Fri Aug 26 10:43:53 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
1.745133	117.237319	0.000000
2.238723	111.263594	0.005005
1.775076	118.264455	0.010010
1.816898	116.372611	0.015014
2.247770	131.092778	0.020019
1.797558	108.856002	0.025024
1.873291	101.944454	0.030029
1.377388	101.193002	0.035034
1.423601	97.402272	0.040038
1.596024	96.916913	0.045043
1.307290	78.429297	0.050048
1.022798	71.029696	0.055053
0.540649	73.316389	0.060058
0.171951	58.400373	0.065062
-0.069570	53.673715	0.070067
-0.526869	47.557005	0.075072
-0.692744	37.791510	0.080077
-1.120028	37.462799	0.085082
-1.090808	32.599083	0.090086
-1.996637	26.046029	0.095091
-2.128846	16.914364	0.100096
-2.321103	12.170556	0.105101
-2.616848	22.985919	0.110106
-2.481007	16.941380	0.115110
-2.855520	6.999586	0.120115
-3.141281	8.603981	0.125120
-3.200510	4.924597	0.130125
-3.961583	3.527922	0.135130
-4.103766	-5.871089	0.140134
-4.246906	1.269642	0.145139
-4.706828	2.787262	0.150144
-4.339698	-7.092832	0.155149
-5.353949	1.708411	0.160154
-5.724936	1.500645	0.165158
-5.620032	-8.699276	0.170163
-6.212491	6.695792	0.175168
-5.684360	-5.813059	0.180173
-5.914921	-5.992070	0.185178
-6.611543	-11.960770	0.190182
-7.057523	-0.679118	0.195187
-7.357677	3.268622	0.200192
-7.085090	-10.450082	0.205197
-7.416384	1.582482	0.210202
-8.198751	2.802303	0.215206
-8.600454	-12.956374	0.220211
-8.910492	-0.417773	0.225216
-8.700524	-8.694730	0.230221
-8.783148	-8.593064	0.235226
-8.760576	-2.313340	0.240230
-8.755637	-3.351569	0.245235
-9.752653	-9.833465	0.250240
-10.342935	-10.380398	0.255245
-10.188775	-3.178393	0.260250
-10.618342	-12.020143	0.265254
-10.179655	-14.919696	0.270259
-10.611845	-5.826280	0.275264
-11.264753	-11.444292	0.280269
-11.745360	-7.882896	0.285274
-11.954318	-8.024144	0.290278
-11.767871	-7.761897	0.295283
-12.172212	-3.604953	0.300288
-11.745253	-11.874567	0.305293
-12.622386	-6.470296	0.310298
-13.233158	-9.892964	0.315302
-13.099375	-16.136482	0.320307
-13.475555	-11.088610	0.325312
-13.433628	-11.692849	0.330317
-14.067794	-14.773364	0.335322
-14.696944	-9.818978	0.340326
-14.712485	-14.413128	0.345331
-14.721869	-16.483641	0.350336
-14.871536	-13.476793	0.355341
-15.138288	-2.972836	0.360346
-15.240297	-12.915918	0.365350
-15.265234	-16.999256	0.370355
-15.587857	-8.302540	0.375360
-15.744721	-5.955774	0.380365
-16.121388	-5.517270	0.385370
-16.626716	-13.780929	0.390374
-16.981161	-7.458324	0.395379
-17.432605	-10.579943	0.400384
-17.362249	-18.578903	0.405389
-17.355878	-14.093615	0.410394
-17.735456	-6.106179	0.415398
-18.368480	-9.724693	0.420403
-18.978994	-4.592880	0.425408
-18.655642	-9.764963	0.430413
-18.791132	-5.431587	0.435418
-19.059098	-3.026395	0.440422
-19.130264	-10.993832	0.445427
-19.733958	-4.015507	0.450432
-20.050102	-12.349749	0.455437
-20.438707	-6.297063	0.460442
-20.388848	-9.218333	0.465446
-20.399874	-12.088994	0.470451
-20.730551	-10.708554	0.475456
-21.021445	-8.249175	0.480461
-22.037027	-10.163025	0.485466
-21.954463	-10.109224	0.490470
-21.885255	-15.599228	0.495475
-21.950643	-7.594275	0.500480
-21.974430	-10.105457	0.505485
-23.095610	0.696045	0.510490
-23.470874	-6.588152	0.515494
-23.235282	1.382598	0.520499
-23.731654	0.833697	0.525504
-23.576837	-6.415976	0.530509
-23.445787	1.824143	0.535514
-23.887733	-2.630855	0.540518
-24.291697	-5.415029	0.545523
-25.034964	-0.971204	0.550528
-24.928101	-11.237864	0.555533
-24.982691	-8.267965	0.560538
-25.457478	0.063317	0.565542
-26.085097	-8.722287	0.570547
-26.232192	-7.617195	0.575552
-26.182245	-9.428036	0.580557
-26.166937	-1.312262	0.585562
-26.705367	-5.252379	0.590566
-26.736153	-11.397510	0.595571
-27.168961	-1.424501	0.600576
-27.510507	-6.670225	0.605581
-27.993314	-1.640550	0.610586
-28.385632	-5.764763	0.615590
-28.023480	-1.904325	0.620595
-28.254936	-4.111100	0.625600
-28.353484	-12.359001	0.630605
-28.925164	-4.623220	0.635610
-29.414671	-2.528374	0.640614
-29.819208	-17.476706	0.645619
-29.512554	-4.341287	0.650624
-29.342054	-16.085788	0.655629
-30.219175	-4.743341	0.660634
-30.936953	-9.516047	0.665638
-30.958904	-9.243499	0.670643
-31.371691	-5.964737	0.675648
-30.954506	-14.337227	0.680653
-31.386595	-7.720969	0.685658
-31.363557	-7.755973	0.690662
-31.681098	-18.633572	0.695667
-32.470133	-17.216567	0.700672
-32.094258	-13.937217	0.705677
-32.582553	-6.723768	0.710682
-32.947876	-14.284746	0.715686
-33.575452	-10.206938	0.720691
-34.117978	-1.830311	0.725696
-34.434674	-6.001097	0.730701
-34.249291	-4.514351	0.735706
-33.821140	-4.296065	0.740710
-33.954962	-10.586500	0.745715
-34.153074	-8.505387	0.750720
-34.730563	-12.126219	0.755725
-35.367351	-15.848546	0.760730
-35.347858	-16.749839	0.765734
-35.135941	-13.925836	0.770739
-36.098666	-8.084309	0.775744
-36.451379	-5.371704	0.780749
-37.151041	-3.753485	0.785754
-37.615330	-1.089943	0.790758
-36.953192	-4.815202	0.795763
-37.319885	-0.588192	0.800768
-37.214375	-2.141936	0.805773
-36.724969	-5.960520	0.810778
-37.463245	-11.622184	0.815782
-37.885260	-12.223789	0.820787
-38.276356	-9.505207	0.825792
-38.943077	-14.621208	0.830797
-39.649687	-11.347317	0.835802
-39.780995	-4.809526	0.840806
-39.497185	-5.581136	0.845811
-39.765821	-4.577340	0.850816
-40.023161	-3.154536	0.855821
-39.872993	-2.206455	0.860826
-40.590130	-6.039656	0.865830
-40.157917	-11.178068	0.870835
-41.530170	-2.700727	0.875840
-41.421127	-14.549550	0.880845
-41.610271	-7.164387	0.885850
-41.798418	-5.429664	0.890854
-41.566243	-9.375870	0.895859
-42.041719	-7.112371	0.900864
-42.492300	0.841831	0.905869
-42.781171	3.405297	0.910874
-43.275792	3.109217	0.915878
-43.192177	-7.770737	0.920883
-43.377062	-5.030479	0.925888
-43.391275	-5.825288	0.930893
-43.984211	-6.238934	0.935898
-44.427090	-3.357270	0.940902
-44.567740	1.441968	0.945907
-45.040375	1.262683	0.950912
-44.831310	-2.271814	0.955917
-44.890439	-8.491624	0.960922
-45.451451	-3.933812	0.965926
-46.215998	-13.539625	0.970931
-46.264489	-0.608329	0.975936
-46.460217	-6.063412	0.980941
-46.587580	-5.904162	0.985946
-46.638263	-2.134466	0.990950
-46.449941	-11.493183	0.995955
-47.572880	-0.982466	1.000960
-47.637813	-11.719069	1.005965
-47.715076	-7.040431	1.010970
-48.085452	-8.953501	1.015974
-47.772276	-5.265767	1.020979
-48.439741	0.415899	1.025984
-49.063939	-1.087504	1.030989
-49.234639	2.536369	1.035994
-49.438801	2.128628	1.040998
-49.268005	-4.437020	1.046003
-49.507235	-7.170913	1.051008
-49.817356	-12.617674	1.056013
-50.199375	-3.494107	1.061018
-50.830053	4.532428	1.066022
-50.605054	-7.445181	1.071027
-50.905573	0.805185	1.076032
-50.934741	-1.040793	1.081037
-51.735624	2.295233	1.086042
-52.183406	1.684986	1.091046
-52.317018	-3.495040	1.096051
-52.579860	-3.507678	1.101056
-52.614491	-3.027518	1.106061
-52.429038	-10.313595	1.111066
-52.909968	-8.055575	1.116070
-52.661768	-10.751469	1.121075
-53.332719	-10.751183	1.126080
-53.482831	-7.010299	1.131085
-54.009714	-10.673810	1.136090
-54.524061	-5.863845	1.141094
-54.720653	-7.854591	1.146099
-55.207259	-3.048945	1.151104
-55.436651	-7.812272	1.156109
-55.340162	-4.888042	1.161114
-55.741325	7.497075	1.166118
-55.300245	-6.839465	1.171123
-55.788224	-5.950209	1.176128
-56.014975	0.346188	1.181133
-56.678139	-2.732975	1.186138
-56.963484	-0.730026	1.191142
-56.641868	-8.790253	1.196147
-56.627771	-8.577100	1.201152
-57.514531	-0.507533	1.206157
-58.185338	-5.705153	1.211162
-58.297062	-2.837086	1.216166
-58.108162	-1.547035	1.221171
-58.545327	-13.257031	1.226176
-58.601058	-2.611931	1.231181
-59.081572	-10.828832	1.236186
-59.974915	-4.621633	1.241190
-59.924468	-4.651413	1.246195
-60.101862	-8.692032	1.251200
-60.004170	-7.748436	1.256205
-60.032502	-11.907173	1.261210
-60.087023	-2.176557	1.266214
-59.947778	-9.300421	1.271219
-60.747640	-5.569099	1.276224
-61.256045	-16.477087	1.281229
-61.213124	-6.185860	1.286234
-62.196727	-14.020718	1.291238
-62.202014	-10.732641	1.296243
-62.959358	-5.372330	1.301248
-62.671772	-7.096787	1.306253
-62.835947	-4.242699	1.311258
-63.205427	5.869143	1.316262
-62.796192	-9.313460	1.321267
-63.286289	-3.504392	1.326272
-63.933556	-2.637789	1.331277
-64.126023	-11.785361	1.336282
-64.315419	-6.004131	1.341286
-64.149438	-7.693837	1.346291
-64.330681	0.057081	1.351296
-64.771668	-9.570636	1.356301
-65.265333	-1.992531	1.361306
-65.818909	2.212958	1.366310
-65.400057	1.973962	1.371315
-65.806017	2.923212	1.376320
-66.717411	-1.575746	1.381325
-66.901363	5.362537	1.386330
-67.373720	3.446363	1.391334
-67.569535	2.075572	1.396339
-67.628813	4.770964	1.401344
-67.476956	4.877249	1.406349
-66.907076	3.146802	1.411354
-67.462890	10.547933	1.416358
-67.683600	-1.660829	1.421363
-68.387536	-2.667777	1.426368
-68.682868	2.142889	1.431373
-69.815515	-5.516910	1.436378
-70.229564	2.169020	1.441382
-69.278835	-5.767705	1.446387
-69.583023	-1.085371	1.451392
-69.924439	3.017485	1.456397
-69.978514	0.251599	1.461402
-70.674683	1.141634	1.466406
-70.992712	-6.695619	1.471411
-71.437156	6.531439	1.476416
-71.609257	6.330672	1.481421
-71.640659	-0.285749	1.486426
-71.951688	-0.189648	1.491430
-71.539921	-5.419787	1.496435
-71.834332	-5.237691	1.501440
-72.711293	1.862274	1.506445
-73.037532	-0.298106	1.511450
-73.430598	-1.454693	1.516454
-73.280093	0.916979	1.521459
-73.150214	6.272026	1.526464
-73.564765	-6.523463	1.531469
-74.083836	-9.577605	1.536474
-74.620500	-1.306292	1.541478
-74.799662	-2.214618	1.546483
-74.994925	-2.737636	1.551488
-75.129481	-1.482641	1.556493
-74.762235	-6.693193	1.561498
-75.355466	1.843184	1.566502
-75.874113	-2.049393	1.571507
-76.043456	4.282357	1.576512
-76.192585	2.005819	1.581517
-76.215982	-3.849406	1.586522
-76.793552	1.966955	1.591526
-76.992147	-8.657090	1.596531
-77.393473	-3.383847	1.601536
-77.426628	-3.052609	1.606541
-77.612579	-9.078669	1.611546
-78.451915	-1.503689	1.616550
-78.458876	2.338291	1.621555
-78.747129	7.426257	1.626560
-79.169231	-1.853238	1.631565
-78.880178	3.116368	1.636570
-79.400734	10.799902	1.641574
-79.215168	-2.996997	1.646579
-80.329171	4.633406	1.651584
-80.610214	4.981095	1.656589
-80.850143	-5.522624	1.661594
-81.215287	1.143321	1.666598
-80.944958	-10.838177	1.671603
-81.158635	-3.544105	1.676608
-81.084414	-7.706155	1.681613
-80.942122	-12.138221	1.686618
-81.401152	0.635536	1.691622
-82.067368	1.897383	1.696627
-82.193563	8.583073	1.701632
-82.156458	-2.182075	1.706637
-82.754121	-7.954212	1.711642
-83.526286	-10.630435	1.716646
-83.759395	-7.034811	1.721651
-84.075437	-6.979057	1.726656
-84.086742	-4.123462	1.731661
-83.939482	-8.391793	1.736666
-84.251124	-11.329539	1.741670
-84.031866	-2.657085	1.746675
-84.614169	-6.675786	1.751680
-85.085124	-7.440607	1.756685
-85.715707	-9.056905	1.761690
-85.927470	-3.430376	1.766694
-85.614880	-4.709488	1.771699
-86.026455	-3.196233	1.776704
-86.227963	-6.685784	1.781709
-86.382567	-8.961469	1.786714
-87.071271	-3.535917	1.791718
-86.998205	-4.315842	1.796723
-87.241273	-4.012029	1.801728
-87.256366	-3.898732	1.806733
-87.994305	-11.787656	1.811738
-88.377930	3.059209	1.816742
-88.504831	-6.892649	1.821747
-88.734943	-1.968757	1.826752
-88.733088	3.374585	1.831757
-88.642850	-3.804922	1.836762
-88.844962	5.312781	1.841766
-89.507447	-1.268651	1.846771
-90.119893	-0.647907	1.851776
-89.787836	5.776611	1.856781
-90.273028	9.003376	1.861786
-91.247163	10.256221	1.866790
-91.433549	0.180748	1.871795
-91.342940	7.949449	1.876800
-91.419285	3.086364	1.881805
-91.197544	-1.819969	1.886810
-91.269061	2.794502	1.891814
-91.403405	-3.018139	1.896819
-92.484805	1.671317	1.901824
-92.880089	-1.851338	1.906829
-92.833185	-1.475619	1.911834
-93.221960	-1.892579	1.916838
-93.316153	-5.022364	1.921843
-94.193169	-0.203386	1.926848
-94.496853	-3.117062	1.931853
-94.313476	-12.563588	1.936858
-94.473520	4.437713	1.941862
-94.669514	-12.640587	1.946867
-94.476165	-10.645735	1.951872
-94.638634	-7.067438	1.956877
-94.875959	-8.124890	1.961882
-95.700290	2.478534	1.966886
-96.131489	-6.160482	1.971891
-96.207369	-4.854514	1.976896
-95.999581	-2.074160	1.981901
-96.556791	5.273403	1.986906
-97.381064	8.252416	1.991910
-97.780029	-2.508106	1.996915
-97.671401	-0.791466	2.006912
-96.617827	-1.091282	2.016909
-96.316562	3.835546	2.026906
-96.275159	-3.601897	2.036902
-96.136009	-0.971756	2.046899
-95.210743	-4.226068	2.056896
-94.600323	-5.657444	2.066893
-93.720019	-4.644193	2.076890
-93.551913	-3.957196	2.086886
-93.679180	0.060701	2.096883
-92.728023	2.947705	2.106880
-92.210373	0.450586	2.116877
-91.446056	-5.468047	2.126874
-90.884838	-0.816106	2.136870
-90.861913	-2.935263	2.146867
-90.079890	-5.080749	2.156864
-89.282436	-6.439879	2.166861
-89.484856	-2.365934	2.176858
-88.836438	-3.990120	2.186854
-88.128498	-4.755623	2.196851
-87.617961	-4.628775	2.206848
-86.865002	-0.066874	2.216845
-86.260389	-7.484306	2.226842
-86.451774	-5.683323	2.236838
-85.939392	-2.994089	2.246835
-85.289983	-3.563584	2.256832
-84.624077	-4.617139	2.266829
-84.024834	-4.941245	2.276826
-83.587504	-7.767969	2.286822
-82.846833	-1.848378	2.296819
-82.696726	0.412604	2.306816
-82.358204	-6.491410	2.316813
-81.366488	3.212514	2.326810
-80.934562	-7.953935	2.336806
-80.855488	-6.128540	2.346803
-80.207693	-4.512068	2.356800
-79.649636	-4.452805	2.366797
-79.345345	-4.879869	2.376794
-78.258838	-3.258848	2.386790
-78.264421	-6.697667	2.396787
-77.528781	3.511782	2.406784
-76.655333	-4.859808	2.416781
-76.781909	3.782831	2.426778
-76.152796	7.271159	2.436774
-75.285841	5.223318	2.446771
-75.139708	6.401564	2.456768
-75.040276	0.881048	2.466765
-74.205887	-1.250417	2.476762
-73.616236	-9.235706	2.486758
-72.944149	-4.277921	2.496755
-72.179977	-3.731246	2.506752
-72.084694	-2.456388	2.516749
-71.820513	-1.217330	2.526746
-71.111425	-7.817923	2.536742
-70.556664	-7.574419	2.546739
-70.071532	-1.108206	2.556736
-69.486512	0.837979	2.566733
-69.332870	-1.368054	2.576730
-68.350837	-3.383128	2.586726
-67.955695	-8.091235	2.596723
-67.911547	-6.798912	2.606720
-66.934201	-2.655239	2.616717
-66.423141	-2.819901	2.626714
-66.448808	-11.944789	2.636710
-65.381839	-10.504452	2.646707
-64.900245	-4.902472	2.656704
-64.884722	-5.129358	2.666701
-64.200910	-3.971475	2.676698
-63.467731	-6.172709	2.686694
-62.769274	-2.001451	2.696691
-62.345838	3.029897	2.706688
-62.125074	0.065834	2.716685
-61.728347	-3.698545	2.726682
-60.718749	-5.654557	2.736678
-60.611901	1.564284	2.746675
-60.394150	3.551815	2.756672
-59.368343	-0.883867	2.766669
-58.859344	-0.763114	2.776666
-58.680315	1.601067	2.786662
-58.039007	0.187056	2.796659
-58.027555	-0.938824	2.806656
-56.624291	7.668357	2.816653
-55.978189	0.985704	2.826650
-56.136326	2.756170	2.836646
-55.968229	3.737766	2.846643
-55.009769	0.345242	2.856640
-54.884803	2.334549	2.866637
-53.624857	6.117454	2.876634
-53.027613	-3.801322	2.886630
-52.931722	4.885874	2.896627
-53.046491	2.373185	2.906624
-52.055871	5.304730	2.916621
-51.543213	2.665841	2.926618
-50.907289	0.010928	2.936614
-50.083480	-2.074542	2.946611
-49.769361	-3.770218	2.956608
-49.707917	1.906685	2.966605
-49.437125	-1.188707	2.976602
-48.644474	-1.013920	2.986598
-48.239948	-5.251501	2.996595
-47.229632	-5.063088	3.006592
-46.758846	-0.149982	3.016589
-46.822242	-5.949245	3.026586
-45.854925	-7.591405	3.036582
-45.771624	-6.656793	3.046579
-44.736757	-6.887172	3.056576
-44.024598	2.305935	3.066573
-43.854504	-6.070182	3.076570
-43.572299	-2.049517	3.086566
-43.273579	-1.344842	3.096563
-42.636980	3.314373	3.106560
-42.402708	-2.078256	3.116557
-41.292636	-8.215443	3.126554
-40.994950	-3.715697	3.136550
-40.433158	3.948648	3.146547
-39.809015	2.534142	3.156544
-39.361490	-3.911691	3.166541
-39.315243	-4.437957	3.176538
-38.710071	-2.783170	3.186534
-38.058011	-6.840720	3.196531
-37.377104	-3.347785	3.206528
-36.584816	-0.198464	3.216525
-36.536910	-2.318345	3.226522
-36.293075	-4.646122	3.236518
-35.377666	2.678072	3.246515
-34.903396	2.617338	3.256512
-34.412517	-5.897422	3.266509
-33.527379	2.774592	3.276506
-33.430545	1.413679	3.286502
-33.458304	-2.892809	3.296499
-32.451057	-8.475476	3.306496
-31.830239	-4.697595	3.316493
-31.633759	-5.535513	3.326490
-30.820675	-8.835711	3.336486
-30.649639	-3.356431	3.346483
-30.125873	-3.770151	3.356480
-29.188977	-5.344221	3.366477
-29.235526	0.153099	3.376474
-28.275182	-5.675683	3.386470
-28.137459	-5.050476	3.396467
-27.647067	1.437096	3.406464
-26.812460	-3.535835	3.416461
-26.405812	-2.670573	3.426458
-25.981184	-3.743579	3.436454
-25.217709	-2.522073	3.446451
-24.545311	-4.748688	3.456448
-24.707370	1.799290	3.466445
-24.188164	-1.737079	3.476442
-23.290884	0.182664	3.486438
-22.807737	1.374960	3.496435
-22.748684	-2.577591	3.506432
-21.898283	-9.811554	3.516429
-21.538868	-1.022842	3.526426
-20.591135	2.295508	3.536422
-20.036392	0.486342	3.546419
-19.896120	1.408916	3.556416
-19.837375	-0.633459	3.566413
-19.204779	-5.045931	3.576410
-18.762876	-0.587643	3.586406
-17.835869	-1.656508	3.596403
-17.550044	4.888258	3.606400
-17.013761	-2.619906	3.616397
-16.055183	-4.368408	3.626394
-15.876748	0.983014	3.636390
-15.715245	5.529308	3.646387
-15.126166	-2.262667	3.656384
-14.624979	4.232729	3.666381
-13.144748	8.313950	3.676378
-13.340801	-1.148706	3.686374
-13.292142	4.279942	3.696371
-12.624076	3.260896	3.706368
-11.765181	-2.143458	3.716365
-11.473862	-4.415274	3.726362
-11.012080	8.123908	3.736358
-10.600358	4.287502	3.746355
-9.996962	6.652135	3.756352
-8.889096	5.501259	3.766349
-8.512040	3.605721	3.776346
-8.398802	9.081334	3.786342
-8.520578	9.762784	3.796339
-7.562964	10.884375	3.806336
-6.868908	7.881465	3.816333
-6.143805	10.623112	3.826330
-5.900041	7.002919	3.836326
-5.481313	7.049032	3.846323
-5.132511	13.865924	3.856320
-4.732998	15.521058	3.866317
-4.042157	21.983765	3.876314
-3.422020	24.501012	3.886310
-2.924990	26.448232	3.896307
-2.690236	37.625823	3.906304
-2.215283	44.106313	3.916301
-1.770172	50.623130	3.926298
-1.571136	58.296466	3.936294
-1.016895	84.946166	3.946291
-0.624093	104.347942	3.956288
0.000000	112.465818	3.961293
0.199582	120.246082	3.966298
0.628549	119.622705	3.971302
1.114759	132.268376	3.976307
0.632929	126.822994	3.981312
0.986512	124.265692	3.986317
1.253531	128.583887	3.991322
1.050459	123.098268	3.996326
0.467375	114.979529	4.001331
0.576680	130.822249	4.006336
1.312216	128.091584	4.011341
1.005053	139.155562	4.016346
0.836340	129.472715	4.021350
0.935608	133.560772	4.026355
1.013248	136.383560	4.031360
1.220625	129.005427	4.036365
0.936187	137.848127	4.041370
1.150605	127.570966	4.046374
0.761968	122.639411	4.051379
1.216711	129.826307	4.056384
1.292613	126.018294	4.061389
0.763545	126.436238	4.066394
0.925933	127.091365	4.071398
1.174260	133.092385	4.076403
1.223736	135.248858	4.081408
1.139038	119.488161	4.086413
0.897577	130.987983	4.091418
1.142617	130.655828	4.096422
1.340849	141.568355	4.101427
1.117329	140.413831	4.106432
1.200184	138.613671	4.111437
1.297963	148.905942	4.116442
1.116057	125.390371	4.121446
0.870556	129.269521	4.126451
1.256438	137.606067	4.131456
1.596265	132.668654	4.136461
1.426002	144.151071	4.141466
1.211552	124.212367	4.146470
1.264220	129.446602	4.151475
0.865110	124.383802	4.156480
1.586511	133.579246	4.161485
1.171970	132.492428	4.166490
1.212789	132.606512	4.171494
1.386914	134.737251	4.176499
1.501741	143.625354	4.181504
1.620710	135.625083	4.186509
1.406086	139.047021	4.191514
1.513240	135.534689	4.196518
1.213996	127.748229	4.201523
1.350434	127.179889	4.206528
1.535671	131.175468	4.211533
1.228348	135.244574	4.216538
1.780945	132.767013	4.221542
1.461394	130.320843	4.226547
1.180593	115.542950	4.231552
1.600979	132.732418	4.236557
1.203262	129.611899	4.241562
1.576651	134.116010	4.246566
1.567846	132.178264	4.251571
1.792149	126.006022	4.256576
1.490645	134.351516	4.261581
1.424721	137.177676	4.266586
1.677222	135.689616	4.271590
1.671270	136.649357	4.276595
1.228736	136.272399	4.281600
1.605151	134.939048	4.286605
1.575280	138.999757	4.291610
1.587850	142.917821	4.296614
1.589366	141.199925	4.301619
1.732717	144.873006	4.306624
1.628374	138.720292	4.311629
1.672936	143.607788	4.316634
1.599770	130.376232	4.321638
1.978646	141.330234	4.326643
1.880766	141.178018	4.331648
2.079448	138.287335	4.336653
1.807311	137.580133	4.341658
1.612263	144.219651	4.346662
1.691984	135.782575	4.351667
1.523537	138.042580	4.356672
1.748767	130.016276	4.361677
1.609343	144.344367	4.366682
1.939494	137.465959	4.371686
2.038097	137.507772	4.376691
1.855063	146.571964	4.381696
2.062268	140.614346	4.386701
1.905178	140.161308	4.391706
1.920691	140.557736	4.396710
2.128551	147.485693	4.401715
2.038609	147.803630	4.406720
2.005803	140.314194	4.411725
1.671066	143.504903	4.416730
1.737339	141.533322	4.421734
1.897027	137.051051	4.426739
1.849835	137.685027	4.431744
2.234633	137.868938	4.436749
1.677546	138.832234	4.441754
2.003094	153.635256	4.446758
2.032217	150.470421	4.451763
1.723332	155.295895	4.456768
2.099196	149.906787	4.461773
1.743735	146.798668	4.466778
2.065342	145.609888	4.471782
2.033453	140.369688	4.476787
1.904441	139.466200	4.481792
1.888159	141.297562	4.486797
1.695626	153.444662	4.491802
1.771128	144.628597	4.496806
1.685077	164.478512	4.501811
2.226878	164.024223	4.506816
2.476680	158.259280	4.511821
2.568813	168.660007	4.516826
2.332207	159.478085	4.521830
2.431571	154.771090	4.526835
1.981343	146.337428	4.531840
2.194693	151.318867	4.536845
2.314533	162.654891	4.541850
2.365399	154.934128	4.546854
2.274005	147.403192	4.551859
2.282399	156.447076	4.556864
2.333763	147.299416	4.561869
1.770035	161.329761	4.566874
2.180124	161.259804	4.571878
2.417810	161.444474	4.576883
2.407410	171.943423	4.581888
2.884900	158.594473	4.586893
2.407790	158.754397	4.591898
2.317705	155.703032	4.596902
2.426552	157.195382	4.601907
2.278867	165.890256	4.606912
2.554882	160.393307	4.611917
2.520829	168.086585	4.616922
2.388401	153.579781	4.621926
2.817187	168.167429	4.626931
2.053076	162.914679	4.631936
2.486824	161.341452	4.636941
2.401986	164.569184	4.641946
2.520543	163.848607	4.646950
2.667194	162.642775	4.651955
2.339452	173.994710	4.656960
2.438797	167.392666	4.661965
2.406630	173.677812	4.666970
2.283489	176.300919	4.671974
2.290218	167.596788	4.676979
2.134362	174.783860	4.681984
2.657752	167.062286	4.686989
2.526076	176.646833	4.691994
2.889856	171.338692	4.696998
2.747561	174.198893	4.702003
2.330076	178.351599	4.707008
2.602893	172.583067	4.712013
2.920170	174.463736	4.717018
2.726303	175.512848	4.722022
2.593001	172.648539	4.727027
2.794358	177.742581	4.732032
2.789608	174.146428	4.737037
2.850877	169.062554	4.742042
2.922050	167.400248	4.747046
2.769325	173.055608	4.752051
2.750812	172.036839	4.757056
2.686591	171.025187	4.762061
2.755851	172.972945	4.767066
3.072930	178.476068	4.772070
2.887756	177.195352	4.777075
2.857948	176.181504	4.782080
3.003132	171.673011	4.787085
2.667481	178.195231	4.792090
2.829656	177.129347	4.797094
2.733803	166.255080	4.802099
2.542544	177.357982	4.807104
2.748815	164.668175	4.812109
2.732711	178.401303	4.817114
3.218165	187.408889	4.822118
3.053499	177.586183	4.827123
2.809693	180.221751	4.832128
3.196663	170.474509	4.837133
2.758437	178.037734	4.842138
3.182486	173.495312	4.847142
3.067791	178.151356	4.852147
2.753116	177.564668	4.857152
3.299132	175.135581	4.862157
3.367603	180.168059	4.867162
2.673240	175.002521	4.872166
3.072418	167.936187	4.877171
3.012251	180.325282	4.882176
3.434645	183.610083	4.887181
3.183162	187.404757	4.892186
3.167068	171.652314	4.897190
3.248124	164.420381	4.902195
3.025047	167.751894	4.907200
3.053772	169.471850	4.912205
3.345378	178.604524	4.917210
3.229460	179.900922	4.922214
3.265305	172.112889	4.927219
2.663871	179.603451	4.932224
3.421818	183.253614	4.937229
3.237233	191.976392	4.942234
3.623762	184.617798	4.947238
3.781121	178.775493	4.952243
3.232152	178.978242	4.957248
3.291981	173.119488	4.962253
2.952441	172.147538	4.967258
2.957679	173.738276	4.972262
3.607899	179.271786	4.977267
3.419581	192.234489	4.982272
3.738076	183.295151	4.987277
3.389100	179.901284	4.992282
2.966407	179.195376	4.997286
3.534209	176.212416	5.002291
3.341631	192.317324	5.007296
3.560719	185.396079	5.012301
3.592433	187.590125	5.017306
3.295513	173.643579	5.022310
3.467487	177.068606	5.027315
3.220386	182.207164	5.032320
3.477851	177.893154	5.037325
3.529978	186.148812	5.042330
3.670188	195.029826	5.047334
3.807088	186.014359	5.052339
3.574906	186.477827	5.057344
3.396019	173.696124	5.062349
3.133616	184.705706	5.067354
3.430357	190.667571	5.072358
3.714339	190.101566	5.077363
3.441219	196.734277	5.082368
3.642002	184.481900	5.087373
3.695873	187.526692	5.092378
3.620257	195.109396	5.097382
3.698178	187.264186	5.102387
3.321478	200.604230	5.107392
3.645979	184.169173	5.112397
3.839437	191.728963	5.117402
3.454908	195.993598	5.122406
3.624431	191.414872	5.127411
3.463229	199.184906	5.132416
3.514886	189.882158	5.137421
3.667320	190.231960	5.142426
3.620413	193.520229	5.147430
3.674819	190.550764	5.152435
3.225376	201.187688	5.157440
3.657575	204.221035	5.162445
3.793888	207.132774	5.167450
3.955482	213.036596	5.172454
4.087537	199.516776	5.177459
4.029795	202.322690	5.182464
4.190371	194.777813	5.187469
3.977636	192.694645	5.192474
3.981738	186.664233	5.197478
3.924087	186.708229	5.202483
3.545629	191.088974	5.207488
3.903057	187.948945	5.212493
3.887530	192.570569	5.217498
3.687430	194.683652	5.222502
4.163102	194.869234	5.227507
3.775355	209.868780	5.232512
4.160245	210.305773	5.237517
4.081555	204.680543	5.242522
3.601766	200.731247	5.247526
4.138179	202.027318	5.252531
3.897172	211.752290	5.257536
4.208602	210.922589	5.262541
4.045369	207.265684	5.267546
4.044102	213.909858	5.272550
3.965405	219.480942	5.277555
4.244676	220.165330	5.282560
3.673349	210.023114	5.287565
3.887288	209.528125	5.292570
4.085895	208.080087	5.297574
3.689711	213.716420	5.302579
4.063757	231.539611	5.307584
4.008443	222.607836	5.312589
4.019079	222.650691	5.317594
4.059874	213.779885	5.322598
3.891741	204.438585	5.327603
3.992423	220.327019	5.332608
4.096776	231.668662	5.337613
4.175863	241.277375	5.342618
4.253051	241.135865	5.347622
4.555914	228.835926	5.352627
4.336020	241.714997	5.357632
4.223637	237.876165	5.362637
4.060099	246.658967	5.367642
4.122760	246.535537	5.372646
4.766947	243.493218	5.377651
4.595712	247.237446	5.382656
4.341972	237.691162	5.387661
4.644999	238.612293	5.392666
4.712185	235.890762	5.397670
4.573454	218.933021	5.402675
4.235408	220.346262	5.407680
4.180361	205.931770	5.412685
4.521957	225.208978	5.417690
4.375256	226.342496	5.422694
4.768177	226.205610	5.427699
4.206341	225.040482	5.432704
4.330087	225.340968	5.437709
4.800118	240.466409	5.442714
4.652913	234.434229	5.447718
4.375128	217.058386	5.452723
4.325703	229.037726	5.457728
4.235658	228.485664	5.462733
4.559147	231.928239	5.467738
4.290808	243.837271	5.472742
4.576845	237.013149	5.477747
4.504435	239.258213	5.482752
4.823993	240.670308	5.487757
4.919885	240.759999	5.492762
4.488954	237.597177	5.497766
4.546233	237.053813	5.502771
4.465643	238.667411	5.507776
4.718274	230.475447	5.512781
4.856415	240.701377	5.517786
4.623729	242.601244	5.522790
5.090112	237.710535	5.527795
4.828319	242.547683	5.532800
4.928550	237.185645	5.537805
5.051284	239.511056	5.542810
4.842272	234.712851	5.547814
4.848753	238.549627	5.552819
4.725741	243.921978	5.557824
4.902981	238.108196	5.562829
5.127828	237.738056	5.567834
4.301778	228.806058	5.572838
4.302296	239.407748	5.577843
4.474726	245.148545	5.582848
4.459095	232.986776	5.587853
4.786281	233.983238	5.592858
4.557040	239.103213	5.597862
4.836319	227.512452	5.602867
4.697084	233.501083	5.607872
4.870475	234.524654	5.612877
5.447111	234.530004	5.617882
5.161256	248.346313	5.622886
4.982656	233.697939	5.627891
4.814248	240.390292	5.632896
4.991684	237.196023	5.637901
5.198723	236.306645	5.642906
4.761458	235.704241	5.647910
5.153859	235.102372	5.652915
4.835787	239.366161	5.657920
4.933165	236.054645	5.662925
4.768801	239.604816	5.667930
5.001224	246.019631	5.672934
4.941866	247.971604	5.677939
5.133163	252.111797	5.682944
5.479633	264.225671	5.687949
5.118225	248.697765	5.692954
4.498796	245.067589	5.697958
5.066007	249.294782	5.702963
5.433805	262.844819	5.707968
5.020492	259.717214	5.712973
5.347068	258.707984	5.717978
5.177276	266.662880	5.722982
5.639248	254.249568	5.727987
5.422425	262.705321	5.732992
5.065428	251.903298	5.737997
5.306228	257.051333	5.743002
5.252031	263.950535	5.748006
5.556235	256.282031	5.753011
4.924741	261.293802	5.758016
5.142274	255.979933	5.763021
5.183469	259.858765	5.768026
5.009358	262.901102	5.773030
5.327882	258.210576	5.778035
5.471133	267.679601	5.783040
5.515937	263.696069	5.788045
5.477374	264.278087	5.793050
5.449358	260.324876	5.798054
5.429087	261.315327	5.803059
5.213275	255.705103	5.808064
5.467545	253.916206	5.813069
5.353871	257.604018	5.818074
4.982934	265.435209	5.823078
5.422468	267.353801	5.828083
5.142022	260.889947	5.833088
5.100340	265.987055	5.838093
5.336925	261.283976	5.843098
5.078182	272.065255	5.848102
5.547325	278.000307	5.853107
5.674536	293.957442	5.858112
5.709820	281.699128	5.863117
5.727958	269.535240	5.868122
5.318043	267.137920	5.873126
5.738619	271.916289	5.878131
5.641631	288.689761	5.883136
5.825740	276.022307	5.888141
5.738454	259.625984	5.893146
5.377499	270.075169	5.898150
5.466154	264.635833	5.903155
5.577468	266.573890	5.908160
5.864890	278.706459	5.913165
6.117447	276.902008	5.918170
5.443266	280.392361	5.923174
5.661521	269.548218	5.928179
5.505515	277.459843	5.933184
6.077976	283.454739	5.938189
5.895181	264.289221	5.943194
5.946318	266.565672	5.948198
5.731583	263.103433	5.953203
5.494387	262.621736	5.958208
5.739328	263.358926	5.963213
6.061485	275.922676	5.968218
5.750834	274.161623	5.973222
5.848518	260.343393	5.978227
5.497249	264.754723	5.983232
5.770583	276.671189	5.988237
5.965138	279.890242	5.993242
5.815247	285.681237	5.998246
5.978423	272.077424	6.003251
5.845854	276.132008	6.008256
5.805292	269.311268	6.013261
5.690539	262.467281	6.018266
5.658384	264.642807	6.023270
5.814815	269.905220	6.028275
5.677947	275.675201	6.033280
5.765505	279.958100	6.038285
6.221918	284.041204	6.043290
5.568626	276.509116	6.048294
5.717619	274.065903	6.053299
5.801623	284.167412	6.058304
5.766120	284.650879	6.063309
6.022299	290.657057	6.068314
6.012672	290.361387	6.073318
5.688695	273.957611	6.078323
5.440500	275.470760	6.083328
5.641329	279.691731	6.088333
6.063397	278.477811	6.093338
5.993391	290.324358	6.098342
5.960947	283.828210	6.103347
5.751161	278.425845	6.108352
5.367575	270.041858	6.113357
5.785266	281.021540	6.118362
5.847916	298.342797	6.123366
5.639247	287.049429	6.128371
5.873119	287.772525	6.133376
5.769503	281.882237	6.138381
5.922736	293.327038	6.143386
5.760764	298.117022	6.148390
5.769277	293.158384	6.153395
5.902059	300.338531	6.158400
5.953452	289.627922	6.163405
6.231774	278.881987	6.168410
5.611947	277.115289	6.173414
5.625649	264.575614	6.178419
5.954201	277.897658	6.183424
5.839377	274.853289	6.188429
5.855768	263.815955	6.193434
5.330115	268.567644	6.198438
5.700108	278.801789	6.203443
6.005162	286.641633	6.208448
6.119871	284.801698	6.213453
5.801952	272.841988	6.218458
5.845874	271.911567	6.223462
5.856049	259.113022	6.228467
5.538395	264.474556	6.233472
6.187239	276.645762	6.238477
5.510017	270.303792	6.243482
5.683956	269.372110	6.248486
5.825565	281.479928	6.253491
5.989901	294.808571	6.258496
5.824947	281.686104	6.263501
5.671912	277.205033	6.268506
5.782819	282.107548	6.273510
6.240903	278.116613	6.278515
5.800940	275.806227	6.283520
5.796643	266.572261	6.288525
5.840558	268.024111	6.293530
5.683137	268.226008	6.298534
5.718205	265.433544	6.303539
5.727093	267.681773	6.308544
5.679886	281.894379	6.313549
5.665740	270.849141	6.318554
6.116189	286.430081	6.323558
6.164232	286.938504	6.328563
5.750832	284.842277	6.333568
5.582397	276.747487	6.338573
5.821143	275.679166	6.343578
5.671610	277.528126	6.348582
5.828639	274.498376	6.353587
5.662580	277.137671	6.358592
5.920304	278.334773	6.363597
6.033271	266.428201	6.368602
5.892094	268.984528	6.373606
5.956659	274.732637	6.378611
5.921228	281.309390	6.383616
5.643541	270.615228	6.388621
5.831488	273.930221	6.393626
5.681159	275.864724	6.398630
5.651864	264.363112	6.403635
5.932250	276.155094	6.408640
5.767274	271.897343	6.413645
6.229936	269.073105	6.418650
5.657081	271.010119	6.423654
5.821356	265.963963	6.428659
5.995195	265.877006	6.433664
5.925326	265.837485	6.438669
5.918994	270.780396	6.443674
5.550212	267.633201	6.448678
5.845358	277.005816	6.453683
5.631275	270.303840	6.458688
5.650852	269.241170	6.463693
5.538659	257.923309	6.468698
5.629935	264.448691	6.473702
5.679405	261.888100	6.478707
5.773360	269.722839	6.483712
5.861988	278.963097	6.488717
5.920509	266.688521	6.493722
5.779541	275.496297	6.498726
6.093171	272.204887	6.503731
5.931520	273.340736	6.508736
5.750004	275.922327	6.513741
6.065451	267.707910	6.518746
5.713772	273.799233	6.523750
6.183361	266.155594	6.528755
5.709567	274.081896	6.533760
5.606024	272.563840	6.538765
5.943392	268.253186	6.543770
5.786212	272.061669	6.548774
5.763097	270.135627	6.553779
6.112916	268.240105	6.558784
5.584955	275.456681	6.563789
5.988107	265.830252	6.568794
5.953668	269.132413	6.573798
5.942194	261.560512	6.578803
6.017303	273.106048	6.583808
5.939486	271.539695	6.588813
5.907145	263.762238	6.593818
5.758849	265.933701	6.598822
5.673695	259.037651	6.603827
5.985853	265.572935	6.608832
5.878342	264.678747	6.613837
6.202656	266.260943	6.618842
5.640651	268.436709	6.623846
6.017450	266.995723	6.628851
6.092457	270.141641	6.633856
5.612025	251.123716	6.638861
5.896620	256.650904	6.643866
5.474999	271.427989	6.648870
5.745770	265.672400	6.653875
5.391891	267.347534	6.658880
4.867325	274.873623	6.663885
5.368057	267.743983	6.668890
5.743589	271.415741	6.673894
5.747302	263.151787	6.678899
5.737381	269.898568	6.683904
5.774255	276.182492	6.688909
5.658746	271.496266	6.693914
5.639186	276.441238	6.698918
6.129870	281.022035	6.703923
5.852593	279.401316	6.708928
5.686506	276.504130	6.713933
5.485644	269.385650	6.718938
6.197277	293.844415	6.723942
6.416053	281.959323	6.728947
6.205087	278.268707	6.733952
6.027757	282.371390	6.738957
5.914598	267.823529	6.743962
5.883753	275.551154	6.748966
5.902339	270.018323	6.753971
5.694322	271.401832	6.758976
5.601576	274.959841	6.763981
5.679977	270.885657	6.768986
5.830342	274.946808	6.773990
5.629868	273.073690	6.778995
6.244436	272.927604	6.784000
6.025051	274.031313	6.789005
6.000104	272.545312	6.794010
5.864009	281.285894	6.799014
5.687786	270.699319	6.804019
6.231314	275.195957	6.809024
5.660808	278.243067	6.814029
5.793751	265.529805	6.819034
5.569499	274.217671	6.824038
5.247983	273.970561	6.829043
5.428480	269.817207	6.834048
5.442702	276.667797	6.839053
5.647277	267.803101	6.844058
5.827204	281.781029	6.849062
5.532940	281.444256	6.854067
5.862676	272.610690	6.859072
5.577825	278.182253	6.864077
5.650590	272.261342	6.869082
5.608762	285.179158	6.874086
5.876961	282.847096	6.879091
6.373564	286.560117	6.884096
5.934538	289.472864	6.889101
6.245493	274.112329	6.894106
5.994281	282.089400	6.899110
5.944025	267.987318	6.904115
5.940561	273.217681	6.909120
5.689835	266.027873	6.914125
6.046357	263.416311	6.919130
5.695327	270.361731	6.924134
5.665823	272.609611	6.929139
5.878836	265.581715	6.934144
5.460094	272.667391	6.939149
5.810570	270.531325	6.944154
5.585889	274.486356	6.949158
5.575128	274.738184	6.954163
5.734542	273.606286	6.959168
5.563137	275.968008	6.964173
5.862992	279.578784	6.969178
5.494185	272.824968	6.974182
5.980096	275.552575	6.979187
5.867188	268.888630	6.984192
5.597647	275.027275	6.989197
5.607241	271.992007	6.994202
6.085243	286.882133	6.999206
5.959671	285.114409	7.004211
6.025039	271.190473	7.009216
5.846397	283.079239	7.014221
6.210516	272.585701	7.019226
5.835245	275.532811	7.024230
5.631019	271.913912	7.029235
5.916702	271.391933	7.034240
5.780747	276.411974	7.039245
6.008914	278.005977	7.044250
5.739514	282.353945	7.049254
5.847678	272.741804	7.054259
5.773849	278.040070	7.059264
5.485495	277.066472	7.064269
5.991079	265.396160	7.069274
5.715931	280.596530	7.074278
5.972973	268.531485	7.079283
5.936227	287.630390	7.084288
5.500842	284.126573	7.089293
5.876830	274.197489	7.094298
5.586692	276.792829	7.099302
5.742783	270.906400	7.104307
6.273204	277.743057	7.109312
5.871823	274.623083	7.114317
5.997273	280.336405	7.119322
6.003099	278.602006	7.124326
5.741774	276.694070	7.129331
5.994773	272.716086	7.134336
5.729684	273.820584	7.139341
6.004895	276.176042	7.144346
5.755917	273.449948	7.149350
5.848980	268.873616	7.154355
5.820543	279.957559	7.159360
5.515391	273.437437	7.164365
5.900515	274.057890	7.169370
5.567531	280.399401	7.174374
5.682986	276.420685	7.179379
6.017915	276.773711	7.184384
5.977025	274.265151	7.189389
6.278516	264.711498	7.194394
5.804964	274.305034	7.199398
5.744810	273.330707	7.204403
5.985403	281.689942	7.209408
5.572918	283.143251	7.214413
5.928024	271.316033	7.219418
5.496836	280.064595	7.224422
5.806012	270.411667	7.229427
5.717503	268.075035	7.234432
5.882589	275.171050	7.239437
5.464635	275.302781	7.244442
5.611481	273.280676	7.249446
5.931451	274.730673	7.254451
6.073556	275.094739	7.259456
5.900792	277.162448	7.264461
6.392249	278.263047	7.269466
6.030597	276.554227	7.274470
6.107625	272.002537	7.279475
5.789765	253.686949	7.284480
5.359404	252.608914	7.289485
5.746679	260.325216	7.294490
5.749152	274.545900	7.299494
6.033010	270.145502	7.304499
6.070790	269.026215	7.309504
5.846251	260.222007	7.314509
5.647456	248.753123	7.319514
5.564394	252.945524	7.324518
5.898190	268.253549	7.329523
5.904549	265.022637	7.334528
5.636871	257.971511	7.339533
5.954988	261.190305	7.344538
5.764898	257.907725	7.349542
5.613078	259.598853	7.354547
5.751374	266.072623	7.359552
5.540641	272.458371	7.364557
5.709567	268.003103	7.369562
5.849077	275.492236	7.374566
5.746658	278.608833	7.379571
5.882915	275.610791	7.384576
5.594974	265.424422	7.389581
5.928218	269.147055	7.394586
5.629159	269.152709	7.399590
6.049875	269.780275	7.404595
6.148835	272.982574	7.409600
5.697414	271.651557	7.414605
6.101935	266.169369	7.419610
5.913483	265.632627	7.424614
5.600475	269.016125	7.429619
5.703461	260.939193	7.434624
5.895470	271.400359	7.439629
5.958854	273.273114	7.444634
5.594449	255.350744	7.449638
5.858243	264.193568	7.454643
5.777745	263.687473	7.459648
5.548170	273.129129	7.464653
5.672671	270.844752	7.469658
5.828051	276.275006	7.474662
5.246199	269.541707	7.479667
5.706896	255.803000	7.484672
5.712319	264.122913	7.489677
5.561972	263.728932	7.494682
5.589200	265.645280	7.499686
5.491587	265.388619	7.504691
5.509078	266.563013	7.509696
5.568335	265.933920	7.514701
5.896145	263.962733	7.519706
5.515243	271.077317	7.524710
5.889933	276.862562	7.529715
6.216819	275.666625	7.534720
5.762062	269.609552	7.539725
6.027156	264.237657	7.544730
5.859334	265.241590	7.549734
6.032045	265.044079	7.554739
5.984135	261.521065	7.559744
5.853088	269.843246	7.564749
5.995249	265.363673	7.569754
5.788528	268.670511	7.574758
5.650461	267.591258	7.579763
5.732804	264.022654	7.584768
6.004906	273.455802	7.589773
5.933376	265.551571	7.594778
5.719837	274.108057	7.599782
5.758275	273.393622	7.604787
6.309776	264.525532	7.609792
5.791066	276.682372	7.614797
5.966118	265.781684	7.619802
6.000262	274.729871	7.624806
5.713256	275.148094	7.629811
6.258232	270.080627	7.634816
5.943767	277.238653	7.639821
5.798094	266.634669	7.644826
5.591638	270.488787	7.649830
5.588354	276.003856	7.654835
5.753845	268.094357	7.659840
5.862020	276.955089	7.664845
6.004131	265.907672	7.669850
5.805610	276.258805	7.674854
5.860667	267.471172	7.679859
5.650842	267.738174	7.684864
5.592124	270.560069	7.689869
5.928007	265.347991	7.694874
6.056611	268.839899	7.699878
5.817545	276.185498	7.704883
6.003179	270.360907	7.709888
5.630235	271.665693	7.714893
5.994991	275.383421	7.719898
5.681294	270.680597	7.724902
5.651637	274.526172	7.729907
6.142376	266.736873	7.734912
5.518500	271.567129	7.739917
5.928585	277.754982	7.744922
5.907684	280.865214	7.749926
5.784273	269.185267	7.754931
5.695666	269.411250	7.759936
5.688300	276.208254	7.764941
5.717224	278.605223	7.769946
5.927789	279.268674	7.774950
5.880331	277.422350	7.779955
6.217488	267.511971	7.784960
5.712064	266.648100	7.789965
5.641452	253.039574	7.794970
5.595340	254.951521	7.799974
5.396936	259.263120	7.804979
6.073393	263.093664	7.809984
5.568549	271.825216	7.814989
5.821833	274.585879	7.819994
6.335191	277.049789	7.824998
5.988792	266.989578	7.830003
5.861597	257.499510	7.835008
5.451914	261.094208	7.840013
5.683368	264.500500	7.845018
5.705597	267.167424	7.850022
5.888012	278.104643	7.855027
6.332503	272.692158	7.860032
5.685416	263.077392	7.865037
5.812746	254.060217	7.870042
5.657742	256.096684	7.875046
5.831927	259.189194	7.880051
6.093319	258.857655	7.885056
