Fri Aug 26 10:40:52 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.194498	96.729070	0.000000
1.431037	113.475593	0.005005
1.284503	95.595106	0.010010
1.297834	101.233877	0.015014
0.996731	94.089700	0.020019
1.119484	84.851611	0.025024
0.735041	80.093177	0.030029
0.767138	73.210334	0.035034
0.469303	64.275016	0.040038
-0.037879	66.536918	0.045043
-0.372716	50.969971	0.050048
-0.912800	49.184324	0.055053
-1.161085	44.211716	0.060058
-0.780906	43.181272	0.065062
-1.478866	35.463008	0.070067
-1.488576	19.484809	0.075072
-1.581571	26.481508	0.080077
-2.428765	23.582612	0.085082
-2.806209	15.191211	0.090086
-2.652663	23.272626	0.095091
-2.815120	9.646680	0.100096
-3.563812	15.872291	0.105101
-3.820622	-2.225039	0.110106
-3.881077	0.062211	0.115110
-3.826806	1.869703	0.120115
-4.256051	3.512039	0.125120
-5.086668	-4.059006	0.130125
-5.631738	7.601716	0.135130
-5.294498	7.052510	0.140134
-5.639956	1.535074	0.145139
-5.406815	3.067951	0.150144
-5.586167	2.539066	0.155149
-6.344985	-4.163657	0.160154
-6.931996	6.867697	0.165158
-7.197040	6.972234	0.170163
-6.849528	-5.502433	0.175168
-6.905429	0.615308	0.180173
-7.226828	5.629140	0.185178
-7.847571	1.771200	0.190182
-8.464873	6.128769	0.195187
-8.283661	1.127266	0.200192
-8.439772	-2.328465	0.205197
-8.331150	0.299446	0.210202
-9.157941	7.964028	0.215206
-9.555412	17.659283	0.220211
-9.446250	-0.631066	0.225216
-9.742996	8.551806	0.230221
-10.109209	6.615710	0.235226
-9.819735	2.840672	0.240230
-11.038343	5.931486	0.245235
-11.055151	-3.180426	0.250240
-11.242570	-6.106112	0.255245
-11.360776	6.908633	0.260250
-11.330064	9.260782	0.265254
-11.506881	1.948598	0.270259
-11.434984	8.600086	0.275264
-12.621535	10.550152	0.280269
-12.781629	9.894887	0.285274
-13.179845	3.847841	0.290278
-12.933646	9.431344	0.295283
-12.888527	-0.215380	0.300288
-14.102655	4.731809	0.305293
-14.226962	0.632065	0.310298
-14.346128	-3.832300	0.315302
-14.636215	8.430946	0.320307
-14.515880	0.129725	0.325312
-14.488825	8.069479	0.330317
-14.618503	3.502348	0.335322
-15.046713	4.413715	0.340326
-15.730431	7.547795	0.345331
-15.623812	5.117313	0.350336
-15.858429	10.361237	0.355341
-16.051374	0.818016	0.360346
-16.414168	9.742260	0.365350
-17.123377	10.833416	0.370355
-16.804332	3.519956	0.375360
-17.468908	11.931219	0.380365
-17.349140	6.053454	0.385370
-17.615146	10.694841	0.390374
-18.193721	7.507360	0.395379
-18.584543	5.233420	0.400384
-18.450195	4.257071	0.405389
-19.020984	-0.700111	0.410394
-18.951282	3.006343	0.415398
-19.255739	7.805572	0.420403
-19.561933	-9.360268	0.425408
-19.819161	1.875993	0.430413
-20.449081	0.926893	0.435418
-20.452476	8.108944	0.440422
-20.233885	8.957570	0.445427
-20.611857	2.119621	0.450432
-21.412748	2.924502	0.455437
-21.270026	3.307227	0.460442
-21.366093	-2.075034	0.465446
-21.542470	7.427608	0.470451
-21.757013	-1.593407	0.475456
-22.399851	0.885755	0.480461
-22.673654	6.904550	0.485466
-22.655372	6.518897	0.490470
-23.318239	1.202738	0.495475
-23.136431	2.743607	0.500480
-23.646187	8.546046	0.505485
-24.216235	-5.623849	0.510490
-24.383783	-1.269870	0.515494
-24.706393	4.063680	0.520499
-24.606536	0.919263	0.525504
-24.795219	6.152870	0.530509
-25.088897	7.087583	0.535514
-24.746746	1.826911	0.540518
-25.742087	1.795223	0.545523
-25.838637	2.990301	0.550528
-26.205880	0.582980	0.555533
-26.596077	4.851407	0.560538
-26.388866	3.870041	0.565542
-26.542476	8.807131	0.570547
-27.030725	1.363109	0.575552
-27.797031	2.896577	0.580557
-27.819958	0.853251	0.585562
-27.821635	-6.612743	0.590566
-27.762297	0.569028	0.595571
-28.000475	-3.854661	0.600576
-28.666199	2.184026	0.605581
-29.121857	5.020013	0.610586
-28.947437	0.630156	0.615590
-29.132706	2.060504	0.620595
-29.239829	-0.172188	0.625600
-30.064103	-0.388693	0.630605
-30.072067	-3.902289	0.635610
-30.423797	7.519526	0.640614
-30.721982	12.311452	0.645619
-30.469146	3.284103	0.650624
-30.908002	0.979678	0.655629
-31.875023	9.042571	0.660634
-31.894149	7.156836	0.665638
-32.162745	7.530837	0.670643
-32.245941	3.149454	0.675648
-32.451287	7.230917	0.680653
-32.389177	13.175267	0.685658
-32.292630	-5.344058	0.690662
-32.979601	13.466500	0.695667
-33.448410	7.269098	0.700672
-33.711885	7.753031	0.705677
-34.263207	14.824248	0.710682
-33.801881	7.877766	0.715686
-34.207815	-0.759119	0.720691
-34.698012	1.335620	0.725696
-35.212059	5.860605	0.730701
-35.007647	-0.318229	0.735706
-34.810748	5.510222	0.740710
-35.516197	13.437480	0.745715
-36.174144	1.815365	0.750720
-36.818839	3.788630	0.755725
-36.738296	3.908961	0.760730
-36.832261	-3.507865	0.765734
-37.240263	4.939374	0.770739
-37.147812	6.677648	0.775744
-36.901506	2.504382	0.780749
-37.309865	10.369564	0.785754
-37.447546	5.885935	0.790758
-38.288683	11.436258	0.795763
-38.449099	-0.174737	0.800768
-38.280681	5.269017	0.805773
-38.635384	5.419151	0.810778
-39.118601	5.215981	0.815782
-39.599785	4.825838	0.820787
-40.079580	3.818564	0.825792
-40.281153	8.560646	0.830797
-40.386440	12.582240	0.835802
-40.362388	-0.209051	0.840806
-40.383107	11.873053	0.845811
-40.463389	3.824525	0.850816
-40.771964	7.438019	0.855821
-41.443789	2.050492	0.860826
-41.346546	-4.073691	0.865830
-41.890622	4.929393	0.870835
-42.448746	8.401413	0.875840
-42.727689	7.078136	0.880845
-42.918584	5.991081	0.885850
-42.662027	3.287324	0.890854
-43.081129	10.676465	0.895859
-43.017403	4.759972	0.900864
-43.288345	7.269815	0.905869
-44.122084	4.109410	0.910874
-44.226114	-5.586851	0.915878
-44.452616	0.734616	0.920883
-44.482594	1.156884	0.925888
-44.520171	6.860496	0.930893
-45.239610	1.879005	0.935898
-45.559077	-3.319780	0.940902
-45.901896	7.578642	0.945907
-45.824922	-8.450987	0.950912
-46.083121	6.085128	0.955917
-46.472120	4.586004	0.960922
-46.004543	3.190787	0.965926
-47.051025	2.183163	0.970931
-47.250028	10.420697	0.975936
-47.451232	4.523308	0.980941
-47.810320	3.560514	0.985946
-47.390617	0.907284	0.990950
-48.338048	17.800088	0.995955
-48.853476	-3.297253	1.000960
-48.722973	6.394881	1.005965
-49.028654	5.107404	1.010970
-48.841602	9.048680	1.015974
-49.458559	9.945144	1.020979
-49.385564	1.009071	1.025984
-50.378461	4.953733	1.030989
-50.592499	10.504491	1.035994
-50.255382	7.895756	1.040998
-50.721972	13.292853	1.046003
-50.900012	5.047580	1.051008
-50.716832	10.261253	1.056013
-51.155390	13.913969	1.061018
-51.474367	-6.470493	1.066022
-51.781207	8.794513	1.071027
-52.158171	0.921890	1.076032
-52.258595	3.421001	1.081037
-53.007586	4.141875	1.086042
-53.286208	7.810815	1.091046
-53.519021	5.651476	1.096051
-53.780692	6.027563	1.101056
-54.042209	7.820949	1.106061
-54.003577	2.079203	1.111066
-53.868787	7.502884	1.116070
-54.087084	11.662292	1.121075
-54.121054	10.585604	1.126080
-54.959885	3.041149	1.131085
-55.400948	3.100328	1.136090
-55.035976	-3.932384	1.141094
-55.319639	4.650513	1.146099
-56.468846	-2.478628	1.151104
-56.631032	4.136537	1.156109
-57.222644	7.417624	1.161114
-56.673245	5.282024	1.166118
-57.196723	12.399522	1.171123
-56.935652	3.219036	1.176128
-56.778225	5.178140	1.181133
-57.068589	6.476158	1.186138
-57.401302	-5.386407	1.191142
-58.065629	13.139054	1.196147
-58.000695	6.523203	1.201152
-58.851647	-1.750168	1.206157
-59.443264	9.310374	1.211162
-59.353675	4.683795	1.216166
-59.535348	4.582368	1.221171
-59.840570	1.548477	1.226176
-60.004089	0.488796	1.231181
-59.833894	5.359649	1.236186
-60.096240	0.636012	1.241190
-60.996670	11.153032	1.246195
-61.449964	6.819781	1.251200
-61.541438	11.690250	1.256205
-61.972228	12.785512	1.261210
-61.211741	7.032610	1.266214
-61.814434	18.705471	1.271219
-61.651448	7.816055	1.276224
-62.489328	5.330157	1.281229
-63.076624	3.890380	1.286234
-62.669118	2.289387	1.291238
-63.055178	15.665369	1.296243
-63.260852	7.101704	1.301248
-63.779155	7.350074	1.306253
-64.394234	5.876660	1.311258
-64.520897	3.102861	1.316262
-64.394832	10.441918	1.321267
-64.545469	6.903080	1.326272
-64.821524	10.210963	1.331277
-64.739408	8.454994	1.336282
-65.489969	10.251760	1.341286
-65.655445	9.236675	1.346291
-66.025566	7.557446	1.351296
-65.896968	14.570253	1.356301
-66.250682	7.668418	1.361306
-66.851188	3.358089	1.366310
-67.216907	12.709882	1.371315
-67.350360	7.137294	1.376320
-67.216561	5.471351	1.381325
-67.621581	9.799033	1.386330
-67.550227	-1.041310	1.391334
-68.457575	5.272272	1.396339
-68.655751	1.120759	1.401344
-68.926183	3.972197	1.406349
-69.272187	6.661401	1.411354
-68.725186	3.653002	1.416358
-68.945788	13.317549	1.421363
-69.641262	4.118322	1.426368
-69.812736	10.361623	1.431373
-70.207020	5.728128	1.436378
-70.140155	3.433547	1.441382
-70.583101	10.342357	1.446387
-70.974331	5.638786	1.451392
-71.172243	6.137821	1.456397
-71.492693	5.573960	1.461402
-71.323910	13.681466	1.466406
-71.910916	14.731451	1.471411
-72.384564	13.220197	1.476416
-72.762044	-0.872113	1.481421
-72.989945	10.467147	1.486426
-72.863650	3.541196	1.491430
-73.165730	8.488746	1.496435
-73.174414	11.160230	1.501440
-73.594700	-0.081278	1.506445
-74.248078	11.305247	1.511450
-74.719637	5.196861	1.516454
-74.453060	0.909712	1.521459
-74.685179	8.187481	1.526464
-74.770029	0.683819	1.531469
-75.363096	3.098286	1.536474
-75.400486	-6.216052	1.541478
-75.951719	2.193374	1.546483
-75.997982	4.589142	1.551488
-76.000266	7.392503	1.556493
-76.324941	10.122677	1.561498
-76.237037	1.522797	1.566502
-77.135565	10.967037	1.571507
-77.712165	7.187646	1.576512
-77.541757	6.860562	1.581517
-78.033377	16.320541	1.586522
-77.775585	1.575677	1.591526
-77.709185	1.498898	1.596531
-78.526010	11.778280	1.601536
-78.750729	2.970818	1.606541
-79.137367	0.322916	1.611546
-79.152626	4.507655	1.616550
-79.462165	6.716631	1.621555
-79.625883	3.069102	1.626560
-80.064772	-1.541627	1.631565
-80.724121	12.345124	1.636570
-80.497753	6.561493	1.641574
-80.989322	5.157431	1.646579
-80.618728	1.012271	1.651584
-81.103362	-1.762737	1.656589
-81.012073	7.002218	1.661594
-81.896710	5.947250	1.666598
-82.268992	9.513718	1.671603
-82.285410	1.360340	1.676608
-81.939960	2.239831	1.681613
-82.664451	5.905428	1.686618
-83.521163	8.066725	1.691622
-83.594039	10.242017	1.696627
-83.765468	-2.544141	1.701632
-83.299272	-0.057326	1.706637
-83.588843	4.040413	1.711642
-83.899670	6.255917	1.716646
-84.692174	-1.023671	1.721651
-85.468181	-0.773140	1.726656
-85.091947	-2.419882	1.731661
-85.456389	1.857188	1.736666
-85.275912	-1.378872	1.741670
-85.351689	-1.158275	1.746675
-85.728538	0.346192	1.751680
-86.257084	-6.389213	1.756685
-86.936926	-2.768534	1.761690
-86.886120	-4.421553	1.766694
-87.011879	1.368549	1.771699
-87.033964	-4.069519	1.776704
-86.932757	-14.715189	1.781709
-87.836640	2.085397	1.786714
-87.832426	-2.935998	1.791718
-88.200039	-2.650980	1.796723
-88.410360	9.337256	1.801728
-88.769058	-6.915592	1.806733
-89.745163	0.038263	1.811738
-89.854087	-4.993989	1.816742
-89.626587	6.334471	1.821747
-89.787587	0.715556	1.826752
-90.050234	1.844748	1.831757
-90.407299	0.005305	1.836762
-89.924750	2.084624	1.841766
-90.269317	1.540338	1.846771
-90.819268	1.432979	1.851776
-91.244535	-1.927059	1.856781
-91.962009	-0.160755	1.861786
-91.766313	1.064747	1.866790
-91.842762	-2.536258	1.871795
-92.424874	-3.397889	1.876800
-92.393502	-2.390404	1.881805
-92.991697	3.055653	1.886810
-92.944584	2.320671	1.891814
-93.260615	9.367903	1.896819
-93.301176	1.230940	1.901824
-93.382466	5.587306	1.906829
-94.581614	19.036103	1.911834
-94.619368	4.852932	1.916838
-94.571304	8.249550	1.921843
-94.834293	5.332467	1.926848
-94.710146	1.814120	1.931853
-94.912596	4.107659	1.936858
-95.291163	6.067962	1.941862
-95.852584	4.791833	1.946867
-96.104802	3.179666	1.951872
-96.075456	0.909910	1.956877
-96.348996	7.893579	1.961882
-96.835902	10.171300	1.966886
-97.527026	4.100265	1.971891
-97.591393	12.111196	1.976896
-97.299395	2.179272	1.981901
-97.653726	6.964118	1.986906
-97.548851	4.489618	1.991910
-98.251550	5.627217	1.996915
-98.852225	2.567028	2.006912
-98.217747	11.803494	2.016909
-98.091317	10.893674	2.026906
-97.428842	13.771342	2.036902
-96.563544	6.316014	2.046899
-96.390823	4.318795	2.056896
-95.707841	10.212104	2.066893
-95.370698	5.202128	2.076890
-95.146748	3.890663	2.086886
-94.269051	5.318850	2.096883
-94.062329	5.235974	2.106880
-93.357769	2.946879	2.116877
-92.505358	8.354488	2.126874
-92.381007	-1.769895	2.136870
-91.700929	2.622367	2.146867
-91.221636	5.500046	2.156864
-90.986433	8.881386	2.166861
-89.946247	8.187246	2.176858
-89.531650	4.951802	2.186854
-89.539606	-0.796370	2.196851
-88.962540	-3.559777	2.206848
-88.228620	7.539660	2.216845
-88.029355	3.393764	2.226842
-86.840246	1.811650	2.236838
-86.436327	2.249253	2.246835
-86.450222	5.789750	2.256832
-86.158972	4.553334	2.266829
-85.359162	-1.304769	2.276826
-84.919339	1.994027	2.286822
-83.881310	-0.796805	2.296819
-83.673276	1.695467	2.306816
-83.575711	4.585066	2.316813
-82.564987	6.784472	2.326810
-82.373782	4.527790	2.336806
-82.116710	6.055778	2.346803
-81.488903	2.413347	2.356800
-80.456061	0.535625	2.366797
-79.718378	5.466934	2.376794
-80.148357	0.424349	2.386790
-79.636486	7.687412	2.396787
-78.095280	5.952277	2.406784
-78.113618	6.724882	2.416781
-78.160296	6.342514	2.426778
-77.553443	0.178676	2.436774
-76.608089	3.696526	2.446771
-76.281450	-1.391007	2.456768
-75.607404	2.226105	2.466765
-75.354393	1.103346	2.476762
-74.781590	4.356095	2.486758
-73.773285	2.849649	2.496755
-73.285438	-1.800497	2.506752
-73.512701	4.633669	2.516749
-73.351532	0.743954	2.526746
-72.621202	4.893983	2.536742
-71.500313	3.544232	2.546739
-71.022323	12.576991	2.556736
-70.838738	7.451542	2.566733
-70.180496	5.163323	2.576730
-69.584309	4.839248	2.586726
-69.422262	2.653628	2.596723
-68.596238	9.674548	2.606720
-68.004092	4.491823	2.616717
-67.882759	7.770519	2.626714
-67.347366	6.467581	2.636710
-66.402775	5.997396	2.646707
-66.224704	0.685912	2.656704
-65.983581	8.257220	2.666701
-65.202123	8.617034	2.676698
-64.796588	5.474865	2.686694
-63.968554	3.765244	2.696691
-63.550502	4.948228	2.706688
-63.487986	6.303774	2.716685
-62.920285	1.267403	2.726682
-62.055474	2.418840	2.736678
-61.803014	5.886188	2.746675
-61.053692	4.508762	2.756672
-60.686664	5.883418	2.766669
-60.422746	5.861326	2.776666
-59.840049	5.380965	2.786662
-59.066929	2.609206	2.796659
-58.848098	-3.491049	2.806656
-57.956447	1.422623	2.816653
-57.632716	3.073276	2.826650
-57.499984	6.445229	2.836646
-56.448410	4.038750	2.846643
-56.126502	3.728870	2.856640
-55.797191	3.721939	2.866637
-55.161230	5.948019	2.876634
-54.646432	1.873368	2.886630
-54.403301	7.182613	2.896627
-53.312166	2.086918	2.906624
-53.034085	4.837542	2.916621
-52.873161	4.492540	2.926618
-52.477618	3.686535	2.936614
-51.520295	-0.526706	2.946611
-51.267055	3.564561	2.956608
-50.491157	4.365555	2.966605
-50.056210	7.208961	2.976602
-49.879432	6.671428	2.986598
-49.079568	2.717113	2.996595
-48.357127	0.374551	3.006592
-48.466952	4.544522	3.016589
-47.745039	1.967631	3.026586
-47.040161	6.270506	3.036582
-46.908811	6.376758	3.046579
-45.745869	7.538796	3.056576
-45.499475	-2.290988	3.066573
-45.391314	0.596962	3.076570
-44.912791	0.484438	3.086566
-44.138139	-4.375085	3.096563
-43.809296	-3.406287	3.106560
-43.034934	4.408272	3.116557
-42.536335	0.418503	3.126554
-42.319307	-5.494576	3.136550
-41.353436	3.940545	3.146547
-40.913492	5.462235	3.156544
-40.880655	1.006472	3.166541
-40.273944	-2.924103	3.176538
-39.413695	3.226703	3.186534
-39.472638	-1.997195	3.196531
-38.620001	-1.334858	3.206528
-38.094501	-0.396679	3.216525
-37.968122	1.028117	3.226522
-36.902139	8.426649	3.236518
-36.620444	10.901120	3.246515
-36.361205	-0.422661	3.256512
-35.331718	9.186286	3.266509
-34.938790	11.953875	3.276506
-34.864836	-0.050627	3.286502
-34.306633	5.003661	3.296499
-33.691262	-0.236530	3.306496
-33.145006	5.405646	3.316493
-32.174884	-0.048165	3.326490
-31.826358	0.876388	3.336486
-31.876797	-1.501056	3.346483
-31.585675	-2.325648	3.356480
-30.580567	-3.917123	3.366477
-30.193518	5.446568	3.376474
-29.004969	-0.380198	3.386470
-28.803218	-1.181372	3.396467
-28.712965	-5.199424	3.406464
-28.458080	-0.455863	3.416461
-27.386545	-3.628868	3.426458
-26.910661	-2.695635	3.436454
-27.000493	1.182961	3.446451
-26.247176	-5.336291	3.456448
-25.812901	-2.771540	3.466445
-25.190683	5.111056	3.476442
-24.288018	1.679249	3.486438
-24.477296	-2.776775	3.496435
-23.602698	-3.603517	3.506432
-23.304588	-6.722623	3.516429
-22.446080	-9.032518	3.526426
-21.903604	-6.994616	3.536422
-22.070395	-1.599374	3.546419
-20.651302	-1.294488	3.556416
-20.168763	4.063012	3.566413
-20.085919	3.213830	3.576410
-19.767351	-1.093190	3.586406
-19.503529	-7.292314	3.596403
-18.988373	2.342860	3.606400
-17.693867	3.189818	3.616397
-17.319978	-2.525946	3.626394
-17.003260	-5.714472	3.636390
-17.013092	6.530282	3.646387
-16.038644	-2.240804	3.656384
-15.707024	0.602851	3.666381
-15.046249	3.534638	3.676378
-14.309819	-1.502662	3.686374
-14.314746	-7.270313	3.696371
-13.515838	-4.284010	3.706368
-12.724874	-0.944851	3.716365
-12.729572	-7.602667	3.726362
-12.499597	-3.944922	3.736358
-11.484729	0.607456	3.746355
-11.283419	-3.161801	3.756352
-10.668779	1.833018	3.766349
-9.881324	-0.307429	3.776346
-9.733283	1.433934	3.786342
-8.919588	-3.960677	3.796339
-8.555282	1.320200	3.806336
-8.206929	6.559214	3.816333
-7.371991	3.160125	3.826330
-6.948241	7.858392	3.836326
-6.530873	6.326749	3.846323
-6.339088	6.936761	3.856320
-5.699694	7.356709	3.866317
-5.394185	16.691924	3.876314
-4.788300	23.690112	3.886310
-4.016340	33.155444	3.896307
-3.577873	36.929619	3.906304
-3.491950	37.708167	3.916301
-2.801115	50.543928	3.926298
-2.571690	63.530732	3.936294
-1.830091	72.424286	3.946291
-1.280532	81.563150	3.956288
-1.147264	89.981236	3.966285
-0.626931	107.493820	3.976282
0.000000	116.255348	3.981286
0.320227	120.859272	3.986291
0.202418	124.012828	3.991296
0.272478	127.016913	3.996301
0.505543	125.265902	4.001306
0.543367	125.471977	4.006310
0.415926	135.814939	4.011315
0.885870	135.937916	4.016320
0.866493	144.897342	4.021325
0.624457	151.142190	4.026330
1.007083	136.599228	4.031334
0.627584	146.101933	4.036339
0.838698	147.720508	4.041344
0.660832	145.932238	4.046349
0.629055	156.839273	4.051354
0.802412	157.214068	4.056358
0.688284	153.435400	4.061363
0.914582	148.401527	4.066368
1.039754	147.262087	4.071373
1.105822	143.157979	4.076378
1.266137	138.570971	4.081382
0.954037	142.207187	4.086387
1.048769	141.145253	4.091392
0.793670	132.117827	4.096397
0.841721	131.275128	4.101402
1.179660	140.991989	4.106406
0.757250	142.744002	4.111411
0.913281	147.155203	4.116416
0.844201	161.946737	4.121421
1.025992	150.196940	4.126426
0.909488	151.170512	4.131430
1.291043	159.469584	4.136435
1.241367	152.270418	4.141440
1.279585	159.449216	4.146445
1.047900	148.871089	4.151450
1.133110	143.568124	4.156454
0.735733	147.859849	4.161459
0.906775	152.866652	4.166464
0.750197	149.037648	4.171469
0.975574	148.866516	4.176474
1.071176	150.376529	4.181478
0.914408	162.451448	4.186483
1.134572	152.438872	4.191488
1.335229	156.858945	4.196493
1.082872	152.696847	4.201498
1.239294	144.684162	4.206502
1.180348	145.243819	4.211507
1.175465	143.327379	4.216512
1.169081	153.468008	4.221517
1.173556	158.276124	4.226522
1.321652	146.218370	4.231526
1.101898	148.862629	4.236531
1.352914	149.589157	4.241536
1.324506	147.720671	4.246541
1.135469	155.770065	4.251546
1.480498	152.169840	4.256550
1.243298	155.639377	4.261555
1.438677	157.681174	4.266560
1.221896	147.480372	4.271565
0.960828	150.390486	4.276570
1.148992	154.787195	4.281574
1.577334	169.555072	4.286579
1.332518	171.007359	4.291584
1.758912	170.267100	4.296589
1.345687	160.976383	4.301594
1.512013	168.514882	4.306598
1.482923	174.046389	4.311603
1.736664	167.170128	4.316608
1.582492	169.307479	4.321613
1.377884	162.790480	4.326618
1.378850	156.937489	4.331622
1.471617	175.759694	4.336627
1.849637	163.533254	4.341632
1.595058	165.537544	4.346637
1.303033	158.777897	4.351642
2.010163	164.912933	4.356646
1.302933	167.522363	4.361651
1.925963	174.973939	4.366656
1.645102	167.016674	4.371661
1.269829	169.359289	4.376666
1.583504	169.822967	4.381670
1.690760	181.660643	4.386675
1.726922	173.116186	4.391680
1.442421	182.357352	4.396685
1.729780	183.707799	4.401690
1.721305	173.449240	4.406694
1.731921	172.444691	4.411699
1.684226	171.632716	4.416704
1.985143	185.540938	4.421709
1.666525	187.982300	4.426714
1.865615	173.977239	4.431718
2.040662	189.948811	4.436723
1.835077	180.208147	4.441728
1.575370	181.257799	4.446733
1.352747	183.601958	4.451738
1.895033	188.680682	4.456742
1.759343	183.608248	4.461747
1.660959	186.287399	4.466752
2.057770	180.894779	4.471757
1.855191	183.254800	4.476762
1.910470	177.010538	4.481766
2.003783	192.586721	4.486771
1.825495	177.843160	4.491776
2.295811	172.916817	4.496781
1.883595	184.028632	4.501786
1.700899	178.533254	4.506790
1.359546	181.598241	4.511795
1.582524	178.463095	4.516800
1.648597	189.873762	4.521805
1.582099	194.325949	4.526810
2.196464	195.824798	4.531814
2.117193	196.068087	4.536819
2.328792	201.464052	4.541824
2.493210	196.003209	4.546829
1.795135	193.666352	4.551834
2.228794	183.573061	4.556838
1.948847	181.117322	4.561843
1.923878	185.737045	4.566848
2.057084	188.797747	4.571853
1.985967	201.624973	4.576858
2.180935	201.040966	4.581862
2.269386	204.779344	4.586867
2.398941	202.636324	4.591872
2.419619	200.481783	4.596877
1.801706	195.648939	4.601882
2.177112	195.119095	4.606886
2.225667	207.067166	4.611891
2.220446	209.276241	4.616896
2.100130	203.641432	4.621901
2.241845	211.243891	4.626906
2.201206	213.569211	4.631910
2.226887	213.482953	4.636915
2.089757	212.153399	4.641920
2.486194	212.253021	4.646925
2.591959	210.686335	4.651930
2.625674	204.882013	4.656934
2.628385	208.475555	4.661939
2.514331	202.390525	4.666944
2.286551	207.715699	4.671949
2.326793	211.711517	4.676954
2.712711	204.820990	4.681958
2.171190	196.404430	4.686963
2.398949	196.213944	4.691968
2.551745	202.786472	4.696973
2.339866	199.165380	4.701978
2.559582	191.775561	4.706982
2.453947	205.936919	4.711987
2.225829	205.902832	4.716992
2.615433	200.694823	4.721997
2.233143	203.699749	4.727002
2.435866	202.266662	4.732006
2.510183	204.520300	4.737011
2.588084	205.210510	4.742016
2.576063	204.633421	4.747021
2.045298	211.359835	4.752026
2.336874	206.002575	4.757030
2.597948	210.334163	4.762035
2.204502	207.620849	4.767040
2.739113	207.354114	4.772045
2.556892	202.200335	4.777050
2.826553	204.452032	4.782054
2.515288	213.314572	4.787059
2.265774	209.930289	4.792064
2.403476	207.017220	4.797069
2.411109	226.640496	4.802074
3.062807	222.043398	4.807078
2.843144	233.988956	4.812083
2.879927	220.752600	4.817088
2.610360	211.765351	4.822093
2.511438	228.886911	4.827098
2.788974	227.464320	4.832102
2.748813	235.300748	4.837107
2.793296	234.262450	4.842112
3.060164	236.495603	4.847117
2.685931	245.377455	4.852122
3.063715	228.883161	4.857126
2.716243	233.401251	4.862131
2.859880	233.711073	4.867136
3.066477	230.568978	4.872141
2.612386	234.009025	4.877146
2.763452	233.261012	4.882150
2.697895	237.124614	4.887155
3.038318	230.668261	4.892160
2.820061	239.801067	4.897165
3.204021	237.691199	4.902170
3.164364	235.463792	4.907174
3.058960	231.914700	4.912179
3.234022	232.333523	4.917184
3.361610	231.108282	4.922189
2.846537	228.869476	4.927194
3.052046	228.334446	4.932198
2.979279	238.855613	4.937203
2.957923	231.506475	4.942208
3.145459	240.180637	4.947213
3.221274	240.731971	4.952218
3.415572	226.828852	4.957222
2.824928	230.840645	4.962227
2.975263	234.142293	4.967232
3.278213	234.500076	4.972237
3.193413	241.919521	4.977242
2.901358	236.941018	4.982246
2.944924	243.343908	4.987251
2.987969	240.008980	4.992256
2.791117	241.260818	4.997261
2.839063	239.336142	5.002266
2.882888	241.771700	5.007270
2.977655	250.128121	5.012275
2.913981	232.544639	5.017280
3.070754	236.338824	5.022285
2.788911	244.570384	5.027290
3.291875	244.643930	5.032294
3.378035	250.809240	5.037299
3.618694	257.595895	5.042304
3.626475	260.967199	5.047309
3.216636	262.144634	5.052314
3.447845	251.608269	5.057318
3.282028	253.747442	5.062323
3.383657	251.399960	5.067328
3.291920	242.938657	5.072333
3.203036	264.133548	5.077338
3.290446	256.587133	5.082342
3.643212	257.357935	5.087347
3.479987	267.250969	5.092352
3.673470	263.171287	5.097357
3.269064	249.601809	5.102362
3.309666	254.170212	5.107366
3.249902	257.659598	5.112371
3.292445	265.245885	5.117376
3.307323	261.323723	5.122381
3.021961	264.519209	5.127386
3.334342	256.365135	5.132390
3.200403	259.862907	5.137395
3.078824	261.928756	5.142400
3.761425	267.112205	5.147405
3.245224	279.632303	5.152410
3.573543	288.762291	5.157414
3.700716	278.447750	5.162419
3.991171	279.649029	5.167424
3.772149	265.731140	5.172429
3.459884	270.984066	5.177434
3.386597	274.352176	5.182438
3.439755	287.444850	5.187443
3.824435	282.604576	5.192448
3.825148	281.569926	5.197453
3.956019	289.734085	5.202458
3.786429	285.619179	5.207462
3.651758	276.781735	5.212467
3.934387	287.598770	5.217472
3.702364	272.945753	5.222477
3.548032	285.751196	5.227482
3.917588	282.697613	5.232486
4.012214	284.869006	5.237491
3.435158	276.363029	5.242496
4.002807	276.435995	5.247501
3.887578	294.259337	5.252506
3.823276	290.007816	5.257510
4.048356	286.555953	5.262515
3.725888	277.285845	5.267520
3.575070	278.318549	5.272525
3.822978	290.874709	5.277530
4.215862	287.738401	5.282534
4.248005	291.545674	5.287539
4.000303	278.065671	5.292544
3.640666	264.650561	5.297549
3.703933	279.516498	5.302554
4.110866	279.329752	5.307558
4.097448	289.740470	5.312563
3.838657	293.694281	5.317568
4.015852	293.299697	5.322573
3.953958	287.247645	5.327578
4.505116	290.119906	5.332582
3.957688	287.901948	5.337587
4.092019	280.952488	5.342592
3.861549	284.322926	5.347597
3.788807	285.738940	5.352602
3.999612	280.650494	5.357606
3.984488	285.417405	5.362611
3.932724	281.961190	5.367616
3.961154	283.276031	5.372621
3.577633	286.151450	5.377626
4.018886	284.162368	5.382630
3.749934	292.483691	5.387635
3.803054	284.955258	5.392640
4.313853	295.667171	5.397645
4.393606	304.298036	5.402650
4.627886	300.990268	5.407654
4.412086	293.563812	5.412659
4.543318	291.088331	5.417664
4.512991	287.018180	5.422669
4.326384	286.319575	5.427674
3.998726	283.978816	5.432678
4.246994	283.310579	5.437683
4.362563	293.618960	5.442688
4.380336	294.255261	5.447693
4.016257	291.879043	5.452698
4.491667	278.501586	5.457702
3.970640	283.420029	5.462707
4.167687	281.699921	5.467712
4.235354	286.042658	5.472717
4.435454	300.210273	5.477722
4.639548	305.094916	5.482726
4.188659	290.912555	5.487731
4.358304	307.774079	5.492736
4.735787	300.941775	5.497741
4.283966	305.871595	5.502746
4.588255	301.831599	5.507750
4.628991	301.388660	5.512755
4.487434	298.560184	5.517760
4.259625	289.278496	5.522765
4.164157	299.923455	5.527770
4.573870	299.783732	5.532774
4.610817	303.039772	5.537779
4.661814	308.811949	5.542784
5.188113	303.620592	5.547789
4.345169	293.890516	5.552794
4.681662	297.887683	5.557798
4.435349	289.390315	5.562803
4.676350	296.787529	5.567808
5.132840	296.241895	5.572813
4.598010	296.853504	5.577818
4.573498	288.916381	5.582822
4.652597	284.193286	5.587827
4.157791	282.811849	5.592832
4.893673	299.164429	5.597837
4.617687	310.770799	5.602842
4.968623	310.893324	5.607846
4.724732	311.782336	5.612851
4.962885	306.765554	5.617856
4.664156	300.468801	5.622861
4.294853	296.033814	5.627866
4.595738	296.645018	5.632870
4.580795	303.636000	5.637875
4.319353	316.771350	5.642880
4.710663	304.280156	5.647885
4.537882	312.153085	5.652890
4.796428	309.040852	5.657894
4.655157	312.539776	5.662899
4.647810	309.513234	5.667904
4.554358	307.069569	5.672909
4.825566	321.757635	5.677914
5.060161	324.720317	5.682918
5.025247	321.198197	5.687923
4.507441	323.553532	5.692928
5.310058	318.989859	5.697933
5.184534	336.273851	5.702938
5.112084	324.168057	5.707942
4.965864	322.039487	5.712947
4.865161	319.005333	5.717952
4.939546	306.892507	5.722957
4.939828	315.776194	5.727962
5.483712	320.696521	5.732966
4.997889	311.262006	5.737971
4.940117	311.198232	5.742976
5.144959	310.707596	5.747981
5.035522	320.826401	5.752986
4.808121	308.140472	5.757990
5.238711	318.858560	5.762995
5.180545	328.206929	5.768000
5.288180	328.079437	5.773005
5.108488	325.623887	5.778010
4.990927	316.201634	5.783014
5.367294	328.854878	5.788019
4.941820	325.934562	5.793024
5.152646	324.256597	5.798029
5.336244	321.405966	5.803034
5.143257	325.273609	5.808038
5.265001	330.563382	5.813043
4.964027	333.498722	5.818048
5.656534	328.370064	5.823053
5.216645	332.715908	5.828058
5.230366	327.658134	5.833062
5.360343	322.518987	5.838067
5.233267	333.418822	5.843072
5.403393	326.897201	5.848077
5.473076	333.675704	5.853082
5.387948	341.319866	5.858086
5.618175	334.909107	5.863091
5.086932	327.481130	5.868096
4.977157	321.458667	5.873101
5.111293	337.326011	5.878106
5.245669	336.324331	5.883110
5.168212	332.938545	5.888115
4.927569	345.010829	5.893120
5.579282	336.949417	5.898125
5.378260	337.480581	5.903130
5.075262	335.838323	5.908134
5.365083	337.881256	5.913139
5.614677	336.289002	5.918144
5.403013	333.525219	5.923149
4.857359	342.845093	5.928154
5.456108	351.879225	5.933158
5.753991	358.929091	5.938163
5.652685	353.218508	5.943168
5.479696	357.193774	5.948173
5.747579	364.302096	5.953178
5.825362	355.314477	5.958182
5.789253	355.044851	5.963187
5.613998	350.614439	5.968192
5.852852	345.493134	5.973197
5.309574	347.039360	5.978202
5.297487	347.025420	5.983206
5.859092	351.867068	5.988211
5.881336	363.828832	5.993216
5.647252	361.055881	5.998221
5.733449	359.387826	6.003226
5.652176	364.497248	6.008230
5.915945	346.198288	6.013235
5.396902	341.536669	6.018240
5.442346	339.441530	6.023245
5.511111	355.388670	6.028250
5.601172	352.460850	6.033254
5.731314	351.304805	6.038259
5.804356	363.008725	6.043264
5.672510	360.593176	6.048269
5.960836	367.783737	6.053274
5.911665	346.635521	6.058278
5.941190	342.312432	6.063283
5.577905	339.635530	6.068288
5.776799	330.774598	6.073293
5.248363	336.706601	6.078298
5.199872	333.604204	6.083302
5.888551	340.014254	6.088307
5.507571	346.423171	6.093312
5.689395	347.122516	6.098317
5.772739	345.122715	6.103322
5.554745	345.963404	6.108326
5.768183	346.392073	6.113331
5.447802	351.484937	6.118336
5.556424	353.265020	6.123341
5.542450	364.356071	6.128346
5.751584	354.851295	6.133350
6.058766	354.945832	6.138355
5.757839	349.592195	6.143360
5.690796	340.038679	6.148365
5.729486	330.753441	6.153370
5.483939	336.676200	6.158374
5.846750	330.301746	6.163379
5.369684	339.142708	6.168384
5.794089	339.380344	6.173389
5.518601	343.086831	6.178394
5.749565	342.101749	6.183398
6.106151	353.783662	6.188403
5.435876	341.533656	6.193408
5.917990	338.902297	6.198413
5.796305	333.413191	6.203418
5.761364	334.690446	6.208422
5.691019	327.861420	6.213427
5.527539	341.709192	6.218432
5.625078	332.019325	6.223437
5.686289	335.043805	6.228442
5.343318	337.020748	6.233446
5.340032	330.184443	6.238451
5.264842	341.237554	6.243456
5.672328	350.731731	6.248461
5.864140	358.190414	6.253466
5.797168	354.534074	6.258470
5.705640	343.497415	6.263475
5.539790	350.012042	6.268480
5.751734	353.430669	6.273485
5.908596	352.305265	6.278490
5.278065	336.894836	6.283494
5.862531	347.329557	6.288499
5.604958	344.531792	6.293504
5.811445	334.714230	6.298509
5.606471	340.130805	6.303514
5.543038	341.039177	6.308518
5.763137	340.653731	6.313523
5.867301	347.468000	6.318528
5.820924	342.723297	6.323533
5.527930	340.478373	6.328538
5.474695	326.164468	6.333542
6.020264	335.478952	6.338547
5.456388	338.980404	6.343552
5.544114	337.274148	6.348557
5.649152	343.632703	6.353562
5.270458	330.378697	6.358566
5.901811	339.322326	6.363571
5.530487	350.136814	6.368576
5.512231	354.698588	6.373581
5.640823	361.385673	6.378586
5.568081	362.368261	6.383590
5.850699	357.255958	6.388595
5.723205	366.836602	6.393600
5.666284	367.225110	6.398605
5.914592	369.068867	6.403610
5.210374	354.413372	6.408614
5.501648	356.569975	6.413619
5.488193	369.208012	6.418624
5.712903	363.051200	6.423629
5.818419	360.693607	6.428634
6.060311	366.312695	6.433638
6.088649	356.168520	6.438643
5.572845	352.790869	6.443648
5.602989	336.878944	6.448653
5.413188	337.822810	6.453658
5.364300	341.550962	6.458662
5.607895	347.214071	6.463667
5.398889	363.713827	6.468672
5.868607	353.102302	6.473677
5.782494	359.265999	6.478682
5.511175	366.277941	6.483686
6.095355	362.194353	6.488691
5.517466	353.615702	6.493696
5.692302	354.923572	6.498701
5.962352	362.442840	6.503706
5.716279	351.737120	6.508710
5.440397	346.746577	6.513715
5.192060	348.332303	6.518720
5.434785	357.459834	6.523725
5.855930	358.178866	6.528730
5.342141	362.846268	6.533734
5.603697	363.634439	6.538739
5.503154	367.177652	6.543744
5.992518	363.415709	6.548749
6.084900	362.316162	6.553754
5.724915	362.093799	6.558758
5.911042	359.793257	6.563763
5.455191	351.648020	6.568768
5.445800	344.085003	6.573773
5.629887	351.468955	6.578778
5.651601	356.299751	6.583782
5.910434	360.378627	6.588787
5.688832	357.220921	6.593792
6.004842	350.872730	6.598797
5.539784	349.929577	6.603802
5.302395	345.141848	6.608806
5.768874	343.164651	6.613811
5.694924	365.537408	6.618816
5.913951	360.827307	6.623821
5.791175	353.639441	6.628826
5.092986	342.020199	6.633830
5.608010	349.033089	6.638835
5.473412	371.095758	6.643840
5.527670	361.722659	6.648845
5.618224	367.725976	6.653850
5.473028	362.256340	6.658854
6.059519	356.998649	6.663859
5.880505	364.398012	6.668864
6.382016	359.631275	6.673869
5.948568	345.917550	6.678874
5.627659	337.836730	6.683878
5.688507	330.806943	6.688883
5.456443	341.242243	6.693888
5.430854	334.596069	6.698893
5.675710	338.167755	6.703898
5.455158	345.418555	6.708902
5.771168	339.930901	6.713907
5.945468	343.605322	6.718912
5.641242	347.866773	6.723917
5.398054	342.171957	6.728922
5.123701	341.455375	6.733926
6.044367	355.222945	6.738931
5.358265	351.770569	6.743936
5.923274	353.254970	6.748941
5.899134	360.095547	6.753946
5.890557	348.748579	6.758950
5.932648	339.991149	6.763955
5.317868	343.532165	6.768960
5.621100	341.608859	6.773965
5.698277	332.969355	6.778970
5.840971	354.144115	6.783974
5.540267	347.480660	6.788979
5.571242	348.450263	6.793984
5.682464	350.204631	6.798989
5.765027	345.455671	6.803994
5.980829	338.139166	6.808998
5.734615	338.497034	6.814003
5.257712	346.581843	6.819008
5.383817	338.406114	6.824013
5.971031	340.757082	6.829018
6.131166	343.437134	6.834022
5.758608	338.176910	6.839027
5.449512	342.261949	6.844032
5.682038	336.426629	6.849037
5.551087	342.138561	6.854042
5.616497	343.665946	6.859046
5.967974	340.985325	6.864051
5.695046	341.730163	6.869056
5.552079	342.581316	6.874061
5.394667	346.883183	6.879066
5.400329	345.006207	6.884070
5.858466	340.736606	6.889075
5.515475	349.651609	6.894080
5.320073	330.750282	6.899085
5.554474	339.708259	6.904090
5.404875	333.989383	6.909094
5.612539	343.378628	6.914099
5.563973	354.225124	6.919104
5.950099	362.887409	6.924109
5.578898	357.500419	6.929114
5.327613	343.419814	6.934118
5.632542	355.783646	6.939123
5.566518	370.065516	6.944128
5.383228	370.062414	6.949133
5.823998	365.599360	6.954138
5.712584	369.754866	6.959142
5.927861	360.900859	6.964147
5.611844	367.616042	6.969152
5.672990	373.358186	6.974157
5.844312	370.050717	6.979162
5.712639	365.562895	6.984166
5.948678	360.033904	6.989171
5.286748	348.342574	6.994176
5.316144	351.175859	6.999181
5.668476	361.877684	7.004186
5.725751	368.031714	7.009190
5.666266	365.354963	7.014195
5.779571	366.824273	7.019200
6.001116	354.492352	7.024205
5.543736	351.558018	7.029210
5.365000	355.385483	7.034214
5.727002	355.370246	7.039219
5.715560	370.883802	7.044224
5.903015	367.652915	7.049229
5.785441	357.822520	7.054234
5.111885	354.722528	7.059238
5.445659	354.243454	7.064243
5.752715	370.545809	7.069248
6.075775	374.677963	7.074253
6.023685	360.661243	7.079258
5.868489	352.766585	7.084262
5.646906	348.276948	7.089267
5.756967	351.923408	7.094272
5.440733	342.253666	7.099277
5.684620	344.313242	7.104282
5.610247	342.521493	7.109286
5.761715	343.991187	7.114291
5.455937	339.283709	7.119296
5.745493	336.682331	7.124301
5.719238	343.010708	7.129306
5.728151	336.355998	7.134310
5.772110	324.295354	7.139315
5.922126	335.569659	7.144320
5.576561	337.126230	7.149325
5.801867	336.676699	7.154330
5.401762	338.213288	7.159334
5.811704	336.327151	7.164339
5.476302	338.688890	7.169344
5.914172	334.419283	7.174349
5.558223	332.595446	7.179354
5.953623	344.701577	7.184358
5.658419	337.388704	7.189363
5.608101	341.389160	7.194368
5.445592	335.615346	7.199373
5.649363	345.460775	7.204378
5.765881	355.598203	7.209382
5.553559	342.504944	7.214387
5.629157	350.823269	7.219392
5.730773	347.210284	7.224397
5.745067	346.179844	7.229402
5.436310	350.018061	7.234406
5.753333	345.523659	7.239411
5.609757	349.320339	7.244416
5.786672	344.313081	7.249421
5.504957	340.639559	7.254426
5.567484	342.325579	7.259430
5.628095	350.000837	7.264435
5.393508	345.215835	7.269440
5.364251	344.179520	7.274445
5.744014	351.336856	7.279450
5.447663	346.748130	7.284454
5.718721	352.682209	7.289459
5.760873	357.601571	7.294464
6.233430	352.526135	7.299469
5.784532	344.702519	7.304474
5.685635	344.955193	7.309478
5.791403	334.761010	7.314483
5.889765	346.710911	7.319488
5.597188	346.218628	7.324493
5.637120	341.780024	7.329498
5.523946	347.299365	7.334502
5.744673	341.775927	7.339507
5.758858	339.239569	7.344512
5.744853	346.942261	7.349517
5.773799	341.619524	7.354522
5.484608	348.153354	7.359526
5.425090	335.624763	7.364531
5.441990	340.595508	7.369536
5.773082	343.324872	7.374541
5.875872	340.382417	7.379546
5.499417	351.539387	7.384550
5.505590	335.703962	7.389555
5.598546	342.080216	7.394560
5.536155	337.885332	7.399565
5.956246	334.675178	7.404570
5.810934	341.942735	7.409574
5.676144	332.478864	7.414579
5.325535	340.243452	7.419584
5.856167	335.446878	7.424589
5.894140	336.219240	7.429594
5.668364	339.253602	7.434598
5.739872	342.384048	7.439603
5.485081	343.939140	7.444608
5.415685	341.681549	7.449613
5.622343	330.658582	7.454618
5.314319	342.950161	7.459622
5.660957	340.460117	7.464627
5.727658	339.835966	7.469632
5.928283	337.862197	7.474637
5.748245	336.529823	7.479642
5.541397	337.501652	7.484646
5.461049	338.172214	7.489651
5.786657	341.949626	7.494656
5.501584	334.211238	7.499661
5.546920	333.194947	7.504666
5.460277	342.142800	7.509670
5.502219	336.700983	7.514675
5.678904	354.146744	7.519680
5.636158	339.122520	7.524685
5.928290	348.188571	7.529690
5.624255	351.636915	7.534694
5.465773	353.765467	7.539699
5.590609	346.403011	7.544704
5.825132	349.080973	7.549709
6.009211	344.407956	7.554714
5.863496	343.424574	7.559718
5.761104	347.648272	7.564723
5.855608	342.302672	7.569728
5.919895	346.506746	7.574733
5.758330	338.413772	7.579738
5.536715	338.302742	7.584742
5.751051	337.367705	7.589747
5.675464	340.590654	7.594752
5.321665	340.936799	7.599757
5.780096	336.078700	7.604762
5.540241	342.693432	7.609766
5.815445	336.022571	7.614771
5.826110	345.701915	7.619776
5.486739	353.844407	7.624781
5.549529	345.086915	7.629786
5.559641	344.227967	7.634790
5.601878	335.179454	7.639795
5.248436	337.828737	7.644800
5.625839	336.767072	7.649805
5.528500	333.472966	7.654810
5.465466	343.932569	7.659814
5.774781	335.016478	7.664819
5.365291	332.470157	7.669824
5.917396	343.805249	7.674829
5.789796	338.503722	7.679834
5.538432	341.829969	7.684838
5.366633	342.562225	7.689843
5.937565	351.603852	7.694848
5.757598	348.404865	7.699853
5.752874	342.286946	7.704858
5.521255	341.484617	7.709862
5.889665	342.455466	7.714867
5.488670	338.009584	7.719872
5.553917	345.899251	7.724877
5.821745	342.339482	7.729882
5.454550	342.308066	7.734886
5.586670	337.627321	7.739891
5.584128	343.964661	7.744896
5.363175	351.585682	7.749901
5.791757	368.909981	7.754906
5.652629	368.121724	7.759910
5.918648	366.454144	7.764915
5.880568	362.366201	7.769920
5.747363	344.986421	7.774925
5.703251	349.944522	7.779930
5.524650	350.481687	7.784934
5.785435	344.619819	7.789939
5.576132	343.168615	7.794944
5.499293	343.291306	7.799949
5.756042	339.894612	7.804954
5.849267	347.457224	7.809958
5.868501	339.567051	7.814963
5.725630	341.088900	7.819968
5.510497	347.418212	7.824973
5.664711	333.046692	7.829978
5.613160	329.596763	7.834982
5.974507	333.912769	7.839987
5.705640	338.608470	7.844992
5.480886	343.050533	7.849997
5.570506	341.865997	7.855002
5.363767	346.501408	7.860006
5.558435	342.642984	7.865011
5.550895	346.902534	7.870016
5.590238	338.034802	7.875021
5.621678	343.680322	7.880026
5.647100	348.855385	7.885030
5.563924	343.107182	7.890035
5.936334	347.722023	7.895040
5.771952	340.088227	7.900045
5.826107	336.957193	7.905050
5.380431	332.610017	7.910054
5.814813	332.729043	7.915059
5.822702	336.315477	7.920064
5.862196	334.477527	7.925069
5.813718	339.110441	7.930074
5.606467	341.319351	7.935078
5.431220	342.909515	7.940083
5.703986	338.959839	7.945088
