
-1471.500377	-2.775129	1.961882
-1475.340079	-7.305678	1.966886
-1479.054378	-1.940710	1.971891
-1483.033295	-5.862344	1.976896
-1486.702539	5.866129	1.981901
-1489.839282	-3.641727	1.986906
-1493.768261	0.095583	1.991910
-1497.810119	-3.943675	1.996915
-1501.989969	0.067033	2.006912
-1502.686454	-0.923442	2.016909
-1499.929879	-3.658995	2.026906
-1497.124504	-3.432400	2.036902
-1495.186890	2.236777	2.046899
-1493.431616	-3.512060	2.056896
-1491.633151	-7.608360	2.066893
-1489.713263	-6.652593	2.076890
-1487.411070	-4.520168	2.086886
-1485.403940	-6.403067	2.096883
-1483.765487	0.446117	2.106880
-1481.954562	4.507721	2.116877
-1479.990843	6.343835	2.126874
-1478.184068	0.924650	2.136870
-1476.352279	-0.895427	2.146867
-1474.366070	-3.734954	2.156864
-1472.171557	-5.087329	2.166861
-1470.664262	-1.678139	2.176858
-1468.729390	-4.645228	2.186854
-1466.739966	-3.637419	2.196851
-1464.689166	-0.454202	2.206848
-1463.017917	3.459260	2.216845
-1461.090553	-6.247060	2.226842
-1459.164729	3.500826	2.236838
-1457.133657	6.273532	2.246835
-1455.560640	-9.128074	2.256832
-1453.745020	-5.463512	2.266829
-1451.666603	-5.992025	2.276826
-1449.676708	-5.285852	2.286822
-1447.819312	1.073572	2.296819
-1446.097457	-1.824654	2.306816
-1444.144199	-5.239925	2.316813
-1442.044393	-6.221848	2.326810
-1440.406204	5.548929	2.336806
-1438.469705	0.825836	2.346803
-1436.747622	1.435956	2.356800
-1434.583360	-5.534100	2.366797
-1432.885793	-3.072707	2.376794
-1430.897196	-8.487809	2.386790
-1429.176713	-7.735323	2.396787
-1427.007174	-0.544819	2.406784
-1425.418409	-3.860663	2.416781
-1423.367283	-2.584804	2.426778
-1421.493143	3.397757	2.436774
-1419.957379	1.194073	2.446771
-1417.595470	1.411244	2.456768
-1415.742558	-5.452105	2.466765
-1413.960080	-3.155869	2.476762
-1412.299643	3.525644	2.486758
-1410.303134	-1.183351	2.496755
-1408.385413	0.066513	2.506752
-1406.497285	-0.164655	2.516749
-1404.592557	-1.102681	2.526746
-1402.453774	2.088613	2.536742
-1400.720188	11.643130	2.546739
-1399.307923	1.720901	2.556736
-1397.142955	-1.680859	2.566733
-1395.312975	3.475121	2.576730
-1393.317164	5.113544	2.586726
-1391.335654	1.624319	2.596723
-1389.679178	7.439654	2.606720
-1387.737806	1.398993	2.616717
-1385.980044	1.477657	2.626714
-1383.912912	3.884661	2.636710
-1381.960416	4.309516	2.646707
-1380.433265	4.906676	2.656704
-1378.224401	2.607892	2.666701
-1376.174243	7.741274	2.676698
-1374.522439	7.514807	2.686694
-1372.742079	6.585665	2.696691
-1370.762076	0.988827	2.706688
-1368.955587	-2.835513	2.716685
-1367.095483	3.678284	2.726682
-1365.356504	4.582593	2.736678
-1363.236365	5.302728	2.746675
-1361.584307	6.170429	2.756672
-1359.439040	6.752337	2.766669
-1357.512533	-1.692209	2.776666
-1355.719827	7.110784	2.786662
-1354.032286	9.292795	2.796659
-1352.081422	1.908552	2.806656
-1350.050655	5.331923	2.816653
-1348.090854	2.809355	2.826650
-1346.577497	9.061315	2.836646
-1344.395903	5.036420	2.846643
-1342.680100	0.028207	2.856640
-1340.595758	1.854607	2.866637
-1338.931643	-1.665871	2.876634
-1337.305606	2.488606	2.886630
-1335.126825	-0.692681	2.896627
-1333.483254	6.269488	2.906624
-1331.237259	6.339514	2.916621
-1329.345477	4.770471	2.926618
-1327.724969	2.840646	2.936614
-1325.531390	-0.535630	2.946611
-1323.962492	4.995356	2.956608
-1322.007501	1.829377	2.966605
-1320.119643	2.752520	2.976602
-1318.273781	7.523925	2.986598
-1316.232246	10.110350	2.996595
-1314.395621	2.101796	3.006592
-1312.489248	8.112454	3.016589
-1310.781460	6.137091	3.026586
-1309.290486	1.805933	3.036582
-1306.872534	2.071088	3.046579
-1305.207901	5.766260	3.056576
-1303.139739	4.963208	3.066573
-1301.249387	1.314965	3.076570
-1299.522475	3.564925	3.086566
-1297.444508	8.806034	3.096563
-1295.619964	-1.243708	3.106560
-1293.913621	6.643171	3.116557
-1292.002479	5.898419	3.126554
-1290.318768	1.744843	3.136550
-1288.229016	5.237776	3.146547
-1286.338806	4.584799	3.156544
-1284.273289	3.373244	3.166541
-1282.572744	3.181674	3.176538
-1280.719543	3.774085	3.186534
-1278.739020	2.020354	3.196531
-1276.928302	3.555873	3.206528
-1274.910316	-3.572212	3.216525
-1273.286754	5.587919	3.226522
-1271.346273	1.167474	3.236518
-1269.429664	1.206593	3.246515
-1267.356577	-1.283513	3.256512
-1265.682555	-0.030841	3.266509
-1263.764026	4.558454	3.276506
-1261.964625	8.909452	3.286502
-1260.324410	7.748616	3.296499
-1258.173699	5.137148	3.306496
-1256.321502	-0.756509	3.316493
-1254.013626	7.804654	3.326490
-1252.370909	7.895516	3.336486
-1250.766176	11.819788	3.346483
-1248.835583	8.247248	3.356480
-1246.971464	4.041146	3.366477
-1245.276022	1.347813	3.376474
-1243.117811	-1.244314	3.386470
-1241.269278	-1.252698	3.396467
-1239.607580	3.314563	3.406464
-1237.579053	-1.778359	3.416461
-1235.445251	3.490187	3.426458
-1233.795200	7.495639	3.436454
-1231.941845	6.494922	3.446451
-1230.034309	10.190754	3.456448
-1228.045456	5.573129	3.466445
-1226.058787	5.533179	3.476442
-1224.363573	2.388323	3.486438
-1222.772462	5.498487	3.496435
-1220.639890	-1.652630	3.506432
-1218.844045	7.795763	3.516429
-1216.858786	-2.107540	3.526426
-1215.077249	2.219512	3.536422
-1213.222404	4.265910	3.546419
-1211.304347	2.225393	3.556416
-1209.241255	4.102683	3.566413
-1207.451054	0.352119	3.576410
-1205.851064	-2.335384	3.586406
-1203.505986	-1.082680	3.596403
-1201.530905	2.354474	3.606400
-1199.953841	-0.924615	3.616397
-1198.148754	-1.366534	3.626394
-1196.343020	-0.303833	3.636390
-1194.505896	-0.322985	3.646387
-1192.406598	4.553235	3.656384
-1190.435112	3.922066	3.666381
-1189.148422	3.269422	3.676378
-1187.212410	12.464894	3.686374
-1184.864558	7.595651	3.696371
-1183.123617	9.335040	3.706368
-1181.252218	9.010418	3.716365
-1179.534483	9.318273	3.726362
-1177.289931	8.390794	3.736358
-1175.281141	6.599469	3.746355
-1173.747511	10.952013	3.756352
-1171.994692	8.372707	3.766349
-1169.786899	8.336898	3.776346
-1168.058230	8.205648	3.786342
-1166.296761	9.752294	3.796339
-1164.495281	13.057788	3.806336
-1162.555792	10.222834	3.816333
-1160.488462	5.660601	3.826330
-1158.694569	8.362581	3.836326
-1156.719500	11.654517	3.846323
-1155.080841	7.582449	3.856320
-1153.039769	8.757531	3.866317
-1151.254736	1.815231	3.876314
-1149.423522	-1.706590	3.886310
-1147.257213	-1.868371	3.896307
-1145.467446	0.032180	3.906304
-1143.582552	0.886470	3.916301
-1141.627329	0.371628	3.926298
-1139.977872	9.576672	3.936294
-1138.551146	11.492682	3.946291
-1136.352380	8.898897	3.956288
-1134.374811	5.262092	3.966285
-1132.420806	3.140098	3.976282
-1130.525112	0.151127	3.986278
-1128.551377	8.574833	3.996275
-1127.040418	10.229482	4.006272
-1124.885730	9.913266	4.016269
-1122.975817	10.007262	4.026266
-1120.917538	3.014953	4.036262
-1119.245215	2.441178	4.046259
-1117.690569	6.550400	4.056256
-1115.275061	2.619342	4.066253
-1113.777149	-0.178086	4.076250
-1112.076342	5.150377	4.086246
-1109.780173	4.869963	4.096243
-1107.957118	-1.284184	4.106240
-1106.152151	4.108147	4.116237
-1104.561014	0.869498	4.126234
-1102.482473	-0.904501	4.136230
-1100.439379	3.380802	4.146227
-1098.437561	2.988014	4.156224
-1096.781570	3.146336	4.166221
-1095.053379	-0.870540	4.176218
-1092.977919	-1.410891	4.186214
-1091.129120	3.941282	4.196211
-1089.121150	0.564912	4.206208
-1087.697210	0.228260	4.216205
-1085.758002	4.487564	4.226202
-1083.327197	3.983535	4.236198
-1081.710297	7.400725	4.246195
-1079.742202	3.503377	4.256192
-1077.950765	4.317408	4.266189
-1076.073763	-2.148501	4.276186
-1074.459042	3.485865	4.286182
-1072.314295	7.349150	4.296179
-1070.445471	4.836624	4.306176
-1068.360657	4.189009	4.316173
-1066.979590	4.325013	4.326170
-1064.971185	0.866489	4.336166
-1062.916099	1.354151	4.346163
-1061.218911	0.962754	4.356160
-1059.408806	4.472213	4.366157
-1057.214124	5.243864	4.376154
-1055.349121	6.409301	4.386150
-1053.809193	9.535669	4.396147
-1051.835309	4.860580	4.406144
-1049.633843	0.445933	4.416141
-1047.847001	6.415944	4.426138
-1046.443060	8.938809	4.436134
-1044.136676	3.539497	4.446131
-1042.164041	-0.238548	4.456128
-1040.696892	-0.397348	4.466125
-1038.657962	5.584456	4.476122
-1037.025668	4.892406	4.486118
-1034.932414	-1.597009	4.496115
-1033.035784	-0.131879	4.506112
-1030.933203	-1.075984	4.516109
-1029.060469	2.420324	4.526106
-1027.088937	3.112432	4.536102
-1025.738616	2.786013	4.546099
-1023.668479	5.903388	4.556096
-1021.637091	2.921220	4.566093
-1019.652781	1.560254	4.576090
-1017.965759	0.311574	4.586086
-1016.315837	-2.211687	4.596083
-1014.401931	-3.250337	4.606080
-1012.280414	-6.717433	4.616077
-1010.420590	-8.947421	4.626074
-1008.577145	-1.006449	4.636070
-1006.955274	2.436841	4.646067
-1004.803559	3.584885	4.656064
-1002.878699	-3.997036	4.666061
-1001.293511	-2.390493	4.676058
-999.225270	-1.919089	4.686054
-997.361004	11.440634	4.696051
-995.164342	12.054135	4.706048
-993.544614	9.212034	4.716045
-991.809506	2.953613	4.726042
-989.937414	-0.276209	4.736038
-988.021157	1.842657	4.746035
-986.063715	5.259139	4.756032
-984.183129	5.201624	4.766029
-982.093480	3.035955	4.776026
-980.536192	6.908012	4.786022
-978.869139	7.317278	4.796019
-976.535122	8.418827	4.806016
-974.737858	1.376799	4.816013
-972.765882	1.443624	4.826010
-971.110944	0.774841	4.836006
-969.348013	1.792461	4.846003
-966.976478	8.752189	4.856000
-965.607836	3.667118	4.865997
-963.466110	1.415769	4.875994
-961.567947	2.165455	4.885990
-959.692001	1.113972	4.895987
-958.053783	5.219417	4.905984
-956.292591	4.247865	4.915981
-954.378093	2.449700	4.925978
-952.174120	2.901020	4.935974
-950.356355	2.048320	4.945971
-948.575143	-0.933255	4.955968
-946.424153	6.477021	4.965965
-944.891942	3.696316	4.975962
-943.128698	3.562862	4.985958
-940.976430	5.501924	4.995955
-939.188672	5.044028	5.005952
-937.279852	7.337810	5.015949
-935.346450	3.045074	5.025946
-933.561079	5.099653	5.035942
-931.761476	7.673007	5.045939
-930.075584	7.444563	5.055936
-927.723819	7.498066	5.065933
-925.790620	7.405344	5.075930
-924.132065	8.299162	5.085926
-922.218252	10.716895	5.095923
-920.458389	0.257749	5.105920
-918.584077	2.593378	5.115917
-916.776598	7.023894	5.125914
-914.590846	2.995560	5.135910
-912.905234	-0.141229	5.145907
-911.000023	4.540504	5.155904
-909.142055	2.452994	5.165901
-907.428380	-0.224070	5.175898
-905.306768	7.426207	5.185894
-903.562472	6.204765	5.195891
-901.499326	8.214957	5.205888
-899.851549	0.192677	5.215885
-897.819933	-0.157336	5.225882
-896.104531	-0.321001	5.235878
-894.167302	2.776690	5.245875
-892.289519	4.112320	5.255872
-890.309362	7.182625	5.265869
-888.119984	3.243735	5.275866
-886.545098	0.562032	5.285862
-884.741107	4.838395	5.295859
-882.970744	6.199102	5.305856
-881.031943	2.316069	5.315853
-879.206457	3.544808	5.325850
-877.232384	7.563460	5.335846
-875.332791	3.183019	5.345843
-873.550849	8.025019	5.355840
-871.811854	6.911816	5.365837
-869.788968	8.210056	5.375834
-867.278169	1.780338	5.385830
-866.021670	4.028468	5.395827
-864.167800	6.686357	5.405824
-862.525875	7.028671	5.415821
-860.283620	0.885049	5.425818
-858.469927	2.049374	5.435814
-856.643306	9.396336	5.445811
-854.622469	-1.769222	5.455808
-852.691615	4.585293	5.465805
-850.856113	7.179815	5.475802
-849.219457	-0.168028	5.485798
-847.408792	4.595190	5.495795
-845.400822	2.114278	5.505792
-843.488913	4.295539	5.515789
-841.559127	-0.958118	5.525786
-839.649180	-1.845996	5.535782
-837.860877	1.461865	5.545779
-835.896343	4.965766	5.555776
-833.827270	0.870894	5.565773
-832.265318	0.411281	5.575770
-830.521516	0.214703	5.585766
-828.547332	-3.378682	5.595763
-826.790543	-2.341025	5.605760
-824.859273	2.792930	5.615757
-822.629230	0.211800	5.625754
-820.961433	5.057878	5.635750
-819.264519	5.044066	5.645747
-817.030580	4.061784	5.655744
-815.113963	3.425490	5.665741
-813.581034	1.930008	5.675738
-811.877472	-1.880630	5.685734
-809.629593	-2.951975	5.695731
-807.744821	-0.526348	5.705728
-805.844500	2.899422	5.715725
-804.112461	5.131574	5.725722
-802.227021	2.989228	5.735718
-800.162444	1.621931	5.745715
-798.603741	12.832802	5.755712
-796.657334	3.029174	5.765709
-794.560313	4.129314	5.775706
-792.664289	3.325804	5.785702
-790.964688	3.483687	5.795699
-788.852699	6.566167	5.805696
-787.325587	4.549003	5.815693
-785.255247	8.298140	5.825690
-783.557326	-1.110497	5.835686
-781.513740	-0.873379	5.845683
-779.679609	-0.792253	5.855680
-777.648509	-2.387863	5.865677
-775.926293	-3.089369	5.875674
-774.212448	-3.334801	5.885670
-772.208549	-4.049748	5.895667
-770.411712	4.915722	5.905664
-768.274646	7.299479	5.915661
-766.549660	2.591767	5.925658
-764.739352	5.981433	5.935654
-762.538316	-0.125515	5.945651
-760.828232	4.371220	5.955648
-759.189636	5.623608	5.965645
-757.118065	0.835246	5.975642
-755.332278	2.335689	5.985638
-753.387402	0.744407	5.995635
-751.458182	5.747702	6.005632
-749.707966	3.622273	6.015629
-747.917283	0.314067	6.025626
-745.805192	3.083940	6.035622
-744.155407	6.069806	6.045619
-742.000908	2.322934	6.055616
-740.418334	2.965344	6.065613
-738.188890	1.052280	6.075610
-736.535090	4.234877	6.085606
-734.805694	8.202759	6.095603
-732.865695	5.882802	6.105600
-730.766239	1.186320	6.115597
-728.945293	7.618512	6.125594
-727.101698	5.531859	6.135590
-725.247693	6.110375	6.145587
-723.389286	3.740307	6.155584
-721.659339	5.916014	6.165581
-719.639476	5.555401	6.175578
-717.692329	6.243774	6.185574
-716.077672	-0.790999	6.195571
-714.130552	3.697891	6.205568
-712.034317	1.888244	6.215565
-710.047266	1.174463	6.225562
-708.368594	-2.112656	6.235558
-706.521089	3.814785	6.245555
-704.656642	4.969541	6.255552
-702.531217	7.012590	6.265549
-700.899266	1.051900	6.275546
-699.071241	8.438245	6.285542
-697.213210	5.981415	6.295539
-695.273747	9.007868	6.305536
-693.443709	4.877099	6.315533
-691.367424	4.355916	6.325530
-689.500369	10.479197	6.335526
-687.893745	3.876773	6.345523
-685.727915	4.013915	6.355520
-683.752373	0.489900	6.365517
-682.175732	3.841182	6.375514
-680.427780	0.430906	6.385510
-678.515980	5.258628	6.395507
-676.425785	6.112072	6.405504
-674.494521	3.627768	6.415501
-672.752342	9.122072	6.425498
-670.654144	4.125841	6.435494
-669.176075	7.357094	6.445491
-667.138489	7.156325	6.455488
-665.267357	7.632679	6.465485
-663.317012	5.941121	6.475482
-661.630373	3.773808	6.485478
-659.417644	3.469271	6.495475
-657.691767	6.971987	6.505472
-655.790773	4.135693	6.515469
-653.850028	2.478835	6.525466
-652.107719	5.743668	6.535462
-650.029963	-2.138741	6.545459
-648.451372	3.789085	6.555456
-646.449524	5.454037	6.565453
-644.541506	2.045053	6.575450
-642.685299	-6.285105	6.585446
-641.242588	5.588625	6.595443
-638.981771	2.915905	6.605440
-636.744884	5.874360	6.615437
-635.264871	3.064292	6.625434
-633.269454	0.050299	6.635430
-631.448277	-2.831643	6.645427
-629.557679	-4.063629	6.655424
-627.663917	5.909632	6.665421
-625.794079	0.616769	6.675418
-624.033356	-5.034446	6.685414
-622.218959	-1.130586	6.695411
-620.044779	-3.388395	6.705408
-618.116666	0.172039	6.715405
-616.523951	-4.888646	6.725402
-614.563811	-1.895430	6.735398
-613.054666	-9.175384	6.745395
-610.836212	2.744955	6.755392
-608.871649	2.851165	6.765389
-606.720821	-0.519214	6.775386
-605.176593	-4.342150	6.785382
-603.401073	4.843183	6.795379
-601.467102	4.815339	6.805376
-599.643593	-0.924839	6.815373
-597.615776	-0.631358	6.825370
-595.767993	-2.549633	6.835366
-593.949785	-1.365297	6.845363
-592.245843	2.311499	6.855360
-590.078937	-4.129319	6.865357
-588.338571	-5.218851	6.875354
-586.674995	0.790179	6.885350
-584.270726	2.008792	6.895347
-582.603018	1.835605	6.905344
-580.786530	-2.690809	6.915341
-578.741284	-2.570622	6.925338
-576.905090	-4.943346	6.935334
-575.220249	0.995980	6.945331
-573.437572	1.188117	6.955328
-571.433111	-4.265158	6.965325
-569.526016	-3.380791	6.975322
-567.617930	-3.953945	6.985318
-565.767110	-2.459008	6.995315
-563.835853	4.928328	7.005312
-562.156239	-5.517770	7.015309
-560.341750	3.241376	7.025306
-558.147582	5.426733	7.035302
-556.416520	0.659772	7.045299
-554.755464	7.420808	7.055296
-552.439872	2.644160	7.065293
-550.441792	6.119266	7.075290
-548.862588	-0.554481	7.085286
-547.130714	3.460518	7.095283
-545.301631	1.482110	7.105280
-543.160278	6.688544	7.115277
-541.293431	1.623587	7.125274
-539.482449	0.170705	7.135270
-537.532282	-5.760185	7.145267
-535.891484	1.351467	7.155264
-534.024435	1.051736	7.165261
-532.069550	-2.077279	7.175258
-529.985982	2.563659	7.185254
-528.423988	0.228454	7.195251
-526.256626	-4.066598	7.205248
-524.546340	3.627647	7.215245
-522.426564	5.188606	7.225242
-520.779231	3.916614	7.235238
-518.783485	9.207908	7.245235
-517.286367	0.941503	7.255232
-515.031723	5.971973	7.265229
-513.207600	2.361753	7.275226
-511.150778	0.065944	7.285222
-509.542339	-1.037197	7.295219
-507.830269	5.516780	7.305216
-506.060367	8.032057	7.315213
-503.798800	0.409350	7.325210
-501.751633	3.137712	7.335206
-500.051138	8.954600	7.345203
-498.210797	9.349162	7.355200
-496.328603	9.039147	7.365197
-494.450101	9.448143	7.375194
-492.925273	11.228889	7.385190
-490.214273	8.688089	7.395187
-488.969099	1.704568	7.405184
-486.993921	5.717071	7.415181
-484.788968	0.808155	7.425178
-483.036970	-4.713676	7.435174
-481.565067	-4.879205	7.445171
-479.732982	3.504570	7.455168
-477.485541	-0.459021	7.465165
-475.648996	1.253004	7.475162
-473.776063	-0.509722	7.485158
-471.937840	1.197301	7.495155
-470.037712	6.243382	7.505152
-468.345020	3.615762	7.515149
-466.127945	2.939658	7.525146
-464.514962	-0.521544	7.535142
-462.583481	0.202700	7.545139
-460.774686	1.259170	7.555136
-458.868596	6.121151	7.565133
-456.818013	2.283753	7.575130
-455.092302	6.427703	7.585126
-453.547769	8.551117	7.595123
-451.305176	6.467268	7.605120
-449.189278	9.560491	7.615117
-447.630270	5.837919	7.625114
-445.647067	8.475495	7.635110
-443.808820	-1.545870	7.645107
-441.933601	3.752106	7.655104
-440.050665	13.379903	7.665101
-437.943291	3.849245	7.675098
-436.434559	8.889964	7.685094
-434.346931	8.465086	7.695091
-432.518833	10.372706	7.705088
-430.609455	4.731037	7.715085
-428.829535	5.948459	7.725082
-427.188956	0.714454	7.735078
-425.102496	2.283980	7.745075
-423.362518	7.576727	7.755072
-421.165811	2.031289	7.765069
-419.508344	2.093536	7.775066
-417.421128	2.701369	7.785062
-415.517499	4.874835	7.795059
-413.724385	7.315424	7.805056
-411.812871	8.688687	7.815053
-410.107807	5.669131	7.825050
-408.007403	1.279081	7.835046
-406.173741	2.691622	7.845043
-404.570988	3.553667	7.855040
-402.495464	1.333910	7.865037
-401.062918	5.608396	7.875034
-398.941935	-0.231246	7.885030
-396.612631	-3.156257	7.895027
-394.993316	3.532619	7.905024
-393.301401	2.321489	7.915021
-391.089835	2.080544	7.925018
-389.397306	4.935106	7.935014
-387.613629	4.997748	7.945011
-385.614605	1.031273	7.955008
-383.738688	5.306030	7.965005
-381.895440	6.237060	7.975002
-379.905476	1.370457	7.984998
-378.075147	8.428288	7.994995
-376.242674	7.357358	8.004992
-374.475545	9.396337	8.014989
-372.709891	6.326079	8.024986
-370.679228	8.881931	8.034982
-368.809473	1.909267	8.044979
-366.912403	4.020662	8.054976
-365.007812	3.388226	8.064973
-363.049097	3.203467	8.074970
-361.060858	5.072942	8.084966
-359.538020	3.615673	8.094963
-357.535424	-1.426613	8.104960
-355.549044	-0.305258	8.114957
-353.582486	7.523474	8.124954
-351.565249	2.578328	8.134950
-350.110548	3.653521	8.144947
-348.239752	9.077022	8.154944
-346.455324	6.390627	8.164941
-344.429872	8.846281	8.174938
-342.541061	10.472700	8.184934
-340.260438	10.238144	8.194931
-338.570689	13.377400	8.204928
-336.926686	13.276064	8.214925
-335.077918	14.220460	8.224922
-333.082600	12.158827	8.234918
-331.145601	8.688612	8.244915
-329.307948	3.221100	8.254912
-327.654187	5.734529	8.264909
-325.641098	11.367438	8.274906
-323.455424	9.019634	8.284902
-321.564694	5.735234	8.294899
-319.987443	7.428777	8.304896
-318.601536	7.446025	8.314893
-316.201059	3.432884	8.324890
-314.388456	3.012542	8.334886
-312.316290	6.809188	8.344883
-310.581634	6.440766	8.354880
-308.821233	8.938763	8.364877
-306.945720	8.107331	8.374874
-305.036375	8.972607	8.384870
-303.203038	1.982118	8.394867
-301.569988	9.300453	8.404864
-299.140731	8.915893	8.414861
-297.204047	14.063657	8.424858
-295.360910	7.158449	8.434854
-293.700556	4.021372	8.444851
-292.053361	6.085874	8.454848
-290.171014	5.109680	8.464845
-287.995341	10.190879	8.474842
-285.925957	6.525882	8.484838
-284.543297	7.085247	8.494835
-282.521959	2.450554	8.504832
-280.596555	11.522240	8.514829
-278.752906	10.345389	8.524826
-276.879526	7.242213	8.534822
-274.730812	3.038772	8.544819
-272.722612	7.461454	8.554816
-271.191964	6.798783	8.564813
-269.488618	7.914863	8.574810
-267.404256	0.459593	8.584807
-265.789523	9.124564	8.594803
-263.725172	7.459338	8.604800
-261.814310	4.512823	8.614797
-259.897237	8.201641	8.624794
-258.115356	5.032557	8.634791
-256.015635	7.815908	8.644787
-254.051575	0.761956	8.654784
-252.416088	10.238363	8.664781
-250.819129	7.948275	8.674778
-248.650356	7.235870	8.684775
-246.764826	9.761311	8.694771
-244.817250	9.423688	8.704768
-243.348756	11.087274	8.714765
-241.030015	6.180933	8.724762
-238.977737	8.619765	8.734759
-237.495017	6.063709	8.744755
-235.843128	0.850125	8.754752
-233.679783	0.116493	8.764749
-231.632730	-1.667523	8.774746
-230.124706	-1.805505	8.784743
-228.044151	1.141981	8.794739
-226.092699	0.274807	8.804736
-224.383881	6.297421	8.814733
-222.436555	1.913009	8.824730
-220.423502	0.191270	8.834727
-218.371887	0.426012	8.844723
-216.987208	-2.232804	8.854720
-214.751616	1.326266	8.864717
-212.996452	0.154114	8.874714
-211.218285	-11.207505	8.884711
-208.967611	-13.110842	8.894707
-207.367501	-9.526135	8.904704
-205.539672	-6.118296	8.914701
-203.554284	-4.942972	8.924698
-202.071984	-11.187361	8.934695
-199.854388	-9.535934	8.944691
-197.942280	-6.812593	8.954688
-196.035268	-8.642125	8.964685
-194.319651	-6.173212	8.974682
-192.401742	-5.959741	8.984679
-190.485656	-6.636505	8.994675
-188.575265	-8.496571	9.004672
-186.792469	-2.973633	9.014669
-184.673122	-1.107563	9.024666
-183.212605	-1.124250	9.034663
-181.366750	-7.278227	9.044659
-179.506166	-4.914542	9.054656
-177.399954	-3.911635	9.064653
-175.471112	-6.341478	9.074650
-173.772002	-8.020973	9.084647
-171.575063	-5.147274	9.094643
-169.631377	-2.839475	9.104640
-168.016744	-3.291273	9.114637
-166.424816	1.122141	9.124634
-164.211211	-0.127871	9.134631
-162.113188	0.101092	9.144627
-160.731000	-2.819402	9.154624
-158.551521	-2.731329	9.164621
-156.584503	-2.220929	9.174618
-154.933001	-0.390703	9.184615
-153.309098	5.094462	9.194611
-151.237725	1.612417	9.204608
-149.066448	-2.883464	9.214605
-147.432374	0.853762	9.224602
-145.376634	0.251064	9.234599
-143.439736	4.802080	9.244595
-141.643953	-2.269147	9.254592
-140.038217	-2.277400	9.264589
-138.141642	4.345321	9.274586
-136.048065	-2.849210	9.284583
-134.220749	-9.491248	9.294579
-132.543076	-3.765177	9.304576
-130.282073	-8.201147	9.314573
-128.630591	-5.845110	9.324570
-126.802646	-4.658809	9.334567
-124.837167	-8.496567	9.344563
-123.116431	-7.455789	9.354560
-121.192345	-3.947978	9.364557
-119.079170	2.700198	9.374554
-117.229038	1.276119	9.384551
-115.393839	-3.361900	9.394547
-113.574411	3.611047	9.404544
-111.572380	0.144835	9.414541
-110.145874	7.283112	9.424538
-107.651055	1.630375	9.434535
-106.161035	7.496939	9.444531
-104.402937	10.221249	9.454528
-102.267942	13.793324	9.464525
-100.648513	3.620776	9.474522
-98.576187	8.565487	9.484519
-96.665227	-0.775672	9.494515
-94.850294	2.304314	9.504512
-93.241666	2.469314	9.514509
-90.808603	5.820156	9.524506
-89.185652	-3.315571	9.534503
-87.227633	2.526862	9.544499
-85.528112	3.169999	9.554496
-83.621529	4.441682	9.564493
-81.792166	-1.744334	9.574490
-79.692681	-0.522371	9.584487
-77.902575	2.312114	9.594483
-76.036485	10.862919	9.604480
-74.227535	0.014360	9.614477
-72.458949	9.678094	9.624474
-70.768519	9.590058	9.634471
-68.410684	3.033947	9.644467
-66.398367	2.274033	9.654464
-64.904702	5.785825	9.664461
-63.128555	0.484630	9.674458
-60.898777	5.696361	9.684455
-59.069622	5.229358	9.694451
-57.278330	2.988918	9.704448
-55.342952	1.931813	9.714445
-53.502455	9.054609	9.724442
-51.692025	9.987973	9.734439
-49.996213	8.309087	9.744435
-47.927767	9.234450	9.754432
-45.927988	0.815474	9.764429
-44.365366	0.068896	9.774426
-42.345089	-1.102796	9.784423
-40.174389	-2.028482	9.794419
-38.713250	3.122731	9.804416
-36.683861	3.070646	9.814413
-34.757478	4.997633	9.824410
-32.874342	-1.493770	9.834407
-30.834663	-0.971174	9.844403
-29.301183	0.778493	9.854400
-27.500054	2.739678	9.864397
-25.386935	4.333725	9.874394
-23.361314	-6.964626	9.884391
-21.537580	-5.835994	9.894387
-19.577488	-1.621734	9.904384
-18.264357	-0.026384	9.914381
-16.257463	3.646729	9.924378
-13.985432	2.761744	9.934375
-12.182021	-2.122185	9.944371
-10.517739	0.334527	9.954368
-8.527890	6.574586	9.964365
-6.756480	2.188398	9.974362
-5.249419	18.487621	9.984359
-3.942446	45.661481	9.994355
-2.409504	91.865313	10.004352
-1.203294	157.048513	10.014349
0.000000	208.869865	10.019354
0.590393	245.977758	10.024359
1.424175	266.629154	10.029363
1.719405	308.724916	10.034368
2.006300	328.957429	10.039373
2.419642	357.166627	10.044378
2.534366	367.255187	10.049383
2.795331	389.822689	10.054387
3.052149	403.890975	10.059392
3.501769	412.864842	10.064397
3.249981	405.452243	10.069402
3.086579	418.105213	10.074407
3.773021	431.663443	10.079411
4.026493	450.805456	10.084416
3.879279	445.090337	10.089421
3.862807	465.483397	10.094426
3.795800	462.663437	10.099431
4.010281	457.114551	10.104435
3.937008	467.482331	10.109440
4.386211	463.542375	10.114445
4.309574	474.079434	10.119450
4.039755	475.505527	10.124455
4.246811	467.657000	10.129459
4.116064	480.106115	10.134464
4.624104	469.557087	10.139469
3.996577	483.252414	10.144474
4.208986	479.610427	10.149479
4.379206	481.992948	10.154483
4.127903	496.016215	10.159488
4.582262	486.729443	10.164493
4.305333	485.376444	10.169498
4.014035	499.634756	10.174503
4.497739	486.536455	10.179507
4.566419	496.173546	10.184512
4.698553	488.510427	10.189517
4.748490	504.371728	10.194522
4.633719	500.006045	10.199527
4.694060	503.800154	10.204531
4.906171	528.946157	10.209536
5.226066	527.523187	10.214541
4.694882	515.965033	10.219546
4.668268	520.928951	10.224551
4.744888	533.318225	10.229555
4.879998	539.623604	10.234560
5.101195	537.451535	10.239565
5.141639	554.147056	10.244570
5.224986	544.025272	10.249575
5.248455	553.179168	10.254579
5.194677	551.254389	10.259584
5.210514	544.869810	10.264589
5.588521	558.879491	10.269594
5.497324	550.824597	10.274599
5.656130	553.257838	10.279603
5.539226	552.123741	10.284608
5.707467	548.884607	10.289613
5.353244	552.536693	10.294618
5.518629	557.320183	10.299623
5.507304	553.901527	10.304627
5.442745	568.312979	10.309632
5.870245	570.160877	10.314637
5.853306	582.639236	10.319642
5.713094	589.717126	10.324647
6.100491	587.039133	10.329651
5.812114	587.011050	10.334656
6.271575	587.248469	10.339661
5.910487	603.763661	10.344666
5.866960	594.931563	10.349671
6.352004	594.595605	10.354675
6.091557	605.222004	10.359680
6.144082	594.988402	10.364685
6.225471	605.082445	10.369690
5.965686	604.849523	10.374695
6.277048	600.344874	10.379699
6.100430	613.306848	10.384704
6.681340	603.231028	10.389709
5.863048	613.988205	10.394714
6.015899	622.981154	10.399719
6.665234	632.421634	10.404723
6.498836	643.449388	10.409728
6.686931	644.624254	10.414733
6.747585	645.481970	10.419738
6.574553	649.313342	10.424743
7.085784	637.639281	10.429747
6.691561	643.991290	10.434752
7.166766	645.017855	10.439757
6.770306	649.832646	10.444762
6.715743	642.937263	10.449767
6.986672	652.884408	10.454771
6.720370	653.901513	10.459776
6.724201	659.548195	10.464781
6.727614	660.899183	10.469786
6.948459	662.962989	10.474791
7.188511	682.736675	10.479795
7.095549	695.832828	10.484800
7.119674	684.282160	10.489805
7.119646	690.847289	10.494810
7.045400	696.528518	10.499815
7.352133	694.114116	10.504819
7.086943	695.908512	10.509824
7.607537	694.688488	10.514829
7.210260	703.203090	10.519834
7.609633	708.255247	10.524839
7.894610	722.790878	10.529843
7.473628	729.032071	10.534848
8.221703	725.621559	10.539853
7.576157	719.779231	10.544858
7.775117	734.058924	10.549863
7.779356	731.695920	10.554867
7.885338	740.254854	10.559872
8.041654	731.682545	10.564877
7.845758	747.979154	10.569882
7.879240	745.657216	10.574887
7.972204	745.606155	10.579891
7.997968	747.587546	10.584896
7.947550	736.875082	10.589901
7.978509	753.159167	10.594906
7.913912	744.219948	10.599911
8.268673	749.115226	10.604915
8.299729	766.484297	10.609920
8.566429	772.989571	10.614925
8.559263	771.891571	10.619930
8.489560	776.846679	10.624935
8.755567	784.402362	10.629939
8.420510	788.570288	10.634944
8.770611	778.352173	10.639949
8.554470	785.899604	10.644954
8.375694	788.575974	10.649959
8.952446	786.047522	10.654963
8.761277	789.022348	10.659968
8.835635	783.899406	10.664973
8.700446	788.290928	10.669978
8.868320	791.773058	10.674983
9.091736	788.714313	10.679987
8.790333	803.485489	10.684992
9.018801	794.002732	10.689997
8.819155	795.037600	10.695002
8.874025	797.268255	10.700007
8.678321	788.633785	10.705011
8.678119	811.478577	10.710016
8.722051	829.050681	10.715021
8.747615	832.566560	10.720026
8.671575	836.037141	10.725031
9.099672	841.925318	10.730035
9.268570	861.105019	10.735040
9.577533	855.318551	10.740045
9.750808	866.636085	10.745050
9.590520	865.936258	10.750055
9.587023	866.670172	10.755059
9.549197	873.837529	10.760064
9.891549	864.276634	10.765069
9.510377	871.785775	10.770074
9.795145	879.253357	10.775079
10.005425	870.229213	10.780083
9.516783	876.722545	10.785088
9.670438	868.488064	10.790093
10.014082	875.451066	10.795098
9.811776	874.352643	10.800103
10.197123	889.582095	10.805107
9.777075	903.019203	10.810112
10.009260	903.923695	10.815117
10.078048	912.170102	10.820122
10.146128	917.792444	10.825127
10.347917	906.850382	10.830131
10.178992	915.540006	10.835136
10.598151	916.499834	10.840141
10.325408	914.944265	10.845146
10.207984	918.287419	10.850151
10.177971	903.759889	10.855155
9.987115	918.575051	10.860160
10.429596	918.692178	10.865165
10.365936	923.114911	10.870170
10.545310	932.583240	10.875175
10.748731	937.649387	10.880179
10.441383	944.173758	10.885184
10.828736	939.119115	10.890189
10.478653	937.709928	10.895194
10.566972	941.002923	10.900199
10.482653	941.000640	10.905203
10.470095	950.535867	10.910208
10.857607	966.184545	10.915213
10.687876	973.630049	10.920218
10.742232	975.409780	10.925223
10.886712	979.846641	10.930227
11.102987	977.757299	10.935232
10.959403	973.921224	10.940237
11.497891	992.427101	10.945242
11.600303	999.007570	10.950247
11.390937	991.356079	10.955251
10.835966	998.552365	10.960256
11.502243	994.680152	10.965261
11.325648	1005.132608	10.970266
11.467991	1010.345725	10.975271
11.630068	1006.602820	10.980275
11.688286	1004.994451	10.985280
11.560100	1012.321377	10.990285
11.723766	1017.258267	10.995290
11.633897	1017.039238	11.000295
11.823862	1010.464243	11.005299
11.809051	1017.254241	11.010304
12.009367	1012.243600	11.015309
11.946831	1024.817925	11.020314
11.906393	1013.764601	11.025319
11.986159	1012.770995	11.030323
11.805043	1022.681682	11.035328
11.837398	1035.620949	11.040333
12.063782	1052.711609	11.045338
12.078662	1052.706120	11.050343
12.591960	1055.179102	11.055347
12.415656	1052.870077	11.060352
12.841499	1052.336962	11.065357
12.571962	1060.698923	11.070362
12.363302	1056.903170	11.075367
12.700602	1046.385694	11.080371
12.514267	1050.649826	11.085376
12.834547	1054.833152	11.090381
12.782313	1050.564568	11.095386
12.557075	1041.087783	11.100391
13.007109	1042.093162	11.105395
12.639566	1037.561042	11.110400
13.030778	1040.222240	11.115405
12.936952	1036.141654	11.120410
12.925762	1032.516271	11.125415
12.749722	1031.038310	11.130419
13.088141	1047.161712	11.135424
13.020883	1055.800508	11.140429
12.989907	1061.211610	11.145434
12.774131	1065.732771	11.150439
13.009907	1059.970513	11.155443
12.590110	1068.086771	11.160448
13.090039	1063.715916	11.165453
12.991654	1067.775202	11.170458
12.777847	1060.688966	11.175463
13.218459	1074.739627	11.180467
13.345049	1085.344067	11.185472
13.334620	1083.029080	11.190477
13.439538	1095.671380	11.195482
13.407438	1096.624347	11.200487
13.533650	1091.786358	11.205491
13.195287	1099.711437	11.210496
13.204709	1091.958758	11.215501
13.275806	1097.941833	11.220506
13.114377	1118.675917	11.225511
13.800975	1118.528591	11.230515
13.815661	1134.831469	11.235520
13.967589	1127.989658	11.240525
13.910716	1122.125812	11.245530
14.045622	1129.988035	11.250535
14.265174	1124.173143	11.255539
14.094680	1129.071902	11.260544
14.130547	1128.067943	11.265549
14.128616	1123.964790	11.270554
14.201343	1128.711206	11.275559
14.420997	1127.670046	11.280563
14.565076	1124.097150	11.285568
14.363189	1114.961968	11.290573
14.464858	1121.440103	11.295578
14.362359	1120.642729	11.300583
14.682306	1117.945436	11.305587
14.352489	1127.701705	11.310592
14.552841	1121.410452	11.315597
14.682987	1125.397030	11.320602
14.575223	1127.648945	11.325607
15.037113	1120.557412	11.330611
14.971692	1123.949092	11.335616
15.006386	1112.401130	11.340621
14.942638	1125.578171	11.345626
14.810095	1127.182714	11.350631
14.839657	1123.410451	11.355635
14.804712	1131.137330	11.360640
14.755681	1128.175591	11.365645
15.074537	1122.204503	11.370650
15.118458	1126.245838	11.375655
15.168487	1121.030458	11.380659
15.163794	1124.809871	11.385664
14.831349	1122.528893	11.390669
15.156620	1125.318903	11.395674
15.138763	1123.170686	11.400679
15.197155	1123.765423	11.405683
15.269782	1140.983221	11.410688
15.744770	1144.850141	11.415693
15.585169	1138.169987	11.420698
15.487361	1143.815722	11.425703
15.637519	1137.194978	11.430707
15.537406	1145.102581	11.435712
15.801331	1143.515005	11.440717
15.741335	1137.452942	11.445722
15.820652	1150.695501	11.450727
16.130483	1142.387066	11.455731
15.825741	1141.248187	11.460736
15.617641	1123.044335	11.465741
15.855751	1133.467008	11.470746
15.727983	1150.010259	11.475751
16.317644	1141.524718	11.480755
15.933889	1161.543646	11.485760
16.012294	1156.454623	11.490765
16.258849	1155.316125	11.495770
15.945234	1155.301526	11.500775
16.591298	1153.758660	11.505779
16.330636	1159.750520	11.510784
16.269549	1146.718024	11.515789
16.787548	1158.110120	11.520794
16.450115	1162.150787	11.525799
16.607222	1151.162050	11.530803
16.583602	1152.817036	11.535808
16.536400	1149.547475	11.540813
16.475103	1149.153563	11.545818
16.476229	1160.131331	11.550823
16.447113	1162.720814	11.555827
16.399478	1167.499058	11.560832
16.607679	1166.568540	11.565837
16.509216	1163.349733	11.570842
16.387968	1165.086529	11.575847
16.772335	1162.118738	11.580851
16.398323	1174.764953	11.585856
16.785559	1189.625387	11.590861
16.870382	1199.454349	11.595866
16.880802	1201.278966	11.600871
17.209560	1202.488217	11.605875
17.159619	1207.063400	11.610880
17.095505	1201.080820	11.615885
17.349274	1205.030354	11.620890
17.298480	1205.968962	11.625895
17.394335	1206.475720	11.630899
17.139057	1210.468600	11.635904
17.303716	1200.360201	11.640909
17.217366	1199.732147	11.645914
17.113417	1207.288711	11.650919
17.440475	1201.218504	11.655923
17.715029	1224.188866	11.660928
17.738479	1223.519642	11.665933
17.562188	1221.179045	11.670938
17.590439	1230.482426	11.675943
17.856731	1233.939502	11.680947
17.774157	1238.677607	11.685952
17.974797	1233.188987	11.690957
18.066478	1241.253722	11.695962
17.738635	1239.382029	11.700967
18.187812	1236.783959	11.705971
17.914559	1240.905881	11.710976
17.796281	1234.443034	11.715981
17.832749	1234.993961	11.720986
17.792783	1233.079506	11.725991
18.082239	1229.775153	11.730995
17.792061	1239.829548	11.736000
18.148491	1237.307777	11.741005
18.341996	1234.006112	11.746010
18.120496	1234.866287	11.751015
18.367988	1250.793092	11.756019
18.482246	1259.145994	11.761024
18.742540	1260.605886	11.766029
18.797000	1260.999390	11.771034
18.738495	1264.997173	11.776039
18.844877	1247.091536	11.781043
18.557476	1246.774690	11.786048
18.783650	1254.346436	11.791053
18.489550	1262.947414	11.796058
18.345007	1275.334748	11.801063
18.750434	1272.499204	11.806067
19.083885	1276.462859	11.811072
18.910944	1273.971897	11.816077
18.864242	1268.710388	11.821082
18.950154	1271.962838	11.826087
19.311603	1261.841933	11.831091
19.004015	1269.934095	11.836096
19.264899	1264.339654	11.841101
19.096433	1261.228192	11.846106
18.971461	1269.835316	11.851111
19.236555	1256.630837	11.856115
19.096681	1268.104297	11.861120
19.335328	1276.490988	11.866125
19.341432	1268.838100	11.871130
19.266849	1266.396112	11.876135
19.426961	1286.588679	11.881139
19.435909	1288.178557	11.886144
19.741353	1291.457502	11.891149
19.862241	1286.071477	11.896154
19.783261	1297.681915	11.901159
20.009481	1295.330725	11.906163
19.877210	1296.515742	11.911168
20.124117	1287.460265	11.916173
19.918450	1272.950920	11.921178
19.875394	1267.092697	11.926183
20.185086	1257.776470	11.931187
19.678534	1269.172789	11.936192
20.154849	1269.820730	11.941197
20.314173	1280.120447	11.946202
20.103601	1274.274746	11.951207
20.133034	1268.236213	11.956211
20.294176	1288.102165	11.961216
20.424413	1280.871051	11.966221
20.216625	1279.431246	11.971226
20.124568	1293.606510	11.976231
20.662233	1281.385209	11.981235
20.402501	1288.420995	11.986240
20.651612	1289.581452	11.991245
20.625424	1288.967455	11.996250
20.419546	1295.720244	12.001255
20.350451	1284.961465	12.006259
20.620232	1290.532855	12.011264
20.516790	1287.461482	12.016269
20.357071	1294.503398	12.021274
20.445298	1295.482921	12.026279
20.704275	1284.157688	12.031283
20.482245	1294.439389	12.036288
20.613176	1297.246238	12.041293
20.722176	1291.392139	12.046298
20.460095	1295.826131	12.051303
20.570050	1294.685755	12.056307
20.674879	1312.400130	12.061312
21.047756	1308.379078	12.066317
20.649567	1294.805661	12.071322
20.486931	1302.570345	12.076327
20.724401	1305.352317	12.081331
20.862065	1326.294477	12.086336
21.101418	1322.528127	12.091341
21.101855	1311.141602	12.096346
20.954111	1302.502329	12.101351
21.001633	1302.322886	12.106355
21.026081	1307.532836	12.111360
21.058072	1291.458956	12.116365
21.051693	1290.400219	12.121370
20.705818	1297.356701	12.126375
21.041737	1290.195286	12.131379
20.802329	1298.468993	12.136384
20.917476	1299.318056	12.141389
21.290184	1299.250761	12.146394
20.939291	1279.314204	12.151399
20.881380	1271.321415	12.156403
20.761142	1271.521994	12.161408
20.856811	1273.545927	12.166413
20.912682	1266.875503	12.171418
20.792059	1275.051396	12.176423
21.012031	1269.848284	12.181427
20.620019	1270.324042	12.186432
20.829775	1267.046587	12.191437
20.567295	1269.621269	12.196442
20.675823	1265.714938	12.201447
21.075762	1260.115667	12.206451
20.746253	1264.453164	12.211456
20.878211	1252.151507	12.216461
20.774229	1265.915454	12.221466
20.513459	1283.147172	12.226471
20.635911	1274.160445	12.231475
20.657177	1274.335300	12.236480
21.006505	1285.051026	12.241485
20.865615	1273.418970	12.246490
20.876217	1270.040806	12.251495
20.834803	1271.550400	12.256499
20.556405	1278.530807	12.261504
20.755940	1277.186894	12.266509
20.771947	1274.243140	12.271514
20.663788	1273.389886	12.276519
21.009341	1270.111273	12.281523
20.735866	1275.792963	12.286528
20.820946	1271.683775	12.291533
20.654795	1277.383043	12.296538
20.724297	1280.860481	12.301543
20.748562	1271.564538	12.306547
20.735843	1288.734619	12.311552
21.153888	1285.272539	12.316557
20.999683	1280.263157	12.321562
20.785028	1270.745106	12.326567
20.824105	1258.720053	12.331571
20.494243	1257.432195	12.336576
20.629633	1268.267194	12.341581
20.816407	1282.563566	12.346586
20.645206	1279.897271	12.351591
20.714918	1276.896060	12.356595
20.757846	1289.835444	12.361600
20.840734	1286.584530	12.366605
20.741682	1283.021988	12.371610
20.695976	1286.106186	12.376615
21.058733	1287.562355	12.381619
20.764146	1282.110126	12.386624
20.734636	1255.727310	12.391629
20.474840	1257.930949	12.396634
20.594483	1270.448042	12.401639
21.034248	1271.038730	12.406643
20.439084	1289.790469	12.411648
20.862866	1282.563000	12.416653
20.750087	1282.549485	12.421658
20.872991	1288.893411	12.426663
20.935463	1278.381755	12.431667
20.641082	1271.385543	12.436672
20.525981	1271.194190	12.441677
20.511052	1283.089313	12.446682
20.719970	1287.241581	12.451687
21.006705	1278.214453	12.456691
20.735609	1293.843948	12.461696
20.746914	1288.166294	12.466701
20.825787	1289.767099	12.471706
20.563719	1289.252230	12.476711
20.943394	1290.948570	12.481715
20.908027	1296.849353	12.486720
20.843280	1279.502446	12.491725
20.566284	1276.964998	12.496730
20.298899	1283.276549	12.501735
20.804733	1274.932045	12.506739
20.885550	1295.761794	12.511744
20.755203	1292.798798	12.516749
20.918292	1293.698566	12.521754
20.769400	1290.495659	12.526759
20.345760	1290.843988	12.531763
20.849035	1297.464742	12.536768
21.235864	1298.179001	12.541773
21.024476	1271.389894	12.546778
20.887513	1269.825244	12.551783
21.042745	1260.454799	12.556787
20.733550	1264.814289	12.561792
20.946150	1268.316211	12.566797
20.809714	1269.650135	12.571802
20.850807	1264.425089	12.576807
20.722200	1261.289922	12.581811
20.467274	1263.506979	12.586816
20.751696	1266.607909	12.591821
20.924291	1264.194309	12.596826
20.861578	1269.637361	12.601831
21.165033	1262.381782	12.606835
20.871104	1259.627825	12.611840
20.776826	1269.777160	12.616845
20.900849	1268.265506	12.621850
20.851687	1267.962703	12.626855
21.145074	1267.337160	12.631859
20.982020	1263.415797	12.636864
20.780839	1250.730429	12.641869
20.892264	1242.434659	12.646874
20.609374	1242.669067	12.651879
20.919833	1232.192012	12.656883
20.374050	1232.799536	12.661888
20.504867	1244.403279	12.666893
20.742254	1262.094873	12.671898
20.928138	1261.721461	12.676903
20.844654	1261.676464	12.681907
20.520562	1255.342637	12.686912
20.528230	1257.640821	12.691917
20.693193	1268.021638	12.696922
20.665830	1277.811772	12.701927
20.677199	1270.806220	12.706931
20.274060	1275.822566	12.711936
20.490700	1276.898308	12.716941
20.906952	1277.383929	12.721946
20.574055	1275.766945	12.726951
20.913382	1275.760172	12.731955
20.767257	1273.293321	12.736960
20.852442	1275.186452	12.741965
21.064165	1272.626251	12.746970
20.509516	1274.343872	12.751975
20.711676	1281.343832	12.756979
20.591501	1272.824768	12.761984
20.997153	1285.674752	12.766989
20.848477	1271.056963	12.771994
20.762466	1273.606652	12.776999
21.267957	1278.104304	12.782003
20.980268	1286.839902	12.787008
20.980952	1263.991208	12.792013
20.813968	1252.470571	12.797018
20.572195	1256.937586	12.802023
20.831503	1245.110823	12.807027
20.706423	1256.343776	12.812032
20.785598	1245.165533	12.817037
20.980077	1247.787182	12.822042
20.625265	1236.252359	12.827047
20.959089	1242.121043	12.832051
20.571537	1250.624948	12.837056
20.485288	1239.984065	12.842061
20.752969	1249.968412	12.847066
20.536186	1255.995893	12.852071
20.524184	1249.904048	12.857075
20.310326	1258.892800	12.862080
20.396257	1280.598563	12.867085
20.923608	1277.846080	12.872090
20.965085	1279.432346	12.877095
20.916645	1282.963292	12.882099
20.277297	1283.650402	12.887104
20.630255	1279.008014	12.892109
20.801700	1282.030766	12.897114
20.613014	1284.913825	12.902119
20.702870	1278.496615	12.907123
20.684653	1281.820874	12.912128
21.054378	1278.879052	12.917133
20.939739	1286.612416	12.922138
20.842635	1289.953991	12.927143
21.085369	1279.833084	12.932147
20.993131	1288.121160	12.937152
20.841194	1269.819848	12.942157
21.136401	1261.508948	12.947162
20.598266	1262.847014	12.952167
20.873023	1259.647509	12.957171
20.985297	1259.921398	12.962176
20.909307	1260.840372	12.967181
21.020399	1255.514272	12.972186
20.791338	1260.430302	12.977191
21.008256	1257.391422	12.982195
20.659265	1257.981752	12.987200
20.749440	1254.776994	12.992205
20.983541	1254.039474	12.997210
20.945818	1261.046144	13.002215
21.025905	1252.181313	13.007219
21.017918	1264.647790	13.012224
20.739608	1261.637433	13.017229
21.197045	1250.236414	13.022234
20.384117	1241.640193	13.027239
20.642120	1241.647969	13.032243
20.808584	1262.076050	13.037248
20.835244	1260.239279	13.042253
20.706516	1247.428809	13.047258
20.601277	1243.384681	13.052263
20.805895	1250.355846	13.057267
20.678486	1257.725352	13.062272
20.920966	1255.381038	13.067277
20.469259	1256.364671	13.072282
20.594922	1256.063947	13.077287
20.661363	1259.251687	13.082291
20.662486	1270.234269	13.087296
20.745014	1276.152512	13.092301
20.680653	1266.845475	13.097306
20.570764	1278.470291	13.102311
20.780478	1275.255924	13.107315
20.736512	1278.169520	13.112320
20.677629	1275.346528	13.117325
20.939670	1265.539542	13.122330
20.776152	1280.801754	13.127335
21.025551	1271.670191	13.132339
21.055730	1274.357477	13.137344
20.548918	1267.663253	13.142349
20.885001	1267.644381	13.147354
20.595493	1269.280284	13.152359
20.804510	1263.427591	13.157363
20.690660	1272.428788	13.162368
20.591815	1278.409079	13.167373
20.509804	1277.363983	13.172378
20.351205	1277.780432	13.177383
20.850262	1274.775400	13.182387
20.355876	1280.055479	13.187392
20.561092	1273.799657	13.192397
20.801713	1273.039017	13.197402
20.434425	1269.320552	13.202407
20.679499	1272.900880	13.207411
20.398032	1278.372519	13.212416
20.478683	1279.741208	13.217421
20.776941	1274.199154	13.222426
20.077746	1284.249427	13.227431
20.683104	1292.667530	13.232435
20.799964	1306.937227	13.237440
20.921247	1308.345174	13.242445
21.202266	1296.890250	13.247450
21.082451	1293.985503	13.252455
20.803662	1278.148880	13.257459
20.556933	1272.875116	13.262464
20.510836	1270.392310	13.267469
20.693646	1275.908175	13.272474
20.135183	1292.032969	13.277479
20.935965	1292.652814	13.282483
21.076509	1303.070670	13.287488
20.734619	1290.437675	13.292493
20.859669	1283.675779	13.297498
20.646642	1281.547628	13.302503
20.746156	1278.976936	13.307507
21.012648	1277.212305	13.312512
20.579051	1279.093559	13.317517
20.639813	1269.941619	13.322522
20.376137	1275.560240	13.327527
20.996842	1276.743435	13.332531
20.882750	1278.718818	13.337536
20.738969	1277.629954	13.342541
21.006965	1279.744681	13.347546
20.955050	1284.845369	13.352551
21.221973	1281.196066	13.357555
20.830362	1284.759669	13.362560
20.973554	1280.078195	13.367565
21.023161	1281.666318	13.372570
20.636676	1289.783692	13.377575
21.012846	1279.542146	13.382579
21.056079	1285.859351	13.387584
21.087272	1289.475375	13.392589
20.982616	1267.297964	13.397594
20.739095	1255.931469	13.402599
20.743978	1255.057031	13.407603
20.625209	1253.030554	13.412608
20.505413	1255.025769	13.417613
21.115145	1254.354500	13.422618
20.912701	1257.135662	13.427623
20.810138	1250.268149	13.432627
20.659837	1252.897480	13.437632
20.353419	1254.283748	13.442637
20.812869	1255.845924	13.447642
20.558573	1262.038675	13.452647
20.807847	1264.183197	13.457651
20.349129	1269.631061	13.462656
20.472658	1283.652071	13.467661
20.708737	1287.309537	13.472666
20.420148	1288.786012	13.477671
20.461547	1286.793911	13.482675
20.785767	1291.195892	13.487680
21.072013	1293.998469	13.492685
21.095646	1290.588258	13.497690
20.968207	1285.681845	13.502695
21.061760	1288.447342	13.507699
20.806817	1286.994556	13.512704
20.607254	1274.323103	13.517709
20.598950	1267.555674	13.522714
20.694831	1288.971258	13.527719
21.040966	1282.347576	13.532723
20.966502	1273.562581	13.537728
20.844640	1258.975223	13.542733
20.877373	1256.560277	13.547738
20.385148	1264.726044	13.552743
21.054415	1252.701412	13.557747
20.768859	1255.741853	13.562752
20.743392	1257.729907	13.567757
20.958564	1252.407709	13.572762
20.671374	1257.924411	13.577767
20.981383	1255.522014	13.582771
20.901321	1255.219408	13.587776
21.001448	1261.577994	13.592781
20.993854	1259.894932	13.597786
20.702229	1262.275550	13.602791
20.959125	1255.336507	13.607795
20.775375	1269.218844	13.612800
20.756348	1260.218418	13.617805
20.898313	1258.628205	13.622810
20.590717	1263.030020	13.627815
20.562020	1258.823857	13.632819
20.574758	1262.064321	13.637824
20.372253	1262.476733	13.642829
20.771365	1269.218175	13.647834
20.532385	1271.915273	13.652839
20.942933	1258.867379	13.657843
20.627448	1259.204764	13.662848
20.776682	1268.777477	13.667853
20.826227	1266.763578	13.672858
20.437066	1267.849207	13.677863
20.752282	1260.020854	13.682867
20.432008	1258.991683	13.687872
20.590924	1263.749629	13.692877
20.627166	1263.411125	13.697882
20.312159	1276.579490	13.702887
20.738841	1277.276351	13.707891
20.811872	1296.352061	13.712896
20.491359	1306.772491	13.717901
20.882017	1304.147470	13.722906
20.663158	1299.768184	13.727911
20.473525	1301.619991	13.732915
20.583427	1306.720109	13.737920
20.739897	1301.632778	13.742925
20.632649	1289.542722	13.747930
20.920022	1299.260591	13.752935
20.896598	1291.994052	13.757939
20.891448	1300.161004	13.762944
20.937663	1300.729303	13.767949
21.226634	1284.617596	13.772954
20.686203	1285.738394	13.777959
20.972092	1260.743553	13.782963
20.551312	1265.382636	13.787968
20.705866	1263.197435	13.792973
20.440602	1263.831185	13.797978
20.374519	1279.309684	13.802983
20.604001	1288.033761	13.807987
20.668221	1297.049151	13.812992
20.751037	1296.370454	13.817997
20.833757	1297.070136	13.823002
20.868505	1306.386723	13.828007
20.785334	1302.171888	13.833011
20.912603	1305.597536	13.838016
20.832853	1304.823334	13.843021
20.628032	1295.190150	13.848026
20.396474	1307.588236	13.853031
20.329561	1303.380271	13.858035
20.550380	1307.980113	13.863040
20.551827	1311.080451	13.868045
20.849178	1304.447193	13.873050
20.872164	1305.713111	13.878055
20.907360	1299.567982	13.883059
20.804613	1310.228091	13.888064
20.739422	1305.874758	13.893069
21.014886	1300.371025	13.898074
20.935467	1302.790347	13.903079
20.651585	1303.294594	13.908083
21.012410	1308.909821	13.913088
20.760508	1305.313302	13.918093
20.746971	1307.707923	13.923098
20.778657	1313.039732	13.928103
21.050002	1306.385388	13.933107
20.526140	1305.811343	13.938112
20.590919	1302.892922	13.943117
20.914585	1301.975521	13.948122
20.540568	1308.450759	13.953127
20.700456	1310.505458	13.958131
20.673984	1314.017136	13.963136
20.671264	1323.429603	13.968141
20.999461	1310.719675	13.973146
20.725444	1322.149913	13.978151
21.142344	1310.566064	13.983155
20.467412	1304.795994	13.988160
20.703924	1299.172309	13.993165
20.885281	1306.891591	13.998170
20.418883	1309.189697	14.003175
20.720765	1310.477368	14.008179
21.136460	1311.806814	14.013184
20.668319	1299.496748	14.018189
20.705114	1299.485183	14.023207
20.650231	1301.897598	14.028224
21.106726	1292.644497	14.033242
20.435550	1301.014828	14.038259
20.329006	1306.738893	14.043277
20.717892	1302.838656	14.048295
20.464608	1318.298158	14.053312
20.762612	1308.315261	14.058330
20.729169	1307.738604	14.063347
20.682132	1309.323916	14.068365
20.805544	1316.867510	14.073383
20.760283	1320.676838	14.078400
20.933806	1314.968903	14.083418
20.889939	1322.811319	14.088435
20.987557	1320.280474	14.093453
20.959325	1316.722048	14.098471
20.836549	1320.005756	14.103488
21.161852	1315.360591	14.108506
21.226945	1322.786073	14.113523
21.019783	1321.203627	14.118541
21.341435	1320.862920	14.123559
21.056571	1323.952254	14.128576
21.164684	1326.412609	14.133594
20.912107	1324.821677	14.138611
20.926958	1328.492429	14.143629
21.008518	1325.714028	14.148647
21.019236	1343.019113	14.153664
20.933391	1344.417133	14.158682
21.228750	1356.879012	14.163699
21.175749	1356.440756	14.168717
21.469601	1346.607935	14.173735
21.041495	1347.985041	14.178752
21.278428	1343.284748	14.183770
21.162153	1361.294389	14.188787
21.002682	1357.502052	14.193805
21.391119	1354.284580	14.198823
21.177486	1356.362095	14.203840
21.412225	1348.841658	14.208858
21.461578	1355.536622	14.213875
21.361846	1350.940363	14.218893
21.661762	1345.437203	14.223911
21.251552	1360.253230	14.228928
21.496503	1353.236114	14.233946
21.398302	1352.463714	14.238963
21.404563	1360.546698	14.243981
21.332278	1350.001475	14.248999
21.472068	1367.139707	14.254016
21.599477	1382.145291	14.259034
22.190554	1371.755373	14.264051
21.741361	1364.524919	14.269069
21.931054	1357.667627	14.274087
21.533968	1352.596541	14.279104
21.674671	1356.063179	14.284122
21.559689	1353.679498	14.289139
21.485878	1362.651448	14.294157
21.745922	1351.200620	14.299175
21.816618	1361.197176	14.304192
21.579863	1355.295111	14.309210
21.844749	1357.400123	14.314227
21.688362	1371.052513	14.319245
22.238363	1358.995421	14.324263
21.812816	1351.575580	14.329280
21.878987	1345.079350	14.334298
22.065514	1345.477509	14.339315
21.830455	1355.437884	14.344333
22.373672	1345.058765	14.349351
22.055708	1360.199860	14.354368
22.125325	1353.397903	14.359386
22.362333	1348.585909	14.364403
22.111733	1352.601035	14.369421
22.323785	1349.962267	14.374439
22.040688	1349.142279	14.379456
22.160746	1348.251694	14.384474
22.594320	1349.156299	14.389491
22.334818	1351.909679	14.394509
22.417143	1346.744825	14.399527
21.891324	1336.408808	14.404544
22.041094	1334.739541	14.409562
22.212909	1343.911406	14.414579
21.681709	1347.873757	14.419597
22.160051	1347.306705	14.424615
21.865577	1353.894485	14.429632
22.113324	1353.702420	14.434650
22.339160	1354.758139	14.439667
21.991424	1359.707425	14.444685
22.351490	1351.553505	14.449703
22.190798	1349.608133	14.454720
22.179897	1346.827172	14.459738
22.445154	1352.057789	14.464755
22.155628	1356.061820	14.469773
22.311661	1354.736052	14.474791
22.001024	1356.317796	14.479808
22.326978	1364.209788	14.484826
22.434220	1371.677337	14.489843
22.078319	1384.081091	14.494861
22.665507	1377.128928	14.499879
22.334479	1385.026619	14.504896
22.789902	1384.779407	14.509914
22.812820	1386.057835	14.514931
22.833631	1383.156976	14.519949
23.179836	1370.199555	14.524967
22.311482	1362.705615	14.529984
22.213057	1352.441419	14.535002
22.724692	1361.650331	14.540019
22.548185	1376.292242	14.545037
22.859727	1370.384515	14.550055
23.021967	1379.317252	14.555072
22.604625	1363.148310	14.560090
22.636442	1353.402899	14.565107
22.718100	1377.512769	14.570125
23.157770	1369.184117	14.575143
22.796043	1364.604473	14.580160
22.703912	1350.947759	14.585178
23.093909	1345.373601	14.590195
22.611955	1349.680462	14.595213
22.627323	1348.880509	14.600231
22.812656	1369.522544	14.605248
22.698006	1374.008358	14.610266
23.153471	1373.699790	14.615283
23.125932	1378.922061	14.620301
23.094286	1370.704763	14.625319
22.975299	1375.617569	14.630336
23.044263	1368.576604	14.635354
23.119657	1370.225768	14.640371
23.093494	1381.966580	14.645389
23.195977	1364.693807	14.650407
23.132722	1368.729393	14.655424
23.002368	1373.659741	14.660442
23.196835	1375.547895	14.665459
23.229288	1377.126828	14.670477
23.088527	1368.330746	14.675495
22.896675	1369.355559	14.680512
22.754513	1367.599142	14.685530
23.213374	1369.517485	14.690547
22.969208	1374.840375	14.695565
23.188212	1371.503630	14.700583
23.263218	1377.428432	14.705600
23.016926	1384.744732	14.710618
23.432403	1377.432985	14.715635
23.071413	1379.110854	14.720653
23.422919	1375.328247	14.725671
23.269128	1380.128626	14.730688
22.890971	1378.323331	14.735706
23.190463	1391.903027	14.740723
23.357601	1414.306711	14.745741
23.416131	1398.495993	14.750759
23.144501	1414.708874	14.755776
23.504533	1411.525809	14.760794
23.958786	1414.286482	14.765811
23.493174	1409.803620	14.770829
23.907558	1406.608740	14.775847
23.506093	1404.476817	14.780864
23.539583	1410.630056	14.785882
23.821764	1398.824867	14.790899
23.442476	1409.791448	14.795917
23.900349	1398.463190	14.800935
24.468743	1396.648492	14.805952
24.291677	1396.159236	14.810970
24.104388	1379.206378	14.815987
24.056837	1382.797432	14.821005
24.121267	1358.049262	14.826023
24.233260	1358.319307	14.831040
24.005688	1372.908011	14.836058
24.032295	1366.139651	14.841075
24.050595	1363.355602	14.846093
23.952159	1362.937177	14.851111
23.732826	1368.729595	14.856128
23.679714	1368.456527	14.861146
23.909534	1365.939195	14.866163
23.879314	1366.620469	14.871181
24.170851	1367.678294	14.876199
23.845905	1371.271118	14.881216
23.578419	1375.057703	14.886234
23.916500	1365.810858	14.891251
24.016397	1363.517174	14.896269
23.962394	1359.679698	14.901287
23.851146	1362.695730	14.906304
24.012207	1369.729967	14.911322
24.248190	1355.416860	14.916339
24.036986	1371.012854	14.921357
24.128417	1358.196757	14.926375
24.221898	1374.227086	14.931392
24.188593	1384.499802	14.936410
24.541974	1385.253602	14.941427
24.518262	1384.676963	14.946445
24.132582	1379.517529	14.951463
24.258837	1370.469639	14.956480
24.017998	1386.724770	14.961498
24.495247	1389.055471	14.966515
23.955138	1396.671904	14.971533
24.011185	1399.370243	14.976551
24.311469	1394.548142	14.981568
24.075735	1396.924923	14.986586
24.443476	1393.125565	14.991603
24.200294	1400.641156	14.996621
24.277618	1391.994323	15.001639
24.533488	1397.937478	15.006656
24.493292	1407.589949	15.011674
24.564737	1400.476212	15.016691
24.450658	1412.698271	15.021709
24.413821	1427.093008	15.026727
24.914081	1433.885980	15.031744
24.732511	1440.219829	15.036762
24.920411	1426.254105	15.041779
24.504642	1419.982579	15.046797
24.567687	1437.886634	15.051815
24.683274	1435.170427	15.056832
24.878085	1441.456829	15.061850
25.005207	1442.155483	15.066867
24.986619	1438.732346	15.071885
24.879749	1433.885509	15.076903
25.035732	1435.097098	15.081920
24.638233	1436.782369	15.086938
24.662201	1434.013134	15.091955
24.957594	1436.604089	15.096973
24.830204	1434.582606	15.101991
25.098625	1442.402019	15.107008
24.718708	1445.712611	15.112026
25.069363	1433.394664	15.117043
25.114156	1442.085043	15.122061
25.083377	1431.323924	15.127079
25.438610	1426.818673	15.132096
25.338377	1427.891798	15.137114
25.186344	1433.712834	15.142131
25.264326	1436.358916	15.147149
25.253701	1438.075292	15.152167
25.414305	1435.973266	15.157184
25.131217	1426.526577	15.162202
25.300375	1415.151545	15.167219
25.110205	1420.995962	15.172237
25.374544	1428.855345	15.177255
25.187795	1427.058841	15.182272
25.138901	1437.599928	15.187290
25.258732	1432.141190	15.192307
25.113172	1431.841967	15.197325
25.181426	1433.251597	15.202343
25.360677	1429.933764	15.207360
25.019374	1428.810014	15.212378
25.540714	1431.934380	15.217395
25.281323	1430.824307	15.222413
25.334018	1433.688359	15.227431
25.394276	1432.465953	15.232448
25.151736	1440.234725	15.237466
25.452308	1431.294278	15.242483
25.504603	1435.992589	15.247501
25.626256	1459.724973	15.252519
25.786522	1458.137392	15.257536
25.627971	1459.086111	15.262554
25.551927	1456.689910	15.267571
25.608300	1462.583112	15.272589
25.618570	1474.423583	15.277607
25.860063	1457.910344	15.282624
25.991600	1454.379886	15.287642
25.824971	1461.423962	15.292659
25.744408	1469.561755	15.297677
25.832523	1469.145033	15.302695
26.181452	1461.903635	15.307712
26.021889	1466.843393	15.312730
26.143272	1465.178639	15.317747
25.981531	1452.525540	15.322765
25.911467	1441.069090	15.327783
26.182768	1445.757643	15.332800
25.712228	1441.355783	15.337818
26.043954	1460.178154	15.342835
26.146328	1452.905298	15.347853
26.109765	1461.968899	15.352871
26.228774	1460.214860	15.357888
26.104190	1466.229737	15.362906
26.195125	1456.624268	15.367923
26.265671	1457.020479	15.372941
26.240493	1461.122378	15.377959
26.095421	1452.709188	15.382976
25.521628	1462.193540	15.387994
26.065814	1461.428788	15.393011
26.171645	1458.748740	15.398029
26.098821	1462.534187	15.403047
26.273541	1458.708969	15.408064
26.047399	1466.210864	15.413082
26.009177	1456.894990	15.418099
26.066000	1460.876841	15.423117
25.725364	1474.717596	15.428135
26.433465	1483.678166	15.433152
26.467859	1493.378574	15.438170
26.417408	1490.301864	15.443187
26.659839	1492.032941	15.448205
26.313921	1496.668155	15.453223
26.507222	1488.041307	15.458240
26.722915	1489.730243	15.463258
26.597985	1497.497590	15.468275
26.813278	1497.333511	15.473293
26.734520	1496.590250	15.478311
26.852409	1484.245677	15.483328
26.525109	1495.081330	15.488346
26.578158	1494.950207	15.493363
26.774078	1493.416712	15.498381
26.826131	1497.253038	15.503399
26.686861	1483.734283	15.508416
26.597858	1503.429229	15.513434
26.835533	1487.788835	15.518451
26.747990	1490.525038	15.523469
26.724828	1502.633568	15.528487
27.024562	1491.280909	15.533504