5.610453	272.669856	7.890061
5.614967	249.900204	7.895066
5.959360	261.865706	7.900070
5.556672	256.844553	7.905075
6.138471	262.012261	7.910080
5.579230	264.469167	7.915085
5.736267	260.993336	7.920090
6.046766	272.780627	7.925094
5.801771	263.808763	7.930099
5.656092	263.543767	7.935104
5.646098	265.272924	7.940109
5.794342	276.370484	7.945114
6.101462	277.066357	7.950118
5.932209	256.842060	7.955123
5.981276	248.634326	7.960128
5.827752	259.522923	7.965146
5.899392	250.575242	7.970163
5.655192	255.031366	7.975181
5.616698	250.319912	7.980198
5.749565	253.644413	7.985216
5.626478	251.215028	7.990234
6.131344	253.891508	7.995251
5.644830	258.994397	8.000269
5.748806	257.886580	8.005286
6.018168	259.387965	8.010304
5.477050	269.437923	8.015322
5.861211	273.032555	8.020339
6.013231	279.241484	8.025357
5.722463	272.571785	8.030374
6.066475	276.661792	8.035392
6.226251	275.510574	8.040410
5.860920	266.293267	8.045427
5.804222	255.727791	8.050445
5.966857	260.227865	8.055462
5.923373	247.905805	8.060480
5.541207	260.774233	8.065498
6.329836	270.008118	8.070515
6.174583	258.110530	8.075533
5.850293	256.914767	8.080550
5.950759	257.464202	8.085568
5.564306	264.962417	8.090586
5.495059	259.971741	8.095603
6.127312	267.027340	8.100621
6.253636	273.353871	8.105638
6.053365	261.819877	8.110656
5.435528	262.692578	8.115674
5.932712	276.869385	8.120691
6.329529	275.965268	8.125709
6.073717	285.623694	8.130726
6.256586	267.248581	8.135744
5.931218	255.980207	8.140762
5.455852	264.101301	8.145779
5.924853	267.925706	8.150797
6.158256	272.051867	8.155814
6.419954	270.004358	8.160832
6.053315	265.545951	8.165850
5.793437	253.090332	8.170867
6.025179	255.604220	8.175885
6.001338	269.212083	8.180902
6.340204	262.570581	8.185920
5.920437	267.830329	8.190938
5.524421	258.627270	8.195955
6.163188	272.390732	8.200973
5.939609	271.860904	8.205990
5.838852	270.251660	8.211008
6.150903	280.768360	8.216026
6.313220	276.682005	8.221043
6.385668	269.766417	8.226061
6.194424	276.647295	8.231078
6.075890	265.968371	8.236096
6.158705	268.783145	8.241114
5.809165	274.322279	8.246131
5.930278	271.119607	8.251149
5.936310	276.685427	8.256166
6.334513	267.216703	8.261184
6.289064	282.850702	8.266202
5.882873	280.481169	8.271219
6.582532	281.445371	8.276237
5.952005	284.955004	8.281254
6.414548	277.240258	8.286272
6.137046	262.701501	8.291290
5.311089	267.058868	8.296307
6.004134	271.378537	8.301325
5.591259	272.938811	8.306342
5.945689	269.491541	8.311360
6.345229	280.947620	8.316378
5.724753	282.161541	8.321395
6.063657	285.097382	8.326413
6.204211	279.483932	8.331430
6.042697	271.099533	8.336448
6.157305	277.046058	8.341466
6.085859	272.806762	8.346483
6.096085	272.988417	8.351501
6.165101	279.800373	8.356518
5.954581	263.878485	8.361536
6.078552	282.206261	8.366554
6.389320	294.648106	8.371571
6.494085	295.610263	8.376589
6.107214	280.987538	8.381606
6.487402	279.230832	8.386624
6.373963	274.881316	8.391642
6.440961	277.578639	8.396659
6.533733	269.274563	8.401677
6.305337	277.947315	8.406694
5.911056	282.650863	8.411712
6.088596	279.653988	8.416730
5.984269	270.809429	8.421747
6.402943	285.831555	8.426765
6.596057	288.370396	8.431782
6.479013	277.716478	8.436800
6.408977	273.230823	8.441818
5.838663	276.453384	8.446835
6.372830	269.011497	8.451853
6.053301	278.888112	8.456870
6.412407	293.764893	8.461888
6.581674	292.296632	8.466906
5.971644	286.134204	8.471923
6.477756	284.389448	8.476941
6.524284	298.207271	8.481958
6.380828	288.245389	8.486976
6.359441	271.845945	8.491994
6.152944	283.273314	8.497011
6.608743	295.055141	8.502029
6.385782	282.991363	8.507046
6.606026	289.192829	8.512064
6.415138	279.916799	8.517082
6.292398	274.861868	8.522099
6.437077	269.793703	8.527117
6.062863	282.847091	8.532134
6.700324	280.561205	8.537152
6.482144	281.460039	8.542170
6.658765	282.445718	8.547187
6.339259	276.613580	8.552205
6.027189	280.581687	8.557223
6.209021	282.516402	8.562240
6.302907	294.294620	8.567258
6.466430	295.089846	8.572275
6.789289	305.232512	8.577293
6.738618	308.355238	8.582311
6.228097	286.812509	8.587328
6.310058	289.188785	8.592346
6.426151	299.890632	8.597363
6.925767	293.331382	8.602381
6.479894	287.301176	8.607399
6.159823	284.315508	8.612416
6.333130	286.996281	8.617434
6.509671	299.941841	8.622451
6.875878	294.826555	8.627469
6.637149	304.643270	8.632487
6.415263	289.568839	8.637504
6.331858	280.714707	8.642522
6.657578	302.296109	8.647539
6.725087	294.532413	8.652557
6.507102	277.879567	8.657575
6.316368	293.394192	8.662592
6.388392	301.057711	8.667610
6.721300	299.466146	8.672627
6.779980	300.564859	8.677645
6.221533	293.353036	8.682663
6.640801	296.030226	8.687680
6.546691	302.795011	8.692698
6.661179	301.044959	8.697715
6.899228	298.669787	8.702733
7.062877	292.349030	8.707751
6.621618	279.233703	8.712768
6.420272	280.574860	8.717786
6.417993	271.869039	8.722803
6.370383	290.109934	8.727821
6.382833	311.585496	8.732839
6.219650	298.171253	8.737856
6.733157	291.076538	8.742874
6.284423	303.425214	8.747891
6.742875	304.108252	8.752909
6.676213	305.961745	8.757927
6.690954	301.402926	8.762944
6.772812	296.906239	8.767962
6.694905	303.444450	8.772979
6.726809	306.393382	8.777997
6.515898	304.551990	8.783015
6.438016	300.313689	8.788032
6.948743	304.141072	8.793050
6.495057	305.584633	8.798067
6.542031	311.860420	8.803085
6.341341	312.317898	8.808103
6.515604	310.725788	8.813120
6.623854	304.505165	8.818138
6.777373	309.647266	8.823155
6.672497	311.983211	8.828173
6.744127	300.697176	8.833191
6.534609	306.583729	8.838208
6.692577	309.263737	8.843226
6.837655	323.350244	8.848243
7.190329	321.705110	8.853261
6.759502	307.890741	8.858279
6.791001	305.427813	8.863296
7.020468	292.327961	8.868314
6.386735	293.667016	8.873331
6.837564	298.011782	8.878349
6.724448	297.092389	8.883367
6.684151	290.194347	8.888384
7.073707	305.959443	8.893402
6.729395	310.693086	8.898419
7.145465	315.478746	8.903437
6.960320	309.947553	8.908455
6.642835	310.154986	8.913472
6.738810	299.736118	8.918490
6.407671	309.661893	8.923507
7.068579	312.399288	8.928525
7.061738	317.108791	8.933543
7.129644	314.128979	8.938560
6.710969	297.895504	8.943578
6.798547	308.131606	8.948595
6.950422	312.270470	8.953613
7.284933	299.324662	8.958631
6.445520	303.554752	8.963648
6.758882	307.804164	8.968666
6.731851	314.277656	8.973683
6.952457	321.043938	8.978701
7.241087	329.923379	8.983719
7.213525	323.941634	8.988736
7.040179	315.193002	8.993754
6.548703	308.977394	8.998771
7.074325	322.919449	9.003789
7.044194	321.646325	9.008807
7.000377	325.222400	9.013824
7.372887	318.443102	9.018842
7.044632	315.518659	9.023859
7.061494	309.507913	9.028877
6.806764	299.194140	9.033895
6.755555	303.607605	9.038912
6.882711	305.055400	9.043930
7.119485	318.531210	9.048947
7.194873	307.452858	9.053965
7.014591	300.989997	9.058983
6.682461	312.897669	9.064000
6.911833	322.082962	9.069018
7.140509	326.225650	9.074035
7.052864	327.138874	9.079053
7.225936	326.856541	9.084071
7.145137	332.312827	9.089088
6.785773	330.251561	9.094106
6.525048	319.702036	9.099123
6.728447	330.633293	9.104141
7.274236	328.055576	9.109159
6.788614	329.223259	9.114176
7.083100	334.113057	9.119194
6.969069	328.801147	9.124211
6.853866	326.263232	9.129229
6.995394	330.716120	9.134247
6.720397	330.689732	9.139264
6.923568	323.412961	9.144282
7.004656	332.255293	9.149299
7.205738	345.032972	9.154317
7.445684	346.804019	9.159335
7.284340	338.933932	9.164352
7.264208	328.176537	9.169370
6.909825	333.101092	9.174387
7.053828	328.957620	9.179405
7.141362	338.209185	9.184423
7.316444	346.781282	9.189440
7.366765	344.003009	9.194458
6.920160	335.356869	9.199475
7.177591	340.129368	9.204493
7.907421	338.895702	9.209511
7.439016	335.232566	9.214528
7.287635	332.324762	9.219546
7.182740	327.191302	9.224563
7.283638	329.451032	9.229581
7.528627	332.291056	9.234599
7.324998	324.465426	9.239616
7.507749	329.284261	9.244634
7.597327	333.161444	9.249651
7.170231	327.974014	9.254669
7.110298	326.882245	9.259687
6.907199	328.296259	9.264704
7.055314	326.439989	9.269722
7.432359	324.964620	9.274739
7.207108	329.493548	9.279757
7.395355	326.106854	9.284775
7.226468	330.964660	9.289792
7.184021	313.350378	9.294810
7.591470	329.371471	9.299827
7.067350	326.228227	9.304845
7.642627	334.397200	9.309863
7.675705	336.285657	9.314880
7.384227	328.887093	9.319898
7.672629	326.851198	9.324915
7.425103	329.373449	9.329933
7.805832	320.532235	9.334951
7.478568	331.931104	9.339968
7.683201	321.302811	9.344986
7.670122	322.182336	9.350003
7.773944	323.958797	9.355021
7.695150	301.162310	9.360039
7.444645	304.925187	9.365056
6.955140	287.042884	9.370074
7.149894	298.745443	9.375091
6.963461	310.592561	9.380109
7.813582	319.993614	9.385127
7.347314	323.427190	9.390144
7.143389	325.847982	9.395162
7.442413	325.738532	9.400179
7.119283	325.435630	9.405197
7.797761	319.426006	9.410215
7.539784	318.393473	9.415232
7.564433	321.264646	9.420250
7.742623	328.984227	9.425267
7.520425	331.051278	9.430285
7.670623	319.238628	9.435303
7.436099	327.937603	9.440320
7.542973	320.820986	9.445338
7.610613	324.808874	9.450355
7.568122	330.237106	9.455373
7.746948	317.590066	9.460391
7.445125	326.160671	9.465408
7.784500	325.155047	9.470426
7.498499	316.240927	9.475443
7.230793	325.014491	9.480461
7.792374	323.033889	9.485479
7.189876	329.262487	9.490496
7.436453	331.070367	9.495514
7.639726	332.815566	9.500531
7.423840	337.491353	9.505549
7.776848	328.528226	9.510567
7.229607	323.570931	9.515584
7.367263	326.759008	9.520602
7.301814	327.902294	9.525619
6.961132	332.884674	9.530637
7.244866	338.896401	9.535655
7.482606	339.500202	9.540672
7.548159	347.877924	9.545690
7.822323	353.509313	9.550707
7.556898	359.650728	9.555725
7.766109	343.941115	9.560743
8.153798	359.368894	9.565760
7.958194	351.797611	9.570778
7.840880	344.898917	9.575795
7.414414	340.598121	9.580813
7.813366	344.007437	9.585831
8.028291	353.772480	9.590848
7.803350	343.305727	9.595866
7.711951	341.212206	9.600883
7.496071	340.299344	9.605901
7.647377	330.559774	9.610919
8.017399	349.568797	9.615936
7.752180	345.643661	9.620954
7.520947	328.667798	9.625971
7.505307	355.266242	9.630989
7.873120	348.228901	9.636007
7.832361	347.831544	9.641024
7.908980	357.889508	9.646042
8.111110	350.123763	9.651059
7.571449	348.882634	9.656077
8.029616	344.993186	9.661095
7.904022	341.996162	9.666112
7.509501	337.305405	9.671130
7.814778	345.286058	9.676147
7.570422	354.769178	9.681165
8.016331	352.440527	9.686183
7.852653	353.100517	9.691200
7.960961	351.483960	9.696218
7.934632	354.407254	9.701235
7.909737	352.745167	9.706253
8.091409	349.211177	9.711271
8.218933	358.289276	9.716288
7.924934	356.574419	9.721306
7.730059	337.891991	9.726323
7.452914	342.157616	9.731341
7.711556	340.003284	9.736359
8.063963	343.826924	9.741376
7.791515	354.358937	9.746394
8.014955	344.734354	9.751411
8.186329	357.074877	9.756429
8.189704	350.791675	9.761447
7.995253	347.780126	9.766464
7.933916	363.867927	9.771482
8.053273	351.309013	9.776499
7.919501	352.226265	9.781517
8.009031	355.125209	9.786535
8.069537	353.216308	9.791552
8.016996	355.361083	9.796570
8.298830	347.582929	9.801587
8.114824	358.221088	9.806605
8.115745	346.548421	9.811623
7.916840	336.140732	9.816640
7.426905	356.230348	9.821658
7.933056	349.048397	9.826675
7.575503	352.373539	9.831693
7.652071	341.724150	9.836711
7.827060	345.547014	9.841728
7.620681	356.952322	9.846746
7.886370	356.150664	9.851763
8.097001	369.352886	9.856781
8.166570	368.840526	9.861799
8.038218	377.368367	9.866816
7.988358	376.293962	9.871834
8.365808	377.229444	9.876851
8.429779	385.553785	9.881869
8.212180	368.982840	9.886887
8.381087	349.786191	9.891904
8.290848	350.308520	9.896922
8.391994	339.418632	9.901939
8.151916	345.922152	9.906957
8.478716	343.896055	9.911975
8.410491	348.659302	9.916992
7.749724	353.000437	9.922010
8.052974	347.872848	9.927027
7.997671	352.536260	9.932045
8.060846	348.077180	9.937063
8.132537	345.465984	9.942080
7.853089	349.832951	9.947098
8.683567	365.273841	9.952115
8.170389	365.985091	9.957133
8.284103	361.707479	9.962151
8.133218	360.595157	9.967168
8.197180	364.217572	9.972186
8.564331	369.875511	9.977203
8.178102	371.769299	9.982221
8.435824	375.317369	9.987239
8.427903	353.008374	9.992256
8.139331	361.034160	9.997274
8.537364	352.127124	10.002291
8.121362	357.143327	10.007309
8.268995	365.050709	10.012327
8.593859	363.034378	10.017344
7.950188	361.929358	10.022362
7.829002	360.843968	10.027379
8.145015	362.369655	10.032397
8.399098	365.044175	10.037415
8.414680	365.881372	10.042432
8.389684	370.000453	10.047450
8.324768	372.866645	10.052467
8.394307	376.920518	10.057485
8.178236	375.742609	10.062503
8.635789	369.006853	10.067520
8.401853	371.164093	10.072538
8.669928	367.736561	10.077555
8.348568	372.902127	10.082573
8.563144	381.433380	10.087591
8.819154	371.030577	10.092608
8.686479	373.184674	10.097626
9.007718	366.621614	10.102643
8.405397	363.048748	10.107661
8.229981	357.579137	10.112679
8.446988	358.460709	10.117696
8.224628	374.579901	10.122714
8.583439	371.605278	10.127731
8.726009	381.914907	10.132749
8.604293	377.598210	10.137767
8.750359	380.485200	10.142784
8.496740	375.456929	10.147802
8.535109	370.408444	10.152819
8.639562	369.638200	10.157837
8.238777	361.811694	10.162855
8.585083	366.469382	10.167872
8.503966	376.851703	10.172890
8.658124	373.208388	10.177907
8.365297	380.089343	10.182925
8.752454	376.845231	10.187943
8.590398	370.613024	10.192960
8.226909	376.583530	10.197978
8.306650	375.463701	10.202995
8.698208	382.938656	10.208013
8.428180	378.118057	10.213031
8.418572	375.273374	10.218048
8.599241	384.472594	10.223066
8.700327	378.205726	10.228083
8.340725	380.262619	10.233101
8.308135	381.978277	10.238119
8.602505	369.082848	10.243136
8.554802	374.420391	10.248154
9.139958	379.359615	10.253171
8.776038	383.402086	10.258189
8.419775	380.497772	10.263207
8.572194	380.332256	10.268224
8.670098	390.727736	10.273242
8.777492	397.375980	10.278259
9.167822	400.657267	10.283277
8.641569	392.761924	10.288295
8.829227	387.983666	10.293312
8.516367	383.226536	10.298330
8.633052	383.950167	10.303347
9.302107	394.862609	10.308365
9.309062	382.276995	10.313383
9.146314	368.417683	10.318400
8.696852	384.575400	10.323418
8.723422	374.807892	10.328435
8.970461	376.981762	10.333453
8.736972	375.456287	10.338471
9.267883	381.618883	10.343488
8.890387	379.989604	10.348506
8.569828	379.904040	10.353523
8.936769	373.542135	10.358541
8.862588	379.275103	10.363559
9.130877	379.498626	10.368576
9.063546	374.750605	10.373594
8.581790	378.906092	10.378611
9.272173	372.692634	10.383629
8.861278	383.369289	10.388647
9.131657	376.192480	10.393664
8.848598	371.045724	10.398682
8.932121	377.164372	10.403699
9.115143	373.933109	10.408717
9.097047	386.135902	10.413735
9.082495	374.301532	10.418752
8.898398	381.900827	10.423770
8.536067	382.336139	10.428787
8.789377	382.694532	10.433805
8.649320	385.455666	10.438823
9.060069	381.150735	10.443840
9.030678	384.405854	10.448858
8.970090	376.898741	10.453875
9.008942	378.609587	10.458893
8.862731	372.223442	10.463911
8.812875	373.503152	10.468928
8.910087	374.340262	10.473946
8.656578	382.392156	10.478963
9.364539	385.002322	10.483981
9.110260	398.882837	10.488999
9.143868	397.350487	10.494016
9.476634	398.412843	10.499034
9.275884	392.549553	10.504051
9.451062	381.837453	10.509069
9.149414	378.255637	10.514087
9.108391	373.667614	10.519104
8.717853	379.026980	10.524122
8.714922	378.705780	10.529139
8.887719	377.044468	10.534157
9.233721	398.616518	10.539175
9.451174	394.960188	10.544192
9.266806	392.590815	10.549210
9.163435	401.569193	10.554227
9.431071	396.232551	10.559245
9.104553	399.912614	10.564263
9.428140	392.516085	10.569280
9.037010	388.976600	10.574298
8.964130	398.758077	10.579315
9.439178	393.291318	10.584333
9.008204	400.361040	10.589351
9.269344	395.571339	10.594368
9.553069	403.539596	10.599386
9.217265	396.185773	10.604403
9.315093	394.289991	10.609421
9.583335	405.763438	10.614439
9.733622	391.413578	10.619456
9.521553	378.155202	10.624474
8.990040	379.276386	10.629491
9.489948	375.361499	10.634509
9.197476	374.880262	10.639527
9.036512	376.546482	10.644544
9.405244	382.264137	10.649562
9.395376	395.387106	10.654579
9.486816	390.178880	10.659597
9.021182	393.195824	10.664615
9.440697	399.252700	10.669632
9.457861	396.069346	10.674650
9.169786	403.097887	10.679667
9.605450	397.021905	10.684685
9.460456	399.357796	10.689703
9.649158	401.714312	10.694720
9.946747	399.333013	10.699738
8.984981	396.816447	10.704755
9.021881	389.130056	10.709773
9.124189	395.009111	10.714791
9.274356	396.989793	10.719808
9.249600	405.776060	10.724826
9.209196	401.667594	10.729843
9.233406	399.836919	10.734861
9.356884	407.356780	10.739879
9.170627	402.756649	10.744896
9.208507	403.836518	10.749914
9.721414	412.971402	10.754931
9.410868	404.872063	10.759949
9.840859	418.724946	10.764967
9.695344	408.801184	10.769984
9.492275	413.153118	10.775002
9.508156	412.964682	10.780019
9.688955	404.741507	10.785037
9.502800	409.377972	10.790055
9.950610	403.252762	10.795072
9.726701	401.444940	10.800090
9.494485	403.377865	10.805107
9.681519	395.128479	10.810125
9.677090	396.085552	10.815143
10.005783	398.858908	10.820160
9.646719	408.845887	10.825178
9.562759	405.820281	10.830195
9.790208	397.618248	10.835213
9.605918	397.451510	10.840231
9.621078	409.645986	10.845248
9.518675	404.461625	10.850266
9.357540	406.254101	10.855283
9.568634	406.306658	10.860301
9.706403	418.923842	10.865319
10.043748	420.913250	10.870336
9.756736	410.367764	10.875354
9.733767	414.294044	10.880371
9.818609	402.974331	10.885389
9.672520	410.930621	10.890407
9.848560	412.225653	10.895424
10.212064	415.530054	10.900442
9.932743	416.634065	10.905459
9.738802	402.732248	10.910477
9.762859	406.786899	10.915495
9.507311	402.822377	10.920512
10.085253	398.810132	10.925530
9.635403	406.084757	10.930547
10.229930	404.300979	10.935565
9.920906	411.178157	10.940583
9.825278	402.739258	10.945600
9.567880	400.759934	10.950618
9.700938	417.650610	10.955635
10.033170	416.778631	10.960653
10.033206	417.387888	10.965671
10.148186	426.669938	10.970688
10.305604	418.655516	10.975706
9.736697	412.609710	10.980723
10.031725	401.405589	10.985741
9.800855	400.217360	10.990759
9.642528	400.254853	10.995776
10.310086	413.095646	11.000794
9.949589	416.080446	11.005811
9.724261	403.164926	11.010829
10.013776	417.787571	11.015847
9.947786	425.803976	11.020864
10.454174	425.453967	11.025882
9.956266	420.290157	11.030899
10.071316	408.621769	11.035917
10.133389	412.591611	11.040935
9.980987	419.229822	11.045952
10.178793	414.320594	11.050970
10.068047	414.022491	11.055987
9.892464	401.802939	11.061005
9.929534	412.441422	11.066023
10.110885	423.496084	11.071040
10.252655	429.400563	11.076058
10.258642	434.196458	11.081075
10.281988	423.798292	11.086093
9.903639	415.289803	11.091111
9.913168	419.438232	11.096128
10.334640	423.942226	11.101146
10.263349	422.609235	11.106163
10.234167	416.006046	11.111181
10.584678	428.135698	11.116199
10.140894	421.130022	11.121216
9.994540	406.018487	11.126234
10.377537	417.319448	11.131251
10.120360	413.825371	11.136269
10.555324	420.523603	11.141287
9.671043	406.770291	11.146304
10.170434	410.757245	11.151322
10.195426	419.592576	11.156339
10.175910	419.832509	11.161357
10.320581	423.581219	11.166375
10.294429	425.078138	11.171392
10.342081	425.493798	11.176410
10.370163	427.720698	11.181427
10.687986	421.341178	11.186445
10.494944	427.521837	11.191463
10.276940	427.202566	11.196480
10.586399	428.757680	11.201498
10.197179	419.032796	11.206515
10.387477	413.910152	11.211533
10.513116	418.179352	11.216551
10.092768	424.158727	11.221568
10.472116	427.956102	11.226586
10.623882	427.169022	11.231603
10.651983	422.279903	11.236621
10.205749	415.669068	11.241639
10.506981	424.022755	11.246656
10.530375	427.471626	11.251674
10.353991	420.717793	11.256691
10.429430	424.341588	11.261709
10.521954	427.262168	11.266727
10.567918	428.908798	11.271744
10.607422	427.384994	11.276762
10.098739	428.108169	11.281779
10.033407	422.794961	11.286797
10.576923	424.777515	11.291815
9.905438	423.512726	11.296832
10.281188	428.068020	11.301850
10.489988	430.563416	11.306867
10.609114	432.842411	11.311885
10.538426	425.153821	11.316903
10.227922	427.051603	11.321920
10.686153	418.753671	11.326938
10.686950	422.344908	11.331955
10.583884	422.345397	11.336973
10.451118	418.244996	11.341991
10.346152	428.697329	11.347008
10.991688	443.106780	11.352026
10.752917	445.062820	11.357043
10.246815	429.682244	11.362061
10.556729	425.604431	11.367079
10.687675	441.144836	11.372096
10.545824	438.693101	11.377114
10.611843	451.933679	11.382131
10.785259	446.248790	11.387149
10.972257	441.505333	11.392167
10.728880	455.030759	11.397184
11.137836	448.958918	11.402202
11.250508	437.114165	11.407219
10.801559	421.772032	11.412237
10.988181	418.852611	11.417255
11.016716	423.392539	11.422272
10.738348	427.522681	11.427290
10.523958	428.127456	11.432307
10.334499	426.926466	11.437325
11.102951	421.625445	11.442343
10.578945	430.252782	11.447360
10.664823	416.001289	11.452378
10.542111	429.122919	11.457395
10.751293	431.283755	11.462413
11.230580	438.154966	11.467431
11.040614	438.610777	11.472448
10.765811	439.474256	11.477466
10.932006	447.372473	11.482483
10.655543	434.177727	11.487501
10.977551	428.655893	11.492519
10.783427	440.217130	11.497536
10.988743	441.529696	11.502554
10.908338	440.188655	11.507571
10.842158	438.501432	11.512589
11.078354	440.484502	11.517607
11.116599	452.634388	11.522624
10.983878	445.009095	11.527642
11.393180	447.470120	11.532659
11.257738	451.937761	11.537677
11.373294	444.409506	11.542695
10.980877	432.924251	11.547712
10.910479	425.084145	11.552730
10.994175	423.780668	11.557747
11.102612	435.853346	11.562765
10.971454	431.752691	11.567783
11.051243	438.263244	11.572800
11.055679	444.659304	11.577818
11.195611	443.299736	11.582835
11.021325	445.435076	11.587853
11.400061	445.524644	11.592871
11.419319	440.728411	11.597888
11.286227	435.132272	11.602906
10.882651	429.016540	11.607923
10.729781	432.944116	11.612941
11.285920	430.494156	11.617959
11.308232	449.194522	11.622976
10.874578	448.100975	11.627994
11.378446	454.939964	11.633011
11.009200	453.751186	11.638029
11.441086	447.085666	11.643047
11.167700	444.039056	11.648064
11.214996	446.455462	11.653082
11.064799	449.325478	11.658099
11.157873	448.358195	11.663117
11.066540	444.844602	11.668135
11.136032	446.203561	11.673152
11.373516	446.040579	11.678170
11.282202	443.132871	11.683187
11.011100	442.597814	11.688205
11.355927	437.564708	11.693223
11.241375	447.235940	11.698240
11.338664	435.907957	11.703258
11.294416	446.136262	11.708275
11.432956	444.126843	11.713293
11.204384	440.915472	11.718311
11.281191	449.313580	11.723328
11.099633	448.613109	11.728346
11.634519	471.080449	11.733363
11.282983	463.003243	11.738381
11.200301	447.979585	11.743399
11.352654	469.405154	11.748416
11.650089	473.556105	11.753434
11.537121	467.616010	11.758451
11.479321	475.126256	11.763469
11.624816	464.358769	11.768487
11.654211	472.540218	11.773504
11.316199	470.238936	11.778522
11.640705	464.012987	11.783539
11.455745	475.910477	11.788557
11.950453	469.964127	11.793575
11.509681	465.725486	11.798592
10.954879	453.347201	11.803610
11.458040	462.458383	11.808627
11.571109	476.209182	11.813645
11.687015	466.907376	11.818663
11.722714	476.640434	11.823680
11.595990	471.182142	11.828698
11.738107	470.172510	11.833715
11.686984	474.627028	11.838733
11.657218	471.981120	11.843751
11.333249	477.207080	11.848768
11.885587	479.144088	11.853786
12.081986	479.842689	11.858803
11.823863	471.798271	11.863821
11.987636	471.886596	11.868839
11.699153	460.416698	11.873856
11.746844	470.624391	11.878874
11.775954	477.231207	11.883891
11.905104	471.477466	11.888909
11.774466	459.686359	11.893927
11.695346	458.777443	11.898944
11.640106	470.821983	11.903962
11.998548	465.376512	11.908979
11.723391	469.089616	11.913997
11.745517	469.285198	11.919015
11.926754	466.839958	11.924032
11.925011	471.220518	11.929050
12.119712	459.224129	11.934067
11.589892	462.311036	11.939085
11.742305	457.014405	11.944103
12.037204	456.369134	11.949120
12.037984	476.515021	11.954138
12.113370	470.378348	11.959155
11.979446	453.573399	11.964173
12.013925	441.933313	11.969191
11.658968	454.213846	11.974208
11.644494	459.385302	11.979226
12.198199	456.872604	11.984243
12.315352	463.314235	11.989261
12.023851	453.589895	11.994279
12.008604	447.006615	11.999296
11.730692	452.581987	12.004314
12.031050	460.970539	12.009331
11.967507	468.169265	12.014349
12.011777	460.759395	12.019367
12.076623	454.034259	12.024384
11.946615	464.582027	12.029402
12.128812	458.501309	12.034419
11.762419	465.977550	12.039437
11.946713	466.643323	12.044455
12.147600	466.946767	12.049472
12.012857	471.733026	12.054490
12.118722	462.132998	12.059507
11.781775	464.779638	12.064525
12.141569	463.496285	12.069543
12.224726	460.267932	12.074560
11.988718	461.627122	12.079578
12.291532	453.735207	12.084595
12.200136	461.073960	12.089613
12.203367	467.949878	12.094631
11.908184	467.948722	12.099648
12.362346	462.216962	12.104666
12.232180	469.432372	12.109683
11.863988	468.707312	12.114701
11.950679	472.998368	12.119719
12.755160	477.174511	12.124736
12.148277	480.346000	12.129754
12.060989	477.324055	12.134771
12.131754	491.797790	12.139789
12.486169	492.478101	12.144807
12.392359	500.997468	12.149824
12.409829	486.475715	12.154842
12.660958	486.698756	12.159859
12.716664	486.668213	12.164877
12.377898	476.862861	12.169895
12.128565	469.473454	12.174912
12.012383	468.674445	12.179930
12.269969	482.585778	12.184947
12.339048	497.858165	12.189965
12.371736	493.018804	12.194983
12.289394	497.266758	12.200000
12.301925	494.768889	12.205018
12.400321	487.662992	12.210035
12.482345	498.285060	12.215053
12.540220	486.622369	12.220071
12.585891	491.431034	12.225088
12.536533	496.860386	12.230106
12.443586	492.712744	12.235123
12.429156	483.207170	12.240141
12.440379	488.687045	12.245159
12.733409	484.274191	12.250176
12.498175	487.517199	12.255194
12.617518	482.929425	12.260211
12.637991	497.369971	12.265229
12.554797	487.660515	12.270247
12.452136	487.708276	12.275264
12.560719	495.842693	12.280282
12.889967	485.286416	12.285299
12.910817	492.109109	12.290317
12.440430	496.464816	12.295335
12.574732	490.707111	12.300352
12.679525	489.472926	12.305370
12.889386	488.777780	12.310387
12.741494	489.612034	12.315405
12.607663	496.433567	12.320423
13.035546	497.137151	12.325440
13.092420	500.991061	12.330458
12.747754	493.973079	12.335475
13.025495	497.827313	12.340493
12.682995	490.767971	12.345511
13.010722	491.405102	12.350528
12.956756	492.319402	12.355546
12.764976	480.525179	12.360563
12.567616	494.693539	12.365581
12.660149	484.940946	12.370599
12.611976	488.000201	12.375616
12.831635	497.531066	12.380634
12.814008	486.053692	12.385651
12.849259	483.811053	12.390669
12.954486	498.014351	12.395687
13.214327	490.040752	12.400704
12.882790	491.733541	12.405722
12.731810	490.804255	12.410739
12.926829	499.628931	12.415757
12.912003	508.293788	12.420775
13.178354	505.535501	12.425792
13.219749	514.175829	12.430810
13.245022	506.573245	12.435827
13.058964	493.847198	12.440845
12.803000	497.358511	12.445863
13.099875	495.125627	12.450880
12.667857	501.479214	12.455898
12.980249	503.179039	12.460915
13.408937	510.641956	12.465933
13.223790	512.611744	12.470951
13.370944	509.468089	12.475968
13.033956	500.179978	12.480986
13.073457	496.516621	12.486003
13.076892	504.058368	12.491021
12.982690	515.935442	12.496039
13.267950	500.889165	12.501056
12.856064	501.732966	12.506074
12.999242	502.894271	12.511091
13.257367	503.286630	12.516109
12.714747	504.936549	12.521127
13.087947	506.450189	12.526144
13.056861	514.596894	12.531162
13.137628	518.077874	12.536179
13.121940	510.876126	12.541197
13.479997	510.710149	12.546215
13.447726	515.218544	12.551232
13.131756	505.299178	12.556250
13.230723	506.278027	12.561267
13.453606	510.863455	12.566285
13.259560	514.541849	12.571303
13.441100	509.991720	12.576320
12.668019	508.518689	12.581338
13.066061	529.644157	12.586355
13.454322	526.352510	12.591373
13.506759	538.222546	12.596391
13.804501	534.257053	12.601408
13.914117	528.957598	12.606426
13.618098	523.329996	12.611443
13.479095	503.164993	12.616461
13.375911	505.544879	12.621479
13.782418	507.596110	12.626496
13.395792	509.193341	12.631514
13.298271	512.474869	12.636531
13.786806	515.021394	12.641549
13.619193	514.318749	12.646567
13.464654	509.779922	12.651584
13.438477	513.040876	12.656602
13.560837	530.523437	12.661619
13.944243	530.937314	12.666637
13.742341	522.221427	12.671655
13.493228	510.098452	12.676672
13.648910	513.498342	12.681690
13.813630	518.130695	12.686707
13.611076	515.868275	12.691725
13.584987	512.518072	12.696743
13.701721	519.370027	12.701760
14.012848	530.041647	12.706778
14.098612	519.668419	12.711795
14.144561	514.694449	12.716813
13.278826	507.587183	12.721831
13.505154	500.776930	12.726848
13.569193	503.818717	12.731866
13.465680	517.369750	12.736883
13.779993	523.812262	12.741901
13.612020	535.628255	12.746919
14.014165	521.519932	12.751936
13.880652	529.206084	12.756954
13.949708	532.941345	12.761971
14.055130	527.017718	12.766989
13.844404	536.378938	12.772007
13.651548	532.527698	12.777024
13.924183	533.078737	12.782042
13.565617	535.192288	12.787059
13.880749	528.626964	12.792077
13.967078	532.141793	12.797095
13.672645	525.917520	12.802112
13.613210	534.766053	12.807130
13.524161	530.545215	12.812147
13.918615	532.674061	12.817165
13.655223	538.382893	12.822183
14.027799	530.634711	12.827200
13.899502	526.603014	12.832218
13.948917	540.871839	12.837235
13.896243	543.063992	12.842253
14.047269	555.347862	12.847271
14.213506	554.372338	12.852288
14.221379	554.753170	12.857306
13.911486	554.776394	12.862323
14.102559	552.184449	12.867341
14.424457	558.262890	12.872359
14.379881	555.843329	12.877376
14.323430	549.285360	12.882394
13.998868	542.601886	12.887411
14.304937	536.571280	12.892429
14.288419	537.249388	12.897447
13.879705	529.815347	12.902464
14.374852	538.233566	12.907482
14.151266	545.854857	12.912499
14.362572	543.559553	12.917517
14.099878	553.020387	12.922535
14.578018	543.965089	12.927552
14.637723	549.238626	12.932570
14.377472	531.071083	12.937587
13.854828	533.311162	12.942605
14.197823	536.883856	12.947623
14.297115	544.079349	12.952640
14.445712	544.059589	12.957658
14.210995	549.912277	12.962675
14.713772	544.788279	12.967693
14.372502	553.071656	12.972711
14.347086	550.519729	12.977728
14.720746	554.336951	12.982746
14.204864	556.137340	12.987763
14.827307	550.679141	12.992781
14.517642	554.962502	12.997799
14.652434	559.381784	13.002816
14.569046	557.782432	13.007834
14.577451	555.812197	13.012851
14.655781	543.145931	13.017869
14.375042	556.942329	13.022887
14.576711	549.466892	13.027904
14.512913	549.019471	13.032922
14.408165	553.668543	13.037939
14.750655	552.889631	13.042957
14.560105	554.936001	13.047975
14.674384	556.616187	13.052992
14.551791	551.472795	13.058010
14.345493	558.412928	13.063027
14.666170	551.486983	13.068045
14.476609	557.563008	13.073063
14.480943	550.433863	13.078080
14.520969	553.444685	13.083098
14.809317	554.110039	13.088115
14.593829	553.686236	13.093133
14.590016	557.271907	13.098151
14.772437	557.827526	13.103168
14.889289	551.356178	13.108186
14.551998	555.972033	13.113203
14.819938	553.257671	13.118221
14.518246	560.045405	13.123239
14.534345	559.421449	13.128256
15.149580	565.378484	13.133274
14.793391	564.020414	13.138291
15.049541	557.426394	13.143309
14.791297	564.421952	13.148327
14.835251	558.719316	13.153344
15.056173	562.509830	13.158362
15.098515	566.466999	13.163379
15.105374	555.575881	13.168397
14.878116	553.374104	13.173415
14.671043	548.991764	13.178432
15.312811	560.665920	13.183450
14.621173	573.718452	13.188467
15.082051	573.874124	13.193485
15.041892	576.351500	13.198503
14.884484	579.049096	13.203520
15.118493	581.553211	13.208538
14.916735	584.131485	13.213555
15.266909	572.707239	13.218573
15.252069	574.319170	13.223591
15.045236	575.462396	13.228608
15.508859	576.567503	13.233626
14.872180	579.245049	13.238643
14.965570	578.078902	13.243661
15.047530	585.182440	13.248679
15.472364	580.193640	13.253696
15.422981	580.094255	13.258714
15.071981	581.660699	13.263731
15.047966	575.018779	13.268749
15.348282	587.364631	13.273767
15.219368	584.134562	13.278784
15.488147	575.881832	13.283802
15.351211	589.984058	13.288819
15.103572	583.490556	13.293837
15.271476	588.195013	13.298855
15.314309	578.298634	13.303872
15.242715	583.573690	13.308890
15.095982	586.376918	13.313907
15.230569	575.759380	13.318925
15.293840	585.059031	13.323943
14.917968	589.598853	13.328960
15.170083	579.060841	13.333978
15.049170	584.715947	13.338995
15.432209	601.100835	13.344013
15.737340	606.818998	13.349031
15.785706	609.885333	13.354048
15.833096	591.303769	13.359066
15.464177	585.797947	13.364083
15.436032	585.701567	13.369101
15.592937	581.079518	13.374119
15.256116	583.464234	13.379136
15.807248	586.761544	13.384154
15.476362	596.583301	13.389171
15.633267	595.394641	13.394189
15.607023	597.932967	13.399207
15.695694	597.622747	13.404224
15.705900	607.069521	13.409242
15.892848	608.441762	13.414259
15.729453	589.214545	13.419277
15.489414	589.403611	13.424295
15.915329	588.261428	13.429312
15.996699	588.823314	13.434330
15.433967	594.212710	13.439347
15.463198	577.192900	13.444365
15.753924	590.698385	13.449383
15.887687	599.750392	13.454400
16.072989	603.126753	13.459418
15.839683	605.296546	13.464435
15.645651	601.003677	13.469453
15.842110	595.797975	13.474471
15.651290	605.247646	13.479488
15.846100	592.181371	13.484506
15.841166	597.581747	13.489523
15.812747	601.893912	13.494541
16.051361	601.197441	13.499559
15.688801	593.699384	13.504576
16.086126	599.535730	13.509594
15.987318	597.023624	13.514611
15.986560	598.791150	13.519629
16.281735	591.812358	13.524647
15.627759	597.329566	13.529664
16.144910	589.208567	13.534682
15.892475	605.607196	13.539699
16.148575	611.989379	13.544717
16.182404	602.078610	13.549735
15.710799	596.844383	13.554752
15.874139	595.228703	13.559770
15.953445	595.200797	13.564787
15.781391	601.015344	13.569805
15.778480	601.511461	13.574823
15.990249	608.591642	13.579840
16.219516	620.153344	13.584858
16.330112	628.341156	13.589875
16.006576	626.895949	13.594893
16.415498	621.123846	13.599911
16.521233	626.163029	13.604928
16.366112	612.699958	13.609946
16.001627	603.902050	13.614963
15.945802	618.831084	13.619981
16.510800	616.281894	13.624999
16.058052	624.393318	13.630016
16.554147	621.056464	13.635034
16.579110	627.162225	13.640051
16.504266	621.345527	13.645069
16.590246	613.118085	13.650087
16.469155	609.687985	13.655104
16.366454	612.386535	13.660122
16.587011	608.758080	13.665139
16.281037	598.789769	13.670157
16.552495	602.345214	13.675175
16.488943	617.710936	13.680192
16.576705	608.921505	13.685210
16.223140	614.325675	13.690227
16.262968	619.880029	13.695245
16.506274	617.952106	13.700263
16.494311	625.395320	13.705280
17.011285	615.917386	13.710298
16.450635	624.001430	13.715315
16.453663	621.202077	13.720333
16.735936	624.153103	13.725351
16.640241	623.565485	13.730368
16.910847	618.528106	13.735386
16.683811	619.311574	13.740403
16.695941	624.052917	13.745421
16.696077	629.610298	13.750439
16.824221	630.164903	13.755456
16.757966	620.900846	13.760474
16.829212	624.547426	13.765491
16.809617	630.950450	13.770509
16.841461	626.297370	13.775527
17.028063	630.509794	13.780544
16.605428	623.873116	13.785562
16.403991	625.807584	13.790579
16.467472	632.112471	13.795597
17.003831	620.766500	13.800615
16.611673	628.265754	13.805632
16.483998	627.705204	13.810650
16.759664	622.846911	13.815667
16.425269	626.383084	13.820685
16.597954	627.104318	13.825703
16.852378	640.271522	13.830720
17.060296	643.041631	13.835738
17.021398	652.436117	13.840755
16.823754	647.642042	13.845773
17.005686	644.029060	13.850791
17.079178	655.198487	13.855808
17.288631	640.741388	13.860826
17.167708	641.265347	13.865843
16.933349	651.545459	13.870861
17.159489	640.184662	13.875879
17.268282	651.979729	13.880896
17.369278	641.610371	13.885914
17.217227	645.607291	13.890931
17.001614	636.416972	13.895949
17.506320	633.883478	13.900967
17.197094	631.703920	13.905984
17.003016	613.772134	13.911002
17.194939	627.507618	13.916019
17.063171	632.987711	13.921037
17.452359	629.358242	13.926055
17.368563	635.436760	13.931072
17.377488	642.725255	13.936090
17.587550	640.351240	13.941107
17.202659	638.035145	13.946125
17.540683	633.324925	13.951143
17.287819	643.712052	13.956160
17.160498	641.586220	13.961178
17.375128	636.081040	13.966195
17.226084	641.787880	13.971213
17.820958	636.990333	13.976231
17.729326	643.294128	13.981248
17.583445	639.669073	13.986266
17.682376	640.294496	13.991283
16.861013	639.456956	13.996301
17.209453	630.216687	14.001319
17.270100	637.901057	14.006336
17.136422	631.752699	14.011354
17.401845	637.511768	14.016371
17.370754	642.878362	14.021389
17.560125	638.547879	14.026407
17.669519	631.121487	14.031424
17.463354	635.215189	14.036442
17.695536	631.509183	14.041459
17.183647	639.468881	14.046477
17.497037	653.561001	14.051495
17.893687	660.754424	14.056512
17.750690	657.797925	14.061530
17.794128	659.564886	14.066547
17.611522	665.027659	14.071565
17.609609	664.384413	14.076583
17.679884	671.691770	14.081600
17.565104	655.208687	14.086618
18.056264	660.033241	14.091635
17.919822	665.848576	14.096653
17.602624	659.015594	14.101671
17.861868	658.255950	14.106688
17.692826	662.334412	14.111706
17.831994	655.001201	14.116723
17.786670	666.091306	14.121741
17.804327	662.352424	14.126759
18.038647	662.095262	14.131776
17.928056	656.542886	14.136794
18.211982	656.621972	14.141811
17.831956	660.878445	14.146829
17.808597	661.507131	14.151847
18.231239	663.486443	14.156864
17.942457	669.760985	14.161882
18.376910	659.276585	14.166899
18.349451	657.807367	14.171917
18.239236	658.796703	14.176935
18.089876	659.555457	14.181952
17.872041	661.672357	14.186970
18.124816	662.264361	14.191987
17.997512	666.109115	14.197005
18.252509	659.253313	14.202023
18.331766	661.469120	14.207040
18.104809	668.529273	14.212058
18.185261	657.626634	14.217075
18.203856	663.597705	14.222093
18.198922	660.843764	14.227111
18.489242	662.723761	14.232128
18.307434	666.589624	14.237146
18.601325	663.902762	14.242163
18.481462	670.457107	14.247181
18.465362	663.861257	14.252199
18.286443	660.231874	14.257216
18.106518	662.049391	14.262234
18.392682	658.937713	14.267251
18.577368	665.697096	14.272269
18.360811	659.678394	14.277287
18.780092	670.528913	14.282304
18.660225	669.367562	14.287322
18.482859	675.934018	14.292339
18.398151	670.106217	14.297357
18.300507	666.549382	14.302375
18.721581	669.952162	14.307392
18.490433	674.235950	14.312410
18.543638	684.790035	14.317427
18.398004	691.824912	14.322445
18.698628	682.538414	14.327463
18.877474	690.248584	14.332480
18.874939	683.126766	14.337498
19.078634	681.047218	14.342515
18.657872	680.525988	14.347533
18.653420	671.230192	14.352551
18.615829	678.440740	14.357568
18.517913	684.010249	14.362586
18.932452	676.454280	14.367603
18.733400	684.340045	14.372621
18.694070	688.590815	14.377639
18.821624	684.320437	14.382656
18.887115	687.466168	14.387674
18.911867	688.844734	14.392691
18.440324	680.470544	14.397709
18.476651	684.873630	14.402727
18.711946	681.810893	14.407744
18.708409	683.127593	14.412762
18.851628	679.280798	14.417779
18.842322	685.271998	14.422797
18.884219	695.269290	14.427815
19.003036	695.601295	14.432832
19.239773	702.096975	14.437850
19.583787	687.558929	14.442867
19.341252	685.867583	14.447885
18.952338	681.721798	14.452903
19.131462	682.012855	14.457920
18.880607	684.516739	14.462938
19.393281	675.926198	14.467955
19.046422	689.363775	14.472973
18.816562	687.209722	14.477991
19.080627	687.108870	14.483008
19.039598	702.051449	14.488026
19.163189	712.572501	14.493043
19.291655	708.194682	14.498061
19.183196	711.250739	14.503079
19.411497	712.307290	14.508096
19.334228	713.054821	14.513114
19.502390	714.672985	14.518131
19.567502	715.571912	14.523149
19.463050	721.341260	14.528167
19.657795	711.414844	14.533184
19.253758	718.635127	14.538202
19.509774	711.031243	14.543219
19.437833	716.142296	14.548237
19.523716	713.257445	14.553255
19.747928	705.759498	14.558272
19.414207	705.363567	14.563290
19.396125	702.731583	14.568307
19.617125	701.656010	14.573325
19.556010	707.424918	14.578343
19.668548	711.734097	14.583360
19.521763	713.347650	14.588378
19.492310	705.138138	14.593395
19.717967	708.050658	14.598413
19.525955	706.146323	14.603431
19.990089	702.385253	14.608448
19.468166	709.377742	14.613466
19.615369	705.287331	14.618483