5.226237	345.719177	7.950093
5.766734	334.128543	7.955098
5.683957	345.261931	7.960102
5.466955	332.042859	7.965107
5.535213	328.735626	7.970112
5.500152	347.501986	7.975117
5.769945	355.967247	7.980122
5.751704	360.049860	7.985139
5.788485	353.978952	7.990157
5.827349	342.880758	7.995174
5.757381	341.263329	8.000192
5.741603	340.521047	8.005210
5.454889	348.290735	8.010227
5.870354	339.724703	8.015245
5.239491	344.578499	8.020262
5.319108	347.892164	8.025280
5.866580	352.313202	8.030298
5.716250	363.027981	8.035315
5.766065	361.855783	8.040333
5.954433	365.313458	8.045350
5.857955	357.789602	8.050368
5.840114	344.396604	8.055386
5.583943	344.417552	8.060403
5.686078	335.815104	8.065421
5.560062	341.344498	8.070438
5.687997	349.961612	8.075456
6.366791	363.583044	8.080474
5.745547	354.787115	8.085491
5.304813	340.689982	8.090509
5.645794	345.600739	8.095526
5.774443	359.673880	8.100544
6.027989	357.081471	8.105562
5.921484	364.450740	8.110579
5.761390	343.506305	8.115597
5.609486	348.765190	8.120614
5.857710	353.807150	8.125632
6.445169	354.820163	8.130650
6.052001	349.248523	8.135667
5.809923	339.147082	8.140685
5.712715	340.396076	8.145702
5.589019	343.006126	8.150720
6.046844	334.884761	8.155738
5.522369	340.734957	8.160755
5.914706	341.863551	8.165773
6.077243	347.947595	8.170790
5.645821	345.335609	8.175808
5.781612	337.810311	8.180826
5.617269	347.302868	8.185843
5.565494	349.302146	8.190861
6.208908	357.548685	8.195878
5.973603	349.386915	8.200896
5.913154	350.238884	8.205914
5.504419	349.996421	8.210931
5.723111	359.473526	8.215949
6.272274	366.967919	8.220966
6.242109	362.308545	8.225984
5.774475	344.372002	8.231002
5.764841	345.963951	8.236019
6.029041	348.731348	8.241037
6.029984	347.235416	8.246054
5.998417	351.402642	8.251072
5.905038	344.992257	8.256090
5.533854	345.349833	8.261107
5.863013	355.841638	8.266125
5.919885	359.051553	8.271142
6.056269	364.966114	8.276160
5.943074	373.242103	8.281178
5.799589	371.124900	8.286195
5.568434	370.147920	8.291213
6.424565	367.174524	8.296230
5.888331	379.767059	8.301248
5.950796	376.522775	8.306266
6.070323	372.707899	8.311283
5.762128	369.243628	8.316301
6.152297	361.804940	8.321318
6.090040	367.564246	8.326336
6.145168	367.811268	8.331354
6.127397	369.331905	8.336371
6.013039	363.158299	8.341389
6.149502	362.032567	8.346406
6.084866	379.862654	8.351424
6.041352	374.801430	8.356442
5.952893	373.177411	8.361459
5.925323	372.361228	8.366477
5.893684	366.348303	8.371494
5.987840	370.262439	8.376512
5.595325	370.269903	8.381530
5.989838	365.755837	8.386547
5.806254	366.415549	8.391565
6.101142	365.445024	8.396582
6.007765	376.665317	8.401600
6.189745	372.682935	8.406618
6.163898	370.140336	8.411635
6.088488	363.493628	8.416653
6.204373	360.512416	8.421670
6.258936	366.190419	8.426688
6.662029	363.874513	8.431706
6.368498	369.792899	8.436723
6.143981	364.141349	8.441741
6.399069	358.465620	8.446758
6.085833	366.371982	8.451776
6.057766	361.387249	8.456794
6.150078	360.388307	8.461811
6.377317	364.818184	8.466829
6.658392	371.688474	8.471846
5.873997	357.995112	8.476864
6.102233	359.568960	8.481882
6.103401	362.784394	8.486899
5.850424	368.459790	8.491917
6.164060	365.693930	8.496934
5.861183	369.228090	8.501952
6.422804	358.689094	8.506970
5.930304	368.115996	8.511987
5.636542	373.636805	8.517005
6.300183	361.216927	8.522022
5.609747	370.800874	8.527040
5.850860	364.256356	8.532058
6.160290	387.967165	8.537075
6.364142	394.006925	8.542093
6.466005	380.787758	8.547110
6.045599	384.958730	8.552128
6.479144	388.838963	8.557146
6.142277	375.618684	8.562163
6.418152	390.306370	8.567181
6.548655	377.016478	8.572199
6.522730	375.919185	8.577216
6.282773	368.026362	8.582234
6.458470	364.997969	8.587251
6.281582	367.748843	8.592269
6.225300	368.868395	8.597287
6.222752	372.633494	8.602304
6.085011	371.503120	8.607322
6.128089	369.612479	8.612339
6.066966	381.705028	8.617357
6.614732	384.251564	8.622375
6.215482	398.586801	8.627392
6.414481	397.558623	8.632410
6.925816	397.696748	8.637427
6.409452	380.436758	8.642445
6.280235	361.828997	8.647463
6.259244	357.316512	8.652480
6.054395	366.525065	8.657498
6.382920	381.725232	8.662515
6.463441	389.683902	8.667533
6.649695	381.885652	8.672551
6.333144	380.076248	8.677568
6.218252	379.270505	8.682586
6.386595	382.346310	8.687603
6.360091	393.161743	8.692621
6.447599	389.727373	8.697639
6.265453	401.703085	8.702656
6.605467	393.928225	8.707674
6.754728	389.143082	8.712691
6.342469	383.902593	8.717709
6.596515	372.139744	8.722727
6.431825	367.267795	8.727744
6.237730	379.056012	8.732762
6.733856	375.630605	8.737779
6.210807	381.206049	8.742797
6.503435	383.034949	8.747815
6.478916	383.430066	8.752832
6.618838	383.559750	8.757850
6.785586	370.040167	8.762867
6.224938	372.099744	8.767885
6.200489	382.675021	8.772903
6.519052	388.122587	8.777920
6.560555	385.509543	8.782938
6.751922	397.594347	8.787955
6.624481	395.219035	8.792973
6.480283	382.915452	8.797991
6.271079	390.508995	8.803008
6.414752	393.030090	8.808026
6.660577	393.837531	8.813043
6.200783	398.500612	8.818061
6.932878	394.129629	8.823079
6.627241	394.148812	8.828096
6.556573	398.233778	8.833114
6.804510	392.237273	8.838131
6.656907	395.346493	8.843149
6.780161	400.423702	8.848167
6.712036	394.690991	8.853184
6.334118	392.168493	8.858202
6.606941	387.585010	8.863219
6.419977	388.551349	8.868237
6.582769	390.684475	8.873255
6.679176	394.399459	8.878272
6.791630	404.303366	8.883290
6.536347	396.952536	8.888307
6.540540	395.837929	8.893325
6.714176	387.038140	8.898343
6.828183	391.684460	8.903360
6.605559	395.149328	8.908378
6.893986	387.316234	8.913395
6.785638	388.907778	8.918413
6.568781	392.021468	8.923431
6.509737	387.912514	8.928448
6.721922	401.805432	8.933466
6.927214	394.641657	8.938483
6.251453	398.959684	8.943501
6.710513	389.661037	8.948519
7.036002	389.430484	8.953536
6.507420	397.468214	8.958554
6.932643	390.895021	8.963571
6.591687	401.765730	8.968589
6.887999	399.668408	8.973607
6.546253	398.355209	8.978624
6.417880	405.585895	8.983642
6.916974	405.688058	8.988659
6.662123	408.656195	8.993677
6.627115	392.176434	8.998695
6.913881	397.559529	9.003712
6.526440	396.878267	9.008730
6.684905	399.062559	9.013747
6.628272	390.992866	9.018765
6.483791	393.448377	9.023783
7.003454	401.449128	9.028800
6.749741	396.979178	9.033818
6.559258	393.370349	9.038835
6.466475	393.940189	9.043853
6.659372	396.942748	9.048871
7.023093	400.682383	9.053888
6.836387	410.162677	9.058906
6.590320	408.897694	9.063923
6.805538	414.572789	9.068941
7.068881	413.035997	9.073959
7.521363	407.865982	9.078976
6.873855	402.987148	9.083994
6.942153	389.798446	9.089011
6.938587	402.052453	9.094029
6.995384	389.929001	9.099047
6.859347	389.259087	9.104064
6.784756	396.459306	9.109082
7.198880	393.160267	9.114099
7.243104	396.290111	9.119117
6.881123	394.582449	9.124135
6.838615	396.113251	9.129152
6.624830	394.802220	9.134170
6.810916	401.965010	9.139187
6.964334	399.621704	9.144205
6.842778	388.485345	9.149223
6.764610	392.947002	9.154240
6.801183	406.646369	9.159258
7.193847	415.298033	9.164275
7.317483	410.150817	9.169293
7.090365	398.945684	9.174311
7.048916	394.916036	9.179328
6.853622	388.022908	9.184346
6.809362	389.617096	9.189363
6.763301	401.265519	9.194381
7.094579	412.252467	9.199399
7.421573	416.755184	9.204416
6.755238	412.538815	9.209434
7.210691	413.039075	9.214451
6.969662	413.310119	9.219469
6.894827	421.857857	9.224487
7.280703	416.988532	9.229504
6.883457	413.118413	9.234522
7.371212	412.244084	9.239539
7.287104	423.421939	9.244557
7.252657	404.098820	9.249575
6.988556	395.458695	9.254592
6.993080	396.262682	9.259610
7.280097	403.725325	9.264627
6.895572	400.651613	9.269645
7.160767	408.313306	9.274663
7.739970	412.511678	9.279680
7.127568	408.391050	9.284698
6.886980	407.781593	9.289715
7.512719	400.631246	9.294733
7.075091	396.660125	9.299751
7.163744	390.505392	9.304768
7.194718	397.768067	9.309786
7.265078	394.219606	9.314803
7.198829	396.347370	9.319821
7.120706	398.997668	9.324839
7.454925	390.340125	9.329856
6.973420	397.988691	9.334874
7.147586	398.883025	9.339891
6.938968	394.122045	9.344909
7.142610	394.131359	9.349927
7.286578	393.051793	9.354944
7.065383	401.830583	9.359962
7.374907	409.012025	9.364979
7.389913	418.962669	9.369997
7.146179	410.019577	9.375015
7.166861	396.573207	9.380032
7.332308	411.035118	9.385050
7.327661	414.267244	9.390067
7.203179	412.853948	9.395085
7.354712	414.711131	9.400103
6.992601	415.843591	9.405120
7.241288	419.531715	9.410138
7.136930	416.581630	9.415155
7.317705	421.034534	9.420173
7.002310	417.341010	9.425191
7.462721	416.527740	9.430208
7.271247	418.769674	9.435226
7.444924	420.642344	9.440243
7.562816	415.369794	9.445261
7.676551	417.119258	9.450279
7.665026	418.623149	9.455296
7.398747	419.497701	9.460314
7.466576	412.838140	9.465331
7.467865	406.349880	9.470349
6.852771	404.602734	9.475367
7.190258	404.894153	9.480384
7.356953	412.987733	9.485402
7.385173	418.016631	9.490419
7.527397	418.704510	9.495437
7.280843	425.294068	9.500455
7.305038	415.577142	9.505472
7.533266	424.481621	9.510490
7.511662	419.044604	9.515507
7.420431	423.391542	9.520525
7.323307	422.750281	9.525543
7.260379	416.947329	9.530560
7.168816	422.818508	9.535578
7.319851	419.219613	9.540595
7.536735	423.285060	9.545613
7.365975	427.972571	9.550631
7.397819	412.848789	9.555648
7.508338	413.289150	9.560666
7.362082	418.001245	9.565683
7.422747	406.315818	9.570701
7.552726	418.160896	9.575719
7.196493	417.859767	9.580736
7.331182	429.315971	9.585754
7.593914	420.830483	9.590771
7.549140	434.204880	9.595789
7.587858	439.314197	9.600807
7.636222	438.034927	9.605824
7.551894	449.222300	9.610842
7.616348	439.420200	9.615859
7.676894	433.563306	9.620877
7.725228	440.088023	9.625895
7.597524	429.634222	9.630912
7.956831	428.009906	9.635930
7.526574	426.499056	9.640947
7.438184	420.002664	9.645965
7.392815	427.255148	9.650983
7.624194	427.279077	9.656000
7.298624	433.612709	9.661018
7.522669	435.398647	9.666035
8.043890	429.965470	9.671053
7.575679	438.981545	9.676071
8.006288	437.128386	9.681088
8.006235	448.807545	9.686106
7.514895	436.122491	9.691123
7.500351	435.061290	9.696141
7.631791	439.682820	9.701159
7.721467	434.493548	9.706176
7.970700	445.262927	9.711194
7.799616	445.005550	9.716211
8.043117	434.121581	9.721229
7.931601	436.884376	9.726247
8.021638	426.242047	9.731264
7.805121	421.791545	9.736282
7.497941	419.302209	9.741299
7.708590	413.901613	9.746317
7.750658	427.366621	9.751335
7.775623	413.957439	9.756352
7.621590	420.460010	9.761370
7.347900	421.963695	9.766387
8.172931	420.128020	9.771405
7.654371	426.179286	9.776423
7.365532	427.442343	9.781440
7.974716	426.306121	9.786458
7.622366	439.744188	9.791475
7.943779	441.215178	9.796493
8.038596	437.359956	9.801511
8.043181	444.923392	9.806528
8.166347	434.695605	9.811546
7.721592	440.672270	9.816563
7.791002	432.573468	9.821581
8.086382	429.763105	9.826599
7.993042	418.972614	9.831616
7.792697	422.610736	9.836634
7.804592	424.587487	9.841651
7.549631	425.624373	9.846669
7.993568	436.256138	9.851687
7.639379	430.574266	9.856704
7.880853	433.635538	9.861722
7.786872	436.600722	9.866739
8.241041	418.167148	9.871757
8.118534	433.450206	9.876775
7.894895	440.231854	9.881792
8.125054	439.255625	9.886810
7.923694	445.352180	9.891827
8.268953	437.844717	9.896845
7.931390	429.020361	9.901863
8.043553	422.300247	9.906880
8.522522	432.983358	9.911898
7.918715	428.870853	9.916915
7.469604	417.324747	9.921933
7.530142	429.979030	9.926951
7.912113	432.062257	9.931968
7.861376	435.856962	9.936986
7.533090	439.448739	9.942003
7.815736	439.739230	9.947021
8.027821	431.037570	9.952039
7.955733	432.367862	9.957056
7.771376	431.989481	9.962074
7.871393	443.539452	9.967091
8.297484	452.012368	9.972109
8.105465	460.934961	9.977127
8.058221	456.451783	9.982144
8.533600	457.539055	9.987162
7.918664	443.857111	9.992179
7.851995	438.221985	9.997197
7.819044	451.607177	10.002215
8.226466	454.405939	10.007232
8.446380	458.865381	10.012250
8.072601	465.263333	10.017267
8.430175	457.643495	10.022285
8.061873	456.530079	10.027303
8.069721	453.698211	10.032320
8.333465	454.373483	10.037338
8.257125	454.315941	10.042355
8.600496	452.735128	10.047373
8.275019	446.405023	10.052391
7.842147	441.091989	10.057408
8.169308	441.820500	10.062426
8.039849	458.963355	10.067443
8.332583	453.704595	10.072461
8.576203	453.335315	10.077479
8.537552	453.174078	10.082496
8.362063	441.938790	10.087514
7.680517	437.169384	10.092531
8.200800	448.237375	10.097549
8.230175	455.257335	10.102567
8.115521	454.404216	10.107584
8.559460	452.990775	10.112602
8.141817	464.100671	10.117619
8.353885	458.444230	10.122637
8.548143	471.633122	10.127655
8.566830	472.930350	10.132672
8.810165	465.820582	10.137690
8.419356	460.684023	10.142707
8.308184	439.100723	10.147725
8.163688	437.283459	10.152743
7.961398	445.242007	10.157760
8.391985	436.550504	10.162778
8.113248	452.877185	10.167795
8.400518	462.848577	10.172813
8.306590	454.522741	10.177831
8.207099	464.636398	10.182848
8.541734	462.892850	10.187866
8.351727	465.639470	10.192883
8.404256	456.031714	10.197901
8.087553	459.252477	10.202919
8.157383	466.228274	10.207936
8.482305	456.811628	10.212954
8.498525	460.892547	10.217971
8.716553	460.091768	10.222989
8.499013	461.125985	10.228007
8.377114	463.148817	10.233024
8.826212	458.301194	10.238042
8.356298	456.957455	10.243059
8.383192	464.208170	10.248077
8.505919	453.996218	10.253095
8.314095	462.527477	10.258112
8.250506	461.486534	10.263130
8.187176	463.796881	10.268147
8.105864	466.371949	10.273165
8.815680	483.775460	10.278183
8.839362	482.395892	10.283200
9.008656	478.412305	10.288218
8.539985	475.010867	10.293235
8.435700	470.624927	10.298253
8.436635	460.971555	10.303271
8.581740	471.384791	10.308288
8.798561	475.150470	10.313306
8.501778	474.231036	10.318323
8.663484	470.368548	10.323341
8.959082	466.264318	10.328359
8.351747	462.755089	10.333376
8.709427	469.979549	10.338394
8.701950	481.022438	10.343411
8.823876	480.586901	10.348429
8.618601	476.447047	10.353447
8.285944	469.852974	10.358464
8.921504	484.361666	10.363482
8.674990	490.007693	10.368499
8.627640	487.026630	10.373517
9.132776	490.971475	10.378535
8.683121	476.635791	10.383552
8.879401	466.425003	10.388570
8.731571	462.241496	10.393587
8.347857	461.840507	10.398605
8.571751	469.524436	10.403623
8.680302	490.675846	10.408640
9.163590	485.841826	10.413658
9.033001	490.188597	10.418675
8.734927	484.968168	10.423693
8.887632	477.601117	10.428711
8.566937	481.062337	10.433728
9.121707	488.540129	10.438746
8.897897	487.060245	10.443763
8.849479	477.613356	10.448781
8.767814	464.978101	10.453799
8.622091	475.076873	10.458816
8.856141	480.944709	10.463834
8.751986	490.061912	10.468851
8.697792	487.435351	10.473869
8.847054	486.093033	10.478887
8.718446	484.759265	10.483904
9.042649	482.373580	10.488922
8.705605	487.992678	10.493939
8.722267	485.168900	10.498957
8.823029	490.498936	10.503975
8.855092	492.573536	10.508992
9.259005	481.746610	10.514010
9.119398	485.204882	10.519027
9.199231	493.681238	10.524045
9.275770	486.379689	10.529063
9.210802	490.675219	10.534080
9.036990	487.268894	10.539098
8.977172	487.716844	10.544115
8.763144	486.459490	10.549133
9.243953	488.732455	10.554151
8.903507	495.563867	10.559168
9.206892	489.221039	10.564186
8.947710	485.360965	10.569203
8.793880	482.424882	10.574221
8.842290	484.064608	10.579239
8.933087	480.077464	10.584256
8.998004	476.662373	10.589274
8.608469	487.042100	10.594291
8.901068	488.937286	10.599309
9.078244	480.802748	10.604327
8.721516	487.078136	10.609344
8.846466	483.174033	10.614362
9.158339	484.375123	10.619379
8.954341	500.046452	10.624397
9.079329	492.197735	10.629415
9.199570	501.582951	10.634432
9.434488	503.995185	10.639450
9.339517	500.336750	10.644467
9.117917	494.864579	10.649485
9.379185	487.591070	10.654503
8.842665	493.856585	10.659520
9.182537	484.223010	10.664538
9.379399	496.076661	10.669555
9.075225	494.451504	10.674573
9.383474	489.565844	10.679591
9.161147	491.140430	10.684608
9.085467	494.494080	10.689626
9.070533	495.932238	10.694643
9.034583	511.444874	10.699661
9.394577	506.731027	10.704679
9.252233	513.941842	10.709696
9.481873	511.425714	10.714714
9.636831	505.576186	10.719731
9.684057	501.412792	10.724749
9.266579	482.079799	10.729767
8.967662	490.157549	10.734784
9.043352	500.468006	10.739802
9.307807	507.896337	10.744819
9.285842	506.621701	10.749837
9.401579	508.241479	10.754855
9.099319	520.425313	10.759872
9.558922	509.624412	10.764890
9.469556	517.123614	10.769907
9.481056	515.158982	10.774925
9.656649	514.923365	10.779943
9.512212	514.276844	10.784960
9.313228	507.876531	10.789978
9.431589	513.711900	10.794995
9.358127	513.057484	10.800013
9.902002	507.491373	10.805031
9.178254	507.108612	10.810048
9.343562	504.646681	10.815066
9.434522	501.192818	10.820083
8.962146	505.198347	10.825101
9.297734	505.852967	10.830119
9.109102	501.117248	10.835136
9.747976	507.714141	10.840154
9.331381	504.680115	10.845171
9.369206	507.703682	10.850189
9.741474	500.381329	10.855207
9.232420	506.339627	10.860224
9.373028	511.553016	10.865242
9.492057	505.728017	10.870259
9.299922	514.881020	10.875277
9.386836	510.916564	10.880295
9.603584	512.246071	10.885312
9.667817	511.491324	10.890330
9.506093	508.856257	10.895347
9.634654	514.077834	10.900365
9.838325	509.303122	10.905383
9.904701	507.702318	10.910400
9.701517	514.433474	10.915418
9.644886	504.205239	10.920435
9.183284	519.784155	10.925453
9.549159	507.609345	10.930471
10.104400	518.454195	10.935488
9.614367	511.316585	10.940506
9.760535	518.315230	10.945523
9.438614	514.332379	10.950541
9.633296	515.491759	10.955559
9.716375	533.390516	10.960576
9.695099	537.190123	10.965594
9.850653	537.891710	10.970611
10.052037	533.821066	10.975629
9.894740	527.922322	10.980647
10.292739	513.012835	10.985664
9.817237	517.246063	10.990682
9.905291	513.152045	10.995699
9.703365	516.506420	11.000717
9.622330	505.622446	11.005735
9.646065	506.716926	11.010752
9.797420	511.515247	11.015770
9.513900	509.445077	11.020787
9.647560	522.532992	11.025805
10.175206	510.711676	11.030823
10.134739	520.203972	11.035840
9.580948	514.982324	11.040858
9.702301	511.391188	11.045875
9.505178	530.087777	11.050893
9.796947	535.365998	11.055911
9.863457	531.347911	11.060928
9.883724	536.368613	11.065946
10.312883	537.854392	11.070963
10.045396	545.008967	11.075981
10.025167	532.951058	11.080999
9.899565	526.031247	11.086016
10.274771	536.061569	11.091034
10.144075	532.878888	11.096051
9.959608	523.683523	11.101069
9.988222	513.300004	11.106087
9.816074	508.284016	11.111104
9.841293	515.875826	11.116122
10.058996	520.029526	11.121139
9.943436	535.179050	11.126157
10.260062	535.480031	11.131175
10.219726	542.558215	11.136192
10.374169	514.940808	11.141210
10.037194	511.815493	11.146227
9.932358	507.240287	11.151245
9.891541	507.107789	11.156263
9.783455	512.902678	11.161280
9.777698	527.817357	11.166298
10.398786	535.149150	11.171315
10.236054	532.378541	11.176333
10.292728	536.418466	11.181351
10.506286	536.388368	11.186368
9.613629	524.119172	11.191386
10.134351	527.007599	11.196403
9.968864	539.640349	11.201421
10.170019	537.747168	11.206439
10.494636	540.991166	11.211456
10.315634	544.092678	11.216474
10.135699	535.294218	11.221491
10.160379	537.079650	11.226509
10.379748	533.170302	11.231527
10.374976	530.201537	11.236544
10.365723	530.171418	11.241562
10.415339	531.981367	11.246579
9.970377	519.437350	11.251597
9.941552	529.732539	11.256615
9.961159	530.480538	11.261632
10.194786	541.927722	11.266650
10.453125	533.203032	11.271667
10.192068	536.531906	11.276685
10.523405	529.777626	11.281703
10.687973	531.806355	11.286720
10.242558	534.791560	11.291738
10.362821	532.522825	11.296755
10.346649	543.750137	11.301773
10.368551	539.477071	11.306791
10.436038	542.537049	11.311808
10.401492	540.617452	11.316826
10.620460	544.392278	11.321843
10.351379	544.412080	11.326861
10.545975	537.142620	11.331879
10.561369	532.551845	11.336896
10.377764	531.955601	11.341914
10.459031	522.939761	11.346931
10.421098	529.083481	11.351949
10.305030	529.764244	11.356967
10.416321	532.104214	11.361984
10.226552	533.512795	11.367002
10.555322	534.042251	11.372019
10.640653	533.675524	11.377037
10.711479	530.057539	11.382055
10.607570	540.402293	11.387072
10.258062	535.672678	11.392090
10.411381	536.541864	11.397107
10.418331	537.657894	11.402125
10.240009	541.548222	11.407143
10.441315	535.483193	11.412160
10.009707	542.685410	11.417178
10.426776	527.488929	11.422195
10.282564	542.734436	11.427213
9.892600	544.934709	11.432231
10.533336	555.125665	11.437248
10.451388	567.142689	11.442266
10.820878	552.474285	11.447283
10.766922	553.672380	11.452301
10.735849	555.128834	11.457319
11.029966	560.015390	11.462336
10.743962	556.888443	11.467354
10.986347	555.553710	11.472371
10.903945	558.586538	11.477389
10.795433	562.652188	11.482407
11.007021	545.916147	11.487424
10.366834	544.867146	11.492442
10.812905	555.975161	11.497459
10.829806	546.221430	11.502477
10.685877	551.008935	11.507495
11.096608	551.500384	11.512512
10.654807	548.116838	11.517530
10.933192	544.034204	11.522547
10.475827	542.530720	11.527565
10.485497	554.549250	11.532583
10.944584	550.810851	11.537600
10.949293	561.567881	11.542618
10.748054	556.234527	11.547635
10.889434	553.454434	11.552653
10.710529	561.522998	11.557671
10.801560	560.508466	11.562688
10.920991	553.020336	11.567706
10.914152	550.742987	11.572723
11.039052	553.825585	11.577741
10.900722	548.274163	11.582759
11.079687	551.190558	11.587776
10.977405	555.700190	11.592794
11.012981	552.898702	11.597811
11.087698	550.103743	11.602829
10.950580	552.450835	11.607847
11.145484	541.555433	11.612864
10.983688	555.838046	11.617882
10.953727	557.650922	11.622899
11.045138	561.038526	11.627917
10.676307	558.820692	11.632935
11.033448	557.670057	11.637952
10.943445	562.998259	11.642970
11.170297	561.760616	11.647987
11.047679	550.163589	11.653005
10.896899	563.920649	11.658023
11.035041	546.110484	11.663040
10.851527	560.383860	11.668058
11.014000	561.873294	11.673075
11.074514	556.082635	11.678093
11.099180	563.488365	11.683111
10.747544	553.119848	11.688128
10.189657	558.669214	11.693146
10.666461	568.529107	11.698163
11.119877	585.593955	11.703181
11.117560	582.877255	11.708199
11.335708	580.119918	11.713216
11.211666	588.577570	11.718234
11.118921	582.615110	11.723251
11.508755	581.030208	11.728269
11.169996	594.800781	11.733287
11.353824	588.852060	11.738304
11.269115	581.013863	11.743322
11.447522	588.487183	11.748339
11.574690	594.775628	11.753357
11.086222	593.964925	11.758375
11.161880	589.285859	11.763392
11.071257	589.833279	11.768410
10.907308	590.354247	11.773427
11.065531	583.570099	11.778445
11.423547	593.571573	11.783463
11.588367	580.045820	11.788480
11.106080	584.936505	11.793498
11.159241	588.260645	11.798515
11.508645	581.506689	11.803533
11.294053	578.791483	11.808551
11.300007	584.047949	11.813568
11.256566	576.260131	11.818586
11.397278	575.247330	11.823603
11.832600	570.004204	11.828621
11.504438	572.904890	11.833639
11.639599	578.693484	11.838656
11.486282	585.480017	11.843674
11.390091	581.676593	11.848691
11.679969	587.302251	11.853709
10.985307	584.223146	11.858727
11.299583	589.226488	11.863744
11.172288	583.973129	11.868762
11.476629	598.953192	11.873779
11.967352	601.628558	11.878797
11.584646	603.499515	11.883815
11.962586	588.713005	11.888832
11.496881	587.968184	11.893850
11.546294	586.313211	11.898867
11.716787	577.785207	11.903885
11.226664	587.164518	11.908903
11.490266	589.423979	11.913920
11.495253	602.636126	11.918938
11.865838	604.708524	11.923955
11.983718	604.627053	11.928973
11.597378	591.398537	11.933991
11.585944	583.687781	11.939008
11.542292	599.977995	11.944026
11.705575	607.160197	11.949043
11.919360	606.249623	11.954061
11.935476	610.109693	11.959079
11.484943	588.055202	11.964096
11.843929	596.118927	11.969114
11.825955	602.777100	11.974131
11.817460	599.079935	11.979149
11.740500	602.840890	11.984167
12.045035	598.078852	11.989184
11.529341	595.798674	11.994202
11.519438	601.370029	11.999219
12.145061	609.966583	12.004237
11.836978	612.280344	12.009255
11.917118	606.811650	12.014272
12.038294	610.030533	12.019290
11.731643	609.911022	12.024307
11.856438	604.170296	12.029325
11.527550	612.823951	12.034343
11.550117	610.665087	12.039360
11.751876	607.137150	12.044378
11.695665	612.412770	12.049395
11.769546	611.719632	12.054413
11.810229	611.609156	12.059431
12.107177	613.418474	12.064448
11.832759	611.634044	12.069466
11.579458	619.663726	12.074483
11.958744	606.054070	12.079501
12.008970	616.538967	12.084519
12.304712	607.426577	12.089536
12.042587	604.712456	12.094554
11.965449	605.819492	12.099571
12.130994	608.908394	12.104589
11.879420	614.343816	12.109607
12.077409	606.742451	12.114624
12.000873	612.664999	12.119642
11.861750	614.722087	12.124659
12.385890	607.773663	12.129677
11.927063	617.788725	12.134695
11.973378	612.868077	12.139712
12.096743	620.741287	12.144730
12.068449	629.543802	12.149747
12.793013	624.362920	12.154765
12.531983	622.898286	12.159783
12.085900	607.855061	12.164800
12.213817	607.055683	12.169818
12.194340	609.406556	12.174835
12.510346	614.393858	12.179853
12.180843	603.630557	12.184871
12.051427	606.487681	12.189888
11.978654	616.928614	12.194906
11.845194	613.680079	12.199923
12.093127	618.027905	12.204941
12.252143	621.272456	12.209959
12.681023	623.755489	12.214976
12.822672	628.182980	12.219994
12.190083	611.067089	12.225011
11.976514	606.303666	12.230029
11.990648	612.836927	12.235047
12.521722	621.271489	12.240064
12.358059	626.809988	12.245082
12.505036	632.195986	12.250099
12.549011	629.803420	12.255117
12.535214	624.235740	12.260135
12.369369	632.419064	12.265152
12.617934	631.203281	12.270170
12.394755	633.185099	12.275187
12.717074	623.825572	12.280205
12.078838	626.178115	12.285223
12.109061	627.202167	12.290240
12.227825	631.803630	12.295258
12.578324	636.627782	12.300275
12.546616	633.331844	12.305293
12.527118	636.585257	12.310311
12.561941	637.873673	12.315328
12.735734	636.511746	12.320346
12.689858	644.345047	12.325363
12.757968	638.849815	12.330381
12.523026	630.804620	12.335399
12.263002	628.620327	12.340416
12.442657	636.181832	12.345434
12.390037	633.845329	12.350451
12.301275	638.842012	12.355469
12.530323	635.795800	12.360487
12.289751	638.152699	12.365504
12.766657	633.193405	12.370522
12.417044	636.409856	12.375539
12.680074	640.244112	12.380557
12.598516	648.038791	12.385575
12.500795	657.189790	12.390592
12.774733	658.996384	12.395610
13.040411	657.534944	12.400627
12.983088	660.305116	12.405645
12.887013	650.676212	12.410663
12.793069	639.368144	12.415680
12.595884	641.838206	12.420698
12.688466	657.510832	12.425715
12.751363	656.418627	12.430733
12.686929	663.516389	12.435751
12.591052	668.116567	12.440768
13.170530	655.883154	12.445786
12.977710	659.084664	12.450803
12.829093	658.189487	12.455821
13.214394	658.795350	12.460839
13.041168	667.973889	12.465856
13.012096	640.908708	12.470874
12.868349	640.596580	12.475891
12.689079	633.905983	12.480909
13.071877	642.956914	12.485927
12.829990	653.534649	12.490944
13.246339	650.112144	12.495962
13.038662	661.520821	12.500979
13.225624	651.459696	12.505997
13.317186	643.363660	12.511015
12.924875	633.039297	12.516032
13.142003	634.479204	12.521050
12.725966	641.928337	12.526067
12.668736	632.466960	12.531085
13.070553	644.774778	12.536103
12.967730	659.395421	12.541120
13.381619	654.013601	12.546138
13.092357	663.847658	12.551155
13.242742	666.718031	12.556173
13.434497	651.370338	12.561191
13.166904	644.535703	12.566208
13.186867	631.237586	12.571226
12.934070	633.523807	12.576243
13.156846	647.756085	12.581261
13.201678	649.241753	12.586279
12.911998	653.029527	12.591296
13.173702	657.798084	12.596314
13.112943	661.846854	12.601331
13.241365	655.736329	12.606349
13.416070	659.003690	12.611367
13.386822	652.078295	12.616384
13.308418	654.854903	12.621402
13.383267	665.560050	12.626419
13.256374	658.208056	12.631437
13.656418	649.546451	12.636455
13.386568	664.858958	12.641472
13.695396	650.225165	12.646490
13.144703	660.295578	12.651507
13.282397	656.288471	12.656525
13.283523	653.997245	12.661543
13.274765	657.277391	12.666560
13.253008	655.586157	12.671578
13.178020	657.983549	12.676595
13.103297	660.279916	12.681613
13.564285	665.654902	12.686631
13.072131	667.902657	12.691648
13.098563	658.444019	12.696666
13.203715	667.042744	12.701683
13.220598	678.400689	12.706701
13.902554	681.879403	12.711719
13.706388	678.867831	12.716736
13.603460	673.481266	12.721754
13.270534	672.999783	12.726771
13.704795	677.201851	12.731789
13.837456	678.099507	12.736807
13.278000	675.583142	12.741824
13.326968	674.821299	12.746842
13.251289	688.923358	12.751859
13.221496	688.678692	12.756877
13.474494	685.480423	12.761895
13.639419	683.791679	12.766912
13.463592	678.814083	12.771930
13.872591	685.793962	12.776947
13.812680	685.566608	12.781965
13.966243	675.630588	12.786983
13.359266	682.128039	12.792000
13.683860	687.148736	12.797018
13.704348	684.415847	12.802035
13.274110	681.551168	12.807053
13.851188	671.539743	12.812071
13.701103	674.870298	12.817088
13.800437	676.609408	12.822106
14.058886	679.286237	12.827123
13.795060	679.109566	12.832141
13.829694	682.067390	12.837159
13.118885	685.889181	12.842176
13.483848	691.039290	12.847194
13.564047	703.949476	12.852211
14.066700	707.292014	12.857229
13.823271	705.035702	12.862247
13.700733	703.167656	12.867264
14.321917	706.031004	12.872282
14.536456	703.618184	12.877299
14.181894	715.434762	12.882317
14.403720	702.319752	12.887335
14.144532	696.307431	12.892352
14.120828	687.326786	12.897370
13.831520	680.044250	12.902387
13.810352	678.895706	12.907405
14.275415	685.585997	12.912423
14.177379	690.202296	12.917440
14.174515	677.393679	12.922458
13.939888	686.351420	12.927475
13.924102	692.075193	12.932493
14.389800	691.475678	12.937511
13.996747	690.804745	12.942528
13.930123	688.946929	12.947546
14.251525	706.805598	12.952563
14.651678	709.113240	12.957581
14.155084	692.708224	12.962599
13.922441	685.653542	12.967616
14.291668	690.881881	12.972634
14.292044	698.692226	12.977651
13.986932	710.542126	12.982669
14.202103	705.143894	12.987687
14.015801	703.052253	12.992704
14.180362	705.532271	12.997722
13.849705	708.253491	13.002739
14.088635	710.826070	13.007757
14.151665	703.444486	13.012775
14.180329	712.320223	13.017792
13.957424	698.693805	13.022810
14.213862	697.221179	13.027827
14.410382	700.305274	13.032845
14.481439	702.679933	13.037863
14.347870	701.798190	13.042880
14.162454	705.244702	13.047898
14.515723	712.709783	13.052915
14.383048	728.534305	13.057933
14.522704	728.777639	13.062951
14.660267	727.613845	13.067968
14.524853	720.957411	13.072986
14.553380	718.062323	13.078003
14.542994	721.588881	13.083021
14.325812	712.430068	13.088039
14.650384	717.930448	13.093056
14.767217	728.117869	13.098074
14.939691	717.784415	13.103091
14.385891	715.563802	13.108109
14.816443	710.842072	13.113127
14.548628	707.888986	13.118144
14.177802	701.906668	13.123162
14.490097	710.880250	13.128179
14.813015	728.290593	13.133197
15.044163	724.492976	13.138215
15.111112	718.739131	13.143232
14.561439	712.566909	13.148250
14.265770	707.251368	13.153267
14.540820	720.172252	13.158285
15.065783	716.754914	13.163303
14.998049	714.534360	13.168320
14.921470	706.776890	13.173338
14.857211	699.759101	13.178355
14.506605	708.394092	13.183373
14.539726	701.471590	13.188391
14.888387	713.421669	13.193408
14.867380	722.705921	13.198426
15.109983	714.062486	13.203443
14.728864	723.071455	13.208461
14.464149	709.186459	13.213479
14.667924	726.151458	13.218496
14.857686	731.568692	13.223514
15.329570	728.064945	13.228531
14.992913	738.909943	13.233549
14.785187	725.034996	13.238567
14.853628	725.330442	13.243584
15.158966	729.293826	13.248602
14.762555	719.850498	13.253619
14.811098	720.799122	13.258637
15.040651	721.479728	13.263655
15.012824	722.465487	13.268672
14.587412	731.882134	13.273690
15.142909	713.852191	13.278707
14.967429	723.233076	13.283725
15.002838	720.340071	13.288743
15.051595	729.461990	13.293760
15.051982	728.647749	13.298778
15.093260	722.187861	13.303795
14.651760	727.217398	13.308813
14.981271	730.151408	13.313831
15.161410	736.318049	13.318848
15.034392	749.001760	13.323866
15.391969	736.670301	13.328883
15.680226	745.117481	13.333901
15.623839	747.732889	13.338919
15.447805	728.112734	13.343936
15.251187	734.606272	13.348954
15.278121	727.583740	13.353971
14.843523	726.550053	13.358989
15.140214	733.184529	13.364007
15.271563	731.545187	13.369024
15.179865	748.865473	13.374042
15.730151	749.862208	13.379059
15.642271	743.630700	13.384077
15.543216	732.648408	13.389095
15.198682	730.855948	13.394112
15.268019	733.230878	13.399130
15.383981	732.256635	13.404147
15.693615	744.837646	13.409165
15.470196	736.538150	13.414183
15.071745	738.054974	13.419200
15.308578	750.416955	13.424218
15.465552	752.156565	13.429235
15.310506	752.502586	13.434253
15.412878	747.308092	13.439271
15.819398	745.057875	13.444288
15.753410	753.541280	13.449306
15.684600	759.065052	13.454323
15.440024	759.096817	13.459341
15.907161	752.614793	13.464359
15.500381	755.303692	13.469376
15.449260	754.270257	13.474394
15.794198	756.463429	13.479411
15.392075	755.430996	13.484429
15.484239	752.585953	13.489447
15.534665	752.347731	13.494464
15.477331	748.254205	13.499482
15.395632	746.865779	13.504499
15.531533	742.574915	13.509517
15.782961	747.685915	13.514535
16.023876	738.979617	13.519552
15.916825	746.570029	13.524570
16.111451	738.391633	13.529587
15.639041	747.165525	13.534605
15.357297	742.387435	13.539623
15.398900	747.752005	13.544640
15.519745	760.668526	13.549658
16.062388	773.083892	13.554675
16.306612	769.804926	13.559693
16.223738	769.906187	13.564711
16.244887	757.248405	13.569728
16.205219	752.233811	13.574746
15.769902	741.019853	13.579763
15.667908	747.530220	13.584781
15.576189	751.126250	13.589799
16.267888	757.071243	13.594816
16.473175	769.725321	13.599834
16.218213	753.535086	13.604851
16.030805	743.756254	13.609869
15.892083	750.165045	13.614887
15.829731	741.913051	13.619904
15.777221	760.432735	13.624922
16.017048	763.368092	13.629939
16.143590	771.774193	13.634957
16.625550	767.479935	13.639975
16.504641	758.050496	13.644992
16.306521	743.886866	13.650010
16.284308	732.782160	13.655027
16.360216	731.908825	13.660045
16.224948	734.852086	13.665063
16.495991	732.133826	13.670080
16.160774	736.654524	13.675098
16.467368	729.938735	13.680115
16.402864	726.849852	13.685133
16.344585	734.110782	13.690151
16.411119	727.467083	13.695168
16.134401	738.012422	13.700186
16.261528	731.485516	13.705203
16.189850	731.130609	13.710221
16.236067	736.731137	13.715239
16.573737	730.234566	13.720256
16.350777	736.069502	13.725274
16.298239	733.568876	13.730291
16.278987	740.202054	13.735309
16.516619	757.849761	13.740327
16.894497	754.818225	13.745344
16.680327	748.666336	13.750362
16.234234	737.495083	13.755379
16.915556	737.098674	13.760397
16.146185	740.591932	13.765415
16.490958	739.676735	13.770432
16.181681	746.516013	13.775450
16.566816	753.919347	13.780467
16.686468	761.051601	13.785485
16.631353	760.261779	13.790503
16.726384	753.405355	13.795520
16.723715	754.399823	13.800538
16.450494	753.221091	13.805555
16.946262	754.863772	13.810573
16.845762	758.814613	13.815591
16.877468	752.141614	13.820608
16.414923	751.506744	13.825626
16.776325	754.757678	13.830643
17.090509	747.917626	13.835661
16.690273	759.451018	13.840679
16.770080	749.920906	13.845696
16.684629	750.442280	13.850714
16.855801	762.072896	13.855731
17.025129	764.056730	13.860749
16.538174	763.633938	13.865767
16.960466	751.352351	13.870784
16.965837	757.776579	13.875802
16.946927	758.132962	13.880819
17.445969	756.673050	13.885837
16.857509	754.505164	13.890855
16.660596	748.249606	13.895872
16.624806	752.256640	13.900890
16.936877	757.815782	13.905907
17.277571	752.587336	13.910925
16.964954	759.651196	13.915943
17.108744	747.760103	13.920960
17.057334	758.055785	13.925978
17.073965	752.284517	13.930995
17.100894	762.047309	13.936013
17.014416	754.300827	13.941031
17.113518	747.042994	13.946048
17.100580	759.544853	13.951066
17.118321	756.714553	13.956083
16.973239	756.484679	13.961101
16.911154	763.184494	13.966119
16.995397	753.814631	13.971136
17.162688	756.000749	13.976154
16.914670	759.901976	13.981171
17.065073	751.989228	13.986189
17.086196	764.334313	13.991207
17.263596	775.553722	13.996224
17.067776	777.865804	14.001242
17.286318	785.519146	14.006259
17.247956	777.891392	14.011277
17.417184	789.541262	14.016295
17.619375	779.569211	14.021312
17.369707	786.339264	14.026330
17.420283	789.673311	14.031347
17.776268	783.975427	14.036365
17.508505	783.060925	14.041383
17.648636	775.474808	14.046400
17.533312	785.414391	14.051418
17.598223	785.028749	14.056435
17.719972	766.031204	14.061453
17.019019	756.565847	14.066471
17.712598	766.073371	14.071488
17.999762	774.994096	14.076506
17.548014	766.954193	14.081523
17.503880	752.804450	14.086541
17.377601	762.717325	14.091559
17.647220	775.755857	14.096576
17.963370	777.461219	14.101594
17.510565	782.719744	14.106611
18.182387	769.932245	14.111629
17.724579	761.107511	14.116647
17.595383	753.623294	14.121664
17.474198	748.185902	14.126682
17.370004	761.673936	14.131699
17.425837	777.292430	14.136717
17.553340	775.177168	14.141735
18.090512	773.165376	14.146752
17.997963	774.978551	14.151770
17.769210	775.620064	14.156787
17.830215	770.141676	14.161805
17.857359	773.454123	14.166823
18.076267	776.077165	14.171840
18.139593	772.838986	14.176858
18.211104	781.619726	14.181875
17.894295	774.268850	14.186893
17.871362	777.510201	14.191911
17.889688	779.100991	14.196928
17.645802	768.715571	14.201946
18.175207	768.904534	14.206963
18.040345	769.310528	14.211981
18.028018	782.310914	14.216999
17.779328	773.358943	14.222016
17.601204	779.852773	14.227034
17.502168	780.013353	14.232051
17.968874	775.263887	14.237069
17.729936	782.511939	14.242087
18.067257	781.449581	14.247104
18.096733	798.164082	14.252122
18.152130	800.891480	14.257139
18.482077	795.222891	14.262157
18.126372	799.418598	14.267175
18.185712	792.968495	14.272192
18.300171	793.282023	14.277210
18.132786	797.224352	14.282227
18.165372	792.662390	14.287245
18.418384	791.171355	14.292263
18.431818	784.479099	14.297280
18.408382	794.319176	14.302298
18.156988	798.517577	14.307315
18.500991	790.546268	14.312333
18.668832	793.786321	14.317351
18.656257	790.935489	14.322368
18.802805	787.293039	14.327386
18.263194	784.205536	14.332403
18.368300	778.707656	14.337421
18.557872	784.080756	14.342439
18.641806	791.246986	14.347456
18.645787	790.126076	14.352474
18.134452	788.987571	14.357491
18.461448	778.036745	14.362509
18.726837	796.096726	14.367527
18.515697	787.321934	14.372544
18.826785	784.098825	14.377562
18.368881	789.228761	14.382579
18.746310	784.950774	14.387597
18.576959	794.974513	14.392615
18.596187	793.040204	14.397632
18.693317	789.730489	14.402650
18.717012	789.187166	14.407667
18.551495	797.563014	14.412685
18.465724	787.541121	14.417703
18.081863	791.697029	14.422720
18.706906	789.021473	14.427738
18.461430	795.147106	14.432755
18.669272	795.382980	14.437773
19.194149	808.504868	14.442791
18.855432	805.392395	14.447808
18.838406	792.516474	14.452826
18.886106	817.089098	14.457843
19.269913	814.684623	14.462861
18.935948	793.892958	14.467879
18.992151	791.997073	14.472896
18.886531	782.527371	14.477914
18.682209	793.667373	14.482931
19.156987	804.610132	14.487949
19.336426	804.872518	14.492967
19.004570	792.768280	14.497984
18.904452	786.058989	14.503002
18.752840	786.843124	14.508019
19.311660	804.346198	14.513037
19.362595	812.984992	14.518055
19.120705	810.649533	14.523072
19.006779	796.712589	14.528090
19.092244	809.420064	14.533107
19.354660	811.058058	14.538125
19.109426	808.956644	14.543143
19.097714	813.843551	14.548160
19.350260	809.414592	14.553178
19.236296	819.211975	14.558195
19.451829	807.940821	14.563213
19.450624	814.612241	14.568231
19.326189	816.531368	14.573248
19.909812	811.530164	14.578266
18.912119	799.333933	14.583283
19.354882	805.910980	14.588301
19.515273	810.288262	14.593319
19.109141	806.504644	14.598336
19.345075	809.058770	14.603354
19.303545	812.069498	14.608371
19.349504	816.896934	14.613389
19.354341	811.054902	14.618407
19.758853	804.664659	14.623424
19.565861	809.488273	14.628442
19.543717	807.708724	14.633459
19.599810	814.636305	14.638477
19.473653	809.676185	14.643495
19.183225	802.898691	14.648512
19.654290	813.955641	14.653530
19.387984	811.841729	14.658547
19.713116	810.216390	14.663565
19.789674	811.056517	14.668583
19.584067	815.301440	14.673600
19.707494	812.306356	14.678618