26.901165	1489.350806	15.538522
26.767543	1497.998101	15.543539
26.851220	1492.017342	15.548557
27.035108	1491.509049	15.553575
27.078649	1492.265083	15.558592
26.820010	1493.699330	15.563610
27.123171	1495.589040	15.568627
27.208327	1487.367204	15.573645
26.691540	1490.353561	15.578663
27.150979	1496.333503	15.583680
27.060585	1513.220749	15.588698
26.839379	1519.386344	15.593715
27.669880	1521.100708	15.598733
27.400919	1523.424606	15.603751
28.011341	1513.258027	15.608768
27.367150	1502.810204	15.613786
27.153556	1498.669374	15.618803
27.503837	1493.072393	15.623821
27.118127	1500.234017	15.628839
27.179673	1493.374293	15.633856
27.423568	1495.347390	15.638874
27.658902	1505.377563	15.643891
27.352894	1488.865096	15.648909
27.093518	1502.475832	15.653927
27.370769	1509.211597	15.658944
27.400570	1523.414111	15.663962
27.552029	1516.738242	15.668979
27.806106	1526.634874	15.673997
27.210562	1530.966983	15.679015
27.376214	1518.762632	15.684032
27.659803	1523.270705	15.689050
27.693369	1519.478210	15.694067
27.798071	1522.198700	15.699085
27.623680	1528.709987	15.704103
27.626970	1524.089376	15.709120
27.391137	1522.918907	15.714138
27.363365	1533.409503	15.719155
27.786989	1527.294280	15.724173
27.583534	1534.828772	15.729191
27.800073	1546.298190	15.734208
28.220423	1561.121951	15.739226
28.008131	1543.945578	15.744243
27.931004	1530.898230	15.749261
27.496158	1539.997875	15.754279
27.895391	1536.428633	15.759296
27.949961	1558.573632	15.764314
28.195539	1553.082994	15.769331
28.204054	1546.691829	15.774349
28.260453	1553.776670	15.779367
28.787368	1542.327960	15.784384
28.571059	1521.405184	15.789402
28.289022	1514.042595	15.794419
28.632487	1512.631074	15.799437
28.329747	1505.912820	15.804455
28.479996	1494.926145	15.809472
28.316262	1512.326899	15.814490
28.135069	1508.250113	15.819507
28.618474	1501.275119	15.824525
28.046876	1502.502873	15.829543
28.251008	1503.277339	15.834560
28.459101	1512.796680	15.839578
28.096438	1504.698173	15.844595
28.515599	1507.806605	15.849613
28.367529	1511.305182	15.854631
28.567604	1504.708083	15.859648
28.526911	1504.051561	15.864666
28.362256	1508.099426	15.869683
28.525099	1498.923707	15.874701
28.557518	1509.160072	15.879719
28.805749	1509.482325	15.884736
28.459351	1511.150015	15.889754
28.773808	1527.883040	15.894771
29.059824	1531.177101	15.899789
28.595708	1521.942487	15.904807
28.658770	1507.870749	15.909824
28.814964	1518.600988	15.914842
28.608645	1529.243545	15.919859
28.852385	1535.142285	15.924877
28.844672	1544.735395	15.929895
28.960066	1542.318084	15.934912
29.138544	1537.720652	15.939930
29.156510	1546.504251	15.944947
29.191674	1532.917515	15.949965
28.702125	1522.888620	15.954983
28.990390	1531.377406	15.960000
29.100114	1537.551575	15.965018
29.053956	1542.716311	15.970035
29.161980	1537.946852	15.975053
29.186914	1546.004151	15.980071
29.456674	1545.663851	15.985088
29.159003	1527.575359	15.990106
29.030202	1523.998316	15.995123
29.073936	1514.632366	16.000141
29.136511	1535.711082	16.005159
29.003412	1541.103623	16.010176
28.966619	1551.743540	16.015194
29.024670	1547.722182	16.020211
29.275957	1544.645312	16.025229
28.786253	1553.287298	16.030247
29.142770	1540.705622	16.035264
29.367372	1537.504018	16.040282
29.121815	1552.291617	16.045299
29.437590	1562.115510	16.050317
29.205235	1572.875513	16.055335
29.195652	1566.867911	16.060352
29.376305	1567.578484	16.065370
29.354608	1572.550559	16.070387
29.654784	1571.598198	16.075405
29.445911	1575.046711	16.080423
29.635965	1563.971048	16.085440
29.548067	1566.013593	16.090458
29.462164	1572.406963	16.095475
29.749533	1565.051060	16.100493
29.225765	1577.370849	16.105511
29.876485	1594.646516	16.110528
29.819193	1595.788313	16.115546
29.881764	1597.208304	16.120563
30.167820	1590.614757	16.125581
30.197661	1597.382947	16.130599
30.074852	1593.328287	16.135616
30.076898	1572.158243	16.140634
30.113233	1566.630186	16.145651
30.242287	1561.950963	16.150669
30.187470	1559.342926	16.155687
30.085859	1566.184766	16.160704
30.179675	1560.821368	16.165722
30.019625	1561.576057	16.170739
30.362954	1560.379279	16.175757
29.960428	1559.823726	16.180775
30.208129	1562.183203	16.185792
30.252811	1562.442752	16.190810
29.960883	1566.373288	16.195827
30.040485	1572.715090	16.200845
30.318440	1589.455582	16.205863
30.461425	1599.310206	16.210880
30.648298	1595.515262	16.215898
30.031236	1598.019753	16.220915
30.138617	1591.767747	16.225933
30.169880	1591.466273	16.230951
30.398300	1602.145726	16.235968
30.529201	1597.127197	16.240986
30.637004	1595.153125	16.246003
30.701072	1584.473509	16.251021
30.603838	1596.974617	16.256039
30.522757	1598.518198	16.261056
30.727752	1593.074132	16.266074
30.484648	1596.768792	16.271091
30.659514	1591.502571	16.276109
31.088573	1589.456810	16.281127
30.682684	1591.536706	16.286144
30.617257	1593.942986	16.291162
30.874387	1594.307869	16.296179
30.752102	1590.687296	16.301197
30.818744	1593.315553	16.306215
30.792673	1596.312541	16.311232
30.994893	1587.699156	16.316250
30.662930	1595.753630	16.321267
30.713871	1590.216155	16.326285
31.014634	1593.295512	16.331303
30.832943	1588.738206	16.336320
31.091241	1591.020490	16.341338
30.879441	1595.214329	16.346355
31.309425	1606.516826	16.351373
31.129712	1602.648997	16.356391
31.075490	1604.055370	16.361408
31.252795	1603.696780	16.366426
31.433045	1616.083645	16.371443
31.165418	1604.085188	16.376461
31.206153	1601.721462	16.381479
31.355050	1617.368040	16.386496
31.427642	1610.981570	16.391514
31.292865	1626.287211	16.396531
31.358313	1619.663554	16.401549
31.301947	1615.713912	16.406567
31.305453	1627.973241	16.411584
31.512201	1622.333035	16.416602
31.319806	1627.849114	16.421619
31.359259	1620.053721	16.426637
31.373558	1617.188461	16.431655
31.059148	1625.684549	16.436672
31.320570	1622.004341	16.441690
31.368980	1625.219127	16.446707
31.298522	1630.331138	16.451725
31.683500	1645.919643	16.456743
31.846449	1651.338154	16.461760
31.931653	1645.506531	16.466778
31.848253	1656.708472	16.471795
32.029192	1655.761753	16.476813
32.031865	1652.075615	16.481831
32.176216	1643.888296	16.486848
32.137342	1626.953950	16.491866
31.657008	1626.297542	16.496883
32.015215	1628.372766	16.501901
32.075137	1630.121959	16.506919
32.115641	1624.423321	16.511936
32.288328	1608.942606	16.516954
31.866914	1614.875108	16.521971
32.075846	1618.216879	16.526989
32.189081	1622.761593	16.532007
31.971998	1632.498271	16.537024
32.133885	1633.381734	16.542042
32.315322	1643.970393	16.547059
32.503445	1644.431231	16.552077
32.430251	1634.024378	16.557095
32.000649	1625.323761	16.562112
32.381453	1632.490612	16.567130
32.391142	1636.610596	16.572147
32.375368	1643.670025	16.577165
32.465801	1642.206038	16.582183
32.470865	1647.188029	16.587200
32.701556	1638.456811	16.592218
32.644981	1650.799677	16.597235
32.494879	1638.935036	16.602253
32.573069	1641.272797	16.607271
32.281930	1640.314855	16.612288
32.402860	1640.574042	16.617306
32.622639	1645.918203	16.622323
32.527837	1646.128425	16.627341
32.884500	1637.027890	16.632359
32.746752	1645.772676	16.637376
33.029564	1645.331188	16.642394
33.113635	1655.964488	16.647411
33.091749	1644.016469	16.652429
33.093973	1647.156038	16.657447
32.895973	1651.328029	16.662464
33.097962	1644.299536	16.667482
33.033454	1646.540503	16.672499
32.627480	1653.656668	16.677517
32.934825	1646.768678	16.682535
33.001754	1651.421465	16.687552
32.937013	1658.931537	16.692570
32.992065	1654.540165	16.697587
32.957619	1653.019800	16.702605
32.943955	1653.194272	16.707623
32.863502	1647.639978	16.712640
32.750835	1646.650422	16.717658
32.954001	1658.730849	16.722675
33.184169	1666.771211	16.727693
33.483109	1672.619518	16.732711
33.378923	1680.901988	16.737728
33.530687	1675.003106	16.742746
33.371726	1682.703618	16.747763
33.622426	1680.528983	16.752781
33.692590	1682.738251	16.757799
33.440792	1689.764559	16.762816
33.603293	1676.199852	16.767834
33.389868	1681.620201	16.772851
33.065669	1682.817946	16.777869
33.033946	1677.171709	16.782887
32.850248	1675.651550	16.787904
33.218762	1683.008371	16.792922
33.462275	1702.783478	16.797939
33.429736	1710.663624	16.802957
33.793443	1704.413160	16.807975
33.489248	1712.170673	16.812992
33.576705	1704.155997	16.818010
33.884272	1707.995672	16.823027
34.061935	1703.414835	16.828045
33.954100	1706.162966	16.833063
33.846112	1709.143941	16.838080
33.912691	1700.808539	16.843098
33.847627	1705.120584	16.848115
33.536598	1703.568032	16.853133
34.178029	1698.079487	16.858151
33.797947	1710.204216	16.863168
33.957900	1729.996621	16.868186
34.228216	1734.973302	16.873203
34.322353	1734.045142	16.878221
34.489206	1728.636212	16.883239
34.715740	1731.125728	16.888256
34.628738	1707.223848	16.893274
34.479268	1698.085233	16.898291
34.386994	1703.066250	16.903309
34.500846	1700.533536	16.908327
34.631284	1699.910275	16.913344
34.284079	1702.776026	16.918362
34.437319	1695.870906	16.923379
34.343386	1704.595367	16.928397
34.509645	1697.629178	16.933415
34.487705	1699.281320	16.938432
34.863061	1688.905137	16.943450
34.627140	1696.451969	16.948467
34.485450	1697.647349	16.953485
34.917673	1712.949166	16.958503
34.911642	1727.369175	16.963520
34.947345	1711.737945	16.968538
34.734709	1699.982333	16.973555
34.797511	1694.910923	16.978573
34.888567	1702.338750	16.983591
35.044024	1715.427321	16.988608
35.046383	1708.530529	16.993626
34.846822	1701.543244	16.998643
34.876160	1716.450767	17.003661
35.108439	1715.152134	17.008679
35.143629	1732.253209	17.013696
35.149288	1728.959850	17.018714
35.350095	1734.789226	17.023731
35.238830	1727.985269	17.028749
35.195726	1711.313420	17.033767
35.105849	1727.410352	17.038784
35.281310	1718.793293	17.043802
35.410109	1726.797945	17.048819
35.237233	1734.686329	17.053837
35.522164	1724.896364	17.058855
35.353989	1726.890385	17.063872
35.417004	1725.185360	17.068890
35.419969	1725.973047	17.073907
35.240428	1725.524287	17.078925
35.356866	1730.136168	17.083943
35.236891	1732.840620	17.088960
35.285227	1721.421697	17.093978
35.361787	1732.376377	17.098995
35.136376	1741.205204	17.104013
35.588633	1728.615176	17.109031
35.403830	1738.595325	17.114048
35.586850	1740.649742	17.119066
35.666803	1747.693167	17.124083
35.735155	1757.565309	17.129101
36.022176	1763.046661	17.134119
35.391699	1763.715147	17.139136
35.705410	1764.399002	17.144154
35.857621	1765.199856	17.149171
35.664007	1771.324187	17.154189
35.849885	1769.047401	17.159207
36.145130	1764.527233	17.164224
36.081334	1768.144570	17.169242
36.184618	1761.962362	17.174259
35.816947	1762.647923	17.179277
36.300751	1761.257257	17.184295
35.835875	1765.424652	17.189312
36.228904	1757.774148	17.194330
36.220589	1760.903625	17.199347
35.993215	1767.787641	17.204365
36.376160	1770.499981	17.209383
36.670523	1789.440431	17.214400
36.457734	1777.911307	17.219418
36.773629	1762.999075	17.224435
36.393708	1758.890989	17.229453
36.405790	1748.324156	17.234471
36.272164	1759.421710	17.239488
36.458386	1776.289525	17.244506
36.367526	1774.210255	17.249523
36.471411	1784.322938	17.254541
36.854137	1784.911626	17.259559
36.609976	1785.273093	17.264576
36.546668	1780.776286	17.269594
36.660089	1788.732299	17.274611
36.659268	1780.509067	17.279629
37.115004	1774.946286	17.284647
36.978576	1780.455069	17.289664
36.895651	1782.329315	17.294682
37.376187	1776.064121	17.299699
36.754000	1782.598176	17.304717
36.949010	1775.090150	17.309735
36.796942	1784.632506	17.314752
36.628800	1781.657880	17.319770
36.800267	1775.407372	17.324787
36.768538	1788.204165	17.329805
37.279352	1790.141024	17.334823
37.248464	1807.807247	17.339840
37.387329	1804.252726	17.344858
37.551388	1796.938399	17.349875
37.223206	1793.093412	17.354893
37.510844	1777.979595	17.359911
37.348309	1775.111047	17.364928
37.403255	1772.113426	17.369946
37.505709	1764.731858	17.374963
37.305743	1775.559206	17.379981
37.331552	1782.295090	17.384999
37.448074	1799.072584	17.390016
37.360993	1798.640536	17.395034
37.975547	1806.863501	17.400051
37.669986	1805.614462	17.405069
37.801281	1800.010606	17.410087
37.737826	1803.110345	17.415104
37.372132	1804.481467	17.420122
37.687572	1806.237907	17.425139
37.422902	1813.090925	17.430157
37.778395	1810.698986	17.435175
37.815114	1810.737215	17.440192
37.503095	1804.525268	17.445210
38.094182	1796.683485	17.450227
37.588506	1807.352753	17.455245
38.026761	1800.012781	17.460263
38.178644	1809.918042	17.465280
37.950383	1799.704913	17.470298
38.087272	1813.893776	17.475315
37.812534	1834.771095	17.480333
38.235679	1829.431369	17.485351
38.680276	1832.149618	17.490368
38.463568	1825.324679	17.495386
38.597100	1821.248733	17.500403
38.150272	1817.723127	17.505421
38.162448	1825.450691	17.510439
38.448177	1826.751738	17.515456
38.390178	1832.646027	17.520474
38.453049	1831.161248	17.525491
38.384792	1834.162654	17.530509
38.619016	1826.238553	17.535527
38.250993	1827.447231	17.540544
38.501421	1825.698145	17.545562
38.584781	1822.666879	17.550579
38.785339	1831.339727	17.555597
38.866317	1829.458783	17.560615
39.105215	1818.141531	17.565632
38.894856	1829.963995	17.570650
38.972587	1825.630306	17.575667
38.618826	1829.809099	17.580685
38.792883	1828.242089	17.585703
38.843181	1824.914059	17.590720
38.755143	1832.075560	17.595738
38.833973	1818.699468	17.600755
38.773563	1829.477068	17.605773
38.698820	1845.991737	17.610791
39.125979	1856.698672	17.615808
38.966309	1855.630864	17.620826
38.884784	1861.528918	17.625843
39.104313	1862.351289	17.630861
39.470207	1855.268237	17.635879
39.392184	1855.858838	17.640896
39.167967	1861.638857	17.645914
39.480004	1858.726063	17.650931
39.346926	1861.613537	17.655949
39.491196	1868.308543	17.660967
39.683898	1861.846175	17.665984
39.291718	1870.155022	17.671002
39.527488	1863.578812	17.676019
39.588410	1863.817686	17.681037
39.669508	1858.069222	17.686055
39.757321	1860.581672	17.691072
39.331094	1868.854261	17.696090
39.764065	1853.552009	17.701107
39.585834	1857.253691	17.706125
39.703248	1856.705650	17.711143
39.575537	1857.606214	17.716160
39.636476	1887.317368	17.721178
40.075087	1883.136115	17.726195
39.893602	1889.309687	17.731213
39.987049	1891.889675	17.736231
40.165401	1891.192693	17.741248
39.954749	1887.479168	17.746266
40.192449	1885.354557	17.751283
40.019752	1890.503417	17.756301
40.179305	1883.875643	17.761319
40.357246	1881.344475	17.766336
39.949140	1887.969494	17.771354
40.281916	1881.905584	17.776371
40.173260	1890.806333	17.781389
40.395525	1891.175212	17.786407
40.460651	1882.587453	17.791424
40.228088	1889.948221	17.796442
40.448448	1887.057123	17.801459
40.153161	1881.294744	17.806477
40.092941	1890.553518	17.811495
40.582331	1907.763265	17.816512
40.469859	1915.071857	17.821530
40.696148	1913.030078	17.826547
40.860738	1917.208810	17.831565
40.977381	1907.997730	17.836583
41.130658	1915.796437	17.841600
40.942219	1920.213958	17.846618
40.951258	1915.486906	17.851635
40.735771	1914.181017	17.856653
40.834208	1916.575372	17.861671
41.083771	1911.229480	17.866688
40.956583	1908.876755	17.871706
41.390829	1907.628483	17.876723
41.215626	1910.426725	17.881741
41.067988	1907.102717	17.886759
41.322055	1903.536091	17.891776
41.067393	1912.421599	17.896794
41.337925	1907.259564	17.901811
40.888296	1912.881275	17.906829
41.102315	1909.767801	17.911847
41.219371	1902.388554	17.916864
41.028861	1906.256596	17.921882
41.037655	1895.755465	17.926899
41.108414	1911.818327	17.931917
40.890209	1918.316324	17.936935
41.429912	1925.669563	17.941952
41.011304	1945.743312	17.946970
41.274237	1931.200388	17.951987
41.448331	1944.332600	17.957005
41.540328	1941.738047	17.962023
41.663013	1938.122363	17.967040
41.471766	1938.188300	17.972058
41.873172	1952.284769	17.977075
41.953432	1967.473095	17.982093
42.056758	1958.775372	17.987111
42.443264	1942.598703	17.992128
42.138327	1939.160554	17.997146
41.891359	1932.697488	18.002163
41.981406	1929.370174	18.007181
42.215891	1929.664742	18.012199
42.026676	1924.192973	18.017216
41.974117	1932.905466	18.022234
42.264361	1943.355860	18.027251
42.506333	1949.515405	18.032269
42.069497	1945.579161	18.037287
42.781889	1944.485523	18.042304
42.590567	1945.891771	18.047322
42.723859	1924.977151	18.052339
42.514027	1916.327827	18.057357
42.511863	1929.805122	18.062375
42.453302	1920.570064	18.067392
42.245533	1926.002972	18.072410
42.298537	1919.804333	18.077427
42.656845	1952.498806	18.082445
42.498851	1951.342629	18.087463
43.042938	1952.064474	18.092480
42.783199	1960.032904	18.097498
42.826480	1959.963114	18.102515
43.010239	1953.538314	18.107533
42.786692	1958.292588	18.112551
42.699669	1952.850917	18.117568
42.756897	1962.376525	18.122586
42.842700	1953.189999	18.127603
43.058872	1960.338438	18.132621
43.017890	1961.340800	18.137639
43.468905	1955.589144	18.142656
42.973846	1962.432570	18.147674
43.391731	1960.170665	18.152691
43.395243	1955.214020	18.157709
43.193631	1953.773771	18.162727
43.396042	1953.503985	18.167744
43.272576	1963.947228	18.172762
43.305848	1954.460748	18.177779
43.394334	1955.957657	18.182797
42.907714	1965.993178	18.187815
43.265098	1957.070093	18.192832
43.049839	1961.557975	18.197850
43.396545	1968.816169	18.202867
43.533021	1973.806414	18.207885
43.506699	1985.782133	18.212903
43.646197	1976.362072	18.217920
43.396178	1979.434972	18.222938
43.606046	1977.699416	18.227955
44.147372	1970.318538	18.232973
43.263124	1975.635188	18.237991
43.635761	1968.186041	18.243008
43.791721	1990.361934	18.248026
43.822359	2002.073736	18.253043
44.110307	2002.489562	18.258061
44.245728	2016.454686	18.263079
44.143584	2011.798036	18.268096
44.033796	2013.806380	18.273114
44.308676	2018.044634	18.278131
44.509058	2012.247195	18.283149
44.357393	2016.249079	18.288167
44.476192	2012.379937	18.293184
44.350680	2013.629394	18.298202
44.032814	2015.023582	18.303219
44.461748	2004.630766	18.308237
44.548309	2009.045355	18.313255
44.494099	2003.050982	18.318272
44.464588	2019.858314	18.323290
44.408502	2020.393510	18.328307
44.721091	2008.059129	18.333325
44.389818	2012.557664	18.338343
44.278362	2007.260664	18.343360
44.470048	2013.409379	18.348378
44.622045	2030.529930	18.353395
44.661969	2038.005412	18.358413
44.669503	2040.474852	18.363431
44.753227	2034.439590	18.368448
44.559229	2038.667684	18.373466
44.866367	2034.593093	18.378483
45.063160	2033.005918	18.383501
44.902956	2043.798807	18.388519
45.322033	2039.740970	18.393536
45.094106	2046.211471	18.398554
45.055633	2064.306319	18.403571
45.433295	2073.833594	18.408589
45.357561	2073.409166	18.413607
45.753352	2073.907688	18.418624
45.329971	2076.610255	18.423642
45.401427	2079.329860	18.428659
45.782972	2070.683658	18.433677
45.725189	2073.788056	18.438695
45.708815	2060.859539	18.443712
45.698235	2045.296686	18.448730
45.382725	2044.344960	18.453747
45.674628	2059.670312	18.458765
45.802577	2057.917136	18.463783
45.942406	2052.915120	18.468800
45.953292	2066.285059	18.473818
45.886226	2065.016836	18.478835
46.072590	2059.568490	18.483853
45.770741	2067.415484	18.488871
45.977043	2067.402283	18.493888
46.163130	2066.060648	18.498906
45.901514	2065.801943	18.503923
46.069897	2066.701702	18.508941
45.668245	2072.123898	18.513959
45.775397	2074.840956	18.518976
45.955277	2075.528081	18.523994
45.834122	2073.862615	18.529011
46.280821	2075.893118	18.534029
46.371697	2093.439585	18.539047
46.550355	2099.666712	18.544064
46.594308	2101.038596	18.549082
46.390779	2097.578729	18.554099
46.548302	2100.183930	18.559117
46.355515	2098.885415	18.564135
46.542028	2094.440695	18.569152
46.562382	2098.381343	18.574170
46.434817	2097.822026	18.579187
46.490167	2094.217043	18.584205
46.383592	2098.729321	18.589223
46.715560	2116.039935	18.594240
46.883845	2124.464043	18.599258
46.745063	2122.461584	18.604275
46.904081	2127.719654	18.609293
46.831024	2124.466290	18.614311
46.886606	2118.051636	18.619328
46.952840	2127.456357	18.624346
47.109706	2123.682582	18.629363
47.333837	2124.928196	18.634381
47.181871	2124.464798	18.639399
47.313949	2126.291425	18.644416
47.493898	2129.336681	18.649434
47.412054	2123.416672	18.654451
47.317606	2125.532703	18.659469
47.466325	2139.020736	18.664487
47.915927	2146.495433	18.669504
47.694169	2139.923640	18.674522
47.107229	2137.228895	18.679539
47.602063	2140.084709	18.684557
47.611918	2148.870752	18.689575
47.922328	2149.683366	18.694592
47.826964	2148.268626	18.699610
47.744028	2144.004516	18.704627
47.904235	2146.233317	18.709645
47.636925	2150.908896	18.714663
48.194112	2141.646284	18.719680
48.432313	2135.098669	18.724698
48.158181	2142.734414	18.729715
48.568145	2134.061618	18.734733
48.007678	2139.187460	18.739751
48.187986	2134.314250	18.744768
48.283036	2140.620801	18.749786
48.398928	2143.620430	18.754803
48.448560	2140.076128	18.759821
48.030258	2153.507520	18.764839
48.619432	2141.261845	18.769856
48.406817	2144.188016	18.774874
48.484620	2143.439415	18.779891
48.449033	2137.496291	18.784909
48.700898	2145.889777	18.789927
48.713360	2148.268780	18.794944
48.881573	2138.368159	18.799962
48.419989	2139.939447	18.804979
48.719099	2129.605005	18.809997
48.453358	2141.735450	18.815015
48.667756	2134.377530	18.820032
49.026173	2139.893261	18.825050
48.851047	2158.538597	18.830067
48.884208	2170.117201	18.835085
48.955872	2172.524521	18.840103
48.979034	2172.211742	18.845120
49.244243	2164.077221	18.850138
49.124718	2170.999285	18.855155
49.480241	2167.381019	18.860173
49.140285	2177.642635	18.865191
49.686771	2155.102798	18.870208
49.575479	2160.613220	18.875226
49.115774	2167.937989	18.880243
49.429138	2160.591015	18.885261
49.645461	2168.756571	18.890279
49.521061	2162.168454	18.895296
49.425217	2168.856274	18.900314
49.606661	2167.180290	18.905331
49.784237	2163.991558	18.910349
49.304039	2165.490307	18.915367
49.760143	2172.956115	18.920384
49.819185	2183.427040	18.925402
49.825605	2197.417632	18.930419
49.860584	2192.722536	18.935437
49.838413	2194.720076	18.940455
49.959131	2191.638728	18.945472
50.225876	2193.471416	18.950490
49.775450	2191.650796	18.955507
50.224225	2188.097882	18.960525
50.094278	2194.831269	18.965543
50.420659	2188.661280	18.970560
50.704709	2182.713566	18.975578
50.223499	2195.574538	18.980595
50.432755	2188.636655	18.985613
50.121878	2194.169483	18.990631
50.136076	2195.148115	18.995648
50.271422	2204.318476	19.000666
50.034670	2219.229623	19.005683
50.497651	2215.050684	19.010701
50.663016	2222.989998	19.015719
50.599536	2219.972631	19.020736
50.961031	2218.374114	19.025754
50.712877	2224.746451	19.030771
51.021960	2217.747011	19.035789
51.099701	2218.323796	19.040807
50.874362	2213.481433	19.045824
51.010038	2214.779706	19.050842
51.134290	2210.032611	19.055859
51.149613	2203.158687	19.060877
51.177615	2210.264896	19.065895
50.943909	2214.411277	19.070912
51.186308	2208.885507	19.075930
51.244419	2230.599921	19.080947
51.439209	2236.978703	19.085965
51.461138	2242.222496	19.090983
51.512430	2241.082470	19.096000
52.089510	2233.661937	19.101018
51.640154	2232.668619	19.106035
51.437981	2218.538603	19.111053
51.678888	2218.960366	19.116071
51.725526	2224.871948	19.121088
51.937923	2230.388192	19.126106
51.589090	2234.423941	19.131123
51.877186	2232.182697	19.136141
51.927879	2224.573966	19.141159
52.085214	2223.786719	19.146176
52.180760	2225.659301	19.151194
51.879443	2227.763506	19.156211
52.142726	2222.556896	19.161229
52.176146	2230.057112	19.166247
52.145490	2228.931730	19.171264
52.566202	2224.888528	19.176282
52.145269	2233.682762	19.181299
52.469913	2220.319798	19.186317
52.583971	2223.644592	19.191335
52.415715	2225.727575	19.196352
52.345888	2221.263921	19.201370
52.349927	2226.571915	19.206387
52.354185	2216.797285	19.211405
52.589938	2227.490189	19.216423
52.744669	2240.482601	19.221440
52.926186	2249.767547	19.226458
52.815940	2242.624958	19.231475
52.602990	2239.903581	19.236493
52.613598	2245.090975	19.241511
52.760664	2259.864650	19.246528
52.700903	2253.668910	19.251546
52.761400	2255.791711	19.256563
52.661584	2253.742903	19.261581
52.994070	2257.999572	19.266599
52.937369	2265.606995	19.271616
53.218342	2271.703824	19.276634
53.291933	2282.259023	19.281651
53.488197	2285.180577	19.286669
53.677784	2279.780404	19.291687
53.487617	2281.871609	19.296704
53.451547	2276.656876	19.301722
53.734992	2276.552715	19.306739
53.940021	2277.257078	19.311757
53.777615	2272.932452	19.316775
53.475625	2272.363191	19.321792
53.808009	2279.236829	19.326810
53.418675	2285.629349	19.331827
53.749839	2279.600930	19.336845
53.626746	2287.005004	19.341863
53.435381	2278.619954	19.346880
53.790380	2279.499403	19.351898
53.901053	2287.955606	19.356915
53.921557	2292.900745	19.361933
54.239208	2301.201239	19.366951
54.126572	2322.263417	19.371968
54.428887	2313.237992	19.376986
54.413822	2313.073678	19.382003
54.401241	2314.062095	19.387021
54.504753	2306.324551	19.392039
54.687607	2313.587813	19.397056
54.538956	2309.316830	19.402074
54.319985	2321.860785	19.407091
54.504126	2313.651015	19.412109
54.385101	2309.974681	19.417127
54.257795	2315.157351	19.422144
54.368542	2308.750333	19.427162
54.429542	2321.174910	19.432179
54.488590	2336.555784	19.437197
54.806773	2337.906764	19.442215
54.700541	2349.264688	19.447232
55.014331	2337.606300	19.452250
55.083828	2334.696701	19.457267
55.384136	2341.008359	19.462285
55.653772	2336.018579	19.467303
55.323146	2343.183623	19.472320
55.505270	2338.033179	19.477338
55.365979	2339.247104	19.482355
55.411849	2341.406861	19.487373
55.367852	2333.451347	19.492391
55.399461	2337.550728	19.497408
55.586864	2328.088191	19.502426
55.324064	2336.970534	19.507443
55.391849	2336.656927	19.512461
55.435211	2332.783214	19.517479
55.481486	2361.372076	19.522496
55.722873	2367.225126	19.527514
55.663419	2376.542292	19.532531
55.785999	2369.417568	19.537549
55.923318	2374.379501	19.542567
55.944290	2358.948933	19.547584
56.260919	2362.659913	19.552602
55.968893	2371.569749	19.557619
55.862882	2361.695408	19.562637
55.889996	2367.688034	19.567655
56.220907	2381.720654	19.572672
56.475766	2379.455585	19.577690
56.533385	2384.711043	19.582707
56.497767	2380.039731	19.587725
56.965241	2383.838355	19.592743
56.350728	2381.064581	19.597760
56.645523	2385.899146	19.602778
56.836620	2384.363971	19.607795
56.787217	2383.368993	19.612813
56.920135	2382.708340	19.617831
56.662645	2392.145984	19.622848
56.875026	2389.093238	19.627866
57.070470	2374.826503	19.632883
56.984532	2377.560255	19.637901
56.766961	2381.829962	19.642919
56.907887	2383.787357	19.647936
56.978079	2377.368686	19.652954
56.780556	2384.451168	19.657971
56.949068	2383.946874	19.662989
57.253822	2383.527827	19.668007
57.132537	2395.564650	19.673024
57.364567	2405.765877	19.678042
57.416714	2408.250288	19.683059
57.435586	2408.292939	19.688077
58.120418	2402.371675	19.693095
57.641306	2402.178326	19.698112
58.166043	2395.434659	19.703130
58.134199	2393.647936	19.708147
58.051874	2405.656529	19.713165
58.547110	2382.151511	19.718183
58.077289	2369.107832	19.723200
57.932217	2363.097126	19.728218
58.242548	2360.378007	19.733235
57.952629	2361.171537	19.738253
57.935945	2361.001188	19.743271
57.999938	2377.497478	19.748288
58.225422	2387.785475	19.753306
58.046947	2401.653940	19.758323
57.808132	2402.461347	19.763341
58.314278	2394.384237	19.768359
58.049917	2405.623479	19.773376
58.268737	2395.276485	19.778394
58.438675	2407.365981	19.783411
58.381069	2421.257664	19.788429
58.479060	2420.661574	19.793447
58.463435	2425.031232	19.798464
58.562939	2427.060526	19.803482
58.663115	2428.071084	19.808499
58.697317	2424.555918	19.813517
59.029686	2421.637413	19.818535
58.699891	2433.677632	19.823552
58.931810	2442.820943	19.828570
59.292710	2448.304933	19.833587
58.963845	2452.787485	19.838605
59.479325	2446.555766	19.843623
59.445064	2457.037049	19.848640
59.527709	2452.648903	19.853658
59.624832	2449.681387	19.858675
59.282841	2460.528745	19.863693
59.852134	2455.124584	19.868711
59.616150	2452.866208	19.873728
59.458075	2453.033830	19.878746
59.746330	2451.807227	19.883763
59.794213	2457.065837	19.888781
59.764339	2451.065039	19.893799
59.661231	2450.307519	19.898816
59.760783	2454.723317	19.903834
59.780251	2452.635006	19.908851
59.724108	2455.704613	19.913869
59.998207	2447.653470	19.918887
59.622471	2459.229870	19.923904
59.971031	2473.579120	19.928922
60.281878	2472.543199	19.933939
60.078566	2479.785541	19.938957
60.200046	2474.334805	19.943975
60.057569	2481.598123	19.948992
60.473959	2479.225472	19.954010
60.176221	2480.795833	19.959027
60.290456	2507.218100	19.964045
60.509422	2495.426832	19.969063
60.881922	2503.009976	19.974080
60.730111	2505.974503	19.979098
60.851428	2502.000214	19.984115
60.506386	2512.548406	19.989133
60.629646	2501.941271	19.994151
60.538181	2504.440737	19.999168
61.143499	2529.281549	20.004186
61.399537	2532.619953	20.009203
61.202394	2540.347455	20.014221
61.290162	2530.657621	20.019239
61.409153	2531.437860	20.024256
61.666165	2533.302035	20.029274
61.753198	2535.789557	20.034291
61.759564	2522.821607	20.039309
61.511620	2505.489318	20.044327
61.430042	2506.528868	20.049344
61.720676	2525.061059	20.054362
61.905313	2527.179047	20.059379
61.930746	2534.491124	20.064397
61.844723	2532.432211	20.069415
61.888206	2533.294499	20.074432
61.908381	2532.594399	20.079450
61.945017	2530.309050	20.084467
61.852540	2534.340178	20.089485
62.072699	2526.890685	20.094503
62.193018	2535.492586	20.099520
61.919154	2526.700510	20.104538
62.379851	2527.272866	20.109555
62.202172	2530.092858	20.114573
62.365802	2525.932471	20.119591
62.145122	2523.836040	20.124608
62.186670	2532.548040	20.129626
62.741693	2543.866729	20.134643
62.679203	2560.238664	20.139661
62.878895	2549.381753	20.144679
62.782486	2560.599047	20.149696
62.623795	2570.297930	20.154714
62.901276	2562.050323	20.159731
62.504655	2563.460265	20.164749
62.668090	2569.431233	20.169767
62.821165	2562.824638	20.174784
62.624007	2573.029144	20.179802
63.279480	2572.293796	20.184819
63.225428	2589.403030	20.189837
63.569112	2579.192525	20.194855
63.338096	2587.837118	20.199872
63.254641	2588.031383	20.204890
63.564368	2575.181764	20.209907
63.297273	2589.318610	20.214925
63.530503	2578.050446	20.219943
63.781107	2579.794515	20.224960
63.722132	2579.777214	20.229978
63.973688	2570.245295	20.234995
63.429262	2581.701602	20.240013
63.875010	2570.512033	20.245031
63.726486	2595.537685	20.250048
63.802956	2610.344214	20.255066
64.117684	2607.129580	20.260083
63.822175	2615.145758	20.265101
64.302883	2606.308018	20.270119
64.151485	2616.017567	20.275136
64.218627	2617.913608	20.280154
64.358816	2612.394550	20.285171
64.061486	2613.332435	20.290189
64.530421	2618.647448	20.295207
64.841724	2632.917844	20.300224
64.655849	2646.922230	20.305242
64.762187	2642.291123	20.310259
64.704087	2644.633478	20.315277
64.960456	2638.876420	20.320295
64.784202	2635.844702	20.325312
64.703420	2638.133252	20.330330
64.866651	2635.811964	20.335347
64.846116	2647.620545	20.340365
64.731656	2638.242134	20.345383
65.105657	2647.257510	20.350400
65.115390	2667.296182	20.355418
65.404649	2665.797239	20.360435
65.327376	2673.832132	20.365453
65.309334	2672.030588	20.370471
65.527829	2665.882327	20.375488
65.712503	2665.492650	20.380506
65.594640	2662.498023	20.385523
65.687616	2667.050230	20.390541
65.758423	2667.082239	20.395559
65.918158	2666.370887	20.400576
65.619109	2664.991727	20.405594
65.696409	2665.021128	20.410611
65.731691	2667.247909	20.415629
65.852257	2675.481725	20.420647
65.969711	2687.200683	20.425664
65.926103	2697.089744	20.430682
66.419415	2691.294877	20.435699
66.132575	2698.460976	20.440717
66.000754	2693.256645	20.445735
66.269783	2690.448876	20.450752
66.183022	2687.044970	20.455770
66.522885	2705.992732	20.460787
66.430389	2726.029697	20.465805
66.555983	2725.415820	20.470823
66.560686	2728.489939	20.475840
66.659271	2730.690115	20.480858
67.059950	2717.733834	20.485875
67.134026	2715.271792	20.490893
66.804199	2726.100887	20.495911
66.771414	2714.672886	20.500928
66.600337	2728.380014	20.505946
67.452091	2740.071579	20.510963
67.491069	2751.449919	20.515981
67.663993	2743.052126	20.520999
67.798647	2749.612991	20.526016
67.793247	2749.554109	20.531034
67.915893	2725.135722	20.536051
67.730149	2721.723210	20.541069
67.743858	2714.839864	20.546087
67.761526	2705.645640	20.551104
67.836388	2715.516607	20.556122
67.893511	2722.761583	20.561139
68.012462	2733.445957	20.566157
67.805890	2746.838616	20.571175
68.163548	2746.208180	20.576192
67.785352	2749.182901	20.581210
68.088244	2740.558292	20.586227
67.984390	2748.297770	20.591245
68.230865	2740.331106	20.596263
68.437107	2738.002944	20.601280
68.095437	2745.870807	20.606298
68.354788	2755.275813	20.611315
68.227945	2767.112456	20.616333
68.203499	2776.241801	20.621351
68.559567	2778.022564	20.626368
68.462089	2777.329416	20.631386
69.021509	2775.880196	20.636403
68.886207	2789.469191	20.641421
68.807418	2797.339993	20.646439
69.113414	2784.016463	20.651456
68.931995	2788.801254	20.656474
69.207219	2787.681322	20.661491
69.142024	2795.855159	20.666509
69.352158	2788.861005	20.671527
69.285498	2798.024627	20.676544
69.108783	2795.680442	20.681562
69.416927	2790.169143	20.686579
68.984064	2793.600170	20.691597
69.506983	2814.265932	20.696615
69.892263	2816.047547	20.701632
69.622398	2826.985931	20.706650
69.532625	2824.452462	20.711667
69.422651	2827.941342	20.716685
69.824931	2823.634259	20.721703
69.770108	2822.238159	20.726720
69.718076	2831.365645	20.731738
70.248232	2842.300735	20.736755
70.291016	2854.060840	20.741773
69.913485	2859.706805	20.746791
70.283125	2853.224436	20.751808
69.946385	2860.992462	20.756826
70.541101	2852.789279	20.761843
70.691570	2845.227242	20.766861
70.400823	2846.005196	20.771879
70.622537	2855.890595	20.776896
70.670274	2871.211693	20.781914
71.214120	2871.245350	20.786931
71.344397	2875.838084	20.791949
71.037163	2877.006467	20.796967
71.383905	2870.799124	20.801984
71.167760	2874.101214	20.807002
71.108543	2881.821058	20.812019
71.429893	2874.746984	20.817037
71.332999	2873.166441	20.822055
71.661944	2869.338288	20.827072
71.321857	2879.713685	20.832090
71.919172	2870.040689	20.837107
71.782787	2871.743465	20.842125
71.396557	2879.499728	20.847143
71.730896	2861.351255	20.852160
71.684977	2872.279915	20.857178
71.723245	2863.838240	20.862195
71.921734	2864.660096	20.867213
72.075409	2870.683873	20.872231
72.178747	2868.147131	20.877248
71.816912	2874.590581	20.882266
71.950107	2882.138935	20.887283
72.015799	2896.074333	20.892301
72.036093	2891.507213	20.897319
72.554708	2890.437345	20.902336
72.440006	2904.773589	20.907354
72.288341	2896.432194	20.912371
72.535191	2901.431902	20.917389
72.724595	2918.479882	20.922407
72.986874	2923.461405	20.927424
73.214829	2917.750461	20.932442
72.850749	2904.233200	20.937459
72.963325	2903.683534	20.942477
73.152766	2913.300378	20.947495
73.525405	2910.892162	20.952512
73.151803	2914.259490	20.957530
73.143990	2914.167954	20.962547
73.453497	2922.585736	20.967565
73.539826	2931.070580	20.972583
73.390436	2915.593439	20.977600
73.025485	2924.294986	20.982618
73.595711	2922.483761	20.987635
73.795720	2922.236370	20.992653
73.585298	2925.466764	20.997671
73.786047	2917.950160	21.002688
73.530729	2920.360196	21.007706
73.839083	2921.922042	21.012723
74.183856	2940.838649	21.017741
73.768438	2952.237697	21.022759
74.201986	2944.833410	21.027776
73.820916	2958.283194	21.032794
73.996482	2955.729412	21.037811
74.224292	2958.847446	21.042829
73.888497	2960.251656	21.047847
74.661602	2971.927635	21.052864
75.080274	2985.838291	21.057882
74.585405	2992.213333	21.062899
74.645183	2984.376213	21.067917
74.629793	2990.846270	21.072935
74.913672	2990.153650	21.077952
74.704129	2988.362941	21.082970
74.985796	2989.792966	21.087987
74.914146	2980.695409	21.093005
74.824834	3004.505647	21.098023
74.585871	3005.490883	21.103040
75.123679	3011.007445	21.108058
74.947984	3013.254553	21.113075
75.087027	3021.782960	21.118093
75.455149	3028.686654	21.123111
76.000526	3031.346590	21.128128
75.930135	3031.405839	21.133146
76.186959	3027.450702	21.138163
76.441604	3030.486597	21.143181
76.100282	3024.272502	21.148199
76.199684	3001.888411	21.153216
76.068934	3001.193480	21.158234
76.458548	3011.190652	21.163251
76.253042	3003.277837	21.168269
76.152604	3013.209999	21.173287
76.625805	3025.648887	21.178304
76.475426	3026.417836	21.183322
76.678964	3026.976952	21.188339
76.618329	3029.465297	21.193357
76.502768	3034.032784	21.198375
76.587192	3026.964958	21.203392
76.894836	3027.154279	21.208410
76.610114	3031.076184	21.213427
76.934536	3031.661645	21.218445
76.844157	3022.663016	21.223463
76.873250	3033.042573	21.228480
77.049346	3027.233664	21.233498
77.087364	3031.466730	21.238515
77.118170	3045.396822	21.243533
76.679552	3057.509967	21.248551
76.957199	3055.201046	21.253568
77.179314	3063.268642	21.258586
77.301852	3074.677172	21.263603
77.449020	3084.422797	21.268621
77.546905	3099.991790	21.273639
77.601718	3097.218107	21.278656
77.919479	3095.606023	21.283674
77.613763	3098.139758	21.288691
77.834332	3092.567584	21.293709
77.830957	3109.111628	21.298727
77.966339	3115.814134	21.303744
78.055705	3122.160562	21.308762
78.007575	3122.913209	21.313779
78.356650	3126.722262	21.318797
78.189349	3129.768046	21.323815
78.664016	3133.850483	21.328832
78.614140	3147.084004	21.333850
78.839392	3151.631000	21.338867
78.598263	3143.592423	21.343885
78.770798	3153.017824	21.348903
78.946023	3152.220598	21.353920
78.992960	3145.399401	21.358938
78.777992	3144.441787	21.363955
79.066918	3149.640180	21.368973
79.160209	3156.187373	21.373991
79.441269	3168.387999	21.379008
79.568518	3175.120935	21.384026
79.453668	3174.919034	21.389043
79.753614	3172.028368	21.394061
79.411841	3178.779467	21.399079
79.730191	3173.822543	21.404096
79.833484	3173.823414	21.409114
79.867699	3171.525766	21.414131
80.241494	3168.624897	21.419149
79.767217	3172.048455	21.424167
80.057727	3163.784275	21.429184
80.189784	3165.694422	21.434202
80.077514	3191.088169	21.439219
80.553084	3196.273333	21.444237
80.350248	3207.665419	21.449255
80.617369	3195.497768	21.454272
80.507347	3197.815453	21.459290
80.470287	3200.235564	21.464307
80.684389	3199.551703	21.469325
80.609281	3204.293716	21.474343
80.771875	3198.048740	21.479360
81.030221	3194.261656	21.484378
80.885871	3194.493958	21.489395
81.062322	3199.220236	21.494413
81.110837	3203.533487	21.499431
81.196317	3219.459355	21.504448
81.324196	3224.012464	21.509466
81.317103	3225.288760	21.514483
81.526383	3214.698857	21.519501
81.171287	3219.500472	21.524519
81.496287	3211.849843	21.529536
81.684640	3203.461913	21.534554
81.506395	3213.248507	21.539571
81.765497	3226.759276	21.544589
81.794366	3238.708340	21.549607
81.927981	3244.407448	21.554624
81.924068	3244.553637	21.559642
82.202373	3248.642250	21.564659
82.206292	3241.838881	21.569677
81.983197	3250.727241	21.574695
82.438958	3260.116197	21.579712
82.078045	3273.726673	21.584730
81.942109	3278.421773	21.589747
82.427061	3270.630757	21.594765
82.704027	3275.519596	21.599783
82.480494	3289.987633	21.604800
82.870684	3306.519481	21.609818
83.074993	3310.842530	21.614835
83.200487	3303.027798	21.619853
83.380529	3309.694953	21.624871
83.432088	3295.874266	21.629888
83.402732	3302.603130	21.634906
83.437105	3302.525316	21.639923
83.822394	3290.831174	21.644941
83.778182	3297.938416	21.649959
83.955886	3299.542379	21.654976
83.848460	3301.611090	21.659994
83.775968	3301.158576	21.665011
84.066620	3297.610956	21.670029
83.607241	3305.490021	21.675047
83.741502	3299.147259	21.680064
84.188937	3321.160697	21.685082
84.157626	3329.622055	21.690099
84.256117	3322.149873	21.695117
84.384186	3327.648519	21.700135
84.240012	3328.838130	21.705152
84.659289	3325.896152	21.710170
84.652963	3334.616265	21.715187
84.570926	3324.034196	21.720205
84.489203	3343.713941	21.725223
84.538986	3357.174041	21.730240
84.716206	3359.512807	21.735258
84.645551	3364.883471	21.740275
84.699404	3356.192810	21.745293
84.746850	3374.422678	21.750311
85.188601	3386.611234	21.755328
85.490525	3386.891151	21.760346
85.360360	3390.214256	21.765363
85.377558	3389.110257	21.770381
85.261693	3395.356591	21.775399
85.210211	3387.659715	21.780416
85.766794	3399.223471	21.785434
85.456100	3420.337691	21.790451
85.848493	3424.937569	21.795469
85.787506	3423.034224	21.800487
86.043930	3420.943385	21.805504
86.097054	3423.194182	21.810522
86.101586	3422.840296	21.815539
86.290256	3417.670340	21.820557
86.121131	3430.841323	21.825575
86.162497	3444.759884	21.830592
86.771757	3442.910124	21.835610
86.376536	3453.157052	21.840627
86.650205	3449.529507	21.845645
86.552779	3452.427338	21.850663
86.814299	3465.978061	21.855680
87.132093	3468.038768	21.860698
86.849930	3477.886161	21.865715
87.437413	3470.921971	21.870733
87.360411	3482.216325	21.875751
87.092214	3483.198386	21.880768
87.314403	3480.113962	21.885786
87.262694	3483.824190	21.890803
87.300863	3476.768244	21.895821
87.561157	3486.031190	21.900839
87.636633	3498.680227	21.905856
87.607419	3503.963308	21.910874
87.480401	3503.744463	21.915891
88.117674	3491.427074	21.920909
87.762331	3510.099720	21.925927
88.165199	3528.348617	21.930944
88.432617	3528.049562	21.935962
88.153715	3540.329573	21.940979
88.418585	3534.057133	21.945997
88.722780	3535.824239	21.951015
88.697623	3531.272822	21.956032
89.094095	3521.100448	21.961050
88.692276	3531.496372	21.966067
88.755293	3529.825751	21.971085
88.885924	3542.515589	21.976103
89.075087	3566.113985	21.981120
89.066678	3563.235447	21.986138
89.147817	3572.222585	21.991155
89.472047	3560.851840	21.996173
89.559499	3562.732967	22.001191
89.446353	3568.542351	22.006208
89.662826	3558.141423	22.011226
89.157662	3573.884968	22.016243
89.702720	3574.657104	22.021261
89.899715	3585.159739	22.026279
89.846165	3596.577092	22.031296
90.197761	3592.926072	22.036314
90.284376	3591.159643	22.041331
90.695726	3584.272261	22.046349
90.634338	3580.514041	22.051367
90.556918	3582.603965	22.056384
90.827322	3575.330794	22.061402
90.518568	3576.272917	22.066419
90.543848	3576.450639	22.071437
90.582750	3583.039736	22.076455
90.553244	3585.076394	22.081472
90.561712	3588.595337	22.086490
90.516486	3580.022608	22.091507
90.582414	3588.695949	22.096525
90.972524	3600.467344	22.101543
90.878070	3603.775361	22.106560
90.994491	3596.193196	22.111578
90.806097	3611.500807	22.116595
91.313175	3628.024605	22.121613
91.610948	3643.221679	22.126631
91.078678	3652.070693	22.131648
91.556202	3643.288699	22.136666
91.642061	3637.750388	22.141683
91.829923	3652.260160	22.146701
91.777210	3662.408559	22.151719
91.675450	3665.717755	22.156736
91.896616	3667.884367	22.161754
91.773788	3676.063950	22.166771
92.030961	3676.546102	22.171789
92.405598	3684.717157	22.176807
92.742999	3695.206134	22.181824
92.805391	3684.648758	22.186842
92.747481	3687.915567	22.191859
92.994052	3688.478862	22.196877
92.973027	3696.108870	22.201895
92.915786	3690.982754	22.206912
93.319823	3686.582321	22.211930
93.183220	3708.254461	22.216947
93.167219	3716.879585	22.221965
93.683732	3712.972533	22.226983
93.432819	3723.405099	22.232000
93.960431	3711.290667	22.237018
93.899660	3717.662083	22.242035
94.086380	3711.774118	22.247053
94.055315	3706.334667	22.252071
94.153350	3714.318573	22.257088
94.409466	3709.030775	22.262106
94.108854	3711.150016	22.267123
93.966701	3708.031608	22.272141
94.304471	3698.295629	22.277159
94.174200	3711.602264	22.282176
94.425219	3706.660621	22.287194
94.683860	3714.762087	22.292211
94.766654	3733.542930	22.297229
94.590384	3740.309583	22.302247
94.868154	3746.479918	22.307264
95.004573	3743.031522	22.312282
95.087127	3742.504708	22.317299
94.971791	3745.477038	22.322317
95.165681	3739.794023	22.327335
94.755412	3738.374279	22.332352
94.929189	3734.885314	22.337370
95.247189	3752.647711	22.342387
95.193499	3755.666065	22.347405
95.669689	3759.993878	22.352423
95.569167	3765.113000	22.357440
95.837733	3754.492015	22.362458
95.628940	3762.579157	22.367475
95.721133	3784.336069	22.372493
95.654855	3789.212167	22.377511
95.923886	3793.871957	22.382528
95.779800	3798.596841	22.387546
96.047654	3821.024348	22.392563
96.439266	3824.397288	22.397581
96.572820	3821.604619	22.402599
96.667828	3824.341249	22.407616
96.920648	3820.366088	22.412634
96.858569	3826.257896	22.417651
96.636888	3825.589224	22.422669
97.047493	3837.075916	22.427687
96.979829	3850.199627	22.432704
97.098074	3850.928925	22.437722
97.314045	3848.683999	22.442739
97.306208	3863.380947	22.447757
97.477776	3855.866161	22.452775
97.416426	3852.046506	22.457792
97.793380	3871.485466	22.462810
97.614465	3882.254367	22.467827
97.825466	3891.229646	22.472845
98.407169	3882.028912	22.477863
97.917117	3889.581990	22.482880
97.917109	3888.728498	22.487898
98.136103	3888.052481	22.492915
98.186534	3912.837038	22.497933
98.766578	3914.760016	22.502951
98.893852	3919.027092	22.507968
98.830396	3920.855236	22.512986
98.718661	3913.449319	22.518003
98.755139	3923.714262	22.523021
99.099932	3907.044131	22.528039
98.870002	3917.638687	22.533056
98.763720	3921.643288	22.538074
98.911158	3929.788567	22.543091
98.875828	3936.957634	22.548109
98.962995	3944.199211	22.553127
98.952886	3966.029346	22.558144
99.401367	3965.636117	22.563162
99.138152	3973.786333	22.568179
99.360089	3983.410500	22.573197
100.110246	3999.346074	22.578215
99.779238	4011.841680	22.583232
99.864959	4013.896995	22.588250
100.089138	4012.748930	22.593267
99.920477	4001.826970	22.598285
100.305806	4002.441311	22.603303
100.192645	4015.637718	22.608320
100.800818	4027.830954	22.613338
100.866224	4034.844763	22.618355
100.820051	4036.308297	22.623373
101.257911	4017.587290	22.628391
100.981780	4024.397530	22.633408
100.933927	4027.176647	22.638426
101.332666	4021.003801	22.643443
101.061548	4020.218708	22.648461
101.165728	4025.048822	22.653479
101.402769	4038.846275	22.658496
101.631592	4049.109739	22.663514
101.878602	4046.573485	22.668531
102.125643	4057.517670	22.673549
102.349134	4045.121062	22.678567
102.073464	4054.919029	22.683584
102.138750	4058.427450	22.688602
102.377081	4050.599049	22.693619
102.334757	4060.985216	22.698637
102.271660	4057.348294	22.703655
102.070859	4061.920251	22.708672
102.425964	4055.461706	22.713690
102.774151	4066.863346	22.718707
102.420611	4097.501775	22.723725
102.435030	4087.087069	22.728743
102.502795	4085.609938	22.733760
102.743274	4102.809276	22.738778
102.872033	4110.980448	22.743795
103.362688	4118.028752	22.748813
103.217542	4123.118140	22.753831
103.300077	4125.085871	22.758848
103.290507	4136.261412	22.763866
103.763356	4146.927357	22.768883
103.481494	4161.184493	22.773901
103.667672	4151.219080	22.778919
103.972705	4151.772285	22.783936
103.913981	4152.576235	22.788954
104.116935	4163.920869	22.793971
104.362432	4182.130384	22.798989
103.974341	4172.885878	22.804007
103.849584	4179.054506	22.809024
104.373949	4185.450029	22.814042
104.901323	4202.044403	22.819059
104.467060	4209.879819	22.824077
104.590012	4213.324800	22.829095
105.160128	4200.822438	22.834112
105.567412	4194.017239	22.839130
105.870640	4188.703664	22.844147
106.063882	4190.174662	22.849165
106.154635	4182.153387	22.854183
106.192525	4187.823287	22.859200
106.139031	4177.012634	22.864218
106.185258	4154.064924	22.869235
105.869549	4151.965313	22.874253
105.821631	4146.231809	22.879271
106.083888	4155.037807	22.884288
106.219605	4167.427650	22.889306
106.546752	4173.833378	22.894323
106.328955	4182.011866	22.899341
106.271138	4183.898932	22.904359
106.337079	4182.728887	22.909376
106.427105	4180.728987	22.914394
106.674471	4176.436783	22.919411
106.270970	4194.219584	22.924429
106.677464	4203.373924	22.929447
106.982490	4210.096295	22.934464
106.981919	4210.097211	22.939482
107.168422	4204.565453	22.944499
107.216854	4218.858082	22.949517
107.492022	4230.240026	22.954535
107.474188	4245.329932	22.959552
107.407361	4249.799554	22.964570
107.991542	4236.909444	22.969587
107.897001	4240.330900	22.974605
108.059271	4248.153024	22.979623
108.081519	4234.484812	22.984640
107.807637	4250.164659	22.989658
108.120453	4258.614943	22.994675
107.945761	4272.801602	22.999693
108.452360	4264.328494	23.004711
108.567207	4273.911715	23.009728
108.361739	4291.688228	23.014746
108.860567	4293.762669	23.019763
108.899689	4304.945520	23.024781
109.024747	4306.435269	23.029799
108.880625	4307.505371	23.034816
109.047164	4317.470575	23.039834
109.363732	4330.077949	23.044851
109.651322	4338.632998	23.049869
109.552149	4329.395028	23.054887
109.900841	4331.454082	23.059904
109.595054	4341.360098	23.064922
110.010072	4325.317875	23.069939
109.726973	4343.888799	23.074957
109.763370	4361.660654	23.079975
109.908748	4360.648640	23.084992
110.041613	4366.298743	23.090010
109.952413	4370.232299	23.095027
110.054957	4391.080618	23.100045
110.529519	4399.188153	23.105063
110.420092	4396.876245	23.110080
110.645285	4410.205496	23.115098
111.089714	4420.931243	23.120115
110.925689	4420.180184	23.125133
111.233585	4420.109883	23.130151
111.656259	4421.988014	23.135168
111.673321	4411.257980	23.140186
111.793494	4409.086462	23.145203
111.686924	4418.431317	23.150221
111.786310	4397.335282	23.155239
112.105058	4407.880456	23.160256
112.001956	4405.821639	23.165274
112.205102	4394.761427	23.170291
112.339847	4403.714566	23.175309
112.239902	4400.560957	23.180327
112.674019	4420.770358	23.185344
112.610004	4429.585283	23.190362
112.638618	4428.407011	23.195379
112.723078	4432.386840	23.200397
112.760589	4433.715917	23.205415
112.844503	4426.224260	23.210432
112.997505	4432.112693	23.215450
113.172367	4428.244206	23.220467
113.156211	4435.871462	23.225485
113.213025	4455.913722	23.230503
113.358324	4461.176399	23.235520
113.132027	4467.458890	23.240538
113.514451	4463.925469	23.245555
113.684826	4476.694741	23.250573
113.832861	4496.259932	23.255591
113.846131	4492.504520	23.260608
113.748790	4491.554017	23.265626
114.113132	4494.512154	23.270643
114.164060	4518.555796	23.275661
114.171831	4525.593192	23.280679
114.273230	4530.962805	23.285696
114.143394	4532.514465	23.290714
114.330233	4533.869301	23.295731
114.556257	4548.408489	23.300749
114.529803	4545.813488	23.305767
114.892494	4559.884835	23.310784
114.990080	4579.642270	23.315802
115.188033	4577.686469	23.320819
115.292327	4581.131365	23.325837
115.134287	4589.751329	23.330855
115.374987	4606.652276	23.335872
115.536133	4612.503295	23.340890
115.779237	4612.236423	23.345907
116.082138	4635.738159	23.350925
116.427383	4636.897816	23.355943
116.562244	4645.682730	23.360960
116.189191	4655.411659	23.365978
116.308965	4647.701760	23.370995
116.548668	4648.900276	23.376013
116.472784	4653.558701	23.381031
116.779818	4665.881523	23.386048
117.102435	4682.881208	23.391066
117.301499	4679.247170	23.396083
117.050539	4682.304250	23.401101
117.054525	4676.629918	23.406119
117.339226	4661.302776	23.411136
117.269047	4696.670998	23.416154
117.796502	4696.006336	23.421171
118.086169	4701.443542	23.426189
117.930907	4702.159069	23.431207
117.769392	4697.592845	23.436224
117.571506	4703.860678	23.441242
118.193355	4706.524476	23.446259
118.325041	4716.433359	23.451277
118.380453	4728.765677	23.456295
118.596138	4725.776439	23.461312
118.674283	4731.950704	23.466330
118.590445	4727.753639	23.471347
118.542751	4730.281902	23.476365
118.563598	4750.711853	23.481383
118.998306	4751.611014	23.486400
118.962319	4763.458374	23.491418
119.050091	4762.426411	23.496435
119.212347	4782.589976	23.501453
119.051669	4793.970269	23.506471
119.374814	4791.730928	23.511488
119.448910	4815.109733	23.516506
119.780738	4826.773404	23.521523
119.848213	4828.208666	23.526541
119.876259	4831.582388	23.531559
120.084324	4833.994361	23.536576
120.028364	4856.425523	23.541594
120.358772	4856.713523	23.546611
120.369238	4860.898013	23.551629
120.611344	4874.453923	23.556647
121.180709	4886.560449	23.561664
121.423660	4895.149690	23.566682
121.441816	4891.372943	23.571699
121.574883	4896.734493	23.576717
121.236628	4886.923017	23.581735
121.756430	4884.350204	23.586752
121.823497	4885.175829	23.591770
122.052771	4883.743669	23.596787
121.898071	4872.531682	23.601805
121.750703	4887.107932	23.606823
122.165867	4900.416776	23.611840
122.097279	4913.693417	23.616858
122.204714	4905.009032	23.621875
122.649030	4902.438026	23.626893
122.654454	4910.572666	23.631911
122.817375	4911.288602	23.636928
122.919383	4931.735758	23.641946
123.113591	4935.472435	23.646963
123.162956	4937.292941	23.651981
123.004033	4941.087503	23.656999
123.516632	4934.678990	23.662016
123.204789	4940.186240	23.667034
123.384417	4941.416389	23.672051
123.580967	4956.363483	23.677069
123.491830	4970.027371	23.682087
124.188576	4963.793244	23.687104
123.818103	4975.729514	23.692122
123.873167	4972.605348	23.697139
124.205435	4975.010126	23.702157
124.187999	4993.183115	23.707175
124.469903	4995.645491	23.712192
124.471477	5007.154273	23.717210
124.445052	5009.431374	23.722227
124.682869	5009.819895	23.727245
124.364111	5012.271061	23.732263
124.936207	5023.953220	23.737280
124.816110	5035.331161	23.742298
124.992787	5033.657195	23.747315
125.199576	5050.311520	23.752333
125.164143	5066.236643	23.757351
125.451574	5061.558594	23.762368
125.401585	5070.019996	23.767386
125.425586	5093.054775	23.772403
125.611037	5097.765288	23.777421
125.726065	5104.637951	23.782439
126.039629	5113.251464	23.787456
126.146008	5125.849769	23.792474
126.440496	5124.012249	23.797491
126.378543	5135.842019	23.802509
126.462758	5151.275328	23.807527
127.067544	5145.420047	23.812544
127.090326	5151.852711	23.817562
127.062473	5151.372564	23.822579
127.621001	5165.183538	23.827597
127.792358	5161.735536	23.832615
127.955443	5160.982628	23.837632
128.064975	5170.036236	23.842650
128.063166	5176.832370	23.847667
128.231666	5170.334654	23.852685
128.098644	5181.613279	23.857703
128.569640	5171.855092	23.862720
128.193546	5181.220591	23.867738
128.287702	5179.134931	23.872755
128.887825	5169.287710	23.877773
128.893218	5193.458510	23.882791
128.927136	5192.858368	23.887808
129.082797	5198.437498	23.892826
129.109928	5197.051704	23.897843
129.349152	5190.401876	23.902861
129.167276	5194.524297	23.907879
129.232066	5193.886190	23.912896
129.373238	5220.187103	23.917914
129.613988	5235.824480	23.922931
129.750189	5230.301936	23.927949
129.599987	5233.169192	23.932967
130.169895	5246.972922	23.937984
130.316497	5258.899347	23.943002
130.003419	5268.712734	23.948019
130.596254	5262.540685	23.953037
130.210753	5271.391639	23.958055
130.539203	5278.374325	23.963072
130.527710	5293.694020	23.968090
130.478950	5297.830646	23.973107
131.096099	5295.409819	23.978125
130.947148	5306.219034	23.983143
131.326900	5320.341890	23.988160
131.521299	5331.186850	23.993178
131.421790	5327.350866	23.998195
131.520566	5321.958561	24.003213
131.788541	5341.859784	24.008231
132.320918	5348.585765	24.013248
132.154286	5344.363961	24.018266
132.399644	5349.338002	24.023283
132.223721	5351.814438	24.028301
132.249315	5350.298274	24.033319
132.276341	5357.682310	24.038336
132.168983	5380.497741	24.043354
132.648195	5387.832504	24.048371
133.203609	5373.188413	24.053389
132.904087	5398.120171	24.058407
133.203029	5412.925522	24.063424
133.400561	5409.188487	24.068442
133.337815	5404.996519	24.073459
133.497656	5407.939463	24.078477
133.900426	5435.165170	24.083495
134.139151	5432.975388	24.088512
134.235521	5438.610482	24.093530
133.926025	5435.601782	24.098547
134.150199	5434.548810	24.103565
134.328104	5456.863344	24.108583
134.563850	5464.106367	24.113600
134.687366	5470.431058	24.118618
134.786334	5478.280453	24.123635
135.143566	5472.422035	24.128653
135.256445	5483.793854	24.133671
135.113900	5487.351492	24.138688
135.246391	5491.146931	24.143706
135.307072	5490.588928	24.148723
135.821576	5489.977443	24.153741
135.799202	5510.712729	24.158759
135.856462	5514.109486	24.163776
136.224313	5521.685511	24.168794
136.282151	5515.595520	24.173811
136.318798	5513.323869	24.178829
136.316579	5524.430842	24.183847
136.519017	5529.257584	24.188864
136.629757	5538.952430	24.193882
136.463451	5548.988851	24.198899
136.946077	5546.255066	24.203917
136.939586	5560.143920	24.208935
137.169104	5571.911828	24.213952
137.391546	5562.421179	24.218970
137.313376	5566.836360	24.223987
137.606909	5575.091432	24.229005
137.637911	5587.523557	24.234023
137.926646	5594.440346	24.239040
138.075985	5597.314195	24.244058
138.100530	5603.539071	24.249075
138.679548	5614.667511	24.254093
138.663036	5628.980516	24.259111
138.603550	5627.224555	24.264128
139.012883	5623.621274	24.269146
138.809314	5635.991712	24.274163
138.861449	5629.935627	24.279181
138.732700	5629.803564	24.284199
139.126006	5646.794666	24.289216
139.430167	5653.713743	24.294234
139.160466	5664.191579	24.299251
139.884272	5656.443849	24.304269
139.554836	5660.257914	24.309287
139.443834	5686.124663	24.314304
139.515284	5685.243151	24.319322
139.674723	5701.107987	24.324339
140.200571	5712.855507	24.329357
140.264011	5726.570507	24.334375
140.070070	5730.499881	24.339392
140.345654	5748.741156	24.344410
140.375686	5762.644046	24.349427
140.793437	5773.356159	24.354445
140.997312	5792.006238	24.359463
140.991808	5784.719336	24.364480
141.669472	5790.317737	24.369498
141.595365	5811.942872	24.374515
142.140490	5808.026004	24.379533
142.082430	5822.558249	24.384551
142.309559	5820.739255	24.389568
142.487235	5818.817211	24.394586
141.979454	5821.001247	24.399603
142.678720	5818.477556	24.404621
142.842206	5835.595212	24.409639
142.614128	5844.500867	24.414656
143.032526	5845.633228	24.419674
142.894772	5849.297975	24.424691
142.862981	5853.549279	24.429709
143.258715	5866.880981	24.434727
143.369250	5870.745321	24.439744
143.508335	5865.794851	24.444762
143.275527	5884.325065	24.449779
143.917322	5900.005414	24.454797
143.815896	5901.518853	24.459815
143.878170	5909.622948	24.464832
143.967939	5917.891033	24.469850
143.816753	5946.825979	24.474867
144.314900	5946.449187	24.479885
144.710287	5967.692846	24.484903
144.879103	5974.280393	24.489920
145.375279	5968.283973	24.494938
145.140692	5978.434638	24.499955
145.229602	5975.703761	24.504973
145.124024	5981.046324	24.509991
145.300506	5998.161310	24.515008
145.743076	6003.274072	24.520026
145.917125	6008.084256	24.525043
146.047648	5995.198092	24.530061
145.698444	6005.568467	24.535079
145.759362	6031.720757	24.540096
146.010597	6027.828664	24.545114
146.288527	6044.995978	24.550131
146.683191	6059.963741	24.555149
146.724201	6069.537087	24.560167
146.831532	6069.650618	24.565184
146.881411	6074.397224	24.570202
147.070700	6089.330887	24.575219
147.629704	6095.170986	24.580237
147.217148	6098.195897	24.585255
147.409316	6101.387957	24.590272
148.168733	6114.789354	24.595290
147.967851	6135.367509	24.600307
147.925223	6131.434913	24.605325
148.013122	6130.239972	24.610343
148.341731	6144.433143	24.615360
149.009603	6148.934105	24.620378
149.107079	6157.830524	24.625395
149.377317	6152.219390	24.630413
148.988746	6158.257024	24.635431
149.188267	6162.613943	24.640448
149.391495	6149.052792	24.645466
149.022691	6175.575980	24.650483
149.432645	6182.152709	24.655501
149.788783	6186.622350	24.660519
149.881092	6200.889445	24.665536
150.127195	6207.246047	24.670554
150.067455	6220.627877	24.675571
150.105805	6219.471515	24.680589
150.235887	6225.712083	24.685607
150.164492	6245.682798	24.690624
150.444736	6253.206294	24.695642
150.456546	6272.580767	24.700659
150.811231	6282.946890	24.705677
150.927871	6287.413050	24.710695
150.827358	6305.987211	24.715712
151.170691	6317.562898	24.720730
151.334157	6329.809298	24.725747
151.389693	6340.747953	24.730765
151.615742	6350.431240	24.735783
151.435620	6369.071675	24.740800
151.838980	6375.809263	24.745818
151.938061	6393.350115	24.750835
152.342692	6414.155481	24.755853
152.869167	6417.652301	24.760871
152.499019	6422.823984	24.765888
152.707263	6434.883941	24.770906
152.738807	6451.422231	24.775923
152.829268	6452.500713	24.780941
153.429070	6470.372528	24.785959
153.107468	6480.717587	24.790976
153.609867	6478.871934	24.795994
153.733633	6488.536213	24.801011
153.737881	6498.455597	24.806029
154.138798	6501.525551	24.811047
154.464893	6503.560200	24.816064
154.716297	6509.279562	24.821082
