Fri Aug 26 10:46:53 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.087804	96.717285	0.000000
0.833302	104.463845	0.005005
0.412046	86.041186	0.010010
0.770047	88.545089	0.015014
0.452429	94.251415	0.020019
0.428476	87.595858	0.025024
0.462732	78.827402	0.030029
-0.034480	72.875105	0.035034
0.106393	68.740642	0.040038
-0.521782	64.308315	0.045043
-0.725517	44.864769	0.050048
-1.273700	46.323383	0.055053
-1.285208	35.189329	0.060058
-1.497204	32.486007	0.065062
-1.752933	23.569745	0.070067
-1.933189	20.984865	0.075072
-2.452063	27.861422	0.080077
-2.522998	8.599713	0.085082
-2.818064	-2.853989	0.090086
-3.306505	8.260279	0.095091
-3.385397	-6.042729	0.100096
-4.230044	-5.714839	0.105101
-4.173036	0.600660	0.110106
-4.385053	0.523178	0.115110
-4.845465	-8.316908	0.120115
-5.077167	-8.555836	0.125120
-5.807130	-14.348482	0.130125
-5.670046	-12.847875	0.135130
-5.533336	-14.036312	0.140134
-6.218335	0.895443	0.145139
-5.901045	-4.152292	0.150144
-6.398183	-11.939490	0.155149
-6.922167	-8.570639	0.160154
-7.200308	-6.809236	0.165158
-7.335205	-13.517082	0.170163
-7.404021	-18.533171	0.175168
-7.706380	0.942118	0.180173
-7.736076	-16.785285	0.185178
-8.321462	-15.649903	0.190182
-8.683405	-4.194682	0.195187
-8.687197	-11.637927	0.200192
-8.899559	-12.303794	0.205197
-9.010739	-11.441554	0.210202
-9.626420	-10.940512	0.215206
-10.305313	-6.902157	0.220211
-9.900361	-5.740639	0.225216
-10.641202	-0.914381	0.230221
-10.402260	-7.408360	0.235226
-10.781221	-1.442585	0.240230
-10.881410	-10.743703	0.245235
-11.550031	-14.565454	0.250240
-11.713259	-9.509602	0.255245
-11.852066	-12.901333	0.260250
-11.709148	-9.971665	0.265254
-12.081259	-8.031121	0.270259
-12.501280	-10.388846	0.275264
-12.844604	-5.649790	0.280269
-13.242133	0.508696	0.285274
-13.245823	-0.047297	0.290278
-13.682165	0.163239	0.295283
-13.202087	-9.291498	0.300288
-14.441923	-15.571050	0.305293
-14.562363	-3.273937	0.310298
-14.631531	-18.537034	0.315302
-14.923091	-8.177907	0.320307
-14.823773	-10.005907	0.325312
-14.764011	-3.833203	0.330317
-15.182076	-7.083383	0.335322
-15.435039	-13.329934	0.340326
-15.999397	-7.582060	0.345331
-16.144313	-7.774390	0.350336
-17.334993	-12.644282	0.355341
-17.040326	-18.457258	0.360346
-17.579761	-12.918903	0.365350
-17.388067	-4.425641	0.370355
-17.434979	-7.053423	0.375360
-17.486697	-15.536371	0.380365
-17.466394	-14.020746	0.385370
-18.197780	-10.214656	0.390374
-18.890545	-4.155733	0.395379
-18.731990	-6.084702	0.400384
-19.043970	-6.219385	0.405389
-18.850932	-8.150559	0.410394
-19.234731	-14.389394	0.415398
-19.834238	-3.846281	0.420403
-19.921431	-9.267621	0.425408
-20.127594	-3.401516	0.430413
-20.427417	-5.932974	0.435418
-21.020748	-5.587267	0.440422
-21.567145	1.651056	0.445427
-21.824789	-14.550775	0.450432
-22.080399	-4.744555	0.455437
-21.754680	-4.788706	0.460442
-21.616598	-5.306663	0.465446
-21.925387	-5.369078	0.470451
-22.291210	-8.662191	0.475456
-22.997611	0.853563	0.480461
-23.178316	-2.727793	0.485466
-23.551063	-3.770472	0.490470
-23.673800	-6.630049	0.495475
-23.519127	-11.975156	0.500480
-24.431352	-5.002569	0.505485
-24.580616	-12.382034	0.510490
-24.619065	-9.803766	0.515494
-25.013035	-1.908992	0.520499
-24.908957	-7.034257	0.525504
-25.020021	-8.105025	0.530509
-25.417325	-9.007844	0.535514
-25.746805	-0.544163	0.540518
-26.282984	4.974708	0.545523
-26.683169	-7.990664	0.550528
-26.660407	-9.031650	0.555533
-26.703025	-5.203090	0.560538
-26.444401	-4.268718	0.565542
-27.192480	6.136186	0.570547
-27.857914	-7.385818	0.575552
-27.986570	4.390576	0.580557
-28.020364	-6.635579	0.585562
-28.053883	-4.678152	0.590566
-29.175111	6.370126	0.595571
-29.087497	-4.288968	0.600576
-29.559051	2.184754	0.605581
-29.807387	-4.255503	0.610586
-29.616675	-6.711482	0.615590
-29.711008	3.015850	0.620595
-29.634483	-2.864403	0.625600
-29.879172	-1.775738	0.630605
-30.437040	-5.703317	0.635610
-30.792420	1.299627	0.640614
-31.313188	-1.418886	0.645619
-30.923453	3.022544	0.650624
-31.741367	1.036807	0.655629
-32.263142	3.130364	0.660634
-32.222609	-1.232060	0.665638
-32.576560	-0.088419	0.670643
-32.707658	-4.689866	0.675648
-32.819268	-7.237974	0.680653
-32.557677	-9.673351	0.685658
-33.299305	-12.123365	0.690662
-34.081545	-9.176198	0.695667
-33.969032	-6.048813	0.700672
-34.284970	-5.951932	0.705677
-34.431471	0.490160	0.710682
-33.998061	-7.887996	0.715686
-34.475926	-6.813644	0.720691
-35.439499	-7.890879	0.725696
-35.625018	-8.478670	0.730701
-35.607322	-14.213723	0.735706
-35.505577	-15.115151	0.740710
-35.947990	-0.942482	0.745715
-36.526550	-13.933858	0.750720
-36.728683	-12.655674	0.755725
-36.708131	-11.643107	0.760730
-36.802691	-10.476581	0.765734
-37.331454	-2.972096	0.770739
-37.254269	-11.468787	0.775744
-38.141479	-6.062938	0.780749
-38.403903	-15.667811	0.785754
-38.474630	-14.906779	0.790758
-38.723817	-11.030240	0.795763
-38.418591	-10.099960	0.800768
-38.735377	-10.009274	0.805773
-39.112410	-15.309557	0.810778
-39.598261	-8.979142	0.815782
-39.876893	-8.290140	0.820787
-40.238346	-15.529001	0.825792
-40.630845	-12.016114	0.830797
-41.017224	-13.009215	0.835802
-41.126574	-18.132883	0.840806
-41.565713	-7.690671	0.845811
-41.313819	-9.444353	0.850816
-41.277709	-6.896675	0.855821
-41.768839	-3.102683	0.860826
-41.762396	-8.456346	0.865830
-42.344382	1.764512	0.870835
-42.274436	-3.640168	0.875840
-42.788926	4.991521	0.880845
-43.015882	-6.153249	0.885850
-43.483971	-11.268518	0.890854
-44.390458	2.457569	0.895859
-44.097721	-3.228564	0.900864
-44.247001	-7.109030	0.905869
-44.310781	-4.770418	0.910874
-44.059881	1.255470	0.915878
-44.538291	-1.042545	0.920883
-44.933201	-2.357011	0.925888
-45.729023	9.374570	0.930893
-45.845614	-0.594690	0.935898
-45.853669	1.349281	0.940902
-46.164934	-2.275019	0.945907
-45.996791	-5.594324	0.950912
-46.986517	-6.879450	0.955917
-47.229824	5.882871	0.960922
-47.302373	-1.736325	0.965926
-47.504381	1.677305	0.970931
-47.408090	-9.378591	0.975936
-47.917263	-4.911096	0.980941
-47.889926	-11.884637	0.985946
-47.974301	-13.677708	0.990950
-48.208289	-6.665195	0.995955
-48.541043	-4.680161	1.000960
-49.521265	-6.903207	1.005965
-50.124609	-0.102094	1.010970
-50.110829	-4.665988	1.015974
-49.876557	0.017938	1.020979
-50.157927	-2.595485	1.025984
-50.460644	-6.546970	1.030989
-50.432098	-5.200301	1.035994
-50.207675	-12.394347	1.040998
-51.466034	-10.372761	1.046003
-51.212728	-11.323096	1.051008
-51.537097	-13.211674	1.056013
-51.830630	-11.900277	1.061018
-51.774099	-14.540999	1.066022
-52.816980	1.186767	1.071027
-52.882464	-17.335459	1.076032
-53.615203	-14.424473	1.081037
-53.488165	-2.349386	1.086042
-53.560800	-6.567642	1.091046
-53.758892	4.922178	1.096051
-53.854574	-5.828592	1.101056
-53.800973	1.256201	1.106061
-53.868818	0.561506	1.111066
-54.278882	-4.559635	1.116070
-54.813793	-5.501138	1.121075
-54.830702	-5.178741	1.126080
-55.274435	-8.042120	1.131085
-55.795001	-13.180854	1.136090
-55.831947	-15.958877	1.141094
-56.209975	-9.104266	1.146099
-56.131207	-14.336315	1.151104
-56.446539	-8.291869	1.156109
-57.301995	-9.942738	1.161114
-57.567405	-7.724589	1.166118
-58.000288	-4.566068	1.171123
-57.799809	-13.939303	1.176128
-57.767566	-14.187689	1.181133
-57.854151	-7.900457	1.186138
-57.990130	-10.008186	1.191142
-58.768649	-5.498755	1.196147
-59.298214	-7.871059	1.201152
-59.520301	-4.871905	1.206157
-59.473059	-10.418576	1.211162
-59.351454	-13.474377	1.216166
-59.857676	-10.336075	1.221171
-60.021307	-15.131763	1.226176
-60.372148	-2.064814	1.231181
-60.991547	-7.118560	1.236186
-60.676723	-6.765560	1.241190
-60.865964	-7.166116	1.246195
-61.302612	-11.928787	1.251200
-61.881654	-3.612908	1.256205
-62.442472	-7.470425	1.261210
-62.223491	-8.962727	1.266214
-62.519123	-2.775818	1.271219
-62.228888	-17.044537	1.276224
-62.395191	-9.188380	1.281229
-63.367020	-7.654317	1.286234
-63.249978	-9.965950	1.291238
-63.722722	-6.747442	1.296243
-63.964197	-12.429487	1.301248
-63.795162	-10.690254	1.306253
-64.503199	0.891615	1.311258
-64.731538	-1.635154	1.316262
-65.243075	-4.377249	1.321267
-64.933151	-12.495737	1.326272
-65.084536	-16.859911	1.331277
-66.135816	-8.249051	1.336282
-66.399040	-9.947839	1.341286
-66.427188	-4.758001	1.346291
-66.627327	-7.406215	1.351296
-66.596163	-17.743307	1.356301
-66.837274	-9.540155	1.361306
-66.522757	-5.586875	1.366310
-67.281934	-8.334702	1.371315
-67.269190	-11.471627	1.376320
-67.498727	-14.602465	1.381325
-68.019731	-17.295628	1.386330
-68.490477	-13.539612	1.391334
-69.006078	-5.341176	1.396339
-69.216523	-17.440766	1.401344
-69.020597	-13.434222	1.406349
-69.292707	-0.790805	1.411354
-69.432727	-15.634755	1.416358
-70.200097	-11.639572	1.421363
-70.930700	-19.314482	1.426368
-71.106426	-10.640638	1.431373
-70.893272	-7.585870	1.436378
-70.967789	-18.336763	1.441382
-71.148294	-8.051877	1.446387
-70.906552	-21.579074	1.451392
-70.941032	-17.470220	1.456397
-71.858148	-16.596388	1.461402
-71.821526	-15.728688	1.466406
-72.535320	-12.548577	1.471411
-72.449900	-17.351404	1.476416
-73.202835	-17.502847	1.481421
-74.034221	-7.224183	1.486426
-74.011630	-17.813031	1.491430
-74.067285	-12.160183	1.496435
-74.261182	-16.966976	1.501440
-74.196558	-4.448756	1.506445
-73.944917	-11.365473	1.511450
-74.006506	-6.730395	1.516454
-74.825438	-13.622788	1.521459
-75.176667	-18.841666	1.526464
-75.221015	-19.049654	1.531469
-75.632974	-10.196664	1.536474
-75.665794	-15.847921	1.541478
-76.384643	-8.544789	1.546483
-76.422434	-15.207640	1.551488
-77.112954	-17.308117	1.556493
-77.043722	-6.704622	1.561498
-76.839183	-12.851566	1.566502
-77.181120	-14.525443	1.571507
-77.744004	-4.282256	1.576512
-78.157760	-13.085305	1.581517
-78.415285	-10.688056	1.586522
-78.303452	-17.848749	1.591526
-78.385683	-10.157538	1.596531
-78.917107	-5.268978	1.601536
-79.560602	-7.759579	1.606541
-79.881684	-0.875869	1.611546
-79.840643	-3.909637	1.616550
-79.867660	-1.836168	1.621555
-79.989980	-12.332856	1.626560
-79.922853	-5.038209	1.631565
-80.600447	-4.828072	1.636570
-81.136509	-18.357548	1.641574
-81.152718	-11.483348	1.646579
-81.541883	-11.251682	1.651584
-81.736710	-11.176822	1.656589
-82.463200	-8.950155	1.661594
-82.724297	-10.348727	1.666598
-82.746919	-12.771487	1.671603
-82.797581	-17.958073	1.676608
-82.639185	-7.858828	1.681613
-82.989367	-9.129638	1.686618
-82.979651	-18.239056	1.691622
-83.846008	-3.655549	1.696627
-83.983252	-13.934784	1.701632
-84.089492	-8.476533	1.706637
-84.730328	-10.667001	1.711642
-84.441442	-12.208151	1.716646
-85.069737	-6.402869	1.721651
-85.819424	-11.664109	1.726656
-86.010364	-6.898163	1.731661
-85.783004	-1.792398	1.736666
-86.004025	-7.306790	1.741670
-86.493709	-5.749724	1.746675
-86.333122	-13.139465	1.751680
-86.144048	-16.724608	1.756685
-86.640101	-10.588753	1.761690
-87.433924	-13.685512	1.766694
-87.797556	-5.649939	1.771699
-87.594901	-10.841168	1.776704
-87.606540	-12.677200	1.781709
-88.095837	-8.880331	1.786714
-88.750848	-12.115759	1.791718
-89.089609	-20.743825	1.796723
-89.477063	-19.822752	1.801728
-89.222381	-11.598725	1.806733
-89.372571	-12.944964	1.811738
-89.451870	-17.121051	1.816742
-89.864781	-10.169265	1.821747
-90.408360	-13.121496	1.826752
-90.555431	-11.899340	1.831757
-91.340278	-1.131226	1.836762
-90.845271	-13.546293	1.841766
-90.989848	-6.788141	1.846771
-91.285505	-11.632871	1.851776
-91.490010	-7.000851	1.856781
-92.077242	-4.890775	1.861786
-91.689664	-15.922417	1.866790
-92.325250	-2.146770	1.871795
-92.870601	-4.548252	1.876800
-92.807525	-7.414612	1.881805
-93.412702	-11.929585	1.886810
-93.686058	-11.329987	1.891814
-93.684151	-3.961912	1.896819
-93.882767	-13.896243	1.901824
-94.521179	-13.995916	1.906829
-94.873831	-2.339676	1.911834
-94.716225	-4.423515	1.916838
-95.311971	-6.956350	1.921843
-94.926371	-4.380834	1.926848
-95.147714	-14.599519	1.931853
-95.881580	0.545473	1.936858
-96.409854	-11.292667	1.941862
-96.581162	-4.751808	1.946867
-96.769369	-14.880741	1.951872
-96.576609	-16.622052	1.956877
-97.000186	-8.925149	1.961882
-96.595947	-9.487710	1.966886
-97.254906	-14.649184	1.971891
-97.993054	-12.828813	1.976896
-97.947745	-12.161775	1.981901
-98.277974	-14.843514	1.986906
-98.006458	-14.110461	1.991910
-98.913500	-11.010988	1.996915
-99.412550	-11.157820	2.006912
-98.707700	-11.568027	2.016909
-98.437456	-12.544106	2.026906
-97.986109	-8.888698	2.036902
-97.350850	-13.960425	2.046899
-96.836667	-11.471011	2.056896
-95.801603	-9.788101	2.066893
-95.643503	-12.248208	2.076890
-95.835273	-0.481554	2.086886
-94.919460	-3.053303	2.096883
-94.474799	-6.654052	2.106880
-93.505878	-7.482332	2.116877
-92.973960	-6.253255	2.126874
-92.789506	-13.250442	2.136870
-92.475125	-14.534324	2.146867
-91.765297	-14.314934	2.156864
-91.436187	-11.939250	2.166861
-90.390362	-10.432239	2.176858
-90.323824	-10.819086	2.186854
-90.396983	-9.638344	2.196851
-89.395764	-8.577369	2.206848
-88.839983	-11.615729	2.216845
-87.942439	-11.130971	2.226842
-87.730517	-9.833064	2.236838
-87.127852	-13.087793	2.246835
-86.969148	-7.711108	2.256832
-86.140179	-1.662694	2.266829
-86.016322	-6.369705	2.276826
-85.048332	-8.265354	2.286822
-84.324210	-3.679932	2.296819
-84.522050	-7.104619	2.306816
-83.837731	-3.764241	2.316813
-83.054790	0.390720	2.326810
-82.428108	-7.429237	2.336806
-82.638712	-8.986161	2.346803
-81.800598	-8.074013	2.356800
-81.145184	-5.828326	2.366797
-80.298249	-3.621962	2.376794
-80.433964	-6.793403	2.386790
-80.081724	-5.694734	2.396787
-78.957424	-15.644837	2.406784
-78.548750	-8.704216	2.416781
-78.412685	-15.237720	2.426778
-77.817554	-8.744267	2.436774
-77.010101	-14.210258	2.446771
-77.042552	-13.596538	2.456768
-76.296399	-9.144422	2.466765
-75.976391	-14.103711	2.476762
-74.850702	-10.011621	2.486758
-74.499441	-12.527144	2.496755
-74.540908	-10.657612	2.506752
-73.961943	-10.731448	2.516749
-73.137807	-9.747434	2.526746
-72.816968	-4.963009	2.536742
-71.787144	-8.246235	2.546739
-71.908796	-8.372538	2.556736
-71.515996	-11.160617	2.566733
-70.619788	-10.640805	2.576730
-70.071059	-10.652915	2.586726
-69.824868	-14.843630	2.596723
-69.194144	-10.664971	2.606720
-68.659646	-13.389583	2.616717
-68.380693	-14.496893	2.626714
-67.389848	-9.455671	2.636710
-67.612458	-11.549235	2.646707
-66.411270	-13.839142	2.656704
-65.930438	-10.942236	2.666701
-65.757796	-10.179890	2.676698
-65.594805	-10.546909	2.686694
-64.620573	-15.908991	2.696691
-64.284840	-7.978194	2.706688
-63.705583	-20.836907	2.716685
-62.831474	-16.053101	2.726682
-62.704342	-10.506779	2.736678
-62.581585	-12.125110	2.746675
-61.664909	-19.987047	2.756672
-61.056695	-21.063263	2.766669
-60.517663	-16.468030	2.776666
-59.647367	-16.932505	2.786662
-59.721750	-16.768405	2.796659
-59.816373	-13.544324	2.806656
-58.736850	-11.782806	2.816653
-58.358664	-10.022961	2.826650
-57.269143	-8.883868	2.836646
-56.849773	-16.361110	2.846643
-56.608936	-13.252614	2.856640
-56.477959	-10.012975	2.866637
-55.954874	-13.286990	2.876634
-55.270522	-16.266176	2.886630
-54.507341	-14.303355	2.896627
-53.836973	-11.888940	2.906624
-53.990688	-16.521054	2.916621
-53.462400	-5.240301	2.926618
-52.626729	-7.153359	2.936614
-52.222832	-11.840618	2.946611
-51.293700	-8.601710	2.956608
-50.887772	-11.968353	2.966605
-50.899832	-6.980046	2.976602
-50.388205	-6.881845	2.986598
-49.533724	-20.363101	2.996595
-49.363861	-18.748212	3.006592
-48.178652	-6.065083	3.016589
-48.096628	-12.447629	3.026586
-48.026913	-13.569876	3.036582
-46.846753	-16.581911	3.046579
-46.309186	-13.925080	3.056576
-46.449118	-17.960646	3.066573
-45.844788	-11.820238	3.076570
-45.252375	-14.319457	3.086566
-44.945540	-15.203034	3.096563
-43.895729	-13.649126	3.106560
-43.792488	-14.928642	3.116557
-43.050316	-19.684406	3.126554
-42.337238	-18.942851	3.136550
-42.129041	-20.637839	3.146547
-41.802151	-16.668456	3.156544
-40.871715	-20.886514	3.166541
-40.811525	-20.375914	3.176538
-40.479187	-12.672662	3.186534
-39.432117	-8.600005	3.196531
-39.125037	-10.386414	3.206528
-38.628115	-10.282755	3.216525
-37.868695	-12.285308	3.226522
-37.451094	-9.476754	3.236518
-37.429432	-14.288225	3.246515
-36.411941	-8.025250	3.256512
-36.031930	-10.475561	3.266509
-36.023265	-2.199238	3.276506
-35.110021	-9.404932	3.286502
-34.801603	-6.325962	3.296499
-33.954838	-7.255593	3.306496
-33.463079	-4.328708	3.316493
-32.910705	-5.402565	3.326490
-32.947447	-6.761654	3.336486
-31.782331	-13.062587	3.346483
-31.472730	-15.349886	3.356480
-31.400181	-8.578666	3.366477
-30.934447	-9.300089	3.376474
-30.371161	-10.673408	3.386470
-28.950241	-6.715976	3.396467
-28.652212	-13.597806	3.406464
-28.598473	-12.439990	3.416461
-28.605716	-9.343550	3.426458
-27.595434	-8.790814	3.436454
-27.374005	-12.182582	3.446451
-26.168835	-12.914600	3.456448
-25.870585	-4.743551	3.466445
-25.750910	-7.897739	3.476442
-25.317592	-7.863370	3.486438
-24.383637	-9.715705	3.496435
-23.997853	-6.458719	3.506432
-23.821334	-10.366166	3.516429
-22.485756	-5.996315	3.526426
-22.577993	-8.227385	3.536422
-22.292438	-4.986469	3.546419
-21.851244	-3.480345	3.556416
-21.342879	-10.474118	3.566413
-20.508271	-11.066079	3.576410
-19.985294	-12.860761	3.586406
-19.757567	-12.911587	3.596403
-18.985080	-6.271518	3.606400
-18.344307	-7.023362	3.616397
-18.384063	-5.157261	3.626394
-17.536981	-7.011910	3.636390
-16.631235	-14.754944	3.646387
-16.622305	-6.361458	3.656384
-16.362402	-6.654871	3.666381
-15.275391	-9.712589	3.676378
-15.241656	-6.400789	3.686374
-14.691045	-6.429030	3.696371
-13.520996	-8.181913	3.706368
-13.520478	-5.767736	3.716365
-13.473995	1.520715	3.726362
-12.692116	-9.066639	3.736358
-12.213395	-10.505984	3.746355
-11.105320	-5.954996	3.756352
-10.644848	-8.750444	3.766349
-10.733688	-10.041235	3.776346
-10.474824	-9.102250	3.786342
-9.439638	-12.782272	3.796339
-9.219924	-6.895578	3.806336
-8.421527	-6.385876	3.816333
-7.922000	-9.402808	3.826330
-7.443345	-11.548540	3.836326
-7.580090	-10.826718	3.846323
-6.691492	-3.545843	3.856320
-5.732200	-2.760260	3.866317
-5.221212	-1.797176	3.876314
-5.062742	-9.588584	3.886310
-4.673600	-3.506530	3.896307
-4.435659	4.015032	3.906304
-3.898941	6.662497	3.916301
-3.384910	16.824124	3.926298
-2.788425	26.871552	3.936294
-2.091722	39.355189	3.946291
-1.624948	44.433681	3.956288
-1.634106	53.938711	3.966285
-1.388813	69.353097	3.976282
-0.843945	94.870225	3.986278
-0.338604	106.294009	3.996275
0.000000	115.211956	4.001280
0.596283	134.677187	4.006285
0.329407	147.408483	4.011290
0.792832	142.315807	4.016294
0.860251	153.163289	4.021299
1.128565	153.697539	4.026304
1.645824	159.542811	4.031309
1.409141	155.286783	4.036314
1.522478	149.286854	4.041318
0.974563	155.146113	4.046323
1.528123	153.921236	4.051328
1.145320	149.052060	4.056333
1.231068	150.959297	4.061338
1.295160	149.554371	4.066342
1.340549	148.601600	4.071347
1.252278	146.391512	4.076352
1.399969	154.619627	4.081357
1.294819	159.524119	4.086362
1.697461	145.367473	4.091366
1.504226	156.704783	4.096371
1.485647	151.547950	4.101376
1.033951	145.879599	4.106381
0.938557	153.190130	4.111386
1.717034	163.221409	4.116390
1.515748	167.454353	4.121395
1.472889	165.952185	4.126400
1.677166	163.709201	4.131405
1.311387	159.814949	4.136410
1.439482	158.029907	4.141414
1.907683	171.538929	4.146419
1.543761	163.711930	4.151424
1.311304	155.516461	4.156429
1.428123	161.889142	4.161434
1.825978	167.835264	4.166438
1.345046	159.618370	4.171443
1.453754	163.306350	4.176448
1.740668	172.835215	4.181453
1.575212	176.527920	4.186458
1.626482	168.107940	4.191462
1.835732	178.480949	4.196467
1.877203	166.455896	4.201472
1.992490	156.769973	4.206477
1.428222	163.748559	4.211482
1.439695	156.499016	4.216486
1.489314	161.910910	4.221491
1.869755	165.297160	4.226496
1.968887	178.683321	4.231501
1.790646	177.436343	4.236506
1.931480	161.991700	4.241510
1.662914	158.547374	4.246515
1.916002	164.180683	4.251520
1.965165	163.629111	4.256525
1.651013	164.766565	4.261530
1.647816	153.124954	4.266534
1.852120	155.773016	4.271539
1.806088	161.259913	4.276544
1.859223	167.588728	4.281549
1.833411	185.062843	4.286554
1.791063	176.521396	4.291558
1.802831	177.921311	4.296563
1.875677	173.620250	4.301568
2.011045	172.545902	4.306573
2.062681	179.937953	4.311578
2.084983	180.039118	4.316582
1.813163	176.655404	4.321587
1.729398	178.326452	4.326592
2.084050	176.569407	4.331597
1.736024	172.833736	4.336602
2.070504	171.456311	4.341606
2.203131	177.798063	4.346611
2.092058	171.345860	4.351616
2.223976	174.163379	4.356621
2.128136	172.909899	4.361626
2.377564	171.684919	4.366630
2.087857	170.556534	4.371635
1.887255	172.347009	4.376640
2.121221	175.616866	4.381645
1.839329	177.337743	4.386650
2.252956	175.805628	4.391654
2.216738	185.084261	4.396659
1.905500	178.245614	4.401664
2.461585	178.852115	4.406669
2.031921	179.393800	4.411674
2.124201	174.899892	4.416678
1.826955	178.967449	4.421683
1.991610	177.546863	4.426688
2.291749	177.386475	4.431693
2.234307	179.480521	4.436698
2.094038	173.406178	4.441702
2.004347	180.481719	4.446707
2.150357	173.594027	4.451712
1.999308	176.189855	4.456717
1.899719	177.493215	4.461722
1.911067	183.170496	4.466726
2.203389	192.844060	4.471731
2.459310	204.200051	4.476736
2.221158	198.368725	4.481741
2.059250	211.077395	4.486746
2.472462	194.906958	4.491750
2.607955	202.178397	4.496755
2.374208	207.087106	4.501760
2.177301	196.975215	4.506765
2.380182	201.610301	4.511770
2.678608	205.736978	4.516774
2.859290	206.427238	4.521779
2.654236	211.318827	4.526784
2.796817	205.058067	4.531789
2.473463	203.327491	4.536794
2.415989	188.511637	4.541798
2.388245	207.915923	4.546803
2.646953	202.526081	4.551808
2.693915	203.582003	4.556813
2.179324	201.659744	4.561818
2.522557	196.959082	4.566822
2.816495	194.806536	4.571827
2.712169	193.120951	4.576832
2.977885	194.772388	4.581837
2.394875	194.752666	4.586842
2.696857	189.618676	4.591846
2.730444	190.353985	4.596851
2.299450	188.611696	4.601856
2.888425	196.492719	4.606861
2.747431	204.759477	4.611866
2.555970	212.546888	4.616870
2.303070	203.551003	4.621875
2.636921	202.575461	4.626880
2.716942	196.172589	4.631885
2.511518	202.019665	4.636890
2.531965	195.085078	4.641894
2.624351	200.692801	4.646899
2.655167	205.035146	4.651904
2.718861	201.418859	4.656909
2.509806	206.791949	4.661914
2.542901	200.776024	4.666918
2.589279	206.438368	4.671923
2.986871	209.046853	4.676928
3.154039	202.386805	4.681933
2.466393	205.157930	4.686938
2.859617	208.336559	4.691942
2.779873	208.409320	4.696947
2.750015	217.645851	4.701952
3.319878	229.373750	4.706957
3.086035	221.583419	4.711962
3.043798	207.448535	4.716966
2.807572	210.440435	4.721971
2.702287	204.012628	4.726976
2.910638	211.029123	4.731981
3.139880	220.956127	4.736986
3.496825	216.550712	4.741990
2.965515	210.246180	4.746995
2.467650	203.230941	4.752000
2.720762	214.834144	4.757005
2.569486	226.263039	4.762010
2.768475	224.286622	4.767014
3.165377	228.274587	4.772019
3.283573	229.316256	4.777024
3.378633	229.792063	4.782029
3.331874	227.278116	4.787034
3.409953	223.900026	4.792038
3.429871	220.173495	4.797043
3.389035	221.284216	4.802048
3.202836	226.710700	4.807053
3.043187	229.314202	4.812058
3.203395	230.343003	4.817062
3.052261	232.461134	4.822067
2.955363	235.687605	4.827072
3.197202	228.585659	4.832077
3.182010	237.494057	4.837082
3.200267	239.452940	4.842086
3.313552	232.700032	4.847091
3.299230	236.217361	4.852096
3.308742	237.402501	4.857101
3.326531	240.725009	4.862106
3.479061	233.905880	4.867110
3.620900	231.065181	4.872115
3.076822	232.678191	4.877120
3.435589	222.910031	4.882125
3.595343	231.079356	4.887130
3.698877	227.067727	4.892134
3.550141	229.546146	4.897139
3.309978	226.015128	4.902144
3.614580	230.469873	4.907149
3.628597	222.644114	4.912154
3.430372	222.042474	4.917158
3.293041	215.031206	4.922163
3.188183	226.013121	4.927168
3.549815	224.267640	4.932173
3.153553	230.410189	4.937178
3.709034	232.658743	4.942182
3.517945	230.891752	4.947187
3.390013	235.809304	4.952192
3.589476	227.084654	4.957197
3.513414	222.585306	4.962202
3.751835	234.352158	4.967206
3.727182	238.978389	4.972211
3.676189	231.181730	4.977216
3.811941	235.574182	4.982221
3.616208	228.483418	4.987226
3.492308	230.708038	4.992230
3.668174	227.495053	4.997235
3.504328	228.393977	5.002240
3.662646	220.096508	5.007245
3.417197	232.508160	5.012250
3.831312	226.568941	5.017254
3.867480	235.678145	5.022259
3.405347	221.007524	5.027264
3.844143	229.304243	5.032269
3.423951	238.829345	5.037274
3.558345	224.878913	5.042278
3.455816	230.558121	5.047283
3.390866	227.686345	5.052288
3.461530	228.178605	5.057293
3.282288	247.407209	5.062298
3.763900	248.496699	5.067302
3.771966	248.277383	5.072307
3.596287	253.933187	5.077312
3.981514	244.964475	5.082317
3.985531	252.841688	5.087322
4.178888	241.935031	5.092326
3.868119	258.861974	5.097331
3.840271	252.260744	5.102336
4.304451	254.052126	5.107341
4.237548	252.506238	5.112346
3.895207	242.334709	5.117350
4.008135	235.006063	5.122355
4.010714	241.893260	5.127360
3.922401	237.187012	5.132365
4.016439	239.921857	5.137370
4.056314	243.120707	5.142374
3.902578	246.789455	5.147379
3.786506	248.183970	5.152384
3.939834	250.941222	5.157389
3.828552	248.127275	5.162394
3.966013	249.099508	5.167398
4.160487	244.339739	5.172403
3.892954	254.078358	5.177408
4.215028	251.092536	5.182413
4.019617	255.387860	5.187418
3.980755	250.616963	5.192422
4.101255	255.862829	5.197427
4.169048	254.362407	5.202432
4.303914	249.997888	5.207437
4.032883	249.543622	5.212442
3.696674	245.587800	5.217446
3.734167	250.542874	5.222451
3.869018	257.811272	5.227456
3.985045	260.827428	5.232461
4.513622	265.323238	5.237466
4.550225	270.338566	5.242470
4.597077	262.377966	5.247475
4.093595	259.068270	5.252480
4.389087	255.102677	5.257485
4.063708	256.343122	5.262490
4.352416	265.083997	5.267494
4.770948	264.278763	5.272499
4.414401	261.246741	5.277504
4.230850	254.929176	5.282509
4.399061	258.003645	5.287514
4.044942	258.925869	5.292518
4.335192	270.168992	5.297523
4.228458	270.075115	5.302528
4.961428	265.645943	5.307533
4.504371	273.050797	5.312538
4.391503	251.061917	5.317542
4.124042	250.771607	5.322547
4.137719	271.988639	5.327552
4.613799	274.692479	5.332557
4.287153	276.961326	5.337562
4.452845	277.552686	5.342566
4.887098	273.024491	5.347571
4.391623	274.541353	5.352576
4.812399	280.850934	5.357581
4.676266	283.476091	5.362586
4.522326	278.742086	5.367590
4.377282	274.050989	5.372595
4.574352	281.502695	5.377600
4.462425	275.034769	5.382605
4.451802	277.599256	5.387610
4.449769	276.305854	5.392614
4.734960	281.554559	5.397619
4.277594	290.006653	5.402624
4.582209	286.058615	5.407629
4.396445	286.315559	5.412634
4.403032	283.037173	5.417638
4.876746	288.968360	5.422643
4.278319	290.767005	5.427648
4.276680	288.255514	5.432653
4.472108	295.122197	5.437658
4.736064	300.943680	5.442662
4.939075	298.017517	5.447667
4.843192	303.509055	5.452672
5.041493	295.176853	5.457677
5.012078	312.550414	5.462682
5.113856	303.458128	5.467686
5.026115	287.292838	5.472691
4.445345	290.303596	5.477696
5.179919	291.261956	5.482701
4.856028	291.027886	5.487706
5.190739	289.628270	5.492710
4.926583	277.356503	5.497715
4.667491	279.665452	5.502720
4.802831	284.238311	5.507725
5.047195	302.600604	5.512730
5.101059	291.358136	5.517734
4.620600	288.411840	5.522739
4.679854	300.981739	5.527744
5.106306	297.229860	5.532749
5.110600	301.759853	5.537754
4.821099	298.065662	5.542758
4.961698	308.019172	5.547763
4.705292	303.668104	5.552768
4.849524	304.205858	5.557773
5.218489	311.434664	5.562778
5.098800	307.385007	5.567782
5.335257	302.242204	5.572787
4.852229	310.448371	5.577792
4.859807	304.543950	5.582797
4.807119	308.301380	5.587802
5.084762	314.035317	5.592806
4.752184	311.407673	5.597811
4.957793	308.012875	5.602816
5.019643	309.376529	5.607821
4.877395	299.091557	5.612826
5.295346	329.531191	5.617830
5.341435	323.956120	5.622835
5.166014	327.590297	5.627840
5.724585	336.561270	5.632845
5.247438	325.483714	5.637850
5.302959	308.995547	5.642854
5.432301	311.168093	5.647859
5.080596	305.110806	5.652864
5.176129	303.995197	5.657869
5.432957	308.818062	5.662874
5.211656	312.250574	5.667878
5.439482	315.559377	5.672883
5.194131	320.897025	5.677888
5.574899	315.908917	5.682893
5.365322	305.991923	5.687898
4.879296	318.475892	5.692902
5.719211	322.973862	5.697907
5.377577	336.738811	5.702912
5.725977	331.812685	5.707917
5.339985	320.198928	5.712922
5.346646	323.219468	5.717926
5.406497	329.869995	5.722931