19.698725	816.037804	14.683635
19.864187	810.704083	14.688653
19.309281	811.099739	14.693671
19.279989	813.723562	14.698688
19.650982	830.495371	14.703706
19.868202	839.076731	14.708723
19.811444	835.118793	14.713741
20.171502	833.327071	14.718759
20.172275	841.636025	14.723776
20.267325	837.323097	14.728794
19.835973	829.346261	14.733811
19.836011	821.488452	14.738829
20.110219	826.646420	14.743847
19.868088	836.832989	14.748864
20.245696	838.655018	14.753882
20.127587	839.967260	14.758899
20.067390	832.563784	14.763917
19.970576	820.536538	14.768935
19.972042	838.211627	14.773952
20.309696	836.922001	14.778970
19.943913	837.177760	14.783987
20.195512	840.666708	14.789005
20.106296	834.091399	14.794023
19.966894	836.262163	14.799040
20.150514	832.465612	14.804058
20.070948	843.153883	14.809075
20.099070	837.197765	14.814093
19.947489	832.755983	14.819111
20.158790	835.541162	14.824128
20.066316	832.040057	14.829146
20.053479	832.294512	14.834163
20.295107	835.507305	14.839181
20.423468	835.550432	14.844199
20.195073	837.621444	14.849216
20.100589	835.559672	14.854234
20.115430	848.423335	14.859251
20.353285	857.462230	14.864269
20.796165	851.337391	14.869287
20.809093	862.004961	14.874304
20.493337	852.539538	14.879322
20.633599	847.708337	14.884339
20.544186	851.417635	14.889357
20.540462	851.512884	14.894375
20.639276	857.310385	14.899392
20.813180	848.428277	14.904410
20.065477	845.979065	14.909427
20.578897	847.180358	14.914445
20.774080	852.950230	14.919463
20.594388	858.273550	14.924480
20.983774	855.899757	14.929498
20.559268	857.026179	14.934515
20.447197	854.433821	14.939533
20.756241	845.843093	14.944551
20.567468	856.851327	14.949568
20.923781	857.821466	14.954586
20.894964	857.343120	14.959603
20.827660	854.260962	14.964621
21.014809	852.871693	14.969639
20.693559	855.682987	14.974656
20.895555	853.420420	14.979674
20.824178	855.902481	14.984691
20.324033	855.169321	14.989709
20.671010	852.871558	14.994727
20.744238	857.363407	14.999744
21.194919	866.609007	15.004762
21.239738	866.835551	15.009779
20.965195	870.437980	15.014797
21.247061	856.410964	15.019815
21.280402	853.783343	15.024832
20.816248	856.345492	15.029850
21.292752	848.789021	15.034867
20.818692	856.108424	15.039885
21.441847	863.676714	15.044903
21.236347	875.448099	15.049920
21.342363	869.423039	15.054938
21.027602	861.405946	15.059955
21.352931	870.144055	15.064973
21.370079	873.663200	15.069991
21.220193	870.991522	15.075008
21.502393	874.794443	15.080026
21.688937	876.766142	15.085043
21.414382	857.593521	15.090061
21.112689	848.820175	15.095079
21.175748	861.603757	15.100096
21.566249	868.185809	15.105114
21.709732	880.142700	15.110131
21.455354	868.793194	15.115149
21.593843	855.034651	15.120167
21.321562	854.540563	15.125184
21.540922	858.416379	15.130202
21.702046	863.052332	15.135219
21.655913	873.116889	15.140237
21.899113	862.005492	15.145255
21.623126	854.730277	15.150272
21.468749	847.704369	15.155290
21.747189	842.681246	15.160307
21.390926	850.562964	15.165325
21.739448	850.341443	15.170343
22.012775	866.298531	15.175360
21.470347	860.222958	15.180378
21.678632	862.592051	15.185395
21.799014	873.861425	15.190413
22.369349	864.049755	15.195431
21.472611	856.394669	15.200448
21.696316	857.603201	15.205466
21.754971	865.000610	15.210483
22.296387	868.718990	15.215501
22.283978	862.526181	15.220519
21.956421	849.127377	15.225536
22.082527	844.648669	15.230554
22.287861	841.735500	15.235571
21.801382	844.635632	15.240589
21.760016	841.726160	15.245607
21.810955	841.756095	15.250624
21.981953	849.442113	15.255642
21.900929	852.288587	15.260659
22.377727	863.937955	15.265677
22.290061	856.841698	15.270695
22.085024	865.962177	15.275712
22.067161	862.073915	15.280730
22.023105	858.091905	15.285747
21.927052	864.326839	15.290765
22.227163	865.431958	15.295783
22.185851	868.865532	15.300800
22.250156	864.102957	15.305818
22.480025	871.912361	15.310835
22.576474	868.246137	15.315853
22.337985	865.121203	15.320871
22.440911	870.009212	15.325888
22.154108	875.759461	15.330906
22.576178	870.398393	15.335923
22.066042	874.583448	15.340941
22.302626	870.683970	15.345959
22.059575	868.080445	15.350976
21.712723	868.752973	15.355994
21.912110	871.281240	15.361011
22.151375	882.664652	15.366029
22.441156	892.386590	15.371047
22.648862	899.786052	15.376064
22.601299	902.387487	15.381082
22.544231	892.594591	15.386099
22.488717	894.752300	15.391117
22.419577	893.617523	15.396135
22.657689	897.417845	15.401152
22.421993	893.008080	15.406170
22.533589	889.588798	15.411187
22.627224	888.109946	15.416205
23.110483	885.551123	15.421223
22.617367	890.967432	15.426240
22.836259	896.212927	15.431258
22.916604	895.073810	15.436275
22.786793	901.288767	15.441293
22.934862	901.063742	15.446311
23.271856	900.673604	15.451328
22.878281	899.721881	15.456346
22.706048	892.272709	15.461363
23.103067	904.322683	15.466381
23.109838	904.936999	15.471399
22.967264	905.274769	15.476416
23.222885	905.888209	15.481434
23.239249	888.607895	15.486451
23.458473	892.758290	15.491469
23.102183	895.956892	15.496487
22.935666	882.236349	15.501504
22.713228	886.584893	15.506522
23.331776	889.183599	15.511539
22.968013	897.003390	15.516557
23.413739	904.987480	15.521575
23.275828	908.903153	15.526592
23.160189	910.432763	15.531610
23.466428	909.179580	15.536627
23.520429	906.958983	15.541645
22.999742	899.980620	15.546663
23.551469	902.870594	15.551680
23.283714	918.700538	15.556698
23.692460	905.578366	15.561715
23.260358	909.410458	15.566733
23.659886	893.216023	15.571751
23.401820	908.596332	15.576768
23.330611	905.577888	15.581786
23.545227	904.320037	15.586803
23.258825	905.393402	15.591821
23.602651	899.085157	15.596839
23.583783	912.260223	15.601856
23.418736	912.377434	15.606874
23.660610	904.352549	15.611891
23.478995	905.343328	15.616909
23.454617	902.869851	15.621927
23.590011	904.335129	15.626944
23.594509	903.472904	15.631962
23.623943	908.659539	15.636979
23.614869	920.315167	15.641997
23.609789	910.646709	15.647015
23.957667	904.407257	15.652032
23.446570	912.660243	15.657050
23.749366	918.722645	15.662067
23.959139	931.884217	15.667085
23.988722	933.763598	15.672103
24.253842	938.610594	15.677120
23.818286	935.582601	15.682138
24.209546	920.011114	15.687155
24.146011	924.442223	15.692173
24.091216	913.976785	15.697191
24.285881	899.281668	15.702208
23.641703	905.699786	15.707226
23.911687	916.305276	15.712243
23.991462	925.340416	15.717261
24.270949	925.113864	15.722279
24.438908	930.708121	15.727296
24.438812	933.011839	15.732314
24.179770	929.691281	15.737331
24.404239	929.807806	15.742349
23.941543	925.569073	15.747367
24.141049	928.722170	15.752384
24.167315	931.643469	15.757402
24.432553	927.651156	15.762419
24.424341	929.839374	15.767437
24.034139	935.902383	15.772455
24.392847	932.523513	15.777472
23.953079	933.617602	15.782490
24.210863	929.478129	15.787507
24.326712	930.460465	15.792525
24.359770	927.110208	15.797543
24.210356	925.640793	15.802560
24.150206	942.659714	15.807578
24.458533	944.546189	15.812595
24.658298	944.603445	15.817613
24.381433	947.246898	15.822631
24.837915	947.491399	15.827648
24.828422	950.951593	15.832666
24.989037	947.145976	15.837683
24.740384	949.286426	15.842701
24.927712	954.000373	15.847719
25.088675	946.486677	15.852736
24.928598	948.704854	15.857754
24.838338	928.727144	15.862771
25.070251	932.885041	15.867789
24.672996	924.659859	15.872807
24.580050	936.293842	15.877824
24.612114	946.974262	15.882842
25.013215	943.124892	15.887859
24.970980	951.844531	15.892877
24.955429	947.634003	15.897895
25.176553	937.665227	15.902912
24.910577	946.921466	15.907930
25.451088	945.155285	15.912947
25.302362	945.749631	15.917965
24.820579	947.847485	15.922983
25.281789	936.055167	15.928000
25.107946	949.459513	15.933018
25.220474	947.621114	15.938035
25.270643	942.740799	15.943053
25.064083	944.148870	15.948071
25.121994	942.281105	15.953088
25.111843	948.348062	15.958106
24.760292	931.737207	15.963123
25.053432	934.317157	15.968141
24.833656	939.788752	15.973159
25.228176	935.337657	15.978176
25.423867	953.437051	15.983194
25.315584	963.912118	15.988211
25.668679	967.031842	15.993229
25.530895	962.518453	15.998247
25.921681	961.665509	16.003264
25.362063	961.127794	16.008282
25.633087	948.579293	16.013299
25.522494	943.026584	16.018317
25.077602	959.095579	16.023335
25.603169	954.523092	16.028352
25.244930	963.332962	16.033370
25.622114	960.430887	16.038387
25.757190	956.944821	16.043405
25.536443	962.205137	16.048423
25.844738	952.115485	16.053440
25.703270	964.864715	16.058458
26.087759	957.249942	16.063475
25.831181	955.450075	16.068493
25.835416	964.146706	16.073511
25.784424	952.525642	16.078528
25.861936	955.334826	16.083546
25.957947	957.708789	16.088563
26.052539	960.770931	16.093581
26.004628	959.765386	16.098599
26.080168	960.495227	16.103616
25.921252	961.681289	16.108634
26.000758	953.189362	16.113651
26.059641	958.412452	16.118669
25.572622	965.815967	16.123687
26.095580	964.314446	16.128704
26.409144	982.834170	16.133722
25.998196	981.771539	16.138739
26.092825	976.587651	16.143757
26.184617	986.539280	16.148775
26.293526	985.058043	16.153792
26.236136	988.812876	16.158810
26.467512	986.305879	16.163827
26.761404	978.354912	16.168845
26.351422	990.413828	16.173863
26.762584	976.773681	16.178880
26.560348	973.832431	16.183898
26.366205	968.901786	16.188915
26.191932	965.526998	16.193933
26.416866	978.913460	16.198951
26.404913	989.013786	16.203968
26.317054	985.309962	16.208986
26.674544	979.643339	16.214003
26.657007	978.973887	16.219021
26.829104	984.469688	16.224039
26.798045	977.288831	16.229056
26.679237	987.733993	16.234074
26.351060	991.477339	16.239091
26.592216	983.604008	16.244109
26.782615	988.200721	16.249127
27.097630	984.033390	16.254144
26.939147	987.362155	16.259162
27.046654	978.360933	16.264179
26.975496	973.518435	16.269197
26.753299	981.246794	16.274215
26.960556	978.797202	16.279232
27.014057	984.030604	16.284250
26.648521	985.059491	16.289267
26.918141	989.517640	16.294285
27.137433	992.251106	16.299303
27.153618	988.663626	16.304320
27.320873	980.615611	16.309338
27.021472	983.155282	16.314355
27.070103	983.933495	16.319373
26.950928	995.972383	16.324391
27.056651	990.108272	16.329408
27.062892	989.201591	16.334426
26.900139	990.315669	16.339443
27.083231	985.007553	16.344461
26.914353	992.781264	16.349479
26.984907	995.739858	16.354496
27.106315	991.631071	16.359514
27.342470	1011.399939	16.364531
27.518888	1013.846597	16.369549
27.612535	1007.185950	16.374567
27.738716	1005.146605	16.379584
27.922841	1005.086376	16.384602
27.303414	1006.716522	16.389619
27.475699	986.458031	16.394637
27.648189	998.053883	16.399655
27.868180	1004.552081	16.404672
27.604491	989.439108	16.409690
27.171875	998.585621	16.414707
27.541022	1001.440922	16.419725
27.714303	1011.023276	16.424743
27.781863	1008.787932	16.429760
27.862236	1001.573936	16.434778
27.456261	1007.765657	16.439795
27.665362	1001.200643	16.444813
27.632113	999.691045	16.449831
27.753304	1002.468189	16.454848
27.606372	1005.495361	16.459866
27.449057	1008.637757	16.464883
27.556288	1010.943709	16.469901
27.735673	1013.910608	16.474919
28.330219	1024.109027	16.479936
28.340459	1016.492538	16.484954
28.271128	1017.888716	16.489971
27.989667	1009.497144	16.494989
27.848444	1008.417763	16.500007
28.251214	1021.460991	16.505024
28.871317	1013.241471	16.510042
28.427486	1008.245550	16.515059
28.637819	999.218841	16.520077
28.070560	995.021617	16.525095
28.141607	991.403503	16.530112
28.246832	989.118117	16.535130
27.979092	998.453551	16.540147
28.153776	988.883293	16.545165
28.257292	994.749533	16.550183
28.250562	1012.470253	16.555200
28.487749	1028.887546	16.560218
28.402639	1024.845618	16.565235
28.528585	1019.404379	16.570253
28.694832	1022.408039	16.575271
28.532861	1028.410299	16.580288
28.628917	1024.245491	16.585306
28.698510	1020.523457	16.590323
28.735480	1019.675106	16.595341
28.871089	1018.997587	16.600359
28.513420	1005.574951	16.605376
28.410879	1014.887829	16.610394
28.545200	1020.657764	16.615411
28.500956	1025.650779	16.620429
28.653365	1021.486665	16.625447
28.666545	1018.316209	16.630464
28.889676	1014.235760	16.635482
28.775362	1024.724425	16.640499
28.752184	1015.547873	16.645517
28.592550	1025.478710	16.650535
28.439215	1024.101415	16.655552
28.915084	1036.779826	16.660570
28.928806	1034.675937	16.665587
29.005385	1036.772072	16.670605
29.039271	1052.845502	16.675623
29.137087	1052.902853	16.680640
29.445276	1044.327941	16.685658
29.379408	1048.690017	16.690675
29.634178	1044.569921	16.695693
29.221831	1032.096201	16.700711
29.221132	1016.247988	16.705728
29.062676	1020.810663	16.710746
29.162378	1042.907686	16.715763
29.450500	1036.178879	16.720781
29.511383	1042.136979	16.725799
29.367608	1048.739166	16.730816
29.677191	1039.097386	16.735834
29.601267	1041.201486	16.740851
29.534258	1041.824138	16.745869
29.521783	1037.912908	16.750887
29.791347	1044.210900	16.755904
29.885272	1046.891311	16.760922
29.416182	1035.625621	16.765939
29.678355	1031.324495	16.770957
29.500022	1031.333323	16.775975
29.212114	1034.972580	16.780992
29.666890	1045.530441	16.786010
29.340681	1037.584477	16.791027
29.434706	1040.062901	16.796045
29.531172	1041.963438	16.801063
29.590944	1046.700425	16.806080
29.404960	1037.060064	16.811098
29.863047	1062.077213	16.816115
29.853794	1060.324034	16.821133
30.023312	1071.844658	16.826151
30.367034	1064.905213	16.831168
30.517138	1055.029480	16.836186
30.171134	1039.780959	16.841203
29.953526	1029.719495	16.846221
29.857604	1033.104799	16.851239
30.277760	1048.811975	16.856256
30.392519	1037.354396	16.861274
29.818708	1035.496616	16.866291
29.873709	1045.043755	16.871309
30.293824	1047.496656	16.876327
30.118128	1049.540553	16.881344
30.297625	1057.881741	16.886362
29.932916	1061.545583	16.891379
30.376963	1058.292257	16.896397
30.507468	1048.037729	16.901415
30.344972	1057.666075	16.906432
30.466089	1062.746963	16.911450
30.161542	1062.664989	16.916467
30.467271	1051.698372	16.921485
30.630238	1049.650139	16.926503
30.526754	1062.996279	16.931520
30.313260	1059.763279	16.936538
30.358395	1060.652491	16.941555
30.406691	1056.078549	16.946573
30.635606	1066.245557	16.951591
30.510999	1086.992168	16.956608
30.753658	1077.414435	16.961626
30.769679	1081.037938	16.966643
31.058962	1082.747513	16.971661
31.178151	1083.940776	16.976679
30.996381	1084.366703	16.981696
31.111504	1081.647421	16.986714
31.012241	1072.785641	16.991731
30.906366	1074.566207	16.996749
30.912005	1070.131446	17.001767
30.849257	1086.320937	17.006784
31.190367	1073.852953	17.011802
30.997240	1080.216685	17.016819
31.075116	1081.441626	17.021837
31.293727	1085.544826	17.026855
30.984063	1076.337108	17.031872
31.324490	1077.281331	17.036890
31.236207	1075.281681	17.041907
31.019374	1078.726844	17.046925
31.439619	1079.633394	17.051943
31.134655	1087.264232	17.056960
31.130960	1071.384879	17.061978
31.372473	1068.832111	17.066995
31.190536	1067.872674	17.072013
31.257015	1074.252788	17.077031
31.165630	1080.177804	17.082048
31.079183	1077.947495	17.087066
31.654614	1096.281399	17.092083
31.388882	1095.139348	17.097101
31.426295	1089.102804	17.102119
31.360331	1094.515784	17.107136
31.357975	1093.165469	17.112154
31.476611	1090.732816	17.117171
31.332033	1084.743543	17.122189
31.248353	1091.175445	17.127207
31.369379	1106.332800	17.132224
31.595437	1115.332638	17.137242
31.552573	1122.727025	17.142259
31.285262	1123.882637	17.147277
31.874413	1110.905796	17.152295
31.642520	1122.529976	17.157312
32.266654	1116.162233	17.162330
32.356254	1110.717157	17.167347
32.090442	1111.452815	17.172365
32.235782	1108.956041	17.177383
31.949756	1117.426541	17.182400
32.016933	1112.518285	17.187418
32.112697	1123.996778	17.192435
32.246782	1122.069797	17.197453
32.396798	1112.803114	17.202471
32.318015	1118.044529	17.207488
32.723248	1119.726588	17.212506
32.483458	1111.868121	17.217523
32.569819	1112.899239	17.222541
32.813102	1102.078013	17.227559
32.034360	1103.543624	17.232576
32.369610	1101.080399	17.237594
32.424374	1111.104135	17.242611
32.111024	1110.124130	17.247629
32.541965	1113.733531	17.252647
32.879384	1125.000831	17.257664
32.563400	1117.242587	17.262682
32.319926	1117.611850	17.267699
32.798622	1129.816518	17.272717
32.830398	1138.067135	17.277735
33.040191	1140.022621	17.282752
33.104242	1122.438010	17.287770
32.653009	1115.451904	17.292787
32.532162	1105.877103	17.297805
32.747644	1111.511356	17.302823
32.217882	1132.097038	17.307840
32.536329	1141.300255	17.312858
32.924393	1132.154289	17.317875
32.740855	1132.672010	17.322893
32.858416	1135.831592	17.327911
33.016335	1140.872058	17.332928
32.562126	1132.093915	17.337946
33.669728	1145.216843	17.342963
33.084008	1144.787327	17.347981
33.476231	1140.229243	17.352999
33.348441	1141.098046	17.358016
33.230395	1139.257656	17.363034
32.967164	1140.851290	17.368051
33.068129	1150.533340	17.373069
33.447392	1152.967370	17.378087
33.437383	1154.878185	17.383104
33.493467	1156.668257	17.388122
33.640257	1151.274226	17.393139
33.308723	1160.846894	17.398157
33.947372	1149.550673	17.403175
33.729755	1157.997918	17.408192
33.790378	1155.874089	17.413210
33.877549	1150.126423	17.418227
33.597584	1154.212590	17.423245
33.955261	1140.886759	17.428263
33.833767	1144.648449	17.433280
33.793134	1147.151011	17.438298
33.698658	1149.791343	17.443315
33.983331	1155.566315	17.448333
34.122804	1155.342625	17.453351
33.960996	1143.801805	17.458368
33.836932	1146.251084	17.463386
33.799861	1150.233161	17.468403
33.490196	1150.912532	17.473421
34.078966	1151.186933	17.478439
33.980656	1150.741489	17.483456
33.832803	1148.716391	17.488474
34.118143	1151.007255	17.493491
33.471991	1153.998568	17.498509
34.203839	1146.878742	17.503527
33.812304	1149.546390	17.508544
34.474144	1162.852344	17.513562
34.582214	1162.198042	17.518579
34.496381	1162.609034	17.523597
34.285899	1149.901830	17.528615
34.471862	1145.315898	17.533632
34.316634	1149.868637	17.538650
34.505250	1160.196608	17.543667
34.615898	1158.686683	17.548685
34.688211	1152.111353	17.553703
34.170006	1143.551451	17.558720
34.228916	1169.375669	17.563738
34.713169	1167.463592	17.568755
34.289263	1180.238016	17.573773
34.606675	1164.415882	17.578791
34.744557	1166.515111	17.583808
34.404263	1164.781905	17.588826
34.466697	1163.339447	17.593843
34.455785	1170.495349	17.598861
34.600375	1167.351744	17.603879
34.734084	1176.075657	17.608896
34.627974	1194.670410	17.613914
34.568285	1187.531796	17.618931
34.882434	1195.874174	17.623949
34.914312	1193.597026	17.628967
35.049529	1189.839493	17.633984
35.120978	1195.748662	17.639002
35.198913	1195.136921	17.644019
34.954585	1198.927216	17.649037
35.139330	1190.327273	17.654055
35.020833	1192.396994	17.659072
35.132945	1192.691961	17.664090
35.379535	1200.644073	17.669107
35.362654	1215.437984	17.674125
35.741057	1219.601543	17.679143
35.603691	1210.796120	17.684160
35.571827	1198.771129	17.689178
35.716362	1194.018065	17.694195
35.142824	1192.011902	17.699213
35.326724	1198.007705	17.704231
35.851211	1208.987157	17.709248
36.067776	1213.321078	17.714266
36.125949	1195.879322	17.719283
35.841959	1191.663193	17.724301
35.724274	1181.784902	17.729319
35.740964	1187.080900	17.734336
35.469973	1187.842613	17.739354
35.973759	1192.901828	17.744371
36.029392	1206.352690	17.749389
36.269887	1200.685278	17.754407
35.843926	1191.751228	17.759424
35.851850	1192.210739	17.764442
36.218533	1195.293674	17.769459
35.916854	1205.805306	17.774477
36.061137	1206.720114	17.779495
36.363089	1207.196963	17.784512
36.153183	1210.972434	17.789530
36.214026	1202.385464	17.794547
36.010441	1209.868027	17.799565
36.393285	1214.185528	17.804583
36.403162	1205.574934	17.809600
36.074104	1219.221400	17.814618
36.263054	1211.677989	17.819635
36.117466	1217.166520	17.824653
36.325675	1214.552645	17.829671
36.691468	1209.954477	17.834688
36.252677	1209.470524	17.839706
36.439363	1209.037512	17.844723
36.582777	1212.978879	17.849741
36.173179	1203.152336	17.854759
36.621815	1216.560953	17.859776
36.632466	1231.353746	17.864794
36.642877	1232.431411	17.869811
36.324526	1244.883332	17.874829
36.662558	1238.159302	17.879847
36.668577	1238.126803	17.884864
36.594380	1236.342693	17.889882
36.932432	1230.871522	17.894899
36.799745	1245.402620	17.899917
37.092400	1228.770083	17.904935
37.382090	1226.241351	17.909952
36.950011	1224.806453	17.914970
36.981846	1221.323786	17.919987
36.943713	1235.171123	17.925005
37.175429	1229.426173	17.930023
37.148476	1226.937273	17.935040
37.097670	1236.018148	17.940058
37.440932	1246.369429	17.945075
37.396997	1259.775873	17.950093
37.765458	1244.251835	17.955111
37.539083	1234.500891	17.960128
37.296458	1227.996658	17.965146
37.310430	1222.812633	17.970163
37.506838	1227.888158	17.975181
37.472282	1243.615809	17.980199
37.523325	1246.457562	17.985216
37.207373	1248.084660	17.990234
37.744100	1246.208587	17.995251
38.126173	1246.912805	18.000269
37.917599	1258.344093	18.005287
37.458147	1247.124104	18.010304
37.451559	1258.539724	18.015322
37.850027	1247.100954	18.020339
38.031249	1252.434471	18.025357
37.492946	1254.799936	18.030375
38.015783	1259.196638	18.035392
37.863842	1263.190313	18.040410
38.100460	1257.968457	18.045427
37.724099	1249.632573	18.050445
37.537818	1261.650531	18.055463
38.114308	1261.986807	18.060480
38.081362	1271.913835	18.065498
38.191691	1269.324660	18.070515
38.324828	1273.605313	18.075533
38.444390	1267.177221	18.080551
38.901545	1256.243707	18.085568
38.427449	1262.692275	18.090586
38.642273	1260.620164	18.095603
38.611334	1261.369752	18.100621
38.737101	1263.612891	18.105639
39.097503	1245.713773	18.110656
38.590828	1240.743349	18.115674
38.551839	1235.652773	18.120691
38.354014	1231.609413	18.125709
38.401712	1245.872585	18.130727
38.810989	1255.841207	18.135744
38.751294	1259.037875	18.140762
38.942335	1258.070850	18.145779
38.977808	1255.487019	18.150797
38.875830	1265.383767	18.155815
39.048219	1248.375458	18.160832
39.229529	1259.559851	18.165850
39.069912	1258.685291	18.170867
38.685082	1257.388201	18.175885
39.050670	1256.220429	18.180903
39.307811	1266.310574	18.185920
38.974579	1256.891836	18.190938
39.047159	1256.669093	18.195955
38.856841	1253.956314	18.200973
38.886784	1256.839224	18.205991
38.802855	1249.997850	18.211008
39.009905	1255.731291	18.216026
39.013464	1271.803329	18.221043
39.427712	1279.145546	18.226061
39.569347	1282.348743	18.231079
39.495686	1282.502220	18.236096
39.225412	1283.538382	18.241114
39.740376	1274.864894	18.246131
39.713928	1276.958164	18.251149
39.272510	1280.854901	18.256167
39.579599	1276.231142	18.261184
39.819009	1273.602933	18.266202
39.606856	1281.434000	18.271219
39.859423	1270.560734	18.276237
39.657393	1275.354322	18.281255
39.773965	1270.605591	18.286272
39.683521	1272.920264	18.291290
40.021163	1277.314246	18.296307
40.028030	1274.725399	18.301325
39.923470	1275.587436	18.306343
39.991506	1278.000512	18.311360
39.927139	1278.064179	18.316378
40.100208	1300.999016	18.321395
40.287576	1299.638081	18.326413
40.376678	1304.228558	18.331431
40.370611	1298.684710	18.336448
40.367302	1301.389766	18.341466
40.332495	1308.154966	18.346483
40.545068	1302.845322	18.351501
40.336485	1310.420224	18.356519
40.533574	1302.522055	18.361536
40.219319	1310.211240	18.366554
40.414229	1302.370215	18.371571
40.690354	1301.169032	18.376589
40.709757	1308.354985	18.381607
40.615993	1300.101311	18.386624
40.581472	1301.561519	18.391642
40.657479	1304.380459	18.396659
40.683967	1292.232710	18.401677
40.419243	1301.955999	18.406695
40.877660	1297.971397	18.411712
40.945676	1296.553306	18.416730
40.652622	1298.836411	18.421747
40.862174	1317.208574	18.426765
41.182628	1324.145688	18.431783
40.945772	1325.454362	18.436800
41.284572	1327.534952	18.441818
41.125356	1329.298601	18.446835
41.212256	1329.259822	18.451853
41.347490	1335.373703	18.456871
41.368151	1316.381843	18.461888
41.054468	1327.655970	18.466906
41.032731	1328.498802	18.471923
41.192481	1329.461702	18.476941
41.276964	1320.921489	18.481959
41.008030	1317.122711	18.486976
41.007804	1323.986675	18.491994
41.209726	1338.260624	18.497011
41.742435	1334.977665	18.502029
41.375668	1346.588276	18.507047
41.674813	1332.476144	18.512064
41.860584	1339.904452	18.517082
41.755379	1347.646313	18.522099
42.059430	1339.210761	18.527117
41.862403	1347.329839	18.532135
41.898836	1338.954890	18.537152
41.953953	1340.104496	18.542170
41.830146	1345.472909	18.547187
42.064705	1336.634764	18.552205
41.825545	1343.409703	18.557223
42.313576	1346.454837	18.562240
42.263731	1341.993932	18.567258
42.100612	1342.956609	18.572275
42.333572	1339.038659	18.577293
41.868996	1344.497997	18.582311
42.050680	1342.462596	18.587328
42.158040	1349.259326	18.592346
42.169787	1364.872577	18.597363
42.430358	1357.788173	18.602381
42.596886	1361.972130	18.607399
42.808065	1369.352313	18.612416
43.068498	1364.694769	18.617434
42.763226	1352.257802	18.622451
42.853922	1341.188786	18.627469
42.327377	1347.115370	18.632487
42.605592	1353.355320	18.637504
42.787948	1358.581394	18.642522
42.757957	1363.026324	18.647539
43.354618	1349.293896	18.652557
42.874323	1365.536027	18.657575
42.958799	1358.302314	18.662592
42.980352	1361.618896	18.667610
42.782798	1367.778290	18.672627
42.972703	1360.057941	18.677645
43.027767	1359.162574	18.682663
42.912711	1356.491711	18.687680
43.264829	1362.489782	18.692698
42.962922	1354.937527	18.697715
43.202348	1347.124266	18.702733
43.196738	1350.558686	18.707751
43.060016	1358.955561	18.712768
43.219851	1359.318840	18.717786
43.173764	1377.027115	18.722803
43.675302	1373.285095	18.727821
43.695846	1378.189225	18.732839
43.167658	1384.816674	18.737856
43.932045	1376.359926	18.742874
43.402116	1383.887060	18.747891
43.622221	1380.728504	18.752909
43.684301	1386.882195	18.757927
43.566696	1382.425518	18.762944
44.028934	1378.557070	18.767962
43.708737	1382.201423	18.772979
43.926573	1377.989170	18.777997
44.082871	1386.289943	18.783015
43.850831	1375.378453	18.788032
43.779247	1382.559666	18.793050
43.985634	1391.351266	18.798067
44.579023	1391.482940	18.803085
44.282457	1394.325188	18.808103
44.263421	1387.615670	18.813120
44.015747	1390.762734	18.818138
44.020544	1402.640582	18.823155
44.578183	1408.019682	18.828173
44.313666	1401.402029	18.833191
43.976835	1403.464742	18.838208
44.341060	1404.181213	18.843226
44.485283	1401.785559	18.848243
44.529509	1401.917527	18.853261
44.394568	1402.446625	18.858279
44.523293	1400.501515	18.863296
44.298437	1398.882858	18.868314
44.420338	1416.609199	18.873331
44.398159	1419.626484	18.878349
44.835901	1424.314191	18.883367
44.789337	1424.905269	18.888384
45.117175	1412.357065	18.893402
44.954653	1424.166302	18.898419
44.902508	1422.583870	18.903437
45.022922	1421.773001	18.908455
44.983197	1422.454534	18.913472
45.392600	1416.710262	18.918490
45.166378	1423.413789	18.923507
45.284641	1414.429608	18.928525
44.919904	1421.968908	18.933543
44.937515	1424.134231	18.938560
45.493863	1433.392080	18.943578
45.563690	1441.261366	18.948595
45.860791	1437.702643	18.953613
45.709936	1431.338684	18.958631
45.381031	1426.580374	18.963648
45.473878	1433.152175	18.968666
45.497575	1449.388498	18.973683
45.772621	1439.603554	18.978701
45.988631	1443.350630	18.983719
46.033124	1449.402938	18.988736
46.166659	1444.291753	18.993754
45.821970	1452.601128	18.998771
46.093202	1437.540192	19.003789
46.095474	1440.698843	19.008807
45.641451	1441.814116	19.013824
45.977487	1437.394095	19.018842
45.636469	1442.663810	19.023859
45.827189	1434.608781	19.028877
46.016206	1432.973021	19.033895
45.892080	1445.426400	19.038912
45.888344	1433.068663	19.043930
45.550184	1458.866758	19.048947
46.176684	1454.306834	19.053965
46.597502	1458.861483	19.058983
46.386804	1458.177905	19.064000
46.761380	1452.827214	19.069018
46.656553	1455.077877	19.074035
47.062849	1451.682034	19.079053
47.170395	1447.354390	19.084071
46.565629	1447.079311	19.089088
47.278813	1441.675904	19.094106
47.186329	1455.377237	19.099123
47.044080	1454.171754	19.104141
47.275435	1450.462316	19.109159
46.697626	1442.735226	19.114176
47.181591	1445.332879	19.119194
47.236866	1444.017747	19.124211
47.112056	1439.770464	19.129229
47.072872	1430.763450	19.134247
47.112622	1441.998401	19.139264
47.090680	1452.715936	19.144282
47.048284	1450.563930	19.149299
46.777422	1450.176902	19.154317
47.129923	1443.374802	19.159335
46.753166	1450.423673	19.164352
47.393480	1460.403777	19.169370
47.614543	1471.686257	19.174387
47.644216	1472.101363	19.179405
47.630238	1473.343788	19.184423
47.877626	1479.301399	19.189440
48.101111	1470.682666	19.194458
47.510018	1469.730104	19.199475
47.668237	1464.728681	19.204493
48.022575	1476.198701	19.209511
47.741735	1477.694118	19.214528
47.660455	1470.277880	19.219546
47.964983	1478.113797	19.224563
47.652309	1472.292579	19.229581
47.843062	1468.908200	19.234599
47.443050	1473.420236	19.239616
47.820470	1467.548381	19.244634
47.834269	1482.931038	19.249651
48.025350	1490.506908	19.254669
48.787287	1494.730741	19.259687
48.534160	1501.460576	19.264704
48.312100	1495.530567	19.269722
48.473975	1508.602192	19.274739
48.600784	1497.158221	19.279757
48.704697	1496.226839	19.284775
48.922613	1502.621400	19.289792
48.906737	1497.763840	19.294810
48.927399	1504.154398	19.299827
48.458996	1487.984101	19.304845
48.868846	1492.543623	19.309863
49.029902	1489.185955	19.314880
48.738029	1486.930772	19.319898
48.511389	1498.765822	19.324915
48.701947	1495.343598	19.329933
48.834125	1491.659060	19.334951
48.516141	1493.444289	19.339968
48.620730	1490.300544	19.344986
49.128608	1501.440556	19.350003
49.000820	1517.343913	19.355021
49.330140	1518.192059	19.360039
49.129218	1528.063330	19.365056
48.929815	1524.143227	19.370074
49.068250	1531.178190	19.375091
48.952824	1525.370427	19.380109
49.462065	1517.006989	19.385127
48.744862	1525.191356	19.390144
49.381754	1539.877435	19.395162
49.756689	1545.436506	19.400179
49.382529	1548.571731	19.405197
49.613985	1533.049839	19.410215
50.019012	1542.530124	19.415232
50.193881	1533.057378	19.420250
50.014546	1532.450967	19.425267
49.991540	1534.540575	19.430285
50.432837	1529.990531	19.435303
50.138761	1531.279726	19.440320
50.178912	1539.993137	19.445338
50.415273	1537.033999	19.450355
50.415044	1530.138459	19.455373
50.542705	1525.596221	19.460391
50.575530	1526.591517	19.465408
50.224434	1526.188577	19.470426
50.881234	1519.137096	19.475443
50.592929	1522.217923	19.480461
50.972667	1520.328395	19.485479
50.959146	1524.956997	19.490496
50.888298	1528.941262	19.495514
51.043215	1508.609141	19.500531
50.747827	1500.471975	19.505549
50.581552	1492.245280	19.510567
50.544695	1498.373388	19.515584
50.641133	1507.232657	19.520602
50.831578	1519.526655	19.525619
50.787401	1518.353236	19.530637
50.889813	1517.415776	19.535655
50.985378	1517.265191	19.540672
50.904943	1515.901754	19.545690
51.077772	1519.115917	19.550707
50.966203	1526.669494	19.555725
51.246006	1512.118410	19.560743
51.151068	1526.422950	19.565760
50.959864	1529.763222	19.570778
50.930986	1538.862928	19.575795
51.182794	1547.174152	19.580813
51.294722	1546.995773	19.585831
51.134215	1551.754567	19.590848
51.277696	1544.397980	19.595866
51.660693	1555.781537	19.600883
51.772327	1568.668520	19.605901
51.852106	1569.113698	19.610919
51.625638	1569.843247	19.615936
51.260272	1570.872139	19.620954
51.615714	1561.645825	19.625971
51.860327	1572.302995	19.630989
51.928374	1568.246566	19.636007
51.632446	1573.234737	19.641024
52.031619	1566.895550	19.646042
52.188214	1578.055588	19.651059
52.567365	1580.786348	19.656077
52.793394	1573.975487	19.661095
52.765207	1561.473142	19.666112
52.749794	1560.421477	19.671130
52.898814	1554.036032	19.676147
52.743706	1561.331310	19.681165
52.713529	1564.425605	19.686183
52.995579	1557.861654	19.691200
52.938248	1565.356309	19.696218
53.010126	1555.359932	19.701235
52.810423	1563.217587	19.706253
53.010326	1554.451003	19.711271
52.867204	1560.144387	19.716288
52.598607	1553.489441	19.721306
52.856458	1549.289853	19.726323
52.650073	1556.744594	19.731341
52.611638	1554.412073	19.736359
52.612537	1556.876667	19.741376
52.868438	1562.599446	19.746394
53.339490	1580.726035	19.751411
53.473464	1583.782153	19.756429
52.964812	1582.264471	19.761447
53.443606	1587.059441	19.766464
53.142487	1582.202087	19.771482
53.404669	1578.806566	19.776499
53.311037	1583.182563	19.781517
53.263592	1580.800948	19.786535
53.060943	1582.934310	19.791552
52.935890	1598.524882	19.796570
53.345016	1603.261275	19.801587
53.380170	1615.516400	19.806605
53.477757	1604.010636	19.811623
53.935026	1615.287991	19.816640
53.784529	1636.162350	19.821658
54.095481	1638.484005	19.826675
54.306098	1643.137702	19.831693
54.514684	1631.204374	19.836711
54.471328	1635.701948	19.841728
53.964759	1632.164169	19.846746
54.083140	1630.267982	19.851763
54.310114	1631.463436	19.856781
54.420172	1632.446713	19.861799
54.532996	1635.212636	19.866816
54.462346	1637.937695	19.871834
54.399239	1629.448716	19.876851
54.640685	1630.528305	19.881869
54.580283	1627.384976	19.886887
54.452056	1626.950490	19.891904
54.334131	1642.480028	19.896922
54.520921	1649.185609	19.901939
54.571053	1657.301061	19.906957
54.622573	1661.777557	19.911975
54.868714	1658.201478	19.916992
54.982431	1654.447195	19.922010
54.752408	1660.558094	19.927027
55.017806	1653.315029	19.932045
54.914923	1671.029282	19.937063
55.145735	1675.307449	19.942080
55.197921	1677.593655	19.947098
55.461483	1674.453529	19.952115
55.511256	1685.008555	19.957133
55.354154	1683.379323	19.962151
55.386511	1684.882800	19.967168
55.414820	1687.166414	19.972186
55.500438	1684.110797	19.977203
55.743251	1680.308007	19.982221
55.742378	1679.863159	19.987239
55.789917	1671.221229	19.992256
55.731246	1677.523212	19.997274
55.864604	1671.058111	20.002291
55.970458	1666.683340	20.007309
55.986825	1665.317443	20.012327
56.219050	1677.958506	20.017344
55.967785	1689.118998	20.022362
56.391180	1688.563911	20.027379
56.457314	1700.814271	20.032397
56.408729	1695.977529	20.037415
56.662193	1691.096917	20.042432
56.551869	1686.260323	20.047450
56.686467	1681.189932	20.052467
56.558897	1665.670172	20.057485
56.662181	1680.202756	20.062503
56.535658	1679.370360	20.067520
56.542333	1687.060233	20.072538
56.663862	1685.756860	20.077555
56.739741	1689.273334	20.082573
56.445916	1689.180218	20.087591
56.972269	1678.036853	20.092608
56.814030	1687.286167	20.097626
56.672946	1683.735657	20.102643
56.876946	1682.700317	20.107661
57.119737	1686.689435	20.112679
57.205146	1699.542726	20.117696
56.763230	1706.939523	20.122714
57.248186	1691.254944	20.127731
57.115555	1700.055297	20.132749
57.101974	1702.222354	20.137767
57.537478	1704.988543	20.142784
57.585639	1702.418452	20.147802
57.645908	1697.574229	20.152819
57.383722	1707.341526	20.157837
57.691420	1721.343685	20.162855
58.119973	1717.363641	20.167872
58.171759	1720.880717	20.172890
58.107164	1719.237078	20.177907
58.215566	1718.803619	20.182925
57.951067	1721.148605	20.187943
58.511309	1717.097563	20.192960
58.203083	1710.521314	20.197978
57.955874	1709.262725	20.202995
58.359486	1717.733436	20.208013
58.259348	1719.197583	20.213031
58.137002	1712.589237	20.218048
58.070762	1714.237459	20.223066
58.178038	1716.915893	20.228083
58.342894	1717.587677	20.233101
58.403313	1713.305177	20.238119
58.427350	1715.958700	20.243136
58.267546	1746.835690	20.248154
58.841139	1748.352738	20.253171
58.764794	1745.256054	20.258189
58.790252	1749.799748	20.263207
59.028987	1745.555752	20.268224
59.004242	1757.144936	20.273242
59.333775	1739.960210	20.278259
59.360331	1737.576520	20.283277
59.269104	1739.288597	20.288295
59.356483	1737.018518	20.293312
59.379221	1728.932705	20.298330
59.242245	1724.908161	20.303347
59.022965	1731.894753	20.308365
59.037868	1743.351519	20.313383
59.749188	1737.029946	20.318400
59.350630	1739.878660	20.323418
59.525200	1731.879663	20.328435
59.405094	1736.278755	20.333453
59.620575	1763.054630	20.338471
60.009303	1752.683752	20.343488
59.993157	1764.713430	20.348506
60.129829	1760.662052	20.353523
60.253258	1758.572556	20.358541
59.574805	1762.323258	20.363559
59.865053	1750.137287	20.368576
59.607675	1763.189165	20.373594
60.020621	1750.848386	20.378611
59.859445	1752.628162	20.383629
60.171085	1769.081885	20.388647
60.405643	1772.333821	20.393664
60.369389	1777.253216	20.398682
60.421208	1772.101010	20.403699
60.525901	1783.821543	20.408717
60.582018	1780.398105	20.413735
60.855842	1776.110768	20.418752
60.756415	1774.860724	20.423770
60.644435	1769.459457	20.428787
60.889530	1773.580784	20.433805
60.938769	1782.624270	20.438823
61.055306	1788.296234	20.443840
61.145487	1798.494730	20.448858
61.397019	1803.511341	20.453875
61.359021	1802.882915	20.458893
61.606298	1795.759382	20.463911
61.626801	1786.550386	20.468928
61.529864	1773.436881	20.473946
61.489432	1771.221411	20.478963
61.362029	1775.154574	20.483981
61.426944	1779.521713	20.488999
61.386527	1782.870114	20.494016
61.524701	1784.852602	20.499034
61.485784	1795.958008	20.504051
61.607309	1787.351841	20.509069
61.823816	1797.022566	20.514087
61.807348	1792.486921	20.519104
61.750914	1795.601125	20.524122
61.906165	1804.303056	20.529139
61.947113	1803.684430	20.534157
62.037358	1807.299681	20.539175
62.367076	1815.570497	20.544192
62.356238	1812.681361	20.549210
62.133170	1817.771869	20.554227
62.399651	1809.673317	20.559245
62.081226	1818.751973	20.564263
62.521017	1814.684948	20.569280
62.574963	1815.175181	20.574298
62.890910	1823.454457	20.579315
63.076970	1827.332515	20.584333
62.303904	1830.548832	20.589351
63.207174	1831.878854	20.594368
63.138541	1827.982507	20.599386
62.936813	1839.009142	20.604403
63.212510	1827.970984	20.609421
63.366977	1837.812342	20.614439
63.420187	1831.170307	20.619456
63.144660	1829.742542	20.624474
63.358555	1836.033703	20.629491
63.539419	1822.769609	20.634509
63.334445	1834.696184	20.639527
63.328144	1820.151525	20.644544
63.308328	1827.905546	20.649562
63.147555	1834.037282	20.654579
63.673031	1825.974141	20.659597
63.419441	1833.590986	20.664615
63.530906	1833.491575	20.669632
63.562250	1838.312096	20.674650
63.740856	1850.646038	20.679667
63.676622	1854.301129	20.684685
63.489963	1855.841875	20.689703
63.602385	1858.131351	20.694720
63.935299	1861.734077	20.699738
64.007093	1876.438988	20.704755
64.101023	1878.280047	20.709773
64.353958	1882.220290	20.714791
64.424797	1882.486980	20.719808
64.184977	1887.946204	20.724826
64.147680	1883.764088	20.729843
64.438169	1879.284776	20.734861
64.487475	1894.220429	20.739879
65.002062	1889.011919	20.744896
65.138904	1900.976841	20.749914
64.941492	1905.088196	20.754931
65.321064	1903.583679	20.759949
64.884424	1904.696272	20.764967
65.254264	1902.432689	20.769984
65.373536	1905.222897	20.775002
65.287766	1911.074727	20.780019
65.435912	1897.850386	20.785037
65.492435	1902.654381	20.790055
65.197117	1899.497085	20.795072
65.644551	1891.345076	20.800090
65.479948	1893.516734	20.805107
65.572810	1892.763785	20.810125
65.611866	1907.546405	20.815143
65.765476	1892.860019	20.820160
65.652328	1888.067993	20.825178
65.419992	1901.791442	20.830195
65.441535	1900.831837	20.835213
65.795037	1908.871766	20.840231
65.879523	1921.428702	20.845248
66.041548	1918.739862	20.850266
66.216741	1921.985289	20.855283
66.370524	1923.734980	20.860301
65.988883	1923.699717	20.865319
65.915382	1924.373905	20.870336
66.320785	1940.481814	20.875354
66.237120	1943.414082	20.880371
66.734361	1931.599722	20.885389
66.467572	1943.665387	20.890407
66.767029	1945.351372	20.895424
66.711985	1952.997318	20.900442
66.522470	1940.453550	20.905459
66.688022	1944.480000	20.910477
66.658788	1943.102246	20.915495
67.122386	1952.109708	20.920512
67.283252	1957.332992	20.925530
67.336354	1965.968852	20.930547
67.452241	1952.727402	20.935565
67.680979	1956.018149	20.940583
67.574856	1957.398037	20.945600
67.699454	1940.933021	20.950618
67.487761	1951.658307	20.955635
67.635855	1955.321387	20.960653
67.396832	1951.006554	20.965671
67.645855	1953.741853	20.970688
67.494200	1958.411009	20.975706
67.543875	1964.005073	20.980723
67.315348	1955.478575	20.985741
67.799519	1966.366938	20.990759
67.739219	1972.909131	20.995776
67.985151	1976.235077	21.000794
67.747185	1976.688708	21.005811
67.916971	1980.424160	21.010829
68.180568	1980.260034	21.015847
68.335821	1979.932888	21.020864
68.259707	1980.238239	21.025882
67.975197	1998.053681	21.030899
68.266169	2006.387426	21.035917
68.710573	2012.914172	21.040935
68.662341	2011.668765	21.045952
68.806268	2009.468746	21.050970
68.509955	2011.304302	21.055987
68.926918	2009.465735	21.061005
69.043810	2012.287891	21.066023
69.255092	2010.910556	21.071040
69.675947	2010.756662	21.076058
69.296724	2008.025839	21.081075
69.597365	1999.177079	21.086093
69.387880	1999.891377	21.091111