154.627798	6528.098355	24.826099
154.755597	6531.653261	24.831117
155.075103	6536.291719	24.836135
155.202077	6542.327560	24.841152
155.523307	6525.903734	24.846170
155.333071	6542.637996	24.851187
155.397112	6561.607180	24.856205
155.530957	6567.074647	24.861223
155.577796	6566.589625	24.866240
156.166469	6581.660741	24.871258
155.941083	6601.214301	24.876275
156.513621	6603.830463	24.881293
156.534420	6594.825298	24.886311
156.761444	6601.814559	24.891328
157.294989	6605.696621	24.896346
157.468414	6615.167378	24.901363
157.332203	6623.851918	24.906381
157.471561	6619.739895	24.911399
157.484103	6617.093464	24.916416
157.684930	6617.030796	24.921434
157.763978	6625.564567	24.926451
158.092426	6637.579559	24.931469
158.478505	6639.778549	24.936487
158.380980	6645.205828	24.941504
158.448617	6646.426443	24.946522
158.593103	6646.846418	24.951539
158.555086	6654.376016	24.956557
158.661563	6674.249707	24.961575
158.526203	6680.414769	24.966592
158.988526	6680.271852	24.971610
158.868040	6702.035502	24.976627
158.871609	6716.674456	24.981645
159.541736	6725.223408	24.986663
159.630540	6746.041831	24.991680
159.567084	6742.906293	24.996698
159.716571	6762.815732	25.001715
159.838617	6784.938175	25.006733
160.231825	6784.954201	25.011751
160.162226	6814.497840	25.016768
160.522831	6823.318084	25.021786
160.841920	6829.839565	25.026803
160.683379	6841.598757	25.031821
161.266111	6843.562636	25.036839
161.011003	6849.086716	25.041856
161.357070	6855.331667	25.046874
161.893693	6871.802482	25.051891
162.086497	6867.913196	25.056909
162.448195	6865.243310	25.061927
162.380836	6870.477810	25.066944
162.583768	6859.856422	25.071962
163.101574	6858.095606	25.076979
162.987824	6854.884659	25.081997
163.373356	6851.783730	25.087015
163.288121	6854.577204	25.092032
163.204205	6849.221343	25.097050
163.564602	6864.520345	25.102067
163.369892	6880.634896	25.107085
163.641905	6882.220290	25.112103
163.320214	6890.201238	25.117120
163.661597	6896.171565	25.122138
163.808575	6919.890636	25.127155
163.826769	6923.445016	25.132173
164.173207	6919.297533	25.137191
164.213093	6947.808188	25.142208
164.550143	6949.273851	25.147226
164.824126	6956.489481	25.152243
164.834953	6977.357643	25.157261
165.244668	6983.143220	25.162279
165.229159	6981.170002	25.167296
165.268700	6981.906503	25.172314
165.654871	7002.452053	25.177331
165.637642	7006.776901	25.182349
166.049962	7009.849080	25.187367
166.223074	7032.114822	25.192384
166.370371	7038.131101	25.197402
166.524452	7041.252330	25.202419
166.317049	7045.836478	25.207437
166.716920	7056.700302	25.212455
166.633401	7067.964595	25.217472
166.957859	7074.986543	25.222490
167.305521	7089.910914	25.227507
167.452032	7108.194116	25.232525
167.900590	7096.967661	25.237543
167.540577	7106.404186	25.242560
167.846044	7124.980733	25.247578
168.219256	7133.184633	25.252595
168.332258	7141.956421	25.257613
168.686923	7158.580102	25.262631
168.658717	7172.154470	25.267648
168.933349	7172.247630	25.272666
168.902962	7170.672540	25.277683
168.770419	7187.315708	25.282701
169.259929	7195.247737	25.287719
169.338044	7203.977913	25.292736
169.347536	7213.335920	25.297754
169.550022	7236.623719	25.302771
169.615979	7236.706875	25.307789
169.918248	7246.603634	25.312807
169.925276	7260.925473	25.317824
170.315389	7265.677227	25.322842
170.534523	7294.500670	25.327859
170.431423	7303.440771	25.332877
171.010060	7296.912148	25.337895
171.046341	7318.585607	25.342912
170.950288	7322.998651	25.347930
171.304404	7323.240445	25.352947
171.303710	7335.729446	25.357965
171.833651	7351.315871	25.362983
172.024518	7357.764395	25.368000
172.187521	7354.758646	25.373018
172.336617	7359.290771	25.378035
172.431695	7381.692225	25.383053
172.886748	7385.258109	25.388071
172.698848	7384.882878	25.393088
172.812232	7384.469052	25.398106
173.179779	7401.279009	25.403123
173.570788	7410.840694	25.408141
173.819630	7406.963579	25.413159
173.387062	7418.037503	25.418176
173.663700	7413.878196	25.423194
173.917085	7426.495149	25.428211
173.795895	7444.385530	25.433229
174.040457	7448.224980	25.438247
174.116009	7465.763768	25.443264
174.242922	7470.689744	25.448282
174.850624	7490.279242	25.453299
174.466551	7501.690926	25.458317
174.899123	7506.110229	25.463335
175.300569	7534.314926	25.468352
175.476157	7539.314998	25.473370
176.017253	7540.486953	25.478387
175.807114	7556.574791	25.483405
175.912048	7556.665112	25.488423
175.996342	7579.415589	25.493440
176.276418	7590.970098	25.498458
176.516185	7592.240460	25.503475
176.590778	7610.003039	25.508493
176.376479	7618.860340	25.513511
176.342879	7635.683374	25.518528
176.777825	7662.353308	25.523546
177.149406	7668.146810	25.528563
177.347835	7695.140932	25.533581
177.917693	7705.650007	25.538599
178.099441	7717.318651	25.543616
178.263473	7718.917420	25.548634
178.437216	7741.483131	25.553651
178.758614	7739.652815	25.558669
178.659349	7741.542216	25.563687
178.932644	7757.228216	25.568704
179.177517	7760.612887	25.573722
179.322208	7764.448671	25.578739
179.345264	7779.096578	25.583757
179.825862	7784.596553	25.588775
180.017483	7800.995937	25.593792
179.935941	7796.947139	25.598810
180.024923	7792.913645	25.603827
180.305763	7823.010088	25.608845
180.412815	7828.510620	25.613863
180.713355	7834.912752	25.618880
180.828766	7830.206978	25.623898
181.236056	7843.435543	25.628915
180.735969	7869.414543	25.633933
181.380127	7870.727471	25.638951
181.435937	7870.199272	25.643968
181.245253	7887.557530	25.648986
181.556477	7899.922519	25.654003
181.438658	7918.848461	25.659021
181.910530	7926.508290	25.664039
182.248782	7937.296816	25.669056
182.324366	7947.413527	25.674074
182.932992	7952.125157	25.679092
182.532238	7971.551092	25.684109
182.724621	7984.340343	25.689127
182.954241	7994.850362	25.694144
182.984066	8002.933232	25.699162
183.329808	8019.604153	25.704180
183.225320	8036.785956	25.709197
183.711988	8050.338049	25.714215
183.954194	8060.236271	25.719232
184.262042	8076.496641	25.724250
185.457721	8076.439032	25.729268
185.215213	8077.566393	25.734285
185.559601	8080.303401	25.739303
185.786046	8077.173295	25.744320
185.453974	8076.193093	25.749338
185.646054	8074.683160	25.754356
186.145353	8094.951332	25.759373
185.978378	8107.138963	25.764391
185.973003	8105.804114	25.769408
186.419004	8110.852152	25.774426
186.637981	8123.961482	25.779444
186.593230	8144.143345	25.784461
186.630069	8147.754061	25.789479
186.517929	8156.836573	25.794496
186.722591	8176.871305	25.799514
186.949603	8187.651781	25.804532
187.235077	8210.751608	25.809549
187.460983	8217.057213	25.814567
187.630790	8241.916534	25.819584
187.391904	8258.467288	25.824602
188.270755	8263.533714	25.829620
188.211139	8289.010420	25.834637
188.458148	8292.874488	25.839655
188.425727	8316.522088	25.844672
188.670867	8323.220482	25.849690
188.942357	8346.596983	25.854708
188.840332	8364.961089	25.859725
189.203729	8384.438453	25.864743
189.235198	8399.877251	25.869760
189.522551	8400.450770	25.874778
190.660287	8405.817095	25.879796
190.825627	8411.610721	25.884813
191.275149	8399.044226	25.889831
191.374114	8402.045871	25.894848
191.276839	8402.135387	25.899866
191.670156	8397.209256	25.904884
191.668129	8403.105499	25.909901
191.810933	8408.592677	25.914919
192.123661	8407.643031	25.919936
191.960782	8438.224189	25.924954
192.062185	8433.839943	25.929972
192.117199	8436.985131	25.934989
192.540321	8434.893001	25.940007
192.755988	8445.652653	25.945024
192.628330	8461.013013	25.950042
192.869332	8456.765066	25.955060
192.545645	8471.354438	25.960077
192.897632	8488.446671	25.965095
193.004466	8500.445389	25.970112
193.003746	8526.511555	25.975130
193.417056	8539.290847	25.980148
193.513521	8559.617581	25.985165
193.796268	8572.105312	25.990183
194.354771	8585.165245	25.995200
194.752642	8589.349614	26.000218
195.308571	8595.239604	26.005236
195.140900	8615.847747	26.010253
195.276260	8626.466490	26.015271
195.589834	8621.787501	26.020288
195.859235	8643.429651	26.025306
196.041616	8643.101584	26.030324
196.115686	8655.525470	26.035341
196.060499	8658.289700	26.040359
196.552698	8675.841388	26.045376
196.204038	8688.876852	26.050394
196.692068	8691.826365	26.055412
196.889671	8718.889750	26.060429
197.057219	8716.428737	26.065447
197.455958	8731.615348	26.070464
197.283184	8752.569165	26.075482
197.500912	8765.139821	26.080500
197.794794	8786.612234	26.085517
197.772454	8793.753636	26.090535
198.271310	8809.842314	26.095552
198.063123	8824.151566	26.100570
198.566570	8836.978518	26.105588
198.641639	8855.274070	26.110605
198.660626	8869.939825	26.115623
199.157623	8875.315229	26.120640
199.506206	8900.054284	26.125658
199.681075	8904.964434	26.130676
199.831830	8919.337345	26.135693
199.996978	8926.670048	26.140711
200.385142	8946.818991	26.145728
200.612932	8963.842646	26.150746
200.625120	8958.045761	26.155764
200.676821	8980.984954	26.160781
200.884672	8985.147793	26.165799
201.316031	8993.999760	26.170816
201.178208	9014.905088	26.175834
201.396991	9017.273158	26.180852
201.519803	9025.994520	26.185869
201.335228	9045.131226	26.190887
201.782097	9061.250498	26.195904
202.143636	9079.908681	26.200922
202.570125	9086.300719	26.205940
202.956920	9108.536278	26.210957
203.183083	9109.571681	26.215975
203.577390	9098.276449	26.220992
203.789500	9115.683656	26.226010
203.891573	9125.065085	26.231028
203.991490	9132.790349	26.236045
204.003119	9140.148418	26.241063
204.531244	9161.153173	26.246080
204.424358	9172.098552	26.251098
204.862048	9170.145259	26.256116
204.754670	9186.759091	26.261133
204.737326	9203.557685	26.266151
205.246834	9198.625364	26.271168
205.336347	9230.731166	26.276186
205.390908	9240.726586	26.281204
205.614214	9249.788544	26.286221
205.473714	9263.667979	26.291239
206.085087	9287.766124	26.296256
206.255708	9311.432106	26.301274
206.680901	9308.733577	26.306292
207.077368	9321.256926	26.311309
207.039850	9332.932278	26.316327
207.971640	9326.906800	26.321344
208.026154	9351.741488	26.326362
208.078873	9355.914604	26.331380
208.171478	9368.571033	26.336397
208.410885	9353.245914	26.341415
208.926923	9361.824906	26.346432
208.916497	9382.909142	26.351450
209.148591	9377.434708	26.356468
209.357100	9374.468915	26.361485
209.458113	9375.617544	26.366503
209.929277	9383.275882	26.371520
209.696975	9408.251610	26.376538
210.074934	9406.987742	26.381556
210.217189	9409.645085	26.386573
210.390015	9436.132548	26.391591
210.810724	9437.786595	26.396608
210.716354	9449.453002	26.401626
210.763547	9448.461030	26.406644
210.996927	9459.504648	26.411661
210.809013	9479.988928	26.416679
211.276691	9485.552591	26.421696
211.249575	9508.542143	26.426714
211.622521	9523.493649	26.431732
212.043179	9533.846417	26.436749
212.329956	9551.367747	26.441767
212.577354	9569.483240	26.446784
212.990671	9566.348220	26.451802
212.974772	9567.419099	26.456820
213.476819	9577.532276	26.461837
213.460469	9591.593684	26.466855
213.668066	9592.479804	26.471872
213.863342	9602.189398	26.476890
213.843534	9626.413110	26.481908
214.541705	9624.902221	26.486925
214.366008	9631.791850	26.491943
214.758893	9644.855116	26.496960
214.656779	9655.942527	26.501978
214.742397	9666.885906	26.506996
215.407367	9686.148873	26.512013
214.960674	9688.880088	26.517031
215.689280	9708.956112	26.522048
215.587560	9723.137100	26.527066
215.594387	9740.233852	26.532084
215.981483	9757.150773	26.537101
215.904527	9769.503648	26.542119
216.412777	9783.773572	26.547136
216.222376	9810.476603	26.552154
216.414962	9836.576396	26.557172
216.786819	9849.510586	26.562189
217.007869	9870.636121	26.567207
217.252942	9892.287494	26.572224
217.600699	9919.586452	26.577242
217.744342	9939.845756	26.582260
218.301065	9952.068248	26.587277
218.302737	9979.437440	26.592295
218.993560	9979.251010	26.597312
219.035303	10001.292641	26.602330
219.090884	10004.827627	26.607348
219.460391	10026.257494	26.612365
219.408554	10038.701024	26.617383
220.002902	10054.234371	26.622400
220.299924	10062.415840	26.627418
220.638276	10083.054713	26.632436
221.037287	10086.864719	26.637453
221.270911	10092.643391	26.642471
221.737787	10098.249124	26.647488
221.660155	10101.773890	26.652506
222.029272	10120.113430	26.657524
222.267220	10118.112771	26.662541
222.262670	10121.678620	26.667559
222.383968	10122.879163	26.672576
222.644229	10148.611807	26.677594
222.463534	10149.518939	26.682612
222.892809	10166.561421	26.687629
222.787280	10186.506631	26.692647
223.071036	10185.259294	26.697664
223.352821	10212.843965	26.702682
223.495638	10233.134488	26.707700
224.080473	10237.264732	26.712717
223.929407	10254.816547	26.717735
224.146024	10264.216630	26.722752
224.762907	10281.333612	26.727770
224.660715	10286.374168	26.732788
224.990407	10296.765971	26.737805
225.189354	10321.865310	26.742823
225.567002	10324.832754	26.747840
225.515549	10340.384355	26.752858
225.757282	10360.967788	26.757876
226.125619	10357.121243	26.762893
226.276997	10382.908635	26.767911
226.212824	10382.038242	26.772928
226.513905	10407.475989	26.777946
226.684265	10426.658602	26.782964
226.834560	10440.549819	26.787981
227.086267	10452.177964	26.792999
227.479428	10482.115065	26.798016
227.667850	10493.625441	26.803034
228.002300	10514.053625	26.808052
228.509199	10523.058159	26.813069
228.171745	10537.451816	26.818087
228.547125	10545.099265	26.823104
229.046519	10563.017593	26.828122
228.945110	10582.869014	26.833140
229.276457	10584.616143	26.838157
229.513181	10616.491692	26.843175
229.603993	10633.121563	26.848192
229.903780	10640.840138	26.853210
229.862974	10664.875651	26.858228
230.451422	10679.574771	26.863245
230.738933	10699.742118	26.868263
230.824888	10729.886089	26.873280
231.456768	10735.407127	26.878298
231.587000	10758.779999	26.883316
232.153696	10759.675451	26.888333
232.258262	10772.700664	26.893351
232.579674	10780.897132	26.898368
233.202118	10784.727187	26.903386
233.132227	10793.745130	26.908404
233.298717	10792.957177	26.913421
233.401177	10814.097825	26.918439
233.445417	10815.132840	26.923456
233.876787	10830.289229	26.928474
233.941817	10845.366301	26.933492
234.094950	10848.815889	26.938509
234.501818	10877.711529	26.943527
234.498406	10885.708378	26.948544
234.895491	10896.194922	26.953562
235.091553	10912.149180	26.958580
235.414875	10910.076569	26.963597
235.342902	10939.481530	26.968615
235.203029	10957.289342	26.973632
235.938183	10967.619729	26.978650
236.234540	10985.480812	26.983668
236.503916	11001.140537	26.988685
236.879873	11023.953234	26.993703
237.243017	11026.791696	26.998720
237.055789	11032.643330	27.003738
237.027174	11051.745516	27.008756
237.374551	11055.085876	27.013773
237.476351	11074.769784	27.018791
237.408352	11091.998051	27.023808
238.181913	11103.239317	27.028826
238.117235	11120.359261	27.033844
238.657882	11145.994605	27.038861
238.840872	11149.759438	27.043879
238.982328	11179.526727	27.048896
239.120419	11189.772212	27.053914
239.413462	11226.207323	27.058932
239.913866	11220.502925	27.063949
239.843863	11245.688388	27.068967
240.043487	11258.720117	27.073984
240.446035	11280.651006	27.079002
240.627102	11298.411993	27.084020
240.981022	11321.398263	27.089037
240.879028	11340.891086	27.094055
241.280248	11368.531437	27.099072
241.880806	11377.272060	27.104090
241.842217	11407.792396	27.109108
242.116043	11404.419515	27.114125
242.050222	11431.883950	27.119143
242.487975	11454.647307	27.124160
242.992897	11461.812372	27.129178
243.141585	11486.784120	27.134196
243.471396	11501.993187	27.139213
243.418394	11521.114019	27.144231
243.949535	11535.335723	27.149248
244.420296	11546.259212	27.154266
244.301382	11564.302680	27.159284
244.643188	11581.038797	27.164301
245.047963	11591.000412	27.169319
245.013263	11605.779115	27.174336
245.264213	11627.227995	27.179354
245.403616	11650.269820	27.184372
245.796910	11665.319780	27.189389
246.226537	11688.105643	27.194407
246.282068	11694.196670	27.199424
246.713340	11710.799821	27.204442
246.539596	11735.592567	27.209460
247.452339	11750.237893	27.214477
247.803686	11761.147123	27.219495
247.984831	11771.420377	27.224512
248.477070	11779.367613	27.229530
248.634065	11790.532951	27.234548
248.892129	11787.672920	27.239565
248.935636	11800.905129	27.244583
249.158583	11822.939420	27.249600
249.523732	11828.947105	27.254618
249.210573	11839.686052	27.259636
249.581974	11859.613125	27.264653
249.793544	11874.265466	27.269671
250.050853	11891.016970	27.274688
250.086946	11913.021557	27.279706
250.169778	11930.686588	27.284724
250.890296	11933.776600	27.289741
250.946141	11954.168698	27.294759
250.840398	11980.562766	27.299776
251.655437	11984.481681	27.304794
251.628026	12009.142534	27.309812
252.062081	12019.093862	27.314829
252.243840	12033.370746	27.319847
252.125957	12053.536439	27.324864
252.545307	12078.383175	27.329882
252.634868	12099.397409	27.334900
252.896666	12111.820195	27.339917
253.393230	12132.940790	27.344935
253.469129	12146.340905	27.349952
253.907044	12162.764429	27.354970
253.869831	12186.273439	27.359988
254.114706	12208.335886	27.365005
254.452581	12234.760823	27.370023
254.710503	12256.755144	27.375040
255.231618	12273.929019	27.380058
255.182829	12290.353521	27.385076
255.703795	12317.605594	27.390093
255.996067	12333.108972	27.395111
255.759808	12357.809782	27.400128
256.527193	12366.265825	27.405146
256.505477	12394.608895	27.410164
257.037534	12418.606639	27.415181
257.367251	12436.475138	27.420199
257.417935	12459.767287	27.425216
257.860394	12479.175962	27.430234
257.803567	12494.236318	27.435252
258.181638	12516.406674	27.440269
258.431484	12528.488522	27.445287
258.574464	12560.907723	27.450304
259.050643	12576.014646	27.455322
259.189560	12597.356228	27.460340
259.393011	12626.797295	27.465357
260.285753	12634.950340	27.470375
260.850423	12636.643404	27.475392
261.203305	12651.439071	27.480410
261.109795	12666.675857	27.485428
261.424227	12669.553689	27.490445
261.579115	12676.548440	27.495463
261.485486	12691.965129	27.500480
262.113570	12694.847478	27.505498
262.059423	12715.694199	27.510516
262.468941	12728.403679	27.515533
262.843721	12743.269935	27.520551
262.443304	12763.052026	27.525568
263.142333	12790.187029	27.530586
263.225383	12803.843188	27.535604
263.072463	12821.678088	27.540621
263.450293	12843.006333	27.545639
263.529960	12877.792592	27.550656
263.922315	12896.814448	27.555674
264.153457	12911.399142	27.560692
264.379240	12939.028014	27.565709
264.665825	12957.023254	27.570727
264.835222	12976.515645	27.575744
265.416342	12997.638531	27.580762
266.094354	13004.931222	27.585780
266.693225	13022.560822	27.590797
267.713561	13012.300529	27.595815
268.054963	13018.663247	27.600832
268.389369	13012.233421	27.605850
268.422116	13017.155962	27.610868
268.412321	13013.893469	27.615885
268.847395	13013.768763	27.620903
268.508455	13024.100972	27.625920
268.888447	13016.322976	27.630938
268.877129	13032.604260	27.635956
268.987444	13046.817329	27.640973
269.400955	13052.279289	27.645991
269.241686	13082.186699	27.651008
269.507725	13085.772888	27.656026
269.775409	13113.955259	27.661044
269.721534	13138.079320	27.666061
270.191917	13148.488154	27.671079
270.091951	13182.116027	27.676096
269.924251	13205.096893	27.681114
270.427002	13235.413188	27.686132
270.582070	13268.008881	27.691149
271.247863	13292.625371	27.696167
271.448731	13327.242792	27.701184
271.551501	13340.579556	27.706202
271.758534	13375.706086	27.711220
272.158977	13404.675684	27.716237
272.894338	13428.557311	27.721255
272.974970	13454.505450	27.726272
273.662934	13480.024543	27.731290
274.276141	13504.306652	27.736308
274.945322	13512.736590	27.741325
274.953242	13517.108885	27.746343
274.893733	13549.767327	27.751360
275.279188	13553.439680	27.756378
275.549932	13564.693082	27.761396
275.787709	13582.800159	27.766413
276.215245	13601.521018	27.771431
276.418843	13614.777500	27.776448
276.692027	13616.179052	27.781466
277.056871	13638.775376	27.786484
277.449760	13654.590155	27.791501
277.731050	13665.878063	27.796519
277.567392	13687.645081	27.801536
277.887035	13699.927307	27.806554
278.181825	13705.538510	27.811572
278.505391	13732.810812	27.816589
278.626259	13747.055323	27.821607
278.671744	13765.928693	27.826624
279.036626	13779.855774	27.831642
279.059391	13793.751303	27.836660
279.016436	13816.102248	27.841677
279.332065	13845.553374	27.846695
279.610601	13865.946482	27.851712
279.581919	13888.835466	27.856730
280.014883	13909.203230	27.861748
280.133792	13951.044911	27.866765
280.353978	13981.043161	27.871783
280.568737	14014.339307	27.876800
281.307136	14036.155016	27.881818
281.702838	14064.965716	27.886836
281.962367	14099.388970	27.891853
282.305508	14115.488267	27.896871
282.592218	14145.670674	27.901888
282.878152	14168.411627	27.906906
283.416405	14185.653423	27.911924
283.764253	14203.245686	27.916941
284.457676	14224.276978	27.921959
284.392741	14242.988167	27.926976
284.771347	14274.320363	27.931994
285.251709	14285.701969	27.937012
285.029494	14316.138132	27.942029
285.530086	14322.728032	27.947047
285.759213	14351.508356	27.952064
285.924872	14366.858342	27.957082
286.636562	14386.089663	27.962100
286.666987	14399.463974	27.967117
287.310942	14409.271439	27.972135
287.524804	14435.325469	27.977152
287.617667	14457.535354	27.982170
287.956329	14468.130323	27.987188
288.059400	14484.727716	27.992205
288.314121	14504.290625	27.997223
288.462102	14531.652758	28.002240
288.582858	14555.933066	28.007258
289.207067	14571.045540	28.012276
289.533383	14599.121722	28.017293
289.622030	14626.490234	28.022311
289.922825	14653.830393	28.027328
290.289643	14677.190272	28.032346
290.464493	14697.094826	28.037364
290.300740	14727.604258	28.042381
290.987462	14745.295560	28.047399
291.210572	14780.746011	28.052416
291.553535	14804.542866	28.057434
292.035776	14830.356898	28.062452
292.183832	14852.686879	28.067469
292.462777	14881.123318	28.072487
292.507750	14902.014192	28.077504
293.098329	14912.692816	28.082522
293.647191	14941.018544	28.087540
293.305604	14972.506419	28.092557
293.932440	14986.136209	28.097575
294.211057	15015.076491	28.102592
294.447198	15035.717632	28.107610
295.321753	15054.555111	28.112628
295.432115	15071.197931	28.117645
295.994835	15083.467425	28.122663
296.069764	15103.305377	28.127680
296.075528	15118.335506	28.132698
296.631823	15134.187770	28.137716
296.749937	15162.484944	28.142733
297.259772	15173.614138	28.147751
297.919719	15176.513649	28.152768
298.495630	15182.360659	28.157786
298.747623	15183.922402	28.162804
299.265293	15211.515157	28.167821
299.302838	15217.801860	28.172839
299.684217	15219.140758	28.177856
299.846518	15224.828158	28.182874
300.116228	15232.801369	28.187892
299.972370	15247.928884	28.192909
300.415977	15260.897994	28.197927
300.375270	15287.225794	28.202944
300.342815	15307.207481	28.207962
300.651852	15336.878726	28.212980
300.701757	15367.541265	28.217997
301.241891	15390.668837	28.223015
301.543175	15417.311973	28.228032
301.923783	15433.375590	28.233050
302.149788	15454.617628	28.238068
302.252719	15486.223171	28.243085
302.686372	15506.898120	28.248103
303.087115	15533.101856	28.253120
303.155086	15568.415885	28.258138
303.473275	15589.157175	28.263156
303.866046	15628.674216	28.268173
304.057231	15650.953312	28.273191
304.162279	15683.049593	28.278208
304.387445	15715.421830	28.283226
305.120314	15747.058195	28.288244
305.234235	15781.722177	28.293261
305.690915	15798.313737	28.298279
306.119279	15827.018720	28.303296
306.263066	15857.076605	28.308314
306.751764	15887.971775	28.313332
307.020997	15911.468952	28.318349
307.331909	15940.788848	28.323367
307.812731	15972.539855	28.328384
307.896631	15998.502598	28.333402
308.808902	16013.294446	28.338420
308.763550	16031.878818	28.343437
309.230605	16047.547459	28.348455
309.557473	16078.564265	28.353472
309.610450	16093.496099	28.358490
310.011133	16127.214676	28.363508
310.235503	16152.188874	28.368525
310.802137	16156.164248	28.373543
311.092574	16178.339519	28.378560
311.085930	16198.625196	28.383578
311.436655	16209.511738	28.388596
312.059422	16240.526783	28.393613
312.025357	16259.250754	28.398631
312.753130	16266.652834	28.403648
312.765275	16295.418532	28.408666
313.106350	16311.081147	28.413684
313.187459	16333.890134	28.418701
313.909415	16356.274217	28.423719
314.083438	16378.715351	28.428736
313.953067	16404.177551	28.433754
314.690897	16420.991285	28.438772
314.772277	16450.781562	28.443789
314.946856	16479.773264	28.448807
315.478561	16502.215832	28.453824
315.522456	16525.986844	28.458842
315.677758	16562.016912	28.463860
315.837947	16602.959213	28.468877
316.445521	16618.844012	28.473895
316.886652	16647.970301	28.478912
317.051701	16681.552464	28.483930
317.671533	16696.117789	28.488948
317.579715	16734.600426	28.493965
318.127330	16755.125241	28.498983
318.950638	16777.953983	28.504000
319.213055	16790.879650	28.509018
319.706704	16818.046473	28.514036
319.814883	16841.726235	28.519053
320.423085	16859.152009	28.524071
320.728961	16873.982287	28.529088
320.937070	16902.685404	28.534106
321.324675	16904.541637	28.539124
321.537579	16929.675798	28.544141
321.785484	16952.281370	28.549159
322.186026	16982.578655	28.554176
322.448199	17006.970494	28.559194
322.870369	17009.428277	28.564212
322.955786	17041.734629	28.569229
323.566380	17064.179812	28.574247
324.086199	17083.747745	28.579264
324.112915	17097.832031	28.584282
324.561634	17111.805768	28.589300
324.549510	17144.090873	28.594317
324.845911	17163.437442	28.599335
325.301696	17186.417487	28.604352
325.477545	17206.117556	28.609370
325.688796	17225.146689	28.614388
325.790487	17252.506659	28.619405
326.006375	17281.753896	28.624423
326.326284	17307.368246	28.629440
326.882343	17345.952679	28.634458
327.092290	17371.887009	28.639476
327.206313	17405.199751	28.644493
327.322673	17432.508884	28.649511
328.089492	17464.643742	28.654528
328.410368	17491.265685	28.659546
328.583572	17514.980205	28.664564
329.226706	17536.206166	28.669581
330.919954	17539.401589	28.674599
331.682574	17547.135346	28.679616
331.562299	17564.668175	28.684634
331.890516	17558.007056	28.689652
331.806149	17554.394276	28.694669
331.840827	17565.040030	28.699687
332.692839	17570.379705	28.704704
332.493847	17592.618669	28.709722
332.922425	17592.807484	28.714740
333.063260	17619.996515	28.719757
333.157552	17641.331351	28.724775
333.227478	17652.773890	28.729792
333.245206	17690.335556	28.734810
333.975098	17703.331182	28.739828
334.092164	17732.043849	28.744845
334.263335	17756.388185	28.749863
334.882759	17781.551656	28.754880
334.838297	17817.255461	28.759898
335.279189	17850.538325	28.764916
335.435485	17878.943047	28.769933
335.623399	17916.110029	28.774951
336.091748	17948.447003	28.779968
336.178176	17990.324008	28.784986
336.529697	18018.589998	28.790004
337.019802	18051.230805	28.795021
337.182950	18095.127756	28.800039
338.090390	18133.570750	28.805056
338.211189	18164.026542	28.810074
338.668853	18191.625532	28.815092
338.870076	18219.722926	28.820109
339.532010	18263.051878	28.825127
340.148683	18272.714014	28.830144
339.981393	18298.642294	28.835162
340.474748	18315.291547	28.840180
341.196559	18349.218912	28.845197
341.161816	18382.513361	28.850215
341.801661	18397.732241	28.855232
341.788532	18424.148771	28.860250
342.269763	18451.786595	28.865268
342.834174	18491.376117	28.870285
343.106322	18520.433250	28.875303
343.553773	18540.127556	28.880320
343.862203	18569.651848	28.885338
344.224883	18593.361835	28.890356
344.479695	18620.355309	28.895373
344.585106	18647.033651	28.900391
345.268567	18681.199751	28.905408
345.556532	18699.851916	28.910426
345.756946	18720.568931	28.915444
346.422608	18739.824760	28.920461
346.580952	18768.846161	28.925479
347.342969	18786.260623	28.930496
347.340825	18808.352619	28.935514
347.555551	18832.029065	28.940532
347.630520	18844.467789	28.945549
348.058458	18866.646848	28.950567
348.711612	18893.785594	28.955584
348.955590	18915.032175	28.960602
349.345676	18941.592815	28.965620
349.612190	18957.032380	28.970637
349.749744	18990.456582	28.975655
350.005608	19015.874495	28.980672
350.017154	19044.329214	28.985690
350.598669	19075.304741	28.990708
351.226914	19105.707491	28.995725
350.882729	19137.218092	29.000743
351.418022	19165.543893	29.005760
351.741008	19205.078028	29.010778
352.285759	19241.255406	29.015796
352.694914	19264.813328	29.020813
352.944987	19301.478393	29.025831
354.043721	19326.234494	29.030848
353.820659	19365.182376	29.035866
354.317858	19383.482303	29.040884
355.002197	19412.701808	29.045901
355.181435	19438.422803	29.050919
355.663256	19455.388138	29.055936
355.689855	19484.447613	29.060954
356.159824	19514.446028	29.065972
356.686884	19541.727664	29.070989
356.938642	19564.762644	29.076007
357.166192	19597.372542	29.081024
357.559146	19628.252434	29.086042
357.860355	19653.987026	29.091060
358.025392	19681.516381	29.096077
358.321834	19724.332781	29.101095
358.586405	19753.834016	29.106112
358.826798	19791.631423	29.111130
359.409754	19824.182794	29.116148
359.877341	19855.347731	29.121165
360.300121	19901.424389	29.126183
360.851834	19920.950659	29.131200
360.831483	19960.775303	29.136218
361.487930	19999.042801	29.141236
361.895892	20015.828367	29.146253
362.144826	20053.016699	29.151271
363.008769	20078.781620	29.156288
362.945090	20101.701495	29.161306
363.228434	20132.346666	29.166324
363.875596	20169.915180	29.171341
363.701459	20192.622444	29.176359
364.513734	20222.759428	29.181376
364.731540	20251.672120	29.186394
364.915876	20283.243728	29.191412
365.309986	20312.410367	29.196429
365.786191	20357.659655	29.201447
366.144799	20372.850870	29.206464
366.483767	20404.248057	29.211482
367.049493	20429.690946	29.216500
367.180006	20454.101487	29.221517
367.699645	20481.608027	29.226535
368.121875	20510.076744	29.231552
368.357678	20544.999867	29.236570
368.439248	20568.404836	29.241588
368.964152	20591.638389	29.246605
369.275152	20629.690386	29.251623
369.654782	20662.334573	29.256640
369.809317	20692.246513	29.261658
370.467864	20718.779204	29.266676
370.597705	20747.910800	29.271693
370.672236	20794.305462	29.276711
371.238211	20816.934274	29.281728
371.712211	20855.701919	29.286746
371.847715	20887.345920	29.291764
372.372169	20923.605239	29.296781
373.026372	20975.224000	29.301799
373.388692	21009.467240	29.306816
373.514134	21046.501585	29.311834
374.193005	21078.004253	29.316852
374.766055	21099.796751	29.321869
374.671296	21134.065058	29.326887
375.091861	21165.092425	29.331904
375.895056	21199.239834	29.336922
375.949342	21244.277357	29.341940
376.335735	21263.008644	29.346957
376.849448	21304.481073	29.351975
376.888965	21327.533954	29.356992
377.599790	21362.406035	29.362010
377.915400	21402.131961	29.367028
378.635340	21431.829196	29.372045
378.636305	21473.861046	29.377063
378.796007	21499.660987	29.382080
379.123736	21527.192064	29.387098
379.564419	21577.052725	29.392116
380.221332	21617.229643	29.397133
380.501536	21656.390067	29.402151
381.006766	21684.863437	29.407168
381.196455	21728.081920	29.412186
381.668664	21752.369140	29.417204
382.485867	21790.003039	29.422221
382.418777	21834.100725	29.427239
382.964414	21860.514723	29.432256
383.408195	21889.683461	29.437274
383.549991	21920.440912	29.442292
384.311453	21942.729883	29.447309
384.367381	21979.124576	29.452327
384.837764	22004.964834	29.457344
385.166125	22047.583995	29.462362
385.444668	22084.349858	29.467380
386.385543	22105.937858	29.472397
386.693745	22139.670783	29.477415
387.096122	22166.276669	29.482432
387.473999	22190.570145	29.487450
388.098123	22196.688908	29.492468
388.902438	22214.476549	29.497485
388.937081	22228.901676	29.502503
389.507436	22246.251704	29.507520
389.824325	22268.067739	29.512538
389.927070	22300.082094	29.517556
390.664770	22305.438506	29.522573
390.605997	22341.860187	29.527591
390.694989	22356.509115	29.532608
391.019521	22387.699901	29.537626
391.016948	22417.843353	29.542644
391.506031	22452.360159	29.547661
392.124322	22480.902803	29.552679
392.852574	22510.451889	29.557696
393.375439	22536.931297	29.562714
393.501174	22562.463503	29.567732
394.402007	22567.167849	29.572749
395.162703	22594.411262	29.577767
395.490721	22611.710519	29.582784
395.980678	22636.302662	29.587802
396.296912	22650.508449	29.592820
396.512672	22672.749938	29.597837
396.441676	22693.179910	29.602855
396.649727	22727.101752	29.607872
397.085224	22754.106621	29.612890
397.253027	22788.621010	29.617908
397.635508	22820.773787	29.622925
397.801926	22857.389184	29.627943
398.258811	22903.757467	29.632960
398.756158	22940.586548	29.637978
398.600080	22976.538423	29.642996
399.120679	23010.183437	29.648013
399.553366	23056.247263	29.653031
399.898747	23099.021710	29.658048
400.115017	23135.290325	29.663066
400.699707	23190.158372	29.668084
401.139888	23231.039503	29.673101
401.315972	23272.737882	29.678119
401.382242	23323.059111	29.683136
402.296151	23363.498834	29.688154
402.668491	23428.296224	29.693172
403.055892	23456.719885	29.698189
403.759230	23506.859054	29.703207
404.224886	23543.669379	29.708224
404.447266	23585.484078	29.713242
404.903962	23638.339494	29.718260
405.643136	23653.919458	29.723277
405.903600	23686.103670	29.728295
406.148728	23724.270498	29.733312
406.785079	23767.465903	29.738330
407.077154	23804.760562	29.743348
407.464406	23842.057472	29.748365
407.685258	23888.661586	29.753383
408.387077	23926.352042	29.758400
408.656954	23951.679191	29.763418
408.783391	23999.593647	29.768436
409.504707	24028.706350	29.773453
409.812977	24072.286481	29.778471
410.181027	24114.039183	29.783488
410.640669	24132.882721	29.788506
410.857951	24176.276769	29.793524
411.295890	24207.052904	29.798541
411.670448	24247.580819	29.803559
412.249924	24285.781577	29.808576
412.918241	24317.570452	29.813594
412.864141	24364.159898	29.818612
413.490102	24398.497646	29.823629
414.469245	24424.668826	29.828647
415.654718	24451.320769	29.833664
416.085257	24455.738280	29.838682
416.441383	24481.687434	29.843700
417.226477	24498.054152	29.848717
417.151485	24527.606589	29.853735
417.263363	24546.439861	29.858752
417.813912	24571.805199	29.863770
417.922315	24600.218642	29.868788
418.712712	24622.123164	29.873805
418.526970	24659.230490	29.878823
418.672826	24691.915510	29.883840
419.268250	24717.711123	29.888858
419.906838	24758.237654	29.893876
420.246551	24794.896849	29.898893
420.590154	24834.291330	29.903911
421.137316	24867.894293	29.908928
421.673779	24892.439197	29.913946
421.738069	24935.922705	29.918964
422.100445	24973.383774	29.923981
422.435629	25003.972218	29.928999
422.531198	25040.126541	29.934016
423.000732	25082.264996	29.939034
423.088772	25129.212143	29.944052
423.892692	25170.739822	29.949069
424.087744	25213.954319	29.954087
424.446295	25271.398997	29.959104
424.905383	25308.419261	29.964122
425.194730	25359.159598	29.969140
426.025762	25402.775079	29.974157
426.917649	25441.104499	29.979175
427.267300	25479.379395	29.984192
427.390989	25514.232059	29.989210
428.122609	25553.783125	29.994228
428.918920	25578.535831	29.999245
429.310112	25607.503137	30.004263
429.617969	25659.802065	30.009280
430.125402	25688.938491	30.014298
430.187882	25727.159685	30.019316
430.609049	25761.261997	30.024333
431.198821	25792.625954	30.029351
431.111111	25843.288460	30.034368
432.244327	25859.974530	30.039386
432.309019	25894.846873	30.044404
432.709337	25924.181197	30.049421
433.419336	25967.567772	30.054439
433.339367	25999.718711	30.059456
434.035351	26028.592524	30.064474
434.035896	26072.513103	30.069492
434.316584	26119.764115	30.074509
435.061059	26157.159194	30.079527
435.606772	26192.437679	30.084544
435.805528	26226.988440	30.089562
436.077321	26267.998712	30.094580
436.444778	26316.318928	30.099597
437.017561	26359.905683	30.104615
437.239261	26410.861013	30.109632
437.736777	26458.153315	30.114650
437.992567	26504.307263	30.119668
438.403885	26555.221020	30.124685
438.962304	26608.257543	30.129703
439.105540	26667.143847	30.134720
439.800866	26705.078242	30.139738
439.886637	26762.884480	30.144756
440.635662	26813.163038	30.149773
441.303748	26862.178348	30.154791
441.400710	26919.673744	30.159808
441.905104	26970.749673	30.164826
442.716727	27006.340532	30.169844
443.648507	27053.450366	30.174861
444.121508	27091.075228	30.179879
444.324672	27133.148840	30.184896
445.400069	27174.123987	30.189914
445.555158	27218.764433	30.194932
446.314245	27243.985754	30.199949
446.699350	27285.959870	30.204967
447.136400	27325.674108	30.209984
447.560525	27352.917047	30.215002
447.756675	27391.447064	30.220020
448.314131	27434.293848	30.225037
448.964695	27472.315181	30.230055
449.207395	27509.982439	30.235072
449.771231	27545.022276	30.240090
449.738739	27592.150226	30.245108
450.174609	27621.339373	30.250125
450.736276	27672.617974	30.255143
450.842127	27724.059177	30.260160
451.431962	27756.708050	30.265178
452.171972	27802.873654	30.270196
452.556036	27845.219694	30.275213
453.458588	27880.007746	30.280231
453.290533	27932.788539	30.285248
453.888663	27968.915850	30.290266
454.705361	27996.934073	30.295284
455.102102	28036.732118	30.300301
455.808668	28062.087577	30.305319
456.143781	28091.690727	30.310336
456.809584	28126.413027	30.315354
457.080711	28156.790754	30.320372
457.602790	28175.622012	30.325389
458.272000	28198.411920	30.330407
458.874968	28230.943051	30.335424
459.112347	28249.575503	30.340442
459.418001	28280.053540	30.345460
459.513592	28312.528573	30.350477
460.142092	28337.211420	30.355495
460.229409	28370.508890	30.360512
460.841681	28410.536680	30.365530
461.304196	28454.903059	30.370548
461.552733	28496.095244	30.375565
462.482017	28523.154094	30.380583
462.448307	28559.797833	30.385600
462.932498	28601.540532	30.390618
463.258761	28640.883263	30.395636
463.524841	28693.728158	30.400653
463.817787	28722.515005	30.405671
464.345465	28783.462560	30.410688
464.744493	28841.420924	30.415706
465.618636	28889.174070	30.420724
465.652445	28940.662121	30.425741
466.466167	28991.802308	30.430759
466.979429	29040.081429	30.435776
467.112241	29076.595792	30.440794
467.917945	29125.101205	30.445812
468.201606	29173.521310	30.450829
468.900195	29220.323186	30.455847
468.997863	29278.026966	30.460864
469.383351	29322.614430	30.465882
470.062703	29377.609869	30.470900
470.185009	29427.580352	30.475917
470.720551	29487.753934	30.480935
470.895242	29548.993827	30.485952
471.248958	29600.418811	30.490970
471.866086	29662.152832	30.495988
472.228948	29722.537600	30.501005
472.819575	29778.804564	30.506023
473.128594	29848.015881	30.511040
474.162004	29893.171469	30.516058
474.919802	29936.024462	30.521076
475.346708	29993.728749	30.526093
476.430552	30026.008781	30.531111
476.939879	30077.847026	30.536128
477.692925	30115.591888	30.541146
477.914759	30152.901385	30.546164
478.261064	30198.320154	30.551181
479.161839	30222.516485	30.556199
479.214227	30269.296662	30.561216
479.830177	30321.161246	30.566234
480.673032	30346.802738	30.571252
480.649597	30383.907552	30.576269
481.364998	30431.242921	30.581287
481.748678	30468.763759	30.586304
482.052506	30490.995719	30.591322
482.222684	30527.037714	30.596340
482.746478	30575.493064	30.601357
483.453790	30604.887039	30.606375
483.314216	30653.315912	30.611392
483.939720	30694.436256	30.616410
484.648449	30738.344094	30.621428
484.994102	30788.481734	30.626445
485.429633	30824.538848	30.631463
485.897499	30878.822829	30.636480
486.175443	30926.106386	30.641498
486.824807	30974.263948	30.646516
487.285269	31021.274411	30.651533
487.890963	31064.690464	30.656551
488.066098	31120.367854	30.661568
488.441824	31175.521735	30.666586
489.228369	31227.368316	30.671604
489.253200	31286.312252	30.676621
489.787497	31334.317405	30.681639
490.476552	31392.051052	30.686656
490.712940	31450.514256	30.691674
491.279575	31514.285470	30.696692
491.576162	31575.275518	30.701709
491.961695	31629.772112	30.706727
492.291361	31688.747733	30.711744
492.859713	31751.780381	30.716762
493.610221	31807.701005	30.721780
494.368249	31871.353272	30.726797
495.166947	31925.195541	30.731815
495.646453	31973.001657	30.736832
496.100710	32027.616290	30.741850
496.874636	32073.370898	30.746868
497.660226	32121.194884	30.751885
498.078867	32163.795650	30.756903
498.469797	32215.697338	30.761920
499.065621	32267.369524	30.766938
499.882516	32320.820867	30.771956
500.120532	32346.010175	30.776973
501.103325	32384.321049	30.781991
501.512222	32436.769092	30.787008
501.817596	32472.152290	30.792026
502.379640	32506.571010	30.797044
502.638992	32567.282210	30.802061
503.442638	32605.073608	30.807079
503.665873	32645.268314	30.812096
504.428495	32682.935599	30.817114
505.391365	32708.311054	30.822132
505.592422	32760.526849	30.827149
506.272909	32792.523522	30.832167
506.800957	32831.607733	30.837184
506.895800	32863.431448	30.842202
507.558796	32900.968509	30.847220
507.759205	32956.640189	30.852237
508.532294	32995.138789	30.857255
508.894985	33027.585338	30.862272
509.109614	33069.115971	30.867290
509.448009	33095.204672	30.872308
510.055322	33146.201556	30.877325
510.599866	33186.221867	30.882343
510.905982	33227.916446	30.887360
511.418926	33259.693236	30.892378
512.120234	33301.514203	30.897396
512.492719	33359.229505	30.902413
512.834794	33402.577068	30.907431
513.309476	33458.414815	30.912448
513.893804	33509.727014	30.917466
514.315694	33546.872038	30.922484
514.792044	33597.725660	30.927501
515.252439	33653.017777	30.932519
515.591100	33708.952123	30.937536
516.088217	33756.721185	30.942554
516.770474	33796.607538	30.947572
517.111556	33861.831420	30.952589
517.788904	33920.267794	30.957607
518.820065	33968.773679	30.962624
519.209041	34027.440800	30.967642
519.814197	34064.508923	30.972660
520.284956	34115.847392	30.977677
520.732205	34167.651644	30.982695
520.852224	34219.330051	30.987712
521.329854	34273.834872	30.992730
521.884396	34322.838611	30.997748
522.096844	34389.302028	31.002765
522.485308	34443.826338	31.007783
523.315912	34503.266589	31.012800
523.317798	34576.645335	31.017818
524.178778	34628.315755	31.022836
524.876039	34699.202297	31.027853
525.135401	34758.127525	31.032871
525.752745	34826.121964	31.037888
526.475599	34884.768872	31.042906
527.169865	34944.175662	31.047924
527.554988	35003.789553	31.052941
528.598019	35052.323512	31.057959
529.463694	35097.551632	31.062976
529.486562	35164.434568	31.067994
530.578924	35199.319867	31.073012
530.750592	35256.037987	31.078029
531.465211	35305.000197	31.083047
531.869029	35349.263662	31.088064
532.466978	35401.047742	31.093082
533.113347	35444.244948	31.098100
533.788023	35508.097871	31.103117
534.008307	35563.339983	31.108135
534.595019	35608.106286	31.113152
534.819840	35650.925018	31.118170
535.387633	35711.407799	31.123188
535.865835	35756.497629	31.128205
536.632449	35811.858488	31.133223
537.202572	35860.804353	31.138240
537.435703	35915.716084	31.143258
538.191517	35959.076914	31.148276
538.575288	36010.305788	31.153293
538.653594	36055.507417	31.158311
539.593322	36099.067916	31.163328
539.845238	36178.581369	31.168346
540.313665	36223.085951	31.173364
540.770269	36278.720029	31.178381
541.329013	36334.448384	31.183399
541.864576	36393.223434	31.188416
541.958967	36460.943621	31.193434
542.777610	36523.900895	31.198452
543.181162	36587.750665	31.203469
543.661143	36656.103927	31.208487
544.566658	36715.161726	31.213504
544.921532	36781.209909	31.218522
545.785616	36838.275578	31.223540
546.021999	36914.200261	31.228557
546.647898	36971.247560	31.233575
547.083851	37030.445901	31.238592
547.492540	37093.937296	31.243610
548.197919	37160.751000	31.248628
548.568736	37230.423150	31.253645
549.035334	37295.025513	31.258663
549.655946	37361.959153	31.263680
550.161085	37438.507171	31.268698
550.719567	37505.187969	31.273716
551.541820	37576.956024	31.278733
552.041817	37642.181922	31.283751
552.951723	37705.170073	31.288768
553.540931	37770.355454	31.293786
554.329718	37820.670746	31.298804
555.167878	37875.161385	31.303821
555.853856	37934.417677	31.308839
556.313907	37988.623602	31.313856
556.671476	38040.771027	31.318874
557.503574	38090.897324	31.323892
557.912985	38160.754797	31.328909
558.510000	38207.979813	31.333927
559.227132	38254.613463	31.338944
559.430188	38321.229527	31.343962
559.820990	38368.697546	31.348980
560.523834	38435.141424	31.353997
560.966309	38492.557357	31.359015
561.620711	38549.110337	31.364032
561.686239	38610.000458	31.369050
562.537514	38670.611123	31.374068
562.949005	38744.748536	31.379085
563.495266	38812.760953	31.384103
564.372116	38866.726698	31.389120
564.819484	38935.879633	31.394138
565.574255	38989.715415	31.399156
566.120058	39061.524337	31.404173
566.434862	39126.063254	31.409191
566.933948	39170.551801	31.414208
567.378119	39238.392960	31.419226
567.831026	39294.234664	31.424244
568.328998	39361.397579	31.429261
568.571123	39420.059589	31.434279
569.346270	39488.104482	31.439296
569.781562	39558.922325	31.444314
570.185101	39622.316786	31.449332
570.555328	39698.546423	31.454349
571.000424	39768.092594	31.459367
572.072605	39840.276690	31.464384
572.351764	39918.738951	31.469402
572.990832	39997.385521	31.474420
573.578999	40067.386356	31.479437
573.924684	40144.408782	31.484455
574.806635	40214.210466	31.489472
574.901993	40291.011648	31.494490
575.583784	40364.805554	31.499508
576.534335	40442.379540	31.504525
577.226798	40527.788388	31.509543
577.794129	40592.363594	31.514560
578.259730	40667.293970	31.519578
578.910773	40735.250059	31.524596
580.037037	40811.375287	31.529613
580.525623	40888.520232	31.534631
581.659842	40935.334512	31.539648
582.059926	41003.410486	31.544666
582.718214	41049.313664	31.549684
583.496304	41119.824747	31.554701
584.263301	41178.762452	31.559719
584.941196	41230.769272	31.564736
585.491026	41295.378303	31.569754
586.027645	41339.894914	31.574772
586.870225	41395.424365	31.579789
587.344515	41452.924047	31.584807
588.288411	41501.839293	31.589824
589.431172	41538.286253	31.594842
590.010470	41578.027636	31.599860
590.924878	41608.701187	31.604877
591.359945	41645.421945	31.609895
592.296008	41685.882682	31.614912
592.812188	41720.061045	31.619930
593.383240	41746.398926	31.624948
593.704455	41791.465146	31.629965
594.015352	41832.416912	31.634983
594.249266	41875.831845	31.640000
594.597199	41927.325572	31.645018
595.134298	41984.135722	31.650036
595.834370	42039.661567	31.655053
596.067297	42087.045207	31.660071
596.774262	42145.715069	31.665088
596.894871	42202.809913	31.670106
597.658332	42261.676200	31.675124
597.687181	42322.637413	31.680141
597.773068	42397.162666	31.685159
598.290945	42452.876575	31.690176
599.259802	42522.732175	31.695194
599.718299	42585.102108	31.700212
600.411157	42653.450265	31.705229
600.806205	42732.340647	31.710247
601.138172	42791.391017	31.715264
601.761124	42871.236208	31.720282
602.387297	42939.416317	31.725300
603.349474	43015.123214	31.730317
603.522395	43091.725815	31.735335
604.400953	43161.437506	31.740352
604.907884	43238.716237	31.745370
605.815048	43295.345590	31.750388
607.206679	43354.314296	31.755405
607.711073	43418.790265	31.760423
608.369623	43476.847776	31.765440
609.054402	43536.525872	31.770458
609.984698	43587.780390	31.775476
610.561953	43642.491852	31.780493
611.133132	43699.623979	31.785511
611.803563	43750.819419	31.790528
612.426856	43800.602971	31.795546
612.962399	43851.249217	31.800564
613.756539	43918.721896	31.805581
614.062103	43985.118067	31.810599
614.851642	44032.412083	31.815616
615.162283	44099.145423	31.820634
615.535170	44160.455790	31.825652
616.196378	44218.253528	31.830669
616.338653	44291.323663	31.835687
617.507820	44359.135814	31.840704
618.113625	44425.583647	31.845722
618.350117	44496.649049	31.850740
618.777461	44566.207954	31.855757
619.371362	44645.147925	31.860775
619.858912	44712.382276	31.865792
620.408622	44785.443228	31.870810
621.219828	44867.876585	31.875828
622.071217	44932.646779	31.880845
622.258472	45008.570961	31.885863
623.337845	45082.264941	31.890880
624.186478	45153.702444	31.895898
624.631559	45238.397900	31.900916
625.368908	45303.755499	31.905933
625.710935	45379.155027	31.910951
626.521992	45448.287228	31.915968
627.446273	45526.755825	31.920986
627.550562	45597.524963	31.926004
628.494544	45657.885214	31.931021
628.710259	45735.155152	31.936039
629.638820	45807.166255	31.941056
630.124267	45888.148255	31.946074
630.571733	45959.387922	31.951092
631.397458	46035.978381	31.956109
631.972836	46112.211516	31.961127
632.678096	46196.005712	31.966144
633.134730	46266.951755	31.971162
633.621405	46326.958059	31.976180
634.378400	46392.884497	31.981197
634.562998	46467.928865	31.986215
635.542555	46536.827144	31.991232
636.169094	46617.685927	31.996250
636.345435	46692.899787	32.001268
637.241102	46761.742896	32.006285
638.117808	46843.272773	32.011303
638.847883	46913.603655	32.016320
639.740078	46974.768623	32.021338
640.329335	47043.617458	32.026356
641.349853	47109.794896	32.031373
641.587957	47192.696450	32.036391
642.222623	47255.733394	32.041408
642.848123	47327.108012	32.046426
643.613793	47407.143695	32.051444
644.663229	47467.827834	32.056461
644.971135	47539.446352	32.061479
645.696218	47603.202153	32.066496
646.495364	47662.181975	32.071514
646.818855	47736.745807	32.076532
648.070091	47795.493168	32.081549
648.536621	47880.557642	32.086567
649.075440	47941.302635	32.091584
650.036715	47999.175502	32.096602
650.544884	48070.559189	32.101620
651.288647	48138.169741	32.106637
651.421816	48209.679964	32.111655
652.088888	48284.207169	32.116672
653.187609	48353.065182	32.121690
653.831626	48418.698499	32.126708
654.372697	48483.477566	32.131725
655.107249	48564.463752	32.136743
655.649941	48627.412953	32.141760
656.493726	48695.423066	32.146778
656.793422	48780.149240	32.151796
657.566131	48847.802069	32.156813
657.924028	48915.360279	32.161831
658.645156	48992.636576	32.166848
659.421292	49055.733142	32.171866
659.805022	49139.734509	32.176884
660.684889	49214.869153	32.181901
661.136114	49288.620824	32.186919
661.909533	49366.972769	32.191936
662.720335	49442.415993	32.196954
663.206011	49516.469211	32.201972
663.909829	49595.937697	32.206989
664.166458	49675.550322	32.212007
664.835685	49758.035479	32.217024
665.276467	49836.518190	32.222042
665.779410	49928.888798	32.227060
666.945494	50010.112641	32.232077
667.207021	50103.311505	32.237095
668.097042	50187.227723	32.242112
669.456478	50250.951990	32.247130
669.776296	50331.182304	32.252148
670.404804	50380.926848	32.257165
671.100453	50458.014746	32.262183
671.420773	50533.168306	32.267200
672.293255	50592.449140	32.272218
673.275031	50675.734514	32.277236
673.737761	50746.949979	32.282253
673.952572	50826.350324	32.287271
674.467620	50902.907163	32.292288
675.949905	50979.461799	32.297306
677.041889	51050.205889	32.302324
677.657789	51109.844877	32.307341
678.870591	51185.300886	32.312359
679.174738	51245.466500	32.317376
680.135317	51308.456458	32.322394
680.355345	51385.529402	32.327412
681.212464	51448.419557	32.332429
681.275725	51522.775563	32.337447
681.597905	51597.008597	32.342464
682.845585	51668.468826	32.347482
683.283014	51746.578568	32.352500
684.458126	51822.403039	32.357517
685.392197	51892.885247	32.362535
685.889400	51965.674895	32.367552
686.819226	52027.163703	32.372570
687.454635	52104.877381	32.377588
688.039928	52171.442776	32.382605
688.502056	52254.777189	32.387623
689.060710	52332.065375	32.392640
689.891957	52402.749003	32.397658
690.215656	52487.069133	32.402676
690.691222	52561.174407	32.407693
691.083201	52648.280727	32.412711
691.829615	52734.488345	32.417728
692.943384	52806.409962	32.422746
693.744215	52893.569145	32.427764
694.984315	52960.023723	32.432781
696.040537	53037.646010	32.437799
696.481388	53113.734851	32.442816
697.347901	53178.005654	32.447834
697.660084	53255.100314	32.452852
698.519635	53314.490028	32.457869
699.018102	53405.831334	32.462887
699.461402	53477.609872	32.467904
700.642140	53550.085602	32.472922
701.358630	53616.865840	32.477940
702.309718	53689.555445	32.482957
702.548981	53762.882621	32.487975
702.893648	53842.670097	32.492992
703.825514	53914.852339	32.498010
704.293751	53992.733308	32.503028
704.990839	54066.086662	32.508045
705.721236	54148.279188	32.513063
705.961726	54216.052765	32.518080
706.984532	54293.177570	32.523098
707.423592	54376.986247	32.528116
708.100702	54451.603749	32.533133
708.953041	54523.883139	32.538151
709.200833	54615.197830	32.543168
710.137756	54688.439753	32.548186
710.659296	54781.965418	32.553204
711.336885	54858.973975	32.558221
711.506589	54954.327337	32.563239
712.181207	55046.965100	32.568256
713.131154	55144.370085	32.573274
713.367060	55250.001659	32.578292
714.329381	55334.852007	32.583309
715.256353	55428.174383	32.588327
715.813198	55538.668199	32.593344
716.864578	55629.462281	32.598362
717.310511	55735.656664	32.603380
718.087118	55829.497463	32.608397
718.479184	55915.381978	32.613415
719.495939	56011.104738	32.618432
720.551633	56110.237369	32.623450
721.632364	56198.014927	32.628468
722.542302	56291.903156	32.633485
724.248238	56352.342335	32.638503
725.275468	56434.119070	32.643520
726.389909	56496.831071	32.648538
726.744603	56575.129395	32.653556
727.298848	56635.898077	32.658573
728.042064	56711.849598	32.663591
728.490348	56787.365391	32.668608
729.617337	56855.822063	32.673626
729.831356	56926.094314	32.678644
730.409559	57004.336781	32.683661
731.239118	57079.859367	32.688679
731.673937	57163.438375	32.693696
732.276820	57247.549779	32.698714
732.905632	57336.863214	32.703732
733.792850	57422.054013	32.708749
733.912880	57516.737199	32.713767
734.194245	57609.791439	32.718784
735.010619	57699.771302	32.723802
735.906188	57807.550836	32.728820
736.592299	57908.321015	32.733837
737.217295	58012.103821	32.738855
737.716469	58119.313709	32.743872
738.509442	58217.599733	32.748890
739.720330	58318.493809	32.753908
740.332028	58419.588008	32.758925
741.223235	58516.120406	32.763943
742.146706	58623.713973	32.768960
743.054645	58707.890786	32.773978
743.720716	58808.192310	32.778996
744.407405	58903.212259	32.784013
745.342276	58993.571027	32.789031
745.966152	59075.022693	32.794048
746.473973	59151.889936	32.799066
747.718590	59237.638371	32.804084
748.696236	59313.894757	32.809101
750.574813	59358.618399	32.814119
751.705439	59430.522291	32.819136
752.329710	59486.707959	32.824154
752.784332	59545.348771	32.829172
752.983608	59608.987400	32.834189
754.109196	59674.344764	32.839207
754.337827	59742.945652	32.844224
755.245805	59818.548998	32.849242
755.681814	59887.486813	32.854260
756.534671	59960.725173	32.859277
757.172509	60032.851917	32.864295
757.468000	60124.991368	32.869312
758.093629	60211.916340	32.874330
758.467562	60303.857895	32.879348
758.877758	60398.948419	32.884365
760.014291	60497.861159	32.889383
760.615822	60586.095735	32.894400
761.441625	60677.512512	32.899418
762.437785	60777.175295	32.904436
763.180346	60874.226654	32.909453
764.072833	60961.658872	32.914471
764.497020	61066.482100	32.919488
765.259548	61156.784033	32.924506
766.068499	61262.658571	32.929524
767.285240	61356.334093	32.934541
768.128191	61438.525312	32.939559
768.760563	61540.659320	32.944576
769.768979	61621.227231	32.949594
770.699961	61717.157239	32.954612
771.458014	61804.409526	32.959629
772.000836	61892.069086	32.964647
772.253903	61998.487796	32.969664
773.024822	62090.984326	32.974682
773.897574	62194.832994	32.979700
774.459132	62297.386560	32.984717
775.536709	62397.468099	32.989735
776.843254	62476.978560	32.994752
778.257397	62551.707094	32.999770
779.425390	62638.459043	33.004788
780.065148	62714.044103	33.009805
781.180631	62787.668503	33.014823
781.927481	62858.001379	33.019840
782.658655	62932.931715	33.024858
783.406876	63015.416454	33.029876
783.681003	63103.566499	33.034893
784.656118	63167.403125	33.039911
784.929139	63253.526664	33.044928
785.588807	63341.019593	33.049946
786.605779	63431.086626	33.054964
786.970751	63523.152652	33.059981
787.938950	63604.307007	33.064999
788.565442	63693.262668	33.070016
789.121825	63771.622141	33.075034
789.894847	63860.479467	33.080052
790.456028	63948.887746	33.085069
791.240792	64028.620410	33.090087
791.848465	64125.716233	33.095104
792.354780	64222.474978	33.100122
793.463225	64311.877894	33.105140
793.876614	64410.979906	33.110157
794.593705	64513.539617	33.115175
795.298727	64622.029650	33.120192
796.368255	64720.987771	33.125210
797.020062	64820.489781	33.130228
797.436180	64922.894311	33.135245
798.450603	65038.610794	33.140263
799.378594	65138.171556	33.145280
800.373892	65233.436372	33.150298
801.754445	65323.612378	33.155316
802.496267	65433.901362	33.160333
803.487535	65513.673671	33.165351
804.155439	65634.593776	33.170368
804.917337	65723.761566	33.175386
805.736262	65821.735642	33.180404
806.017578	65923.191031	33.185421
807.158573	66020.341056	33.190439
807.616870	66123.190599	33.195456
808.428830	66232.364399	33.200474
809.467471	66336.256578	33.205492
809.986312	66451.248730	33.210509
810.985052	66553.177554	33.215527
811.915129	66661.472720	33.220544
812.644431	66763.009667	33.225562
813.573668	66869.505786	33.230580
814.327615	66980.085954	33.235597
815.006925	67094.949002	33.240615
815.780189	67207.188793	33.245632
816.527875	67316.148369	33.250650
817.319894	67424.716150	33.255668
817.842251	67541.855758	33.260685
819.279435	67644.832387	33.265703
819.691639	67764.423027	33.270720
820.612576	67884.198761	33.275738
821.784121	67986.587747	33.280756
822.345257	68105.594531	33.285773
823.449535	68214.710867	33.290791
824.177376	68321.663965	33.295808
825.049812	68432.126145	33.300826
826.435898	68522.379388	33.305844
827.030932	68638.288417	33.310861
827.934925	68734.974896	33.315879
829.083295	68842.287201	33.320896
829.591786	68947.130630	33.325914
830.660067	69041.019001	33.330932
831.110314	69148.791578	33.335949
832.201941	69248.754936	33.340967
832.426814	69363.495206	33.345984
833.073946	69453.693468	33.351002
833.988710	69557.009753	33.356020
834.638903	69661.752322	33.361037
835.154301	69769.770662	33.366055
835.693005	69891.331713	33.371072
836.269350	70002.241602	33.376090
837.604232	70115.855577	33.381108
838.103403	70239.206773	33.386125
838.860916	70355.138005	33.391143
839.474963	70496.138131	33.396160
840.228940	70608.166760	33.401178
841.474215	70732.084667	33.406196
842.074608	70859.783256	33.411213
842.859460	70980.092414	33.416231
843.918289	71114.455069	33.421248
844.887012	71241.889000	33.426266
845.716338	71355.445262	33.431284
846.437265	71490.401321	33.436301
847.705032	71618.061779	33.441319
848.135401	71740.599250	33.446336
848.966334	71870.308581	33.451354
850.170527	71997.861550	33.456372
850.649971	72140.676690	33.461389
851.779744	72260.420596	33.466407
852.627542	72389.353425	33.471424
853.541436	72526.377346	33.476442
854.761997	72644.662100	33.481460
855.493990	72773.451556	33.486477
856.403805	72897.518544	33.491495
857.457145	73027.395915	33.496512
858.102073	73152.069036	33.501530
859.305564	73262.271781	33.506548
860.316775	73392.935485	33.511565
861.600376	73494.355808	33.516583
862.448139	73611.081600	33.521600
862.956687	73728.437107	33.526618
864.109203	73847.295914	33.531636
864.723714	73966.158897	33.536653
865.594173	74076.981553	33.541671
866.624612	74195.912411	33.546688
866.959091	74314.177443	33.551706
868.335983	74425.888304	33.556724
869.332033	74550.571125	33.561741
870.984297	74637.233102	33.566759
872.651390	74745.992582	33.571776
872.604580	74859.341687	33.576794
873.998380	74951.095509	33.581812
874.705042	75052.267952	33.586829
875.535165	75155.658425	33.591847
876.080278	75255.435667	33.596864
876.914661	75366.612438	33.601882
878.106912	75456.397277	33.606900
878.847356	75556.524109	33.611917
880.062990	75655.444565	33.616935
880.863279	75750.279445	33.621952
881.258628	75849.375627	33.626970
882.188409	75940.398850	33.631988
882.809609	76043.707037	33.637005
883.744104	76130.698228	33.642023
884.600702	76224.382451	33.647040
885.441915	76336.435630	33.652058
886.239627	76429.662488	33.657076
886.633051	76545.314687	33.662093
887.226566	76647.922503	33.667111
888.313213	76756.203732	33.672128
888.720396	76878.239023	33.677146
889.891483	77003.357857	33.682164