5.442967	340.953361	5.727936
5.770941	331.114007	5.732941
5.603566	322.737488	5.737946
5.175214	328.378873	5.742950
5.586591	328.780124	5.747955
5.568958	330.538963	5.752960
5.773778	325.929420	5.757965
5.726266	330.938879	5.762970
5.357680	316.528857	5.767974
5.375565	323.742728	5.772979
5.737696	329.172454	5.777984
5.252168	328.409901	5.782989
5.693422	326.212257	5.787994
5.561583	325.404127	5.792998
5.764240	324.262347	5.798003
5.720877	323.551172	5.803008
5.834178	329.873841	5.808013
5.518451	320.185335	5.813018
5.408403	332.519028	5.818022
5.932441	330.843161	5.823027
5.864950	327.895835	5.828032
5.790064	329.853412	5.833037
5.637702	331.630065	5.838042
5.448977	329.214136	5.843046
6.046299	332.449594	5.848051
5.888943	328.529181	5.853056
6.043991	330.213679	5.858061
6.189374	329.957164	5.863066
5.875773	326.329995	5.868070
5.946232	334.968845	5.873075
5.930420	332.655705	5.878080
5.741651	324.526122	5.883085
5.297256	320.568145	5.888090
5.628173	330.194647	5.893094
5.842317	321.334789	5.898099
5.466017	329.872356	5.903104
5.668056	331.255313	5.908109
5.800293	343.323503	5.913114
5.703781	342.981265	5.918118
5.787082	340.118025	5.923123
5.614737	344.476217	5.928128
6.029910	341.583452	5.933133
6.046703	350.338231	5.938138
5.721024	353.034039	5.943142
6.369693	350.911665	5.948147
6.411297	353.876151	5.953152
6.168904	345.989021	5.958157
6.163907	338.805242	5.963162
6.006438	335.327765	5.968166
6.167575	339.013946	5.973171
6.140811	337.335254	5.978176
5.939631	327.812404	5.983181
6.091730	335.179387	5.988186
5.722583	342.516799	5.993190
6.361439	349.491630	5.998195
6.054822	356.819312	6.003200
6.076749	354.446511	6.008205
6.415746	357.371021	6.013210
6.368693	357.378582	6.018214
6.235305	342.479509	6.023219
6.033042	345.649639	6.028224
5.929567	333.020626	6.033229
6.046563	353.225100	6.038234
6.097449	353.312324	6.043238
6.558429	350.554792	6.048243
5.966705	356.772109	6.053248
6.398135	360.258025	6.058253
6.199482	356.423128	6.063258
5.450651	352.411306	6.068262
6.450103	352.831726	6.073267
6.170312	373.116983	6.078272
6.273594	363.809298	6.083277
6.666096	364.365347	6.088282
5.955576	355.276121	6.093286
5.932539	343.564709	6.098291
6.042043	357.696026	6.103296
6.582992	363.885687	6.108301
6.192829	347.504840	6.113306
6.224721	356.143378	6.118310
6.346312	338.366756	6.123315
6.007415	336.341198	6.128320
6.222262	334.023782	6.133325
6.035271	337.378192	6.138330
6.021378	345.837195	6.143334
6.330389	337.184019	6.148339
6.031446	334.750448	6.153344
6.090202	341.442278	6.158349
6.036413	341.384450	6.163354
6.251961	349.485032	6.168358
6.430387	355.550802	6.173363
6.540878	355.676201	6.178368
6.282686	341.356537	6.183373
6.375744	340.681068	6.188378
5.885590	334.344774	6.193382
5.987587	336.202046	6.198387
5.813862	335.368800	6.203392
5.945046	341.378645	6.208397
6.327493	347.001364	6.213402
6.050714	350.733583	6.218406
6.408815	354.553614	6.223411
5.962872	343.806542	6.228416
6.327927	340.380585	6.233421
5.877242	348.141977	6.238426
5.981709	351.935059	6.243430
6.581873	356.365964	6.248435
6.415305	360.555583	6.253440
6.110157	350.764174	6.258445
5.978265	346.839793	6.263450
6.061684	346.747947	6.268454
6.266029	339.651795	6.273459
6.142764	352.420988	6.278464
6.305770	353.876462	6.283469
6.201904	341.598676	6.288474
5.655315	340.484966	6.293478
6.296256	349.734182	6.298483
6.236169	359.266555	6.303488
6.259594	358.624073	6.308493
6.317599	362.949568	6.313498
6.296769	351.120750	6.318502
6.372007	331.940335	6.323507
5.851410	338.143407	6.328512
5.904421	336.771828	6.333517
6.225688	348.728335	6.338522
6.509246	355.742668	6.343526
6.415664	344.383921	6.348531
6.215150	347.923934	6.353536
6.133098	337.999721	6.358541
6.226900	340.563777	6.363546
5.863979	333.084556	6.368550
6.392770	341.028798	6.373555
5.924527	342.437023	6.378560
5.925656	334.818863	6.383565
5.986308	338.577636	6.388570
6.177788	355.708042	6.393574
6.364374	350.180690	6.398579
6.289942	346.073358	6.403584
6.030589	342.241589	6.408589
6.275373	336.774781	6.413594
5.520283	337.547470	6.418598
6.228437	353.534422	6.423603
6.367575	355.670648	6.428608
6.598236	351.591742	6.433613
6.573034	344.638894	6.438618
5.993642	343.596729	6.443622
6.173502	328.746970	6.448627
5.678238	340.365536	6.453632
5.720080	344.358190	6.458637
6.392591	361.587711	6.463642
6.472049	355.238652	6.468646
6.167415	344.634092	6.473651
6.165419	346.703706	6.478656
6.339435	345.904901	6.483661
6.188226	339.145679	6.488666
6.012544	337.284531	6.493670
5.985926	339.395942	6.498675
6.069522	346.254747	6.503680
6.256904	355.251885	6.508685
6.342506	356.165760	6.513690
6.127363	350.289673	6.518694
6.413706	339.915801	6.523699
5.887987	344.762441	6.528704
6.197023	344.005888	6.533709
6.227804	348.205906	6.538714
6.496321	338.461226	6.543718
6.065395	331.843632	6.548723
6.006113	333.102763	6.553728
6.107253	329.369890	6.558733
6.123122	341.905444	6.563738
6.128044	352.272404	6.568742
6.194118	336.807611	6.573747
5.988064	344.122795	6.578752
6.166916	347.189295	6.583757
6.626264	354.571723	6.588762
6.031736	342.332366	6.593766
6.492062	333.361408	6.598771
5.894819	335.362350	6.603776
6.026242	338.316012	6.608781
6.079017	333.334675	6.613786
6.150989	343.675371	6.618790
6.148746	342.372506	6.623795
5.999398	340.700244	6.628800
6.309186	349.615046	6.633805
6.349638	352.734733	6.638810
5.911702	350.683465	6.643814
6.275788	353.920440	6.648819
6.184696	358.209037	6.653824
6.382343	351.616954	6.658829
6.352406	339.308677	6.663834
6.188760	340.663151	6.668838
6.405117	327.807177	6.673843
6.388303	336.522890	6.678848
6.162446	332.736527	6.683853
6.367107	332.957994	6.688858
5.956280	331.693435	6.693862
6.079384	329.798423	6.698867
6.052493	335.892989	6.703872
6.105691	339.950311	6.708877
6.128404	335.789892	6.713882
5.997403	336.313554	6.718886
6.349760	334.003202	6.723891
6.281003	335.520069	6.728896
6.277239	331.458685	6.733901
6.181374	334.548973	6.738906
6.019471	332.204796	6.743910
6.250964	333.766663	6.748915
6.455618	332.498023	6.753920
6.312502	330.824792	6.758925
6.215969	328.805791	6.763930
6.262465	338.745495	6.768934
6.054693	327.366573	6.773939
5.964574	340.023030	6.778944
5.947679	335.792849	6.783949
6.303757	331.843115	6.788954
6.381250	333.289756	6.793958
6.084727	331.817577	6.798963
6.183771	335.285638	6.803968
6.345386	328.348001	6.808973
6.055044	326.976099	6.813978
6.137919	338.071221	6.818982
6.037356	323.056323	6.823987
6.197975	327.134882	6.828992
6.410797	333.597080	6.833997
6.059538	331.155837	6.839002
6.184756	334.917211	6.844006
6.178189	337.749991	6.849011
5.923525	336.786979	6.854016
6.149813	340.165628	6.859021
6.117686	344.698138	6.864026
6.288344	334.500467	6.869030
6.551828	327.088232	6.874035
6.445765	346.061943	6.879040
6.206585	335.402905	6.884045
6.258139	330.285719	6.889050
6.388441	334.191833	6.894054
6.363094	333.759422	6.899059
6.226298	335.346993	6.904064
6.351318	336.495173	6.909069
6.267779	331.908378	6.914074
6.177639	327.417523	6.919078
6.107812	326.992038	6.924083
5.931985	329.933427	6.929088
6.153528	335.280641	6.934093
6.136954	332.989766	6.939098
6.374625	347.765499	6.944102
6.333842	333.943496	6.949107
6.098770	335.479930	6.954112
5.928890	335.981171	6.959117
6.331355	329.929839	6.964122
5.824162	340.480928	6.969126
6.035334	330.688233	6.974131
5.943382	339.491576	6.979136
6.271025	336.330869	6.984141
6.112666	332.268245	6.989146
6.292465	340.529411	6.994150
6.442881	334.289533	6.999155
6.117502	338.532347	7.004160
6.056962	343.167356	7.009165
6.649678	331.768200	7.014170
6.181516	336.235721	7.019174
6.282320	329.522685	7.024179
5.855069	332.958794	7.029184
5.904129	333.903667	7.034189
6.295515	331.315160	7.039194
6.429892	340.393308	7.044198
6.586220	332.858551	7.049203
6.032061	321.315268	7.054208
6.024671	318.273166	7.059213
6.014792	323.646917	7.064218
6.047145	333.082627	7.069222
6.379957	337.415949	7.074227
6.258525	338.140599	7.079232
5.769596	332.148959	7.084237
6.448828	325.836240	7.089242
6.209073	335.020092	7.094246
6.083205	335.163310	7.099251
6.196284	348.376586	7.104256
6.359181	339.518371	7.109261
6.111465	322.941364	7.114266
5.694499	317.413082	7.119270
6.021751	321.478351	7.124275
6.206006	330.282976	7.129280
6.400583	338.855048	7.134285
6.607095	334.729287	7.139290
6.062957	330.002238	7.144294
6.045584	321.358758	7.149299
6.069407	321.640018	7.154304
5.589200	334.730525	7.159309
6.216958	334.247047	7.164314
6.176775	343.934499	7.169318
6.231987	337.516455	7.174323
6.176743	339.081838	7.179328
6.077250	339.973912	7.184333
6.051654	334.239159	7.189338
6.171180	344.012474	7.194342
6.449256	340.290016	7.199347
6.438982	340.222249	7.204352
6.298950	352.576443	7.209357
6.683177	335.087959	7.214362
5.957906	333.587623	7.219366
5.926789	320.846114	7.224371
5.759158	326.519671	7.229376
6.232141	334.561182	7.234381
6.413107	339.629982	7.239386
6.167057	344.645047	7.244390
6.388151	346.379374	7.249395
6.121092	347.645546	7.254400
5.814896	338.018821	7.259405
5.990100	344.727322	7.264410
5.768861	349.539211	7.269414
6.243219	342.154248	7.274419
5.927757	346.332245	7.279424
6.037498	343.015641	7.284429
6.013241	349.429337	7.289434
6.370390	346.558260	7.294438
6.176231	340.612470	7.299443
6.192392	338.382936	7.304448
6.317240	342.884678	7.309453
6.531395	346.464531	7.314458
6.113163	355.926115	7.319462
6.382429	351.989893	7.324467
6.425609	345.570557	7.329472
6.018639	345.403205	7.334477
6.291598	344.607977	7.339482
6.287095	345.244820	7.344486
6.371707	345.560907	7.349491
6.322742	330.914451	7.354496
5.755111	330.417778	7.359501
6.288283	338.620761	7.364506
6.248554	338.377248	7.369510
6.139466	321.503416	7.374515
5.964613	325.504494	7.379520
6.209717	339.380570	7.384525
6.151797	336.627902	7.389530
6.251278	345.236929	7.394534
6.343901	347.149445	7.399539
6.195757	340.060718	7.404544
5.742990	336.088223	7.409549
6.125012	345.352440	7.414554
5.911033	350.900345	7.419558
6.239817	349.109346	7.424563
6.300586	347.477135	7.429568
6.429701	338.715928	7.434573
6.183730	344.003059	7.439578
5.866532	335.108866	7.444582
6.272317	339.819963	7.449587
6.432488	340.282472	7.454592
6.174292	339.936934	7.459597
6.108338	322.528045	7.464602
5.702260	342.921514	7.469606
6.204359	341.935588	7.474611
6.214488	347.473909	7.479616
5.834233	344.799900	7.484621
6.264761	340.202666	7.489626
6.274480	345.057687	7.494630
6.292894	343.264394	7.499635
6.169657	349.962416	7.504640
5.896190	345.781671	7.509645
6.135051	349.367169	7.514650
6.403657	346.104922	7.519654
6.024187	350.669368	7.524659
6.505304	346.956424	7.529664
6.260904	342.869229	7.534669
6.341804	340.297425	7.539674
6.217708	342.911225	7.544678
5.980613	331.305915	7.549683
6.234776	348.765072	7.554688
6.201095	347.381681	7.559693
6.263028	339.339605	7.564698
6.236623	336.297297	7.569702
6.040312	327.564617	7.574707
6.134433	334.216137	7.579712
5.898226	345.974704	7.584717
6.217784	350.819451	7.589722
5.787351	355.034333	7.594726
6.114136	351.225195	7.599731
6.229237	351.799124	7.604736
6.005535	345.851605	7.609741
6.462875	344.572096	7.614746
6.191063	352.337277	7.619750
6.302006	345.755532	7.624755
6.346777	343.461432	7.629760
6.028072	346.175135	7.634765
6.017431	344.908377	7.639770
5.999318	347.629063	7.644774
6.147540	350.285886	7.649779
6.394727	342.806580	7.654784
6.201990	345.190627	7.659789
6.150177	348.701160	7.664794
5.835174	353.252406	7.669798
5.992117	347.707524	7.674803
5.955721	344.878738	7.679808
6.161268	351.063668	7.684813
5.906355	345.443708	7.689818
5.871193	343.155726	7.694822
6.045468	341.838032	7.699827
6.124796	344.341068	7.704832
5.959448	347.597199	7.709837
6.115246	349.930144	7.714842
6.176392	359.791650	7.719846
6.303814	351.837448	7.724851
6.333123	353.607963	7.729856
5.946073	347.549837	7.734861
6.169241	346.423845	7.739866
6.044350	347.835559	7.744870
5.887089	339.859248	7.749875
6.258399	337.457361	7.754880
6.298379	343.025833	7.759885
6.406392	344.239935	7.764890
6.186882	349.674807	7.769894
5.987929	350.310288	7.774899
6.084103	341.468788	7.779904
6.341589	342.612162	7.784909
6.408606	338.153783	7.789914
6.416833	342.553461	7.794918
6.421723	347.181448	7.799923
6.424613	333.248242	7.804928
6.246335	345.174957	7.809933
6.359234	347.359559	7.814938
6.325866	349.649191	7.819942
6.486689	342.575633	7.824947
6.641348	334.939896	7.829952
5.862890	334.748127	7.834957
6.127978	327.563429	7.839962
6.362673	337.331464	7.844966
6.079189	328.906582	7.849971
6.001497	327.666084	7.854976
5.862822	335.375728	7.859981
6.588735	336.686611	7.864986
6.557780	337.156732	7.869990
6.135397	331.502740	7.874995
5.936735	314.797882	7.880000
5.799334	329.195406	7.885005
6.362351	329.705922	7.890010
6.239245	335.711066	7.895014
6.059157	329.772581	7.900019
6.431341	332.068669	7.905024
6.179811	327.201152	7.910029
5.887116	320.653787	7.915034
5.782944	330.047478	7.920038
6.127246	341.481544	7.925043
6.635136	340.086598	7.930048
6.190143	344.199342	7.935053
6.374589	332.208864	7.940058
5.885533	333.133118	7.945062
6.166046	336.781729	7.950067
6.401956	341.326290	7.955072
5.921347	330.726990	7.960077
6.314099	326.695618	7.965082
6.078076	338.299130	7.970086
6.219876	341.339761	7.975091
6.142065	332.819580	7.980096
5.892321	340.711032	7.985101
6.491293	337.422660	7.990106
6.017008	344.899827	7.995110
6.060495	351.619348	8.000115
6.175309	346.656572	8.005133
6.217283	349.749114	8.010150
6.376750	347.815357	8.015168
6.290719	354.238100	8.020186
5.834335	333.475841	8.025203
6.149666	347.715728	8.030221
6.033672	343.126785	8.035238
6.046560	345.024711	8.040256
6.273336	343.493864	8.045274
6.266270	351.008786	8.050291
6.278392	347.794689	8.055309
6.119928	344.777557	8.060326
6.611644	340.153954	8.065344
6.171235	344.448165	8.070362
6.017296	344.810022	8.075379
5.978177	343.348975	8.080397
6.180170	341.875632	8.085414
6.277806	341.444122	8.090432
5.955020	351.813567	8.095450
6.043870	341.092872	8.100467
6.536872	340.754431	8.105485
6.138102	347.497249	8.110502
6.104911	339.752395	8.115520
6.215313	346.150862	8.120538
6.175736	340.035314	8.125555
6.553177	341.286374	8.130573
6.384168	343.499784	8.135590
6.626642	346.791471	8.140608
6.462424	347.565162	8.145626
5.961199	342.114751	8.150643
6.522468	342.835443	8.155661
6.145208	344.491172	8.160678
6.497796	335.654360	8.165696
6.456680	347.403142	8.170714
6.367616	345.318742	8.175731
6.895620	343.561123	8.180749
6.128442	342.797226	8.185766
6.182196	348.475560	8.190784
6.219907	357.308884	8.195802
6.064144	340.314986	8.200819
6.341374	346.962021	8.205837
6.065268	354.411541	8.210854
6.368169	347.220239	8.215872
6.452054	342.786358	8.220890
6.181805	355.451245	8.225907
6.444161	347.269071	8.230925
6.058766	346.335284	8.235942
6.110348	352.929095	8.240960
6.637009	351.282132	8.245978
6.321574	346.519124	8.250995
6.483318	334.887725	8.256013
6.573749	351.437848	8.261030
6.438006	345.627590	8.266048
6.189970	351.801014	8.271066
5.962597	355.225813	8.276083
6.518553	357.998503	8.281101
6.984571	364.480457	8.286118
6.979256	361.635128	8.291136
6.952223	352.507136	8.296154
6.753952	353.876235	8.301171
6.680325	346.636265	8.306189
6.516561	354.216609	8.311206
6.436243	351.572298	8.316224
6.652831	348.771312	8.321242
6.614004	354.656558	8.326259
6.594367	348.522123	8.331277
6.534101	352.066063	8.336294
6.671957	352.849525	8.341312
6.239248	346.242945	8.346330
6.056204	356.593792	8.351347
6.554035	349.599345	8.356365
6.609723	355.267914	8.361382
6.678948	345.219269	8.366400
6.644932	353.057108	8.371418
6.483850	356.774527	8.376435
6.898011	352.525895	8.381453
6.494367	343.510191	8.386470
6.356257	345.649366	8.391488
6.157384	342.436565	8.396506
6.639083	342.844615	8.401523
6.732581	341.902535	8.406541
6.681587	347.262680	8.411558
6.506252	340.694922	8.416576
6.451664	345.740062	8.421594
6.728544	353.087706	8.426611
6.381304	345.495882	8.431629
6.702511	343.057285	8.436646
6.679036	344.601129	8.441664
6.525300	347.127726	8.446682
6.465252	351.305916	8.451699
6.712653	344.315750	8.456717
6.720360	357.432797	8.461734
6.403068	351.025986	8.466752
6.559609	344.870434	8.471770
6.544434	360.032746	8.476787
6.358969	355.293679	8.481805
6.829433	346.883454	8.486822
6.446313	353.399787	8.491840
6.709727	353.816578	8.496858
6.767583	352.362521	8.501875
6.795761	353.472312	8.506893
6.761382	347.460088	8.511910
6.696356	354.308728	8.516928
6.723609	346.122136	8.521946
6.490016	355.127081	8.526963
6.594463	350.718398	8.531981
6.713052	355.316878	8.536998
6.597695	358.026839	8.542016
6.551734	347.317663	8.547034
6.447710	372.367830	8.552051
7.172269	366.912744	8.557069
7.001550	365.257600	8.562087
6.738740	351.041550	8.567104
7.126557	350.403921	8.572122
6.711207	345.940477	8.577139
6.500793	345.878805	8.582157
6.654843	344.706401	8.587175
6.649262	353.540152	8.592192
6.832461	362.865196	8.597210
6.936171	370.217720	8.602227
6.917236	356.465443	8.607245
6.781398	357.272583	8.612263
6.432026	352.230849	8.617280
6.999444	356.084140	8.622298
6.923439	367.958282	8.627315
6.807273	363.069574	8.632333
6.504028	359.642658	8.637351
6.626764	373.950420	8.642368
6.959091	371.775162	8.647386
6.792175	377.516265	8.652403
6.949795	374.348934	8.657421
7.284334	374.824076	8.662439
6.871257	373.099374	8.667456
7.221566	369.251980	8.672474
6.709938	361.887705	8.677491
6.621756	366.183882	8.682509
6.950847	359.979370	8.687527
6.786182	369.790902	8.692544
7.048915	367.071087	8.697562
7.139638	375.536422	8.702579
6.802984	358.987216	8.707597
6.670718	356.723359	8.712615
6.457371	371.102379	8.717632
6.993508	368.721829	8.722650
7.207965	378.540607	8.727667
7.171711	365.564153	8.732685
7.200562	377.541890	8.737703
7.221665	364.297744	8.742720
7.287503	351.166557	8.747738
6.773889	355.702530	8.752755
6.721534	359.712275	8.757773
6.912451	354.460194	8.762791
6.800444	361.827366	8.767808
7.230627	367.541768	8.772826
7.040818	368.704433	8.777843
6.796192	356.697656	8.782861
7.127593	358.946759	8.787879
6.915179	373.814761	8.792896
7.161220	372.116818	8.797914
7.140324	376.216339	8.802931
7.058681	364.648060	8.807949
7.045844	360.345994	8.812967
6.777002	355.408480	8.817984
6.955230	360.530978	8.823002
7.018655	370.013523	8.828019
6.869212	373.599753	8.833037
7.144440	374.393383	8.838055
7.074869	374.685304	8.843072
7.175893	367.263506	8.848090
7.125418	374.371807	8.853107
7.008790	366.119250	8.858125
7.072792	365.876003	8.863143
6.778887	366.486859	8.868160
7.086098	372.109961	8.873178
7.178956	372.234588	8.878195
7.272358	372.554779	8.883213
7.146324	374.329178	8.888231
6.962868	385.503730	8.893248
7.148087	380.716408	8.898266
7.018640	374.529638	8.903283
6.837797	377.691589	8.908301
7.349293	372.944983	8.913319
6.806182	371.966326	8.918336
6.908923	369.255642	8.923354
7.153780	375.712077	8.928371
7.061203	375.723571	8.933389
7.321355	374.307440	8.938407
7.343088	376.734141	8.943424
7.199575	372.316724	8.948442
6.987688	377.556769	8.953459
6.824496	373.707277	8.958477
7.163007	377.810797	8.963495
7.170929	385.354957	8.968512
7.404913	371.550666	8.973530
7.227050	377.325030	8.978547
7.091123	372.739183	8.983565
7.401798	373.148616	8.988583
7.019285	381.665546	8.993600
7.367861	386.427031	8.998618
7.550104	396.809385	9.003635
7.260718	384.736978	9.008653
7.078531	372.799359	9.013671
7.256516	386.981771	9.018688
7.275233	384.508218	9.023706
7.411902	392.168028	9.028723
7.402545	396.978934	9.033741
7.446001	375.674921	9.038759
7.290911	371.694787	9.043776
7.484446	375.994439	9.048794
7.304760	375.555615	9.053811
7.304285	373.318570	9.058829
7.308398	377.979058	9.063847
7.293570	381.515929	9.068864
7.145137	377.509512	9.073882
7.398590	380.919410	9.078899
7.311836	391.574005	9.083917
7.578257	378.477836	9.088935
7.230919	383.937778	9.093952
7.394753	387.844445	9.098970
7.756231	386.737569	9.103987
7.049356	382.594047	9.109005
7.411705	390.673132	9.114023
7.432995	391.411631	9.119040
7.492650	391.932728	9.124058
7.463337	386.077484	9.129075
7.032267	391.619890	9.134093
8.035684	384.392085	9.139111
7.304479	402.332441	9.144128
7.408010	385.610538	9.149146
7.301684	383.544600	9.154163
7.713095	392.300823	9.159181
7.786843	378.994823	9.164199
7.342243	386.735665	9.169216
7.300252	379.017409	9.174234
7.422718	381.005570	9.179251
7.426523	387.139796	9.184269
7.458646	382.073368	9.189287
7.552418	396.657044	9.194304
7.911753	381.403719	9.199322
7.550646	376.467942	9.204339
7.224590	379.441074	9.209357
7.526102	376.961360	9.214375
7.326564	386.008353	9.219392
7.621678	390.749762	9.224410
7.859936	398.832393	9.229427
7.370376	389.123177	9.234445
7.542925	390.816377	9.239463
7.322975	394.609239	9.244480
7.152822	400.824201	9.249498
7.325919	398.635864	9.254515
7.574764	404.189172	9.259533
7.721850	406.230304	9.264551
7.665799	408.842681	9.269568
7.785116	405.343654	9.274586
7.553487	404.417479	9.279603
7.663343	407.622533	9.284621
8.031202	401.683356	9.289639
7.609435	403.405977	9.294656
8.025725	399.617728	9.299674
7.834197	404.217169	9.304691
7.510308	400.285399	9.309709
7.635719	397.883591	9.314727
7.877231	402.245204	9.319744
7.719137	386.267746	9.324762
7.346215	389.532185	9.329779
7.610130	402.237008	9.334797
7.863632	408.335520	9.339815
7.884778	404.006062	9.344832
7.618860	401.362240	9.349850
8.056981	407.921134	9.354867
7.499871	392.930401	9.359885
7.791068	395.220481	9.364903
7.627717	395.116768	9.369920
7.682661	393.486444	9.374938
7.814482	396.268375	9.379955
7.752433	407.020113	9.384973
7.846363	401.142521	9.389991
7.761438	401.282205	9.395008
7.795845	398.932434	9.400026
7.814797	388.061656	9.405043
7.495408	404.274868	9.410061
8.021315	394.499057	9.415079
7.792733	400.338127	9.420096
7.799676	405.338991	9.425114
7.948475	398.597675	9.430131
7.886828	398.257231	9.435149
7.842142	392.073036	9.440167
7.579453	382.543084	9.445184
7.826372	393.019502	9.450202
8.229542	393.613341	9.455219
7.691138	390.503886	9.460237
7.652569	393.728891	9.465255
7.815637	403.883872	9.470272
7.940702	403.675296	9.475290
7.910556	397.129091	9.480307
7.912403	403.105845	9.485325
8.051410	405.018853	9.490343
7.915620	404.014643	9.495360
7.727731	397.906388	9.500378
8.066910	389.103194	9.505395
8.101679	404.462885	9.510413
7.813361	394.110137	9.515431
7.854397	395.435668	9.520448
7.585112	407.671273	9.525466
7.968597	404.339389	9.530483
7.750144	403.638370	9.535501
8.143562	404.874325	9.540519
7.967607	413.475869	9.545536
7.864365	403.097454	9.550554
8.078418	397.867003	9.555571
8.139633	399.340864	9.560589
8.034990	404.838762	9.565607
8.024764	402.170907	9.570624
7.661339	404.013826	9.575642
8.021982	400.502471	9.580659
7.933590	405.003808	9.585677
8.338892	403.262132	9.590695
8.060474	405.899663	9.595712
8.376090	409.290422	9.600730
8.072009	400.672577	9.605747
7.908430	400.597301	9.610765
8.140750	395.480765	9.615783
7.985190	406.370133	9.620800
7.867501	418.026747	9.625818
7.793244	406.687654	9.630835
7.733199	399.716935	9.635853
8.049242	406.537820	9.640871
8.101205	407.653378	9.645888
8.172181	406.964098	9.650906
8.217504	403.789001	9.655923
7.769936	406.749500	9.660941
7.746649	406.415706	9.665959
8.127290	395.485454	9.670976
7.852264	406.342932	9.675994
8.156917	403.152703	9.681011
7.790968	408.542971	9.686029
8.193324	412.049606	9.691047
8.362198	418.095029	9.696064
8.065713	415.074129	9.701082
8.498329	418.500319	9.706099
8.309756	401.972197	9.711117
8.088518	391.407044	9.716135
8.028287	405.595003	9.721152
8.145139	411.740037	9.726170
8.431717	417.697710	9.731187
8.057688	415.244279	9.736205
8.209293	411.677110	9.741223
8.551680	425.177578	9.746240
8.479660	419.865435	9.751258
8.270076	403.567790	9.756275
8.050966	408.894171	9.761293
8.104679	405.440070	9.766311
8.227897	406.781208	9.771328
8.376606	424.439427	9.776346
8.188600	420.278222	9.781363
8.482234	423.697651	9.786381
8.395350	424.323612	9.791399
8.228112	420.635678	9.796416
8.226741	431.977559	9.801434
8.530141	417.793214	9.806451
8.298597	416.267450	9.811469
8.447410	414.641444	9.816487
8.044613	406.285108	9.821504
8.257819	414.750325	9.826522
8.356398	421.008656	9.831539
8.435950	423.098173	9.836557
7.937241	420.537927	9.841575
8.258438	410.194406	9.846592
8.299751	429.396688	9.851610
8.543151	423.123448	9.856627
8.434500	417.135387	9.861645
8.371524	422.024072	9.866663
8.696081	419.749038	9.871680
8.718531	429.528315	9.876698
8.678174	429.042551	9.881715
8.490818	422.511347	9.886733
8.526770	418.574037	9.891751
8.610759	412.647498	9.896768
8.409228	419.892940	9.901786
8.572374	420.675622	9.906803
8.454356	420.132526	9.911821
7.922913	421.960583	9.916839
8.404883	420.333195	9.921856
8.416097	434.153464	9.926874
8.496043	433.525899	9.931891
8.853837	428.216257	9.936909
8.482367	422.357473	9.941927
8.631470	428.080945	9.946944
8.367505	421.744696	9.951962
8.604751	420.707651	9.956979
8.709288	425.551321	9.961997
8.766878	434.059711	9.967015
8.698118	416.869166	9.972032
8.286456	428.170789	9.977050
8.602795	423.684918	9.982067
8.521374	421.959064	9.987085
8.510189	431.926607	9.992103
8.642625	423.834051	9.997120
8.632169	435.559183	10.002138
8.867083	429.328286	10.007155
8.597291	425.858281	10.012173
8.457747	427.003657	10.017191
8.638770	424.823550	10.022208
8.358445	433.419264	10.027226
8.452322	431.505177	10.032243
8.522615	427.682434	10.037261
8.416390	424.985343	10.042279
8.623692	419.112183	10.047296
8.490029	428.641223	10.052314
8.315397	427.952314	10.057331
8.275611	427.182452	10.062349
8.711374	440.387541	10.067367
8.819380	452.223622	10.072384
8.958288	448.762559	10.077402
9.114375	436.018027	10.082419
8.723749	429.464823	10.087437
8.515369	427.045556	10.092455
8.472198	417.402516	10.097472
8.610943	429.268508	10.102490
8.807917	435.694553	10.107507
9.266192	444.383548	10.112525
8.665965	443.183416	10.117543
8.686539	437.853695	10.122560
8.958588	442.437771	10.127578
9.041299	438.209167	10.132595
8.896899	432.993492	10.137613
8.575718	427.499243	10.142631
8.764126	433.696258	10.147648
8.407809	438.466525	10.152666
9.016591	442.114588	10.157683
9.348245	454.793123	10.162701
8.940896	447.822812	10.167719
8.723091	428.462277	10.172736
8.905926	441.305978	10.177754
8.915690	431.449571	10.182771
9.085162	433.941636	10.187789
8.611898	425.924450	10.192807
8.787385	436.961100	10.197824
8.982514	437.432705	10.202842
9.161633	448.279457	10.207859
8.962211	446.161737	10.212877
8.974436	446.384122	10.217895
9.001142	442.508204	10.222912
9.063443	433.880634	10.227930
9.020678	435.638919	10.232947
8.938923	433.294607	10.237965
8.828543	436.335149	10.242983
8.927517	443.944048	10.248000
9.108718	449.555238	10.253018
8.905891	442.673000	10.258035
8.886717	446.115891	10.263053
9.115663	449.892519	10.268071
9.156623	446.225811	10.273088
9.135559	452.376554	10.278106
9.054830	454.408983	10.283123
9.279535	448.451056	10.288141
9.131398	432.061770	10.293159
9.160204	426.557210	10.298176
8.827502	430.175139	10.303194
8.890582	432.418693	10.308211
9.183109	443.197295	10.313229
8.967561	449.113242	10.318247
9.078292	449.497006	10.323264
9.488101	459.105540	10.328282
9.109613	452.919649	10.333299
9.203562	438.433398	10.338317
9.053581	441.164541	10.343335
8.883182	449.796794	10.348352
9.213993	454.731469	10.353370
9.350728	452.829641	10.358387
9.335875	448.916013	10.363405
9.122103	449.779472	10.368423
9.157939	449.717326	10.373440
9.357773	452.567567	10.378458
9.217624	447.635235	10.383475
9.167277	434.553633	10.388493
9.410901	449.480077	10.393511
9.041904	436.100963	10.398528
9.092966	444.594596	10.403546
9.119416	444.656982	10.408563
9.388426	441.175665	10.413581
9.150422	444.210834	10.418599
9.251946	439.433372	10.423616
9.081992	440.747578	10.428634
9.075257	443.743584	10.433651
9.740993	439.572521	10.438669
9.525364	444.579650	10.443687
9.462881	442.696218	10.448704
9.434011	444.739505	10.453722
9.221333	438.701364	10.458739
9.334689	441.337860	10.463757
8.994631	449.163434	10.468775
9.328552	444.879938	10.473792
9.310141	438.436027	10.478810
9.224871	454.051126	10.483827
9.419770	445.339792	10.488845
9.231578	451.409264	10.493863
8.984671	448.459531	10.498880
9.374565	449.247934	10.503898
9.283845	456.902152	10.508915
9.443013	439.496225	10.513933
9.337154	435.852378	10.518951
9.739854	443.391899	10.523968
9.541964	443.994119	10.528986
9.350675	445.542011	10.534003
9.388315	444.229943	10.539021
9.356674	454.386867	10.544039
9.233391	440.369918	10.549056
9.431009	450.437499	10.554074
9.300224	449.495621	10.559091
9.422009	438.488886	10.564109
9.178162	438.634380	10.569127
9.485299	446.340252	10.574144
9.717550	457.226073	10.579162
9.344371	454.781971	10.584179