69.658146	2004.463296	21.096128
69.770463	2002.236640	21.101146
69.851343	2005.657720	21.106163
69.571522	1999.461967	21.111181
69.404981	1998.187642	21.116199
69.841000	2012.454086	21.121216
69.924128	2013.100735	21.126234
69.911831	2019.584976	21.131251
69.748412	2022.823178	21.136269
70.140590	2022.370776	21.141287
70.053188	2019.004354	21.146304
70.377187	2024.969156	21.151322
70.130032	2020.131683	21.156339
69.820725	2010.087097	21.161357
70.566303	2010.191929	21.166375
70.082294	2008.780830	21.171392
70.499578	2028.251214	21.176410
70.703877	2037.832448	21.181427
70.643937	2038.917958	21.186445
70.755733	2045.048356	21.191463
70.808666	2044.557250	21.196480
70.840360	2045.669522	21.201498
70.784385	2039.255858	21.206515
70.987339	2038.189102	21.211533
70.660524	2048.960773	21.216551
71.029050	2054.079168	21.221568
71.253223	2051.879273	21.226586
71.350678	2064.749887	21.231603
71.607002	2061.500362	21.236621
71.659355	2062.599951	21.241639
71.607516	2059.960167	21.246656
71.648556	2051.416900	21.251674
71.505618	2060.159071	21.256691
71.581965	2060.601640	21.261709
71.819222	2061.063339	21.266727
71.762805	2060.696560	21.271744
71.807806	2052.405153	21.276762
71.915868	2063.424722	21.281779
71.745469	2062.548644	21.286797
72.123671	2065.528948	21.291815
71.986080	2088.102889	21.296832
72.221054	2083.666886	21.301850
72.035021	2083.938856	21.306867
72.577034	2084.154282	21.311885
72.294894	2083.879453	21.316903
72.465273	2082.994501	21.321920
72.639715	2088.184150	21.326938
72.433005	2089.794313	21.331955
72.515030	2094.799527	21.336973
72.867494	2101.501576	21.341991
73.080917	2107.038630	21.347008
73.081208	2108.136859	21.352026
72.966548	2106.791329	21.357043
72.656567	2104.109674	21.362061
72.457817	2102.278593	21.367079
72.581207	2109.748495	21.372096
72.826340	2115.974928	21.377114
73.190271	2132.013724	21.382131
73.602976	2123.220043	21.387149
73.542367	2129.945388	21.392167
73.349386	2138.947866	21.397184
73.805058	2146.627995	21.402202
73.930389	2152.368137	21.407219
74.078242	2165.988411	21.412237
74.422773	2154.999299	21.417255
74.057954	2151.840154	21.422272
74.699909	2152.260939	21.427290
74.593252	2156.850554	21.432307
74.556112	2157.083564	21.437325
74.384206	2140.715024	21.442343
74.142909	2147.815665	21.447360
74.647440	2139.531571	21.452378
74.473698	2151.361971	21.457395
74.456452	2154.403859	21.462413
74.597317	2145.428417	21.467431
74.353664	2146.053361	21.472448
74.343393	2145.900314	21.477466
74.796850	2159.305736	21.482483
74.742706	2166.869578	21.487501
75.243420	2171.815938	21.492519
75.076304	2168.240979	21.497536
75.472360	2170.379032	21.502554
75.430101	2164.928918	21.507571
75.456599	2173.423845	21.512589
75.361987	2166.400735	21.517607
75.192089	2167.099408	21.522624
75.318615	2162.276304	21.527642
75.391594	2181.503800	21.532659
75.433228	2198.451263	21.537677
75.565872	2191.288613	21.542695
75.915711	2203.248980	21.547712
75.978992	2186.799597	21.552730
75.963103	2188.847145	21.557747
76.180230	2199.461631	21.562765
76.334985	2204.013714	21.567783
75.951475	2211.982325	21.572800
76.085394	2213.028196	21.577818
76.359637	2209.236181	21.582835
75.987452	2222.953245	21.587853
76.446933	2207.966500	21.592871
76.369118	2225.866759	21.597888
77.053668	2226.306162	21.602906
76.901046	2228.163552	21.607923
77.011627	2246.195454	21.612941
76.877086	2242.009458	21.617959
77.112527	2246.978205	21.622976
76.776186	2237.625707	21.627994
77.095038	2246.163519	21.633011
77.011891	2236.001539	21.638029
77.155991	2236.048532	21.643047
76.852589	2239.561047	21.648064
77.285004	2249.880096	21.653082
77.613586	2252.296923	21.658099
77.892528	2262.775582	21.663117
77.939300	2258.690749	21.668135
77.923373	2264.686464	21.673152
77.699547	2257.061705	21.678170
77.728699	2256.375468	21.683187
77.575610	2265.617966	21.688205
78.249008	2269.868397	21.693223
78.232678	2280.973742	21.698240
78.159821	2281.641530	21.703258
78.601154	2284.889771	21.708275
78.528483	2292.500735	21.713293
78.684479	2281.667139	21.718311
78.470471	2291.837532	21.723328
78.826546	2287.464680	21.728346
78.838812	2269.776543	21.733363
78.608967	2285.803777	21.738381
78.830572	2278.860786	21.743399
78.811285	2277.809681	21.748416
78.888303	2280.786419	21.753434
78.807557	2283.033436	21.758451
78.961827	2298.458045	21.763469
79.448440	2303.659118	21.768487
79.503992	2306.541366	21.773504
79.103955	2301.942227	21.778522
79.250991	2295.260164	21.783539
79.614393	2305.495310	21.788557
79.491407	2298.848974	21.793575
79.462413	2321.942822	21.798592
79.947330	2322.795187	21.803610
80.165869	2325.431142	21.808627
79.926778	2335.419260	21.813645
80.004438	2326.788104	21.818663
80.054500	2334.626146	21.823680
80.112470	2333.531450	21.828698
80.284305	2326.305836	21.833715
80.039590	2333.343962	21.838733
80.474183	2338.461620	21.843751
80.542738	2352.772925	21.848768
80.278927	2351.961872	21.853786
80.844238	2351.665557	21.858803
80.529233	2348.681669	21.863821
81.188787	2347.076716	21.868839
81.072267	2349.872146	21.873856
80.893468	2350.720543	21.878874
80.717332	2353.127597	21.883891
80.783875	2366.299905	21.888909
81.057308	2361.128806	21.893927
81.244453	2365.451810	21.898944
81.035710	2372.831512	21.903962
81.480507	2369.164399	21.908979
81.848535	2384.786190	21.913997
81.671125	2382.853921	21.919015
81.976072	2378.769893	21.924032
82.217485	2390.737798	21.929050
82.423330	2375.736751	21.934067
81.962937	2378.241717	21.939085
82.442516	2383.756355	21.944103
82.633528	2379.058862	21.949120
82.287164	2371.661429	21.954138
82.571397	2377.165451	21.959155
82.517852	2373.629577	21.964173
82.537292	2371.284783	21.969191
82.627124	2374.022840	21.974208
82.386676	2384.140593	21.979226
82.324712	2368.613165	21.984243
82.342166	2377.125377	21.989261
82.611409	2385.929773	21.994279
82.845469	2398.836167	21.999296
82.929407	2402.607165	22.004314
82.726262	2400.079256	22.009331
83.087258	2398.789044	22.014349
82.971728	2400.460784	22.019367
83.212143	2407.543335	22.024384
83.442747	2420.049467	22.029402
83.237061	2416.578301	22.034419
83.289827	2428.906985	22.039437
83.794099	2424.198580	22.044455
83.810965	2427.863253	22.049472
83.750188	2425.452041	22.054490
84.134678	2426.228522	22.059507
84.162610	2440.893385	22.064525
84.332171	2446.828721	22.069543
84.454706	2436.659852	22.074560
84.054014	2444.968936	22.079578
84.543844	2440.319584	22.084595
84.403987	2435.998661	22.089613
84.238522	2439.432930	22.094631
84.562740	2445.006492	22.099648
84.105141	2455.252775	22.104666
84.580676	2458.107531	22.109683
84.526179	2467.663011	22.114701
84.386061	2463.862867	22.119719
84.562786	2475.695724	22.124736
84.727321	2489.531413	22.129754
85.174001	2479.962196	22.134771
85.390728	2482.790974	22.139789
85.523722	2481.826610	22.144807
85.543703	2477.108379	22.149824
85.941943	2477.933219	22.154842
85.959869	2478.615284	22.159859
85.660860	2484.071280	22.164877
86.147825	2496.777411	22.169895
86.537707	2501.842113	22.174912
85.928165	2491.948149	22.179930
86.594312	2490.963898	22.184947
86.476248	2489.524187	22.189965
86.704076	2490.378715	22.194983
86.621355	2481.507348	22.200000
86.051318	2479.954957	22.205018
86.586781	2493.344707	22.210035
86.704629	2493.843946	22.215053
86.565630	2499.852589	22.220071
87.190272	2494.099712	22.225088
86.714044	2508.887309	22.230106
87.125827	2499.411884	22.235123
86.830774	2490.497827	22.240141
87.201645	2492.276895	22.245159
87.068609	2498.407695	22.250176
87.206805	2518.023059	22.255194
87.551170	2521.179136	22.260211
87.388626	2519.626418	22.265229
87.475084	2523.094069	22.270247
87.865096	2521.019789	22.275264
87.585962	2520.283702	22.280282
87.946736	2519.883521	22.285299
87.651306	2522.908818	22.290317
87.839182	2530.517190	22.295335
88.053687	2534.353100	22.300352
87.737689	2542.368155	22.305370
88.149531	2540.953243	22.310387
88.285130	2536.504196	22.315405
88.057351	2540.203826	22.320423
88.324329	2543.655999	22.325440
88.698242	2562.164812	22.330458
88.520082	2566.453215	22.335475
88.548859	2567.812146	22.340493
88.809409	2565.189927	22.345511
88.944197	2567.097286	22.350528
89.005861	2571.099023	22.355546
88.907468	2564.309893	22.360563
88.439885	2572.989240	22.365581
89.248187	2581.179589	22.370599
89.626832	2576.455987	22.375616
89.284424	2579.195095	22.380634
89.730666	2579.987218	22.385651
89.794205	2580.671654	22.390669
90.146963	2585.552797	22.395687
89.924162	2578.000330	22.400704
90.187565	2583.015314	22.405722
89.919904	2587.727944	22.410739
90.353932	2596.169090	22.415757
90.443339	2604.499780	22.420775
90.298189	2606.453883	22.425792
90.417621	2602.496526	22.430810
90.659009	2598.614864	22.435827
90.870113	2600.223142	22.440845
90.656118	2599.584217	22.445863
91.082750	2599.584067	22.450880
90.928079	2600.352975	22.455898
90.957408	2588.989761	22.460915
91.138245	2583.141839	22.465933
91.264786	2595.951497	22.470951
91.554710	2590.528436	22.475968
90.906157	2586.766398	22.480986
91.078056	2600.945037	22.486003
91.327540	2614.868591	22.491021
91.434361	2611.607528	22.496039
91.758934	2611.762135	22.501056
91.348327	2618.355947	22.506074
91.738478	2616.016525	22.511091
91.893531	2631.618038	22.516109
92.015308	2650.513365	22.521127
92.425734	2638.178684	22.526144
92.165329	2645.585477	22.531162
92.139081	2642.531334	22.536179
92.345481	2636.767785	22.541197
92.168452	2643.953296	22.546215
92.709381	2641.281102	22.551232
92.773279	2661.473126	22.556250
92.717093	2664.505383	22.561267
92.958498	2668.340291	22.566285
92.827316	2671.614619	22.571303
93.147356	2656.311512	22.576320
92.839647	2655.478874	22.581338
92.810412	2668.726282	22.586355
93.293420	2673.028546	22.591373
93.198536	2688.479657	22.596391
93.765433	2685.945437	22.601408
93.421425	2686.276727	22.606426
93.692485	2680.288484	22.611443
94.221991	2677.233022	22.616461
93.638686	2687.543194	22.621479
93.693948	2687.140078	22.626496
93.724912	2709.944199	22.631514
93.863131	2706.286878	22.636531
94.027601	2706.497973	22.641549
94.268894	2711.421754	22.646567
94.610494	2720.132991	22.651584
94.479821	2738.739484	22.656602
95.071927	2732.268856	22.661619
95.342635	2724.838324	22.666637
95.399934	2723.803675	22.671655
95.489170	2696.764300	22.676672
95.415258	2692.215278	22.681690
95.264558	2693.643191	22.686707
95.514472	2693.806267	22.691725
95.228149	2694.516773	22.696743
95.206402	2697.521582	22.701760
95.268277	2707.990113	22.706778
95.255071	2709.402932	22.711795
95.198328	2717.851112	22.716813
95.425415	2727.091466	22.721831
95.509755	2720.602059	22.726848
96.096619	2736.240584	22.731866
95.804860	2748.250711	22.736883
95.944396	2748.847575	22.741901
96.188771	2760.521751	22.746919
96.352414	2759.379016	22.751936
96.434497	2758.264760	22.756954
96.218795	2755.003388	22.761971
96.384376	2764.616288	22.766989
96.250526	2783.119170	22.772007
96.611030	2775.545237	22.777024
96.411554	2778.991178	22.782042
96.168706	2793.875228	22.787059
96.613446	2800.285438	22.792077
96.916516	2815.920875	22.797095
97.185175	2810.873479	22.802112
97.312647	2827.852357	22.807130
97.631042	2835.648840	22.812147
97.895152	2822.917052	22.817165
97.743466	2829.325448	22.822183
97.742942	2827.750634	22.827200
97.316985	2838.771763	22.832218
97.603268	2842.369326	22.837235
98.125044	2855.224941	22.842253
97.855637	2862.548010	22.847271
98.303817	2852.618567	22.852288
98.554216	2848.375652	22.857306
98.603452	2855.724855	22.862323
98.847057	2861.197478	22.867341
98.469325	2872.586696	22.872359
98.729938	2868.143352	22.877376
99.053985	2863.778504	22.882394
98.716261	2864.863128	22.887411
99.186562	2873.093612	22.892429
99.300419	2866.526966	22.897447
99.634803	2866.449653	22.902464
98.958393	2863.695532	22.907482
99.558264	2879.590958	22.912499
100.165225	2890.776381	22.917517
99.729317	2895.007151	22.922535
99.763438	2894.717786	22.927552
100.082497	2886.130837	22.932570
99.749942	2889.354498	22.937587
100.295980	2883.389654	22.942605
100.321586	2882.486174	22.947623
100.262372	2888.558271	22.952640
100.463494	2885.190950	22.957658
100.530432	2887.689630	22.962675
100.713393	2899.127281	22.967693
100.899874	2909.551281	22.972711
100.989527	2906.640010	22.977728
101.603198	2907.857405	22.982746
100.803483	2917.169352	22.987763
101.225844	2911.984377	22.992781
101.334708	2915.407586	22.997799
101.155794	2902.678439	23.002816
101.181769	2904.479686	23.007834
101.233628	2902.710500	23.012851
101.362660	2904.527263	23.017869
100.901579	2910.043338	23.022887
101.702608	2924.272619	23.027904
101.708542	2924.413717	23.032922
101.825043	2932.787683	23.037939
101.955691	2926.208933	23.042957
101.978580	2935.904107	23.047975
102.250784	2950.029532	23.052992
102.581620	2951.893784	23.058010
102.227268	2962.985900	23.063027
102.478840	2963.723135	23.068045
102.343634	2959.110998	23.073063
102.428471	2955.506122	23.078080
102.696115	2964.121686	23.083098
102.787631	2979.433562	23.088115
102.920319	2980.826843	23.093133
103.271236	2972.654658	23.098151
103.081267	2980.741812	23.103168
103.210514	2982.990939	23.108186
103.384787	2995.888135	23.113203
103.716532	2995.937477	23.118221
103.759439	2997.010189	23.123239
103.556786	3005.935703	23.128256
103.947957	2998.161223	23.133274
103.563977	3004.814152	23.138291
104.376771	3019.635030	23.143309
104.240405	3025.517193	23.148327
103.979591	3028.546653	23.153344
103.879297	3031.999292	23.158362
103.886431	3042.220894	23.163379
104.439869	3033.527949	23.168397
104.729903	3044.276767	23.173415
104.795832	3047.504693	23.178432
105.247317	3045.196698	23.183450
105.034267	3050.383834	23.188467
105.384488	3058.241737	23.193485
105.667685	3056.846816	23.198503
105.428128	3060.822969	23.203520
105.922203	3054.673635	23.208538
105.770599	3064.777938	23.213555
105.909317	3051.532124	23.218573
105.964564	3051.596110	23.223591
106.047849	3053.249580	23.228608
106.091045	3051.595349	23.233626
105.888614	3058.349433	23.238643
106.365711	3053.452573	23.243661
106.036061	3057.729961	23.248679
106.026936	3064.321393	23.253696
106.683975	3067.482541	23.258714
106.560455	3086.400737	23.263731
106.875581	3074.512987	23.268749
106.996360	3073.907137	23.273767
106.617895	3078.555086	23.278784
107.330626	3092.125991	23.283802
107.029446	3105.302438	23.288819
107.579676	3098.740360	23.293837
107.349923	3103.330444	23.298855
107.413855	3100.656701	23.303872
107.734385	3094.316599	23.308890
107.353551	3107.574885	23.313907
107.640331	3116.660964	23.318925
107.892277	3119.247650	23.323943
107.879909	3132.754733	23.328960
108.114076	3125.711620	23.333978
107.965891	3131.557784	23.338995
108.382245	3140.137654	23.344013
108.441519	3148.501694	23.349031
108.566775	3150.994487	23.354048
108.474143	3146.864878	23.359066
108.657086	3157.923959	23.364083
108.585799	3150.265601	23.369101
108.760550	3150.165799	23.374119
109.121573	3165.268597	23.379136
109.176068	3172.001659	23.384154
109.092471	3174.331291	23.389171
109.596604	3170.462254	23.394189
109.146947	3168.152517	23.399207
109.171900	3179.747507	23.404224
109.659004	3189.708251	23.409242
109.294280	3202.152965	23.414259
110.093472	3194.734645	23.419277
109.877046	3204.940647	23.424295
109.644458	3210.462267	23.429312
110.122508	3217.877413	23.434330
109.987340	3223.077722	23.439347
110.410639	3231.978484	23.444365
110.374609	3244.179526	23.449383
111.114029	3237.534287	23.454400
111.448530	3223.490916	23.459418
111.767394	3226.521687	23.464435
111.961005	3220.122397	23.469453
112.162924	3215.183120	23.474471
111.529793	3207.126163	23.479488
111.770630	3199.662213	23.484506
111.787101	3198.955822	23.489523
111.916405	3194.217226	23.494541
112.349937	3194.279128	23.499559
112.266951	3197.536579	23.504576
111.888842	3187.681944	23.509594
111.935550	3202.675902	23.514611
112.088679	3206.663541	23.519629
112.238235	3212.633808	23.524647
112.337788	3211.450524	23.529664
112.418828	3214.587756	23.534682
112.305048	3223.486916	23.539699
112.261095	3231.305268	23.544717
112.747760	3243.020940	23.549735
112.387244	3252.633950	23.554752
112.494233	3261.539787	23.559770
112.845142	3275.366003	23.564787
113.196808	3277.350138	23.569805
113.417480	3276.220585	23.574823
113.581661	3292.105306	23.579840
113.394097	3302.679299	23.584858
113.470218	3297.150443	23.589875
113.357435	3299.749753	23.594893
113.811937	3313.395749	23.599911
113.895717	3329.128899	23.604928
114.274673	3318.711301	23.609946
114.048714	3327.747913	23.614963
114.519828	3335.284123	23.619981
114.812655	3344.779680	23.624999
114.416340	3345.074938	23.630016
114.955504	3350.356510	23.635034
114.961300	3343.459335	23.640051
114.938704	3348.156101	23.645069
115.406988	3352.318794	23.650087
115.310952	3364.459823	23.655104
115.831518	3363.905344	23.660122
115.693419	3371.085083	23.665139
115.497668	3363.600666	23.670157
116.116495	3359.328677	23.675175
115.784593	3367.649567	23.680192
115.816709	3360.615727	23.685210
115.822833	3363.389062	23.690227
115.993414	3371.211948	23.695245
116.542217	3379.171636	23.700263
116.528863	3385.612347	23.705280
116.245591	3382.314037	23.710298
116.839138	3382.556180	23.715315
116.567416	3386.281761	23.720333
116.894331	3378.820116	23.725351
116.493862	3387.846054	23.730368
116.999715	3401.231625	23.735386
116.926494	3410.345497	23.740403
116.702829	3413.498641	23.745421
116.754402	3417.473732	23.750439
117.374110	3429.522307	23.755456
117.833113	3437.196162	23.760474
117.974642	3436.419792	23.765491
117.978835	3434.878909	23.770509
118.340110	3433.585426	23.775527
118.404768	3450.984979	23.780544
118.542772	3455.969233	23.785562
118.585146	3454.671744	23.790579
118.145796	3459.682764	23.795597
118.644062	3465.870258	23.800615
118.542967	3463.594587	23.805632
118.786849	3456.944359	23.810650
119.018230	3470.562088	23.815667
118.872224	3480.640502	23.820685
119.356038	3481.306882	23.825703
119.207751	3486.048502	23.830720
119.409080	3492.203331	23.835738
119.457661	3492.265200	23.840755
119.612401	3502.940671	23.845773
120.076523	3500.387623	23.850791
119.993759	3512.662403	23.855808
120.009124	3515.891973	23.860826
120.109706	3504.482370	23.865843
120.186450	3523.101566	23.870861
120.426709	3519.829033	23.875879
120.593304	3534.769884	23.880896
120.696192	3529.508224	23.885914
121.164074	3519.868877	23.890931
120.826524	3534.304318	23.895949
121.044752	3520.865876	23.900967
120.638234	3540.251541	23.905984
121.087662	3548.154183	23.911002
121.440391	3556.649472	23.916019
121.059259	3563.134882	23.921037
121.776989	3570.683295	23.926055
121.657797	3575.332034	23.931072
121.815648	3583.232744	23.936090
122.000941	3580.577910	23.941107
122.037907	3585.795710	23.946125
122.312156	3586.848220	23.951143
122.699210	3601.584367	23.956160
122.501158	3592.660970	23.961178
122.800065	3590.881659	23.966195
122.707110	3602.877182	23.971213
123.150730	3594.431473	23.976231
123.044701	3599.005575	23.981248
123.057178	3605.000471	23.986266
123.260795	3614.333311	23.991283
123.463546	3623.246512	23.996301
123.567935	3618.858870	24.001319
123.836987	3617.829076	24.006336
123.223077	3614.721075	24.011354
124.190501	3618.266404	24.016371
123.895949	3646.974053	24.021389
124.223269	3634.853631	24.026407
124.009719	3640.138856	24.031424
124.248136	3643.570440	24.036442
124.462764	3634.756365	24.041459
124.189884	3637.336463	24.046477
124.783405	3641.981568	24.051495
125.159585	3656.953014	24.056512
125.075952	3663.215392	24.061530
125.286582	3661.970598	24.066547
125.120363	3670.720331	24.071565
125.119709	3667.684123	24.076583
125.229889	3664.627503	24.081600
125.320034	3660.324132	24.086618
125.777863	3672.533792	24.091635
125.697181	3686.667394	24.096653
125.675249	3692.617175	24.101671
125.880322	3689.144934	24.106688
125.810080	3691.434678	24.111706
126.481069	3702.547516	24.116723
126.603129	3714.897856	24.121741
126.823800	3706.054399	24.126759
126.603134	3707.060877	24.131776
126.806194	3713.212355	24.136794
126.971896	3720.913059	24.141811
127.133284	3732.938508	24.146829
127.606788	3735.755914	24.151847
127.557921	3735.750894	24.156864
127.091137	3736.628410	24.161882
127.827106	3721.515302	24.166899
127.506174	3739.275010	24.171917
127.518184	3746.633528	24.176935
127.702592	3742.747868	24.181952
127.657067	3749.831282	24.186970
128.179910	3761.140815	24.191987
128.408627	3786.134362	24.197005
128.597098	3782.730969	24.202023
128.277349	3771.869548	24.207040
128.638150	3773.713441	24.212058
128.852731	3794.700748	24.217075
128.409309	3806.088154	24.222093
128.851223	3808.825272	24.227111
128.762601	3811.720739	24.232128
129.147202	3824.071311	24.237146
129.561897	3827.879488	24.242163
129.426835	3834.563403	24.247181
129.749049	3843.862117	24.252199
130.239318	3847.595407	24.257216
130.056543	3857.168438	24.262234
130.418784	3856.139904	24.267251
130.319781	3855.262089	24.272269
130.212791	3857.879515	24.277287
130.526084	3860.920730	24.282304
130.685184	3875.806218	24.287322
130.944448	3869.838356	24.292339
131.064580	3879.594648	24.297357
131.268347	3882.188946	24.302375
131.149093	3867.152055	24.307392
131.188542	3887.636482	24.312410
131.784604	3883.797171	24.317427
131.772996	3889.758035	24.322445
131.720387	3893.361229	24.327463
132.035962	3886.248333	24.332480
131.882579	3891.694704	24.337498
132.247050	3900.415580	24.342515
132.061443	3926.411244	24.347533
132.466585	3916.197542	24.352551
132.534569	3920.498443	24.357568
132.384557	3929.532999	24.362586
132.550380	3929.254676	24.367603
132.714014	3941.532417	24.372621
132.823613	3940.076081	24.377639
133.177704	3947.179419	24.382656
133.289277	3940.483331	24.387674
133.191452	3936.818323	24.392691
133.512358	3960.797215	24.397709
133.611989	3974.972407	24.402727
134.036053	3963.076583	24.407744
133.615337	3968.627723	24.412762
133.864244	3967.888270	24.417779
134.484331	3986.170846	24.422797
134.380484	3987.661003	24.427815
134.583859	3986.742416	24.432832
134.739778	3983.463993	24.437850
134.981754	3981.523069	24.442867
134.783217	3989.902387	24.447885
135.110194	3997.009967	24.452903
135.376355	4007.387478	24.457920
135.355983	4013.229808	24.462938
135.323817	4005.643903	24.467955
135.414143	4010.455825	24.472973
135.861720	4017.393133	24.477991
136.159899	4026.575743	24.483008
136.179262	4020.951345	24.488026
136.321490	4024.827236	24.493043
136.263427	4022.121850	24.498061
136.133357	4016.659595	24.503079
136.665512	4019.720420	24.508096
136.635842	4044.587269	24.513114
137.084363	4035.869150	24.518131
137.091541	4040.409957	24.523149
136.915216	4038.792969	24.528167
137.263946	4034.682816	24.533184
137.163482	4053.077643	24.538202
137.498521	4068.601879	24.543219
137.769259	4063.806317	24.548237
137.652761	4056.593340	24.553255
137.723204	4057.702860	24.558272
138.006819	4084.398994	24.563290
138.637404	4079.560028	24.568307
138.731035	4080.347151	24.573325
138.872828	4088.111705	24.578343
138.930927	4080.338118	24.583360
138.900725	4085.178294	24.588378
139.073717	4080.470540	24.593395
139.122097	4086.109655	24.598413
139.083086	4092.642990	24.603431
139.591604	4098.229406	24.608448
139.135693	4103.991228	24.613466
139.467324	4098.359220	24.618483
139.627320	4098.125990	24.623501
139.215196	4118.321164	24.628519
140.215455	4125.645915	24.633536
139.799481	4123.409716	24.638554
140.171776	4139.322752	24.643571
140.605125	4147.619547	24.648589
140.435496	4148.962142	24.653607
140.766281	4145.457617	24.658624
140.672955	4159.473616	24.663642
140.629714	4175.757544	24.668659
141.242522	4175.068742	24.673677
141.220650	4181.324839	24.678695
141.688782	4173.433716	24.683712
141.487306	4197.147055	24.688730
142.101588	4198.680084	24.693747
142.207563	4208.356693	24.698765
142.126212	4202.293406	24.703783
142.225444	4200.491466	24.708800
142.154784	4198.870638	24.713818
142.282235	4199.598844	24.718835
142.208762	4202.744522	24.723853
142.418558	4219.557235	24.728871
142.560249	4206.439522	24.733888
142.404960	4216.974303	24.738906
142.789230	4230.038538	24.743923
143.316539	4240.242959	24.748941
143.480719	4253.167877	24.753959
143.370159	4243.971715	24.758976
143.475383	4262.038035	24.763994
143.624162	4263.583573	24.769011
144.275665	4258.264695	24.774029
144.400890	4266.028749	24.779047
144.809928	4268.733180	24.784064
144.274336	4268.119010	24.789082
144.297464	4266.158471	24.794099
144.421488	4274.172066	24.799117
144.529700	4290.997504	24.804135
145.014821	4287.020721	24.809152
144.995760	4290.669272	24.814170
145.141276	4309.502673	24.819187
145.290798	4316.451782	24.824205
145.618119	4325.487971	24.829223
145.743446	4318.846417	24.834240
145.367949	4331.618687	24.839258
145.838411	4335.440386	24.844275
146.053253	4341.309328	24.849293
145.974769	4362.652246	24.854311
146.644829	4373.178561	24.859328
146.226066	4370.036887	24.864346
146.944288	4374.198784	24.869363
146.936447	4360.141549	24.874381
146.752824	4369.228902	24.879399
147.133377	4384.579037	24.884416
147.266082	4397.187008	24.889434
147.377336	4394.158506	24.894451
147.530853	4405.172433	24.899469
147.449041	4415.522290	24.904487
147.734601	4412.962197	24.909504
147.986967	4417.392329	24.914522
148.091360	4436.263828	24.919539
148.665745	4433.696642	24.924557
148.465907	4447.233895	24.929575
148.893700	4432.676356	24.934592
148.875377	4444.316772	24.939610
149.051279	4457.479895	24.944627
149.529038	4455.767348	24.949645
149.447778	4464.150721	24.954663
149.372015	4454.223067	24.959680
149.102277	4460.779831	24.964698
149.692621	4469.775143	24.969715
149.945679	4468.091266	24.974733
150.118808	4481.207493	24.979751
150.579569	4471.742353	24.984768
150.455268	4470.650655	24.989786
150.336152	4479.418695	24.994803
150.651596	4485.537158	24.999821
150.634029	4504.705478	25.004839
151.172422	4496.658083	25.009856
150.818367	4502.252665	25.014874
150.875822	4507.824214	25.019891
150.482118	4512.225544	25.024909
150.607101	4527.369391	25.029927
151.157539	4543.870546	25.034944
151.093207	4554.555495	25.039962
151.515547	4578.891869	25.044979
152.018917	4570.733107	25.049997
152.580821	4578.946958	25.055015
152.493007	4587.953220	25.060032
152.713230	4591.252094	25.065050
152.669914	4609.834286	25.070067
152.928791	4607.710749	25.075085
152.810133	4607.382015	25.080103
153.163279	4602.242059	25.085120
153.149600	4607.177649	25.090138
153.057822	4623.681016	25.095155
153.661784	4624.833764	25.100173
153.526590	4628.304766	25.105191
153.681413	4625.095840	25.110208
154.168591	4651.054081	25.115226
154.000255	4650.647858	25.120243
154.733288	4651.070319	25.125261
154.536309	4654.573041	25.130279
154.741188	4647.672780	25.135296
155.164367	4671.207419	25.140314
155.177893	4672.957123	25.145331
155.658630	4674.785595	25.150349
155.581536	4676.984993	25.155367
155.318226	4677.556263	25.160384
155.416596	4671.464838	25.165402
155.385781	4687.857765	25.170419
155.904565	4694.948384	25.175437
155.871758	4700.259436	25.180455
156.503505	4702.247472	25.185472
156.723288	4716.767528	25.190490
156.259649	4728.007150	25.195507
156.670763	4721.011625	25.200525
156.597845	4731.215081	25.205543
156.916724	4739.094383	25.210560
157.294067	4741.961643	25.215578
157.354412	4749.938017	25.220595
157.594965	4741.857974	25.225613
158.000986	4755.815629	25.230631
158.031202	4766.369194	25.235648
158.234983	4762.963236	25.240666
158.272889	4766.745053	25.245683
158.463517	4761.235800	25.250701
158.567295	4764.562304	25.255719
158.402429	4764.095565	25.260736
158.787059	4771.336514	25.265754
158.668012	4780.388768	25.270771
159.131874	4780.685849	25.275789
159.484390	4807.820538	25.280807
159.483387	4806.772752	25.285824
159.649157	4807.075210	25.290842
159.926208	4808.654484	25.295859
159.885661	4808.351462	25.300877
160.054147	4822.592353	25.305895
160.553408	4826.567496	25.310912
160.558765	4830.019811	25.315930
160.364757	4835.318123	25.320947
160.488678	4837.101158	25.325965
160.858242	4835.310728	25.330983
161.415302	4850.677968	25.336000
161.652779	4846.177772	25.341018
161.197002	4847.697539	25.346035
161.782765	4840.097147	25.351053
161.730239	4851.698959	25.356071
161.879390	4864.150030	25.361088
162.205772	4867.801731	25.366106
162.019750	4877.356867	25.371123
162.288873	4863.372910	25.376141
162.305748	4876.933559	25.381159
162.217634	4899.446496	25.386176
162.248302	4899.195514	25.391194
162.575197	4904.835712	25.396211
162.631634	4925.366015	25.401229
162.953912	4931.199484	25.406247
162.884324	4943.350079	25.411264
163.291286	4956.307143	25.416282
163.050293	4967.755296	25.421299
163.683710	4974.196884	25.426317
164.046157	4980.194564	25.431335
164.047706	4974.904073	25.436352
164.388354	4975.857949	25.441370
164.754995	5000.159371	25.446387
165.096218	4998.243923	25.451405
164.946288	5001.900366	25.456423
165.274625	5004.664821	25.461440
165.533941	5001.695235	25.466458
165.526843	4998.202118	25.471475
165.726768	5008.120202	25.476493
165.710085	5024.227151	25.481511
166.028237	5027.132080	25.486528
166.416580	5019.227763	25.491546
166.438366	5029.422955	25.496563
166.527989	5018.882138	25.501581
166.740267	5041.976623	25.506599
166.153651	5044.716239	25.511616
166.576526	5046.954632	25.516634
166.455463	5064.334147	25.521651
166.735605	5070.511966	25.526669
166.810803	5079.351050	25.531687
166.878633	5096.038324	25.536704
167.507654	5106.991272	25.541722
167.605563	5118.191053	25.546739
167.497782	5130.098356	25.551757
168.078521	5141.194572	25.556775
168.125340	5147.386647	25.561792
168.663694	5148.978930	25.566810
168.594747	5156.830413	25.571827
169.182470	5172.474082	25.576845
169.204879	5177.120123	25.581863
168.742692	5184.107985	25.586880
169.240902	5191.520810	25.591898
169.704279	5196.281280	25.596915
169.954884	5206.008505	25.601933
170.268647	5205.221028	25.606951
169.806934	5209.964546	25.611968
170.384043	5216.279258	25.616986
170.555558	5218.023356	25.622003
170.579727	5220.011350	25.627021
170.927520	5226.929940	25.632039
170.787942	5240.439462	25.637056
171.221313	5244.952095	25.642074
171.415664	5243.214157	25.647091
171.317417	5257.143387	25.652109
171.389753	5268.265173	25.657127
171.557917	5272.408755	25.662144
171.593366	5281.970656	25.667162
171.507040	5302.621463	25.672180
171.986517	5307.480465	25.677197
172.466960	5316.865783	25.682215
172.470930	5331.700862	25.687232
172.954211	5337.995502	25.692250
173.072122	5341.484052	25.697268
173.048218	5359.117027	25.702285
173.264907	5354.894562	25.707303
173.607857	5364.620121	25.712320
173.462931	5372.032140	25.717338
174.144780	5387.146824	25.722356
174.288306	5376.426955	25.727373
174.266864	5376.221958	25.732391
174.340306	5382.122724	25.737408
174.616073	5394.488157	25.742426
174.672169	5396.335469	25.747444
174.674172	5396.593991	25.752461
175.090199	5405.247595	25.757479
175.252793	5425.272669	25.762496
175.952254	5417.228204	25.767514
176.328899	5423.286952	25.772532
176.222679	5416.996702	25.777549
176.038546	5413.275388	25.782567
175.667031	5425.290231	25.787584
175.764143	5418.722113	25.792602
176.229739	5428.545404	25.797620
176.256960	5439.497552	25.802637
176.789306	5443.249879	25.807655
176.674430	5456.853569	25.812672
177.068620	5460.112891	25.817690
177.492926	5476.325192	25.822708
177.480328	5482.539258	25.827725
177.646075	5482.917490	25.832743
177.670397	5495.363175	25.837760
178.438982	5518.703093	25.842778
178.271634	5515.417907	25.847796
178.349427	5514.342030	25.852813
178.714794	5512.829967	25.857831
179.086630	5528.517025	25.862848
179.490341	5527.810229	25.867866
179.924140	5528.490794	25.872884
179.861569	5529.179195	25.877901
179.588880	5525.197023	25.882919
179.610626	5526.008029	25.887936
179.826701	5526.469966	25.892954
179.879353	5537.790688	25.897972
179.970028	5550.557521	25.902989
180.397714	5552.703688	25.908007
180.204429	5576.319696	25.913024
180.453880	5580.204480	25.918042
180.801271	5588.392215	25.923060
181.402676	5594.393933	25.928077
181.760496	5595.502998	25.933095
181.590009	5593.755541	25.938112
181.786788	5588.472355	25.943130
182.307810	5605.430450	25.948148
182.179999	5622.082378	25.953165
182.537807	5616.761487	25.958183
182.663577	5620.902279	25.963200
182.565548	5618.026108	25.968218
182.952080	5623.707751	25.973236
183.004376	5646.505940	25.978253
183.131182	5642.979226	25.983271
183.282002	5649.972836	25.988288
183.320793	5652.855073	25.993306
183.772055	5664.259018	25.998324
183.747757	5669.764736	26.003341
183.744334	5683.029270	26.008359
184.000475	5689.469878	26.013376
184.135837	5707.577137	26.018394
184.813062	5716.082900	26.023412
184.610649	5734.700480	26.028429
184.853309	5724.624702	26.033447
184.939391	5750.886866	26.038464
185.256538	5759.306663	26.043482
185.583903	5749.874257	26.048500
185.505935	5770.158127	26.053517
185.542956	5781.317290	26.058535
185.817461	5794.516539	26.063552
185.955334	5800.287457	26.068570
186.543654	5804.937094	26.073588
186.521575	5801.698685	26.078605
186.799262	5816.286364	26.083623
186.864584	5829.824398	26.088640
187.020677	5831.015391	26.093658
187.190149	5844.622449	26.098676
187.274860	5855.546957	26.103693
187.656876	5860.377089	26.108711
187.843928	5861.645337	26.113728
187.824529	5881.459344	26.118746
187.894485	5882.717414	26.123764
187.958128	5891.435583	26.128781
188.418232	5893.788239	26.133799
188.557230	5904.199263	26.138816
188.935922	5923.001191	26.143834
189.522249	5924.336702	26.148852
189.441623	5940.463886	26.153869
189.925240	5929.807539	26.158887
190.262717	5939.344860	26.163904
190.450608	5936.354677	26.168922
190.926932	5942.874734	26.173940
190.831906	5943.025261	26.178957
190.853250	5929.142197	26.183975
191.500400	5936.708913	26.188992
191.482327	5931.484331	26.194010
191.540621	5923.346913	26.199028
191.422789	5934.236712	26.204045
191.929037	5946.351988	26.209063
191.922416	5950.942770	26.214080
191.702409	5959.531518	26.219098
191.817413	5963.257388	26.224116
191.920977	5973.074206	26.229133
192.148358	5973.338683	26.234151
192.154985	6000.945681	26.239168
192.418425	5996.254920	26.244186
192.730656	6021.418474	26.249204
192.769095	6035.772106	26.254221
192.956937	6046.661731	26.259239
193.492782	6049.532934	26.264256
193.647892	6067.766899	26.269274
193.926326	6081.742283	26.274292
194.198102	6089.228610	26.279309
194.797480	6098.074967	26.284327
194.816748	6106.427661	26.289344
194.789183	6113.297702	26.294362
195.151052	6116.688443	26.299380
195.489010	6136.475500	26.304397
195.252453	6139.406995	26.309415
195.659805	6150.426655	26.314432
195.667528	6162.493422	26.319450
195.902686	6170.462142	26.324468
195.958311	6169.818987	26.329485
196.418493	6179.801362	26.334503
196.770743	6195.548865	26.339520
196.777216	6196.340181	26.344538
196.917365	6202.739053	26.349556
196.868818	6218.422708	26.354573
197.337861	6225.325959	26.359591
197.703528	6240.935675	26.364608
197.603963	6256.185368	26.369626
197.718396	6245.561063	26.374644
198.171196	6270.317959	26.379661
198.810808	6265.022455	26.384679
199.048581	6265.184305	26.389696
199.029026	6267.226572	26.394714
199.214845	6281.314385	26.399732
199.303271	6292.570029	26.404749
199.385578	6285.492519	26.409767
200.092714	6294.126480	26.414784
199.890397	6293.147831	26.419802
199.862758	6301.886721	26.424820
200.018168	6316.086624	26.429837
200.388111	6320.571522	26.434855
200.194663	6328.117751	26.439872
200.368466	6333.949536	26.444890
200.834263	6337.889188	26.449908
200.915123	6347.485616	26.454925
201.072493	6373.696539	26.459943
201.466271	6371.848530	26.464960
201.374223	6371.199948	26.469978
202.093584	6386.394857	26.474996
201.833500	6388.575599	26.480013
202.146357	6407.350396	26.485031
202.503591	6411.859393	26.490048
202.351293	6427.085871	26.495066
202.944069	6429.809376	26.500084
203.457505	6440.954749	26.505101
203.282639	6440.609477	26.510119
203.397178	6458.196705	26.515136
203.298057	6475.997149	26.520154
203.966542	6472.404883	26.525172
204.048576	6487.405525	26.530189
204.009062	6488.033550	26.535207
204.408937	6499.404983	26.540224
204.895207	6514.083860	26.545242
205.293285	6505.372421	26.550260
205.688672	6518.834324	26.555277
205.909994	6527.373568	26.560295
206.056011	6525.923985	26.565312
206.294939	6536.711248	26.570330
206.317945	6530.700384	26.575348
206.179558	6537.474196	26.580365
206.618659	6553.069590	26.585383
206.838662	6547.457368	26.590400
206.742326	6564.850245	26.595418
206.966870	6573.837266	26.600436
207.060792	6591.759292	26.605453
207.418400	6604.580006	26.610471
207.836801	6609.912912	26.615488
207.933778	6626.031989	26.620506
208.090981	6615.991124	26.625524
208.384824	6632.774043	26.630541
208.438717	6632.156395	26.635559
208.902975	6646.961920	26.640576
208.841865	6662.363803	26.645594
209.142029	6666.073616	26.650612
209.104723	6677.784706	26.655629
209.278870	6694.567376	26.660647
209.661040	6690.994391	26.665664
209.958277	6705.298785	26.670682
210.121278	6710.791441	26.675700
210.514394	6724.509548	26.680717
210.787601	6737.791758	26.685735
211.006742	6749.412459	26.690752
210.897993	6748.141421	26.695770
211.253220	6760.571175	26.700788
211.207331	6776.958856	26.705805
211.644644	6778.068249	26.710823
211.843471	6795.011322	26.715840
211.894432	6807.150702	26.720858
212.133409	6812.255902	26.725876
212.555460	6816.335055	26.730893
212.882809	6826.398445	26.735911
213.003181	6839.221534	26.740928
213.054524	6844.138137	26.745946
213.040007	6840.409063	26.750964
213.578431	6852.867180	26.755981
213.671433	6863.595278	26.760999
214.197817	6857.512252	26.766016
214.379923	6866.998485	26.771034
214.456856	6878.000578	26.776052
214.904592	6882.820752	26.781069
214.611046	6893.763732	26.786087
215.154658	6898.868880	26.791104
215.374429	6905.795416	26.796122
215.213876	6903.929483	26.801140
215.663637	6911.161148	26.806157
215.737605	6927.666047	26.811175
216.277071	6926.429820	26.816192
216.373290	6941.921088	26.821210
216.441666	6951.526090	26.826228
217.018909	6952.244361	26.831245
217.005568	6957.357317	26.836263
217.304704	6978.218333	26.841280
217.322672	6979.702394	26.846298
217.548043	6993.086942	26.851316
217.924116	7002.599870	26.856333
217.992948	7025.072050	26.861351
218.158834	7016.197640	26.866368
218.262451	7035.839060	26.871386
218.529161	7036.731954	26.876404
218.881928	7048.079495	26.881421
219.264135	7062.554037	26.886439
219.419413	7071.021740	26.891456
219.230613	7079.138940	26.896474
219.712944	7091.002998	26.901492
220.042733	7097.502089	26.906509
220.311246	7112.448955	26.911527
220.793025	7125.853660	26.916544
220.525701	7143.756703	26.921562
221.025859	7136.336009	26.926580
221.359055	7152.387204	26.931597
221.258705	7166.602330	26.936615
222.130730	7165.109118	26.941632
222.286920	7165.299464	26.946650
222.325740	7176.320297	26.951668
222.621057	7188.043064	26.956685
222.387274	7190.099844	26.961703
222.954711	7199.699886	26.966720
223.274084	7202.497645	26.971738
222.955951	7213.072133	26.976756
223.462867	7221.857669	26.981773
223.661076	7245.228622	26.986791
223.844099	7246.870105	26.991808
223.751356	7252.759466	26.996826
224.212502	7267.831155	27.001844
224.374501	7282.671626	27.006861
224.234741	7293.461468	27.011879
225.017066	7300.016452	27.016896
225.463843	7317.997900	27.021914
225.318919	7319.305309	27.026932
225.861876	7334.389571	27.031949
225.539628	7342.852822	27.036967
225.920045	7354.041561	27.041984
226.193343	7368.905812	27.047002
226.399613	7373.577455	27.052020
226.840909	7386.594043	27.057037
227.368040	7392.434295	27.062055
227.451436	7399.994686	27.067072
227.380408	7419.720531	27.072090
227.786111	7419.098595	27.077108
228.115833	7428.773649	27.082125
228.159734	7447.720819	27.087143
228.697191	7446.263890	27.092160
228.786221	7454.615808	27.097178
228.795464	7445.131042	27.102196
229.071393	7457.327378	27.107213
229.414752	7468.149442	27.112231
229.929529	7467.706251	27.117248
230.190795	7462.295683	27.122266
230.342102	7486.902280	27.127284
230.808547	7484.518803	27.132301
230.662601	7487.862586	27.137319
230.695261	7490.108372	27.142336
230.949749	7487.918895	27.147354
231.044365	7508.783945	27.152372
231.756615	7511.719471	27.157389
231.534692	7517.594302	27.162407
231.900499	7533.479752	27.167424
231.875342	7547.153104	27.172442
231.926187	7547.476661	27.177460
232.244482	7554.612245	27.182477
232.582127	7572.569893	27.187495
232.616677	7584.384022	27.192512
233.091282	7594.541716	27.197530
233.656756	7599.084883	27.202548
233.699451	7606.238139	27.207565
233.720565	7618.657355	27.212583
234.246198	7631.834619	27.217600
234.421950	7630.812820	27.222618
234.177138	7645.426482	27.227636
234.868539	7662.091626	27.232653
234.605007	7663.761630	27.237671
235.454804	7677.557728	27.242688
235.437489	7693.199898	27.247706
235.477057	7706.607579	27.252724
236.002124	7709.730127	27.257741
236.198555	7728.069804	27.262759
236.340337	7740.302998	27.267776
236.840514	7751.009263	27.272794
236.832823	7768.073782	27.277812
237.531522	7768.867889	27.282829
237.673574	7784.870473	27.287847
237.789765	7787.138017	27.292864
238.633034	7783.442525	27.297882
238.655551	7803.823492	27.302900
238.699227	7815.045997	27.307917
238.566291	7824.654385	27.312935
238.699955	7825.997380	27.317952