890.516228	77113.730657	33.687181
891.689020	77241.859147	33.692199
892.427509	77354.977141	33.697216
893.156318	77474.727411	33.702234
894.295493	77593.205876	33.707252
894.875360	77721.501256	33.712269
895.725906	77852.933593	33.717287
896.648708	77983.160689	33.722304
897.406275	78108.250973	33.727322
898.107425	78236.549244	33.732340
899.237668	78371.726469	33.737357
900.044559	78506.248120	33.742375
900.938317	78644.030987	33.747392
901.832453	78791.150559	33.752410
902.695590	78906.678163	33.757428
903.324949	79046.667533	33.762445
904.575135	79191.362977	33.767463
905.779284	79322.925446	33.772480
906.220240	79466.278803	33.777498
907.588533	79593.550191	33.782516
908.800717	79719.172115	33.787533
910.105670	79845.936811	33.792551
911.033019	79976.871137	33.797568
912.143062	80092.106928	33.802586
913.297309	80212.153119	33.807604
913.538645	80346.169930	33.812621
914.712386	80458.357084	33.817639
915.824934	80585.934456	33.822656
916.495025	80723.103051	33.827674
917.615373	80841.982505	33.832692
918.408578	80972.685289	33.837709
919.293530	81098.038933	33.842727
920.107763	81217.936440	33.847744
920.859684	81342.535173	33.852762
921.801888	81466.560714	33.857780
922.461412	81608.655058	33.862797
923.484601	81733.130780	33.867815
924.816179	81861.875931	33.872832
925.115268	81996.918300	33.877850
926.832014	82113.864155	33.882868
928.124739	82229.133301	33.887885
928.685553	82359.338073	33.892903
929.909086	82467.469475	33.897920
930.547725	82580.018726	33.902938
931.808870	82683.169870	33.907956
932.484606	82794.601699	33.912973
933.042346	82905.363790	33.917991
934.340330	83006.576112	33.923008
935.196356	83140.045213	33.928026
936.117540	83246.584986	33.933044
936.901488	83357.471520	33.938061
937.497404	83476.019495	33.943079
938.663912	83603.233696	33.948096
939.502194	83720.935234	33.953114
940.532563	83844.037761	33.958132
941.156881	83975.279298	33.963149
941.992267	84102.966477	33.968167
942.946249	84234.157168	33.973184
943.177496	84370.578573	33.978202
944.723972	84502.056005	33.983220
945.257150	84636.509029	33.988237
946.284772	84778.085703	33.993255
947.168885	84914.931510	33.998272
948.048889	85068.534033	34.003290
949.297593	85202.573305	34.008308
950.181686	85344.435825	34.013325
950.885222	85492.511753	34.018343
952.435645	85627.441478	34.023360
953.244882	85775.066273	34.028378
954.084410	85912.083661	34.033396
954.999971	86056.456129	34.038413
955.674564	86195.822122	34.043431
956.916625	86338.810388	34.048448
957.963596	86482.791766	34.053466
959.235594	86620.687035	34.058484
960.473453	86749.672897	34.063501
961.527961	86894.041557	34.068519
962.517479	87028.576163	34.073536
963.371552	87160.989552	34.078554
964.751561	87294.395053	34.083572
965.558842	87422.214084	34.088589
966.780601	87558.359143	34.093607
968.140808	87673.545983	34.098624
968.953854	87793.284894	34.103642
970.050077	87912.941476	34.108660
971.318024	88057.170163	34.113677
971.699514	88178.377386	34.118695
972.813449	88302.807652	34.123712
973.599272	88431.034467	34.128730
974.554823	88562.713096	34.133748
975.354385	88682.522319	34.138765
976.066110	88830.809668	34.143783
976.740480	88958.323773	34.148800
978.216529	89091.301405	34.153818
979.532524	89217.956089	34.158836
980.549437	89351.451038	34.163853
981.252565	89482.479773	34.168871
982.332451	89596.728585	34.173888
983.174650	89722.588871	34.178906
983.982230	89838.387404	34.183924
984.702412	89955.990189	34.188941
985.317928	90088.560625	34.193959
986.390506	90218.889942	34.198976
987.761559	90353.264348	34.203994
988.367088	90478.085194	34.209012
989.480021	90605.507545	34.214029
989.931933	90750.744043	34.219047
991.403213	90882.525411	34.224064
992.075067	91028.848180	34.229082
993.042859	91173.784050	34.234100
994.549209	91309.445647	34.239117
995.933674	91437.259703	34.244135
997.542904	91539.683403	34.249152
998.154533	91680.106588	34.254170
998.994094	91801.469771	34.259188
1000.159985	91935.481731	34.264205
1001.005165	92067.546905	34.269223
1002.074369	92185.865088	34.274240
1003.267397	92312.860837	34.279258
1004.084641	92442.706361	34.284276
1005.432815	92571.804070	34.289293
1006.447849	92697.337669	34.294311
1007.961524	92807.290161	34.299328
1008.994679	92938.217439	34.304346
1009.772308	93061.273517	34.309364
1010.682980	93180.899899	34.314381
1011.385003	93315.740374	34.319399
1012.457291	93438.195055	34.324416
1013.221273	93575.772363	34.329434
1013.836026	93706.637899	34.334452
1015.275979	93836.784682	34.339469
1015.728041	93971.434857	34.344487
1017.270715	94108.214770	34.349504
1018.132415	94256.925976	34.354522
1019.552917	94388.135410	34.359540
1020.712396	94514.826489	34.364557
1021.317455	94646.818681	34.369575
1022.564595	94785.003407	34.374592
1023.533964	94925.453445	34.379610
1024.561771	95065.926694	34.384628
1025.616894	95202.183600	34.389645
1026.372054	95342.113664	34.394663
1027.276435	95474.562837	34.399680
1028.171542	95629.742718	34.404698
1028.641496	95763.995958	34.409716
1029.792839	95926.063870	34.414733
1030.791040	96079.895696	34.419751
1032.027537	96217.015515	34.424768
1032.937411	96374.032683	34.429786
1033.613086	96530.423965	34.434804
1035.123231	96684.013989	34.439821
1036.107532	96841.016232	34.444839
1037.046453	96976.986032	34.449856
1037.661290	97120.928574	34.454874
1038.582577	97265.057351	34.459892
1039.691389	97410.580619	34.464909
1040.337683	97563.244869	34.469927
1041.600168	97711.307769	34.474944
1042.129793	97869.199206	34.479962
1043.311129	98030.619440	34.484980
1044.394089	98189.987707	34.489997
1045.343377	98362.379347	34.495015
1046.367002	98518.153221	34.500032
1047.515253	98676.502241	34.505050
1048.490520	98844.875985	34.510068
1050.113640	99000.386959	34.515085
1050.954133	99170.454778	34.520103
1051.952270	99317.228849	34.525120
1053.362620	99479.913530	34.530138
1054.562275	99630.472625	34.535156
1055.791274	99796.054460	34.540173
1056.556886	99956.997604	34.545191
1057.530462	100114.422610	34.550208
1058.559030	100270.922520	34.555226
1059.760107	100447.902156	34.560244
1060.931957	100612.195547	34.565261
1061.943168	100773.978454	34.570279
1063.381691	100926.368188	34.575296
1064.514697	101085.147441	34.580314
1065.597418	101252.610524	34.585332
1066.713731	101402.023846	34.590349
1067.545489	101568.168735	34.595367
1068.608634	101724.451485	34.600384
1069.907171	101875.958555	34.605402
1070.694105	102041.911467	34.610420
1071.938392	102200.073175	34.615437
1073.163220	102356.144607	34.620455
1074.514457	102502.838375	34.625472
1076.098277	102657.095628	34.630490
1076.998754	102812.772427	34.635508
1078.167286	102961.908995	34.640525
1079.154026	103116.390791	34.645543
1080.598750	103261.555759	34.650560
1081.615269	103411.839390	34.655578
1082.137766	103572.156402	34.660596
1083.317430	103714.417499	34.665613
1083.902019	103876.080886	34.670631
1085.124033	104031.644991	34.675648
1086.766465	104182.188348	34.680666
1087.721804	104336.031330	34.685684
1089.035874	104488.483008	34.690701
1089.775464	104648.304497	34.695719
1090.948766	104795.363575	34.700736
1092.135879	104948.774987	34.705754
1093.182385	105109.537980	34.710772
1094.392641	105247.126766	34.715789
1095.449472	105405.909334	34.720807
1096.469484	105541.182229	34.725824
1097.643179	105684.645844	34.730842
1099.689460	105787.411961	34.735860
1101.550792	105902.149929	34.740877
1102.552912	106028.669709	34.745895
1103.890056	106134.011929	34.750912
1105.086590	106251.654558	34.755930
1105.398709	106375.216513	34.760948
1106.254672	106490.243774	34.765965
1107.254407	106613.621653	34.770983
1108.385646	106744.111787	34.776000
1109.033333	106876.059217	34.781018
1110.000888	107016.006799	34.786036
1110.916638	107152.659753	34.791053
1111.434375	107304.294062	34.796071
1112.347555	107464.689017	34.801088
1113.668135	107608.305328	34.806106
1114.164396	107768.331903	34.811124
1115.644247	107933.411952	34.816141
1116.494002	108099.479415	34.821159
1117.269457	108279.597957	34.826176
1118.434311	108441.725203	34.831194
1119.443566	108619.625502	34.836212
1120.414154	108791.052030	34.841229
1121.696752	108983.677820	34.846247
1122.649017	109141.375006	34.851264
1123.901483	109312.140090	34.856282
1124.837818	109506.394780	34.861300
1125.914235	109684.260517	34.866317
1127.640318	109865.695395	34.871335
1128.200608	110047.804398	34.876352
1129.739612	110230.126227	34.881370
1130.365105	110423.779333	34.886388
1131.770228	110597.649663	34.891405
1132.797350	110795.140966	34.896423
1133.965485	110977.945089	34.901440
1135.326437	111177.899332	34.906458
1136.216027	111359.452940	34.911476
1137.551456	111548.533010	34.916493
1138.293947	111734.195627	34.921511
1139.582934	111931.078325	34.926528
1140.923179	112114.160988	34.931546
1142.207383	112304.077888	34.936564
1143.356979	112500.240298	34.941581
1144.736407	112685.384603	34.946599
1145.543018	112879.344618	34.951616
1147.201855	113058.965168	34.956634
1148.127000	113258.074888	34.961652
1148.959786	113435.347963	34.966669
1150.387718	113623.966958	34.971687
1151.648631	113812.759536	34.976704
1152.891056	113994.871309	34.981722
1154.140484	114189.948550	34.986740
1155.500587	114368.613080	34.991757
1156.446788	114564.437823	34.996775
1157.352448	114742.974686	35.001792
1158.767770	114906.839092	35.006810
1159.809237	115082.349591	35.011828
1160.698835	115248.066134	35.016845
1161.850051	115420.358057	35.021863
1163.455364	115600.828297	35.026880
1164.375953	115777.287161	35.031898
1165.301307	115950.258036	35.036916
1166.717363	116120.594261	35.041933
1168.000999	116316.144619	35.046951
1168.540158	116495.879045	35.051968
1169.946291	116675.109658	35.056986
1170.520656	116869.092902	35.062004
1171.585706	117052.432467	35.067021
1173.017896	117249.276940	35.072039
1174.329236	117446.977898	35.077056
1175.543897	117641.764242	35.082074
1176.611333	117840.159157	35.087092
1177.933930	118032.645587	35.092109
1179.143921	118233.946087	35.097127
1180.055405	118428.115419	35.102144
1181.786437	118615.026295	35.107162
1182.782552	118820.506361	35.112180
1183.932737	119012.672918	35.117197
1185.625053	119211.206938	35.122215
1186.550530	119403.475435	35.127232
1187.874764	119597.372600	35.132250
1188.972236	119791.357921	35.137268
1190.656227	119976.570083	35.142285
1192.489268	120157.973225	35.147303
1193.042380	120347.141800	35.152320
1194.764275	120528.337223	35.157338
1195.882762	120722.205795	35.162356
1196.848624	120907.361425	35.167373
1198.101707	121087.698067	35.172391
1199.129132	121277.583143	35.177408
1200.506758	121470.174868	35.182426
1201.432193	121652.150591	35.187444
1202.899353	121846.174639	35.192461
1204.077272	122028.252123	35.197479
1205.012639	122231.191218	35.202496
1206.581338	122414.070463	35.207514
1207.939063	122607.180246	35.212532
1208.901520	122790.209135	35.217549
1210.542077	122975.917917	35.222567
1211.471743	123168.973180	35.227584
1212.886964	123346.994254	35.232602
1214.236397	123536.654315	35.237620
1215.776487	123702.283274	35.242637
1217.081948	123891.015553	35.247655
1217.938169	124078.832623	35.252672
1219.489030	124249.922392	35.257690
1220.795376	124431.793207	35.262708
1221.992535	124602.979459	35.267725
1223.142506	124777.454934	35.272743
1224.059824	124955.261847	35.277760
1225.187787	125119.077740	35.282778
1226.260445	125291.656158	35.287796
1226.829169	125462.403103	35.292813
1227.957968	125643.600967	35.297831
1229.332020	125832.196593	35.302848
1230.199719	126010.829013	35.307866
1231.451777	126207.528257	35.312884
1232.134341	126402.457372	35.317901
1233.718108	126588.478773	35.322919
1235.073366	126794.489035	35.327936
1236.621742	126978.365249	35.332954
1237.895569	127166.377998	35.337972
1239.045423	127351.814861	35.342989
1240.669189	127531.958494	35.348007
1241.538117	127738.015165	35.353024
1242.993343	127921.101762	35.358042
1244.020106	128123.766540	35.363060
1245.206178	128322.657698	35.368077
1246.504155	128519.505574	35.373095
1247.463851	128727.683471	35.378112
1249.239500	128924.774999	35.383130
1249.897053	129118.688518	35.388148
1251.336640	129323.146050	35.393165
1253.404319	129517.699640	35.398183
1254.316601	129725.221106	35.403200
1255.619597	129919.582350	35.408218
1256.771011	130124.015557	35.413236
1258.201701	130310.441097	35.418253
1259.420264	130518.021107	35.423271
1260.628185	130720.650662	35.428288
1262.136182	130910.995378	35.433306
1263.308466	131119.271333	35.438324
1264.187114	131330.104077	35.443341
1265.862592	131523.619033	35.448359
1267.009519	131734.386806	35.453376
1268.111913	131935.711549	35.458394
1269.301854	132145.246570	35.463412
1270.055859	132359.489659	35.468429
1271.464049	132572.185975	35.473447
1272.799158	132792.636984	35.478464
1273.917452	133012.769397	35.483482
1275.217753	133227.058866	35.488500
1276.549551	133449.492053	35.493517
1278.144102	133659.784795	35.498535
1279.499928	133884.954387	35.503552
1281.221081	134084.675449	35.508570
1282.429891	134289.408304	35.513588
1283.845990	134490.967269	35.518605
1285.397191	134703.796056	35.523623
1286.382374	134920.403685	35.528640
1287.813099	135112.904808	35.533658
1289.390842	135320.969540	35.538676
1290.501860	135528.793171	35.543693
1292.097031	135717.331360	35.548711
1293.556045	135908.654815	35.553728
1294.670148	136076.490450	35.558746
1295.750056	136261.401279	35.563764
1296.810038	136440.525436	35.568781
1298.075392	136629.958290	35.573799
1299.490968	136828.251530	35.578816
1300.938463	136999.929758	35.583834
1302.045132	137194.650376	35.588852
1302.820388	137393.796871	35.593869
1304.414904	137587.922982	35.598887
1305.686068	137785.434603	35.603904
1306.764249	137972.498102	35.608922
1308.309409	138175.075769	35.613940
1309.476958	138376.346202	35.618957
1310.817952	138574.891143	35.623975
1311.792888	138789.361934	35.628992
1313.173397	138983.315767	35.634010
1314.540652	139202.340098	35.639028
1315.906858	139403.737974	35.644045
1317.359992	139608.760582	35.649063
1319.064128	139817.090429	35.654080
1320.701902	140011.174791	35.659098
1322.366915	140202.505952	35.664116
1323.443398	140399.204042	35.669133
1324.672514	140599.909348	35.674151
1326.155482	140808.306564	35.679168
1327.545838	141009.939490	35.684186
1328.755019	141206.773832	35.689204
1329.925496	141402.677735	35.694221
1331.186576	141605.336407	35.699239
1332.706541	141810.566139	35.704256
1334.137219	142007.091631	35.709274
1336.012721	142201.342372	35.714292
1337.152189	142409.577035	35.719309
1338.531432	142599.688640	35.724327
1339.654624	142805.926031	35.729344
1341.017485	143004.141740	35.734362
1342.321484	143215.207499	35.739380
1343.332300	143417.943305	35.744397
1344.311461	143623.955577	35.749415
1345.388295	143849.612474	35.754432
1346.693527	144064.473641	35.759450
1348.201637	144275.552230	35.764468
1349.255571	144512.992748	35.769485
1350.740236	144725.497740	35.774503
1352.073741	144947.281215	35.779520
1353.578661	145164.539240	35.784538
1354.878156	145390.095873	35.789556
1356.004211	145614.591592	35.794573
1357.848433	145844.957714	35.799591
1358.733722	146071.700542	35.804608
1360.386904	146298.525773	35.809626
1361.634832	146521.614247	35.814644
1362.519720	146750.871866	35.819661
1364.008515	146974.140745	35.824679
1365.160484	147195.525260	35.829696
1366.983410	147400.629670	35.834714
1368.363505	147617.303299	35.839732
1369.567452	147829.544265	35.844749
1370.676212	148046.314637	35.849767
1371.869071	148268.562118	35.854784
1373.172146	148494.596656	35.859802
1374.781692	148707.121255	35.864820
1375.825626	148938.359583	35.869837
1377.016962	149166.102635	35.874855
1378.591814	149395.256892	35.879872
1380.066611	149631.350438	35.884890
1381.419822	149857.323179	35.889908
1382.620078	150092.132595	35.894925
1384.445465	150311.301759	35.899943
1385.803039	150546.266937	35.904960
1387.279556	150771.199548	35.909978
1389.098994	151000.110737	35.914996
1390.718337	151236.623999	35.920013
1392.119377	151453.041104	35.925031
1393.626932	151680.751495	35.930048
1395.021528	151905.121716	35.935066
1396.672056	152126.181819	35.940084
1397.812267	152347.248431	35.945101
1399.566225	152567.547032	35.950119
1400.743861	152789.092421	35.955136
1401.904063	153017.818104	35.960154
1403.896680	153245.538252	35.965172
1405.044938	153474.395753	35.970189
1406.312806	153692.230629	35.975207
1407.988508	153921.970964	35.980224
1409.709792	154151.629556	35.985242
1410.969743	154362.281077	35.990260
1412.202877	154598.055512	35.995277
1413.837393	154816.409975	36.000295
1415.142274	155049.741756	36.005312
1416.322310	155274.105305	36.010330
1417.552772	155501.594152	36.015348
1418.601238	155748.931579	36.020365
1420.275048	155976.213673	36.025383
1421.334885	156218.785157	36.030400
1422.392906	156467.229406	36.035418
1424.302502	156711.305046	36.040436
1425.442280	156966.992832	36.045453
1426.884674	157201.522072	36.050471
1428.484811	157448.669981	36.055488
1429.824114	157711.483204	36.060506
1431.388180	157940.659732	36.065524
1432.436238	158189.434979	36.070541
1434.838841	158429.171110	36.075559
1436.485545	158668.052598	36.080576
1438.522192	158881.499664	36.085594
1440.337624	159108.970088	36.090612
1441.587173	159341.477447	36.095629
1443.038638	159555.110369	36.100647
1444.849576	159755.943044	36.105664
1445.958675	159962.747049	36.110682
1447.372235	160166.168740	36.115700
1448.190279	160364.169887	36.120717
1450.135776	160575.600041	36.125735
1451.192863	160783.621829	36.130752
1452.120367	160999.730834	36.135770
1453.783330	161208.128047	36.140788
1454.776266	161434.488654	36.145805
1456.145622	161659.687574	36.150823
1458.078746	161876.390315	36.155840
1459.068619	162112.419201	36.160858
1460.553811	162338.035154	36.165876
1462.044553	162578.261322	36.170893
1463.193609	162808.664018	36.175911
1464.740208	163039.499621	36.180928
1466.302161	163283.764771	36.185946
1467.476938	163515.651694	36.190964
1468.806163	163770.191742	36.195981
1470.265186	164011.408973	36.200999
1471.922029	164258.671332	36.206016
1473.162090	164512.913644	36.211034
1474.502368	164761.992582	36.216052
1476.203125	165024.840254	36.221069
1477.648457	165260.842516	36.226087
1479.498240	165508.019189	36.231104
1481.216697	165758.452570	36.236122
1483.341859	165982.492699	36.241140
1485.003899	166229.615218	36.246157
1486.260686	166467.430755	36.251175
1488.226944	166694.328793	36.256192
1490.095101	166928.828534	36.261210
1492.069364	167152.392307	36.266228
1493.147988	167372.497543	36.271245
1494.465115	167599.199765	36.276263
1496.361388	167829.159862	36.281280
1497.710266	168054.426494	36.286298
1499.379346	168267.568455	36.291316
1501.057375	168496.400342	36.296333
1502.525219	168726.104147	36.301351
1504.165970	168952.433236	36.306368
1505.022290	169173.878000	36.311386
1506.393251	169402.510405	36.316404
1507.807109	169643.250971	36.321421
1509.669294	169863.639308	36.326439
1511.050841	170094.963249	36.331456
1512.179843	170326.036946	36.336474
1513.858313	170556.339750	36.341492
1515.083809	170794.796094	36.346509
1516.605892	171037.697222	36.351527
1517.992710	171274.837012	36.356544
1519.527492	171529.016094	36.361562
1521.019860	171767.918001	36.366580
1522.275099	172012.402454	36.371597
1523.808100	172251.338891	36.376615
1525.186951	172492.597307	36.381632
1526.100848	172730.873868	36.386650
1527.666272	172958.684307	36.391668
1528.641022	173196.801763	36.396685
1530.022049	173451.017607	36.401703
1531.713084	173694.999181	36.406720
1533.342979	173955.179035	36.411738
1534.865717	174201.803699	36.416756
1536.379621	174453.759378	36.421773
1538.184372	174699.669928	36.426791
1540.303239	174932.275083	36.431808
1541.631959	175196.316605	36.436826
1543.238397	175437.531177	36.441844
1544.734747	175687.645103	36.446861
1546.148471	175939.245309	36.451879
1547.900604	176191.732100	36.456896
1549.304348	176451.672061	36.461914
1550.809988	176709.592980	36.466932
1552.363912	176973.356426	36.471949
1553.797713	177238.206323	36.476967
1555.764195	177497.530610	36.481984
1556.846021	177753.495431	36.487002
1558.704115	178016.684315	36.492020
1560.206857	178286.642796	36.497037
1561.385545	178545.159864	36.502055
1563.181880	178826.163798	36.507072
1564.477285	179096.312645	36.512090
1566.446903	179357.995079	36.517108
1567.749516	179640.909833	36.522125
1569.238826	179918.341127	36.527143
1570.949276	180181.643052	36.532160
1572.388302	180466.914201	36.537178
1573.799175	180735.164591	36.542196
1575.430542	181027.590235	36.547213
1577.045448	181305.809867	36.552231
1578.816049	181589.475131	36.557248
1579.841665	181876.216927	36.562266
1582.179626	182159.237499	36.567284
1583.672935	182445.819923	36.572301
1585.202013	182725.508707	36.577319
1587.289834	182994.591731	36.582336
1589.118210	183268.082482	36.587354
1590.843763	183544.395451	36.592372
1592.716441	183818.643879	36.597389
1594.104620	184096.777599	36.602407
1595.708095	184354.766924	36.607424
1597.152422	184627.502234	36.612442
1599.073219	184904.883851	36.617460
1601.228208	185168.360745	36.622477
1602.184494	185434.186729	36.627495
1604.356047	185701.889602	36.632512
1605.812808	185961.548321	36.637530
1607.648728	186223.419703	36.642548
1609.475084	186468.721611	36.647565
1610.871928	186726.566895	36.652583
1612.560944	186968.517856	36.657600
1614.131780	187216.617983	36.662618
1615.713345	187459.070785	36.667636
1617.041335	187704.394961	36.672653
1618.627263	187953.981340	36.677671
1620.028092	188185.426411	36.682688
1621.432575	188443.089658	36.687706
1622.487420	188691.749111	36.692724
1624.106626	188945.777017	36.697741
1625.929989	189211.550412	36.702759
1627.242167	189480.388707	36.707776
1628.860881	189750.816898	36.712794
1630.187425	190022.828569	36.717812
1632.083310	190285.258847	36.722829
1633.127748	190558.549341	36.727847
1635.228278	190826.445102	36.732864
1636.893884	191113.726738	36.737882
1638.885583	191388.572046	36.742900
1640.719105	191652.986735	36.747917
1642.760446	191927.383020	36.752935
1644.339251	192187.043869	36.757952
1646.384192	192450.477464	36.762970
1649.109503	192688.079442	36.767988
1650.979608	192937.126255	36.773005
1652.388145	193196.679857	36.778023
1654.486791	193438.065428	36.783040
1655.726158	193682.672641	36.788058
1657.277554	193934.960605	36.793076
1658.845582	194181.371014	36.798093
1660.104621	194446.031452	36.803111
1661.674784	194699.221369	36.808128
1663.000008	194965.092412	36.813146
1664.738647	195225.708248	36.818164
1666.271169	195496.816243	36.823181
1667.561958	195773.865809	36.828199
1669.713257	196043.545780	36.833216
1671.006874	196320.724763	36.838234
1672.114312	196599.318237	36.843252
1674.000970	196890.430903	36.848269
1675.357135	197174.991377	36.853287
1676.884833	197456.111919	36.858304
1678.710532	197745.094018	36.863322
1680.516245	198035.147046	36.868340
1682.184740	198337.078299	36.873357
1683.909490	198627.883597	36.878375
1686.221226	198908.265422	36.883392
1687.534774	199195.991326	36.888410
1689.181084	199492.474753	36.893428
1691.141238	199775.353962	36.898445
1692.537800	200067.488462	36.903463
1694.804416	200351.743630	36.908480
1696.255513	200646.601582	36.913498
1698.067474	200925.105798	36.918516
1699.923879	201212.261151	36.923533
1701.339729	201487.784738	36.928551
1703.279938	201751.383538	36.933568
1704.925187	202020.552059	36.938586
1706.648177	202280.912958	36.943604
1708.680544	202531.388461	36.948621
1710.308288	202787.971477	36.953639
1712.150933	203038.987110	36.958656
1713.856740	203316.199999	36.963674
1715.677353	203563.946482	36.968692
1717.485208	203820.480191	36.973709
1718.651546	204083.996991	36.978727
1720.426101	204346.225198	36.983744
1722.462357	204621.043569	36.988762
1723.814837	204872.830562	36.993780
1725.845043	205147.563536	36.998797
1727.480606	205419.428113	37.003815
1729.074233	205686.375254	37.008832
1730.630424	205959.016591	37.013850
1731.963985	206242.725921	37.018868
1734.176439	206517.385594	37.023885
1735.678823	206809.385664	37.028903
1737.503277	207086.686545	37.033920
1739.108661	207365.292950	37.038938
1740.835503	207650.457185	37.043956
1742.732075	207928.207503	37.048973
1744.629617	208218.856814	37.053991
1746.584640	208493.452134	37.059008
1748.288977	208785.480470	37.064026
1749.819702	209069.692285	37.069044
1751.905931	209355.492952	37.074061
1753.548222	209640.134001	37.079079
1755.421221	209927.748463	37.084096
1757.115619	210215.722679	37.089114
1758.593095	210506.055881	37.094132
1761.261806	210788.330217	37.099149
1762.916571	211081.672089	37.104167
1764.583857	211360.439004	37.109184
1766.620862	211640.240247	37.114202
1768.177651	211922.074058	37.119220
1769.973380	212198.805635	37.124237
1771.671521	212486.408641	37.129255
1773.459995	212776.080669	37.134272
1775.521649	213058.004301	37.139290
1777.011537	213352.931530	37.144308
1778.889117	213631.674808	37.149325
1780.663264	213930.139710	37.154343
1782.401844	214212.144943	37.159360
1784.122283	214496.134821	37.164378
1785.730335	214799.073567	37.169396
1787.723158	215081.575319	37.174413
1789.406619	215388.694447	37.179431
1791.235166	215661.664468	37.184448
1793.181196	215956.644964	37.189466
1795.091952	216243.443189	37.194484
1797.033232	216526.403449	37.199501
1798.796582	216806.752248	37.204519
1800.495232	217064.309562	37.209536
1802.227003	217338.380745	37.214554
1804.258446	217601.410186	37.219572
1805.677829	217858.557655	37.224589
1807.130706	218132.269888	37.229607
1808.879431	218395.753437	37.234624
1810.658005	218671.993461	37.239642
1812.124209	218951.775751	37.244660
1814.171056	219239.694516	37.249677
1815.451405	219533.843306	37.254695
1817.338910	219807.188147	37.259712
1819.333119	220106.457058	37.264730
1820.886948	220418.138631	37.269748
1823.115898	220694.568721	37.274765
1824.606429	220991.318230	37.279783
1826.216887	221346.292010	37.284800
1828.207467	221657.515776	37.289818
1829.786632	221957.162670	37.294836
1831.438586	222261.840038	37.299853
1833.665140	222576.471064	37.304871
1835.648596	222886.837509	37.309888
1837.677834	223195.813890	37.314906
1839.002178	223507.214334	37.319924
1841.631319	223794.765918	37.324941
1844.278173	224084.855267	37.329959
1846.423096	224377.069673	37.334976
1848.604705	224664.860499	37.339994
1850.307558	224955.763117	37.345012
1852.486635	225238.147116	37.350029
1854.225711	225521.617762	37.355047
1856.338519	225802.300009	37.360064
1858.296841	226082.753770	37.365082
1860.071261	226363.910662	37.370100
1862.109759	226636.417297	37.375117
1863.748701	226925.343393	37.380135
1865.701447	227211.935002	37.385152
1867.360605	227486.510891	37.390170
1868.951629	227780.831528	37.395188
1871.191840	228060.853461	37.400205
1872.997926	228354.786367	37.405223
1875.173424	228632.610907	37.410240
1876.954276	228912.505311	37.415258
1879.226167	229195.243309	37.420276
1881.408768	229466.212191	37.425293
1883.056022	229741.076418	37.430311
1884.996964	230020.466353	37.435328
1887.368264	230289.960138	37.440346
1889.176947	230564.115523	37.445364
1890.858316	230830.469555	37.450381
1892.605565	231102.401331	37.455399
1894.112787	231391.413714	37.460416
1896.166126	231660.377833	37.465434
1897.586840	231938.383092	37.470452
1899.526758	232223.418128	37.475469
1901.451429	232494.817827	37.480487
1902.928547	232761.031969	37.485504
1904.914684	233026.048555	37.490522
1906.779102	233293.472594	37.495540
1908.731061	233555.499085	37.500557
1910.637872	233824.873502	37.505575
1912.278811	234081.236173	37.510592
1914.351499	234355.639949	37.515610
1915.715129	234642.525995	37.520628
1917.392258	234919.610117	37.525645
1919.214185	235198.703894	37.530663
1920.911406	235489.069780	37.535680
1922.608794	235779.842836	37.540698
1924.247932	236080.963220	37.545716
1926.271333	236388.576373	37.550733
1928.193152	236699.863977	37.555751
1930.167034	237010.890244	37.560768
1932.346205	237312.131624	37.565786
1933.565147	237629.603831	37.570804
1935.837711	237945.969994	37.575821
1937.487296	238264.594864	37.580839
1939.314117	238594.114215	37.585856
1941.520806	238917.529211	37.590874
1943.313425	239250.942019	37.595892
1945.599742	239575.438435	37.600909
1947.163176	239905.054194	37.605927
1949.093686	240237.990795	37.610944
1951.237473	240574.653658	37.615962
1952.586157	240919.774781	37.620980
1954.799628	241256.987317	37.625997
1957.108282	241596.624086	37.631015
1958.918043	241947.466171	37.636032
1961.214286	242290.434237	37.641050
1963.503485	242636.655587	37.646068
1965.241909	242970.976384	37.651085
1967.396999	243313.410837	37.656103
1969.671749	243641.780823	37.661120
1972.106609	243966.544779	37.666138
1973.832848	244317.025660	37.671156
1976.016571	244639.392678	37.676173
1978.523277	244966.535339	37.681191
1980.411169	245294.945410	37.686208
1982.418916	245613.989785	37.691226
1984.684841	245936.194430	37.696244
1986.394104	246257.776920	37.701261
1988.537265	246590.162878	37.706279
1990.606131	246920.376915	37.711296
1992.731613	247236.612165	37.716314
1994.489639	247559.358273	37.721332
1996.391675	247887.314865	37.726349
1998.646284	248208.967545	37.731367
2000.191034	248531.165356	37.736384
2002.265509	248855.057886	37.741402
2004.566526	249197.661334	37.746420
2006.855206	249497.872566	37.751437
2009.246849	249789.406141	37.756455
2011.685682	250084.387358	37.761472
2013.983898	250355.996619	37.766490
2015.765730	250636.909023	37.771508
2017.616559	250907.548706	37.776525
2020.134770	251181.105736	37.781543
2021.550559	251466.980116	37.786560
2023.440235	251754.405496	37.791578
2025.036831	252035.984636	37.796596
2027.133305	252317.205499	37.801613
2029.195549	252613.520933	37.806631
2030.981269	252912.598725	37.811648
2033.083433	253193.464418	37.816666
2034.904917	253507.092804	37.821684
2036.781031	253801.026483	37.826701
2038.655878	254107.534830	37.831719
2040.468237	254428.253344	37.836736
2042.294964	254738.479018	37.841754
2044.376276	255063.093219	37.846772
2046.533653	255376.747516	37.851789
2048.831260	255700.820368	37.856807
2050.690225	256020.441700	37.861824
2052.659485	256334.660719	37.866842
2054.951249	256665.264360	37.871860
2057.011692	256978.758571	37.876877
2058.923133	257300.837478	37.881895
2061.046907	257637.083135	37.886912
2063.467663	257959.132967	37.891930
2065.382618	258288.528601	37.896948
2067.677003	258612.402938	37.901965
2069.600419	258938.444964	37.906983
2071.747522	259274.587581	37.912000
2074.314925	259592.018401	37.917018
2076.551839	259921.441302	37.922036
2078.313435	260246.900973	37.927053
2080.401559	260574.620883	37.932071
2082.735548	260905.096482	37.937088
2084.464583	261228.835066	37.942106
2086.586685	261570.166635	37.947124
2088.676994	261901.037649	37.952141
2090.833877	262228.494467	37.957159
2092.616009	262567.493193	37.962176
2095.081586	262905.621773	37.967194
2097.423713	263248.546039	37.972212
2099.117632	263579.608650	37.977229
2101.369021	263915.892377	37.982247
2103.464896	264259.949014	37.987264
2105.628007	264587.737332	37.992282
2107.672916	264929.821216	37.997300
2109.886399	265258.211776	38.002317
2112.176556	265598.504507	38.007335
2113.783312	265946.425241	38.012352
2115.767102	266277.037686	38.017370
2118.061124	266617.889453	38.022388
2120.291510	266960.301153	38.027405
2122.858512	267290.491548	38.032423
2125.223723	267594.879060	38.037440
2127.511207	267890.946805	38.042458
2129.701866	268188.884501	38.047476
2131.552271	268494.649720	38.052493
2133.647785	268788.208036	38.057511
2135.324339	269100.148720	38.062528
2137.179377	269407.768077	38.067546
2139.478853	269714.732800	38.072564
2141.346704	270040.513769	38.077581
2143.363999	270358.523146	38.082599
2145.231482	270691.823819	38.087616
2147.125857	271016.279976	38.092634
2149.061814	271355.234970	38.097652
2150.918515	271691.890931	38.102669
2153.799646	272036.208756	38.107687
2155.472811	272381.200918	38.112704
2157.886097	272736.135523	38.117722
2159.755802	273083.281358	38.122740
2161.943029	273441.020921	38.127757
2164.086473	273793.940833	38.132775
2166.340627	274153.473518	38.137792
2168.580131	274503.406065	38.142810
2170.883240	274869.485117	38.147828
2172.934495	275226.128644	38.152845
2175.501591	275582.207694	38.157863
2177.796773	275936.754842	38.162880
2180.089638	276289.879741	38.167898
2182.510255	276648.192043	38.172916
2184.629336	277007.339622	38.177933
2186.804155	277362.693195	38.182951
2189.335525	277718.980887	38.187968
2191.626287	278079.371198	38.192986
2193.679705	278438.274850	38.198004
2195.899038	278790.166157	38.203021
2197.940403	279147.445686	38.208039
2200.205924	279504.460911	38.213056
2202.405676	279864.331603	38.218074
2204.516731	280232.421486	38.223092
2206.750506	280596.478013	38.228109
2208.934361	280957.493881	38.233127
2210.992273	281323.788016	38.238144
2213.375745	281689.319029	38.243162
2215.844680	282049.171347	38.248180
2217.782309	282426.026258	38.253197
2220.062609	282786.212864	38.258215
2222.205403	283153.559333	38.263232
2224.699021	283526.286189	38.268250
2227.241749	283889.682007	38.273268
2229.099254	284267.589783	38.278285
2231.738719	284635.186589	38.283303
2233.557410	285008.882959	38.288320
2236.090428	285374.768586	38.293338
2238.569912	285731.212427	38.298356
2240.583872	286104.241727	38.303373
2242.945389	286453.285906	38.308391
2245.062463	286805.213641	38.313408
2247.829826	287119.568541	38.318426
2250.057882	287440.994473	38.323444
2252.206752	287784.939629	38.328461
2254.177257	288104.754556	38.333479
2256.606173	288437.096290	38.338496
2258.825121	288765.685934	38.343514
2260.999729	289088.998465	38.348532
2262.785609	289429.315922	38.353549
2265.340762	289767.580393	38.358567
2267.328315	290115.028618	38.363584
2269.521031	290466.152661	38.368602
2271.516975	290813.497043	38.373620
2273.566204	291170.815736	38.378637
2275.979029	291519.363196	38.383655
2278.086084	291889.220570	38.388672
2280.416893	292256.501656	38.393690
2282.687744	292621.530862	38.398708
2285.113841	292997.762750	38.403725
2287.236366	293352.551741	38.408743
2289.635007	293733.003551	38.413760
2291.765843	294101.583488	38.418778
2294.500298	294471.743641	38.423796
2296.600352	294849.573577	38.428813
2299.172042	295220.748893	38.433831
2301.475880	295606.368987	38.438848
2303.843310	295969.497436	38.443866
2306.217075	296344.359933	38.448884
2308.710139	296733.656497	38.453901
2311.106797	297105.872062	38.458919
2313.442222	297481.500437	38.463936
2315.708936	297866.867819	38.468954
2318.139160	298235.341693	38.473972
2320.392218	298614.638603	38.478989
2322.673186	298992.990399	38.484007
2324.828476	299379.820005	38.489024
2327.077277	299758.251397	38.494042
2329.794329	300142.831049	38.499060
2332.157725	300539.175902	38.504077
2334.378236	300913.138451	38.509095
2336.841008	301301.667442	38.514112
2339.055908	301692.393862	38.519130
2341.851625	302065.779836	38.524148
2344.049837	302453.153999	38.529165
2346.376482	302833.038899	38.534183
2348.860948	303217.215962	38.539200
2351.205894	303608.297762	38.544218
2353.913180	303980.956271	38.549236
2356.029319	304360.387900	38.554253
2358.585425	304744.549482	38.559271
2361.091682	305125.492018	38.564288
2363.198326	305512.618358	38.569306
2365.986586	305880.610594	38.574324
2368.203748	306252.451591	38.579341
2370.881080	306623.507383	38.584359
2373.254764	306982.951531	38.589376
2375.067808	307322.823801	38.594394
2377.487819	307671.641387	38.599412
2379.305769	308030.459447	38.604429
2381.270294	308373.098860	38.609447
2383.550821	308734.457745	38.614464
2385.851843	309108.004214	38.619482
2388.572697	309460.629795	38.624500
2390.589733	309837.825755	38.629517
2393.042645	310202.962818	38.634535
2395.509605	310578.180106	38.639552
2398.008967	310948.184156	38.644570
2400.751809	311331.102067	38.649588
2402.556429	311710.027307	38.654605
2405.145495	312093.906755	38.659623
2407.862244	312469.662331	38.664640
2410.042786	312859.344039	38.669658
2412.541427	313235.893502	38.674676
2414.980633	313624.337693	38.679693
2417.802097	314006.370201	38.684711
2420.007995	314397.337593	38.689728
2422.217203	314792.112763	38.694746
2424.853117	315180.748569	38.699764
2427.147774	315582.644097	38.704781
2429.719681	315973.903030	38.709799
2432.015901	316376.074511	38.714816
2434.035113	316782.377335	38.719834
2436.867159	317177.831739	38.724852
2439.275952	317593.060294	38.729869
2441.702343	317991.090035	38.734887
2444.377950	318405.358458	38.739904
2446.701289	318828.214431	38.744922
2449.446387	319225.629703	38.749940
2451.643038	319642.127314	38.754957
2454.078109	320036.769123	38.759975
2456.483577	320458.182351	38.764992
2458.944587	320868.765730	38.770010
2461.611898	321278.019289	38.775028
2464.301134	321696.715031	38.780045
2467.025198	322113.447719	38.785063
2469.743983	322513.849353	38.790080
2472.191224	322926.914110	38.795098
2474.894270	323323.784368	38.800116
2477.314356	323734.944786	38.805133
2479.753336	324131.954666	38.810151
2482.430627	324534.283401	38.815168
2484.918921	324950.658535	38.820186
2487.415278	325340.491928	38.825204
2490.006489	325738.231791	38.830221
2492.778445	326143.381871	38.835239
2495.334125	326542.520118	38.840256
2497.663936	326951.418446	38.845274
2500.352085	327336.005730	38.850292
2503.157155	327723.899309	38.855309
2505.896995	328101.744998	38.860327
2508.593751	328462.911447	38.865344
2510.661566	328821.331672	38.870362
2513.086495	329161.714451	38.875380
2515.762866	329521.431620	38.880397
2517.983997	329862.579950	38.885415
2520.426307	330217.556769	38.890432
2522.523766	330587.111793	38.895450
2525.060699	330938.540407	38.900468
2527.462649	331314.163399	38.905485
2529.372494	331688.161057	38.910503
2532.349774	332064.806301	38.915520
2534.127143	332456.723224	38.920538
2536.607662	332835.728491	38.925556
2538.862433	333238.611414	38.930573
2541.320762	333639.479137	38.935591
2543.709174	334046.119748	38.940608
2546.196658	334463.102386	38.945626
2548.840833	334862.029145	38.950644
2551.525145	335291.697084	38.955661
2553.974234	335714.467559	38.960679
2556.618976	336134.715981	38.965696
2559.052349	336556.391789	38.970714
2561.517539	336971.915135	38.975732
2564.288555	337405.973857	38.980749
2567.221407	337825.505710	38.985767
2570.000991	338248.029885	38.990784
2571.973485	338681.647995	38.995802
2575.048528	339102.824814	39.000820
2577.750396	339533.706353	39.005837
2579.970882	339962.122189	39.010855
2583.227507	340394.230255	39.015872
2585.741449	340831.251691	39.020890
2588.172615	341260.285381	39.025908
2590.586116	341698.611475	39.030925
2593.330211	342134.343115	39.035943
2596.171443	342569.015286	39.040960
2598.789231	343008.289757	39.045978
2601.706360	343443.476762	39.050996
2603.909247	343880.424003	39.056013
2606.567094	344315.036374	39.061031
2609.686501	344753.025229	39.066048
2611.795927	345191.399293	39.071066
2614.693601	345630.203718	39.076084
2617.115017	346070.501968	39.081101
2619.555772	346517.927673	39.086119
2622.509154	346959.734228	39.091136
2625.004498	347406.103420	39.096154
2627.817524	347850.768604	39.101172
2630.161047	348290.376511	39.106189
2632.927419	348741.337902	39.111207
2635.827596	349183.998483	39.116224
2638.323786	349630.755887	39.121242
2640.932483	350073.887020	39.126260
2643.829577	350520.878255	39.131277
2646.318818	350953.333740	39.136295
2649.115458	351367.764267	39.141312
2651.459867	351783.456310	39.146330
2653.873914	352187.127013	39.151348
2656.830049	352593.399548	39.156365
2659.349597	353011.059587	39.161383
2661.800901	353425.604830	39.166400
2664.313090	353849.554626	39.171418
2666.699623	354263.316527	39.176436
2669.430117	354694.636898	39.181453
2672.020800	355114.020165	39.186471
2674.989239	355544.940295	39.191488
2677.130924	355986.978559	39.196506
2679.840352	356428.618428	39.201524
2682.365922	356874.243206	39.206541
2685.054100	357323.797891	39.211559
2687.379815	357768.862504	39.216576
2689.921021	358226.782969	39.221594
2692.639364	358691.092656	39.226612
2695.366987	359167.148039	39.231629
2697.869135	359634.325671	39.236647
2700.682477	360099.850490	39.241664
2703.487754	360594.001440	39.246682
2706.080377	361059.831049	39.251700
2708.965945	361542.284437	39.256717
2711.336770	362036.996745	39.261735
2714.465122	362513.716615	39.266752
2716.928089	363009.495356	39.271770
2719.711890	363491.589418	39.276788
2722.397985	363987.576117	39.281805
2725.382854	364485.768819	39.286823
2728.671713	364960.103129	39.291840
2731.310220	365461.994448	39.296858
2734.300591	365943.395404	39.301876
2737.563281	366428.250151	39.306893
2740.156247	366917.875079	39.311911
2743.142393	367391.571789	39.316928
2746.190459	367871.318616	39.321946
2749.056019	368345.988458	39.326964
2752.016583	368833.046982	39.331981
2754.710343	369312.225057	39.336999
2757.665221	369773.593627	39.342016
2760.024022	370267.278155	39.347034
2762.811393	370737.290450	39.352052
2765.707038	371218.419876	39.357069
2768.248722	371695.666862	39.362087
2770.984300	372167.879050	39.367104
2773.891906	372659.418867	39.372122
2776.746166	373139.010436	39.377140
2779.943784	373623.109268	39.382157
2782.098075	374104.119903	39.387175
2785.396590	374580.528900	39.392192
2787.909823	375068.245871	39.397210
2790.327333	375553.587190	39.402228
2793.101675	376033.715744	39.407245
2795.395920	376524.595947	39.412263
2798.365441	376982.203236	39.417280
2801.155523	377447.546413	39.422298
2803.952991	377899.284392	39.427316
2806.599417	378350.863539	39.432333
2809.213347	378817.867560	39.437351
2811.634879	379278.934628	39.442368
2814.155634	379752.944256	39.447386
2816.412538	380234.473730	39.452404
2819.554255	380721.336752	39.457421
2821.817466	381217.947313	39.462439
2824.743183	381713.381092	39.467456
2827.173631	382227.329148	39.472474
2829.986105	382728.170960	39.477492
2832.745016	383245.604625	39.482509
2835.398705	383775.020878	39.487527
2838.424386	384302.189251	39.492544
2840.975974	384827.649608	39.497562
2843.958816	385365.311163	39.502580
2846.823361	385902.121194	39.507597
2849.476319	386450.700772	39.512615
2852.247319	386995.702406	39.517632
2855.092726	387548.623028	39.522650
2858.222199	388105.142589	39.527668
2861.205100	388660.941214	39.532685
2863.992438	389224.929007	39.537703
2866.607804	389779.550997	39.542720
2869.602877	390334.180288	39.547738
2872.518545	390898.704471	39.552756
2876.018613	391460.235884	39.557773
2878.734894	392034.435955	39.562791
2881.824105	392603.267186	39.567808
2884.872281	393163.422446	39.572826
2887.963736	393729.090129	39.577844
2891.240753	394287.567820	39.582861
2893.857289	394857.653785	39.587879
2896.901024	395413.690124	39.592896
2899.970631	395969.586426	39.597914
2903.285474	396525.257217	39.602932
2906.719180	397080.621040	39.607949
2909.562752	397635.130824	39.612967
2912.439800	398192.415222	39.617984
2915.419282	398745.997412	39.623002
2918.302208	399314.063464	39.628020
2920.927606	399855.918086	39.633037
2923.551079	400414.599382	39.638055
2927.049407	400972.802972	39.643072
2929.862211	401525.654391	39.648090
2932.730030	402095.144623	39.653108
2935.675573	402659.440464	39.658125
2938.508725	403214.439815	39.663143
2941.317648	403777.976852	39.668160
2944.070069	404351.196994	39.673178
2946.950876	404919.747148	39.678196
2949.931626	405486.521974	39.683213
2952.531165	406048.504979	39.688231
2955.508670	406578.933860	39.693248
2958.179037	407117.361864	39.698266
2960.692244	407674.690067	39.703284
2964.032545	408206.224854	39.708301
2966.981236	408751.829669	39.713319
2969.680039	409281.495437	39.718336
2972.440390	409831.749187	39.723354
2975.459286	410391.330133	39.728372
2978.153849	410952.219272	39.733389
2981.104239	411529.709336	39.738407
2984.060888	412093.424911	39.743424
2987.105994	412655.214931	39.748442
2989.831369	413228.272232	39.753460
2992.784882	413811.521012	39.758477
2995.834557	414396.263527	39.763495
2998.476384	414980.552005	39.768512
3001.602361	415581.908578	39.773530
3004.220331	416183.054275	39.778548
3007.559834	416787.367537	39.783565
3010.223300	417410.932304	39.788583
3013.396367	418016.842348	39.793600
3016.335359	418635.547467	39.798618
3018.665454	419261.582257	39.803636
3021.715022	419885.208846	39.808653
3025.312666	420527.281881	39.813671
3028.206048	421161.470456	39.818688
3031.752826	421782.822311	39.823706
3034.766135	422431.708598	39.828724
3038.163494	423057.159796	39.833741
3041.292686	423697.966590	39.838759
3044.539587	424329.695479	39.843776
3048.043864	424955.795608	39.848794
3050.848667	425588.578470	39.853812
3054.029384	426211.559417	39.858829
3057.098520	426845.258843	39.863847
3060.271674	427481.206578	39.868864
3063.291653	428109.133607	39.873882
3066.448430	428753.792456	39.878900
3069.931551	429377.056728	39.883917
3072.526120	430024.762271	39.888935
3075.608801	430660.673031	39.893952
3078.873473	431293.297578	39.898970
3082.095116	431937.158584	39.903988
3084.804210	432579.691712	39.909005
3087.742278	433228.883822	39.914023
3091.506453	433855.592285	39.919040
3094.357781	434504.993658	39.924058
3097.233002	435162.959346	39.929076
3100.594348	435799.711734	39.934093
3103.353832	436457.130255	39.939111
3106.287012	437106.249252	39.944128
3110.041681	437751.372652	39.949146
3113.046076	438407.966843	39.954164
3116.110423	439048.076433	39.959181
3119.306727	439685.920496	39.964199
3122.248552	440299.887806	39.969216
3125.189404	440895.307343	39.974234
3128.380408	441513.863234	39.979252
3131.487467	442114.391387	39.984269
3134.498232	442718.109693	39.989287
3137.320975	443324.931109	39.994304
3140.806993	443949.403093	39.999322
3143.789591	444562.800356	40.004340
3146.679018	445167.083852	40.009357
3149.619065	445808.047215	40.014375
3152.789001	446421.113831	40.019392
3156.060239	447051.360144	40.024410
3159.353665	447689.027368	40.029428
3162.577180	448328.915578	40.034445
3165.161824	448962.053858	40.039463
3168.218771	449619.801247	40.044480
3171.060689	450270.528452	40.049498
3174.043421	450941.511263	40.054516
3177.382816	451607.205005	40.059533
3180.425216	452291.247579	40.064551
3183.510381	452961.598339	40.069568
3186.707268	453647.853187	40.074586
3189.232905	454344.770171	40.079604
3192.595876	455031.412219	40.084621
3195.836863	455738.091495	40.089639
3198.550035	456443.263304	40.094656
3202.285169	457148.099371	40.099674
3205.223606	457876.061381	40.104692
3208.854994	458601.157611	40.109709
3211.838940	459324.005012	40.114727
3214.923038	460050.101340	40.119744
3218.462428	460763.301827	40.124762
3221.049820	461507.489468	40.129780
3224.799185	462238.416009	40.134797
3227.888765	462991.983784	40.139815
3231.027532	463741.672940	40.144832
3234.743476	464479.003482	40.149850
3237.718507	465232.105924	40.154868
3240.972542	465988.273483	40.159885
3243.973192	466741.217135	40.164903
3247.390407	467492.854196	40.169920
3250.516694	468245.875863	40.174938
3253.469759	469019.025545	40.179956
3257.090213	469778.033012	40.184973
3260.085210	470542.067334	40.189991
3263.747279	471313.906864	40.195008
3267.147920	472070.741081	40.200026
3270.563701	472846.354325	40.205044
3273.552451	473610.932808	40.210061
3277.244843	474377.140838	40.215079
3280.158201	475156.689030	40.220096
3283.940629	475907.101593	40.225114
3287.488416	476667.381125	40.230132
3291.217467	477420.273180	40.235149
3294.702922	478162.559954	40.240167
3297.495349	478881.575608	40.245184
3300.643659	479594.443382	40.250202
3303.933250	480301.905397	40.255220
3307.035460	480994.158388	40.260237
3310.374817	481719.099573	40.265255
3313.179612	482441.369289	40.270272
3316.362333	483151.878478	40.275290
3319.275896	483890.400412	40.280308
3322.810120	484619.902202	40.285325
3325.910543	485347.120511	40.290343
3328.539399	486105.915836	40.295360
3332.216711	486850.923522	40.300378
3335.159765	487612.792407	40.305396
3338.434619	488378.064302	40.310413
3341.860907	489146.565111	40.315431
3344.880329	489928.587367	40.320448
3348.076821	490701.456045	40.325466
3351.540716	491504.155026	40.330484
3354.735096	492297.517250	40.335501
3358.207940	493096.408128	40.340519
3361.538769	493891.296797	40.345536
3365.170198	494692.871378	40.350554
3368.348220	495500.240004	40.355572
3371.952940	496307.303487	40.360589
3375.719253	497119.305033	40.365607
3379.107576	497918.604803	40.370624
3383.049355	498726.062805	40.375642
3386.287600	499534.959098	40.380660
3389.582349	500346.637409	40.385677
3393.257130	501158.218764	40.390695
3396.440297	501977.868000	40.395712
3399.897938	502809.854765	40.400730
3402.791386	503630.583904	40.405748
3406.042221	504464.746438	40.410765
3409.589667	505301.699523	40.415783
3412.494106	506133.263045	40.420800
3416.048839	506984.064873	40.425818
3419.423046	507832.380544	40.430836
3422.924652	508692.746239	40.435853
3426.474011	509536.408453	40.440871
3429.606707	510399.875696	40.445888
3433.231598	511252.372946	40.450906
3436.843108	512121.530472	40.455924
3440.256752	512972.814281	40.460941
3443.842679	513832.503665	40.465959
3447.489024	514713.075519	40.470976
3450.989972	515555.537807	40.475994
3454.360956	516431.724435	40.481012
3457.653400	517298.394592	40.486029
3461.572121	518153.571995	40.491047
3464.895953	519012.733082	40.496064
3468.756906	519864.653460	40.501082
3472.415195	520733.354704	40.506100
3476.476510	521567.504381	40.511117
3480.597536	522384.347657	40.516122
3483.687951	523169.088224	40.521127
3486.995781	523883.847447	40.526132
3489.723202	524562.323671	40.531136
3492.704905	525168.704883	40.536141
3495.699587	525708.091632	40.541146
3497.901013	526205.332904	40.546151
3500.588935	526635.364586	40.551156
3503.045337	527012.709185	40.556160
3505.090952	527336.337471	40.561165
3506.847526	527607.092602	40.566170
3508.422827	527831.833193	40.571175
3510.195488	527996.048107	40.576180
3512.000014	528149.340646	40.581184
3512.785707	528241.493807	40.586189
3514.072659	528291.522219	40.591194
3515.158991	528318.487785	40.596199
3515.979072	528301.631175	40.601204
3516.560840	528273.896664	40.606208
3517.251301	528220.018283	40.611213
3517.799487	528141.955777	40.616218
3518.407266	528042.557418	40.621223
3519.422364	527918.129251	40.626228
3519.828913	527779.494458	40.631232
3520.289083	527627.306066	40.636237
3520.869249	527442.601606	40.641242
3520.850389	527252.026170	40.646247
3521.474491	527053.260621	40.651252
3521.496598	526837.303231	40.656256
3521.639239	526607.627462	40.661261
3521.600590	526376.814600	40.666266
3521.775717	526141.567486	40.671271
3521.884279	525897.735210	40.676276
3522.044571	525654.598651	40.681280
3521.600691	525400.737465	40.686285
3521.842295	525134.986962	40.691290
3521.685871	524879.555752	40.696295
3521.509986	524616.288847	40.701300
3521.684920	524347.806357	40.706304
3521.400318	524076.561322	40.711309
3521.445233	523813.398044	40.716314
3521.117987	523548.570601	40.721319
3521.043474	523268.988611	40.726324
3520.834374	523007.975498	40.731328
3520.273293	522745.092819	40.736333
3520.468940	522474.958272	40.741338
3520.256362	522216.056198	40.746343
3520.065029	521951.535053	40.751348
3519.797759	521692.633288	40.756352
3519.814396	521436.260916	40.761357
3519.791265	521173.722813	40.766362
3519.158106	520927.708272	40.771367
3518.932888	520666.457905	40.776372
3518.854891	520414.938106	40.781376
3518.468117	520170.743941	40.786381
3518.497132	519914.598553	40.791386
3518.079236	519675.811981	40.796391
3518.300010	519449.207708	40.801396
3517.887316	519213.295660	40.806400
3517.956315	518968.050874	40.811405
3517.557820	518723.280846	40.816410
3517.317990	518501.893950	40.821415
3517.120892	518260.675377	40.826420
3516.723755	518035.362923	40.831424
3516.724324	517824.851413	40.836429
3516.359023	517594.319460	40.841434
3516.047995	517377.075357	40.846439
3515.958570	517171.980653	40.851444
3515.781611	516958.452027	40.856448
3515.246617	516756.052260	40.861453
3515.547059	516558.018843	40.866458
3514.966395	516360.931486	40.871463
3514.918249	516155.918871	40.876468
3514.783865	515962.650361	40.881472
3514.471969	515777.094887	40.886477
3514.468358	515580.513987	40.891482
3513.904533	515400.304456	40.896487
3513.836249	515223.908973	40.901492
3513.792834	515043.360468	40.906496
3513.717556	514868.075015	40.911501
3513.482636	514696.201625	40.916506
3513.123547	514527.127867	40.921511
3512.982274	514355.691387	40.926516
3513.251075	514186.616116	40.931520
3513.026105	514031.931071	40.936525
3512.912559	513862.761241	40.941530
3512.802427	513711.191030	40.946535
3512.131732	513549.339053	40.951540
3511.994546	513389.424438	40.956544
3512.028330	513245.616766	40.961549
3511.971561	513089.733114	40.966554
3511.810769	512950.404888	40.971559
3511.789792	512794.057612	40.976564
3511.692466	512661.039816	40.981568
3511.631647	512523.310933	40.986573
3511.196050	512378.457236	40.991578
3510.820480	512243.861453	40.996583
3510.989899	512110.240744	41.001588
3510.984049	511986.004947	41.006592
3510.709371	511861.102533	41.011597
3510.720137	511726.239239	41.016602
3510.385374	511602.558484	41.021607
3510.409938	511475.886006	41.026612
3510.464882	511355.682929	41.031616
3510.339010	511229.234742	41.036621
3510.084714	511111.405840	41.041626
3509.990995	511002.656604	41.046631
3509.872058	510882.781202	41.051636
3509.587205	510772.037167	41.056640
3509.536809	510662.165960	41.061645
3509.841259	510543.435395	41.066650
3509.502016	510438.566171	41.071655
3509.285406	510338.280618	41.076660
3509.383375	510221.199333	41.081664
3509.278941	510123.626673	41.086669
3509.066574	510018.178319	41.091674
3508.733601	509925.952711	41.096679
3509.137802	509809.781446	41.101684
3508.901475	509727.354269	41.106688
3508.411490	509635.202504	41.111693
3508.656809	509537.115894	41.116698
3508.653232	509451.817427	41.121703
3508.537347	509365.271464	41.126708
3508.789582	509269.357729	41.131712
3508.618019	509179.885225	41.136717
3508.690428	509085.719066	41.141722
3508.592013	508994.210283	41.146727
3508.590157	508901.876242	41.151732
3508.288120	508815.913473	41.156736
3508.015977	508732.728264	41.161741
3508.230087	508649.668177	41.166746
3507.994852	508563.693590	41.171751
3508.066896	508480.199784	41.176756
3507.996691	508397.183419	41.181760
3507.575337	508323.127057	41.186765
3508.095458	508252.058535	41.191770
3507.877927	508175.945476	41.196775
3507.812883	508087.007019	41.201780
3507.955820	508010.583273	41.206784
3507.539144	507933.235697	41.211789
3507.900198	507847.011500	41.216794
3507.301396	507790.082812	41.221799
3507.642110	507709.376278	41.226804
3507.242270	507634.352202	41.231808
3507.195281	507564.230657	41.236813
3507.264557	507501.376625	41.241818
3507.051706	507444.739986	41.246823
3507.050593	507368.993956	41.251828
3506.944338	507315.932562	41.256832
3506.659128	507234.209569	41.261837
3506.973573	507183.813632	41.266842
3506.681301	507121.015366	41.271847
3506.744716	507052.493485	41.276852
3506.592070	507002.676846	41.281856
3506.485666	506932.764537	41.286861
3506.880821	506883.417573	41.291866
3506.479784	506832.981905	41.296871
3506.268340	506770.422596	41.301876
3506.470931	506722.522427	41.306880
3506.401851	506672.590431	41.311885
3506.530563	506610.128584	41.316890
3506.575359	506556.534983	41.321895
3506.560687	506506.391506	41.326900
3506.471251	506447.455044	41.331904
3506.278261	506395.517778	41.336909
3506.483240	506337.040425	41.341914
3506.136581	506296.563158	41.346919
3506.084336	506229.979188	41.351924
3506.584564	506184.611203	41.356928
3506.085538	506134.644416	41.361933
3505.972357	506083.857461	41.366938
3505.539446	506046.935423	41.371943
3506.053801	505989.015234	41.376948
3505.908739	505961.864464	41.381952
3506.045067	505904.307362	41.386957
3506.222959	505843.859115	41.391962
3506.044716	505817.016983	41.396967
3505.722324	505760.645184	41.401972
3505.851304	505712.956289	41.406976
3505.657231	505672.149831	41.411981
3506.182723	505633.405510	41.416986
3505.804454	505589.591741	41.421991
3505.565294	505542.466607	41.426996
3505.775616	505507.516527	41.432000
3506.042799	505474.328540	41.437005
3505.669224	505431.626927	41.442010
3505.754334	505382.729558	41.447015
3505.632888	505345.098945	41.452020
3505.830168	505302.711626	41.457024
3505.494702	505261.724137	41.462029
3505.594074	505216.518209	41.467034
3505.448949	505165.430000	41.472039
3505.603511	505135.902747	41.477044
3505.562741	505091.781358	41.482048
3505.524709	505057.426293	41.487053
3505.919829	505008.124639	41.492058
3505.540927	504982.982928	41.497063
3505.336569	504940.050944	41.502068
3505.631474	504905.339322	41.507072
3505.545148	504866.993646	41.512077
3505.540215	504826.762591	41.517082
3505.463440	504795.449507	41.522087
3505.562578	504758.187616	41.527092
3505.356400	504717.380843	41.532096
3505.289178	504686.774545	41.537101
3505.315106	504646.588806	41.542106
3505.244544	504610.922233	41.547111
3505.322406	504578.066114	41.552116
3505.505993	504539.980701	41.557120
3505.021003	504507.972520	41.562125
3505.185668	504477.683456	41.567130
3505.206135	504445.139803	41.572135
3505.300313	504409.699819	41.577140
3505.223690	504377.525638	41.582144
3504.981527	504336.217591	41.587149
3505.652165	504312.832116	41.592154
3505.286043	504268.962512	41.597159
3505.020701	504237.475805	41.602164
3505.251061	504206.315555	41.607168
3505.362272	504176.692325	41.612173
3505.535506	504136.583352	41.617178
3505.272085	504096.492697	41.622183
3505.298462	504073.967861	41.627188
3505.269232	504044.619648	41.632192
3505.326571	504013.132145	41.637197
3505.665062	503965.506598	41.642202
3505.407935	503940.546577	41.647207
3505.333116	503904.373154	41.652212
3505.054149	503869.497149	41.657216
3505.289804	503832.211716	41.662221
3505.379340	503794.949301	41.667226
3505.017644	503766.513529	41.672231
3505.076585	503740.187426	41.677236
3505.350248	503707.298732	41.682240
3505.154007	503683.695177	41.687245
3505.246065	503647.039364	41.692250
3504.972892	503617.931435	41.697255
3504.989603	503582.856297	41.702260
3505.362793	503553.494269	41.707264
3504.854127	503521.943520	41.712269
3505.214259	503479.475453	41.717274
3505.261060	503460.792969	41.722279
3505.060247	503415.022531	41.727284
3505.132666	503385.353491	41.732288
3505.055275	503364.463681	41.737293
3505.401997	503327.766952	41.742298
3505.174497	503299.663488	41.747303
3504.796739	503261.410983	41.752308
3505.223882	503236.949137	41.757312
3505.276496	503205.663381	41.762317
3505.423127	503174.868819	41.767322
3504.766924	503151.185419	41.772327
3504.891965	503103.135782	41.777332
3505.231688	503082.736432	41.782336
3505.025681	503045.468536	41.787341
3505.182097	503020.087566	41.792346
3504.976006	502992.435731	41.797351
3505.031576	502962.363752	41.802356
3505.039069	502928.604671	41.807360
3504.957504	502903.919102	41.812365
3504.927508	502869.406658	41.817370
3504.952600	502850.726961	41.822375
3504.964419	502814.841280	41.827380
3504.538016	502787.679455	41.832384
3504.755183	502765.122792	41.837389
3505.002893	502739.929439	41.842394
3504.887762	502715.501973	41.847399
3504.768860	502682.875871	41.852404
3504.668040	502661.432196	41.857408
3504.942751	502649.089993	41.862413
3505.335229	502612.637612	41.867418
3505.259041	502586.128697	41.872423
3505.048527	502553.162547	41.877428
3505.036165	502522.290754	41.882432
3504.918246	502496.395655	41.887437
3505.055777	502463.576778	41.892442
3505.190318	502430.859539	41.897447
3504.916898	502398.965919	41.902452
3504.840592	502382.123828	41.907456
3504.573603	502343.649373	41.912461
3504.736429	502332.589969	41.917466
3504.782095	502310.565968	41.922471
3504.668288	502270.852422	41.927476
3504.916514	502251.833144	41.932480
3504.661596	502228.591212	41.937485
3504.593125	502199.246134	41.942490
3504.718347	502169.263027	41.947495
3504.726305	502156.304666	41.952500
3504.788237	502131.139812	41.957504
3504.550400	502119.333781	41.962509
3504.746946	502081.848385	41.967514
3504.563902	502058.493642	41.972519
3504.540766	502045.843799	41.977524
3505.066384	502014.481176	41.982528
3504.911092	501994.614345	41.987533
3504.907482	501960.602103	41.992538
3504.778676	501939.819966	41.997543
3504.903229	501915.910271	42.002548
3504.835142	501889.145961	42.007552
3504.679632	501876.567535	42.012557
3504.929302	501823.736953	42.017562
3504.757625	501821.739534	42.022567
3504.984512	501794.574154	42.027572
3505.219602	501748.021895	42.032576
3504.818181	501731.078728	42.037581