19.966045	706.173354	14.623501
19.934613	708.359064	14.628519
19.795024	705.449362	14.633536
19.684567	706.063209	14.638554
19.703140	707.786711	14.643571
19.865188	711.337122	14.648589
19.747020	709.781041	14.653607
19.842143	699.573504	14.658624
19.535191	704.853683	14.663642
19.921436	703.256935	14.668659
19.844100	708.428784	14.673677
19.904604	704.812606	14.678695
20.202059	706.158182	14.683712
19.926575	710.291095	14.688730
19.867348	706.277005	14.693747
19.934007	713.521827	14.698765
19.931859	707.772675	14.703783
20.045394	707.941405	14.708800
19.848341	705.820110	14.713818
19.743917	708.528410	14.718835
19.940202	708.397087	14.723853
19.826982	714.966193	14.728871
20.284958	720.947766	14.733888
20.650965	731.509979	14.738906
20.695272	727.678574	14.743923
20.558099	706.632611	14.748941
19.962650	714.785229	14.753959
20.449340	703.674149	14.758976
19.663077	704.699321	14.763994
19.856595	704.095071	14.769011
19.995984	723.354992	14.774029
19.854804	730.493330	14.779047
20.110921	716.252960	14.784064
20.091850	727.613563	14.789082
20.423857	731.083869	14.794099
20.596236	731.994498	14.799117
20.742801	728.323891	14.804135
20.734492	715.156611	14.809152
20.580113	725.948162	14.814170
20.867785	720.687197	14.819187
20.800727	731.477779	14.824205
20.647454	735.336058	14.829223
20.817682	728.963630	14.834240
20.709352	728.756661	14.839258
21.108032	714.307909	14.844275
20.404594	708.014712	14.849293
20.338159	701.682297	14.854311
20.755823	709.336357	14.859328
20.520821	723.898912	14.864346
20.575587	723.606591	14.869363
20.956052	721.559475	14.874381
20.679428	722.820869	14.879399
20.878560	717.425372	14.884416
20.681673	727.844857	14.889434
20.509843	727.625685	14.894451
20.697963	722.799929	14.899469
20.621981	727.409855	14.904487
20.951044	719.605252	14.909504
20.655708	719.244368	14.914522
21.012233	715.730416	14.919539
21.161139	727.544535	14.924557
20.812056	723.540857	14.929575
21.242614	724.291371	14.934592
21.121994	731.069912	14.939610
20.917879	722.474188	14.944627
21.059621	722.013695	14.949645
20.927756	721.674694	14.954663
21.244097	724.298551	14.959680
21.112778	727.159360	14.964698
21.192023	731.546309	14.969715
21.193690	731.038199	14.974733
21.081095	718.764442	14.979751
21.063030	729.399076	14.984768
20.936052	730.873851	14.989786
20.677509	725.148834	14.994803
20.934560	724.061335	14.999821
20.658784	730.920836	15.004839
20.853773	717.936490	15.009856
21.128471	736.907123	15.014874
21.311428	745.411916	15.019891
21.709360	747.480290	15.024909
22.042745	743.480800	15.029927
21.552467	728.794913	15.034944
21.438635	725.859107	15.039962
21.354491	727.911019	15.044979
21.386803	722.752927	15.049997
21.364410	716.300044	15.055015
21.464119	713.226854	15.060032
21.387524	719.061290	15.065050
20.977295	721.066145	15.070067
21.755244	735.893863	15.075085
21.583392	744.728446	15.080103
21.727463	737.034686	15.085120
21.623438	742.374797	15.090138
21.841752	741.956029	15.095155
21.821755	721.699668	15.100173
21.373703	720.396913	15.105191
21.390688	730.874616	15.110208
21.568014	739.913600	15.115226
21.577131	739.953425	15.120243
21.885754	736.989711	15.125261
21.894464	748.140881	15.130279
21.860637	745.246262	15.135296
21.754819	746.878685	15.140314
21.634754	742.249227	15.145331
21.879249	741.816915	15.150349
21.699151	746.547195	15.155367
21.955540	747.214377	15.160384
21.603547	754.177270	15.165402
21.751563	745.889617	15.170419
21.814881	741.367302	15.175437
21.280728	749.210598	15.180455
21.625302	744.284740	15.185472
21.598323	751.724034	15.190490
21.522511	765.431884	15.195507
22.198522	763.584893	15.200525
21.882603	775.206334	15.205543
22.296958	769.748910	15.210560
22.307860	774.799745	15.215578
22.096818	771.475134	15.220595
22.287962	768.327740	15.225613
22.057987	776.265696	15.230631
22.270676	768.646444	15.235648
22.275999	762.113491	15.240666
22.017456	775.695169	15.245683
22.491716	765.425410	15.250701
22.602911	762.981567	15.255719
22.452507	757.239703	15.260736
22.229747	761.045692	15.265754
21.880964	768.453047	15.270771
22.267298	767.973405	15.275789
22.410859	772.886823	15.280807
22.097879	770.048287	15.285824
22.492519	765.401799	15.290842
22.665323	760.316493	15.295859
22.678908	762.577250	15.300877
22.493154	775.614278	15.305895
22.504237	758.849578	15.310912
22.416107	765.869220	15.315930
22.207703	774.860984	15.320947
22.576479	764.014372	15.325965
22.483579	767.273138	15.330983
22.618453	759.523998	15.336000
22.530080	760.591988	15.341018
22.353587	773.128968	15.346035
22.555144	775.761237	15.351053
22.776612	796.068780	15.356071
22.823011	791.485972	15.361088
23.022031	789.321935	15.366106
23.042654	792.954340	15.371123
23.041006	780.625398	15.376141
22.563193	774.902947	15.381159
22.878501	765.008221	15.386176
23.102748	776.324660	15.391194
22.790215	779.027504	15.396211
23.185406	771.566023	15.401229
22.852876	758.048415	15.406247
22.754766	767.007224	15.411264
23.095637	777.216782	15.416282
23.061020	795.639204	15.421299
23.080367	795.816288	15.426317
22.964282	791.804719	15.431335
23.102051	788.135470	15.436352
23.415342	795.578606	15.441370
23.345039	793.548017	15.446387
22.820859	773.714071	15.451405
22.907488	781.356589	15.456423
22.957574	792.141591	15.461440
23.514122	791.083195	15.466458
23.094743	797.646352	15.471475
23.420383	791.978677	15.476493
23.238231	791.802135	15.481511
23.194200	794.295923	15.486528
23.511122	779.459071	15.491546
23.194998	795.779431	15.496563
23.453517	782.750433	15.501581
23.480054	789.572355	15.506599
23.329291	779.825924	15.511616
23.589954	783.534560	15.516634
23.443137	779.199584	15.521651
23.210369	780.706612	15.526669
23.225064	779.458033	15.531687
23.135708	785.925622	15.536704
23.325921	778.205726	15.541722
23.471475	787.287550	15.546739
23.333252	784.642703	15.551757
23.412666	786.978418	15.556775
23.143951	796.014295	15.561792
23.644908	804.012025	15.566810
23.471039	810.871469	15.571827
23.671937	811.818687	15.576845
23.636182	810.205584	15.581863
23.747484	800.683420	15.586880
24.055143	803.516919	15.591898
23.597686	805.993028	15.596915
24.033582	807.664187	15.601933
23.930356	803.252992	15.606951
24.119683	805.457990	15.611968
23.789999	801.694265	15.616986
23.916982	799.860171	15.622003
24.108098	807.499055	15.627021
24.335022	806.170095	15.632039
24.195524	814.658857	15.637056
24.305078	807.775152	15.642074
24.165318	806.916683	15.647091
23.960885	789.513339	15.652109
23.830002	796.217765	15.657127
23.848410	799.989369	15.662144
24.261380	802.456185	15.667162
24.286572	808.107549	15.672179
23.646849	811.243183	15.677197
23.922661	812.115621	15.682215
23.870460	811.641142	15.687232
24.413804	803.096256	15.692250
24.388188	804.804558	15.697267
23.852574	807.832466	15.702285
24.264166	808.336634	15.707303
23.671463	813.550885	15.712320
24.451904	804.962771	15.717338
24.884347	830.277205	15.722355
24.620627	817.304246	15.727373
24.392561	802.968783	15.732391
24.133613	804.053867	15.737408
24.396179	801.813664	15.742426
24.566696	827.052111	15.747443
24.517067	828.726285	15.752461
24.469744	821.497779	15.757479
24.598397	832.630327	15.762496
24.747704	829.486280	15.767514
24.602734	836.902955	15.772531
24.964581	839.065319	15.777549
24.769328	828.615747	15.782567
24.521007	833.763762	15.787584
24.847590	823.207700	15.792602
24.986601	832.075975	15.797619
24.905125	833.508961	15.802637
25.051752	822.425509	15.807655
24.725757	806.988160	15.812672
24.521128	801.560830	15.817690
24.445763	812.226525	15.822707
24.544361	819.961868	15.827725
24.776615	823.422477	15.832743
24.567844	835.718380	15.837760
24.786697	827.362857	15.842778
24.972609	833.825474	15.847795
24.832740	832.755588	15.852813
24.977756	835.191546	15.857831
24.885309	837.112223	15.862848
25.036625	832.954872	15.867866
25.043065	829.766799	15.872883
24.951216	830.491359	15.877901
25.233870	830.558022	15.882919
25.227502	843.545080	15.887936
25.334625	840.237189	15.892954
25.282956	833.978166	15.897971
24.864052	842.160157	15.902989
25.451310	839.765256	15.908007
25.155846	846.940285	15.913024
25.622310	847.555829	15.918042
25.224279	846.172694	15.923059
25.281847	848.432925	15.928077
25.391322	846.857166	15.933095
25.264407	851.203661	15.938112
25.947312	854.903375	15.943130
25.765083	853.590779	15.948147
25.496895	846.118946	15.953165
25.631450	846.306495	15.958183
25.581789	851.906411	15.963200
25.787136	841.384993	15.968218
25.463953	834.054269	15.973235
25.345166	837.162447	15.978253
25.648524	847.314772	15.983271
25.636097	847.960697	15.988288
25.583013	851.396312	15.993306
25.554936	852.877788	15.998323
25.301681	849.868997	16.003341
25.754704	849.044462	16.008359
25.549130	851.942098	16.013376
25.740383	847.724878	16.018394
25.762959	849.166911	16.023411
25.547060	851.687466	16.028429
25.830192	844.792500	16.033447
25.606151	851.151697	16.038464
25.787603	870.398917	16.043482
25.938151	869.066065	16.048499
26.022944	879.094650	16.053517
26.421433	869.770727	16.058535
26.151712	865.792530	16.063552
26.214333	866.098574	16.068570
26.347294	876.769740	16.073587
26.040033	865.485536	16.078605
26.336353	863.969046	16.083623
26.069727	867.103403	16.088640
26.319112	866.342131	16.093658
26.345135	867.326045	16.098675
26.013568	867.750266	16.103693
26.424437	865.417539	16.108711
26.052172	869.571869	16.113728
25.644788	878.310649	16.118746
26.001351	876.456581	16.123763
26.293579	884.840289	16.128781
26.526208	872.534766	16.133799
26.146421	869.848623	16.138816
25.960856	872.203516	16.143834
26.356740	868.086972	16.148851
26.224874	892.630993	16.153869
26.786591	891.549697	16.158887
26.732647	896.705335	16.163904
26.869424	890.303344	16.168922
26.751581	877.361277	16.173939
26.358766	875.841631	16.178957
26.635107	882.530023	16.183975
26.784314	888.171570	16.188992
26.966766	871.522091	16.194010
26.641449	868.025909	16.199027
26.483035	881.301750	16.204045
27.060297	885.175705	16.209063
27.046468	886.910581	16.214080
26.793146	876.738261	16.219098
26.787730	880.526214	16.224115
26.697438	878.564998	16.229133
27.053854	883.871331	16.234151
27.085112	890.692557	16.239168
27.159602	887.001582	16.244186
27.041335	889.068293	16.249203
27.078879	889.324594	16.254221
27.116800	891.401701	16.259239
27.067549	879.446168	16.264256
27.383111	876.781147	16.269274
26.962749	878.001817	16.274291
27.157466	879.303443	16.279309
27.336819	874.428520	16.284327
27.221397	884.535617	16.289344
27.286781	878.031140	16.294362
27.289405	882.474236	16.299379
27.062421	886.564926	16.304397
27.317747	884.221700	16.309415
27.289534	883.828689	16.314432
27.417434	884.885104	16.319450
27.297117	882.038643	16.324467
27.372718	886.423041	16.329485
27.480733	887.343700	16.334503
27.254096	885.160719	16.339520
27.502290	882.922743	16.344538
27.321325	888.517869	16.349555
27.122565	886.794442	16.354573
27.345622	878.188937	16.359591
27.046503	885.803199	16.364608
27.425213	890.721062	16.369626
27.631122	900.105965	16.374643
27.481003	909.663067	16.379661
27.682752	908.057158	16.384679
27.383477	913.837967	16.389696
27.633538	905.291359	16.394714
27.847958	904.519750	16.399731
27.682353	906.429735	16.404749
28.110648	916.023014	16.409767
27.961270	912.512054	16.414784
27.670290	914.574101	16.419802
27.992252	912.412998	16.424819
27.837229	907.747914	16.429837
28.064143	910.309984	16.434855
27.891564	908.143830	16.439872
27.729626	913.445672	16.444890
28.346876	915.877543	16.449907
28.220050	915.323163	16.454925
28.135199	906.339559	16.459943
27.920109	913.672510	16.464960
27.920343	922.038584	16.469978
28.241024	925.444421	16.474995
27.966996	931.363313	16.480013
28.334748	927.733966	16.485031
28.468044	926.580518	16.490048
28.638691	925.818879	16.495066
28.787330	921.014996	16.500083
28.416143	926.863809	16.505101
28.463568	923.666182	16.510119
28.535108	911.713911	16.515136
28.460540	913.060622	16.520154
28.259905	923.666994	16.525171
28.153403	930.093124	16.530189
28.370954	924.776747	16.535207
28.658985	928.689432	16.540224
28.382709	924.084247	16.545242
28.745481	926.555741	16.550259
28.398173	934.852857	16.555277
28.655007	944.087845	16.560295
28.774351	928.356995	16.565312
28.902995	924.922664	16.570330
28.977732	932.753288	16.575347
28.853812	938.828690	16.580365
28.818574	928.884312	16.585383
28.513266	925.700579	16.590400
28.611736	929.832123	16.595418
28.610706	926.566302	16.600435
28.780782	937.673532	16.605453
28.595715	930.018311	16.610471
28.755850	935.260547	16.615488
29.081545	956.533485	16.620506
29.252931	952.578106	16.625523
29.417274	950.693999	16.630541
29.216863	950.981038	16.635559
29.450510	940.937986	16.640576
29.154419	936.055021	16.645594
29.094835	939.614739	16.650611
29.423553	938.535004	16.655629
29.289656	934.096993	16.660647
29.200233	925.675815	16.665664
29.128873	931.761965	16.670682
29.756736	934.002841	16.675699
29.535742	936.833465	16.680717
29.631189	921.267285	16.685735
29.462819	915.401937	16.690752
29.108051	925.745135	16.695770
28.825909	934.158334	16.700787
29.342560	945.981612	16.705805
29.459473	940.264339	16.710823
29.381024	951.517568	16.715840
29.340803	958.403596	16.720858
29.585089	949.826309	16.725875
29.255896	949.783110	16.730893
29.364301	951.211787	16.735911
29.711917	951.814282	16.740928
29.759938	971.025581	16.745946
29.867393	967.916428	16.750963
29.885344	967.453113	16.755981
29.742634	964.335574	16.760999
30.154888	972.978343	16.766016
29.751673	966.070273	16.771034
30.082012	965.611968	16.776051
30.087967	972.834790	16.781069
29.797638	962.860683	16.786087
30.003627	964.365685	16.791104
29.901317	970.131624	16.796122
30.038661	964.745673	16.801139
30.159645	969.337617	16.806157
29.897323	974.153342	16.811175
29.881701	976.039982	16.816192
30.114455	975.079326	16.821210
30.592073	967.999400	16.826227
30.277142	967.748856	16.831245
30.103688	965.185206	16.836263
30.341558	972.444502	16.841280
30.235768	965.000982	16.846298
30.453469	965.825673	16.851315
30.392058	967.460669	16.856333
30.569884	968.222142	16.861351
30.616875	957.308751	16.866368
30.247596	965.773401	16.871386
30.286313	969.693355	16.876403
30.450617	967.888146	16.881421
30.290771	965.571682	16.886439
30.499560	969.629256	16.891456
30.082319	959.447696	16.896474
30.384815	973.910990	16.901491
30.365401	988.960896	16.906509
30.418751	992.364188	16.911527
31.128909	996.088090	16.916544
31.063188	990.036324	16.921562
30.960534	989.623343	16.926579
30.975132	992.003890	16.931597
30.749755	994.159873	16.936615
31.014494	992.739806	16.941632
30.883301	993.189636	16.946650
30.865714	984.416422	16.951667
30.954776	994.494900	16.956685
30.766656	987.360831	16.961703
30.980456	989.552575	16.966720
31.117333	997.976303	16.971738
30.882092	993.683443	16.976755
30.968679	993.263088	16.981773
30.647884	997.018120	16.986791
30.985670	978.665490	16.991808
30.639651	998.537763	16.996826
30.909488	1008.805851	17.001843
31.258030	1013.570658	17.006861
31.342332	1019.007760	17.011879
31.697210	1013.247103	17.016896
31.491592	1014.932958	17.021914
31.696198	1014.058732	17.026931
31.792766	1015.132656	17.031949
31.478012	1020.104877	17.036967
31.619857	1008.293072	17.041984
31.729379	1009.636374	17.047002
31.735252	1008.868829	17.052019
31.607757	1007.500363	17.057037
31.530562	1011.523579	17.062055
31.957785	1005.256205	17.067072
31.891167	1005.288887	17.072090
32.020958	1002.138382	17.077107
31.525810	988.563867	17.082125
31.797435	997.402110	17.087143
31.998879	1006.715181	17.092160
31.743637	1008.951554	17.097178
31.896649	1007.419495	17.102195
32.142244	1005.241869	17.107213
32.016938	1010.651644	17.112231
31.862777	999.536019	17.117248
31.834219	999.831016	17.122266
31.923716	1003.033024	17.127283
32.219953	1002.128754	17.132301
31.749668	1013.919549	17.137319
32.079377	1011.725670	17.142336
32.019318	1005.505761	17.147354
31.826154	1008.029110	17.152371
32.077797	1007.485228	17.157389
31.695743	1008.024608	17.162407
32.181332	1012.042251	17.167424
31.943405	1029.426766	17.172442
32.244316	1030.330022	17.177459
32.537996	1028.533065	17.182477
32.253083	1030.035610	17.187495
32.552372	1024.744346	17.192512
32.635049	1032.573777	17.197530
32.083708	1035.689377	17.202547
32.393809	1034.950202	17.207565
32.678429	1032.390960	17.212583
32.762054	1030.601462	17.217600
32.329314	1039.820789	17.222618
31.886056	1037.466391	17.227635
31.879872	1030.774188	17.232653
32.393210	1041.089588	17.237671
33.020577	1052.065731	17.242688
32.805632	1040.647123	17.247706
33.281355	1051.100928	17.252723
33.321500	1050.018779	17.257741
32.834399	1040.510762	17.262759
32.895236	1030.229480	17.267776
32.999058	1037.392911	17.272794
33.041569	1038.876035	17.277811
33.079208	1041.518086	17.282829
32.849510	1045.445135	17.287847
33.143201	1052.209784	17.292864
33.290631	1045.537838	17.297882
33.356694	1052.268501	17.302899
33.167791	1047.125822	17.307917
33.217991	1052.969028	17.312935
33.142048	1050.623710	17.317952
33.099696	1045.893711	17.322970
33.260726	1047.639247	17.327987
33.543356	1039.194801	17.333005
33.350844	1049.850475	17.338023
33.664624	1035.320009	17.343040
33.607142	1042.398103	17.348058
33.347758	1050.769945	17.353075
33.533654	1038.828186	17.358093
33.131630	1042.397060	17.363111
33.442232	1047.953570	17.368128
33.607298	1047.634604	17.373146
33.533994	1042.587536	17.378163
33.517467	1044.995026	17.383181
33.430215	1049.821383	17.388199
33.455924	1040.706888	17.393216
33.334204	1045.810006	17.398234
33.768596	1064.689854	17.403251
33.989684	1069.906861	17.408269
34.017685	1067.365478	17.413287
33.967944	1071.835709	17.418304
34.262800	1074.557637	17.423322
33.771614	1074.501790	17.428339
34.417040	1064.817430	17.433357
34.229597	1077.350018	17.438375
34.375509	1058.266638	17.443392
34.006610	1047.077121	17.448410
33.732530	1046.646648	17.453427
33.976220	1054.719261	17.458445
33.761421	1082.056691	17.463463
34.160432	1072.574793	17.468480
34.257046	1067.551755	17.473498
34.070790	1064.838606	17.478515
34.300231	1055.493570	17.483533
34.095579	1067.255666	17.488551
34.212348	1064.406976	17.493568
34.281564	1072.983283	17.498586
34.453685	1074.862794	17.503603
34.725364	1081.886499	17.508621
34.214178	1072.909229	17.513639
34.718025	1093.204704	17.518656
34.778988	1087.391955	17.523674
34.659062	1100.062368	17.528691
34.473768	1093.707294	17.533709
34.829974	1102.895335	17.538727
34.758721	1088.595186	17.543744
35.029562	1095.578003	17.548762
34.902344	1098.801147	17.553779
35.124086	1085.118097	17.558797
34.614298	1079.350032	17.563815
34.591365	1076.548337	17.568832
34.477668	1085.771662	17.573850
34.608923	1092.571085	17.578867
35.056568	1089.241688	17.583885
35.133376	1094.222393	17.588903
35.216169	1083.369622	17.593920
35.338418	1093.162124	17.598938
35.144606	1098.263859	17.603955
35.196690	1086.607987	17.608973
35.103287	1085.281544	17.613991
35.034814	1089.022555	17.619008
35.350491	1083.148059	17.624026
34.935208	1094.346524	17.629043
35.039599	1084.497084	17.634061
35.278041	1100.923881	17.639079
36.024357	1092.012744	17.644096
36.030570	1091.425021	17.649114
35.810259	1085.154297	17.654131
35.947425	1074.984181	17.659149
35.997724	1081.486937	17.664167
35.867669	1082.659265	17.669184
35.903297	1072.590165	17.674202
35.775228	1080.089516	17.679219
35.667813	1071.169301	17.684237
35.958066	1068.940533	17.689255
35.964657	1071.458036	17.694272
35.943065	1070.694764	17.699290
35.704171	1080.991609	17.704307
36.040144	1073.577092	17.709325
35.525498	1080.095224	17.714343
35.738163	1068.259730	17.719360
35.778501	1063.362219	17.724378
35.629704	1072.407967	17.729395
35.741629	1070.235366	17.734413
35.627461	1074.822925	17.739431
36.111181	1088.175666	17.744448
36.260446	1086.849309	17.749466
35.945675	1104.286886	17.754483
36.234911	1095.510028	17.759501
36.386871	1095.660156	17.764519
36.435155	1096.325040	17.769536
36.642858	1093.986046	17.774554
36.138769	1097.839063	17.779571
36.339071	1093.137543	17.784589
36.142290	1094.304481	17.789607
36.123286	1104.671244	17.794624
36.444624	1096.488986	17.799642
36.192072	1096.339180	17.804659
36.575593	1089.523163	17.809677
36.902911	1110.149098	17.814695
36.747155	1110.369227	17.819712
36.691218	1099.765262	17.824730
36.479672	1102.569194	17.829747
36.756372	1106.420568	17.834765
37.084911	1115.593989	17.839783
36.849450	1116.019031	17.844800
37.244501	1114.897400	17.849818
37.211804	1115.316118	17.854835
36.904108	1101.863808	17.859853
36.626915	1103.791187	17.864871
36.705022	1112.612281	17.869888
37.005003	1112.385916	17.874906
37.275724	1121.331658	17.879923
37.245884	1126.764475	17.884941
37.440373	1122.534063	17.889959
37.218646	1120.807877	17.894976
37.473039	1113.062065	17.899994
37.253433	1122.112552	17.905011
37.549093	1112.078683	17.910029
37.007987	1117.868807	17.915047
37.307991	1121.031751	17.920064
37.514738	1112.453918	17.925082
37.435038	1118.478315	17.930099
37.479372	1115.028672	17.935117
37.562579	1108.070059	17.940135
37.262341	1119.610388	17.945152
37.304127	1110.098882	17.950170
37.318466	1117.718086	17.955187
37.332371	1117.624624	17.960205
37.327789	1123.605769	17.965223
37.625969	1135.996517	17.970240
37.863162	1136.474200	17.975258
37.602567	1148.544859	17.980275
38.146022	1141.994254	17.985293
38.187990	1146.709000	17.990311
37.942621	1142.487108	17.995328
37.953587	1134.110160	18.000346
38.264701	1141.661077	18.005363
38.315108	1135.505975	18.010381
38.099254	1143.489232	18.015399
37.991853	1144.837917	18.020416
38.453124	1137.015703	18.025434
38.133907	1140.164607	18.030451
38.279546	1138.368599	18.035469
38.206356	1133.946333	18.040487
38.366804	1140.296263	18.045504
38.624417	1126.970511	18.050522
38.308592	1141.359800	18.055539
38.457210	1145.622442	18.060557
38.491864	1137.071391	18.065575
38.293704	1136.272492	18.070592
38.218693	1135.921475	18.075610
38.327495	1145.577246	18.080627
38.327239	1134.753153	18.085645
38.425001	1133.018248	18.090663
38.359307	1156.088045	18.095680
38.815345	1162.164743	18.100698
38.863412	1160.260849	18.105715
38.573004	1162.436443	18.110733
38.621306	1157.057986	18.115751
38.830805	1158.855947	18.120768
38.811600	1154.605151	18.125786
38.798421	1159.328486	18.130803
38.945025	1157.750075	18.135821
38.624701	1159.677864	18.140839
38.399327	1165.674465	18.145856
38.963957	1168.272354	18.150874
39.263294	1186.507487	18.155891
39.182311	1184.797251	18.160909
39.017464	1186.031807	18.165927
39.172823	1184.966425	18.170944
39.150008	1177.206941	18.175962
38.917686	1186.366737	18.180979
39.330233	1184.163096	18.185997
39.236366	1181.615424	18.191015
39.324501	1192.268513	18.196032
39.728927	1196.008502	18.201050
39.967572	1200.452800	18.206067
39.523805	1193.074429	18.211085
39.770147	1184.698680	18.216103
39.445530	1179.763285	18.221120
39.593981	1192.944243	18.226138
39.527017	1202.245558	18.231155
39.479470	1200.179821	18.236173
40.104610	1198.059843	18.241191
39.655592	1198.606499	18.246208
40.076276	1192.576762	18.251226
40.055897	1201.400611	18.256243
39.965231	1204.895794	18.261261
40.173217	1199.852222	18.266279
40.267423	1201.368337	18.271296
40.212215	1198.745217	18.276314
40.185263	1201.832848	18.281331
40.103392	1201.899464	18.286349
40.303632	1199.473256	18.291367
39.996101	1194.692986	18.296384
40.348583	1198.046588	18.301402
40.487833	1197.015272	18.306419
40.415589	1196.708005	18.311437
40.967514	1192.115814	18.316455
40.343605	1196.561862	18.321472
40.426595	1191.758661	18.326490
40.582720	1189.591787	18.331507
40.483924	1200.763134	18.336525
40.535050	1193.172011	18.341543
40.485657	1192.649747	18.346560
40.432424	1201.955237	18.351578
40.661834	1198.265324	18.356595
40.753906	1196.752204	18.361613
41.008985	1182.921878	18.366631
40.632933	1195.026323	18.371648
40.676696	1193.577530	18.376666
40.753938	1197.264319	18.381683
40.884779	1220.776969	18.386701
41.096965	1222.356768	18.391719
40.850035	1218.674743	18.396736
41.026846	1217.192610	18.401754
41.064826	1221.731271	18.406771
41.031315	1222.916979	18.411789
41.111717	1216.422663	18.416807
41.065785	1218.421346	18.421824
41.083050	1213.751447	18.426842
41.271075	1213.015493	18.431859
41.357518	1213.750179	18.436877
41.219448	1212.064608	18.441895
41.822913	1221.977918	18.446912
41.629622	1215.295842	18.451930
41.464544	1207.116682	18.456947
40.879468	1218.862369	18.461965
41.955405	1230.926963	18.466983
41.695798	1231.999550	18.472000
41.635142	1236.408406	18.477018
41.898517	1241.606257	18.482035
41.788544	1237.795607	18.487053
41.988763	1240.137819	18.492071
42.111157	1242.782483	18.497088
42.307555	1236.459449	18.502106
42.246241	1240.896810	18.507123
42.014632	1234.034500	18.512141
42.249049	1225.054675	18.517159
41.845490	1229.084572	18.522176
42.066760	1229.662567	18.527194
42.035025	1228.156098	18.532211
41.781941	1233.775184	18.537229
42.267413	1232.926646	18.542247
41.921795	1228.786613	18.547264
41.981100	1222.002090	18.552282
42.151039	1219.675272	18.557299
42.081752	1228.901224	18.562317
42.351502	1235.511881	18.567335
42.551761	1250.647726	18.572352
42.784025	1251.984560	18.577370
42.291612	1246.617679	18.582387
42.279684	1242.829632	18.587405
42.940534	1249.985317	18.592423
42.842353	1248.766902	18.597440
42.634477	1245.504825	18.602458
42.895578	1240.232066	18.607475
42.639535	1245.330908	18.612493
42.726104	1242.382750	18.617511
42.558123	1240.865935	18.622528
42.549149	1245.333018	18.627546
43.084490	1244.309457	18.632563
42.690670	1242.591119	18.637581
42.788265	1248.057780	18.642599
43.188431	1264.194461	18.647616
43.425564	1259.225230	18.652634
43.693073	1259.164865	18.657651
43.296615	1260.145153	18.662669
43.315895	1242.864323	18.667687
43.103693	1245.248658	18.672704
43.251433	1257.710251	18.677722
43.879831	1259.824854	18.682739
43.649990	1252.428931	18.687757
43.619948	1241.527359	18.692775
43.308218	1239.127209	18.697792
43.699874	1253.403280	18.702810
43.827458	1262.835284	18.707827
43.728638	1255.598840	18.712845
43.758633	1257.655133	18.717863
43.628704	1258.565520	18.722880
44.077785	1261.414944	18.727898
44.296151	1260.080972	18.732915
43.707430	1248.202873	18.737933
43.968600	1257.816046	18.742951
43.730165	1262.886906	18.747968
43.917154	1256.073023	18.752986
43.971555	1263.389406	18.758003
43.460936	1267.820989	18.763021
43.766607	1260.098688	18.768039
43.972318	1264.762724	18.773056
44.100453	1272.234889	18.778074
44.378813	1274.075789	18.783091
44.215547	1290.161362	18.788109
44.225052	1288.569572	18.793127
44.395251	1286.583532	18.798144
44.390040	1289.961284	18.803162
44.580465	1284.860463	18.808179
44.352707	1284.451174	18.813197
44.912450	1280.981213	18.818215
44.355554	1284.410145	18.823232
44.198661	1283.459646	18.828250
44.682375	1273.263864	18.833267
44.265227	1276.996085	18.838285
44.769930	1295.202511	18.843303
44.925923	1291.161091	18.848320
45.227345	1309.105690	18.853338
45.003031	1303.952670	18.858355
45.014186	1311.935373	18.863373
45.137295	1313.153506	18.868391
45.085815	1314.228408	18.873408
45.068171	1305.994690	18.878426
45.127698	1307.781302	18.883443
45.125872	1308.681214	18.888461
45.173730	1308.913825	18.893479
45.225385	1305.844860	18.898496
44.950934	1297.973022	18.903514
45.506470	1297.340792	18.908531
45.218193	1308.967743	18.913549
45.115677	1300.968149	18.918567
45.624170	1300.437917	18.923584
45.106396	1302.437488	18.928602
45.380751	1311.004063	18.933619
45.555260	1329.151479	18.938637
45.702608	1319.658140	18.943655
45.725022	1324.861974	18.948672
45.705784	1322.391026	18.953690
46.129150	1317.029864	18.958707
45.999184	1328.310286	18.963725
45.952178	1322.583698	18.968743
45.820100	1321.351621	18.973760
45.810484	1333.537964	18.978778
46.367628	1323.687328	18.983795
46.110736	1322.320049	18.988813
46.086216	1322.260970	18.993831
46.099300	1322.950278	18.998848
45.850646	1325.280338	19.003866
46.188539	1317.489879	19.008883
45.785033	1321.829058	19.013901
46.215264	1341.789140	19.018919
46.835003	1338.496020	19.023936
46.555650	1345.144873	19.028954
46.929447	1350.092033	19.033971
46.609420	1330.803193	19.038989
46.514341	1320.801641	19.044007
46.521762	1332.388880	19.049024
46.414819	1347.831416	19.054042
46.634436	1340.138257	19.059059
46.688463	1344.772282	19.064077
46.675050	1342.237308	19.069095
47.150112	1342.920961	19.074112
46.881094	1340.485744	19.079130
47.005752	1339.466160	19.084147
47.168693	1351.142807	19.089165
46.982349	1349.010300	19.094183
47.220834	1340.058185	19.099200
46.838308	1343.630395	19.104218
47.081360	1333.699267	19.109235
46.883922	1347.316047	19.114253
46.937144	1354.418055	19.119271
47.513462	1359.437828	19.124288
47.533501	1367.245601	19.129306
47.563008	1364.700786	19.134323
47.603721	1364.634706	19.139341
47.465607	1357.019328	19.144359
47.819905	1359.340723	19.149376
47.431795	1361.203347	19.154394
47.657321	1352.423659	19.159411
47.851047	1361.753898	19.164429
47.783169	1359.145350	19.169447
48.015356	1347.773694	19.174464
47.803569	1350.606105	19.179482
47.972018	1354.701606	19.184499
47.948669	1357.447874	19.189517
48.003852	1365.348006	19.194535
48.113845	1360.616294	19.199552
47.933530	1358.009473	19.204570
47.919662	1355.957409	19.209587
48.160407	1365.232992	19.214605
47.850180	1367.967122	19.219623
48.372258	1374.614285	19.224640
48.441639	1381.584399	19.229658
48.504976	1376.610636	19.234675
48.696118	1385.531032	19.239693
48.875221	1382.483236	19.244711
48.405199	1361.914358	19.249728
48.431273	1363.232810	19.254746
48.713532	1362.867190	19.259763
48.458958	1375.312608	19.264781
48.746567	1377.978906	19.269799
48.929725	1369.395156	19.274816
48.826795	1379.383823	19.279834
48.815660	1379.161713	19.284851
49.028553	1371.188719	19.289869
48.652604	1371.897573	19.294887
49.058438	1368.997517	19.299904
49.036141	1381.656085	19.304922
48.908770	1373.152239	19.309939
48.872497	1367.414498	19.314957
48.706807	1375.468944	19.319975
49.239032	1373.413906	19.324992
49.202551	1381.823781	19.330010
49.135126	1392.472808	19.335027
49.108647	1396.759616	19.340045
49.438548	1405.822522	19.345063
49.478946	1396.516208	19.350080
49.218094	1399.201630	19.355098
49.580160	1392.429865	19.360115
49.588908	1403.508855	19.365133
49.487995	1402.167778	19.370151
49.365363	1402.209182	19.375168
49.663647	1405.845820	19.380186
49.899130	1421.787376	19.385203
49.959333	1417.931257	19.390221
49.766572	1415.752403	19.395239
50.211535	1419.142142	19.400256
49.825025	1424.662139	19.405274
49.734943	1410.241586	19.410291
50.003408	1409.142802	19.415309
50.147803	1417.148988	19.420327
50.315524	1408.113182	19.425344
49.932620	1418.006605	19.430362
49.988489	1423.249440	19.435379
50.398255	1433.518078	19.440397
50.374521	1442.184776	19.445415
50.871399	1440.880013	19.450432
50.825031	1436.450340	19.455450
50.831242	1441.874483	19.460467
50.488085	1442.653975	19.465485
50.775209	1446.724709	19.470503
50.835306	1440.078837	19.475520
50.889198	1445.842700	19.480538
50.876787	1443.449569	19.485555
50.802947	1442.893234	19.490573
50.876779	1448.688708	19.495591
51.015139	1442.156884	19.500608
50.692051	1443.567575	19.505626
50.487710	1449.526281	19.510643
51.206867	1441.401849	19.515661
50.534665	1446.240490	19.520679
51.153770	1448.962486	19.525696
51.281798	1459.663174	19.530714
51.150347	1458.885431	19.535731
51.265722	1460.130026	19.540749
51.269475	1461.887467	19.545767
51.484628	1456.265188	19.550784
51.405439	1468.983170	19.555802
51.380792	1454.154756	19.560819
51.388059	1449.312781	19.565837
51.719116	1471.522786	19.570855
51.851562	1475.532401	19.575872
52.155506	1477.725951	19.580890
52.136720	1470.915621	19.585907
51.958519	1458.926127	19.590925
52.146956	1453.093411	19.595943
52.128022	1444.004596	19.600960
52.213502	1446.244779	19.605978
52.028827	1451.064321	19.610995
52.111728	1445.588870	19.616013
51.598047	1456.105441	19.621031
52.118989	1465.043957	19.626048
52.249082	1475.476085	19.631066
52.481202	1477.980623	19.636083
52.565013	1480.126394	19.641101
52.313337	1477.325535	19.646119
52.573577	1472.513596	19.651136
52.776647	1479.901597	19.656154
52.171532	1477.588118	19.661171
52.555891	1470.014424	19.666189
52.595546	1474.641253	19.671207
52.744438	1476.660124	19.676224
52.382663	1480.336428	19.681242
52.817439	1486.943576	19.686259
53.334276	1490.366320	19.691277
53.252353	1489.666073	19.696295
52.910484	1497.303029	19.701312
53.046323	1496.673021	19.706330
53.269791	1498.888570	19.711347
53.574546	1492.595912	19.716365
53.388502	1496.289041	19.721383
53.413046	1484.788678	19.726400
53.135361	1488.941048	19.731418
53.111859	1494.568652	19.736435
53.275508	1484.239543	19.741453
53.583957	1491.159855	19.746471
53.634953	1492.417631	19.751488
53.636923	1496.024682	19.756506
53.594484	1494.892247	19.761523
53.813792	1487.404204	19.766541
53.516846	1494.885840	19.771559
53.986837	1492.010489	19.776576
53.927336	1488.952487	19.781594
53.798315	1489.749134	19.786611
53.784325	1498.669966	19.791629
53.683982	1512.063468	19.796647
54.114045	1512.223951	19.801664
54.217513	1520.548986	19.806682
54.138776	1514.334963	19.811699
53.990940	1516.712468	19.816717
54.149699	1519.168472	19.821735
54.350011	1510.190657	19.826752
54.385909	1514.177443	19.831770
54.489930	1508.951153	19.836787
54.283166	1513.310241	19.841805
54.492401	1532.834722	19.846823
54.950953	1526.234080	19.851840
54.787659	1535.064565	19.856858
54.466704	1538.204342	19.861875
55.210522	1527.134772	19.866893
54.933311	1534.196778	19.871911
55.250584	1529.912440	19.876928
54.852866	1535.513113	19.881946
55.100105	1533.963183	19.886963
54.889933	1535.267936	19.891981
54.725572	1542.369181	19.896999
54.850458	1532.320639	19.902016
54.906030	1530.005276	19.907034
54.929335	1526.561983	19.912051
55.250779	1531.529968	19.917069
55.308002	1545.227173	19.922087
55.643685	1556.479421	19.927104
55.825126	1550.483659	19.932122
55.632219	1555.452836	19.937139
55.879495	1548.250752	19.942157
55.790367	1535.780270	19.947175
55.984089	1530.113967	19.952192
55.865299	1521.176362	19.957210
55.351777	1524.058934	19.962227
55.986915	1526.503887	19.967245
55.581237	1545.445612	19.972263
55.872501	1544.254906	19.977280
55.914199	1545.226951	19.982298
56.013806	1548.399081	19.987315
56.133913	1550.056363	19.992333
56.059178	1549.569593	19.997351
56.105807	1543.683186	20.002368
56.232365	1538.447067	20.007386
55.729951	1539.282916	20.012403
56.212839	1548.817545	20.017421
56.361091	1567.572062	20.022439
56.677795	1572.581823	20.027456
56.606398	1561.557104	20.032474
56.546219	1571.870588	20.037491
57.053278	1565.685265	20.042509
56.757634	1567.120095	20.047527
56.860594	1562.301061	20.052544
57.177757	1565.537154	20.057562
56.920657	1567.565597	20.062579
56.998384	1554.415860	20.067597
57.040361	1561.696429	20.072615
57.366228	1563.832926	20.077632
57.221253	1555.334890	20.082650
57.043871	1561.437762	20.087667
57.065998	1560.781274	20.092685
57.247148	1581.547279	20.097703
57.360759	1583.751541	20.102720
57.567665	1576.183339	20.107738
57.309263	1590.254773	20.112755
57.426066	1590.366198	20.117773
57.046946	1593.524507	20.122791
57.536962	1593.101289	20.127808
57.582151	1584.946023	20.132826
57.931683	1604.559195	20.137843
58.114514	1603.511603	20.142861
58.082270	1591.859063	20.147879
57.924719	1591.344160	20.152896
58.067174	1595.087151	20.157914
58.018406	1611.331915	20.162931
57.998589	1605.294884	20.167949
58.166670	1604.565175	20.172967
58.252341	1607.717395	20.177984
58.326986	1602.448313	20.183002
58.270295	1599.778026	20.188019
58.344456	1600.199054	20.193037
58.221886	1604.396729	20.198055
58.402963	1606.000341	20.203072
58.377688	1601.437952	20.208090
58.624115	1625.554848	20.213107
58.566167	1633.122409	20.218125
59.103361	1634.913581	20.223143
59.095769	1635.328403	20.228160
58.842199	1632.007095	20.233178
58.984558	1632.079827	20.238195
58.976794	1635.413860	20.243213
58.636769	1633.762847	20.248231
58.716526	1633.293048	20.253248
59.128772	1629.625074	20.258266
59.183472	1635.063818	20.263283
59.136933	1626.679813	20.268301
59.180806	1630.599110	20.273319
59.429882	1645.128074	20.278336
59.848329	1647.944460	20.283354
59.611113	1655.688269	20.288371
60.003491	1654.851051	20.293389
59.633858	1645.034078	20.298407
59.660135	1642.085774	20.303424
59.563806	1642.725855	20.308442
59.523075	1653.197308	20.313459
59.652107	1647.736704	20.318477
59.629897	1645.629100	20.323495
59.388885	1647.232160	20.328512
59.956219	1647.544845	20.333530
60.062217	1659.397822	20.338547
60.173614	1671.183693	20.343565
60.410095	1672.280056	20.348583
60.618835	1667.485551	20.353600
60.503364	1655.337830	20.358618
60.560889	1662.423512	20.363635
60.716760	1651.783085	20.368653
61.004035	1659.874435	20.373671
60.616903	1653.291803	20.378688
60.537291	1644.960276	20.383706
60.540296	1658.514527	20.388723
60.837294	1655.741826	20.393741
60.866048	1657.280794	20.398759
60.700276	1656.896560	20.403776
60.985895	1651.130702	20.408794
60.780124	1656.925594	20.413811
60.636304	1664.566501	20.418829
61.124530	1665.166065	20.423847
61.188894	1680.462293	20.428864
61.398759	1683.292225	20.433882
61.604480	1686.255350	20.438899
61.019865	1688.378981	20.443917
61.337196	1691.293170	20.448935
61.311837	1694.194442	20.453952
61.546358	1688.483866	20.458970
61.337301	1684.111020	20.463987
61.582973	1693.436501	20.469005
61.428988	1687.931585	20.474023
61.271797	1700.425184	20.479040
61.918504	1696.076892	20.484058
62.062424	1697.323371	20.489075
62.232832	1713.833912	20.494093
62.513213	1712.111545	20.499111
61.974073	1714.265970	20.504128
62.637968	1700.008666	20.509146
62.205979	1711.891789	20.514163
62.165143	1705.832749	20.519181
62.165564	1709.963962	20.524199
62.482234	1711.628526	20.529216
62.448718	1701.229001	20.534234
62.369621	1714.613035	20.539251
62.456685	1712.835557	20.544269
62.429013	1712.638109	20.549287
62.691610	1734.896972	20.554304
63.192332	1732.831019	20.559322
63.002987	1728.515055	20.564339
63.017519	1739.186243	20.569357
62.873758	1740.269226	20.574375
62.832819	1738.278139	20.579392
62.773409	1744.047116	20.584410
62.901929	1733.177363	20.589427
62.842187	1735.317113	20.594445
63.264398	1738.344372	20.599463
63.134895	1753.828642	20.604480
63.314928	1757.527946	20.609498
63.465551	1759.533957	20.614515
63.765790	1757.584425	20.619533
63.914207	1747.693049	20.624551
63.676160	1757.090720	20.629568
64.220958	1747.992878	20.634586
64.339993	1753.090273	20.639603
64.005156	1747.913305	20.644621
64.162673	1739.996108	20.649639
63.682612	1733.853960	20.654656
63.584049	1740.244431	20.659674
63.915201	1744.709178	20.664691
64.029280	1747.273159	20.669709
64.199363	1741.260165	20.674727
64.060961	1753.940230	20.679744
64.259492	1745.966150	20.684762
64.319103	1742.444578	20.689779
64.170124	1757.395381	20.694797
64.462303	1756.545356	20.699815
64.576631	1761.615083	20.704832
64.820030	1764.335662	20.709850
64.674153	1763.639049	20.714867
64.358526	1766.822218	20.719885
64.918416	1772.179193	20.724903
64.771043	1773.186999	20.729920
64.536816	1772.794484	20.734938
64.979278	1786.829537	20.739955
65.005425	1796.160848	20.744973
65.258064	1791.990656	20.749991
65.179051	1793.186641	20.755008
65.318646	1789.352796	20.760026
65.160927	1792.167391	20.765043
65.350161	1783.049149	20.770061
65.618921	1781.401170	20.775079
65.406522	1800.013261	20.780096
65.721972	1802.839397	20.785114
65.898684	1812.327160	20.790131
65.893369	1809.904472	20.795149
66.381109	1807.638554	20.800167
66.357207	1817.495237	20.805184
66.153353	1814.295547	20.810202
66.075666	1808.545176	20.815219
66.267204	1814.991496	20.820237
66.485749	1809.485347	20.825255
66.161553	1809.627564	20.830272
66.517884	1799.366107	20.835290
66.394531	1810.699454	20.840307
66.304414	1807.062321	20.845325
66.699461	1804.346917	20.850343
66.646354	1807.807967	20.855360
66.793782	1807.195079	20.860378
66.925529	1801.036550	20.865395
66.821235	1808.156952	20.870413
66.978758	1793.363011	20.875431
67.076560	1801.446055	20.880448
66.718483	1804.970365	20.885466
66.754026	1799.372788	20.890483
66.745481	1799.115554	20.895501
67.025002	1808.139170	20.900519
67.117886	1825.198389	20.905536
67.003400	1820.514130	20.910554
67.104601	1825.661660	20.915571
67.327500	1824.323786	20.920589
67.333726	1823.281586	20.925607
67.266397	1832.008911	20.930624
67.381427	1846.836630	20.935642
67.763238	1847.850415	20.940659
67.918216	1853.169468	20.945677
67.849355	1852.514511	20.950695
68.029601	1853.221996	20.955712
67.611815	1851.267478	20.960730
68.087527	1844.739790	20.965747
68.005289	1848.520974	20.970765
68.542766	1843.788852	20.975783
67.648761	1845.761849	20.980800
68.056044	1852.057822	20.985818
68.113789	1853.986783	20.990835
68.116518	1872.385568	20.995853
68.377013	1879.120986	21.000871
68.437820	1869.776534	21.005888
68.832628	1864.971942	21.010906
69.160435	1856.829357	21.015923
68.887603	1868.829820	21.020941
69.107926	1859.343769	21.025959
69.176588	1866.049087	21.030976
69.006670	1862.354938	21.035994
69.027668	1865.675068	21.041011
69.089608	1868.228249	21.046029
69.420331	1860.261939	21.051047
69.199825	1866.324290	21.056064