238.674398	7845.205173	27.322970
239.327550	7863.038218	27.327988
239.593533	7861.566698	27.333005
239.827088	7882.318988	27.338023
240.087025	7888.633503	27.343040
240.236156	7906.412467	27.348058
240.442011	7917.110983	27.353076
240.904987	7912.237137	27.358093
240.932223	7929.640478	27.363111
241.049733	7946.070059	27.368128
241.503766	7956.932007	27.373146
242.097403	7978.404964	27.378164
241.851358	7992.450833	27.383181
242.112779	7997.956966	27.388199
242.513440	8010.923498	27.393216
242.132622	8016.756928	27.398234
242.397757	8035.073587	27.403252
243.045103	8057.223343	27.408269
243.258643	8062.462290	27.413287
243.389243	8092.332489	27.418304
243.719681	8092.874559	27.423322
244.031770	8110.735688	27.428340
244.502278	8117.083796	27.433357
244.433258	8128.046220	27.438375
244.820118	8138.909262	27.443392
245.498507	8149.805850	27.448410
245.147426	8149.121763	27.453428
245.371671	8162.238992	27.458445
245.608333	8171.622696	27.463463
245.723054	8197.511376	27.468480
245.907043	8199.844184	27.473498
246.389617	8223.841399	27.478516
246.754599	8228.946320	27.483533
246.798375	8251.168178	27.488551
247.249519	8257.929765	27.493568
247.451983	8270.687402	27.498586
247.497182	8294.370800	27.503604
247.504860	8291.032607	27.508621
247.882461	8313.966573	27.513639
248.347254	8327.886244	27.518656
248.558136	8337.160392	27.523674
248.891831	8356.183347	27.528692
249.282957	8355.519454	27.533709
249.444358	8388.823369	27.538727
249.627771	8389.732458	27.543744
250.315542	8394.815585	27.548762
250.036444	8422.840082	27.553780
250.894237	8425.083802	27.558797
251.227085	8431.166159	27.563815
251.392941	8441.353448	27.568832
251.415594	8454.574882	27.573850
251.544264	8462.479096	27.578868
251.846788	8469.349140	27.583885
251.886748	8479.827559	27.588903
251.878681	8501.088567	27.593920
252.548389	8508.722301	27.598938
252.615478	8535.569151	27.603956
252.960576	8549.027747	27.608973
253.364729	8560.652362	27.613991
253.285600	8582.783256	27.619008
253.829087	8584.902290	27.624026
253.842230	8603.366086	27.629044
254.131712	8614.364540	27.634061
254.461928	8645.963060	27.639079
254.781158	8650.870010	27.644096
255.110596	8664.646840	27.649114
255.186151	8678.008581	27.654132
255.651557	8688.585052	27.659149
255.759021	8706.175532	27.664167
256.090761	8721.811586	27.669184
256.794681	8732.107850	27.674202
256.695555	8752.025762	27.679220
257.062491	8757.566210	27.684237
257.183341	8763.028157	27.689255
257.453664	8783.068540	27.694272
258.192362	8784.544724	27.699290
258.216857	8792.793639	27.704308
257.867144	8810.862665	27.709325
258.486069	8815.880857	27.714343
258.771414	8828.708063	27.719360
259.177501	8844.241088	27.724378
259.689589	8862.248608	27.729396
259.713229	8864.454922	27.734413
260.150858	8870.312740	27.739431
260.235136	8878.722872	27.744448
260.773664	8870.127372	27.749466
261.179483	8890.080477	27.754484
261.062606	8903.718598	27.759501
261.478010	8894.599226	27.764519
261.413464	8904.784756	27.769536
261.726752	8907.384825	27.774554
262.079654	8926.800021	27.779572
261.847735	8928.481001	27.784589
262.313426	8947.992317	27.789607
262.487990	8958.440579	27.794624
262.931418	8972.092549	27.799642
262.620746	8985.277855	27.804660
262.816411	9006.498254	27.809677
263.101959	9012.471352	27.814695
263.554742	9037.992861	27.819712
264.400708	9031.704672	27.824730
265.316732	9053.273921	27.829748
265.684417	9047.442207	27.834765
265.674948	9050.405105	27.839783
265.869684	9053.677187	27.844800
265.927592	9049.797475	27.849818
266.026468	9062.180298	27.854836
265.954251	9064.878293	27.859853
266.318485	9074.564628	27.864871
266.591676	9099.662706	27.869888
266.809991	9110.476790	27.874906
267.124734	9127.410278	27.879924
267.066628	9131.173215	27.884941
267.381031	9141.467208	27.889959
267.939013	9160.759164	27.894976
267.951931	9181.395719	27.899994
268.110117	9193.169529	27.905012
268.685726	9205.636087	27.910029
269.350854	9216.942652	27.915047
269.680112	9235.004257	27.920064
269.922005	9229.248900	27.925082
270.320967	9240.126495	27.930100
270.692665	9247.390183	27.935117
271.443606	9238.259448	27.940135
271.089570	9248.133472	27.945152
271.423758	9253.325560	27.950170
272.251478	9265.506647	27.955188
272.211022	9264.976216	27.960205
272.181948	9273.123183	27.965223
272.726828	9273.420373	27.970240
272.859577	9289.128931	27.975258
272.580436	9287.031796	27.980276
272.858547	9297.568317	27.985293
273.541064	9307.719848	27.990311
273.422802	9318.087614	27.995328
273.598419	9335.061896	28.000346
273.693378	9354.855523	28.005364
273.950173	9374.863925	28.010381
274.381583	9390.636574	28.015399
274.370539	9412.685242	28.020416
274.808766	9418.271621	28.025434
275.307068	9435.505166	28.030452
275.365965	9453.773252	28.035469
275.947798	9455.987452	28.040487
276.209236	9474.037749	28.045504
276.538425	9486.230293	28.050522
276.608578	9503.953630	28.055540
276.992082	9513.040475	28.060557
277.307123	9520.799308	28.065575
277.311133	9532.982521	28.070592
277.979117	9551.986236	28.075610
278.502922	9569.054916	28.080628
278.659521	9574.972498	28.085645
278.825933	9577.633417	28.090663
278.496671	9596.940825	28.095680
279.162386	9614.461043	28.100698
279.554162	9631.566122	28.105716
279.360873	9654.581159	28.110733
279.953364	9651.438986	28.115751
280.185790	9676.269508	28.120768
280.756867	9670.734292	28.125786
281.251277	9686.737339	28.130804
281.556764	9703.278136	28.135821
281.351214	9702.141939	28.140839
281.734340	9717.170951	28.145856
282.176000	9732.721287	28.150874
282.155629	9734.659873	28.155892
282.189006	9751.855590	28.160909
282.889315	9756.637204	28.165927
283.887056	9756.649204	28.170944
284.524136	9756.531074	28.175962
284.769900	9756.420191	28.180980
284.610577	9749.397917	28.185997
285.208136	9753.377789	28.191015
284.767294	9753.326441	28.196032
285.168885	9765.899403	28.201050
285.526398	9780.913511	28.206068
285.465787	9790.536914	28.211085
285.704919	9792.924487	28.216103
285.801322	9807.688796	28.221120
286.173678	9825.324346	28.226138
286.695431	9829.309722	28.231156
286.556890	9863.850133	28.236173
286.856388	9860.942979	28.241191
287.194723	9884.169164	28.246208
287.228451	9905.403174	28.251226
287.688217	9917.932451	28.256244
287.790949	9946.745963	28.261261
288.243377	9967.062380	28.266279
288.480865	9984.804327	28.271296
288.747796	10003.533109	28.276314
289.757170	10012.642740	28.281332
289.471448	10033.566693	28.286349
289.869303	10051.043779	28.291367
290.103969	10064.097587	28.296384
290.356981	10087.839328	28.301402
290.908345	10081.296709	28.306420
291.546309	10095.822224	28.311437
291.755912	10106.455120	28.316455
292.138603	10118.949173	28.321472
292.411832	10135.429072	28.326490
292.789578	10138.003495	28.331508
292.830492	10158.220005	28.336525
293.498659	10161.456467	28.341543
293.165796	10168.536572	28.346560
293.577477	10188.098651	28.351578
293.681255	10202.767404	28.356596
293.607961	10220.090668	28.361613
294.009771	10245.182901	28.366631
294.157301	10267.542576	28.371648
294.547300	10285.674682	28.376666
295.002439	10294.570788	28.381684
295.127493	10331.300139	28.386701
295.652213	10349.641823	28.391719
295.558974	10368.518611	28.396736
296.012296	10387.944963	28.401754
296.540482	10401.944736	28.406772
296.632245	10427.293872	28.411789
297.296148	10440.375841	28.416807
297.511234	10465.036458	28.421824
297.688707	10481.790480	28.426842
298.316519	10484.357595	28.431860
298.496237	10506.958824	28.436877
298.925855	10517.807138	28.441895
299.104284	10534.374770	28.446912
299.638038	10553.624587	28.451930
300.181145	10562.355570	28.456948
300.121019	10574.015844	28.461965
300.729375	10568.127244	28.466983
300.512882	10584.958480	28.472000
300.983298	10590.035014	28.477018
301.285341	10601.032693	28.482036
301.368128	10618.493057	28.487053
301.416871	10627.364184	28.492071
301.783021	10648.424146	28.497088
302.180094	10661.917234	28.502106
302.771241	10669.781964	28.507124
302.888231	10686.896062	28.512141
303.151828	10703.286398	28.517159
303.752996	10722.990041	28.522176
303.658183	10729.070272	28.527194
303.924408	10749.252345	28.532212
304.571149	10768.705817	28.537229
304.959861	10782.563403	28.542247
305.251442	10799.852502	28.547264
305.424334	10817.166410	28.552282
305.838771	10827.392089	28.557300
306.047097	10838.455018	28.562317
306.063363	10850.681389	28.567335
307.153865	10851.496745	28.572352
306.884842	10882.052514	28.577370
307.604161	10890.772006	28.582388
307.781548	10906.853878	28.587405
308.307406	10922.988868	28.592423
308.372655	10929.006355	28.597440
308.842743	10953.728958	28.602458
308.679538	10957.878052	28.607476
308.828498	10981.706596	28.612493
309.174656	11002.716393	28.617511
309.582057	11013.675811	28.622528
309.680188	11035.778866	28.627546
310.190320	11051.929046	28.632564
310.311206	11077.198749	28.637581
310.653032	11089.216716	28.642599
311.350428	11116.824850	28.647616
311.132434	11137.928944	28.652634
311.499444	11152.137511	28.657652
312.199911	11183.947938	28.662669
312.415831	11197.927459	28.667687
312.793995	11221.711152	28.672704
312.915149	11237.833639	28.677722
313.370911	11253.752485	28.682740
313.703654	11273.176429	28.687757
314.014748	11300.144000	28.692775
314.049325	11313.662420	28.697792
314.624992	11335.754635	28.702810
314.914891	11345.235858	28.707828
314.946551	11371.479748	28.712845
315.460203	11400.433613	28.717863
315.823027	11408.814153	28.722880
316.215207	11429.564659	28.727898
316.864971	11443.053707	28.732916
317.412990	11471.778143	28.737933
317.723880	11485.812562	28.742951
317.840395	11488.819385	28.747968
317.754510	11503.739718	28.752986
318.202870	11511.219706	28.758004
318.508546	11533.098423	28.763021
319.307548	11551.840653	28.768039
319.952243	11553.947441	28.773056
320.384040	11560.530112	28.778074
321.368575	11559.325354	28.783092
321.992716	11553.872898	28.788109
321.895558	11560.749479	28.793127
322.216724	11554.674781	28.798144
321.715798	11554.004413	28.803162
322.456094	11547.586598	28.808180
322.389024	11552.014512	28.813197
322.521631	11563.768543	28.818215
322.717305	11575.613805	28.823232
322.788411	11584.144041	28.828250
323.349016	11586.437592	28.833268
323.348127	11604.546581	28.838285
323.607081	11628.554595	28.843303
324.131485	11640.358194	28.848320
323.972179	11671.580210	28.853338
324.288385	11684.047772	28.858356
324.491012	11700.947379	28.863373
324.443790	11717.374362	28.868391
324.859964	11745.314552	28.873408
325.137800	11771.628035	28.878426
325.998018	11794.219606	28.883444
325.959323	11817.718457	28.888461
326.507564	11841.741701	28.893479
326.614478	11859.651009	28.898496
327.019508	11887.056345	28.903514
327.452465	11907.289493	28.908532
327.821518	11923.936039	28.913549
328.021404	11943.308737	28.918567
328.560155	11961.766656	28.923584
328.709516	11993.443221	28.928602
329.419220	12001.732133	28.933620
329.774014	12030.531716	28.938637
330.089027	12055.744096	28.943655
330.780778	12056.005848	28.948672
330.780088	12093.964466	28.953690
331.416106	12096.697891	28.958708
331.626531	12117.834275	28.963725
331.669114	12136.887473	28.968743
332.167865	12156.093870	28.973760
332.711792	12180.595032	28.978778
332.870044	12190.188753	28.983796
333.616603	12202.346518	28.988813
333.696813	12222.833859	28.993831
333.951357	12237.164964	28.998848
334.252524	12266.386918	29.003866
334.580947	12283.321145	29.008884
334.763772	12295.039395	29.013901
335.103495	12317.381070	29.018919
335.638350	12329.022432	29.023936
336.069073	12354.191937	29.028954
336.527044	12369.246170	29.033972
336.572458	12375.314576	29.038989
336.755981	12408.044361	29.044007
337.331099	12418.874288	29.049024
337.608358	12442.931017	29.054042
337.517337	12462.507426	29.059060
338.128745	12485.637491	29.064077
338.124844	12499.860617	29.069095
338.534863	12521.212686	29.074112
338.704419	12563.355038	29.079130
339.251563	12586.627858	29.084148
339.557930	12601.159585	29.089165
339.855379	12627.496475	29.094183
340.530450	12644.812834	29.099200
340.916484	12672.351740	29.104218
341.038235	12695.934072	29.109236
341.727226	12709.976856	29.114253
341.884878	12736.294611	29.119271
342.590009	12743.482495	29.124288
343.306375	12764.828199	29.129306
343.302669	12774.785316	29.134324
343.497467	12787.563030	29.139341
343.907386	12806.982863	29.144359
343.897627	12823.875492	29.149376
344.360681	12829.661136	29.154394
344.457469	12849.316073	29.159412
344.896088	12868.213620	29.164429
345.044346	12891.782596	29.169447
345.810225	12904.168331	29.174464
346.091071	12917.197994	29.179482
346.319939	12942.841807	29.184500
346.541544	12954.576535	29.189517
346.926544	12973.867791	29.194535
347.356381	12981.041785	29.199552
348.246783	13006.794271	29.204570
348.340028	13008.980765	29.209588
349.117800	13029.057231	29.214605
349.541443	13046.905727	29.219623
350.050378	13044.972836	29.224640
350.021749	13067.290643	29.229658
350.381354	13077.065044	29.234676
351.097376	13085.366087	29.239693
350.952871	13093.842154	29.244711
351.116109	13111.156522	29.249728
351.473979	13120.527010	29.254746
351.746625	13142.216956	29.259764
352.251461	13154.094029	29.264781
352.141926	13189.144455	29.269799
352.893178	13200.676881	29.274816
353.130529	13211.957743	29.279834
353.332575	13245.159778	29.284852
353.505007	13258.740237	29.289869
353.958562	13286.152687	29.294887
354.312033	13299.591307	29.299904
354.753411	13327.233080	29.304922
355.052756	13357.581219	29.309940
355.670410	13378.668250	29.314957
355.573303	13404.799229	29.319975
356.290311	13419.352921	29.324992
356.511323	13439.191238	29.330010
356.618114	13467.722152	29.335028
357.296165	13488.670429	29.340045
357.359482	13522.715607	29.345063
357.915579	13541.112377	29.350080
358.334989	13566.171576	29.355098
358.563629	13588.854160	29.360116
359.117838	13605.002836	29.365133
359.358123	13628.097344	29.370151
359.899880	13651.056524	29.375168
360.516710	13669.942920	29.380186
360.572292	13690.590426	29.385204
361.229893	13712.824265	29.390221
360.986900	13738.151030	29.395239
361.185566	13763.911186	29.400256
361.892913	13781.454098	29.405274
362.561159	13798.349414	29.410292
363.263849	13814.443573	29.415309
363.396944	13841.221437	29.420327
363.865230	13853.436229	29.425344
363.859449	13869.697575	29.430362
363.883248	13891.866081	29.435380
364.542825	13917.494689	29.440397
365.026796	13942.298012	29.445415
365.273770	13973.141621	29.450432
365.681931	13980.657278	29.455450
365.934235	14006.014662	29.460468
365.848055	14036.998666	29.465485
366.325194	14065.561247	29.470503
367.197901	14091.971679	29.475520
367.447935	14103.775330	29.480538
367.523230	14124.644459	29.485556
367.781932	14144.104999	29.490573
368.117561	14172.162381	29.495591
368.832410	14188.968682	29.500608
370.079393	14191.203076	29.505626
370.575538	14205.905450	29.510644
370.744773	14203.074762	29.515661
370.912299	14220.035776	29.520679
371.165109	14223.710272	29.525696
371.894081	14230.822384	29.530714
372.060361	14252.861755	29.535732
372.696694	14260.828341	29.540749
372.851094	14276.897722	29.545767
373.269156	14282.308695	29.550784
373.781428	14291.058856	29.555802
373.780831	14302.983759	29.560820
374.272142	14318.754396	29.565837
374.471479	14342.339332	29.570855
374.559693	14364.523626	29.575872
375.169722	14369.955268	29.580890
375.267852	14400.750109	29.585908
375.396651	14422.347067	29.590925
375.764658	14449.452396	29.595943
376.002016	14479.733029	29.600960
376.555980	14501.639698	29.605978
376.666561	14535.543536	29.610996
377.291498	14548.662869	29.616013
377.588483	14575.182554	29.621031
378.082986	14608.720417	29.626048
378.228827	14635.020541	29.631066
378.517824	14668.037832	29.636084
378.766322	14688.975360	29.641101
379.481093	14714.634351	29.646119
379.892215	14743.002952	29.651136
380.445884	14767.243830	29.656154
380.613939	14801.262360	29.661172
381.069903	14812.349076	29.666189
381.992404	14847.895628	29.671207
382.269058	14872.858768	29.676224
382.950130	14885.356915	29.681242
383.111129	14911.945611	29.686260
383.361089	14922.644428	29.691277
383.468845	14951.000562	29.696295
383.989925	14973.216078	29.701312
384.454240	14994.764609	29.706330
384.828051	15027.532457	29.711348
385.617167	15043.307865	29.716365
386.379724	15040.239408	29.721383
387.460832	15046.491673	29.726400
387.904779	15061.818682	29.731418
388.157487	15068.326248	29.736436
388.235439	15067.954076	29.741453
388.549275	15076.318614	29.746471
388.816920	15085.707282	29.751488
389.366391	15097.278601	29.756506
389.216118	15121.114737	29.761524
389.976538	15131.828949	29.766541
390.184052	15153.313418	29.771559
389.784402	15169.106615	29.776576
390.440309	15177.253717	29.781594
391.028907	15212.284456	29.786612
391.101668	15229.191643	29.791629
391.262473	15253.595365	29.796647
391.696718	15285.327829	29.801664
392.172885	15300.877407	29.806682
392.209057	15333.215137	29.811700
392.657313	15348.563814	29.816717
392.879755	15381.570595	29.821735
392.928033	15413.830779	29.826752
393.623479	15438.593658	29.831770
393.869550	15469.594587	29.836788
394.582373	15486.329715	29.841805
395.287373	15520.006958	29.846823
395.599571	15540.720743	29.851840
395.951984	15556.855124	29.856858
396.060359	15588.300889	29.861876
396.434511	15612.675014	29.866893
397.159431	15634.107899	29.871911
397.035101	15658.626010	29.876928
397.824066	15677.816070	29.881946
398.169080	15713.065672	29.886964
398.388356	15744.229131	29.891981
398.877960	15770.000399	29.896999
399.502864	15794.098846	29.902016
400.131704	15812.916025	29.907034
400.727992	15841.677487	29.912052
400.958771	15865.354161	29.917069
401.357933	15887.134926	29.922087
401.609349	15912.207579	29.927104
402.625874	15928.409434	29.932122
402.824612	15957.990960	29.937140
402.941225	15972.968554	29.942157
403.869549	15991.038135	29.947175
403.981026	16004.222619	29.952192
404.562148	16015.066311	29.957210
405.040508	16047.841742	29.962228
405.401791	16063.940429	29.967245
405.876392	16087.427818	29.972263
406.080248	16104.195351	29.977280
406.641482	16112.161776	29.982298
407.046410	16140.533419	29.987316
407.458338	16154.476614	29.992333
408.076937	16170.983819	29.997351
408.519002	16194.476405	30.002368
408.783267	16202.059563	30.007386
409.174347	16223.226087	30.012404
409.415421	16248.313423	30.017421
409.560986	16263.147768	30.022439
409.416282	16299.093731	30.027456
409.952213	16324.498478	30.032474
410.539878	16356.771028	30.037492
410.739967	16378.927610	30.042509
411.388291	16410.135902	30.047527
411.616916	16443.749964	30.052544
412.372936	16466.451781	30.057562
412.461776	16499.490762	30.062580
412.867223	16529.865337	30.067597
413.695333	16548.472188	30.072615
414.568798	16565.161146	30.077632
415.254460	16581.629840	30.082650
415.356345	16601.941651	30.087668
415.833475	16619.987317	30.092685
416.306156	16637.022992	30.097703
415.993073	16658.877616	30.102720
416.539647	16688.030261	30.107738
417.138665	16713.154076	30.112756
417.485401	16738.996267	30.117773
418.165081	16760.551163	30.122791
418.178054	16788.871079	30.127808
418.562197	16801.969444	30.132826
419.283754	16835.030523	30.137844
419.305928	16859.173609	30.142861
419.895412	16883.124176	30.147879
420.201532	16913.486395	30.152896
420.906650	16932.889754	30.157914
421.382033	16956.182260	30.162932
421.477351	16981.877567	30.167949
422.086779	16998.279525	30.172967
421.953025	17019.636023	30.177984
422.808847	17038.494875	30.183002
423.245200	17059.254142	30.188020
422.975268	17087.024739	30.193037
423.670482	17102.980716	30.198055
423.987885	17135.789379	30.203072
424.808214	17152.376574	30.208090
425.406378	17182.706386	30.213108
426.017904	17208.299522	30.218125
426.560698	17221.360840	30.223143
426.726896	17252.282327	30.228160
427.373344	17270.106415	30.233178
427.461366	17298.762837	30.238196
427.686333	17316.456754	30.243213
427.990435	17331.914746	30.248231
428.458384	17376.143827	30.253248
428.750051	17402.680890	30.258266
429.043263	17422.679509	30.263284
429.817378	17457.600191	30.268301
430.543626	17480.070949	30.273319
430.910783	17509.514934	30.278336
432.246104	17513.861727	30.283354
432.878969	17521.388023	30.288372
433.459694	17525.005793	30.293389
433.922473	17538.218762	30.298407
433.769116	17550.921210	30.303424
434.303403	17568.538777	30.308442
434.802220	17580.804905	30.313460
435.011964	17606.546402	30.318477
435.097397	17619.698145	30.323495
435.583731	17643.570961	30.328512
436.040346	17665.243724	30.333530
436.180273	17689.240014	30.338548
436.429629	17721.109524	30.343565
436.912191	17749.082944	30.348583
437.151577	17777.618594	30.353600
437.817369	17811.135398	30.358618
438.124523	17840.349173	30.363636
438.319920	17868.929709	30.368653
439.031538	17894.858785	30.373671
439.343255	17936.934007	30.378688
439.554744	17971.696834	30.383706
440.505935	17997.392914	30.388724
440.511222	18034.626444	30.393741
441.476885	18049.062846	30.398759
441.889614	18086.548913	30.403776
442.147701	18116.920502	30.408794
442.551281	18145.980745	30.413812
442.699217	18185.435024	30.418829
443.531170	18206.948884	30.423847
444.295375	18229.041882	30.428864
444.470788	18260.961696	30.433882
445.180790	18280.251943	30.438900
445.660230	18315.807572	30.443917
445.976916	18345.380718	30.448935
446.381317	18386.179000	30.453952
447.118592	18395.338241	30.458970
447.372738	18425.414007	30.463988
447.568790	18449.686788	30.469005
448.181349	18468.177438	30.474023
448.980043	18494.611796	30.479040
449.179402	18518.309256	30.484058
449.672254	18530.507424	30.489076
450.620623	18555.048585	30.494093
451.648096	18568.389145	30.499111
451.690897	18572.842642	30.504128
452.145800	18584.219158	30.509146
452.937755	18594.848282	30.514164
453.056411	18617.440226	30.519181
453.302462	18613.718800	30.524199
453.570030	18635.074617	30.529216
453.930333	18654.602887	30.534234
454.307306	18676.573472	30.539252
454.071916	18698.121374	30.544269
454.788735	18729.711291	30.549287
455.101263	18759.007742	30.554304
455.559109	18793.828455	30.559322
455.870256	18813.819403	30.564340
456.369847	18848.355741	30.569357
456.954187	18873.762631	30.574375
457.207245	18906.903354	30.579392
457.914808	18937.629536	30.584410
458.225834	18960.886871	30.589428
458.330514	18987.726875	30.594445
459.027387	19010.526190	30.599463
459.737302	19050.355928	30.604480
460.010510	19075.969461	30.609498
460.691214	19102.233488	30.614516
460.674296	19141.633243	30.619533
461.268664	19167.272711	30.624551
461.704425	19204.043450	30.629568
461.826421	19242.815284	30.634586
462.654410	19274.571994	30.639604
463.024649	19320.823450	30.644621
463.658228	19348.238660	30.649639
464.292924	19382.047322	30.654656
464.408351	19412.405240	30.659674
465.353785	19457.183879	30.664692
465.373427	19495.460408	30.669709
466.237600	19520.407604	30.674727
467.076740	19546.281132	30.679744
467.380703	19577.658716	30.684762
467.871492	19600.541349	30.689780
468.167720	19640.063943	30.694797
468.965494	19664.617318	30.699815
469.616399	19686.306320	30.704832
470.001005	19721.525484	30.709850
470.674063	19743.318505	30.714868
470.737423	19772.194065	30.719885
471.520892	19793.906775	30.724903
471.889149	19821.736714	30.729920
472.090642	19861.476677	30.734938
472.583534	19872.848036	30.739956
472.934941	19913.689360	30.744973
473.298489	19946.631430	30.749991
474.005313	19975.501887	30.755008
474.499733	20009.693600	30.760026
475.191515	20029.853989	30.765044
475.830184	20059.240619	30.770061
476.590489	20079.895831	30.775079
477.376189	20104.521139	30.780096
477.325376	20131.089976	30.785114
478.049635	20147.107129	30.790132
478.087468	20166.251174	30.795149
478.489467	20192.155706	30.800167
478.824062	20214.905426	30.805184
478.947932	20251.676149	30.810202
479.655158	20279.782509	30.815220
480.395083	20307.599506	30.820237
480.659800	20338.611655	30.825255
481.431728	20370.549469	30.830272
481.547575	20408.282086	30.835290
482.382691	20431.554358	30.840308
482.694616	20456.974132	30.845325
482.997043	20478.970992	30.850343
483.490862	20504.924825	30.855360
483.584325	20541.726099	30.860378
484.152181	20563.182598	30.865396
484.426224	20594.092609	30.870413
484.774005	20627.139370	30.875431
485.430897	20661.964022	30.880448
485.457933	20695.806377	30.885466
485.982504	20733.134807	30.890484
486.535308	20778.242966	30.895501
487.441476	20822.000978	30.900519
488.294818	20855.866610	30.905536
488.257014	20898.666055	30.910554
489.057461	20917.174013	30.915572
489.382377	20951.987678	30.920589
489.752182	20988.430854	30.925607
490.671934	21017.554026	30.930624
490.969559	21056.510614	30.935642
491.536918	21091.507924	30.940660
491.968633	21129.609763	30.945677
492.224958	21164.933632	30.950695
492.719233	21187.868128	30.955712
492.913077	21237.778311	30.960730
493.999868	21279.082969	30.965748
494.154251	21317.803320	30.970765
494.528633	21361.064029	30.975783
495.114744	21392.211042	30.980800
495.664731	21440.417187	30.985818
496.086086	21478.129571	30.990836
496.534444	21516.166382	30.995853
497.447293	21561.315065	31.000871
497.900563	21596.002473	31.005888
497.853332	21641.269209	31.010906
498.690163	21675.480024	31.015924
498.986187	21722.405826	31.020941
499.638695	21765.662036	31.025959
500.100606	21799.893523	31.030976
500.479939	21846.212706	31.035994
501.265987	21879.818882	31.041012
502.045213	21926.644672	31.046029
502.494975	21969.231527	31.051047
503.094857	21989.698897	31.056064
503.654645	22037.323664	31.061082
504.728958	22066.620208	31.066100
505.237366	22094.121936	31.071117
505.406235	22119.844151	31.076135
506.061018	22156.005014	31.081152
506.457800	22188.579186	31.086170
507.165582	22214.047023	31.091188
507.331344	22261.076527	31.096205
508.161960	22285.805002	31.101223
509.013809	22305.159294	31.106240
509.051812	22348.986351	31.111258
509.753713	22376.749013	31.116276
510.509004	22406.399026	31.121293
510.902572	22436.794140	31.126311
511.398756	22462.472165	31.131328
511.840731	22491.785637	31.136346
512.517115	22516.266705	31.141364
513.201761	22535.009056	31.146381
513.580236	22560.673939	31.151399
514.199578	22581.960338	31.156416
514.375330	22609.887382	31.161434
515.014488	22632.080660	31.166452
515.809221	22663.955463	31.171469
516.132875	22693.192872	31.176487
516.923363	22708.986971	31.181504
516.953983	22743.438887	31.186522
517.584311	22756.142762	31.191540
518.054723	22786.393754	31.196557
517.837594	22811.810465	31.201575
519.099211	22834.058721	31.206592
518.813317	22868.067254	31.211610
519.628977	22885.285646	31.216628
519.998175	22920.904710	31.221645
520.608495	22959.411962	31.226663
520.780239	22985.880488	31.231680
520.969136	23018.576854	31.236698
521.615478	23061.375578	31.241716
521.896047	23096.591703	31.246733
522.573768	23136.580083	31.251751
522.948490	23167.630108	31.256768
523.306197	23215.030088	31.261786
523.918766	23258.548543	31.266804
524.624217	23306.052581	31.271821
525.099681	23365.908366	31.276839
526.025582	23388.234787	31.281856
526.627079	23432.785353	31.286874
527.155932	23477.296776	31.291892
528.107048	23512.605142	31.296909
528.304576	23549.187283	31.301927
528.797352	23578.317519	31.306944
529.872046	23613.594189	31.311962
530.129835	23641.781634	31.316980
530.612304	23674.717738	31.321997
531.252385	23729.240904	31.327015
532.021764	23753.734302	31.332032
532.433592	23792.116089	31.337050
532.950125	23822.917570	31.342068
533.610539	23851.883087	31.347085
533.737553	23895.383736	31.352103
534.272734	23923.395693	31.357120
534.659930	23974.394852	31.362138
534.927836	24019.017620	31.367156
535.992698	24051.598274	31.372173
536.073053	24096.560057	31.377191
536.591532	24140.739655	31.382208
537.434606	24183.061496	31.387226
537.706545	24228.252842	31.392244
537.945384	24260.722296	31.397261
538.470761	24313.110020	31.402279
539.314622	24354.736974	31.407296
539.963229	24393.127293	31.412314
540.324844	24450.027629	31.417332
541.314469	24491.682732	31.422349
541.887830	24543.001928	31.427367
542.286881	24572.047096	31.432384
543.004073	24616.038824	31.437402
543.389592	24647.569752	31.442420
544.331497	24682.913226	31.447437
544.656558	24731.857524	31.452455
545.251201	24763.059062	31.457472
545.846068	24795.973200	31.462490
546.129750	24839.697974	31.467508
546.963381	24876.404703	31.472525
547.361277	24917.268077	31.477543
548.175344	24956.884990	31.482560
548.706449	24990.972173	31.487578
549.069309	25022.557775	31.492596
549.730208	25051.954690	31.497613
551.094345	25079.175664	31.502631
552.506847	25090.767095	31.507648
553.174834	25111.618901	31.512666
553.716960	25129.728652	31.517684
554.319082	25136.106195	31.522701
554.283291	25162.793184	31.527719
554.593385	25171.402789	31.532736
554.895369	25193.645098	31.537754
554.855281	25216.850711	31.542772
555.492594	25229.624600	31.547789
556.052884	25268.782386	31.552807
556.674136	25298.160557	31.557824
557.182304	25332.018065	31.562842
557.277095	25369.264136	31.567860
557.954331	25390.626687	31.572877
557.931577	25434.368863	31.577895
558.607824	25463.321613	31.582912
559.221541	25509.941457	31.587930
559.358993	25556.755626	31.592948
560.348256	25597.168099	31.597965
560.202179	25629.630175	31.602983
561.024651	25686.184204	31.608000
561.971588	25734.060889	31.613018
562.371401	25779.779328	31.618036
562.861592	25823.739527	31.623053
563.110104	25874.885189	31.628071
563.783230	25920.466600	31.633088
564.430645	25974.773544	31.638106
564.933090	26026.587885	31.643124
565.881096	26068.480263	31.648141
566.590455	26128.743970	31.653159
566.997399	26149.435255	31.658176
567.841328	26202.385035	31.663194
568.051054	26246.573096	31.668212
568.841934	26286.581761	31.673229
569.164586	26324.900120	31.678247
570.033311	26363.215703	31.683264
570.657123	26407.402854	31.688282
571.117062	26461.443253	31.693300
571.879635	26494.251907	31.698317
572.446831	26556.788956	31.703335
572.884534	26588.883610	31.708352
573.478702	26637.164963	31.713370
573.789459	26686.350084	31.718388
574.906262	26717.694575	31.723405
575.768378	26765.827080	31.728423
576.102942	26801.913487	31.733440
576.874046	26839.265550	31.738458
577.355074	26880.922626	31.743476
578.286837	26923.931658	31.748493
578.582067	26968.815846	31.753511
579.288070	27001.375003	31.758528
579.926228	27041.516383	31.763546
580.306713	27084.124919	31.768564
581.187053	27113.541248	31.773581
581.856832	27158.177941	31.778599
582.072055	27195.718323	31.783616
582.737263	27232.247004	31.788634
582.963490	27270.645367	31.793652
583.691179	27309.471363	31.798669
584.263555	27357.403889	31.803687
584.909797	27394.782736	31.808704
585.841749	27423.249754	31.813722
586.284861	27472.194966	31.818740
587.116950	27498.952183	31.823757
587.930916	27525.724897	31.828775
588.167783	27568.306246	31.833792
588.905039	27601.841161	31.838810
589.318743	27635.420180	31.843828
590.091818	27670.226352	31.848845
590.462956	27716.901693	31.853863
591.004722	27735.936626	31.858880
592.045951	27765.480547	31.863898
591.892641	27811.074787	31.868916
592.705023	27845.369504	31.873933
593.751343	27866.474970	31.878951
593.842214	27901.248689	31.883968
594.750080	27924.480488	31.888986
595.208418	27957.250389	31.894004
596.003521	27984.715580	31.899021
596.070349	28018.399795	31.904039
596.555920	28054.085690	31.909056
597.410584	28087.976042	31.914074
597.558633	28132.639213	31.919092
598.257614	28166.004043	31.924109
598.982526	28204.889069	31.929127
599.297215	28258.805173	31.934144
600.351078	28283.443108	31.939162
600.639974	28336.750336	31.944180
601.068029	28372.306688	31.949197
601.364660	28422.654885	31.954215
601.809476	28475.167083	31.959232
602.628431	28520.554666	31.964250
602.910649	28572.125364	31.969268
603.394985	28623.690010	31.974285
604.489789	28679.950856	31.979303
604.809724	28732.451552	31.984320
605.608925	28784.587021	31.989338
605.808277	28834.079111	31.994356
606.514627	28883.827396	31.999373
607.444108	28938.148927	32.004391
608.404450	28995.468185	32.009408
609.146721	29038.106660	32.014426
609.539885	29091.279527	32.019444
610.205703	29136.698639	32.024461
610.991520	29184.583274	32.029479
611.429161	29228.192415	32.034496
611.872042	29279.012981	32.039514
612.218494	29335.885160	32.044532
613.225976	29390.865767	32.049549
614.285335	29422.349801	32.054567
614.605215	29482.330107	32.059584
615.703000	29527.145557	32.064602
616.162941	29573.634328	32.069620
616.695773	29620.598574	32.074637
617.716887	29661.304958	32.079655
618.227229	29712.703950	32.084672
618.772768	29758.427611	32.089690
619.246330	29793.220821	32.094708
619.780919	29834.964090	32.099725
620.376245	29878.196085	32.104743
621.080984	29930.842220	32.109760
621.752971	29968.746426	32.114778
622.744531	30005.621179	32.119796
623.115952	30059.191847	32.124813
623.788472	30089.574037	32.129831
624.260172	30136.744934	32.134848
625.087505	30186.275269	32.139866
625.657494	30233.184560	32.144884
626.541989	30272.383696	32.149901
626.949386	30311.834171	32.154919
627.441518	30358.281777	32.159936
628.232100	30400.226548	32.164954
628.920008	30442.579306	32.169972
629.204360	30488.667633	32.174989
630.256062	30525.710953	32.180007
630.670299	30574.364657	32.185024
631.292312	30608.731574	32.190042
631.730946	30662.097384	32.195060
632.396918	30704.770162	32.200077
633.427968	30744.750192	32.205095
633.450326	30795.349184	32.210112
634.011048	30826.325110	32.215130
634.759072	30869.731378	32.220148
635.311426	30918.313820	32.225165
636.052093	30960.912286	32.230183
636.618380	31004.505164	32.235200
636.587798	31046.212439	32.240218
637.196635	31088.414474	32.245236
637.625822	31136.106312	32.250253
638.820941	31185.423755	32.255271
639.061063	31250.965564	32.260288
639.836797	31301.555978	32.265306
640.310741	31354.241674	32.270324
640.856717	31414.748696	32.275341
641.862632	31460.644680	32.280359
642.783382	31518.090917	32.285376
643.313525	31563.245709	32.290394
643.508587	31617.088088	32.295412
644.235270	31679.084938	32.300429
645.089777	31713.701972	32.305447
646.095042	31775.181618	32.310464
646.800628	31827.181324	32.315482
647.508633	31870.033290	32.320500
648.234256	31925.551306	32.325517
649.420948	31969.409972	32.330535
649.452396	32022.981752	32.335552
650.098014	32062.038139	32.340570
650.895322	32105.382429	32.345588
651.521787	32163.767634	32.350605
652.377395	32208.759372	32.355623
652.824302	32264.663059	32.360640
653.873453	32293.251360	32.365658
654.813736	32334.614107	32.370676
655.555439	32380.034866	32.375693
656.613583	32416.555859	32.380711
656.913244	32452.392112	32.385728
657.574045	32487.021626	32.390746
657.898424	32532.975504	32.395764
658.558709	32581.589290	32.400781
659.165730	32626.266602	32.405799
659.454094	32676.506344	32.410816
660.300251	32721.911589	32.415834
661.027275	32768.682057	32.420852
661.520232	32824.011098	32.425869
662.236071	32865.972497	32.430887
662.763855	32926.739627	32.435904
663.574901	32981.981637	32.440922
664.155111	33030.684800	32.445940
664.532978	33073.685467	32.450957
665.693615	33123.676700	32.455975
666.101720	33173.096092	32.460992
666.979750	33220.406730	32.466010
667.552610	33273.473854	32.471028
667.955273	33322.995601	32.476045
668.940592	33357.278901	32.481063
669.772302	33416.988600	32.486080
670.557347	33461.715851	32.491098
671.289807	33520.992422	32.496116
671.648466	33570.502638	32.501133
672.452596	33598.220477	32.506151
673.571750	33654.453144	32.511168
674.513265	33682.750321	32.516186
674.956733	33719.742297	32.521204
675.495004	33755.720662	32.526221
676.094716	33803.038010	32.531239
676.711700	33860.696049	32.536256
677.208090	33897.155348	32.541274
678.184678	33940.791657	32.546292
678.334516	33997.549155	32.551309
679.127767	34035.859184	32.556327
679.767328	34075.571482	32.561344
680.709805	34118.834130	32.566362
681.120520	34160.940460	32.571380
681.369802	34206.549323	32.576397
682.213677	34248.076282	32.581415
682.660267	34292.668321	32.586432
683.211241	34345.147254	32.591450
683.835708	34394.358812	32.596468
684.214717	34455.438041	32.601485
684.756805	34515.771295	32.606503
685.342025	34566.664826	32.611520
686.202733	34625.488296	32.616538
687.226033	34682.389857	32.621556
687.439772	34744.722224	32.626573
688.374690	34787.639684	32.631591
689.116916	34847.373701	32.636608
689.782355	34910.059853	32.641626
690.421897	34971.460406	32.646644
690.978792	35036.743463	32.651661
692.108073	35098.826867	32.656679
692.914074	35165.696470	32.661696
693.605639	35212.844619	32.666714
694.271669	35266.180464	32.671732
694.908427	35331.881945	32.676749
695.729759	35384.947327	32.681767
696.566333	35436.018798	32.686784
697.482577	35484.865016	32.691802
698.835759	35529.103562	32.696820
699.739090	35595.162699	32.701837
700.354319	35629.722297	32.706855
700.682491	35673.848828	32.711872
701.404103	35725.697634	32.716890
702.496576	35766.992877	32.721908
702.859773	35820.061116	32.726925
703.718681	35856.309296	32.731943
704.612067	35912.089950	32.736960
705.061288	35953.681701	32.741978
705.965950	36000.735204	32.746996
706.445534	36060.165767	32.752013
707.227751	36104.797902	32.757031
707.520741	36155.860882	32.762048
707.962369	36212.654775	32.767066
708.980605	36262.214053	32.772084
709.482378	36327.781556	32.777101
710.322737	36377.444669	32.782119
710.824892	36435.348912	32.787136
711.142138	36490.139527	32.792154
711.788599	36543.886307	32.797172
712.908818	36612.678040	32.802189
713.773156	36661.029197	32.807207
714.169970	36722.877284	32.812224
714.800304	36796.810714	32.817242
715.367977	36855.787162	32.822260
716.051236	36919.273196	32.827277
716.677237	36989.799760	32.832295
717.436862	37048.620395	32.837312
718.369973	37115.722954	32.842330
719.254572	37183.168411	32.847348
719.357335	37238.753128	32.852365
720.204926	37295.619496	32.857383
720.833297	37373.519947	32.862400
721.532413	37445.908342	32.867418
722.857715	37504.363945	32.872436
723.267478	37574.021853	32.877453
723.960997	37635.175079	32.882471
724.601016	37701.458793	32.887488
725.449743	37767.754486	32.892506
726.590486	37818.101388	32.897524
727.017269	37878.341987	32.902541
728.876289	37900.273348	32.907559
730.034595	37937.117136	32.912576
731.097705	37975.291099	32.917594
731.978072	38015.485490	32.922612
732.522718	38051.116031	32.927629
733.022046	38076.370418	32.932647
734.052040	38104.830476	32.937664
734.361714	38148.079702	32.942682
735.184460	38174.472690	32.947700
735.587047	38220.546884	32.952717
736.107218	38261.113986	32.957735
737.050470	38299.047917	32.962752
737.652401	38353.097060	32.967770
738.368819	38388.410536	32.972788
739.637583	38432.383697	32.977805
740.094251	38475.218632	32.982823
740.887703	38516.211625	32.987840
741.500346	38563.537563	32.992858
742.216341	38592.818639	32.997876
742.849096	38653.029347	33.002893
743.236258	38695.881865	33.007911
743.838090	38738.511338	33.012928
744.508177	38794.435456	33.017946
745.374968	38839.022191	33.022964
745.844376	38914.682742	33.027981
746.325976	38967.689762	33.032999
747.234638	39026.979554	33.038016
747.672957	39090.143356	33.043034
748.542115	39148.585913	33.048052
749.222997	39223.967996	33.053069
750.008702	39278.800310	33.058087
750.753247	39352.497098	33.063104
751.564773	39412.688418	33.068122
753.000729	39461.348991	33.073140
753.318235	39521.377207	33.078157
754.079601	39592.972637	33.083175
754.677981	39641.277051	33.088192
755.766037	39709.691629	33.093210
756.702898	39761.889815	33.098228
757.688811	39823.060653	33.103245
758.377017	39880.837709	33.108263
759.116662	39930.290732	33.113280
759.614580	39997.356191	33.118298
760.871276	40042.422263	33.123316
761.333384	40090.881699	33.128333
762.568105	40152.286672	33.133351
763.165747	40209.458935	33.138368
763.640481	40268.946160	33.143386
764.583897	40329.694998	33.148404
765.303927	40386.475546	33.153421
765.860991	40439.765333	33.158439
766.944121	40492.682444	33.163456
767.647701	40557.769747	33.168474
767.968155	40605.474495	33.173492
768.853642	40670.729870	33.178509
769.382108	40729.855830	33.183527
770.300398	40788.668293	33.188544
771.012507	40856.152084	33.193562
771.708484	40907.979439	33.198580
772.913388	40972.155122	33.203597
773.337032	41031.108483	33.208615
774.530302	41085.325367	33.213632
774.757613	41149.653752	33.218650
775.533403	41210.273028	33.223668
776.428328	41275.718478	33.228685
776.923159	41336.527304	33.233703
777.855165	41395.611221	33.238720
778.604445	41450.985945	33.243738
779.270222	41517.498689	33.248756
780.196944	41573.788460	33.253773
781.087422	41631.329960	33.258791
782.354134	41662.679815	33.263808
783.261311	41709.726427	33.268826
784.045877	41766.247534	33.273844
784.754993	41811.320291	33.278861
785.279902	41871.170899	33.283879
786.026159	41911.058190	33.288896
786.762653	41979.110870	33.293914
787.327940	42033.351966	33.298932
787.996683	42090.537058	33.303949
788.582576	42155.388123	33.308967
789.737342	42197.843434	33.313984
790.264699	42269.667495	33.319002
791.004719	42328.543474	33.324020
791.983754	42392.587715	33.329037