3504.746974	501695.760672	42.042586
3504.757506	501673.842665	42.047591
3504.729280	501645.502615	42.052596
3504.977675	501618.637259	42.057600
3504.772737	501601.257989	42.062605
3504.749407	501562.338403	42.067610
3504.847607	501550.529494	42.072615
3504.871652	501512.564008	42.077620
3504.712936	501498.517966	42.082624
3504.562574	501468.020461	42.087629
3504.894846	501451.315370	42.092634
3504.601640	501422.206993	42.097639
3504.862611	501387.038283	42.102644
3505.023552	501364.286265	42.107648
3504.465397	501341.951575	42.112653
3504.842893	501312.382694	42.117658
3504.569225	501284.030246	42.122663
3504.535318	501271.887719	42.127668
3504.944375	501247.628460	42.132672
3504.394801	501233.795837	42.137677
3504.938304	501196.203119	42.142682
3505.122573	501179.217468	42.147687
3504.585291	501158.144663	42.152692
3504.817057	501119.791190	42.157696
3504.567632	501106.569045	42.162701
3504.757732	501073.789910	42.167706
3504.659620	501050.774737	42.172711
3504.381659	501030.824984	42.177716
3504.866797	501002.605236	42.182720
3504.228136	500985.243300	42.187725
3504.727280	500971.852119	42.192730
3504.627165	500945.547006	42.197735
3504.626659	500924.540934	42.202740
3504.744988	500886.660446	42.207744
3504.578874	500879.397823	42.212749
3504.928135	500840.114064	42.217754
3504.901342	500829.842962	42.222759
3504.737905	500800.814292	42.227764
3505.161478	500755.191385	42.232768
3504.578657	500743.034023	42.237773
3505.006082	500718.771143	42.242778
3504.593896	500692.211275	42.247783
3504.636974	500672.210377	42.252788
3504.480852	500646.014911	42.257792
3504.283345	500636.985516	42.262797
3504.464643	500609.319355	42.267802
3504.066569	500584.781826	42.272807
3504.409393	500569.795266	42.277812
3504.376889	500559.322438	42.282816
3504.410865	500543.625397	42.287821
3504.100043	500521.604911	42.292826
3504.346932	500500.812329	42.297831
3504.505614	500493.498212	42.302836
3504.586671	500455.167133	42.307840
3504.621714	500447.973777	42.312845
3504.749376	500419.354045	42.317850
3504.677314	500402.408171	42.322855
3504.546472	500382.181343	42.327860
3504.735498	500368.737492	42.332864
3504.411703	500336.645659	42.337869
3504.601785	500310.850551	42.342874
3504.486656	500294.012620	42.347879
3504.776296	500271.694440	42.352884
3504.874317	500241.813628	42.357888
3504.401978	500234.295429	42.362893
3504.893362	500199.138581	42.367898
3504.701537	500173.909835	42.372903
3504.535313	500147.209039	42.377908
3504.754650	500125.154887	42.382912
3504.321874	500107.658313	42.387917
3504.651124	500084.776824	42.392922
3504.635490	500061.393000	42.397927
3504.729502	500035.055862	42.402932
3504.768390	500013.181954	42.407936
3504.622021	499987.388941	42.412941
3504.954746	499960.507763	42.417946
3504.598435	499939.101190	42.422951
3504.439876	499911.538289	42.427956
3504.396322	499888.715475	42.432960
3504.603365	499876.432673	42.437965
3504.620978	499856.434889	42.442970
3504.597209	499846.010882	42.447975
3504.507870	499809.072104	42.452980
3504.405016	499789.447629	42.457984
3504.375720	499776.645289	42.462989
3504.505702	499751.466323	42.467994
3504.348210	499731.141731	42.472999
3504.419728	499706.630013	42.478004
3504.765624	499694.578244	42.483008
3504.696235	499674.847113	42.488013
3504.369301	499647.512902	42.493018
3504.575710	499636.191835	42.498023
3504.418203	499608.932028	42.503028
3504.607752	499578.883781	42.508032
3504.140607	499576.780946	42.513037
3504.634127	499542.179307	42.518042
3504.285278	499535.400612	42.523047
3504.189387	499521.039355	42.528052
3504.536839	499495.876279	42.533056
3504.514021	499484.641970	42.538061
3504.364531	499456.621343	42.543066
3504.626880	499446.556853	42.548071
3504.366945	499413.845812	42.553076
3504.577146	499396.145668	42.558080
3504.151136	499376.622441	42.563085
3504.769312	499348.581552	42.568090
3504.722199	499330.517040	42.573095
3504.724567	499307.686229	42.578100
3504.583375	499285.434922	42.583104
3504.397092	499272.049571	42.588109
3504.406325	499245.775298	42.593114
3504.178949	499226.979843	42.598119
3504.348167	499218.246121	42.603124
3504.683932	499188.022244	42.608128
3504.361534	499181.644211	42.613133
3504.421551	499148.629004	42.618138
3504.830718	499136.212505	42.623143
3504.437188	499113.646513	42.628148
3504.736477	499099.475569	42.633152
3504.512244	499068.327554	42.638157
3504.750701	499047.028396	42.643162
3504.646061	499029.478902	42.648167
3504.506509	498994.621915	42.653172
3504.669938	498972.524563	42.658176
3504.327302	498966.453390	42.663181
3504.311523	498930.007406	42.668186
3504.533646	498915.747269	42.673191
3504.606470	498886.728776	42.678196
3504.504719	498869.229291	42.683200
3504.392848	498854.414419	42.688205
3504.401282	498820.495546	42.693210
3504.551279	498814.953935	42.698215
3504.168923	498790.006474	42.703220
3504.466142	498772.646327	42.708224
3504.226395	498746.663796	42.713229
3504.318182	498735.714646	42.718234
3504.548657	498713.859497	42.723239
3504.259929	498695.680667	42.728244
3504.627766	498682.004797	42.733248
3504.297810	498659.883799	42.738253
3504.452788	498641.736030	42.743258
3504.495936	498619.100395	42.748263
3504.328941	498607.483335	42.753268
3504.533782	498587.150802	42.758272
3504.664516	498561.463813	42.763277
3504.487507	498534.661075	42.768282
3504.477701	498516.994843	42.773287
3504.766456	498491.586523	42.778292
3504.513349	498470.668127	42.783296
3504.454564	498453.212071	42.788301
3504.634076	498427.618430	42.793306
3504.384556	498414.546182	42.798311
3504.340069	498388.076651	42.803316
3504.671151	498377.595706	42.808321
3504.417291	498357.183542	42.813325
3504.553116	498338.329751	42.818330
3504.124590	498313.135802	42.823335
3504.457983	498280.177044	42.828340
3504.517906	498275.763251	42.833345
3504.091268	498248.341421	42.838349
3504.207917	498244.627403	42.843354
3504.033899	498213.925597	42.848359
3503.981674	498208.668888	42.853364
3504.387701	498192.151612	42.858369
3504.118777	498179.386011	42.863373
3504.168086	498158.166326	42.868378
3504.146536	498153.866632	42.873383
3504.032615	498131.407087	42.878388
3504.022159	498110.298043	42.883393
3503.861925	498108.045269	42.888397
3503.967219	498101.295498	42.893402
3504.094960	498085.834617	42.898407
3503.900265	498070.019684	42.903412
3504.364215	498066.301360	42.908417
3504.454048	498055.149605	42.913421
3504.313861	498028.846549	42.918426
3504.158990	498017.834700	42.923431
3504.023896	497993.302682	42.928436
3504.412038	497976.686785	42.933441
3503.799252	497970.101091	42.938445
3504.275437	497935.195358	42.943450
3504.448294	497931.067386	42.948455
3504.090532	497921.353191	42.953460
3504.448533	497906.767027	42.958465
3504.260064	497893.532873	42.963469
3504.220789	497866.757999	42.968474
3504.111857	497855.080651	42.973479
3504.285303	497838.042928	42.978484
3504.222462	497818.511231	42.983489
3504.039855	497807.149254	42.988493
3504.214153	497789.453211	42.993498
3504.168298	497763.793000	42.998503
3504.252452	497756.185796	43.003508
3503.967414	497748.231932	43.008513
3504.090646	497733.277726	43.013517
3503.929296	497723.228621	43.018522
3504.398588	497721.534438	43.023527
3504.133243	497698.288267	43.028532
3504.242019	497672.350354	43.033537
3504.215564	497656.508466	43.038541
3504.354029	497631.122693	43.043546
3504.174441	497628.467905	43.048551
3504.040030	497609.858575	43.053556
3504.212860	497589.327473	43.058561
3504.031358	497569.966144	43.063565
3504.171187	497560.223732	43.068570
3503.990755	497537.976470	43.073575
3504.278214	497536.665399	43.078580
3504.369353	497517.210293	43.083585
3504.145569	497502.462627	43.088589
3504.216933	497492.731000	43.093594
3504.217111	497478.909828	43.098599
3504.189977	497449.550437	43.103604
3504.283267	497437.587721	43.108609
3504.063704	497430.990302	43.113613
3504.297185	497408.373694	43.118618
3504.080143	497403.649075	43.123623
3503.981332	497388.020899	43.128628
3504.281513	497351.623043	43.133633
3503.888531	497352.900254	43.138637
3503.845926	497341.920875	43.143642
3504.058633	497319.155557	43.148647
3503.997194	497303.825166	43.153652
3504.139957	497307.346567	43.158657
3503.767170	497293.837343	43.163661
3504.386943	497267.159922	43.168666
3504.028532	497257.799866	43.173671
3503.882211	497249.013814	43.178676
3504.049033	497218.610838	43.183681
3503.865905	497216.260315	43.188685
3504.131991	497211.914933	43.193690
3504.203257	497196.006569	43.198695
3504.208763	497182.336213	43.203700
3504.642342	497165.813648	43.208705
3504.266448	497151.950414	43.213709
3504.124945	497121.950406	43.218714
3504.330344	497126.069479	43.223719
3504.087345	497099.325671	43.228724
3504.045748	497074.170092	43.233729
3504.004291	497074.733592	43.238733
3504.230676	497049.586250	43.243738
3504.055999	497043.285364	43.248743
3504.044789	497030.275703	43.253748
3503.854690	497008.130575	43.258753
3503.740157	497015.692342	43.263757
3504.005429	496999.297486	43.268762
3504.119705	496997.912495	43.273767
3503.965476	496972.015151	43.278772
3504.158138	496965.706805	43.283777
3503.934783	496965.489004	43.288781
3504.171969	496944.845745	43.293786
3504.182673	496920.137342	43.298791
3503.950254	496911.516621	43.303796
3504.182562	496897.000143	43.308801
3503.740526	496882.792756	43.313805
3504.047407	496875.453751	43.318810
3504.080128	496871.145173	43.323815
3503.861759	496846.928537	43.328820
3504.285384	496831.571706	43.333825
3504.003232	496833.793383	43.338829
3504.115980	496813.220272	43.343834
3504.471125	496794.735241	43.348839
3504.296354	496775.928918	43.353844
3504.185376	496746.480384	43.358849
3504.058841	496745.032179	43.363853
3504.200825	496730.124811	43.368858
3504.162211	496721.321479	43.373863
3504.147682	496700.059549	43.378868
3504.298851	496685.150694	43.383873
3504.336484	496674.664521	43.388877
3503.980283	496653.102136	43.393882
3504.403754	496647.466010	43.398887
3504.261118	496612.858066	43.403892
3504.205707	496599.146270	43.408897
3503.986297	496590.422081	43.413901
3504.099598	496565.848869	43.418906
3504.097633	496566.659291	43.423911
3504.074137	496545.702376	43.428916
3504.225642	496526.489816	43.433921
3504.156973	496511.362417	43.438925
3504.119277	496504.330876	43.443930
3504.402571	496477.705486	43.448935
3504.100937	496467.070299	43.453940
3504.410092	496452.490691	43.458945
3504.037959	496434.829068	43.463949
3504.152870	496433.747714	43.468954
3504.208661	496407.765740	43.473959
3503.983662	496385.372218	43.478964
3504.068869	496376.802299	43.483969
3504.041457	496374.427053	43.488973
3504.114900	496346.366366	43.493978
3504.232689	496330.804304	43.498983
3504.002772	496328.511690	43.503988
3504.100192	496304.598830	43.508993
3503.916965	496302.400094	43.513997
3504.018571	496290.485940	43.519002
3504.019984	496282.384893	43.524007
3504.114902	496250.877798	43.529012
3504.336072	496237.425795	43.534017
3504.111114	496237.106977	43.539021
3504.249848	496210.048370	43.544026
3504.169083	496209.453607	43.549031
3504.475289	496179.735693	43.554036
3504.067844	496151.700085	43.559041
3504.262607	496152.327538	43.564045
3504.243939	496125.951886	43.569050
3504.490690	496114.217197	43.574055
3503.782595	496102.785318	43.579060
3504.070180	496077.880116	43.584065
3504.328766	496074.143221	43.589069
3504.137462	496061.414488	43.594074
3504.310408	496041.337301	43.599079
3504.320925	496026.399507	43.604084
3504.366143	496008.215823	43.609089
3504.005081	495992.121586	43.614093
3504.016913	495985.942747	43.619098
3504.171009	495960.906591	43.624103
3504.309471	495945.644721	43.629108
3504.183506	495938.272494	43.634113
3504.350258	495916.829102	43.639117
3504.185389	495900.096196	43.644122
3504.163663	495881.517916	43.649127
3503.907637	495864.394334	43.654132
3504.351720	495841.438703	43.659137
3504.039226	495847.260138	43.664141
3504.131701	495828.309331	43.669146
3504.266526	495805.908855	43.674151
3504.207654	495801.867660	43.679156
3504.463746	495775.346809	43.684161
3504.339953	495767.214692	43.689165
3504.242132	495744.395226	43.694170
3504.328628	495728.179382	43.699175
3504.061013	495713.437190	43.704180
3504.354965	495675.720541	43.709185
3503.915581	495677.106463	43.714189
3503.908411	495666.829321	43.719194
3503.942438	495655.482386	43.724199
3504.156176	495642.537443	43.729204
3504.100817	495626.850252	43.734209
3504.039559	495620.733474	43.739213
3504.086828	495607.662922	43.744218
3504.180386	495594.028088	43.749223
3504.060530	495595.110349	43.754228
3504.196158	495568.962665	43.759233
3504.112963	495550.545660	43.764237
3504.320840	495538.259791	43.769242
3504.478710	495512.564203	43.774247
3504.037375	495507.418848	43.779252
3504.133204	495492.872194	43.784257
3504.153310	495469.729950	43.789261
3504.040543	495449.950437	43.794266
3504.198414	495459.039405	43.799271
3504.122055	495428.368086	43.804276
3504.360057	495413.444467	43.809281
3503.805090	495405.279076	43.814285
3503.929996	495381.461928	43.819290
3504.273867	495366.774703	43.824295
3504.149302	495364.870378	43.829300
3504.170649	495330.993577	43.834305
3504.023325	495328.789048	43.839309
3503.936836	495322.321727	43.844314
3504.103150	495306.599223	43.849319
3504.120600	495286.849585	43.854324
3504.704615	495269.440767	43.859329
3504.358219	495246.305537	43.864333
3504.123416	495233.076768	43.869338
3504.102455	495220.928123	43.874343
3503.973759	495199.986291	43.879348
3504.149707	495188.009034	43.884353
3504.052030	495182.049766	43.889357
3503.965184	495153.354347	43.894362
3504.317418	495144.336575	43.899367
3503.944979	495144.851183	43.904372
3504.433431	495119.811662	43.909377
3503.822464	495096.566160	43.914381
3504.145134	495103.249474	43.919386
3504.264475	495088.496248	43.924391
3504.131024	495058.947275	43.929396
3504.035255	495043.772310	43.934401
3503.949193	495051.836727	43.939405
3504.114176	495028.012786	43.944410
3503.953348	495015.278505	43.949415
3503.785972	495007.406109	43.954420
3504.220968	494988.096489	43.959425
3504.415524	494966.900761	43.964429
3503.881128	494962.985177	43.969434
3504.043903	494946.300878	43.974439
3504.005197	494922.458361	43.979444
3504.327892	494910.761533	43.984449
3504.089813	494906.292759	43.989453
3503.986336	494876.232411	43.994458
3504.094339	494861.582064	43.999463
3503.778325	494863.252349	44.004468
3504.143222	494840.105446	44.009473
3503.758853	494825.178454	44.014477
3503.352444	494805.697830	44.019482
3503.628878	494803.375623	44.024487
3503.799393	494804.057592	44.029492
3503.856438	494810.327288	44.034497
3503.952924	494785.298631	44.039501
3503.886862	494771.283339	44.044506
3503.766777	494762.593209	44.049511
3503.620999	494773.857166	44.054516
3503.660103	494762.407607	44.059521
3503.856725	494746.933007	44.064525
3503.520077	494739.391058	44.069530
3503.783505	494733.374567	44.074535
3504.075024	494720.214140	44.079540
3504.190874	494707.587818	44.084545
3503.998836	494697.238083	44.089549
3504.093524	494694.539511	44.094554
3504.068191	494677.631527	44.099559
3503.951496	494666.966056	44.104564
3504.190655	494642.066558	44.109569
3504.141057	494628.402999	44.114573
3503.814063	494615.087085	44.119578
3503.879273	494590.012471	44.124583
3504.117566	494592.354692	44.129588
3503.861104	494582.217615	44.134593
3503.447336	494589.068156	44.139597
3503.430789	494565.171036	44.144602
3504.056013	494546.033426	44.149607
3503.609016	494548.838418	44.154612
3503.801328	494538.630383	44.159617
3504.103309	494540.608098	44.164621
3503.595808	494519.978539	44.169626
3503.761436	494507.192305	44.174631
3503.885764	494504.489021	44.179636
3503.714919	494490.490076	44.184641
3503.900524	494499.929585	44.189645
3503.910719	494496.231633	44.194650
3504.211532	494463.929388	44.199655
3503.978228	494461.080083	44.204660
3503.932085	494450.403335	44.209665
3504.119141	494431.081686	44.214669
3504.154760	494409.100268	44.219674
3503.929554	494408.528276	44.224679
3503.935729	494395.108905	44.229684
3504.106107	494368.802111	44.234689
3503.799178	494369.357020	44.239693
3503.815816	494369.810149	44.244698
3504.224127	494350.453444	44.249703
3503.863418	494338.256644	44.254708
3503.664120	494321.831551	44.259713
3503.763584	494319.486620	44.264717
3503.632856	494322.494834	44.269722
3503.788102	494302.671720	44.274727
3503.868702	494289.696232	44.279732
3504.107657	494270.163667	44.284737
3503.766793	494277.863611	44.289741
3503.683076	494273.522190	44.294746
3503.827925	494239.725125	44.299751
3503.786624	494231.832467	44.304756
3503.926750	494226.696114	44.309761
3503.593318	494232.622638	44.314765
3503.825569	494227.674268	44.319770
3504.009404	494205.010910	44.324775
3503.619389	494196.109996	44.329780
3503.985767	494181.468903	44.334785
3503.627625	494181.829367	44.339789
3503.618815	494180.362348	44.344794
3504.059029	494176.545725	44.349799
3503.817817	494160.380294	44.354804
3503.881030	494155.407986	44.359809
3503.735258	494155.279156	44.364813
3503.966858	494150.685322	44.369818
3503.433699	494120.235927	44.374823
3503.358383	494111.386503	44.379828
3503.803144	494095.618952	44.384833
3503.641824	494100.708132	44.389837
3503.507007	494101.691571	44.394842
3503.807904	494099.618592	44.399847
3503.804303	494100.378745	44.404852
3503.949516	494073.619779	44.409857
3503.953737	494061.263841	44.414861
3504.184471	494051.657102	44.419866
3504.211952	494041.373572	44.424871
3503.938178	494026.479084	44.429876
3504.223087	494008.154258	44.434881
3503.819420	494015.509780	44.439885
3503.798783	493992.118929	44.444890
3503.969574	493974.672931	44.449895
3503.941310	493974.221706	44.454900
3504.163479	493963.046534	44.459905
3503.882545	493940.658861	44.464909
3503.929097	493928.042957	44.469914
3504.157858	493922.689962	44.474919
3504.045231	493927.366397	44.479924
3504.053204	493892.881414	44.484929
3503.854038	493880.051132	44.489933
3503.871346	493876.959575	44.494938
3504.078132	493870.749208	44.499943
3503.795161	493850.184680	44.504948
3504.073556	493834.139381	44.509953
3503.830833	493834.177784	44.514957
3503.720955	493819.510408	44.519962
3503.718718	493799.863557	44.524967
3503.584690	493791.428357	44.529972
3504.180719	493782.371386	44.534977
3503.923447	493792.438271	44.539981
3503.996789	493768.323361	44.544986
3504.106598	493749.671493	44.549991
3503.972637	493741.134984	44.554996
3503.871790	493731.124752	44.560001
3503.849813	493716.088939	44.565005
3503.572531	493703.979805	44.570010
3504.106023	493696.704990	44.575015
3503.624544	493701.794246	44.580020
3504.192907	493687.222112	44.585025
3503.811848	493667.280534	44.590029
3503.837646	493650.059698	44.595034
3504.285523	493647.912799	44.600039
3504.015334	493643.398153	44.605044
3503.907501	493614.247909	44.610049
3503.686017	493618.789715	44.615053
3504.007695	493600.408035	44.620058
3503.820980	493600.336310	44.625063
3503.889877	493581.690739	44.630068
3504.010023	493561.923015	44.635073
3503.727822	493568.651860	44.640077
3503.467304	493561.502495	44.645082
3503.733173	493547.990821	44.650087
3504.001728	493538.631027	44.655092
3503.838985	493520.579026	44.660097
3503.461471	493524.993603	44.665101
3503.581823	493524.518876	44.670106
3503.978944	493506.935386	44.675111
3503.620092	493493.826246	44.680116
3503.834282	493477.031214	44.685121
3503.894687	493475.046816	44.690125
3503.822610	493467.614439	44.695130
3504.196077	493468.163104	44.700135
3503.854793	493451.202656	44.705140
3503.639297	493437.817626	44.710145
3503.757413	493434.406232	44.715149
3503.669387	493431.533803	44.720154
3503.783646	493428.274932	44.725159
3503.661796	493412.140615	44.730164
3503.815739	493393.025666	44.735169
3503.503588	493389.479719	44.740173
3503.539580	493386.537042	44.745178
3503.876611	493386.635723	44.750183
3503.726044	493393.141272	44.755188
3503.871591	493367.140804	44.760193
3503.869783	493356.962799	44.765197
3503.748961	493354.450011	44.770202
3503.564004	493346.022657	44.775207
3503.692185	493349.496490	44.780212
3504.227671	493329.713507	44.785217
3504.254840	493309.149992	44.790221
3503.821643	493302.432929	44.795226
3504.198906	493292.802636	44.800231
3503.931407	493286.110014	44.805236
3504.105123	493263.599016	44.810241
3503.894330	493259.530636	44.815245
3504.118101	493249.722026	44.820250
3504.141853	493218.524808	44.825255
3503.603522	493214.254995	44.830260
3503.734262	493210.689647	44.835265
3503.755106	493214.889416	44.840269
3503.752189	493185.519356	44.845274
3504.016557	493169.222502	44.850279
3503.777747	493162.069551	44.855284
3504.078515	493150.071241	44.860289
3503.958216	493138.544591	44.865293
3503.979720	493127.198076	44.870298
3503.958310	493112.566794	44.875303
3504.022187	493114.177188	44.880308
3503.893897	493088.827282	44.885313
3504.128317	493086.916617	44.890317
3504.027636	493079.184768	44.895322
3504.054886	493064.191282	44.900327
3503.827816	493053.795519	44.905332
3504.049069	493038.315594	44.910337
3504.069952	493031.070905	44.915341
3503.888872	493018.034606	44.920346
3503.652141	492996.347749	44.925351
3503.736245	492988.181540	44.930356
3503.901016	492984.914607	44.935361
3504.098284	492977.945854	44.940365
3503.904070	492951.289553	44.945370
3504.002135	492940.943614	44.950375
3503.850702	492943.702126	44.955380
3503.835472	492927.297335	44.960385
3503.907590	492913.258787	44.965389
3503.399574	492899.109368	44.970394
3504.041952	492895.716288	44.975399
3503.808214	492896.057110	44.980404
3503.884886	492889.664422	44.985409
3503.826729	492865.569118	44.990413
3503.705861	492856.169254	44.995418
3503.859480	492848.295834	45.000423
3503.796348	492851.344242	45.005428
3504.149400	492837.919551	45.010433
3503.868702	492816.441993	45.015437
3503.535800	492804.492979	45.020442
3504.035576	492797.071223	45.025447
3503.617151	492802.758437	45.030452
3503.826102	492777.456080	45.035457
3503.887432	492764.583846	45.040461
3503.932631	492752.119274	45.045466
3503.803841	492755.988318	45.050471
3503.591878	492756.224419	45.055476
3503.782436	492744.243268	45.060481
3503.791014	492734.772241	45.065485
3503.686290	492733.168346	45.070490
3503.873944	492717.997305	45.075495
3503.627849	492719.352887	45.080500
3503.894178	492719.057628	45.085505
3503.619525	492698.541141	45.090509
3503.469172	492683.220937	45.095514
3503.814620	492678.152981	45.100519
3503.362499	492683.035312	45.105524
3503.538677	492674.499929	45.110529
3503.908671	492671.453705	45.115533
3503.733647	492667.582101	45.120538
3503.782613	492638.658736	45.125543
3503.630199	492635.948282	45.130548
3503.870703	492622.288022	45.135553
3504.065306	492632.638595	45.140557
3503.971547	492610.624845	45.145562
3503.731611	492587.469441	45.150567
3503.627553	492588.650660	45.155572
3503.372257	492590.666033	45.160577
3503.725239	492579.874475	45.165581
3503.928044	492586.020609	45.170586
3503.843964	492573.373788	45.175591
3503.580332	492553.868211	45.180596
3503.759621	492538.090658	45.185601
3503.705188	492542.505040	45.190605
3503.616798	492535.125507	45.195610
3503.971896	492531.879052	45.200615
3503.713155	492514.448930	45.205620
3503.938899	492499.119767	45.210625
3503.791325	492499.193772	45.215629
3503.474584	492493.116335	45.220634
3503.682702	492492.475788	45.225639
3503.500481	492490.023227	45.230644
3503.579249	492469.703828	45.235649
3503.709055	492463.758364	45.240653
3503.694403	492458.494062	45.245658
3503.928076	492448.227696	45.250663
3503.781834	492453.871994	45.255668
3504.006724	492442.999322	45.260673
3503.889472	492419.267266	45.265677
3503.523743	492405.196259	45.270682
3503.794294	492407.989432	45.275687
3503.657260	492402.845741	45.280692
3503.706945	492400.660360	45.285697
3503.972757	492397.985046	45.290701
3503.877046	492374.502733	45.295706
3503.816093	492362.864937	45.300711
3503.603896	492364.721598	45.305716
3503.751468	492360.950863	45.310721
3504.016847	492356.401888	45.315725
3503.937904	492327.751462	45.320730
3503.762417	492316.992642	45.325735
3503.595708	492315.702356	45.330740
3503.717830	492315.075396	45.335745
3503.418014	492292.840631	45.340749
3503.474454	492276.626501	45.345754
3503.740704	492266.962583	45.350759
3503.671964	492265.859375	45.355764
3503.799934	492258.901306	45.360769
3503.789035	492261.232574	45.365773
3503.837735	492257.376162	45.370778
3503.731423	492230.350439	45.375783
3503.708560	492218.554607	45.380788
3503.991358	492209.748950	45.385793
3503.711078	492216.731188	45.390797
3503.638582	492214.362530	45.395802
3503.845906	492201.011056	45.400807
3503.712450	492189.182044	45.405812
3503.818512	492179.999175	45.410817
3504.048292	492172.467923	45.415821
3504.087577	492166.435388	45.420826
3504.113963	492143.895677	45.425831
3503.797340	492137.007836	45.430836
3504.197366	492118.814872	45.435841
3504.124425	492106.368540	45.440845
3503.826876	492090.817902	45.445850
3504.059483	492075.841800	45.450855
3503.912475	492078.852950	45.455860
3503.998457	492057.721689	45.460865
3504.020592	492051.742470	45.465869
3503.851102	492037.589523	45.470874
3504.197282	492037.737412	45.475879
3503.897962	492024.871028	45.480884
3504.116393	492006.706658	45.485889
3504.104394	492005.645108	45.490893
3503.855422	491987.959735	45.495898
3504.195641	491959.191845	45.500903
3504.013334	491961.297032	45.505908
3503.695745	491949.547614	45.510913
3503.775761	491936.823780	45.515917
3503.761580	491925.786025	45.520922
3503.797294	491915.044232	45.525927
3503.718466	491917.842061	45.530932
3503.923017	491906.162013	45.535937
3503.772247	491890.841220	45.540941
3503.480505	491884.202564	45.545946
3503.871014	491862.719092	45.550951
3503.782773	491858.276533	45.555956
3503.767769	491855.442959	45.560961
3504.026865	491857.883529	45.565965
3503.897473	491835.469352	45.570970
3503.713735	491829.623887	45.575975
3503.728202	491829.570996	45.580980
3503.614087	491811.205785	45.585985
3503.874330	491820.128441	45.590989
3503.593636	491797.383634	45.595994
3503.835362	491777.442863	45.600999
3503.670773	491778.633700	45.606004
3503.563491	491781.537334	45.611009
3503.745296	491773.962861	45.616013
3503.683323	491767.034631	45.621018
3503.826784	491739.766143	45.626023
3503.355281	491740.499066	45.631028
3503.464886	491727.213340	45.636033
3503.495050	491726.145109	45.641037
3503.414757	491722.308976	45.646042
3503.851167	491731.203830	45.651047
3503.389151	491727.681249	45.656052
3503.561252	491724.058437	45.661057
3503.609569	491720.151332	45.666061
3503.326788	491696.140658	45.671066
3503.901321	491686.123853	45.676071
3503.560016	491685.013049	45.681076
3503.551070	491660.351329	45.686081
3503.705131	491666.353543	45.691085
3503.631477	491673.961684	45.696090
3503.565245	491667.793736	45.701095
3503.884069	491671.440324	45.706100
3503.961797	491659.020521	45.711105
3503.791875	491642.993547	45.716109
3503.865003	491643.235242	45.721114
3503.833124	491629.921167	45.726119
3503.485530	491617.467277	45.731124
3503.811650	491596.145606	45.736129
3504.095668	491584.857942	45.741133
3503.646504	491589.689445	45.746138
3504.054066	491589.169273	45.751143
3503.914538	491567.566668	45.756148
3503.975335	491552.971806	45.761153
3504.032819	491549.721580	45.766157
3503.915497	491532.420112	45.771162
3504.010248	491508.754670	45.776167
3503.617750	491499.194478	45.781172
3503.818289	491494.858117	45.786177
3503.998905	491492.246785	45.791181
3503.525122	491481.889136	45.796186
3503.732449	491462.206683	45.801191
3503.786313	491453.690074	45.806196
3503.924564	491453.921478	45.811201
3503.617355	491454.273936	45.816205
3503.495716	491452.368742	45.821210
3503.856727	491443.955511	45.826215
3503.477728	491425.327925	45.831220
3503.558375	491417.971873	45.836225
3503.830219	491408.053407	45.841229
3503.658383	491408.840263	45.846234
3503.866788	491402.071736	45.851239
3503.632850	491403.982571	45.856244
3503.729913	491393.889149	45.861249
3503.874413	491362.517795	45.866253
3503.569719	491373.606362	45.871258
3503.775391	491357.063980	45.876263
3503.643127	491363.668633	45.881268
3503.573634	491365.604123	45.886273
3503.677382	491345.380836	45.891277
3503.609157	491323.260237	45.896282
3503.895474	491318.606413	45.901287
3503.843884	491317.449793	45.906292
3503.745712	491305.918506	45.911297
3503.979743	491307.755383	45.916301
3503.655307	491300.058160	45.921306
3504.004347	491290.178075	45.926311
3503.976817	491291.144702	45.931316
3503.761438	491282.012199	45.936321
3503.947644	491259.547444	45.941325
3503.731032	491247.224534	45.946330
3503.912054	491237.674844	45.951335
3503.525760	491241.483614	45.956340
3503.862804	491240.923936	45.961345
3503.622550	491225.211585	45.966349
3503.558392	491213.370998	45.971354
3503.666933	491194.109032	45.976359
3503.493374	491199.403516	45.981364
3503.491281	491192.820118	45.986369
3503.716896	491193.493516	45.991373
3503.557213	491201.166091	45.996378
3503.692409	491199.068342	46.001383
3503.544584	491176.757574	46.006388
3503.640569	491155.015975	46.011393
3503.664790	491151.568360	46.016397
3503.661648	491138.350681	46.021402
3503.977891	491130.096320	46.026407
3503.879522	491139.734366	46.031412
3503.518817	491133.866009	46.036417
3503.506979	491115.483945	46.041421
3503.569296	491100.483332	46.046426
3503.840817	491099.275627	46.051431
3503.649282	491117.892506	46.056436
3503.735312	491101.115585	46.061441
3503.713792	491105.626395	46.066445
3503.354715	491086.539520	46.071450
3503.742447	491071.791316	46.076455
3503.636437	491070.238124	46.081460
3503.384070	491064.656490	46.086465
3503.792346	491041.548635	46.091469
3503.861078	491049.083879	46.096474
3504.007593	491051.339773	46.101479
3503.777370	491041.297892	46.106484
3504.112477	491015.213528	46.111489
3504.292064	491004.043310	46.116493
3503.917400	490995.290357	46.121498
3503.917703	490975.589470	46.126503
3504.114286	490967.759110	46.131508
3503.929795	490966.218315	46.136513
3503.878330	490951.590082	46.141517
3503.812722	490936.255043	46.146522
3503.929919	490932.336886	46.151527
3503.644938	490930.001650	46.156532
3503.972187	490918.352235	46.161537
3504.187565	490896.591465	46.166541
3504.020795	490887.805601	46.171546
3504.142958	490874.466639	46.176551
3504.183305	490852.277675	46.181556
3503.788154	490842.312402	46.186561
3504.000998	490838.936206	46.191565
3503.637091	490826.535009	46.196570
3503.910846	490804.866196	46.201575
3503.912295	490794.179818	46.206580
3503.701674	490788.591502	46.211585
3503.775189	490782.553109	46.216589
3503.621922	490784.299319	46.221594
3504.225551	490761.818632	46.226599
3503.930124	490747.482029	46.231604
3503.858163	490744.302769	46.236609
3503.857136	490741.162943	46.241613
3503.808529	490724.103092	46.246618
3503.679613	490690.849293	46.251623
3503.832519	490699.232351	46.256628
3503.616763	490682.452111	46.261633
3503.828914	490690.876454	46.266637
3503.232312	490688.894317	46.271642
3503.816425	490683.332289	46.276647
3503.667197	490660.615960	46.281652
3503.623059	490651.962539	46.286657
3503.900408	490650.146134	46.291661
3503.333289	490656.617187	46.296666
3503.356176	490650.130941	46.301671
3503.844973	490648.584989	46.306676
3503.770294	490640.037682	46.311681
3504.000170	490611.487741	46.316685
3503.606471	490603.750531	46.321690
3503.853365	490596.215940	46.326695
3503.666384	490597.815559	46.331700
3503.562361	490596.413951	46.336705
3503.713040	490589.198441	46.341709
3503.540113	490575.196865	46.346714
3503.714755	490565.192025	46.351719
3503.803847	490565.279274	46.356724
3503.543368	490554.279637	46.361729
3504.020693	490554.305520	46.366733
3503.461694	490553.532931	46.371738
3503.793131	490521.624158	46.376743
3503.899837	490523.481238	46.381748
3503.863483	490510.622888	46.386753
3503.550321	490501.657397	46.391757
3503.458307	490522.538218	46.396762
3503.700914	490506.951524	46.401767
3503.571886	490494.107811	46.406772
3503.534307	490465.397337	46.411777
3503.592120	490469.237359	46.416781
3503.910593	490471.516789	46.421786
3503.629687	490468.066631	46.426791
3503.764311	490473.160669	46.431796
3503.748791	490443.281809	46.436801
3503.737551	490431.584302	46.441805
3503.355507	490425.161983	46.446810
3503.506659	490409.640310	46.451815
3503.443090	490418.412237	46.456820
3503.416313	490417.606164	46.461825
3503.641148	490409.973692	46.466829
3503.467404	490419.978548	46.471834
3503.600343	490421.932785	46.476839
3503.513705	490417.590921	46.481844
3503.463405	490410.052585	46.486849
3503.918285	490387.797549	46.491853
3503.621303	490378.981380	46.496858
3503.856189	490375.095152	46.501863
3503.845185	490383.909432	46.506868
3503.594557	490375.693694	46.511873
3503.697162	490368.586992	46.516877
3503.763089	490348.115372	46.521882
3503.752466	490337.379995	46.526887
3503.703768	490331.208834	46.531892
3503.721061	490324.976593	46.536897
3503.947870	490339.020563	46.541901
3503.288516	490312.585942	46.546906
3503.702274	490281.170215	46.551911
3503.726370	490289.928345	46.556916
3503.549333	490278.358242	46.561921
3503.925962	490285.490599	46.566925
3503.715124	490280.864455	46.571930
3503.829097	490278.668664	46.576935
3504.265102	490266.039364	46.581940
3503.966308	490244.156520	46.586945
3504.030253	490243.133512	46.591949
3503.968140	490220.605467	46.596954
3503.732607	490213.552152	46.601959
3504.141065	490193.330104	46.606964
3503.889290	490202.030586	46.611969
3503.876973	490176.151911	46.616973
3503.845861	490166.736500	46.621978
3503.825354	490153.267634	46.626983
3503.989089	490149.038075	46.631988
3503.887878	490138.316902	46.636993
3504.120480	490128.403964	46.641997
3503.393725	490114.286993	46.647002
3503.683141	490094.184949	46.652007
3503.839018	490104.391108	46.657012
3503.852849	490105.300612	46.662017
3503.804263	490082.517026	46.667021
3503.706160	490069.617486	46.672026
3504.140213	490052.987207	46.677031
3504.197132	490070.198374	46.682036
3503.894023	490035.248932	46.687041
3504.047660	490024.183528	46.692045
3503.710296	490024.692718	46.697050
3503.877365	490004.660564	46.702055
3503.810351	489995.250742	46.707060
3503.787287	489985.023606	46.712065
3503.823893	489964.708145	46.717069
3503.707142	489971.209540	46.722074
3503.870475	489967.587776	46.727079
3503.621089	489951.166729	46.732084
3503.689883	489939.000435	46.737089
3503.701607	489922.234204	46.742093
3503.660780	489930.698876	46.747098
3503.925577	489918.805475	46.752103
3503.804555	489919.128529	46.757108
3503.637300	489912.975970	46.762113
3503.574824	489885.939922	46.767117
3503.500285	489869.592462	46.772122
3503.774334	489879.729418	46.777127
3503.559787	489878.193282	46.782132
3503.987317	489876.505010	46.787137
3503.825629	489861.285572	46.792141
3503.639096	489867.899329	46.797146
3503.855041	489846.542435	46.802151
3503.625944	489852.504500	46.807156
3503.672123	489849.306415	46.812161
3503.732472	489855.627913	46.817165
3503.727434	489833.900750	46.822170
3503.850822	489811.748077	46.827175
3503.558030	489806.071158	46.832180
3503.497204	489808.157383	46.837185
3503.348401	489801.242148	46.842189
3503.468210	489810.441207	46.847194
3503.820140	489795.545717	46.852199
3503.798304	489797.372539	46.857204
3503.397955	489775.049366	46.862209
3503.529853	489760.239275	46.867213
3503.245156	489760.638850	46.872218
3503.667459	489758.647505	46.877223
3503.430632	489764.306931	46.882228
3503.330782	489766.703218	46.887233
3503.493451	489757.763454	46.892237
3503.315057	489753.942422	46.897242
3503.612239	489754.959100	46.902247
3503.619112	489749.336095	46.907252
3503.431009	489757.064400	46.912257
3503.442611	489747.439435	46.917261
3503.418617	489754.432726	46.922266
3503.732011	489734.681045	46.927271
3503.513644	489726.915758	46.932276
3503.559747	489713.081509	46.937281
3503.682048	489693.208045	46.942285
3503.317625	489706.890105	46.947290
3503.721568	489693.505765	46.952295
3503.467001	489708.335373	46.957300
3503.124954	489697.601368	46.962305
3503.606011	489704.616145	46.967309
3503.644174	489703.445237	46.972314
3503.366107	489703.286634	46.977319
3503.573368	489705.836979	46.982324
3503.140389	489687.418785	46.987329
3503.673290	489675.330907	46.992333
3503.433409	489678.661012	46.997338
3503.347667	489659.681420	47.002343
3503.698506	489675.529629	47.007348
3503.411642	489671.624429	47.012353
3503.739154	489663.367643	47.017357
3503.610883	489667.085297	47.022362
3503.798815	489659.711597	47.027367
3503.371076	489669.402459	47.032372
3503.304857	489670.172691	47.037377
3503.835451	489662.846127	47.042381
3503.665288	489637.700738	47.047386
3503.444772	489623.705972	47.052391
3503.899482	489627.635377	47.057396
3503.799943	489614.381211	47.062401
3503.971194	489607.617911	47.067405
3503.842328	489602.117614	47.072410
3503.632215	489586.905608	47.077415
3503.865656	489570.661154	47.082420
3503.612694	489559.659744	47.087425
3503.964465	489557.021092	47.092429
3503.618837	489555.505649	47.097434
3503.836822	489529.792276	47.102439
3503.516372	489534.401362	47.107444
3503.559669	489521.023255	47.112449
3503.485667	489524.732358	47.117453
3503.532376	489527.054862	47.122458
3503.598709	489524.309375	47.127463
3503.652452	489521.667177	47.132468
3503.689049	489514.013447	47.137473
3504.235686	489489.970135	47.142477
3503.980166	489482.210618	47.147482
3504.055710	489489.542818	47.152487
3503.992679	489467.773749	47.157492
3503.821525	489451.086653	47.162497
3503.934923	489433.949372	47.167501
3503.578052	489441.248641	47.172506
3503.774392	489421.768380	47.177511
3503.795678	489412.648204	47.182516
3503.784877	489393.960393	47.187521
3503.762844	489391.026258	47.192525
3503.730746	489382.471647	47.197530
3503.304266	489383.298834	47.202535
3503.639358	489399.605609	47.207540
3503.879264	489379.257382	47.212545
3504.067760	489353.953624	47.217549
3503.780423	489355.822455	47.222554
3503.807836	489326.036331	47.227559
3503.644475	489339.281681	47.232564
3503.575555	489335.291312	47.237569
3503.720166	489311.969761	47.242573
3503.541042	489302.931858	47.247578
3503.629514	489303.323107	47.252583
3503.971283	489301.293795	47.257588
3503.631405	489292.331946	47.262593
3504.110836	489285.367870	47.267597
3503.746433	489271.192987	47.272602
3503.916665	489264.075178	47.277607
3504.111332	489248.393720	47.282612
3503.206372	489243.725084	47.287617
3503.465693	489228.742486	47.292621
3503.129694	489215.170866	47.297626
3503.160585	489225.650508	47.302631
3503.710522	489230.122092	47.307636
3503.356455	489217.363724	47.312641
3503.604542	489197.267256	47.317645
3503.192243	489215.819615	47.322650
3503.478691	489210.962654	47.327655
3503.463056	489205.292393	47.332660
3503.562127	489211.759937	47.337665
3503.348635	489207.994991	47.342669
3503.649221	489210.176105	47.347674
3503.981553	489210.427512	47.352679
3503.867068	489200.214399	47.357684
3503.553713	489183.954741	47.362689
3503.773063	489163.761480	47.367693
3503.348446	489174.414449	47.372698
3503.582120	489157.815054	47.377703
3503.566710	489164.452658	47.382708
3503.486751	489161.375694	47.387713
3503.679972	489160.534793	47.392717
3503.712215	489169.596057	47.397722
3503.868362	489150.932266	47.402727
3504.070474	489140.415830	47.407732
3503.846750	489128.751097	47.412737
3503.997478	489123.358416	47.417741
3503.761016	489108.859287	47.422746
3503.788321	489089.354752	47.427751
3503.949136	489080.060410	47.432756
3503.960466	489077.171603	47.437761
3503.870548	489060.724570	47.442765
3503.923247	489047.648542	47.447770
3503.979253	489032.090122	47.452775
3503.890173	489035.244553	47.457780
3503.829873	489024.516278	47.462785
3503.895589	488997.408041	47.467789
3503.634442	488991.219370	47.472794
3503.324904	488984.987695	47.477799
3503.788091	488971.644129	47.482804
3503.705779	488989.840649	47.487809
3503.834753	488978.829180	47.492813
3503.626077	488965.237255	47.497818
3503.875285	488942.810421	47.502823
3503.861814	488945.243809	47.507828
3503.418538	488943.693098	47.512833
3503.952159	488928.616255	47.517837
3503.591752	488931.155133	47.522842
3503.602331	488904.106128	47.527847
3503.959351	488892.248154	47.532852
3503.330474	488893.006051	47.537857
3503.888414	488891.043828	47.542861
3503.643881	488885.612254	47.547866
3503.600169	488888.962140	47.552871
3503.581659	488864.247603	47.557876
3503.420920	488854.548120	47.562881
3503.657647	488841.544162	47.567885
3503.642570	488848.941586	47.572890
3503.774996	488843.450416	47.577895
3503.787527	488842.536761	47.582900
3503.526678	488839.690939	47.587905
3503.659805	488834.402259	47.592909
3503.394910	488816.817704	47.597914
3503.653094	488803.557075	47.602919
3503.373811	488800.815462	47.607924
3503.106613	488805.061752	47.612929
3503.643956	488790.034861	47.617933
3503.300224	488802.093478	47.622938
3503.420594	488797.161360	47.627943
3503.664843	488796.160425	47.632948
3503.734054	488808.660276	47.637953
3503.543530	488792.228911	47.642957
3503.419679	488803.796914	47.647962
3503.624528	488792.925296	47.652967
3503.726369	488779.385457	47.657972
3503.404869	488782.424714	47.662977
3504.074400	488760.640338	47.667981
3503.746313	488751.524414	47.672986
3503.459450	488769.753478	47.677991
3503.703367	488766.726558	47.682996
3503.772314	488751.165862	47.688001
3503.666990	488727.072678	47.693005
3503.504527	488723.147615	47.698010
3503.638038	488717.909493	47.703015
3503.583011	488713.106379	47.708020
3503.757254	488724.576662	47.713025
3503.488516	488709.018655	47.718029
3503.741358	488717.133548	47.723034
3503.594872	488695.326127	47.728039
3503.749969	488673.825569	47.733044
3503.299579	488674.200704	47.738049
3503.601648	488657.691361	47.743053
3503.520525	488672.190461	47.748058
3503.571048	488664.939395	47.753063
3503.670837	488670.951150	47.758068
3503.370812	488673.075309	47.763073
3503.913996	488663.112510	47.768077
3503.783058	488638.618052	47.773082
3503.889393	488621.430499	47.778087
3503.486804	488628.433398	47.783092
3503.526111	488615.409839	47.788097
3503.991357	488616.653273	47.793101
3503.376360	488613.458183	47.798106
3503.751462	488580.526194	47.803111
3503.981450	488582.161376	47.808116
3503.360692	488579.473705	47.813121
3503.725901	488578.605594	47.818125
3503.623949	488579.128261	47.823130
3503.825283	488579.906898	47.828135
3503.624866	488552.536180	47.833140
3503.923739	488546.562752	47.838145
3503.873378	488531.527248	47.843149
3503.648211	488532.170695	47.848154
3503.683771	488527.353215	47.853159
3503.794882	488510.519367	47.858164
3503.651057	488502.387229	47.863169
3503.577247	488495.054447	47.868173
3503.529887	488486.856403	47.873178
3503.569352	488484.976091	47.878183
3503.819689	488494.357768	47.883188
3503.104674	488488.392626	47.888193
3503.909882	488478.590920	47.893197
3503.750079	488468.739136	47.898202
3503.775681	488449.284860	47.903207
3503.876687	488435.744907	47.908212
3503.548953	488446.332319	47.913217
3503.708889	488430.149155	47.918221
3503.796338	488436.517498	47.923226
3503.554036	488418.219875	47.928231
3503.790430	488404.455893	47.933236
3503.711394	488418.954856	47.938241
3503.931649	488394.860439	47.943245
3503.781144	488410.130484	47.948250
3503.783633	488395.339777	47.953255
3503.691806	488364.709901	47.958260
3503.416528	488366.019750	47.963265
3503.512604	488358.052238	47.968269
3503.512662	488355.165102	47.973274
3503.773478	488351.831533	47.978279
3503.339815	488358.484879	47.983284
3503.790701	488358.717561	47.988289
3503.981747	488340.300714	47.993293
3503.847390	488332.369615	47.998298
3503.815314	488316.824529	48.003303
3504.104830	488318.703585	48.008308
3503.786023	488314.499237	48.013313
3503.833109	488281.466618	48.018317
3503.708308	488267.911584	48.023322
3503.505940	488261.206859	48.028327
3503.649568	488258.347668	48.033332
3503.711179	488272.875164	48.038337
3503.740295	488266.437765	48.043341
3503.610856	488245.994741	48.048346
3503.632882	488230.694294	48.053351
3503.771637	488225.100641	48.058356
3503.584592	488225.535463	48.063361
3503.825041	488213.847448	48.068365
3503.449241	488215.679719	48.073370
3503.814080	488217.901447	48.078375
3504.104999	488196.784098	48.083380
3503.778538	488180.778908	48.088385
3503.902997	488176.605769	48.093389
3503.669448	488177.301205	48.098394
3503.849344	488153.010249	48.103399
3503.827016	488142.933955	48.108404
3503.480544	488135.745436	48.113409
3503.496638	488125.004575	48.118413
3503.639690	488133.137074	48.123418
3503.526520	488130.419759	48.128423
3503.621980	488118.957213	48.133428
3503.532761	488129.912322	48.138433
3503.856010	488104.079066	48.143437
3503.617965	488088.819612	48.148442
3503.692109	488090.682082	48.153447
3503.498855	488086.609795	48.158452
3503.447851	488085.199618	48.163457
3503.698500	488076.397112	48.168461
3503.461310	488078.815320	48.173466
3503.381191	488068.393552	48.178471
3503.573385	488076.062432	48.183476
3503.478261	488056.120307	48.188481
3503.733859	488039.820383	48.193485
3503.560525	488037.821704	48.198490
3503.470918	488031.656255	48.203495
3503.773076	488030.190253	48.208500
3503.535991	488024.858558	48.213505
3503.513407	488022.126909	48.218509
3503.368516	488033.951973	48.223514
3503.610416	488025.758661	48.228519
3503.611914	487996.025188	48.233524
3503.305094	487997.694618	48.238529
3503.632866	487974.494425	48.243533
3503.565210	487999.578392	48.248538
3503.563148	487974.606827	48.253543
3503.845963	487980.944443	48.258548
3503.782933	487983.841665	48.263553
3503.687936	487972.561095	48.268557
3503.618541	487956.008550	48.273562
3503.627160	487938.886476	48.278567
3503.711323	487940.747376	48.283572
3503.433052	487947.224344	48.288577
3503.441986	487932.786829	48.293581
3503.641984	487933.059174	48.298586
3503.657912	487944.706914	48.303591
3503.655001	487937.464015	48.308596
3503.404008	487910.201668	48.313601
3503.621661	487903.329119	48.318605
3503.393256	487902.554807	48.323610
3503.733048	487882.645061	48.328615
3503.782890	487892.869181	48.333620
3503.513609	487892.050677	48.338625
3504.070731	487886.897328	48.343629
3503.578969	487881.656502	48.348634
3503.606546	487856.680096	48.353639
3503.501777	487850.719598	48.358644
3503.542795	487848.383098	48.363649
3503.539815	487845.040484	48.368653
3503.296043	487851.106805	48.373658
3503.561880	487852.179197	48.378663
3503.582853	487839.107349	48.383668
3503.484494	487856.952921	48.388673
3503.636683	487838.592382	48.393677
3503.799755	487826.511132	48.398682
3503.624744	487811.241491	48.403687
3503.786292	487804.631042	48.408692
3503.362401	487808.497093	48.413697
3503.692851	487798.314200	48.418701
3503.561329	487796.207580	48.423706
3503.675459	487805.155247	48.428711
3504.047495	487786.354681	48.433716
3503.566509	487773.007553	48.438721
3503.792197	487762.182704	48.443725
3503.648920	487758.912904	48.448730
3503.934857	487745.343227	48.453735
3503.803569	487742.881988	48.458740
3503.773502	487720.497851	48.463745
3503.819146	487718.109950	48.468749
3503.666318	487715.398843	48.473754
3503.925977	487716.978758	48.478759
3503.816256	487701.445440	48.483764
3503.491530	487687.870937	48.488769
3503.786831	487678.453344	48.493773
3503.439007	487671.416823	48.498778
3503.377465	487671.426589	48.503783
3503.497579	487672.572680	48.508788
3503.426029	487679.523602	48.513793
3503.596321	487679.901953	48.518797
3503.405489	487676.589002	48.523802
3503.286933	487663.691049	48.528807
3503.559505	487657.721500	48.533812
3503.436660	487684.840762	48.538817
3503.516303	487658.133636	48.543821
3503.646686	487637.395617	48.548826
3503.311122	487626.963328	48.553831
3503.256580	487622.058552	48.558836
3503.407613	487629.480850	48.563841
3503.727913	487616.969383	48.568845
3503.606026	487614.810566	48.573850
3503.525318	487609.707306	48.578855
3503.703683	487621.886763	48.583860
3503.278675	487623.017713	48.588865
3503.659261	487623.514788	48.593869
3503.719751	487618.237251	48.598874
3503.646875	487591.148906	48.603879
3503.665809	487579.900747	48.608884
3503.524813	487586.457448	48.613889
3503.737381	487568.948224	48.618893
3503.353774	487583.242698	48.623898
3503.457366	487572.740964	48.628903
3503.734479	487567.479827	48.633908
3503.511917	487569.237284	48.638913
3503.535860	487537.118801	48.643917
3503.609821	487537.360419	48.648922
3503.545742	487536.154885	48.653927
3503.672108	487527.827658	48.658932
3503.483551	487540.673015	48.663937
3503.840489	487524.508594	48.668941
3503.744006	487535.718465	48.673946
3503.568569	487510.976310	48.678951
3503.748388	487499.449402	48.683956
3503.665816	487487.052184	48.688961
3503.558764	487497.200007	48.693965
3503.688869	487490.797036	48.698970
3503.537823	487493.606937	48.703975
3503.619146	487497.241231	48.708980
3503.491584	487492.297309	48.713985
3503.927456	487472.270638	48.718989
3503.497056	487449.949460	48.723994
3503.503332	487440.172198	48.728999
3504.111028	487439.974872	48.734004
3503.738756	487435.829432	48.739009
3503.399910	487436.693501	48.744013
3503.763705	487427.214302	48.749018
3503.403473	487402.298597	48.754023
3503.931363	487387.677331	48.759028
3503.425196	487397.938947	48.764033
3503.870327	487388.548182	48.769037
3503.670885	487398.913280	48.774042
3503.491623	487397.675288	48.779047
3503.616041	487382.813864	48.784052
3503.512901	487364.898463	48.789057
3503.560160	487347.415165	48.794061
3503.705329	487359.296110	48.799066
3503.752950	487347.587387	48.804071
3503.697178	487335.692381	48.809076
3503.303735	487351.609534	48.814081
3503.878296	487336.474304	48.819085
3503.658451	487322.730998	48.824090
3503.709330	487309.248820	48.829095
3503.702996	487302.766042	48.834100
3503.641752	487306.118979	48.839105
3503.859036	487301.069845	48.844109
3503.729876	487310.562749	48.849114
3503.911609	487286.017120	48.854119
3503.792056	487267.040469	48.859124
3503.668964	487267.971751	48.864129
3503.623209	487258.607859	48.869133
3503.607701	487261.598990	48.874138
3503.371469	487255.608429	48.879143
3503.561678	487260.593242	48.884148
3503.461206	487247.489527	48.889153
3503.880322	487216.169173	48.894157
3503.909750	487217.481591	48.899162
3503.556044	487216.828367	48.904167
3503.586794	487212.973759	48.909172
3503.276438	487211.148616	48.914177
3503.648590	487212.406862	48.919181
3503.794060	487201.695684	48.924186
3503.501094	487189.331527	48.929191
3503.559178	487165.565114	48.934196
3503.545995	487163.135786	48.939201
3503.714367	487161.994796	48.944205
3503.502142	487163.902622	48.949210
3503.582268	487159.229716	48.954215
3503.903203	487166.625340	48.959220
3503.642225	487161.449144	48.964225
3503.721439	487127.801576	48.969229
3503.714986	487124.662006	48.974234
3503.493723	487130.775653	48.979239
3503.699542	487117.167537	48.984244
3503.375777	487116.053678	48.989249
3503.989583	487115.450142	48.994253
3503.686726	487110.483173	48.999258
3503.719273	487094.420318	49.004263
3503.641680	487078.273547	49.009268
3503.782336	487074.857438	49.014273
3503.589966	487073.874774	49.019277
3503.714924	487072.740641	49.024282
3503.633620	487062.217196	49.029287
3503.573293	487045.206525	49.034292
3503.569479	487040.597514	49.039297
3503.688533	487030.700904	49.044301
3503.619759	487032.180823	49.049306
3503.391857	487030.646562	49.054311
3503.969471	487019.107143	49.059316
3503.339769	487034.403382	49.064321
3503.474553	487023.440515	49.069325
3503.570642	487019.879475	49.074330
3503.556122	486998.606453	49.079335
3503.671778	486998.284276	49.084340
3503.454339	486983.425920	49.089345
3503.541664	486977.333473	49.094349
3503.538228	486980.373395	49.099354
3503.451037	486981.299017	49.104359
3503.803271	486979.217152	49.109364
3503.549702	486980.523662	49.114369
3503.424396	486972.793185	49.119373
3503.779374	486964.024331	49.124378
3503.318474	486956.296237	49.129383
3503.735401	486947.264304	49.134388
3503.378652	486952.487619	49.139393
3503.586651	486948.858221	49.144397
3503.418817	486940.425272	49.149402
3503.382883	486948.434603	49.154407
3503.550115	486931.945075	49.159412
3503.562697	486949.925930	49.164417
3503.484516	486939.097989	49.169421
3503.813852	486943.250401	49.174426
3503.849298	486914.573641	49.179431
3503.760149	486899.492318	49.184436
3503.618293	486895.968865	49.189441
3503.471991	486896.650555	49.194445
3503.721832	486896.661758	49.199450
3503.336437	486892.163681	49.204455
3503.833508	486890.717440	49.209460
3503.232102	486875.159852	49.214465
3503.384372	486859.837714	49.219469
3503.566929	486847.955387	49.224474
3503.707007	486856.798088	49.229479
3503.818078	486848.878230	49.234484
3503.400196	486856.289444	49.239489
3503.724417	486846.056372	49.244493
3503.514611	486849.990088	49.249498
3503.207873	486855.965365	49.254503
3503.686914	486848.949808	49.259508
3503.408383	486827.363733	49.264513
3503.482445	486806.583056	49.269517
3503.466698	486814.994501	49.274522
3503.692351	486805.486174	49.279527
3503.748551	486798.486779	49.284532
3503.736281	486802.895842	49.289537
3503.848806	486793.405391	49.294541
3503.631788	486795.617947	49.299546
3503.385241	486785.019155	49.304551
3503.570782	486759.763059	49.309556
3503.713553	486762.627938	49.314561
3503.792405	486764.945700	49.319565
3503.974784	486767.247098	49.324570
3503.735622	486751.784120	49.329575
3503.909108	486745.424698	49.334580
3503.571144	486729.774694	49.339585
3503.677607	486721.247635	49.344589
3503.912745	486711.281854	49.349594
3503.563072	486720.961876	49.354599
3504.219420	486704.597467	49.359604
3503.996602	486692.829775	49.364609
3503.581376	486678.509008	49.369613
3503.898813	486674.760947	49.374618
3503.773772	486670.424290	49.379623
3503.993921	486652.811714	49.384628
3503.662503	486637.363225	49.389633
3503.645285	486628.399765	49.394637
3503.595934	486626.381338	49.399642
3503.549654	486626.034095	49.404647
3503.852017	486616.665519	49.409652
3503.863271	486604.404865	49.414657
3503.508608	486590.023801	49.419661
3503.739537	486581.375693	49.424666
3503.745227	486573.117781	49.429671
3503.459769	486569.616965	49.434676
3503.693223	486577.381245	49.439681
3504.040919	486569.525182	49.444685
3503.876285	486548.022101	49.449690
3503.713034	486530.115416	49.454695
3503.889172	486526.693601	49.459700
3503.670070	486525.107251	49.464705
3503.803934	486516.170514	49.469709
3503.893592	486494.525864	49.474714
3503.747035	486481.682191	49.479719
3504.049306	486483.204819	49.484724
3503.431223	486482.795983	49.489729
3503.754244	486469.320851	49.494733
3503.640106	486445.935363	49.499738
3503.618828	486439.961225	49.504743
3503.638940	486437.678513	49.509748
3503.439221	486440.242975	49.514753
3503.525366	486426.450655	49.519757
3503.610926	486435.048884	49.524762
3503.425931	486441.866218	49.529767
3503.762544	486428.034309	49.534772
3503.550369	486429.232998	49.539777
3503.611362	486402.324431	49.544781
3503.597044	486399.084670	49.549786
3503.385350	486405.247692	49.554791
3503.838349	486389.624357	49.559796
3503.553813	486402.434994	49.564801
3503.768769	486384.468390	49.569805
3503.897386	486379.686315	49.574810
3503.599370	486357.900158	49.579815
3503.638463	486340.771829	49.584820
3503.641573	486344.013448	49.589825
3503.846533	486339.928499	49.594829
3503.808283	486340.694443	49.599834
3503.366884	486337.572835	49.604839
3503.741764	486309.398745	49.609844
3503.788558	486309.695331	49.614849
3503.591076	486291.793833	49.619853
3503.541617	486300.058861	49.624858
3503.395755	486295.016205	49.629863
3503.987411	486281.802425	49.634868
3503.697550	486291.929127	49.639873
3503.374807	486267.765873	49.644877
3503.722210	486250.234127	49.649882
3503.390143	486253.478082	49.654887
3503.501200	486242.417203	49.659892
3503.462661	486250.579212	49.664897
3503.322153	486251.969215	49.669901
3503.667272	486250.546946	49.674906
3503.600393	486243.465487	49.679911
3504.086526	486241.514352	49.684916
3503.570206	486234.909191	49.689921
3503.349592	486224.863222	49.694925
3503.428481	486222.064617	49.699930
3503.741997	486213.504605	49.704935
3503.590107	486208.108274	49.709940
3503.401436	486217.965732	49.714945
3503.458843	486206.609366	49.719949
3503.569856	486206.997118	49.724954
3503.425565	486220.444259	49.729959
3503.505497	486208.476441	49.734964
3503.223132	486221.793433	49.739969
3503.460342	486208.686286	49.744973
3503.650307	486204.553020	49.749978
3503.648328	486181.352110	49.754983
3503.689455	486168.731849	49.759988
3503.231026	486164.853037	49.764993
3503.479128	486164.965832	49.769997
3503.727381	486165.483867	49.775002
3503.225752	486164.448721	49.780007
3503.488838	486157.669679	49.785012
3503.253152	486160.341180	49.790017
3503.478384	486154.631935	49.795021
3503.452857	486157.624823	49.800026
3503.314652	486161.851309	49.805031
3503.479730	486165.067356	49.810036
3503.332311	486165.546616	49.815041
3503.602654	486146.507221	49.820045
3503.668080	486129.323882	49.825050
3503.494588	486118.713171	49.830055
3503.728365	486117.764414	49.835060
3503.519062	486119.671880	49.840065
3503.242404	486117.385381	49.845069
3503.681179	486118.886462	49.850074
3503.580614	486117.939894	49.855079
3503.826131	486116.280069	49.860084
3503.249925	486119.461321	49.865089
3503.660846	486103.084534	49.870093
3503.531915	486078.079876	49.875098
3503.436944	486078.145584	49.880103
3503.494821	486063.546941	49.885108
3503.533892	486073.013869	49.890113
3503.236417	486064.955631	49.895117
3503.440539	486063.403661	49.900122
3503.515641	486076.461618	49.905127
3503.769202	486059.451111	49.910132
3503.390449	486061.334709	49.915137
3503.819852	486067.548480	49.920141
3503.919329	486046.205720	49.925146
3503.544225	486037.501183	49.930151
3503.829538	486029.300154	49.935156
3503.527337	486020.178821	49.940161
3503.603049	486023.459676	49.945165
3503.661397	486023.957074	49.950170
3503.066059	486024.507137	49.955175
3503.489611	486017.449391	49.960180
3503.127179	486032.552208	49.965185
3503.460516	486021.152117	49.970189
3503.666778	486016.357678	49.975194
3503.428897	485988.837213	49.980199
3503.730910	485976.834147	49.985204
3503.485687	485983.205238	49.990209
3503.105728	485971.107331	49.995213
3503.411453	485973.085379	50.000218
3503.242459	485974.631879	50.005223
3503.350747	485979.781952	50.010228
3503.573432	485984.255384	50.015233
3503.612773	485969.912891	50.020237
3503.326023	485975.328040	50.025242
3503.143927	485970.797608	50.030247
3503.491180	485972.465142	50.035252
3503.606045	485979.032610	50.040257
3503.573079	485971.793714	50.045261
3503.450038	485973.282293	50.050266
3503.654335	485962.611781	50.055271
3503.694890	485935.047227	50.060276
3503.453545	485935.541339	50.065281
3503.556094	485934.208048	50.070285
3503.937090	485920.166124	50.075290
3503.568620	485926.708690	50.080295
3503.659983	485923.350827	50.085300
3503.565888	485913.234038	50.090305
3503.700773	485902.118537	50.095309
3503.726654	485890.463015	50.100314
3503.955302	485892.858524	50.105319
3503.959279	485876.444549	50.110324
3503.735613	485882.406998	50.115329
3503.615660	485865.303382	50.120333
3503.818734	485838.776833	50.125338
3503.801859	485838.779538	50.130343
3503.968142	485838.905269	50.135348
3503.646787	485832.877055	50.140353
3503.623863	485817.379139	50.145357
3503.563380	485789.222441	50.150362
3503.300125	485793.823385	50.155367
3503.573254	485778.785232	50.160372
3503.316360	485783.233196	50.165377
3503.482728	485782.599031	50.170381
3503.894300	485765.867242	50.175386
3503.530396	485781.933007	50.180391
3503.881641	485783.245316	50.185396
3504.021071	485767.772356	50.190401
3503.676067	485746.347541	50.195405
3503.734197	485747.807500	50.200410
3503.421069	485748.920871	50.205415
3503.675827	485736.418534	50.210420
3503.628077	485737.034028	50.215425
3503.248756	485741.045423	50.220429
3503.434222	485724.754609	50.225434
3503.507982	485725.300237	50.230439
3503.930633	485698.738787	50.235444
3503.610509	485698.434811	50.240449
3503.608772	485686.884849	50.245453
3503.439963	485687.519479	50.250458
3503.215630	485691.962318	50.255463
3503.452548	485688.784044	50.260468
3503.336383	485693.767035	50.265473
3503.493603	485689.284221	50.270477
3503.587803	485687.952233	50.275482
3503.360760	485699.031841	50.280487
3503.229796	485690.389875	50.285492
3503.247052	485689.272685	50.290497
3503.476437	485688.020647	50.295501
3503.669449	485674.210893	50.300506
3503.306219	485664.592445	50.305511
3503.779055	485648.002847	50.310516
3503.635362	485644.732748	50.315521
3503.485059	485659.701009	50.320525
3503.407391	485655.052678	50.325530
3503.496026	485658.990123	50.330535
3503.640730	485645.643917	50.335540