9.394989	451.088512	10.589197
9.669489	466.417243	10.594215
9.828241	466.989182	10.599232
9.843110	454.853578	10.604250
9.433681	455.040631	10.609267
9.641681	440.915300	10.614285
9.767044	445.686309	10.619303
9.614747	444.687823	10.624320
9.690131	440.327822	10.629338
9.314530	437.155142	10.634355
9.285898	440.867736	10.639373
9.746325	458.329139	10.644391
9.910939	464.750765	10.649408
9.779654	455.591617	10.654426
9.531955	450.369930	10.659443
9.822791	441.599482	10.664461
9.333682	440.192710	10.669479
9.679943	452.165257	10.674496
10.047527	466.498085	10.679514
9.665729	454.929146	10.684531
9.693743	449.935919	10.689549
9.824061	453.797328	10.694567
9.834192	456.708663	10.699584
9.641813	438.789452	10.704602
9.291080	454.035646	10.709619
10.073244	455.548735	10.714637
10.110086	465.048092	10.719655
9.647244	466.401590	10.724672
9.645208	449.926427	10.729690
9.478044	455.730707	10.734707
9.684318	465.632854	10.739725
9.836941	469.462394	10.744743
9.817756	476.354434	10.749760
10.186896	457.786069	10.754778
10.436999	473.689780	10.759795
9.934243	458.640038	10.764813
9.938811	443.315670	10.769831
9.843032	448.442989	10.774848
9.877065	446.415147	10.779866
9.448017	449.407482	10.784883
9.934339	436.939721	10.789901
10.143158	441.536797	10.794919
9.726782	451.330763	10.799936
9.817575	446.801112	10.804954
9.891956	448.304484	10.809971
9.924915	453.995557	10.814989
10.203453	452.248368	10.820007
10.044873	455.457357	10.825024
9.951646	447.765982	10.830042
9.933942	451.697773	10.835059
9.935564	444.408179	10.840077
10.210503	441.929438	10.845095
10.009072	442.756262	10.850112
10.148409	447.225308	10.855130
9.978748	447.094177	10.860147
9.821906	445.755587	10.865165
10.015741	439.385922	10.870183
9.763832	434.010268	10.875200
10.235496	454.931676	10.880218
10.010553	458.419229	10.885235
10.020260	468.178422	10.890253
10.378786	464.837790	10.895271
9.893497	467.791549	10.900288
9.948597	449.776993	10.905306
10.089387	464.413361	10.910323
9.971262	465.154636	10.915341
10.241936	469.489635	10.920359
9.998341	475.561430	10.925376
10.237992	470.147099	10.930394
10.340541	470.607873	10.935411
10.322270	465.814344	10.940429
10.177734	467.083571	10.945447
10.201879	470.257801	10.950464
10.331682	466.148086	10.955482
9.961146	450.913670	10.960499
9.773053	464.929089	10.965517
10.197525	464.929505	10.970535
10.138278	472.862839	10.975552
10.488100	471.284422	10.980570
10.528940	474.717975	10.985587
10.165416	461.962812	10.990605
10.306076	459.713249	10.995623
10.303315	469.120949	11.000640
10.632402	471.506120	11.005658
9.989230	463.603730	11.010675
10.290166	467.640541	11.015693
10.390026	464.049861	11.020711
10.070858	470.385874	11.025728
10.075385	467.359122	11.030746
10.302030	471.669420	11.035763
10.254454	466.760538	11.040781
10.101668	472.957042	11.045799
9.913668	469.852973	11.050816
10.215159	473.422660	11.055834
10.376480	477.216135	11.060851
10.277875	462.062442	11.065869
10.371795	464.995445	11.070887
10.202608	469.916458	11.075904
10.182850	467.881210	11.080922
10.211010	462.168465	11.085939
10.583073	467.544826	11.090957
10.014468	461.817702	11.095975
10.409748	485.054673	11.100992
10.699705	482.759773	11.106010
11.012449	482.042314	11.111027
10.574039	481.463897	11.116045
10.575713	474.499316	11.121063
10.428997	478.627917	11.126080
10.853227	468.186273	11.131098
10.469661	472.796698	11.136115
10.421594	475.085963	11.141133
10.710280	468.688898	11.146151
10.449452	469.575461	11.151168
10.493035	471.380263	11.156186
10.432726	479.506261	11.161203
10.658441	474.747322	11.166221
10.538650	471.531651	11.171239
10.425192	469.154402	11.176256
10.234654	468.767756	11.181274
10.519757	484.968972	11.186291
10.740417	484.316341	11.191309
10.709843	483.339924	11.196327
10.557062	483.095716	11.201344
10.400230	485.808998	11.206362
10.563034	492.423412	11.211379
10.621536	498.896284	11.216397
10.901751	492.509996	11.221415
10.945230	501.594947	11.226432
10.962929	487.013235	11.231450
10.371402	490.908150	11.236467
10.823985	488.054620	11.241485
10.815368	481.956292	11.246503
10.755727	476.531756	11.251520
11.007099	483.681463	11.256538
10.725735	475.060045	11.261555
10.461359	469.111991	11.266573
10.819999	476.046186	11.271591
10.880780	492.105617	11.276608
10.808232	489.561057	11.281626
10.949184	481.157894	11.286643
10.576131	478.458160	11.291661
10.849670	484.137030	11.296679
11.150705	494.835447	11.301696
11.024858	486.158254	11.306714
10.945913	474.763046	11.311731
10.726065	480.061162	11.316749
10.883955	473.785440	11.321767
11.113972	475.210937	11.326784
11.161678	466.412062	11.331802
10.864876	471.949365	11.336819
11.077625	478.546531	11.341837
11.113319	474.268437	11.346855
10.647272	472.384722	11.351872
10.774392	470.213002	11.356890
11.035527	470.911006	11.361907
10.891530	468.099874	11.366925
11.111022	456.711858	11.371943
11.096022	467.020826	11.376960
10.763758	476.186355	11.381978
11.071304	471.506190	11.386995
10.370115	475.904148	11.392013
10.835109	477.589692	11.397031
11.125005	495.134484	11.402048
11.167500	487.971047	11.407066
11.279161	485.855378	11.412083
11.000682	482.822196	11.417101
10.748103	470.425278	11.422119
10.662734	485.595471	11.427136
11.255353	480.429125	11.432154
11.282744	484.827251	11.437171
11.004817	494.407189	11.442189
11.170289	481.326663	11.447207
11.564210	487.785176	11.452224
11.066808	486.240842	11.457242
11.358999	473.478248	11.462259
10.722632	477.465344	11.467277
11.239895	477.703766	11.472295
11.267162	496.065743	11.477312
11.145609	490.802314	11.482330
11.453766	491.328903	11.487347
11.325328	485.261852	11.492365
11.180482	480.932975	11.497383
10.781080	477.779772	11.502400
10.912334	488.129094	11.507418
11.217928	483.922580	11.512435
11.083921	487.064635	11.517453
11.049982	488.745815	11.522471
10.901318	492.268833	11.527488
10.873697	491.386627	11.532506
11.170380	487.856812	11.537523
10.640429	494.616954	11.542541
11.514266	506.753539	11.547559
11.378422	508.639927	11.552576
11.394347	516.252321	11.557594
11.521685	499.712789	11.562611
11.169560	506.164394	11.567629
11.541865	507.201681	11.572647
11.348030	508.907758	11.577664
11.329466	506.200162	11.582682
11.541932	500.076873	11.587699
11.523620	503.510174	11.592717
11.750103	501.288267	11.597735
11.464782	498.006850	11.602752
11.252563	498.759620	11.607770
11.706630	495.085384	11.612787
11.500300	501.208188	11.617805
11.645624	489.847477	11.622823
11.299501	498.008517	11.627840
11.238547	496.068039	11.632858
11.270171	492.213435	11.637875
11.383708	496.847450	11.642893
11.564403	500.044646	11.647911
11.642236	508.360579	11.652928
11.507008	505.156774	11.657946
11.455259	501.094251	11.662963
11.432218	506.481649	11.667981
11.593355	515.147517	11.672999
11.479841	513.950493	11.678016
11.837017	508.599899	11.683034
12.213972	508.699228	11.688051
11.902466	505.920482	11.693069
11.594116	495.545548	11.698087
11.710450	492.226841	11.703104
11.454356	490.288345	11.708122
11.686273	485.127667	11.713139
11.729456	491.590299	11.718157
11.765726	483.803011	11.723175
11.799229	481.548039	11.728192
11.798811	482.412993	11.733210
11.761472	479.320177	11.738227
11.793738	479.754027	11.743245
11.929872	482.487964	11.748263
11.501709	482.201429	11.753280
11.470450	478.306127	11.758298
11.783002	483.975768	11.763315
11.367503	487.723360	11.768333
11.773462	493.037648	11.773351
12.008158	508.252698	11.778368
11.611990	502.700676	11.783386
11.912809	501.401274	11.788403
11.740626	500.311211	11.793421
11.983784	496.458383	11.798439
12.062043	497.279531	11.803456
11.756068	491.584088	11.808474
11.687472	485.207931	11.813491
11.662374	497.067922	11.818509
11.470707	505.583597	11.823527
12.010400	505.329399	11.828544
11.794932	505.722928	11.833562
11.820236	505.722380	11.838579
11.864792	513.939360	11.843597
12.132029	514.652193	11.848615
11.933789	513.165416	11.853632
11.565375	511.257028	11.858650
12.062127	508.156788	11.863667
11.953299	512.806494	11.868685
11.929137	516.149194	11.873703
12.231086	515.165182	11.878720
11.907303	518.081181	11.883738
11.715426	510.727017	11.888755
11.797275	509.083027	11.893773
12.064124	514.857619	11.898791
12.251802	521.449237	11.903808
11.726706	524.497562	11.908826
11.983258	513.359350	11.913843
12.044158	518.894621	11.918861
11.695256	524.253868	11.923879
11.947521	516.975711	11.928896
12.368691	532.805505	11.933914
12.556623	527.317162	11.938931
12.111449	515.612890	11.943949
12.149605	522.057381	11.948967
12.247475	513.660911	11.953984
11.975301	505.732295	11.959002
12.277339	521.498581	11.964019
12.437379	525.500539	11.969037
12.228598	512.519283	11.974055
12.244509	512.444461	11.979072
12.239290	518.195146	11.984090
12.337237	503.215934	11.989107
12.351933	501.926368	11.994125
12.201730	505.096194	11.999143
12.307629	511.504889	12.004160
12.225910	513.158798	12.009178
12.324035	508.325045	12.014195
12.551112	514.989418	12.019213
12.144740	512.695636	12.024231
12.386875	505.318080	12.029248
12.325338	514.829625	12.034266
12.312472	517.656191	12.039283
12.438350	522.042149	12.044301
12.450965	530.058990	12.049319
12.531294	515.382301	12.054336
12.253266	513.800653	12.059354
12.525604	519.744799	12.064371
12.363340	517.674931	12.069389
12.375905	532.864629	12.074407
12.693811	531.041878	12.079424
12.411246	519.031431	12.084442
12.728652	523.996613	12.089459
12.684368	510.361768	12.094477
12.186449	514.775422	12.099495
12.733998	511.888169	12.104512
12.321769	508.878963	12.109530
12.560957	508.895604	12.114547
12.603161	510.243052	12.119565
12.837634	512.617715	12.124583
12.516254	501.938705	12.129600
12.352015	510.677321	12.134618
12.469146	507.052387	12.139635
12.734742	524.550501	12.144653
12.653739	521.555991	12.149671
12.400818	519.269874	12.154688
12.626483	526.401511	12.159706
12.774030	526.883682	12.164723
13.087530	529.160840	12.169741
12.602903	523.278616	12.174759
12.644956	505.423819	12.179776
12.352928	510.625890	12.184794
12.835596	521.551652	12.189811
12.908703	522.603968	12.194829
12.496560	521.993058	12.199847
12.942193	521.261219	12.204864
13.085265	530.052979	12.209882
12.728285	516.845495	12.214899
12.670967	503.988980	12.219917
12.711598	500.981847	12.224935
12.872621	502.803079	12.229952
12.561121	510.084613	12.234970
12.773067	524.293403	12.239987
12.828933	520.605425	12.245005
12.735652	528.023397	12.250023
13.107660	528.801966	12.255040
13.108189	527.344197	12.260058
12.966969	524.977575	12.265075
13.198096	514.969895	12.270093
12.583164	505.867090	12.275111
12.780354	511.652527	12.280128
12.670169	515.156936	12.285146
12.684827	525.732708	12.290163
12.755646	529.432992	12.295181
12.676831	530.635189	12.300199
12.858024	527.479939	12.305216
12.516620	529.628698	12.310234
12.728259	533.092471	12.315251
12.908084	517.671328	12.320269
12.825904	532.247797	12.325287
12.906363	523.525842	12.330304
12.907893	537.852607	12.335322
12.847405	543.337361	12.340339
13.358439	545.542742	12.345357
13.467867	547.037510	12.350375
13.557591	534.360042	12.355392
13.165038	526.500651	12.360410
12.756146	521.102077	12.365427
12.868653	516.865660	12.370445
12.702888	533.156052	12.375463
13.700892	534.872219	12.380480
13.629867	539.569693	12.385498
13.347979	533.488649	12.390515
13.155413	523.010468	12.395533
13.004120	532.217274	12.400551
13.087728	525.340898	12.405568
13.049161	524.274209	12.410586
13.326266	542.976018	12.415603
13.462617	546.561964	12.420621
13.094600	544.069711	12.425639
13.397491	542.274542	12.430656
13.438527	536.957384	12.435674
13.155400	533.142309	12.440691
13.272443	534.837854	12.445709
13.314708	548.924765	12.450727
13.189492	552.055997	12.455744
13.175800	542.174779	12.460762
13.568813	544.026165	12.465779
13.358746	538.113810	12.470797
13.158615	542.550531	12.475815
13.003797	545.519119	12.480832
13.643726	547.335217	12.485850
13.512780	546.708927	12.490867
13.694194	542.471242	12.495885
13.907652	542.084808	12.500903
13.621474	544.799304	12.505920
13.362050	531.939523	12.510938
13.152474	538.977991	12.515955
13.400254	528.456492	12.520973
13.428607	539.288905	12.525991
13.535043	542.696479	12.531008
13.819732	553.731978	12.536026
13.528436	554.250920	12.541043
13.995864	549.369123	12.546061
13.462532	547.019368	12.551079
13.502663	541.797020	12.556096
13.610130	548.928135	12.561114
13.482704	554.764127	12.566131
13.586326	549.011204	12.571149
13.250211	555.583406	12.576167
13.625626	545.266078	12.581184
13.671158	555.174368	12.586202
13.410868	558.194092	12.591219
13.384073	546.229008	12.596237
13.194863	548.969431	12.601255
13.755397	553.120471	12.606272
13.725707	551.875680	12.611290
13.318103	553.113291	12.616307
13.490071	549.978408	12.621325
13.616815	565.491169	12.626343
14.182642	563.560389	12.631360
13.672168	556.214787	12.636378
13.581716	564.616906	12.641395
13.879750	564.394021	12.646413
13.680125	565.674987	12.651431
13.725303	569.218331	12.656448
13.999544	570.715842	12.661466
13.952547	577.078941	12.666483
14.210613	567.205888	12.671501
13.958205	573.749285	12.676519
13.987537	559.263529	12.681536
14.167026	561.018779	12.686554
13.773283	553.822254	12.691571
13.999934	558.555434	12.696589
13.758121	560.196405	12.701607
13.901910	552.124113	12.706624
14.197709	559.585657	12.711642
13.726816	566.522816	12.716659
14.354504	559.820482	12.721677
14.036077	557.588738	12.726695
13.862603	559.291650	12.731712
14.342339	557.869717	12.736730
13.978230	553.344595	12.741747
13.961242	540.197763	12.746765
13.997739	555.317485	12.751783
14.128607	568.371332	12.756800
14.433798	560.264440	12.761818
13.783144	558.731337	12.766835
14.333927	553.240138	12.771853
14.241684	561.364834	12.776871
13.950156	556.560179	12.781888
14.084947	561.553805	12.786906
13.663061	557.492096	12.791923
14.062860	552.630295	12.796941
14.356342	563.654964	12.801959
14.026787	565.464225	12.806976
14.405702	561.221031	12.811994
14.163785	563.070294	12.817011
14.503622	554.683465	12.822029
14.176584	563.030904	12.827047
13.940132	569.811647	12.832064
14.522509	568.215949	12.837082
14.413723	567.633542	12.842099
13.915173	568.159507	12.847117
13.916042	559.162760	12.852135
14.163531	571.084496	12.857152
14.590476	564.656403	12.862170
14.196677	576.646432	12.867187
14.421178	561.675869	12.872205
14.279022	565.251535	12.877223
14.148007	571.621402	12.882240
14.196459	567.975592	12.887258
14.395350	588.579880	12.892275
14.473408	584.446637	12.897293
14.743769	592.849394	12.902311
14.797871	583.904304	12.907328
14.721616	566.055243	12.912346
14.827645	573.063520	12.917363
14.483638	569.911142	12.922381
14.350800	562.781285	12.927399
13.892722	573.235036	12.932416
14.346640	575.872175	12.937434
14.698885	582.962037	12.942451
14.687011	577.375404	12.947469
14.856388	587.996550	12.952487
14.496963	594.676532	12.957504
14.888681	585.833504	12.962522
14.755699	586.491893	12.967539
14.677116	574.799930	12.972557
14.761497	561.662545	12.977575
14.742930	569.463362	12.982592
14.419846	563.470769	12.987610
14.772709	579.828772	12.992627
14.744571	585.980663	12.997645
14.945717	585.359468	13.002663
14.629094	589.378854	13.007680
14.926806	585.085184	13.012698
14.987639	587.755125	13.017715
14.961851	585.777605	13.022733
14.645373	571.932638	13.027751
14.661897	571.703092	13.032768
14.812703	575.958954	13.037786
14.775658	601.210445	13.042803
14.862181	598.792575	13.047821
15.234210	585.392645	13.052839
15.169382	592.269747	13.057856
15.078156	567.496285	13.062874
14.735744	566.940786	13.067891
14.747338	567.141180	13.072909
14.723240	569.713893	13.077927
14.713400	584.064556	13.082944
14.900902	580.510698	13.087962
15.057696	590.792990	13.092979
15.211359	587.619927	13.097997
15.403590	583.396327	13.103015
15.311649	588.560956	13.108032
15.016919	576.653346	13.113050
15.181866	569.988342	13.118067
14.838963	570.199751	13.123085
15.105280	567.615042	13.128103
15.018499	589.462968	13.133120
15.447665	582.453876	13.138138
14.973967	575.493845	13.143155
15.141266	576.982761	13.148173
15.255071	579.369909	13.153191
15.103372	589.813836	13.158208
15.359996	589.900344	13.163226
15.005216	578.500680	13.168243
15.164714	584.661225	13.173261
15.261965	581.364407	13.178279
14.914593	588.585288	13.183296
15.235510	581.391087	13.188314
15.049858	585.585732	13.193331
15.112557	577.450318	13.198349
15.153774	572.413976	13.203367
15.197777	584.310602	13.208384
15.408750	586.326030	13.213402
15.222306	594.033079	13.218419
15.454764	594.227487	13.223437
15.306311	586.393177	13.228455
15.019131	587.034550	13.233472
15.300261	591.260658	13.238490
15.403839	585.810676	13.243507
15.200682	578.934748	13.248525
15.182890	583.254731	13.253543
15.307867	590.089657	13.258560
15.693912	602.882902	13.263578
15.628396	599.775518	13.268595
15.179661	596.895052	13.273613
15.595865	612.381721	13.278631
15.641781	623.025266	13.283648
15.525130	622.955304	13.288666
15.662708	614.230723	13.293683
15.898089	609.653273	13.298701
15.755280	595.459367	13.303719
15.534709	593.404880	13.308736
15.496376	591.012762	13.313754
15.617293	594.607433	13.318771
15.353251	600.625651	13.323789
15.770947	610.554920	13.328807
15.909207	622.329602	13.333824
15.720558	603.797439	13.338842
15.604446	604.579430	13.343859
15.611340	612.250073	13.348877
16.022608	618.320939	13.353895
15.679819	610.586301	13.358912
16.137841	611.023291	13.363930
16.064039	600.911566	13.368947
15.557011	600.381697	13.373965
15.777283	588.513811	13.378983
15.819425	599.631281	13.384000
15.794011	596.691217	13.389018
15.751457	592.453680	13.394035
15.753444	599.437142	13.399053
16.215363	610.725939	13.404071
16.136987	604.404909	13.409088
15.806441	595.115773	13.414106
15.809389	592.461617	13.419123
15.624751	602.771830	13.424141
15.978821	609.003071	13.429159
15.912247	618.941474	13.434176
16.138764	618.590873	13.439194
16.046708	610.694125	13.444211
15.796397	622.254761	13.449229
16.294008	619.813908	13.454247
16.087518	615.100133	13.459264
15.972215	609.977702	13.464282
16.140956	610.084204	13.469299
16.343067	617.607695	13.474317
16.190052	612.251302	13.479335
16.166447	609.336200	13.484352
15.847738	601.234913	13.489370
15.998545	604.632435	13.494387
16.111275	608.313587	13.499405
16.235131	611.175683	13.504423
16.059430	611.540934	13.509440
16.235778	612.507755	13.514458
16.236149	623.366666	13.519475
16.282537	624.707160	13.524493
16.542124	618.226212	13.529511
16.482544	616.534807	13.534528
16.548001	614.887048	13.539546
16.504898	592.027875	13.544563
16.217826	589.879604	13.549581
16.182500	586.401463	13.554599
15.769982	594.888453	13.559616
16.221899	601.533630	13.564634
16.232528	610.093596	13.569651
15.943813	608.873352	13.574669
16.226145	605.554024	13.579687
16.217814	612.384469	13.584704
16.076292	614.476872	13.589722
16.630281	616.943808	13.594739
16.045514	616.504933	13.599757
16.418642	602.195980	13.604775
16.355001	616.984219	13.609792
16.804480	630.865788	13.614810
16.869311	624.897982	13.619827
16.702155	616.315516	13.624845
16.307801	605.190230	13.629863
16.447797	620.779869	13.634880
16.251839	612.362830	13.639898
16.742024	621.132148	13.644915
16.791264	632.201199	13.649933
16.878265	630.758359	13.654951
16.571040	618.975738	13.659968
16.582366	614.998040	13.664986
16.904142	623.238177	13.670003
16.778377	621.033231	13.675021
16.716799	619.692418	13.680039
16.780335	613.529165	13.685056
16.691302	619.946159	13.690074
16.657776	607.511883	13.695091
16.562618	613.535368	13.700109
16.847300	632.523259	13.705127
16.925534	622.252157	13.710144
16.918665	634.731072	13.715162
17.275931	635.433049	13.720179
16.912149	625.741988	13.725197
16.480756	611.107024	13.730215
16.748963	614.391598	13.735232
16.683430	628.892974	13.740250
16.966191	630.717356	13.745267
17.240490	632.965918	13.750285
17.073108	629.978527	13.755303
17.049347	631.020685	13.760320
17.014103	627.807601	13.765338
17.429738	629.863750	13.770355
16.729337	619.786460	13.775373
17.072993	615.343624	13.780391
17.110083	617.275679	13.785408
16.845268	626.121525	13.790426
17.163840	624.052518	13.795443
17.066778	629.811226	13.800461
17.067285	633.326826	13.805479
17.361502	642.031994	13.810496
17.050165	642.544591	13.815514
17.296828	638.766924	13.820531
17.107078	637.865773	13.825549
17.237193	632.711436	13.830567
17.173121	633.788272	13.835584
17.009819	641.501205	13.840602
16.912683	628.975836	13.845619
17.346722	640.092273	13.850637
17.553671	642.228250	13.855655
17.304038	633.996277	13.860672
17.386300	634.318209	13.865690
17.463458	633.271363	13.870707
17.308622	640.127785	13.875725
17.400501	631.501826	13.880743
17.393741	630.903532	13.885760
17.250541	632.491288	13.890778
17.442405	631.792644	13.895795
17.199774	627.131829	13.900813
17.305021	629.706502	13.905831
17.333982	626.249901	13.910848
16.963857	626.244649	13.915866
17.191880	624.811411	13.920883
17.090031	627.714963	13.925901
17.048835	636.406082	13.930919
17.349105	643.721804	13.935936
17.206167	657.430552	13.940954
17.601873	653.481358	13.945971
17.678626	656.890420	13.950989
17.928972	656.678114	13.956007
17.971604	655.885944	13.961024
17.639041	652.555050	13.966042
17.614735	648.040112	13.971059
17.442368	663.596374	13.976077
17.458975	663.631893	13.981095
17.624038	654.593754	13.986112
17.635630	667.871366	13.991130
17.740918	657.719103	13.996147
17.856060	661.936359	14.001165
17.475583	653.914090	14.006183
18.030875	653.569102	14.011200
17.472463	660.207509	14.016218
17.722355	661.547878	14.021235
17.887539	658.483458	14.026253
18.108915	649.985645	14.031271
18.065787	649.465594	14.036288
18.291139	660.665028	14.041306
18.127272	658.576459	14.046323
18.003379	653.054579	14.051341
18.212416	648.017333	14.056359
18.107688	647.674125	14.061376
18.055507	648.973165	14.066394
17.982892	638.413125	14.071411
17.919755	637.833076	14.076429
18.017778	637.496170	14.081447
18.376701	639.387586	14.086464
17.933294	636.771362	14.091482
17.772451	634.423559	14.096499
17.954487	639.876893	14.101517
18.071444	648.824251	14.106535
18.286191	645.654290	14.111552
18.364605	647.882861	14.116570
18.180104	636.911068	14.121587
18.401824	635.440942	14.126605
18.177713	637.675590	14.131623
18.285409	630.637639	14.136640
18.032012	645.363931	14.141658
18.165040	644.671291	14.146675
18.322843	646.082799	14.151693
17.853793	645.673243	14.156711
18.216413	642.956768	14.161728
17.865754	648.597182	14.166746
18.164382	653.839871	14.171763
18.262217	654.307696	14.176781
18.259166	647.148130	14.181799
18.765648	639.192892	14.186816
18.403508	655.147910	14.191834
18.362050	656.647246	14.196851
18.379279	641.077748	14.201869
18.416105	643.325416	14.206887
18.461887	645.877793	14.211904
18.481760	648.595145	14.216922
18.569569	645.539618	14.221939
18.467269	651.270748	14.226957
18.070139	654.905065	14.231975
18.433352	649.502999	14.236992
18.178154	653.686398	14.242010
18.188243	647.679771	14.247027
18.605253	657.280981	14.252045
18.528239	668.164591	14.257063
18.719027	670.691239	14.262080
18.514126	678.656810	14.267098
18.918028	682.324200	14.272115
18.719656	666.728289	14.277133
18.648797	675.591298	14.282151
18.753943	667.651198	14.287168
18.627660	669.267880	14.292186
18.732182	671.792181	14.297203
18.637196	672.968503	14.302221
18.469693	671.937659	14.307239
18.580941	673.441622	14.312256
18.557187	673.180477	14.317274
18.528063	669.515167	14.322291
18.822271	663.884007	14.327309
18.809037	672.589724	14.332327
19.006750	670.697313	14.337344
18.650121	676.272396	14.342362
18.812654	676.155811	14.347379
19.033271	683.323009	14.352397
19.103792	692.122990	14.357415
19.370593	680.437140	14.362432
19.007997	682.298893	14.367450
19.047527	667.779903	14.372467
18.753112	663.805617	14.377485
18.977481	679.328524	14.382503
19.197015	680.733579	14.387520
19.298707	690.204025	14.392538
19.563590	686.212079	14.397555
19.167095	674.212953	14.402573
19.115057	679.724835	14.407591
19.020050	666.798333	14.412608
19.160093	670.724546	14.417626
19.041817	659.540463	14.422643
19.409880	661.802831	14.427661
18.712883	671.265081	14.432679
19.060189	678.175875	14.437696
19.335181	694.688115	14.442714
19.642950	700.516356	14.447731
19.472495	689.311977	14.452749
19.307660	695.800760	14.457767
19.819909	691.533620	14.462784
19.686597	680.629567	14.467802
18.924239	671.426557	14.472819
19.530223	676.870699	14.477837
19.568588	681.825725	14.482855
19.286595	671.225685	14.487872
19.484214	673.593485	14.492890
19.393208	682.671065	14.497907
19.553978	679.007745	14.502925
19.547362	681.763939	14.507943
19.692252	683.284754	14.512960
19.735628	676.502944	14.517978
19.579860	682.434907	14.522995
19.441503	669.404703	14.528013
19.328053	675.573063	14.533031
19.724225	683.129481	14.538048
19.589836	690.241506	14.543066
19.711750	690.131245	14.548083
19.994926	681.062080	14.553101
19.759846	677.583465	14.558119
19.740345	676.961908	14.563136
19.834276	673.877021	14.568154
19.420066	682.304358	14.573171
19.604078	684.453379	14.578189
19.428650	694.768523	14.583207
19.663973	693.529796	14.588224
19.604552	690.232105	14.593242
19.668747	688.108024	14.598259
19.751819	688.953678	14.603277
19.778827	691.976028	14.608295
19.798241	691.326322	14.613312
20.056926	682.586007	14.618330
19.701103	689.117146	14.623347
20.158873	683.002937	14.628365
20.227868	690.354687	14.633383
20.044926	693.191983	14.638400
20.157218	692.180688	14.643418
19.789253	692.134076	14.648435
20.028722	688.389075	14.653453
20.074042	688.009882	14.658471
20.036734	688.281005	14.663488
20.248730	695.118202	14.668506
20.000121	692.118202	14.673523
20.101991	688.590278	14.678541
20.015636	687.076599	14.683559
20.122228	693.179149	14.688576
20.168564	690.982111	14.693594
20.299981	705.730587	14.698611
20.600817	708.710307	14.703629
19.895394	701.366595	14.708647
20.387722	699.008602	14.713664
20.352912	706.928769	14.718682
20.158379	711.945311	14.723699
20.659191	706.550205	14.728717
20.742658	711.106909	14.733735
20.512428	702.641516	14.738752
20.568451	686.428485	14.743770
19.861606	686.860656	14.748787
20.346635	696.312446	14.753805
20.505495	700.971014	14.758823
20.682742	718.580903	14.763840
20.765154	713.888391	14.768858
20.184269	699.447038	14.773875
20.681058	698.240183	14.778893
20.208275	711.930904	14.783911
20.491142	715.052273	14.788928
20.707386	711.680101	14.793946
20.399700	717.954455	14.798963
20.734725	706.567226	14.803981
20.695665	721.272832	14.808999
20.726416	716.594675	14.814016
20.873727	715.846162	14.819034
20.864638	717.548740	14.824051
21.057190	705.192801	14.829069
20.822188	712.699185	14.834087
20.709342	712.944202	14.839104
20.732952	709.261206	14.844122
20.503557	710.912880	14.849139
20.597456	710.251576	14.854157
20.638562	713.369562	14.859175
20.561983	713.738316	14.864192
20.728439	710.493813	14.869210
20.681557	706.121227	14.874227
20.661916	702.135707	14.879245
20.518196	700.043997	14.884263
20.210811	718.149049	14.889280
20.992255	726.109389	14.894298
20.777743	731.002818	14.899315
20.853830	734.244746	14.904333
21.082247	739.318516	14.909351
21.110124	727.101808	14.914368
21.271056	725.688474	14.919386
20.850167	725.820511	14.924403
21.321889	731.026805	14.929421
21.264374	723.702124	14.934439
21.095250	730.623920	14.939456
21.502966	721.314444	14.944474
21.633795	729.312970	14.949491
21.388128	722.140657	14.954509
21.625257	740.870988	14.959527
21.307930	731.702795	14.964544
21.264659	728.468853	14.969562
21.278017	739.502533	14.974579
21.161667	731.107756	14.979597
21.389962	737.282887	14.984615
21.014471	739.638945	14.989632
21.451890	736.936056	14.994650
20.960278	731.484027	14.999667
21.135032	732.002992	15.004685
21.571241	733.652019	15.009703
21.177164	724.953357	15.014720
21.562933	731.675152	15.019738
21.416994	736.807208	15.024755
21.541687	730.069519	15.029773
21.533796	721.446427	15.034791
21.444091	721.274443	15.039808
21.625401	728.829621	15.044826
21.376544	723.109431	15.049843
21.833799	729.390919	15.054861
21.573292	722.321899	15.059879
21.338029	735.922010	15.064896
21.132220	737.768824	15.069914
21.404004	745.057466	15.074931
21.697055	739.388593	15.079949
22.127284	746.570518	15.084967
21.762249	741.726765	15.089984
22.145164	745.157601	15.095002
22.032823	749.747958	15.100019
22.017338	746.667472	15.105037
22.307101	749.506915	15.110055
22.344854	741.542563	15.115072
22.017334	726.395884	15.120090
21.726523	727.852000	15.125107
21.599430	724.012590	15.130125
21.843932	735.710847	15.135143
21.894094	743.223337	15.140160
22.211044	734.981994	15.145178
22.210847	749.334445	15.150195
22.245033	748.291128	15.155213
22.371553	741.543683	15.160231