69.269485	1862.880028	21.061082
69.559884	1855.734225	21.066099
69.415859	1865.060508	21.071117
69.584642	1860.799210	21.076135
69.537364	1874.916895	21.081152
69.645302	1880.325333	21.086170
69.978362	1885.714502	21.091187
69.790228	1872.956231	21.096205
69.822728	1870.439281	21.101223
70.069081	1880.140308	21.106240
69.628473	1881.332635	21.111258
70.491804	1881.138477	21.116275
69.751959	1888.944863	21.121293
70.281227	1877.463498	21.126311
70.163438	1887.107611	21.131328
70.157465	1901.449268	21.136346
70.670175	1908.921786	21.141363
70.274374	1919.211983	21.146381
69.930707	1907.639283	21.151399
70.126205	1916.474057	21.156416
70.242339	1921.373128	21.161434
70.859918	1929.413174	21.166451
70.727151	1935.963680	21.171469
71.050392	1930.523248	21.176487
70.924472	1935.826097	21.181504
70.960473	1932.746838	21.186522
71.042170	1924.112344	21.191539
70.970125	1928.964973	21.196557
71.115437	1939.458122	21.201575
71.159529	1955.821291	21.206592
71.280963	1953.552424	21.211610
72.031079	1950.611297	21.216627
71.389478	1957.203162	21.221645
72.149380	1940.699476	21.226663
72.427714	1934.085717	21.231680
72.220414	1942.055374	21.236698
72.452398	1935.007001	21.241715
72.172811	1933.040425	21.246733
72.159491	1924.307111	21.251751
72.321503	1910.414970	21.256768
71.905383	1909.403808	21.261786
72.265128	1916.796000	21.266803
72.471943	1923.173706	21.271821
72.666073	1925.305510	21.276839
72.996869	1933.945652	21.281856
72.777851	1929.299731	21.286874
72.239362	1906.490706	21.291891
72.335541	1914.820216	21.296909
72.530466	1926.949870	21.301927
72.751222	1918.322132	21.306944
72.591135	1923.286301	21.311962
73.006011	1921.710239	21.316979
72.734689	1928.105583	21.321997
72.678148	1925.125943	21.327015
72.757029	1935.001403	21.332032
72.749676	1950.817133	21.337050
73.031819	1951.180540	21.342067
73.158622	1956.633404	21.347085
73.256246	1951.341706	21.352103
73.229888	1955.808517	21.357120
73.598625	1973.121587	21.362138
73.787726	1991.324212	21.367155
73.772713	1983.402210	21.372173
74.146719	1991.893635	21.377191
73.874580	1986.615314	21.382208
73.757051	1985.434576	21.387226
74.034382	1975.251593	21.392243
74.142775	1978.037408	21.397261
74.260543	1980.960625	21.402279
74.281997	1979.934981	21.407296
73.919407	1980.442953	21.412314
74.187327	1984.362161	21.417331
74.119208	1994.235293	21.422349
74.372368	2000.634214	21.427367
74.678765	1999.277015	21.432384
74.526232	2001.147208	21.437402
74.634023	1996.554533	21.442419
74.619937	1999.656079	21.447437
74.800529	2000.111041	21.452455
75.013539	2007.409347	21.457472
74.912096	2010.537119	21.462490
75.030165	2018.008008	21.467507
75.130702	2028.782748	21.472525
75.071236	2015.770802	21.477543
75.511511	2020.063988	21.482560
75.323166	2026.601089	21.487578
75.686762	2012.999389	21.492595
75.451151	2018.783264	21.497613
75.795119	2037.570922	21.502631
76.211034	2039.081204	21.507648
75.807032	2047.296138	21.512666
76.344985	2035.213690	21.517683
75.998490	2033.569958	21.522701
75.817738	2039.083355	21.527719
75.910061	2037.529099	21.532736
75.739327	2048.759515	21.537754
76.218636	2044.948467	21.542771
76.005719	2047.834814	21.547789
75.908767	2046.272155	21.552807
76.154343	2058.829534	21.557824
76.282671	2068.104050	21.562842
76.491846	2062.473045	21.567859
76.442907	2068.751760	21.572877
76.629962	2065.727859	21.577895
77.097776	2076.325518	21.582912
77.140112	2082.037735	21.587930
77.525104	2081.877024	21.592947
77.806916	2076.906923	21.597965
77.395113	2069.813557	21.602983
77.214432	2059.730240	21.608000
77.297068	2056.091407	21.613018
77.563029	2060.932474	21.618035
77.667369	2072.688149	21.623053
77.525146	2066.379672	21.628071
77.635713	2066.110201	21.633088
77.719213	2083.063825	21.638106
77.790058	2072.105011	21.643123
78.013221	2074.983431	21.648141
77.963210	2074.821016	21.653159
78.024522	2073.915399	21.658176
77.672997	2074.598384	21.663194
78.070043	2067.928222	21.668211
78.207541	2071.312307	21.673229
77.671105	2069.262623	21.678247
78.131249	2089.626004	21.683264
78.050518	2095.104909	21.688282
78.620738	2101.340888	21.693299
78.893196	2099.199976	21.698317
78.402359	2110.246728	21.703335
78.829394	2099.828917	21.708352
78.405870	2103.726410	21.713370
78.534288	2108.961308	21.718387
78.521117	2118.813330	21.723405
78.954214	2122.883585	21.728423
78.940406	2116.842289	21.733440
79.090577	2130.935746	21.738458
78.992208	2139.929999	21.743475
79.473291	2134.730031	21.748493
79.676433	2139.025450	21.753511
80.241636	2145.432648	21.758528
79.953132	2143.678885	21.763546
79.891563	2132.724871	21.768563
79.618852	2140.591186	21.773581
79.513206	2146.541069	21.778599
80.188508	2140.057943	21.783616
80.000550	2139.803390	21.788634
80.094624	2137.756522	21.793651
80.349913	2153.648310	21.798669
80.150666	2160.518533	21.803687
80.520560	2163.525609	21.808704
80.400697	2170.437128	21.813722
80.596955	2167.042528	21.818739
80.658826	2163.731971	21.823757
80.754317	2164.001361	21.828775
80.984692	2159.329595	21.833792
80.672934	2164.595170	21.838810
80.711643	2168.550105	21.843827
80.970240	2164.950130	21.848845
80.992197	2174.509520	21.853863
81.404585	2175.370233	21.858880
81.422884	2187.524409	21.863898
81.367385	2184.601371	21.868915
81.684810	2186.104908	21.873933
81.213019	2186.945485	21.878951
81.557407	2180.876802	21.883968
81.592483	2184.371534	21.888986
81.200629	2185.007150	21.894003
82.014206	2186.559679	21.899021
82.258671	2199.208853	21.904039
82.165389	2201.887240	21.909056
82.276098	2205.632146	21.914074
82.158376	2207.831475	21.919091
82.449871	2208.830939	21.924109
82.350457	2198.880065	21.929127
82.537520	2200.141954	21.934144
82.531390	2204.927588	21.939162
82.640359	2207.429311	21.944179
82.560131	2204.175587	21.949197
82.329772	2211.028582	21.954215
82.799499	2200.228505	21.959232
82.292198	2203.410033	21.964250
82.635928	2214.112305	21.969267
82.897094	2220.402756	21.974285
82.866557	2225.498325	21.979303
83.355672	2230.008032	21.984320
83.129597	2230.867161	21.989338
83.226852	2236.195315	21.994355
83.360432	2231.541757	21.999373
83.271926	2244.413228	22.004391
83.251046	2246.505960	22.009408
83.123160	2252.292073	22.014426
83.630935	2254.248846	22.019443
83.649754	2255.063536	22.024461
83.423260	2269.206278	22.029479
83.862027	2263.245957	22.034496
84.043700	2266.279199	22.039514
83.986281	2277.066058	22.044531
84.223989	2271.900787	22.049549
83.637166	2283.890450	22.054567
84.109656	2287.743158	22.059584
84.292464	2295.803722	22.064602
84.623743	2297.077881	22.069619
84.616429	2293.071130	22.074637
84.320290	2307.862256	22.079655
84.908206	2317.800694	22.084672
84.760404	2318.777036	22.089690
84.835472	2322.555921	22.094707
85.246556	2316.167521	22.099725
85.304713	2320.715945	22.104743
85.564524	2313.413767	22.109760
85.532188	2322.107479	22.114778
85.455521	2322.457327	22.119795
85.654063	2324.806257	22.124813
85.665344	2343.270470	22.129831
86.198949	2336.073987	22.134848
86.207576	2338.386212	22.139866
86.045979	2349.353445	22.144883
86.405832	2344.134421	22.149901
86.441692	2343.917606	22.154919
86.440029	2338.909512	22.159936
86.493867	2340.078538	22.164954
86.613452	2338.952383	22.169971
86.575067	2333.561821	22.174989
86.246188	2338.713340	22.180007
86.668123	2335.952644	22.185024
86.449386	2334.576188	22.190042
86.521241	2342.635112	22.195059
86.581215	2344.838351	22.200077
86.442179	2348.884120	22.205095
86.726610	2353.293174	22.210112
86.810977	2363.370001	22.215130
86.928902	2369.427169	22.220147
86.783666	2364.839079	22.225165
87.095549	2378.730817	22.230183
86.962696	2387.149857	22.235200
87.291757	2386.429771	22.240218
87.108011	2381.601503	22.245235
87.771187	2390.407882	22.250253
88.400474	2398.749295	22.255271
88.647382	2397.085728	22.260288
89.058583	2398.205430	22.265306
88.173763	2383.772118	22.270323
88.720963	2367.427399	22.275341
88.582684	2379.827003	22.280359
88.236690	2375.850871	22.285376
88.646815	2367.960344	22.290394
88.522369	2372.010158	22.295411
88.853065	2365.880425	22.300429
88.787730	2363.309206	22.305447
88.856336	2375.291563	22.310464
88.858202	2370.951985	22.315482
88.633289	2376.342965	22.320499
88.864213	2378.746824	22.325517
88.725954	2397.117603	22.330535
88.806749	2389.013236	22.335552
88.991637	2393.352587	22.340570
89.184289	2402.765594	22.345587
89.152394	2403.278898	22.350605
89.580358	2405.642615	22.355623
89.346888	2405.395144	22.360640
89.764309	2418.115381	22.365658
89.671805	2412.363967	22.370675
89.781793	2413.694681	22.375693
89.414143	2427.272506	22.380711
89.663678	2428.941279	22.385728
90.292123	2429.964040	22.390746
89.957225	2434.693617	22.395763
90.559541	2426.167186	22.400781
90.276131	2430.936087	22.405799
90.426972	2443.278096	22.410816
90.869960	2449.508759	22.415834
90.730244	2453.620934	22.420851
90.874625	2442.397963	22.425869
90.931788	2455.805521	22.430887
90.653477	2452.093408	22.435904
91.142594	2458.354764	22.440922
90.913188	2457.273470	22.445939
91.239134	2463.654914	22.450957
91.319303	2468.395621	22.455975
91.519763	2480.654187	22.460992
91.779092	2481.197895	22.466010
91.830124	2477.680671	22.471027
91.486166	2466.615773	22.476045
91.570213	2476.048885	22.481063
91.522679	2483.372170	22.486080
92.012145	2483.359304	22.491098
92.139586	2493.997582	22.496115
92.106415	2502.644171	22.501133
92.650487	2500.303123	22.506151
92.256698	2495.750540	22.511168
92.709980	2493.420472	22.516186
92.784807	2500.689997	22.521203
92.556238	2498.361939	22.526221
92.540137	2497.332645	22.531239
92.822670	2497.828557	22.536256
92.980410	2509.683510	22.541274
92.934607	2519.553457	22.546291
93.036854	2511.474099	22.551309
93.281388	2514.570185	22.556327
93.269824	2523.784662	22.561344
93.391134	2520.073437	22.566362
93.514767	2516.869973	22.571379
93.528851	2510.843137	22.576397
93.408454	2527.393395	22.581415
93.956636	2535.296188	22.586432
94.361733	2546.071162	22.591450
93.727177	2541.432969	22.596467
93.850139	2538.283258	22.601485
94.228637	2538.726358	22.606503
94.120121	2534.946763	22.611520
94.140994	2532.942808	22.616538
94.084322	2550.815012	22.621555
94.501170	2547.960395	22.626573
94.727184	2567.066798	22.631591
94.448677	2568.887230	22.636608
94.960826	2563.871666	22.641626
94.882431	2573.251219	22.646643
94.728044	2558.621983	22.651661
95.187873	2564.244105	22.656679
95.204620	2565.769241	22.661696
95.403248	2557.662232	22.666714
95.194822	2566.121527	22.671731
94.869835	2580.630169	22.676749
95.475493	2583.048302	22.681767
95.290239	2581.218456	22.686784
95.542447	2579.273159	22.691802
95.617336	2588.998112	22.696819
95.575201	2605.697215	22.701837
95.960946	2609.680273	22.706855
95.621418	2606.482627	22.711872
95.883678	2605.896019	22.716890
95.811765	2629.353721	22.721907
96.261240	2626.067946	22.726925
96.380700	2626.491414	22.731943
96.218948	2640.756922	22.736960
96.797490	2634.313934	22.741978
96.920751	2634.863052	22.746995
96.898572	2635.258076	22.752013
97.300708	2654.542294	22.757031
96.923488	2658.470569	22.762048
97.163962	2648.232979	22.767066
96.943652	2657.707260	22.772083
97.176454	2655.944872	22.777101
97.474101	2653.698980	22.782119
97.270194	2659.983093	22.787136
97.886595	2670.977729	22.792154
98.044788	2685.796267	22.797171
98.279148	2672.766501	22.802189
98.752902	2668.580617	22.807207
98.654554	2660.772284	22.812224
98.495359	2642.447987	22.817242
98.420681	2637.094544	22.822259
98.245481	2642.193818	22.827277
98.559110	2648.766609	22.832295
98.586136	2658.925119	22.837312
98.687641	2658.773825	22.842330
98.679867	2666.416068	22.847347
98.924365	2661.871373	22.852365
99.099692	2655.731015	22.857383
98.998328	2660.392731	22.862400
99.036455	2654.358948	22.867418
98.531339	2674.548206	22.872435
99.054534	2682.230875	22.877453
99.469060	2687.475050	22.882471
98.954740	2692.160040	22.887488
99.542167	2690.285627	22.892506
99.712910	2707.907968	22.897523
99.634524	2715.119377	22.902541
99.603011	2706.281209	22.907559
99.806033	2713.003799	22.912576
99.996148	2713.346835	22.917594
99.862919	2732.802860	22.922611
99.921701	2733.964830	22.927629
100.379264	2733.840157	22.932647
100.994908	2744.219523	22.937664
100.563654	2739.874699	22.942682
100.477840	2752.496785	22.947699
100.990695	2757.690955	22.952717
101.235907	2751.722736	22.957735
100.995763	2753.635052	22.962752
101.160640	2758.097538	22.967770
101.033732	2754.607963	22.972787
101.261697	2762.529152	22.977805
101.596853	2757.821981	22.982823
101.541853	2758.610315	22.987840
101.501530	2755.801595	22.992858
101.621206	2748.072898	22.997875
101.803184	2760.830036	23.002893
102.216289	2769.786000	23.007911
102.099464	2780.898018	23.012928
102.165975	2777.763366	23.017946
102.309470	2774.768221	23.022963
102.212359	2781.221957	23.027981
102.303241	2776.994665	23.032999
102.114893	2776.191005	23.038016
102.217843	2771.005543	23.043034
102.174183	2787.320012	23.048051
102.364890	2795.067119	23.053069
102.688035	2794.212228	23.058087
102.226431	2808.489837	23.063104
102.748198	2813.897249	23.068122
103.219004	2818.204812	23.073139
102.929177	2827.617416	23.078157
103.545224	2831.627790	23.083175
103.575511	2841.274609	23.088192
104.035187	2839.085526	23.093210
103.795376	2838.608640	23.098227
103.794654	2843.737616	23.103245
103.960768	2842.724117	23.108263
103.611590	2843.343642	23.113280
104.061692	2841.844076	23.118298
104.072551	2861.587104	23.123315
103.880167	2869.280269	23.128333
104.280583	2868.852040	23.133351
104.559571	2870.462616	23.138368
104.854994	2867.964557	23.143386
104.571702	2885.335841	23.148403
104.748159	2884.671056	23.153421
104.938688	2885.913519	23.158439
105.167394	2890.643837	23.163456
105.417221	2889.194385	23.168474
105.214129	2889.109450	23.173491
105.249861	2889.583833	23.178509
105.381308	2905.536599	23.183527
105.690189	2909.607439	23.188544
105.630902	2912.100740	23.193562
105.986816	2915.258458	23.198579
105.685992	2925.193581	23.203597
105.824259	2918.490806	23.208615
106.149977	2926.235886	23.213632
106.651630	2922.525328	23.218650
106.743935	2935.201869	23.223667
106.039938	2936.722475	23.228685
106.660317	2930.370708	23.233703
106.706678	2934.485582	23.238720
106.713987	2937.719671	23.243738
107.413316	2949.474813	23.248755
107.158362	2959.958289	23.253773
107.427288	2956.801560	23.258791
107.396647	2966.391654	23.263808
107.580906	2966.871320	23.268826
107.401834	2957.806669	23.273843
107.404420	2962.329191	23.278861
107.590054	2960.918133	23.283879
107.763927	2971.006615	23.288896
107.879764	2954.649621	23.293914
108.317787	2966.167721	23.298931
108.340196	2981.698832	23.303949
108.274845	2982.151082	23.308967
108.334999	2981.002580	23.313984
108.265267	2975.623017	23.319002
108.586181	2978.817756	23.324019
108.743291	2979.506797	23.329037
108.673622	2981.297911	23.334055
108.580301	2975.874679	23.339072
108.481967	2976.612959	23.344090
108.898587	2988.869779	23.349107
109.047008	2997.923877	23.354125
109.070505	2997.970936	23.359143
108.851968	3000.009314	23.364160
109.081972	3007.305383	23.369178
109.445282	3013.712768	23.374195
109.447021	3022.505665	23.379213
109.713381	3022.770558	23.384231
109.390665	3018.525544	23.389248
109.895318	3035.016826	23.394266
110.274156	3044.713640	23.399283
110.163238	3044.434454	23.404301
110.197817	3044.640750	23.409319
110.285493	3043.825664	23.414336
110.474795	3038.516217	23.419354
110.715830	3046.937321	23.424371
110.845826	3061.075680	23.429389
111.019739	3063.365420	23.434407
111.030012	3070.114997	23.439424
111.197061	3064.666982	23.444442
111.198866	3063.025735	23.449459
111.328254	3063.356140	23.454477
111.442338	3075.407632	23.459495
111.389349	3088.482481	23.464512
111.776417	3085.158998	23.469530
112.187688	3091.814590	23.474547
111.736825	3099.163048	23.479565
111.989203	3085.757755	23.484583
111.918944	3081.429234	23.489600
112.241470	3102.875655	23.494618
112.369499	3103.351455	23.499635
112.419545	3100.528612	23.504653
112.722996	3101.744040	23.509671
112.568096	3103.567373	23.514688
112.375721	3100.924299	23.519706
113.278372	3113.468489	23.524723
113.074795	3127.216975	23.529741
113.132794	3126.087736	23.534759
113.040769	3127.513078	23.539776
113.327080	3134.248108	23.544794
113.608435	3131.578615	23.549811
113.371640	3130.627831	23.554829
113.880614	3142.362239	23.559847
114.072194	3140.659877	23.564864
113.859057	3148.198584	23.569882
113.897800	3140.507568	23.574899
114.246388	3144.610153	23.579917
114.143702	3147.179679	23.584935
113.843002	3152.547972	23.589952
114.363396	3160.761515	23.594970
114.748435	3171.811418	23.599987
114.518673	3176.111364	23.605005
114.876741	3170.699856	23.610023
114.847520	3193.331049	23.615040
114.670111	3200.674847	23.620058
115.337608	3193.725452	23.625075
115.333923	3195.765119	23.630093
115.304007	3199.611032	23.635111
115.312797	3199.452076	23.640128
115.414107	3213.875919	23.645146
115.910717	3219.009630	23.650163
115.719033	3218.840856	23.655181
115.766735	3209.115853	23.660199
115.854642	3218.147922	23.665216
116.204713	3237.320940	23.670234
116.281927	3235.112453	23.675251
116.486643	3248.784840	23.680269
116.696712	3232.864253	23.685287
116.560269	3248.852721	23.690304
116.607754	3241.709472	23.695322
116.888182	3240.473004	23.700339
116.643307	3251.381161	23.705357
116.829602	3266.694476	23.710375
117.155988	3264.125263	23.715392
117.243006	3264.203463	23.720410
117.381327	3269.430847	23.725427
117.410929	3281.738654	23.730445
117.397199	3281.545330	23.735463
117.557535	3289.104853	23.740480
117.800303	3292.788397	23.745498
118.207306	3298.561004	23.750515
118.250009	3306.561776	23.755533
118.814808	3305.839671	23.760551
118.901637	3308.442837	23.765568
118.503476	3314.249278	23.770586
119.129888	3296.338550	23.775603
118.934846	3299.872483	23.780621
119.055977	3300.415642	23.785639
119.285490	3300.130792	23.790656
118.860363	3303.198717	23.795674
118.815524	3302.117040	23.800691
119.335758	3319.691881	23.805709
119.554575	3318.048385	23.810727
119.372690	3327.895776	23.815744
119.337929	3338.424093	23.820762
119.840117	3329.846549	23.825779
120.043198	3348.512333	23.830797
119.957922	3345.019318	23.835815
120.275914	3342.505055	23.840832
120.023079	3353.869003	23.845850
120.314597	3356.651771	23.850867
120.590925	3376.076288	23.855885
120.674818	3374.251798	23.860903
120.833206	3381.849538	23.865920
121.022093	3378.247552	23.870938
120.923978	3381.113080	23.875955
121.199759	3393.906563	23.880973
121.555525	3390.976109	23.885991
121.752336	3394.281774	23.891008
121.742087	3407.302857	23.896026
121.467060	3390.495021	23.901043
122.005272	3387.583504	23.906061
121.969177	3387.472565	23.911079
122.116121	3398.641739	23.916096
122.289688	3408.938822	23.921114
122.577954	3411.791542	23.926131
122.316494	3429.668097	23.931149
122.387444	3426.254897	23.936167
122.655379	3415.248799	23.941184
122.488901	3420.034471	23.946202
122.915050	3438.192191	23.951219
122.847357	3439.026716	23.956237
122.992610	3435.977533	23.961255
123.127818	3435.416993	23.966272
123.499892	3435.940024	23.971290
123.668756	3450.495567	23.976307
123.756477	3458.618802	23.981325
123.515700	3457.021599	23.986343
123.983957	3462.661631	23.991360
123.750822	3459.945945	23.996378
124.189114	3442.231640	24.001395
124.107726	3461.011268	24.006413
124.363289	3473.034686	24.011431
124.542672	3476.428298	24.016448
124.641834	3481.418812	24.021466
124.865137	3478.111286	24.026483
124.988149	3471.464336	24.031501
124.806161	3473.781134	24.036519
125.060182	3472.147924	24.041536
124.891443	3490.467752	24.046554
125.252997	3496.152813	24.051571
125.054634	3502.026049	24.056589
125.237612	3508.105037	24.061607
125.311385	3510.637672	24.066624
125.563764	3526.887782	24.071642
125.835277	3528.480646	24.076659
126.116843	3527.142983	24.081677
125.865860	3532.213275	24.086695
126.050392	3548.063660	24.091712
126.238389	3552.693180	24.096730
126.307018	3542.333497	24.101747
126.619274	3556.462806	24.106765
126.410132	3566.289321	24.111783
126.740232	3564.480135	24.116800
126.904395	3571.269065	24.121818
127.791585	3580.524058	24.126835
127.629987	3592.713504	24.131853
127.726299	3585.805547	24.136871
128.045678	3584.834426	24.141888
127.888701	3598.516048	24.146906
128.104314	3591.277048	24.151923
128.226331	3590.488154	24.156941
128.137517	3584.619010	24.161959
128.199111	3581.030489	24.166976
128.190728	3594.183978	24.171994
128.420452	3612.388236	24.177011
128.540837	3617.438608	24.182029
128.777580	3614.738116	24.187047
129.221610	3604.888070	24.192064
128.933405	3624.719527	24.197082
129.185833	3628.859289	24.202099
129.150951	3642.203156	24.207117
129.099141	3639.171995	24.212135
129.910337	3635.574068	24.217152
129.644984	3639.750260	24.222170
129.477549	3646.868593	24.227187
130.125927	3659.367538	24.232205
129.623957	3666.670525	24.237223
130.189075	3664.086181	24.242240
130.299561	3654.161789	24.247258
130.204091	3678.773394	24.252275
130.409006	3686.925829	24.257293
130.628361	3688.094424	24.262311
130.882022	3681.184025	24.267328
130.220559	3706.085787	24.272346
130.506560	3705.334481	24.277363
131.251254	3712.392892	24.282381
131.351591	3736.077717	24.287399
131.401228	3736.228021	24.292416
131.499389	3727.770005	24.297434
131.996584	3730.097874	24.302451
132.046834	3736.749946	24.307469
132.061863	3746.869906	24.312487
132.019201	3756.452823	24.317504
132.354956	3766.106235	24.322522
132.217422	3761.933212	24.327539
132.168660	3767.401336	24.332557
132.495553	3775.459070	24.337575
132.851807	3787.050397	24.342592
132.719772	3793.771902	24.347610
133.043379	3786.938948	24.352627
133.068067	3786.755418	24.357645
133.058723	3793.672446	24.362663
133.469010	3808.825099	24.367680
133.491484	3815.216398	24.372698
133.289925	3817.589943	24.377715
133.668820	3826.835827	24.382733
133.702590	3830.813990	24.387751
134.421811	3823.155614	24.392768
134.764270	3823.272954	24.397786
134.798904	3830.246274	24.402803
134.837315	3824.085806	24.407821
134.950131	3823.244677	24.412839
134.764811	3811.169497	24.417856
134.838405	3814.926831	24.422874
134.796876	3816.663147	24.427891
135.319349	3829.844627	24.432909
135.206529	3834.628367	24.437927
135.617077	3834.239573	24.442944
135.735148	3840.063652	24.447962
135.869395	3835.860923	24.452979
136.089923	3846.715917	24.457997
136.048080	3863.245702	24.463015
136.218919	3861.852660	24.468032
135.852805	3866.606407	24.473050
136.123273	3865.166291	24.478067
136.570022	3870.090171	24.483085
136.469145	3896.066422	24.488103
136.834033	3886.108607	24.493120
136.510592	3897.821609	24.498138
136.943599	3900.178431	24.503155
137.149499	3907.232430	24.508173
137.138311	3925.566044	24.513191
137.651914	3918.719242	24.518208
137.635524	3924.700003	24.523226
137.524593	3938.153773	24.528243
137.948835	3933.142052	24.533261
138.155781	3944.548412	24.538279
138.335111	3934.761493	24.543296
138.445599	3956.185131	24.548314
138.602136	3969.660407	24.553331
138.881421	3958.750057	24.558349
138.778518	3959.580619	24.563367
139.066689	3957.089854	24.568384
138.992069	3956.309464	24.573402
139.092565	3962.082663	24.578419
139.417667	3973.745242	24.583437
139.492643	3978.607095	24.588455
139.590931	3977.632501	24.593472
140.005406	3986.153294	24.598490
139.653385	3989.326734	24.603507
140.226248	3995.351497	24.608525
139.953168	4008.085680	24.613543
139.906664	4001.736369	24.618560
140.360554	4013.003323	24.623578
140.367575	4032.700887	24.628595
140.621943	4031.272733	24.633613
140.716812	4033.271900	24.638631
140.991364	4034.839086	24.643648
140.765778	4053.051551	24.648666
140.880049	4057.465426	24.653683
141.280520	4050.636189	24.658701
141.165548	4073.884690	24.663719
141.471970	4077.403826	24.668736
141.956973	4082.697410	24.673754
141.663670	4081.774309	24.678771
141.988225	4100.551368	24.683789
142.395701	4106.336788	24.688807
142.633869	4103.822225	24.693824
142.606742	4099.076424	24.698842
142.520430	4111.374438	24.703859
142.965684	4103.430343	24.708877
142.768026	4109.575108	24.713895
143.076150	4130.734615	24.718912
143.202696	4132.927709	24.723930
143.119164	4138.376108	24.728947
143.202518	4134.212797	24.733965
143.370065	4146.714347	24.738983
143.544409	4153.779667	24.744000
144.164726	4150.788966	24.749018
143.975924	4152.100046	24.754035
144.359230	4159.861945	24.759053
144.461297	4170.656669	24.764071
144.666300	4162.775204	24.769088
144.569088	4179.695813	24.774106
144.716029	4179.742595	24.779123
145.324024	4196.682834	24.784141
145.368062	4204.172472	24.789159
145.182170	4205.672482	24.794176
145.515287	4193.598394	24.799194
145.027272	4198.674212	24.804211
145.786074	4201.242327	24.809229
145.675923	4217.420093	24.814247
145.756000	4222.388533	24.819264
146.097952	4228.282040	24.824282
145.855791	4231.974994	24.829299
146.338395	4238.651471	24.834317
146.723440	4248.527880	24.839335
146.919592	4252.771238	24.844352
147.093459	4238.471447	24.849370
146.947473	4252.896747	24.854387
147.181936	4262.099058	24.859405
147.299761	4268.857590	24.864423
147.233305	4274.069802	24.869440
147.217979	4285.220599	24.874458
147.349335	4290.250514	24.879475
148.159423	4294.167885	24.884493
147.803351	4298.973837	24.889511
147.885456	4317.062911	24.894528
148.163948	4316.783046	24.899546
148.178805	4323.813293	24.904563
148.813022	4331.697176	24.909581
149.028268	4339.835673	24.914599
149.139583	4341.153698	24.919616
149.275959	4340.438288	24.924634
149.454105	4349.355871	24.929651
149.478820	4334.956129	24.934669
149.515162	4355.694230	24.939687
149.537227	4362.047910	24.944704
149.816636	4367.667129	24.949722
149.611421	4366.155842	24.954739
150.320941	4386.170524	24.959757
150.275286	4388.851288	24.964775
150.268112	4381.122704	24.969792
150.765767	4382.194358	24.974810
150.459251	4397.796836	24.979827
151.000753	4408.213963	24.984845
151.267005	4418.680262	24.989863
151.057756	4417.936595	24.994880
151.248850	4415.987994	24.999898
151.328814	4430.633922	25.004915
151.581483	4431.772128	25.009933
151.756472	4440.567150	25.014951
151.858395	4436.198871	25.019968
152.322736	4447.230899	25.024986
152.358678	4461.040955	25.030003
152.239920	4462.224366	25.035021
152.833655	4471.231968	25.040039
152.661958	4457.639175	25.045056
152.928478	4457.698904	25.050074
152.747520	4465.204741	25.055091
153.065131	4475.577855	25.060109
153.347544	4482.497068	25.065127
153.293377	4488.891069	25.070144
153.663815	4476.911987	25.075162
153.488690	4492.500403	25.080179
153.906446	4499.669999	25.085197
153.755744	4507.202707	25.090215
153.839973	4515.895109	25.095232
154.496719	4525.558925	25.100250
154.740354	4527.598113	25.105267
154.504797	4536.094115	25.110285
154.553925	4537.702755	25.115303
154.819766	4539.984685	25.120320
155.047363	4551.344024	25.125338
155.343189	4561.928901	25.130355
155.068103	4562.319152	25.135373
155.341614	4564.719834	25.140391
155.436308	4566.655960	25.145408
155.859217	4556.657181	25.150426
156.054688	4564.429561	25.155443
156.165773	4591.118715	25.160461
156.678528	4592.077558	25.165479
156.953036	4595.065178	25.170496
157.316176	4586.101517	25.175514
156.904218	4588.002896	25.180531
157.391316	4583.170595	25.185549
157.193844	4600.508068	25.190567
157.276878	4603.866391	25.195584
157.679106	4597.882590	25.200602
157.912646	4604.231838	25.205619
157.987348	4601.496458	25.210637
157.872723	4606.429033	25.215655
157.706951	4620.049667	25.220672
158.270664	4620.435582	25.225690
158.345337	4639.656126	25.230707
158.657683	4644.692682	25.235725
159.114093	4653.582874	25.240743
158.663096	4663.564424	25.245760
159.424764	4666.943358	25.250778
159.169358	4667.037001	25.255795
159.134750	4680.252178	25.260813
159.504522	4682.937748	25.265831
159.690782	4685.951748	25.270848
160.297680	4681.561606	25.275866
160.208493	4695.299786	25.280883
160.739680	4707.075949	25.285901
160.938094	4707.253601	25.290919
160.711547	4708.879925	25.295936
161.038164	4705.562405	25.300954
160.997893	4708.633773	25.305971
160.863274	4707.607023	25.310989
161.414689	4701.688340	25.316007
161.393966	4714.184874	25.321024
162.016689	4715.511685	25.326042
161.690993	4717.055598	25.331059
161.954496	4715.446054	25.336077
162.194968	4708.799302	25.341095
162.298154	4709.645158	25.346112
162.419293	4719.670232	25.351130
162.928734	4744.034441	25.356147
162.984781	4745.121213	25.361165
162.932779	4732.579605	25.366183
162.888340	4739.262570	25.371200
162.976601	4733.889449	25.376218
163.073902	4737.917893	25.381235
163.321410	4738.242567	25.386253
163.642882	4751.664340	25.391271
163.424478	4759.327637	25.396288
163.588200	4753.320946	25.401306
163.821679	4771.399531	25.406323
164.274445	4772.572892	25.411341
164.040280	4787.280641	25.416359
164.090897	4793.216535	25.421376
164.543092	4792.956967	25.426394
164.895688	4806.396031	25.431411
164.847297	4806.814121	25.436429
164.930150	4817.839486	25.441447
165.331735	4824.336252	25.446464
165.546158	4826.427369	25.451482
165.442527	4835.985629	25.456499
165.774421	4848.323194	25.461517
166.178112	4856.621971	25.466535
165.695563	4857.107657	25.471552
166.112312	4872.354891	25.476570
166.028862	4878.478978	25.481587
165.803398	4888.662270	25.486605
166.692845	4895.038917	25.491623
166.377892	4919.736882	25.496640
166.938084	4925.066356	25.501658
167.097673	4944.078302	25.506675
167.033841	4949.182979	25.511693
167.551438	4958.546734	25.516711
168.076472	4967.641036	25.521728
168.147206	4966.837972	25.526746
168.343502	4965.683932	25.531763
168.620394	4975.530231	25.536781
168.584783	4983.449244	25.541799
168.647571	4988.234356	25.546816
169.068930	4992.127179	25.551834
168.965333	5011.489504	25.556851
169.160947	5026.730263	25.561869
169.468544	5025.839816	25.566887
169.250550	5033.099135	25.571904
169.374288	5037.934743	25.576922
169.401391	5046.241735	25.581939
169.420281	5052.510927	25.586957
169.841830	5059.891640	25.591975
170.273127	5082.560818	25.596992
170.512711	5094.887671	25.602010
170.655556	5104.022606	25.607027
170.799828	5105.152481	25.612045
171.055985	5102.799118	25.617063
171.185604	5126.793695	25.622080
171.701814	5119.201108	25.627098
171.996342	5120.837880	25.632115
171.934091	5133.082336	25.637133
172.654588	5123.147393	25.642151
172.373782	5131.063611	25.647168
172.838082	5122.948815	25.652186
172.883739	5128.503656	25.657203
173.061557	5123.949789	25.662221
173.312924	5116.581514	25.667239
173.005490	5124.075749	25.672256
173.287524	5138.681319	25.677274
173.248943	5151.679659	25.682292
173.364201	5155.446568	25.687309
173.381083	5152.420241	25.692327
173.440193	5165.851604	25.697344
173.897122	5178.065762	25.702362
174.093169	5182.145218	25.707380
174.263529	5201.528223	25.712397
174.490620	5196.767807	25.717415
174.481557	5199.682887	25.722432
174.640224	5206.381750	25.727450
174.903459	5213.929217	25.732468
174.944257	5221.473440	25.737485
175.711582	5226.975928	25.742503
175.320138	5224.271994	25.747520
175.534054	5237.704561	25.752538
175.953185	5255.101327	25.757556
176.099364	5257.146302	25.762573
176.204934	5261.397688	25.767591
176.223294	5278.175066	25.772608
176.465934	5281.398188	25.777626
176.925071	5279.764451	25.782644
176.967178	5285.979605	25.787661
177.437926	5294.192387	25.792679
177.483347	5311.385400	25.797696
177.454259	5302.390915	25.802714
178.154833	5304.428495	25.807732
177.223031	5308.866651	25.812749
177.654106	5304.958275	25.817767
177.833962	5322.960532	25.822784
177.672963	5334.305107	25.827802
178.242833	5355.983999	25.832820
178.327490	5371.573758	25.837837
178.797196	5362.981378	25.842855
179.030756	5375.782839	25.847872
179.140325	5393.508865	25.852890
179.662375	5389.737821	25.857908
179.625094	5394.551245	25.862925
179.919315	5395.967132	25.867943
180.301201	5417.874228	25.872960
180.144866	5423.751010	25.877978
180.516210	5420.363267	25.882996
180.591164	5427.877006	25.888013
181.222253	5432.775774	25.893031
181.235328	5433.929252	25.898048
181.255281	5435.069033	25.903066
181.722188	5414.911504	25.908084
181.907371	5431.287424	25.913101
182.432381	5413.450377	25.918119
182.233353	5422.686047	25.923136
182.415125	5444.595922	25.928154
182.374277	5447.096170	25.933172
182.505637	5459.894663	25.938189
182.733349	5450.475025	25.943207
182.530075	5451.024566	25.948224
182.821617	5467.254540	25.953242
183.420064	5472.177341	25.958260
183.415696	5479.444613	25.963277
183.508295	5483.448703	25.968295
183.393296	5501.124571	25.973312
183.738502	5506.651830	25.978330
183.600765	5507.535233	25.983348
183.908363	5532.452759	25.988365
184.174098	5526.006953	25.993383
184.202334	5542.789351	25.998400
184.007205	5562.261209	26.003418
184.418954	5573.845044	26.008436
184.347711	5580.447263	26.013453
184.787764	5595.116983	26.018471
184.900757	5608.148869	26.023488
185.469530	5627.770173	26.028506
185.593834	5642.659545	26.033524
185.689533	5643.471889	26.038541
186.104999	5662.230101	26.043559
186.710674	5661.735138	26.048576
186.713387	5672.448371	26.053594
186.813402	5669.781491	26.058612
187.313089	5675.133235	26.063629
187.357193	5679.075473	26.068647
187.482463	5684.734884	26.073664
187.630425	5691.391400	26.078682
187.962135	5690.430880	26.083700
187.989444	5680.294214	26.088717
188.145978	5691.280228	26.093735
188.186666	5703.344898	26.098752
188.588945	5707.689083	26.103770
188.421311	5703.510828	26.108788
188.706503	5718.716125	26.113805
188.741871	5719.518925	26.118823
188.939422	5736.508729	26.123840
188.851973	5745.029583	26.128858
189.294317	5749.553780	26.133876
189.434859	5763.323287	26.138893
189.708162	5775.683232	26.143911
190.171264	5782.928351	26.148928
190.308702	5796.035481	26.153946
190.379585	5799.673699	26.158964
190.497446	5806.413859	26.163981
190.840812	5817.364548	26.168999
191.018209	5835.156203	26.174016
190.980585	5830.774593	26.179034
191.608809	5849.629296	26.184052
191.510834	5859.875353	26.189069
191.794067	5860.541715	26.194087
192.037022	5869.184800	26.199104
192.150479	5889.887393	26.204122
192.488915	5883.218649	26.209140
192.784332	5896.452773	26.214157
192.783184	5907.157275	26.219175
193.037571	5906.252975	26.224192
192.857503	5922.212708	26.229210
193.535621	5925.895303	26.234228
193.816957	5940.668928	26.239245
193.788240	5946.387116	26.244263
194.031765	5958.619243	26.249280
193.978807	5963.861403	26.254298
194.131565	5964.800613	26.259316
194.236274	5985.394194	26.264333
194.798550	5988.431944	26.269351
194.737240	6003.934487	26.274368
195.011118	6011.723690	26.279386
195.411949	6015.556799	26.284404
195.671476	6032.294168	26.289421
196.007030	6032.690389	26.294439
195.992123	6039.991092	26.299456
195.780465	6055.564436	26.304474
196.075127	6059.581387	26.309492
196.774562	6068.323957	26.314509
196.829528	6084.045213	26.319527
197.217750	6087.334200	26.324544
197.081343	6090.262935	26.329562
197.301884	6090.493979	26.334580
197.517983	6106.051275	26.339597
197.537099	6108.008802	26.344615
197.642908	6114.381624	26.349632
198.140167	6130.655922	26.354650
197.985617	6135.509895	26.359668
198.189097	6139.803063	26.364685
198.482549	6147.535613	26.369703
198.744233	6156.961929	26.374720
198.933085	6181.491620	26.379738
199.356016	6179.793996	26.384756
199.642752	6187.218256	26.389773
199.913864	6194.540780	26.394791
200.468198	6197.601899	26.399808
200.335890	6202.206207	26.404826
200.675642	6199.375659	26.409844
200.866804	6195.668594	26.414861
201.366188	6187.093306	26.419879
201.571511	6185.129677	26.424896
201.106844	6188.759808	26.429914
201.357635	6191.634590	26.434932
201.784952	6200.069200	26.439949
201.641345	6207.513117	26.444967
201.793163	6212.493030	26.449984
202.188169	6226.712555	26.455002
202.533611	6232.694562	26.460020
202.327689	6242.364184	26.465037
202.505927	6237.882579	26.470055
203.093648	6253.637835	26.475072
203.072299	6268.670349	26.480090
203.218610	6261.472647	26.485108
203.279966	6279.879415	26.490125
203.431485	6296.195063	26.495143
203.411933	6297.754575	26.500160
203.804938	6316.842098	26.505178
204.534537	6315.560751	26.510196
204.137003	6339.525356	26.515213
204.517501	6351.420752	26.520231
204.975263	6355.671225	26.525248
205.142472	6372.821024	26.530266
205.868569	6357.508682	26.535284
206.344445	6355.603927	26.540301
206.236906	6356.615250	26.545319
206.647265	6350.026684	26.550336
206.819754	6378.953314	26.555354
206.944720	6380.521900	26.560372
207.073724	6380.457842	26.565389
206.989820	6381.443390	26.570407
207.222656	6380.728668	26.575424
207.001220	6385.769897	26.580442
207.591310	6389.513643	26.585460
207.595483	6402.891337	26.590477
207.616516	6406.171259	26.595495
208.015412	6424.232047	26.600512
207.929700	6435.275165	26.605530
208.372891	6442.056455	26.610548
208.365031	6449.435142	26.615565
208.453503	6474.173415	26.620583
208.879728	6472.367923	26.625600
208.805903	6502.586315	26.630618
209.034601	6506.285335	26.635636
209.602704	6512.785196	26.640653
209.603555	6522.069219	26.645671
209.936278	6540.200403	26.650688
210.258192	6554.179025	26.655706
210.530799	6564.983344	26.660724
210.918104	6575.315242	26.665741
210.972939	6593.884335	26.670759
211.268643	6594.574038	26.675776
210.993969	6599.996109	26.680794
211.232245	6611.175140	26.685812
211.484833	6616.493029	26.690829
211.724515	6637.745032	26.695847
212.223935	6641.177803	26.700864
212.209754	6669.789869	26.705882
212.687861	6673.759455	26.710900
212.684647	6688.167609	26.715917
212.929102	6695.153556	26.720935
213.276753	6698.471069	26.725952
213.682559	6714.763284	26.730970
213.880975	6729.645161	26.735988
214.042906	6725.582669	26.741005
214.295471	6729.666301	26.746023
214.388360	6730.112947	26.751040
214.605874	6747.602509	26.756058
214.713795	6751.058372	26.761076
215.040855	6752.185147	26.766093
215.365627	6760.465516	26.771111
215.454448	6765.613227	26.776128
215.647351	6775.634574	26.781146
215.750545	6784.249345	26.786164
215.977973	6790.076286	26.791181
215.925177	6804.432272	26.796199
216.657948	6808.062346	26.801216
216.641262	6823.214546	26.806234
216.510851	6827.007423	26.811252
216.870450	6839.944972	26.816269
216.793879	6847.732272	26.821287
217.144556	6863.480766	26.826304
217.333444	6884.971409	26.831322
217.709188	6895.257937	26.836340
218.005751	6902.838798	26.841357
217.741510	6923.456152	26.846375
218.434608	6925.697123	26.851392
219.018635	6949.367650	26.856410
218.826027	6959.865815	26.861428
219.003553	6959.412228	26.866445
218.928441	6983.608431	26.871463
219.769989	6993.484715	26.876480
219.861723	7014.715994	26.881498
219.962684	7023.078680	26.886516
220.566414	7030.545479	26.891533
220.495259	7041.242602	26.896551
220.592726	7044.564404	26.901568
221.242293	7060.440159	26.906586
221.007851	7066.550604	26.911604
221.618984	7080.692951	26.916621
221.626576	7091.100042	26.921639
221.943691	7094.100386	26.926656
222.206411	7113.972978	26.931674
222.211865	7118.347716	26.936692
222.568528	7136.317922	26.941709
222.816310	7145.263917	26.946727
223.252748	7148.438260	26.951744
223.294289	7159.670353	26.956762
223.384884	7162.567073	26.961780
223.950678	7178.490698	26.966797
223.955763	7181.025070	26.971815
224.181526	7198.791581	26.976832
224.531866	7219.108389	26.981850
224.548994	7220.750660	26.986868
225.333760	7235.140740	26.991885
225.771175	7234.223667	26.996903
226.440807	7221.599567	27.001920
226.541716	7225.347041	27.006938
226.641373	7225.584293	27.011956
226.727754	7221.877551	27.016973
226.872632	7227.029291	27.021991
226.978959	7227.243408	27.027008
226.917458	7218.628691	27.032026
227.243202	7240.897128	27.037044
227.697456	7251.411554	27.042061
227.569232	7255.112629	27.047079
228.022292	7262.432511	27.052096
228.190656	7276.454533	27.057114
228.014137	7289.548476	27.062132
228.091985	7285.296913	27.067149
228.338515	7283.017381	27.072167
228.808304	7289.526513	27.077184
229.185871	7296.211006	27.082202
229.014244	7314.554067	27.087220
229.333042	7320.654227	27.092237
229.363251	7321.050666	27.097255
229.623462	7334.363922	27.102272
229.840783	7351.844621	27.107290
229.715015	7360.081759	27.112308
230.603383	7366.614144	27.117325
230.706643	7372.536368	27.122343
230.930628	7385.713242	27.127360
231.188357	7388.959646	27.132378
231.329829	7404.798000	27.137396
231.718184	7418.264995	27.142413
231.692304	7426.890693	27.147431
231.824662	7446.780785	27.152448
232.245190	7454.752971	27.157466
232.528472	7473.476802	27.162484
232.840872	7473.485209	27.167501
232.787851	7490.859755	27.172519
233.067839	7500.280758	27.177536
233.296778	7514.722869	27.182554
233.581892	7530.216965	27.187572
233.993339	7531.444300	27.192589
234.131070	7547.033964	27.197607
234.553762	7553.695741	27.202624
234.819430	7572.861225	27.207642
235.135340	7583.466833	27.212660
235.331067	7586.590336	27.217677
235.214718	7595.312277	27.222695
235.751294	7602.729785	27.227712
235.716087	7609.819603	27.232730
236.050742	7636.633092	27.237748
236.417370	7631.717733	27.242765
236.650164	7648.766965	27.247783
236.856059	7665.921422	27.252800
237.179251	7673.138568	27.257818
237.098703	7691.871911	27.262836
237.820764	7692.593144	27.267853
237.609046	7714.642766	27.272871
237.978561	7712.552393	27.277888
238.258517	7725.057840	27.282906