792.660204	42456.843690	33.334055
793.576316	42522.820852	33.339072
794.313466	42587.029809	33.344090
795.417902	42650.758013	33.349108
796.087369	42708.709911	33.354125
796.650317	42766.387596	33.359143
797.968007	42835.022892	33.364160
798.497112	42895.621976	33.369178
799.506047	42958.670193	33.374196
800.349762	43023.546930	33.379213
800.722952	43080.325203	33.384231
801.817316	43153.904456	33.389248
802.828199	43222.158615	33.394266
803.522601	43277.793161	33.399284
804.458585	43344.288342	33.404301
804.935292	43403.056378	33.409319
806.032905	43458.957518	33.414336
806.408408	43528.405774	33.419354
807.456984	43597.755798	33.424372
808.105570	43666.459885	33.429389
809.014650	43729.804155	33.434407
810.133274	43788.207630	33.439424
811.253326	43847.224584	33.444442
812.364152	43896.635102	33.449460
813.575246	43941.583474	33.454477
814.247971	43997.893681	33.459495
815.236051	44045.805576	33.464512
815.771000	44112.087179	33.469530
815.950486	44170.252010	33.474548
816.807989	44228.855427	33.479565
817.130624	44295.252854	33.484583
818.408983	44349.540446	33.489600
819.040656	44416.731402	33.494618
820.093992	44475.399866	33.499636
820.732657	44529.913985	33.504653
821.562785	44595.803181	33.509671
822.644981	44643.853527	33.514688
823.459299	44717.627051	33.519706
824.293601	44776.918674	33.524724
825.265313	44830.028031	33.529741
826.360000	44879.481202	33.534759
827.633301	44929.747974	33.539776
828.413622	44986.043934	33.544794
829.180949	45037.237334	33.549812
829.926688	45083.240919	33.554829
830.624783	45136.431552	33.559847
831.508323	45180.231561	33.564864
832.324424	45237.123516	33.569882
833.012681	45291.435683	33.574900
833.995295	45334.486799	33.579917
834.635500	45386.010744	33.584935
835.398062	45432.961280	33.589952
835.662726	45487.523307	33.594970
836.077431	45539.152289	33.599988
837.062848	45586.992009	33.605005
837.403379	45646.173033	33.610023
838.086278	45708.647237	33.615040
839.118676	45781.751427	33.620058
839.475593	45856.112297	33.625076
840.440250	45930.821616	33.630093
840.715843	46004.139225	33.635111
841.840531	46087.484215	33.640128
842.726981	46164.869670	33.645146
843.558605	46232.705501	33.650164
844.432832	46304.317800	33.655181
845.099972	46390.151635	33.660199
845.843759	46469.983182	33.665216
846.935195	46548.192052	33.670234
847.795592	46637.128106	33.675252
848.911114	46708.653523	33.680269
849.637077	46796.086558	33.685287
850.575799	46869.639040	33.690304
851.706669	46952.828120	33.695322
852.871090	47028.104639	33.700340
854.234106	47097.543103	33.705357
854.972669	47175.366249	33.710375
855.583401	47236.299693	33.715392
856.667287	47303.802150	33.720410
857.402680	47375.888623	33.725428
858.647993	47444.517743	33.730445
859.191508	47518.532409	33.735463
860.274643	47585.846037	33.740480
861.134761	47649.974499	33.745498
861.726986	47727.227651	33.750516
862.841624	47799.813155	33.755533
863.579007	47862.784628	33.760551
864.279520	47930.386588	33.765568
865.300190	47994.826331	33.770586
866.269257	48074.792963	33.775604
866.971164	48140.491083	33.780621
867.673316	48214.774342	33.785639
868.752864	48301.019386	33.790656
869.941733	48375.550055	33.795674
870.398220	48457.805769	33.800692
871.506546	48518.924588	33.805709
872.341407	48590.898212	33.810727
873.161318	48665.563183	33.815744
874.173031	48736.345648	33.820762
874.971535	48811.507904	33.825780
875.982738	48882.031510	33.830797
876.730571	48954.873925	33.835815
877.331327	49024.664705	33.840832
878.842594	49087.803802	33.845850
879.828870	49159.407682	33.850868
880.590977	49220.145732	33.855885
881.695815	49280.577523	33.860903
883.501952	49324.286247	33.865920
884.863593	49383.501561	33.870938
885.489828	49437.377815	33.875956
887.330687	49455.774261	33.880973
888.620106	49487.112613	33.885991
889.383962	49520.658627	33.891008
890.192990	49559.341361	33.896026
890.743742	49597.026764	33.901044
891.571683	49628.570010	33.906061
892.270676	49667.010654	33.911079
892.684434	49698.745006	33.916096
893.418782	49745.974612	33.921114
894.020818	49780.906474	33.926132
894.929046	49824.281414	33.931149
895.498549	49867.259952	33.936167
895.823844	49910.036162	33.941184
896.886045	49961.726270	33.946202
897.673496	50019.862131	33.951220
898.777241	50075.323215	33.956237
899.131730	50136.190417	33.961255
899.566592	50194.438547	33.966272
900.680590	50267.867168	33.971290
901.124337	50336.003398	33.976308
902.205039	50393.088557	33.981325
903.158293	50474.369419	33.986343
903.664791	50544.900785	33.991360
904.288744	50611.668436	33.996378
904.817595	50698.419502	34.001396
906.055166	50772.324013	34.006413
906.752329	50864.212459	34.011431
907.733492	50949.343901	34.016448
908.276564	51037.916263	34.021466
909.020731	51125.679408	34.026484
910.148525	51218.717061	34.031501
910.840024	51314.619670	34.036519
911.624393	51414.893057	34.041536
913.326118	51500.319312	34.046554
913.997759	51591.025074	34.051572
915.220238	51672.331514	34.056589
916.475041	51771.096894	34.061607
917.507333	51859.495003	34.066624
918.259560	51925.594749	34.071642
919.562055	52020.183964	34.076660
920.849733	52101.216004	34.081677
921.577744	52186.391397	34.086695
922.307139	52266.644045	34.091712
923.179387	52345.077699	34.096730
924.038743	52433.315081	34.101748
925.004044	52506.704350	34.106765
926.267317	52592.544568	34.111783
926.786748	52685.727091	34.116800
927.671321	52766.773574	34.121818
928.865618	52847.575968	34.126836
929.908650	52936.229601	34.131853
930.754110	53011.701956	34.136871
931.590390	53102.084242	34.141888
932.873905	53179.501186	34.146906
933.500318	53262.279098	34.151924
934.459243	53334.254526	34.156941
935.464793	53420.150558	34.161959
936.424248	53507.072872	34.166976
937.567749	53583.272679	34.171994
938.351882	53675.595308	34.177012
939.718304	53753.653024	34.182029
940.324837	53831.728037	34.187047
940.938189	53917.775532	34.192064
942.154049	54000.122580	34.197082
942.898189	54087.770313	34.202100
944.259581	54163.419187	34.207117
944.975468	54242.339158	34.212135
945.921250	54333.797572	34.217152
946.696181	54406.564301	34.222170
947.573060	54494.104291	34.227188
948.634584	54579.249122	34.232205
950.119662	54661.271807	34.237223
950.749679	54755.970426	34.242240
951.898763	54826.357749	34.247258
953.161756	54900.138487	34.252276
954.035767	54963.652241	34.257293
955.479988	55018.135518	34.262311
956.444659	55081.856969	34.267328
957.805195	55129.151906	34.272346
958.420308	55191.909205	34.277364
959.685957	55244.471670	34.282381
960.207147	55303.636721	34.287399
960.965847	55366.194936	34.292416
961.991198	55419.244511	34.297434
962.512596	55487.946900	34.302452
963.453593	55557.596723	34.307469
964.424215	55625.482827	34.312487
965.187145	55696.901105	34.317504
966.106293	55777.427306	34.322522
967.152943	55854.054549	34.327540
967.928150	55935.515000	34.332557
969.133948	56013.681135	34.337575
969.766527	56092.575942	34.342592
971.069565	56150.456938	34.347610
971.531521	56240.852552	34.352628
972.675073	56312.169128	34.357645
973.617179	56398.712399	34.362663
974.735906	56474.324162	34.367680
975.569804	56564.663105	34.372698
977.114119	56643.145678	34.377716
978.002471	56719.249745	34.382733
979.145579	56795.852345	34.387751
979.469017	56874.607994	34.392768
980.766865	56961.148559	34.397786
981.838619	57052.123174	34.402804
982.662749	57133.966158	34.407821
983.790894	57218.072141	34.412839
984.772721	57303.080913	34.417856
986.100183	57370.226588	34.422874
987.205931	57454.647004	34.427892
988.114204	57530.332838	34.432909
989.555784	57601.391685	34.437927
990.292341	57685.553933	34.442944
991.117572	57757.918024	34.447962
991.952421	57840.875658	34.452980
992.847536	57917.419180	34.457997
994.352784	58002.121104	34.463015
994.845203	58082.708833	34.468032
996.076404	58172.207176	34.473050
997.043933	58249.626561	34.478068
997.675021	58327.364390	34.483085
999.035488	58406.476295	34.488103
1000.174012	58489.895229	34.493120
1001.146719	58568.669284	34.498138
1001.941124	58651.338528	34.503156
1003.026390	58728.487951	34.508173
1004.321990	58818.535643	34.513191
1005.069926	58905.554891	34.518208
1005.977272	58978.504817	34.523226
1007.046002	59058.512401	34.528244
1007.692993	59149.466115	34.533261
1009.255515	59227.479589	34.538279
1009.920906	59326.602371	34.543296
1010.920208	59403.292617	34.548314
1011.897438	59493.443009	34.553332
1012.954581	59582.422998	34.558349
1013.929275	59667.726033	34.563367
1015.118759	59761.357265	34.568384
1015.914616	59839.074293	34.573402
1016.878241	59926.658603	34.578420
1017.928758	60016.407090	34.583437
1019.027535	60089.621715	34.588455
1019.751712	60183.206735	34.593472
1020.873926	60264.899982	34.598490
1021.855846	60350.527095	34.603508
1022.840279	60428.976212	34.608525
1023.776469	60505.787358	34.613543
1024.583530	60593.157899	34.618560
1025.489085	60669.005872	34.623578
1026.849524	60753.309520	34.628596
1027.370945	60843.934629	34.633613
1028.776985	60912.717323	34.638631
1029.826172	61008.280457	34.643648
1030.758479	61093.791296	34.648666
1031.755697	61172.696558	34.653684
1032.668018	61269.231499	34.658701
1033.741791	61353.708432	34.663719
1034.675172	61442.727116	34.668736
1035.598018	61526.886318	34.673754
1037.205822	61626.745268	34.678772
1038.568830	61709.963037	34.683789
1039.847277	61784.199219	34.688807
1041.048351	61875.716158	34.693824
1042.372578	61958.725582	34.698842
1043.810996	62009.655391	34.703860
1044.639552	62089.653308	34.708877
1046.060723	62153.923727	34.713895
1047.419067	62224.540605	34.718912
1048.030448	62298.787218	34.723930
1048.961502	62374.003460	34.728948
1049.852880	62459.405136	34.733965
1050.867324	62531.722286	34.738983
1051.617535	62615.848771	34.744000
1052.756019	62693.034064	34.749018
1053.842551	62773.829638	34.754036
1054.525353	62869.140498	34.759053
1055.280414	62949.215936	34.764071
1056.449872	63041.457442	34.769088
1057.159119	63130.593057	34.774106
1058.286503	63219.233436	34.779124
1058.680494	63331.410999	34.784141
1060.517179	63418.795867	34.789159
1062.059732	63514.222261	34.794176
1062.922252	63600.385682	34.799194
1064.092827	63680.538068	34.804212
1064.980231	63777.485493	34.809229
1066.143554	63863.951184	34.814247
1067.066107	63963.261504	34.819264
1068.281188	64053.037041	34.824282
1069.582501	64148.079258	34.829300
1070.558401	64241.906350	34.834317
1071.427329	64329.166497	34.839335
1072.306155	64416.526699	34.844352
1073.532777	64508.796386	34.849370
1075.152774	64607.367623	34.854388
1076.372148	64695.574761	34.859405
1077.598128	64782.692278	34.864423
1078.624899	64853.558154	34.869440
1079.769231	64935.358335	34.874458
1081.086800	65017.929509	34.879476
1081.924354	65110.084703	34.884493
1083.031598	65191.720556	34.889511
1084.083212	65266.578550	34.894528
1085.190548	65352.811184	34.899546
1086.115182	65436.894689	34.904564
1087.200017	65520.586340	34.909581
1087.998153	65607.304813	34.914599
1088.992471	65695.183286	34.919616
1089.950081	65795.514691	34.924634
1091.332152	65882.839636	34.929652
1091.938486	65972.647143	34.934669
1093.092725	66058.570992	34.939687
1093.959788	66141.975709	34.944704
1095.027307	66232.275824	34.949722
1096.520096	66305.814650	34.954740
1096.791924	66400.417819	34.959757
1097.754016	66487.968505	34.964775
1098.891347	66571.883386	34.969792
1100.487511	66665.338039	34.974810
1101.689520	66748.800246	34.979828
1102.672546	66847.726304	34.984845
1103.812632	66934.402421	34.989863
1104.881566	67018.519364	34.994880
1106.045454	67120.324437	34.999898
1107.211432	67201.963959	35.004916
1107.903004	67302.602317	35.009933
1108.675141	67396.080284	35.014951
1109.732128	67488.140318	35.019968
1111.135641	67600.325337	35.024986
1112.800160	67694.798837	35.030004
1113.270358	67801.412617	35.035021
1114.639486	67904.569154	35.040039
1115.900770	67995.510176	35.045056
1117.028592	68105.138019	35.050074
1118.568289	68189.419810	35.055092
1119.660397	68297.844686	35.060109
1120.776258	68388.619786	35.065127
1122.043559	68472.792947	35.070144
1123.318630	68574.314230	35.075162
1124.533030	68668.304186	35.080180
1125.572244	68758.453011	35.085197
1126.467034	68853.297532	35.090215
1127.474489	68936.917464	35.095232
1128.975157	69050.974262	35.100250
1130.460523	69139.864580	35.105268
1131.636464	69234.736391	35.110285
1132.803859	69325.519436	35.115303
1134.627571	69403.872276	35.120320
1135.296073	69500.242411	35.125338
1136.347056	69588.594015	35.130356
1137.429067	69676.751129	35.135373
1138.737373	69762.606439	35.140391
1139.493179	69859.578531	35.145408
1140.515272	69952.982548	35.150426
1141.854132	70040.923622	35.155444
1142.624529	70133.392318	35.160461
1143.267834	70238.254203	35.165479
1144.681551	70339.589866	35.170496
1145.766163	70456.377139	35.175514
1147.245822	70545.684763	35.180532
1148.176708	70644.234587	35.185549
1149.808189	70745.702573	35.190567
1150.991093	70851.534097	35.195584
1151.697786	70949.499402	35.200602
1152.955201	71045.188348	35.205620
1154.026542	71153.571411	35.210637
1155.373636	71246.853488	35.215655
1156.642966	71343.846153	35.220672
1157.758132	71453.300151	35.225690
1158.924763	71553.273174	35.230708
1160.480563	71656.605566	35.235725
1161.370039	71745.958495	35.240743
1162.503506	71851.307815	35.245760
1163.847535	71937.424357	35.250778
1164.579864	72030.931565	35.255796
1166.234911	72130.526796	35.260813
1167.462779	72223.197638	35.265831
1168.480428	72322.753491	35.270848
1169.470316	72419.438992	35.275866
1170.697539	72505.220941	35.280884
1171.680881	72589.495940	35.285901
1172.779574	72671.068159	35.290919
1174.067556	72758.234682	35.295936
1174.825465	72847.814474	35.300954
1176.432108	72937.097807	35.305972
1177.820260	73018.651375	35.310989
1178.623785	73113.937199	35.316007
1179.910096	73197.166382	35.321024
1180.534624	73290.948143	35.326042
1182.004327	73382.508812	35.331060
1182.535977	73492.467402	35.336077
1184.236854	73580.737628	35.341095
1185.403015	73675.905693	35.346112
1186.586788	73784.320058	35.351130
1187.277323	73868.568702	35.356148
1188.523232	73973.009673	35.361165
1189.946982	74078.284674	35.366183
1190.812921	74193.779921	35.371200
1191.974368	74305.809766	35.376218
1193.626021	74401.829494	35.381236
1194.874282	74510.730761	35.386253
1196.081885	74617.460169	35.391271
1197.414788	74730.174425	35.396288
1198.475078	74836.914970	35.401306
1199.660532	74946.017781	35.406324
1200.818177	75040.229368	35.411341
1202.563343	75139.745853	35.416359
1204.218363	75243.051432	35.421376
1205.468730	75345.711052	35.426394
1206.750858	75437.219294	35.431412
1207.764887	75540.093778	35.436429
1209.134454	75646.270055	35.441447
1210.011924	75734.548888	35.446464
1211.393736	75845.689502	35.451482
1212.411701	75942.902745	35.456500
1213.201275	76054.693755	35.461517
1214.299900	76158.925480	35.466535
1215.630000	76273.597381	35.471552
1217.019102	76388.843279	35.476570
1218.387236	76497.581916	35.481588
1219.708308	76599.209241	35.486605
1220.439933	76715.749601	35.491623
1221.827181	76829.578906	35.496640
1223.120145	76947.223629	35.501658
1224.453052	77045.582553	35.506676
1226.126011	77156.645223	35.511693
1227.519374	77256.591624	35.516711
1228.646556	77354.933017	35.521728
1229.930738	77459.508214	35.526746
1231.057110	77568.149416	35.531764
1232.361673	77667.047045	35.536781
1233.200771	77777.317279	35.541799
1234.705757	77874.816325	35.546816
1235.452831	77996.490283	35.551834
1236.840935	78097.568035	35.556852
1238.326119	78210.057705	35.561869
1239.412530	78329.045347	35.566887
1240.674520	78418.856557	35.571904
1242.162108	78537.415278	35.576922
1243.240762	78642.964437	35.581940
1244.468461	78752.937405	35.586957
1245.239638	78867.162455	35.591975
1246.693766	78971.349580	35.596992
1247.937444	79084.893898	35.602010
1249.230068	79203.561844	35.607028
1250.664755	79307.740597	35.612045
1251.781703	79416.859313	35.617063
1253.162911	79518.969520	35.622080
1254.500866	79618.020992	35.627098
1255.585961	79709.092810	35.632116
1256.589760	79810.426694	35.637133
1257.365519	79910.390193	35.642151
1258.717711	80016.079383	35.647168
1259.868101	80125.056322	35.652186
1261.019202	80233.488807	35.657204
1262.179553	80342.046967	35.662221
1263.835606	80454.658539	35.667239
1264.982555	80560.622459	35.672256
1266.313922	80675.603928	35.677274
1267.219664	80781.859616	35.682292
1268.828914	80893.808774	35.687309
1270.014096	81018.151728	35.692327
1270.986177	81122.472633	35.697344
1272.665120	81239.226723	35.702362
1273.659138	81362.460704	35.707380
1275.351177	81463.021978	35.712397
1276.711855	81585.312993	35.717415
1278.028357	81689.062940	35.722432
1279.526742	81810.826713	35.727450
1280.252993	81929.049617	35.732468
1282.051985	82041.759354	35.737485
1283.313961	82158.974934	35.742503
1284.756557	82268.168130	35.747520
1286.138094	82393.018743	35.752538
1287.620034	82502.346091	35.757556
1288.976777	82609.298693	35.762573
1290.403737	82716.950302	35.767591
1292.051825	82829.078503	35.772608
1293.171557	82942.619766	35.777626
1294.391923	83044.501787	35.782644
1296.183192	83144.774868	35.787661
1297.165215	83248.950048	35.792679
1298.398467	83362.335946	35.797696
1300.017910	83465.221679	35.802714
1301.040300	83568.352763	35.807732
1302.521338	83673.642858	35.812749
1303.283257	83787.800697	35.817767
1304.575773	83892.690142	35.822784
1306.528672	83997.147744	35.827802
1307.562108	84115.483991	35.832820
1309.746986	84212.316464	35.837837
1310.583474	84318.520196	35.842855
1312.360637	84406.597848	35.847872
1314.097156	84497.203621	35.852890
1314.973670	84610.840068	35.857908
1316.355037	84701.818543	35.862925
1317.591865	84797.900917	35.867943
1319.239443	84888.116294	35.872960
1320.558503	84986.011142	35.877978
1321.814909	85076.756832	35.882996
1323.027970	85175.416425	35.888013
1323.697247	85286.262103	35.893031
1325.169519	85392.966398	35.898048
1326.625953	85501.929064	35.903066
1327.199647	85605.682184	35.908084
1328.707437	85715.866795	35.913101
1329.570577	85833.869143	35.918119
1330.773573	85945.825402	35.923136
1332.212067	86052.651434	35.928154
1333.350560	86183.676825	35.933172
1335.042695	86296.736774	35.938189
1336.331715	86402.966445	35.943207
1337.580842	86526.651859	35.948224
1338.907042	86644.281301	35.953242
1339.703760	86761.866911	35.958260
1341.846801	86877.253935	35.963277
1342.998984	86983.608399	35.968295
1344.028571	87084.913490	35.973312
1345.565452	87182.198936	35.978330
1346.415969	87301.349690	35.983348
1348.179811	87406.305252	35.988365
1349.146438	87514.946188	35.993383
1350.760146	87631.850553	35.998400
1351.997229	87736.509117	36.003418
1352.614321	87860.133808	36.008436
1354.293014	87978.752890	36.013453
1355.575454	88104.454715	36.018471
1356.827884	88218.312873	36.023488
1358.122175	88342.860665	36.028506
1359.802783	88460.340852	36.033524
1361.381872	88579.104584	36.038541
1362.446145	88706.490389	36.043559
1363.795396	88838.103139	36.048576
1365.530066	88960.139128	36.053594
1366.433689	89084.104531	36.058612
1368.041053	89209.646428	36.063629
1369.155494	89342.425862	36.068647
1370.830837	89473.217618	36.073664
1372.057040	89605.081038	36.078682
1372.906404	89735.432214	36.083700
1374.599693	89863.308045	36.088717
1375.740900	90006.719170	36.093735
1377.630430	90138.823885	36.098752
1378.985409	90273.914610	36.103770
1380.182753	90418.560972	36.108788
1381.934608	90555.010628	36.113805
1383.002593	90689.919774	36.118823
1384.535146	90826.772336	36.123840
1386.138414	90961.662756	36.128858
1387.301637	91101.020087	36.133876
1389.164720	91240.332500	36.138893
1390.463218	91373.345773	36.143911
1391.519907	91517.081440	36.148928
1393.198401	91654.941643	36.153946
1394.445438	91791.323389	36.158964
1396.422361	91920.494614	36.163981
1398.057568	92044.535826	36.168999
1399.317919	92175.137788	36.174016
1400.860735	92302.109515	36.179034
1402.314877	92445.344122	36.184052
1404.257278	92559.694426	36.189069
1405.966505	92683.942194	36.194087
1407.392288	92805.142002	36.199104
1408.841692	92907.706993	36.204122
1410.202011	93029.944524	36.209140
1411.759139	93149.249412	36.214157
1413.593694	93256.850845	36.219175
1414.604324	93376.013534	36.224192
1416.211375	93483.030111	36.229210
1417.491772	93609.287636	36.234228
1418.773876	93725.215364	36.239245
1419.781398	93841.984789	36.244263
1421.037057	93968.387065	36.249280
1422.538506	94078.806383	36.254298
1423.795057	94208.657122	36.259316
1425.174137	94336.892266	36.264333
1426.237879	94462.565931	36.269351
1428.152688	94582.315047	36.274368
1429.575122	94703.598925	36.279386
1430.771162	94844.539978	36.284404
1432.234439	94971.674569	36.289421
1433.628168	95099.314850	36.294439
1434.616416	95238.325336	36.299456
1436.269220	95353.783185	36.304474
1437.289960	95471.152457	36.309492
1438.585663	95589.594832	36.314509
1440.291211	95713.120209	36.319527
1441.738680	95822.628819	36.324544
1443.278207	95941.237393	36.329562
1444.667259	96071.455577	36.334580
1446.142626	96181.544193	36.339597
1447.367876	96304.119916	36.344615
1448.898345	96428.803535	36.349632
1450.524650	96558.505129	36.354650
1451.852486	96683.031157	36.359668
1453.450476	96800.100075	36.364685
1454.879754	96920.187273	36.369703
1456.316460	97048.830248	36.374720
1458.352952	97170.978857	36.379738
1459.036896	97297.623068	36.384756
1460.584018	97420.368543	36.389773
1462.265697	97551.282544	36.394791
1463.905387	97683.889599	36.399808
1465.139671	97804.213335	36.404826
1466.427087	97949.121892	36.409844
1467.827376	98086.648392	36.414861
1469.261346	98218.351628	36.419879
1470.511066	98362.456625	36.424896
1472.409708	98497.181826	36.429914
1473.607890	98644.756899	36.434932
1475.171681	98791.578516	36.439949
1476.778159	98930.166784	36.444967
1477.682507	99080.578545	36.449984
1479.581181	99226.640120	36.455002
1481.075713	99382.095673	36.460020
1482.174706	99515.859390	36.465037
1483.645415	99669.608614	36.470055
1484.745465	99827.282860	36.475072
1486.516433	99981.062902	36.480090
1487.984778	100144.804573	36.485108
1489.589579	100295.620089	36.490125
1492.030211	100428.189923	36.495143
1493.953477	100575.597615	36.500160
1495.351400	100713.046996	36.505178
1497.152189	100855.898373	36.510196
1498.614568	100994.467235	36.515213
1500.142321	101126.231173	36.520231
1501.686611	101270.873842	36.525248
1503.540611	101389.745330	36.530266
1504.995482	101527.823190	36.535284
1506.238409	101653.903124	36.540301
1508.151365	101794.471784	36.545319
1509.307872	101935.703946	36.550336
1511.052816	102068.299998	36.555354
1512.996258	102198.253964	36.560372
1514.298948	102324.504674	36.565389
1515.806371	102452.968077	36.570407
1517.135109	102580.027130	36.575424
1518.985806	102710.986477	36.580442
1520.762357	102847.270191	36.585460
1522.191673	102958.707776	36.590477
1524.047515	103092.469803	36.595495
1525.141349	103219.694666	36.600512
1526.522169	103340.650096	36.605530
1528.253541	103462.553029	36.610548
1529.473010	103601.170698	36.615565
1530.711110	103725.940715	36.620583
1532.146054	103861.799976	36.625600
1533.603801	103991.075854	36.630618
1535.212588	104132.918997	36.635636
1536.422648	104262.703604	36.640653
1538.531030	104392.627838	36.645671
1539.897577	104529.311927	36.650688
1541.037585	104646.708695	36.655706
1542.589907	104762.051056	36.660724
1543.751349	104883.413927	36.665741
1545.208440	105008.103930	36.670759
1546.140720	105149.232514	36.675776
1548.058506	105272.228827	36.680794
1549.518441	105398.225817	36.685812
1550.734982	105548.162123	36.690829
1552.705983	105685.302054	36.695847
1554.188376	105840.130646	36.700864
1555.157245	105975.779372	36.705882
1557.205131	106113.530379	36.710900
1558.095894	106262.392053	36.715917
1560.081535	106403.336561	36.720935
1561.446049	106562.586714	36.725952
1563.036290	106705.559406	36.730970
1564.787003	106865.689186	36.735988
1566.094922	107019.434460	36.741005
1568.180903	107171.372863	36.746023
1569.706792	107330.461998	36.751040
1571.388872	107472.802275	36.756058
1573.101193	107624.040026	36.761076
1574.790009	107778.972095	36.766093
1576.426466	107937.222607	36.771111
1577.692894	108090.877693	36.776128
1579.328717	108239.175496	36.781146
1580.587027	108396.967069	36.786164
1582.421169	108550.928940	36.791181
1584.129052	108700.827952	36.796199
1586.003133	108861.670622	36.801216
1587.294499	109015.858524	36.806234
1589.389740	109165.318827	36.811252
1591.108303	109322.586461	36.816269
1592.784285	109469.678582	36.821287
1594.830780	109626.579521	36.826304
1596.262434	109773.406604	36.831322
1597.862297	109925.432764	36.836340
1599.632481	110074.972916	36.841357
1601.185136	110234.768675	36.846375
1602.432211	110379.762875	36.851392
1604.104712	110537.474298	36.856410
1606.140902	110680.533479	36.861428
1607.353247	110835.223581	36.866445
1609.334014	110976.479134	36.871463
1610.751568	111127.435563	36.876480
1612.382467	111286.120606	36.881498
1613.803120	111438.726494	36.886516
1615.459613	111591.359741	36.891533
1617.253133	111738.760086	36.896551
1618.911693	111893.385352	36.901568
1620.410383	112054.757595	36.906586
1622.415395	112195.468898	36.911604
1623.746612	112349.335440	36.916621
1625.291240	112498.679967	36.921639
1627.201595	112650.174886	36.926656
1628.667377	112801.181623	36.931674
1630.969906	112944.474777	36.936692
1632.568021	113088.410794	36.941709
1634.561249	113223.446296	36.946727
1635.856325	113372.579645	36.951744
1637.456854	113510.898671	36.956762
1639.195175	113652.887386	36.961780
1640.316177	113795.556135	36.966797
1642.614776	113933.095950	36.971815
1644.153573	114076.182715	36.976832
1645.052509	114214.702400	36.981850
1647.188516	114349.732561	36.986868
1648.846051	114480.018235	36.991885
1650.434607	114601.728836	36.996903
1652.247070	114732.676171	37.001920
1653.642929	114854.785410	37.006938
1655.371569	114970.451053	37.011956
1656.363921	115110.430817	37.016973
1658.008349	115241.063682	37.021991
1659.000503	115376.262981	37.027008
1660.920672	115520.906794	37.032026
1662.600438	115664.193440	37.037044
1663.908652	115809.098511	37.042061
1665.749560	115944.104375	37.047079
1667.799691	116093.473756	37.052096
1669.665131	116247.134104	37.057114
1671.258378	116390.145312	37.062132
1672.691779	116546.715234	37.067149
1674.971825	116688.263562	37.072167
1676.616157	116832.397355	37.077184
1677.794514	116990.010839	37.082202
1679.359355	117136.187561	37.087220
1681.046787	117293.938717	37.092237
1682.905288	117447.846089	37.097255
1684.404308	117607.784136	37.102272
1686.067119	117773.227556	37.107290
1687.696180	117928.136583	37.112308
1689.058594	118108.087946	37.117325
1691.117479	118256.031315	37.122343
1693.054889	118424.047771	37.127360
1694.542889	118587.961822	37.132378
1696.177807	118751.244872	37.137396
1698.089030	118921.423929	37.142413
1700.012218	119091.995099	37.147431
1701.579278	119254.897659	37.152448
1702.815654	119428.621487	37.157466
1704.873430	119598.146533	37.162484
1706.296650	119768.620957	37.167501
1707.864630	119934.989159	37.172519
1709.671993	120110.123995	37.177536
1711.278096	120300.055998	37.182554
1713.611990	120457.085440	37.187572
1714.795056	120643.025837	37.192589
1716.849587	120814.078931	37.197607
1718.985657	120982.583095	37.202624
1720.484320	121146.379573	37.207642
1722.481061	121315.147882	37.212660
1724.259971	121493.667643	37.217677
1726.063302	121656.340612	37.222695
1728.459399	121821.167290	37.227712
1730.171688	121979.479366	37.232730
1732.168493	122129.223247	37.237748
1733.664999	122299.266089	37.242765
1735.609160	122452.863075	37.247783
1737.726368	122603.960057	37.252800
1739.508899	122749.477324	37.257818
1741.391514	122899.609794	37.262836
1742.952306	123047.065509	37.267853
1744.767506	123207.155182	37.272871
1746.488759	123349.550831	37.277888
1747.933537	123514.811751	37.282906
1749.208560	123667.350508	37.287924
1751.265147	123824.576159	37.292941
1752.584346	123985.114054	37.297959
1754.665208	124132.036158	37.302976
1756.018002	124293.102872	37.307994
1758.051317	124451.894997	37.313012
1759.803244	124610.389020	37.318029
1761.476367	124777.281504	37.323047
1763.555666	124922.303819	37.328064
1765.187882	125073.891616	37.333082
1766.852423	125205.976066	37.338100
1768.410484	125346.272914	37.343117
1769.971873	125492.950996	37.348135
1771.744406	125637.338556	37.353152
1773.029192	125785.405510	37.358170
1775.056561	125926.925347	37.363188
1776.509965	126071.008894	37.368205
1778.406247	126228.332307	37.373223
1780.414189	126379.308290	37.378240
1781.808565	126539.996871	37.383258
1783.341229	126698.342878	37.388276
1785.186107	126870.088953	37.393293
1786.831826	127039.278615	37.398311
1788.657786	127192.518807	37.403328
1790.048543	127364.033134	37.408346
1791.787283	127539.909105	37.413364
1793.473696	127728.481070	37.418381
1795.139591	127915.598062	37.423399
1797.445615	128094.699445	37.428416
1798.811621	128275.051693	37.433434
1800.928378	128452.661599	37.438452
1803.112424	128631.987272	37.443469
1804.499499	128826.688049	37.448487
1806.302793	129011.695141	37.453504
1807.951110	129203.806821	37.458522
1810.051220	129385.394473	37.463540
1811.810645	129575.790416	37.468557
1813.558440	129762.573026	37.473575
1815.365904	129951.554846	37.478592
1817.360165	130152.320809	37.483610
1819.355451	130337.189629	37.488628
1821.453356	130530.366574	37.493645
1823.287192	130713.612720	37.498663
1825.360860	130896.327491	37.503680
1827.457140	131076.387706	37.508698
1829.176958	131256.037806	37.513716
1831.332416	131437.600216	37.518733
1833.347451	131624.907656	37.523751
1835.309075	131802.771419	37.528768
1837.010444	131987.337815	37.533786
1838.952145	132161.716849	37.538804
1840.870364	132340.566583	37.543821
1842.464855	132523.718093	37.548839
1844.709743	132699.435145	37.553856
1846.223040	132875.774311	37.558874
1848.190661	133060.989003	37.563892
1849.921752	133247.091435	37.568909
1851.624683	133427.044971	37.573927
1853.959486	133601.952251	37.578944
1856.283516	133770.682411	37.583962
1858.635027	133935.716456	37.588980
1860.945104	134098.600438	37.593997
1862.641645	134256.796741	37.599015
1864.536709	134417.297501	37.604032
1866.081132	134594.184316	37.609050
1867.980937	134760.890559	37.614068
1869.855221	134919.645254	37.619085
1871.260836	135087.749307	37.624103
1873.163238	135242.414826	37.629120
1875.003219	135429.067778	37.634138
1876.785592	135593.803163	37.639156
1878.778509	135766.348467	37.644173
1880.069786	135945.348384	37.649191
1881.764166	136120.339817	37.654208
1883.702891	136298.923124	37.659226
1885.625298	136467.637121	37.664244
1887.375965	136636.936818	37.669261
1888.798765	136809.117984	37.674279
1890.513991	136969.478157	37.679296
1892.181379	137145.670567	37.684314
1894.060065	137303.011663	37.689332
1895.896921	137478.062263	37.694349
1898.058865	137649.801607	37.699367
1899.505211	137822.795065	37.704384
1901.326949	138003.002159	37.709402
1903.029516	138181.946799	37.714420
1905.187783	138373.346409	37.719437
1906.698654	138558.921226	37.724455
1908.578365	138732.713561	37.729472
1911.020904	138916.596586	37.734490
1912.811355	139113.564077	37.739508
1914.881276	139296.047189	37.744525
1916.635290	139486.943201	37.749543
1918.916863	139672.542071	37.754560
1920.598874	139865.976237	37.759578
1922.731526	140056.879074	37.764596
1924.642684	140257.512834	37.769613
1926.841631	140446.160666	37.774631
1928.475639	140635.874359	37.779648
1930.500099	140834.919257	37.784666
1932.377649	141030.840505	37.789684
1934.177726	141226.305044	37.794701
1935.967855	141431.277481	37.799719
1937.769467	141635.893651	37.804736
1940.063448	141831.017259	37.809754
1942.313607	142040.019904	37.814772
1943.909123	142246.180972	37.819789
1945.861142	142450.599490	37.824807
1948.021340	142639.046174	37.829824
1950.172432	142850.961331	37.834842
1952.076322	143053.625757	37.839860
1954.025298	143266.894071	37.844877
1956.029901	143467.082377	37.849895
1958.214741	143671.596653	37.854912
1960.247705	143882.887357	37.859930
1962.492961	144081.301937	37.864948
1964.527541	144277.287899	37.869965
1966.130204	144483.406434	37.874983
1968.547481	144680.971658	37.880000
1970.698814	144887.628363	37.885018
1972.118405	145088.256902	37.890036
1974.764387	145291.487609	37.895053
1976.588432	145488.412191	37.900071
1978.622700	145679.225312	37.905088
1980.461146	145895.187359	37.910106
1982.737648	146091.485406	37.915124
1984.893188	146283.081522	37.920141
1986.932264	146481.816851	37.925159
1988.682745	146668.870151	37.930176
1991.233127	146870.027794	37.935194
1993.114071	147057.684128	37.940212
1995.648087	147245.645662	37.945229
1997.568497	147437.841136	37.950247
2000.137463	147608.130565	37.955264
2002.049816	147788.727593	37.960282
2003.587657	147961.780637	37.965300
2005.728651	148137.735857	37.970317
2007.837904	148332.913404	37.975335
2009.472824	148509.088250	37.980352
2011.549102	148698.192444	37.985370
2013.298163	148885.038139	37.990388
2015.386916	149064.038178	37.995405
2017.220378	149261.102549	38.000423
2018.963848	149456.620414	38.005440
2021.136858	149636.624708	38.010458
2022.467368	149811.112303	38.015476
2024.279449	149983.304222	38.020493
2026.238246	150164.422542	38.025511
2028.260550	150343.665686	38.030528
2030.041099	150516.473490	38.035546
2031.702720	150706.499771	38.040564
2034.398956	150880.257850	38.045581
2036.287913	151063.979492	38.050599
2038.357821	151255.073859	38.055616
2040.277498	151446.065339	38.060634
2042.093328	151650.173355	38.065652
2043.959623	151837.658402	38.070669
2045.866670	152046.196436	38.075687
2047.881521	152244.208134	38.080704
2049.994623	152451.674749	38.085722
2051.633625	152666.413278	38.090740
2054.242515	152869.412254	38.095757
2056.155466	153088.057541	38.100775
2058.084423	153311.220217	38.105792
2060.553489	153522.938640	38.110810
2062.317085	153737.166817	38.115828
2064.138414	153949.787370	38.120845
2066.157138	154182.993199	38.125863
2068.064777	154400.324208	38.130880
2070.132386	154619.256003	38.135898
2072.408894	154856.638935	38.140916
2074.991996	155077.853384	38.145933
2076.770898	155295.614038	38.150951
2078.966670	155526.906320	38.155968
2081.432625	155739.268157	38.160986
2083.594356	155964.880376	38.166004
2085.809705	156183.236546	38.171021
2088.276711	156404.956511	38.176039
2090.965471	156613.389615	38.181056
2093.183441	156816.234905	38.186074
2095.401950	157033.692421	38.191092
2097.952146	157232.653631	38.196109
2100.163527	157443.614044	38.201127
2102.108074	157653.816956	38.206144
2104.315081	157843.198230	38.211162
2106.258904	158056.665253	38.216180
2108.426672	158254.216770	38.221197
2110.446949	158465.210518	38.226215
2112.184356	158674.459021	38.231232
2114.381741	158882.430624	38.236250
2116.029385	159096.582163	38.241268
2118.280177	159308.203108	38.246285
2120.126652	159528.901324	38.251303
2122.256544	159752.958560	38.256320
2124.436302	159976.412168	38.261338
2126.383300	160203.038564	38.266356
2128.699794	160422.549628	38.271373
2130.417354	160642.256240	38.276391
2132.604213	160870.802834	38.281408
2135.246294	161084.222486	38.286426
2137.249183	161309.663505	38.291444
2139.456453	161532.305870	38.296461
2141.749397	161749.666972	38.301479
2143.849772	161967.147657	38.306496
2146.601165	162175.196372	38.311514
2148.521938	162399.067058	38.316532
2150.900260	162607.556111	38.321549
2153.314646	162816.992417	38.326567
2155.262938	163025.067298	38.331584
2157.557061	163218.691786	38.336602
2159.878999	163433.235555	38.341620
2161.994098	163640.765906	38.346637
2164.053215	163839.469142	38.351655
2165.742587	164041.391859	38.356672
2168.016165	164220.701266	38.361690
2169.671867	164417.005968	38.366708
2171.906467	164605.679587	38.371725
2173.913138	164796.458707	38.376743
2175.675200	164998.347627	38.381760
2177.930971	165191.755333	38.386778
2179.609542	165404.209137	38.391796
2181.780836	165609.299175	38.396813
2184.014826	165822.061441	38.401831
2185.915597	166040.564269	38.406848
2188.468065	166255.474822	38.411866
2190.427985	166480.089587	38.416884
2192.291886	166688.988901	38.421901
2194.195862	166926.450124	38.426919
2195.977767	167160.299897	38.431936
2198.407539	167380.883089	38.436954
2200.929068	167631.899628	38.441972
2203.227395	167872.908596	38.446989
2205.233565	168106.167965	38.452007
2207.363992	168350.061492	38.457024
2209.956703	168586.748212	38.462042
2212.238791	168837.831690	38.467060
2214.231075	169072.086754	38.472077
2216.891721	169326.985633	38.477095
2218.423882	169565.961050	38.482112
2221.088516	169821.686365	38.487130
2223.407197	170070.267084	38.492148
2225.904929	170310.364396	38.497165
2228.504914	170547.754747	38.502183
2230.679808	170796.246023	38.507200
2233.242749	171034.799161	38.512218
2235.696864	171276.277714	38.517236
2237.998399	171503.826260	38.522253
2240.566134	171746.888530	38.527271
2242.832461	171990.176255	38.532288
2245.273600	172210.873919	38.537306
2247.557481	172450.465386	38.542324
2250.174480	172679.593665	38.547341
2252.042644	172914.108719	38.552359
2254.266851	173145.356543	38.557376
2256.697013	173381.321980	38.562394
2259.035719	173617.619811	38.567412
2261.482660	173846.231999	38.572429
2263.564803	174077.415811	38.577447
2265.799475	174314.074771	38.582464
2268.611741	174541.032178	38.587482
2270.475069	174764.684053	38.592500
2272.712971	174998.512889	38.597517
2274.897745	175243.842443	38.602535
2276.958766	175477.535121	38.607552
2279.235532	175722.496263	38.612570
2281.524011	175961.475464	38.617588
2283.365496	176205.566129	38.622605
2285.697512	176441.936814	38.627623
2287.949128	176686.942842	38.632640
2290.448328	176928.279333	38.637658
2292.490004	177180.100403	38.642676
2294.848931	177423.745862	38.647693
2296.922495	177672.769789	38.652711
2299.326556	177930.631963	38.657728
2301.888979	178165.841478	38.662746
2303.893926	178418.281468	38.667764
2306.230620	178662.289487	38.672781
2309.037366	178910.085429	38.677799
2311.173056	179165.631117	38.682816
2313.534722	179404.227691	38.687834
2316.112154	179623.692415	38.692852
2318.741623	179842.667032	38.697869
2321.164642	180045.724614	38.702887
2323.692774	180253.490268	38.707904
2325.900548	180447.820065	38.712922
2327.962726	180658.478319	38.717940
2330.442976	180863.865441	38.722957
2333.532681	181051.862212	38.727975
2335.198305	181257.986551	38.732992
2337.351110	181471.146979	38.738010
2339.584916	181686.784306	38.743028
2341.665387	181904.630238	38.748045
2343.482012	182127.318000	38.753063
2345.893326	182350.878877	38.758080
2348.170182	182587.617538	38.763098
2350.052919	182820.887753	38.768116
2352.145068	183053.871966	38.773133
2354.173021	183302.182037	38.778151
2356.981139	183553.749346	38.783168
2359.163096	183812.602572	38.788186
2361.249150	184064.054988	38.793204
2363.600933	184320.952832	38.798221
2366.148453	184576.246156	38.803239
2368.429188	184825.689110	38.808256
2370.690932	185159.282455	38.813274
2373.135960	185425.693260	38.818292
2375.622224	185701.927809	38.823309
2378.328470	185961.162214	38.828327
2380.227719	186236.803785	38.833344
2382.575100	186497.720942	38.838362
2385.401229	186774.083274	38.843380
2387.543048	187040.723242	38.848397
2390.433374	187302.827883	38.853415
2392.822895	187578.904679	38.858432
2395.242347	187846.519448	38.863450
2397.678866	188111.389058	38.868468
2399.906236	188385.588179	38.873485
2402.816960	188662.069226	38.878503
2405.049169	188931.925589	38.883520
2407.416313	189213.064590	38.888538
2410.186871	189482.889309	38.893556
2412.668618	189747.298604	38.898573
2415.323756	190018.336368	38.903591
2417.726433	190292.182686	38.908608
2420.142416	190563.843163	38.913626
2422.969349	190827.439222	38.918644
2425.319527	191103.759457	38.923661
2427.751443	191355.048193	38.928679
2430.207893	191633.918572	38.933696
2432.610976	191902.078875	38.938714
2435.422667	192166.035887	38.943732
2437.443874	192440.810168	38.948749
2440.512462	192697.692369	38.953767
2443.206900	192950.035792	38.958784
2445.525290	193206.832591	38.963802
2448.382970	193463.596791	38.968820
2450.389489	193727.961843	38.973837
2453.496910	193964.138848	38.978855
2455.741586	194211.906408	38.983872
2458.296479	194463.436325	38.988890
2461.099619	194718.204838	38.993908
2463.477404	194974.132290	38.998925
2465.581325	195217.224441	39.003943
2468.059561	195466.482090	39.008960
2470.461532	195709.020723	39.013978
2472.856172	195961.924680	39.018996
2475.057573	196218.313766	39.024013
2477.496399	196474.361561	39.029031
2479.540175	196718.761219	39.034048
2481.933114	196952.641532	39.039066
2484.199078	197199.369787	39.044084
2486.185105	197439.258193	39.049101
2488.437270	197675.371537	39.054119
2490.921829	197926.461503	39.059136
2492.987606	198176.753412	39.064154
2495.498281	198422.734408	39.069172
2497.843290	198680.578844	39.074189
2500.206811	198946.727251	39.079207
2502.481488	199208.647830	39.084224
2505.038159	199483.022734	39.089242
2507.106528	199753.663812	39.094260
2509.424194	200025.536663	39.099277