21.953950	739.387316	15.165248
22.059315	736.799241	15.170266
21.959373	745.527961	15.175283
22.203791	748.393399	15.180301
22.367447	748.178811	15.185319
22.201178	749.388327	15.190336
22.161850	745.125005	15.195354
22.538092	755.688797	15.200371
21.902656	743.815186	15.205389
21.832665	735.937037	15.210407
22.199663	752.984101	15.215424
22.101607	740.578713	15.220442
22.178312	749.873206	15.225459
22.586534	755.632178	15.230477
22.278519	746.484617	15.235495
22.384347	743.186434	15.240512
22.287235	744.110635	15.245530
22.164980	761.028759	15.250547
22.148087	742.545447	15.255565
22.503814	746.984034	15.260583
21.927705	755.345096	15.265600
22.805057	766.544066	15.270618
22.914637	776.745456	15.275635
22.624582	760.396898	15.280653
22.636947	748.125787	15.285671
22.516520	747.242239	15.290688
22.799070	749.505310	15.295706
22.485230	754.578307	15.300723
22.867352	750.167317	15.305741
22.562138	745.276380	15.310759
22.513439	760.400074	15.315776
22.832015	770.127121	15.320794
22.968542	771.873302	15.325811
22.955605	767.769963	15.330829
23.029559	761.775444	15.335847
22.840574	752.047631	15.340864
22.732256	752.020551	15.345882
23.099147	758.997754	15.350899
22.873901	757.489914	15.355917
22.729869	758.377241	15.360935
22.641161	771.642145	15.365952
23.087015	768.366754	15.370970
22.818893	763.665692	15.375987
23.077231	768.270921	15.381005
23.286328	765.051327	15.386023
23.099065	773.740009	15.391040
23.560690	767.003495	15.396058
23.438992	771.873017	15.401075
22.927842	759.191115	15.406093
23.087472	755.026198	15.411111
23.127777	773.894503	15.416128
23.214893	778.870367	15.421146
23.332453	776.756902	15.426163
23.340717	770.545396	15.431181
23.600333	772.168274	15.436199
23.395426	762.988873	15.441216
22.882255	750.490324	15.446234
23.206156	755.142145	15.451251
23.119195	776.488570	15.456269
23.357322	769.433412	15.461287
23.105740	770.444779	15.466304
23.086937	770.785605	15.471322
23.139145	766.059913	15.476339
23.258535	769.503383	15.481357
23.363877	765.249089	15.486375
23.627567	769.869264	15.491392
23.501099	772.063480	15.496410
23.791157	777.960774	15.501427
23.672244	772.330787	15.506445
23.614902	769.158986	15.511463
23.754710	769.276306	15.516480
23.383410	772.455357	15.521498
23.267400	770.665429	15.526515
23.577255	768.903866	15.531533
23.825237	767.432796	15.536551
23.719240	776.910380	15.541568
23.686654	778.023346	15.546586
23.948482	794.941662	15.551603
23.939104	783.718456	15.556621
23.739851	773.304282	15.561639
23.832558	781.460242	15.566656
23.685473	773.663505	15.571674
23.940696	780.001712	15.576691
23.848965	792.238338	15.581709
24.181457	782.069564	15.586727
23.921778	794.985574	15.591744
24.043053	793.587877	15.596762
24.136178	784.832265	15.601779
23.537117	796.649278	15.606797
23.898056	779.953198	15.611815
23.683308	795.386789	15.616832
23.762281	789.858527	15.621850
23.979646	790.036353	15.626867
23.931952	796.503778	15.631885
23.654079	790.510381	15.636903
24.201810	792.675367	15.641920
24.115358	791.568782	15.646938
24.124648	801.520721	15.651955
24.119384	811.648497	15.656973
24.382421	810.932453	15.661991
24.625301	805.735263	15.667008
24.287062	803.875792	15.672026
24.635502	802.534242	15.677043
24.296746	805.995403	15.682061
24.518006	799.242653	15.687079
24.309950	800.004254	15.692096
24.455807	798.953015	15.697114
24.685343	802.868479	15.702131
24.484746	812.502817	15.707149
24.351031	795.110586	15.712167
24.692457	803.082667	15.717184
24.392252	809.602035	15.722202
25.118914	806.488038	15.727219
24.543155	804.488828	15.732237
24.607992	791.868699	15.737255
24.714724	809.054166	15.742272
24.576186	807.952533	15.747290
24.724341	810.665716	15.752307
24.774317	815.549545	15.757325
24.743607	809.268357	15.762343
25.095821	816.456145	15.767360
24.411732	805.208590	15.772378
24.960871	806.704346	15.777395
24.599231	820.781777	15.782413
24.816095	814.676630	15.787431
24.843878	810.790998	15.792448
24.814233	816.097468	15.797466
24.969894	806.155023	15.802483
24.826337	809.734112	15.807501
24.816922	800.940810	15.812519
25.067312	816.305155	15.817536
24.812223	811.895533	15.822554
24.860217	805.311765	15.827571
24.728007	803.126734	15.832589
25.091406	801.662937	15.837607
24.722945	803.446722	15.842624
25.048703	814.034188	15.847642
25.401592	817.731639	15.852659
25.575840	825.701358	15.857677
25.670996	808.169340	15.862695
25.264022	807.459788	15.867712
24.985221	813.177426	15.872730
25.195151	805.082098	15.877747
25.208947	807.951896	15.882765
24.754120	812.715510	15.887783
25.585038	814.997349	15.892800
25.451110	824.394102	15.897818
25.529184	818.307407	15.902835
25.307446	828.639306	15.907853
25.703826	829.802249	15.912871
25.535912	828.080355	15.917888
25.392159	830.548662	15.922906
25.607801	827.533160	15.927923
25.320127	832.349647	15.932941
25.560341	827.771389	15.937959
25.885072	829.485117	15.942976
25.538014	829.826560	15.947994
25.751910	817.871154	15.953011
25.744953	828.598791	15.958029
25.654929	825.845469	15.963047
25.539150	821.448868	15.968064
25.629534	819.248112	15.973082
25.723532	816.251551	15.978099
25.689006	822.959927	15.983117
25.475473	828.241384	15.988135
25.969466	826.009345	15.993152
25.847047	830.389858	15.998170
25.463878	821.721007	16.003187
25.595338	828.889524	16.008205
26.217640	833.242447	16.013223
26.194779	834.410707	16.018240
25.495459	832.399173	16.023258
25.496077	842.551297	16.028275
26.126724	839.430153	16.033293
25.935780	846.472153	16.038311
26.299481	851.695302	16.043328
26.330659	850.239046	16.048346
26.563422	836.772250	16.053363
26.182838	839.864398	16.058381
26.445781	837.198127	16.063399
26.250618	844.963445	16.068416
26.489118	850.887725	16.073434
26.399527	841.267460	16.078451
26.076761	848.535107	16.083469
25.999354	847.341905	16.088487
26.765510	840.267622	16.093504
26.369813	849.149735	16.098522
26.499767	840.899590	16.103539
26.211016	841.437077	16.108557
26.165751	838.115065	16.113575
26.448417	842.729149	16.118592
26.320759	841.726804	16.123610
26.808376	835.317569	16.128627
26.667311	848.268797	16.133645
26.448425	848.180039	16.138663
26.801999	840.223274	16.143680
26.614973	845.002004	16.148698
26.684440	841.984012	16.153715
26.814093	846.767084	16.158733
26.483286	846.752555	16.163751
26.440427	847.835568	16.168768
26.487992	853.041668	16.173786
26.182400	860.685334	16.178803
26.499944	856.413758	16.183821
26.859237	862.524357	16.188839
26.821009	867.847958	16.193856
26.916706	877.527717	16.198874
27.095737	868.004467	16.203891
26.803337	878.839692	16.208909
27.012244	869.791462	16.213927
27.319069	862.097580	16.218944
26.794071	869.160041	16.223962
27.114728	869.596336	16.228979
27.028579	873.453671	16.233997
26.910186	870.423899	16.239015
27.089532	872.273874	16.244032
26.855636	870.268765	16.249050
27.027767	859.111924	16.254067
27.208838	863.082283	16.259085
27.279968	868.956890	16.264103
27.231435	865.739520	16.269120
27.193474	866.029683	16.274138
27.131896	867.683644	16.279155
27.342494	862.327366	16.284173
27.353926	863.925779	16.289191
27.634675	859.729357	16.294208
27.238942	876.396687	16.299226
27.309800	866.095035	16.304243
27.284610	863.347392	16.309261
27.360833	876.182760	16.314279
27.798111	886.863357	16.319296
27.898853	879.381431	16.324314
27.246839	865.910361	16.329331
28.111851	870.541078	16.334349
27.653378	867.150854	16.339367
27.543608	859.092656	16.344384
27.159109	877.083646	16.349402
27.444602	877.973530	16.354419
27.914023	880.526252	16.359437
27.815589	884.947224	16.364455
27.812801	881.119983	16.369472
27.623037	878.726158	16.374490
28.020377	886.979900	16.379507
28.039453	879.718967	16.384525
28.325413	888.681158	16.389543
28.525856	877.917520	16.394560
28.081278	885.743778	16.399578
27.755090	864.487265	16.404595
27.880403	866.377210	16.409613
28.043417	879.028658	16.414631
28.379779	880.851032	16.419648
28.010063	881.918667	16.424666
28.070464	882.887777	16.429683
27.870239	875.695704	16.434701
28.139731	884.370128	16.439719
28.437329	877.558127	16.444736
28.468022	884.571945	16.449754
28.494179	885.442248	16.454771
28.414669	883.520395	16.459789
28.012644	881.904372	16.464807
28.270700	879.800577	16.469824
28.523876	887.243650	16.474842
28.361836	885.984729	16.479859
28.383746	885.703848	16.484877
27.916926	893.861770	16.489895
28.412077	880.751711	16.494912
28.137548	886.061617	16.499930
28.244620	890.785102	16.504947
28.522726	880.732035	16.509965
28.341868	889.460801	16.514983
28.477428	882.431035	16.520000
28.287963	895.301472	16.525018
28.427370	900.083041	16.530035
28.979178	900.975642	16.535053
28.857632	910.253750	16.540071
28.967655	914.645429	16.545088
28.967891	909.056806	16.550106
28.615708	894.131570	16.555123
28.668021	897.345672	16.560141
28.772240	904.130304	16.565159
28.917649	900.980560	16.570176
29.094180	908.249387	16.575194
29.373943	902.172285	16.580211
29.226802	887.619066	16.585229
28.680282	885.419637	16.590247
28.992717	885.800409	16.595264
28.937933	898.299592	16.600282
28.741697	895.774231	16.605299
28.944716	900.220854	16.610317
29.217460	905.180475	16.615335
29.286297	895.279900	16.620352
29.156925	903.704017	16.625370
28.979082	909.617402	16.630387
29.272967	900.587483	16.635405
29.271603	905.485642	16.640423
29.210364	901.746392	16.645440
29.324435	912.190153	16.650458
29.152301	909.900874	16.655475
29.452168	905.411136	16.660493
29.089501	910.810510	16.665511
29.263238	899.874295	16.670528
29.239184	902.355533	16.675546
29.153156	904.253140	16.680563
29.480634	913.559167	16.685581
29.345637	922.088308	16.690599
29.297035	929.082932	16.695616
29.598149	925.959433	16.700634
29.640363	940.368549	16.705651
29.731399	926.579774	16.710669
29.765508	926.334863	16.715687
29.668861	926.321744	16.720704
29.914677	926.624528	16.725722
29.129321	926.261055	16.730739
29.409127	922.885259	16.735757
29.479757	931.688497	16.740775
29.664906	940.155178	16.745792
30.070139	949.777315	16.750810
30.094268	956.631240	16.755827
30.124865	949.049755	16.760845
29.961174	959.022403	16.765863
30.114690	959.809765	16.770880
30.473820	958.113095	16.775898
30.539268	941.273526	16.780915
30.629707	918.819167	16.785933
29.949764	929.250866	16.790951
30.336484	918.029019	16.795968
30.525696	913.868927	16.800986
30.353128	910.516229	16.806003
30.141265	918.022252	16.811021
30.256718	920.131485	16.816039
30.333318	922.568652	16.821056
30.257107	921.337390	16.826074
30.007863	922.585082	16.831091
30.148950	927.438979	16.836109
30.123720	920.696158	16.841127
30.036596	932.073800	16.846144
30.344603	947.959454	16.851162
30.127723	951.139740	16.856179
30.122716	946.605942	16.861197
30.294452	949.533221	16.866215
30.432606	954.037293	16.871232
30.686582	953.240606	16.876250
31.009021	950.767023	16.881267
30.885750	952.559983	16.886285
30.553463	954.849381	16.891303
30.591087	943.501994	16.896320
30.398917	950.632586	16.901338
30.710155	951.483752	16.906355
30.969091	960.058874	16.911373
31.022569	970.158659	16.916391
30.946299	960.469986	16.921408
31.356574	950.582490	16.926426
30.701445	945.891143	16.931443
31.265524	943.474611	16.936461
30.952497	943.895962	16.941479
30.806509	943.754828	16.946496
30.956869	953.211526	16.951514
31.194940	958.719350	16.956531
31.146416	961.056086	16.961549
31.416600	963.854432	16.966567
30.969733	962.743992	16.971584
31.291897	964.893627	16.976602
31.157637	968.730072	16.981619
31.169849	965.768310	16.986637
31.312266	970.107623	16.991655
31.403478	960.468611	16.996672
31.484710	962.646292	17.001690
31.476958	971.531179	17.006707
31.466157	962.939981	17.011725
31.547757	967.594870	17.016743
31.172584	965.633837	17.021760
31.120516	969.485887	17.026778
31.100274	968.842345	17.031795
31.436970	966.577975	17.036813
31.431973	972.098402	17.041831
31.128764	968.958535	17.046848
31.618304	973.729789	17.051866
31.885743	989.306221	17.056883
32.082029	985.362757	17.061901
31.977561	989.630062	17.066919
31.816480	991.593013	17.071936
32.128690	991.361605	17.076954
32.083376	984.921685	17.081971
31.519706	964.276374	17.086989
31.638183	974.700552	17.092007
31.933021	985.633756	17.097024
31.828421	984.807691	17.102042
31.950884	985.757677	17.107059
32.220632	994.574124	17.112077
32.512855	987.592508	17.117095
32.467462	990.739789	17.122112
32.842872	970.853963	17.127130
32.367280	962.455049	17.132147
31.802870	960.652865	17.137165
31.905746	972.483781	17.142183
32.286463	977.562309	17.147200
32.365181	971.264026	17.152218
32.066938	988.411735	17.157235
32.084223	990.949664	17.162253
32.235875	989.894355	17.167271
32.134382	979.638407	17.172288
32.114232	980.739982	17.177306
32.340415	981.733779	17.182323
32.677699	978.083940	17.187341
32.666059	978.455211	17.192359
32.508524	979.328873	17.197376
32.565046	973.911344	17.202394
32.135270	991.126872	17.207411
32.337909	995.911244	17.212429
32.754641	995.407946	17.217447
32.414534	1002.615240	17.222464
32.597259	1005.644957	17.227482
32.697384	1003.688812	17.232499
32.736506	1012.067812	17.237517
32.941047	1007.046943	17.242535
32.847369	1005.808928	17.247552
32.936839	1006.943930	17.252570
32.607350	1012.634810	17.257587
32.870808	1014.313917	17.262605
32.975851	1010.236333	17.267623
32.556497	1014.110864	17.272640
33.073724	1010.455092	17.277658
33.720573	1021.702736	17.282675
33.433156	1017.623140	17.287693
33.667171	1007.242355	17.292711
33.406544	998.882538	17.297728
33.619402	997.379049	17.302746
33.291785	995.893439	17.307763
33.393882	998.137301	17.312781
33.671324	985.783730	17.317799
33.109863	1006.582625	17.322816
33.611762	995.645750	17.327834
33.521460	997.515631	17.332851
33.272209	990.839221	17.337869
33.518963	995.490494	17.342887
33.327907	992.241644	17.347904
33.333575	991.865462	17.352922
33.524481	997.396420	17.357939
33.388649	995.372873	17.362957
33.780262	999.670239	17.367975
33.878972	1007.402496	17.372992
33.936749	1004.834414	17.378010
33.794049	1005.828842	17.383027
33.805877	1000.847448	17.388045
33.940423	994.139683	17.393063
33.741109	1004.619669	17.398080
34.020725	1008.921851	17.403098
34.010375	1012.502331	17.408115
34.107198	1016.078748	17.413133
34.301496	1007.755393	17.418151
33.912382	996.799456	17.423168
34.159949	997.253445	17.428186
33.671419	1003.152118	17.433203
34.196970	1009.003356	17.438221
34.191768	1001.215987	17.443239
33.911585	1014.390965	17.448256
34.303229	1004.695686	17.453274
34.080662	1009.808192	17.458291
34.027012	1011.893272	17.463309
34.363536	1007.625016	17.468327
34.433835	1009.378377	17.473344
34.214145	1002.949820	17.478362
34.257581	1007.200413	17.483379
33.919309	1000.231751	17.488397
34.529545	1015.262535	17.493415
34.181121	1025.380746	17.498432
34.461531	1021.237987	17.503450
34.420683	1033.514192	17.508467
34.558332	1041.391878	17.513485
34.526213	1033.851679	17.518503
34.601232	1026.809192	17.523520
34.721445	1032.048214	17.528538
34.479134	1027.349374	17.533555
34.563003	1030.899409	17.538573
34.796074	1027.767552	17.543591
34.755346	1028.228559	17.548608
34.868810	1025.746478	17.553626
34.902429	1045.774277	17.558643
34.909259	1054.218284	17.563661
35.187819	1046.276263	17.568679
34.876113	1054.974989	17.573696
34.832240	1051.008944	17.578714
35.296943	1052.956519	17.583731
35.166264	1061.844812	17.588749
35.306462	1051.336599	17.593767
35.132034	1059.411203	17.598784
35.245707	1052.223833	17.603802
35.236657	1050.202631	17.608819
34.633660	1050.751181	17.613837
35.265704	1045.534355	17.618855
35.426393	1058.776422	17.623872
35.259156	1058.256748	17.628890
35.368993	1058.097873	17.633907
35.061002	1056.151615	17.638925
35.476177	1054.058051	17.643943
35.296517	1063.380000	17.648960
35.535838	1072.185445	17.653978
35.742467	1069.638359	17.658995
35.538194	1075.243492	17.664013
36.065069	1073.527006	17.669031
35.879577	1077.579732	17.674048
35.859199	1069.062556	17.679066
36.047315	1060.673867	17.684083
35.847708	1056.302882	17.689101
35.535452	1055.382914	17.694119
35.867601	1060.298616	17.699136
35.944171	1074.374292	17.704154
36.367984	1084.586894	17.709171
35.820050	1079.604269	17.714189
36.260621	1077.733963	17.719207
35.934213	1085.396745	17.724224
36.227402	1081.422394	17.729242
36.274714	1079.423970	17.734259
36.066280	1082.845959	17.739277
36.135044	1074.166580	17.744295
36.046142	1086.522887	17.749312
36.250103	1085.670865	17.754330
36.614660	1072.713541	17.759347
36.256669	1081.381618	17.764365
36.461071	1078.146919	17.769383
36.548276	1069.666641	17.774400
36.547932	1077.240783	17.779418
36.304741	1079.229150	17.784435
36.427793	1083.722984	17.789453
36.591674	1077.935262	17.794471
36.417895	1075.065555	17.799488
36.562463	1077.252323	17.804506
36.939495	1071.712280	17.809523
36.449435	1075.083442	17.814541
36.847660	1073.456413	17.819559
36.538732	1069.522163	17.824576
36.788428	1062.509269	17.829594
36.672340	1072.436700	17.834611
37.224151	1086.230111	17.839629
36.988212	1079.497947	17.844647
36.774318	1071.332788	17.849664
36.989018	1086.942763	17.854682
37.194134	1085.282684	17.859699
37.204441	1087.417774	17.864717
37.225119	1079.310763	17.869735
37.063139	1076.634877	17.874752
37.200873	1090.562188	17.879770
37.303971	1082.234063	17.884787
37.080211	1086.084467	17.889805
37.583138	1084.043508	17.894823
37.453506	1082.688010	17.899840
37.636259	1085.673556	17.904858
37.717334	1069.948576	17.909875
37.326767	1071.316110	17.914893
37.363681	1070.606862	17.919911
37.660669	1055.394226	17.924928
37.441793	1060.408344	17.929946
37.642111	1056.770347	17.934963
37.236313	1072.735691	17.939981
37.436870	1078.265171	17.944999
37.756079	1079.487484	17.950016
37.412861	1088.399415	17.955034
37.576011	1080.001981	17.960051
37.438094	1086.215317	17.965069
37.518759	1088.673965	17.970087
37.769657	1079.688518	17.975104
37.727601	1080.875561	17.980122
37.760720	1090.328496	17.985139
37.449310	1102.716301	17.990157
37.870119	1095.149738	17.995175
38.142025	1100.522951	18.000192
37.946700	1109.661172	18.005210
37.931054	1100.897094	18.010227
37.693728	1103.155947	18.015245
38.220884	1096.816202	18.020263
37.836737	1102.487218	18.025280
38.044564	1100.552163	18.030298
38.341939	1108.790015	18.035315
38.427508	1126.304129	18.040333
38.224921	1129.816734	18.045351
38.598779	1121.844062	18.050368
38.586210	1123.001270	18.055386
38.924879	1115.744131	18.060403
38.403259	1115.563651	18.065421
38.247266	1114.628817	18.070439
38.327984	1123.626237	18.075456
38.397387	1124.388834	18.080474
38.700499	1130.154826	18.085491
38.679745	1126.462873	18.090509
38.829525	1125.089114	18.095527
38.840425	1120.035248	18.100544
38.850059	1120.942848	18.105562
38.930984	1113.022100	18.110579
38.921636	1118.240295	18.115597
38.866777	1121.455345	18.120615
39.161447	1120.100053	18.125632
39.015129	1118.463129	18.130650
39.362712	1107.739559	18.135667
38.907465	1116.495378	18.140685
39.238183	1116.567198	18.145703
39.267419	1117.926178	18.150720
39.042232	1114.979263	18.155738
39.603802	1107.766316	18.160755
39.163289	1122.206557	18.165773
39.372971	1116.133983	18.170791
39.557981	1110.535464	18.175808
39.592359	1112.325985	18.180826
39.482478	1111.122042	18.185843
39.589614	1109.511929	18.190861
39.435522	1104.344902	18.195879
39.810274	1106.590508	18.200896
39.553009	1112.068205	18.205914
39.735917	1100.597112	18.210931
39.346958	1105.385261	18.215949
39.427071	1109.377706	18.220967
40.025241	1124.139065	18.225984
39.647920	1132.014919	18.231002
39.561674	1127.695694	18.236019
40.136981	1133.952635	18.241037
39.847955	1134.360786	18.246055
39.966493	1137.381585	18.251072
39.978344	1137.499895	18.256090
39.959937	1135.972442	18.261107
39.842673	1136.243398	18.266125
39.473353	1136.263265	18.271143
39.771547	1130.221087	18.276160
40.147233	1129.313925	18.281178
40.018332	1137.425656	18.286195
40.228364	1141.158041	18.291213
40.368001	1149.783386	18.296231
40.368221	1146.369028	18.301248
40.528068	1154.871309	18.306266
40.512756	1149.941435	18.311283
40.458305	1140.978253	18.316301
40.469256	1154.041734	18.321319
40.590304	1150.116260	18.326336
40.514294	1158.762562	18.331354
40.882322	1153.239675	18.336371
40.977260	1151.375838	18.341389
40.971634	1142.935225	18.346407
40.850077	1127.355351	18.351424
40.579261	1130.351564	18.356442
40.782714	1124.308359	18.361459
40.858552	1129.563786	18.366477
40.964982	1145.228539	18.371495
41.292743	1142.646805	18.376512
40.903570	1132.422935	18.381530
40.808141	1133.394230	18.386547
40.894278	1146.559608	18.391565
40.810861	1148.157036	18.396583
41.035235	1150.214623	18.401600
41.044951	1153.959264	18.406618
41.151661	1152.131464	18.411635
41.006710	1135.539063	18.416653
40.822060	1158.690485	18.421671
40.979242	1149.801644	18.426688
41.416743	1161.810959	18.431706
41.434462	1165.841533	18.436723
41.929084	1157.067407	18.441741
41.441435	1154.735703	18.446759
41.648495	1156.698157	18.451776
41.603745	1165.415334	18.456794
41.482818	1167.438323	18.461811
41.517910	1157.299861	18.466829
41.757205	1162.526693	18.471847
41.835391	1167.589263	18.476864
42.059542	1170.309603	18.481882
41.694736	1166.652274	18.486899
41.985335	1158.443241	18.491917
41.811594	1165.561583	18.496935
42.114778	1162.835350	18.501952
42.229682	1168.412909	18.506970
41.982810	1160.385387	18.511987
42.261662	1162.810032	18.517005
41.764270	1171.818592	18.522023
41.975862	1157.430203	18.527040
42.171547	1162.209391	18.532058
42.340855	1164.225061	18.537075
42.422069	1163.445796	18.542093
42.156805	1165.623801	18.547111
42.458992	1156.103313	18.552128
42.197493	1171.755947	18.557146
42.176033	1161.544236	18.562163
41.934241	1165.864522	18.567181
42.232835	1178.536100	18.572199
42.327177	1178.509024	18.577216
42.643621	1185.917126	18.582234
42.679337	1179.461363	18.587251
42.460884	1184.260856	18.592269
42.440316	1192.841737	18.597287
42.794031	1175.224921	18.602304
42.550332	1180.571139	18.607322
42.650729	1181.508792	18.612339
42.557170	1186.456097	18.617357
42.622390	1201.158487	18.622375
43.492685	1205.428712	18.627392
43.191977	1202.181116	18.632410
42.989196	1186.781094	18.637427
43.304446	1179.647495	18.642445
43.082134	1188.518560	18.647463
43.382033	1183.362876	18.652480
43.357777	1183.243812	18.657498
43.010159	1182.073723	18.662515
43.730741	1184.606321	18.667533
43.098626	1187.393709	18.672551
43.318571	1186.526571	18.677568
43.641622	1197.872078	18.682586
43.272322	1203.626021	18.687603
43.740188	1192.640677	18.692621
43.733811	1209.493849	18.697639
43.722552	1200.530223	18.702656
43.712278	1198.382962	18.707674
43.883655	1193.263064	18.712691
44.081797	1194.419028	18.717709
43.993051	1195.739580	18.722727
43.831018	1186.083071	18.727744
43.939278	1182.658196	18.732762
43.915868	1190.491597	18.737779
43.970192	1190.120458	18.742797
43.688624	1194.248129	18.747815
43.895818	1189.946318	18.752832
43.776239	1192.698088	18.757850
43.555252	1200.634838	18.762867
43.927548	1193.445015	18.767885
43.791598	1203.432416	18.772903
44.464021	1210.330669	18.777920
44.213707	1207.037357	18.782938
44.335195	1215.097516	18.787955
44.548244	1215.377005	18.792973
44.661795	1218.947703	18.797991
44.426025	1221.080097	18.803008
44.412218	1219.996888	18.808026
44.151149	1212.706854	18.813043
44.699852	1219.251989	18.818061
44.130934	1220.394839	18.823079
44.575626	1211.177182	18.828096
44.879310	1219.676035	18.833114
44.457118	1216.743996	18.838131
44.539168	1216.652562	18.843149
44.803175	1229.910228	18.848167
45.136280	1236.586767	18.853184
45.067637	1238.642650	18.858202
45.356154	1241.466588	18.863219
45.403148	1224.673805	18.868237
45.220425	1221.884362	18.873255
44.881474	1207.016762	18.878272
44.930318	1221.677538	18.883290
45.411567	1223.805593	18.888307
45.491279	1228.176823	18.893325
45.612752	1233.267386	18.898343
45.426674	1224.968438	18.903360
45.666800	1210.537694	18.908378
45.383324	1215.262112	18.913395
45.229329	1212.035853	18.918413
45.458588	1224.270136	18.923431
45.538387	1230.395977	18.928448
45.939178	1232.246226	18.933466
45.550931	1239.871365	18.938483
46.046544	1228.278920	18.943501
45.835105	1232.117970	18.948519
45.853748	1232.585518	18.953536
45.880840	1233.733403	18.958554
46.034957	1233.984198	18.963571
45.596414	1215.304111	18.968589
45.809956	1236.680041	18.973607
45.934884	1231.002475	18.978624
46.184343	1228.988341	18.983642
46.001997	1232.516749	18.988659
46.058299	1229.260901	18.993677
45.731021	1237.346760	18.998695
45.794238	1241.483876	19.003712
45.588080	1238.404589	19.008730
45.819997	1252.181664	19.013747
46.078954	1257.752601	19.018765
46.143219	1254.646987	19.023783
46.449392	1249.600760	19.028800
46.304342	1242.630321	19.033818
46.199612	1255.765536	19.038835
46.513738	1260.964968	19.043853
46.919673	1278.467222	19.048871
46.813843	1264.222843	19.053888
46.976705	1265.633613	19.058906
46.818358	1265.750021	19.063923
46.906968	1261.113206	19.068941
46.753276	1256.208003	19.073959
47.226954	1262.338802	19.078976
47.323866	1264.678180	19.083994
46.956598	1257.994798	19.089011
47.030833	1264.317177	19.094029
46.944512	1267.429854	19.099047
47.266180	1268.478228	19.104064
47.678214	1268.641530	19.109082
47.405872	1273.600916	19.114099
47.786400	1258.321452	19.119117
47.188023	1254.271280	19.124135
47.170370	1256.808376	19.129152
47.334721	1258.244160	19.134170
47.396501	1269.327435	19.139187
47.873461	1269.755183	19.144205
47.297045	1264.868457	19.149223
47.470156	1267.647252	19.154240
47.954593	1261.481358	19.159258
47.737240	1259.994336	19.164275
47.686396	1264.177619	19.169293
47.747161	1272.575463	19.174311
47.282034	1266.541630	19.179328
47.555930	1263.460181	19.184346
47.491146	1273.872042	19.189363
47.671816	1285.968765	19.194381
48.012142	1288.718373	19.199399
48.213266	1294.421402	19.204416
48.317082	1286.812594	19.209434
48.312940	1293.194524	19.214451
48.095515	1285.421137	19.219469
48.117373	1287.175755	19.224487
48.355893	1292.683613	19.229504
48.308208	1289.904693	19.234522
48.109159	1293.394688	19.239539
48.059599	1292.436962	19.244557
48.225873	1300.316617	19.249575
48.310681	1306.501665	19.254592
48.618895	1307.454306	19.259610
48.452920	1309.960853	19.264627
48.730966	1312.300438	19.269645
48.535903	1314.678970	19.274663
48.465568	1297.822335	19.279680
48.956372	1298.004931	19.284698
48.762727	1299.903557	19.289715
48.885833	1305.590335	19.294733
49.137032	1301.177504	19.299751
49.150655	1300.538145	19.304768
49.096127	1303.298739	19.309786
49.039772	1312.929825	19.314803
48.976129	1305.624793	19.319821
49.263237	1308.919178	19.324839
49.419437	1324.516379	19.329856
49.387671	1320.766139	19.334874
49.361123	1326.302654	19.339891
49.401321	1330.389726	19.344909
49.783458	1326.477212	19.349927
49.523710	1333.252404	19.354944
49.668395	1328.578438	19.359962
49.161235	1328.790180	19.364979
49.504305	1327.342131	19.369997
49.861165	1325.323887	19.375015
49.628550	1327.348504	19.380032
49.787874	1330.268312	19.385050
49.628641	1328.292551	19.390067
49.565132	1329.937388	19.395085
49.911787	1333.967280	19.400103
49.873930	1328.037316	19.405120
50.079307	1324.808733	19.410138
49.989356	1339.465969	19.415155
50.431648	1342.789848	19.420173
50.462002	1339.771550	19.425191
50.111608	1347.987291	19.430208
50.184268	1352.533220	19.435226
50.330078	1355.041722	19.440243
50.398624	1358.811961	19.445261
50.982550	1335.674325	19.450279
50.881532	1342.882400	19.455296
50.742259	1327.137851	19.460314
50.771436	1324.116584	19.465331
50.910386	1327.484533	19.470349
51.030356	1309.222320	19.475367
50.644393	1311.188760	19.480384
50.869740	1301.462408	19.485402
50.638860	1309.448084	19.490419
50.948047	1320.893659	19.495437
51.194574	1321.111132	19.500455
50.874030	1329.647266	19.505472
51.129268	1320.588439	19.510490
51.153657	1330.573037	19.515507
51.073790	1329.563223	19.520525
50.956869	1321.846756	19.525543
50.849958	1327.550419	19.530560
51.044668	1318.863935	19.535578
51.200897	1328.831161	19.540595
51.023412	1332.062185	19.545613
51.767794	1329.279859	19.550631
51.697580	1349.049610	19.555648
51.625863	1348.458250	19.560666
51.890463	1352.617687	19.565683
51.532057	1344.698965	19.570701
51.696324	1343.950943	19.575719
51.703253	1343.410454	19.580736
51.942956	1341.202166	19.585754
51.674211	1352.460030	19.590771
51.935381	1350.832225	19.595789
52.175413	1352.467674	19.600807
51.851745	1347.525794	19.605824
52.020514	1341.847679	19.610842
51.903934	1352.955620	19.615859
51.664383	1345.267703	19.620877
51.847462	1350.197228	19.625895
51.604059	1357.288622	19.630912
52.129495	1364.105679	19.635930
51.991816	1375.611397	19.640947
52.458887	1374.402815	19.645965
52.273569	1366.286720	19.650983
52.351081	1370.560497	19.656000