238.229794	7744.521891	27.287924
238.606676	7750.894120	27.292941
238.684959	7768.119051	27.297959
239.304380	7796.725779	27.302976
239.250607	7807.439583	27.307994
239.585298	7815.722044	27.313012
240.040782	7818.678866	27.318029
240.061791	7834.040704	27.323047
240.271529	7848.672327	27.328064
240.902790	7858.332422	27.333082
240.885819	7874.912478	27.338100
241.249015	7881.173233	27.343117
241.389271	7887.430815	27.348135
241.616816	7902.533253	27.353152
242.130582	7906.636466	27.358170
242.149588	7918.702814	27.363188
242.922195	7919.318322	27.368205
243.047700	7921.572020	27.373223
243.191931	7943.506517	27.378240
243.440225	7949.333737	27.383258
243.514781	7944.804720	27.388276
243.880652	7951.311327	27.393293
244.062674	7971.121643	27.398311
244.145301	7975.367762	27.403328
244.225765	7992.958773	27.408346
244.329885	8003.619696	27.413364
244.886416	8004.685571	27.418381
245.164813	8013.027397	27.423399
245.374234	8024.435928	27.428416
245.285889	8023.960569	27.433434
245.627054	8033.492288	27.438452
246.186635	8049.082997	27.443469
246.284254	8051.697793	27.448487
246.073321	8062.710871	27.453504
246.611427	8074.860667	27.458522
246.631171	8094.472234	27.463540
246.989478	8089.056087	27.468557
247.380532	8113.942037	27.473575
247.606397	8118.241657	27.478592
247.943996	8127.180462	27.483610
248.051513	8139.214232	27.488628
248.812526	8141.154340	27.493645
248.887392	8156.631185	27.498663
248.864869	8161.973414	27.503680
249.222367	8171.499504	27.508698
248.921049	8188.436656	27.513716
249.682699	8198.130301	27.518733
249.856719	8223.217509	27.523751
250.215428	8235.051226	27.528768
250.783833	8233.880094	27.533786
250.704752	8254.823696	27.538804
250.901987	8262.692089	27.543821
251.330306	8283.086330	27.548839
251.626140	8287.933891	27.553856
251.911897	8294.891920	27.558874
251.694052	8311.554155	27.563892
252.322916	8320.498221	27.568909
253.122154	8333.658827	27.573927
252.776937	8333.561255	27.578944
252.977724	8347.648500	27.583962
253.240942	8360.595815	27.588980
253.626129	8377.479930	27.593997
254.218695	8388.579629	27.599015
253.676075	8394.504869	27.604032
254.333021	8408.300150	27.609050
254.361052	8423.367779	27.614068
254.763416	8435.545261	27.619085
255.155708	8447.247604	27.624103
255.248656	8467.375399	27.629120
255.914429	8469.971255	27.634138
256.204999	8486.646049	27.639156
256.506296	8487.454926	27.644173
256.838329	8492.521057	27.649191
256.884237	8492.886663	27.654208
257.463867	8497.229165	27.659226
257.582724	8518.382186	27.664244
257.602944	8518.142478	27.669261
257.560985	8513.382054	27.674279
257.941533	8532.688506	27.679296
258.186300	8537.013695	27.684314
258.364015	8555.155217	27.689332
258.257365	8556.911591	27.694349
258.437008	8585.373332	27.699367
259.037525	8602.078903	27.704384
259.799515	8605.587983	27.709402
259.707601	8619.970416	27.714420
260.195928	8628.219853	27.719437
260.255062	8637.363272	27.724455
260.558557	8656.126201	27.729472
260.767215	8658.783781	27.734490
260.950503	8673.088682	27.739508
261.172239	8687.397080	27.744525
261.411877	8693.396367	27.749543
261.724360	8716.527386	27.754560
262.201173	8715.162117	27.759578
262.106011	8736.898044	27.764596
262.433351	8746.214445	27.769613
262.599255	8753.188149	27.774631
262.805086	8768.806130	27.779648
262.676105	8783.428087	27.784666
263.241435	8802.655540	27.789684
263.135210	8806.132501	27.794701
263.585634	8832.206725	27.799719
263.910796	8851.897832	27.804736
264.297244	8858.568885	27.809754
264.660483	8883.734874	27.814772
264.763646	8896.331784	27.819789
265.041566	8912.128091	27.824807
265.004059	8933.687945	27.829824
265.573181	8948.782261	27.834842
265.852415	8968.827928	27.839860
266.427766	8967.172629	27.844877
267.206032	8972.987122	27.849895
267.261231	8991.722748	27.854912
267.501499	8987.454979	27.859930
267.477130	9011.952186	27.864948
267.791517	9018.407201	27.869965
268.341494	9034.000241	27.874983
267.924980	9049.276504	27.880000
268.395221	9058.507671	27.885018
268.772868	9078.074033	27.890036
268.812099	9088.363667	27.895053
269.572029	9098.645291	27.900071
269.669863	9129.207495	27.905088
269.970246	9133.603095	27.910106
270.374980	9153.563124	27.915124
270.486890	9162.850130	27.920141
270.886162	9173.544707	27.925159
270.996663	9190.374458	27.930176
271.236215	9200.437222	27.935194
271.635973	9215.747556	27.940212
271.782416	9227.286609	27.945229
271.917084	9237.889817	27.950247
272.374055	9265.516972	27.955264
272.665251	9271.110614	27.960282
272.923723	9284.150874	27.965300
273.271812	9303.561059	27.970317
273.533751	9310.100114	27.975335
273.719564	9330.119674	27.980352
274.151152	9340.638827	27.985370
274.401707	9357.917350	27.990388
274.496172	9368.586878	27.995405
274.771976	9381.769741	28.000423
274.910211	9401.998847	28.005440
275.345305	9410.237980	28.010458
275.475745	9433.167760	28.015476
275.846710	9445.072962	28.020493
276.069510	9455.997239	28.025511
276.224721	9473.208625	28.030528
276.632722	9492.246598	28.035546
276.912490	9511.686580	28.040564
277.344616	9528.447621	28.045581
277.917291	9539.945769	28.050599
277.754103	9551.640576	28.055616
278.220908	9562.637432	28.060634
278.248564	9589.204770	28.065652
278.393662	9609.890836	28.070669
279.332393	9613.666222	28.075687
279.457874	9635.779295	28.080704
279.535826	9634.794942	28.085722
279.931491	9662.621670	28.090740
280.259490	9663.375928	28.095757
280.609732	9672.060934	28.100775
280.662403	9685.550277	28.105792
281.100639	9692.687160	28.110810
281.173111	9706.533364	28.115828
281.210106	9713.994777	28.120845
282.035691	9722.817340	28.125863
281.743291	9743.732689	28.130880
282.310092	9760.987610	28.135898
282.538055	9777.499664	28.140916
282.697143	9786.969075	28.145933
283.409189	9796.882828	28.150951
283.401718	9814.220891	28.155968
283.872354	9825.315183	28.160986
284.283954	9834.609542	28.166004
284.223329	9846.544307	28.171021
284.987209	9857.210932	28.176039
284.911901	9868.434448	28.181056
285.329140	9876.768131	28.186074
285.263133	9895.599315	28.191092
285.264098	9918.407771	28.196109
285.981735	9936.924399	28.201127
285.807552	9945.245998	28.206144
286.333805	9964.133438	28.211162
286.655437	9980.220638	28.216180
287.310970	9998.781726	28.221197
287.601655	10008.878014	28.226215
288.027399	10023.843980	28.231232
288.009006	10034.667226	28.236250
288.107399	10051.673296	28.241268
288.543452	10070.514898	28.246285
289.512542	10062.221480	28.251303
290.205074	10063.948293	28.256320
290.708937	10076.079483	28.261338
290.985830	10067.795950	28.266356
291.158920	10072.906206	28.271373
291.386213	10067.576189	28.276391
291.284704	10074.481518	28.281408
291.980124	10085.913537	28.286426
292.500417	10087.967115	28.291444
291.921572	10096.954833	28.296461
292.084647	10092.020003	28.301479
292.401795	10102.484788	28.306496
292.447531	10122.116555	28.311514
293.121074	10137.350296	28.316532
293.269866	10154.108655	28.321549
293.494331	10161.743132	28.326567
293.678028	10188.182840	28.331584
293.866786	10193.328579	28.336602
294.125890	10205.592680	28.341620
294.339742	10220.705458	28.346637
294.766392	10224.863803	28.351655
294.852529	10253.929932	28.356672
295.028956	10269.989472	28.361690
295.322375	10283.662783	28.366708
295.523147	10311.618704	28.371725
296.088403	10321.732406	28.376743
295.991944	10342.166414	28.381760
296.741179	10367.173287	28.386778
296.883907	10387.472228	28.391796
297.196981	10406.958481	28.396813
297.330681	10416.094324	28.401831
298.099802	10443.879868	28.406848
297.947559	10460.723258	28.411866
298.863541	10473.229426	28.416884
298.816378	10488.739844	28.421901
299.064056	10505.391558	28.426919
299.665946	10517.883508	28.431936
299.999901	10530.852902	28.436954
300.254713	10540.974009	28.441972
300.809248	10557.947415	28.446989
300.792431	10558.742765	28.452007
300.929503	10577.896652	28.457024
301.385508	10592.125843	28.462042
301.849191	10597.876164	28.467060
301.759376	10617.908447	28.472077
301.751718	10630.463796	28.477095
301.997252	10650.121847	28.482112
302.197163	10665.634993	28.487130
302.923111	10686.560199	28.492148
303.297097	10706.706659	28.497165
303.730530	10706.361545	28.502183
303.909099	10727.179412	28.507200
304.526683	10727.648667	28.512218
305.225615	10726.135010	28.517236
305.679154	10739.300639	28.522253
305.819350	10761.668511	28.527271
306.202313	10760.005124	28.532288
306.186837	10755.539959	28.537306
306.700981	10776.409833	28.542324
306.720750	10798.998576	28.547341
306.924125	10795.130822	28.552359
307.461257	10826.751477	28.557376
307.625890	10832.475807	28.562394
308.086403	10845.024719	28.567412
308.153551	10858.796830	28.572429
308.373117	10870.679156	28.577447
308.603144	10879.686561	28.582464
308.751184	10900.979838	28.587482
309.465542	10921.929217	28.592500
309.393750	10947.159415	28.597517
309.961381	10957.759347	28.602535
310.048085	10980.978858	28.607552
310.049733	10999.844827	28.612570
310.721016	11010.267620	28.617588
310.864364	11030.636630	28.622605
311.235512	11056.489508	28.627623
312.037810	11076.471804	28.632640
311.953850	11095.098597	28.637658
312.294368	11111.742714	28.642676
312.157443	11129.727340	28.647693
312.603699	11140.302067	28.652711
313.184957	11162.342836	28.657728
313.218865	11189.312485	28.662746
313.479113	11205.356623	28.667764
314.133354	11234.414769	28.672781
314.548474	11247.109951	28.677799
315.499092	11252.809929	28.682816
315.877073	11260.717765	28.687834
316.650895	11261.626869	28.692852
317.038800	11261.724575	28.697869
317.155516	11262.312872	28.702887
317.257084	11273.860181	28.707904
317.290482	11286.810586	28.712922
317.660433	11291.448473	28.717940
317.626210	11316.310203	28.722957
318.210912	11319.459036	28.727975
318.192974	11341.830118	28.732992
318.530826	11347.928648	28.738010
318.622720	11363.784418	28.743028
319.275817	11386.142653	28.748045
319.197764	11404.550962	28.753063
319.616622	11416.667844	28.758080
319.783450	11430.484850	28.763098
320.410562	11438.641314	28.768116
321.246698	11453.332982	28.773133
321.173172	11475.580260	28.778151
321.157383	11483.770525	28.783168
321.598544	11498.129023	28.788186
321.797343	11511.180135	28.793204
322.027107	11537.074635	28.798221
322.573475	11542.572401	28.803239
323.183141	11562.433645	28.808256
323.053515	11566.666267	28.813274
323.377980	11575.059364	28.818292
323.490680	11597.868264	28.823309
323.808553	11616.868763	28.828327
324.234839	11635.634530	28.833344
324.269017	11650.896427	28.838362
325.033271	11670.149562	28.843380
325.073856	11696.664207	28.848397
325.262826	11716.057473	28.853415
325.814057	11735.053339	28.858432
325.859605	11762.385126	28.863450
326.806109	11764.388331	28.868468
327.228169	11792.908806	28.873485
327.607618	11798.786289	28.878503
328.111208	11809.936632	28.883520
328.431280	11825.842526	28.888538
328.833964	11839.834676	28.893556
329.312989	11842.532722	28.898573
329.205212	11858.498937	28.903591
329.668061	11865.617039	28.908608
330.014645	11879.646372	28.913626
330.357883	11894.351972	28.918644
330.421968	11913.837511	28.923661
330.547614	11930.961038	28.928679
331.231644	11946.541972	28.933696
331.449987	11965.649893	28.938714
331.963425	11991.074573	28.943732
332.181488	12000.428566	28.948749
332.088600	12014.548522	28.953767
332.680769	12027.775578	28.958784
332.577072	12050.189274	28.963802
333.030209	12071.591109	28.968820
333.294951	12091.162427	28.973837
333.706019	12118.917794	28.978855
334.212249	12133.415061	28.983872
334.638517	12155.702168	28.988890
335.111906	12156.809664	28.993908
335.375733	12185.093282	28.998925
335.576623	12204.734655	29.003943
336.173576	12220.016761	29.008960
336.496843	12240.734841	29.013978
337.209791	12253.962200	29.018996
337.565720	12274.684705	29.024013
337.728268	12279.042517	29.029031
338.480337	12288.389303	29.034048
338.464449	12303.220603	29.039066
338.989882	12304.263167	29.044084
339.136583	12332.151581	29.049101
339.465183	12339.634956	29.054119
339.906623	12350.940553	29.059136
340.294913	12363.252271	29.064154
340.560898	12379.498616	29.069172
340.945404	12386.057565	29.074189
341.066653	12407.691443	29.079207
341.551668	12411.793830	29.084224
341.544120	12433.583572	29.089242
341.886388	12440.815399	29.094260
342.147688	12461.278119	29.099277
342.469374	12495.922356	29.104295
343.099385	12502.294711	29.109312
343.106483	12517.571001	29.114330
343.673180	12536.249497	29.119348
343.922861	12558.466684	29.124365
344.277655	12570.310090	29.129383
345.334592	12569.956297	29.134400
345.501776	12577.089124	29.139418
345.690962	12582.336504	29.144436
345.869317	12592.056959	29.149453
345.940751	12605.880209	29.154471
346.466631	12619.822185	29.159488
346.516784	12641.394771	29.164506
346.891578	12654.937154	29.169524
347.146925	12660.673183	29.174541
347.408760	12694.262934	29.179559
347.886802	12705.894613	29.184576
348.092120	12733.468191	29.189594
348.397930	12748.309757	29.194612
348.862978	12758.427754	29.199629
349.401343	12786.956895	29.204647
349.716569	12804.029598	29.209664
349.863142	12833.911344	29.214682
350.150545	12850.757901	29.219700
350.655155	12869.440079	29.224717
350.991605	12880.171830	29.229735
351.645081	12898.549816	29.234752
351.824999	12922.777189	29.239770
352.234061	12942.159560	29.244788
352.476561	12953.401757	29.249805
352.801987	12981.891715	29.254823
353.214269	13003.433600	29.259840
353.395288	13019.014791	29.264858
353.830963	13036.324737	29.269876
354.540588	13059.332998	29.274893
354.726413	13077.338709	29.279911
355.280365	13085.902016	29.284928
355.307655	13117.530121	29.289946
355.569447	13135.328274	29.294964
356.287843	13152.840624	29.299981
356.245830	13174.361853	29.304999
356.834762	13195.926983	29.310016
357.092563	13205.805911	29.315034
357.453068	13238.942327	29.320052
357.995104	13249.001236	29.325069
358.257902	13276.399291	29.330087
358.861241	13288.504453	29.335104
359.047936	13314.663893	29.340122
359.420851	13331.582830	29.345140
359.906166	13344.631663	29.350157
359.962926	13372.339828	29.355175
360.342590	13394.676711	29.360192
360.970919	13409.253849	29.365210
361.238440	13427.641912	29.370228
361.885007	13432.398323	29.375245
361.804443	13454.939559	29.380263
362.279126	13477.659643	29.385280
362.798168	13492.039122	29.390298
363.127626	13515.078704	29.395316
363.570227	13533.196454	29.400333
363.712801	13553.473578	29.405351
363.960613	13579.911241	29.410368
364.619505	13592.702694	29.415386
364.688327	13618.211424	29.420404
365.239111	13636.606119	29.425421
365.379263	13658.721651	29.430439
365.674624	13668.294969	29.435456
366.116032	13710.732383	29.440474
366.462331	13730.617975	29.445492
367.067234	13746.954842	29.450509
366.809907	13773.130357	29.455527
367.485716	13789.503591	29.460544
367.819571	13806.343770	29.465562
367.828664	13830.529424	29.470580
368.850547	13842.077140	29.475597
368.909573	13869.987789	29.480615
369.167930	13882.225991	29.485632
369.892375	13899.775990	29.490650
370.010637	13920.117294	29.495668
370.332181	13932.358322	29.500685
370.963931	13967.667533	29.505703
370.991164	13989.532602	29.510720
371.784203	14012.617463	29.515738
371.773187	14038.334983	29.520756
372.351195	14050.463527	29.525773
372.486668	14072.491847	29.530791
372.914743	14099.502192	29.535808
373.115840	14117.948637	29.540826
373.710790	14152.941804	29.545844
374.010853	14166.891660	29.550861
374.214735	14193.097007	29.555879
374.852117	14222.756107	29.560896
375.156749	14240.037029	29.565914
375.424334	14261.347074	29.570932
375.976831	14284.112857	29.575949
376.774725	14303.117128	29.580967
377.313390	14310.568584	29.585984
377.947641	14326.307671	29.591002
378.130218	14350.855419	29.596020
378.297513	14365.129264	29.601037
378.702891	14382.966240	29.606055
379.109049	14402.682157	29.611072
379.688681	14417.195021	29.616090
380.037589	14431.911193	29.621108
380.594710	14439.438779	29.626125
380.807825	14465.245148	29.631143
381.906525	14457.412839	29.636160
382.610554	14456.138127	29.641178
382.831796	14473.002746	29.646196
383.270335	14476.550688	29.651213
383.443818	14484.475931	29.656231
383.729709	14489.831953	29.661248
384.129238	14496.604051	29.666266
383.935231	14517.752548	29.671284
384.625423	14527.830131	29.676301
384.870405	14552.245259	29.681319
385.104780	14559.614705	29.686336
385.489279	14572.809564	29.691354
385.844097	14595.502280	29.696372
386.317614	14604.764109	29.701389
386.726551	14639.158672	29.706407
386.533267	14648.110620	29.711424
387.219116	14674.630045	29.716442
387.260904	14694.472471	29.721460
387.834915	14712.536153	29.726477
387.905269	14725.543166	29.731495
388.527223	14746.170122	29.736512
388.959686	14776.079900	29.741530
388.698532	14802.118468	29.746548
389.084721	14821.834772	29.751565
389.855089	14856.018710	29.756583
390.196458	14880.261347	29.761600
390.720767	14905.751424	29.766618
390.799935	14935.094299	29.771636
391.499499	14960.437156	29.776653
391.431182	14988.126094	29.781671
391.777819	15013.445012	29.786688
392.225044	15042.219129	29.791706
392.973080	15073.804606	29.796724
393.498070	15099.237990	29.801741
393.904368	15120.884277	29.806759
394.286638	15142.442743	29.811776
395.022460	15158.059331	29.816794
395.214968	15176.966078	29.821812
395.532561	15180.855117	29.826829
396.002179	15207.851096	29.831847
396.076039	15231.049407	29.836864
396.582974	15241.020097	29.841882
396.610435	15271.464276	29.846900
397.440412	15287.517936	29.851917
397.787187	15312.584574	29.856935
398.281872	15338.465144	29.861952
398.816349	15360.859196	29.866970
398.906078	15388.003002	29.871988
399.177706	15409.032622	29.877005
399.637568	15428.902313	29.882023
399.809950	15450.667505	29.887040
400.719812	15472.924293	29.892058
400.988823	15501.341543	29.897076
401.431324	15519.830721	29.902093
402.006285	15544.675803	29.907111
402.502009	15570.651274	29.912128
402.909649	15585.352880	29.917146
403.266756	15620.730026	29.922164
403.521141	15613.919328	29.927181
404.389496	15629.799915	29.932199
404.782453	15653.669145	29.937216
405.101886	15666.379045	29.942234
405.141771	15691.756094	29.947252
406.085400	15709.725281	29.952269
406.232652	15727.161545	29.957287
406.486563	15754.839327	29.962304
407.280652	15771.385359	29.967322
407.830194	15787.344136	29.972340
408.600677	15795.650727	29.977357
408.862437	15817.096069	29.982375
408.610126	15824.109087	29.987392
409.532811	15839.716094	29.992410
409.451203	15869.041217	29.997428
410.254099	15883.902600	30.002445
410.542392	15893.989789	30.007463
410.543680	15930.354603	30.012480
411.063749	15944.227296	30.017498
411.220752	15962.376035	30.022516
411.545161	15983.641261	30.027533
412.287812	16015.396528	30.032551
412.744384	16045.778293	30.037568
412.868026	16058.853718	30.042586
413.260858	16078.709255	30.047604
413.618279	16104.896485	30.052621
414.355802	16133.595471	30.057639
414.597797	16162.340060	30.062656
414.889848	16185.991946	30.067674
415.339275	16215.629721	30.072692
415.945835	16241.421456	30.077709
416.123038	16269.481453	30.082727
416.447037	16288.144584	30.087744
417.114399	16321.323873	30.092762
417.041905	16355.632241	30.097780
417.491432	16373.900066	30.102797
418.362093	16402.490293	30.107815
418.528791	16428.347600	30.112832
419.066812	16443.335933	30.117850
419.595856	16478.428908	30.122868
420.230909	16507.886633	30.127885
421.190617	16524.799179	30.132903
421.579055	16541.437458	30.137920
422.265003	16543.500720	30.142938
422.658983	16556.367003	30.147956
422.950657	16567.467872	30.152973
423.607255	16574.923971	30.157991
423.170787	16588.617570	30.163008
423.616377	16599.738714	30.168026
423.800433	16614.968634	30.173044
424.183413	16639.093321	30.178061
424.913500	16658.236843	30.183079
425.060546	16691.162981	30.188096
425.396955	16700.943053	30.193114
425.726245	16727.542951	30.198132
426.159295	16753.867741	30.203149
426.339859	16780.386637	30.208167
426.563823	16802.227455	30.213184
427.263684	16831.533457	30.218202
427.625564	16864.334851	30.223220
427.876544	16898.363261	30.228237
428.389503	16920.528763	30.233255
428.997854	16947.549818	30.238272
429.351885	16970.687665	30.243290
430.129569	17004.318416	30.248308
430.619506	17032.122380	30.253325
431.173463	17056.151486	30.258343
431.432273	17089.578900	30.263360
432.289737	17109.859056	30.268378
432.248250	17132.022680	30.273396
432.789187	17151.142447	30.278413
433.373882	17167.886532	30.283431
433.539225	17198.201754	30.288448
434.051524	17218.706320	30.293466
434.875174	17252.889410	30.298484
434.942155	17271.388205	30.303501
435.708444	17292.166004	30.308519
435.999697	17324.786506	30.313536
436.530731	17347.824604	30.318554
436.860959	17363.556680	30.323572
437.223757	17400.578667	30.328589
438.396185	17401.571346	30.333607
439.062208	17412.639695	30.338624
440.033758	17432.712918	30.343642
439.965700	17437.925884	30.348660
440.097671	17448.998430	30.353677
440.530408	17467.841610	30.358695
440.646999	17484.305087	30.363712
441.479617	17499.747438	30.368730
442.007966	17510.985729	30.373748
442.398735	17533.363634	30.378765
443.128789	17551.418345	30.383783
443.244377	17569.461340	30.388800
443.777961	17582.707718	30.393818
444.028876	17604.867426	30.398836
444.360080	17620.394251	30.403853
444.750230	17641.009884	30.408871
444.753532	17666.474198	30.413888
445.333263	17689.776764	30.418906
445.781247	17719.000147	30.423924
446.044320	17745.662299	30.428941
446.276414	17771.501753	30.433959
446.796039	17810.101530	30.438976
447.268377	17829.756983	30.443994
447.826808	17856.114298	30.449012
448.511157	17891.226735	30.454029
449.202572	17908.340206	30.459047
449.357746	17924.621167	30.464064
449.855910	17946.818583	30.469082
450.290146	17973.890297	30.474100
450.839505	17990.886975	30.479117
451.060647	18009.829958	30.484135
451.678574	18034.611563	30.489152
451.745568	18053.957626	30.494170
452.366748	18073.526982	30.499188
452.398426	18103.731770	30.504205
452.581079	18133.862563	30.509223
453.135932	18157.946602	30.514240
453.927374	18191.773124	30.519258
454.102851	18217.337706	30.524276
454.563232	18239.440263	30.529293
455.463051	18262.510486	30.534311
455.558558	18297.506857	30.539328
455.773291	18331.859307	30.544346
456.532864	18356.341307	30.549364
456.856026	18387.132901	30.554381
457.842129	18407.517591	30.559399
458.060975	18440.959882	30.564416
458.546625	18466.729204	30.569434
459.149700	18491.159929	30.574452
459.242366	18519.372185	30.579469
460.175597	18543.606276	30.584487
460.226562	18570.934334	30.589504
460.590136	18603.052970	30.594522
461.229586	18642.905572	30.599540
461.457116	18674.900204	30.604557
462.416507	18688.118958	30.609575
462.810182	18721.540833	30.614592
463.006738	18752.700182	30.619610
464.303855	18771.248971	30.624628
464.647750	18789.415500	30.629645
465.799802	18806.969779	30.634663
466.272692	18833.354380	30.639680
466.445747	18844.004369	30.644698
466.951459	18867.105081	30.649716
467.335099	18889.220326	30.654733
468.041897	18894.625776	30.659751
467.903842	18926.279727	30.664768
468.432708	18940.064769	30.669786
468.881882	18964.867519	30.674804
469.193699	18983.557269	30.679821
470.094340	18996.513723	30.684839
470.397351	19013.467524	30.689856
470.865737	19043.289905	30.694874
471.686334	19060.238982	30.699892
471.567418	19085.863174	30.704909
472.258486	19105.555366	30.709927
472.260319	19133.959550	30.714944
472.950206	19163.760269	30.719962
473.256537	19190.853595	30.724980
473.294095	19226.940988	30.729997
473.991892	19251.680129	30.735015
474.670633	19285.721957	30.740032
474.979123	19316.245647	30.745050
475.401085	19341.312141	30.750068
476.267229	19365.260772	30.755085
477.101099	19376.781113	30.760103
477.524979	19411.355622	30.765120
477.992293	19432.605562	30.770138
478.430001	19449.418736	30.775156
478.980887	19478.142284	30.780173
479.425014	19507.065710	30.785191
479.940527	19526.975194	30.790208
479.985093	19554.640473	30.795226
480.980483	19573.887743	30.800244
480.877760	19607.975979	30.805261
481.230092	19623.949688	30.810279
481.295591	19660.501053	30.815296
482.203681	19694.368899	30.820314
482.892670	19714.422151	30.825332
483.068252	19749.724562	30.830349
483.692067	19762.933118	30.835367
484.059250	19796.095613	30.840384
484.655690	19811.589222	30.845402
484.929409	19836.850016	30.850420
485.490191	19866.893038	30.855437
486.149561	19898.468650	30.860455
486.480794	19924.402940	30.865472
486.682996	19947.331058	30.870490
487.573992	19979.306680	30.875508
487.488999	20007.605611	30.880525
487.984274	20040.938120	30.885543
488.589620	20073.482757	30.890560
488.858274	20113.617227	30.895578
489.527881	20147.965248	30.900596
489.804254	20183.417019	30.905613
490.407021	20214.250110	30.910631
491.467331	20254.299534	30.915648
491.562459	20284.504144	30.920666
492.186136	20318.259400	30.925684
492.501817	20353.383139	30.930701
493.322430	20376.929430	30.935719
493.979274	20402.428261	30.940736
494.277785	20435.766803	30.945754
495.397371	20466.987375	30.950772
495.357003	20495.065247	30.955789
496.018370	20522.282058	30.960807
496.493236	20558.626054	30.965824
496.652611	20588.088226	30.970842
497.657414	20616.205743	30.975860
497.689251	20660.737728	30.980877
498.644367	20678.128503	30.985895
498.734639	20712.030660	30.990912
499.456013	20763.348674	30.995930
500.256055	20774.761386	31.000948
500.351746	20808.151090	31.005965
501.547418	20836.093890	31.010983
501.471130	20864.177882	31.016000
502.322494	20888.667738	31.021018
503.114641	20901.699224	31.026036
503.677328	20934.921670	31.031053
504.709569	20955.118628	31.036071
505.097165	20962.160238	31.041088
505.229734	20991.052226	31.046106
505.952891	21004.871669	31.051124
505.993132	21039.483509	31.056141
506.334328	21061.904786	31.061159
506.620759	21083.311048	31.066176
507.482579	21115.754309	31.071194
508.208572	21140.263999	31.076212
508.341909	21170.204972	31.081229
508.707039	21206.276609	31.086247
509.311285	21228.246433	31.091264
509.689892	21258.016672	31.096282
510.178799	21280.541570	31.101300
511.051577	21315.618216	31.106317
511.292966	21337.221318	31.111335
511.728523	21367.949571	31.116352
512.219211	21404.558045	31.121370
512.486033	21430.359032	31.126388
512.548710	21475.589406	31.131405
513.199459	21506.524475	31.136423
514.198540	21536.362822	31.141440
514.728961	21579.549262	31.146458
515.789172	21609.738356	31.151476
516.101833	21634.635251	31.156493
516.537610	21650.749269	31.161511
516.925099	21688.593805	31.166528
517.070762	21712.821762	31.171546
517.657376	21733.114173	31.176564
518.250291	21767.047313	31.181581
518.941281	21786.363114	31.186599
519.430397	21813.248377	31.191616
519.674065	21851.393631	31.196634
520.160309	21881.015366	31.201652
520.624229	21907.538203	31.206669
520.883083	21936.392963	31.211687
521.514592	21968.007841	31.216704
521.998936	22008.750783	31.221722
522.834427	22044.516943	31.226740
522.961184	22082.478648	31.231757
523.548573	22117.171486	31.236775
523.862669	22146.106413	31.241792
524.469016	22197.951570	31.246810
525.395231	22231.245986	31.251828
525.900852	22265.161980	31.256845
526.256018	22294.987984	31.261863
526.948148	22324.989050	31.266880
527.202980	22376.099560	31.271898
528.209925	22402.829188	31.276916
528.583854	22447.191898	31.281933
529.146211	22479.500785	31.286951
529.893892	22501.664540	31.291968
530.213013	22548.531919	31.296986
530.754045	22588.224633	31.302004
531.348251	22620.086477	31.307021
532.112022	22644.074019	31.312039
532.549369	22677.337874	31.317056
532.812735	22717.421608	31.322074
533.599767	22753.834799	31.327092
533.860863	22779.101339	31.332109
535.257008	22805.303330	31.337127
535.870323	22832.101138	31.342144
536.334194	22867.831860	31.347162
536.946179	22888.260527	31.352180
537.426647	22916.184935	31.357197
537.736532	22939.390445	31.362215
538.490856	22963.392483	31.367232
538.721352	23006.420210	31.372250
539.022178	23033.551290	31.377268
539.800231	23064.311011	31.382285
539.747657	23093.986851	31.387303
540.745856	23123.707681	31.392320
541.238828	23164.502211	31.397338
541.910598	23194.027524	31.402356
542.573321	23226.593723	31.407373
542.521651	23266.936137	31.412391
543.411626	23284.257220	31.417408
543.935245	23331.315779	31.422426
544.901531	23363.386295	31.427444
545.331272	23379.654321	31.432461
545.708909	23411.936616	31.437479
546.332219	23453.659307	31.442496
546.522292	23490.647034	31.447514
547.223335	23521.033990	31.452532
547.835280	23554.088882	31.457549
548.335917	23580.020570	31.462567
549.288841	23612.611735	31.467584
549.528592	23650.925360	31.472602
550.039877	23684.394243	31.477620
550.384606	23714.103944	31.482637
551.049380	23752.522215	31.487655
551.912562	23775.320290	31.492672
552.101120	23828.258456	31.497690
552.946549	23847.419530	31.502708
553.305656	23882.801875	31.507725
553.615063	23916.049807	31.512743
554.225403	23941.598375	31.517760
554.536148	23976.906266	31.522778
554.880501	24000.069734	31.527796
555.684699	24035.029182	31.532813
556.053749	24075.490995	31.537831
556.927155	24097.245171	31.542848
557.309784	24142.393901	31.547866
558.191584	24180.071452	31.552884
558.897318	24208.904184	31.557901
559.129104	24235.636896	31.562919
559.722373	24271.267846	31.567936
560.154232	24307.890845	31.572954
560.209629	24345.779511	31.577972
561.200229	24381.873309	31.582989
561.266161	24422.357736	31.588007
562.293389	24463.943832	31.593024
562.822689	24512.653655	31.598042
562.548944	24543.642600	31.603060
563.808434	24583.252730	31.608077
564.395168	24619.074900	31.613095
565.275709	24661.486811	31.618112
565.703834	24707.754597	31.623130
566.699319	24735.424439	31.628148
567.611553	24765.243262	31.633165
567.960948	24805.475793	31.638183
568.855147	24826.627178	31.643200
569.528436	24857.608208	31.648218
570.136368	24884.630805	31.653236
571.466748	24901.315987	31.658253
571.994611	24920.249474	31.663271
572.472269	24938.476689	31.668288
573.132389	24964.410630	31.673306
573.581494	24987.685327	31.678324
574.407835	25004.328991	31.683341
574.525431	25032.717310	31.688359
575.147595	25050.239618	31.693376
575.336574	25082.162171	31.698394
576.218712	25098.670836	31.703412
577.065723	25119.608694	31.708429
577.392654	25154.890868	31.713447
577.748932	25168.915696	31.718464
578.328601	25210.345516	31.723482
578.466916	25233.877429	31.728500
579.098961	25261.351795	31.733517
579.056704	25302.651116	31.738535
579.793236	25338.457575	31.743552
580.239171	25373.696329	31.748570
580.551328	25419.604633	31.753588
581.504732	25458.006532	31.758605
581.919871	25513.106815	31.763623
582.980197	25544.654309	31.768640
583.272427	25586.963856	31.773658
583.683133	25631.574396	31.778676
584.619190	25665.972674	31.783693
584.884120	25706.087445	31.788711
585.476565	25747.826053	31.793728
586.251891	25779.677395	31.798746
586.722852	25823.849235	31.803764
587.539335	25856.016602	31.808781
587.969757	25900.801624	31.813799
588.824349	25925.183455	31.818816
589.480994	25964.631057	31.823834
589.798045	26010.249234	31.828852
590.653831	26039.573155	31.833869
591.071722	26082.755285	31.838887
591.934261	26122.683055	31.843904
592.890939	26148.193168	31.848922
593.295975	26173.201437	31.853940
593.770976	26191.683002	31.858957
594.077661	26218.457257	31.863975
594.557527	26248.731115	31.868992
595.350747	26274.127795	31.874010
595.759099	26309.727957	31.879028
596.284142	26331.418721	31.884045
596.844052	26366.432912	31.889063
597.144536	26411.214018	31.894080
597.753609	26446.454534	31.899098
598.379512	26485.478182	31.904116
599.111413	26524.668685	31.909133
599.638623	26568.725961	31.914151
599.891955	26602.385239	31.919168
600.586037	26657.837071	31.924186
601.343427	26692.113237	31.929204
602.568646	26728.035698	31.934221
602.633471	26775.932182	31.939239
602.918649	26817.777721	31.944256
603.536271	26856.613772	31.949274
604.131383	26906.905506	31.954292
604.784873	26949.755766	31.959309
605.283845	26999.538124	31.964327
606.097799	27043.804603	31.969344
607.009746	27087.044693	31.974362
607.501433	27138.926835	31.979380
608.628748	27177.071094	31.984397
609.010177	27211.059055	31.989415
609.532169	27245.808902	31.994432
610.169409	27286.336552	31.999450
610.225079	27321.133841	32.004468
611.623802	27366.934306	32.009485
611.984551	27409.584621	32.014503
612.400095	27439.478417	32.019520
613.240801	27487.540212	32.024538
613.959734	27535.134411	32.029556
614.442330	27572.526535	32.034573
615.209201	27610.329540	32.039591
615.971814	27656.653151	32.044608
616.597894	27702.757947	32.049626
617.322072	27738.166087	32.054644
617.902626	27773.760978	32.059661
618.779487	27814.549440	32.064679
619.394711	27833.750169	32.069696
620.156772	27882.071639	32.074714
620.616153	27909.974683	32.079732
621.417854	27927.661164	32.084749
622.097319	27967.311376	32.089767
622.638902	27998.241895	32.094784
623.486911	28039.964413	32.099802
623.663885	28076.627621	32.104820
624.317908	28100.038345	32.109837
624.692822	28144.103791	32.114855
625.332755	28177.623332	32.119872
626.428892	28201.287695	32.124890
626.855613	28251.931325	32.129908
627.805615	28280.371596	32.134925
628.435503	28308.608916	32.139943
628.530487	28351.302578	32.144960
629.648951	28373.389838	32.149978
629.528635	28423.594443	32.154996
630.166204	28457.999700	32.160013
630.608316	28504.994559	32.165031
631.180117	28549.137682	32.170048
631.885299	28586.490699	32.175066
632.654868	28634.528357	32.180084
633.472553	28665.966808	32.185101
633.970312	28709.717280	32.190119
634.500682	28753.671354	32.195136
635.305894	28782.956562	32.200154
635.647861	28821.510604	32.205172
636.432767	28861.285199	32.210189
637.304340	28894.738256	32.215207
637.801088	28935.796725	32.220224
638.495891	28966.837598	32.225242
638.568217	29008.373134	32.230260
639.269185	29042.586205	32.235277
639.745985	29084.811107	32.240295
640.263188	29137.914290	32.245312
640.993221	29183.740779	32.250330
641.452412	29222.884131	32.255348
642.613984	29277.701455	32.260365
643.346903	29320.354718	32.265383
643.374524	29359.622403	32.270400
644.245219	29406.084867	32.275418
644.739335	29448.566981	32.280436
645.557916	29501.990806	32.285453
646.589928	29542.644797	32.290471
646.937656	29588.658126	32.295488
647.499617	29634.069318	32.300506
648.186097	29698.184057	32.305524
648.999993	29732.165786	32.310541
649.658796	29781.051433	32.315559
650.359322	29832.155711	32.320576
651.240457	29862.536832	32.325594
651.495785	29911.283324	32.330612
652.461730	29961.885169	32.335629
653.512785	29999.825354	32.340647
653.928689	30038.218468	32.345664
654.803878	30084.827156	32.350682
655.793011	30122.663428	32.355700
656.686037	30144.806669	32.360717
657.197670	30189.771802	32.365735
657.921068	30228.762162	32.370752
658.686322	30257.657468	32.375770
659.173312	30291.653087	32.380788
659.707086	30331.090359	32.385805
660.519958	30362.911441	32.390823
661.120686	30401.036253	32.395840
661.688846	30439.298953	32.400858
662.434931	30481.592269	32.405876
663.182424	30513.758788	32.410893
663.997830	30545.706183	32.415911
663.951341	30590.714827	32.420928
664.692574	30626.371846	32.425946
665.744029	30672.682612	32.430964
666.466854	30715.036920	32.435981
667.459647	30748.682738	32.440999
667.663891	30784.271913	32.446016
668.841027	30817.743756	32.451034
669.161417	30861.260929	32.456052
669.998261	30886.112941	32.461069
670.445857	30925.337196	32.466087
670.927417	30969.392110	32.471104
671.691309	31007.568501	32.476122
672.307939	31051.842779	32.481140
672.699919	31094.685548	32.486157
673.513830	31136.590363	32.491175
674.025159	31178.378008	32.496192
674.816031	31214.711036	32.501210
675.231916	31267.443555	32.506228
675.790118	31309.344277	32.511245
676.404205	31353.132839	32.516263
676.806809	31405.311482	32.521280
677.705655	31446.141685	32.526298
678.440090	31495.070196	32.531316
679.171680	31533.334767	32.536333
679.795882	31580.162912	32.541351
680.575154	31626.398078	32.546368
681.448272	31654.140663	32.551386
682.265575	31695.793219	32.556404
682.487374	31732.898480	32.561421
683.298763	31764.431160	32.566439
683.581488	31814.442206	32.571456
684.348058	31856.836296	32.576474
684.811512	31907.464242	32.581492
685.779478	31944.453725	32.586509
686.885224	31995.209481	32.591527
687.505809	32041.571423	32.596544
688.461817	32078.392321	32.601562
689.325669	32114.835681	32.606580
689.827029	32153.826309	32.611597
690.183649	32196.423989	32.616615
690.759277	32240.587074	32.621632
691.996490	32287.650121	32.626650
691.852873	32338.329367	32.631668
692.482898	32383.065894	32.636685
693.344351	32444.146399	32.641703
693.825570	32494.595997	32.646720
694.679075	32521.641069	32.651738
694.948205	32579.071628	32.656756
695.978644	32642.339070	32.661773
696.618140	32696.576630	32.666791
697.264198	32753.626574	32.671808
698.190811	32810.152531	32.676826
699.096806	32867.883027	32.681844
699.632118	32929.439297	32.686861
700.781025	32971.529582	32.691879
701.472427	33017.142997	32.696896
702.220900	33060.996423	32.701914
703.208106	33110.053758	32.706932
703.906921	33149.900599	32.711949
704.696809	33191.889167	32.716967
705.027337	33241.946772	32.721984
705.662985	33293.607068	32.727002
706.275757	33338.063834	32.732020
707.044388	33381.250972	32.737037
708.456540	33426.550774	32.742055
708.724310	33485.450772	32.747072
709.761203	33526.914755	32.752090
710.354643	33570.015755	32.757108
711.021707	33610.121304	32.762125
712.007126	33650.784303	32.767143
712.504646	33701.019320	32.772160
712.804945	33737.502669	32.777178
714.003051	33786.844874	32.782196
714.336119	33841.329095	32.787213
714.977241	33890.284078	32.792231
715.697066	33935.130074	32.797248
716.724858	33985.397026	32.802266
717.405350	34035.288244	32.807284
717.570835	34080.473737	32.812301
718.651378	34134.197479	32.817319
719.222252	34183.303173	32.822336
720.495591	34232.539880	32.827354
720.903416	34274.033723	32.832372
721.660974	34320.967384	32.837389
722.722124	34359.697956	32.842407
723.270097	34401.663383	32.847424
724.114283	34447.173936	32.852442
724.880188	34491.647244	32.857460
725.360513	34543.612986	32.862477
726.552020	34580.901115	32.867495
727.061126	34619.667524	32.872512
727.454656	34651.023038	32.877530
728.118779	34684.207943	32.882548
728.799470	34735.074460	32.887565
729.541069	34761.020763	32.892583
730.037849	34804.645148	32.897600
730.598823	34847.349179	32.902618
731.498181	34908.753422	32.907636
732.028727	34951.171561	32.912653
732.769472	34994.353713	32.917671
733.254432	35040.964703	32.922688
734.549680	35087.904888	32.927706
735.173205	35137.308098	32.932724
735.712364	35181.470413	32.937741
736.547706	35229.272841	32.942759
736.835171	35284.178866	32.947776
737.888791	35332.965505	32.952794
738.755874	35385.777263	32.957812
739.120855	35436.814748	32.962829
740.371349	35488.504856	32.967847
741.319593	35547.399530	32.972864
741.906826	35604.833094	32.977882
742.193966	35651.362413	32.982900
742.853521	35699.382953	32.987917
743.734026	35751.232463	32.992935
744.397443	35813.934310	32.997952
745.273261	35860.100564	33.002970
746.206657	35922.899809	33.007988
746.767325	35984.827793	33.013005
747.734638	36026.750139	33.018023
748.899383	36079.074685	33.023040
749.646120	36127.196435	33.028058
750.222947	36185.252840	33.033076
751.100715	36227.138938	33.038093
752.262355	36272.793697	33.043111
752.707056	36317.763460	33.048128
753.458325	36367.617555	33.053146
754.148495	36416.071240	33.058164
755.090682	36462.234797	33.063181
756.011076	36501.174580	33.068199
756.934646	36557.458150	33.073216
757.837986	36598.221814	33.078234
758.620243	36642.128021	33.083252
759.301883	36686.144827	33.088269
760.214521	36721.684383	33.093287
760.660645	36764.707344	33.098304
761.233779	36814.710357	33.103322
762.016411	36855.309932	33.108340
762.169315	36910.234782	33.113357
763.241835	36963.271413	33.118375
764.142399	37016.107309	33.123392
764.802018	37073.192117	33.128410
765.851145	37126.529989	33.133428
766.457431	37178.741832	33.138445
767.189173	37225.546837	33.143463
767.814677	37278.527374	33.148480
768.429375	37330.725632	33.153498
769.340334	37386.937477	33.158516
769.745782	37441.147780	33.163533
770.911549	37497.718621	33.168551
771.804036	37553.857900	33.173568
772.323831	37604.648840	33.178586
773.157774	37658.148004	33.183604
773.557333	37715.970587	33.188621
774.316086	37772.984920	33.193639
774.954165	37838.763536	33.198656
775.813449	37884.677492	33.203674
777.139496	37934.761948	33.208692
777.265150	37993.386735	33.213709
778.261884	38053.437993	33.218727
778.894752	38095.207796	33.223744
779.655266	38134.959568	33.228762
780.860142	38182.780666	33.233780
781.350470	38233.976068	33.238797
782.193070	38284.452778	33.243815
783.077967	38336.061271	33.248832
784.010541	38373.301523	33.253850
784.705550	38417.895262	33.258868
785.724145	38473.068772	33.263885
786.548991	38512.570931	33.268903
787.500863	38568.539207	33.273920
788.051004	38608.261368	33.278938
789.179366	38654.571419	33.283956
789.903782	38710.600767	33.288973
790.359820	38763.655617	33.293991