3503.413122	485653.785406	50.340545
3503.745851	485650.895936	50.345549
3503.465194	485619.886215	50.350554
3503.215808	485612.326777	50.355559
3503.271745	485600.666328	50.360564
3503.385775	485607.234055	50.365569
3503.064465	485609.361913	50.370573
3503.479606	485596.074245	50.375578
3503.033413	485597.056678	50.380583
3503.590787	485602.895759	50.385588
3503.483256	485606.813562	50.390593
3503.399697	485597.809445	50.395597
3503.679292	485597.005399	50.400602
3503.312611	485601.470759	50.405607
3503.362656	485587.987498	50.410612
3503.129528	485607.021641	50.415617
3503.146495	485612.034270	50.420621
3503.333040	485603.595374	50.425626
3503.268507	485606.239898	50.430631
3503.447413	485606.211657	50.435636
3503.406272	485610.726878	50.440641
3503.466421	485595.215651	50.445645
3503.416565	485597.756537	50.450650
3503.315113	485601.318765	50.455655
3503.475392	485592.833357	50.460660
3503.227164	485598.698457	50.465665
3503.396136	485597.911896	50.470669
3503.648197	485596.453631	50.475674
3503.487090	485591.109242	50.480679
3503.693677	485577.601229	50.485684
3503.724866	485568.021708	50.490689
3503.740410	485557.482124	50.495693
3504.131352	485551.138595	50.500698
3503.539686	485552.447981	50.505703
3503.684797	485551.766509	50.510708
3503.729996	485522.224908	50.515713
3503.378236	485514.833592	50.520717
3503.777775	485510.008477	50.525722
3503.548973	485508.575552	50.530727
3503.842505	485494.243185	50.535732
3503.607959	485473.053902	50.540737
3503.446594	485438.377534	50.545741
3503.439547	485388.073467	50.550746
3503.220035	485340.943774	50.555751
3503.443022	485264.006488	50.560756
3503.278453	485189.916477	50.565761
3503.147262	485096.873822	50.570765
3502.995829	485010.470495	50.575770
3502.758821	484904.474440	50.580775
3502.558206	484789.504968	50.585780
3502.249189	484676.882385	50.590785
3501.980550	484542.924015	50.595789
3502.042232	484400.502527	50.600794
3501.743910	484263.456493	50.605799
3501.772949	484103.457950	50.610804
3501.522816	483950.949772	50.615809
3501.231284	483770.733660	50.620813
3501.002785	483593.039135	50.625818
3500.316350	483411.007500	50.630823
3500.198268	483222.855112	50.635828
3499.944767	483022.967769	50.640833
3499.630052	482810.218713	50.645837
3499.468386	482598.304479	50.650842
3498.954199	482399.414603	50.655847
3498.581905	482168.933917	50.660852
3498.297426	481937.575253	50.665857
3498.031089	481716.040867	50.670861
3497.785452	481469.469656	50.675866
3497.661609	481217.961019	50.680871
3497.055916	480966.119945	50.685876
3496.682968	480711.350535	50.690881
3496.123867	480446.472688	50.695885
3496.213283	480167.806917	50.700890
3495.279199	479906.376194	50.705895
3495.139560	479613.043263	50.710900
3494.630247	479337.247513	50.715905
3494.176125	479042.334197	50.720909
3493.824238	478749.984862	50.725914
3493.046906	478454.708469	50.730919
3492.843698	478142.612968	50.735924
3492.397617	477844.386458	50.740929
3491.777467	477533.563618	50.745933
3491.526836	477211.122245	50.750938
3490.296569	476898.966894	50.755943
3490.205994	476578.111831	50.760948
3489.781110	476256.645593	50.765953
3489.135437	475930.140677	50.770957
3488.788813	475592.229717	50.775962
3488.389118	475262.329865	50.780967
3487.951671	474926.398856	50.785972
3487.104497	474589.057087	50.790977
3486.324297	474240.040747	50.795981
3485.995524	473905.140074	50.800986
3485.341313	473550.516130	50.805991
3485.007064	473199.890721	50.810996
3484.352944	472852.097907	50.816001
3483.750693	472499.069607	50.821005
3483.408935	472137.071938	50.826010
3482.747346	471787.335847	50.831015
3482.311401	471420.727220	50.836020
3481.545480	471054.569795	50.841025
3480.530544	470696.455408	50.846029
3480.357314	470314.981969	50.851034
3479.817907	469952.774370	50.856039
3479.020824	469586.443775	50.861044
3478.242910	469213.208362	50.866049
3477.527768	468835.291764	50.871053
3477.361351	468463.112396	50.876058
3476.556934	468083.269594	50.881063
3475.917811	467704.002228	50.886068
3475.477900	467336.510899	50.891073
3474.607840	466957.520088	50.896077
3474.523229	466560.042239	50.901082
3473.775107	466187.255315	50.906087
3473.022329	465789.919315	50.911092
3472.181186	465394.973214	50.916097
3471.016535	465016.653430	50.921101
3470.910533	464633.899764	50.926106
3469.634067	464254.316320	50.931111
3469.375722	463863.408156	50.936116
3468.858033	463471.570278	50.941121
3468.243466	463100.077525	50.946125
3467.567791	462713.068771	50.951130
3466.712366	462327.197267	50.956135
3466.237856	461938.874891	50.961140
3465.360209	461549.392017	50.966145
3464.801109	461167.865573	50.971149
3464.471663	460769.659629	50.976154
3463.233554	460390.255732	50.981159
3462.818686	459989.360782	50.986164
3462.144314	459609.296256	50.991169
3461.203964	459216.890376	50.996173
3460.825432	458821.649491	51.001178
3459.896473	458445.510947	51.006183
3459.420666	458049.104881	51.011188
3458.588967	457667.864984	51.016193
3457.924727	457276.294049	51.021197
3456.965061	456888.567662	51.026202
3456.133587	456512.076506	51.031207
3455.647988	456119.797481	51.036212
3454.912851	455737.697546	51.041217
3454.150456	455362.140019	51.046221
3453.632482	454979.739171	51.051226
3452.663645	454597.758247	51.056231
3452.283480	454209.487990	51.061236
3451.334767	453840.022860	51.066241
3450.620028	453454.887493	51.071245
3450.020551	453073.380547	51.076250
3449.170436	452699.314782	51.081255
3448.512429	452311.055970	51.086260
3448.078059	451943.000914	51.091265
3447.272293	451558.659752	51.096269
3446.731984	451180.460805	51.101274
3445.738644	450806.640466	51.106279
3445.153342	450428.994464	51.111284
3444.798692	450050.798369	51.116289
3443.910891	449670.701285	51.121293
3443.316744	449290.044077	51.126298
3442.310506	448911.171208	51.131303
3442.027621	448537.404923	51.136308
3441.063998	448150.240935	51.141313
3440.389475	447786.471442	51.146317
3439.941205	447409.211521	51.151322
3438.941742	447033.402985	51.156327
3438.440857	446654.971996	51.161332
3437.566023	446287.556807	51.166337
3437.025417	445903.587943	51.171341
3436.163104	445522.912047	51.176346
3435.315155	445161.565767	51.181351
3434.464354	444784.327631	51.186356
3433.726852	444421.886790	51.191361
3433.010828	444055.985505	51.196365
3432.626119	443685.508708	51.201370
3431.403954	443320.488374	51.206375
3431.016207	442962.843140	51.211380
3430.062587	442594.825252	51.216385
3429.572784	442235.713314	51.221389
3428.916018	441871.089311	51.226394
3427.914982	441518.697513	51.231399
3427.529923	441148.791081	51.236404
3427.187928	440795.167813	51.241409
3426.077889	440437.954962	51.246413
3425.470313	440071.519489	51.251418
3424.858062	439715.334278	51.256423
3424.451665	439344.921710	51.261428
3423.338405	438986.317541	51.266433
3422.652814	438629.417486	51.271437
3422.386413	438260.515012	51.276442
3421.415178	437903.522752	51.281447
3420.414254	437540.970564	51.286452
3419.669555	437194.035892	51.291457
3419.124010	436845.541725	51.296461
3418.550397	436482.703540	51.301466
3417.737139	436127.184156	51.306471
3417.062487	435779.685718	51.311476
3416.230830	435429.313087	51.316481
3415.540843	435077.262960	51.321485
3414.801493	434719.757176	51.326490
3414.066791	434373.543752	51.331495
3413.374810	434027.699706	51.336500
3412.724232	433693.066686	51.341505
3411.866623	433347.950533	51.346509
3411.282688	432994.509188	51.351514
3410.317926	432652.523641	51.356519
3409.547801	432308.852353	51.361524
3408.629699	431965.072926	51.366529
3408.140857	431635.668967	51.371533
3407.599982	431290.322819	51.376538
3406.687087	430966.487492	51.381543
3405.880171	430622.367975	51.386548
3405.725782	430291.116605	51.391553
3404.868893	429959.540423	51.396557
3404.061130	429616.728254	51.401562
3403.354606	429291.773005	51.406567
3402.583878	428950.368352	51.411572
3401.884939	428616.464753	51.416577
3400.666750	428294.650869	51.421581
3400.334520	427964.972818	51.426586
3399.464425	427647.159281	51.431591
3398.974575	427321.891611	51.436596
3398.287660	426996.981282	51.441601
3397.489858	426684.655816	51.446605
3397.048460	426347.914787	51.451610
3396.620122	426023.612075	51.456615
3395.975839	425699.847544	51.461620
3394.841592	425366.581635	51.466625
3394.398642	425042.955168	51.471629
3393.991622	424711.648839	51.476634
3393.144573	424386.173542	51.481639
3392.331625	424047.583071	51.486644
3391.513036	423732.712240	51.491649
3390.739400	423411.658567	51.496653
3390.246412	423092.487142	51.501658
3389.501600	422771.370606	51.506663
3388.622326	422436.656914	51.511668
3387.890778	422115.048009	51.516673
3387.219274	421802.925871	51.521677
3386.620820	421481.847376	51.526682
3385.748920	421172.010535	51.531687
3385.109758	420852.607707	51.536692
3384.621679	420542.474546	51.541697
3383.788988	420227.591352	51.546701
3383.164260	419902.764633	51.551706
3382.478841	419592.194887	51.556711
3381.829936	419268.634805	51.561716
3381.031461	418956.907364	51.566721
3380.201784	418650.770281	51.571725
3379.556671	418327.808504	51.576730
3378.586476	418028.647671	51.581735
3378.194716	417717.934668	51.586740
3377.474861	417405.898280	51.591745
3376.706822	417099.912567	51.596749
3376.071322	416780.742517	51.601754
3375.326621	416487.423964	51.606759
3374.636129	416177.046322	51.611764
3373.627982	415874.185049	51.616769
3372.975937	415576.955381	51.621773
3372.341521	415268.185117	51.626778
3371.848643	414969.856954	51.631783
3371.403082	414677.539812	51.636788
3370.355386	414374.008509	51.641793
3369.840026	414075.649323	51.646797
3369.465609	413762.096075	51.651802
3368.307250	413466.449401	51.656807
3367.638552	413163.557044	51.661812
3367.188266	412868.325968	51.666817
3366.121029	412569.200235	51.671821
3365.600230	412272.170285	51.676826
3364.669568	411987.221000	51.681831
3363.991424	411686.678102	51.686836
3363.522233	411397.381297	51.691841
3362.560214	411093.014928	51.696845
3361.956835	410797.965333	51.701850
3361.170618	410510.234713	51.706855
3360.767064	410228.260008	51.711860
3360.097962	409933.009006	51.716865
3359.180568	409653.930854	51.721869
3358.874117	409346.749466	51.726874
3357.707860	409061.352185	51.731879
3357.225727	408767.712030	51.736884
3356.405057	408484.236849	51.741889
3355.528606	408193.703038	51.746893
3355.137217	407907.232113	51.751898
3354.351140	407623.794295	51.756903
3353.778932	407339.074764	51.761908
3353.219694	407052.393670	51.766913
3352.128034	406781.017190	51.771917
3351.810276	406486.592154	51.776922
3351.086624	406205.876164	51.781927
3350.528033	405917.608728	51.786932
3350.112502	405635.542694	51.791937
3349.260988	405340.784548	51.796941
3348.601971	405058.167239	51.801946
3347.438594	404775.525469	51.806951
3346.879620	404486.609473	51.811956
3346.205950	404199.691426	51.816961
3345.586493	403918.430070	51.821965
3345.006298	403632.000401	51.826970
3344.198516	403356.940088	51.831975
3343.686307	403072.985469	51.836980
3342.643134	402795.237870	51.841985
3342.067161	402518.227328	51.846989
3341.655019	402229.826695	51.851994
3340.626053	401958.373185	51.856999
3340.007483	401684.031045	51.862004
3339.327376	401393.047172	51.867009
3338.660407	401128.265300	51.872013
3338.136569	400848.715637	51.877018
3337.623304	400573.991524	51.882023
3337.011660	400292.976634	51.887028
3336.027602	400021.753910	51.892033
3335.387574	399745.238039	51.897037
3334.865394	399454.364292	51.902042
3333.580008	399193.884163	51.907047
3333.154771	398913.387149	51.912052
3332.573767	398642.826430	51.917057
3331.429938	398381.351479	51.922061
3331.085172	398107.139237	51.927066
3330.372451	397840.405924	51.932071
3329.463370	397563.660029	51.937076
3328.867609	397300.335774	51.942081
3327.862303	397036.794562	51.947085
3327.575236	396757.274289	51.952090
3326.781918	396498.398388	51.957095
3326.232284	396237.829486	51.962100
3325.827232	395967.219151	51.967105
3325.097877	395703.013653	51.972109
3324.389421	395426.726803	51.977114
3323.651954	395171.670746	51.982119
3322.879519	394900.143869	51.987124
3322.309694	394635.472601	51.992129
3321.198977	394380.825559	51.997133
3321.005327	394109.455074	52.002138
3319.975187	393853.977785	52.007143
3319.277032	393584.869412	52.012148
3318.817204	393327.213193	52.017153
3318.087150	393073.614909	52.022157
3317.457729	392805.201461	52.027162
3316.887665	392547.887375	52.032167
3315.868532	392279.582330	52.037172
3315.205088	392018.541542	52.042177
3314.425173	391756.551032	52.047181
3313.952534	391493.086100	52.052186
3312.833443	391232.314892	52.057191
3312.449155	390990.952999	52.062196
3312.186172	390729.330714	52.067201
3311.008974	390475.809645	52.072205
3310.504506	390215.137094	52.077210
3309.725433	389972.762726	52.082215
3308.887709	389703.087049	52.087220
3308.602964	389447.306993	52.092225
3307.653021	389194.249352	52.097229
3307.020302	388937.249281	52.102234
3306.407312	388690.771449	52.107239
3305.575514	388430.468148	52.112244
3305.032246	388176.855852	52.117249
3304.542823	387927.530682	52.122253
3303.891902	387676.042457	52.127258
3303.082954	387422.187154	52.132263
3302.571974	387161.976525	52.137268
3301.883997	386910.463413	52.142273
3300.972297	386661.425174	52.147277
3300.387881	386406.433794	52.152282
3299.483717	386156.729748	52.157287
3298.591474	385904.758844	52.162292
3298.191040	385658.913386	52.167297
3297.508703	385410.262674	52.172301
3296.752745	385162.054246	52.177306
3295.868403	384919.611789	52.182311
3295.422039	384672.037737	52.187316
3294.927339	384428.258898	52.192321
3293.847102	384180.883551	52.197325
3293.187796	383930.210207	52.202330
3292.661495	383685.719434	52.207335
3291.958073	383446.977206	52.212340
3291.293741	383205.200889	52.217345
3290.519217	382961.202430	52.222349
3290.108852	382714.677876	52.227354
3289.004749	382485.860609	52.232359
3288.318169	382241.207784	52.237364
3287.993400	381991.892847	52.242369
3286.875274	381755.316433	52.247373
3286.562330	381523.443464	52.252378
3286.265285	381275.060477	52.257383
3285.156711	381035.400687	52.262388
3284.671406	380800.193409	52.267393
3283.626817	380557.036134	52.272397
3283.130187	380315.011478	52.277402
3282.404646	380086.526924	52.282407
3282.022663	379846.922864	52.287412
3281.409493	379598.426477	52.292417
3280.451303	379366.439125	52.297421
3280.012291	379124.881193	52.302426
3279.304963	378892.190048	52.307431
3278.691104	378656.125339	52.312436
3277.819608	378409.595304	52.317441
3277.140581	378173.181913	52.322445
3276.538488	377930.040014	52.327450
3275.697977	377700.974709	52.332455
3274.947851	377454.902794	52.337460
3274.508482	377218.344055	52.342465
3273.815900	376988.615352	52.347469
3272.944111	376747.009593	52.352474
3272.198449	376516.294564	52.357479
3271.502789	376282.416191	52.362484
3270.831117	376058.274846	52.367489
3270.218348	375830.103947	52.372493
3269.993169	375587.167984	52.377498
3269.335642	375352.972950	52.382503
3268.440940	375116.473866	52.387508
3267.844754	374871.404711	52.392513
3267.179957	374641.302127	52.397517
3266.294806	374401.719462	52.402522
3265.760676	374170.576061	52.407527
3264.867282	373935.926890	52.412532
3264.380816	373705.790851	52.417537
3263.636384	373480.247754	52.422541
3263.080012	373241.801924	52.427546
3262.086117	373015.558046	52.432551
3261.674006	372788.915649	52.437556
3260.972821	372547.105413	52.442561
3259.964403	372317.018796	52.447565
3259.244762	372082.993074	52.452570
3258.826259	371854.693091	52.457575
3258.173185	371633.424763	52.462580
3257.303831	371404.099764	52.467585
3256.464807	371182.476894	52.472589
3256.148152	370946.931070	52.477594
3255.277434	370720.960621	52.482599
3254.367954	370493.773987	52.487604
3253.892033	370270.460771	52.492609
3253.066490	370064.424696	52.497613
3252.481420	369834.206741	52.502618
3251.646718	369609.878342	52.507623
3250.842722	369393.939307	52.512628
3250.495477	369176.375060	52.517633
3249.591899	368960.500492	52.522637
3249.282448	368733.642139	52.527642
3248.505685	368523.800288	52.532647
3247.692558	368303.430517	52.537652
3247.389913	368080.154896	52.542657
3246.677800	367863.252392	52.547661
3246.071479	367640.048006	52.552666
3245.622358	367418.471334	52.557671
3244.790166	367187.896842	52.562676
3244.276535	366957.423409	52.567681
3243.235334	366746.317354	52.572685
3242.703109	366514.368917	52.577690
3242.057971	366298.898348	52.582695
3241.293359	366073.879260	52.587700
3240.850483	365848.553720	52.592705
3239.952805	365630.804602	52.597709
3239.375157	365403.971585	52.602714
3238.411879	365189.716383	52.607719
3237.751729	364964.217242	52.612724
3237.478932	364744.991073	52.617729
3236.322738	364528.371593	52.622733
3235.642540	364313.075178	52.627738
3235.435430	364102.867963	52.632743
3234.431006	363872.761693	52.637748
3233.962672	363651.983693	52.642753
3233.049417	363433.310531	52.647757
3232.434092	363220.085128	52.652762
3231.591837	363011.220152	52.657767
3230.887179	362787.600203	52.662772
3230.422566	362569.411762	52.667777
3229.373540	362358.999004	52.672781
3228.922965	362149.839196	52.677786
3228.213426	361939.319955	52.682791
3227.563830	361729.477298	52.687796
3227.045614	361507.348420	52.692801
3226.116722	361311.822739	52.697805
3226.003531	361087.439531	52.702810
3225.103899	360870.940506	52.707815
3224.387041	360657.668601	52.712820
3223.896218	360441.382849	52.717825
3222.813714	360242.034774	52.722829
3222.232245	360012.936784	52.727834
3221.489835	359803.074845	52.732839
3220.952521	359598.574108	52.737844
3220.296284	359375.515619	52.742849
3219.370949	359171.532484	52.747853
3218.922647	358955.844029	52.752858
3218.009864	358749.261600	52.757863
3217.599682	358555.322084	52.762868
3217.126194	358341.212578	52.767873
3216.384293	358128.111576	52.772877
3215.632948	357903.458236	52.777882
3215.181586	357711.990246	52.782887
3214.132051	357498.146320	52.787892
3213.957722	357278.106569	52.792897
3213.074584	357065.786733	52.797901
3212.418798	356859.155705	52.802906
3211.672051	356640.196133	52.807911
3211.143295	356429.115347	52.812916
3210.241316	356209.415014	52.817921
3209.290703	356011.682956	52.822925
3208.833127	355796.236657	52.827930
3208.367622	355593.438404	52.832935
3207.351796	355389.810262	52.837940
3206.822313	355182.388910	52.842945
3206.069752	354977.343257	52.847949
3205.633108	354766.164603	52.852954
3204.990978	354560.361797	52.857959
3204.251016	354353.911975	52.862964
3203.981495	354136.825632	52.867969
3202.787009	353938.996858	52.872973
3202.020976	353724.125037	52.877978
3201.279522	353517.443060	52.882983
3200.654156	353315.297309	52.887988
3199.968696	353114.000108	52.892993
3199.272325	352916.623070	52.897997
3198.790040	352709.667844	52.903002
3198.341496	352500.797740	52.908007
3197.507774	352298.324728	52.913012
3197.020781	352092.207658	52.918017
3196.096261	351890.434591	52.923021
3195.454631	351678.283290	52.928026
3194.954362	351474.634573	52.933031
3194.111031	351270.988451	52.938036
3193.273772	351058.153025	52.943041
3192.487869	350868.443064	52.948045
3192.304921	350659.650961	52.953050
3191.288021	350470.485151	52.958055
3190.805958	350264.512956	52.963060
3190.581794	350058.880939	52.968065
3189.456952	349858.557167	52.973069
3188.779811	349652.333553	52.978074
3188.093134	349445.423489	52.983079
3187.181505	349239.998950	52.988084
3186.800607	349030.901047	52.993089
3185.949167	348839.005565	52.998093
3185.448846	348644.966848	53.003098
3184.866493	348444.653896	53.008103
3183.923243	348240.503218	53.013108
3183.327904	348035.278679	53.018113
3182.512484	347839.938060	53.023117
3182.082090	347632.064407	53.028122
3181.205395	347436.859338	53.033127
3180.461914	347239.138210	53.038132
3180.079799	347038.864904	53.043137
3178.891809	346848.593869	53.048141
3178.710506	346653.759670	53.053146
3177.778091	346451.560618	53.058151
3177.014741	346258.751540	53.063156
3176.466487	346059.824605	53.068161
3175.633848	345871.097605	53.073165
3174.939607	345675.144948	53.078170
3174.154948	345476.177039	53.083175
3173.553490	345288.506030	53.088180
3173.261274	345097.756576	53.093185
3172.517019	344920.211828	53.098189
3171.985117	344706.005775	53.103194
3171.251277	344514.586141	53.108199
3170.345617	344327.443781	53.113204
3170.028555	344122.008474	53.118209
3169.238994	343927.999493	53.123213
3168.821668	343735.101850	53.128218
3167.947666	343539.755914	53.133223
3167.082114	343349.906021	53.138228
3166.741783	343150.732666	53.143233
3165.773963	342964.486727	53.148237
3165.391940	342757.224299	53.153242
3164.585257	342572.809797	53.158247
3163.476834	342381.417109	53.163252
3163.170708	342184.042391	53.168257
3162.349103	342000.188500	53.173261
3161.721367	341805.765236	53.178266
3160.983614	341612.809668	53.183271
3160.610793	341432.624878	53.188276
3159.836893	341229.491978	53.193281
3158.990933	341043.475417	53.198285
3158.658968	340840.500407	53.203290
3158.093862	340657.161916	53.208295
3157.083261	340462.693168	53.213300
3156.436686	340264.067948	53.218305
3155.489663	340079.235422	53.223309
3155.247631	339888.843387	53.228314
3154.429920	339701.698318	53.233319
3153.595082	339514.657225	53.238324
3153.021588	339316.322911	53.243329
3152.250627	339135.303536	53.248333
3151.672510	338942.721739	53.253338
3150.863889	338757.608894	53.258343
3149.916484	338577.837728	53.263348
3149.794209	338396.459065	53.268353
3149.046719	338206.396524	53.273357
3148.322180	338021.293710	53.278362
3147.558250	337842.280596	53.283367
3146.844217	337653.254835	53.288372
3146.421388	337457.487468	53.293377
3145.309579	337275.269443	53.298381
3145.035846	337090.703604	53.303386
3144.520306	336903.629865	53.308391
3143.671561	336719.484900	53.313396
3143.252902	336533.183932	53.318401
3142.199811	336342.757022	53.323405
3141.581997	336161.221457	53.328410
3141.320547	335979.501727	53.333415
3140.384688	335793.076869	53.338420
3139.939798	335599.878638	53.343425
3138.843529	335416.278376	53.348429
3138.347038	335231.284404	53.353434
3137.668034	335041.609236	53.358439
3137.003069	334854.629780	53.363444
3136.474964	334665.846147	53.368449
3135.846362	334484.944212	53.373453
3135.304371	334291.986741	53.378458
3134.408406	334110.133284	53.383463
3133.801717	333925.051383	53.388468
3133.254870	333730.642031	53.393473
3132.551760	333546.643596	53.398477
3131.407719	333360.499619	53.403482
3131.247605	333164.627318	53.408487
3130.198704	332988.192184	53.413492
3129.581875	332802.116051	53.418497
3129.035072	332625.956974	53.423501
3128.589724	332437.943396	53.428506
3127.576743	332249.993680	53.433511
3126.784784	332073.311944	53.438516
3126.356737	331878.013101	53.443521
3125.705701	331700.926273	53.448525
3125.241006	331518.921509	53.453530
3124.646182	331327.288114	53.458535
3123.614971	331156.293764	53.463540
3123.377573	330955.234086	53.468545
3122.456086	330781.930220	53.473549
3121.579496	330587.895429	53.478554
3121.216220	330401.671131	53.483559
3120.366157	330223.568389	53.488564
3119.956189	330035.593893	53.493569
3118.787687	329863.370766	53.498573
3118.360480	329675.678135	53.503578
3117.898001	329490.994788	53.508583
3117.078347	329314.769032	53.513588
3116.582554	329116.265701	53.518593
3115.948092	328939.373280	53.523597
3115.273383	328754.747168	53.528602
3114.340573	328569.066692	53.533607
3113.682312	328391.056544	53.538612
3113.230024	328193.485916	53.543617
3112.655262	328025.772823	53.548621
3111.161643	327836.258531	53.553626
3111.082567	327657.620380	53.558631
3110.401702	327480.477332	53.563636
3109.793517	327289.039406	53.568641
3109.001474	327120.238501	53.573645
3108.326591	326930.897963	53.578650
3107.587688	326759.134516	53.583655
3106.695398	326577.083635	53.588660
3106.546684	326389.237060	53.593665
3105.846464	326226.962967	53.598669
3104.820066	326040.731145	53.603674
3104.706185	325861.890742	53.608679
3103.593268	325691.406266	53.613684
3103.228651	325505.424925	53.618689
3102.277355	325327.097754	53.623693
3101.631995	325137.213617	53.628698
3100.923016	324964.932374	53.633703
3100.072036	324788.446771	53.638708
3099.740633	324608.263149	53.643713
3098.920310	324435.769266	53.648717
3098.125585	324253.494021	53.653722
3097.609329	324079.831003	53.658727
3097.003132	323901.878960	53.663732
3096.304238	323713.731355	53.668737
3095.407328	323552.679736	53.673741
3094.699619	323386.098276	53.678746
3094.077725	323206.110354	53.683751
3093.260916	323037.177585	53.688756
3092.835203	322858.099943	53.693761
3091.906195	322690.253612	53.698765
3091.238641	322517.069619	53.703770
3090.835216	322348.986680	53.708775
3090.282435	322170.207784	53.713780
3089.605961	321993.535934	53.718785
3088.552362	321829.195865	53.723789
3088.311871	321655.662489	53.728794
3087.658743	321486.497084	53.733799
3087.004311	321311.118908	53.738804
3086.591599	321128.139994	53.743809
3085.691727	320953.411029	53.748813
3084.978614	320780.612728	53.753818
3084.269959	320601.065984	53.758823
3083.612275	320430.015103	53.763828
3083.080049	320254.182650	53.768833
3082.192120	320089.762213	53.773837
3081.537304	319899.256873	53.778842
3081.006959	319725.001744	53.783847
3080.113067	319561.447007	53.788852
3079.662733	319375.007623	53.793857
3079.238246	319208.653514	53.798861
3078.313049	319032.677195	53.803866
3077.792999	318856.712814	53.808871
3076.884946	318686.920485	53.813876
3076.311777	318505.107489	53.818881
3075.424682	318330.677026	53.823885
3074.773499	318161.199569	53.828890
3074.354122	317995.326278	53.833895
3073.513034	317836.292500	53.838900
3073.029855	317649.243771	53.843905
3071.950575	317476.140749	53.848909
3071.011823	317305.663307	53.853914
3070.686768	317133.025952	53.858919
3069.788659	316972.828478	53.863924
3069.346437	316812.609518	53.868929
3068.468427	316651.593521	53.873933
3068.058501	316479.630476	53.878938
3067.453847	316313.452598	53.883943
3066.669429	316147.404741	53.888948
3066.207758	315978.861068	53.893953
3065.381324	315814.729040	53.898957
3064.709642	315649.299091	53.903962
3064.312049	315471.908683	53.908967
3063.134064	315314.248216	53.913972
3062.661095	315143.311376	53.918977
3061.953612	314987.409301	53.923981
3061.365055	314817.686987	53.928986
3060.750905	314648.936054	53.933991
3059.928527	314488.799003	53.938996
3059.338927	314315.001862	53.944001
3058.787693	314156.807543	53.949005
3057.981870	313998.704203	53.954010
3057.533425	313824.043604	53.959015
3056.487749	313650.648564	53.964020
3056.253584	313493.498005	53.969025
3055.503120	313337.243764	53.974029
3054.882068	313168.287824	53.979034
3054.496628	312990.814858	53.984039
3053.527089	312835.689503	53.989044
3053.023636	312657.445282	53.994049
3052.077962	312488.234082	53.999053
3051.467877	312329.155121	54.004058
3050.732957	312159.477168	54.009063
3050.053072	312002.827867	54.014068
3049.677348	311830.826253	54.019073
3048.744098	311666.144438	54.024077
3048.096837	311496.629843	54.029082
3047.668428	311332.631563	54.034087
3046.776192	311174.512312	54.039092
3046.152104	310999.518474	54.044097
3045.675908	310840.518052	54.049101
3044.880510	310672.426203	54.054106
3044.339978	310505.057705	54.059111
3043.260555	310348.316546	54.064116
3043.141064	310166.799059	54.069121
3042.090186	310004.628974	54.074125
3041.344784	309842.104742	54.079130
3041.151089	309677.252079	54.084135
3040.058304	309513.076239	54.089140
3039.446593	309336.397259	54.094145
3038.577408	309183.772014	54.099149
3038.389222	309021.922406	54.104154
3037.920270	308842.546299	54.109159
3036.825750	308686.085434	54.114164
3036.569422	308515.969857	54.119169
3035.704360	308352.087430	54.124173
3034.858697	308184.025462	54.129178
3034.535445	308012.621065	54.134183
3033.419977	307861.484640	54.139188
3032.874514	307691.591939	54.144193
3031.972627	307533.774935	54.149197
3031.686477	307377.362721	54.154202
3031.055117	307205.955050	54.159207
3030.158477	307051.548941	54.164212
3029.944989	306880.813184	54.169217
3029.205743	306717.901845	54.174221
3028.478205	306548.596663	54.179226
3027.907565	306364.598407	54.184231
3027.071032	306200.428549	54.189236
3026.172329	306041.004884	54.194241
3025.775321	305874.294910	54.199245
3024.810275	305712.716789	54.204250
3024.151918	305542.584463	54.209255
3023.462881	305383.661598	54.214260
3023.073040	305209.259075	54.219265
3022.249622	305061.179950	54.224269
3021.633572	304891.855003	54.229274
3020.762286	304728.121750	54.234279
3020.175002	304563.732175	54.239284
3019.350319	304404.371253	54.244289
3018.730879	304249.026711	54.249293
3017.970321	304090.164594	54.254298
3017.399475	303927.350541	54.259303
3016.578659	303779.167767	54.264308
3016.117609	303611.904924	54.269313
3015.268017	303458.200286	54.274317
3014.800657	303285.386502	54.279322
3014.376172	303132.658332	54.284327
3013.463453	302979.497959	54.289332
3012.894776	302819.101567	54.294337
3012.232857	302662.030338	54.299341
3011.605174	302497.186386	54.304346
3011.164094	302336.234487	54.309351
3010.255493	302178.132216	54.314356
3009.764243	302005.015116	54.319361
3009.141167	301847.071033	54.324365
3008.380023	301688.562918	54.329370
3008.091793	301519.029324	54.334375
3007.116065	301362.515733	54.339380
3006.340466	301196.955257	54.344385
3005.688270	301039.065886	54.349389
3005.226296	300870.755999	54.354394
3004.782652	300699.870932	54.359399
3003.558161	300539.856075	54.364404
3003.243579	300376.259074	54.369409
3002.524693	300221.180745	54.374413
3001.732348	300052.693090	54.379418
3000.931888	299882.653092	54.384423
3000.085095	299729.911988	54.389428
2999.659753	299563.453989	54.394433
2998.690888	299410.502714	54.399437
2998.271263	299252.396519	54.404442
2997.958547	299085.996618	54.409447
2997.101627	298931.626526	54.414452
2996.659595	298768.430107	54.419457
2995.876658	298606.535358	54.424461
2994.816717	298445.499237	54.429466
2994.402988	298276.593339	54.434471
2993.390826	298112.467878	54.439476
2993.176922	297953.207392	54.444481
2992.262170	297791.409155	54.449485
2991.481457	297641.304275	54.454490
2991.232885	297482.303524	54.459495
2990.625086	297323.410429	54.464500
2989.714975	297157.128728	54.469505
2989.104294	296993.167899	54.474509
2988.328017	296835.115990	54.479514
2987.638610	296675.191112	54.484519
2987.016550	296525.340345	54.489524
2986.433721	296351.951779	54.494529
2986.243878	296188.382040	54.499533
2985.330891	296031.548049	54.504538
2984.835681	295868.382913	54.509543
2984.181327	295713.952561	54.514548
2983.439680	295540.639343	54.519553
2982.787246	295367.566522	54.524557
2981.943311	295208.174237	54.529562
2981.271112	295037.982044	54.534567
2980.605626	294875.887201	54.539572
2980.010610	294707.159610	54.544577
2979.397229	294544.852522	54.549581
2978.672700	294390.992547	54.554586
2978.202192	294216.896737	54.559591
2977.555586	294063.380730	54.564596
2976.804078	293889.329132	54.569601
2976.104685	293724.488303	54.574605
2975.720517	293557.509132	54.579610
2974.823552	293394.787649	54.584615
2974.115980	293222.205670	54.589620
2973.702069	293053.702786	54.594625
2973.039179	292888.371677	54.599629
2972.206859	292728.491826	54.604634
2972.081376	292549.323004	54.609639
2971.068821	292376.635857	54.614644
2970.420719	292203.407010	54.619649
2969.732187	292039.174457	54.624653
2969.241110	291878.043036	54.629658
2968.161977	291707.403343	54.634663
2967.472964	291547.067060	54.639668
2967.137076	291359.882913	54.644673
2966.104897	291203.140720	54.649677
2965.522345	291043.984236	54.654682
2964.793391	290866.106675	54.659687
2963.872757	290700.330984	54.664692
2963.165878	290538.137753	54.669697
2962.694159	290380.465906	54.674701
2962.034005	290216.125798	54.679706
2961.588248	290053.126905	54.684711
2960.829423	289894.099497	54.689716
2960.067248	289730.080857	54.694721
2959.529263	289567.045338	54.699725
2958.614673	289403.509052	54.704730
2958.280720	289237.996141	54.709735
2957.314488	289076.530729	54.714740
2957.003130	288911.421538	54.719745
2956.020729	288754.950192	54.724749
2955.371795	288589.410371	54.729754
2954.980784	288423.473079	54.734759
2954.055919	288260.447137	54.739764
2953.901686	288080.184719	54.744769
2953.422950	287923.760552	54.749773
2952.321369	287746.423908	54.754778
2951.959417	287579.921272	54.759783
2950.997074	287418.938259	54.764788
2950.349601	287248.711403	54.769793
2949.943917	287082.368245	54.774797
2948.889792	286905.583928	54.779802
2948.584440	286734.564082	54.784807
2947.615302	286581.400408	54.789812
2947.056567	286411.490171	54.794817
2946.385563	286241.062798	54.799821
2946.026880	286071.528218	54.804826
2945.250696	285891.108406	54.809831
2944.709004	285726.874520	54.814836
2943.969990	285565.702496	54.819841
2943.287383	285393.366470	54.824845
2942.276222	285218.943063	54.829850
2941.395032	285048.446556	54.834855
2940.639410	284894.840905	54.839860
2940.702886	284736.699546	54.844865
2939.797772	284568.473288	54.849869
2939.200023	284404.222265	54.854874
2938.585356	284224.056283	54.859879
2937.672189	284068.055803	54.864884
2937.194348	283892.757906	54.869889
2936.723385	283727.187686	54.874893
2935.953924	283561.231705	54.879898
2935.465817	283383.872321	54.884903
2934.482443	283225.998029	54.889908
2933.975701	283049.813010	54.894913
2933.226418	282884.159223	54.899917
2932.587294	282718.437006	54.904922
2932.170764	282547.229301	54.909927
2931.347849	282371.654407	54.914932
2930.806760	282198.428854	54.919937
2930.097423	282023.905536	54.924941
2929.212182	281860.947126	54.929946
2928.646079	281677.792762	54.934951
2927.861501	281524.750942	54.939956
2927.385998	281342.830080	54.944961
2926.669064	281169.148171	54.949965
2926.176316	281007.069726	54.954970
2925.755920	280827.279332	54.959975
2924.770178	280659.268339	54.964980
2924.162000	280491.426747	54.969985
2923.653075	280324.919223	54.974989
2922.772204	280146.602318	54.979994
2922.376238	279975.772691	54.984999
2921.165904	279802.499658	54.990004
2920.605779	279627.977575	54.995009
2919.949753	279465.313412	55.000013
2919.001918	279299.741092	55.005018
2918.859923	279128.743750	55.010023
2918.086784	278959.730957	55.015028
2917.494722	278790.816810	55.020033
2916.909438	278622.971233	55.025037
2916.061452	278447.781400	55.030042
2915.801492	278272.982343	55.035047
2915.089491	278105.156754	55.040052
2914.616618	277935.077537	55.045057
2913.729781	277761.498266	55.050061
2912.688645	277580.633982	55.055066
2912.407416	277406.602233	55.060071
2911.486097	277239.344519	55.065076
2911.048056	277064.981005	55.070081
2910.282748	276898.029650	55.075085
2909.681126	276726.671805	55.080090
2909.119839	276540.153874	55.085095
2908.381670	276374.904566	55.090100
2907.882878	276183.716001	55.095105
2907.150690	276004.381709	55.100109
2906.373394	275832.975220	55.105114
2905.609100	275648.170292	55.110119
2905.012585	275477.295473	55.115124
2904.505116	275310.608837	55.120129
2903.692654	275139.640860	55.125133
2902.810152	274966.544625	55.130138
2902.245767	274787.922321	55.135143
2901.401514	274619.200596	55.140148
2900.574231	274444.287367	55.145153
2899.942005	274279.097652	55.150157
2899.346200	274112.857972	55.155162
2898.639902	273936.550310	55.160167
2898.316335	273776.379953	55.165172
2897.764934	273591.337595	55.170177
2896.776030	273426.586413	55.175181
2895.838890	273258.312409	55.180186
2895.572260	273085.526227	55.185191
2894.557008	272922.332823	55.190196
2893.989080	272745.366622	55.195201
2893.619285	272582.886041	55.200205
2892.958565	272418.133915	55.205210
2892.242555	272245.902859	55.210215
2891.325234	272072.201064	55.215220
2891.041186	271899.392289	55.220225
2890.388291	271736.651002	55.225229
2889.804821	271570.053021	55.230234
2889.403452	271396.906333	55.235239
2888.427519	271222.679099	55.240244
2887.450664	271046.083482	55.245249
2887.194837	270878.364058	55.250253
2886.385667	270710.146501	55.255258
2886.006963	270527.853236	55.260263
2885.113543	270359.547208	55.265268
2884.571251	270176.541334	55.270273
2884.000600	270001.893595	55.275277
2882.968545	269832.845572	55.280282
2882.554435	269656.390341	55.285287
2881.620319	269494.407073	55.290292
2881.135634	269309.100129	55.295297
2880.650744	269129.141604	55.300301
2879.985949	268957.463334	55.305306
2879.279299	268788.796990	55.310311
2878.482421	268624.067088	55.315316
2877.906598	268443.460970	55.320321
2877.318934	268277.653833	55.325325
2876.459334	268099.741446	55.330330
2875.961009	267923.809367	55.335335
2875.287616	267752.616684	55.340340
2874.227419	267571.578160	55.345345
2873.974176	267403.146031	55.350349
2873.322066	267224.895446	55.355354
2872.862567	267046.792701	55.360359
2871.753734	266865.227285	55.365364
2871.333826	266698.884695	55.370369
2870.460833	266531.264089	55.375373
2869.596174	266356.689414	55.380378
2869.337076	266175.753752	55.385383
2868.241789	266008.321338	55.390388
2867.873980	265835.425488	55.395393
2867.270046	265668.552102	55.400397
2866.623834	265499.673493	55.405402
2866.245208	265325.557087	55.410407
2865.160542	265148.369035	55.415412
2864.719394	264975.867164	55.420417
2864.337956	264800.987379	55.425421
2863.618788	264622.493746	55.430426
2862.812718	264435.991519	55.435431
2862.207426	264263.668754	55.440436
2861.465629	264082.988702	55.445441
2860.822409	263909.627914	55.450445
2859.671017	263737.977626	55.455450
2859.530559	263567.975571	55.460455
2859.146848	263395.312508	55.465460
2858.263061	263207.065916	55.470465
2857.744839	263033.099997	55.475469
2856.872400	262856.617993	55.480474
2856.067767	262673.045261	55.485479
2855.377953	262494.828179	55.490484
2854.844523	262319.387899	55.495489
2854.262574	262150.144093	55.500493
2853.594307	261979.564247	55.505498
2853.265258	261795.840303	55.510503
2852.378793	261611.720843	55.515508
2851.996567	261426.783082	55.520513
2851.566583	261239.968379	55.525517
2850.505725	261069.069189	55.530522
2849.660551	260873.381267	55.535527
2849.162687	260695.058428	55.540532
2848.060740	260515.354227	55.545537
2847.613555	260333.865589	55.550541
2847.125043	260160.889828	55.555546
2846.178110	259989.820441	55.560551
2845.854375	259809.407710	55.565556
2845.255147	259619.233674	55.570561
2844.682974	259438.402114	55.575565
2843.845265	259257.892871	55.580570
2843.485039	259076.162100	55.585575
2842.701428	258899.260941	55.590580
2841.970643	258709.643221	55.595585
2841.255901	258520.889000	55.600589
2840.497276	258343.271183	55.605594
2839.958026	258154.744128	55.610599
2839.439161	257978.743998	55.615604
2838.720110	257790.882386	55.620609
2838.038777	257608.159374	55.625613
2837.133671	257431.074776	55.630618
2836.539536	257241.436568	55.635623
2835.910083	257065.683839	55.640628
2835.001319	256876.554168	55.645633
2834.111901	256697.124653	55.650637
2833.342675	256521.801959	55.655642
2833.243576	256340.795943	55.660647
2832.351347	256182.632499	55.665652
2831.747743	255992.283764	55.670657
2831.231694	255809.561506	55.675661
2830.379195	255632.113467	55.680666
2829.492782	255453.219316	55.685671
2828.912315	255273.130846	55.690676
2828.502293	255096.479075	55.695681
2827.767967	254910.481436	55.700685
2826.891741	254737.571071	55.705690
2826.583932	254563.322952	55.710695
2826.029763	254390.591088	55.715700
2825.432489	254212.721855	55.720705
2824.665714	254020.567154	55.725709
2823.776862	253844.807259	55.730714
2823.032443	253668.489844	55.735719
2822.565584	253484.896021	55.740724
2821.877804	253304.546193	55.745729
2821.569066	253121.666222	55.750733
2820.484589	252945.454266	55.755738
2820.157863	252757.127588	55.760743
2819.612676	252578.385761	55.765748
2818.871140	252395.855181	55.770753
2818.342271	252206.236809	55.775757
2817.736157	252027.989042	55.780762
2816.950217	251834.133358	55.785767
2816.401091	251643.143589	55.790772
2815.825676	251456.767660	55.795777
2815.053321	251270.652317	55.800781
2814.149793	251087.053677	55.805786
2813.443356	250889.137265	55.810791
2813.077012	250715.589658	55.815796
2812.541769	250524.980931	55.820801
2811.801025	250340.695193	55.825805
2810.856377	250150.253596	55.830810
2810.256652	249963.017301	55.835815
2809.647901	249777.514366	55.840820
2809.084983	249586.096183	55.845825
2808.190649	249400.587975	55.850829
2807.539619	249206.204634	55.855834
2806.995431	249020.386754	55.860839
2806.419957	248839.208909	55.865844
2805.365301	248662.054428	55.870849
2804.944512	248472.932511	55.875853
2804.111577	248286.269916	55.880858
2803.250677	248100.477828	55.885863
2802.785252	247923.027154	55.890868
2802.248559	247729.035019	55.895873
2801.936466	247551.967957	55.900877
2800.587834	247371.882007	55.905882
2800.259273	247176.380599	55.910887
2799.631844	246997.250463	55.915892
2798.699605	246810.172516	55.920897
2798.069107	246640.109176	55.925901
2797.273375	246454.385230	55.930906
2797.259991	246267.493525	55.935911
2796.321262	246092.793935	55.940916
2795.860861	245895.201480	55.945921
2795.142273	245707.072513	55.950925
2794.307196	245531.313111	55.955930
2793.779388	245340.276801	55.960935
2792.898940	245156.554308	55.965940
2792.116552	244967.647015	55.970945
2791.877550	244779.876274	55.975949
2790.463518	244605.355701	55.980954
2790.199501	244421.536576	55.985959
2789.421465	244244.929439	55.990964
2788.850786	244052.857650	55.995969
2788.492551	243870.938649	56.000973
2787.585317	243690.762095	56.005978
2787.006123	243501.544579	56.010983
2786.471964	243320.188978	56.015988
2785.503804	243143.053201	56.020993
2785.358600	242950.279021	56.025997
2784.082765	242765.196421	56.031002
2783.594140	242580.269533	56.036007
2782.890503	242396.650224	56.041012
2782.150123	242217.773502	56.046017
2781.372299	242025.839413	56.051021
2780.679013	241859.255353	56.056026
2780.311609	241671.152955	56.061031
2779.884470	241497.473444	56.066036
2779.051863	241313.112220	56.071041
2778.577316	241127.013889	56.076045
2777.229067	240944.237320	56.081050
2777.110621	240759.993016	56.086055
2776.281546	240584.774196	56.091060
2775.989506	240399.462960	56.096065
2775.479083	240214.925076	56.101069
2774.462949	240030.136537	56.106074
2773.993027	239837.062194	56.111079
2773.083620	239654.065330	56.116084
2772.246051	239465.353337	56.121089
2771.854477	239278.710028	56.126093
2771.126573	239097.391421	56.131098
2770.673050	238908.415804	56.136103
2769.998799	238728.184255	56.141108
2769.048093	238540.535749	56.146113
2768.787920	238348.474736	56.151117
2767.653682	238165.414024	56.156122
2767.536408	237973.763915	56.161127
2766.873453	237792.793628	56.166132
2766.054744	237595.067497	56.171137
2765.537677	237402.437679	56.176141
2764.860614	237214.569838	56.181146
2764.299512	237022.024061	56.186151
2762.855082	236838.734598	56.191156
2762.772909	236644.840448	56.196161
2762.248094	236457.688269	56.201165
2761.334050	236272.431456	56.206170
2760.791544	236079.400624	56.211175
2760.122756	235896.015405	56.216180
2759.232554	235706.095968	56.221185
2758.993162	235521.573926	56.226189
2758.065683	235334.080112	56.231194
2757.254809	235135.898980	56.236199
2756.413274	234959.035964	56.241204
2755.981933	234774.902150	56.246209
2755.543931	234569.431464	56.251213
2754.806244	234397.441933	56.256218
2754.430623	234194.279288	56.261223
2753.703029	234008.895170	56.266228
2752.636566	233810.757118	56.271233
2752.238998	233625.143201	56.276237
2751.591859	233439.212680	56.281242
2750.955843	233235.176570	56.286247
2750.340791	233055.963918	56.291252
2749.571473	232867.201987	56.296257
2749.254451	232671.468356	56.301261
2748.544456	232491.533363	56.306266
2747.432330	232287.218180	56.311271
2746.528196	232099.701316	56.316276
2746.270307	231911.827836	56.321281
2745.358203	231723.829186	56.326285
2744.477112	231531.599220	56.331290
2744.210312	231342.149607	56.336295
2743.435271	231153.952150	56.341300
2742.713393	230978.248677	56.346305
2742.113677	230782.156328	56.351309
2741.663961	230603.329517	56.356314
2740.546134	230407.752888	56.361319
2739.779177	230222.433278	56.366324
2739.412207	230043.339830	56.371329
2739.109254	229852.116652	56.376333
2738.273318	229668.234973	56.381338
2737.781676	229467.468782	56.386343
2737.086986	229277.658355	56.391348
2736.319385	229094.607269	56.396353
2735.675501	228903.261881	56.401357
2734.948897	228710.911538	56.406362
2734.150966	228508.464626	56.411367
2734.055236	228328.898799	56.416372
2733.401483	228142.470719	56.421377
2732.712653	227947.595370	56.426381
2731.885163	227755.390414	56.431386
2731.527321	227545.543128	56.436391
2730.597059	227355.697789	56.441396
2729.969835	227170.591591	56.446401
2729.053990	226972.749975	56.451405
2728.445675	226779.748650	56.456410
2727.885980	226579.712797	56.461415
2727.236179	226387.355467	56.466420
2726.327913	226190.634766	56.471425
2725.867949	226003.556862	56.476429
2725.186850	225811.498613	56.481434
2724.549547	225609.656917	56.486439
2723.729172	225414.935533	56.491444
2722.936533	225234.137214	56.496449
2722.420857	225037.217030	56.501453
2721.578378	224843.327973	56.506458
2721.058691	224655.638802	56.511463
2720.474852	224470.875450	56.516468
2719.617184	224279.281588	56.521473
2719.139530	224090.772337	56.526477
2718.481454	223896.576276	56.531482
2718.139863	223703.667216	56.536487
2717.376454	223512.582190	56.541492
2716.240713	223323.771632	56.546497
2716.059511	223128.572614	56.551501
2714.899190	222941.829126	56.556506
2714.598971	222742.818192	56.561511
2714.033778	222556.885177	56.566516
2713.304745	222364.664532	56.571521
2713.008984	222163.935834	56.576525
2711.931507	221975.526659	56.581530
2711.696169	221777.526307	56.586535
2710.864839	221580.066415	56.591540
2709.973619	221379.090386	56.596545
2709.429571	221181.267775	56.601549
2708.771372	220986.722555	56.606554
2708.129213	220789.247480	56.611559
2707.779876	220586.138245	56.616564
2706.929698	220395.914834	56.621569
2706.107546	220198.431637	56.626573
2705.394903	220006.596240	56.631578
2704.870453	219806.139140	56.636583
2704.125372	219611.305752	56.641588
2703.120852	219415.546542	56.646593
2702.666376	219224.716090	56.651597
2702.190351	219032.603885	56.656602
2701.360126	218836.093042	56.661607
2700.795850	218637.567566	56.666612
2699.971368	218448.083415	56.671617
2699.504748	218248.652489	56.676621
2698.916549	218061.881428	56.681626
2698.319533	217854.541987	56.686631
2697.530975	217671.609690	56.691636
2696.698468	217462.272039	56.696641
2696.374838	217266.779935	56.701645
2695.293915	217075.036095	56.706650
2694.707142	216871.058354	56.711655
2693.711050	216685.908459	56.716660
2693.136090	216489.809151	56.721665
2692.861884	216293.599105	56.726669
2691.915666	216115.851006	56.731674
2691.415739	215921.701648	56.736679
2691.069247	215723.175300	56.741684
2690.131883	215527.008837	56.746689
2689.729222	215340.075609	56.751693
2688.721546	215147.409023	56.756698
2688.032357	214949.117406	56.761703
2687.491213	214755.868878	56.766708
2686.769874	214564.202325	56.771713
2686.324034	214365.428365	56.776717
2685.334540	214172.277989	56.781722
2684.660188	213976.672576	56.786727
2684.221244	213784.428916	56.791732
2683.449152	213589.896573	56.796737
2682.806086	213390.889455	56.801741
2681.862732	213202.647700	56.806746
2681.609171	213011.026051	56.811751
2680.917576	212822.732767	56.816756
2680.124718	212619.487763	56.821761
2679.520542	212418.135443	56.826765
2678.744195	212240.154301	56.831770
2678.471663	212042.734488	56.836775
2678.109363	211844.985840	56.841780
2676.677741	211642.023275	56.846785
2676.559183	211444.415431	56.851789
2675.795580	211258.467297	56.856794
2675.332564	211051.865709	56.861799
2674.194831	210855.401185	56.866804
2673.434132	210661.308538	56.871809
2673.094748	210457.769409	56.876813
2672.210215	210267.859551	56.881818
2671.621571	210082.625344	56.886823
2671.227458	209878.460370	56.891828
2670.296923	209677.855668	56.896833
2669.701636	209476.943948	56.901837
2668.518560	209283.927942	56.906842
2668.357347	209097.572556	56.911847
2667.443410	208901.384150	56.916852
2666.928002	208710.771453	56.921857
2666.363793	208506.777932	56.926861
2665.448674	208316.802509	56.931866
2664.776172	208131.778318	56.936871
2664.471595	207934.605555	56.941876
2663.449461	207740.945263	56.946881
2663.202456	207548.270046	56.951885
2662.263360	207356.341442	56.956890
2661.623528	207159.542489	56.961895
2661.161169	206966.495981	56.966900
2660.462031	206773.500334	56.971905
2660.120186	206579.417822	56.976909
2658.909260	206386.033612	56.981914
2658.372861	206188.343311	56.986919
2657.638407	205989.832351	56.991924
2656.854785	205798.609547	56.996929
2656.560911	205605.362585	57.001933
2655.647611	205410.241760	57.006938
2655.186381	205202.336068	57.011943
2654.482776	205011.141329	57.016948
2653.488420	204820.133274	57.021953
2653.339871	204622.806766	57.026957
2652.231376	204432.632564	57.031962
2651.641273	204234.702832	57.036967
2651.199427	204052.734607	57.041972
2650.317743	203846.211202	57.046977
2649.829903	203655.419455	57.051981
2648.902982	203459.034733	57.056986
2648.359952	203266.445902	57.061991
2647.738702	203083.707431	57.066996
2647.064215	202892.438762	57.072001
2646.755293	202691.262845	57.077005
2645.736926	202494.654154	57.082010
2645.535002	202296.567841	57.087015
2644.779719	202092.690519	57.092020
2644.038722	201902.352018	57.097025
2643.520266	201700.207503	57.102029
2642.514712	201505.585485	57.107034
2641.955519	201301.107328	57.112039
2641.673995	201109.324362	57.117044
2640.482354	200918.424346	57.122049
2640.304116	200708.339637	57.127053
2639.191881	200521.513339	57.132058
2638.757551	200314.423044	57.137063
2638.307322	200120.748701	57.142068
2637.504765	199920.742704	57.147073
2637.050321	199717.131905	57.152077
2636.163307	199518.858696	57.157082
2635.751986	199308.332745	57.162087
2635.019197	199111.932662	57.167092
2634.198530	198904.858058	57.172097
2633.716154	198697.743380	57.177101
2633.046317	198499.566770	57.182106
2632.446532	198302.028774	57.187111
2631.924968	198105.942493	57.192116
2630.594165	197899.945167	57.197121
2630.219630	197685.220547	57.202125
2629.214039	197500.258413	57.207130
2628.908583	197302.092170	57.212135
2628.580916	197108.689253	57.217140
2627.497440	196908.611807	57.222145
2626.970752	196694.577027	57.227149
2626.313663	196493.479265	57.232154
2625.647254	196285.156207	57.237159
2624.793145	196084.269390	57.242164
2623.863421	195889.312208	57.247169
2623.297522	195684.474872	57.252173
2622.751004	195501.775670	57.257178
2622.187232	195294.979996	57.262183
2621.505130	195096.029328	57.267188
2620.770332	194901.566708	57.272193
2620.164527	194696.930507	57.277197
2619.332064	194508.528843	57.282202
2618.485863	194301.387504	57.287207
2618.198412	194113.677121	57.292212
2617.388020	193910.068989	57.297217
2616.751351	193715.175487	57.302221
2616.080197	193524.181709	57.307226
2615.436191	193322.203701	57.312231
2614.934929	193126.260405	57.317236
2613.972906	192936.409206	57.322241
2613.259340	192739.368661	57.327245
2612.382122	192539.733765	57.332250
2611.940608	192341.201205	57.337255
2611.896380	192152.365430	57.342260
2610.921902	191967.609329	57.347265
2610.354727	191753.512799	57.352269
2609.182927	191565.074244	57.357274
2608.598570	191361.326249	57.362279
2608.416457	191167.910273	57.367284
2607.433319	190972.459043	57.372289
2607.006665	190765.889445	57.377293
2606.309345	190585.751338	57.382298
2605.682939	190379.176873	57.387303
2604.865444	190190.242207	57.392308
2603.962042	189998.357448	57.397313
2603.485969	189793.848240	57.402317
2602.703336	189597.327537	57.407322
2602.143816	189401.841004	57.412327
2601.688220	189209.646719	57.417332
2601.320592	189009.754766	57.422337
2600.727141	188806.667886	57.427341
2599.820506	188609.687453	57.432346
2598.959947	188403.184089	57.437351
2598.651838	188199.151309	57.442356
2597.621623	188010.488018	57.447361
2597.030433	187807.774035	57.452365
2596.228523	187612.905822	57.457370
2595.493494	187412.150140	57.462375
2595.073692	187209.093543	57.467380
2594.070501	187019.717533	57.472385
2593.469620	186822.301790	57.477389
2592.535042	186626.937129	57.482394
2591.992114	186431.511234	57.487399
2591.528501	186231.442815	57.492404
2590.837728	186045.303557	57.497409
2590.575881	185845.306623	57.502413
2590.176461	185657.863311	57.507418
2589.219963	185446.783033	57.512423
2589.177464	185238.421275	57.517428
2587.651502	185039.442373	57.522433
2587.265760	184834.431754	57.527437
2586.533639	184645.060777	57.532442
2586.157262	184441.564313	57.537447
2585.718175	184238.282247	57.542452
2584.515378	184031.903625	57.547457
2583.954443	183828.668165	57.552461
2583.018678	183631.459269	57.557466
2582.349262	183423.090756	57.562471
2582.049858	183221.025128	57.567476
2581.241175	183027.169859	57.572481
2580.472126	182831.032102	57.577485
2579.883404	182631.635526	57.582490
2579.602928	182428.527396	57.587495
2578.964168	182219.574526	57.592500
2577.874884	182021.493950	57.597505
2577.531247	181811.135137	57.602509
2576.703607	181611.526634	57.607514
2576.031478	181410.469697	57.612519
2575.221747	181208.227045	57.617524
2574.632768	181006.128439	57.622529
2574.167291	180798.337910	57.627533
2573.223338	180608.012888	57.632538
2572.307720	180396.110636	57.637543
2572.109847	180199.716102	57.642548
2571.030742	180004.517883	57.647553
2570.720586	179797.458052	57.652557
2569.970773	179601.166440	57.657562
2569.316988	179398.118926	57.662567
2568.698215	179196.644100	57.667572
2567.985206	178991.063928	57.672577
2567.831538	178799.273406	57.677581
2566.854967	178601.953873	57.682586
2566.171292	178383.334276	57.687591
2565.466971	178177.171575	57.692596
2564.729879	177987.397852	57.697601
2563.926218	177776.088724	57.702605
2563.132689	177571.405872	57.707610
2562.856401	177376.474121	57.712615
2562.177648	177181.823286	57.717620
2561.372015	176970.391349	57.722625
2560.766481	176775.921598	57.727629
2559.990855	176576.163120	57.732634
2559.424550	176375.622010	57.737639
2558.769173	176170.695216	57.742644
2557.984595	175968.829739	57.747649
2557.477679	175769.337836	57.752653
2556.953020	175566.606416	57.757658
2556.139677	175362.522686	57.762663
2555.216122	175161.611673	57.767668
2554.656655	174968.325997	57.772673
2554.005591	174760.047853	57.777677
2553.288666	174564.944854	57.782682
2552.827271	174362.425607	57.787687
2552.078513	174165.981419	57.792692
2551.321597	173968.725506	57.797697
2550.697000	173766.196954	57.802701
2550.038992	173570.987669	57.807706
2549.380247	173367.487235	57.812711
2548.657609	173161.632402	57.817716
2548.127037	172964.790679	57.822721
2547.728881	172766.288328	57.827725
2547.014064	172558.642135	57.832730
2546.168352	172352.251395	57.837735
2545.730093	172148.620491	57.842740
2544.420869	171965.438779	57.847745
2544.584984	171761.078519	57.852749
2543.696342	171558.882812	57.857754
2543.141858	171356.889534	57.862759
2542.478739	171146.902542	57.867764
2541.486568	170945.947265	57.872769
2541.278534	170735.572421	57.877773
2540.272078	170536.821598	57.882778
2539.493371	170328.777614	57.887783
2539.206781	170125.095009	57.892788
2538.212588	169929.130385	57.897793
2537.839466	169726.023135	57.902797
2537.362067	169520.250215	57.907802
2536.730255	169309.327122	57.912807
2536.216643	169098.182982	57.917812
2535.091493	168891.066370	57.922817
2534.577238	168678.398637	57.927821
2534.007344	168484.141721	57.932826
2533.255186	168268.576449	57.937831
2532.783430	168061.818563	57.942836
2531.827772	167859.016969	57.947841
2531.200523	167648.763547	57.952845
2530.463616	167444.009345	57.957850
2529.639466	167232.759425	57.962855
2529.202239	167034.585039	57.967860
2528.259104	166839.213094	57.972865
2527.767058	166629.973903	57.977869
2526.871291	166440.038934	57.982874
2526.445084	166232.088541	57.987879
2525.853274	166018.392617	57.992884
2524.971573	165816.582115	57.997889
2524.773267	165616.012244	58.002893
2523.800176	165417.766028	58.007898
2523.415014	165206.635967	58.012903
2522.664786	164997.675714	58.017908
2521.690548	164791.155333	58.022913
2521.426616	164579.590027	58.027917
2520.618826	164383.192288	58.032922
2520.038739	164177.515649	58.037927
2519.416848	163972.431675	58.042932
2518.447209	163764.009076	58.047937
2517.584275	163557.071105	58.052941
2517.176900	163354.537709	58.057946
2516.767751	163130.848433	58.062951
2516.076787	162881.737796	58.067956
2515.419839	162675.217198	58.072961
2515.141041	162457.970394	58.077965
2514.289083	162255.780587	58.082970
2513.471829	162044.940665	58.087975
2512.971856	161830.885840	58.092980
2512.019561	161633.292558	58.097985
2511.420305	161428.499076	58.102989
2510.576981	161218.291126	58.107994
2509.846886	161009.083580	58.112999
2509.361447	160791.231181	58.118004
2508.551459	160588.891546	58.123009
2508.091972	160385.060855	58.128013
2507.436957	160186.983475	58.133018
2506.528274	159978.598538	58.138023
2505.826869	159770.512527	58.143028
2505.291161	159566.113804	58.148033
2504.744576	159354.356947	58.153037
2503.609130	159156.425057	58.158042
2502.984666	158954.764596	58.163047
2502.744156	158747.959177	58.168052
2501.664107	158557.726055	58.173057
2501.521438	158338.830118	58.178061
2500.474046	158148.072818	58.183066
2499.792836	157944.583801	58.188071
2499.433873	157735.947072	58.193076
2498.364459	157540.314889	58.198081
2497.950672	157336.329391	58.203085
2497.085598	157145.434290	58.208090
2496.327149	156932.276484	58.213095
2495.771094	156729.295981	58.218100
2494.658852	156538.379855	58.223105
2494.438148	156332.971329	58.228109
2493.833820	156144.176112	58.233114
2493.338565	155937.554963	58.238119
2492.776928	155743.060163	58.243124
2492.103390	155532.414579	58.248129
2491.489544	155324.811690	58.253133
2490.661024	155118.133921	58.258138
2489.888575	154922.495023	58.263143
2489.410563	154716.755657	58.268148
2488.588703	154516.321929	58.273153
2488.118890	154306.325378	58.278157
2487.296383	154105.004389	58.283162
2486.494300	153911.015821	58.288167
2486.051819	153712.319042	58.293172
2485.260469	153511.492410	58.298177
2485.066005	153297.734129	58.303181
2483.919432	153101.910887	58.308186
2483.434832	152899.297894	58.313191
2482.681137	152689.750502	58.318196
2481.796245	152499.583804	58.323201
2481.355904	152290.777329	58.328205
2480.566558	152089.475937	58.333210
2480.102961	151892.077128	58.338215
2479.538636	151694.237885	58.343220
2478.926417	151487.421141	58.348225
2478.437757	151276.569637	58.353229
2477.541332	151076.956450	58.358234
2476.586353	150875.116763	58.363239
2476.205443	150668.509999	58.368244
2475.305360	150476.349179	58.373249
2474.921737	150279.506617	58.378253
2474.218552	150065.659227	58.383258
2473.492088	149865.136804	58.388263
2473.116999	149652.866974	58.393268
2472.320508	149459.348503	58.398273
2471.788438	149247.830656	58.403277
2470.992273	149046.307577	58.408282
2470.030563	148836.563594	58.413287
2469.570921	148624.466423	58.418292
2468.632362	148416.043277	58.423297
2467.943780	148218.397350	58.428301
2467.623301	148013.742424	58.433306
2466.823687	147813.727285	58.438311
2466.499470	147616.624635	58.443316
2465.669606	147412.905794	58.448321
2464.837203	147203.634930	58.453325
2464.232038	147005.080960	58.458330
2463.486497	146794.680655	58.463335
2462.926370	146595.639178	58.468340
2461.872202	146394.377039	58.473345
2461.187496	146195.942411	58.478349
2460.593959	145994.228552	58.483354
2460.095376	145792.907593	58.488359
2459.885166	145591.821787	58.493364
2458.840921	145396.893081	58.498369
2458.560789	145183.214611	58.503373
2457.806474	144989.932632	58.508378
2456.843331	144785.044621	58.513383
2456.639013	144573.162801	58.518388
2455.470351	144364.840927	58.523393
2454.988733	144164.823920	58.528397
2454.133959	143960.724724	58.533402
2453.137782	143762.037208	58.538407
2452.745463	143565.339237	58.543412
2452.069980	143375.600122	58.548417
2451.293295	143162.344624	58.553421
2450.843661	142974.732380	58.558426
2449.918943	142776.942072	58.563431
2449.812735	142570.090351	58.568436
2448.911362	142369.554279	58.573441
2448.455166	142173.713964	58.578445
2447.848977	141969.334412	58.583450
2447.043165	141754.479565	58.588455
2446.695874	141562.971533	58.593460
2445.865790	141364.209659	58.598465
2445.432593	141151.104302	58.603469
2444.534543	140941.199853	58.608474
2443.275926	140742.687866	58.613479
2443.178013	140531.439627	58.618484
2442.618554	140339.083524	58.623489
2441.855211	140132.060288	58.628493
2441.366417	139927.968100	58.633498