52.314888	1372.661835	19.661018
52.396700	1366.621708	19.666035
52.413272	1371.447775	19.671053
52.808972	1378.789969	19.676071
52.657605	1381.871768	19.681088
52.870482	1387.658205	19.686106
53.112296	1387.876414	19.691123
53.141223	1391.356180	19.696141
53.538334	1384.304429	19.701159
53.207664	1373.856715	19.706176
52.833794	1363.633484	19.711194
53.413759	1370.940674	19.716211
53.014303	1381.663482	19.721229
53.619811	1380.972992	19.726247
53.727737	1381.013229	19.731264
53.569463	1362.535506	19.736282
53.473138	1350.280902	19.741299
53.211807	1359.353788	19.746317
53.633389	1368.743233	19.751335
53.324758	1371.877917	19.756352
53.573644	1377.674524	19.761370
53.699865	1380.353340	19.766387
53.686627	1385.846775	19.771405
53.878236	1374.793877	19.776423
53.745480	1382.451881	19.781440
53.890497	1372.832672	19.786458
53.836066	1378.613387	19.791475
53.524429	1378.971414	19.796493
53.911607	1367.992213	19.801511
53.784017	1379.682556	19.806528
54.139269	1387.753735	19.811546
54.325784	1395.677619	19.816563
54.016862	1406.253802	19.821581
54.347365	1398.871586	19.826599
54.099305	1401.981066	19.831616
54.269234	1398.915780	19.836634
54.796521	1399.903746	19.841651
54.438308	1397.160533	19.846669
54.575688	1388.883732	19.851687
54.740353	1400.421287	19.856704
54.660730	1399.992104	19.861722
54.676452	1396.442739	19.866739
54.784763	1394.854508	19.871757
54.918877	1395.682781	19.876775
54.579339	1396.534306	19.881792
54.917580	1401.332390	19.886810
54.574301	1396.160018	19.891827
55.074536	1408.592082	19.896845
55.246303	1415.574677	19.901863
55.398109	1411.243566	19.906880
55.059997	1416.743411	19.911898
55.167330	1416.042120	19.916915
55.247302	1417.970742	19.921933
55.282758	1414.825403	19.926951
55.301544	1414.365119	19.931968
55.631306	1403.754600	19.936986
55.537371	1408.582103	19.942003
55.522720	1417.761780	19.947021
55.387196	1409.088798	19.952039
55.390082	1417.063373	19.957056
55.630735	1427.967416	19.962074
55.841719	1427.900089	19.967091
56.031449	1436.255840	19.972109
56.124751	1433.606426	19.977127
56.391101	1425.060216	19.982144
56.666784	1423.572158	19.987162
56.479999	1412.808525	19.992179
56.351317	1410.386182	19.997197
55.964393	1394.105770	20.002215
56.237812	1399.074893	20.007232
56.484233	1404.019818	20.012250
56.175514	1401.533988	20.017267
56.445914	1413.399075	20.022285
56.695685	1413.575020	20.027303
56.306468	1409.381793	20.032320
56.583602	1423.641115	20.037338
56.819895	1422.903966	20.042355
56.654601	1425.965850	20.047373
56.743450	1423.433896	20.052391
56.744361	1428.284508	20.057408
56.925341	1428.846707	20.062426
56.732569	1420.624450	20.067443
56.858458	1431.044586	20.072461
56.942189	1429.100414	20.077479
56.880044	1431.013294	20.082496
56.521981	1424.962737	20.087514
57.162357	1437.088977	20.092531
56.946689	1459.008530	20.097549
57.121949	1452.789721	20.102567
57.167817	1452.830153	20.107584
57.082470	1456.987295	20.112602
57.186624	1447.639498	20.117619
57.221906	1465.849748	20.122637
57.476258	1466.940174	20.127655
58.086133	1467.618637	20.132672
58.266689	1460.240807	20.137690
58.404669	1443.051795	20.142707
58.061809	1445.175642	20.147725
57.915702	1441.588347	20.152743
58.077934	1442.349128	20.157760
57.867072	1439.434642	20.162778
58.111809	1436.818454	20.167795
57.929014	1437.793901	20.172813
58.303427	1440.572940	20.177831
58.451324	1448.995172	20.182848
58.503511	1432.539059	20.187866
58.454643	1434.692871	20.192883
58.399783	1444.544704	20.197901
58.274807	1447.997950	20.202919
58.668122	1446.630431	20.207936
58.678163	1454.013767	20.212954
58.667892	1457.647973	20.217971
58.910943	1462.694427	20.222989
58.789226	1458.557371	20.228007
58.685132	1451.545758	20.233024
58.409688	1464.821317	20.238042
59.069598	1456.971220	20.243059
58.839722	1457.354388	20.248077
58.650774	1461.631804	20.253095
58.781599	1458.537882	20.258112
58.752453	1463.907585	20.263130
59.351115	1480.373319	20.268147
59.286064	1476.091735	20.273165
58.908241	1476.109770	20.278183
59.203545	1480.191872	20.283200
59.494917	1478.631938	20.288218
59.459826	1480.455403	20.293235
59.551010	1488.261626	20.298253
59.481210	1486.404468	20.303271
59.461065	1484.918282	20.308288
59.132788	1492.600463	20.313306
59.681366	1500.120880	20.318323
59.313568	1495.308907	20.323341
59.771863	1508.470259	20.328359
59.976316	1500.463834	20.333376
59.798728	1507.314663	20.338394
60.199807	1502.430317	20.343411
60.013910	1498.243283	20.348429
60.499762	1499.597473	20.353447
60.410141	1498.150505	20.358464
60.433356	1497.623256	20.363482
60.530432	1493.430036	20.368499
60.221688	1498.701268	20.373517
60.321388	1499.550683	20.378535
60.283842	1493.421798	20.383552
60.363392	1510.990878	20.388570
60.981535	1515.944232	20.393587
60.566033	1520.357922	20.398605
60.931918	1515.119284	20.403623
61.360439	1507.018008	20.408640
61.020334	1519.700908	20.413658
61.231181	1517.131012	20.418675
60.818569	1510.404100	20.423693
60.906999	1508.282460	20.428711
61.203670	1508.135519	20.433728
61.110990	1519.665881	20.438746
61.473107	1509.318510	20.443763
61.557546	1514.108802	20.448781
61.814222	1518.708175	20.453799
61.320456	1509.219906	20.458816
61.664444	1509.621027	20.463834
61.287006	1517.222509	20.468851
61.453870	1517.726948	20.473869
61.353022	1519.226135	20.478887
61.691696	1516.964546	20.483904
61.379812	1536.014727	20.488922
61.841392	1533.825519	20.493939
62.072501	1534.465125	20.498957
61.575359	1534.728959	20.503975
62.277776	1544.999438	20.508992
62.027554	1535.261794	20.514010
62.147550	1534.751034	20.519027
61.775841	1528.746748	20.524045
61.930176	1542.305751	20.529063
62.979386	1541.558797	20.534080
62.704529	1542.715843	20.539098
63.056543	1555.152152	20.544115
63.067462	1542.988017	20.549133
62.680633	1530.349323	20.554151
62.702814	1526.316081	20.559168
62.740143	1520.285984	20.564186
62.797419	1522.164501	20.569203
62.696572	1522.587543	20.574221
62.804911	1538.747814	20.579239
63.053930	1541.300236	20.584256
63.162908	1551.464295	20.589274
63.103250	1544.325805	20.594291
62.999542	1545.112216	20.599309
62.709462	1548.632213	20.604327
62.695172	1548.300153	20.609344
62.882254	1561.749928	20.614362
63.475619	1560.322852	20.619379
63.402147	1571.165436	20.624397
63.473526	1570.779011	20.629415
63.944038	1562.526003	20.634432
63.879248	1569.296177	20.639450
63.900649	1568.324232	20.644467
64.176033	1564.882731	20.649485
63.864356	1564.647466	20.654503
63.736944	1558.816577	20.659520
63.921531	1568.255650	20.664538
63.966646	1555.656986	20.669555
64.506359	1566.142162	20.674573
64.281143	1565.126561	20.679591
64.215679	1547.732434	20.684608
64.741581	1550.683568	20.689626
64.060070	1553.090530	20.694643
64.609621	1560.408847	20.699661
64.448507	1563.886676	20.704679
64.524566	1555.426837	20.709696
63.807290	1563.122276	20.714714
64.115388	1567.997683	20.719731
64.369945	1583.059081	20.724749
64.371716	1579.114213	20.729767
64.996416	1576.767058	20.734784
64.856127	1575.896027	20.739802
64.731070	1578.860152	20.744819
65.132139	1574.442855	20.749837
65.018778	1594.961224	20.754855
65.328490	1601.114515	20.759872
65.373508	1598.999623	20.764890
65.463028	1603.921695	20.769907
65.773445	1598.376083	20.774925
65.334084	1611.472140	20.779943
65.809921	1587.647249	20.784960
65.660394	1601.821661	20.789978
65.386067	1601.053551	20.794995
65.470698	1602.034707	20.800013
65.556016	1606.998461	20.805031
65.997958	1604.446222	20.810048
65.688358	1607.767294	20.815066
65.693043	1603.354899	20.820083
65.903137	1608.516980	20.825101
66.027980	1623.614388	20.830119
66.223003	1622.476549	20.835136
66.316461	1620.593959	20.840154
66.424016	1616.673640	20.845171
66.378999	1618.410300	20.850189
66.218432	1627.436075	20.855207
66.676202	1624.531068	20.860224
66.798280	1614.931078	20.865242
66.660083	1617.161938	20.870259
66.717846	1625.787639	20.875277
66.552686	1623.847482	20.880295
66.666925	1631.426111	20.885312
67.025488	1632.923209	20.890330
66.946651	1633.484841	20.895347
66.857394	1626.802216	20.900365
66.468189	1637.766583	20.905383
66.983857	1630.112441	20.910400
67.071090	1631.247832	20.915418
66.797492	1630.735232	20.920435
67.054704	1638.777609	20.925453
67.168289	1659.456382	20.930471
67.743712	1651.489963	20.935488
67.704393	1655.122421	20.940506
67.606715	1657.779332	20.945523
67.817341	1653.735657	20.950541
67.432229	1658.438145	20.955559
67.826534	1659.841316	20.960576
67.751044	1644.490508	20.965594
67.785730	1646.104306	20.970611
68.052040	1644.743924	20.975629
67.946748	1649.977212	20.980647
68.277405	1641.048495	20.985664
68.459030	1648.487249	20.990682
68.130599	1651.088565	20.995699
68.201529	1654.606026	21.000717
68.482255	1663.430565	21.005735
68.937809	1676.756575	21.010752
68.722130	1672.305887	21.015770
68.575477	1672.366827	21.020787
69.171106	1665.587022	21.025805
68.848289	1656.315060	21.030823
68.894322	1656.030411	21.035840
69.012415	1660.834439	21.040858
68.939326	1659.116634	21.045875
68.947479	1660.845020	21.050893
69.081405	1671.286137	21.055911
69.181600	1658.719851	21.060928
69.136561	1665.859380	21.065946
68.866712	1667.703635	21.070963
68.927052	1662.600891	21.075981
68.922834	1671.706489	21.080999
69.437207	1682.091535	21.086016
69.607585	1684.372192	21.091034
69.371438	1686.555193	21.096051
69.592384	1682.456255	21.101069
69.663958	1690.259308	21.106087
69.500410	1692.165912	21.111104
69.644261	1690.474290	21.116122
69.674681	1704.693352	21.121139
69.943858	1700.176636	21.126157
69.924354	1720.560613	21.131175
70.271834	1705.860284	21.136192
70.049060	1709.164701	21.141210
69.842874	1712.523341	21.146227
70.159082	1703.126615	21.151245
70.239518	1726.865524	21.156263
70.967600	1722.738112	21.161280
71.387286	1717.986514	21.166298
71.091788	1703.806027	21.171315
71.140259	1703.148604	21.176333
71.376589	1696.797123	21.181351
71.354569	1697.558199	21.186368
71.666530	1700.091376	21.191386
71.352652	1690.726484	21.196403
71.320177	1689.245356	21.201421
71.259759	1690.053436	21.206439
71.132522	1689.009950	21.211456
71.489484	1684.934016	21.216474
71.121592	1685.411263	21.221491
71.407718	1690.091304	21.226509
71.354980	1690.973930	21.231527
71.388193	1686.531826	21.236544
71.843300	1702.909662	21.241562
71.702130	1709.792770	21.246579
71.862393	1707.439011	21.251597
71.936758	1711.804880	21.256615
71.675490	1715.560271	21.261632
71.968322	1717.761906	21.266650
71.552480	1712.733286	21.271667
71.699106	1708.712186	21.276685
71.712369	1737.094406	21.281703
72.028366	1743.562356	21.286720
72.058930	1739.057534	21.291738
71.941633	1752.220318	21.296755
72.072834	1738.958008	21.301773
72.401192	1755.863725	21.306791
72.616890	1766.339504	21.311808
72.889818	1762.260858	21.316826
72.856033	1762.111715	21.321843
73.242754	1758.981056	21.326861
73.039415	1759.855574	21.331879
72.925183	1760.883481	21.336896
72.805864	1758.364955	21.341914
72.707569	1755.388708	21.346931
72.829761	1750.929579	21.351949
72.752721	1760.968081	21.356967
73.388497	1775.537931	21.361984
73.748301	1773.291955	21.367002
73.824719	1788.561148	21.372019
73.528740	1781.121676	21.377037
73.678085	1781.098660	21.382055
73.548565	1785.259599	21.387072
73.903809	1777.340028	21.392090
73.251324	1781.875888	21.397107
74.155825	1778.027119	21.402125
73.880758	1783.002848	21.407143
74.059360	1803.144631	21.412160
74.463504	1797.546494	21.417178
73.942240	1804.400450	21.422195
74.464352	1806.408603	21.427213
74.726855	1799.387115	21.432231
74.536522	1805.116542	21.437248
74.850487	1805.153105	21.442266
74.803596	1800.985384	21.447283
74.648692	1794.814705	21.452301
74.626820	1794.635304	21.457319
74.705645	1796.516807	21.462336
75.115659	1786.467940	21.467354
74.837710	1790.560469	21.472371
74.980736	1783.453445	21.477389
75.328801	1785.823218	21.482407
74.785508	1786.993671	21.487424
75.252871	1800.100178	21.492442
75.152531	1808.501266	21.497459
75.500718	1812.341675	21.502477
75.671468	1810.030452	21.507495
75.764818	1812.875402	21.512512
75.766486	1811.496249	21.517530
75.788544	1819.288132	21.522547
75.648522	1814.437452	21.527565
75.764465	1798.251951	21.532583
75.647424	1814.327638	21.537600
75.937729	1820.525053	21.542618
76.174226	1833.361406	21.547635
76.024089	1830.301697	21.552653
76.072723	1833.393461	21.557671
76.087307	1847.987500	21.562688
76.176082	1836.401199	21.567706
76.178507	1838.865820	21.572723
76.322278	1848.065236	21.577741
76.539218	1855.208235	21.582759
76.619601	1862.978432	21.587776
77.046741	1864.995067	21.592794
76.634906	1862.222258	21.597811
76.760022	1856.847432	21.602829
77.093900	1856.726255	21.607847
76.805746	1861.498910	21.612864
77.278336	1859.443654	21.617882
77.198200	1877.173661	21.622899
77.630231	1883.775080	21.627917
77.606331	1875.646245	21.632935
77.403478	1880.897946	21.637952
77.697356	1873.306636	21.642970
77.895549	1884.075554	21.647987
77.917638	1877.441773	21.653005
77.888057	1875.957023	21.658023
77.806406	1877.207089	21.663040
77.904296	1879.334950	21.668058
77.707745	1874.985379	21.673075
77.865371	1876.627396	21.678093
78.165147	1872.251044	21.683111
77.912069	1872.899774	21.688128
78.353081	1873.762341	21.693146
78.150759	1876.665959	21.698163
78.502221	1889.617002	21.703181
78.907310	1896.724412	21.708199
78.875035	1898.269760	21.713216
78.707005	1895.190734	21.718234
78.550661	1895.966420	21.723251
78.984196	1900.206985	21.728269
78.809765	1897.924247	21.733287
78.755434	1909.493073	21.738304
78.865209	1897.928710	21.743322
78.591132	1895.339582	21.748339
78.644124	1905.581990	21.753357
78.894935	1909.519635	21.758375
79.362875	1912.486167	21.763392
79.397708	1911.022944	21.768410
79.405746	1912.126501	21.773427
79.952665	1928.436599	21.778445
79.982701	1932.064627	21.783463
79.864842	1924.045076	21.788480
80.121003	1924.362048	21.793498
80.017690	1924.555101	21.798515
80.011244	1930.612557	21.803533
80.321744	1927.733586	21.808551
80.249471	1936.594285	21.813568
80.532282	1929.064637	21.818586
80.517042	1934.700570	21.823603
80.219346	1932.392835	21.828621
80.638917	1926.621837	21.833639
80.284148	1929.975248	21.838656
80.304349	1923.688895	21.843674
80.336342	1928.335980	21.848691
80.827126	1944.579092	21.853709
81.311166	1943.869624	21.858727
81.372858	1947.861970	21.863744
81.621758	1948.126422	21.868762
81.522757	1953.627074	21.873779
81.510077	1938.922666	21.878797
81.456212	1922.974936	21.883815
81.114091	1923.754300	21.888832
81.678475	1935.804348	21.893850
81.911697	1932.691246	21.898867
81.656802	1947.901701	21.903885
81.733477	1939.078653	21.908903
81.533571	1948.719809	21.913920
81.707469	1938.407806	21.918938
81.788696	1942.778976	21.923955
81.348313	1943.482118	21.928973
82.060937	1949.557019	21.933991
82.184844	1958.399809	21.939008
82.092954	1967.689628	21.944026
81.947995	1963.698090	21.949043
81.911893	1969.037468	21.954061
82.123745	1972.220614	21.959079
82.524721	1987.783442	21.964096
82.622036	1990.637271	21.969114
82.814708	1984.371383	21.974131
82.496185	1990.477448	21.979149
82.848008	1986.001444	21.984167
82.746884	1993.818893	21.989184
83.125892	2006.153481	21.994202
83.265030	2003.402168	21.999219
83.629364	2005.851494	22.004237
83.811257	2000.562463	22.009255
83.649109	2007.792948	22.014272
83.871718	2006.401472	22.019290
84.040592	1993.918935	22.024307
83.696319	1984.631207	22.029325
83.816343	1975.514202	22.034343
83.527869	1979.835639	22.039360
83.876610	1996.107225	22.044378
83.910803	1995.496197	22.049395
83.837901	2006.686110	22.054413
84.260583	1992.349394	22.059431
83.870151	1998.839058	22.064448
84.159908	2001.438854	22.069466
84.381953	2006.750676	22.074483
84.120316	2016.571899	22.079501
84.422631	2016.995302	22.084519
84.465127	2035.369120	22.089536
84.446341	2025.800310	22.094554
84.764345	2025.937235	22.099571
84.678352	2029.431862	22.104589
85.017597	2046.475021	22.109607
85.052733	2049.123936	22.114624
85.171432	2043.945722	22.119642
85.602122	2048.761148	22.124659
85.608459	2042.117135	22.129677
85.878783	2046.711365	22.134695
85.604148	2040.499278	22.139712
85.569784	2044.935809	22.144730
85.860461	2035.836387	22.149747
85.493055	2039.791415	22.154765
85.852946	2044.488469	22.159783
85.845182	2049.536269	22.164800
85.637308	2048.306491	22.169818
86.235774	2046.888053	22.174835
86.147263	2057.777457	22.179853
86.470242	2060.189045	22.184871
86.317811	2058.057502	22.189888
86.109693	2060.744291	22.194906
86.317706	2057.890725	22.199923
86.643545	2057.799202	22.204941
86.468363	2067.079949	22.209959
86.742680	2078.054893	22.214976
86.832115	2077.807664	22.219994
87.407029	2078.475818	22.225011
87.271533	2076.133343	22.230029
87.225702	2073.486561	22.235047
87.190950	2081.912281	22.240064
87.041188	2076.801103	22.245082
87.281470	2078.019997	22.250099
87.604439	2085.601037	22.255117
87.980785	2097.702562	22.260135
88.147286	2087.830303	22.265152
87.806983	2082.594147	22.270170
87.917510	2077.253087	22.275187
87.797150	2094.380473	22.280205
87.973507	2090.307320	22.285223
88.081956	2092.338884	22.290240
88.101083	2098.493406	22.295258
88.136936	2090.490876	22.300275
88.327511	2098.291359	22.305293
88.321886	2094.773583	22.310311
88.448879	2101.526723	22.315328
88.772907	2123.716531	22.320346
88.782447	2127.174211	22.325363
88.516212	2131.170315	22.330381
89.000568	2128.150630	22.335399
89.090040	2121.184360	22.340416
88.990257	2129.957915	22.345434
89.245910	2119.951831	22.350451
88.914470	2122.285427	22.355469
89.184261	2117.875814	22.360487
89.253233	2119.534812	22.365504
89.439365	2118.641336	22.370522
89.582565	2131.145274	22.375539
89.497613	2141.775387	22.380557
89.521502	2134.544753	22.385575
89.596589	2147.557950	22.390592
89.547996	2142.285827	22.395610
89.745906	2137.991546	22.400627
90.015976	2159.186204	22.405645
89.790364	2162.333347	22.410663
90.158694	2167.963286	22.415680
89.796730	2158.444680	22.420698
90.380347	2158.448729	22.425715
90.225613	2173.138827	22.430733
90.196910	2177.397775	22.435751
90.521498	2176.605822	22.440768
90.339583	2186.910213	22.445786
91.068018	2185.439970	22.450803
91.267257	2198.645323	22.455821
91.352123	2191.673431	22.460839
91.487710	2190.674206	22.465856
91.838411	2201.766728	22.470874
91.953501	2172.297542	22.475891
91.715963	2168.203601	22.480909
91.846608	2168.514872	22.485927
91.847767	2170.724104	22.490944
91.792200	2172.967415	22.495962
91.977008	2170.653958	22.500979
91.879841	2173.121508	22.505997
91.818386	2179.850366	22.511015
92.087575	2185.230644	22.516032
92.285368	2191.038628	22.521050
92.757267	2185.505566	22.526067
92.550975	2191.174481	22.531085
92.645131	2190.064936	22.536103
92.490015	2190.505910	22.541120
92.450464	2188.161106	22.546138
92.726242	2186.366842	22.551155
92.581756	2183.773275	22.556173
93.089301	2202.791265	22.561191
93.382257	2207.811226	22.566208
93.078346	2218.750043	22.571226
93.427807	2203.168482	22.576243
93.260363	2214.758272	22.581261
93.017065	2208.459193	22.586279
93.471907	2207.457601	22.591296
93.176067	2211.688717	22.596314
93.162766	2227.597137	22.601331
93.298416	2227.547849	22.606349
93.608262	2233.306841	22.611367
93.678713	2237.585082	22.616384
93.577462	2251.862952	22.621402
94.056810	2246.448638	22.626419
94.119255	2256.661373	22.631437
93.892564	2262.816351	22.636455
94.217723	2261.749736	22.641472
94.349577	2267.151421	22.646490
94.553993	2270.651376	22.651507
94.848538	2286.862233	22.656525
94.384807	2279.959939	22.661543
95.035889	2270.917902	22.666560
94.775883	2281.307093	22.671578
94.962527	2276.828330	22.676595
94.880307	2289.493715	22.681613
95.145051	2294.338200	22.686631
95.548715	2304.791343	22.691648
95.537491	2307.112979	22.696666
95.812551	2299.044709	22.701683
95.693117	2301.446311	22.706701
95.611307	2298.066596	22.711719
96.138435	2301.519469	22.716736
95.805005	2300.735281	22.721754
95.875947	2299.528351	22.726771
96.219622	2304.534130	22.731789
95.897815	2296.584037	22.736807
95.973469	2301.391688	22.741824
96.250579	2319.243248	22.746842
96.544644	2318.837917	22.751859
96.486178	2323.660144	22.756877
96.413778	2326.761370	22.761895
96.882448	2316.772507	22.766912
96.759693	2320.238198	22.771930
96.874165	2326.744050	22.776947
97.138836	2331.310829	22.781965
97.203126	2333.977339	22.786983
97.369376	2332.338977	22.792000
97.419913	2334.423769	22.797018
97.430172	2331.083365	22.802035
97.530057	2334.388156	22.807053
97.830488	2335.190580	22.812071
97.923656	2314.192110	22.817088
97.803612	2317.168200	22.822106
97.982913	2318.803728	22.827123
98.516863	2325.133809	22.832141
98.181991	2329.367873	22.837159
98.601642	2338.736042	22.842176
98.503794	2342.131583	22.847194
98.653319	2345.428648	22.852211
98.893016	2337.126010	22.857229
98.809931	2344.012941	22.862247
99.031430	2332.869586	22.867264
98.833690	2342.431715	22.872282
99.043266	2331.334401	22.877299
99.074898	2333.706176	22.882317
99.097806	2340.447208	22.887335
99.030753	2333.495757	22.892352
99.399121	2334.581110	22.897370
99.187646	2342.024549	22.902387
99.224351	2344.114652	22.907405
99.240124	2359.336967	22.912423
99.470957	2359.758884	22.917440
99.664928	2357.144156	22.922458
99.607132	2362.767914	22.927475
99.829733	2369.361093	22.932493
100.323674	2380.459830	22.937511
100.389289	2379.405213	22.942528
99.757749	2386.046170	22.947546
99.790636	2386.981775	22.952563
100.298663	2391.349725	22.957581
100.089129	2407.131056	22.962599
100.581569	2420.161528	22.967616
100.681506	2408.140745	22.972634
100.482454	2405.101177	22.977651
101.040780	2419.513189	22.982669
100.747316	2426.903152	22.987687
101.022437	2438.026525	22.992704
101.282474	2431.289216	22.997722
101.121538	2432.207660	23.002739
101.472260	2432.999102	23.007757
101.036372	2451.643501	23.012775
101.592840	2446.617935	23.017792
101.869705	2458.113458	23.022810
102.279221	2449.815889	23.027827
102.413091	2445.405265	23.032845
102.264954	2453.315447	23.037863
102.350082	2449.044964	23.042880
102.310051	2445.939602	23.047898
102.548172	2448.301335	23.052915
103.012521	2446.982649	23.057933
102.651090	2441.282587	23.062951
102.970531	2441.602341	23.067968
102.635913	2447.243976	23.072986
102.737741	2443.665218	23.078003
102.992704	2441.290307	23.083021
102.861560	2458.097807	23.088039
102.895491	2461.232997	23.093056
103.163768	2466.323149	23.098074
103.230588	2467.363935	23.103091
103.112637	2468.291468	23.108109
103.333472	2483.999549	23.113127
103.662636	2485.460271	23.118144
103.783814	2489.711738	23.123162
103.602578	2493.918765	23.128179
103.902454	2482.554817	23.133197
104.050751	2502.468561	23.138215
104.461362	2515.360353	23.143232
104.262243	2519.522830	23.148250
104.258855	2516.891466	23.153267
104.446196	2511.036509	23.158285
104.184162	2512.377824	23.163303
104.502495	2517.491758	23.168320
104.946083	2527.471724	23.173338
104.604854	2543.327331	23.178355
105.227402	2544.461493	23.183373
105.123883	2541.179792	23.188391
105.208374	2531.537824	23.193408
105.448828	2534.603001	23.198426
105.562420	2555.528980	23.203443
105.688045	2551.959119	23.208461
105.905294	2558.120825	23.213479
105.850293	2554.077276	23.218496
106.114119	2550.495367	23.223514
105.625052	2553.901362	23.228531
106.140567	2549.112534	23.233549
105.901429	2553.117136	23.238567
106.218379	2566.579009	23.243584
106.315882	2576.155260	23.248602
106.730366	2574.020603	23.253619
106.714258	2571.956143	23.258637
106.733780	2571.318976	23.263655
106.763151	2571.999499	23.268672
106.948150	2584.339444	23.273690
106.945684	2596.588655	23.278707
107.303491	2592.237812	23.283725
107.201177	2595.763494	23.288743
107.332298	2596.642787	23.293760
107.394512	2591.245975	23.298778
107.269777	2598.874846	23.303795
107.343657	2600.163868	23.308813
107.709647	2611.396287	23.313831
107.876818	2620.371535	23.318848
108.137101	2615.518278	23.323866
108.073062	2622.901005	23.328883
108.389153	2611.928957	23.333901
108.302623	2628.701266	23.338919
108.552111	2631.714555	23.343936
108.663894	2641.039290	23.348954
108.762786	2644.625181	23.353971
109.305226	2640.681115	23.358989
109.355355	2633.294705	23.364007
109.063549	2629.411094	23.369024
109.060244	2636.475079	23.374042
108.812554	2639.565777	23.379059
109.423211	2643.065678	23.384077
109.437734	2634.845301	23.389095
109.089802	2635.786557	23.394112
109.575841	2650.516148	23.399130
109.654554	2655.648492	23.404147
110.033590	2656.022094	23.409165
109.955863	2663.763603	23.414183
109.789163	2661.186049	23.419200
110.003198	2655.131214	23.424218
110.134690	2659.346399	23.429235
110.301640	2668.552097	23.434253
110.588699	2676.410401	23.439271
110.499678	2672.646698	23.444288
110.409948	2670.085564	23.449306
110.473360	2674.301884	23.454323
110.767604	2675.938486	23.459341
111.075356	2690.657995	23.464359
111.300125	2691.440655	23.469376
111.504151	2694.470502	23.474394
111.307785	2699.115468	23.479411
111.800245	2695.437968	23.484429
111.704250	2698.757543	23.489447
111.651605	2694.931364	23.494464
111.424713	2698.659514	23.499482
111.389149	2717.065121	23.504499
111.852496	2710.286586	23.509517
111.938501	2720.565349	23.514535
112.243780	2733.587317	23.519552
112.383944	2733.329026	23.524570
112.531057	2745.974807	23.529587
112.649294	2744.324948	23.534605
112.805942	2748.836064	23.539623
112.846569	2740.299124	23.544640
112.756160	2745.741871	23.549658
112.816169	2755.693316	23.554675
113.118303	2764.928513	23.559693
113.249687	2768.935440	23.564711
113.276699	2763.613491	23.569728
113.402396	2761.839381	23.574746
113.501957	2785.535687	23.579763
113.632259	2789.776337	23.584781
113.807643	2793.915286	23.589799
113.805843	2788.534694	23.594816
113.756546	2785.301316	23.599834
114.140691	2799.488269	23.604851
114.452681	2806.171843	23.609869
114.434686	2810.451367	23.614887
114.282949	2805.602242	23.619904
114.559800	2795.933339	23.624922
114.522723	2820.367394	23.629939
114.875815	2835.979446	23.634957
114.838897	2837.364638	23.639975
115.129125	2834.608612	23.644992
115.163795	2824.264125	23.650010
115.054543	2840.800307	23.655027
115.752700	2836.595248	23.660045
116.163069	2843.373983	23.665063
116.086191	2852.630362	23.670080
116.514474	2834.302812	23.675098
116.575894	2824.493850	23.680115
116.624336	2812.979475	23.685133
116.470199	2796.844590	23.690151
116.442075	2809.161063	23.695168
116.352705	2808.660772	23.700186
116.233387	2816.165804	23.705203
116.672103	2823.505056	23.710221
116.638082	2830.031054	23.715239
116.791316	2833.229792	23.720256
117.290151	2838.700758	23.725274
116.709079	2838.431668	23.730291
116.894829	2836.209506	23.735309
117.240668	2843.607412	23.740327
117.376209	2853.458780	23.745344
117.521670	2859.338251	23.750362
117.397117	2855.867247	23.755379
117.502857	2863.564497	23.760397
117.490894	2863.929546	23.765415
117.677293	2882.711056	23.770432
117.904643	2877.490438	23.775450
117.973714	2882.829494	23.780467
118.326838	2884.239177	23.785485
118.299001	2892.976655	23.790503
118.219049	2901.946334	23.795520
118.728756	2901.548447	23.800538
118.890183	2899.513117	23.805555
118.720217	2907.742507	23.810573
118.920622	2907.522175	23.815591
118.760552	2917.400666	23.820608
119.408560	2923.886789	23.825626
119.228036	2927.926533	23.830643
119.133476	2920.650903	23.835661
119.432311	2927.712147	23.840679
119.496449	2945.278723	23.845696
120.149029	2941.339537	23.850714
119.845959	2960.165774	23.855731
120.246362	2948.722758	23.860749
120.676735	2947.677596	23.865767
120.550613	2943.480915	23.870784
120.644998	2936.365228	23.875802
120.922876	2953.822788	23.880819
121.116114	2956.362007	23.885837
120.952379	2964.562047	23.890855
121.065315	2966.447832	23.895872
121.112911	2966.276540	23.900890
120.923193	2967.900147	23.905907
121.137999	2967.832222	23.910925
121.648568	2964.653670	23.915943
121.198546	2987.031340	23.920960
121.798260	2987.834541	23.925978
121.685510	2985.627273	23.930995
121.916868	2990.840099	23.936013
122.120282	2989.754524	23.941031
122.031774	2993.101393	23.946048
122.048950	3008.740647	23.951066
122.233027	3013.089753	23.956083
122.406976	3011.320731	23.961101
123.004997	3006.298011	23.966119
122.569245	3020.073094	23.971136
122.531871	3027.941034	23.976154
122.776179	3023.983337	23.981171
122.742562	3037.203470	23.986189
123.032228	3043.745428	23.991207
123.454992	3049.351390	23.996224
123.386580	3055.179009	24.001242
123.920815	3061.935386	24.006259
123.803827	3066.915261	24.011277
123.978988	3058.006896	24.016295
123.804707	3067.994990	24.021312
124.227954	3074.355200	24.026330
124.378831	3073.915336	24.031347
124.352185	3080.699078	24.036365
124.584499	3088.723893	24.041383
124.496920	3089.353209	24.046400