791.072276	38815.184601	33.299008
791.452845	38871.432310	33.304026
792.316226	38909.727684	33.309044
792.839357	38981.958973	33.314061
793.611041	39037.817394	33.319079
794.639083	39096.589283	33.324096
795.343485	39169.425363	33.329114
796.056193	39224.363842	33.334132
796.533060	39291.790904	33.339149
797.941750	39355.639242	33.344167
798.387469	39418.600547	33.349184
799.636760	39477.762735	33.354202
800.698513	39522.592571	33.359220
801.277991	39583.408685	33.364237
802.325748	39641.603506	33.369255
803.057636	39700.448435	33.374272
803.551913	39759.368456	33.379290
804.676720	39807.370052	33.384308
805.566013	39880.546540	33.389325
806.477307	39939.452727	33.394343
806.890963	39992.915607	33.399360
807.643324	40055.653954	33.404378
808.458114	40112.438084	33.409396
809.425440	40182.947311	33.414413
809.864594	40239.708034	33.419431
810.952598	40310.122999	33.424448
811.960075	40371.867595	33.429466
812.774993	40424.554439	33.434484
813.281999	40495.117362	33.439501
814.332269	40550.999562	33.444519
815.077264	40610.003022	33.449536
815.767767	40672.879266	33.454554
817.219652	40739.362188	33.459572
817.492629	40804.972666	33.464589
818.604877	40855.419727	33.469607
819.442146	40913.005641	33.474624
820.355489	40970.529269	33.479642
821.305434	41031.114682	33.484660
821.883956	41099.568731	33.489677
822.810620	41150.292017	33.494695
823.789209	41195.833944	33.499712
824.702034	41256.160135	33.504730
825.792081	41310.589791	33.509748
826.074760	41370.609624	33.514765
827.064210	41419.881779	33.519783
828.317943	41479.143597	33.524800
828.864111	41537.813695	33.529818
829.533659	41581.089752	33.534836
830.384180	41642.856058	33.539853
831.415639	41695.183387	33.544871
832.345765	41745.534366	33.549888
832.954479	41806.668367	33.554906
833.824068	41853.594751	33.559924
834.333852	41906.218829	33.564941
834.975040	41948.949784	33.569959
835.641329	41999.215924	33.574976
836.069726	42064.255737	33.579994
837.027909	42108.088751	33.585012
837.851557	42173.687182	33.590029
838.643945	42237.184537	33.595047
840.044385	42283.238614	33.600064
840.532706	42344.354905	33.605082
841.350426	42407.621118	33.610100
842.023306	42469.739969	33.615117
843.059663	42528.766499	33.620135
844.002111	42587.763531	33.625152
844.479377	42668.856305	33.630170
845.145903	42721.299814	33.635188
845.981865	42796.809277	33.640205
846.487719	42857.791441	33.645223
847.579369	42925.633692	33.650240
848.589661	43003.241905	33.655258
849.460901	43068.981071	33.660276
850.739188	43144.486120	33.665293
851.466572	43212.278432	33.670311
852.868888	43270.275929	33.675328
853.562786	43331.805709	33.680346
854.625478	43383.961422	33.685364
855.551787	43450.787390	33.690381
856.481422	43508.384711	33.695399
857.379730	43558.839673	33.700416
857.866731	43623.115947	33.705434
858.914351	43682.624523	33.710452
859.560485	43752.682895	33.715469
860.465526	43818.570833	33.720487
861.739193	43878.898651	33.725504
862.380895	43943.619839	33.730522
863.670075	43996.646249	33.735540
864.438086	44061.278541	33.740557
865.242719	44127.220978	33.745575
866.456635	44177.836956	33.750592
866.789099	44243.125829	33.755610
868.028673	44304.067342	33.760628
868.533475	44355.635379	33.765645
869.664951	44412.590073	33.770663
870.603795	44470.865276	33.775680
870.946013	44531.744689	33.780698
871.882800	44592.424182	33.785716
872.754654	44659.730351	33.790733
873.412219	44735.894087	33.795751
874.534636	44794.217468	33.800768
874.947417	44865.675649	33.805786
876.371631	44933.219262	33.810804
877.552277	44996.645121	33.815821
878.133461	45060.120198	33.820839
879.002397	45122.114759	33.825856
879.865010	45185.989174	33.830874
880.983135	45257.712023	33.835892
881.628992	45317.268541	33.840909
882.246082	45381.788995	33.845927
883.159004	45437.300132	33.850944
884.513331	45499.934983	33.855962
885.421461	45565.049554	33.860980
886.936854	45624.496838	33.865997
887.877036	45683.711208	33.871015
888.677307	45734.009246	33.876032
889.142174	45792.292101	33.881050
889.822992	45851.800319	33.886068
890.650334	45911.323842	33.891085
891.386899	45973.986600	33.896103
892.450667	46015.350174	33.901120
893.318438	46085.406678	33.906138
894.253390	46135.317754	33.911156
895.245635	46174.516663	33.916173
895.687596	46230.375091	33.921191
896.512951	46284.440682	33.926208
897.144341	46350.625408	33.931226
898.488882	46409.753449	33.936244
899.379539	46472.880710	33.941261
899.808286	46538.376375	33.946279
900.964882	46598.033918	33.951296
901.745884	46660.255181	33.956314
902.181344	46726.990245	33.961332
903.338578	46792.727508	33.966349
903.975146	46861.101737	33.971367
905.092262	46932.102602	33.976384
905.974440	47006.644918	33.981402
906.966882	47083.498327	33.986420
907.875773	47150.749277	33.991437
908.430666	47222.167531	33.996455
909.611530	47304.508769	34.001472
910.409896	47378.192346	34.006490
911.267112	47448.400234	34.011508
912.467453	47519.839154	34.016525
913.201299	47597.158422	34.021543
914.363527	47667.262573	34.026560
914.901951	47749.673804	34.031578
915.880607	47814.967368	34.036596
916.678753	47906.815570	34.041613
917.766090	47991.400739	34.046631
918.664970	48060.674063	34.051648
919.596193	48145.872463	34.056666
920.612866	48220.954565	34.061684
921.607760	48298.659458	34.066701
922.766788	48387.334485	34.071719
923.651218	48450.639052	34.076736
925.003913	48513.219272	34.081754
926.194661	48588.496920	34.086772
927.233227	48650.468458	34.091789
927.695094	48727.871869	34.096807
929.085447	48776.401964	34.101824
930.209465	48852.424756	34.106842
931.031298	48923.743543	34.111860
932.321303	48983.348648	34.116877
932.999767	49051.318050	34.121895
934.257268	49112.592465	34.126912
934.843303	49186.972933	34.131930
935.779556	49246.317456	34.136948
936.699727	49305.506468	34.141965
937.113339	49385.924819	34.146983
938.288417	49443.979982	34.152000
939.235822	49522.006449	34.157018
939.974972	49595.390084	34.162036
941.043191	49659.415960	34.167053
942.268028	49733.097716	34.172071
942.914203	49795.449784	34.177088
943.717409	49870.937504	34.182106
944.632477	49932.216805	34.187124
945.547707	50008.699845	34.192141
946.383953	50088.396871	34.197159
947.638448	50156.716447	34.202176
948.635289	50232.099289	34.207194
949.321141	50300.064918	34.212212
950.849455	50370.006508	34.217229
951.490804	50431.291786	34.222247
952.377860	50507.281035	34.227264
953.397664	50576.878497	34.232282
954.334411	50642.313212	34.237300
955.386290	50695.202498	34.242317
956.422459	50753.225654	34.247335
957.952807	50802.826527	34.252352
958.421514	50856.787669	34.257370
959.231715	50924.451063	34.262388
960.074458	50969.717650	34.267405
960.714182	51046.816473	34.272423
961.972233	51103.464604	34.277440
962.704565	51169.533721	34.282458
963.489541	51236.379412	34.287476
964.600090	51303.952874	34.292493
965.428387	51362.636322	34.297511
966.412610	51425.066727	34.302528
967.499257	51498.225170	34.307546
968.051970	51564.437267	34.312564
969.296256	51643.968587	34.317581
969.975520	51719.222229	34.322599
971.083258	51798.958830	34.327616
972.247425	51861.564879	34.332634
973.020460	51936.848923	34.337652
974.064355	52016.254527	34.342669
974.795520	52087.768073	34.347687
976.187077	52168.183099	34.352704
977.243682	52240.310846	34.357722
978.484948	52315.219508	34.362740
979.707032	52379.355536	34.367757
980.495504	52450.557554	34.372775
981.332311	52521.676335	34.377792
982.868585	52586.112044	34.382810
983.718425	52660.937214	34.387828
984.734947	52719.746658	34.392845
985.625892	52796.457836	34.397863
986.573249	52875.906712	34.402880
987.516246	52937.784434	34.407898
988.052830	53020.847598	34.412916
989.409870	53092.874270	34.417933
990.357008	53166.762061	34.422951
991.220047	53238.106742	34.427968
992.007373	53325.061524	34.432986
992.825636	53405.342256	34.438004
994.194518	53479.620992	34.443021
994.964540	53563.263547	34.448039
995.999932	53645.681771	34.453056
997.285877	53722.454731	34.458074
997.986778	53801.204742	34.463092
999.197599	53875.604257	34.468109
1000.394580	53967.351213	34.473127
1000.975435	54042.583366	34.478144
1002.296062	54108.271822	34.483162
1003.194039	54199.971309	34.488180
1004.416318	54272.218754	34.493197
1005.388588	54352.048440	34.498215
1006.379784	54425.945995	34.503232
1007.596189	54502.219749	34.508250
1008.365636	54587.119008	34.513268
1009.543640	54660.874314	34.518285
1010.467297	54731.037051	34.523303
1011.424108	54813.383004	34.528320
1012.695131	54893.035125	34.533338
1013.388872	54967.676786	34.538356
1014.600487	55041.541959	34.543373
1015.637853	55117.636739	34.548391
1016.964425	55193.193136	34.553408
1018.595604	55227.935150	34.558426
1019.736154	55299.957989	34.563444
1021.016274	55358.505190	34.568461
1021.928436	55423.735640	34.573479
1022.918733	55484.505234	34.578496
1023.622876	55541.003541	34.583514
1024.496950	55591.868534	34.588532
1025.304194	55645.731068	34.593549
1026.176797	55705.158932	34.598567
1026.976963	55755.940854	34.603584
1027.985572	55820.676419	34.608602
1028.801746	55896.814461	34.613620
1029.770412	55949.595695	34.618637
1030.601037	56024.016863	34.623655
1031.536825	56091.681965	34.628672
1032.242906	56164.635744	34.633690
1033.336098	56247.003421	34.638708
1034.398945	56320.636264	34.643725
1035.421375	56400.072671	34.648743
1036.233143	56481.636926	34.653760
1037.185964	56565.748954	34.658778
1038.114302	56660.883392	34.663796
1039.144834	56738.389404	34.668813
1040.525306	56825.068535	34.673831
1041.344774	56913.702298	34.678848
1042.458744	57000.765305	34.683866
1043.483296	57091.570230	34.688884
1044.307783	57178.387817	34.693901
1045.573331	57265.966146	34.698919
1046.914815	57352.216563	34.703936
1048.222206	57432.485433	34.708954
1049.020961	57524.656222	34.713972
1050.228640	57611.580282	34.718989
1051.360899	57697.535402	34.724007
1051.870688	57782.796595	34.729024
1053.635478	57866.615918	34.734042
1054.348328	57966.308014	34.739060
1055.342734	58048.950430	34.744077
1056.475678	58131.008276	34.749095
1057.362004	58240.047913	34.754112
1058.730482	58322.076076	34.759130
1059.854731	58420.699676	34.764148
1060.959229	58498.883411	34.769165
1061.611998	58588.530324	34.774183
1063.063337	58677.863388	34.779200
1064.008417	58764.781851	34.784218
1064.956349	58855.928154	34.789236
1066.147681	58941.669648	34.794253
1067.374653	59041.982381	34.799271
1068.428192	59132.879102	34.804288
1069.390908	59229.872850	34.809306
1070.378224	59312.185233	34.814324
1071.117669	59404.536993	34.819341
1072.775451	59502.999671	34.824359
1073.840241	59599.061233	34.829376
1074.970029	59672.117931	34.834394
1075.772428	59764.125794	34.839412
1077.042798	59861.884356	34.844429
1078.200724	59949.014453	34.849447
1078.993337	60039.917204	34.854464
1080.807905	60125.179759	34.859482
1082.093337	60214.879778	34.864500
1083.467688	60288.096476	34.869517
1084.609671	60358.874654	34.874535
1085.369350	60455.303569	34.879552
1086.852492	60521.503370	34.884570
1087.919055	60615.036768	34.889588
1088.652908	60693.690365	34.894605
1089.915362	60766.033416	34.899623
1091.133382	60849.175931	34.904640
1092.205388	60907.712071	34.909658
1093.366346	60988.528234	34.914676
1094.425736	61058.517404	34.919693
1095.372473	61117.409028	34.924711
1095.944040	61193.247371	34.929728
1096.986649	61255.409623	34.934746
1097.848282	61330.950044	34.939764
1099.148362	61408.834165	34.944781
1100.073974	61489.745582	34.949799
1100.792974	61571.449026	34.954816
1101.460094	61647.767638	34.959834
1102.562503	61722.835012	34.964852
1103.985752	61819.773683	34.969869
1104.727409	61910.121595	34.974887
1105.661062	62006.497870	34.979904
1107.056361	62090.351284	34.984922
1108.054410	62175.311293	34.989940
1109.325862	62276.934385	34.994957
1110.769298	62365.092095	34.999975
1111.752901	62455.682871	35.004992
1112.852729	62542.502048	35.010010
1113.772744	62645.523371	35.015028
1115.319737	62733.299118	35.020045
1116.407754	62812.714631	35.025063
1117.629220	62912.164152	35.030080
1118.942424	63000.306414	35.035098
1120.112689	63095.187783	35.040116
1121.087990	63180.471302	35.045133
1122.260058	63276.087409	35.050151
1123.447906	63365.181052	35.055168
1124.530010	63450.904667	35.060186
1125.530540	63545.320396	35.065204
1126.857364	63628.765532	35.070221
1127.835195	63712.942639	35.075239
1129.390620	63814.711412	35.080256
1131.017190	63888.557926	35.085274
1132.435528	63975.452813	35.090292
1133.540968	64059.047801	35.095309
1134.774819	64121.428049	35.100327
1135.547374	64207.177124	35.105344
1137.364974	64283.964161	35.110362
1138.284079	64371.780118	35.115380
1139.134654	64465.057815	35.120397
1140.317133	64533.163745	35.125415
1141.203035	64620.099434	35.130432
1142.655874	64709.770714	35.135450
1143.392229	64790.741337	35.140468
1144.065538	64877.419791	35.145485
1145.853751	64956.606525	35.150503
1146.748659	65052.766378	35.155520
1148.152945	65127.860352	35.160538
1149.519099	65211.057739	35.165556
1150.365035	65304.218986	35.170573
1151.420583	65385.097521	35.175591
1152.561129	65479.391119	35.180608
1153.453623	65563.613048	35.185626
1155.038524	65657.325333	35.190644
1155.525521	65746.447902	35.195661
1156.876375	65826.686768	35.200679
1157.686464	65927.738092	35.205696
1159.095465	66022.903613	35.210714
1160.133980	66124.996462	35.215732
1161.067343	66214.722304	35.220749
1162.639865	66305.266999	35.225767
1163.722459	66408.139196	35.230784
1164.345921	66500.142877	35.235802
1165.427137	66602.338632	35.240820
1166.800597	66696.195308	35.245837
1168.205686	66801.905975	35.250855
1169.133706	66905.848916	35.255872
1170.263133	67000.580439	35.260890
1171.714388	67090.830244	35.265908
1172.712943	67180.188457	35.270925
1173.834511	67260.037011	35.275943
1174.638871	67355.428269	35.280960
1176.225071	67436.097788	35.285978
1177.249325	67531.936671	35.290996
1178.382882	67623.681396	35.296013
1179.926046	67708.910845	35.301031
1181.097363	67808.032941	35.306048
1181.900264	67892.593112	35.311066
1183.097926	67982.208061	35.316084
1184.583665	68078.344393	35.321101
1185.692614	68165.441136	35.326119
1186.692632	68262.375571	35.331136
1187.884391	68353.930235	35.336154
1189.133245	68456.474554	35.341172
1190.103250	68551.318948	35.346189
1191.688164	68653.799083	35.351207
1192.685210	68752.856977	35.356224
1193.824013	68850.690140	35.361242
1195.277929	68954.958445	35.366260
1196.427442	69059.888745	35.371277
1198.262456	69146.128632	35.376295
1198.788053	69256.690930	35.381312
1200.315970	69344.245667	35.386330
1201.325389	69444.545353	35.391348
1202.233225	69548.603451	35.396365
1204.313578	69638.504685	35.401383
1205.502962	69735.453175	35.406400
1206.973091	69822.144703	35.411418
1207.882331	69914.382086	35.416436
1209.468691	70004.329822	35.421453
1211.016436	70086.495358	35.426471
1212.345494	70175.261636	35.431488
1213.517885	70280.826539	35.436506
1214.797114	70356.620230	35.441524
1215.626570	70446.193400	35.446541
1217.354216	70536.868192	35.451559
1218.098144	70623.555119	35.456576
1218.984701	70718.097495	35.461594
1220.475883	70800.869328	35.466612
1221.508083	70909.346130	35.471629
1222.845967	71006.934809	35.476647
1223.758558	71103.412228	35.481664
1224.998908	71201.840024	35.486682
1226.605080	71303.377463	35.491700
1227.346922	71399.489941	35.496717
1229.073791	71493.651026	35.501735
1230.120724	71590.020672	35.506752
1231.144648	71692.270832	35.511770
1232.421318	71776.864916	35.516788
1233.686578	71874.797425	35.521805
1235.170877	71975.444548	35.526823
1236.481378	72072.294211	35.531840
1237.796799	72166.230453	35.536858
1239.528379	72244.675908	35.541876
1240.192099	72348.187888	35.546893
1241.745251	72431.677154	35.551911
1243.225648	72528.160084	35.556928
1244.311333	72621.867736	35.561946
1245.514210	72711.314526	35.566964
1246.389406	72808.538624	35.571981
1247.785503	72895.384850	35.576999
1248.798191	72992.664217	35.582016
1249.776890	73091.874420	35.587034
1251.197613	73191.256842	35.592052
1251.763103	73288.822221	35.597069
1252.820683	73390.047790	35.602087
1254.261010	73484.374583	35.607104
1255.061799	73595.786293	35.612122
1256.659521	73679.310557	35.617140
1257.525366	73784.113949	35.622157
1258.782668	73885.335649	35.627175
1260.051269	73982.540809	35.632192
1261.536280	74090.364901	35.637210
1262.678419	74187.514496	35.642228
1263.691118	74289.244453	35.647245
1265.083095	74397.096931	35.652263
1266.190515	74505.437459	35.657280
1267.646997	74609.531505	35.662298
1268.987203	74712.174743	35.667316
1270.422457	74815.158243	35.672333
1271.497856	74928.876078	35.677351
1273.037285	75030.805532	35.682368
1274.028573	75147.400043	35.687386
1275.478633	75245.024882	35.692404
1276.874090	75367.675471	35.697421
1277.921698	75472.279845	35.702439
1279.600864	75594.937978	35.707456
1280.652066	75708.358869	35.712474
1282.459901	75822.017143	35.717492
1283.769925	75923.909687	35.722509
1284.908907	76025.043879	35.727527
1286.147395	76143.086271	35.732544
1287.589005	76253.471904	35.737562
1288.707614	76352.647075	35.742580
1289.830111	76478.169994	35.747597
1291.225730	76589.045511	35.752615
1292.784357	76696.070551	35.757632
1294.125010	76812.845885	35.762650
1295.521414	76914.006664	35.767668
1296.563187	77022.278850	35.772685
1297.565262	77139.133620	35.777703
1299.311340	77244.472186	35.782720
1300.779247	77352.552680	35.787738
1302.909844	77446.811268	35.792756
1303.913093	77567.430017	35.797773
1305.442749	77665.228544	35.802791
1306.876232	77754.580230	35.807808
1308.384647	77862.947803	35.812826
1309.782300	77964.834362	35.817844
1310.651639	78067.880316	35.822861
1312.260305	78158.054812	35.827879
1313.749423	78259.750879	35.832896
1314.261408	78370.555819	35.837914
1315.944327	78469.055449	35.842932
1317.327151	78566.157960	35.847949
1318.608541	78667.913208	35.852967
1320.248350	78767.624110	35.857984
1321.119118	78865.314113	35.863002
1322.649015	78969.806180	35.868020
1324.187427	79068.089748	35.873037
1325.388030	79173.001227	35.878055
1326.866691	79276.805661	35.883072
1327.846766	79381.828270	35.888090
1328.669098	79472.370173	35.893108
1330.187294	79585.265735	35.898125
1331.354433	79696.708813	35.903143
1333.333364	79791.746522	35.908160
1334.686645	79894.622628	35.913178
1336.336825	79990.269620	35.918196
1337.069488	80088.314830	35.923213
1338.503551	80190.355975	35.928231
1340.452866	80294.230326	35.933248
1341.571205	80393.686194	35.938266
1343.157378	80477.081128	35.943284
1344.037014	80566.312758	35.948301
1345.164384	80653.795767	35.953319
1346.389671	80749.334136	35.958336
1347.610776	80837.702651	35.963354
1349.193140	80916.285154	35.968372
1350.402275	81005.302200	35.973389
1351.776195	81093.052276	35.978407
1353.125171	81172.824747	35.983424
1354.126109	81285.630347	35.988442
1355.527735	81378.926256	35.993460
1356.589296	81485.844552	35.998477
1358.002407	81597.675041	36.003495
1359.270773	81691.018070	36.008512
1360.249021	81806.933373	36.013530
1361.593307	81913.049103	36.018548
1362.906851	82026.670569	36.023565
1363.905793	82144.864615	36.028583
1365.247634	82256.784836	36.033600
1366.486424	82379.567067	36.038618
1368.162710	82502.155034	36.043636
1369.568733	82630.056369	36.048653
1370.955422	82746.102009	36.053671
1372.669447	82864.567868	36.058688
1373.918849	82987.389096	36.063706
1375.401332	83105.879333	36.068724
1376.995965	83227.760944	36.073741
1378.411162	83347.377656	36.078759
1379.812453	83470.633468	36.083776
1381.382844	83588.364477	36.088794
1382.667818	83701.933758	36.093812
1384.204347	83820.038442	36.098829
1385.149439	83933.395463	36.103847
1386.896470	84053.926466	36.108864
1388.108378	84182.359158	36.113882
1389.692580	84301.548103	36.118900
1391.211071	84423.003195	36.123917
1392.529072	84544.958834	36.128935
1393.810947	84663.144650	36.133952
1395.177205	84784.967087	36.138970
1396.432839	84906.414455	36.143988
1398.513650	85027.543831	36.149005
1399.783633	85143.668072	36.154023
1401.687350	85264.762655	36.159040
1403.109097	85386.325577	36.164058
1404.717269	85494.542363	36.169076
1406.237323	85607.487045	36.174093
1407.393419	85715.572282	36.179111
1409.014676	85818.859040	36.184128
1410.240255	85943.128532	36.189146
1411.856453	86056.148703	36.194164
1413.150793	86170.828715	36.199181
1414.548478	86273.277547	36.204199
1416.373639	86383.250598	36.209216
1417.624451	86496.899588	36.214234
1418.319755	86613.245891	36.219252
1419.746985	86717.605145	36.224269
1421.366925	86834.530714	36.229287
1422.837094	86940.772208	36.234304
1424.015289	87067.512252	36.239322
1425.362825	87183.556559	36.244340
1426.829980	87299.341937	36.249357
1428.405247	87431.838285	36.254375
1429.895959	87539.447359	36.259392
1431.296484	87653.305650	36.264410
1433.089198	87774.896852	36.269428
1434.213428	87889.559407	36.274445
1435.666628	88009.620372	36.279463
1436.980677	88111.125561	36.284480
1438.036797	88229.817234	36.289498
1439.505687	88334.112402	36.294516
1440.826238	88427.849357	36.299533
1442.083963	88544.407256	36.304551
1443.401523	88661.881413	36.309568
1444.968989	88769.622443	36.314586
1446.441334	88885.692062	36.319604
1447.966067	89001.158357	36.324621
1449.152010	89109.682364	36.329639
1450.816905	89212.809562	36.334656
1452.100989	89339.441523	36.339674
1453.282575	89446.357962	36.344692
1455.023767	89577.177949	36.349709
1456.278818	89704.018752	36.354727
1458.191026	89812.242187	36.359744
1459.323712	89940.535120	36.364762
1460.929205	90070.149083	36.369780
1462.397719	90193.689018	36.374797
1463.810738	90307.656964	36.379815
1465.027701	90430.831481	36.384832
1466.374244	90561.527107	36.389850
1468.024777	90690.642481	36.394868
1469.700988	90822.023001	36.399885
1471.385307	90954.505450	36.404903
1473.263183	91069.012277	36.409920
1474.191341	91205.871918	36.414938
1475.876198	91341.676534	36.419956
1477.668772	91461.331059	36.424973
1478.999842	91602.400908	36.429991
1480.542192	91715.555602	36.435008
1481.955083	91845.600101	36.440026
1483.365086	91975.392125	36.445044
1485.133325	92101.060525	36.450061
1486.281173	92238.245523	36.455079
1487.956181	92360.672222	36.460096
1489.519531	92485.132020	36.465114
1491.101853	92628.296832	36.470132
1492.781202	92760.711922	36.475149
1494.009479	92900.523682	36.480167
1495.651852	93020.486580	36.485184
1496.863778	93157.158760	36.490202
1497.954978	93293.229281	36.495220
1499.934693	93424.586524	36.500237
1501.412664	93560.053017	36.505255
1503.192223	93692.367824	36.510272
1504.571587	93819.333297	36.515290
1506.274600	93958.252126	36.520308
1508.005926	94085.531492	36.525325
1509.697329	94217.469356	36.530343
1511.814703	94324.041908	36.535360
1513.366537	94446.407402	36.540378
1514.589944	94570.713109	36.545396
1516.187066	94683.819575	36.550413
1517.464218	94813.935850	36.555431
1518.971323	94941.114216	36.560448
1520.245236	95062.181813	36.565466
1521.751916	95196.738399	36.570484
1523.425407	95315.450529	36.575501
1524.444080	95448.588448	36.580519
1526.028193	95581.385415	36.585536
1527.612680	95708.706989	36.590554
1528.827907	95844.363823	36.595572
1530.715788	95977.127873	36.600589
1531.807002	96110.092540	36.605607
1533.579197	96249.467202	36.610624
1534.977634	96379.786635	36.615642
1536.220703	96529.461732	36.620660
1537.911088	96656.567868	36.625677
1539.219732	96785.812820	36.630695
1540.874432	96900.895849	36.635712
1542.575519	97030.892003	36.640730
1543.761765	97142.981183	36.645748
1545.449690	97257.844850	36.650765
1547.274915	97371.825574	36.655783
1548.688749	97491.866684	36.660800
1550.662893	97610.299866	36.665818
1552.090303	97742.585284	36.670836
1553.362451	97853.776260	36.675853
1554.724890	97985.895334	36.680871
1556.362126	98115.842507	36.685888
1558.148902	98235.143849	36.690906
1559.397071	98386.589017	36.695924
1561.285279	98501.983803	36.700941
1562.401558	98646.998236	36.705959
1563.953807	98777.544476	36.710976
1565.524883	98910.674423	36.715994
1566.701703	99048.379314	36.721012
1568.749696	99185.087162	36.726029
1570.410703	99322.641809	36.731047
1571.668471	99467.156206	36.736064
1573.359764	99610.348728	36.741082
1574.879515	99755.470185	36.746100
1576.366363	99895.501114	36.751117
1578.196276	100041.754583	36.756135
1579.509090	100192.602383	36.761152
1581.359869	100344.317972	36.766170
1582.973009	100490.898798	36.771188
1584.762827	100638.758588	36.776205
1586.580779	100778.817877	36.781223
1587.954527	100922.078318	36.786240
1589.261403	101065.907624	36.791258
1590.972573	101216.786933	36.796276
1593.204564	101351.434181	36.801293
1594.984129	101498.361311	36.806311
1596.774225	101649.775495	36.811328
1598.205745	101785.322484	36.816346
1599.593488	101934.924251	36.821364
1601.368951	102067.249334	36.826381
1602.907851	102209.969917	36.831399
1604.413138	102358.528382	36.836416
1606.590432	102495.610416	36.841434
1608.332014	102642.193594	36.846452
1610.160410	102754.443246	36.851469
1611.824443	102891.835028	36.856487
1613.792162	103023.069038	36.861504
1615.244036	103153.623140	36.866522
1616.680120	103284.636646	36.871540
1618.415492	103427.813713	36.876557
1620.246647	103564.142621	36.881575
1621.192049	103689.566680	36.886592
1623.382141	103817.422015	36.891610
1624.610600	103948.571889	36.896628
1626.351075	104082.114991	36.901645
1627.818838	104218.706006	36.906663
1629.380437	104348.448946	36.911680
1631.205321	104487.140921	36.916698
1632.481225	104627.744721	36.921716
1634.465353	104747.330808	36.926733
1635.958970	104886.836753	36.931751
1637.276721	105028.158438	36.936768
1639.079599	105162.558337	36.941786
1640.588644	105315.833490	36.946804
1642.453252	105444.062691	36.951821
1644.150604	105580.243133	36.956839
1645.358470	105711.745457	36.961856
1647.516175	105844.774173	36.966874
1648.363694	105981.519609	36.971892
1649.998442	106102.851290	36.976909
1651.616680	106226.950171	36.981927
1653.237326	106353.179345	36.986944
1654.832346	106475.748489	36.991962
1656.127287	106622.279142	36.996980
1657.830494	106748.281374	37.001997
1659.334633	106893.487275	37.007015
1660.863970	107033.744635	37.012032
1662.446262	107168.047339	37.017050
1664.077667	107314.034069	37.022068
1665.954761	107458.829278	37.027085
1667.622259	107598.014986	37.032103
1669.171591	107752.055667	37.037120
1670.922907	107895.414053	37.042138
1672.692436	108043.043519	37.047156
1674.194926	108189.611974	37.052173
1676.046620	108343.430713	37.057191
1677.690066	108489.788295	37.062208
1679.346941	108640.899664	37.067226
1681.187570	108796.611562	37.072244
1682.780403	108943.904635	37.077261
1685.125028	109091.563195	37.082279
1686.396177	109250.168230	37.087296
1688.336577	109399.869234	37.092314
1689.884725	109560.499565	37.097332
1691.723051	109705.437023	37.102349
1693.525197	109864.355318	37.107367
1695.038442	110017.422545	37.112384
1696.584436	110175.976322	37.117402
1698.236371	110332.523362	37.122420
1700.038999	110489.301272	37.127437
1702.132926	110638.996360	37.132455
1703.445499	110806.276073	37.137472
1705.423838	110956.155356	37.142490
1706.990286	111124.157953	37.147508
1709.038133	111272.696193	37.152525
1711.029793	111421.142348	37.157543
1712.622493	111579.137163	37.162560
1714.723634	111729.381057	37.167578
1716.456608	111894.216294	37.172596
1718.270032	112029.731874	37.177613
1719.824904	112188.204509	37.182631
1721.733475	112349.856712	37.187648
1723.721129	112490.990424	37.192666
1725.707017	112630.501656	37.197684
1727.228340	112777.428712	37.202701
1728.977376	112920.744542	37.207719
1730.900039	113066.938159	37.212736
1733.113130	113205.718739	37.217754
1734.669505	113357.956603	37.222772
1736.471426	113483.485755	37.227789
1738.336692	113633.393870	37.232807
1739.661483	113778.022016	37.237824
1741.095743	113920.984968	37.242842
1742.524048	114063.327961	37.247860
1744.151841	114215.697823	37.252877
1745.577450	114365.208129	37.257895
1747.301337	114525.820789	37.262912
1749.251116	114685.219494	37.267930
1750.766282	114842.657274	37.272948
1752.446980	114998.852405	37.277965
1754.129519	115152.257655	37.282983
1756.686774	115303.942026	37.288000
1759.025062	115440.466748	37.293018
1760.832320	115570.910619	37.298036
1762.715826	115718.554175	37.303053
1764.667959	115842.381198	37.308071
1766.130999	115969.265330	37.313088
1767.574280	116100.630186	37.318106
1769.018349	116229.141627	37.323124
1770.243178	116357.256400	37.328141
1771.770740	116488.926599	37.333159
1773.406382	116641.660432	37.338176
1775.222718	116779.311384	37.343194
1776.613482	116931.868899	37.348212
1778.067456	117083.554711	37.353229
1779.837936	117229.027595	37.358247
1781.238286	117391.047540	37.363264
1783.276090	117546.474859	37.368282
1784.955577	117728.582041	37.373300
1786.449086	117892.225870	37.378317
1788.378080	118055.866053	37.383335
1790.065041	118231.772035	37.388352
1791.974514	118396.431457	37.393370
1793.087472	118579.315861	37.398388
1794.829417	118756.154351	37.403405
1796.805981	118937.371279	37.408423
1798.652049	119129.403759	37.413440
1800.839819	119309.067465	37.418458
1802.610911	119497.878947	37.423476
1804.482065	119678.811379	37.428493
1806.875567	119858.407595	37.433511
1808.423065	120042.550581	37.438528
1810.152571	120214.235108	37.443546
1812.186000	120394.587531	37.448564
1813.687534	120580.693698	37.453581
1815.963002	120763.661306	37.458599
1818.345238	120934.892274	37.463616
1820.040814	121109.668505	37.468634
1821.985051	121288.504094	37.473652
1824.036515	121464.203280	37.478669
1826.088867	121633.839609	37.483687
1827.586510	121812.353870	37.488704
1829.708257	121993.943135	37.493722
1831.512884	122164.698574	37.498740
1833.024480	122339.635801	37.503757
1834.983532	122515.075013	37.508775
1836.539066	122702.641732	37.513792
1838.834454	122882.660448	37.518810
1840.220789	123069.227711	37.523828
1841.990662	123242.137102	37.528845
1844.745844	123411.113546	37.533863
1846.573573	123593.961089	37.538880
1848.448492	123775.990234	37.543898
1850.432419	123950.480497	37.548916
1852.262099	124127.799130	37.553933
1854.306197	124294.606522	37.558951
1855.634467	124473.679279	37.563968
1857.646769	124643.525046	37.568986
1859.443085	124827.080856	37.574004
1861.473503	124998.878978	37.579021
1863.646133	125160.836504	37.584039
1865.782000	125338.341180	37.589056
1867.621830	125519.026251	37.594074
1869.485166	125683.913825	37.599092
1871.053668	125856.485235	37.604109
1873.052965	126013.677648	37.609127
1874.727927	126182.986114	37.614144
1876.117613	126351.235941	37.619162
1878.130949	126538.482914	37.624180
1879.877227	126712.489249	37.629197
1882.124806	126886.050383	37.634215
1883.954900	127066.591579	37.639232
1885.671393	127237.039755	37.644250
1887.758837	127393.196100	37.649268
1889.487096	127560.966829	37.654285
1891.077133	127709.843303	37.659303
1892.862860	127877.073511	37.664320
1894.447859	128035.213547	37.669338
1896.344968	128201.488874	37.674356
1897.702805	128374.839490	37.679373
1899.514098	128553.423559	37.684391
1901.171828	128735.990759	37.689408
1902.811825	128909.870610	37.694426
1904.273476	129097.443380	37.699444
1905.839481	129287.690508	37.704461
1908.153451	129490.179828	37.709479
1910.012485	129690.419078	37.714496
1911.796045	129890.912089	37.719514
1914.204189	130087.109178	37.724532
1915.891865	130288.862396	37.729549
1917.524404	130482.238436	37.734567
1919.704314	130700.157532	37.739584
1921.699073	130895.991291	37.744602
1923.705404	131105.971378	37.749620
1925.756417	131324.522739	37.754637
1927.930670	131527.081546	37.759655
1929.729329	131734.089909	37.764672
1930.951267	131940.592667	37.769690
1933.493656	132146.865524	37.774708
1935.551534	132374.417205	37.779725
1937.544182	132579.990991	37.784743
1939.754689	132793.474900	37.789760
1941.492180	133008.670306	37.794778
1943.635831	133217.332308	37.799796
1945.283580	133438.799328	37.804813
1947.384554	133648.853097	37.809831
1949.174867	133861.646262	37.814848
1951.202844	134079.149135	37.819866
1953.833008	134299.274807	37.824884
1955.851484	134512.479701	37.829901
1957.812294	134723.220205	37.834919
1959.680105	134940.638013	37.839936
1961.441088	135149.064120	37.844954
1963.470120	135364.707774	37.849972
1965.486211	135579.415461	37.854989
1967.939517	135795.769201	37.860007
1970.276650	135998.437385	37.865024
1971.952830	136205.955241	37.870042
1974.333227	136415.775474	37.875060
1976.288485	136634.520241	37.880077
1977.988842	136831.047916	37.885095
1980.333047	137056.205937	37.890112
1982.113709	137258.572949	37.895130
1984.158761	137459.935270	37.900148
1986.240678	137679.464775	37.905165
1988.464948	137872.577903	37.910183
1990.123261	138081.477552	37.915200
1992.251187	138298.375986	37.920218
1994.396659	138502.760161	37.925236
1995.929447	138708.890320	37.930253
1998.346365	138914.706124	37.935271
1999.834064	139114.880642	37.940288
2002.123104	139334.753739	37.945306
2004.058166	139540.710733	37.950324
2005.785878	139741.941946	37.955341
2007.974994	139959.866476	37.960359
2009.811103	140176.641335	37.965376
2011.724621	140397.237729	37.970394
2014.098050	140599.412721	37.975412
2015.976253	140812.719344	37.980429
2017.894681	141027.949671	37.985447
2020.131364	141230.745082	37.990464
2021.535354	141439.191521	37.995482
2023.787103	141625.805247	38.000500
2025.577814	141826.197819	38.005517
2027.894407	141991.557991	38.010535
2030.139148	142185.396218	38.015552
2032.147983	142386.505935	38.020570
2034.098889	142564.831954	38.025588
2035.887498	142765.279484	38.030605
2037.535830	142962.005708	38.035623
2039.454491	143161.584293	38.040640
2041.525160	143371.838953	38.045658
2043.689023	143580.379338	38.050676
2045.686303	143802.272702	38.055693
2047.832346	143997.136074	38.060711
2049.728699	144213.792642	38.065728
2051.585686	144429.466320	38.070746
2053.639957	144654.565624	38.075764
2055.893236	144859.645274	38.080781
2058.089299	145082.985646	38.085799
2060.147438	145303.949688	38.090816
2061.510063	145521.151870	38.095834
2063.958447	145751.449235	38.100852
2066.136733	145985.381556	38.105869
2067.998771	146208.601179	38.110887
2070.004917	146433.195497	38.115904
2072.440478	146665.072818	38.120922
2074.605554	146889.200164	38.125940
2077.356335	147104.555712	38.130957
2079.428205	147334.004927	38.135975
2081.960050	147548.672925	38.140992
2083.930360	147774.129050	38.146010
2085.776195	147985.008986	38.151028
2088.250223	148211.429401	38.156045
2090.590532	148425.305786	38.161063
2093.682635	148624.329705	38.166080
2095.782621	148836.036614	38.171098
2097.834694	149041.303839	38.176116
2099.897722	149246.379758	38.181133
2101.667445	149457.175883	38.186151
2104.262147	149661.142523	38.191168
2106.270753	149886.754024	38.196186
2108.201981	150099.812303	38.201204
2110.594984	150298.075457	38.206221
2112.349150	150523.703842	38.211239
2114.645416	150722.174008	38.216256
2116.344930	150938.381512	38.221274
2118.712378	151140.256637	38.226292
2120.531015	151361.956213	38.231309
2122.614988	151576.773604	38.236327
2124.454826	151799.499823	38.241344
2126.432288	152013.231158	38.246362
2128.509676	152230.070404	38.251380
2130.138316	152463.393278	38.256397
2132.113506	152699.125785	38.261415
2134.696773	152927.618046	38.266432
2136.413099	153165.182633	38.271450
2138.529402	153407.598520	38.276468
2140.524780	153636.946799	38.281485
2142.567814	153876.824622	38.286503
2144.783187	154112.893808	38.291520
2146.441462	154354.864582	38.296538
2148.632892	154593.808359	38.301556
2150.822070	154846.844075	38.306573
2153.005947	155083.645746	38.311591
2155.444581	155328.748919	38.316608
2157.282452	155574.238599	38.321626
2159.878957	155812.464283	38.326644
2162.143187	156048.343395	38.331661
2164.056041	156264.550833	38.336679
2166.055607	156480.834435	38.341696
2168.423346	156706.722149	38.346714
2170.591369	156920.975401	38.351732
2172.467453	157149.302534	38.356749
2174.630505	157370.984603	38.361767
2176.995416	157586.250587	38.366784
2178.675074	157818.965182	38.371802
2180.742551	158049.779560	38.376820
2182.805354	158293.455554	38.381837
2184.723873	158532.559390	38.386855
2187.218622	158758.155805	38.391872
2189.325028	159005.839520	38.396890
2191.817265	159237.442893	38.401908
2194.696224	159471.157840	38.406925
2196.898902	159706.019937	38.411943
2199.416580	159939.843672	38.416960
2201.447969	160174.734210	38.421978
2203.791861	160400.575959	38.426996
2206.092416	160635.070875	38.432013
2208.133822	160884.765429	38.437031
2210.467074	161108.618198	38.442048
2212.789545	161349.752146	38.447066
2215.547701	161574.086351	38.452084
2217.915616	161808.600545	38.457101
2220.053792	162040.244034	38.462119
2222.700482	162257.805780	38.467136
2225.331353	162486.251045	38.472154
2227.233593	162699.740525	38.477172
2229.432683	162938.157365	38.482189
2231.542343	163181.096064	38.487207
2233.667647	163407.541126	38.492224
2235.866274	163647.027099	38.497242
2237.687068	163872.645134	38.502260
2240.246103	164112.406813	38.507277
2242.358138	164364.706582	38.512295
2244.685813	164594.437938	38.517312
2246.727029	164839.234362	38.522330
2248.651689	165079.441057	38.527348
2251.592218	165313.980290	38.532365
2253.420254	165564.449723	38.537383
2256.013612	165814.927941	38.542400
2257.890370	166066.953312	38.547418
2260.212505	166322.008260	38.552436
2262.352910	166567.455719	38.557453
2264.233510	166826.669560	38.562471
2266.539291	167078.136704	38.567488
2268.654266	167341.607480	38.572506
2270.598623	167614.006254	38.577524
2273.114942	167871.487166	38.582541
2274.958065	168145.986039	38.587559
2276.994052	168412.279136	38.592576
2279.205886	168683.586566	38.597594
2281.239658	168960.471342	38.602612
2284.209573	169237.859048	38.607629
2286.037707	169525.189607	38.612647
2288.817335	169795.371704	38.617664
2291.131444	170076.750021	38.622682
2293.115393	170360.669468	38.627700
2295.778920	170629.793446	38.632717
2297.822397	170922.327274	38.637735
2300.746241	171177.788451	38.642752
2302.750626	171452.274721	38.647770
2305.176952	171716.106608	38.652788
2307.502590	171982.621573	38.657805
2309.786102	172262.273348	38.662823
2311.841280	172527.359394	38.667840
2313.919738	172785.852636	38.672858
2316.830309	173046.629816	38.677876
2319.656743	173283.942796	38.682893
2321.674464	173531.273950	38.687911
2324.300179	173757.001118	38.692928
2326.840750	173990.767248	38.697946
2328.812958	174231.187350	38.702964
2330.910410	174483.296210	38.707981
2332.961108	174732.606889	38.712999
2335.334937	174977.169783	38.718016
2337.759684	175232.798223	38.723034
2339.596198	175483.541355	38.728052
2341.873326	175739.372144	38.733069
2344.243107	176011.341428	38.738087
2346.338375	176272.484640	38.743104
2348.321633	176551.957036	38.748122
2350.530273	176823.433449	38.753140
2353.131616	177109.071804	38.758157
2355.100704	177390.111116	38.763175
2357.284835	177669.086146	38.768192
2360.078728	177956.119634	38.773210
2362.091011	178235.986767	38.778228
2365.282185	178524.687338	38.783245
2367.685743	178813.003505	38.788263
2370.323694	179092.725252	38.793280
2372.762877	179382.840972	38.798298
2374.995091	179670.221532	38.803316
2377.453476	179948.094533	38.808333
2379.480456	180248.410873	38.813351
2382.029316	180541.662623	38.818368
2384.180117	180834.062953	38.823386
2386.644222	181136.320651	38.828404
2389.277403	181426.082624	38.833421
2391.226888	181734.898871	38.838439
2393.737183	182034.383942	38.843456
2396.234559	182332.856057	38.848474
2398.548360	182650.355631	38.853492
2401.337214	182950.359036	38.858509
2403.554842	183251.061848	38.863527
2406.190425	183553.834037	38.868544
2408.838970	183853.328734	38.873562
2411.930950	184134.366675	38.878580
2414.855265	184423.457532	38.883597
2417.339119	184716.503809	38.888615
2419.887645	184988.815358	38.893632
2423.102609	185345.526439	38.898650
2425.572636	185626.487601	38.903668
2428.747856	185892.659080	38.908685
2430.942059	186167.010078	38.913703
2433.114124	186431.840518	38.918720
2435.602742	186694.971414	38.923738
2437.557317	186963.265967	38.928756
2440.334545	187231.153785	38.933773
2442.508973	187514.045628	38.938791
2444.462558	187783.586993	38.943808
2446.871998	188061.185989	38.948826
2449.258429	188340.567260	38.953844
2452.118928	188615.938501	38.958861
2454.876899	188905.372520	38.963879
2456.608592	189175.993255	38.968896
2459.125269	189453.071084	38.973914
2461.137753	189745.849102	38.978932
2463.866888	190021.980863	38.983949
2466.240825	190306.779235	38.988967
2468.580187	190579.137569	38.993984
2471.332452	190854.378722	38.999002
2473.662505	191142.869023	39.004020
2476.174493	191434.963980	39.009037
2478.509132	191699.629319	39.014055
2480.760733	191972.334740	39.019072
2482.807739	192235.598191	39.024090
2484.862663	192508.259223	39.029108
2487.013149	192770.517097	39.034125
2489.019370	193066.835014	39.039143
2491.404346	193346.660351	39.044160
2493.809354	193634.255866	39.049178
2495.766325	193929.313433	39.054196
2498.282824	194219.026596	39.059213
2500.921640	194528.254791	39.064231
2503.058619	194848.281092	39.069248
2505.857266	195156.800065	39.074266
2507.617122	195477.115183	39.079284