2440.698224	139724.159849	58.638503
2439.879980	139511.292265	58.643508
2439.120517	139320.994562	58.648513
2438.664245	139104.019428	58.653517
2437.949696	138894.595661	58.658522
2437.183658	138685.435630	58.663527
2436.748588	138484.635411	58.668532
2435.648723	138273.981159	58.673537
2435.425686	138073.620187	58.678541
2434.365477	137870.623614	58.683546
2433.764067	137669.791746	58.688551
2433.478437	137460.183035	58.693556
2432.656482	137263.683081	58.698561
2431.680491	137049.130285	58.703565
2431.363144	136851.219107	58.708570
2430.550266	136646.006576	58.713575
2430.114984	136429.898869	58.718580
2429.287990	136231.666121	58.723585
2428.647844	136033.138307	58.728589
2427.864572	135824.484021	58.733594
2427.196168	135616.740403	58.738599
2426.749842	135402.966849	58.743604
2425.899363	135213.396045	58.748609
2425.153895	135000.790799	58.753613
2424.833495	134791.867273	58.758618
2423.751517	134598.183122	58.763623
2423.198779	134388.283061	58.768628
2422.374129	134190.343323	58.773633
2421.928644	133984.735609	58.778637
2421.500241	133781.464027	58.783642
2420.521885	133577.544291	58.788647
2420.110387	133368.734425	58.793652
2419.082729	133176.207189	58.798657
2418.663783	132970.539006	58.803661
2417.954140	132760.790021	58.808666
2416.969383	132569.123851	58.813671
2416.356698	132355.437374	58.818676
2415.752239	132165.657107	58.823681
2415.356085	131953.692248	58.828685
2414.728514	131755.052176	58.833690
2413.910911	131550.295791	58.838695
2413.520118	131340.252685	58.843700
2412.554598	131151.476394	58.848705
2412.038715	130947.273532	58.853709
2411.631745	130744.198039	58.858714
2410.543486	130533.268073	58.863719
2410.093866	130317.081601	58.868724
2409.155462	130115.479372	58.873729
2408.344670	129921.784029	58.878733
2407.662117	129717.489511	58.883738
2407.357540	129526.066391	58.888743
2406.572146	129320.241532	58.893748
2405.757190	129126.615867	58.898753
2405.439188	128926.079653	58.903757
2404.767308	128721.943145	58.908762
2404.225431	128523.960093	58.913767
2403.619318	128309.211064	58.918772
2402.942499	128108.813845	58.923777
2402.093754	127898.094451	58.928781
2401.387601	127702.035693	58.933786
2400.335636	127500.838737	58.938791
2399.936509	127288.465182	58.943796
2399.330099	127095.519174	58.948801
2398.804028	126892.439879	58.953805
2398.250089	126693.976573	58.958810
2397.400973	126489.516389	58.963815
2396.816941	126287.136561	58.968820
2396.350958	126083.304457	58.973825
2395.715695	125875.182872	58.978829
2395.260634	125671.110827	58.983834
2394.077989	125466.152420	58.988839
2393.732219	125251.335256	58.993844
2392.888675	125051.024942	58.998849
2392.310232	124842.724471	59.003853
2391.667382	124633.597685	59.008858
2391.070828	124433.316281	59.013863
2390.141689	124224.822200	59.018868
2389.539099	124023.668582	59.023873
2388.862607	123816.648748	59.028877
2388.182848	123610.824683	59.033882
2387.607045	123411.728552	59.038887
2387.401335	123200.994392	59.043892
2386.454205	122994.734918	59.048897
2385.735719	122782.421896	59.053901
2385.137570	122575.208769	59.058906
2384.166626	122373.719616	59.063911
2383.726603	122161.989584	59.068916
2382.815985	121959.376602	59.073921
2382.648322	121752.444470	59.078925
2381.932945	121546.743567	59.083930
2381.092643	121342.917890	59.088935
2380.542457	121130.769155	59.093940
2379.929568	120924.625138	59.098945
2379.299301	120710.968814	59.103949
2378.593338	120504.830143	59.108954
2377.714910	120299.266401	59.113959
2377.374345	120087.943526	59.118964
2376.342366	119886.902025	59.123969
2376.026595	119672.493275	59.128973
2375.183597	119461.540792	59.133978
2374.461231	119253.973518	59.138983
2374.223792	119044.363086	59.143988
2373.336936	118835.955528	59.148993
2372.264645	118619.586867	59.153997
2371.772281	118419.556642	59.159002
2371.122677	118214.595153	59.164007
2370.863977	118004.621955	59.169012
2369.615327	117797.283080	59.174017
2369.257537	117582.650670	59.179021
2368.361910	117376.312937	59.184026
2367.751298	117177.485405	59.189031
2367.238506	116964.571205	59.194036
2366.457482	116761.355964	59.199041
2365.922172	116553.114216	59.204045
2365.060352	116336.959854	59.209050
2364.406818	116141.777911	59.214055
2363.705347	115927.734318	59.219060
2362.902232	115726.066870	59.224065
2362.348754	115518.433085	59.229069
2361.660826	115307.705829	59.234074
2361.008182	115116.847704	59.239079
2360.851018	114909.130667	59.244084
2360.076577	114696.638661	59.249089
2359.443698	114480.863630	59.254093
2358.537299	114274.679634	59.259098
2357.618187	114073.354722	59.264103
2357.377095	113866.224433	59.269108
2356.554452	113659.124591	59.274113
2355.894450	113448.757476	59.279117
2355.269092	113244.187511	59.284122
2354.190281	113043.606998	59.289127
2354.072865	112840.235464	59.294132
2353.010436	112634.280068	59.299137
2352.640211	112425.430501	59.304141
2351.921143	112213.731327	59.309146
2351.104338	112013.517366	59.314151
2350.715758	111816.822793	59.319156
2349.898597	111614.029146	59.324161
2349.111058	111395.189189	59.329165
2348.648847	111185.996530	59.334170
2347.916431	110991.431874	59.339175
2347.410133	110785.130734	59.344180
2346.690757	110581.473318	59.349185
2346.004559	110377.057152	59.354189
2345.315399	110164.602880	59.359194
2344.717628	109962.822377	59.364199
2344.328012	109756.460579	59.369204
2343.409012	109554.524956	59.374209
2342.719061	109326.378668	59.379213
2342.178096	109115.623314	59.384218
2341.415228	108917.139258	59.389223
2340.940073	108700.672363	59.394228
2340.168137	108487.744462	59.399233
2339.592412	108281.430967	59.404237
2339.213734	108077.327892	59.409242
2338.493759	107855.869106	59.414247
2337.756806	107650.741380	59.419252
2336.910182	107439.484278	59.424257
2336.465281	107229.218613	59.429261
2335.875889	107010.437195	59.434266
2334.958847	106803.765283	59.439271
2334.260541	106585.233413	59.444276
2333.514135	106378.810923	59.449281
2332.871122	106159.849039	59.454285
2332.424249	105956.986560	59.459290
2331.416065	105738.708216	59.464295
2331.059028	105528.183345	59.469300
2330.246587	105326.615045	59.474305
2329.920252	105102.784329	59.479309
2329.283264	104889.765295	59.484314
2328.442134	104681.564271	59.489319
2328.015155	104460.496358	59.494324
2327.292769	104248.448268	59.499329
2326.779722	104028.730335	59.504333
2325.953509	103812.369450	59.509338
2324.786037	103600.588063	59.514343
2324.550004	103385.945581	59.519348
2323.483374	103181.155881	59.524353
2323.038199	102963.257833	59.529357
2322.720965	102745.728491	59.534362
2321.593239	102545.826163	59.539367
2321.131415	102320.590466	59.544372
2320.519345	102110.624866	59.549377
2319.990420	101893.092582	59.554381
2319.469365	101676.170063	59.559386
2318.501485	101461.540677	59.564391
2318.130215	101243.215516	59.569396
2317.297035	101043.152443	59.574401
2316.361837	100818.501072	59.579405
2316.284119	100597.699529	59.584410
2315.255330	100385.189377	59.589415
2314.954009	100171.785589	59.594420
2314.023629	99956.155568	59.599425
2313.463070	99733.986221	59.604429
2312.634132	99518.781867	59.609434
2311.844669	99311.432262	59.614439
2311.558167	99080.605575	59.619444
2310.312031	98875.488920	59.624449
2309.588651	98660.751557	59.629453
2309.484818	98443.831175	59.634458
2308.296896	98232.609275	59.639463
2308.124425	98017.581254	59.644468
2307.460315	97807.028644	59.649473
2306.823381	97589.135336	59.654477
2306.162217	97371.000593	59.659482
2305.348129	97157.813911	59.664487
2305.003935	96942.398300	59.669492
2303.994706	96730.483328	59.674497
2303.254369	96510.187636	59.679501
2302.703217	96294.531928	59.684506
2301.726069	96073.504286	59.689511
2301.158371	95863.512481	59.694516
2300.177044	95660.114147	59.699521
2299.887388	95438.514377	59.704525
2299.278965	95225.725478	59.709530
2298.527688	95025.816128	59.714535
2298.201408	94804.596225	59.719540
2297.574237	94591.416765	59.724545
2296.678281	94382.112311	59.729549
2296.246697	94155.093874	59.734554
2295.547075	93946.478952	59.739559
2294.956191	93724.696536	59.744564
2293.992339	93507.433474	59.749569
2293.878414	93294.578137	59.754573
2293.143299	93068.988601	59.759578
2291.825758	92861.515449	59.764583
2291.499190	92637.013262	59.769588
2290.542493	92418.979732	59.774593
2290.252621	92210.912145	59.779597
2289.769047	91988.806623	59.784602
2288.870101	91771.607314	59.789607
2288.108617	91554.083980	59.794612
2287.662113	91341.591801	59.799617
2287.035070	91120.177208	59.804621
2286.312766	90895.920314	59.809626
2285.177493	90685.477602	59.814631
2285.127766	90476.842991	59.819636
2284.496023	90261.321809	59.824641
2283.545061	90043.463040	59.829645
2282.921914	89814.306684	59.834650
2282.388489	89608.293192	59.839655
2282.003950	89379.617115	59.844660
2281.014368	89158.932878	59.849665
2280.364292	88942.419531	59.854669
2279.882319	88716.714005	59.859674
2279.050950	88509.357015	59.864679
2278.306052	88283.723049	59.869684
2277.688003	88073.198150	59.874689
2276.839091	87847.356992	59.879693
2276.489470	87631.569850	59.884698
2275.718101	87404.738365	59.889703
2275.499375	87182.893272	59.894708
2274.528576	86972.669610	59.899713
2274.000585	86739.080313	59.904718
2273.469568	86513.836650	59.909722
2272.457561	86297.191667	59.914727
2271.816026	86075.963895	59.919732
2271.373027	85863.917750	59.924737
2270.573490	85624.716430	59.929742
2269.752834	85404.373453	59.934746
2269.239942	85198.671364	59.939751
2268.664525	84964.341935	59.944756
2267.761478	84746.117012	59.949761
2267.281150	84528.664005	59.954766
2266.807325	84304.493148	59.959770
2265.965515	84092.451821	59.964775
2265.519377	83863.913897	59.969780
2264.597462	83645.513132	59.974785
2264.089871	83416.165784	59.979790
2263.463288	83199.294728	59.984794
2262.524231	82971.827083	59.989799
2262.051652	82747.057724	59.994804
2261.021493	82529.902628	59.999809
2260.438808	82302.277951	60.004814
2259.852225	82084.321887	60.009818
2259.235286	81876.672134	60.014823
2258.240555	81659.729583	60.019828
2257.865961	81440.567742	60.024833
2257.180378	81217.971739	60.029838
2256.790352	80999.032463	60.034842
2255.836561	80780.831345	60.039847
2255.152881	80550.364463	60.044852
2253.913648	80336.389751	60.049857
2253.476571	80127.398006	60.054862
2253.025282	79906.756155	60.059866
2252.094875	79698.258911	60.064871
2251.694084	79473.747893	60.069876
2251.202188	79263.303315	60.074881
2250.501825	79043.134769	60.079886
2250.059302	78826.140565	60.084890
2249.152865	78613.296913	60.089895
2249.009169	78386.836831	60.094900
2248.167006	78173.670686	60.099905
2247.079364	77949.272541	60.104910
2246.749597	77730.510385	60.109914
2245.896277	77523.632458	60.114919
2245.218789	77303.922482	60.119924
2244.211496	77074.908138	60.124929
2243.870193	76857.988394	60.129934
2243.261591	76639.111055	60.134938
2242.325804	76428.252713	60.139943
2242.021469	76203.540399	60.144948
2241.236433	75995.311186	60.149953
2240.452094	75777.896628	60.154958
2239.708740	75554.737443	60.159962
2238.954761	75346.433932	60.164967
2238.660287	75124.957013	60.169972
2237.697977	74908.017201	60.174977
2237.222892	74693.498735	60.179982
2236.615150	74482.146102	60.184986
2235.811833	74269.122419	60.189991
2235.559994	74043.164973	60.194996
2234.590034	73825.965597	60.200001
2233.772572	73611.861415	60.205006
2233.309866	73382.371664	60.210010
2232.534888	73180.289874	60.215015
2232.068436	72962.747566	60.220020
2231.396603	72742.750482	60.225025
2230.564458	72525.264606	60.230030
2230.501385	72306.303416	60.235034
2229.269831	72096.145511	60.240039
2228.810983	71869.611943	60.245044
2228.110915	71657.372546	60.250049
2227.285032	71433.569124	60.255054
2226.961926	71209.213375	60.260058
2226.162938	70998.510703	60.265063
2225.638841	70777.587070	60.270068
2224.597942	70563.468749	60.275073
2224.005260	70339.431666	60.280078
2223.600792	70118.806808	60.285082
2222.728164	69905.790108	60.290087
2222.292391	69683.154466	60.295092
2221.311353	69466.650579	60.300097
2220.859828	69254.745943	60.305102
2220.237761	69033.325346	60.310106
2219.415344	68820.641813	60.315111
2218.547016	68607.423163	60.320116
2218.250511	68384.127783	60.325121
2217.291784	68162.669097	60.330126
2216.776004	67946.120887	60.335130
2215.728906	67735.891578	60.340135
2215.104030	67511.891907	60.345140
2214.590598	67305.572684	60.350145
2213.782475	67095.711390	60.355150
2213.172851	66875.535639	60.360154
2212.460009	66675.930009	60.365159
2211.823660	66463.711351	60.370164
2211.171239	66252.691353	60.375169
2210.277500	66033.010396	60.380174
2209.912500	65830.920102	60.385178
2209.014556	65622.634263	60.390183
2208.665223	65406.202003	60.395188
2208.013097	65207.285858	60.400193
2206.993932	64994.295499	60.405198
2206.622653	64778.579869	60.410202
2206.022608	64573.376934	60.415207
2205.236190	64353.888094	60.420212
2204.673060	64146.590997	60.425217
2204.160061	63930.939046	60.430222
2203.248914	63718.949396	60.435226
2202.198296	63523.640991	60.440231
2201.814610	63306.728137	60.445236
2200.934132	63098.995681	60.450241
2200.237676	62902.855452	60.455246
2199.698949	62678.654595	60.460250
2198.976568	62485.508269	60.465255
2198.563083	62274.335880	60.470260
2197.888380	62074.677130	60.475265
2196.707855	61859.107055	60.480270
2196.481459	61656.753973	60.485274
2195.448062	61457.358080	60.490279
2195.200070	61245.800517	60.495284
2194.640312	61042.243781	60.500289
2193.552841	60842.195010	60.505294
2192.935893	60636.435784	60.510298
2192.247780	60433.368167	60.515303
2191.762299	60227.440611	60.520308
2190.789949	60031.994383	60.525313
2190.082953	59825.017450	60.530318
2190.035049	59620.100235	60.535322
2188.702799	59424.274279	60.540327
2187.940692	59221.342314	60.545332
2187.371354	59021.097825	60.550337
2186.397084	58833.625227	60.555342
2186.001794	58633.771937	60.560346
2185.625746	58445.442345	60.565351
2184.955048	58234.837252	60.570356
2183.985918	58052.125831	60.575361
2183.272441	57862.548456	60.580366
2182.867797	57663.745231	60.585370
2182.070572	57475.916400	60.590375
2181.603646	57263.229540	60.595380
2180.543879	57075.215375	60.600385
2180.050404	56882.742466	60.605390
2179.452000	56693.440480	60.610394
2178.398830	56493.584844	60.615399
2177.976543	56306.528119	60.620404
2177.185811	56112.670381	60.625409
2176.320915	55922.937528	60.630414
2176.099251	55728.522000	60.635418
2174.773593	55552.366975	60.640423
2174.543333	55355.966131	60.645428
2173.543639	55173.398812	60.650433
2172.871391	54982.781153	60.655438
2172.611339	54799.616027	60.660442
2171.904903	54624.517273	60.665447
2170.877372	54430.350948	60.670452
2170.254955	54250.606389	60.675457
2169.394118	54071.075471	60.680462
2168.579631	53879.517222	60.685466
2167.668977	53707.908910	60.690471
2166.774686	53540.302572	60.695476
2166.142545	53369.070969	60.700481
2165.525818	53202.021778	60.705486
2164.596211	53031.637959	60.710490
2163.910802	52871.057886	60.715495
2163.140402	52697.854727	60.720500
2162.787835	52538.531626	60.725505
2161.517848	52391.502797	60.730510
2160.931619	52228.963540	60.735514
2160.102063	52081.604732	60.740519
2159.434467	51931.617368	60.745524
2158.837776	51778.063572	60.750529
2157.595049	51639.222028	60.755534
2157.177735	51478.551670	60.760538
2156.011896	51342.111210	60.765543
2155.835412	51193.820747	60.770548
2154.769578	51057.907617	60.775553
2154.190389	50929.176370	60.780558
2153.547444	50788.189682	60.785562
2152.934512	50652.410256	60.790567
2152.209987	50512.416316	60.795572
2151.281923	50389.907487	60.800577
2150.778147	50250.168482	60.805582
2150.225692	50112.868080	60.810586
2149.553289	49985.268886	60.815591
2148.662545	49861.299257	60.820596
2147.955824	49729.404641	60.825601
2147.274014	49597.307733	60.830606
2146.673535	49469.612225	60.835610
2145.654010	49352.493776	60.840615
2144.855474	49228.365222	60.845620
2144.169572	49096.241037	60.850625
2143.427219	48976.461615	60.855630
2143.111349	48864.862756	60.860634
2142.208157	48739.808305	60.865639
2141.737513	48621.247256	60.870644
2140.764645	48512.946841	60.875649
2139.882496	48394.193189	60.880654
2139.925654	48278.494948	60.885658
2139.191506	48173.224127	60.890663
2138.412759	48044.200524	60.895668
2137.690051	47934.747260	60.900673
2136.957502	47813.936527	60.905678
2136.461744	47702.183710	60.910682
2135.436153	47589.380024	60.915687
2135.163418	47465.632726	60.920692
2134.310566	47361.979875	60.925697
2133.541654	47244.376898	60.930702
2133.042683	47131.884825	60.935706
2132.333435	47023.978733	60.940711
2131.668711	46905.542203	60.945716
2131.003502	46805.361371	60.950721
2130.127107	46689.259527	60.955726
2129.561041	46579.615830	60.960730
2128.650609	46472.564294	60.965735
2128.432048	46359.339930	60.970740
2127.993062	46254.201360	60.975745
2126.855370	46153.725957	60.980750
2126.373179	46035.244179	60.985754
2125.790605	45939.382237	60.990759
2125.192935	45822.612444	60.995764
2124.263335	45707.749615	61.000769
2123.861609	45610.605061	61.005774
2123.231623	45490.897864	61.010778
2122.645634	45383.346025	61.015783
2121.552746	45280.736693	61.020788
2121.268381	45165.911044	61.025793
2120.406508	45063.563644	61.030798
2119.634123	44957.612789	61.035802
2118.982731	44854.110401	61.040807
2118.086707	44746.614833	61.045812
2117.272437	44660.990458	61.050817
2116.616097	44549.994788	61.055822
2116.442668	44445.359449	61.060826
2115.840486	44345.505275	61.065831
2114.924236	44238.041353	61.070836
2114.360567	44137.388414	61.075841
2113.620783	44037.763414	61.080846
2113.020449	43927.626239	61.085850
2112.492891	43832.314267	61.090855
2112.075241	43733.092160	61.095860
2111.111681	43626.053831	61.100865
2110.301836	43525.664877	61.105870
2109.830583	43421.987447	61.110874
2108.833176	43321.853976	61.115879
2108.221235	43214.955309	61.120884
2107.511656	43109.024715	61.125889
2106.859308	43022.705934	61.130894
2106.468232	42913.895541	61.135898
2105.310604	42827.038062	61.140903
2104.796152	42727.555603	61.145908
2104.172116	42628.382049	61.150913
2103.228867	42526.309170	61.155918
2102.958769	42436.846130	61.160922
2102.140260	42342.160913	61.165927
2101.501099	42247.789294	61.170932
2100.908674	42150.150383	61.175937
2100.079037	42066.716954	61.180942
2099.514119	41970.564159	61.185946
2098.595949	41874.322486	61.190951
2098.358672	41776.423786	61.195956
2097.669879	41678.483446	61.200961
2096.798775	41598.502579	61.205966
2096.288947	41500.199656	61.210970
2095.313093	41417.602108	61.215975
2094.917182	41326.185239	61.220980
2094.369243	41228.731061	61.225985
2093.586112	41131.181945	61.230990
2093.170355	41039.200559	61.235994
2092.000372	40948.733849	61.240999
2091.903001	40843.991199	61.246004
2091.361042	40758.134234	61.251009
2090.167184	40665.095696	61.256014
2089.967910	40564.674518	61.261018
2089.034614	40474.574337	61.266023
2088.055834	40386.489739	61.271028
2087.636283	40304.040108	61.276033
2086.974793	40206.094349	61.281038
2086.311197	40121.350768	61.286042
2085.542754	40031.014911	61.291047
2084.877866	39930.106927	61.296052
2084.074630	39851.230128	61.301057
2083.324741	39762.190723	61.306062
2083.362102	39674.056058	61.311066
2082.684867	39579.994460	61.316071
2081.536716	39485.982811	61.321076
2081.308266	39391.025792	61.326081
2080.393229	39311.500499	61.331086
2079.834431	39214.342496	61.336090
2078.784517	39129.097600	61.341095
2078.070094	39033.266407	61.346100
2077.807880	38948.834885	61.351105
2076.825608	38863.672277	61.356110
2076.512719	38777.866378	61.361114
2075.735215	38693.222272	61.366119
2074.900613	38605.059186	61.371124
2074.472098	38511.251740	61.376129
2073.696660	38415.367317	61.381134
2072.999269	38336.292624	61.386138
2072.403032	38252.771211	61.391143
2071.510567	38164.153257	61.396148
2071.178238	38074.060516	61.401153
2069.981487	37998.196633	61.406158
2069.710885	37898.992807	61.411162
2068.786701	37820.947663	61.416167
2068.040645	37736.244856	61.421172
2067.694813	37654.123579	61.426177
2066.806551	37563.563763	61.431182
2066.275066	37478.262287	61.436186
2065.735094	37403.947149	61.441191
2065.332996	37317.056279	61.446196
2064.708361	37222.849224	61.451201
2063.711703	37145.256563	61.456206
2063.394625	37063.351731	61.461210
2062.319344	36974.857543	61.466215
2061.514876	36887.438394	61.471220
2061.136388	36799.180724	61.476225
2060.387429	36713.318546	61.481230
2059.803299	36624.673964	61.486234
2059.006467	36558.844077	61.491239
2058.490337	36470.334937	61.496244
2057.898871	36372.814321	61.501249
2056.543835	36291.267635	61.506254
2056.374758	36205.836052	61.511258
2055.641680	36133.464979	61.516263
2055.047690	36055.418288	61.521268
2054.360165	35971.555948	61.526273
2053.981622	35883.416892	61.531278
2053.356572	35796.178839	61.536282
2052.159576	35714.059836	61.541287
2051.760489	35629.552809	61.546292
2051.240808	35544.595917	61.551297
2050.406621	35467.928817	61.556302
2049.635806	35381.520559	61.561306
2049.132036	35311.854156	61.566311
2048.615712	35212.450669	61.571316
2047.665860	35137.271757	61.576321
2047.016138	35066.208645	61.581326
2046.556228	34971.986484	61.586330
2045.752369	34899.424928	61.591335
2045.131540	34820.231321	61.596340
2044.541298	34744.709455	61.601345
2043.476960	34663.004457	61.606350
2043.161152	34574.260170	61.611354
2042.449823	34499.057342	61.616359
2042.006348	34414.968092	61.621364
2041.399771	34336.087451	61.626369
2040.187520	34263.498647	61.631374
2040.021094	34164.715973	61.636378
2039.010904	34093.540361	61.641383
2038.346954	34002.847219	61.646388
2037.862862	33931.563521	61.651393
2037.301780	33857.542440	61.656398
2036.544864	33772.701748	61.661402
2036.003375	33700.882910	61.666407
2035.199134	33628.375943	61.671412
2034.388176	33537.925180	61.676417
2033.421557	33462.682210	61.681422
2033.230754	33379.599552	61.686426
2032.467285	33304.724890	61.691431
2031.833642	33226.294725	61.696436
2031.520364	33143.765260	61.701441
2030.259085	33070.595248	61.706446
2029.971555	32981.562601	61.711450
2029.296116	32909.600930	61.716455
2029.055542	32831.933594	61.721460
2028.276472	32751.983212	61.726465
2027.490644	32673.527666	61.731470
2026.836351	32590.797486	61.736474
2025.759456	32506.466017	61.741479
2024.961126	32431.351152	61.746484
2024.715938	32347.563271	61.751489
2023.816105	32271.243699	61.756494
2023.461579	32193.742825	61.761498
2022.489772	32122.111321	61.766503
2021.788314	32036.504301	61.771508
2021.099954	31959.809698	61.776513
2020.221941	31896.093865	61.781518
2020.016284	31814.302971	61.786522
2019.394834	31745.621482	61.791527
2018.692894	31667.021507	61.796532
2017.962094	31575.280891	61.801537
2016.830930	31512.038114	61.806542
2016.198954	31434.953020	61.811546
2016.126677	31367.954162	61.816551
2015.452224	31281.485585	61.821556
2014.691362	31204.696973	61.826561
2014.001175	31137.079733	61.831566
2013.468888	31041.467669	61.836570
2012.756659	30979.133819	61.841575
2012.039191	30897.243832	61.846580
2011.414265	30826.387741	61.851585
2010.741274	30751.491342	61.856590
2010.305794	30673.590156	61.861594
2009.335749	30595.687277	61.866599
2008.848827	30513.866898	61.871604
2008.113523	30436.537432	61.876609
2007.106952	30365.257241	61.881614
2007.029758	30275.098184	61.886618
2006.160518	30200.110626	61.891623
2005.644558	30129.809071	61.896628
2004.995978	30041.096091	61.901633
2004.069901	29971.004094	61.906638
2003.371410	29890.433873	61.911642
2002.737499	29817.632237	61.916647
2002.258648	29751.744153	61.921652
2001.284590	29670.016366	61.926657
2000.395074	29597.063521	61.931662
1999.760324	29523.681888	61.936666
1999.166923	29456.395924	61.941671
1998.578176	29381.437124	61.946676
1998.181451	29306.748385	61.951681
1997.125563	29240.318803	61.956686
1996.890054	29162.582664	61.961690
1996.044330	29085.812720	61.966695
1995.432815	29006.631313	61.971700
1995.046713	28933.983879	61.976705
1993.690307	28866.129443	61.981710
1993.288934	28780.385940	61.986714
1992.675769	28724.969754	61.991719
1991.670567	28653.047484	61.996724
1991.446493	28578.623801	62.001729
1991.034665	28517.479246	62.006734
1990.354088	28432.996827	62.011738
1989.766045	28360.783714	62.016743
1988.579106	28285.566272	62.021748
1988.382400	28204.052655	62.026753
1987.366199	28135.723873	62.031758
1986.925823	28052.244855	62.036762
1986.320742	27977.129231	62.041767
1985.275592	27913.946785	62.046772
1984.782291	27829.439361	62.051777
1984.273039	27770.978249	62.056782
1983.688961	27697.800607	62.061786
1982.613352	27623.314241	62.066791
1982.039787	27547.340931	62.071796
1981.342820	27467.769839	62.076801
1980.569243	27414.931795	62.081806
1979.998391	27334.861084	62.086810
1979.497777	27262.716394	62.091815
1978.767610	27199.106021	62.096820
1978.127384	27136.061394	62.101825
1977.529880	27057.026292	62.106830
1976.965950	26978.986226	62.111834
1976.278956	26911.215406	62.116839
1975.774007	26835.664236	62.121844
1975.088024	26757.624075	62.126849
1974.212065	26696.269394	62.131854
1973.614318	26613.257985	62.136858
1973.164543	26550.344967	62.141863
1972.495518	26477.245572	62.146868
1971.825510	26392.522531	62.151873
1970.992393	26311.897449	62.156878
1970.491880	26243.403988	62.161882
1969.574408	26175.644410	62.166887
1968.923137	26099.416173	62.171892
1968.521827	26028.698726	62.176897
1967.748669	25954.098609	62.181902
1967.069048	25879.604835	62.186906
1966.771988	25792.761956	62.191911
1965.823352	25732.902597	62.196916
1965.097189	25653.346671	62.201921
1964.486790	25577.701246	62.206926
1964.048789	25505.121669	62.211930
1962.990455	25433.448059	62.216935
1962.101920	25364.407841	62.221940
1961.846454	25277.662236	62.226945
1960.890883	25209.621351	62.231950
1960.365330	25131.649700	62.236954
1959.934076	25070.109803	62.241959
1959.045276	24998.379638	62.246964
1958.371866	24918.294573	62.251969
1957.470545	24854.306802	62.256974
1956.971469	24779.970331	62.261978
1956.117004	24716.845203	62.266983
1955.217778	24655.329060	62.271988
1955.154513	24586.001669	62.276993
1954.218879	24524.060604	62.281998
1953.611492	24434.561538	62.287002
1953.094427	24371.887284	62.292007
1952.281595	24296.321900	62.297012
1951.722703	24231.437246	62.302017
1951.118737	24169.881633	62.307022
1950.729641	24091.992102	62.312026
1949.568935	24011.923382	62.317031
1948.818655	23949.061157	62.322036
1948.328982	23873.024767	62.327041
1947.629948	23814.360197	62.332046
1947.051107	23749.746803	62.337050
1946.496964	23687.073228	62.342055
1945.920672	23606.113012	62.347060
1945.127384	23537.860015	62.352065
1944.420377	23470.688138	62.357070
1944.231828	23384.434158	62.362074
1943.670673	23318.036575	62.367079
1942.521016	23246.934539	62.372084
1942.169624	23168.178037	62.377089
1941.045197	23098.845502	62.382094
1940.515818	23031.170317	62.387098
1939.892118	22962.743619	62.392103
1938.776194	22889.302763	62.397108
1938.505235	22816.744418	62.402113
1937.552730	22751.814565	62.407118
1937.287221	22679.122529	62.412122
1936.408923	22622.324408	62.417127
1935.515773	22549.311714	62.422132
1935.039009	22485.651421	62.427137
1934.343341	22414.500003	62.432142
1933.827337	22350.963348	62.437146
1933.294971	22280.364628	62.442151
1932.775337	22212.341577	62.447156
1932.351206	22138.281121	62.452161
1931.458876	22058.447337	62.457166
1930.900193	21986.514892	62.462170
1930.210733	21920.358304	62.467175
1929.452405	21849.875547	62.472180
1929.038082	21762.845008	62.477185
1928.094974	21700.647676	62.482190
1927.440990	21628.230586	62.487194
1926.624801	21558.624514	62.492199
1926.022909	21486.612767	62.497204
1925.502368	21418.135308	62.502209
1924.821415	21351.000653	62.507214
1924.327030	21271.631173	62.512218
1923.698130	21199.960598	62.517223
1922.541490	21135.960444	62.522228
1922.153895	21052.812746	62.527233
1921.567577	20986.592376	62.532238
1920.916405	20905.593886	62.537242
1920.073260	20831.925848	62.542247
1919.371364	20759.718533	62.547252
1919.162684	20695.293336	62.552257
1918.323301	20630.306876	62.557262
1917.525826	20557.414536	62.562266
1916.575684	20477.272637	62.567271
1915.900089	20417.705798	62.572276
1915.673031	20338.667298	62.577281
1914.945450	20272.313661	62.582286
1914.069153	20204.594328	62.587290
1913.148384	20134.320311	62.592295
1912.923093	20071.348310	62.597300
1912.082097	19997.625021	62.602305
1911.474658	19929.127568	62.607310
1910.896816	19848.266577	62.612314
1910.054026	19782.903224	62.617319
1909.175437	19714.334880	62.622324
1908.634147	19648.674343	62.627329
1908.108029	19581.262522	62.632334
1907.515312	19514.844494	62.637338
1907.134296	19439.289428	62.642343
1905.984385	19379.678276	62.647348
1905.712869	19296.215905	62.652353
1904.847889	19235.799393	62.657358
1904.504411	19163.331730	62.662362
1903.630022	19080.963335	62.667367
1902.689777	19012.210488	62.672372
1902.291805	18946.134221	62.677377
1901.374084	18881.984556	62.682382
1900.794504	18806.949986	62.687386
1899.648788	18751.681846	62.692391
1899.175769	18685.054132	62.697396
1898.586249	18618.850189	62.702401
1897.992469	18552.860750	62.707406
1897.257822	18496.117108	62.712410
1896.663182	18428.319306	62.717415
1895.895890	18360.478554	62.722420
1895.664928	18286.793191	62.727425
1894.956485	18232.204680	62.732430
1894.314208	18156.672424	62.737434
1893.734433	18093.847151	62.742439
1892.926765	18024.766971	62.747444
1892.507499	17941.674351	62.752449
1891.909543	17883.928407	62.757454
1890.637404	17810.527034	62.762458
1890.350889	17738.606770	62.767463
1889.845559	17672.283360	62.772468
1889.011505	17599.512850	62.777473
1888.206853	17536.523047	62.782478
1887.797841	17460.396663	62.787482
1887.217253	17395.725962	62.792487
1886.445831	17318.619755	62.797492
1886.145048	17245.857018	62.802497
1885.043642	17184.837127	62.807502
1884.720776	17110.571200	62.812506
1883.727403	17033.236811	62.817511
1883.422432	16966.205743	62.822516
1882.673780	16893.969651	62.827521
1881.847085	16830.723947	62.832526
1881.179645	16759.704039	62.837530
1880.541699	16678.964737	62.842535
1879.869078	16615.180198	62.847540
1879.390197	16534.447180	62.852545
1878.393224	16467.001048	62.857550
1877.689272	16397.010413	62.862554
1877.440310	16325.057385	62.867559
1876.370741	16265.859050	62.872564
1875.867499	16187.717777	62.877569
1875.027024	16117.321278	62.882574
1874.779077	16046.336117	62.887578
1873.913180	15969.515856	62.892583
1872.951066	15915.495945	62.897588
1872.408768	15844.733476	62.902593
1871.888668	15787.165320	62.907598
1871.216900	15714.041858	62.912602
1870.673413	15636.350594	62.917607
1870.037550	15574.389787	62.922612
1869.215754	15496.976454	62.927617
1868.335666	15431.101601	62.932622
1867.879421	15361.714675	62.937626
1867.109386	15303.911753	62.942631
1866.501589	15228.170461	62.947636
1865.841160	15150.396521	62.952641
1865.143124	15084.034395	62.957646
1864.384436	15015.930785	62.962650
1863.755784	14943.714761	62.967655
1863.055009	14887.762620	62.972660
1862.627366	14817.521295	62.977665
1861.567170	14754.917964	62.982670
1861.073507	14681.083981	62.987674
1860.677472	14616.024174	62.992679
1859.873252	14562.012759	62.997684
1859.293657	14481.050566	63.002689
1858.682710	14423.249871	63.007694
1857.989169	14358.875704	63.012698
1857.239438	14286.005125	63.017703
1856.580757	14214.396428	63.022708
1856.086416	14138.498556	63.027713
1855.061519	14081.796495	63.032718
1854.677356	14005.021436	63.037722
1853.874780	13937.339214	63.042727
1853.448523	13874.409756	63.047732
1852.531772	13806.818626	63.052737
1852.047122	13740.608174	63.057742
1851.009912	13669.525590	63.062746
1850.786100	13608.868473	63.067751
1850.063168	13542.275081	63.072756
1849.657501	13473.136074	63.077761
1848.560634	13411.324576	63.082766
1848.217066	13332.997356	63.087770
1847.375997	13255.662024	63.092775
1846.481662	13192.872924	63.097780
1846.490782	13125.737058	63.102785
1845.671404	13049.260220	63.107790
1844.970579	12979.800581	63.112794
1844.249924	12922.292085	63.117799
1843.450855	12846.275294	63.122804
1843.017201	12769.014362	63.127809
1841.849078	12705.394285	63.132814
1841.367160	12636.356402	63.137818
1840.852997	12563.744770	63.142823
1839.752087	12510.043208	63.147828
1839.941851	12425.120092	63.152833
1839.204696	12357.699714	63.157838
1838.352868	12292.386286	63.162842
1837.642052	12225.018934	63.167847
1836.998556	12148.032985	63.172852
1836.294506	12075.419309	63.177857
1835.489163	12011.481658	63.182862
1834.769207	11928.651922	63.187866
1834.261009	11861.399602	63.192871
1833.584936	11793.230068	63.197876
1832.842467	11718.937478	63.202881
1832.182845	11650.195649	63.207886
1831.300916	11576.260284	63.212890
1830.839042	11522.477124	63.217895
1829.846827	11457.749047	63.222900
1829.602061	11376.476934	63.227905
1828.632545	11315.443124	63.232910
1828.172535	11244.495740	63.237914
1827.516740	11174.984725	63.242919
1826.577145	11115.449766	63.247924
1826.125607	11042.910421	63.252929
1825.303808	10990.896212	63.257934
1824.655969	10933.068752	63.262938
1824.011288	10852.363413	63.267943
1823.366689	10795.254799	63.272948
1822.990542	10719.595362	63.277953
1822.059012	10669.731702	63.282958
1821.495545	10599.551787	63.287962
1821.156195	10519.946222	63.292967
1820.192037	10463.373287	63.297972
1819.814476	10387.374477	63.302977
1819.274916	10322.798933	63.307982
1818.430903	10267.687088	63.312986
1817.915590	10189.475633	63.317991
1817.104839	10118.928108	63.322996
1816.645933	10038.259556	63.328001
1815.458448	9986.859978	63.333006
1814.715282	9908.791690	63.338010
1814.469560	9846.492003	63.343015
1813.458524	9781.140729	63.348020
1813.068318	9709.357462	63.353025
1812.342229	9637.885874	63.358030
1811.951760	9578.363480	63.363034
1811.091760	9513.847413	63.368039
1810.217830	9439.869166	63.373044
1809.982799	9365.130240	63.378049
1808.942361	9305.066752	63.383054
1807.954838	9244.717383	63.388058
1807.355228	9173.232654	63.393063
1806.751248	9109.621673	63.398068
1806.328801	9053.646927	63.403073
1805.146816	8992.182694	63.408078
1804.849849	8932.051950	63.413082
1804.233452	8866.055795	63.418087
1803.339725	8812.159156	63.423092
1802.418858	8733.249453	63.428097
1801.892913	8683.727580	63.433102
1801.311998	8617.656667	63.438106
1801.027562	8548.537448	63.443111
1800.213642	8491.064474	63.448116
1799.602813	8426.650790	63.453121
1799.062313	8372.367502	63.458126
1798.706656	8303.217332	63.463130
1797.863279	8232.370645	63.468135
1796.707877	8162.568275	63.473140
1796.449205	8090.619593	63.478145
1795.630973	8045.340905	63.483150
1794.948166	7987.686134	63.488154
1794.327239	7921.140652	63.493159
1793.868383	7847.389934	63.498164
1793.569304	7782.390303	63.503169
1792.247382	7719.733887	63.508174
1791.740451	7651.448952	63.513178
1791.207313	7579.822818	63.518183
1790.170861	7527.050032	63.523188
1789.760475	7451.638884	63.528193
1789.026030	7403.013847	63.533198
1788.368743	7331.703659	63.538202
1787.727179	7267.149572	63.543207
1787.118891	7202.721431	63.548212
1786.780009	7139.404895	63.553217
1785.592115	7078.426742	63.558222
1785.073099	7016.638958	63.563226
1784.699042	6944.858870	63.568231
1783.682570	6896.831288	63.573236
1783.003485	6820.532001	63.578241
1782.443144	6758.359004	63.583246
1782.233258	6695.523206	63.588250
1781.566625	6630.317177	63.593255
1780.359615	6567.178012	63.598260
1779.958446	6498.441391	63.603265
1779.034360	6428.406896	63.608270
1778.540816	6369.868506	63.613274
1778.024080	6303.422952	63.618279
1777.170664	6245.496743	63.623284
1776.455376	6184.175069	63.628289
1775.599187	6122.354620	63.633294
1774.957665	6060.953902	63.638298
1774.511051	5995.592665	63.643303
1773.912983	5935.114777	63.648308
1773.233045	5873.913402	63.653313
1772.664237	5815.901867	63.658318
1771.889851	5742.471586	63.663322
1771.385323	5683.149647	63.668327
1770.270265	5627.438148	63.673332
1769.970022	5549.943064	63.678337
1769.357998	5490.680772	63.683342
1768.424050	5426.346759	63.688346
1767.950738	5364.665071	63.693351
1767.073047	5305.565605	63.698356
1766.600236	5233.775548	63.703361
1765.720392	5187.308157	63.708366
1765.062867	5126.524355	63.713370
1764.723034	5057.880895	63.718375
1763.557405	4997.781712	63.723380
1762.947371	4936.797904	63.728385
1762.650583	4881.545307	63.733390
1761.847853	4821.208588	63.738394
1761.095298	4764.705302	63.743399
1760.219052	4702.861633	63.748404
1759.562433	4644.490834	63.753409
1759.085882	4590.887139	63.758414
1758.294846	4532.204499	63.763418
1757.989587	4473.585336	63.768423
1757.289412	4423.212094	63.773428
1756.731569	4357.428551	63.778433
1755.925600	4290.826587	63.783438
1755.255011	4230.576199	63.788442
1754.320283	4172.566920	63.793447
1753.268968	4126.537870	63.798452
1752.836385	4066.234580	63.803457
1751.955560	4012.660915	63.808462
1751.303984	3956.692837	63.813466
1750.753418	3908.616359	63.818471
1750.067316	3859.434526	63.823476
1750.043359	3795.047497	63.828481
1749.118327	3744.236713	63.833486
1748.562626	3688.983959	63.838490
1747.695467	3621.609218	63.843495
1747.086625	3573.280463	63.848500
1746.549349	3509.461242	63.853505
1745.564371	3458.448027	63.858510
1744.996811	3403.722694	63.863514
1744.933893	3339.115133	63.868519
1743.873022	3286.470998	63.873524
1743.426482	3217.424810	63.878529
1742.655895	3165.951901	63.883534
1741.742441	3112.645381	63.888538
1741.185586	3052.329708	63.893543
1740.665255	2998.426464	63.898548
1740.321116	2942.648438	63.903553
1739.320938	2888.541053	63.908558
1738.121083	2828.247985	63.913562
1738.140026	2772.467356	63.918567
1737.168755	2722.610663	63.923572
1736.581754	2660.599528	63.928577
1735.548415	2602.516698	63.933582
1734.829965	2534.487706	63.938586
1734.542352	2493.503218	63.943591
1733.846923	2443.616284	63.948596
1733.379679	2379.800319	63.953601
1732.504948	2328.417872	63.958606
1731.428583	2276.947762	63.963610
1731.241013	2225.346922	63.968615
1730.338698	2177.113546	63.973620
1729.626222	2117.538547	63.978625
1729.130301	2063.518945	63.983630
1728.390325	2018.804249	63.988634
1727.870336	1965.085345	63.993639
1726.681389	1913.993206	63.998644
1726.432591	1863.496347	64.003649
1725.820575	1820.128550	64.008654
1725.012175	1767.481336	64.013658
1724.370017	1704.934166	64.018663
1723.608853	1659.309981	64.023668
1723.284506	1604.797991	64.028673
1722.452377	1563.807179	64.033678
1721.535005	1506.671558	64.038682
1721.214999	1456.192937	64.043687
1720.327560	1413.587687	64.048692
1720.099231	1355.793591	64.053697
1719.034097	1306.169562	64.058702
1718.398882	1251.232772	64.063706
1717.770996	1217.625231	64.068711
1716.909708	1165.987683	64.073716
1716.275368	1115.976519	64.078721
1715.429944	1065.885504	64.083726
1714.696584	1028.724646	64.088730
1714.338736	980.108326	64.093735
1713.393307	940.626812	64.098740
1713.120183	884.624573	64.103745
1712.387606	849.413295	64.108750
1711.513741	800.048430	64.113754
1711.316810	757.690265	64.118759
1709.875528	713.131190	64.123764
1709.384366	658.251036	64.128769
1708.707540	619.041565	64.133774
1707.966556	580.392773	64.138778
1707.434561	531.895504	64.143783
1706.807560	508.872860	64.148788
1706.092285	456.853507	64.153793
1705.166322	408.542233	64.158798
1704.437248	394.278922	64.163802
1704.039613	340.517405	64.168807
1703.035318	313.017183	64.173812
1702.219803	268.244966	64.178817
1701.762939	247.491817	64.183822
1701.172784	214.823650	64.188826
1700.935330	180.265501	64.193831
1699.535405	142.422726	64.198836
1699.249570	109.466758	64.203841
1698.086725	82.188495	64.208846
1696.997868	66.902431	64.213850
1696.075615	38.630393	64.218855
1693.434698	67.988885	64.223860
1692.705949	71.408433	64.228865
1692.624655	79.596407	64.233870
1692.328788	64.357856	64.238874
1691.814100	77.023880	64.243879
1691.105570	78.502120	64.248884
1690.854683	81.159784	64.253889
1690.053702	80.564798	64.258894
1688.925220	82.390447	64.263898
1688.581165	80.320954	64.268903
1687.868577	86.101822	64.273908
1687.519772	82.504996	64.278913
1686.580286	87.295297	64.283918
1685.341380	91.250056	64.288922
1685.249064	83.100768	64.293927
1684.633017	94.757876	64.298932
1684.103809	80.210820	64.303937
1683.502679	90.471511	64.308942
1683.095003	88.804790	64.313946
1683.042907	82.688141	64.318951
1681.533617	86.752082	64.323956
1681.325091	83.856805	64.328961
1680.480327	85.465500	64.333966
1679.651721	90.656089	64.338970
1679.088761	77.401209	64.343975
1678.009106	90.787778	64.348980
1677.265046	88.846481	64.353985
1676.527677	87.370906	64.358990
1676.355763	91.356455	64.363994
1676.024330	82.677441	64.368999
1675.354799	90.645043	64.374004
1674.956629	83.962040	64.379009
1674.253654	88.370995	64.384014
1672.515113	93.930059	64.389018
1671.902994	87.249502	64.394023
1671.151829	93.627869	64.399028
1670.624012	92.634678	64.404033
1670.695221	84.850504	64.409038
1670.056297	94.483261	64.414042
1669.864392	85.755275	64.419047
1668.394930	97.634685	64.424052
1667.693939	92.228246	64.429057
1667.257891	82.499819	64.434062
1666.593042	90.914538	64.439066
1666.352357	86.283393	64.444071
1665.323862	89.624410	64.449076
1664.575405	90.705296	64.454081
1664.061335	84.504336	64.459086
1663.108336	90.053738	64.464090
1662.735325	83.951798	64.469095
1661.580376	88.178661	64.474100
1660.817046	82.526661	64.479105
1660.206525	83.475248	64.484110
1659.875509	87.935507	64.489114
1659.946506	84.205766	64.494119
1658.591236	97.760709	64.499124
1658.410540	93.266692	64.504129
1657.167759	84.760839	64.509134
1656.696248	90.790428	64.514138
1656.622671	86.068082	64.519143
1655.317868	91.148242	64.524148
1654.765806	90.201484	64.529153
1653.947170	90.484534	64.534158
1653.817291	88.791035	64.539162
1653.038026	87.397817	64.544167
1651.812059	90.264000	64.549172
1651.857326	87.490837	64.554177
1650.719902	86.490411	64.559182
1649.947644	94.453837	64.564186
1650.085287	89.467699	64.569191
1648.839346	87.107816	64.574196
1647.748800	88.042774	64.579201
1647.217649	87.245663	64.584206
1647.052313	88.173994	64.589210
1646.979929	82.899520	64.594215
1645.326902	87.792148	64.599220
1645.019534	87.016258	64.604225
1644.494089	86.314436	64.609230
1643.692643	91.182171	64.614234
1642.632708	83.194491	64.619239
1642.151393	80.463981	64.624244
1641.924605	78.524102	64.629249
1640.976998	79.866868	64.634254
1639.833499	81.346412	64.639258
1640.257353	71.506626	64.644263
1638.888711	81.294727	64.649268
1637.875967	79.143812	64.654273
1637.930785	86.822879	64.659278
1637.219061	84.195206	64.664282
1636.321508	80.795954	64.669287
1635.361315	90.668987	64.674292
1635.302418	79.926587	64.679297
1634.300853	83.936702	64.684302
1633.666499	94.366685	64.689306
1633.522435	80.539064	64.694311
1632.320033	86.594879	64.699316
1631.788068	76.523731	64.704321
1631.162804	80.677494	64.709326
1630.321066	85.628904	64.714330
1629.924029	84.277474	64.719335
1629.028336	83.738555	64.724340
1628.551186	77.260504	64.729345
1628.406140	81.132971	64.734350
1627.424606	87.896454	64.739354
1626.883528	83.559045	64.744359
1626.345499	82.083357	64.749364
1625.597893	94.024725	64.754369
1624.604052	82.071506	64.759374
1623.152789	88.266211	64.764378
1623.057877	83.492064	64.769383
1622.688063	91.402597	64.774388
1621.956754	84.911305	64.779393
1621.014353	87.913803	64.784398
1620.081707	88.609219	64.789402
1620.580792	81.231743	64.794407
1619.477915	86.844393	64.799412
1618.631926	82.760434	64.804417
1618.262611	79.961673	64.809422
1617.540728	87.890291	64.814426
1617.086506	78.513279	64.819431
1616.226108	79.458995	64.824436
1615.272081	75.206121	64.829441
1614.343111	76.620054	64.834446
1614.164590	83.872558	64.839450
1613.500566	77.077266	64.844455
1612.484094	90.818094	64.849460
1611.415184	81.202844	64.854465
1611.515342	83.106143	64.859470
1610.779951	92.858313	64.864474
1610.086204	80.646112	64.869479
1609.096115	85.606904	64.874484
1608.733623	84.346184	64.879489
1608.048574	80.157812	64.884494
1607.344667	83.358969	64.889498
1607.211049	79.918785	64.894503
1606.580532	79.730410	64.899508
1606.081423	75.482537	64.904513
1605.469216	73.731630	64.909518
1603.928783	76.371823	64.914522
1603.147663	70.102925	64.919527
1602.174387	68.977094	64.924532
1601.726769	70.232553	64.929537
1602.180820	73.043154	64.934542
1600.866329	76.107927	64.939546
1600.558401	81.933331	64.944551
1599.686560	84.166103	64.949556
1599.270694	79.695267	64.954561
1598.773317	77.222789	64.959566
1597.510465	84.964541	64.964570
1596.600344	79.178190	64.969575
1595.770327	77.271077	64.974580
1595.739317	82.249807	64.979585
1594.748995	72.137956	64.984590
1593.980592	84.683451	64.989594
1593.385906	79.517197	64.994599
1592.615759	82.255791	64.999604
1592.572303	79.301182	65.004609
1592.306997	77.897290	65.009614
1591.364205	76.181564	65.014618
1591.176776	77.659040	65.019623
1590.076369	82.985874	65.024628
1588.942411	76.856618	65.029633
1588.541241	81.318565	65.034638
1587.881668	84.159442	65.039642
1587.828430	67.992956	65.044647
1586.107598	78.838409	65.049652
1585.281287	80.753287	65.054657
1584.555952	89.802110	65.059662
1584.494236	84.612679	65.064666
1583.776589	80.148793	65.069671
1582.912228	85.534323	65.074676
1582.267831	87.849236	65.079681
1581.770207	82.103008	65.084686
1581.303052	82.528934	65.089690
1581.050390	76.951948	65.094695
1580.139035	74.441169	65.099700
1579.403671	73.181351	65.104705
1578.338405	78.982004	65.109710
1577.419328	86.328518	65.114714
1577.002784	80.492138	65.119719
1576.310119	86.205208	65.124724
1575.785892	83.418451	65.129729
1575.398436	72.141636	65.134734
1574.681614	83.940916	65.139738
1574.568546	78.068935	65.144743
1573.236566	83.096675	65.149748
1572.318589	81.351781	65.154753
1571.929381	78.349606	65.159758
1571.086273	84.036117	65.164762
1570.732255	73.821598	65.169767
1570.092829	79.901526	65.174772
1569.541561	75.759721	65.179777
1569.072249	73.907271	65.184782
1567.791981	84.761586	65.189786
1567.124909	76.060236	65.194791
1566.309764	79.913019	65.199796
1565.523366	84.445640	65.204801
1565.325644	82.258297	65.209806
1564.763361	86.736386	65.214810
1564.432764	74.698322	65.219815
1563.928956	77.172251	65.224820
1563.011873	81.638904	65.229825
1562.117144	69.062847	65.234830
1561.360046	77.202071	65.239834
1561.275323	73.873972	65.244839
1560.132631	72.604763	65.249844
1558.960955	77.890892	65.254849
1558.096963	79.206209	65.259854
1557.509041	78.970077	65.264858
1557.558533	78.471813	65.269863
1556.918980	80.473721	65.274868
1556.028015	82.185991	65.279873
1555.332823	74.440027	65.284878
1554.750199	84.259392	65.289882
1554.518063	76.930288	65.294887
1553.940875	81.008618	65.299892
1552.589242	71.879879	65.304897
1551.835926	74.365070	65.309902
1550.436982	82.759252	65.314906
1550.790788	72.143683	65.319911
1550.425204	64.581898	65.324916
1549.741727	72.141715	65.329921
1549.141934	75.618080	65.334926
1548.283147	81.594096	65.339930
1547.967482	75.021020	65.344935
1546.810553	80.536625	65.349940
1546.090954	73.713917	65.354945
1545.357445	73.646003	65.359950
1544.607504	74.813890	65.364954
1544.329462	74.156357	65.369959
1543.748107	75.267494	65.374964
1543.078340	81.410597	65.379969
1541.964195	78.840591	65.384974
1541.087165	84.496229	65.389978
1540.529316	73.057262	65.394983
1540.112203	78.835362	65.399988
1539.101927	74.009556	65.404993
1539.192741	73.799620	65.409998
1538.434159	78.143321	65.415002
1538.231191	72.750837	65.420007
1537.888805	68.082259	65.425012
1536.613562	73.613513	65.430017
1535.736825	75.760347	65.435022
1535.027205	76.947062	65.440026
1534.708478	72.566463	65.445031
1533.055140	79.274294	65.450036
1532.395453	79.562087	65.455041
1532.617173	79.678282	65.460046
1531.816837	76.960643	65.465050
1531.377852	78.549059	65.470055
1530.707222	77.990182	65.475060
1529.899203	83.817786	65.480065
1528.851403	78.035994	65.485070
1527.897881	85.118333	65.490074
1527.710401	76.834379	65.495079
1526.979175	81.547479	65.500084
1526.508995	71.259967	65.505089
1526.225897	69.597134	65.510094
1525.411943	81.340891	65.515098
1524.503051	71.903693	65.520103
1523.634950	74.779296	65.525108
1522.885069	75.406279	65.530113
1522.698991	76.218063	65.535118
1522.034971	80.652399	65.540122
1521.507237	66.669737	65.545127
1520.227168	77.866235	65.550132
1519.096578	78.689337	65.555137
1518.898894	79.033028	65.560142
1518.187179	86.635193	65.565146
1517.636951	73.129192	65.570151
1517.350496	89.035909	65.575156
1517.010986	81.332783	65.580161
1516.541804	77.677846	65.585166
1515.260821	78.494886	65.590170
1514.640232	71.976581	65.595175
1514.354801	75.131759	65.600180
1513.458882	74.168713	65.605185
1512.559856	76.052589	65.610190
1511.576274	76.536939	65.615194
1511.236992	69.754734	65.620199
1510.476486	73.501076	65.625204
1510.046307	76.791221	65.630209
1509.785049	72.601770	65.635214
1508.613199	79.398682	65.640218
1507.495899	65.206938	65.645223
1506.477049	75.592368	65.650228
1506.076341	71.608006	65.655233
1505.875583	65.429848	65.660238
1505.575093	75.237494	65.665242
1505.490943	71.092439	65.670247
1504.754545	80.078372	65.675252
1503.167631	75.713229	65.680257
1502.633942	69.616362	65.685262
1502.010589	72.352151	65.690266
1501.615378	75.625702	65.695271
1500.902074	68.953400	65.700276
1499.539157	74.575874	65.705281
1499.105235	71.755863	65.710286
1497.973625	82.473037	65.715290
1497.729527	69.128135	65.720295
1497.439081	83.668248	65.725300
1496.801811	83.241274	65.730305
1496.889671	69.409951	65.735310
1495.663047	86.510026	65.740314
1494.830277	80.328221	65.745319
1493.940271	84.289116	65.750324
1493.407706	83.391336	65.755329
1493.335867	83.640913	65.760334
1492.210589	82.343736	65.765338
1491.152601	84.949902	65.770343
1490.339024	79.613459	65.775348
1489.838094	76.253736	65.780353
1489.477152	76.219671	65.785358
1489.056818	79.632836	65.790362
1488.667780	76.097634	65.795367
1487.708156	83.491617	65.800372
1486.721372	85.974505	65.805377
1486.209439	80.629549	65.810382
1485.353745	84.359487	65.815386
1485.341612	80.693424	65.820391
1484.471736	89.733696	65.825396
1483.159294	85.733378	65.830401
1482.586922	85.441175	65.835406
1481.951721	88.828565	65.840410
1481.506329	87.282992	65.845415
1481.121637	89.646543	65.850420
1480.402353	75.382089	65.855425
1480.139155	85.421937	65.860430
1478.806801	90.484476	65.865434
1478.355679	82.072113	65.870439
1477.833892	86.099075	65.875444
1477.024803	79.058797	65.880449
1475.953183	75.720387	65.885454
1474.948105	89.237084	65.890458
1474.741225	74.970047	65.895463
1474.100507	84.902734	65.900468
1473.642154	79.998702	65.905473
1473.369309	76.035026	65.910478
1472.724863	83.531889	65.915482
1472.119003	74.279945	65.920487
1471.026807	78.518986	65.925492
1470.458638	70.688212	65.930497
1470.257679	74.851843	65.935502
1468.697848	78.594343	65.940506
1467.963423	69.936852	65.945511
1467.419761	74.172296	65.950516
1466.903764	76.957263	65.955521
1466.447471	70.835490	65.960526
1465.786651	73.930482	65.965530
1465.741701	71.433439	65.970535
1464.435222	72.357058	65.975540
1463.332642	83.080669	65.980545
1463.008031	75.411461	65.985550
1462.531812	76.466481	65.990554
1462.390202	72.893539	65.995559
1461.036811	71.489127	66.000564
1460.108658	78.168477	66.005569
1459.764254	74.354950	66.010574
1459.200243	80.836078	66.015578
1459.035751	74.589081	66.020583
1457.697573	73.836693	66.025588
1456.966050	77.053313	66.030593
1456.325876	75.078229	66.035598
1455.871476	78.588276	66.040602
1455.448678	71.567041	66.045607
1454.867846	74.303967	66.050612
1453.209575	75.573665	66.055617
1453.113246	73.122635	66.060622
1452.070778	76.308250	66.065626
1451.811182	71.631260	66.070631
1451.821502	73.786949	66.075636
1450.882040	70.927447	66.080641
1449.993435	73.183428	66.085646
1448.969396	82.092086	66.090650
1448.819241	77.172194	66.095655
1448.424409	79.472703	66.100660
1447.054170	74.541721	66.105665
1446.327675	70.845696	66.110670
1445.376338	82.299063	66.115674
1445.005757	79.614076	66.120679
1444.978157	76.981811	66.125684
1444.171100	83.331259	66.130689
1443.784782	76.484000	66.135694
1442.610143	78.995183	66.140698
1441.594471	82.152890	66.145703
1441.204788	82.284250	66.150708
1440.850304	83.856096	66.155713
1440.449330	76.202183	66.160718
1439.341777	78.557623	66.165722
1438.468151	78.767479	66.170727
1437.934501	82.318511	66.175732
1437.368691	80.451461	66.180737
1437.320946	78.470531	66.185742
1435.675243	86.525514	66.190746
1434.998380	78.046542	66.195751
1434.330670	87.447357	66.200756
1434.102500	82.503594	66.205761
1433.967932	75.152697	66.210766
1432.780176	88.946022	66.215770
1431.698077	78.344204	66.220775
1431.122813	80.883130	66.225780
1430.480350	81.929887	66.230785
1430.006929	77.042454	66.235790
1429.793786	91.663326	66.240794
1429.137085	80.684808	66.245799
1427.821276	77.585507	66.250804
1427.487683	82.405741	66.255809
1427.107790	80.209520	66.260814
1426.425461	86.920775	66.265818
1425.715149	76.914310	66.270823
1424.507178	77.877486	66.275828
1423.710288	80.200902	66.280833
1423.671890	72.153471	66.285838
1423.025018	79.933003	66.290842
1422.528241	67.531885	66.295847
1421.616536	75.184773	66.300852
1420.565102	77.370451	66.305857
1420.609724	70.489397	66.310862
1419.668166	82.321266	66.315866
1419.130822	75.395516	66.320871
1418.090307	76.623817	66.325876
1417.205731	74.952521	66.330881
1416.763417	79.630762	66.335886
1416.281819	82.225767	66.340890
1415.677810	82.984137	66.345895
1414.816659	76.335363	66.350900
1413.583222	83.044330	66.355905
1413.586237	67.015597	66.360910
1412.784389	80.055292	66.365914
1412.562665	82.823458	66.370919
1412.002226	82.307022	66.375924
1411.052295	79.531200	66.380929
1410.546618	78.190768	66.385934
1409.729486	83.922078	66.390938
1409.013818	75.936568	66.395943
1408.080124	78.456776	66.400948
1406.842962	77.831863	66.405953
1406.532200	77.379821	66.410958
1405.852123	83.318008	66.415962
1405.564398	85.298720	66.420967
1405.296833	85.360211	66.425972
1404.914447	82.675530	66.430977
1404.513182	80.596251	66.435982
1403.102916	84.067431	66.440986
1402.571414	77.098178	66.445991
1401.823477	75.126046	66.450996
1400.561834	79.319507	66.456001
1400.144580	78.461767	66.461006
1399.469768	81.447034	66.466010
1399.198768	80.507699	66.471015
1398.808271	73.959163	66.476020
1397.799204	78.162940	66.481025
1396.998611	75.746589	66.486030
1396.192382	84.986498	66.491034
1395.882753	66.053806	66.496039
1395.516165	77.426848	66.501044
1394.589274	82.218390	66.506049
1394.030770	70.167716	66.511054
1393.139737	82.242297	66.516058
1392.897608	80.508312	66.521063
1391.915021	73.897775	66.526068
1390.916486	80.883227	66.531073
1390.528833	82.504506	66.536078
1389.868443	79.261617	66.541082
1389.426854	76.125876	66.546087
1388.535280	77.865105	66.551092
1387.424089	81.992079	66.556097
1387.081438	72.682556	66.561102
1386.473938	82.031226	66.566106
1386.301644	76.537691	66.571111
1385.186778	82.527648	66.576116
1384.076174	78.340760	66.581121
1383.717636	71.339290	66.586126
1383.056490	83.599684	66.591130
1383.080432	74.440047	66.596135
1382.325703	79.183724	66.601140
1381.209325	84.401210	66.606145
1380.609655	80.055833	66.611150
1379.605257	81.114403	66.616154
1379.713416	76.867823	66.621159
1378.661102	74.013672	66.626164
1377.504771	78.220365	66.631169
1376.986466	75.043205	66.636174
1376.569761	84.035116	66.641178
1376.211383	71.222499	66.646183
1375.576808	75.625375	66.651188
1374.297155	77.599765	66.656193
1373.992267	77.066369	66.661198
1372.838514	77.424856	66.666202
1372.430939	78.822221	66.671207
1372.158909	79.523098	66.676212
1371.599596	75.054614	66.681217
1370.951008	72.104749	66.686222
1369.841210	75.575489	66.691226
1369.286083	72.244911	66.696231
1368.941078	67.192002	66.701236
1368.216974	73.547201	66.706241
1367.466118	68.186645	66.711246
1366.504572	73.510408	66.716250
1366.098990	71.294628	66.721255
1365.921782	77.640162	66.726260
1364.700187	75.759107	66.731265
1364.188885	62.043555	66.736270
1363.163885	72.721740	66.741274
1362.843238	74.952118	66.746279
1362.287537	76.887123	66.751284
1361.128600	80.889232	66.756289
1360.618536	74.648296	66.761294
1359.925156	82.414733	66.766298
1359.423075	80.256871	66.771303
1359.199709	71.954998	66.776308
1358.149810	74.381731	66.781313
1357.496836	70.707163	66.786318
1356.894928	85.457634	66.791322
1356.076321	81.451424	66.796327
1355.758607	73.662870	66.801332
1354.706926	80.696206	66.806337
1354.215540	71.692614	66.811342
1353.553396	80.696734	66.816346
1353.040931	74.402565	66.821351
1352.196250	78.835694	66.826356
1351.263489	80.510519	66.831361
1350.914898	72.871957	66.836366
1350.155195	81.678697	66.841370
1349.487790	80.643111	66.846375
1349.234788	83.056705	66.851380
1347.789746	80.343848	66.856385
1347.248327	75.033580	66.861390
1346.618163	85.390387	66.866394
1346.017449	76.631258	66.871399
1345.735037	68.881252	66.876404
1345.379038	77.464538	66.881409
1344.765895	73.239588	66.886414
1343.604856	76.912451	66.891418
1343.038195	70.067080	66.896423
1342.295843	71.927682	66.901428
1341.338604	84.667242	66.906433
1340.941821	69.230362	66.911438
1340.316482	76.050841	66.916442
1339.819686	74.699551	66.921447
1339.424900	73.035574	66.926452
1337.973908	81.975870	66.931457
1337.514709	75.916090	66.936462
1336.543812	83.277216	66.941466
1336.219519	80.550195	66.946471
1335.858556	78.653758	66.951476
1335.515735	80.988590	66.956481
1334.476213	71.070772	66.961486
1333.550192	81.990282	66.966490
1333.021688	78.341663	66.971495
1332.672583	81.502248	66.976500
1331.805379	81.685887	66.981505
1331.007398	70.903340	66.986510
1330.111298	79.435298	66.991514
1329.858139	79.652204	66.996519
1329.399508	80.236093	67.001524
1328.120472	75.066753	67.006529
1327.584719	71.239515	67.011534
1327.058506	82.188505	67.016538
1326.576921	76.518643	67.021543
1326.181820	71.656633	67.026548
1324.945369	79.747535	67.031553
1324.627913	70.432446	67.036558
1323.854803	85.460876	67.041562
1323.253400	83.492278	67.046567
1322.633595	82.666754	67.051572
1321.092811	82.397662	67.056577
1320.774616	74.837851	67.061582
1320.451718	75.649323	67.066586
1319.907690	77.561979	67.071591
1319.739183	79.517437	67.076596
1318.618261	84.283080	67.081601
1317.950428	74.172133	67.086606
1316.965292	78.436789	67.091610
1316.711990	78.283132	67.096615
1316.065288	66.642329	67.101620
1314.971425	77.713105	67.106625
1314.583736	72.864111	67.111630
1313.992722	76.356473	67.116634
1313.464070	73.665101	67.121639
1312.266471	75.292159	67.126644
1311.310198	74.436553	67.131649
1311.107474	67.933880	67.136654
1310.643243	71.497548	67.141658
1310.413119	74.796914	67.146663
1309.529920	78.901862	67.151668
1308.409056	76.241568	67.156673
1308.303831	71.877527	67.161678
1307.241727	76.581781	67.166682
1306.832261	75.535160	67.171687
1305.639343	70.776345	67.176692
1305.072600	76.102013	67.181697
1304.635054	69.109969	67.186702
1304.324600	80.969258	67.191706
1303.475095	78.227975	67.196711
1302.677765	77.276138	67.201716
1301.749296	78.538710	67.206721
1301.462598	77.420531	67.211726
1301.254865	80.393060	67.216730
1299.960864	78.389507	67.221735
1299.369269	79.746754	67.226740
1298.672215	75.498887	67.231745
1298.221998	79.031946	67.236750
1297.125537	86.165464	67.241754
1296.271365	76.883672	67.246759
1295.989305	78.701065	67.251764
1295.275959	82.999788	67.256769
1295.223875	71.500993	67.261774
1294.331995	77.091249	67.266778
1293.451733	78.764055	67.271783
1292.784469	79.165078	67.276788
1291.947894	79.321783	67.281793
1291.982944	75.698690	67.286798
1290.752062	82.642268	67.291802
1289.940510	85.316564	67.296807
1289.422666	81.308288	67.301812
1288.912548	82.384499	67.306817
1288.568271	70.933740	67.311822
1286.978055	72.142260	67.316826
1286.401868	80.077734	67.321831
1285.745930	69.586439	67.326836
1285.131212	78.091015	67.331841
1285.182915	81.561618	67.336846
1284.745306	78.489921	67.341850
1283.733021	78.854340	67.346855
1283.062749	72.071192	67.351860
1282.485458	73.621711	67.356865
1282.003078	71.875477	67.361870
1280.746904	78.105560	67.366874
1279.834600	82.450113	67.371879
1279.559688	73.487816	67.376884
1278.823765	77.304426	67.381889
1277.977330	70.768489	67.386894
1277.142710	80.530179	67.391898
1276.637692	83.270857	67.396903
1276.442605	80.193716	67.401908
1275.757510	77.893083	67.406913
1275.690295	80.009057	67.411918
1274.030420	87.514445	67.416922
1273.452196	78.100476	67.421927
1272.868612	81.785632	67.426932
1272.237047	87.924293	67.431937
1271.935569	78.829022	67.436942
1270.616509	85.364004	67.441946
1270.266288	76.150328	67.446951
1269.834982	74.790216	67.451956