124.482846	3079.357026	24.051418
124.541878	3088.911135	24.056435
124.744439	3101.545379	24.061453
125.343773	3098.198333	24.066471
125.017259	3097.419343	24.071488
125.159108	3099.382699	24.076506
125.247346	3102.421174	24.081523
125.151948	3114.612616	24.086541
125.567787	3111.777026	24.091559
125.795246	3122.008747	24.096576
125.479367	3122.048694	24.101594
126.009126	3131.119240	24.106611
126.380657	3144.636174	24.111629
126.568884	3139.408946	24.116647
126.290134	3148.390762	24.121664
126.320554	3147.190085	24.126682
126.395377	3154.112708	24.131699
126.690446	3161.654364	24.136717
127.010253	3169.469912	24.141735
127.020640	3179.814366	24.146752
127.209272	3172.706005	24.151770
127.273337	3174.125999	24.156787
127.471090	3186.518027	24.161805
127.844612	3186.835690	24.166823
127.848540	3189.085646	24.171840
128.029237	3191.415389	24.176858
128.002886	3180.022889	24.181875
128.094485	3188.135935	24.186893
128.365020	3193.068136	24.191911
128.337993	3196.108792	24.196928
128.266772	3212.055507	24.201946
128.377069	3216.652861	24.206963
128.313536	3209.930922	24.211981
128.723654	3220.696056	24.216999
128.990855	3223.504695	24.222016
129.107552	3228.385109	24.227034
129.321633	3225.495697	24.232051
129.163581	3238.612262	24.237069
129.324586	3239.370157	24.242087
129.567630	3252.537906	24.247104
129.944384	3254.979160	24.252122
129.837362	3254.386920	24.257139
129.928292	3265.555265	24.262157
130.247406	3264.473754	24.267175
130.981607	3274.711883	24.272192
130.895203	3266.121880	24.277210
130.979299	3263.508348	24.282227
130.757581	3267.781825	24.287245
130.917871	3257.534308	24.292263
131.264513	3274.956226	24.297280
131.097597	3269.342392	24.302298
131.292466	3269.495345	24.307315
131.283111	3280.082799	24.312333
131.575445	3284.528739	24.317351
131.613111	3293.073155	24.322368
131.923365	3292.561131	24.327386
131.906942	3289.619223	24.332403
131.925399	3280.823518	24.337421
131.966889	3285.579942	24.342439
132.223333	3312.269808	24.347456
132.363768	3317.929281	24.352474
132.219192	3304.948619	24.357491
132.143966	3323.111684	24.362509
132.666539	3327.720627	24.367527
132.860277	3331.424448	24.372544
132.776022	3336.121559	24.377562
133.064296	3336.897517	24.382579
133.062379	3357.271148	24.387597
133.539757	3357.272808	24.392615
133.473340	3364.678303	24.397632
133.518367	3361.931968	24.402650
133.991344	3361.729162	24.407667
134.046305	3366.350951	24.412685
134.017444	3375.417064	24.417703
134.240240	3387.918956	24.422720
134.264086	3389.575629	24.427738
134.539970	3387.471927	24.432755
134.397686	3380.626468	24.437773
134.837496	3373.636731	24.442791
135.218600	3383.481720	24.447808
135.273311	3384.527601	24.452826
135.582549	3379.196248	24.457843
135.405071	3392.770439	24.462861
135.776120	3388.414187	24.467879
135.707484	3388.248363	24.472896
135.801776	3389.051369	24.477914
135.554913	3392.779614	24.482931
135.870023	3402.082557	24.487949
136.203873	3414.652393	24.492967
136.273825	3411.381400	24.497984
136.192196	3418.113862	24.503002
136.582800	3411.109677	24.508019
136.367537	3417.471578	24.513037
136.693424	3432.245684	24.518055
136.835203	3433.508415	24.523072
136.706058	3439.411893	24.528090
137.178907	3437.337486	24.533107
137.089745	3465.138711	24.538125
137.295775	3460.997506	24.543143
137.775002	3455.819567	24.548160
137.471084	3451.199113	24.553178
138.186616	3464.299767	24.558195
138.123516	3476.865169	24.563213
138.530974	3468.327584	24.568231
139.317930	3465.977024	24.573248
138.838759	3475.375262	24.578266
138.907168	3465.110371	24.583283
138.686660	3471.236392	24.588301
138.874213	3467.593585	24.593319
139.011127	3479.446110	24.598336
138.940869	3481.019602	24.603354
139.670796	3482.714695	24.608371
139.426802	3487.127408	24.613389
139.473576	3496.974012	24.618407
139.584863	3506.681174	24.623424
139.504244	3512.892741	24.628442
139.941495	3512.758620	24.633459
140.260741	3518.308256	24.638477
140.081838	3516.063879	24.643495
140.482439	3515.029634	24.648512
140.582443	3538.726864	24.653530
141.101339	3545.586812	24.658547
140.779967	3538.333619	24.663565
140.549322	3539.850025	24.668583
141.081941	3536.636380	24.673600
141.204215	3544.744811	24.678618
141.507394	3552.623084	24.683635
141.616268	3551.504852	24.688653
141.539271	3552.186192	24.693671
142.178570	3544.713992	24.698688
141.930792	3553.473408	24.703706
142.094087	3568.970463	24.708723
142.126549	3578.705717	24.713741
141.857647	3576.311222	24.718759
142.136914	3576.899221	24.723776
142.437492	3588.909398	24.728794
142.619008	3598.848704	24.733811
143.107066	3609.706092	24.738829
143.414012	3599.975262	24.743847
143.351441	3597.753794	24.748864
143.026788	3602.630432	24.753882
143.402126	3604.093527	24.758899
143.572699	3612.330187	24.763917
143.372632	3625.387294	24.768935
143.990654	3625.310246	24.773952
143.880917	3624.772072	24.778970
144.337390	3634.681214	24.783987
144.592996	3644.422793	24.789005
144.378109	3640.795264	24.794023
144.679263	3643.939556	24.799040
144.861726	3647.698854	24.804058
144.855292	3638.502852	24.809075
144.843001	3653.673821	24.814093
144.780804	3658.424393	24.819111
144.856996	3659.406978	24.824128
145.250072	3669.152417	24.829146
145.642426	3679.270409	24.834163
146.015003	3694.845458	24.839181
145.746000	3691.570373	24.844199
146.210437	3686.631389	24.849216
146.429280	3700.633324	24.854234
146.729979	3694.185901	24.859251
146.845135	3705.814714	24.864269
146.871566	3694.798731	24.869287
147.194841	3701.963788	24.874304
147.279384	3707.048181	24.879322
147.486325	3706.252389	24.884339
147.455054	3697.404254	24.889357
147.693800	3704.844440	24.894375
147.601246	3694.598166	24.899392
147.441828	3709.990931	24.904410
147.841856	3721.499653	24.909427
147.850909	3729.155515	24.914445
147.917117	3720.939221	24.919463
148.545104	3735.275169	24.924480
148.374815	3753.535530	24.929498
148.449072	3750.241711	24.934515
148.544485	3746.026133	24.939533
148.687805	3757.735813	24.944551
149.198041	3762.012228	24.949568
149.085261	3769.055827	24.954586
149.638736	3769.642172	24.959603
149.550297	3770.896582	24.964621
149.472117	3778.869047	24.969639
149.732552	3792.694140	24.974656
149.488578	3803.690867	24.979674
149.777264	3800.259498	24.984691
149.987750	3816.828858	24.989709
149.794686	3822.515162	24.994727
150.620377	3818.062774	24.999744
150.443556	3836.942863	25.004762
151.002370	3844.017649	25.009779
151.224153	3834.991173	25.014797
151.514236	3836.492812	25.019815
152.083475	3827.011399	25.024832
151.959216	3831.272990	25.029850
152.111147	3817.614544	25.034867
152.264722	3822.116940	25.039885
152.109460	3819.966688	25.044903
152.290962	3808.077460	25.049920
152.477717	3818.281197	25.054938
152.275068	3819.970018	25.059955
152.848593	3839.452914	25.064973
153.076113	3840.405636	25.069991
153.343562	3850.505296	25.075008
153.216627	3848.536850	25.080026
152.775174	3838.622566	25.085043
152.988430	3839.577509	25.090061
153.191969	3841.521874	25.095079
153.544687	3837.648121	25.100096
153.827627	3854.300923	25.105114
154.188558	3859.740017	25.110131
154.209998	3853.774736	25.115149
153.882755	3860.580322	25.120167
153.914813	3864.905959	25.125184
154.194534	3872.125209	25.130202
154.415422	3877.551394	25.135219
154.668611	3877.998275	25.140237
154.342022	3883.279291	25.145255
154.930922	3893.470961	25.150272
154.930527	3905.439833	25.155290
154.972472	3918.730911	25.160307
155.360214	3916.451920	25.165325
155.272602	3929.558019	25.170343
155.606733	3934.127021	25.175360
155.547384	3949.472847	25.180378
155.557340	3957.040290	25.185395
156.138311	3962.937537	25.190413
156.100508	3981.518380	25.195431
156.690484	3985.495213	25.200448
156.386921	3983.535313	25.205466
156.565486	3991.467899	25.210483
156.968935	4001.104590	25.215501
156.900633	4010.120350	25.220519
157.285369	4013.431603	25.225536
157.772890	4016.427006	25.230554
157.506153	4022.958104	25.235571
157.998776	4026.688130	25.240589
157.867378	4033.854670	25.245607
158.591806	4035.960993	25.250624
158.599723	4051.466873	25.255642
158.359171	4060.316941	25.260659
158.566472	4058.394280	25.265677
158.970500	4058.943934	25.270695
159.026658	4070.837828	25.275712
159.367466	4084.369721	25.280730
159.388108	4080.216207	25.285747
159.573716	4080.503175	25.290765
159.848592	4075.337939	25.295783
159.853202	4075.365864	25.300800
159.564879	4097.180005	25.305818
159.976958	4102.222985	25.310835
160.083435	4105.274572	25.315853
160.094128	4123.806979	25.320871
160.135370	4132.073481	25.325888
160.507965	4138.015854	25.330906
160.436624	4148.389370	25.335923
160.752634	4157.689407	25.340941
160.917641	4174.086266	25.345959
161.531524	4180.464534	25.350976
161.595810	4187.471259	25.355994
161.110480	4190.419307	25.361011
161.857712	4202.492919	25.366029
161.610708	4213.730247	25.371047
162.018770	4208.156010	25.376064
162.344759	4215.090437	25.381082
162.522633	4233.637960	25.386099
163.022138	4232.424150	25.391117
162.587450	4245.398291	25.396135
162.997943	4238.182374	25.401152
163.371069	4239.857343	25.406170
163.657998	4254.780225	25.411187
163.685388	4244.638062	25.416205
163.897845	4254.935890	25.421223
163.901808	4255.828751	25.426240
164.056657	4259.516725	25.431258
164.077644	4251.240948	25.436275
164.182116	4248.655665	25.441293
164.290637	4264.139751	25.446311
164.669181	4267.423608	25.451328
164.517195	4270.070420	25.456346
164.718778	4269.300689	25.461363
164.786171	4281.890523	25.466381
164.780886	4294.415928	25.471399
164.646709	4296.621241	25.476416
165.003596	4323.271716	25.481434
165.242907	4325.122187	25.486451
165.498781	4333.096544	25.491469
165.894569	4349.082026	25.496487
166.476638	4343.193429	25.501504
166.688323	4341.958139	25.506522
166.833607	4356.628556	25.511539
167.238411	4364.027379	25.516557
166.810991	4360.514858	25.521575
166.966924	4362.469849	25.526592
167.243492	4364.450246	25.531610
167.039771	4376.833004	25.536627
167.665842	4374.747264	25.541645
167.742876	4383.715332	25.546663
167.800900	4390.593700	25.551680
167.884901	4403.215752	25.556698
168.360638	4418.677518	25.561715
167.994152	4426.704623	25.566733
168.683482	4419.508350	25.571751
168.984568	4429.940829	25.576768
169.544074	4435.737416	25.581786
169.427612	4427.814375	25.586803
169.346349	4436.576700	25.591821
169.308253	4433.003551	25.596839
169.634395	4441.800296	25.601856
169.761393	4445.861939	25.606874
169.965909	4454.466150	25.611891
169.921032	4447.295797	25.616909
170.285920	4464.400389	25.621927
170.706278	4473.305580	25.626944
170.428825	4475.066077	25.631962
170.361434	4486.970011	25.636979
170.636654	4492.084911	25.641997
170.971396	4494.842203	25.647015
171.080996	4510.534652	25.652032
171.131850	4523.174574	25.657050
171.221642	4528.937004	25.662067
171.825501	4541.273051	25.667085
172.350321	4554.252689	25.672103
172.185834	4557.867342	25.677120
171.984443	4562.362061	25.682138
172.434362	4570.066427	25.687156
172.248708	4576.332588	25.692173
172.572754	4579.896437	25.697191
173.154540	4610.003286	25.702208
173.251565	4604.303752	25.707226
173.541135	4609.899379	25.712244
173.571477	4608.869063	25.717261
173.508211	4615.737992	25.722279
174.057055	4627.653394	25.727296
174.282434	4623.928714	25.732314
174.290601	4632.071181	25.737332
174.189037	4629.094965	25.742349
174.524678	4644.651334	25.747367
175.098576	4638.208388	25.752384
175.559227	4635.403464	25.757402
175.362759	4633.048051	25.762420
175.498243	4626.364040	25.767437
175.977156	4627.577523	25.772455
175.865321	4634.630780	25.777472
175.960163	4627.722678	25.782490
175.834205	4637.710428	25.787508
176.395361	4644.965081	25.792525
176.190169	4647.613919	25.797543
176.330723	4662.323197	25.802560
176.488331	4654.291103	25.807578
176.422330	4674.780357	25.812596
176.659974	4681.491989	25.817613
176.858589	4679.605335	25.822631
176.910803	4694.034847	25.827648
177.058114	4698.446902	25.832666
177.206984	4714.758384	25.837684
177.582341	4726.394689	25.842701
177.975386	4743.413095	25.847719
177.827588	4751.175876	25.852736
178.226464	4755.675036	25.857754
178.130859	4764.155674	25.862772
178.574588	4775.904467	25.867789
178.699732	4793.766360	25.872807
178.705175	4796.417146	25.877824
179.212396	4803.235205	25.882842
179.307603	4804.180172	25.887860
179.455852	4815.943430	25.892877
179.714000	4825.843073	25.897895
180.451029	4831.438546	25.902912
180.399424	4826.778453	25.907930
180.393069	4840.156639	25.912948
180.927102	4847.197803	25.917965
181.335499	4847.469038	25.922983
181.194568	4849.214629	25.928000
181.577699	4845.964059	25.933018
181.437577	4848.022011	25.938036
181.564484	4852.494096	25.943053
181.914539	4872.281197	25.948071
181.810961	4876.757608	25.953088
181.905012	4874.224362	25.958106
182.433593	4886.600774	25.963124
182.378226	4898.474698	25.968141
182.515062	4899.391093	25.973159
182.671939	4897.122674	25.978176
183.319306	4908.101241	25.983194
183.004870	4922.228183	25.988212
183.347398	4934.122250	25.993229
183.599078	4920.930379	25.998247
183.454172	4938.130571	26.003264
183.825875	4931.359168	26.008282
183.878945	4953.304260	26.013300
184.003651	4964.326357	26.018317
184.435714	4970.259747	26.023335
184.288903	4972.179870	26.028352
184.630152	4979.986555	26.033370
184.673792	4991.188582	26.038388
184.434833	5000.865852	26.043405
184.946981	5005.581017	26.048423
185.063647	5030.540192	26.053440
185.654665	5024.454283	26.058458
185.555309	5040.432241	26.063476
185.523208	5056.178789	26.068493
186.060299	5059.706408	26.073511
186.453803	5066.403387	26.078528
186.735519	5073.373446	26.083546
186.998611	5092.281045	26.088564
186.830196	5095.574456	26.093581
187.385252	5094.067860	26.098599
187.294053	5098.662344	26.103616
187.527059	5106.741611	26.108634
187.186927	5113.685398	26.113652
187.749711	5118.178069	26.118669
188.083651	5112.299450	26.123687
188.292909	5135.912319	26.128704
188.433046	5134.312495	26.133722
188.852730	5134.348398	26.138740
189.132285	5136.208470	26.143757
188.792382	5136.469953	26.148775
189.224587	5159.514697	26.153792
189.401305	5156.829656	26.158810
189.299079	5162.025606	26.163828
189.891067	5169.471373	26.168845
190.346876	5174.059626	26.173863
190.143293	5182.042761	26.178880
190.411000	5185.937465	26.183898
190.522701	5192.088099	26.188916
190.715737	5200.315673	26.193933
191.125202	5200.848737	26.198951
190.724428	5213.657305	26.203968
190.832517	5222.529415	26.208986
190.736979	5236.013315	26.214004
191.046381	5248.973330	26.219021
191.630862	5258.573040	26.224039
191.948644	5273.012170	26.229056
192.317992	5280.634689	26.234074
192.475446	5287.523169	26.239092
192.922275	5300.215618	26.244109
192.965562	5301.402277	26.249127
192.961156	5318.606206	26.254144
193.086926	5315.714431	26.259162
193.450887	5328.110462	26.264180
193.501363	5331.436122	26.269197
193.767794	5334.674501	26.274215
193.805694	5349.210927	26.279232
194.192610	5354.741125	26.284250
194.449490	5360.351544	26.289268
194.416265	5365.259035	26.294285
194.817132	5370.562953	26.299303
194.841106	5378.842181	26.304320
195.395440	5389.122151	26.309338
195.253872	5401.562216	26.314356
195.353156	5398.873413	26.319373
195.705576	5401.110422	26.324391
195.882644	5423.049402	26.329408
196.442071	5423.363421	26.334426
196.654194	5424.747915	26.339444
197.194855	5429.562919	26.344461
197.142290	5437.967726	26.349479
197.208725	5446.063608	26.354496
196.889177	5441.624996	26.359514
197.542829	5437.552541	26.364532
197.657687	5457.777780	26.369549
198.070894	5461.154313	26.374567
198.025878	5462.613567	26.379584
198.071187	5459.759548	26.384602
198.557104	5473.673927	26.389620
198.736279	5485.827373	26.394637
198.591329	5491.080573	26.399655
198.441105	5497.016409	26.404672
199.321388	5512.927489	26.409690
199.473108	5517.566329	26.414708
199.257237	5515.785157	26.419725
199.536049	5529.027912	26.424743
199.660618	5543.992917	26.429760
199.957032	5538.767098	26.434778
200.100193	5557.090950	26.439796
199.987958	5574.570747	26.444813
200.576844	5577.130811	26.449831
200.809392	5591.091040	26.454848
200.806617	5595.163676	26.459866
201.052979	5594.153334	26.464884
201.119320	5609.730362	26.469901
201.551074	5610.995450	26.474919
201.602857	5628.446606	26.479936
201.831503	5634.980068	26.484954
202.395971	5638.977026	26.489972
202.250279	5643.993643	26.494989
202.502739	5651.814442	26.500007
202.805510	5660.912137	26.505024
203.130664	5666.865559	26.510042
203.755794	5673.968622	26.515060
203.690226	5679.203204	26.520077
204.288661	5672.339409	26.525095
204.624024	5676.327853	26.530112
204.645849	5679.253996	26.535130
204.869048	5673.521858	26.540148
204.650431	5681.296061	26.545165
205.181270	5678.767302	26.550183
205.469495	5680.925957	26.555200
205.421325	5694.267088	26.560218
205.192480	5691.174780	26.565236
205.678149	5695.322909	26.570253
205.683674	5708.968193	26.575271
206.111089	5715.069852	26.580288
206.356378	5713.857650	26.585306
206.654145	5717.100688	26.590324
207.404302	5726.463363	26.595341
207.621023	5730.688094	26.600359
208.068084	5729.899026	26.605376
208.048111	5726.963588	26.610394
208.216041	5724.939559	26.615412
208.156522	5718.929450	26.620429
208.178280	5724.567119	26.625447
208.248932	5724.449031	26.630464
208.074619	5721.910100	26.635482
208.494709	5718.858802	26.640500
208.699685	5742.286888	26.645517
208.854115	5742.591366	26.650535
209.001622	5749.664653	26.655552
209.165142	5762.467822	26.660570
208.900364	5761.723289	26.665588
209.061134	5773.807191	26.670605
209.368319	5787.613905	26.675623
209.464753	5807.586716	26.680640
209.870909	5824.256870	26.685658
210.486657	5844.161496	26.690676
210.391470	5861.001278	26.695693
210.906898	5868.086775	26.700711
210.989239	5876.988466	26.705728
210.626757	5893.582641	26.710746
211.092567	5904.653214	26.715764
211.472478	5919.326245	26.720781
211.493298	5924.481158	26.725799
211.706723	5940.670051	26.730816
212.261388	5955.533712	26.735834
213.052589	5954.290164	26.740852
212.960262	5975.492065	26.745869
213.345299	5978.847829	26.750887
213.675873	5979.573130	26.755904
213.709251	5973.769438	26.760922
214.016970	5991.888181	26.765940
213.769631	6012.675487	26.770957
214.008421	6009.462970	26.775975
214.221433	6009.537368	26.780992
214.364083	6027.189410	26.786010
214.551652	6028.375749	26.791028
214.544487	6043.588953	26.796045
214.961098	6051.384368	26.801063
215.097655	6061.057398	26.806080
215.383744	6075.884055	26.811098
215.849848	6088.103714	26.816116
215.744994	6087.157496	26.821133
215.725412	6100.172495	26.826151
215.718893	6099.504535	26.831168
216.162872	6130.231970	26.836186
216.954542	6120.787346	26.841204
217.207806	6126.180756	26.846221
217.681744	6136.473668	26.851239
218.101595	6134.369337	26.856256
218.150071	6145.142016	26.861274
218.680126	6131.596579	26.866292
218.557052	6134.905213	26.871309
219.038315	6130.553251	26.876327
219.071174	6130.510491	26.881344
219.247923	6146.481155	26.886362
219.771539	6157.403990	26.891380
219.675765	6159.748753	26.896397
219.275653	6149.021813	26.901415
220.039413	6154.228427	26.906432
219.652903	6173.793859	26.911450
220.385358	6178.108861	26.916468
220.194195	6188.439061	26.921485
220.255712	6202.738898	26.926503
221.029117	6208.401744	26.931520
220.665243	6231.177203	26.936538
221.320810	6232.230718	26.941556
221.301807	6252.237771	26.946573
221.258008	6261.765370	26.951591
221.862052	6278.761837	26.956608
221.809412	6298.676320	26.961626
222.431946	6303.582983	26.966644
222.431282	6308.798171	26.971661
222.970209	6312.287873	26.976679
222.978802	6311.860618	26.981696
223.009394	6330.512130	26.986714
223.720528	6329.865013	26.991732
223.620306	6347.968704	26.996749
223.812050	6356.698918	27.001767
224.380824	6369.587785	27.006784
224.273911	6388.197630	27.011802
224.229963	6383.861086	27.016820
224.971884	6404.895723	27.021837
225.000231	6412.590749	27.026855
225.012882	6417.778641	27.031872
225.427609	6431.960532	27.036890
225.911990	6432.564048	27.041908
225.838502	6449.546202	27.046925
226.383141	6455.361540	27.051943
226.565360	6456.116272	27.056960
226.695938	6468.751447	27.061978
226.821311	6493.944868	27.066996
227.001680	6497.540938	27.072013
227.007303	6511.205746	27.077031
227.402335	6521.448027	27.082048
227.589186	6528.386065	27.087066
228.040219	6524.464875	27.092084
228.394039	6534.745147	27.097101
228.709042	6555.720154	27.102119
228.829477	6560.752409	27.107136
228.662782	6555.601558	27.112154
228.795673	6568.763616	27.117172
229.002588	6583.208420	27.122189
229.326439	6594.642443	27.127207
229.730329	6604.340433	27.132224
229.611090	6617.990036	27.137242
229.877101	6620.663655	27.142260
230.040180	6641.681354	27.147277
229.766322	6653.461010	27.152295
230.752115	6661.392201	27.157312
230.833994	6686.895708	27.162330
231.230569	6688.917659	27.167348
231.617237	6688.870322	27.172365
231.493797	6713.493530	27.177383
232.199366	6717.172027	27.182400
231.862980	6739.429286	27.187418
232.504170	6743.992235	27.192436
232.701478	6757.917806	27.197453
232.538535	6771.432274	27.202471
233.232387	6772.805010	27.207488
233.532974	6795.165201	27.212506
233.786671	6804.454202	27.217524
233.802778	6804.448773	27.222541
234.143966	6818.557181	27.227559
234.782702	6824.610531	27.232576
234.582652	6843.674130	27.237594
235.008237	6847.768744	27.242612
235.417726	6848.437601	27.247629
235.201759	6862.860073	27.252647
235.561159	6871.876953	27.257664
235.565516	6880.352480	27.262682
235.826259	6890.145514	27.267700
236.205387	6905.624442	27.272717
236.384346	6923.214875	27.277735
237.005027	6917.758243	27.282752
236.877980	6929.849838	27.287770
237.053377	6939.975023	27.292788
237.381080	6952.314671	27.297805
237.878846	6972.551422	27.302823
238.162131	6972.457046	27.307840
238.170349	6983.507970	27.312858
238.558671	6991.336604	27.317876
238.914189	6995.255909	27.322893
238.943037	7016.544324	27.327911
239.316788	7024.337360	27.332928
239.423394	7036.013831	27.337946
239.528010	7044.375964	27.342964
240.054937	7051.362273	27.347981
239.792729	7062.988849	27.352999
240.301081	7072.793941	27.358016
240.592953	7091.579174	27.363034
240.860948	7095.894103	27.368052
241.338224	7101.341318	27.373069
240.943176	7122.878947	27.378087
241.275870	7131.259277	27.383104
241.550890	7148.130996	27.388122
241.823468	7153.581685	27.393140
242.153850	7174.741261	27.398157
242.210262	7188.108237	27.403175
242.689081	7200.774935	27.408192
242.922131	7218.767619	27.413210
243.011581	7220.988975	27.418228
243.478335	7236.763912	27.423245
243.609016	7257.799989	27.428263
244.055409	7265.805955	27.433280
244.402484	7264.745119	27.438298
244.605575	7279.146872	27.443316
245.091646	7282.471366	27.448333
244.759687	7297.120590	27.453351
245.715857	7300.075154	27.458368
245.775216	7310.982569	27.463386
245.860234	7318.637584	27.468404
246.527796	7319.900810	27.473421
246.177233	7308.666689	27.478439
246.568615	7318.988907	27.483456
246.827800	7327.207144	27.488474
247.478162	7334.123835	27.493492
247.468778	7333.175316	27.498509
247.670962	7337.380587	27.503527
247.964273	7347.301384	27.508544
248.090985	7357.399653	27.513562
248.184463	7354.572565	27.518580
248.249360	7367.281723	27.523597
248.791592	7379.323083	27.528615
248.994018	7376.182285	27.533632
249.096949	7392.645374	27.538650
249.088000	7406.275235	27.543668
249.031654	7408.699254	27.548685
249.085801	7425.312027	27.553703
249.907194	7445.091679	27.558720
250.016404	7462.302034	27.563738
250.265002	7474.966883	27.568756
250.421931	7492.441329	27.573773
250.715915	7516.902762	27.578791
250.867230	7525.434629	27.583808
251.100393	7541.075724	27.588826
251.807190	7558.748747	27.593844
252.111879	7567.383032	27.598861
252.458527	7571.925753	27.603879
252.928949	7574.829712	27.608896
253.274053	7581.175269	27.613914
253.527304	7594.840215	27.618932
254.083470	7594.924336	27.623949
254.104841	7608.426508	27.628967
254.308056	7612.729545	27.633984
254.535280	7627.383525	27.639002
254.236657	7638.842503	27.644020
255.050903	7639.056918	27.649037
255.011299	7662.926470	27.654055
255.323536	7663.342162	27.659072
255.510814	7671.625416	27.664090
255.565553	7684.055408	27.669108
255.908019	7696.974134	27.674125
256.156455	7711.264988	27.679143
256.217314	7716.603588	27.684160
256.487855	7727.456273	27.689178
256.692820	7737.277386	27.694196
257.434747	7746.961238	27.699213
257.135955	7761.754043	27.704231
257.719669	7777.145032	27.709248
258.203277	7787.178503	27.714266
258.189083	7798.422823	27.719284
258.659472	7810.005267	27.724301
258.982915	7826.645929	27.729319
259.022135	7834.494550	27.734336
259.313481	7850.524625	27.739354
259.622009	7863.950708	27.744372
259.944294	7867.461814	27.749389
260.066786	7876.143552	27.754407
260.395428	7888.401605	27.759424
260.749835	7898.483664	27.764442
260.938756	7912.076780	27.769460
261.462302	7907.484206	27.774477
261.400908	7923.859703	27.779495
261.855208	7941.455599	27.784512
262.178389	7941.032997	27.789530
262.356856	7963.091614	27.794548
262.936550	7963.377279	27.799565
262.624420	7966.204245	27.804583
263.179932	7970.651409	27.809600
263.131738	7989.809360	27.814618
263.320203	7990.585284	27.819636
263.370180	8003.101471	27.824653
263.598310	8029.269136	27.829671
263.640112	8028.520973	27.834688
264.360208	8041.573726	27.839706
264.166352	8059.352725	27.844724
264.683140	8073.014882	27.849741
264.869820	8086.374858	27.854759
265.246777	8100.301894	27.859776
266.058564	8115.824980	27.864794
266.478851	8120.779412	27.869812
266.476155	8136.495617	27.874829
266.777925	8158.740476	27.879847
266.465560	8154.300081	27.884864
267.005688	8168.934190	27.889882
267.170140	8174.825056	27.894900
267.684167	8193.166419	27.899917
267.910408	8197.800653	27.904935
267.847366	8218.324983	27.909952
268.305945	8226.105325	27.914970
268.448812	8244.264590	27.919988
268.672531	8255.661571	27.925005
269.079099	8279.910755	27.930023
269.145429	8284.187907	27.935040
269.638977	8300.578366	27.940058
269.547698	8317.489245	27.945076
270.416146	8330.888481	27.950093
270.730488	8356.759056	27.955111
271.178595	8361.889173	27.960128
271.506484	8387.707170	27.965146
271.244142	8395.227290	27.970164
271.366628	8398.785390	27.975181
271.834984	8413.639233	27.980199
271.999829	8435.918372	27.985216
272.528164	8441.979980	27.990234
272.508675	8455.659614	27.995252
273.076101	8467.666197	28.000269
273.084242	8484.028208	28.005287
273.391726	8500.874016	28.010304
274.025764	8520.440905	28.015322
274.280514	8531.593288	28.020340
274.710122	8546.270161	28.025357
274.825131	8553.627413	28.030375
274.865114	8566.394947	28.035392
275.196571	8572.212584	28.040410
275.662424	8593.807322	28.045428
275.935111	8597.417846	28.050445
276.355529	8615.887859	28.055463
276.519458	8634.429394	28.060480
276.915644	8639.987565	28.065498
277.024541	8651.847816	28.070516
277.766663	8646.700113	28.075533
277.795131	8658.891757	28.080551
278.009485	8676.592011	28.085568
278.529847	8677.600431	28.090586
278.571100	8692.549407	28.095604
278.994054	8699.520966	28.100621
279.196464	8701.194522	28.105639
279.173101	8718.758186	28.110656
279.707432	8724.026522	28.115674
280.067572	8731.727691	28.120692
280.293512	8744.715809	28.125709
280.474616	8752.520631	28.130727
280.588203	8774.318807	28.135744
280.805944	8781.388645	28.140762
281.002898	8786.681109	28.145780
281.344992	8803.865931	28.150797
281.729805	8803.433718	28.155815
281.318572	8824.132898	28.160832
281.755851	8835.945300	28.165850
282.026932	8850.940708	28.170868
282.435073	8866.520959	28.175885
282.530636	8873.720353	28.180903
283.197863	8910.239431	28.185920
283.317515	8905.747380	28.190938
283.626413	8924.948577	28.195956
283.937015	8946.324799	28.200973
284.437675	8962.730526	28.205991
284.530655	8974.239862	28.211008
285.313886	8982.651925	28.216026
285.782465	8982.961225	28.221044
285.853981	8994.906445	28.226061
286.085079	9001.885887	28.231079
286.568170	9007.083354	28.236096
286.809865	9026.781321	28.241114
286.697816	9031.992520	28.246132
287.133131	9037.456320	28.251149
287.654352	9055.680608	28.256167
287.621839	9075.231887	28.261184
288.043108	9086.898556	28.266202
288.407210	9091.858841	28.271220
288.677338	9098.046110	28.276237
288.915325	9115.721005	28.281255
288.951035	9135.324870	28.286272
289.447930	9139.541501	28.291290
289.522278	9153.121798	28.296308
289.682646	9166.789742	28.301325
289.907242	9188.069132	28.306343
290.079909	9207.613864	28.311360
290.577579	9222.735314	28.316378
290.698333	9250.815740	28.321396
290.828469	9264.425319	28.326413
291.285052	9292.188319	28.331431
291.300738	9310.630479	28.336448
292.178358	9326.485319	28.341466