2510.316337	195793.500082	39.084301
2512.608650	196120.160389	39.089319
2514.968837	196443.178504	39.094336
2517.517905	196772.492945	39.099354
2520.309795	197104.488334	39.104372
2522.792691	197437.701057	39.109389
2525.458676	197768.828524	39.114407
2528.251114	198106.033478	39.119424
2531.271232	198439.749128	39.124442
2533.609788	198779.541023	39.129460
2536.577497	199106.153796	39.134477
2539.322714	199441.667170	39.139495
2541.948358	199780.933973	39.144512
2545.101293	200104.014549	39.149530
2547.060045	200436.502587	39.154548
2550.241098	200764.330314	39.159565
2552.788395	201095.483406	39.164583
2555.144436	201432.966686	39.169600
2557.901233	201761.472068	39.174618
2560.541746	202098.429763	39.179636
2563.300937	202429.247669	39.184653
2566.075114	202754.500730	39.189671
2568.774286	203089.063376	39.194688
2571.370215	203414.675612	39.199706
2574.016682	203743.557498	39.204724
2576.744259	204070.191913	39.209741
2579.729098	204391.630116	39.214759
2581.948591	204723.018818	39.219776
2584.629395	205046.080398	39.224794
2587.165592	205378.589453	39.229812
2589.724578	205704.693996	39.234829
2592.178309	206029.316671	39.239847
2594.863315	206360.762655	39.244864
2597.501155	206697.093872	39.249882
2600.046005	207038.698511	39.254900
2602.455170	207373.618397	39.259917
2605.114842	207706.467556	39.264935
2607.549127	208046.897009	39.269952
2610.320458	208379.069292	39.274970
2612.855767	208715.749738	39.279988
2615.360487	209046.745093	39.285005
2618.191770	209376.572334	39.290023
2620.694958	209719.457559	39.295040
2623.841263	210060.871383	39.300058
2626.067932	210403.241678	39.305076
2629.301401	210715.657550	39.310093
2632.220584	211055.228148	39.315111
2634.906617	211384.826481	39.320128
2637.350080	211707.629409	39.325146
2640.124028	212030.178037	39.330164
2642.761344	212364.408503	39.335181
2645.328358	212684.576699	39.340199
2647.797257	213025.439019	39.345216
2650.661906	213336.390859	39.350234
2652.957540	213661.403549	39.355252
2656.047357	213954.233532	39.360269
2658.223090	214249.670171	39.365287
2660.597105	214557.193769	39.370304
2662.989584	214864.359101	39.375322
2665.277545	215169.356227	39.380340
2667.678705	215478.400582	39.385357
2670.495044	215796.119471	39.390375
2673.113889	216108.102675	39.395392
2675.370705	216421.717486	39.400410
2678.229846	216766.206077	39.405428
2680.418870	217086.843368	39.410445
2683.232779	217428.036989	39.415463
2685.440959	217770.468286	39.420480
2688.313176	218101.263097	39.425498
2691.636567	218442.759169	39.430516
2694.172345	218772.743011	39.435533
2697.340481	219113.653950	39.440551
2699.887120	219449.885848	39.445568
2702.573294	219800.144612	39.450586
2705.237704	220151.397699	39.455604
2707.711631	220493.255708	39.460621
2710.808550	220837.023836	39.465639
2713.349651	221190.760772	39.470656
2716.262314	221534.507044	39.475674
2719.061549	221899.966151	39.480692
2721.511890	222251.075576	39.485709
2724.833138	222607.511450	39.490727
2727.088804	222967.212546	39.495744
2729.907449	223328.070919	39.500762
2732.735919	223692.840069	39.505780
2735.605820	224047.009333	39.510797
2738.415755	224417.700643	39.515815
2740.906628	224791.718777	39.520832
2743.762584	225159.227490	39.525850
2746.794848	225529.045962	39.530868
2749.546118	225886.053695	39.535885
2752.567316	226248.608320	39.540903
2755.123267	226618.069032	39.545920
2758.616183	226978.441664	39.550938
2761.375004	227341.545118	39.555956
2764.196209	227696.509504	39.560973
2767.903886	228043.435208	39.565991
2770.266323	228392.373880	39.571008
2773.312949	228742.095141	39.576026
2776.298525	229085.271566	39.581044
2779.226469	229434.198179	39.586061
2781.870809	229794.575233	39.591079
2784.568932	230148.364143	39.596096
2787.120346	230493.792420	39.601114
2790.118784	230849.058559	39.606132
2792.414378	231204.332299	39.611149
2795.141938	231578.693260	39.616167
2798.037671	231934.305117	39.621184
2801.664944	232254.491428	39.626202
2804.776625	232602.930795	39.631220
2807.463012	232941.655625	39.636237
2810.589360	233280.946885	39.641255
2813.251272	233627.016838	39.646272
2816.062856	233961.783942	39.651290
2818.826399	234308.320288	39.656308
2821.548885	234659.613291	39.661325
2823.984558	234993.853880	39.666343
2826.979644	235346.475731	39.671360
2828.898208	235690.144856	39.676378
2831.949020	236054.138335	39.681396
2834.761065	236411.995526	39.686413
2837.386403	236760.507464	39.691431
2839.640298	237110.651907	39.696448
2842.345725	237450.513465	39.701466
2844.900446	237791.668327	39.706484
2847.180498	238135.787006	39.711501
2850.347325	238468.437323	39.716519
2852.704898	238825.575250	39.721536
2855.222574	239169.732049	39.726554
2857.946192	239533.671147	39.731572
2860.328583	239894.436656	39.736589
2863.458854	240259.708757	39.741607
2866.027256	240648.007098	39.746624
2868.466146	241025.630223	39.751642
2871.076953	241414.530545	39.756660
2873.675948	241807.979314	39.761677
2877.162945	242195.573551	39.766695
2879.601913	242604.643573	39.771712
2882.680165	243004.061826	39.776730
2885.462547	243404.389153	39.781748
2888.728080	243823.667509	39.786765
2891.822365	244221.760201	39.791783
2894.487968	244627.006318	39.796800
2897.545177	245033.283062	39.801818
2900.774104	245445.222550	39.806836
2903.795009	245862.502784	39.811853
2907.176547	246268.828243	39.816871
2909.654738	246690.712907	39.821888
2912.902332	247102.265047	39.826906
2915.901850	247519.164055	39.831924
2919.090865	247937.531396	39.836941
2922.307757	248348.120280	39.841959
2924.713622	248760.968245	39.846976
2927.836732	249185.210915	39.851994
2931.072698	249598.842218	39.857012
2933.928194	250017.942411	39.862029
2936.905935	250432.018301	39.867047
2940.376983	250857.167925	39.872064
2943.510756	251267.534111	39.877082
2946.464798	251684.023695	39.882100
2949.722788	252089.897669	39.887117
2953.017651	252504.833310	39.892135
2955.898411	252915.818777	39.897152
2959.175086	253322.931248	39.902170
2962.497019	253718.858823	39.907188
2965.104392	254125.793804	39.912205
2968.484857	254520.643210	39.917223
2971.550285	254937.106372	39.922240
2974.477922	255338.450516	39.927258
2977.488826	255747.477127	39.932276
2980.360147	256143.213988	39.937293
2983.306976	256540.385797	39.942311
2986.273544	256946.926338	39.947328
2989.458152	257349.342125	39.952346
2992.550928	257754.412641	39.957364
2995.013610	258158.081274	39.962381
2998.171533	258564.510705	39.967399
3001.088089	258972.246400	39.972416
3003.995433	259387.170538	39.977434
3007.293161	259779.857876	39.982452
3010.768784	260183.463820	39.987469
3014.216359	260578.843048	39.992487
3017.504918	260971.908863	39.997504
3020.439148	261351.820403	40.002522
3023.674440	261735.798644	40.007540
3026.148679	262132.797205	40.012557
3029.335349	262518.405943	40.017575
3032.643496	262902.394249	40.022592
3035.614414	263294.713995	40.027610
3038.567320	263678.729450	40.032628
3041.159231	264055.865638	40.037645
3044.353277	264421.096047	40.042663
3046.998795	264780.873489	40.047680
3049.749574	265137.483803	40.052698
3053.026587	265489.464544	40.057716
3055.559459	265849.179605	40.062733
3058.575964	266209.351511	40.067751
3061.252067	266580.623628	40.072768
3063.827319	266955.948470	40.077786
3066.823037	267341.391343	40.082804
3069.843548	267729.597291	40.087821
3072.668731	268126.162794	40.092839
3075.231029	268522.462790	40.097856
3078.067666	268939.824432	40.102874
3081.026673	269339.005485	40.107892
3083.614193	269765.215397	40.112909
3086.629521	270186.937530	40.117927
3090.060037	270614.637800	40.122944
3092.780679	271056.212084	40.127962
3096.008679	271491.914599	40.132980
3099.085407	271938.432445	40.137997
3101.997792	272382.687846	40.143015
3105.030896	272828.649214	40.148032
3108.435846	273284.582262	40.153050
3111.699188	273744.192081	40.158068
3114.643325	274201.106231	40.163085
3117.706050	274654.418518	40.168103
3121.247089	275106.942805	40.173120
3124.979676	275573.783755	40.178138
3128.421439	276016.007557	40.183156
3131.605046	276483.258874	40.188173
3135.111679	276937.987799	40.193191
3138.648661	277388.773054	40.198208
3141.624043	277836.265506	40.203226
3145.045298	278281.730561	40.208244
3148.272059	278733.775327	40.213261
3151.417139	279180.243200	40.218279
3154.709167	279637.021384	40.223296
3157.644767	280094.842675	40.228314
3161.229488	280536.332912	40.233332
3164.483255	280973.224815	40.238349
3168.483250	281412.258115	40.243367
3171.891161	281857.424761	40.248384
3174.983738	282285.014210	40.253402
3178.406343	282715.825591	40.258420
3181.502333	283163.800653	40.263437
3184.918179	283594.404622	40.268455
3188.485610	284027.851839	40.273472
3191.242109	284462.260542	40.278490
3194.552129	284892.187365	40.283508
3197.777027	285326.873252	40.288525
3201.233729	285756.492512	40.293543
3204.509561	286191.495065	40.298560
3207.246738	286617.919768	40.303578
3210.451444	287046.325785	40.308596
3213.257397	287482.662688	40.313613
3216.492949	287926.268162	40.318631
3219.375191	288360.987666	40.323648
3222.685251	288813.538858	40.328666
3225.740257	289257.671185	40.333684
3228.900422	289702.520423	40.338701
3231.953172	290150.480996	40.343719
3235.539590	290592.921674	40.348736
3238.301346	291048.614625	40.353754
3241.630510	291501.930793	40.358772
3244.804448	291960.701358	40.363789
3248.199793	292412.629456	40.368807
3250.968468	292867.038398	40.373824
3254.022544	293300.808324	40.378842
3257.447406	293728.880914	40.383860
3260.712623	294152.049718	40.388877
3263.669711	294575.212685	40.393895
3267.316985	294991.207034	40.398912
3270.112269	295417.334285	40.403930
3273.426533	295829.997767	40.408948
3276.753362	296269.949137	40.413965
3279.684482	296701.047394	40.418983
3282.891923	297126.260120	40.424000
3285.964121	297582.286423	40.429018
3288.898670	298025.103415	40.434036
3292.696788	298472.504645	40.439053
3296.009409	298917.083683	40.444071
3299.620626	299369.711230	40.449088
3302.297634	299830.985100	40.454106
3305.705772	300287.140128	40.459124
3309.066579	300752.615590	40.464141
3312.138226	301223.615516	40.469159
3315.433039	301690.489434	40.474176
3318.360034	302184.147899	40.479194
3321.897772	302653.717280	40.484212
3324.978933	303141.834161	40.489229
3328.495708	303634.371911	40.494247
3332.289636	304115.159416	40.499264
3335.303831	304600.607679	40.504282
3338.691819	305092.060108	40.509300
3342.843242	305589.075105	40.514317
3346.440727	306080.409286	40.519335
3349.677142	306567.505034	40.524352
3353.060286	307061.274490	40.529370
3356.722274	307547.812220	40.534388
3360.309313	308041.337187	40.539405
3363.721136	308521.710840	40.544423
3367.307072	309008.093746	40.549440
3370.840871	309505.546596	40.554458
3374.300778	309986.050672	40.559476
3377.426170	310478.886794	40.564493
3381.269638	310973.179773	40.569511
3384.686848	311454.817971	40.574528
3387.599085	311952.088400	40.579546
3391.235355	312434.596259	40.584564
3395.055773	312937.121053	40.589581
3398.497720	313436.044588	40.594599
3402.042539	313919.515776	40.599616
3405.174867	314404.568867	40.604634
3408.486613	314899.030036	40.609652
3412.216415	315390.629097	40.614669
3415.697636	315885.738413	40.619687
3419.393866	316372.332412	40.624704
3422.906852	316866.969182	40.629722
3426.473736	317342.051044	40.634740
3430.455554	317833.685654	40.639757
3433.476693	318314.272844	40.644775
3437.271729	318785.370184	40.649792
3440.621455	319273.838772	40.654810
3444.025195	319754.731249	40.659828
3447.234953	320235.420182	40.664845
3450.748807	320713.569579	40.669863
3454.133621	321193.383142	40.674880
3457.522017	321692.323835	40.679898
3460.621326	322177.930941	40.684916
3464.480632	322668.083168	40.689933
3467.526776	323152.900677	40.694951
3471.200721	323648.398929	40.699968
3474.453416	324139.186519	40.704986
3478.056975	324627.350945	40.710004
3481.699098	325110.073678	40.715021
3484.783622	325595.805123	40.720026
3488.666600	326019.376772	40.725031
3491.569640	326415.954747	40.730036
3494.319090	326759.312655	40.735040
3497.313462	327072.257725	40.740045
3499.936763	327336.444796	40.745050
3502.372806	327542.968807	40.750055
3504.605561	327729.123228	40.755060
3506.362700	327878.671356	40.760064
3508.264892	327965.648151	40.765069
3510.586104	328033.634862	40.770074
3512.217317	328045.743340	40.775079
3513.326560	328047.402368	40.780084
3514.663166	328007.361166	40.785088
3515.732607	327944.265189	40.790093
3516.121360	327859.984673	40.795098
3517.384254	327741.635542	40.800103
3517.687238	327620.637402	40.805108
3518.312410	327478.298193	40.810112
3519.104306	327314.031394	40.815117
3519.429610	327147.521767	40.820122
3519.638294	326959.611570	40.825127
3519.835306	326769.667336	40.830132
3520.187453	326565.224221	40.835136
3520.424857	326343.500444	40.840141
3520.178059	326130.245216	40.845146
3520.639038	325905.024736	40.850151
3520.750093	325672.607662	40.855156
3520.447325	325434.784478	40.860160
3520.827576	325194.258929	40.865165
3520.808205	324947.052992	40.870170
3520.866916	324700.316749	40.875175
3520.504471	324454.967376	40.880180
3520.521656	324202.027581	40.885184
3520.278846	323947.549484	40.890189
3519.893807	323708.889652	40.895194
3519.877038	323459.105064	40.900199
3519.466792	323209.609164	40.905204
3519.115188	322967.963478	40.910208
3518.800088	322729.439802	40.915213
3518.659812	322505.286522	40.920218
3518.567013	322257.058433	40.925223
3518.031384	322026.451491	40.930228
3517.901763	321790.615737	40.935232
3517.747452	321553.408732	40.940237
3517.283864	321332.734011	40.945242
3517.278120	321107.280376	40.950247
3516.773842	320899.737139	40.955252
3516.247363	320671.843602	40.960256
3516.734530	320454.603575	40.965261
3516.002036	320249.356963	40.970266
3516.133983	320032.907882	40.975271
3515.729243	319821.425991	40.980276
3515.677044	319615.383586	40.985280
3515.490423	319410.429672	40.990285
3514.825591	319205.498325	40.995290
3515.125152	319005.580653	41.000295
3514.486920	318811.328921	41.005300
3514.177452	318607.942321	41.010304
3514.382380	318422.284316	41.015309
3514.156298	318244.630617	41.020314
3513.716588	318054.975157	41.025319
3513.583152	317873.158422	41.030324
3513.340211	317683.725175	41.035328
3513.377856	317513.253219	41.040333
3513.131666	317333.817997	41.045338
3513.015054	317156.855300	41.050343
3512.926491	316983.296909	41.055348
3512.406704	316806.802653	41.060352
3512.452208	316639.862738	41.065357
3512.127918	316484.505594	41.070362
3512.156195	316313.521652	41.075367
3511.650997	316148.980965	41.080372
3511.427219	316003.478619	41.085376
3511.443454	315844.326062	41.090381
3511.454050	315686.827671	41.095386
3511.645857	315528.282778	41.100391
3511.225982	315379.475790	41.105396
3510.856772	315239.591301	41.110400
3511.133380	315080.319217	41.115405
3510.674396	314946.732505	41.120410
3510.591476	314793.392984	41.125415
3510.750417	314659.454833	41.130420
3510.567424	314509.386818	41.135424
3510.310090	314366.250799	41.140429
3510.082893	314229.343580	41.145434
3510.275503	314096.314556	41.150439
3510.034019	313967.856424	41.155444
3509.982637	313829.317638	41.160448
3509.782356	313693.702330	41.165453
3509.659849	313561.789492	41.170458
3509.573506	313421.422888	41.175463
3509.385522	313293.590689	41.180468
3509.141076	313171.059530	41.185472
3509.312319	313041.389575	41.190477
3508.924689	312926.106513	41.195482
3508.995493	312798.690704	41.200487
3509.130215	312686.939016	41.205492
3508.721141	312563.795747	41.210496
3508.666507	312441.385813	41.215501
3508.510157	312331.663332	41.220506
3508.744277	312217.986638	41.225511
3508.440006	312099.609641	41.230516
3508.375538	311981.118694	41.235520
3508.318914	311870.565355	41.240525
3507.941434	311762.987974	41.245530
3508.130929	311658.935456	41.250535
3507.493706	311547.606548	41.255540
3507.892532	311441.383508	41.260544
3507.845575	311340.369733	41.265549
3507.715038	311243.770951	41.270554
3507.776316	311131.034614	41.275559
3507.400465	311040.326245	41.280564
3507.328435	310940.460612	41.285568
3507.826432	310831.014534	41.290573
3507.427519	310733.056928	41.295578
3507.451031	310627.602986	41.300583
3507.800143	310529.808475	41.305588
3507.665092	310433.488675	41.310592
3507.940551	310329.877929	41.315597
3507.467139	310240.048419	41.320602
3507.477262	310128.997176	41.325607
3507.334704	310029.318754	41.330612
3507.085845	309923.498507	41.335616
3507.374912	309834.669257	41.340621
3507.163772	309738.283570	41.345626
3507.169408	309641.456806	41.350631
3507.386064	309547.828798	41.355636
3507.230543	309442.578262	41.360640
3507.406613	309339.998756	41.365645
3506.796636	309252.936971	41.370650
3506.805482	309152.317087	41.375655
3506.904441	309053.464292	41.380660
3506.877307	308968.805148	41.385664
3507.009331	308875.570734	41.390669
3506.907664	308781.609082	41.395674
3506.769418	308686.431457	41.400679
3506.942095	308607.262725	41.405684
3507.136055	308518.776704	41.410688
3507.024191	308414.585969	41.415693
3506.773882	308320.417537	41.420698
3507.086801	308232.879507	41.425703
3507.285982	308143.577671	41.430708
3506.603146	308044.742716	41.435712
3506.664396	307953.935125	41.440717
3506.866774	307874.862390	41.445722
3506.958310	307782.980958	41.450727
3506.336201	307688.691046	41.455732
3506.620352	307597.440948	41.460736
3506.536332	307504.059431	41.465741
3506.395775	307423.130728	41.470746
3506.539492	307333.632482	41.475751
3506.485040	307244.114017	41.480756
3506.372363	307159.923163	41.485760
3506.555715	307075.151685	41.490765
3506.124247	306991.570022	41.495770
3505.958717	306908.964775	41.500775
3506.049732	306818.125040	41.505780
3506.029543	306741.451862	41.510784
3505.994891	306653.456177	41.515789
3506.030436	306581.685669	41.520794
3505.876394	306500.604886	41.525799
3506.224194	306423.797615	41.530804
3506.125444	306346.754331	41.535808
3506.241482	306261.864716	41.540813
3505.946960	306180.881627	41.545818
3505.834296	306094.042308	41.550823
3506.173126	306019.424427	41.555828
3506.013376	305950.635493	41.560832
3506.044625	305869.957500	41.565837
3505.822843	305797.487903	41.570842
3505.917610	305707.892596	41.575847
3505.556842	305633.408465	41.580852
3505.954841	305549.822590	41.585856
3505.680604	305476.393630	41.590861
3505.531556	305408.951109	41.595866
3505.895055	305325.242990	41.600871
3505.522498	305255.086523	41.605876
3505.714768	305183.976787	41.610880
3505.903101	305108.490268	41.615885
3505.594718	305035.982170	41.620890
3505.680423	304954.887068	41.625895
3505.683852	304876.476843	41.630900
3505.465508	304804.132553	41.635904
3505.646629	304722.945890	41.640909
3505.568184	304656.916574	41.645914
3505.448758	304587.101550	41.650919
3505.269471	304505.767033	41.655924
3504.935750	304437.563036	41.660928
3505.251194	304359.841515	41.665933
3505.359746	304307.423731	41.670938
3505.132714	304236.708787	41.675943
3505.120735	304168.988816	41.680948
3505.369818	304097.995996	41.685952
3505.413175	304030.725332	41.690957
3505.220654	303964.483837	41.695962
3505.089100	303897.927369	41.700967
3505.422112	303832.316526	41.705972
3505.704042	303753.377715	41.710976
3505.915081	303692.850241	41.715981
3505.638964	303611.809346	41.720986
3505.522961	303532.524923	41.725991
3505.398206	303461.996615	41.730996
3505.136924	303396.783109	41.736000
3505.460487	303332.572874	41.741005
3505.130765	303251.997870	41.746010
3505.429504	303187.562269	41.751015
3505.264500	303115.283685	41.756020
3505.397047	303036.748798	41.761024
3505.780366	302965.020944	41.766029
3505.450979	302896.025298	41.771034
3505.265984	302812.983855	41.776039
3505.595611	302747.143131	41.781044
3505.349955	302684.802225	41.786048
3505.477044	302612.808359	41.791053
3505.271881	302542.978502	41.796058
3505.295513	302468.786333	41.801063
3505.159601	302400.447103	41.806068
3505.027585	302345.316120	41.811072
3504.949489	302265.463980	41.816077
3505.307016	302209.442252	41.821082
3505.495373	302128.657665	41.826087
3505.038011	302068.003286	41.831092
3504.647729	301993.060437	41.836096
3505.195930	301931.918563	41.841101
3504.952575	301864.104385	41.846106
3505.224062	301802.547306	41.851111
3505.320938	301730.607854	41.856116
3505.121537	301655.380318	41.861120
3505.302642	301580.347977	41.866125
3504.666442	301519.517197	41.871130
3504.929094	301452.005524	41.876135
3504.784288	301394.457691	41.881140
3504.715530	301334.429193	41.886144
3504.729545	301273.344246	41.891149
3504.466569	301215.025621	41.896154
3504.827625	301145.818468	41.901159
3504.638974	301080.590824	41.906164
3504.454787	301029.182504	41.911168
3504.684938	300950.553012	41.916173
3504.606363	300902.284112	41.921178
3504.604041	300839.750487	41.926183
3504.787198	300784.237989	41.931188
3504.759017	300722.675409	41.936192
3504.872098	300662.948741	41.941197
3504.398408	300597.332196	41.946202
3504.569863	300543.348368	41.951207
3504.764710	300481.954423	41.956212
3504.424178	300425.632246	41.961216
3505.368476	300357.122331	41.966221
3504.586122	300298.119993	41.971226
3504.654933	300223.688640	41.976231
3504.734372	300169.998732	41.981236
3505.073778	300113.468619	41.986240
3504.930744	300050.625113	41.991245
3504.517447	299994.593785	41.996250
3504.864090	299918.337154	42.001255
3504.843046	299862.626430	42.006260
3504.669661	299809.739070	42.011264
3504.589973	299739.198864	42.016269
3504.679605	299683.496188	42.021274
3504.300594	299619.263598	42.026279
3504.729061	299551.723773	42.031284
3504.781276	299496.484868	42.036288
3504.667924	299437.275692	42.041293
3504.625718	299380.142456	42.046298
3504.461147	299320.126656	42.051303
3504.754039	299266.504461	42.056308
3504.586737	299205.827205	42.061312
3504.324814	299137.528933	42.066317
3504.436069	299084.952918	42.071322
3504.037458	299029.300109	42.076327
3504.437776	298969.934144	42.081332
3504.584932	298917.301479	42.086336
3504.608259	298855.092488	42.091341
3504.337033	298791.402119	42.096346
3504.303071	298740.528235	42.101351
3504.540228	298679.380228	42.106356
3504.487848	298627.720082	42.111360
3504.795303	298557.219940	42.116365
3504.560322	298506.784366	42.121370
3504.314633	298448.892811	42.126375
3504.467638	298397.684091	42.131380
3504.580376	298338.642186	42.136384
3504.334731	298263.162674	42.141389
3504.520990	298210.192375	42.146394
3504.360582	298146.229502	42.151399
3504.747097	298096.969482	42.156404
3504.625723	298045.930402	42.161408
3504.415622	297982.484131	42.166413
3504.362547	297933.088751	42.171418
3504.658244	297870.352682	42.176423
3504.530483	297806.715230	42.181428
3504.565197	297755.855222	42.186432
3504.588345	297691.379665	42.191437
3504.387422	297640.199881	42.196442
3504.897224	297581.477190	42.201447
3504.857264	297509.349907	42.206452
3504.467763	297455.603096	42.211456
3504.550588	297395.139492	42.216461
3504.107570	297339.059220	42.221466
3504.277093	297284.563477	42.226471
3504.749639	297220.730141	42.231476
3504.177339	297162.480845	42.236480
3504.097480	297100.158711	42.241485
3504.013586	297059.905056	42.246490
3504.524971	297008.512047	42.251495
3504.233833	296947.902538	42.256500
3503.883018	296897.279929	42.261504
3504.178684	296840.727873	42.266509
3504.148373	296784.302847	42.271514
3504.090279	296737.070743	42.276519
3504.005643	296697.427829	42.281524
3503.973583	296643.624632	42.286528
3504.099839	296581.168047	42.291533
3503.936947	296530.923127	42.296538
3504.068709	296484.577595	42.301543
3504.054345	296424.255358	42.306548
3503.784665	296381.102988	42.311552
3504.042666	296322.010936	42.316557
3503.936755	296276.796723	42.321562
3503.873905	296230.328549	42.326567
3503.835880	296172.707809	42.331572
3503.720927	296116.702559	42.336576
3504.221435	296069.561158	42.341581
3504.234370	296029.011725	42.346586
3504.185864	295974.854114	42.351591
3504.189058	295917.913955	42.356596
3504.153444	295865.968707	42.361600
3504.498226	295809.178916	42.366605
3504.034382	295749.256820	42.371610
3504.083075	295696.687412	42.376615
3504.224718	295652.452342	42.381620
3504.315028	295605.018044	42.386624
3504.256468	295528.971286	42.391629
3504.221707	295489.319785	42.396634
3503.595448	295434.004337	42.401639
3503.821801	295383.086958	42.406644
3503.918146	295349.829349	42.411648
3504.017428	295284.448365	42.416653
3503.996277	295243.827328	42.421658
3504.074734	295186.849291	42.426663
3504.005351	295131.574171	42.431668
3503.826836	295085.453987	42.436672
3504.125296	295026.812500	42.441677
3504.011889	294982.591159	42.446682
3503.793596	294938.157020	42.451687
3503.858451	294885.635279	42.456692
3503.794792	294834.660738	42.461696
3504.211757	294786.614956	42.466701
3503.782418	294732.057284	42.471706
3503.834434	294675.464680	42.476711
3504.006388	294630.104138	42.481716
3504.069302	294584.964163	42.486720
3504.118968	294533.946275	42.491725
3504.174963	294489.520025	42.496730
3504.106927	294433.302232	42.501735
3504.159742	294376.861944	42.506740
3503.669637	294321.346084	42.511744
3504.046770	294262.844324	42.516749
3503.851792	294215.529667	42.521754
3503.817576	294169.539041	42.526759
3504.115434	294120.849440	42.531764
3503.684729	294075.149530	42.536768
3503.885088	294026.347752	42.541773
3503.858449	293977.453985	42.546778
3503.286761	293942.492268	42.551783
3503.706401	293894.343532	42.556788
3503.354986	293855.427484	42.561792
3503.599201	293800.280505	42.566797
3503.499750	293759.645182	42.571802
3503.585927	293711.726373	42.576807
3503.669017	293666.480745	42.581812
3503.636058	293626.725898	42.586816
3503.701140	293568.501112	42.591821
3503.309003	293527.911178	42.596826
3503.557937	293479.075941	42.601831
3503.653616	293448.897395	42.606836
3503.312125	293396.259391	42.611840
3503.797734	293350.034517	42.616845
3503.539844	293320.929119	42.621850
3503.682297	293267.197502	42.626855
3503.758984	293218.134310	42.631860
3503.461164	293184.020454	42.636864
3503.899715	293130.420823	42.641869
3503.769075	293083.044351	42.646874
3503.677884	293023.265153	42.651879
3503.935036	292980.741058	42.656884
3503.555641	292938.290533	42.661888
3504.186905	292878.984233	42.666893
3503.890074	292837.640810	42.671898
3503.755763	292787.108257	42.676903
3503.992114	292733.692471	42.681908
3503.754844	292679.968514	42.686912
3503.498813	292640.145912	42.691917
3503.609479	292604.491769	42.696922
3503.540626	292558.658035	42.701927
3503.657111	292506.991653	42.706932
3503.599290	292471.465471	42.711936
3503.402657	292417.836781	42.716941
3503.494313	292376.458046	42.721946
3503.538975	292337.199379	42.726951
3503.890183	292284.172611	42.731956
3503.856018	292242.456992	42.736960
3503.712534	292187.521611	42.741965
3503.565407	292141.623379	42.746970
3503.632695	292086.858751	42.751975
3503.930557	292046.033178	42.756980
3503.770534	291999.678652	42.761984
3503.627482	291948.255829	42.766989
3503.682679	291910.675306	42.771994
3503.403856	291863.066393	42.776999
3503.808425	291817.056614	42.782004
3503.620870	291778.521023	42.787009
3503.711190	291725.814382	42.792013
3503.566302	291679.813637	42.797018
3503.486615	291629.398907	42.802023
3503.625199	291583.404889	42.807028
3503.604350	291541.304891	42.812033
3503.693076	291493.536676	42.817037
3503.734788	291451.426881	42.822042
3503.499596	291403.174436	42.827047
3503.628204	291351.759754	42.832052
3503.257899	291312.132264	42.837057
3503.370911	291279.658945	42.842061
3503.492167	291236.823869	42.847066
3503.432571	291191.725893	42.852071
3503.455062	291154.811849	42.857076
3503.180968	291108.245305	42.862081
3503.464643	291068.668627	42.867085
3503.121323	291022.316437	42.872090
3503.141919	290975.194821	42.877095
3503.163449	290936.702539	42.882100
3503.488641	290900.708562	42.887105
3503.498498	290859.316086	42.892109
3503.624409	290822.920326	42.897114
3503.583726	290777.615461	42.902119
3503.579140	290732.737697	42.907124
3503.550127	290682.467052	42.912129
3503.449809	290645.317260	42.917133
3503.657201	290602.570169	42.922138
3503.662988	290560.567188	42.927143
3503.621790	290519.793376	42.932148
3503.600946	290471.557768	42.937153
3503.554972	290418.463938	42.942157
3503.298423	290375.305224	42.947162
3503.458622	290328.950536	42.952167
3503.706689	290286.222357	42.957172
3503.759708	290250.372186	42.962177
3503.719064	290197.990110	42.967181
3503.647972	290156.635226	42.972186
3503.532734	290106.453908	42.977191
3503.319116	290057.051543	42.982196
3503.196957	290025.963348	42.987201
3503.243920	289974.229315	42.992205
3503.309278	289938.198854	42.997210
3503.110012	289903.838748	43.002215
3502.894225	289864.899074	43.007220
3503.377520	289833.792938	43.012225
3503.252673	289779.208927	43.017229
3503.314902	289745.062606	43.022234
3502.878004	289709.135629	43.027239
3503.227150	289662.852877	43.032244
3503.305983	289629.620339	43.037249
3503.163312	289588.810806	43.042253
3503.476857	289552.486943	43.047258
3503.175627	289505.948896	43.052263
3503.143703	289466.751260	43.057268
3503.130043	289428.645383	43.062273
3503.383166	289374.053122	43.067277
3503.574026	289338.995593	43.072282
3503.020890	289301.940935	43.077287
3503.560907	289264.130648	43.082292
3503.376003	289222.920151	43.087297
3503.343474	289181.431352	43.092301
3503.086033	289134.809852	43.097306
3502.996233	289105.498130	43.102311
3503.204985	289057.403919	43.107316
3503.590929	289022.392230	43.112321
3503.337145	288976.330090	43.117325
3503.347006	288940.180421	43.122330
3503.117142	288898.773060	43.127335
3503.301512	288848.696872	43.132340
3503.245941	288814.797498	43.137345
3503.247056	288772.514044	43.142349
3503.408444	288731.656652	43.147354
3503.171482	288695.697995	43.152359
3503.188994	288656.492173	43.157364
3503.193694	288620.164931	43.162369
3503.289790	288574.277170	43.167373
3502.811147	288549.226066	43.172378
3502.893276	288509.399138	43.177383
3503.131750	288472.729954	43.182388
3503.368400	288434.457255	43.187393
3503.445294	288397.227667	43.192397
3503.024751	288353.965826	43.197402
3503.098681	288325.290150	43.202407
3503.013064	288277.113884	43.207412
3503.221051	288254.170565	43.212417
3503.198427	288192.874148	43.217421
3503.017140	288163.678064	43.222426
3503.200650	288125.820764	43.227431
3503.260189	288079.556490	43.232436
3503.250621	288043.765742	43.237441
3503.185752	288001.339314	43.242445
3502.955104	287959.753278	43.247450
3502.615355	287928.137878	43.252455
3503.072967	287895.023705	43.257460
3502.847147	287858.655540	43.262465
3502.648701	287830.531172	43.267469
3502.729141	287799.334007	43.272474
3502.956866	287766.662856	43.277479
3503.072092	287727.135786	43.282484
3503.093207	287697.347943	43.287489
3503.065264	287658.937765	43.292493
3503.290328	287621.964707	43.297498
3503.097252	287587.475122	43.302503
3503.332677	287536.779014	43.307508
3502.882337	287505.867963	43.312513
3503.115498	287478.949139	43.317517
3502.903106	287429.722778	43.322522
3502.777886	287398.633798	43.327527
3503.437594	287358.538093	43.332532
3503.055513	287322.346691	43.337537
3503.426674	287285.401625	43.342541
3503.629840	287237.103287	43.347546
3503.256044	287198.339345	43.352551
3502.997520	287155.637021	43.357556
3503.228227	287124.874385	43.362561
3502.894897	287076.048440	43.367565
3503.131173	287044.648468	43.372570
3503.076414	287003.874552	43.377575
3503.184445	286963.864457	43.382580
3502.987853	286928.534984	43.387585
3503.089361	286891.071597	43.392589
3503.435727	286859.094344	43.397594
3503.037244	286816.337209	43.402599
3503.265833	286772.311424	43.407604
3502.969888	286736.208129	43.412609
3503.314880	286699.979619	43.417613
3503.324351	286658.482688	43.422618
3503.104534	286623.233040	43.427623
3503.126135	286578.475613	43.432628
3502.960256	286542.962954	43.437633
3502.879562	286500.690773	43.442637
3503.020826	286469.458061	43.447642
3502.943175	286440.346920	43.452647
3503.232166	286401.504835	43.457652
3503.015507	286369.564047	43.462657
3503.141949	286343.476015	43.467661
3502.982551	286304.627276	43.472666
3502.546461	286260.093606	43.477671
3503.031935	286228.119862	43.482676
3502.999013	286187.418424	43.487681
3502.780508	286149.546185	43.492685
3503.059053	286115.848010	43.497690
3503.008458	286085.994233	43.502695
3503.140524	286050.409493	43.507700
3503.112888	286014.009480	43.512705
3502.924846	285977.328917	43.517709
3502.833692	285920.979871	43.522714
3502.948707	285899.374011	43.527719
3503.304562	285851.916481	43.532724
3503.032403	285824.235521	43.537729
3503.002688	285791.119767	43.542733
3503.057246	285756.565246	43.547738
3502.964642	285715.363655	43.552743
3502.938827	285675.322708	43.557748
3503.032182	285641.042127	43.562753
3503.017369	285596.493379	43.567757
3502.632570	285563.992844	43.572762
3502.483668	285533.899543	43.577767
3503.166967	285499.985331	43.582772
3503.006893	285459.863318	43.587777
3503.037479	285425.134153	43.592781
3503.065349	285387.961430	43.597786
3502.558210	285356.039909	43.602791
3502.616517	285317.487681	43.607796
3502.828761	285289.527460	43.612801
3502.860304	285251.132108	43.617805
3502.950193	285225.533038	43.622810
3502.747417	285195.575262	43.627815
3502.832680	285161.728486	43.632820
3502.864518	285125.369661	43.637825
3502.825689	285086.857877	43.642829
3503.063604	285056.551424	43.647834
3502.746466	285029.589968	43.652839
3503.002592	285004.855980	43.657844
3502.844813	284965.395230	43.662849
3503.008251	284923.058621	43.667853
3502.900127	284888.401686	43.672858
3502.735862	284858.412312	43.677863
3502.941252	284804.791140	43.682868
3502.756874	284781.780401	43.687873
3502.807700	284749.440815	43.692877
3502.789357	284711.078382	43.697882
3503.206769	284687.490260	43.702887
3502.998953	284653.612468	43.707892
3503.077643	284612.790891	43.712897
3502.908372	284577.939651	43.717901
3502.967512	284541.219853	43.722906
3502.686533	284504.934837	43.727911
3502.954986	284463.421728	43.732916
3502.663386	284440.503936	43.737921
3502.700799	284409.617402	43.742925
3502.654204	284374.390553	43.747930
3502.936004	284355.176795	43.752935
3502.734787	284306.353761	43.757940
3502.580237	284269.183364	43.762945
3502.719158	284242.634341	43.767949
3502.556748	284208.061889	43.772954
3502.708024	284189.173898	43.777959
3502.555006	284147.191561	43.782964
3502.726507	284125.474521	43.787969
3502.846363	284095.058728	43.792973
3502.952958	284053.545104	43.797978
3502.944219	284016.097298	43.802983
3502.919237	283984.889325	43.807988
3502.867615	283952.718062	43.812993
3502.641800	283911.968919	43.817997
3502.889348	283883.391634	43.823002
3502.438531	283846.445325	43.828007
3502.611234	283816.199397	43.833012
3502.406399	283785.986748	43.838017
3502.613110	283753.342398	43.843021
3502.848688	283731.207928	43.848026
3502.965048	283689.412525	43.853031
3502.994750	283655.573663	43.858036
3502.874204	283631.763395	43.863041
3502.708791	283596.198224	43.868045
3502.516190	283560.764558	43.873050
3502.750126	283534.913323	43.878055
3502.925028	283492.395851	43.883060
3502.565995	283465.236639	43.888065
3502.825115	283439.763330	43.893069
3503.037756	283399.633045	43.898074
3502.885386	283370.354024	43.903079
3502.504452	283324.002307	43.908084
3502.889208	283300.978893	43.913089
3502.873981	283274.758997	43.918093
3502.682897	283231.916440	43.923098
3502.783657	283201.197728	43.928103
3502.555597	283171.064806	43.933108
3502.912812	283137.505695	43.938113
3502.655784	283116.313287	43.943117
3502.718438	283082.188977	43.948122
3502.703241	283040.159074	43.953127
3502.905682	283012.555892	43.958132
3502.498881	282982.068822	43.963137
3502.500369	282958.290255	43.968141
3502.948259	282927.110066	43.973146
3502.796689	282893.604555	43.978151
3502.360398	282860.856183	43.983156
3502.656734	282829.190357	43.988161
3502.267377	282804.937923	43.993165
3502.742430	282766.675864	43.998170
3502.277915	282735.255689	44.003175
3502.324963	282708.720387	44.008180
3502.433430	282682.710155	44.013185
3502.351934	282665.665564	44.018189
3502.327212	282634.813382	44.023194
3502.502448	282609.123699	44.028199
3502.635138	282572.289596	44.033204
3502.814085	282552.302127	44.038209
3502.586127	282521.965243	44.043213
3502.893138	282482.074346	44.048218
3502.922821	282458.774948	44.053223
3502.553923	282425.099364	44.058228
3502.323397	282388.525361	44.063233
3502.250580	282355.872950	44.068237
3502.586730	282329.445274	44.073242
3502.729334	282313.027663	44.078247
3502.594887	282281.148582	44.083252
3502.712521	282249.052045	44.088257
3502.196548	282224.309937	44.093261
3502.463292	282190.586248	44.098266
3502.637141	282160.670408	44.103271
3502.501767	282133.272211	44.108276
3502.735757	282105.561935	44.113281
3502.578139	282078.905494	44.118285
3502.703554	282036.496695	44.123290
3502.660244	282013.946828	44.128295
3502.876027	281969.283520	44.133300
3502.735496	281942.573451	44.138305
3502.507619	281912.949156	44.143309
3502.720189	281893.083569	44.148314
3502.362239	281861.137245	44.153319
3502.842020	281826.540081	44.158324
3502.891669	281800.054959	44.163329
3502.768403	281763.311192	44.168333
3502.876066	281733.660069	44.173338
3502.525283	281697.002592	44.178343
3502.781242	281662.974825	44.183348
3502.704116	281635.440080	44.188353
3502.902569	281598.315196	44.193357
3502.986469	281574.192378	44.198362
3502.696716	281544.959452	44.203367
3502.769453	281507.293979	44.208372
3503.034875	281471.838927	44.213377
3502.615083	281441.964252	44.218381
3502.884401	281401.340306	44.223386
3502.918573	281368.187075	44.228391
3503.018377	281327.131197	44.233396
3502.930447	281309.832695	44.238401
3502.600599	281263.675378	44.243405
3502.963342	281226.932092	44.248410
3502.769986	281199.135216	44.253415
3502.874074	281165.258148	44.258420
3502.479831	281136.779643	44.263425
3502.621675	281103.507700	44.268429
3502.761086	281062.852863	44.273434
3502.592246	281033.269944	44.278439
3502.622614	281005.972830	44.283444
3502.590619	280979.169142	44.288449
3502.603086	280946.553749	44.293453
3502.707658	280911.709027	44.298458
3502.443425	280883.057436	44.303463
3502.412937	280863.738584	44.308468
3502.683387	280837.473351	44.313473
3502.706931	280821.201230	44.318477
3502.707916	280775.679535	44.323482
3502.508204	280752.720804	44.328487
3502.699157	280711.344885	44.333492
3502.520714	280683.469115	44.338497
3502.385904	280653.193338	44.343501
3502.775161	280622.912375	44.348506
3502.429163	280588.061237	44.353511
3502.789669	280566.288255	44.358516
3502.820094	280549.378512	44.363521
3502.682106	280509.708547	44.368525
3502.672018	280472.335492	44.373530
3502.641020	280434.787454	44.378535
3502.249134	280411.222030	44.383540
3502.328876	280377.042874	44.388545
3502.387718	280356.666140	44.393549
3502.303819	280320.806620	44.398554
3502.255297	280302.559739	44.403559
3502.454293	280268.718413	44.408564
3502.440683	280239.263780	44.413569
3502.812217	280219.933122	44.418573
3502.685049	280191.870970	44.423578
3502.669207	280159.005039	44.428583
3502.755642	280132.437215	44.433588
3502.548365	280097.487881	44.438593
3502.616711	280071.228368	44.443597
3502.669804	280036.976825	44.448602
3502.299774	280000.321502	44.453607
3502.524712	279981.089973	44.458612
3502.556145	279948.165674	44.463617
3502.466451	279918.646375	44.468621
3502.799945	279881.779677	44.473626
3502.190086	279857.586040	44.478631
3502.738833	279827.661837	44.483636
3502.779956	279799.853410	44.488641
3502.284417	279767.494774	44.493645
3502.627602	279745.367811	44.498650
3502.661437	279709.387838	44.503655
3502.904307	279679.663935	44.508660
3502.662074	279645.509090	44.513665
3502.339474	279625.980775	44.518669
3502.724637	279588.138415	44.523674
3502.657731	279558.539049	44.528679
3502.630688	279521.830120	44.533684
3502.567495	279493.554073	44.538689
3502.600155	279471.297131	44.543693
3502.428530	279433.286736	44.548698
3501.899686	279414.172361	44.553703
3502.117710	279399.142672	44.558708
3502.304019	279365.302916	44.563713
3502.337360	279345.184478	44.568717
3502.457542	279300.992726	44.573722
3502.307454	279298.648511	44.578727
3502.493361	279266.489140	44.583732
3502.956268	279228.889104	44.588737
3502.348519	279199.602901	44.593741
3502.357219	279174.523526	44.598746
3502.121223	279151.519032	44.603751
3502.328944	279120.349151	44.608756
3502.482638	279106.245981	44.613761
3502.089177	279081.458297	44.618765
3502.498222	279041.345993	44.623770
3502.602080	279014.927827	44.628775
3502.608362	278997.308608	44.633780
3502.714003	278960.324160	44.638785
3502.485567	278936.198175	44.643789
3502.416517	278900.386592	44.648794
3502.258764	278869.629925	44.653799
3502.563927	278843.053073	44.658804
3502.432240	278824.029510	44.663809
3502.341879	278792.345755	44.668813
3502.355382	278765.534199	44.673818
3502.144922	278743.951385	44.678823
3502.101156	278712.693172	44.683828
3502.488557	278696.618576	44.688833
3502.146527	278659.958249	44.693837
3502.249338	278637.384625	44.698842
3502.373229	278618.143017	44.703847
3502.186440	278605.212993	44.708852
3502.593793	278573.731762	44.713857
3502.131599	278551.678860	44.718861
3502.564347	278509.653063	44.723866