1269.238183	70.545343	67.456961
1268.356981	67.042710	67.461966
1267.648669	68.897919	67.466970
1266.964747	76.697559	67.471975
1266.796965	69.568012	67.476980
1265.671910	79.989324	67.481985
1264.567911	69.709632	67.486990
1263.958277	74.379802	67.491994
1263.670710	80.910044	67.496999
1263.445543	78.058462	67.502004
1262.777944	80.426021	67.507009
1261.982863	82.630923	67.512014
1261.065695	80.233154	67.517018
1260.464727	79.876162	67.522023
1259.928518	74.643938	67.527028
1258.523041	87.341252	67.532033
1258.199242	84.139497	67.537038
1257.805538	84.292025	67.542042
1257.443594	86.674063	67.547047
1256.949883	79.227329	67.552052
1255.405204	89.057781	67.557057
1255.099263	76.834525	67.562062
1254.470021	77.710486	67.567066
1254.006312	73.305680	67.572071
1253.046891	80.928357	67.577076
1252.070226	76.772275	67.582081
1251.651640	74.249499	67.587086
1251.224144	78.390812	67.592090
1250.960098	81.020636	67.597095
1249.944504	76.200535	67.602100
1248.668476	79.380787	67.607105
1248.545820	79.121206	67.612110
1248.218202	78.632441	67.617114
1247.223537	77.560612	67.622119
1246.455915	71.236084	67.627124
1245.660320	79.332610	67.632129
1245.063745	70.553935	67.637134
1244.648539	70.399222	67.642138
1244.158322	70.781566	67.647143
1243.252210	67.345983	67.652148
1242.180071	73.080035	67.657153
1241.553641	63.566517	67.662158
1241.255233	72.296766	67.667162
1241.069837	73.256694	67.672167
1240.321079	73.828385	67.677172
1239.573475	73.278672	67.682177
1239.291579	68.805536	67.687182
1237.805905	84.617496	67.692186
1236.912235	69.229701	67.697191
1236.492319	76.869093	67.702196
1236.023134	79.608809	67.707201
1235.752624	64.730635	67.712206
1234.561590	68.597546	67.717210
1233.780636	81.335904	67.722215
1233.518977	72.942371	67.727220
1232.831383	84.068421	67.732225
1232.070515	74.467467	67.737230
1230.855253	78.423392	67.742234
1230.298876	78.440942	67.747239
1230.289706	76.540620	67.752244
1229.299177	80.580658	67.757249
1229.135090	69.787241	67.762254
1227.998441	82.071227	67.767258
1227.203049	75.722735	67.772263
1226.995096	78.572300	67.777268
1226.173177	77.003074	67.782273
1225.409874	67.418285	67.787278
1224.868832	69.090785	67.792282
1224.152106	70.354405	67.797287
1223.550810	71.355240	67.802292
1222.479198	79.003650	67.807297
1221.659826	70.507997	67.812302
1221.028081	76.023790	67.817306
1220.262002	76.279695	67.822311
1220.497785	76.718481	67.827316
1219.797170	72.248855	67.832321
1219.298788	64.624685	67.837326
1218.456025	64.877015	67.842330
1217.742589	69.905900	67.847335
1217.221129	67.431030	67.852340
1215.924582	77.294575	67.857345
1215.170369	67.071251	67.862350
1214.573807	75.249671	67.867354
1213.732302	76.746027	67.872359
1213.625162	66.072871	67.877364
1213.072804	74.395649	67.882369
1212.383108	65.865188	67.887374
1211.435562	67.731647	67.892378
1210.925461	72.937935	67.897383
1210.503003	65.904092	67.902388
1209.198355	76.328749	67.907393
1208.750417	66.898820	67.912398
1208.488692	72.969209	67.917402
1207.876786	69.020071	67.922407
1207.036434	70.694442	67.927412
1205.884748	74.340643	67.932417
1205.566485	68.528147	67.937422
1205.031602	74.656169	67.942426
1204.324316	71.710956	67.947431
1203.434748	70.318078	67.952436
1202.774056	71.971764	67.957441
1202.246817	69.018419	67.962446
1201.832741	76.043446	67.967450
1201.406301	75.084698	67.972455
1200.154510	74.518984	67.977460
1199.250986	71.944027	67.982465
1198.916009	74.080505	67.987470
1198.918921	73.138634	67.992474
1197.784057	78.737598	67.997479
1197.120393	68.780580	68.002484
1196.220235	76.668238	68.007489
1195.940876	67.241465	68.012494
1194.537875	76.530587	68.017498
1193.658737	76.824980	68.022503
1193.493450	68.537557	68.027508
1192.810854	82.947630	68.032513
1192.358440	72.922322	68.037518
1192.330558	70.797894	68.042522
1191.550904	70.735843	68.047527
1190.946870	76.095846	68.052532
1190.151153	75.531722	68.057537
1189.327197	74.890087	68.062542
1188.209316	77.862288	68.067546
1187.533137	79.480594	68.072551
1187.191536	78.650283	68.077556
1186.514324	78.735946	68.082561
1185.321055	75.437516	68.087566
1184.777496	66.248307	68.092570
1184.141818	68.653384	68.097575
1183.938284	69.253498	68.102580
1183.615962	69.667500	68.107585
1182.847823	69.004374	68.112590
1182.061179	78.370521	68.117594
1181.244439	71.839362	68.122599
1180.853860	73.795449	68.127604
1179.361894	77.085770	68.132609
1179.038815	79.904761	68.137614
1178.282271	77.864680	68.142618
1177.836637	77.519274	68.147623
1177.665391	69.592348	68.152628
1176.256545	75.589710	68.157633
1175.811867	74.427286	68.162638
1175.238965	73.722073	68.167642
1174.720153	76.794545	68.172647
1174.378841	78.058397	68.177652
1173.017913	84.185339	68.182657
1172.541360	75.423868	68.187662
1171.895597	75.799424	68.192666
1171.574300	83.399485	68.197671
1170.981074	70.651086	68.202676
1169.856185	86.946594	68.207681
1169.241386	73.350063	68.212686
1168.879063	77.894186	68.217690
1167.786245	76.060557	68.222695
1167.072066	72.042540	68.227700
1166.752293	77.351029	68.232705
1165.954026	65.948857	68.237710
1165.272630	66.938790	68.242714
1164.454054	72.033295	68.247719
1163.858227	67.621140	68.252724
1163.054533	73.784037	68.257729
1162.951608	71.073877	68.262734
1162.309453	72.883898	68.267738
1160.920802	75.225811	68.272743
1160.711733	73.081316	68.277748
1159.887357	83.278223	68.282753
1159.855392	75.548342	68.287758
1158.535433	80.066579	68.292762
1157.716790	71.657569	68.297767
1157.343521	68.605629	68.302772
1156.834436	73.190440	68.307777
1156.492054	63.718508	68.312782
1155.614337	77.128281	68.317786
1154.463884	72.093130	68.322791
1154.288565	69.760341	68.327796
1153.386826	81.699480	68.332801
1153.197257	73.009066	68.337806
1152.000422	77.408374	68.342810
1151.219213	71.965987	68.347815
1151.175661	67.510150	68.352820
1149.781965	78.906211	68.357825
1149.075351	77.230362	68.362830
1148.719288	78.578565	68.367834
1148.013319	76.554105	68.372839
1147.961541	70.899508	68.377844
1146.859249	74.351795	68.382849
1146.130481	70.862811	68.387854
1145.354923	72.437009	68.392858
1144.921536	77.918113	68.397863
1144.983649	72.988150	68.402868
1143.758165	79.908850	68.407873
1143.006349	67.889014	68.412878
1142.260185	64.702422	68.417882
1141.152063	76.436265	68.422887
1140.483002	63.266281	68.427892
1139.875499	74.215594	68.432897
1139.526772	73.178265	68.437902
1139.223617	73.275407	68.442906
1138.219550	74.578446	68.447911
1137.571118	68.059959	68.452916
1136.538880	79.147797	68.457921
1136.599465	62.863955	68.462926
1136.168690	71.258866	68.467930
1134.946077	70.220185	68.472935
1134.489292	73.938814	68.477940
1133.721311	72.824668	68.482945
1132.968022	69.330127	68.487950
1132.090750	71.108165	68.492954
1131.377316	74.312526	68.497959
1131.046708	66.970778	68.502964
1130.238638	74.459026	68.507969
1129.974337	76.577963	68.512974
1128.563935	69.512045	68.517978
1127.844572	74.273811	68.522983
1127.715985	68.877440	68.527988
1126.990318	72.640415	68.532993
1126.819955	70.303686	68.537998
1125.742189	72.246082	68.543002
1124.955884	62.950425	68.548007
1124.404753	67.455194	68.553012
1123.730560	75.846250	68.558017
1123.149718	68.243105	68.563022
1122.572784	69.626443	68.568026
1121.581428	70.481186	68.573031
1121.359399	67.570777	68.578036
1120.370316	71.825087	68.583041
1119.523998	69.671572	68.588046
1119.012460	69.486471	68.593050
1118.227105	71.229393	68.598055
1118.208647	59.816749	68.603060
1116.881056	71.525580	68.608065
1115.975701	68.192429	68.613070
1115.760292	76.378045	68.618074
1115.138059	77.514699	68.623079
1114.853387	75.147267	68.628084
1113.708783	69.830508	68.633089
1112.980342	74.182135	68.638094
1112.525104	69.454316	68.643098
1112.075419	78.669106	68.648103
1111.315140	68.555600	68.653108
1110.313616	76.864683	68.658113
1109.579967	70.504840	68.663118
1109.176800	65.757702	68.668122
1108.472643	78.056505	68.673127
1108.083359	71.528344	68.678132
1107.065956	74.126623	68.683137
1106.709572	79.849375	68.688142
1106.224952	80.552555	68.693146
1105.452304	75.569295	68.698151
1104.501698	67.022028	68.703156
1103.498418	76.201875	68.708161
1103.019214	71.200324	68.713166
1102.696318	68.419504	68.718170
1102.421878	73.561512	68.723175
1101.284187	64.755424	68.728180
1100.675218	70.108341	68.733185
1100.298799	69.578473	68.738190
1098.766966	73.103838	68.743194
1098.099162	76.968004	68.748199
1097.654560	66.753826	68.753204
1097.311751	78.020588	68.758209
1097.391260	68.434248	68.763214
1096.205714	73.214984	68.768218
1095.353870	68.479295	68.773223
1095.007817	74.115246	68.778228
1094.116608	76.882692	68.783233
1093.101597	76.011282	68.788238
1092.597244	63.844872	68.793242
1092.184452	70.030758	68.798247
1091.775672	59.585383	68.803252
1090.515763	75.288939	68.808257
1089.522196	76.112507	68.813262
1089.540948	66.069053	68.818266
1088.902821	72.839568	68.823271
1088.176455	70.517171	68.828276
1086.925263	81.133651	68.833281
1086.387450	73.755484	68.838286
1086.218096	73.069676	68.843290
1085.334463	79.964405	68.848295
1085.562270	78.486861	68.853300
1084.090767	78.383512	68.858305
1083.304174	74.228807	68.863310
1082.911984	76.555750	68.868314
1081.714079	81.623890	68.873319
1081.202583	73.514559	68.878324
1080.791206	78.848666	68.883329
1080.174510	74.936595	68.888334
1079.728508	71.278070	68.893338
1078.760352	74.068801	68.898343
1078.320367	73.094883	68.903348
1077.383109	70.058560	68.908353
1076.751122	70.092902	68.913358
1076.313902	70.526771	68.918362
1075.181782	74.710811	68.923367
1074.844179	67.617770	68.928372
1074.098997	74.670248	68.933377
1073.775609	70.875525	68.938382
1073.089915	72.228866	68.943386
1071.945235	76.238286	68.948391
1071.700014	62.029498	68.953396
1071.205028	67.449443	68.958401
1070.099867	65.611515	68.963406
1069.318873	73.578020	68.968410
1068.474649	69.342602	68.973415
1068.284201	69.612636	68.978420
1067.744956	80.655183	68.983425
1066.895022	72.670660	68.988430
1065.920434	67.339495	68.993434
1065.293717	79.332671	68.998439
1065.307404	72.614255	69.003444
1064.714397	63.951773	69.008449
1063.320508	70.732135	69.013454
1062.915714	72.998006	69.018458
1062.595327	74.006229	69.023463
1061.940668	62.560759	69.028468
1060.900626	69.554489	69.033473
1059.900699	69.161667	69.038478
1059.780896	71.658168	69.043482
1059.169865	67.373041	69.048487
1058.401275	70.292880	69.053492
1057.466619	69.102771	69.058497
1056.618431	74.085322	69.063502
1056.235719	69.615638	69.068506
1055.787564	82.368891	69.073511
1055.437108	74.339603	69.078516
1054.208174	80.226403	69.083521
1053.987070	74.215549	69.088526
1053.547751	68.627344	69.093530
1052.299118	75.834039	69.098535
1051.655257	73.548990	69.103540
1051.002401	67.518517	69.108545
1050.459386	70.719440	69.113550
1049.613483	69.821144	69.118554
1048.537588	73.554701	69.123559
1048.624946	64.449668	69.128564
1047.844498	76.114062	69.133569
1047.470427	71.620927	69.138574
1046.638364	63.436454	69.143578
1045.791542	69.552623	69.148583
1045.333213	58.670441	69.153588
1044.698690	64.629830	69.158593
1043.237149	63.119850	69.163598
1042.684230	70.821415	69.168602
1041.944828	73.099522	69.173607
1042.088244	64.699934	69.178612
1041.674863	76.346932	69.183617
1040.854992	64.637592	69.188622
1039.845672	68.764261	69.193626
1039.381740	63.919572	69.198631
1038.729883	67.634554	69.203636
1037.646419	81.100741	69.208641
1036.844215	74.930026	69.213646
1036.381891	70.767903	69.218650
1035.812594	73.534615	69.223655
1035.900024	68.654246	69.228660
1034.506259	76.303509	69.233665
1033.774139	68.234026	69.238670
1033.462298	75.633887	69.243674
1032.300982	69.968167	69.248679
1031.277145	69.497157	69.253684
1030.663342	69.604312	69.258689
1030.073333	74.000166	69.263694
1029.931908	77.644983	69.268698
1029.722745	76.563388	69.273703
1029.574370	71.501336	69.278708
1028.149645	85.196866	69.283713
1027.645996	76.048660	69.288718
1026.925957	74.553180	69.293722
1025.201016	86.426203	69.298727
1025.259814	64.722645	69.303732
1024.321436	67.649005	69.308737
1024.267455	72.232391	69.313742
1023.775019	70.938822	69.318746
1022.297946	72.197311	69.323751
1021.879239	69.040661	69.328756
1021.093049	75.978250	69.333761
1020.902060	73.442961	69.338766
1020.485164	76.857214	69.343770
1019.125860	80.306290	69.348775
1018.666364	71.327685	69.353780
1018.156303	71.948195	69.358785
1017.532356	70.136231	69.363790
1016.447448	69.283858	69.368794
1015.748270	72.880219	69.373799
1015.366336	61.195833	69.378804
1015.043219	75.813653	69.383809
1014.316140	72.053206	69.388814
1013.300869	68.732852	69.393818
1012.818716	61.847331	69.398823
1012.509850	67.911032	69.403828
1011.457764	72.613798	69.408833
1010.338625	66.613372	69.413838
1010.082152	68.382563	69.418842
1009.331008	69.478251	69.423847
1009.083064	68.875917	69.428852
1007.867592	75.459185	69.433857
1007.455298	70.098505	69.438862
1007.008366	66.962118	69.443866
1006.232149	79.390674	69.448871
1005.102726	68.560081	69.453876
1004.386883	72.051862	69.458881
1004.091801	73.391957	69.463886
1003.629338	67.124625	69.468890
1002.916616	73.344049	69.473895
1002.966327	63.536955	69.478900
1001.758370	67.501276	69.483905
1001.672334	69.167656	69.488910
1000.367625	73.935853	69.493914
999.248711	74.555471	69.498919
999.046501	64.249139	69.503924
998.348687	69.631980	69.508929
997.258511	77.609850	69.513934
996.839463	71.982163	69.518938
996.133881	74.882532	69.523943
995.828013	68.394741	69.528948
994.988524	75.654631	69.533953
994.051411	71.388290	69.538958
993.663813	66.517272	69.543962
992.887549	71.683939	69.548967
992.447828	63.897534	69.553972
991.411819	76.110382	69.558977
990.393725	68.636777	69.563982
990.234681	64.915267	69.568986
989.699227	70.045195	69.573991
989.507287	58.469360	69.578996
988.317859	68.658146	69.584001
987.230115	67.486115	69.589006
987.160651	60.186428	69.594010
986.591933	70.445185	69.599015
986.022002	57.731008	69.604020
984.849383	65.450757	69.609025
984.270649	65.464033	69.614030
984.140974	67.506366	69.619034
983.166740	68.722714	69.624039
982.075975	69.708446	69.629044
981.343433	67.661457	69.634049
980.996183	73.674499	69.639054
980.833335	64.566705	69.644058
979.369212	66.745678	69.649063
979.050948	63.587248	69.654068
978.262847	70.684421	69.659073
977.740370	72.970607	69.664078
977.472845	59.938652	69.669082
976.276465	69.649154	69.674087
975.819574	63.144400	69.679092
975.055016	73.059007	69.684097
974.774712	69.471911	69.689102
973.725800	64.212539	69.694106
972.888569	75.696747	69.699111
972.684112	69.475099	69.704116
971.979884	76.092151	69.709121
971.598975	68.003076	69.714126
970.537142	62.509219	69.719130
969.696568	60.476271	69.724135
969.359950	61.589588	69.729140
968.235899	70.990540	69.734145
967.291921	66.854614	69.739150
967.091791	67.736478	69.744154
966.498509	74.397377	69.749159
966.305672	71.054985	69.754164
965.126412	73.581302	69.759169
963.763280	73.724131	69.764174
963.722941	65.735408	69.769178
963.197681	76.042451	69.774183
963.394793	72.388849	69.779188
962.304829	66.191416	69.784193
961.310412	68.448623	69.789198
960.955899	65.070458	69.794202
959.442212	75.055390	69.799207
959.016242	65.823887	69.804212
958.388109	68.276699	69.809217
957.814340	69.618568	69.814222
957.723854	66.903290	69.819226
956.854847	71.474441	69.824231
955.806801	62.628937	69.829236
955.392539	62.346388	69.834241
954.882932	66.350990	69.839246
954.007157	68.799055	69.844250
953.103156	72.465871	69.849255
952.470591	64.306462	69.854260
951.893815	64.660057	69.859265
951.356674	66.986427	69.864270
950.729273	65.902008	69.869274
949.683952	75.325134	69.874279
949.168059	71.520063	69.879284
948.783284	66.905650	69.884289
948.220993	67.042475	69.889294
947.450620	68.628520	69.894298
946.340055	73.988746	69.899303
946.255252	66.395033	69.904308
945.734684	69.073583	69.909313
944.933709	72.392845	69.914318
943.933717	64.678263	69.919322
942.904790	74.147667	69.924327
943.017881	63.792749	69.929332
942.522565	72.880769	69.934337
941.426230	69.764159	69.939342
940.729826	68.487295	69.944346
940.092246	75.454870	69.949351
939.780743	72.114019	69.954356
938.419367	68.112336	69.959361
937.941673	70.992223	69.964366
937.743713	67.410953	69.969370
937.156551	73.670335	69.974375
935.945572	63.232810	69.979380
935.296714	69.957750	69.984385
934.982061	78.226968	69.989390
934.905942	61.827718	69.994394
933.252859	63.912208	69.999399
932.479497	63.951737	70.004404
931.989692	65.368559	70.009409
931.824320	66.997103	70.014414
931.237753	61.850257	70.019418
929.813152	72.533808	70.024423
929.484831	60.601218	70.029428
928.897872	62.265313	70.034433
928.160404	71.830263	70.039438
927.245963	69.864278	70.044442
926.333719	75.121988	70.049447
926.161618	67.111660	70.054452
925.700024	67.364929	70.059457
925.053711	70.306345	70.064462
924.762675	62.050018	70.069466
923.412446	70.529766	70.074471
923.030591	73.381789	70.079476
922.509828	67.183679	70.084481
921.620203	79.764339	70.089486
920.814396	65.810379	70.094490
920.081469	77.241729	70.099495
919.967349	65.106315	70.104500
919.274055	69.821401	70.109505
918.174488	73.120380	70.114510
917.864498	64.461792	70.119514
916.835579	74.830068	70.124519
916.383499	74.358001	70.129524
915.403659	63.707085	70.134529
914.418827	66.210365	70.139534
914.285580	65.701751	70.144538
913.873440	69.832775	70.149543
913.542618	66.089726	70.154548
912.276467	67.633256	70.159553
911.829706	69.666129	70.164558
911.286061	64.719038	70.169562
910.529617	72.173890	70.174567
910.097022	70.732048	70.179572
909.442254	68.612780	70.184577
908.421413	74.897031	70.189582
907.253896	71.534721	70.194586
906.524711	72.442439	70.199591
906.306815	65.653661	70.204596
905.776212	71.982894	70.209601
905.462139	77.612193	70.214606
904.459623	66.715730	70.219610
903.460519	66.781733	70.224615
903.036275	53.959248	70.229620
902.794389	72.367750	70.234625
902.431288	77.271567	70.239630
901.521440	63.644838	70.244634
900.480051	72.009212	70.249639
899.649677	61.367634	70.254644
898.676673	57.900258	70.259649
898.048370	71.563696	70.264654
897.717244	60.897857	70.269658
897.176384	66.077543	70.274663
897.023997	60.494177	70.279668
895.856180	57.732744	70.284673
894.741592	69.813039	70.289678
894.529719	63.226732	70.294682
893.971773	63.933735	70.299687
893.352182	62.568967	70.304692
892.196315	57.867555	70.309697
891.813560	62.213099	70.314702
891.568933	60.624652	70.319706
890.805549	74.416825	70.324711
890.023141	62.482396	70.329716
889.349798	65.713550	70.334721
888.631743	63.539706	70.339726
888.359225	57.721571	70.344730
887.076112	61.136505	70.349735
886.201890	58.159615	70.354740
885.727395	63.902752	70.359745
885.210226	68.592968	70.364750
885.264585	59.747091	70.369754
883.889181	64.796250	70.374759
883.448628	56.320880	70.379764
882.665005	63.649172	70.384769
881.536084	54.832352	70.389774
880.267782	58.837867	70.394778
879.680318	61.582268	70.399783
879.539685	56.817051	70.404788
879.239971	57.517651	70.409793
878.421049	61.334950	70.414798
877.729384	55.216097	70.419802
876.837148	59.166490	70.424807
876.370205	49.176719	70.429812
876.103431	60.109670	70.434817
875.561886	59.634504	70.439822
875.294904	47.327899	70.444826
874.001001	57.976471	70.449831
873.361626	48.290112	70.454836
873.242879	55.626121	70.459841
872.128522	57.093471	70.464846
871.226110	62.877908	70.469850
870.656830	69.121838	70.474855
870.308381	66.829247	70.479860
870.054067	60.759057	70.484865
868.555771	68.757769	70.489870
868.177280	56.202401	70.494874
867.320471	66.694680	70.499879
866.571226	65.462519	70.504884
865.477325	55.231912	70.509889
865.068038	66.417786	70.514894
864.896596	59.388234	70.519898
864.217872	59.179332	70.524903
863.794845	63.294747	70.529908
862.808068	52.566122	70.534913
861.777649	60.864101	70.539918
861.715268	56.572134	70.544922
861.028550	56.102731	70.549927
860.462745	57.763473	70.554932
859.492215	60.264497	70.559937
859.004236	52.485814	70.564942
858.891567	59.928090	70.569946
857.182766	56.074797	70.574951
856.751546	50.944251	70.579956
856.197122	55.842248	70.584961
855.941265	60.826765	70.589966
854.783946	53.842172	70.594970
853.779520	60.035513	70.599975
853.499936	53.873157	70.604980
853.274165	54.188252	70.609985
852.562724	60.871124	70.614990
851.611954	58.926722	70.619994
850.698993	70.361502	70.624999
850.573171	56.837095	70.630004
849.855328	56.506690	70.635009
848.586056	58.083863	70.640014
848.405402	59.465684	70.645018
847.613266	65.117459	70.650023
847.243870	65.521648	70.655028
846.220032	57.826682	70.660033
845.668935	55.888052	70.665038
844.949693	63.294414	70.670042
844.430597	65.556430	70.675047
843.434242	55.297694	70.680052
842.704400	63.907383	70.685057
842.008755	67.810728	70.690062
841.657497	56.249246	70.695066
841.362596	62.176691	70.700071
840.811191	60.115108	70.705076
840.100497	53.368516	70.710081
839.167272	64.633055	70.715086
838.757037	55.060042	70.720090
837.348961	65.690538	70.725095
836.894268	55.317200	70.730100
836.495804	63.244939	70.735105
835.853355	59.102075	70.740110
835.073924	64.203051	70.745114
833.913814	66.051439	70.750119
833.586210	65.780348	70.755124
833.139494	63.170668	70.760129
832.799220	63.507145	70.765134
831.958887	51.224002	70.770138
830.844576	71.715750	70.775143
830.428995	63.465075	70.780148
830.082954	60.776293	70.785153
828.891528	62.419932	70.790158
828.336625	55.818856	70.795162
827.577678	65.270545	70.800167
827.329295	62.728645	70.805172
826.797835	67.093137	70.810177
826.096253	63.382312	70.815182
825.179891	60.393230	70.820186
824.541686	67.870277	70.825191
823.965876	61.370299	70.830196
822.647535	60.816945	70.835201
821.823327	68.192714	70.840206
822.232369	67.831173	70.845210
821.240885	65.926379	70.850215
821.063860	55.046799	70.855220
820.048326	69.765364	70.860225
819.128142	77.586925	70.865230
818.644846	69.127831	70.870234
818.101619	62.868673	70.875239
817.372278	61.005730	70.880244
816.368765	66.227537	70.885249
815.880962	73.286408	70.890254
815.880115	65.639923	70.895258
814.359817	67.585079	70.900263
814.068399	65.225073	70.905268
813.737339	64.684875	70.910273
812.569027	68.698161	70.915278
812.022876	64.426433	70.920282
811.450931	70.118862	70.925287
811.121225	65.058895	70.930292
809.677429	62.699404	70.935297
808.765276	67.130809	70.940302
808.562151	62.364507	70.945306
808.063565	69.075010	70.950311
807.767347	60.376409	70.955316
807.049245	66.972044	70.960321
806.061267	59.301351	70.965326
805.711409	58.152289	70.970330
804.144738	70.430735	70.975335
803.335905	63.351267	70.980340
803.016646	66.655386	70.985345
802.822041	71.297421	70.990350
802.465428	69.242684	70.995354
801.740193	71.198479	71.000359
800.861735	66.785687	71.005364
799.871341	64.082789	71.010369
799.019469	69.589546	71.015374
798.711793	62.173258	71.020378
798.146009	69.146772	71.025383
797.581541	64.215643	71.030388
796.713034	60.873600	71.035393
796.271604	67.164997	71.040398
795.669693	64.458605	71.045402
794.643725	71.104832	71.050407
793.576708	68.094011	71.055412
793.380876	63.463745	71.060417
793.225009	72.004155	71.065422
792.892457	64.508248	71.070426
791.553950	66.462324	71.075431
790.931700	73.541025	71.080436
790.372888	68.139063	71.085441
789.159958	70.051074	71.090446
788.495685	54.705859	71.095450
787.910288	64.200891	71.100455
787.738515	60.919823	71.105460
787.261309	62.605901	71.110465
786.134069	66.677314	71.115470
785.485989	68.325939	71.120474
784.864476	73.709297	71.125479
784.593218	61.341882	71.130484
783.839347	65.322318	71.135489
782.531816	66.317411	71.140494
782.369816	61.248099	71.145498
781.624211	72.545868	71.150503
780.854187	75.626861	71.155508
780.028293	73.544333	71.160513
779.478249	67.934398	71.165518
779.348724	68.177406	71.170522
778.664618	68.707400	71.175527
777.410804	65.201199	71.180532
776.610271	61.889343	71.185537
776.179557	62.571386	71.190542
776.046602	62.441203	71.195546
774.909768	68.179412	71.200551
774.048906	64.001951	71.205556
773.536801	56.075744	71.210561
772.953968	71.072366	71.215566
772.910727	58.903622	71.220570
771.797915	71.644417	71.225575
770.977103	64.421789	71.230580
770.667095	65.590819	71.235585
769.567922	74.417022	71.240590
769.242604	66.577768	71.245594
768.416859	71.807562	71.250599
767.915044	64.426917	71.255604
766.512043	67.838918	71.260609
765.530225	72.956366	71.265614
765.803055	71.843793	71.270618
765.111093	71.370520	71.275623
764.754896	65.117870	71.280628
764.232541	66.580904	71.285633
763.035907	68.925572	71.290638
762.413844	70.339825	71.295642
761.600021	71.193250	71.300647
761.197254	61.190133	71.305652
760.514822	68.611155	71.310657
759.708740	71.380926	71.315662
759.370253	63.091186	71.320666
758.764340	69.170654	71.325671
757.821466	66.774022	71.330676
757.048410	68.456744	71.335681
756.449285	67.363143	71.340686
756.082487	61.724043	71.345690
754.929934	65.515647	71.350695
754.004967	66.374153	71.355700
753.973337	63.875024	71.360705
752.919870	69.921668	71.365710
752.949463	60.130417	71.370714
751.762259	66.296124	71.375719
751.191610	52.440437	71.380724
750.637064	58.163218	71.385729
749.968654	66.714261	71.390734
749.531119	51.843901	71.395738
748.340845	63.326006	71.400743
747.658762	61.643219	71.405748
747.563913	62.654993	71.410753
746.764175	63.977689	71.415758
745.607276	50.317845	71.420762
744.921584	61.557188	71.425767
744.652197	54.527480	71.430772
744.405469	57.138811	71.435777
743.305669	66.611669	71.440782
742.753433	56.496740	71.445786
741.890790	53.466024	71.450791
741.623393	54.577809	71.455796
740.747498	46.245912	71.460801
739.597417	58.251472	71.465806
739.481349	54.264529	71.470810
738.958550	55.306592	71.475815
737.960538	58.009153	71.480820
737.176759	58.767915	71.485825
736.289109	63.335788	71.490830
736.060162	55.749286	71.495834
735.278844	64.561158	71.500839
734.699005	59.162563	71.505844
734.267429	60.727844	71.510849
733.282499	68.432000	71.515854
733.120053	63.507843	71.520858
731.971082	68.355446	71.525863
731.449571	56.961450	71.530868
730.890905	61.615716	71.535873
730.349364	66.333490	71.540878
729.434827	60.928262	71.545882
728.221760	69.433565	71.550887
727.878482	54.899863	71.555892
727.587281	54.965189	71.560897
726.892394	61.074596	71.565902
725.993806	50.115959	71.570906
725.364083	57.817172	71.575911
725.026236	59.834309	71.580916
724.723027	57.668581	71.585921
723.359860	65.172764	71.590926
722.981023	57.474510	71.595930
722.412882	66.009593	71.600935
721.179226	64.316864	71.605940
720.255005	55.101688	71.610945
719.710171	59.919334	71.615950
719.228921	62.517545	71.620954
718.739582	68.704615	71.625959
718.208689	56.742837	71.630964
718.423470	59.231802	71.635969
717.009948	61.391825	71.640974
716.996006	58.114021	71.645978
715.376604	62.028859	71.650983
714.352103	51.877175	71.655988
714.005526	53.540887	71.660993
713.701843	57.085383	71.665998
713.456214	56.257207	71.671002
712.295797	63.216602	71.676007
711.488473	60.244896	71.681012
710.989003	63.869453	71.686017
710.056883	67.965023	71.691022
709.125196	60.887809	71.696026
708.407843	61.550848	71.701031
707.992318	64.307330	71.706036
707.943991	59.264083	71.711041
707.489561	63.389248	71.716046
706.881692	57.917854	71.721050
705.807127	64.899851	71.726055
705.227917	63.689552	71.731060
704.220134	60.517955	71.736065
703.144277	65.155231	71.741070
702.757515	60.263643	71.746074
702.205307	59.022237	71.751079
701.737736	65.133302	71.756084
701.159472	64.993605	71.761089
700.372453	63.549890	71.766094
700.009377	61.166618	71.771098
699.234439	61.241163	71.776103
698.167124	59.804235	71.781108
697.342405	54.217564	71.786113
696.448584	67.286208	71.791118
696.204812	57.500645	71.796122
695.785195	63.416417	71.801127
695.391491	64.122542	71.806132
694.973205	63.694021	71.811137
694.049465	66.398966	71.816142
693.443451	67.493712	71.821146
692.078228	60.009299	71.826151
691.190273	65.479253	71.831156
690.954012	62.899170	71.836161
690.171843	68.434281	71.841166
690.171314	60.314673	71.846170
689.481700	68.004934	71.851175
688.585050	60.054826	71.856180
688.091546	63.432432	71.861185
687.173191	58.668073	71.866190
686.255561	58.385299	71.871194
685.453260	61.655958	71.876199
684.845543	66.627127	71.881204
684.726598	55.927559	71.886209
683.840724	70.696474	71.891214
683.257785	62.898263	71.896218
682.387692	59.960217	71.901223
681.855362	62.153407	71.906228
681.500881	61.678459	71.911233
680.322900	69.041211	71.916238
679.830427	56.043578	71.921242
679.290115	65.394250	71.926247
678.893643	60.461635	71.931252
678.268521	57.183385	71.936257
677.284517	54.804375	71.941262
676.912461	54.978777	71.946266
675.906412	53.826993	71.951271
674.614132	61.744108	71.956276
674.358200	51.872181	71.961281
673.729304	64.867102	71.966286
673.637507	56.998573	71.971290
673.087017	57.046847	71.976295
671.918870	52.711781	71.981300
671.345949	51.475259	71.986305
670.689568	62.186398	71.991310
670.226624	62.066190	71.996314
669.107494	54.063214	72.001319
668.404795	52.028920	72.006324
668.062990	50.350319	72.011329
667.520796	63.859711	72.016334
666.714055	57.929566	72.021338
665.841991	61.233417	72.026343
665.615774	58.975013	72.031348
665.002521	58.230616	72.036353
663.740248	61.068326	72.041358
663.173933	63.490859	72.046362
662.589221	58.512531	72.051367
662.403918	58.641426	72.056372
661.587500	46.994802	72.061377
660.185189	60.287924	72.066382
660.005390	57.653122	72.071386
659.520140	57.344081	72.076391
658.934938	61.797583	72.081396
658.229636	53.883253	72.086401
657.064682	60.994777	72.091406
656.885634	45.468281	72.096410
656.301214	54.942667	72.101415
655.343509	61.847725	72.106420
654.421809	57.534921	72.111425
654.069785	71.394083	72.116430
653.859632	62.774848	72.121434
652.917276	57.590126	72.126439
651.579061	61.165334	72.131444
651.349533	57.153889	72.136449
650.862505	57.728226	72.141454
650.112584	59.307945	72.146458
649.588092	57.240546	72.151463
648.940177	60.850905	72.156468
648.282943	55.068848	72.161473
647.362955	56.278259	72.166478
647.257491	53.056035	72.171482
646.291364	61.059994	72.176487
645.416879	58.326089	72.181492
645.290053	55.291769	72.186497
643.866608	64.344692	72.191502
643.287340	56.812417	72.196506
642.597320	59.284616	72.201511
642.344755	64.826861	72.206516
642.257449	55.757561	72.211521
640.707937	63.411305	72.216526
640.244221	49.762561	72.221530
639.474748	52.588034	72.226535
639.223937	58.576275	72.231540
638.237456	57.281042	72.236545
637.185829	64.973769	72.241550
636.932805	58.849798	72.246554
636.684067	59.228494	72.251559
635.694746	61.026116	72.256564
635.240651	56.960550	72.261569
634.051792	67.171449	72.266574
634.026899	59.461003	72.271578
632.996058	56.747272	72.276583
632.267121	59.476407	72.281588
632.126623	51.804876	72.286593
631.177680	59.304631	72.291598
630.153592	51.343311	72.296602
629.647699	56.482775	72.301607
629.056673	62.526776	72.306612
628.732190	50.841244	72.311617
627.536834	63.555798	72.316622
626.847555	55.743006	72.321626
626.399861	62.443847	72.326631
625.862309	61.119700	72.331636
624.943607	56.897895	72.336641
623.857947	61.240294	72.341646
623.601326	55.034898	72.346650
623.070351	57.376116	72.351655
622.607542	56.677155	72.356660
621.847852	55.967128	72.361665
620.875937	68.061055	72.366670
620.574629	55.323157	72.371674
620.303597	61.063884	72.376679
619.197889	72.324415	72.381684
618.618677	58.061707	72.386689
617.944528	71.942208	72.391694
616.974660	68.602183	72.396698
615.938138	61.079661	72.401703
615.358789	70.556409	72.406708
615.062294	70.345047	72.411713
614.618048	70.639765	72.416718
614.183791	63.847646	72.421722
613.346450	62.068200	72.426727
612.257924	61.610821	72.431732
611.810748	58.316865	72.436737
611.212389	65.070089	72.441742
610.706492	63.515400	72.446746
609.417788	67.560562	72.451751
609.014275	61.230327	72.456756
608.705074	56.780569	72.461761
608.176361	61.969404	72.466766
607.327644	62.014727	72.471770
606.531031	61.077197	72.476775
605.904499	59.819266	72.481780
605.582793	57.621810	72.486785
604.445536	67.370339	72.491790
603.933881	49.212854	72.496794
603.173671	61.202099	72.501799
602.502766	61.621227	72.506804
602.243391	51.607938	72.511809
600.784970	56.178447	72.516814
600.328015	59.715825	72.521818
600.051670	53.150877	72.526823
599.417265	52.111821	72.531828
599.058234	54.525006	72.536833
597.482342	59.581005	72.541838
597.359956	55.456309	72.546842
596.923215	61.789556	72.551847
596.099815	60.700177	72.556852
595.203103	48.826674	72.561857
594.463298	63.378370	72.566862
594.027346	59.251576	72.571866
593.501910	59.560805	72.576871
592.674330	63.598762	72.581876
591.718718	55.014695	72.586881
591.139986	59.380446	72.591886
591.074088	53.806998	72.596890
590.400735	56.167745	72.601895
589.341940	56.099879	72.606900
588.834430	50.926352	72.611905
588.318892	58.538439	72.616910
587.716186	57.185255	72.621914
586.917814	52.281983	72.626919
585.744368	57.710704	72.631924
585.562166	53.918812	72.636929
584.305363	61.947010	72.641934
583.598511	60.061635	72.646938
582.993710	57.584421	72.651943
582.359551	60.623324	72.656948
582.491418	57.276570	72.661953
582.030466	65.725213	72.666958
580.785859	57.180873	72.671962
580.207342	59.435055	72.676967
579.455975	60.079893	72.681972
579.186689	59.585083	72.686977
577.932737	59.671307	72.691982
577.641722	57.464236	72.696986
576.868108	70.808651	72.701991
576.141920	62.402511	72.706996
575.426098	58.708229	72.712001
574.629896	64.234565	72.717006
574.188067	66.015969	72.722010
573.819030	60.184876	72.727015
572.591904	62.379944	72.732020
571.806032	63.411903	72.737025
570.778903	64.446020	72.742030
570.585582	59.593034	72.747034
570.415337	61.219217	72.752039
569.799995	64.904831	72.757044
570.001509	61.162207	72.762049
568.819095	66.792639	72.767054
567.831877	68.003326	72.772058
566.380345	61.453679	72.777063
565.581864	63.090044	72.782068
565.618966	67.233130	72.787073
564.662732	64.209501	72.792078
564.655837	65.123692	72.797082
563.969403	65.854386	72.802087
562.923096	70.677822	72.807092
562.845752	70.098823	72.812097
561.576998	66.246612	72.817102
560.946755	61.027984	72.822106
559.963895	53.247788	72.827111
559.323169	61.450676	72.832116
559.341515	64.322573	72.837121
558.741023	62.281493	72.842126
557.743786	66.414293	72.847130
556.908938	60.146469	72.852135
556.281117	66.133267	72.857140
555.920766	58.348530	72.862145
554.587043	65.212590	72.867150
553.794142	56.023882	72.872154
554.033255	65.162106	72.877159
553.436288	64.620146	72.882164
552.764519	63.006735	72.887169
551.387592	62.402934	72.892174
551.071373	59.509177	72.897178
550.562733	64.921904	72.902183
549.661945	66.484684	72.907188
548.864473	59.318356	72.912193
548.250898	59.856099	72.917198
547.948482	56.468136	72.922202
547.636576	61.893680	72.927207
546.139956	64.000802	72.932212
545.684179	64.172789	72.937217
545.391223	68.723264	72.942222
544.755001	53.507730	72.947226
543.708475	53.319658	72.952231
543.050207	62.861020	72.957236
542.536823	56.955157	72.962241
541.726164	62.412841	72.967246
541.537326	58.871168	72.972250
540.900880	63.192506	72.977255
540.117814	61.486442	72.982260
539.181912	51.426392	72.987265
537.783853	58.313320	72.992270
537.700700	57.900828	72.997274
537.284963	56.812763	73.002279
536.587048	59.070204	73.007284
536.314298	50.967170	73.012289
534.901079	57.369237	73.017294
534.431489	53.176854	73.022298
534.343005	52.804635	73.027303
533.276762	59.115162	73.032308
532.391961	51.467593	73.037313
531.394122	50.620490	73.042318
530.975851	47.217871	73.047322
531.017462	51.934242	73.052327
530.231925	54.677149	73.057332
529.395718	60.616721	73.062337
528.843977	56.639274	73.067342
528.371059	53.191743	73.072346
527.234637	55.224149	73.077351
526.187458	66.740309	73.082356
526.018561	58.368417	73.087361
525.387319	57.387224	73.092366
524.860183	52.634732	73.097370
524.040124	53.325222	73.102375
522.973663	60.088372	73.107380
522.659819	45.658862	73.112385
522.233691	57.911865	73.117390
521.280608	57.995921	73.122394
520.551359	55.915439	73.127399
520.135010	60.782036	73.132404
519.945120	59.497148	73.137409
518.297490	62.103004	73.142414
517.865873	51.159963	73.147418
517.244339	52.220952	73.152423
516.879548	61.832260	73.157428
516.338222	56.372402	73.162433
515.495615	56.063548	73.167438
514.407431	48.852087	73.172442
513.967540	57.265837	73.177447
513.661244	53.689263	73.182452
513.061885	50.239802	73.187457
511.914999	54.718152	73.192462
511.777449	54.520906	73.197466
511.997412	54.847025	73.202471
511.162184	58.236519	73.207476
510.408308	57.694334	73.212481
509.263599	55.199072	73.217486
508.128531	45.530314	73.222490
507.220180	48.466256	73.227495
506.439610	56.254614	73.232500
505.383538	45.628680	73.237505
504.100517	61.731909	73.242510
504.195332	49.498643	73.247514
503.552546	55.035247	73.252519
503.293382	56.741830	73.257524
502.991508	50.829093	73.262529
502.565471	62.418191	73.267534
501.534298	51.822981	73.272538
500.829022	55.000964	73.277543
499.979150	62.754636	73.282548
499.957666	51.159638	73.287553
499.032758	53.300286	73.292558
498.208842	43.380116	73.297562
497.736898	54.691094	73.302567
497.192331	48.075857	73.307572
496.843811	49.804560	73.312577
495.655383	54.377844	73.317582
495.006586	47.446477	73.322586
494.267731	53.335854	73.327591
492.968579	53.855098	73.332596
492.781437	49.083143	73.337601
491.746939	47.349345	73.342606
491.708242	54.418698	73.347610
491.475188	57.396874	73.352615
490.272527	55.171050	73.357620
489.483495	49.346966	73.362625
488.930675	55.905294	73.367630
488.775544	45.910119	73.372634
487.709258	55.297293	73.377639
486.631462	56.173936	73.382644
486.478229	53.815617	73.387649
485.933451	53.769983	73.392654
484.922169	53.407587	73.397658
484.256658	54.570207	73.402663
483.452048	61.894049	73.407668
483.358626	46.185220	73.412673
482.570142	45.773137	73.417678
481.425750	56.751282	73.422682
480.753656	53.698191	73.427687
480.117801	56.316342	73.432692
479.796894	47.796794	73.437697
479.322134	54.199184	73.442702
478.538273	46.817834	73.447706
477.574830	47.610030	73.452711
477.070882	56.216914	73.457716
476.869110	53.866329	73.462721
475.697983	59.685810	73.467726
475.124999	56.703663	73.472730
474.695937	52.608916	73.477735
474.127755	52.245316	73.482740
473.223492	54.893614	73.487745
472.235675	62.386997	73.492750
471.618534	57.726127	73.497754
471.285376	51.730071	73.502759
470.207609	55.850498	73.507764
469.448558	47.424413	73.512769
468.817931	56.417332	73.517774
468.297634	48.434177	73.522778
468.248799	52.332326	73.527783
467.362268	51.658326	73.532788
466.473884	51.946560	73.537793
465.712065	56.399850	73.542798
465.181103	50.996704	73.547802
465.180579	45.974248	73.552807
463.727020	54.664619	73.557812
463.371062	47.399603	73.562817
462.723734	60.107320	73.567822
462.009549	63.491737	73.572826
461.235264	54.732188	73.577831
460.175273	57.995081	73.582836
460.266435	54.963894	73.587841
459.344874	54.295478	73.592846
458.477431	51.363405	73.597850
457.917125	48.440745	73.602855
457.275710	57.172035	73.607860
456.916613	52.834334	73.612865
455.861787	54.503688	73.617870
455.148215	50.832744	73.622874
454.810171	47.977174	73.627879
454.282736	52.746358	73.632884
453.269368	50.957170	73.637889
452.514991	49.189796	73.642894
451.734374	50.725576	73.647898
451.662236	40.501147	73.652903
450.858555	59.685065	73.657908
450.182423	54.945293	73.662913
449.499674	60.854128	73.667918
448.998357	52.036901	73.672922
448.076131	56.816950	73.677927
447.101649	58.594932	73.682932
446.767459	47.458198	73.687937
446.434325	52.026114	73.692942
445.450660	52.903546	73.697946
444.744484	54.178310	73.702951
443.797786	63.948571	73.707956
443.652582	47.027442	73.712961
442.514801	57.752235	73.717966
441.789649	50.106078	73.722970
441.507612	45.245173	73.727975
440.808376	45.921169	73.732980
440.757581	44.152082	73.737985
439.282183	49.868667	73.742990
438.313875	49.185631	73.747994
438.225470	53.733478	73.752999
437.654859	52.338950	73.758004
437.087867	44.229206	73.763009
435.920899	51.062014	73.768014
435.385955	43.838140	73.773018
435.091156	48.447256	73.778023
433.708102	52.132217	73.783028
433.173796	46.426840	73.788033
432.712439	50.685606	73.793038
432.187694	52.743593	73.798042
432.086403	37.275735	73.803047
430.973559	44.964083	73.808052
430.200610	44.954818	73.813057
429.819235	54.090952	73.818062
429.142650	45.872517	73.823066
428.092151	48.108893	73.828071
427.403738	49.792415	73.833076
426.885781	47.156328	73.838081
426.377042	47.240582	73.843086
425.326032	44.105962	73.848090
424.671609	43.120605	73.853095
423.648127	53.284720	73.858100
423.807551	37.612895	73.863105
423.108965	51.653412	73.868110
422.342655	47.831610	73.873114
421.697562	48.178865	73.878119
420.721366	47.279474	73.883124
420.599331	40.396665	73.888129
419.749179	54.890265	73.893134
418.883040	36.157000	73.898138
418.271544	44.317398	73.903143
417.580910	52.529835	73.908148
417.292197	47.975924	73.913153
416.243193	53.028494	73.918158
415.650320	48.436317	73.923162
415.137157	51.580555	73.928167
414.624885	51.523449	73.933172
413.740698	56.478796	73.938177
412.631607	55.617931	73.943182
412.723008	47.234548	73.948186
411.933322	48.029044	73.953191
410.551349	51.671267	73.958196
410.184103	51.218893	73.963201
409.682651	47.771207	73.968206
409.294986	49.843624	73.973210
408.784346	45.493812	73.978215
407.555882	48.878187	73.983220
406.984934	46.955443	73.988225
406.009885	44.478930	73.993230
406.038287	48.760582	73.998234
405.098047	46.680643	74.003239
404.386575	48.883506	74.008244
403.882014	47.707119	74.013249
403.515809	46.942345	74.018254
402.481193	49.505783	74.023258
401.890197	45.867364	74.028263
401.283002	50.715497	74.033268
400.751973	45.181496	74.038273
399.409464	47.268874	74.043278
399.071893	50.085514	74.048282
398.862395	47.881249	74.053287
398.075124	56.258900	74.058292
396.895072	46.975840	74.063297
396.379551	43.916751	74.068302
395.542245	44.116447	74.073306
395.397801	40.954072	74.078311
394.425948	52.292677	74.083316
393.511406	49.699294	74.088321
393.160848	56.154443	74.093326
392.617169	55.009523	74.098330
392.517493	45.794001	74.103335
391.195441	57.776617	74.108340
390.410908	49.718897	74.113345
389.856078	49.427306	74.118350
389.567009	50.444807	74.123354
388.867239	42.452432	74.128359
387.813520	53.129153	74.133364
387.463863	45.886804	74.138369
386.600619	49.645072	74.143374
385.629298	50.389673	74.148378
385.171471	47.690398	74.153383
384.516456	53.456053	74.158388
384.340171	45.435451	74.163393
383.649172	50.137670	74.168398
382.415048	46.384125	74.173402
381.946374	47.781907	74.178407
381.221848	45.241827	74.183412
380.741527	45.763106	74.188417
379.556011	52.401774	74.193422
378.971468	50.255701	74.198426
378.928068	48.436552	74.203431
378.342024	54.744726	74.208436
378.059803	42.953183	74.213441
376.760276	42.020181	74.218446
376.156353	44.551263	74.223450
375.553983	48.438271	74.228455
374.153380	48.751395	74.233460
373.736680	44.325121	74.238465
372.868743	51.619654	74.243470
372.740641	44.733084	74.248474
372.285152	43.496845	74.253479
371.665459	53.894671	74.258484
370.871527	51.603772	74.263489
370.377608	49.315527	74.268494
369.737319	47.698732	74.273498
368.612806	42.341320	74.278503
367.579858	53.899403	74.283508
367.521559	41.308937	74.288513
366.929905	46.310716	74.293518
366.337441	50.073147	74.298522
365.544322	36.716699	74.303527
364.790065	54.653266	74.308532
364.324868	42.230147	74.313537
363.273668	39.494553	74.318542
362.202820	39.370358	74.323546
361.980553	38.071723	74.328551
361.290427	47.799530	74.333556
361.562127	37.916133	74.338561
360.828612	40.515178	74.343566
360.166763	38.285238	74.348570
359.323909	34.879359	74.353575
357.956697	36.729422	74.358580
357.345075	42.406161	74.363585
356.789487	50.879360	74.368590
356.306014	43.957965	74.373594
355.285654	47.698703	74.378599
354.265164	55.353444	74.383604
353.974413	50.389862	74.388609
353.548053	56.987981	74.393614
352.979225	50.963277	74.398618
352.800209	43.439854	74.403623
351.614628	56.722215	74.408628
351.221763	38.517531	74.413633
350.612344	43.372333	74.418638
349.629686	53.041111	74.423642
348.960909	44.102374	74.428647
348.304983	47.807113	74.433652
348.085821	44.309723	74.438657
346.886107	45.721516	74.443662
345.920113	47.472951	74.448666
345.550261	51.236177	74.453671
345.128074	47.846836	74.458676
344.529407	50.038045	74.463681
343.577406	56.546474	74.468686
342.850250	54.598179	74.473690
342.651849	50.532932	74.478695
341.622125	53.797356	74.483700
340.850514	45.124168	74.488705
340.093489	43.995916	74.493710
339.965620	49.154019	74.498714
339.677863	50.814710	74.503719
338.499222	47.580623	74.508724
337.673578	50.410401	74.513729
337.292342	47.993818	74.518734
336.520580	56.875211	74.523738
335.031568	47.270845	74.528743
334.375006	59.450195	74.533748
334.378433	55.855827	74.538753
333.753000	55.452499	74.543758
333.418561	47.595881	74.548762
332.996581	40.246803	74.553767
331.913960	47.208132	74.558772
331.455544	41.973236	74.563777
330.449459	46.596375	74.568782
329.336259	50.526961	74.573786
328.909125	41.127100	74.578791
328.312442	52.768626	74.583796
328.034812	42.827698	74.588801
327.656320	49.877079	74.593806
326.584487	50.435873	74.598810
326.026093	49.767974	74.603815
325.071398	51.911853	74.608820
324.481307	49.886526	74.613825
323.610895	41.650138	74.618830
322.887512	50.200546	74.623834
322.774926	42.105149	74.628839
321.914121	48.964897	74.633844
321.336737	47.464245	74.638849
320.437353	39.938949	74.643854
319.813640	48.139158	74.648858
319.434284	42.950011	74.653863
318.445496	49.901122	74.658868
317.586461	46.712299	74.663873
317.130625	47.519846	74.668878
316.680700	48.015793	74.673882
316.644810	44.727314	74.678887
315.210826	54.561077	74.683892
314.578620	47.267584	74.688897
314.158061	45.264125	74.693902
313.575170	47.217861	74.698906
312.903425	49.222030	74.703911
312.018070	51.394285	74.708916
311.421656	41.750174	74.713921
310.211223	42.610185	74.718926
309.300508	41.255705	74.723930
309.032165	43.231847	74.728935
308.587857	51.308849	74.733940
308.064211	43.786746	74.738945
308.050708	47.324446	74.743950
306.961690	42.057602	74.748954
306.320154	39.081699	74.753959
305.373103	48.374230	74.758964
304.294190	48.817468	74.763969
303.573519	46.007141	74.768974
302.861404	54.929496	74.773978
303.215317	42.533534	74.778983
302.144486	46.807459	74.783988
301.368070	46.992750	74.788993
300.643016	42.204059	74.793998
299.848312	50.358988	74.799002
299.621303	51.464378	74.804007
299.158739	50.211934	74.809012
298.089524	45.913334	74.814017
297.427632	41.746931	74.819022
296.880972	45.703923	74.824026
296.525673	44.902735	74.829031
295.292055	45.293366	74.834036
295.175263	48.546332	74.839041
294.225606	52.028245	74.844046
293.062171	51.046787	74.849050
292.405394	45.340472	74.854055
291.792047	41.732455	74.859060
291.891465	51.947860	74.864065
291.268926	46.223472	74.869070
290.071216	46.597343	74.874074
289.311432	43.909950	74.879079
288.569904	53.070382	74.884084
288.641531	49.837305	74.889089
287.963316	39.611735	74.894094
286.639215	42.661326	74.899098
286.148430	36.092778	74.904103
285.576265	42.963296	74.909108
285.210887	41.432015	74.914113
284.222578	44.330314	74.919118
283.510233	53.755753	74.924122
283.133432	43.617754	74.929127
282.093372	43.479225	74.934132
281.044756	42.738090	74.939137
280.727735	49.427594	74.944142
280.359843	56.661372	74.949146
280.284468	49.025244	74.954151
278.798379	51.982391	74.959156
278.296940	50.490144	74.964161
277.719337	49.604547	74.969166
277.156682	45.822874	74.974170
276.400524	50.093960	74.979175
275.383651	53.168704	74.984180
274.958615	49.492827	74.989185
274.416281	39.627223	74.994190
273.532925	44.090470	74.999194
273.085253	45.096995	75.004199
272.230396	56.998879	75.009204
271.973013	43.714767	75.014209
271.237455	48.909813	75.019214
270.247525	58.124040	75.024218
269.881050	48.441709	75.029223
269.304387	44.952430	75.034228
268.425396	47.789155	75.039233
267.743503	45.759554	75.044238
266.864073	48.042842	75.049242
266.520691	46.586905	75.054247
265.738229	51.306885	75.059252
264.935648	48.254162	75.064257
264.507215	47.308520	75.069262
263.644043	45.971709	75.074266
263.356303	39.213105	75.079271
262.302101	54.562424	75.084276
261.781603	48.716123	75.089281
261.515658	42.264702	75.094286
260.289665	47.632544	75.099290
259.776017	52.401139	75.104295
258.827844	52.777825	75.109300
258.291213	44.243832	75.114305
257.955509	47.230498	75.119310
257.320638	60.429838	75.124314
256.374161	48.389396	75.129319
255.550190	49.446447	75.134324
255.404282	51.201229	75.139329
255.007363	48.216307	75.144334
253.732896	54.303084	75.149338
252.978126	49.265256	75.154343
252.128634	53.231107	75.159348
251.897475	60.745865	75.164353
251.488377	56.483982	75.169358
250.398745	65.182682	75.174362
250.158891	46.384356	75.179367
249.503697	49.704226	75.184372
248.660153	49.627424	75.189377
247.554042	47.539298	75.194382
247.129202	46.170465	75.199386
246.674566	45.519161	75.204391
246.168571	54.813942	75.209396
245.159310	50.401732	75.214401
244.256261	47.970578	75.219406
243.424019	46.862232	75.224410
243.743863	43.897093	75.229415
242.796671	56.532788	75.234420
241.643749	47.699653	75.239425
241.380416	49.692349	75.244430
241.141235	50.878531	75.249434
240.208379	41.821086	75.254439
238.962529	52.888023	75.259444
238.915825	40.101767	75.264449
238.346844	46.153353	75.269454
237.169834	47.960546	75.274458
236.695218	36.912492	75.279463
235.577208	45.599940	75.284468
235.542630	39.122680	75.289473
234.998991	43.817209	75.294478
234.040517	52.662155	75.299482
233.426876	44.968341	75.304487
232.614691	54.293012	75.309492
232.162713	43.520465	75.314497
231.105610	45.122465	75.319502
230.318589	52.125018	75.324506
230.048417	49.706518	75.329511
229.454399	49.326594	75.334516
229.341826	46.271116	75.339521
228.478398	40.730231	75.344526
227.727512	52.232349	75.349530
227.017947	46.789935	75.354535
225.871709	57.648614	75.359540
225.237296	56.806778	75.364545
224.658733	51.551635	75.369550
224.150223	52.441712	75.374554
223.676279	44.146893	75.379559
222.276090	49.922567	75.384564
221.602792	46.330436	75.389569
221.107769	53.947180	75.394574
220.905390	48.781877	75.399578
220.711789	38.953735	75.404583
219.666803	49.477726	75.409588
218.951145	44.693872	75.414593
218.422668	48.725249	75.419598
217.504015	51.702355	75.424602
216.681029	41.755356	75.429607
216.027986	53.167762	75.434612
215.886751	51.607065	75.439617
215.486743	44.844289	75.444622
213.935151	50.661451	75.449626
213.390545	39.679753	75.454631
213.118522	58.622820	75.459636
212.212364	50.125673	75.464641
211.365642	44.113778	75.469646
210.305564	55.406576	75.474650
210.175725	45.224493	75.479655
209.502763	52.319253	75.484660
209.323897	55.970046	75.489665
208.763447	48.050141	75.494670
207.597261	59.757249	75.499674
207.224058	45.728375	75.504679
206.186278	56.595000	75.509684
205.173771	53.856462	75.514689
204.704856	51.616306	75.519694
203.936685	53.730492	75.524698
203.994883	43.638280	75.529703
203.389506	54.475390	75.534708
202.460067	46.808279	75.539713
201.715841	52.140342	75.544718
201.196301	56.304340	75.549722
200.295871	54.052557	75.554727
199.086300	53.885895	75.559732
198.466521	55.736729	75.564737
198.221930	47.963588	75.569742
197.804025	59.762710	75.574746
197.842777	47.055871	75.579751
196.718811	56.617915	75.584756
195.684357	52.698596	75.589761
195.641364	56.523268	75.594766
193.838915	51.720303	75.599770
193.298915	46.220905	75.604775
192.963145	49.552939	75.609780
192.541752	46.922013	75.614785
192.251338	48.149483	75.619790
190.995065	55.941217	75.624794
190.427446	40.495716	75.629799
189.871994	52.261570	75.634804
189.310618	49.569384	75.639809
188.555481	46.871822	75.644814
187.617910	52.915954	75.649818
187.397000	45.066501	75.654823
186.713401	48.712610	75.659828
185.417124	51.817743	75.664833
184.768084	48.757915	75.669838
184.206730	54.697911	75.674842
184.106298	44.408643	75.679847
183.456413	46.338396	75.684852
182.316300	46.009282	75.689857
181.902524	52.859298	75.694862
181.117794	49.423716	75.699866
180.931276	47.455507	75.704871
179.894414	53.535972	75.709876
179.350710	46.334070	75.714881
178.936907	42.136034	75.719886
177.632045	53.428445	75.724890
176.848425	40.948926	75.729895
176.466471	50.178203	75.734900
175.920011	42.240311	75.739905
175.607749	45.787793	75.744910
174.604825	53.548601	75.749914
174.086361	45.137892	75.754919
173.384148	38.853818	75.759924
172.940519	45.341164	75.764929
171.825652	47.597368	75.769934
170.946574	49.063777	75.774938
170.789789	31.668343	75.779943
170.104140	42.248591	75.784948
169.488761	48.734938	75.789953
168.624345	44.042629	75.794958
167.982341	50.178410	75.799962
167.645305	40.723228	75.804967
166.271301	58.274514	75.809972
165.655231	48.567353	75.814977
165.205436	49.634159	75.819982
164.541393	53.420659	75.824986
164.591987	37.559635	75.829991
163.468437	56.778814	75.834996
162.860106	52.632296	75.840001
162.662770	41.193124	75.845006
161.082313	47.270382	75.850010
160.584379	42.366678	75.855015
159.862292	47.802452	75.860020
159.435191	51.513326	75.865025
159.218515	45.952923	75.870030
157.773557	47.812337	75.875034
157.444096	38.018486	75.880039
156.711367	42.339481	75.885044
156.380629	40.651312	75.890049
155.215870	43.483177	75.895054
154.559625	47.861364	75.900058
154.536634	42.363119	75.905063
153.582309	47.020646	75.910068
152.531175	47.913680	75.915073
152.038237	33.022417	75.920078
151.378941	51.913680	75.925082
151.234760	43.823343	75.930087
149.966593	44.317326	75.935092
149.049368	53.237721	75.940097
148.678226	51.136527	75.945102
148.354161	56.633420	75.950106
148.025377	50.783389	75.955111
146.728753	54.978263	75.960116
145.831647	51.945385	75.965121
145.545019	48.823051	75.970126
145.179567	60.312617	75.975130
144.444089	43.003143	75.980135
143.358767	50.179437	75.985140
142.788516	40.266288	75.990145
142.437282	52.422204	75.995150
141.708577	50.769108	76.000154
140.929441	34.281887	76.005159
140.013357	42.799977	76.010164
139.802353	49.657086	76.015169
139.422114	40.416956	76.020174
137.989106	50.387838	76.025178
137.812254	37.564007	76.030183
137.044643	46.809048	76.035188
136.195716	53.491915	76.040193
135.594276	47.724788	76.045198
134.594150	50.462603	76.050202
134.543377	40.208004	76.055207
133.965294	45.918863	76.060212
132.939371	42.138563	76.065217
132.481878	45.171470	76.070222
131.516760	51.622132	76.075226
130.995852	43.470445	76.080231
129.781282	54.291166	76.085236
129.031470	46.500830	76.090241
128.667564	45.850850	76.095246
128.213194	54.036706	76.100250
128.257396	39.214334	76.105255
127.387666	49.142708	76.110260
126.575571	50.664683	76.115265
125.987165	41.243287	76.120270
125.287064	48.172079	76.125274
124.454596	42.358219	76.130279
123.640432	50.741795	76.135284
122.960542	57.889719	76.140289
122.812630	46.868444	76.145294
121.406554	50.823741	76.150298
120.875421	44.663788	76.155303
119.992077	50.633062	76.160308
119.617976	55.603352	76.165313
119.554573	43.535707	76.170318
118.212714	51.342695	76.175322
117.440046	36.362008	76.180327
116.755643	46.697643	76.185332
116.707191	34.170309	76.190337
116.173188	38.552663	76.195342
115.173716	47.916684	76.200346
114.612361	44.434468	76.205351
113.935217	42.558696	76.210356
113.395992	46.240147	76.215361
112.630841	42.104461	76.220366
111.677992	44.975092	76.225370
111.598404	46.340838	76.230375
110.387387	47.111153	76.235380
109.839539	44.153483	76.240385
109.323098	46.623365	76.245390
108.671186	48.474613	76.250394
107.788223	40.426403	76.255399
106.756926	53.723664	76.260404
106.297292	49.040944	76.265409
106.282295	47.471164	76.270414
105.440760	48.179408	76.275418
104.958296	41.109689	76.280423
104.143431	45.801762	76.285428
103.373621	47.572465	76.290433
102.479856	48.547657	76.295438
101.639126	56.702091	76.300442
101.008185	39.163086	76.305447
100.308556	46.806161	76.310452
100.035439	49.248281	76.315457
99.947609	40.923464	76.320462
98.776197	45.948362	76.325466
98.192844	46.315817	76.330471
97.332400	49.863995	76.335476
96.445289	44.517750	76.340481
95.692988	50.644327	76.345486
95.064748	45.081758	76.350490
94.563929	46.156714	76.355495
94.141162	51.008610	76.360500
93.636445	53.065045	76.365505
92.943216	37.510310	76.370510
91.992113	49.041225	76.375514
91.534036	37.145339	76.380519
90.414213	47.936768	76.385524
90.118622	38.851885	76.390529
89.806241	41.650347	76.395534
88.839077	45.500972	76.400538
87.932012	37.191690	76.405543
87.278076	48.430790	76.410548
86.832884	47.852126	76.415553
86.414394	51.192633	76.420558
85.264349	47.441610	76.425562
84.736789	39.784583	76.430567
84.042372	43.356749	76.435572
83.557439	50.006811	76.440577
82.675816	43.879111	76.445582
81.601349	43.992157	76.450586
81.273916	40.043717	76.455591
81.049242	46.797351	76.460596
80.496656	48.735266	76.465601
79.539942	44.251676	76.470606
78.572138	46.719431	76.475610
78.363489	46.454703	76.480615
77.636889	50.770012	76.485620
76.606621	51.765406	76.490625
75.695053	35.614725	76.495630
75.039246	46.081423	76.500634
75.058505	40.682101	76.505639
74.337938	49.441842	76.510644
73.623339	46.698430	76.515649
72.712821	41.314929	76.520654
72.183522	44.996381	76.525658
71.765609	51.227329	76.530663
71.256636	41.372240	76.535668
70.220596	43.792533	76.540673
69.837161	38.466898	76.545678
69.083299	50.880988	76.550682
68.017318	43.232564	76.555687
67.275819	46.790166	76.560692
66.762983	45.279285	76.565697
66.648391	41.796792	76.570702
66.008208	50.840180	76.575706
64.887113	47.858829	76.580711
64.181316	47.878392	76.585716
63.692790	46.524482	76.590721
63.102499	47.777715	76.595726
61.645300	47.570190	76.600730
61.506958	40.644296	76.605735
60.919848	39.556844	76.610740
60.344476	41.638744	76.615745
60.228937	39.599303	76.620750
58.833167	40.025375	76.625754
58.273699	36.509760	76.630759
57.738755	52.526937	76.635764
57.276827	44.181364	76.640769
56.443598	38.933776	76.645774
55.452294	43.989891	76.650778
55.210360	41.221563	76.655783
54.915959	44.010853	76.660788
53.510087	37.645085	76.665793
53.134912	43.290478	76.670798
52.282251	41.646143	76.675802
51.749660	39.348370	76.680807
50.794922	46.969066	76.685812
50.221263	50.219209	76.690817
49.869004	47.034818	76.695822
49.330516	46.291270	76.700826
48.308771	42.097185	76.705831
47.634964	40.604098	76.710836
47.074256	51.361562	76.715841
46.885261	47.269622	76.720846
46.011201	58.394034	76.725850
45.058703	45.432154	76.730855
44.698255	37.425215	76.735860
43.858280	42.518698	76.740865
43.552159	49.547095	76.745870
42.300509	52.440179	76.750874
41.862827	44.406131	76.755879
41.098541	50.671827	76.760884
39.981839	53.674274	76.765889
39.573182	42.338217	76.770894
38.434074	47.271257	76.775898
38.412674	43.094242	76.780903
38.268816	54.420730	76.785908
37.371531	53.996184	76.790913
36.558050	42.426654	76.795918
35.944023	56.414315	76.800922
35.518316	43.822579	76.805927
34.947302	53.020519	76.810932
33.790879	50.981519	76.815937
33.386504	47.971022	76.820942
32.730257	52.022812	76.825946
31.803682	45.517529	76.830951
30.718047	53.313652	76.835956
30.532260	50.558448	76.840961
30.365941	49.108998	76.845966
29.612124	65.485951	76.850970
28.845700	39.366375	76.855975
27.834193	53.165121	76.860980
27.559635	46.924846	76.865985
26.775563	47.562450	76.870990
25.779493	55.243366	76.875994
25.278207	43.866894	76.880999
24.858818	53.788121	76.886004
23.960009	45.953784	76.891009
23.307688	36.733430	76.896014
22.468751	46.617494	76.901018
21.969376	38.525487	76.906023
21.628070	41.035258	76.911028
20.347655	50.862010	76.916033
19.609559	37.343986	76.921038
18.590732	43.858441	76.926042
18.662193	50.522265	76.931047
18.295265	45.052080	76.936052
17.841496	50.426167	76.941057
17.177684	47.575325	76.946062
16.019388	48.608512	76.951066
15.723017	38.495606	76.956071
14.663899	46.968739	76.961076
13.763018	46.073271	76.966081
13.567899	40.246105	76.971086
12.764934	46.227818	76.976090
12.396874	47.425114	76.981095
11.328423	41.743558	76.986100
10.734726	48.507171	76.991105
10.514229	40.485799	76.996110
9.366072	45.954877	77.001114
8.656177	47.700281	77.006119
8.046740	47.534182	77.011124
7.501309	50.174286	77.016129
7.298728	47.044874	77.021134
6.142919	55.525554	77.026139
5.683435	37.591818	77.031143
5.371459	40.073258	77.036148
4.078363	47.175512	77.041153
3.093569	38.027121	77.046158