292.350566	9337.938346	28.346484
292.366996	9366.912892	28.351501
293.068481	9377.910992	28.356519
293.144732	9403.570679	28.361536
293.514173	9416.328551	28.366554
293.585375	9431.052455	28.371572
294.148568	9452.936136	28.376589
294.761441	9456.591742	28.381607
294.654719	9480.758239	28.386624
295.339105	9486.050793	28.391642
295.776433	9516.715466	28.396660
295.933772	9520.997679	28.401677
296.353874	9534.177129	28.406695
296.530219	9546.377907	28.411712
296.703436	9563.548683	28.416730
296.629578	9575.213813	28.421748
297.243484	9590.983647	28.426765
297.671715	9609.803893	28.431783
297.377052	9629.096628	28.436800
298.018077	9640.858883	28.441818
298.481545	9656.172290	28.446836
298.796283	9669.753427	28.451853
299.426371	9679.787228	28.456871
300.019364	9698.338803	28.461888
300.308230	9690.694524	28.466906
300.170882	9695.834073	28.471924
300.685721	9727.753093	28.476941
300.805153	9722.433674	28.481959
300.834176	9735.238449	28.486976
301.513915	9746.432749	28.491994
301.461369	9755.821436	28.497012
301.119880	9767.020031	28.502029
301.613392	9775.490193	28.507047
302.111016	9788.616711	28.512064
302.626995	9793.796652	28.517082
302.886935	9824.265284	28.522100
303.383085	9832.618242	28.527117
303.948162	9848.645324	28.532135
303.932814	9853.608058	28.537152
304.300998	9860.765393	28.542170
304.365766	9875.916886	28.547188
304.359030	9890.700647	28.552205
304.962123	9897.237324	28.557223
304.805464	9919.530413	28.562240
305.383385	9939.495892	28.567258
305.405636	9960.697164	28.572276
305.869489	9977.851491	28.577293
306.531634	10007.099071	28.582311
306.863898	10023.430922	28.587328
307.450464	10032.559225	28.592346
307.897172	10047.095706	28.597364
307.746278	10055.277969	28.602381
308.489596	10062.995816	28.607399
308.519388	10084.568620	28.612416
309.063130	10093.498394	28.617434
309.089314	10105.975504	28.622452
309.183986	10125.287073	28.627469
309.441130	10137.753505	28.632487
310.115009	10148.709004	28.637504
310.238454	10163.706358	28.642522
310.927403	10172.859837	28.647540
310.902629	10198.820511	28.652557
311.030432	10207.679329	28.657575
311.334302	10236.597851	28.662592
311.716149	10244.359420	28.667610
312.385495	10263.108060	28.672628
312.398289	10278.324804	28.677645
312.832214	10290.545959	28.682663
313.267444	10308.746981	28.687680
313.625199	10317.907890	28.692698
313.720846	10328.404133	28.697716
314.038576	10340.772864	28.702733
314.386801	10360.840862	28.707751
314.290927	10378.745750	28.712768
314.828507	10401.749096	28.717786
315.290775	10415.680382	28.722804
315.669660	10434.105001	28.727821
316.021106	10447.734668	28.732839
315.963681	10469.450949	28.737856
316.342080	10495.289278	28.742874
316.791930	10504.442256	28.747892
316.850793	10519.393118	28.752909
317.481188	10532.363724	28.757927
317.636663	10562.733004	28.762944
317.800673	10572.167323	28.767962
318.862205	10592.645494	28.772980
318.958903	10616.071374	28.777997
319.270467	10621.469661	28.783015
319.664027	10648.338319	28.788032
319.743854	10654.419966	28.793050
320.235865	10672.855626	28.798068
320.969081	10670.392582	28.803085
321.513382	10670.974297	28.808103
321.822977	10686.760867	28.813120
322.098303	10695.094917	28.818138
322.377425	10690.258709	28.823156
322.352916	10697.228066	28.828173
322.822436	10705.276136	28.833191
322.955622	10722.703652	28.838208
323.155816	10720.743524	28.843226
323.461365	10721.441347	28.848244
323.419742	10736.019661	28.853261
324.051921	10743.748782	28.858279
324.185594	10761.062590	28.863296
324.547550	10776.888446	28.868314
324.396071	10794.372977	28.873332
324.831793	10827.095565	28.878349
325.671398	10825.689474	28.883367
325.992716	10830.922115	28.888384
326.262137	10848.502199	28.893402
326.928505	10869.013780	28.898420
327.232792	10879.976732	28.903437
327.533748	10886.870230	28.908455
327.790917	10898.048922	28.913472
327.882870	10903.497268	28.918490
328.497975	10922.220287	28.923508
328.525087	10945.726879	28.928525
328.717199	10944.914151	28.933543
329.127849	10965.977161	28.938560
329.521342	10978.852348	28.943578
329.681441	10992.265920	28.948596
329.974952	11020.066362	28.953613
330.199928	11036.819965	28.958631
330.698859	11055.207564	28.963648
330.841874	11070.161553	28.968666
331.377475	11085.193365	28.973684
331.579453	11112.310387	28.978701
332.233301	11123.980021	28.983719
332.627247	11142.832417	28.988736
332.700544	11167.996107	28.993754
333.459065	11172.545064	28.998772
333.388137	11193.781189	29.003789
333.517430	11200.976233	29.008807
333.949922	11227.321831	29.013824
334.221228	11250.601337	29.018842
334.991637	11270.026759	29.023860
335.342572	11286.896750	29.028877
335.374453	11297.864467	29.033895
335.868079	11321.734643	29.038912
335.664235	11348.618377	29.043930
336.411134	11354.968991	29.048948
336.374621	11385.082160	29.053965
336.832035	11402.813479	29.058983
336.998939	11422.380379	29.064000
337.387223	11449.569925	29.069018
338.015899	11467.400946	29.074036
338.007127	11495.700687	29.079053
338.279651	11504.963862	29.084071
338.672024	11539.866858	29.089088
339.136660	11568.497177	29.094106
339.787684	11584.149254	29.099124
339.788934	11605.715627	29.104141
340.271044	11619.581574	29.109159
340.657040	11627.747248	29.114176
341.282420	11649.184928	29.119194
341.785521	11660.578396	29.124212
341.993784	11680.729597	29.129229
342.698696	11707.557623	29.134247
343.215587	11714.133626	29.139264
343.554397	11725.227477	29.144282
343.866885	11727.139940	29.149300
344.514596	11740.004493	29.154317
344.552287	11747.081389	29.159335
344.793097	11753.239375	29.164352
344.989918	11754.633054	29.169370
345.596373	11766.291524	29.174388
345.216103	11777.184751	29.179405
345.518869	11798.546523	29.184423
346.088712	11798.846432	29.189440
346.158394	11825.239882	29.194458
346.569411	11825.463473	29.199476
346.682474	11859.554831	29.204493
347.042508	11869.432933	29.209511
347.181200	11892.200242	29.214528
347.479396	11911.545124	29.219546
348.097836	11936.602872	29.224564
348.202925	11966.034979	29.229581
348.725002	11977.725664	29.234599
349.436246	11995.803262	29.239616
349.581776	12016.059320	29.244634
350.264633	12019.211952	29.249652
350.299450	12051.361248	29.254669
350.762697	12065.650432	29.259687
351.170196	12086.241545	29.264704
351.255642	12109.450008	29.269722
351.741921	12124.480863	29.274740
352.002374	12154.059591	29.279757
352.358496	12165.769914	29.284775
352.785473	12189.490531	29.289792
353.385737	12208.855004	29.294810
353.469267	12224.305459	29.299828
353.756586	12254.259086	29.304845
353.991047	12279.579165	29.309863
354.223676	12292.676079	29.314880
354.639901	12324.595947	29.319898
355.298419	12345.546136	29.324916
355.780882	12371.664523	29.329933
355.796840	12382.281688	29.334951
356.331122	12394.507545	29.339968
356.546857	12418.210814	29.344986
357.192953	12439.541969	29.350004
357.461675	12470.203009	29.355021
358.180537	12485.990537	29.360039
358.614031	12506.578063	29.365056
358.580323	12516.047301	29.370074
359.524429	12528.354700	29.375092
359.639289	12548.136129	29.380109
360.136573	12554.939682	29.385127
360.613045	12580.184596	29.390144
360.721246	12591.813788	29.395162
360.830936	12604.759540	29.400180
361.522597	12619.581983	29.405197
362.352922	12624.596945	29.410215
362.842739	12633.466865	29.415232
363.045641	12653.222067	29.420250
363.408259	12647.687125	29.425268
363.522286	12663.126878	29.430285
363.855709	12677.338849	29.435303
364.626558	12694.833129	29.440320
364.525365	12719.037679	29.445338
364.495533	12717.318413	29.450356
364.924684	12729.873477	29.455373
364.931868	12752.027586	29.460391
365.638019	12774.398157	29.465408
365.542684	12800.626040	29.470426
366.173979	12818.126373	29.475444
366.536820	12848.656538	29.480461
366.867233	12868.038440	29.485479
367.407038	12883.020519	29.490496
367.737793	12906.444398	29.495514
368.080713	12927.011750	29.500532
368.611826	12939.200563	29.505549
368.713726	12957.430794	29.510567
369.271540	12967.752357	29.515584
369.478636	12988.580916	29.520602
369.594747	13012.313073	29.525620
370.168570	13022.827959	29.530637
370.004046	13044.863884	29.535655
370.861559	13060.848201	29.540672
370.816800	13101.863089	29.545690
371.471921	13117.263184	29.550708
371.656612	13140.394309	29.555725
371.537984	13169.831546	29.560743
372.281609	13193.740972	29.565760
372.472131	13221.958597	29.570778
373.372822	13240.926840	29.575796
373.762103	13260.258929	29.580813
373.855329	13292.407562	29.585831
374.401936	13318.732013	29.590848
374.673319	13334.242553	29.595866
375.112067	13359.857541	29.600884
375.268005	13385.106066	29.605901
375.787711	13403.830629	29.610919
376.459078	13431.433708	29.615936
376.691657	13454.560920	29.620954
377.290937	13472.606846	29.625972
377.723898	13486.188140	29.630989
377.970611	13511.972179	29.636007
378.331706	13531.867883	29.641024
378.606777	13566.641320	29.646042
379.344644	13591.812157	29.651060
379.602336	13603.800807	29.656077
380.229215	13626.787896	29.661095
381.164405	13639.959531	29.666112
380.956787	13664.425018	29.671130
381.408528	13678.253004	29.676148
381.767047	13690.860759	29.681165
382.396991	13705.586298	29.686183
382.910353	13713.846740	29.691200
383.181489	13738.035681	29.696218
383.530014	13741.436452	29.701236
384.257399	13752.824698	29.706253
384.596882	13768.729210	29.711271
384.730131	13787.836430	29.716288
385.247507	13801.824819	29.721306
385.442708	13821.999292	29.726324
386.157568	13827.102033	29.731341
386.345965	13852.728242	29.736359
386.820280	13876.402559	29.741376
386.974409	13888.110664	29.746394
386.817554	13900.795636	29.751412
387.131081	13924.387674	29.756429
387.724776	13948.514035	29.761447
388.839550	13944.437455	29.766464
388.834794	13978.879413	29.771482
389.729429	13976.185559	29.776500
390.239200	13999.826089	29.781517
390.567333	14011.826139	29.786535
391.203914	14015.478967	29.791552
391.535800	14035.007105	29.796570
391.416076	14034.407013	29.801588
391.702245	14053.462272	29.806605
391.796728	14067.655646	29.811623
391.897320	14084.232373	29.816640
392.166643	14113.790686	29.821658
392.428615	14136.149916	29.826676
393.174381	14166.243634	29.831693
393.196880	14189.982367	29.836711
393.645496	14206.252378	29.841728
394.117562	14235.750895	29.846746
394.458453	14257.463217	29.851764
395.228171	14272.739044	29.856781
395.291972	14299.338981	29.861799
395.440375	14314.781046	29.866816
395.528799	14341.525637	29.871834
395.770216	14368.928586	29.876852
396.581400	14393.618528	29.881869
396.787543	14418.131102	29.886887
396.898988	14447.796622	29.891904
397.284684	14474.823559	29.896922
397.902009	14505.866284	29.901940
398.669605	14525.841863	29.906957
399.135809	14564.942364	29.911975
399.497825	14585.653819	29.916992
400.132978	14611.549416	29.922010
400.522995	14637.249513	29.927028
400.907345	14653.668870	29.932045
401.437328	14686.765621	29.937063
401.914486	14704.402234	29.942080
402.740986	14719.555890	29.947098
402.952110	14737.556078	29.952116
403.683248	14751.031857	29.957133
403.899209	14773.534799	29.962151
404.138533	14786.247109	29.967168
404.345360	14810.696921	29.972186
404.529193	14835.178766	29.977204
405.701032	14855.461261	29.982221
405.432762	14878.775558	29.987239
405.847864	14894.271317	29.992256
405.966592	14923.124802	29.997274
406.457309	14951.888838	30.002292
407.228891	14981.139762	30.007309
407.549966	14997.003957	30.012327
408.048674	15021.392807	30.017344
409.109778	15039.845215	30.022362
409.337474	15047.048515	30.027380
409.882868	15069.127857	30.032397
410.273387	15089.140626	30.037415
410.527206	15105.520689	30.042432
410.800838	15117.924695	30.047450
411.215034	15134.396668	30.052468
411.936282	15154.828587	30.057485
412.183941	15180.955828	30.062503
412.483641	15204.797947	30.067520
412.826329	15214.393109	30.072538
412.797602	15229.775062	30.077556
413.381543	15260.682099	30.082573
413.666465	15280.582022	30.087591
414.251162	15306.546428	30.092608
414.902477	15325.555591	30.097626
415.088087	15336.198529	30.102644
415.856551	15346.842321	30.107661
416.371051	15382.210291	30.112679
416.700409	15403.016150	30.117696
417.195283	15420.944385	30.122714
416.949592	15445.029622	30.127732
417.759822	15453.336199	30.132749
418.312257	15488.869005	30.137767
418.605934	15507.166575	30.142784
419.177541	15525.837783	30.147802
419.172321	15552.620758	30.152820
419.811631	15572.907970	30.157837
419.961459	15595.419020	30.162855
420.321270	15624.056012	30.167872
421.234205	15637.450430	30.172890
421.518807	15658.010873	30.177908
421.622817	15675.087459	30.182925
421.902180	15697.107880	30.187943
422.315700	15719.274830	30.192960
422.777458	15738.174951	30.197978
422.921744	15765.329734	30.202996
423.732037	15786.016923	30.208013
424.298962	15805.061811	30.213031
424.442615	15824.895862	30.218048
425.592284	15839.071566	30.223066
425.418260	15867.135105	30.228084
425.946617	15881.713921	30.233101
426.250239	15898.614348	30.238119
426.949684	15924.103777	30.243136
427.192137	15951.663597	30.248154
427.480940	15968.566393	30.253172
428.194494	15993.339938	30.258189
428.297249	16024.531573	30.263207
428.513634	16041.085658	30.268224
429.807274	16058.173200	30.273242
430.096600	16071.889250	30.278260
430.827623	16091.812161	30.283277
431.404438	16100.569103	30.288295
431.793025	16114.222355	30.293312
432.243715	16118.792031	30.298330
432.270005	16140.116468	30.303348
432.898301	16150.732001	30.308365
433.304038	16174.764116	30.313383
433.618822	16195.996326	30.318400
433.941604	16217.555785	30.323418
434.041264	16239.478473	30.328436
434.426924	16259.856438	30.333453
434.882007	16279.276106	30.338471
435.368140	16299.745856	30.343488
436.111407	16328.725321	30.348506
436.144477	16363.124632	30.353524
436.569256	16383.881961	30.358541
437.417512	16404.358616	30.363559
437.792601	16425.701712	30.368576
438.571209	16452.749243	30.373594
439.101941	16475.536819	30.378612
439.408767	16490.794902	30.383629
439.734643	16512.628992	30.388647
439.730512	16541.102927	30.393664
440.677458	16549.372910	30.398682
440.741495	16581.550586	30.403700
441.346383	16601.234675	30.408717
441.939536	16628.927219	30.413735
442.024543	16651.383274	30.418752
442.237661	16676.222978	30.423770
442.670046	16707.999252	30.428788
442.966762	16736.616146	30.433805
443.483357	16767.940386	30.438823
443.884543	16796.825366	30.443840
444.547952	16830.508326	30.448858
444.634409	16862.525058	30.453876
445.206631	16881.409112	30.458893
445.599719	16912.320105	30.463911
446.154357	16948.335364	30.468928
446.469680	16971.539239	30.473946
447.223975	17011.626403	30.478964
448.154247	17030.979173	30.483981
448.869617	17044.541155	30.488999
449.307865	17059.466541	30.494016
450.024499	17069.219198	30.499034
450.159411	17098.411399	30.504052
450.434680	17111.520790	30.509069
450.868014	17129.409673	30.514087
451.008467	17147.950601	30.519104
451.311804	17173.231727	30.524122
452.029222	17201.622735	30.529140
452.154371	17217.696151	30.534157
452.594291	17236.594835	30.539175
452.558517	17269.929427	30.544192
453.213230	17293.999988	30.549210
453.665343	17331.048973	30.554228
454.466958	17353.454298	30.559245
454.790311	17366.638500	30.564263
455.244751	17401.618411	30.569280
455.946943	17422.684275	30.574298
456.039326	17451.883632	30.579316
456.478169	17487.131446	30.584333
456.979396	17499.432076	30.589351
457.313691	17534.130867	30.594368
458.018794	17552.827491	30.599386
458.266691	17586.333251	30.604404
458.859566	17621.560489	30.609421
459.457747	17647.898684	30.614439
459.741388	17667.059015	30.619456
460.278444	17690.633538	30.624474
460.940043	17718.598111	30.629492
461.518911	17744.478289	30.634509
462.234518	17767.974572	30.639527
462.348654	17802.651266	30.644544
462.597320	17815.727375	30.649562
463.305539	17843.697507	30.654580
463.677206	17877.999429	30.659597
464.119745	17896.440351	30.664615
464.441337	17929.076084	30.669632
464.949653	17950.008460	30.674650
465.579401	17988.433491	30.679668
465.923485	18004.874627	30.684685
466.404261	18045.237105	30.689703
466.659097	18072.191572	30.694720
467.654267	18090.395031	30.699738
467.792452	18135.410048	30.704756
468.203436	18159.838660	30.709773
468.577867	18184.765748	30.714791
468.964024	18224.909588	30.719808
469.446367	18258.285253	30.724826
470.292706	18295.344207	30.729844
470.342594	18317.605510	30.734861
471.193938	18353.255015	30.739879
471.590403	18392.557382	30.744896
472.138673	18425.133393	30.749914
472.394096	18452.220964	30.754932
473.087984	18480.137391	30.759949
473.670541	18506.018015	30.764967
473.828813	18538.793915	30.769984
474.296660	18556.505019	30.775002
474.680209	18586.422015	30.780020
475.396911	18627.159614	30.785037
475.952032	18658.945263	30.790055
476.458641	18686.360472	30.795072
476.950867	18715.906968	30.800090
477.358228	18751.057747	30.805108
478.029613	18782.768641	30.810125
478.653933	18796.905140	30.815143
478.799487	18827.200706	30.820160
479.447282	18849.388490	30.825178
479.835255	18881.219478	30.830196
480.822041	18915.894978	30.835213
481.253301	18931.192480	30.840231
481.365878	18968.581752	30.845248
481.972543	18979.379115	30.850266
482.553013	19007.339230	30.855284
483.374598	19020.977679	30.860301
483.825728	19036.076324	30.865319
484.235235	19057.082138	30.870336
484.482640	19067.581691	30.875354
485.054798	19095.852793	30.880372
485.474200	19114.260573	30.885389
485.728131	19125.890003	30.890407
486.308991	19150.084935	30.895424
486.688616	19171.998953	30.900442
487.171309	19187.579264	30.905460
487.018007	19216.203551	30.910477
488.001676	19246.445108	30.915495
488.350616	19280.753049	30.920512
488.886750	19305.473191	30.925530
489.083340	19339.413255	30.930548
489.234156	19368.653783	30.935565
489.992391	19397.332280	30.940583
490.234384	19437.576884	30.945600
490.716634	19459.645830	30.950618
491.329465	19486.527575	30.955636
492.578541	19509.355372	30.960653
493.415355	19533.441440	30.965671
493.333667	19565.782592	30.970688
494.215090	19593.039647	30.975706
494.710206	19610.020919	30.980724
495.352415	19640.480510	30.985741
495.427698	19661.810677	30.990759
496.246417	19704.063571	30.995776
496.385563	19729.155627	31.000794
496.576329	19745.539976	31.005812
497.456236	19784.883619	31.010829
498.341598	19808.166417	31.015847
498.701281	19839.933880	31.020864
499.451154	19865.644959	31.025882
499.669571	19881.304876	31.030900
499.845352	19910.049532	31.035917
500.401563	19934.640989	31.040935
501.078441	19969.707786	31.045952
501.394537	20006.157582	31.050970
502.025738	20024.729108	31.055988
502.486508	20055.009100	31.061005
502.920721	20080.826466	31.066023
503.344907	20121.543237	31.071040
503.591719	20153.474095	31.076058
504.301139	20184.069387	31.081076
504.826251	20219.747835	31.086093
505.538345	20249.729965	31.091111
505.942602	20270.586274	31.096128
506.184450	20298.702050	31.101146
507.040434	20339.996495	31.106164
507.396494	20374.747516	31.111181
508.089385	20399.324599	31.116199
508.993336	20430.648163	31.121216
509.215701	20468.945658	31.126234
509.595276	20490.621079	31.131252
510.132033	20509.485767	31.136269
510.538465	20547.066085	31.141287
510.870221	20580.589221	31.146304
511.155939	20610.789918	31.151322
511.834056	20649.901357	31.156340
512.278905	20684.139970	31.161357
512.895793	20712.071590	31.166375
513.353386	20756.493252	31.171392
514.010736	20787.306095	31.176410
514.256429	20803.455324	31.181428
515.006871	20844.046988	31.186445
515.863545	20878.025964	31.191463
516.133540	20908.318022	31.196480
516.845438	20935.337980	31.201498
517.005174	20959.676536	31.206516
517.572068	20982.770222	31.211533
518.109293	21014.922641	31.216551
518.473794	21041.857826	31.221568
519.176067	21077.402845	31.226586
519.418667	21101.469627	31.231604
519.684037	21136.292981	31.236621
520.250570	21172.156265	31.241639
520.593356	21203.423105	31.246656
521.334376	21237.123747	31.251674
522.162191	21275.157965	31.256692
522.667089	21314.405107	31.261709
522.893536	21343.282982	31.266727
523.572792	21372.892843	31.271744
523.811335	21406.804685	31.276762
524.579514	21437.784531	31.281780
524.950127	21478.303951	31.286797
525.652266	21516.313972	31.291815
526.347255	21554.874884	31.296832
526.651847	21589.061089	31.301850
527.656888	21609.193449	31.306868
528.228823	21645.473774	31.311885
528.658827	21671.230705	31.316903
529.487046	21705.512513	31.321920
530.351443	21713.857608	31.326938
531.359474	21731.917162	31.331956
531.718857	21755.385261	31.336973
532.428614	21767.463421	31.341991
532.943507	21788.493677	31.347008
533.486800	21807.308049	31.352026
534.049720	21827.269358	31.357044
534.206706	21850.263596	31.362061
534.559947	21872.702869	31.367079
534.747390	21898.820106	31.372096
535.096864	21915.042552	31.377114
535.944359	21948.645697	31.382132
536.088129	21988.190509	31.387149
536.586523	22019.459696	31.392167
537.154843	22057.864393	31.397184
537.505244	22095.020410	31.402202
538.235302	22124.989975	31.407220
538.548805	22167.611171	31.412237
539.322340	22213.351765	31.417255
539.933702	22234.455942	31.422272
540.063127	22282.925535	31.427290
541.006393	22310.701202	31.432308
541.185672	22355.308811	31.437325
541.894853	22389.667211	31.442343
542.178412	22426.000185	31.447360
542.677907	22467.133445	31.452378
543.664347	22502.282952	31.457396
543.816352	22539.552834	31.462413
544.459165	22573.429021	31.467431
545.309654	22613.162045	31.472448
546.014706	22643.344811	31.477466
546.361813	22672.938828	31.482484
546.993879	22711.992029	31.487501
547.612761	22746.472526	31.492519
548.528887	22782.612897	31.497536
548.829241	22812.454517	31.502554
549.160928	22833.786120	31.507572
549.734899	22875.148751	31.512589
550.386959	22916.789981	31.517607
550.825930	22940.183910	31.522624
551.534060	22978.435934	31.527642
552.007312	23005.053563	31.532660
552.572419	23046.967679	31.537677
553.203542	23086.230289	31.542695
553.671206	23104.261487	31.547712
553.849574	23135.670724	31.552730
554.801015	23167.003896	31.557748
555.581983	23195.001962	31.562765
555.750861	23221.326040	31.567783
555.914132	23245.970175	31.572800
556.668417	23281.782790	31.577818
557.434331	23305.518031	31.582836
557.790080	23350.966111	31.587853
558.594013	23375.182082	31.592871
559.101613	23409.219768	31.597888
558.865899	23435.360672	31.602906
560.034549	23469.466166	31.607924
560.365201	23522.134912	31.612941
560.933988	23551.152289	31.617959
561.572585	23594.003982	31.622976
561.799633	23632.951432	31.627994
563.004381	23666.678819	31.633012
563.360691	23717.473627	31.638029
563.599168	23757.639137	31.643047
564.424616	23783.577386	31.648064
564.630068	23821.018287	31.653082
565.012822	23871.803052	31.658100
565.748484	23907.537545	31.663117
566.580881	23945.816323	31.668135
567.351126	23985.469802	31.673152
568.168816	24026.095455	31.678170
568.871808	24056.268055	31.683188
570.303274	24073.808855	31.688205
570.857403	24096.522698	31.693223
571.678282	24120.913881	31.698240
572.177401	24141.462512	31.703258
572.906832	24151.883424	31.708276
573.254090	24189.441966	31.713293
573.403090	24205.691179	31.718311
573.615876	24228.483588	31.723328
574.298256	24262.950516	31.728346
575.053630	24298.448828	31.733364
575.761957	24334.333687	31.738381
576.214893	24346.680907	31.743399
576.916640	24384.987188	31.748416
576.957770	24426.979462	31.753434
577.831165	24459.015635	31.758452
578.230142	24484.717860	31.763469
578.559300	24526.254745	31.768487
579.037075	24554.706369	31.773504
579.721315	24595.808957	31.778522
580.294832	24634.394775	31.783540
580.696350	24667.490572	31.788557
581.375287	24702.875114	31.793575
582.091456	24743.328451	31.798592
583.013037	24773.183732	31.803610
583.468079	24802.416543	31.808628
583.718276	24838.108209	31.813645
584.436577	24878.612044	31.818663
584.656971	24908.570365	31.823680
585.187977	24958.696544	31.828698
585.987729	24995.370939	31.833716
586.718187	25032.643907	31.838733
586.937934	25074.647650	31.843751
587.760397	25110.623569	31.848768
588.168405	25160.434463	31.853786
588.844488	25198.139617	31.858804
589.447470	25236.747287	31.863821
590.434199	25283.833116	31.868839
591.230762	25311.022819	31.873856
591.701481	25345.050590	31.878874
591.803729	25372.721324	31.883892
592.451052	25414.665535	31.888909
592.960508	25453.338740	31.893927
593.947230	25474.678633	31.898944
594.497024	25504.049390	31.903962
594.975040	25532.527646	31.908980
595.632886	25565.483908	31.913997
595.983735	25604.112577	31.919015
596.378776	25631.744407	31.924032
596.910176	25672.550691	31.929050
597.811452	25702.745469	31.934068
598.535499	25740.463135	31.939085
598.973513	25777.599741	31.944103
600.015391	25811.217079	31.949120
600.288142	25849.567667	31.954138
600.486508	25877.615961	31.959156
601.337966	25920.205671	31.964173
601.474728	25957.534862	31.969191
603.085587	25990.375062	31.974208
603.883502	26024.422567	31.979226
604.022226	26047.942719	31.984244
604.565581	26085.088773	31.989261
605.050255	26127.818181	31.994279
605.862389	26163.108727	31.999296
606.571443	26203.357560	32.004314
607.112346	26229.943677	32.009332
607.867848	26271.891797	32.014349
608.708350	26308.511690	32.019367
609.172589	26335.811397	32.024384
609.408113	26379.420679	32.029402
609.950689	26415.145469	32.034420
610.787246	26457.523756	32.039437
610.956868	26493.641704	32.044455
611.421249	26529.265109	32.049472
611.877504	26585.442603	32.054490
612.323084	26629.436847	32.059508
613.040917	26679.260148	32.064525
613.726234	26732.640522	32.069543
614.630513	26768.594034	32.074560
615.601324	26815.957693	32.079578
616.294303	26851.451277	32.084596
616.897602	26882.718075	32.089613
617.493634	26939.272961	32.094631
618.342042	26965.755297	32.099648
618.957843	27000.407937	32.104666
619.588358	27035.304832	32.109684
620.407938	27067.435712	32.114701
620.408071	27113.194163	32.119719
621.375601	27152.557744	32.124736
621.927150	27193.623098	32.129754
622.606123	27229.656746	32.134772
623.342367	27260.366211	32.139789
623.934585	27309.110896	32.144807
625.113479	27337.267705	32.149824
625.404582	27375.106389	32.154842
626.052624	27408.958353	32.159860
626.559765	27445.132900	32.164877
627.075169	27482.412281	32.169895
627.791307	27512.948291	32.174912
628.331995	27555.134767	32.179930
628.965828	27603.665110	32.184948
629.296432	27630.450138	32.189965
629.608708	27685.724003	32.194983
630.436673	27713.638909	32.200000
630.984481	27763.099481	32.205018
631.673612	27807.690410	32.210036
632.624351	27848.069225	32.215053
632.635185	27895.648057	32.220071
633.578475	27930.725340	32.225088
633.990973	27971.327239	32.230106
635.132619	28009.173748	32.235124
635.303026	28038.607254	32.240141
635.791363	28086.636798	32.245159
636.692963	28126.006214	32.250176
637.422182	28154.101432	32.255194
637.637907	28203.412514	32.260212
638.326139	28236.949895	32.265229
639.338284	28279.285701	32.270247
639.822842	28307.804773	32.275264
641.060173	28340.112821	32.280282
641.922132	28367.650420	32.285300
642.676344	28404.281219	32.290317
643.042404	28432.875799	32.295335
643.581048	28453.865125	32.300352
644.209414	28493.650705	32.305370
644.558739	28534.649120	32.310388
645.499250	28569.810108	32.315405
646.318965	28605.761083	32.320423
646.593556	28636.266388	32.325440
647.217291	28679.314521	32.330458
648.007251	28720.175187	32.335476
648.624655	28758.692528	32.340493
648.969347	28804.672932	32.345511
649.665902	28842.716697	32.350528
650.370799	28885.581970	32.355546
651.411542	28905.678222	32.360564
652.707899	28931.031506	32.365581
652.963778	28969.738261	32.370599
653.705177	29002.409001	32.375616
653.961138	29037.942835	32.380634
654.947045	29072.282241	32.385652
655.699369	29109.350737	32.390669
655.952651	29154.549734	32.395687
656.696291	29188.351852	32.400704
656.940086	29232.743429	32.405722
657.718064	29277.437519	32.410740
658.173838	29315.020298	32.415757
658.399152	29372.726849	32.420775
659.250539	29410.810778	32.425792
659.689151	29459.932171	32.430810
660.617790	29514.685214	32.435828
661.008101	29557.202647	32.440845
661.490554	29612.404668	32.445863
662.364866	29664.442226	32.450880
663.473750	29714.818901	32.455898
664.061732	29763.683891	32.460916
665.294255	29797.316095	32.465933
665.807215	29856.894502	32.470951
666.313010	29892.529988	32.475968
667.393684	29927.551394	32.480986
668.104392	29972.687306	32.486004
668.777085	30005.692718	32.491021
669.238539	30050.463051	32.496039
669.869405	30094.878411	32.501056
670.714938	30124.127643	32.506074
671.552078	30167.588163	32.511092
672.636121	30193.349017	32.516109