2511.979094	200306.238390	39.104295
2514.672833	200594.920676	39.109312
2517.033421	200889.091388	39.114330
2519.916587	201180.437861	39.119348
2522.263492	201468.134164	39.124365
2525.144822	201756.332044	39.129383
2527.154515	202053.302861	39.134400
2530.012327	202342.521481	39.139418
2532.410433	202645.605650	39.144436
2534.661539	202953.641297	39.149453
2537.409377	203258.374048	39.154471
2540.104774	203558.339788	39.159488
2542.278280	203877.185171	39.164506
2545.110929	204178.832530	39.169524
2547.924945	204505.631943	39.174541
2550.835204	204808.970200	39.179559
2553.133437	205116.341605	39.184576
2555.799639	205436.789482	39.189594
2558.825066	205743.413614	39.194612
2561.306147	206055.406722	39.199629
2563.969623	206369.327940	39.204647
2566.720288	206675.284925	39.209664
2569.084023	206991.362154	39.214682
2572.451274	207291.457574	39.219700
2574.719922	207606.229527	39.224717
2577.180024	207916.145532	39.229735
2580.197123	208218.278121	39.234752
2582.284977	208531.606096	39.239770
2585.138890	208834.501563	39.244788
2587.840009	209144.305468	39.249805
2590.622547	209460.320895	39.254823
2593.000400	209760.039965	39.259840
2596.204669	210070.681231	39.264858
2598.926222	210373.878590	39.269876
2601.432918	210685.264222	39.274893
2603.969524	210985.671276	39.279911
2606.780410	211286.366216	39.284928
2609.052659	211596.442974	39.289946
2611.943308	211895.424108	39.294964
2614.923649	212193.680288	39.299981
2617.301721	212494.393020	39.304999
2620.148002	212799.580422	39.310016
2622.604281	213110.392200	39.315034
2625.360568	213407.541244	39.320052
2627.995539	213703.464654	39.325069
2630.207794	214002.451738	39.330087
2632.675485	214308.105903	39.335104
2635.162285	214620.032073	39.340122
2637.996170	214929.592754	39.345140
2640.664100	215236.588329	39.350157
2643.085856	215534.172251	39.355175
2646.032372	215833.884860	39.360192
2648.605442	216146.103672	39.365210
2651.187464	216441.351558	39.370228
2654.106166	216756.844924	39.375245
2656.420143	217033.310661	39.380263
2658.862794	217311.255364	39.385280
2661.398329	217592.564490	39.390298
2663.856129	217866.467929	39.395316
2666.157529	218143.037858	39.400333
2668.969458	218437.235023	39.405351
2671.523513	218726.188451	39.410368
2673.890265	219031.683744	39.415386
2676.735414	219323.259576	39.420404
2679.632617	219608.400233	39.425421
2682.141206	219911.866958	39.430439
2684.924583	220206.958538	39.435456
2687.213925	220517.699779	39.440474
2689.709752	220824.217344	39.445492
2692.315420	221145.528480	39.450509
2694.958994	221455.579840	39.455527
2697.721264	221778.416471	39.460544
2700.050169	222111.406053	39.465562
2702.974914	222432.744158	39.470580
2705.799723	222761.439674	39.475597
2708.348424	223098.612390	39.480615
2711.194361	223423.544962	39.485632
2713.982558	223760.324882	39.490650
2716.878116	224089.009648	39.495668
2719.707872	224435.208117	39.500685
2722.383716	224768.576102	39.505703
2725.194646	225107.257951	39.510720
2727.902587	225455.888845	39.515738
2730.570409	225788.953277	39.520756
2733.764837	226132.224416	39.525773
2736.408424	226458.128649	39.530791
2739.319938	226815.670073	39.535808
2742.297000	227156.383753	39.540826
2745.166631	227492.388949	39.545844
2748.188717	227829.513554	39.550861
2751.037264	228162.524240	39.555879
2754.055732	228500.081149	39.560896
2756.681332	228824.997083	39.565914
2760.105055	229152.430756	39.570932
2762.820383	229485.461852	39.575949
2766.045769	229820.979279	39.580967
2769.031784	230141.062785	39.585984
2771.768971	230465.478181	39.591002
2774.144911	230792.388457	39.596020
2776.991361	231118.971339	39.601037
2779.637520	231443.451311	39.606055
2782.580812	231773.524580	39.611072
2785.055017	232101.181096	39.616090
2787.833397	232434.302767	39.621108
2790.532807	232767.639774	39.626125
2793.305906	233101.879663	39.631143
2796.000181	233437.782869	39.636160
2799.250018	233786.453775	39.641178
2801.694393	234119.245343	39.646196
2804.395050	234458.296956	39.651213
2807.500457	234794.414701	39.656231
2810.058683	235129.880635	39.661248
2812.537044	235471.684283	39.666266
2815.373789	235809.138641	39.671284
2818.420987	236150.395933	39.676301
2821.267763	236498.466912	39.681319
2824.075205	236824.137618	39.686336
2827.006925	237176.869026	39.691354
2829.784888	237503.229605	39.696372
2832.382668	237837.747080	39.701389
2835.111163	238185.580777	39.706407
2838.295465	238532.250816	39.711424
2840.734408	238862.879805	39.716442
2843.400907	239174.471188	39.721460
2846.491676	239494.811243	39.726477
2848.626177	239811.870292	39.731495
2851.544976	240128.349681	39.736512
2854.009756	240440.758610	39.741530
2856.976196	240761.523045	39.746548
2859.820824	241091.400459	39.751565
2862.142627	241422.222535	39.756583
2865.473058	241749.559397	39.761600
2867.885320	242089.714948	39.766618
2870.906581	242430.308730	39.771636
2873.867054	242753.891357	39.776653
2876.208214	243115.217397	39.781671
2879.100458	243456.795111	39.786688
2882.302201	243827.486884	39.791706
2885.386556	244174.012625	39.796724
2888.012655	244542.252484	39.801741
2890.696320	244892.243440	39.806759
2893.507356	245245.745003	39.811776
2897.046882	245616.431950	39.816794
2900.226099	245969.925783	39.821812
2903.648306	246327.750458	39.826829
2906.255600	246698.301050	39.831847
2909.109555	247057.101916	39.836864
2911.915587	247421.980794	39.841882
2914.795771	247789.540095	39.846900
2918.089194	248155.052960	39.851917
2920.802975	248522.357257	39.856935
2923.971550	248889.132781	39.861952
2927.042821	249253.458651	39.866970
2929.914879	249626.349933	39.871988
2933.307348	249984.426103	39.877005
2936.290289	250360.804021	39.882023
2939.668606	250723.834232	39.887040
2942.390808	251088.820088	39.892058
2945.136333	251456.087668	39.897076
2948.707197	251824.292842	39.902093
2951.296416	252185.892998	39.907111
2954.682015	252542.694433	39.912128
2957.954115	252905.863139	39.917146
2960.601329	253273.852929	39.922164
2963.769455	253624.411402	39.927181
2966.654485	254007.273124	39.932199
2969.541994	254362.572776	39.937216
2972.618381	254726.732663	39.942234
2975.930951	255091.540689	39.947252
2978.414111	255461.760304	39.952269
2981.199189	255832.897182	39.957287
2984.229836	256207.728804	39.962304
2987.252763	256582.382767	39.967322
2990.444208	256956.044202	39.972340
2993.178933	257319.132628	39.977357
2996.132877	257702.862257	39.982375
2999.484857	258063.769642	39.987392
3002.826297	258431.027823	39.992410
3006.168307	258798.996050	39.997428
3009.003342	259165.213227	40.002445
3011.845399	259531.428209	40.007463
3014.891124	259890.955465	40.012480
3017.600180	260260.643378	40.017498
3020.578688	260630.847007	40.022516
3023.835357	260993.767113	40.027533
3026.497085	261362.341290	40.032551
3029.512711	261731.875209	40.037568
3032.688135	262108.317244	40.042586
3035.573350	262478.758002	40.047604
3038.843326	262849.569443	40.052621
3041.873300	263206.472535	40.057639
3044.597904	263548.385389	40.062656
3047.584919	263904.962665	40.067674
3050.554678	264241.145659	40.072692
3053.363340	264578.394028	40.077709
3056.300083	264916.180165	40.082727
3058.906938	265262.652276	40.087744
3062.058409	265605.838179	40.092762
3064.689518	265967.670611	40.097780
3067.923004	266317.216510	40.102797
3071.102394	266691.254118	40.107815
3074.159263	267041.561531	40.112832
3076.960465	267404.835415	40.117850
3079.622897	267780.346262	40.122868
3083.252776	268156.416262	40.127885
3086.100412	268526.587098	40.132903
3089.275937	268896.680071	40.137920
3092.669946	269266.407416	40.142938
3096.065944	269644.488959	40.147956
3099.539853	270024.004521	40.152973
3102.655910	270409.542703	40.157991
3106.030323	270774.365266	40.163008
3109.082691	271158.259322	40.168026
3112.143374	271542.201235	40.173044
3114.717485	271913.645472	40.178061
3117.753973	272309.473827	40.183079
3120.603196	272703.602519	40.188096
3123.801863	273110.525974	40.193114
3126.555086	273508.221525	40.198132
3129.720182	273911.743199	40.203149
3133.077143	274326.306066	40.208167
3135.979453	274748.277252	40.213184
3139.076183	275151.727402	40.218202
3142.064027	275581.807900	40.223220
3145.468787	275994.602619	40.228237
3148.727508	276430.629984	40.233255
3151.677443	276852.100364	40.238272
3154.768097	277281.266943	40.243290
3158.136929	277719.174804	40.248308
3161.289656	278149.266628	40.253325
3164.136921	278586.057196	40.258343
3167.645952	279011.974723	40.263360
3171.050265	279447.454731	40.268378
3174.015510	279879.115134	40.273396
3177.700098	280315.816265	40.278413
3180.968039	280751.005206	40.283431
3184.474798	281178.536071	40.288448
3187.899839	281607.169120	40.293466
3190.933966	282026.439224	40.298484
3194.691300	282449.251102	40.303501
3197.910781	282863.103950	40.308519
3201.573161	283277.799649	40.313536
3205.336637	283692.197855	40.318554
3208.598539	284100.145543	40.323572
3211.876913	284499.708482	40.328589
3214.867825	284902.157885	40.333607
3218.032933	285304.831758	40.338624
3221.661325	285714.820494	40.343642
3224.661673	286130.998739	40.348660
3227.948878	286527.374353	40.353677
3231.181382	286928.428339	40.358695
3234.071693	287343.067236	40.363712
3237.584915	287737.597614	40.368730
3240.342848	288153.343871	40.373748
3243.903537	288548.369812	40.378765
3247.092428	288960.260467	40.383783
3250.327069	289361.121467	40.388800
3253.488507	289767.831348	40.393818
3256.272253	290166.446841	40.398836
3259.511592	290542.467104	40.403853
3262.636056	290915.938514	40.408871
3265.569598	291295.658123	40.413888
3268.496102	291681.673359	40.418906
3271.293602	292066.284393	40.423924
3274.184679	292442.931315	40.428941
3277.491929	292854.930287	40.433959
3280.186323	293268.621390	40.438976
3283.642283	293682.216535	40.443994
3286.746135	294090.633371	40.449012
3289.941282	294510.534579	40.454029
3293.311435	294930.913356	40.459047
3295.996051	295368.939599	40.464064
3299.769265	295792.550044	40.469082
3302.720759	296233.524136	40.474100
3305.893612	296669.662004	40.479117
3309.284415	297115.664046	40.484135
3312.550155	297561.098136	40.489152
3316.118626	298013.767919	40.494170
3319.192922	298479.636355	40.499188
3322.594587	298925.317764	40.504205
3325.909032	299386.495361	40.509223
3329.275473	299839.917988	40.514240
3333.113883	300300.371723	40.519258
3336.771801	300765.368465	40.524276
3341.187019	301209.528121	40.529293
3344.822561	301652.256889	40.534311
3348.425193	302100.622796	40.539328
3352.080630	302543.137998	40.544346
3355.340691	302994.265941	40.549364
3358.594290	303429.575997	40.554381
3362.135218	303886.440413	40.559399
3365.626539	304331.631513	40.564416
3369.075476	304777.789995	40.569434
3372.123948	305230.429180	40.574452
3375.765588	305664.644680	40.579469
3379.403956	306116.016544	40.584487
3382.455693	306564.175784	40.589504
3386.308001	307012.739509	40.594522
3389.493522	307470.642486	40.599540
3393.163482	307920.495591	40.604557
3396.431627	308358.477209	40.609575
3399.789488	308826.062450	40.614592
3403.265246	309262.531506	40.619610
3406.459949	309720.945155	40.624628
3410.103932	310178.751534	40.629645
3413.934074	310619.315841	40.634663
3417.325063	311072.787426	40.639680
3420.996593	311519.586557	40.644698
3424.462990	311971.971821	40.649716
3427.439584	312410.850300	40.654733
3431.163039	312855.572860	40.659751
3434.689437	313307.199880	40.664768
3437.904129	313753.693504	40.669786
3441.417869	314206.379685	40.674804
3444.593177	314653.149900	40.679821
3448.315613	315114.499792	40.684839
3451.476692	315567.202003	40.689856
3455.213780	316012.602503	40.694874
3458.702179	316464.077368	40.699892
3462.224641	316907.878170	40.704909
3465.778504	317357.202060	40.709927
3468.950885	317816.681078	40.714944
3472.275075	318269.964983	40.719962
3475.449508	318711.543272	40.724980
3478.791217	319170.220476	40.729997
3482.911174	319627.426779	40.735015
3486.315473	320067.942287	40.740020
3489.429157	320460.294534	40.745024
3492.595540	320841.161192	40.750029
3495.909161	321158.247402	40.755034
3498.348452	321419.574649	40.760039
3501.026866	321659.544097	40.765044
3503.110020	321830.941729	40.770048
3505.477533	321977.312218	40.775053
3507.649320	322078.505683	40.780058
3509.455396	322144.775792	40.785063
3510.839589	322191.115614	40.790068
3512.411743	322168.458320	40.795072
3513.973054	322144.708780	40.800077
3514.789347	322076.453309	40.805082
3516.273142	321985.910076	40.810087
3516.452146	321895.315291	40.815092
3517.481978	321765.664343	40.820096
3518.198067	321623.367096	40.825101
3518.587682	321468.450844	40.830106
3519.042873	321288.490342	40.835111
3518.968437	321108.484294	40.840116
3519.641788	320907.855871	40.845120
3520.232370	320705.280442	40.850125
3520.201709	320492.090065	40.855130
3520.665340	320263.684234	40.860135
3520.315484	320042.603664	40.865140
3520.489931	319797.143825	40.870144
3520.408337	319558.667984	40.875149
3520.343001	319317.491484	40.880154
3520.405103	319071.358100	40.885159
3520.260001	318833.625985	40.890164
3520.324015	318578.406739	40.895168
3520.229957	318327.154160	40.900173
3520.194205	318075.916516	40.905178
3520.015840	317822.282590	40.910183
3519.577791	317570.646709	40.915188
3519.595121	317326.367851	40.920192
3519.601502	317068.909884	40.925197
3519.472917	316818.315640	40.930202
3519.522897	316567.488659	40.935207
3518.430295	316318.390125	40.940212
3518.600294	316067.796111	40.945216
3518.482003	315826.430746	40.950221
3518.077954	315581.342871	40.955226
3518.070905	315341.102581	40.960231
3517.749377	315114.242671	40.965236
3517.490399	314868.390499	40.970240
3517.212760	314630.046000	40.975245
3517.160610	314396.703183	40.980250
3516.836574	314166.098621	40.985255
3516.673001	313946.027508	40.990260
3516.261110	313710.498058	40.995264
3516.262434	313507.879829	41.000269
3515.550062	313276.160790	41.005274
3515.843184	313068.686112	41.010279
3515.614963	312851.647853	41.015284
3515.464406	312638.871340	41.020288
3515.451077	312429.609443	41.025293
3514.971506	312223.345421	41.030298
3514.888150	312013.838115	41.035303
3514.335463	311823.156550	41.040308
3514.389093	311617.646624	41.045312
3514.114950	311417.047024	41.050317
3513.786052	311233.885763	41.055322
3513.586357	311029.074317	41.060327
3513.590689	310846.750336	41.065332
3513.536732	310662.628029	41.070336
3513.398931	310471.698368	41.075341
3512.906125	310282.273655	41.080346
3513.042758	310115.067109	41.085351
3512.864183	309932.030166	41.090356
3512.691297	309747.261249	41.095360
3512.467884	309577.615069	41.100365
3512.469146	309402.309506	41.105370
3511.865879	309222.491426	41.110375
3511.967076	309063.022746	41.115380
3512.264986	308889.806759	41.120384
3511.890768	308723.641931	41.125389
3511.925059	308554.181122	41.130394
3511.785153	308396.401890	41.135399
3511.347745	308235.614714	41.140404
3511.448353	308074.692395	41.145408
3511.224197	307924.075618	41.150413
3510.881361	307758.284374	41.155418
3511.000255	307602.879903	41.160423
3510.532420	307459.984969	41.165428
3510.703099	307301.848545	41.170432
3510.763252	307157.827205	41.175437
3510.535432	307016.293311	41.180442
3510.702768	306859.581121	41.185447
3510.307134	306727.488470	41.190452
3510.145186	306566.449454	41.195456
3510.545576	306423.263766	41.200461
3509.698003	306272.611786	41.205466
3509.930560	306128.382531	41.210471
3509.670937	305999.600610	41.215476
3509.800898	305861.519754	41.220480
3509.497360	305724.116758	41.225485
3509.461234	305587.638846	41.230490
3509.538181	305449.488775	41.235495
3509.353284	305327.335769	41.240500
3509.327785	305188.895546	41.245504
3509.190188	305060.703052	41.250509
3509.384758	304938.082879	41.255514
3509.182982	304800.585220	41.260519
3509.194410	304670.714345	41.265524
3509.017036	304541.406966	41.270528
3509.062574	304413.464311	41.275533
3508.704456	304294.033479	41.280538
3508.928609	304157.842120	41.285543
3508.840285	304040.710107	41.290548
3508.728913	303915.310181	41.295552
3508.484174	303782.193900	41.300557
3508.376014	303672.291953	41.305562
3508.693263	303548.071501	41.310567
3508.524127	303427.718521	41.315572
3508.237141	303311.582896	41.320576
3508.571055	303191.736450	41.325581
3508.360697	303074.035907	41.330586
3508.212990	302952.914995	41.335591
3507.910590	302836.042657	41.340596
3508.175067	302728.803953	41.345600
3508.141924	302615.299599	41.350605
3507.941028	302508.489175	41.355610
3508.266750	302390.118325	41.360615
3508.084139	302279.181582	41.365620
3508.001291	302168.636296	41.370624
3507.779139	302055.236511	41.375629
3507.634809	301951.037605	41.380634
3507.872061	301821.964429	41.385639
3507.538135	301730.443726	41.390644
3507.626142	301620.150680	41.395648
3507.822604	301502.510609	41.400653
3507.584402	301399.292382	41.405658
3507.384900	301292.326604	41.410663
3507.295383	301188.983032	41.415668
3507.602161	301072.546517	41.420672
3507.368536	300976.834909	41.425677
3507.452180	300873.514690	41.430682
3507.315017	300764.629312	41.435687
3507.524500	300663.910614	41.440692
3507.499859	300571.983498	41.445696
3507.363145	300464.828156	41.450701
3507.014633	300355.134945	41.455706
3507.239214	300246.141336	41.460711
3507.291724	300149.849261	41.465716
3507.482477	300054.146348	41.470720
3507.454184	299944.097062	41.475725
3506.949318	299844.607897	41.480730
3507.100237	299748.783391	41.485735
3506.536834	299662.028974	41.490740
3507.203067	299554.441481	41.495744
3507.222076	299452.375788	41.500749
3506.544121	299361.490035	41.505754
3506.448793	299266.262958	41.510759
3506.806467	299170.787059	41.515764
3506.589897	299062.012470	41.520768
3506.540404	298973.318987	41.525773
3506.648830	298880.935652	41.530778
3506.676138	298787.699406	41.535783
3506.521031	298708.566579	41.540788
3506.445911	298611.502663	41.545792
3506.436969	298517.991630	41.550797
3506.222890	298436.678680	41.555802
3506.482973	298335.591527	41.560807
3506.424527	298238.498917	41.565812
3506.668074	298150.318487	41.570816
3506.549308	298061.634339	41.575821
3506.387269	297981.458004	41.580826
3506.666510	297889.402793	41.585831
3506.451184	297802.693129	41.590836
3506.130462	297705.818586	41.595840
3506.723621	297622.495331	41.600845
3506.438339	297522.255175	41.605850
3506.561450	297429.434472	41.610855
3506.489852	297349.879493	41.615860
3506.376674	297259.666038	41.620864
3506.297266	297163.287533	41.625869
3506.124131	297071.988627	41.630874
3506.318717	296984.399426	41.635879
3506.625471	296903.079585	41.640884
3506.281757	296802.210925	41.645888
3506.384009	296716.035612	41.650893
3506.222298	296626.439591	41.655898
3505.941379	296540.272734	41.660903
3505.715160	296449.922874	41.665908
3505.940820	296369.454860	41.670912
3506.171384	296281.808083	41.675917
3505.843061	296199.262491	41.680922
3505.554127	296117.728795	41.685927
3505.835194	296038.677099	41.690932
3505.745494	295959.377548	41.695936
3506.068984	295870.010294	41.700941
3505.804034	295792.239553	41.705946
3506.183985	295705.688623	41.710951
3505.931477	295627.584828	41.715956
3505.945458	295532.945377	41.720960
3506.104867	295455.209966	41.725965
3505.964390	295378.386551	41.730970
3505.887099	295291.804345	41.735975
3505.955821	295206.930160	41.740980
3505.968954	295132.398830	41.745984
3506.214274	295035.406262	41.750989
3505.772260	294957.534695	41.755994
3506.045695	294863.057422	41.760999
3505.589257	294785.976950	41.766004
3505.624593	294710.881640	41.771008
3505.798012	294626.168505	41.776013
3505.498755	294553.008674	41.781018
3505.706124	294460.017385	41.786023
3505.646999	294384.452729	41.791028
3505.825276	294312.821914	41.796032
3505.531906	294219.119084	41.801037
3505.632582	294143.987434	41.806042
3505.851410	294065.782768	41.811047
3505.706521	294000.412756	41.816052
3505.242567	293909.434160	41.821056
3505.558955	293832.512188	41.826061
3505.425715	293765.765560	41.831066
3505.421440	293681.333279	41.836071
3505.456838	293601.731091	41.841076
3505.511168	293532.485913	41.846080
3505.498030	293455.258370	41.851085
3505.851754	293372.933599	41.856090
3505.322021	293307.419079	41.861095
3505.785086	293225.611642	41.866100
3505.606746	293149.987616	41.871104
3505.605631	293063.619408	41.876109
3505.269814	292982.037778	41.881114
3505.213384	292915.990993	41.886119
3505.482041	292845.973482	41.891124
3505.258176	292767.581470	41.896128
3505.273086	292690.374042	41.901133
3505.174479	292613.107815	41.906138
3505.155735	292532.188982	41.911143
3505.150504	292476.850355	41.916148
3505.172850	292389.153872	41.921152
3504.948020	292318.830721	41.926157
3504.979412	292251.624066	41.931162
3505.487836	292180.804825	41.936167
3505.518132	292107.896206	41.941172
3505.253061	292038.266288	41.946176
3504.908880	291962.895693	41.951181
3504.901625	291895.821940	41.956186
3505.029195	291825.647029	41.961191
3504.822156	291748.676596	41.966196
3505.139588	291685.446770	41.971200
3505.064174	291617.034181	41.976205
3504.623209	291540.583545	41.981210
3505.162014	291473.882560	41.986215
3505.112751	291409.284004	41.991220
3505.164024	291335.632997	41.996224
3505.289062	291268.767078	42.001229
3505.054661	291193.913031	42.006234
3505.196533	291117.931202	42.011239
3505.049762	291050.190941	42.016244
3505.140077	290981.751863	42.021248
3505.233035	290905.395551	42.026253
3504.758126	290838.087958	42.031258
3504.855325	290757.632420	42.036263
3504.963042	290692.092284	42.041268
3504.749604	290624.412847	42.046272
3504.470432	290559.314615	42.051277
3504.698820	290499.686729	42.056282
3505.092841	290425.319460	42.061287
3504.721878	290359.675273	42.066292
3504.739007	290290.304958	42.071296
3504.849987	290219.112582	42.076301
3504.790989	290156.448910	42.081306
3504.912383	290086.349375	42.086311
3504.938897	290018.377388	42.091316
3504.504035	289956.026568	42.096320
3504.636944	289883.939437	42.101325
3504.548273	289828.891460	42.106330
3504.751593	289763.284571	42.111335
3505.020349	289688.681367	42.116340
3504.683478	289636.395668	42.121344
3504.740828	289553.220976	42.126349
3504.751757	289490.113008	42.131354
3504.879936	289430.117866	42.136359
3504.920683	289369.627146	42.141364
3505.006049	289307.576583	42.146368
3505.147404	289235.258298	42.151373
3504.841366	289165.147896	42.156378
3504.637037	289088.021050	42.161383
3504.483554	289026.694710	42.166388
3504.771678	288958.069928	42.171392
3505.005014	288885.915133	42.176397
3505.146247	288822.608036	42.181402
3505.079271	288756.609417	42.186407
3504.846900	288689.974594	42.191412
3504.731979	288621.666741	42.196416
3505.027090	288540.821215	42.201421
3504.581465	288488.602419	42.206426
3504.954543	288412.275901	42.211431
3504.576772	288354.115009	42.216436
3504.689808	288279.687148	42.221440
3504.685011	288217.344088	42.226445
3504.344405	288151.489261	42.231450
3504.496008	288088.485318	42.236455
3504.424539	288031.472948	42.241460
3504.253930	287965.820592	42.246464
3504.496713	287902.827739	42.251469
3504.377311	287845.237155	42.256474
3504.373678	287773.550772	42.261479
3504.173134	287716.914612	42.266484
3504.076386	287672.761672	42.271488
3504.395269	287604.868934	42.276493
3504.451680	287543.737649	42.281498
3504.267950	287485.036647	42.286503
3504.433072	287424.804792	42.291508
3504.313248	287369.810489	42.296512
3504.098351	287312.947101	42.301517
3504.346818	287253.491294	42.306522
3504.550149	287189.612895	42.311527
3504.506602	287139.010635	42.316532
3504.712447	287070.982196	42.321536
3504.600150	287005.319811	42.326541
3504.324868	286942.966721	42.331546
3504.687806	286879.903281	42.336551
3504.547314	286817.147238	42.341556
3504.470170	286747.813264	42.346560
3504.653245	286692.007542	42.351565
3504.163638	286633.938907	42.356570
3504.184114	286569.273730	42.361575
3504.275945	286505.692060	42.366580
3503.921350	286455.545004	42.371584
3504.342215	286387.100547	42.376589
3504.276975	286337.799390	42.381594
3504.043391	286266.579944	42.386599
3504.259644	286220.697132	42.391604
3504.013360	286155.589374	42.396608
3504.281735	286094.016454	42.401613
3504.112115	286047.429840	42.406618
3504.165032	285986.272215	42.411623
3504.070358	285939.724781	42.416628
3504.259186	285880.302494	42.421632
3504.620837	285821.566079	42.426637
3504.442002	285761.844492	42.431642
3504.409957	285703.143781	42.436647
3504.518617	285643.606474	42.441652
3503.869257	285581.513996	42.446656
3504.637036	285509.272362	42.451661
3504.268902	285457.268246	42.456666
3504.046391	285397.222184	42.461671
3504.055690	285340.882314	42.466676
3504.019573	285288.571825	42.471680
3503.766739	285223.413276	42.476685
3504.132803	285175.138853	42.481690
3504.352590	285119.555245	42.486695
3503.959239	285052.229009	42.491700
3504.122684	284991.842493	42.496704
3504.146510	284940.642566	42.501709
3504.107581	284886.066437	42.506714
3503.918171	284829.960735	42.511719
3504.396063	284762.320432	42.516724
3503.723507	284714.181850	42.521728
3503.983231	284648.866622	42.526733
3504.021407	284603.163184	42.531738
3503.819085	284556.224228	42.536743
3503.863379	284495.652153	42.541748
3503.728050	284445.367665	42.546752
3504.039357	284386.485108	42.551757
3503.623530	284330.796109	42.556762
3503.679307	284283.205806	42.561767
3503.787312	284224.100164	42.566772
3503.821720	284178.040616	42.571776
3504.021456	284120.473573	42.576781
3503.973794	284077.227153	42.581786
3504.370390	284026.630463	42.586791
3504.087587	283959.158669	42.591796
3504.017708	283904.230166	42.596800
3504.206591	283855.218642	42.601805
3504.091735	283804.319502	42.606810
3504.248319	283741.870829	42.611815
3504.195631	283683.247990	42.616820
3503.889143	283628.076046	42.621824
3503.991940	283581.139872	42.626829
3504.111051	283522.617458	42.631834
3504.029246	283461.733149	42.636839
3504.367815	283413.207197	42.641844
3503.851485	283353.357841	42.646848
3503.726207	283289.985199	42.651853
3503.855747	283236.909087	42.656858
3504.174962	283188.513287	42.661863
3504.323365	283137.165359	42.666868
3503.690222	283079.472485	42.671872
3504.060731	283024.933026	42.676877
3503.808714	282966.035105	42.681882
3503.785136	282912.320649	42.686887
3504.018090	282862.843321	42.691892
3503.569345	282821.262453	42.696896
3503.785845	282753.839105	42.701901
3503.773927	282706.614697	42.706906
3503.796814	282655.540544	42.711911
3503.906581	282609.570083	42.716916
3503.787552	282557.372291	42.721920
3503.677280	282505.198557	42.726925
3503.490033	282456.168221	42.731930
3503.676731	282406.264973	42.736935
3503.711769	282351.929958	42.741940
3503.475130	282314.007349	42.746944
3503.426638	282254.007892	42.751949
3503.856624	282208.521985	42.756954
3503.969130	282161.456070	42.761959
3503.816503	282101.930955	42.766964
3503.886022	282049.652536	42.771968
3503.816744	281999.661544	42.776973
3503.725924	281944.531116	42.781978
3503.739149	281890.861088	42.786983
3503.832858	281846.318354	42.791988
3503.880692	281800.586148	42.796993
3503.846150	281738.114547	42.801997
3503.523482	281689.002927	42.807002
3503.550573	281640.040521	42.812007
3503.795156	281582.209859	42.817012
3503.621260	281531.903854	42.822017
3503.739755	281481.628693	42.827021
3503.562319	281440.157566	42.832026
3503.402690	281380.607490	42.837031
3503.662882	281331.888657	42.842036
3503.508586	281285.347423	42.847041
3503.916661	281235.459840	42.852045
3503.765360	281185.557432	42.857050
3503.406596	281129.729760	42.862055
3503.634398	281085.292993	42.867060
3503.586010	281037.360309	42.872065
3503.661131	280981.770520	42.877069
3503.858825	280941.437334	42.882074
3503.310144	280889.305205	42.887079
3503.761807	280839.919763	42.892084
3503.360362	280792.296455	42.897089
3503.784044	280747.141595	42.902093
3503.988335	280697.998230	42.907098
3503.683313	280641.652633	42.912103
3503.744882	280592.124053	42.917108
3503.467097	280552.322918	42.922113
3503.650014	280488.059700	42.927117
3503.379776	280450.701467	42.932122
3503.378948	280403.219246	42.937127
3503.468053	280362.622586	42.942132
3503.041424	280306.626636	42.947137
3503.640665	280267.198068	42.952141
3503.550959	280218.609331	42.957146
3503.378553	280173.215905	42.962151
3503.583639	280123.359163	42.967156
3503.484230	280081.900592	42.972161
3503.582789	280035.548364	42.977165
3503.548446	279977.938073	42.982170
3503.608653	279931.133471	42.987175
3504.183095	279879.055002	42.992180
3503.478169	279830.790888	42.997185
3503.354936	279772.099496	43.002189
3503.448883	279724.449338	43.007194
3503.170878	279690.350806	43.012199
3503.572934	279648.992183	43.017204
3503.430343	279601.837035	43.022209
3503.541264	279550.925248	43.027213
3503.549612	279502.626310	43.032218
3503.487526	279454.032782	43.037223
3503.582735	279402.104939	43.042228
3503.553582	279367.432876	43.047233
3503.801972	279308.123174	43.052237
3503.561481	279252.479375	43.057242
3503.442388	279211.812654	43.062247
3503.830688	279162.894253	43.067252
3503.528058	279119.302667	43.072257
3503.476952	279063.654720	43.077261
3503.366176	279023.012064	43.082266
3503.551282	278976.289278	43.087271
3503.613612	278928.745382	43.092276
3503.121470	278879.276381	43.097281
3503.458474	278830.365750	43.102285
3503.426188	278781.792616	43.107290
3503.015432	278741.400173	43.112295
3503.249519	278695.789846	43.117300
3502.867433	278654.170802	43.122305
3503.136773	278612.577667	43.127309
3502.784538	278570.877552	43.132314
3503.008526	278534.943625	43.137319
3502.923193	278492.514505	43.142324
3503.125194	278458.468030	43.147329
3503.362245	278416.574290	43.152333
3503.128180	278367.370324	43.157338
3503.192104	278327.158402	43.162343
3503.238958	278291.277386	43.167348
3502.952461	278249.617789	43.172353
3503.392173	278203.084059	43.177357
3503.415784	278160.204976	43.182362
3503.420322	278116.896010	43.187367
3503.533398	278072.195263	43.192372
3503.262648	278027.095929	43.197377
3503.296490	277983.043974	43.202381
3503.211159	277938.857775	43.207386
3502.999069	277893.927460	43.212391
3503.550071	277852.773839	43.217396
3503.461322	277814.545873	43.222401
3503.107566	277768.873714	43.227405
3503.195173	277719.873889	43.232410
3503.366098	277671.701269	43.237415
3503.712761	277635.034940	43.242420
3503.240778	277589.966668	43.247425
3503.232505	277547.728728	43.252429
3503.257691	277492.933444	43.257434
3502.903013	277448.228747	43.262439
3503.324154	277407.273326	43.267444
3503.025583	277380.993409	43.272449
3502.971147	277320.609039	43.277453
3503.155079	277292.013465	43.282458
3503.201880	277251.854576	43.287463
3503.489548	277206.922482	43.292468
3502.890774	277162.051922	43.297473
3503.035989	277116.199894	43.302477
3503.316401	277077.888664	43.307482
3503.386876	277037.725983	43.312487
3503.684011	276987.012684	43.317492
3503.255649	276947.640486	43.322497
3503.121280	276895.441164	43.327501
3503.299356	276858.393336	43.332506
3503.367078	276813.215176	43.337511
3503.049749	276769.217189	43.342516
3502.818911	276728.464718	43.347521
3503.085632	276688.602314	43.352525
3503.207313	276642.473607	43.357530
3503.129582	276611.143262	43.362535
3502.996495	276561.642384	43.367540
3503.387568	276521.200406	43.372545
3503.152114	276470.391429	43.377549
3503.276063	276424.109477	43.382554
3503.184050	276385.397571	43.387559
3503.265930	276346.098443	43.392564
3503.140126	276308.333817	43.397569
3503.149224	276260.287368	43.402573
3503.106150	276220.141947	43.407578
3503.065730	276181.701986	43.412583
3503.214463	276137.580206	43.417588
3503.073060	276100.327132	43.422593
3503.232031	276054.141362	43.427597
3503.291548	276012.223055	43.432602
3502.908642	275981.016338	43.437607
3503.172908	275936.418169	43.442612
3502.961124	275898.768575	43.447617
3503.152542	275855.200145	43.452621
3503.333852	275817.820340	43.457626
3503.128024	275770.010736	43.462631
3503.400196	275723.628934	43.467636
3503.574449	275677.567879	43.472641
3503.319225	275624.215322	43.477645
3503.509856	275586.604808	43.482650
3503.254805	275546.059198	43.487655
3503.370091	275502.196891	43.492660
3503.300859	275454.747766	43.497665
3503.024674	275408.247427	43.502669
3503.130245	275371.541198	43.507674
3502.869800	275338.278270	43.512679
3502.650828	275289.579283	43.517684
3502.977841	275261.520874	43.522689
3502.959021	275213.198078	43.527693
3503.216605	275172.317897	43.532698
3503.218363	275133.692649	43.537703
3503.384088	275081.012615	43.542708
3502.842130	275046.138383	43.547713
3502.842950	274997.990634	43.552717
3503.000889	274961.759842	43.557722
3502.997422	274924.815767	43.562727
3503.054969	274883.330034	43.567732
3502.817618	274838.070943	43.572737
3502.602342	274818.804609	43.577741
3503.134289	274774.546078	43.582746
3502.895091	274740.872218	43.587751
3502.895786	274697.358316	43.592756
3503.299673	274656.709729	43.597761
3503.328552	274614.693630	43.602765
3503.163895	274570.467007	43.607770
3502.963453	274539.944273	43.612775
3503.083658	274488.875029	43.617780
3502.962281	274453.655022	43.622785
3503.331014	274412.298861	43.627789
3503.233837	274372.517419	43.632794
3502.897075	274320.042406	43.637799
3503.341956	274287.713228	43.642804
3503.088400	274252.946554	43.647809
3502.980037	274196.081971	43.652813
3502.930569	274152.066356	43.657818
3503.015884	274121.677235	43.662823
3503.049404	274077.394051	43.667828
3502.941984	274044.947030	43.672833
3503.073640	274006.046429	43.677837
3502.998174	273959.666816	43.682842
3502.719654	273924.852967	43.687847
3503.046221	273885.412744	43.692852
3503.097098	273855.512660	43.697857
3502.886793	273807.015153	43.702861
3502.950094	273768.048694	43.707866
3502.920674	273729.529497	43.712871
3503.052817	273686.147387	43.717876
3502.849921	273650.888806	43.722881
3502.792063	273609.624098	43.727885
3502.887442	273580.149844	43.732890
3502.955691	273536.548443	43.737895
3503.143702	273494.532485	43.742900
3502.739662	273460.883765	43.747905
3502.888152	273425.137558	43.752909
3502.890052	273376.581322	43.757914
3502.898853	273342.282687	43.762919
3503.026965	273307.838162	43.767924
3502.646594	273273.319978	43.772929
3502.906639	273236.283233	43.777933
3502.876442	273199.317099	43.782938
3502.661504	273160.088116	43.787943
3502.923206	273124.120470	43.792948
3503.188205	273083.314507	43.797953
3503.120882	273039.937647	43.802957
3503.085046	273000.222404	43.807962
3502.999423	272964.512435	43.812967
3503.174661	272917.354843	43.817972
3502.912351	272882.563509	43.822977
3502.709870	272845.598571	43.827981
3502.796710	272809.530694	43.832986
3502.765223	272772.513654	43.837991
3502.730850	272723.733534	43.842996
3502.587372	272692.386484	43.848001
3502.755497	272662.085807	43.853005
3503.155899	272631.036033	43.858010
3502.799021	272586.354508	43.863015
3502.999015	272551.058244	43.868020
3502.673352	272515.843763	43.873025
3502.719113	272480.393235	43.878029
3502.883857	272437.565592	43.883034
3502.719674	272410.804864	43.888039
3502.487098	272365.645563	43.893044
3502.515212	272333.049494	43.898049
3502.493334	272300.486654	43.903053
3502.590326	272265.155377	43.908058
3502.424733	272231.570922	43.913063
3502.592224	272192.893085	43.918068
3502.583598	272169.774649	43.923073
3502.650507	272138.496510	43.928077
3502.979641	272103.561904	43.933082
3502.733334	272078.850841	43.938087
3502.792921	272023.639200	43.943092
3502.288312	271986.848224	43.948097
3502.514843	271953.711891	43.953101
3502.606051	271927.318671	43.958106
3502.855210	271898.023615	43.963111
3503.283894	271865.645124	43.968116
3502.651006	271830.274478	43.973121
3502.729729	271783.258604	43.978125
3502.888512	271754.104876	43.983130
3502.318946	271713.962854	43.988135
3502.992309	271678.821738	43.993140
3502.853257	271643.883419	43.998145
3503.034482	271601.409279	44.003149
3502.919896	271563.131536	44.008154
3502.648448	271530.836411	44.013159
3502.969082	271487.474798	44.018164
3503.192839	271451.996157	44.023169
3503.198501	271410.822372	44.028173
3503.147610	271367.900453	44.033178
3502.760967	271322.255342	44.038183
3502.724947	271275.893620	44.043188
3502.921010	271244.951544	44.048193
3502.887641	271216.082167	44.053197
3502.811381	271184.444032	44.058202
3502.733170	271146.185912	44.063207
3502.565613	271107.763442	44.068212
3502.656914	271069.784462	44.073217
3502.714965	271040.442475	44.078221
3502.796652	270997.143271	44.083226
3502.204376	270972.613050	44.088231
3502.426506	270936.879833	44.093236
3502.340051	270901.958501	44.098241
3502.449130	270871.386310	44.103245
3502.415298	270842.567810	44.108250
3502.306548	270813.659109	44.113255
3502.681635	270782.383463	44.118260
3502.476810	270753.617006	44.123265
3502.349517	270714.449683	44.128269
3502.598132	270682.735355	44.133274
3502.239606	270658.015898	44.138279
3502.515794	270635.158296	44.143284
3502.400552	270605.206565	44.148289
3502.429344	270561.609830	44.153293
3502.367018	270523.145273	44.158298
3502.242785	270506.792032	44.163303
3502.706545	270469.136784	44.168308
3502.503665	270439.987983	44.173313
3502.433119	270412.702828	44.178317
3502.831520	270385.650245	44.183322
3502.627218	270347.946128	44.188327
3502.711745	270298.967937	44.193332
3502.916656	270282.767141	44.198337
3502.525762	270239.490189	44.203341
3502.663688	270201.198037	44.208346
3502.314185	270169.831233	44.213351
3502.758994	270135.005176	44.218356
3502.632439	270108.390681	44.223361
3502.505308	270080.299419	44.228365
3502.817701	270042.896717	44.233370
3502.578815	270006.852931	44.238375
3502.612129	269952.458921	44.243380
3502.716862	269927.947270	44.248385
3502.429669	269903.471137	44.253389
3502.603729	269871.819056	44.258394
3502.492177	269844.132705	44.263399
3502.522554	269804.380272	44.268404
3502.756987	269766.836811	44.273409
3502.984757	269739.988831	44.278413
3502.903421	269700.966701	44.283418
3502.425789	269668.091884	44.288423
3502.759612	269632.544481	44.293428
3502.776886	269606.722277	44.298433
3502.097535	269567.844075	44.303437
3502.259666	269531.992331	44.308442
3502.559542	269507.348350	44.313447
3502.695839	269472.315421	44.318452
3502.620231	269443.757613	44.323457
3502.693261	269403.743740	44.328461
3502.611337	269369.406771	44.333466
3502.566422	269335.573292	44.338471
3502.913537	269299.743599	44.343476
3502.843577	269259.013485	44.348481
3502.679794	269227.948482	44.353485
3502.742146	269197.892269	44.358490
3502.556246	269166.346888	44.363495
3503.043015	269119.495311	44.368500
3502.860748	269089.451666	44.373505
3502.457910	269053.407560	44.378509
3502.609387	269023.082790	44.383514
3502.389139	269004.121516	44.388519
3502.760963	268968.848042	44.393524
3502.637966	268923.720901	44.398529
3502.547073	268892.415275	44.403533
3503.078491	268857.091462	44.408538
3502.723690	268824.044455	44.413543
3502.350703	268787.919213	44.418548
3502.776818	268747.519093	44.423553
3502.374750	268723.085990	44.428557
3503.021262	268685.528898	44.433562
3502.608716	268661.886772	44.438567
3502.598688	268617.022001	44.443572
3502.914236	268582.953916	44.448577
3502.760370	268546.081510	44.453581
3502.944462	268508.392600	44.458586
3502.496454	268468.001070	44.463591
3502.867077	268432.498414	44.468596
3502.673828	268405.129912	44.473601
3502.893451	268372.655408	44.478605
3502.496247	268332.357768	44.483610
3502.402161	268305.686781	44.488615
3502.648925	268268.904706	44.493620
3502.715653	268241.495701	44.498625
3502.242715	268212.388229	44.503629
3502.523587	268174.022078	44.508634
3502.285377	268148.901281	44.513639
3502.306565	268117.883521	44.518644
3502.675603	268084.672692	44.523649
3502.185838	268051.519102	44.528653
3502.726870	268013.621672	44.533658
3502.271736	267996.250019	44.538663
3502.610472	267964.902698	44.543668
3502.497514	267933.014532	44.548673
3502.402030	267899.493972	44.553677
3502.421932	267864.911442	44.558682
3502.451193	267836.158587	44.563687
3502.685487	267803.274191	44.568692
3502.546521	267773.427101	44.573697
3502.324312	267733.840421	44.578701
3502.479176	267709.014831	44.583706
3502.633289	267679.554985	44.588711
3502.516113	267641.199637	44.593716
3502.560290	267608.039197	44.598721
3502.526450	267581.867907	44.603725
3502.704158	267542.040672	44.608730
3502.424820	267517.639090	44.613735
3501.961872	267481.705600	44.618740
3502.056085	267461.574688	44.623745
3501.801152	267438.340615	44.628749
3502.283478	267409.135177	44.633754
3502.099204	267391.874048	44.638759
3502.178634	267350.457820	44.643764
3502.050128	267333.009757	44.648769
3502.032352	267304.518701	44.653773
3502.365695	267276.940617	44.658778
3502.099775	267247.622394	44.663783
3502.331815	267206.971731	44.668788
3502.698299	267185.881701	44.673793
3502.634243	267157.015849	44.678797
3502.739832	267121.146536	44.683802
3502.439671	267098.937969	44.688807
3502.800446	267055.950013	44.693812
3502.891916	267028.154861	44.698817
3502.535897	266989.658179	44.703821
3502.340435	266952.689784	44.708826
3502.578748	266935.439207	44.713831
3502.558963	266895.184095	44.718836
3502.769086	266857.159464	44.723841
3502.637408	266827.641980	44.728845
3502.574629	266786.578674	44.733850
3502.547740	266766.670175	44.738855
3502.433900	266727.779211	44.743860