3502.124903	278483.217418	44.728871
3501.876764	278458.254157	44.733876
3502.397543	278437.015754	44.738881
3502.250344	278414.022682	44.743885
3502.893562	278389.378980	44.748890
3502.462831	278356.016704	44.753895
3502.388417	278337.060490	44.758900
3502.474332	278297.532750	44.763905
3502.488278	278274.209035	44.768909
3502.424742	278246.620014	44.773914
3502.525095	278219.336466	44.778919
3502.100044	278196.488409	44.783924
3502.302878	278158.470033	44.788929
3502.355277	278138.730222	44.793933
3502.702969	278110.211503	44.798938
3502.427731	278085.201418	44.803943
3502.324230	278057.924075	44.808948
3502.522779	278029.352155	44.813953
3502.254580	278006.887002	44.818957
3502.581732	277982.699723	44.823962
3502.326505	277950.913977	44.828967
3502.384659	277919.665045	44.833972
3502.619699	277895.975825	44.838977
3502.644503	277867.558184	44.843981
3502.806202	277829.571510	44.848986
3502.366651	277809.475339	44.853991
3502.320380	277781.476098	44.858996
3502.714302	277747.985235	44.864001
3502.342288	277724.925101	44.869005
3502.491324	277693.891082	44.874010
3502.337669	277661.936649	44.879015
3502.591378	277642.903745	44.884020
3502.279267	277613.774621	44.889025
3502.392281	277586.539804	44.894029
3502.607366	277560.765813	44.899034
3502.466069	277544.340420	44.904039
3502.718975	277505.040902	44.909044
3502.526602	277465.657890	44.914049
3502.446611	277448.229970	44.919053
3502.666101	277413.645838	44.924058
3502.394270	277390.570016	44.929063
3502.118254	277371.492175	44.934068
3502.249894	277345.501952	44.939073
3502.448135	277324.542586	44.944077
3502.275449	277294.780590	44.949082
3502.371342	277265.918837	44.954087
3502.185674	277231.499516	44.959092
3502.243396	277203.738494	44.964097
3502.109705	277182.601597	44.969101
3502.188266	277168.280620	44.974106
3501.928529	277147.265170	44.979111
3502.110916	277128.268702	44.984116
3502.128526	277101.990614	44.989121
3502.168300	277067.256071	44.994125
3502.406679	277035.138535	44.999130
3501.928051	277017.085111	45.004135
3502.214290	276988.982923	45.009140
3502.242924	276966.904117	45.014145
3502.106512	276939.835195	45.019149
3502.443868	276910.986661	45.024154
3502.418648	276895.128671	45.029159
3502.003491	276871.744010	45.034164
3502.436640	276837.661058	45.039169
3502.054927	276824.379159	45.044173
3502.498022	276787.901312	45.049178
3502.486298	276776.547782	45.054183
3502.374887	276742.345843	45.059188
3502.444686	276706.180658	45.064193
3502.184316	276694.305668	45.069197
3502.341072	276660.953097	45.074202
3502.309038	276641.226050	45.079207
3502.312480	276617.037806	45.084212
3502.452548	276593.439359	45.089217
3502.322707	276568.100636	45.094221
3502.295885	276538.824879	45.099226
3502.127551	276514.357803	45.104231
3502.245906	276492.188521	45.109236
3502.181254	276455.458542	45.114241
3502.280729	276439.555597	45.119245
3502.158036	276413.044505	45.124250
3502.130694	276399.681930	45.129255
3502.229974	276366.669174	45.134260
3502.452267	276343.974456	45.139265
3502.110351	276318.464967	45.144269
3502.286861	276283.225046	45.149274
3502.216754	276266.151785	45.154279
3502.446513	276241.648139	45.159284
3502.505930	276213.122677	45.164289
3502.190766	276202.350969	45.169293
3502.513911	276155.554290	45.174298
3502.259394	276143.347313	45.179303
3502.152446	276103.721186	45.184308
3502.314490	276082.537978	45.189313
3502.097897	276066.225843	45.194317
3502.446562	276044.504361	45.199322
3502.495234	276018.221085	45.204327
3502.322143	275984.894101	45.209332
3502.196635	275949.140887	45.214337
3502.526433	275936.282805	45.219341
3502.182425	275904.459135	45.224346
3502.096682	275891.538404	45.229351
3501.669993	275864.972594	45.234356
3502.296212	275838.446618	45.239361
3502.339083	275824.640181	45.244365
3502.070915	275790.742305	45.249370
3502.323065	275773.949789	45.254375
3502.493760	275748.589503	45.259380
3502.538622	275712.427754	45.264385
3502.326836	275704.873473	45.269389
3502.324989	275665.892771	45.274394
3502.348411	275641.115518	45.279399
3502.345760	275620.365198	45.284404
3502.610948	275589.745133	45.289409
3502.379365	275561.417493	45.294413
3502.517184	275533.567048	45.299418
3502.779859	275507.097538	45.304423
3502.314722	275477.813222	45.309428
3502.587804	275453.277136	45.314433
3502.422074	275407.854632	45.319437
3502.231771	275389.705052	45.324442
3501.970235	275359.166865	45.329447
3502.244524	275346.215484	45.334452
3502.144600	275325.785764	45.339457
3501.949795	275295.644551	45.344461
3502.200870	275270.500762	45.349466
3502.174813	275251.943672	45.354471
3502.047336	275218.380126	45.359476
3502.209918	275203.994804	45.364481
3502.133548	275189.824894	45.369485
3502.335085	275169.271840	45.374490
3502.245868	275146.676187	45.379495
3502.131311	275125.764927	45.384500
3501.842940	275091.156985	45.389505
3502.190641	275062.611722	45.394509
3502.174078	275046.064565	45.399514
3502.233062	275030.651414	45.404519
3502.076000	275003.763291	45.409524
3502.223208	274979.883189	45.414529
3501.928666	274958.490664	45.419533
3502.253682	274939.446028	45.424538
3501.881787	274909.154001	45.429543
3501.869829	274894.770325	45.434548
3501.957666	274858.397821	45.439553
3502.154911	274856.050348	45.444557
3502.419102	274819.548538	45.449562
3502.425893	274798.287312	45.454567
3502.346791	274771.208750	45.459572
3502.405352	274736.521212	45.464577
3502.677038	274715.651590	45.469581
3502.550475	274684.633842	45.474586
3502.025758	274659.024974	45.479591
3502.069396	274629.686647	45.484596
3502.149733	274605.689536	45.489601
3502.109184	274588.993250	45.494605
3502.142081	274562.762887	45.499610
3501.858400	274551.145829	45.504615
3502.221148	274528.377830	45.509620
3502.268139	274505.455268	45.514625
3502.125463	274488.291083	45.519629
3502.189788	274465.696814	45.524634
3502.221381	274438.575457	45.529639
3501.858953	274414.723576	45.534644
3502.244174	274383.753384	45.539649
3502.060024	274370.796806	45.544653
3502.384004	274340.701825	45.549658
3502.066606	274328.275209	45.554663
3501.784099	274300.311526	45.559668
3502.088542	274274.293434	45.564673
3502.403740	274260.011509	45.569677
3502.077081	274231.112591	45.574682
3501.867694	274207.389606	45.579687
3501.900619	274176.728778	45.584692
3502.252089	274162.517577	45.589697
3501.779935	274146.397602	45.594701
3502.410518	274120.761560	45.599706
3501.968512	274095.088725	45.604711
3502.146007	274073.622519	45.609716
3502.381521	274049.855720	45.614721
3502.199972	274029.947619	45.619725
3501.981461	274003.476124	45.624730
3501.981789	273986.391431	45.629735
3502.019783	273960.465628	45.634740
3502.173777	273935.260159	45.639745
3502.007124	273917.055655	45.644749
3502.286430	273899.316448	45.649754
3502.071990	273878.700499	45.654759
3501.929280	273859.855711	45.659764
3501.938901	273821.559830	45.664769
3501.616168	273824.181917	45.669773
3502.142753	273785.194490	45.674778
3502.180692	273780.376515	45.679783
3501.865535	273758.223036	45.684788
3502.251232	273739.423304	45.689793
3501.901945	273723.411437	45.694797
3502.365484	273687.158195	45.699802
3502.391227	273677.860821	45.704807
3502.594083	273653.793450	45.709812
3502.557907	273619.603969	45.714817
3502.211919	273602.242085	45.719821
3502.066215	273562.264311	45.724826
3502.307659	273531.010638	45.729831
3502.206111	273451.712712	45.734836
3501.940372	273334.221827	45.739841
3501.543777	273182.733874	45.744845
3501.497132	272986.632549	45.749850
3500.720942	272743.080999	45.754855
3499.507445	272461.658078	45.759860
3498.867705	272130.697113	45.764865
3497.825094	271774.360615	45.769869
3496.540849	271372.889717	45.774874
3495.378256	270942.472483	45.779879
3493.982731	270474.022546	45.784884
3492.714582	269980.927711	45.789889
3491.117131	269460.585050	45.794893
3489.566498	268887.752461	45.799898
3487.848056	268290.141156	45.804903
3485.581303	267675.550858	45.809908
3483.647252	267036.841674	45.814913
3481.415341	266364.918850	45.819917
3479.484618	265663.660965	45.824922
3477.557035	264955.293247	45.829927
3474.857042	264211.085117	45.834932
3472.780491	263443.856585	45.839937
3469.831863	262652.974189	45.844941
3467.138486	261850.281582	45.849946
3464.864723	261023.682568	45.854951
3462.036572	260183.667271	45.859956
3459.444210	259324.382837	45.864961
3456.485155	258461.202194	45.869965
3453.587884	257575.137580	45.874970
3450.816729	256676.594297	45.879975
3447.820601	255765.397702	45.884980
3444.855334	254846.804924	45.889985
3441.472675	253907.719537	45.894989
3438.393286	252958.699760	45.899994
3435.279881	252004.356673	45.904999
3432.139623	251046.981310	45.910004
3428.823140	250070.476330	45.915009
3425.583039	249103.122014	45.920013
3422.542302	248106.214474	45.925018
3418.994261	247120.942722	45.930023
3415.637275	246120.992173	45.935028
3412.226192	245112.182208	45.940033
3408.855084	244113.624783	45.945037
3405.239613	243094.981063	45.950042
3401.962253	242083.207657	45.955047
3398.246761	241055.020304	45.960052
3394.951757	240036.823561	45.965057
3391.355478	239017.956932	45.970061
3387.646719	237987.236045	45.975066
3384.304111	236972.831329	45.980071
3380.535476	235937.121785	45.985076
3377.265255	234908.488714	45.990081
3373.207595	233874.067007	45.995085
3369.503747	232841.269037	46.000090
3365.988877	231813.609981	46.005095
3362.110959	230782.160009	46.010100
3358.790142	229756.607229	46.015105
3354.987723	228735.330728	46.020109
3351.093002	227708.235389	46.025114
3347.567690	226687.321956	46.030119
3343.479168	225662.624603	46.035124
3340.145752	224644.609984	46.040129
3336.473528	223626.852096	46.045133
3332.888255	222607.553048	46.050138
3328.959515	221590.880593	46.055143
3325.226297	220564.449585	46.060148
3321.859481	219547.488261	46.065153
3318.106229	218537.821788	46.070157
3314.280302	217518.948671	46.075162
3310.414160	216501.128098	46.080167
3306.492179	215496.384004	46.085172
3303.029416	214486.731909	46.090177
3299.235881	213485.869805	46.095181
3295.767782	212493.288250	46.100186
3291.829285	211482.878752	46.105191
3287.494954	210498.715860	46.110196
3284.491115	209506.199675	46.115201
3280.425493	208519.812159	46.120205
3276.817100	207543.748536	46.125210
3273.162637	206559.470161	46.130215
3269.248837	205581.043332	46.135220
3265.833967	204588.026984	46.140225
3261.757195	203604.669053	46.145229
3257.755547	202634.649580	46.150234
3254.205390	201676.713042	46.155239
3250.410586	200704.023556	46.160244
3246.618158	199742.468548	46.165249
3242.595313	198788.417040	46.170253
3238.725428	197827.446251	46.175258
3234.959641	196880.370257	46.180263
3231.009666	195931.368338	46.185268
3227.703934	194984.513738	46.190273
3223.669337	194048.678721	46.195277
3219.831095	193121.325494	46.200282
3216.162464	192198.256407	46.205287
3212.380467	191270.551774	46.210292
3208.939792	190340.916848	46.215297
3205.026109	189434.892643	46.220301
3201.317727	188517.664734	46.225306
3197.320662	187603.137713	46.230311
3193.207670	186695.257254	46.235316
3189.688329	185800.508157	46.240321
3186.017424	184901.537988	46.245325
3182.115789	184003.834044	46.250330
3178.232080	183115.862563	46.255335
3174.874271	182229.676271	46.260340
3171.065589	181350.927287	46.265345
3167.249008	180464.549098	46.270349
3163.469557	179588.791672	46.275354
3159.812035	178711.267033	46.280359
3155.724430	177852.965561	46.285364
3152.177219	176991.813298	46.290369
3148.152798	176127.128612	46.295373
3144.100333	175277.657676	46.300378
3140.592447	174429.129337	46.305383
3136.599793	173587.865365	46.310388
3132.901212	172744.616943	46.315393
3129.009040	171910.560759	46.320397
3125.157839	171087.289581	46.325402
3121.802714	170257.063471	46.330407
3117.771248	169434.844323	46.335412
3113.834134	168617.075119	46.340417
3110.062669	167813.966394	46.345421
3106.347459	166998.039775	46.350426
3102.637634	166210.787658	46.355431
3098.671995	165403.549119	46.360436
3095.121897	164602.747189	46.365441
3091.099174	163823.552425	46.370445
3087.170421	163039.069942	46.375450
3083.274086	162258.015766	46.380455
3079.387339	161491.123247	46.385460
3075.970264	160738.434942	46.390465
3072.057898	159976.808705	46.395469
3068.100218	159215.173405	46.400474
3064.371703	158463.312068	46.405479
3060.525511	157731.320285	46.410484
3056.921044	156977.841769	46.415489
3053.116726	156254.936051	46.420493
3048.939785	155519.701239	46.425498
3045.236038	154801.112259	46.430503
3040.869073	154080.510125	46.435508
3037.301192	153362.847090	46.440513
3033.590134	152676.789250	46.445517
3029.608628	151980.982839	46.450522
3025.618116	151287.642682	46.455527
3021.240405	150599.016450	46.460532
3017.922993	149924.919288	46.465537
3013.936835	149268.737525	46.470541
3009.909598	148597.121729	46.475546
3006.225652	147936.442820	46.480551
3002.298670	147292.428855	46.485556
2998.491936	146645.464722	46.490561
2994.287770	146019.400802	46.495565
2991.002105	145382.233094	46.500570
2987.452609	144752.710864	46.505575
2983.342462	144139.799731	46.510580
2979.895125	143510.442602	46.515585
2975.829333	142899.893773	46.520589
2971.715150	142303.394293	46.525594
2968.200951	141690.369900	46.530599
2963.908755	141102.043186	46.535604
2960.392884	140519.697278	46.540609
2956.479183	139950.436083	46.545613
2952.855776	139378.375655	46.550618
2949.199994	138808.375563	46.555623
2945.472622	138242.960962	46.560628
2941.715736	137669.529937	46.565633
2937.520125	137115.155980	46.570637
2933.908769	136566.804423	46.575642
2930.120100	136012.011535	46.580647
2926.369646	135479.520890	46.585652
2923.191673	134934.632823	46.590657
2919.578609	134402.438858	46.595661
2916.160890	133866.162713	46.600666
2912.134170	133329.275433	46.605671
2908.532779	132796.819047	46.610676
2905.039031	132269.046403	46.615681
2901.302486	131739.346209	46.620685
2897.524725	131208.475883	46.625690
2894.259057	130614.858685	46.630695
2890.214835	130095.542867	46.635700
2886.952959	129576.582279	46.640705
2883.682150	129074.725105	46.645709
2879.977152	128563.859508	46.650714
2876.210440	128037.873321	46.655719
2872.547343	127527.217386	46.660724
2868.958423	127016.619793	46.665729
2865.403425	126506.341220	46.670733
2861.806769	126002.752974	46.675738
2858.627358	125490.749695	46.680743
2854.786620	124983.676181	46.685748
2851.118400	124479.698233	46.690753
2847.644972	123979.600842	46.695757
2843.865455	123483.067571	46.700762
2840.928312	122973.742179	46.705767
2837.066599	122485.755291	46.710772
2833.714258	121982.052307	46.715777
2829.987365	121481.962290	46.720781
2826.021883	120983.925163	46.725786
2822.782465	120474.501197	46.730791
2819.018414	119988.094551	46.735796
2815.466208	119494.081776	46.740801
2812.070792	119011.864876	46.745805
2808.442799	118519.694988	46.750810
2805.089292	118027.145421	46.755815
2801.394006	117540.772003	46.760820
2798.149505	117047.557021	46.765825
2794.124690	116559.594503	46.770829
2790.743526	116066.172139	46.775834
2787.249905	115570.217993	46.780839
2783.779718	115097.269141	46.785844
2779.908084	114612.156719	46.790849
2776.548459	114133.684638	46.795853
2773.024425	113648.492772	46.800858
2769.717141	113159.726232	46.805863
2765.269590	112678.848813	46.810868
2762.221386	112197.861772	46.815873
2758.785168	111724.976999	46.820877
2754.831186	111250.360949	46.825882
2751.477711	110766.541886	46.830887
2747.695903	110302.655016	46.835892
2744.059404	109829.852113	46.840897
2740.223437	109361.243916	46.845901
2736.745195	108907.791409	46.850906
2732.929995	108440.641664	46.855911
2729.298329	107978.758232	46.860916
2725.700767	107524.630459	46.865921
2722.317775	107072.941535	46.870925
2718.152927	106631.893420	46.875930
2714.776816	106170.185236	46.880935
2711.227596	105729.714036	46.885940
2707.522224	105292.272881	46.890945
2703.763594	104849.926228	46.895949
2699.754673	104415.022498	46.900954
2696.438614	103986.346889	46.905959
2692.744709	103562.248089	46.910964
2689.207890	103130.872202	46.915969
2685.169725	102701.003574	46.920973
2681.349351	102279.279686	46.925978
2677.865283	101858.703664	46.930983
2673.991301	101464.301014	46.935988
2670.406977	101042.327506	46.940993
2666.966121	100641.143648	46.945997
2663.369334	100239.989011	46.951002
2659.685733	99830.477074	46.956007
2655.837645	99439.005544	46.961012
2652.004617	99041.956955	46.966017
2648.726413	98657.650694	46.971021
2645.039844	98271.163072	46.976026
2641.577134	97870.118845	46.981031
2637.863196	97482.869806	46.986036
2634.274126	97089.099195	46.991041
2630.831890	96710.205110	46.996045
2627.183758	96329.390528	47.001050
2623.891944	95943.492638	47.006055
2620.450599	95566.658255	47.011060
2616.743252	95177.454130	47.016065
2613.009427	94793.431077	47.021069
2609.379420	94412.726030	47.026074
2606.317666	94031.606843	47.031079
2603.016153	93665.791202	47.036084
2599.578762	93266.949654	47.041089
2596.442200	92895.500946	47.046093
2592.243282	92506.000424	47.051098
2588.983123	92117.172020	47.056103
2585.790876	91731.120756	47.061108
2582.181402	91346.041494	47.066113
2579.039967	90957.882929	47.071117
2575.499934	90577.008438	47.076122
2572.379701	90178.882370	47.081127
2568.613053	89785.499781	47.086132
2565.008508	89388.565004	47.091137
2561.642556	89002.309032	47.096141
2557.913622	88613.154257	47.101146
2554.489524	88203.209809	47.106151
2550.994426	87809.099674	47.111156
2547.444176	87424.392181	47.116161
2543.763763	87029.292264	47.121165
2540.714085	86632.130349	47.126170
2537.271176	86234.272784	47.131175
2533.540474	85839.107884	47.136180
2530.231608	85455.557561	47.141185
2526.347702	85061.405311	47.146189
2523.239093	84659.858686	47.151194
2519.859239	84253.176921	47.156199
2516.101170	83863.759845	47.161204
2512.687150	83462.086970	47.166209
2509.194510	83066.262572	47.171213
2505.547329	82673.147988	47.176218
2502.159200	82260.106515	47.181223
2498.781163	81868.790364	47.186228
2495.432612	81461.279901	47.191233
2491.821392	81054.209981	47.196237
2488.221063	80665.536357	47.201242
2484.714218	80262.411941	47.206247
2481.106162	79862.459040	47.211252
2477.823543	79460.365554	47.216257
2474.224582	79065.109456	47.221261
2470.718065	78658.337693	47.226266
2467.494521	78249.000473	47.231271
2463.731529	77850.497856	47.236276
2460.514082	77451.827231	47.241281
2456.933264	77033.965684	47.246285
2453.384706	76635.282308	47.251290
2449.996415	76223.473771	47.256295
2446.248892	75824.287181	47.261300
2442.787828	75412.032428	47.266305
2439.506019	75004.365852	47.271309
2435.783374	74601.078989	47.276314
2432.362413	74186.449385	47.281319
2428.490483	73791.287030	47.286324
2425.137812	73383.072023	47.291329
2421.890212	72966.758216	47.296333
2418.010791	72573.926172	47.301338
2414.676386	72155.645040	47.306343
2411.308044	71754.873036	47.311348
2407.904674	71346.811607	47.316353
2403.984797	70945.794945	47.321357
2400.426965	70533.605545	47.326362
2397.171349	70122.823051	47.331367
2393.774403	69725.025871	47.336372
2390.060466	69312.124654	47.341377
2386.938751	68897.563530	47.346381
2383.291810	68500.604873	47.351386
2379.993015	68084.503722	47.356391
2376.333150	67674.489540	47.361396
2373.261155	67261.864054	47.366401
2369.442728	66853.354015	47.371405
2365.681379	66443.952994	47.376410
2362.451078	66018.493245	47.381415
2358.524738	65615.656349	47.386420
2354.822616	65202.197560	47.391425
2351.349329	64797.570430	47.396429
2347.730477	64394.463996	47.401434
2344.492702	63977.582828	47.406439
2341.060018	63573.026240	47.411444
2337.823763	63157.675376	47.416449
2333.971157	62754.504826	47.421453
2330.738427	62344.517125	47.426458
2327.325645	61930.216988	47.431463
2323.685351	61520.414253	47.436468
2320.174890	61111.194660	47.441473
2316.545863	60691.300947	47.446477
2312.935315	60285.036208	47.451482
2309.735579	59872.387516	47.456487
2306.366666	59467.634444	47.461492
2302.761312	59042.657089	47.466497
2299.567616	58633.918290	47.471501
2295.747951	58213.322782	47.476506
2292.173160	57788.495928	47.481511
2288.917986	57384.762508	47.486516
2285.627297	56966.923676	47.491521
2282.125132	56542.469204	47.496525
2278.375734	56123.790110	47.501530
2274.772495	55699.956406	47.506535
2271.094593	55284.681691	47.511540
2267.776114	54868.228988	47.516545
2264.092195	54460.031064	47.521549
2260.423334	54043.596655	47.526554
2257.027060	53616.113743	47.531559
2253.639183	53204.135770	47.536564
2250.196519	52781.832969	47.541569
2246.604357	52372.534144	47.546573
2243.246578	51961.594724	47.551578
2239.554534	51542.734349	47.556583
2236.356203	51124.458073	47.561588
2232.670521	50704.438307	47.566593
2229.173890	50275.154657	47.571597
2225.580810	49862.373439	47.576602
2222.713268	49446.442073	47.581607
2218.667849	49021.218933	47.586612
2215.129359	48598.766367	47.591617
2211.727272	48181.875586	47.596621
2208.052461	47754.081314	47.601626
2204.825107	47333.151382	47.606631
2201.085145	46921.150217	47.611636
2197.467788	46491.874045	47.616641
2194.182982	46078.390430	47.621645
2190.391693	45660.769495	47.626650
2186.927976	45233.243802	47.631655
2183.606217	44812.299557	47.636660
2179.753375	44395.612320	47.641665
2176.619778	43979.366307	47.646669
2173.078944	43562.252940	47.651674
2169.321599	43143.627509	47.656679
2166.065461	42725.046135	47.661684
2162.348789	42307.057987	47.666689
2158.766380	41888.422789	47.671693
2155.160855	41470.946839	47.676698
2151.815015	41054.915791	47.681703
2148.140197	40636.337901	47.686708
2145.137092	40216.547591	47.691713
2141.663856	39796.629308	47.696717
2137.822985	39377.638616	47.701722
2134.377920	38962.480861	47.706727
2130.823104	38540.963873	47.711732
2127.151514	38111.504192	47.716737
2124.030621	37702.837512	47.721741
2120.172808	37285.392586	47.726746
2116.911363	36858.214402	47.731751
2113.132041	36445.718376	47.736756
2109.949450	36030.538401	47.741761
2106.244088	35605.964684	47.746765
2102.972642	35200.126794	47.751770
2099.421968	34769.732957	47.756775
2095.900488	34355.817509	47.761780
2092.108300	33926.416567	47.766785
2088.678711	33495.827043	47.771789
2085.030194	33091.324394	47.776794
2081.979384	32668.108697	47.781799
2078.189135	32259.701850	47.786804
2074.812422	31837.681867	47.791809
2071.323184	31407.962211	47.796813
2067.710964	30988.860781	47.801818
2064.328960	30567.361768	47.806823
2060.600651	30151.318357	47.811828
2056.846024	29737.657567	47.816833
2053.522632	29307.917716	47.821837
2050.045621	28888.394312	47.826842
2046.768413	28474.253746	47.831847
2043.097473	28055.347911	47.836852
2039.512059	27647.969994	47.841857
2036.087697	27220.951078	47.846861
2032.365392	26806.140618	47.851866
2028.971942	26377.493519	47.856871
2025.183866	25962.450791	47.861876
2021.545476	25550.491584	47.866881
2018.191991	25131.767813	47.871885
2014.695740	24718.979849	47.876890
2011.159558	24305.395641	47.881895
2007.936476	23892.031000	47.886900
2004.085337	23477.112810	47.891905
2000.550671	23067.830316	47.896909
1997.060415	22652.372667	47.901914
1993.195732	22239.782015	47.906919
1989.842863	21838.180825	47.911924
1986.411452	21419.198736	47.916929
1982.975944	21012.876205	47.921933
1978.890600	20609.640357	47.926938
1975.932321	20201.879410	47.931943
1972.286898	19801.486455	47.936948
1968.726250	19392.347586	47.941953
1965.107481	18991.891057	47.946957
1961.585535	18582.902486	47.951962
1957.876284	18181.304972	47.956967
1954.273356	17779.965226	47.961972
1950.625835	17374.156732	47.966977
1947.342467	16973.097483	47.971981
1943.780245	16584.518626	47.976986
1940.346935	16183.125495	47.981991
1936.470499	15784.130686	47.986996
1932.831087	15378.400980	47.992001
1929.615468	14993.533490	47.997005
1925.769418	14601.920185	48.002010
1922.415935	14203.877475	48.007015
1918.460480	13817.762083	48.012020
1914.852420	13427.275696	48.017025
1911.659477	13041.934400	48.022029
1907.818753	12662.948061	48.027034
1903.951366	12284.476842	48.032039
1899.911668	11925.208734	48.037044
1895.862498	11557.268601	48.042049
1892.265653	11192.934256	48.047053
1888.266929	10840.746227	48.052058
1884.185009	10497.979377	48.057063
1880.219526	10160.366736	48.062068
1876.354761	9832.424356	48.067073
1872.432590	9505.724843	48.072077
1868.971927	9184.118682	48.077082
1865.626215	8862.762916	48.082087
1861.986666	8544.142532	48.087092
1858.157414	8231.814635	48.092097
1854.539948	7919.645796	48.097101
1850.951791	7622.771115	48.102106
1847.074699	7314.542754	48.107111
1843.704207	7023.524394	48.112116
1839.609811	6720.558785	48.117121
1836.881997	6418.116563	48.122125
1833.090677	6126.794976	48.127130
1829.601196	5830.351664	48.132135
1826.038803	5534.051096	48.137140
1822.312217	5250.363441	48.142145
1818.797214	4958.913050	48.147149
1815.209307	4676.276054	48.152154
1811.957790	4383.135669	48.157159
1808.425426	4101.173011	48.162164
1804.720294	3812.982493	48.167169
1801.089139	3527.534848	48.172173
1797.555701	3250.708651	48.177178
1793.822126	2962.536119	48.182183
1789.888721	2688.891230	48.187188
1786.424411	2429.960318	48.192193
1783.418658	2148.632811	48.197197
1779.311907	1897.140751	48.202202
1775.708226	1624.913044	48.207207
1771.803640	1377.203103	48.212212
1768.166327	1121.750889	48.217217
1763.992313	887.843158	48.222221
1758.961217	676.883051	48.227226
1754.140616	470.290351	48.232231
1748.997976	295.504775	48.237236
1743.894456	142.933694	48.242241
1739.057084	0.949386	48.247245
1729.292475	32.059523	48.252250
1720.810748	59.844294	48.257255
1716.720865	74.217918	48.262260
1713.737035	73.363274	48.267265
1712.320260	68.522056	48.272269
1710.220487	72.208952	48.277274
1707.705509	74.951246	48.282279
1705.171087	63.295333	48.287284
1701.911445	64.043329	48.292289
1699.171562	60.993066	48.297293
1695.453346	58.386133	48.302298
1691.305664	61.392034	48.307303
1687.809990	57.168609	48.312308
1684.463679	63.960134	48.317313
1681.502203	53.987357	48.322317
1678.139385	59.297668	48.327322
1674.802866	55.046311	48.332327
1671.375622	61.065830	48.337332
1668.136453	69.159950	48.342337
1664.697538	63.611587	48.347341
1661.125721	70.324319	48.352346
1657.288886	67.365697	48.357351
1654.220856	63.999520	48.362356
1650.735765	68.003270	48.367361
1647.832355	63.368132	48.372365
1644.368207	65.150860	48.377370
1640.589072	57.083357	48.382375
1637.133696	61.933520	48.387380
1633.494812	71.466068	48.392385
1630.008454	70.876305	48.397389
1626.321011	71.554851	48.402394
1623.108749	68.381966	48.407399
1620.051053	62.236445	48.412404
1615.977516	65.964793	48.417409
1612.756719	54.596063	48.422413
1609.343920	68.826333	48.427418
1606.166771	61.826221	48.432423
1602.896727	52.148255	48.437428
1598.961680	60.008999	48.442433
1595.909117	58.162168	48.447437
1592.202458	67.240198	48.452442
1588.874534	57.583894	48.457447
1585.151461	58.989316	48.462452
1581.648630	62.151119	48.467457
1578.404095	63.320711	48.472461
1574.893306	64.848115	48.477466
1571.258306	63.098265	48.482471
1567.915668	61.419969	48.487476
1564.128448	62.262746	48.492481
1560.845301	62.745496	48.497485
1557.519268	57.654138	48.502490
1554.013240	59.883146	48.507495
1550.684100	51.252083	48.512500
1546.719425	54.855925	48.517505
1543.379369	54.850832	48.522509
1540.042055	58.568998	48.527514
1536.373354	52.173748	48.532519
1532.835714	56.786786	48.537524
1529.493285	53.298821	48.542529
1526.337410	45.134336	48.547533
1523.070749	54.542505	48.552538
1519.521153	53.177997	48.557543
1515.775922	46.294798	48.562548
1511.782225	52.915009	48.567553
1508.578793	50.699369	48.572557
1504.757334	61.038603	48.577562
1501.971509	59.615329	48.582567
1498.465904	46.364257	48.587572
1494.588463	53.349182	48.592577
1490.990946	53.463259	48.597581
1487.292179	63.403754	48.602586
1484.151445	53.939794	48.607591
1481.071038	56.918797	48.612596
1477.349433	56.992080	48.617601
1474.291194	54.390018	48.622605
1470.138994	57.263765	48.627610
1466.620501	48.314182	48.632615
1463.104154	50.351817	48.637620
1459.444162	57.786946	48.642625
1456.504763	53.673120	48.647629
1452.760783	59.507833	48.652634
1449.240203	60.941861	48.657639
1445.654818	53.056205	48.662644
1442.076774	52.702193	48.667649
1439.181598	52.017270	48.672653
1435.504653	59.534132	48.677658
1431.858031	64.572259	48.682663
1428.465318	53.084793	48.687668
1424.745566	59.529495	48.692673
1421.374630	49.759699	48.697677
1417.591888	54.667153	48.702682
1414.520693	52.848550	48.707687
1411.302593	42.631035	48.712692
1407.297400	51.053186	48.717697
1403.902538	50.281530	48.722701
1399.742259	60.379278	48.727706
1396.531000	49.486827	48.732711
1393.515596	50.592296	48.737716
1390.123502	60.750809	48.742721
1386.464678	53.648538	48.747725
1383.135117	53.720920	48.752730
1379.323028	52.868676	48.757735
1376.044314	56.264525	48.762740
1372.534054	48.702543	48.767745
1368.771968	45.653237	48.772749
1365.276543	64.521690	48.777754
1361.867376	62.534237	48.782759
1358.707900	48.818037	48.787764
1354.894272	51.060138	48.792769
1351.493459	46.556245	48.797773
1347.734024	58.439204	48.802778
1344.403179	67.496709	48.807783
1341.175529	48.210350	48.812788
1337.334881	62.697024	48.817793
1333.546195	63.451469	48.822797
1330.406540	62.459765	48.827802
1326.892730	57.457776	48.832807
1323.991960	55.966990	48.837812
1320.126232	53.272337	48.842817
1316.479134	55.017130	48.847821
1312.855631	52.553690	48.852826
1309.288770	51.644302	48.857831
1305.618641	55.240282	48.862836
1302.268058	56.622553	48.867841
1299.134302	43.898932	48.872845
1295.212954	56.398704	48.877850
1291.627899	53.521165	48.882855
1288.608968	50.394159	48.887860
1284.918320	50.301295	48.892865
1281.362710	41.256289	48.897869
1277.995716	54.590410	48.902874
1274.505273	61.303144	48.907879
1271.172330	48.303650	48.912884
1267.106936	55.200786	48.917889
1264.174079	46.824462	48.922893
1260.500952	44.571231	48.927898
1257.015466	51.039586	48.932903
1253.601805	53.323842	48.937908
1249.825925	53.981391	48.942913
1246.428701	56.082759	48.947917
1243.112159	57.478718	48.952922
1239.433734	57.039113	48.957927
1235.838938	51.312604	48.962932
1232.341290	47.870985	48.967937
1229.083454	47.403880	48.972941
1225.334877	55.782934	48.977946
1221.638758	53.710453	48.982951
1218.483085	46.558370	48.987956
1214.641780	55.581435	48.992961
1211.410156	47.805271	48.997965
1208.040290	53.113537	49.002970
1204.247347	48.866850	49.007975
1201.163835	47.619654	49.012980
1197.149732	55.885019	49.017985
1193.884973	46.560640	49.022989
1190.611164	50.246797	49.027994
1186.915911	57.184399	49.032999
1183.320740	53.577634	49.038004
1180.090721	56.105390	49.043009
1176.481199	50.719698	49.048013
1172.973937	57.672331	49.053018
1169.661627	54.227180	49.058023
1166.541121	56.174752	49.063028
1162.456601	48.275095	49.068033
1158.842188	50.685518	49.073037
1155.392372	56.670610	49.078042
1151.536695	53.060107	49.083047
1148.447717	57.808973	49.088052
1144.775250	53.967477	49.093057
1141.250574	45.771878	49.098061
1137.629776	47.411355	49.103066
1133.684604	57.791999	49.108071
1130.747414	52.304825	49.113076
1127.534829	65.270074	49.118081
1124.090095	53.904659	49.123085
1120.849216	53.599438	49.128090
1116.933839	53.462482	49.133095
1113.366721	53.676270	49.138100
1109.561729	58.799178	49.143105
1105.966773	52.234335	49.148109
1102.857487	55.268477	49.153114
1099.537356	55.848775	49.158119
1095.997589	49.525276	49.163124
1092.474633	56.404426	49.168129
1088.986130	59.358396	49.173133
1085.463543	54.924113	49.178138
1081.961830	55.994576	49.183143
1078.745516	56.299293	49.188148
1074.767992	60.098162	49.193153
1071.029755	54.188366	49.198157
1067.568602	62.399307	49.203162
1064.194468	52.772441	49.208167
1061.142829	43.797721	49.213172
1057.271657	58.665621	49.218177
1053.595339	52.334910	49.223181
1050.415160	58.202108	49.228186
1046.430895	52.355923	49.233191
1043.195396	46.298278	49.238196
1039.869386	49.299722	49.243201
1036.733571	48.133449	49.248205
1032.914747	49.133059	49.253210
1029.367132	57.746592	49.258215
1025.803478	42.359679	49.263220
1021.982588	54.375590	49.268225
1019.004641	54.447059	49.273229
1015.955970	51.669559	49.278234
1011.597794	54.489994	49.283239
1008.287082	47.355751	49.288244
1004.486665	51.921144	49.293249
1001.137367	49.570085	49.298253
997.402233	60.851330	49.303258
993.649754	53.358754	49.308263
990.841482	49.433380	49.313268
987.401450	53.942677	49.318273
984.214495	54.208032	49.323277
980.653805	52.598548	49.328282
976.740325	58.693789	49.333287
973.108326	51.286866	49.338292
969.765614	58.384735	49.343297
966.427730	50.748536	49.348301
962.900982	53.607231	49.353306
958.847301	63.761171	49.358311
955.528017	54.280808	49.363316
952.101216	62.885031	49.368321
948.815129	52.912294	49.373325
945.474569	50.439661	49.378330
941.871031	49.865052	49.383335
938.531474	57.278800	49.388340
934.679129	64.117489	49.393345
931.132437	56.089863	49.398349
927.646468	46.429816	49.403354
924.009969	61.413045	49.408359
921.040188	50.989288	49.413364
917.260050	54.488533	49.418369
913.821836	54.777189	49.423373
910.069139	50.318644	49.428378
906.737595	54.830042	49.433383
903.503265	45.611710	49.438388
899.787900	56.728530	49.443393
896.212826	54.390483	49.448397
892.951930	55.432971	49.453402
889.150322	57.103784	49.458407
885.695187	54.585720	49.463412
882.319467	46.281562	49.468417
878.650967	49.099057	49.473421
875.025099	45.835633	49.478426
871.542369	46.279917	49.483431
868.020430	46.641722	49.488436
864.377660	48.613671	49.493441
861.503122	39.915135	49.498445
857.953822	43.074736	49.503450
854.188976	52.421264	49.508455
850.971114	50.359807	49.513460
846.670847	47.533555	49.518465
843.532667	47.879916	49.523469
840.378508	45.292862	49.528474
836.692943	47.451807	49.533479
833.402214	51.735397	49.538484
829.384397	53.541112	49.543489
825.938526	47.886400	49.548493
822.473421	49.719969	49.553498
818.896130	47.584755	49.558503
815.404706	41.402476	49.563508
812.117967	48.751059	49.568513
808.867006	42.515529	49.573517
805.241764	36.569215	49.578522
801.791022	43.623794	49.583527
798.516530	37.278039	49.588532
794.421832	42.205627	49.593537
791.066578	38.280009	49.598541
787.625108	47.993806	49.603546
783.851296	58.407899	49.608551
781.050188	43.272496	49.613556
777.226592	42.529688	49.618561
773.520895	43.173204	49.623565
770.321827	49.653947	49.628570
766.500209	41.466681	49.633575
763.123293	39.034535	49.638580
759.220736	34.978991	49.643585
755.446615	38.850627	49.648589
752.616675	30.347648	49.653594
748.883687	33.792111	49.658599
745.641812	39.447466	49.663604
742.306269	42.592785	49.668609
738.746231	35.076637	49.673613
735.365698	36.042854	49.678618
731.667588	45.470744	49.683623
728.156908	35.871537	49.688628
724.476327	42.012794	49.693633
720.723910	52.100860	49.698637
717.105608	41.863523	49.703642
714.133852	51.295401	49.708647
710.486587	41.809204	49.713652
706.700744	48.473040	49.718657
703.818346	46.096794	49.723661
700.306515	48.820317	49.728666
696.736303	53.185391	49.733671
693.199808	41.169988	49.738676
689.290329	54.484154	49.743681
686.059824	53.525648	49.748685
682.693323	35.071002	49.753690
678.915699	44.881422	49.758695
675.443615	39.309913	49.763700
672.044620	52.101694	49.768705
668.235964	47.984089	49.773709
664.954292	46.024336	49.778714
661.635298	49.334762	49.783719
658.363130	46.702830	49.788724
654.579109	53.806141	49.793729
651.216123	47.053413	49.798733
647.171654	46.724650	49.803738
643.808304	53.889021	49.808743
640.682394	51.000210	49.813748
637.229775	57.419196	49.818753
633.025340	57.422214	49.823757
629.946722	47.002804	49.828762
626.193528	48.732549	49.833767
622.880667	39.741631	49.838772
619.497994	44.501448	49.843777
616.039576	45.546241	49.848781
612.574665	42.434968	49.853786
608.747074	48.640250	49.858791
605.771638	52.181930	49.863796
602.145597	49.418437	49.868801
598.757287	45.431557	49.873805
594.896799	38.139374	49.878810
591.176618	45.017617	49.883815
587.903240	39.301297	49.888820
584.499649	40.467269	49.893825
581.018604	40.933471	49.898829
577.353201	40.131266	49.903834
573.432084	35.857186	49.908839
570.591283	36.005426	49.913844
566.771847	41.709579	49.918849
563.260232	45.261966	49.923853
560.343182	39.898293	49.928858
556.089057	45.407533	49.933863
553.034270	39.255402	49.938868
549.502712	39.175829	49.943873
546.162783	45.415927	49.948877
542.772928	42.071523	49.953882
538.921259	47.730079	49.958887
535.373543	33.448109	49.963892
531.411688	41.544030	49.968897
528.227374	36.867360	49.973901
525.250857	38.457224	49.978906
521.615644	44.831875	49.983911
517.705523	41.416613	49.988916
514.159450	47.875463	49.993921
510.529102	48.368081	49.998925
506.977725	36.364534	50.003930
503.276893	41.822444	50.008935
500.161709	36.888250	50.013940
496.958765	46.738927	50.018945
493.505293	55.853510	50.023949
489.775730	52.862547	50.028954
485.878479	49.941982	50.033959
482.769068	38.739646	50.038964
479.735314	45.760967	50.043969
475.796031	53.565490	50.048973
472.412671	49.929026	50.053978
468.670544	57.323216	50.058983
465.441677	48.015536	50.063988
462.114895	54.003665	50.068993
458.211508	51.485848	50.073997
454.817926	47.325809	50.079002
451.235151	50.066730	50.084007
447.937131	58.919840	50.089012
444.384392	56.148124	50.094017
440.565569	49.852368	50.099021
437.338141	55.806050	50.104026
433.739849	51.405806	50.109031
430.301106	44.851572	50.114036
426.578895	62.246212	50.119041
423.079673	49.741022	50.124045
419.893958	45.668848	50.129050
416.268036	50.599428	50.134055
412.522990	44.355467	50.139060
408.877996	48.472788	50.144065
405.918311	48.348495	50.149069
402.694428	38.837582	50.154074
398.644910	49.446468	50.159079
395.198928	49.084680	50.164084
391.794933	45.027510	50.169089
388.258331	46.862767	50.174093
384.987315	52.456252	50.179098
381.489877	55.063677	50.184103
377.899962	46.672745	50.189108
374.041640	52.079260	50.194113
370.397785	48.413768	50.199117
367.233201	44.679989	50.204122
363.278787	45.327480	50.209127
359.937013	55.357964	50.214132
356.585576	54.665095	50.219137
353.342838	48.678293	50.224141
350.149800	42.066841	50.229146
346.404942	43.504265	50.234151
342.526977	42.007541	50.239156
339.075530	47.170386	50.244161
335.389986	50.164596	50.249165
332.127670	51.704064	50.254170
328.662260	52.835401	50.259175
325.113234	49.420901	50.264180
321.765685	45.987690	50.269185
318.348909	44.555208	50.274189
314.694067	42.046178	50.279194
310.903148	56.797189	50.284199
307.786380	48.474974	50.289204
304.311278	52.597494	50.294209
300.409393	45.425708	50.299213
296.960200	49.677068	50.304218
293.360967	61.645845	50.309223
290.259840	43.260718	50.314228
286.755815	44.239887	50.319233
283.285009	44.805772	50.324237
279.885839	45.218139	50.329242
275.978581	51.034070	50.334247
272.328671	50.969796	50.339252
268.962978	48.972562	50.344257
265.352918	46.557805	50.349261
262.121218	45.558413	50.354266
258.553166	52.830608	50.359271
255.268972	43.338604	50.364276
251.815987	46.388364	50.369281
248.113180	49.208107	50.374285
244.570688	44.185459	50.379290
241.309827	41.456920	50.384295
237.619374	41.920969	50.389300
233.829843	45.602079	50.394305
230.242478	38.678729	50.399309
227.128327	43.131027	50.404314
223.955035	45.824042	50.409319
220.404899	48.762384	50.414324
216.921697	41.968347	50.419329
212.868410	47.345123	50.424333
209.820394	38.474405	50.429338
205.820352	43.137392	50.434343
202.322224	50.341758	50.439348
198.795863	49.983021	50.444353
195.256816	45.412251	50.449357
192.109836	38.682930	50.454362
188.545382	53.734032	50.459367
184.882649	47.629158	50.464372
181.604658	45.371517	50.469377
177.723112	56.542713	50.474381
174.466216	47.201495	50.479386
171.210900	51.163263	50.484391
167.633495	51.533794	50.489396
164.002245	46.939421	50.494401
160.271051	52.958900	50.499405
156.856309	42.629889	50.504410
153.427370	44.454741	50.509415
150.206265	49.983528	50.514420
146.693522	52.204232	50.519425
143.120871	57.718153	50.524429
139.415326	43.780382	50.529434
135.447510	58.685487	50.534439
132.673013	47.453226	50.539444
129.048280	47.881750	50.544449
125.419168	52.895112	50.549453
122.410733	50.598675	50.554458
118.217213	49.337775	50.559463
115.025736	44.516759	50.564468
111.815561	40.612956	50.569473
107.791436	52.176501	50.574477
104.429858	48.777147	50.579482
100.383127	51.628310	50.584487
97.540703	38.660292	50.589492
94.342439	36.886949	50.594497
90.456319	40.801407	50.599501
87.093366	40.309681	50.604506
83.117093	45.807355	50.609511
79.539431	50.711474	50.614516
76.718478	50.477038	50.619521
72.980097	50.037438	50.624525
69.655626	46.315946	50.629530
65.937824	46.290748	50.634535
62.498416	38.619917	50.639540
58.935721	41.867109	50.644545
54.749298	51.459654	50.649549
51.917644	41.922547	50.654554
48.043889	50.726114	50.659559
44.899516	46.014831	50.664564
41.979266	48.320466	50.669569
37.730420	49.678219	50.674573
34.502777	48.788957	50.679578
30.478226	46.688704	50.684583
27.049050	43.872512	50.689588
23.967394	39.141979	50.694593
20.229904	45.573728	50.699597
16.928240	39.083654	50.704602
13.441990	45.498432	50.709607
9.964126	44.081836	50.714612
6.287483	45.480214	50.719617
2.774789	45.154180	50.724621