3502.366787	266706.782016	44.748865
3502.572119	266661.679119	44.753869
3502.804880	266624.847676	44.758874
3502.215285	266599.348275	44.763879
3502.408850	266561.122397	44.768884
3502.506941	266526.221662	44.773889
3502.404630	266497.590746	44.778893
3502.559526	266471.822676	44.783898
3502.105611	266445.003465	44.788903
3502.572689	266414.730624	44.793908
3502.788541	266385.413568	44.798913
3502.553241	266349.215066	44.803917
3502.700020	266308.118952	44.808922
3502.443382	266286.540027	44.813927
3502.486938	266252.869951	44.818932
3502.362445	266205.475493	44.823937
3502.218668	266197.527653	44.828941
3502.062640	266158.846744	44.833946
3502.156360	266136.194710	44.838951
3502.570513	266117.083224	44.843956
3502.484009	266082.261988	44.848961
3502.324419	266059.471107	44.853965
3502.437323	266022.123351	44.858970
3502.179338	265989.213102	44.863975
3502.379530	265957.020928	44.868980
3502.259441	265941.150079	44.873985
3502.022952	265906.453978	44.878989
3502.526681	265873.017735	44.883994
3502.283193	265847.056859	44.888999
3502.005447	265821.228628	44.894004
3502.316483	265797.931564	44.899009
3502.063510	265772.532354	44.904013
3502.314830	265734.526352	44.909018
3502.378469	265714.170669	44.914023
3502.192073	265685.374358	44.919028
3502.303256	265653.221402	44.924033
3502.215991	265624.307792	44.929037
3502.588011	265593.896714	44.934042
3502.590689	265563.950526	44.939047
3502.429706	265530.795857	44.944052
3502.308636	265498.475282	44.949057
3502.203696	265474.224311	44.954061
3502.304734	265446.580017	44.959066
3502.311248	265413.348317	44.964071
3502.292003	265399.193252	44.969076
3502.112978	265369.682709	44.974081
3502.046424	265343.184890	44.979085
3502.583500	265306.178292	44.984090
3502.149900	265290.457984	44.989095
3502.188484	265253.579867	44.994100
3502.351396	265231.069649	44.999105
3502.203496	265203.311243	45.004109
3502.517983	265166.975838	45.009114
3502.204182	265138.733947	45.014119
3502.437700	265111.781946	45.019124
3502.229153	265079.067424	45.024129
3502.350536	265051.063359	45.029133
3502.615667	265015.244865	45.034138
3502.248810	264995.796350	45.039143
3502.267439	264957.622556	45.044148
3502.578977	264934.197898	45.049153
3502.267210	264905.395413	45.054157
3502.385089	264873.877779	45.059162
3502.277808	264840.281639	45.064167
3502.453666	264807.659999	45.069172
3502.614233	264779.318728	45.074177
3502.003738	264753.542009	45.079181
3502.540272	264718.496036	45.084186
3502.497433	264694.540790	45.089191
3502.500879	264659.552289	45.094196
3502.717216	264633.646874	45.099201
3502.089505	264605.479151	45.104205
3502.521755	264571.213287	45.109210
3502.145376	264544.508833	45.114215
3502.140835	264510.591027	45.119220
3502.294379	264483.142021	45.124225
3502.255848	264471.612659	45.129229
3502.038752	264442.846244	45.134234
3502.078657	264412.970324	45.139239
3502.051084	264378.648630	45.144244
3502.290100	264362.619799	45.149249
3501.972254	264338.961911	45.154253
3502.035267	264303.200089	45.159258
3502.098344	264279.584769	45.164263
3502.519338	264255.557244	45.169268
3502.305763	264225.007713	45.174273
3502.177825	264205.547336	45.179277
3502.601514	264167.361151	45.184282
3502.260460	264135.761925	45.189287
3502.331767	264116.728886	45.194292
3502.071716	264073.046888	45.199297
3502.010950	264052.506523	45.204301
3502.404993	264020.130796	45.209306
3502.337536	263999.820642	45.214311
3501.924845	263962.452076	45.219316
3502.191720	263953.829013	45.224321
3502.118700	263930.616760	45.229325
3502.232028	263895.050688	45.234330
3502.132290	263873.548702	45.239335
3502.016220	263842.627384	45.244340
3502.014242	263824.624278	45.249345
3502.430767	263795.504442	45.254349
3502.346758	263757.448044	45.259354
3502.497587	263738.937319	45.264359
3502.439166	263711.953995	45.269364
3502.773802	263679.154512	45.274369
3502.126690	263643.324722	45.279373
3502.365541	263607.458911	45.284378
3502.076393	263574.629142	45.289383
3502.168637	263547.036646	45.294388
3502.321386	263520.300524	45.299393
3502.051113	263501.447853	45.304397
3502.206960	263458.872257	45.309402
3502.219998	263445.908742	45.314407
3502.203938	263405.218791	45.319412
3502.477541	263384.015115	45.324417
3502.098020	263361.843555	45.329421
3502.432658	263321.149929	45.334426
3502.177912	263302.804099	45.339431
3502.280696	263269.913248	45.344436
3502.782559	263245.465479	45.349441
3502.079494	263218.964317	45.354445
3502.056167	263183.164628	45.359450
3502.216810	263173.081083	45.364455
3502.012181	263143.930408	45.369460
3502.089797	263105.262942	45.374465
3502.000156	263089.870752	45.379469
3501.999822	263054.551272	45.384474
3502.098337	263039.842808	45.389479
3502.281569	263015.266317	45.394484
3502.282307	262982.187541	45.399489
3502.185689	262960.583029	45.404493
3502.061264	262923.576680	45.409498
3502.056638	262910.870497	45.414503
3501.976421	262881.012844	45.419508
3502.572705	262850.082251	45.424513
3502.341504	262833.744393	45.429517
3502.060788	262794.572354	45.434522
3502.095449	262773.431206	45.439527
3501.802619	262749.718145	45.444532
3502.019271	262718.795661	45.449537
3502.175537	262701.684475	45.454541
3502.256960	262681.707413	45.459546
3502.136064	262654.300648	45.464551
3502.327071	262631.709115	45.469556
3502.626600	262595.477022	45.474561
3502.341046	262564.225207	45.479565
3502.225971	262535.697055	45.484570
3502.022589	262505.807536	45.489575
3502.086111	262481.300485	45.494580
3502.141617	262455.292250	45.499585
3501.847540	262434.074869	45.504589
3501.887316	262412.347165	45.509594
3501.844771	262387.805669	45.514599
3501.935418	262362.530425	45.519604
3502.137576	262339.555125	45.524609
3502.141019	262314.217045	45.529613
3501.894620	262292.330131	45.534618
3501.978530	262263.872804	45.539623
3501.761019	262250.843164	45.544628
3502.125598	262224.786780	45.549633
3502.073427	262193.192964	45.554637
3502.176093	262170.182182	45.559642
3501.992970	262148.871086	45.564647
3501.651461	262124.325124	45.569652
3502.145852	262097.280843	45.574657
3502.089524	262081.017522	45.579661
3501.944894	262056.364514	45.584666
3502.244547	262029.528775	45.589671
3502.022396	261992.460928	45.594676
3502.427467	261966.958411	45.599681
3501.958935	261942.202992	45.604685
3502.099758	261921.783646	45.609690
3502.163132	261887.930848	45.614695
3501.789850	261867.311378	45.619700
3501.965057	261835.987659	45.624705
3502.011246	261812.832802	45.629709
3501.990645	261796.130975	45.634714
3502.309635	261777.084452	45.639719
3502.121133	261753.380409	45.644724
3502.341136	261720.139812	45.649729
3502.051684	261700.194823	45.654733
3502.313826	261671.225775	45.659738
3502.282373	261647.293551	45.664743
3501.907433	261621.224780	45.669748
3502.397549	261580.811902	45.674753
3502.336593	261560.653076	45.679757
3502.362895	261530.803951	45.684762
3502.511826	261503.813286	45.689767
3502.282623	261472.959838	45.694772
3502.583338	261444.876007	45.699777
3502.308343	261415.302923	45.704781
3502.453127	261380.826143	45.709786
3502.388447	261361.100768	45.714791
3502.501545	261338.266448	45.719796
3502.332193	261290.291097	45.724801
3501.752406	261275.000395	45.729805
3502.241374	261226.362342	45.734810
3502.245376	261213.934740	45.739815
3502.054557	261182.591404	45.744820
3502.201572	261146.280717	45.749825
3501.900925	261082.970236	45.754829
3501.581428	260964.428709	45.759834
3501.302633	260814.456670	45.764839
3500.799247	260613.054131	45.769844
3500.241834	260361.900460	45.774849
3499.073028	260096.478931	45.779853
3498.218906	259777.708708	45.784858
3497.559129	259416.558265	45.789863
3495.927499	259024.770084	45.794868
3494.888152	258587.279459	45.799873
3493.410275	258127.369255	45.804877
3492.192529	257626.773362	45.809882
3490.226701	257095.172493	45.814887
3488.686043	256543.486942	45.819892
3487.207022	255953.590202	45.824897
3484.911797	255341.865929	45.829901
3482.971004	254697.232084	45.834906
3480.653877	254029.479282	45.839911
3478.196090	253344.173262	45.844916
3476.392410	252622.701289	45.849921
3473.749359	251894.276687	45.854925
3470.782330	251131.009245	45.859930
3468.209661	250368.924682	45.864935
3465.359261	249577.694317	45.869940
3463.093550	248768.109169	45.874945
3460.429651	247948.522597	45.879949
3457.521697	247106.100399	45.884954
3454.898622	246259.377019	45.889959
3451.636230	245389.726563	45.894964
3448.544528	244502.243779	45.899969
3445.340898	243612.584512	45.904973
3442.341011	242715.224132	45.909978
3439.534882	241799.442148	45.914983
3435.950599	240881.714991	45.919988
3432.551121	239948.598460	45.924993
3429.452780	239017.189334	45.929997
3425.983001	238078.551141	45.935002
3422.530282	237126.078120	45.940007
3419.109049	236172.986386	45.945012
3415.847704	235205.222867	45.950017
3412.192008	234251.577308	45.955021
3408.754495	233289.363789	45.960026
3405.755992	232329.092255	45.965031
3401.841656	231349.809050	45.970036
3398.700394	230367.704478	45.975041
3394.884081	229395.967840	45.980045
3391.373524	228413.995122	45.985050
3387.990061	227438.216410	45.990055
3384.053684	226453.812884	45.995060
3380.518695	225472.046412	46.000065
3376.966774	224496.242363	46.005069
3373.189832	223500.098337	46.010074
3369.713868	222512.847614	46.015079
3365.705615	221542.413601	46.020084
3362.145751	220559.405468	46.025089
3358.511854	219583.541352	46.030093
3354.468207	218599.388592	46.035098
3351.031156	217629.634881	46.040103
3347.337424	216663.488579	46.045108
3343.612571	215684.385555	46.050113
3339.830047	214716.525527	46.055117
3335.972265	213739.893022	46.060122
3332.207252	212790.754890	46.065127
3328.339973	211822.916159	46.070132
3324.905549	210862.017034	46.075137
3321.006871	209903.842183	46.080141
3317.468935	208947.015471	46.085146
3314.076040	207993.684515	46.090151
3309.525674	207038.576553	46.095156
3306.197432	206084.988903	46.100161
3302.184860	205136.401895	46.105165
3298.462580	204198.623435	46.110170
3295.038579	203263.528186	46.115175
3290.962397	202330.525659	46.120180
3287.150890	201386.841591	46.125185
3283.191016	200469.417003	46.130189
3279.646468	199543.885400	46.135194
3275.876142	198629.523387	46.140199
3271.587121	197715.782406	46.145204
3268.195161	196785.023246	46.150209
3264.199903	195888.361612	46.155213
3260.377666	194982.103626	46.160218
3256.974449	194080.395930	46.165223
3252.922801	193177.012804	46.170228
3249.244816	192290.945558	46.175233
3245.304936	191399.908776	46.180237
3241.469235	190516.960374	46.185242
3237.783856	189640.870837	46.190247
3233.891447	188767.443152	46.195252
3230.254999	187886.597766	46.200257
3226.602848	187022.415728	46.205261
3222.466206	186164.223836	46.210266
3218.920074	185294.055469	46.215271
3214.915572	184446.832391	46.220276
3211.696332	183582.433750	46.225281
3207.401522	182750.548623	46.230285
3203.788645	181902.370090	46.235290
3199.826446	181060.466559	46.240295
3196.253858	180227.422060	46.245300
3192.440080	179392.767746	46.250305
3188.834187	178564.454511	46.255309
3185.350365	177734.627927	46.260314
3181.385933	176906.704714	46.265319
3177.319393	176099.327485	46.270324
3173.981334	175279.521582	46.275329
3169.573594	174476.452753	46.280333
3165.871689	173667.706276	46.285338
3162.361109	172871.222994	46.290343
3158.384929	172083.489541	46.295348
3154.675370	171291.356362	46.300353
3150.851070	170497.772728	46.305357
3147.011000	169720.124869	46.310362
3143.119531	168944.771874	46.315367
3139.650383	168181.785400	46.320372
3136.028906	167407.629068	46.325377
3131.832661	166648.005547	46.330381
3128.343894	165882.654058	46.335386
3124.341477	165127.777805	46.340391
3120.510314	164386.744899	46.345396
3117.001950	163632.992357	46.350401
3113.413905	162897.831591	46.355405
3109.307161	162153.570039	46.360410
3105.639511	161420.385877	46.365415
3101.756400	160696.471479	46.370420
3098.066364	159963.714990	46.375425
3094.147540	159246.772332	46.380429
3090.229806	158533.057931	46.385434
3086.674930	157826.168224	46.390439
3082.620564	157116.513648	46.395444
3078.760240	156417.057176	46.400449
3075.058041	155733.989409	46.405453
3071.326699	155055.973976	46.410458
3067.403579	154365.307886	46.415463
3063.540867	153696.593905	46.420468
3060.028810	153018.772094	46.425473
3056.161591	152343.609867	46.430477
3052.191066	151686.237435	46.435482
3048.743102	151028.486097	46.440487
3044.252087	150387.066652	46.445492
3040.115914	149734.273822	46.450497
3036.464097	149104.102968	46.455501
3032.794771	148466.218052	46.460506
3029.036271	147844.108403	46.465511
3025.396046	147222.649429	46.470516
3021.517328	146605.943176	46.475521
3018.082609	145998.871393	46.480525
3014.007993	145393.738714	46.485530
3010.592329	144790.801085	46.490535
3006.297735	144192.079185	46.495540
3002.932469	143602.317531	46.500545
2999.154261	143019.867040	46.505549
2995.452106	142437.640616	46.510554
2991.980215	141855.079912	46.515559
2987.418361	141280.011785	46.520564
2983.941771	140701.002799	46.525569
2980.203108	140148.620249	46.530573
2976.568999	139592.792617	46.535578
2972.988561	139028.578792	46.540583
2968.958169	138481.986364	46.545588
2965.229521	137926.740198	46.550593
2961.708421	137386.798871	46.555597
2957.583706	136856.143262	46.560602
2953.880315	136311.141293	46.565607
2950.346052	135783.052447	46.570612
2946.882687	135256.701606	46.575617
2943.269474	134734.603824	46.580621
2939.861652	134215.456997	46.585626
2936.444524	133680.059755	46.590631
2932.725522	133160.057746	46.595636
2928.863349	132637.985180	46.600641
2925.288699	132126.839524	46.605645
2921.977116	131610.799594	46.610650
2918.101051	131088.938569	46.615655
2914.261219	130576.071594	46.620660
2911.043190	130062.134531	46.625665
2907.772554	129478.658098	46.630669
2903.964044	128974.353463	46.635674
2900.494936	128461.950398	46.640679
2897.032232	127956.090512	46.645684
2893.866209	127437.483797	46.650689
2890.081615	126933.950514	46.655693
2886.271698	126428.748382	46.660698
2882.924129	125931.760622	46.665703
2879.132950	125424.316699	46.670708
2875.480708	124920.622239	46.675713
2872.291475	124412.397784	46.680717
2868.355031	123914.407169	46.685722
2864.878663	123412.497524	46.690727
2861.396068	122913.545772	46.695732
2857.469147	122409.162581	46.700737
2853.800848	121919.129401	46.705741
2850.312396	121420.032127	46.710746
2847.021527	120937.570350	46.715751
2843.495394	120449.390235	46.720756
2839.633800	119948.767539	46.725761
2836.205615	119464.221742	46.730765
2832.177758	118979.139550	46.735770
2828.955412	118490.441096	46.740775
2825.199171	118009.512771	46.745780
2822.067421	117528.620546	46.750785
2818.240263	117049.076150	46.755789
2814.818586	116568.838992	46.760794
2811.300850	116079.836323	46.765799
2807.522843	115604.638949	46.770804
2803.855069	115117.096490	46.775809
2800.175804	114643.930607	46.780813
2796.446756	114180.454830	46.785818
2793.106758	113706.243785	46.790823
2789.533178	113235.304847	46.795828
2786.098880	112762.926319	46.800833
2782.410522	112298.972387	46.805837
2778.725183	111822.996208	46.810842
2775.189444	111358.140712	46.815847
2771.848304	110901.766683	46.820852
2768.231573	110433.121693	46.825857
2764.433249	109977.428289	46.830861
2760.886465	109510.691739	46.835866
2757.447655	109050.924237	46.840871
2753.914780	108595.054956	46.845876
2750.004808	108139.530028	46.850881
2746.706875	107687.551729	46.855885
2742.874042	107240.518843	46.860890
2739.572756	106778.878650	46.865895
2735.801416	106331.428542	46.870900
2732.090748	105878.089130	46.875905
2728.506517	105437.575230	46.880909
2724.822610	104998.239360	46.885914
2721.351457	104554.579562	46.890919
2717.268307	104116.448684	46.895924
2713.520944	103688.249705	46.900929
2710.085119	103259.918769	46.905933
2706.822853	102827.867441	46.910938
2703.075494	102400.040984	46.915943
2699.153024	101981.920171	46.920948
2695.135887	101557.629381	46.925953
2691.691618	101143.308846	46.930957
2687.964269	100731.033128	46.935962
2684.164043	100328.395490	46.940967
2680.139033	99916.939037	46.945972
2676.273843	99519.621600	46.950977
2672.704109	99129.787161	46.955981
2669.161584	98743.295802	46.960986
2665.771323	98344.088849	46.965991
2661.968075	97970.140634	46.970996
2658.594402	97576.418352	46.976001
2654.733384	97200.378506	46.981005
2650.757258	96819.785928	46.986010
2647.459333	96451.330702	46.991015
2644.007179	96074.452735	46.996020
2640.684112	95697.991292	47.001025
2637.092296	95315.997371	47.006029
2633.204673	94942.441382	47.011034
2630.219786	94574.544137	47.016039
2626.800139	94202.207720	47.021044
2623.279971	93824.960948	47.026049
2619.814859	93445.117942	47.031053
2616.326205	93081.916936	47.036058
2613.083217	92698.109405	47.041063
2609.164578	92325.492190	47.046068
2605.889188	91960.441555	47.051073
2602.370071	91576.564067	47.056077
2598.852982	91203.593179	47.061082
2595.601566	90824.969418	47.066087
2592.151455	90457.956537	47.071092
2588.730901	90072.977433	47.076097
2585.178814	89684.910849	47.081101
2581.801823	89308.193527	47.086106
2578.243317	88925.347107	47.091111
2574.579212	88543.436837	47.096116
2571.005774	88161.021888	47.101121
2568.186861	87775.496118	47.106125
2564.178760	87396.690691	47.111130
2560.834921	87015.461846	47.116135
2557.444380	86639.581082	47.121140
2553.905044	86251.532251	47.126145
2550.231042	85869.328011	47.131149
2546.785518	85484.184056	47.136154
2543.419418	85096.542936	47.141159
2539.819141	84707.787442	47.146164
2536.418512	84323.973152	47.151169
2532.993535	83933.981318	47.156173
2529.034103	83545.602337	47.161178
2526.446952	83152.429347	47.166183
2522.605764	82772.185041	47.171188
2519.168148	82385.239605	47.176193
2515.727051	81987.045719	47.181197
2512.080327	81596.155090	47.186202
2508.542208	81206.358060	47.191207
2504.820680	80819.592614	47.196212
2501.208022	80418.551628	47.201217
2498.005885	80040.454857	47.206221
2494.053828	79653.500113	47.211226
2490.858888	79259.485430	47.216231
2487.153031	78879.539586	47.221236
2484.285503	78499.328796	47.226241
2480.336118	78098.830982	47.231245
2476.791101	77707.344156	47.236250
2473.421473	77308.990216	47.241255
2469.906577	76922.069311	47.246260
2466.432708	76528.251498	47.251265
2463.013578	76131.522650	47.256269
2459.332926	75744.047426	47.261274
2455.885912	75343.994493	47.266279
2452.421341	74959.976499	47.271284
2448.712552	74566.338111	47.276289
2445.767514	74164.256272	47.281293
2441.887242	73777.069030	47.286298
2438.761701	73380.246181	47.291303
2435.086094	72986.168768	47.296308
2431.576589	72586.293775	47.301313
2427.886660	72188.840085	47.306317
2424.015515	71799.775601	47.311322
2421.023315	71394.162328	47.316327
2417.485125	71011.139754	47.321332
2413.867413	70615.438121	47.326337
2410.536828	70212.606613	47.331341
2406.660024	69818.068365	47.336346
2403.058268	69425.727878	47.341351
2399.506544	69040.736676	47.346356
2396.151218	68641.628002	47.351361
2393.173711	68240.600410	47.356365
2388.957072	67851.293231	47.361370
2386.158855	67455.607559	47.366375
2382.662350	67061.940964	47.371380
2378.832101	66670.414371	47.376385
2375.796900	66266.671833	47.381389
2371.683201	65870.174493	47.386394
2368.370242	65462.254298	47.391399
2364.862804	65075.367304	47.396404
2361.324775	64670.420962	47.401409
2357.946603	64275.535209	47.406413
2354.308074	63875.612365	47.411418
2350.810439	63477.451073	47.416423
2347.229302	63079.854938	47.421428
2343.872340	62677.026100	47.426433
2340.511880	62275.200728	47.431437
2336.514159	61880.988761	47.436442
2333.250836	61482.201042	47.441447
2329.885942	61096.572075	47.446452
2326.175207	60691.216044	47.451457
2322.955973	60285.675993	47.456461
2319.380246	59887.832162	47.461466
2315.908257	59491.025713	47.466471
2312.023810	59083.971949	47.471476
2308.537433	58681.317602	47.476481
2305.551392	58285.127843	47.481485
2302.090450	57892.857388	47.486490
2298.422193	57471.564586	47.491495
2294.879347	57081.185581	47.496500
2291.231135	56681.089773	47.501505
2288.047363	56265.897365	47.506509
2284.148859	55862.738869	47.511514
2280.886619	55463.478966	47.516519
2277.432671	55064.166779	47.521524
2273.753376	54660.613885	47.526529
2270.515761	54256.897628	47.531533
2266.782564	53849.820487	47.536538
2263.086260	53458.877737	47.541543
2259.344484	53056.155051	47.546548
2256.356584	52658.175048	47.551553
2252.687536	52234.019145	47.556557
2248.953144	51841.320396	47.561562
2245.669746	51435.832879	47.566567
2242.113212	51039.808650	47.571572
2238.576788	50628.963647	47.576577
2235.485528	50230.013678	47.581581
2231.537957	49825.901020	47.586586
2228.502574	49420.873312	47.591591
2224.536457	49017.519898	47.596596
2220.802181	48619.522547	47.601601
2217.568232	48202.337419	47.606605
2213.917255	47814.914398	47.611610
2210.647975	47408.480956	47.616615
2207.108756	47013.918945	47.621620
2203.604956	46615.743225	47.626625
2200.187567	46208.701131	47.631629
2196.539428	45802.285769	47.636634
2193.293674	45392.067074	47.641639
2189.453202	44984.535885	47.646644
2186.000051	44594.600699	47.651649
2182.873066	44189.427198	47.656653
2179.134951	43777.120598	47.661658
2175.613956	43367.254632	47.666663
2172.125716	42965.197168	47.671668
2168.524257	42556.183095	47.676673
2165.039233	42147.938423	47.681677
2161.315015	41748.577695	47.686682
2158.017106	41340.128672	47.691687
2153.907873	40946.092602	47.696692
2150.464632	40543.653923	47.701697
2147.327311	40135.868150	47.706701
2143.451811	39736.542351	47.711706
2140.093976	39329.180097	47.716711
2136.919913	38932.479855	47.721716
2132.981386	38533.287474	47.726721
2129.569729	38129.379748	47.731725
2126.016285	37738.238088	47.736730
2122.694529	37329.861904	47.741735
2119.276089	36934.643877	47.746740
2115.662509	36537.827972	47.751745
2112.348086	36129.067847	47.756749
2108.789810	35729.906523	47.761754
2105.243984	35327.746084	47.766759
2101.593233	34923.898111	47.771764
2098.231391	34530.306979	47.776769
2095.121738	34118.479441	47.781773
2091.392794	33724.187170	47.786778
2088.030632	33308.934935	47.791783
2084.195641	32910.998182	47.796788
2080.330682	32503.465064	47.801793
2077.079601	32098.094348	47.806797
2073.096333	31706.237397	47.811802
2070.084578	31289.259535	47.816807
2066.385781	30892.208395	47.821812
2063.029167	30497.183977	47.826817
2059.477718	30093.952486	47.831821
2055.675423	29694.411844	47.836826
2052.532134	29295.454469	47.841831
2049.038934	28900.627662	47.846836
2045.259114	28502.684618	47.851841
2041.873311	28101.437229	47.856845
2038.270557	27701.429116	47.861850
2034.970593	27297.668529	47.866855
2031.196976	26904.394041	47.871860
2027.840803	26505.315206	47.876865
2024.324361	26102.106328	47.881869
2020.708115	25715.781192	47.886874
2016.729285	25318.146937	47.891879
2013.303593	24922.766021	47.896884
2009.828774	24528.243176	47.901889
2006.528520	24123.393021	47.906893
2002.923683	23735.786406	47.911898
1999.515042	23338.989632	47.916903
1995.946697	22950.911110	47.921908
1992.379285	22560.223649	47.926913
1988.913365	22160.817590	47.931917
1984.774718	21772.413767	47.936922
1981.706806	21377.288234	47.941927
1978.370151	20990.459993	47.946932
1974.802961	20605.176482	47.951937
1971.385182	20217.172535	47.956941
1967.582691	19824.840235	47.961946
1964.393734	19429.474991	47.966951
1960.700074	19041.714631	47.971956
1957.421872	18650.971120	47.976961
1954.208539	18255.069771	47.981965
1950.347046	17868.239290	47.986970
1946.517130	17466.274816	47.991975
1943.001864	17080.986358	47.996980
1939.298625	16691.412478	48.001985
1936.280946	16305.156432	48.006989
1932.239024	15922.161159	48.011994
1928.852123	15534.781143	48.016999
1925.311800	15144.526161	48.022004
1921.932816	14768.527476	48.027009
1918.502469	14373.528080	48.032013
1914.563452	13999.525093	48.037018
1910.970437	13608.989948	48.042023
1907.252610	13228.021397	48.047028
1903.843320	12854.069344	48.052033
1900.204733	12476.744399	48.057037
1896.604874	12100.411865	48.062042
1893.387822	11716.527626	48.067047
1889.290021	11343.462956	48.072052
1886.085977	10972.954208	48.077057
1882.625429	10603.914035	48.082061
1878.877890	10239.044110	48.087066
1875.651841	9873.726630	48.092071
1872.111448	9508.120204	48.097076
1867.984569	9142.742016	48.102081
1863.984431	8772.888299	48.107085
1860.548577	8410.908233	48.112090
1856.786161	8064.431852	48.117095
1853.134334	7713.554816	48.122100
1849.295233	7378.044869	48.127105
1845.333698	7043.952667	48.132109
1840.968498	6714.363372	48.137114
1837.298384	6384.098980	48.142119
1833.327602	6075.926845	48.147124
1829.318392	5772.560443	48.152129
1825.554522	5461.467572	48.157133
1821.827090	5164.627786	48.162138
1818.276635	4868.008963	48.167143
1814.142889	4578.571116	48.172148
1810.443169	4303.269314	48.177153
1807.113853	4016.208838	48.182157
1803.814830	3745.216883	48.187162
1800.196311	3469.668285	48.192167
1796.827602	3188.667765	48.197172
1793.186214	2923.443444	48.202177
1789.414066	2655.462058	48.207181
1785.589868	2386.480240	48.212186
1781.957431	2119.409024	48.217191
1778.094650	1869.599527	48.222196
1774.276378	1617.885018	48.227201
1770.752675	1361.600578	48.232205
1767.285047	1127.214854	48.237210
1763.307634	886.327526	48.242215
1759.632496	637.610221	48.247220
1754.781805	442.598011	48.252225
1749.704483	268.877365	48.257229
1744.054060	112.024901	48.262234
1736.387387	41.091442	48.267239
1726.857738	66.444936	48.272244
1720.464809	72.444945	48.277249
1717.014146	69.236151	48.282253
1714.699298	76.828713	48.287258
1712.741198	77.835817	48.292263
1710.576775	71.582640	48.297268
1707.678431	72.568406	48.302273
1704.917308	65.231197	48.307277
1701.338066	81.451884	48.312282
1697.589223	77.061972	48.317287
1695.270413	72.120463	48.322292
1691.094967	81.337705	48.327297
1687.778421	69.015486	48.332301
1684.042667	68.467469	48.337306
1680.727723	67.933051	48.342311
1677.996593	67.355223	48.347316
1675.066266	72.316445	48.352321
1671.715314	75.394280	48.357325
1668.058367	76.855620	48.362330
1664.089814	72.310087	48.367335
1660.950588	73.855362	48.372340
1657.052343	81.064787	48.377345
1654.270246	64.796484	48.382349
1650.556837	71.113440	48.387354
1647.202383	68.038375	48.392359
1643.885435	76.100114	48.397364
1640.147308	78.317567	48.402369
1637.246014	77.500474	48.407373
1633.711492	86.443960	48.412378
1629.693082	74.215170	48.417383
1626.556936	69.714089	48.422388
1622.856617	72.517275	48.427393
1619.380130	75.358390	48.432397
1616.448215	76.368370	48.437402
1612.867904	71.534629	48.442407
1609.778665	66.690896	48.447412
1605.636479	71.733172	48.452417
1602.410437	68.698236	48.457421
1599.079215	76.249674	48.462426
1595.193775	75.690162	48.467431
1591.918492	68.037527	48.472436
1588.403813	82.204395	48.477441
1584.746147	76.588601	48.482445
1581.422770	75.068421	48.487450
1578.031903	66.997184	48.492455
1575.063227	66.174766	48.497460
1571.369469	74.975354	48.502465
1567.647081	70.780659	48.507469
1564.212133	68.755833	48.512474
1560.523382	81.810853	48.517479
1557.269189	68.640568	48.522484
1553.601640	75.146543	48.527489
1550.183873	66.136708	48.532493
1546.621327	69.646112	48.537498
1543.272980	73.182288	48.542503
1539.831653	66.438184	48.547508
1536.550002	70.577742	48.552513
1533.268965	68.377105	48.557517
1529.354179	69.777349	48.562522
1525.682450	69.943876	48.567527
1522.559034	55.133428	48.572532
1518.650607	67.656324	48.577537
1515.493846	59.798597	48.582541
1511.637725	66.988811	48.587546
1508.235576	72.358830	48.592551
1504.770527	75.947975	48.597556
1501.411116	79.444749	48.602561
1498.297637	64.566313	48.607565
1494.738610	71.419226	48.612570
1491.060181	70.517461	48.617575
1487.549199	70.108485	48.622580
1483.778684	78.177549	48.627585
1480.483283	69.816224	48.632589
1476.654448	69.703492	48.637594
1473.340388	71.083006	48.642599
1469.936008	64.741282	48.647604
1466.378276	62.115490	48.652609
1463.467750	62.669739	48.657613
1459.874500	66.158618	48.662618
1455.829449	56.303651	48.667623
1452.756717	60.239853	48.672628
1449.363970	61.672744	48.677633
1445.995278	68.942117	48.682637
1442.382219	71.810828	48.687642
1438.439773	73.620343	48.692647
1434.878545	62.519494	48.697652
1431.031887	71.005365	48.702657
1428.103884	60.571579	48.707661
1424.875615	70.720226	48.712666
1421.378379	63.193914	48.717671
1417.692001	62.438926	48.722676
1413.965860	73.614183	48.727681
1410.589867	63.588645	48.732685
1407.559412	71.941149	48.737690
1403.946068	73.186920	48.742695
1400.447489	66.416948	48.747700
1396.616761	61.625381	48.752705
1393.305419	66.089102	48.757709
1389.343834	61.947484	48.762714
1385.668677	60.678231	48.767719
1382.777315	56.322581	48.772724
1378.938700	56.644811	48.777729
1375.695613	57.092644	48.782733
1371.982381	57.778168	48.787738
1368.504203	58.983921	48.792743
1365.675190	58.864275	48.797748
1361.861180	68.743427	48.802753
1358.663777	68.608355	48.807757
1354.920337	68.665840	48.812762
1351.181518	75.236700	48.817767
1347.407961	69.819315	48.822772
1343.906808	65.685129	48.827777
1340.538971	61.498557	48.832781
1337.614423	74.380838	48.837786
1333.790216	66.585896	48.842791
1330.263754	60.566915	48.847796
1326.592376	67.633471	48.852801
1323.136718	59.107298	48.857805
1319.248233	61.481057	48.862810
1316.235496	62.987687	48.867815
1312.853461	57.686538	48.872820
1309.232068	56.930939	48.877825
1305.678326	58.980516	48.882829
1302.549111	70.793678	48.887834
1298.735482	67.382007	48.892839
1295.306821	55.653123	48.897844
1291.176149	67.865767	48.902849
1287.933377	64.675288	48.907853
1284.955457	65.107165	48.912858
1281.324617	62.489612	48.917863
1277.989547	64.574757	48.922868
1274.323016	71.966425	48.927873
1270.939317	60.894925	48.932877
1267.600612	65.799505	48.937882
1263.519916	66.754206	48.942887
1260.094112	63.880118	48.947892
1256.821950	67.913812	48.952897
1253.142999	66.594545	48.957901
1250.003480	68.003857	48.962906
1245.784479	68.606770	48.967911
1242.724433	61.809694	48.972916
1238.986602	67.250959	48.977921
1235.486765	60.538158	48.982925
1232.288897	64.212281	48.987930
1228.579484	66.532865	48.992935
1225.380905	66.195511	48.997940
1221.868449	69.981876	49.002945
1218.033759	66.877211	49.007949
1215.020938	59.237570	49.012954
1211.081872	69.085573	49.017959
1207.769052	61.375571	49.022964
1203.896307	67.226974	49.027969
1200.700166	62.747944	49.032973
1197.602949	63.486296	49.037978
1193.583156	71.492932	49.042983
1190.467539	58.930740	49.047988
1186.772438	59.224325	49.052993
1183.358112	64.463380	49.057997
1179.854052	66.274284	49.063002
1176.123664	60.318706	49.068007
1173.040035	49.766830	49.073012
1168.979995	59.832973	49.078017
1165.747776	57.434959	49.083021
1162.182775	59.856456	49.088026
1158.357861	65.349244	49.093031
1155.095787	59.675110	49.098036
1151.754006	64.788981	49.103041
1148.161458	57.729964	49.108045
1144.639304	53.086558	49.113050
1141.129289	62.437512	49.118055
1137.633761	57.669740	49.123060
1134.212362	63.444564	49.128065
1130.746763	67.982933	49.133069
1127.388359	59.410020	49.138074
1123.693181	58.131261	49.143079
1120.550954	49.667072	49.148084
1116.873100	58.629704	49.153089
1112.911171	63.182056	49.158093
1109.507796	61.010003	49.163098
1106.337401	68.982503	49.168103
1103.262386	56.654453	49.173108
1099.165085	58.051513	49.178113
1095.514891	60.112959	49.183117
1092.222658	59.454844	49.188122
1088.347674	62.687052	49.193127
1085.010577	51.845619	49.198132
1081.550001	61.802638	49.203137
1078.085722	51.534652	49.208141
1074.845015	55.424256	49.213146
1070.971018	58.178592	49.218151
1067.798258	61.187602	49.223156
1064.348519	66.928879	49.228161
1060.388501	60.939463	49.233165
1057.086740	58.748436	49.238170
1053.339710	69.556794	49.243175
1050.276390	55.306564	49.248180
1046.796305	57.297244	49.253185
1043.271740	65.587461	49.258189
1039.561401	55.503313	49.263194
1035.810899	74.737166	49.268199
1032.482301	57.646092	49.273204
1028.943555	62.702045	49.278209
1025.651570	57.102189	49.283213
1022.670463	57.759210	49.288218
1018.553116	65.075531	49.293223
1015.253572	61.049215	49.298228
1011.423881	57.519868	49.303233
1007.801785	63.585364	49.308237
1004.905950	56.253410	49.313242
1001.234856	58.276991	49.318247
997.566166	53.020512	49.323252
993.812519	63.121228	49.328257
990.441677	62.076733	49.333261
987.110103	58.858988	49.338266
983.461842	65.656212	49.343271
980.522956	62.339377	49.348276
976.330264	51.710241	49.353281
972.910893	55.130962	49.358285
969.611217	56.685449	49.363290
966.248207	61.106620	49.368295
963.180238	54.766398	49.373300
959.197700	48.628652	49.378305
955.254259	52.820639	49.383309
952.030049	53.009315	49.388314
948.496269	61.639485	49.393319
944.990269	52.080363	49.398324
941.329492	58.063300	49.403329
938.230089	59.868184	49.408333
934.703628	56.484634	49.413338
931.060688	52.704772	49.418343
927.921590	54.500017	49.423348
923.886305	56.425275	49.428353
920.241206	63.399177	49.433357
916.865242	61.507616	49.438362
913.029006	63.791026	49.443367
910.147754	53.270969	49.448372
906.529168	66.160033	49.453377
903.112074	70.741488	49.458381
899.694098	60.738404	49.463386
895.969169	67.098322	49.468391
892.414294	57.420267	49.473396
889.102147	63.035734	49.478401
885.455319	67.301779	49.483405
882.533658	50.871893	49.488410
878.648613	59.778204	49.493415
875.043821	51.784689	49.498420
870.997402	52.443042	49.503425
867.726476	63.322819	49.508429
864.699973	67.406884	49.513434
860.878714	71.503935	49.518439
857.407534	57.994269	49.523444
854.030265	63.316159	49.528449
850.433632	62.794039	49.533453
847.173452	61.909503	49.538458
843.479211	59.399956	49.543463
840.121179	57.432849	49.548468
836.608876	58.444653	49.553473
832.904695	62.763922	49.558477
829.665549	57.586135	49.563482
825.806116	66.130967	49.568487
822.545739	54.711341	49.573492
818.632326	58.484223	49.578497
815.393878	67.068429	49.583501
812.074765	56.989865	49.588506
808.179172	57.979082	49.593511
804.858287	59.897548	49.598516
801.352126	63.217902	49.603521
797.753830	57.861914	49.608525
794.901315	56.214747	49.613530
790.769384	71.240132	49.618535
787.438214	65.276258	49.623540
784.423776	70.038646	49.628545
780.692438	65.576550	49.633549
776.950892	57.424008	49.638554
772.892405	59.144092	49.643559
769.567899	54.267500	49.648564
766.415284	56.729242	49.653569
762.742138	62.037087	49.658573
759.242719	50.246571	49.663578
755.892331	64.672571	49.668583
752.598464	61.379388	49.673588
748.863107	57.427281	49.678593
745.276814	63.616934	49.683597
741.937664	62.070836	49.688602
738.036095	62.026463	49.693607
734.793448	58.114715	49.698612
731.569027	55.933838	49.703617
727.842785	58.301385	49.708621
724.701300	56.196182	49.713626
720.781297	61.207106	49.718631
717.628414	49.223452	49.723636
713.742629	58.322873	49.728641
710.158455	62.769001	49.733645
706.958591	49.875191	49.738650
703.220893	61.748268	49.743655
700.163226	58.462616	49.748660
696.468951	54.690781	49.753665
692.754212	52.605220	49.758669
689.217010	51.653099	49.763674
685.536419	54.212856	49.768679
682.293726	52.449275	49.773684
678.556279	62.104564	49.778689
675.324787	54.160540	49.783693
672.309066	53.889692	49.788698
668.512720	60.131031	49.793703
665.381503	54.411297	49.798708
661.357107	46.767878	49.803713
657.498483	57.701180	49.808717
653.978014	54.323068	49.813722
650.243507	60.836351	49.818727
647.408667	47.743365	49.823732
643.755105	51.785855	49.828737
640.018159	63.108335	49.833741
636.650994	47.842505	49.838746
633.345165	51.457547	49.843751
630.209575	44.289531	49.848756
626.954007	49.228664	49.853761
622.855641	45.244509	49.858765
619.328056	41.693509	49.863770
615.398380	52.688490	49.868775
612.131772	52.488342	49.873780
608.687894	52.720744	49.878785
605.290886	47.985179	49.883789
601.848544	48.397672	49.888794
598.013826	44.416770	49.893799
594.427024	44.241161	49.898804
590.994606	53.273173	49.903809
587.621421	47.739816	49.908813
584.603992	36.978444	49.913818
580.790513	45.642676	49.918823
577.007227	47.247178	49.923828
574.018122	54.523932	49.928833
570.343936	53.947485	49.933837
566.703105	49.920585	49.938842
563.047402	56.307713	49.943847
559.893593	49.208981	49.948852
556.062069	55.085653	49.953857
552.204974	49.981966	49.958861
549.146293	46.225105	49.963866
545.947716	52.553725	49.968871
542.428100	46.043445	49.973876
539.057841	49.200299	49.978881
535.262581	49.895528	49.983885
531.606992	43.754424	49.988890
528.296006	48.037817	49.993895
524.521160	54.554224	49.998900
520.921969	44.936937	50.003905
517.143117	58.436234	50.008909
514.265979	46.672287	50.013914
510.720736	48.828186	50.018919
507.086768	58.666686	50.023924
503.956481	42.962228	50.028929
500.386070	59.494692	50.033933
496.783940	50.972502	50.038938
492.986438	50.775924	50.043943
489.111300	50.816056	50.048948
485.778952	48.171135	50.053953
482.583792	53.936090	50.058957
479.512833	40.474953	50.063962
475.681551	54.444309	50.068967
472.356343	50.051921	50.073972
468.576366	56.758954	50.078977
465.225031	54.714928	50.083981
461.969624	45.034643	50.088986
457.952980	54.379072	50.093991
454.149116	57.090922	50.098996
450.809667	52.915884	50.104001
447.703813	60.922652	50.109005
444.270042	61.071245	50.114010
440.861902	52.854216	50.119015
437.013261	55.430672	50.124020
433.722360	58.856753	50.129025
429.855485	55.817337	50.134029
426.722615	48.047831	50.139034
423.120918	60.665357	50.144039
419.459296	57.578170	50.149044
415.989027	58.203839	50.154049
412.070837	55.621658	50.159053
408.817574	52.831561	50.164058
405.620313	51.772774	50.169063
401.960498	47.419836	50.174068
398.707641	52.776173	50.179073
394.935961	56.805441	50.184077
391.722193	49.010571	50.189082
387.805633	51.433095	50.194087
384.661434	49.018320	50.199092
381.116056	44.638080	50.204097
377.575032	51.545195	50.209101
374.224773	47.700878	50.214106
371.011929	46.046586	50.219111
366.875228	48.474911	50.224116
363.317306	47.763338	50.229121
359.532068	51.256893	50.234125
356.450786	47.411833	50.239130
352.584314	49.048296	50.244135
349.548652	51.358995	50.249140
346.246925	51.142202	50.254145
342.178126	57.410167	50.259149
339.187571	48.856073	50.264154
335.647540	52.188072	50.269159
332.174798	53.231743	50.274164
328.609347	47.177883	50.279169
324.876294	54.254100	50.284173
321.633068	50.548149	50.289178
317.676090	49.221681	50.294183
314.222806	52.119407	50.299188
311.115207	56.051625	50.304193
307.479129	56.807523	50.309197
304.386781	40.372729	50.314202
300.463154	50.310114	50.319207
297.017785	47.021607	50.324212
293.419272	50.875233	50.329217
289.954342	59.308061	50.334221
286.548069	50.726951	50.339226
282.618623	53.980381	50.344231
279.201204	60.159597	50.349236
275.699479	54.573540	50.354241
271.836326	56.057642	50.359245
268.930735	47.151820	50.364250
265.388810	48.481511	50.369255
262.183842	50.011837	50.374260
258.954309	46.800463	50.379265
254.577057	52.126225	50.384269
251.281739	48.178464	50.389274
247.952841	48.462613	50.394279
244.079340	50.097023	50.399284
240.790270	50.827379	50.404289
237.347157	49.344993	50.409293
233.975538	45.725484	50.414298
230.003121	61.384086	50.419303
226.808255	57.626327	50.424308
223.599929	44.196125	50.429313
219.867898	53.034364	50.434317
216.183259	57.012137	50.439322
212.910720	54.063722	50.444327
209.652067	49.778073	50.449332
206.143525	55.019213	50.454337
202.162947	63.902481	50.459341
199.055256	45.072027	50.464346
195.165514	53.409650	50.469351
191.379071	51.683338	50.474356
188.388092	56.138400	50.479361
184.701127	54.244745	50.484365
181.354079	55.439705	50.489370
177.722708	55.688699	50.494375
174.328244	61.310707	50.499380
171.398843	54.452347	50.504385
167.371802	52.304763	50.509389
164.199595	53.950221	50.514394
160.248450	64.717628	50.519399
156.553863	61.388851	50.524404
153.406565	46.778600	50.529409
149.551616	55.012737	50.534413
146.490268	58.159504	50.539418
143.024489	56.414912	50.544423
139.163736	66.722169	50.549428
135.712491	54.712331	50.554433
131.721209	52.786972	50.559437
128.782897	48.144586	50.564442
125.275665	55.261592	50.569447
121.656054	55.122794	50.574452
118.412961	49.806542	50.579457
114.795348	50.230570	50.584461
111.352698	42.566304	50.589466
107.824719	55.963280	50.594471
104.439130	54.351739	50.599476
100.689290	47.924844	50.604481
96.948391	58.697483	50.609485
93.736401	55.379001	50.614490
90.506885	51.408367	50.619495
86.604482	52.952389	50.624500
82.896966	56.576244	50.629505
79.468359	53.826152	50.634509
76.129826	55.671518	50.639514
72.644752	63.414654	50.644519
69.146629	65.025447	50.649524
66.101739	38.959415	50.654529
62.158347	48.792328	50.659533
59.164403	56.054046	50.664538
55.192308	59.725425	50.669543
51.722143	54.327481	50.674548
48.224192	58.899453	50.679553
44.363194	57.751072	50.684557
41.064018	52.766260	50.689562
37.527978	50.210069	50.694567
34.299043	56.347305	50.699572
30.638506	48.134861	50.704577
27.219452	52.188361	50.709581
23.914639	49.115293	50.714586
20.214410	46.483431	50.719591
16.721355	47.520815	50.724596
13.218098	48.812882	50.729601
9.254932	47.632961	50.734605
6.289010	47.838482	50.739610
2.658736	57.730219	50.744615