673.103095	30232.259175	32.521127
673.795990	30267.904113	32.526144
674.611070	30296.159585	32.531162
675.094367	30342.001755	32.536180
675.523424	30369.881257	32.541197
676.201778	30411.401115	32.546215
676.581823	30441.399633	32.551232
677.406420	30488.061328	32.556250
677.681454	30528.955191	32.561268
678.190225	30564.724125	32.566285
679.431277	30610.720747	32.571303
679.885393	30640.113824	32.576320
680.456773	30668.091679	32.581338
680.900787	30713.390837	32.586356
681.537230	30750.170593	32.591373
682.026801	30789.520778	32.596391
682.786627	30838.462711	32.601408
683.686058	30878.735394	32.606426
684.233525	30926.174501	32.611444
684.850628	30958.216603	32.616461
685.221008	30997.686881	32.621479
685.701785	31055.503771	32.626496
686.711126	31100.930702	32.631514
686.986557	31156.971911	32.636532
687.549046	31198.473461	32.641549
688.339747	31267.861554	32.646567
689.230675	31324.332085	32.651584
689.938013	31363.036276	32.656602
690.871552	31416.023591	32.661620
691.965170	31452.094953	32.666637
692.491719	31508.730177	32.671655
693.355080	31548.971853	32.676672
694.162713	31592.718120	32.681690
694.663295	31645.381482	32.686708
695.538401	31686.670984	32.691725
696.367558	31733.840512	32.696743
696.871597	31779.170589	32.701760
697.380610	31823.159799	32.706778
698.375481	31867.541272	32.711796
699.264186	31922.958062	32.716813
699.906565	31966.484297	32.721831
700.594695	32008.840306	32.726848
701.486998	32044.608991	32.731866
701.886540	32086.472736	32.736884
702.815210	32139.418407	32.741901
703.428011	32176.741728	32.746919
704.134215	32228.571696	32.751936
704.729189	32274.027775	32.756954
705.571881	32328.618335	32.761972
706.016503	32374.540565	32.766989
706.845763	32437.939803	32.772007
707.203118	32476.447681	32.777024
708.328747	32513.634878	32.782042
708.940733	32568.970030	32.787060
709.681039	32625.764679	32.792077
710.637708	32664.084779	32.797095
710.920580	32716.500259	32.802112
711.900017	32762.207329	32.807130
712.441428	32812.458631	32.812148
713.338012	32852.678697	32.817165
714.083272	32906.483049	32.822183
714.580913	32959.112261	32.827200
715.497422	33005.531404	32.832218
716.093997	33052.588402	32.837236
716.892067	33093.279454	32.842253
717.645817	33144.326687	32.847271
718.131969	33188.120033	32.852288
718.918781	33240.161241	32.857306
719.703855	33289.231462	32.862324
720.312733	33337.090092	32.867341
721.026233	33381.765159	32.872359
721.955280	33435.004880	32.877376
722.582679	33479.820003	32.882394
722.921603	33544.063911	32.887412
724.220048	33578.665627	32.892429
724.468230	33638.125411	32.897447
725.153630	33683.538872	32.902464
725.863311	33737.610111	32.907482
726.760964	33791.304505	32.912500
727.336473	33837.544654	32.917517
727.937920	33880.524895	32.922535
728.336247	33942.137030	32.927552
728.925629	33969.673968	32.932570
729.535761	34030.570581	32.937588
730.386698	34087.389910	32.942605
731.740628	34127.705616	32.947623
732.091823	34179.058286	32.952640
733.117870	34232.430348	32.957658
733.275514	34295.313849	32.962676
733.945636	34339.510885	32.967693
734.821873	34409.439839	32.972711
735.342921	34463.548634	32.977728
736.410907	34521.271071	32.982746
736.957835	34573.536281	32.987764
737.937371	34630.925051	32.992781
739.069564	34685.457725	32.997799
739.467246	34743.677113	33.002816
740.300331	34790.252291	33.007834
740.765238	34850.838789	33.012852
741.688160	34916.949653	33.017869
742.573936	34979.917847	33.022887
743.433903	35029.549511	33.027904
744.599163	35074.802761	33.032922
745.793498	35114.841721	33.037940
746.840869	35154.966861	33.042957
747.546066	35196.656462	33.047975
748.379058	35232.730677	33.052992
749.208496	35271.189163	33.058010
750.054607	35323.637275	33.063028
750.538805	35358.166355	33.068045
751.561016	35394.021709	33.073063
752.101993	35436.331684	33.078080
753.056509	35475.504510	33.083098
753.602200	35523.883771	33.088116
754.045435	35567.644493	33.093133
754.859486	35606.807814	33.098151
755.379934	35663.088495	33.103168
755.760322	35707.776097	33.108186
756.502429	35758.319339	33.113204
757.084183	35814.192538	33.118221
758.151209	35864.179625	33.123239
758.555918	35929.078134	33.128256
759.536970	35975.051185	33.133274
759.715282	36039.245494	33.138292
760.810721	36100.850251	33.143309
761.919611	36148.902995	33.148327
762.341556	36224.093496	33.153344
763.256133	36275.262389	33.158362
764.091185	36334.461359	33.163380
764.723623	36384.966258	33.168397
765.586915	36447.076062	33.173415
765.931898	36510.550312	33.178432
766.911061	36562.095547	33.183450
768.065409	36624.723315	33.188468
768.497804	36691.523093	33.193485
769.398426	36739.249176	33.198503
770.402753	36793.857774	33.203520
771.360694	36844.433233	33.208538
772.353588	36895.249974	33.213556
773.073543	36952.792940	33.218573
773.948724	36994.213009	33.223591
774.586163	37041.234599	33.228608
775.349425	37098.670045	33.233626
776.304832	37146.616150	33.238644
776.921652	37194.874323	33.243661
777.688207	37242.299916	33.248679
778.233085	37293.307490	33.253696
778.951464	37336.403012	33.258714
779.756017	37382.292761	33.263732
780.287796	37427.668617	33.268749
781.207443	37469.727668	33.273767
781.717399	37507.980681	33.278784
782.326710	37555.368213	33.283802
783.137725	37614.182430	33.288820
784.256406	37657.968770	33.293837
785.066306	37709.562099	33.298855
785.941906	37773.488669	33.303872
786.362221	37814.614377	33.308890
787.301676	37870.045229	33.313908
787.740519	37921.026541	33.318925
789.084732	37970.817338	33.323943
789.709120	38026.828815	33.328960
790.555713	38080.390260	33.333978
791.363948	38138.807968	33.338996
791.537060	38194.966014	33.344013
792.449101	38251.483448	33.349031
793.312394	38310.398937	33.354048
794.142919	38368.156145	33.359066
794.891014	38420.791554	33.364084
795.808601	38490.348075	33.369101
797.038976	38532.525258	33.374119
798.188101	38591.757473	33.379136
798.733581	38642.970522	33.384154
799.570630	38688.156078	33.389172
799.752839	38752.389535	33.394189
800.628925	38804.721392	33.399207
802.038334	38875.783533	33.404224
803.080539	38913.937227	33.409242
804.557119	38947.527163	33.414260
806.522857	38965.130355	33.419277
807.252674	39006.216488	33.424295
808.096978	39036.104385	33.429312
808.877107	39057.490459	33.434330
809.652450	39086.301464	33.439348
810.021018	39119.558245	33.444365
810.898533	39149.757321	33.449383
811.679264	39184.164219	33.454400
812.089059	39229.657728	33.459418
813.062732	39255.206593	33.464436
813.857456	39296.074488	33.469453
814.930651	39329.183962	33.474471
815.265956	39363.135599	33.479488
816.044461	39405.903398	33.484506
816.739226	39458.201830	33.489524
817.045449	39507.285068	33.494541
817.419287	39546.815040	33.499559
818.392044	39597.059516	33.504576
819.280123	39650.536199	33.509594
820.289725	39698.985488	33.514612
820.527461	39769.708074	33.519629
821.224342	39817.807897	33.524647
821.963219	39876.607906	33.529664
823.078323	39935.311565	33.534682
824.388515	39999.828471	33.539700
824.517000	40049.326373	33.544717
825.487700	40107.199223	33.549735
826.206882	40165.826007	33.554752
827.012064	40232.370052	33.559770
827.864791	40292.930555	33.564788
828.528853	40355.500068	33.569805
829.129767	40407.069144	33.574823
830.095488	40477.098883	33.579840
830.960334	40536.690572	33.584858
831.769702	40596.626246	33.589876
832.261342	40657.142785	33.594893
833.325701	40708.988269	33.599911
834.001090	40775.630073	33.604928
834.898225	40833.952687	33.609946
835.479213	40904.752016	33.614964
836.144045	40959.809818	33.619981
837.184779	41015.043246	33.624999
838.001699	41081.448923	33.630016
838.925241	41147.686419	33.635034
839.839681	41207.171031	33.640052
840.378946	41275.359740	33.645069
841.576843	41330.537880	33.650087
842.114837	41393.958504	33.655104
842.973760	41466.797149	33.660122
844.279099	41524.931577	33.665140
844.959847	41597.722499	33.670157
846.145389	41660.448586	33.675175
846.885172	41720.214766	33.680192
847.759599	41776.291880	33.685210
848.915795	41835.759545	33.690228
849.672668	41894.511601	33.695245
850.334862	41950.641173	33.700263
851.101790	42020.719458	33.705280
851.934018	42077.290911	33.710298
853.117499	42129.589254	33.715316
854.329088	42196.714819	33.720333
855.644499	42240.024433	33.725351
856.578840	42293.873563	33.730368
857.419025	42344.910312	33.735386
858.499513	42403.948570	33.740404
858.724184	42453.120701	33.745421
859.949809	42506.450650	33.750439
860.744202	42557.836561	33.755456
861.013490	42610.335282	33.760474
862.292491	42667.578716	33.765492
862.777892	42731.264387	33.770509
863.547431	42790.193964	33.775527
864.486639	42854.188842	33.780544
864.998734	42916.156840	33.785562
866.324863	42980.363826	33.790580
867.186468	43025.238320	33.795597
868.096667	43089.168821	33.800615
869.331333	43159.835724	33.805632
869.669204	43219.415544	33.810650
871.250388	43274.690713	33.815668
871.544982	43332.576141	33.820685
872.749222	43391.382733	33.825703
873.577812	43447.667322	33.830720
874.219742	43514.354275	33.835738
875.125171	43571.531709	33.840756
875.961614	43629.782651	33.845773
877.147776	43689.067234	33.850791
878.000711	43744.918681	33.855808
878.871397	43810.913101	33.860826
879.547738	43869.088392	33.865844
880.385618	43933.975050	33.870861
881.111470	43991.731817	33.875879
881.990771	44056.454254	33.880896
882.795799	44119.904411	33.885914
883.892375	44185.365086	33.890932
884.426000	44253.462686	33.895949
885.250255	44316.366435	33.900967
886.445650	44374.949305	33.905984
887.403150	44444.777907	33.911002
888.220640	44503.584402	33.916020
889.024134	44575.322352	33.921037
889.990144	44632.031336	33.926055
890.644795	44697.929187	33.931072
891.596143	44759.005329	33.936090
892.924168	44811.173670	33.941108
893.763386	44866.182460	33.946125
894.485516	44903.928350	33.951143
895.057560	44954.664959	33.956160
896.191973	45017.788083	33.961178
896.966798	45065.121872	33.966196
897.818735	45130.465272	33.971213
898.772376	45178.416673	33.976231
899.395772	45246.174404	33.981248
900.052226	45322.308631	33.986266
901.246033	45380.375696	33.991284
902.237685	45441.466411	33.996301
902.858357	45504.791070	34.001319
903.857493	45565.140855	34.006336
904.550716	45633.217824	34.011354
905.774118	45699.751229	34.016372
906.501168	45775.970897	34.021389
907.076181	45841.511300	34.026407
908.051565	45914.960055	34.031424
908.867769	45982.974662	34.036442
910.141636	46062.311039	34.041460
910.545217	46139.607077	34.046477
911.469505	46216.676832	34.051495
912.922734	46286.971725	34.056512
913.642631	46371.525722	34.061530
914.709591	46439.730412	34.066548
915.381305	46514.303806	34.071565
916.516908	46600.261573	34.076583
917.457779	46659.294918	34.081600
918.267044	46733.948843	34.086618
919.673387	46801.228811	34.091636
920.305320	46869.274783	34.096653
921.397059	46946.561362	34.101671
922.649951	47023.228467	34.106688
923.261064	47086.856398	34.111706
924.337719	47160.755264	34.116724
925.309857	47236.998665	34.121741
926.140854	47298.397790	34.126759
927.231994	47362.736221	34.131776
928.307478	47438.160788	34.136794
929.161229	47503.169193	34.141812
929.995656	47581.427953	34.146829
930.708817	47643.839580	34.151847
932.189013	47712.597443	34.156864
932.745449	47796.498982	34.161882
934.282825	47854.715075	34.166900
934.948422	47918.406454	34.171917
935.950753	47993.799975	34.176935
936.580115	48058.914493	34.181952
937.254665	48138.737375	34.186970
938.642764	48205.746005	34.191988
939.386082	48272.937444	34.197005
940.141958	48346.890115	34.202023
941.530656	48413.171721	34.207040
942.301591	48474.678279	34.212058
943.434037	48542.290756	34.217076
944.479364	48608.873117	34.222093
945.521034	48686.224038	34.227111
946.095888	48756.195180	34.232128
947.032641	48825.477543	34.237146
947.998031	48890.036006	34.242164
948.890041	48968.284253	34.247181
949.450065	49037.790396	34.252199
950.524426	49103.648445	34.257216
951.601524	49181.704119	34.262234
952.678112	49260.361178	34.267252
953.676234	49325.409261	34.272269
954.350483	49384.851829	34.277287
955.798975	49450.190788	34.282304
956.622731	49518.581789	34.287322
958.050976	49572.333579	34.292340
958.625408	49632.026420	34.297357
959.392053	49688.469137	34.302375
960.537288	49743.195427	34.307392
961.222605	49808.116423	34.312410
962.311618	49865.907635	34.317428
962.800054	49932.656465	34.322445
963.421932	50001.719350	34.327463
964.567224	50077.053215	34.332480
965.083687	50144.184240	34.337498
966.355929	50223.206421	34.342516
967.220042	50300.995368	34.347533
968.242914	50388.193460	34.352551
969.306776	50452.430976	34.357568
970.198296	50538.321404	34.362586
971.115818	50616.147392	34.367604
972.232527	50688.868297	34.372621
973.240919	50772.343430	34.377639
973.967410	50844.600416	34.382656
975.199163	50923.738867	34.387674
976.535225	51003.184040	34.392692
978.380832	51060.297363	34.397709
979.807725	51106.732380	34.402727
981.708480	51169.911526	34.407744
982.633847	51222.252232	34.412762
983.395065	51269.063267	34.417780
984.615614	51311.285220	34.422797
984.902858	51369.160723	34.427815
986.087206	51420.050577	34.432832
986.632208	51474.159435	34.437850
987.608004	51536.395266	34.442868
988.874196	51601.964869	34.447885
989.496188	51653.740023	34.452903
990.531888	51713.796717	34.457920
991.467614	51778.241366	34.462938
992.011543	51840.988158	34.467956
992.849743	51907.511088	34.472973
993.840623	51986.595761	34.477991
994.948722	52057.411420	34.483008
995.971112	52126.051321	34.488026
996.605765	52212.430875	34.493044
997.272560	52278.899291	34.498061
998.259289	52361.592585	34.503079
999.588745	52442.505394	34.508096
999.900593	52530.916911	34.513114
1001.309737	52607.129128	34.518132
1002.433938	52681.582569	34.523149
1003.174936	52763.391704	34.528167
1004.396611	52844.101216	34.533184
1005.292341	52928.360972	34.538202
1006.313198	53006.640823	34.543220
1007.475156	53089.214506	34.548237
1008.851145	53171.533693	34.553255
1009.627392	53243.638532	34.558272
1010.542108	53325.732656	34.563290
1011.709265	53409.160916	34.568308
1012.502665	53481.447325	34.573325
1013.196491	53574.099949	34.578343
1014.633806	53645.432366	34.583360
1015.481688	53730.702269	34.588378
1016.336796	53804.112767	34.593396
1017.755968	53891.528095	34.598413
1018.617149	53979.093885	34.603431
1019.655344	54061.184019	34.608448
1020.740074	54132.503194	34.613466
1021.900692	54213.625598	34.618484
1022.810485	54275.954948	34.623501
1023.716067	54341.974401	34.628519
1025.012798	54399.934415	34.633536
1025.770295	54481.664710	34.638554
1026.811054	54546.208223	34.643572
1027.838425	54608.241712	34.648589
1028.855665	54684.515367	34.653607
1030.147129	54758.246939	34.658624
1031.106456	54812.064885	34.663642
1032.259984	54884.653931	34.668660
1033.643667	54955.384834	34.673677
1034.471996	55023.487563	34.678695
1035.360793	55090.011657	34.683712
1036.602481	55157.385957	34.688730
1037.466911	55226.559465	34.693748
1038.925272	55297.089918	34.698765
1039.948571	55373.428138	34.703783
1040.622671	55439.809440	34.708800
1041.347106	55512.384937	34.713818
1042.414598	55587.830990	34.718836
1043.336661	55658.990246	34.723853
1044.395388	55745.955950	34.728871
1045.460212	55829.358080	34.733888
1046.761010	55906.616752	34.738906
1047.814275	55980.414525	34.743924
1049.104117	56060.225803	34.748941
1050.348106	56117.141371	34.753959
1051.587017	56183.797565	34.758976
1052.749614	56259.173991	34.763994
1053.955945	56322.937143	34.769012
1055.889105	56367.987451	34.774029
1056.845965	56440.352401	34.779047
1058.028492	56494.892537	34.784064
1058.979167	56556.810167	34.789082
1060.210877	56611.690994	34.794100
1060.959748	56668.722924	34.799117
1061.796476	56738.791168	34.804135
1062.711486	56802.695883	34.809152
1063.492972	56866.482319	34.814170
1064.341106	56950.820793	34.819188
1065.299450	57011.681500	34.824205
1066.077094	57091.360780	34.829223
1067.228338	57173.671933	34.834240
1068.235473	57244.284730	34.839258
1069.072266	57323.335345	34.844276
1070.626724	57409.856549	34.849293
1071.001939	57489.435242	34.854311
1071.849498	57566.801487	34.859328
1073.439699	57648.248494	34.864346
1074.505855	57744.391013	34.869364
1075.547015	57821.152003	34.874381
1076.283986	57908.998440	34.879399
1077.762141	57997.837414	34.884416
1078.539116	58079.387152	34.889434
1079.352386	58165.064427	34.894452
1080.717951	58239.947143	34.899469
1081.833049	58346.888281	34.904487
1082.802990	58423.516707	34.909504
1083.593713	58523.293853	34.914522
1084.324230	58615.061645	34.919540
1085.591739	58699.511863	34.924557
1086.837828	58799.238254	34.929575
1087.695226	58885.082105	34.934592
1089.180445	58978.069283	34.939610
1090.232287	59073.706651	34.944628
1091.821847	59160.614772	34.949645
1092.548959	59251.929794	34.954663
1093.637793	59343.872432	34.959680
1094.983811	59421.413880	34.964698
1095.821311	59504.889482	34.969716
1097.429328	59579.542396	34.974733
1098.247249	59653.926094	34.979751
1098.868410	59717.985553	34.984768
1100.170661	59808.137123	34.989786
1100.888759	59895.993708	34.994804
1102.228734	59968.480522	34.999821
1102.956317	60061.520157	35.004839
1104.341521	60150.039701	35.009856
1105.056589	60229.764387	35.014874
1106.124254	60318.068123	35.019892
1107.784926	60413.438760	35.024909
1109.053422	60500.534572	35.029927
1109.792559	60573.104049	35.034944
1111.446478	60662.216598	35.039962
1112.310915	60748.426723	35.044980
1113.650725	60840.798017	35.049997
1114.899421	60929.639137	35.055015
1115.754941	61010.439567	35.060032
1116.762637	61095.090458	35.065050
1118.022642	61188.076822	35.070068
1119.485388	61272.163762	35.075085
1120.124636	61363.120560	35.080103
1121.628418	61444.479827	35.085120
1122.811540	61529.649288	35.090138
1123.659484	61614.466095	35.095156
1124.983014	61701.190467	35.100173
1126.130290	61786.106864	35.105191
1127.517269	61888.647155	35.110208
1128.846508	61966.161309	35.115226
1130.095143	62053.164442	35.120244
1131.170998	62131.832660	35.125261
1131.973366	62218.209523	35.130279
1133.432331	62305.756853	35.135296
1134.841824	62381.050585	35.140314
1135.774154	62471.358152	35.145332
1137.535689	62547.426854	35.150349
1138.617007	62624.304330	35.155367
1139.556915	62696.905792	35.160384
1141.171558	62765.490313	35.165402
1141.889209	62847.223458	35.170420
1143.050653	62928.147143	35.175437
1144.313375	63005.263439	35.180455
1145.147126	63084.168611	35.185472
1146.638445	63174.024567	35.190490
1147.382581	63244.214567	35.195508
1148.262716	63337.723948	35.200525
1149.625647	63419.700379	35.205543
1150.511093	63509.936728	35.210560
1151.739132	63584.952168	35.215578
1152.824412	63692.434043	35.220596
1153.801702	63778.358633	35.225613
1154.656787	63870.291271	35.230631
1156.004943	63958.627682	35.235648
1157.057486	64052.302825	35.240666
1158.169054	64153.831803	35.245684
1159.373693	64242.546074	35.250701
1160.512556	64328.744949	35.255719
1161.934673	64427.036026	35.260736
1163.491691	64506.472521	35.265754
1164.450993	64615.117506	35.270772
1165.104765	64693.283425	35.275789
1166.548228	64791.635918	35.280807
1167.451843	64896.998767	35.285824
1168.422019	64988.246524	35.290842
1169.268225	65089.016575	35.295860
1170.467667	65184.382422	35.300877
1171.753026	65267.459572	35.305895
1172.681652	65351.307921	35.310912
1174.191043	65443.385055	35.315930
1175.356735	65528.703867	35.320948
1176.654860	65609.595963	35.325965
1178.030638	65692.578138	35.330983
1178.918953	65783.809864	35.336000
1180.540705	65861.676795	35.341018
1181.475405	65945.101989	35.346036
1182.812040	66032.706751	35.351053
1184.073314	66114.530546	35.356071
1185.334098	66200.799162	35.361088
1186.852102	66279.728174	35.366106
1188.068111	66359.426196	35.371124
1189.055074	66435.848889	35.376141
1190.568497	66524.858694	35.381159
1191.517951	66612.076208	35.386176
1192.502064	66691.216229	35.391194
1194.009703	66786.242579	35.396212
1195.197053	66870.308944	35.401229
1196.058631	66953.508247	35.406247
1197.135159	67053.123288	35.411264
1198.141752	67141.694971	35.416282
1199.503367	67235.625071	35.421300
1200.582805	67333.771864	35.426317
1202.147726	67428.633411	35.431335
1202.869402	67526.494732	35.436352
1204.300562	67620.257136	35.441370
1205.972195	67711.335868	35.446388
1206.899933	67805.481225	35.451405
1208.107154	67896.537931	35.456423
1209.617126	67989.725912	35.461440
1210.939686	68079.992861	35.466458
1212.103999	68170.664659	35.471476
1213.408448	68260.529837	35.476493
1214.803552	68350.229258	35.481511
1215.703036	68441.456103	35.486528
1217.143932	68531.028725	35.491546
1218.456272	68631.056427	35.496564
1219.254441	68727.428790	35.501581
1220.705196	68818.469857	35.506599
1221.732841	68916.934701	35.511616
1223.148067	69013.085450	35.516634
1224.057370	69108.042596	35.521652
1225.354060	69208.410565	35.526669
1226.675512	69310.161765	35.531687
1227.833667	69407.303787	35.536704
1229.625439	69496.141299	35.541722
1230.630255	69590.331845	35.546740
1231.583780	69689.210086	35.551757
1232.862717	69781.193104	35.556775
1233.838699	69883.918481	35.561792
1235.128649	69972.018899	35.566810
1236.524814	70067.669969	35.571828
1237.673281	70173.523041	35.576845
1239.070868	70272.404039	35.581863
1239.928216	70377.828344	35.586880
1241.304211	70480.246859	35.591898
1242.557023	70576.732640	35.596916
1243.652808	70667.683488	35.601933
1245.102582	70775.714736	35.606951
1245.911287	70885.745911	35.611968
1247.361340	70989.370706	35.616986
1248.915433	71087.660527	35.622004
1249.618019	71203.788634	35.627021
1250.982526	71294.813822	35.632039
1252.584009	71408.371272	35.637056
1253.909022	71499.061366	35.642074
1254.838046	71593.688895	35.647092
1255.834357	71674.096134	35.652109
1257.219259	71767.120863	35.657127
1258.440394	71861.602570	35.662144
1259.730949	71947.094216	35.667162
1260.695817	72040.400600	35.672180
1262.195409	72134.890608	35.677197
1263.289597	72227.100979	35.682215
1264.928304	72331.550289	35.687232
1266.086459	72427.854976	35.692250
1267.030431	72508.665540	35.697268
1268.468336	72611.450047	35.702285
1270.186247	72714.166041	35.707303
1271.293355	72817.294146	35.712320
1272.789132	72906.201997	35.717338
1273.901647	73000.704695	35.722356
1275.151085	73102.633853	35.727373
1276.413617	73202.547509	35.732391
1277.787530	73304.901372	35.737408
1278.717948	73406.463382	35.742426
1280.374464	73503.593691	35.747444
1281.536201	73595.507004	35.752461
1283.314864	73703.347087	35.757479
1284.260083	73802.539766	35.762496
1285.725305	73897.104751	35.767514
1287.138953	73996.047915	35.772532
1288.449987	74097.907974	35.777549
1289.995857	74198.199256	35.782567
1291.266266	74294.632579	35.787584
1292.535411	74388.001197	35.792602
1293.676934	74492.878399	35.797620
1294.857744	74596.419924	35.802637
1296.395739	74697.892285	35.807655
1297.506307	74802.167528	35.812672
1298.667814	74907.689237	35.817690
1300.094148	75004.316179	35.822708
1301.245082	75111.600995	35.827725
1302.378285	75215.962989	35.832743
1303.744832	75331.258483	35.837760
1304.964394	75426.019113	35.842778
1306.643972	75545.206178	35.847796
1307.676010	75650.041610	35.852813
1309.643386	75751.983133	35.857831
1310.798866	75856.762154	35.862848
1312.219723	75962.361636	35.867866
1313.830382	76063.751843	35.872884
1315.012887	76155.088019	35.877901
1316.943457	76252.692333	35.882919
1318.069132	76339.933808	35.887936
1319.879117	76437.139539	35.892954
1321.046180	76527.934685	35.897972
1321.862677	76620.874816	35.902989
1323.306307	76707.839975	35.908007
1324.920387	76809.042431	35.913024
1326.152760	76898.295890	35.918042
1327.327820	76991.295486	35.923060
1328.256188	77094.847894	35.928077
1329.664612	77187.596489	35.933095
1330.979019	77298.816841	35.938112
1332.462793	77394.087949	35.943130
1333.723015	77490.306265	35.948148
1334.980504	77588.121490	35.953165
1336.452813	77681.786575	35.958183
1337.395515	77777.472604	35.963200
1338.976364	77877.189391	35.968218
1340.286839	77979.140189	35.973236
1341.444854	78085.688262	35.978253
1342.896331	78180.118379	35.983271
1343.656999	78273.136171	35.988288
1344.806495	78363.965503	35.993306
1346.156060	78447.365757	35.998324
1347.215505	78556.933369	36.003341
1348.672149	78654.924099	36.008359
1350.022274	78751.500234	36.013376
1351.255243	78851.958805	36.018394
1352.567174	78951.163944	36.023412
1353.654714	79069.343766	36.028429
1354.457355	79167.400109	36.033447
1356.066452	79289.008878	36.038464
1357.712279	79398.032494	36.043482
1359.404933	79510.963880	36.048500
1360.480605	79624.903911	36.053517
1361.756271	79729.869106	36.058535
1363.280809	79853.697891	36.063552
1364.627448	79971.689212	36.068570
1366.276536	80084.262318	36.073588
1367.243024	80200.426106	36.078605
1368.715371	80310.468497	36.083623
1369.729733	80435.354801	36.088640
1371.030677	80553.761116	36.093658
1372.991622	80665.945969	36.098676
1374.386129	80795.804402	36.103693
1375.745696	80913.556986	36.108711
1376.961903	81033.194782	36.113728
1378.426080	81153.250592	36.118746
1380.203778	81279.453506	36.123764
1380.769882	81405.389467	36.128781
1382.362728	81529.291079	36.133799
1384.503228	81652.056413	36.138816
1385.872771	81773.738659	36.143834
1387.797709	81883.564762	36.148852
1388.594882	82005.362438	36.153869
1390.080586	82116.208052	36.158887
1391.883072	82245.705619	36.163904
1393.270849	82368.147792	36.168922
1394.759614	82471.645732	36.173940
1396.190205	82595.691323	36.178957
1397.640480	82701.970849	36.183975
1398.981374	82815.527819	36.188992
1400.253728	82935.393025	36.194010
1401.245479	83046.268490	36.199028
1402.923494	83170.240077	36.204045
1404.538252	83273.987417	36.209063
1405.964773	83390.346190	36.214080
1407.830598	83508.284228	36.219098
1409.340552	83627.038379	36.224116
1410.571519	83743.910517	36.229133
1412.293728	83848.720232	36.234151
1413.946410	83954.909590	36.239168
1414.940230	84060.492332	36.244186
1416.720140	84174.733973	36.249204
1417.527874	84283.425506	36.254221
1419.138149	84393.791805	36.259239
1420.121673	84519.157116	36.264256
1421.760226	84628.265493	36.269274
1423.264302	84743.882793	36.274292
1424.536024	84857.129216	36.279309
1425.765410	84975.197711	36.284327
1427.404177	85086.563262	36.289344
1428.584591	85210.659166	36.294362
1430.270419	85324.653935	36.299380
1431.506691	85441.544839	36.304397
1432.754344	85554.252881	36.309415
1434.352943	85669.656445	36.314432
1435.356605	85787.712715	36.319450
1437.102960	85905.539824	36.324468
1438.512263	86013.206558	36.329485
1439.956158	86116.902081	36.334503
1441.496476	86222.052884	36.339520
1442.787101	86327.090872	36.344538
1444.023551	86430.832478	36.349556
1445.374902	86548.292840	36.354573
1446.747284	86651.342468	36.359591
1447.869938	86765.988131	36.364608
1449.782567	86880.485944	36.369626
1451.433875	86986.167132	36.374644
1452.929594	87100.388556	36.379661
1453.988220	87216.655310	36.384679
1455.430564	87327.996686	36.389696
1456.847206	87449.315529	36.394714
1458.470049	87568.435821	36.399732
1459.928613	87692.739806	36.404749
1461.404913	87800.161941	36.409767
1462.792027	87918.445951	36.414784
1464.158660	88044.894704	36.419802
1465.869408	88158.453161	36.424820
1467.014110	88284.924816	36.429837
1468.846917	88414.356694	36.434855
1470.522233	88530.203175	36.439872
1471.595986	88654.837247	36.444890
1473.526055	88771.620827	36.449908
1474.775625	88897.876022	36.454925
1476.816747	89014.998118	36.459943
1478.777960	89127.456798	36.464960
1480.268474	89247.757716	36.469978
1482.132972	89354.643518	36.474996
1483.024330	89469.373739	36.480013
1484.791891	89585.362071	36.485031
1486.461108	89704.610501	36.490048
1487.143678	89826.281487	36.495066
1488.935797	89935.981434	36.500084
1490.271277	90060.327204	36.505101
1491.841590	90186.170423	36.510119
1493.217568	90301.246639	36.515136
1494.837991	90422.355857	36.520154
1496.364816	90544.126484	36.525172
1497.704901	90681.388472	36.530189
1498.838747	90806.630533	36.535207
1500.433786	90923.753525	36.540224
1501.944481	91066.212287	36.545242
1503.491210	91189.744090	36.550260
1505.101778	91318.209277	36.555277
1505.973150	91457.144667	36.560295
1507.879910	91580.622036	36.565312
1509.268359	91722.811427	36.570330
1511.173701	91845.732444	36.575348
1512.557238	91983.107666	36.580365
1514.268796	92104.957246	36.585383
1515.897747	92235.704829	36.590400
1517.468495	92360.657199	36.595418
1519.060160	92486.126477	36.600436
1520.649689	92615.031373	36.605453
1522.342794	92743.692553	36.610471
1523.963544	92860.743001	36.615488
1525.235204	92985.364253	36.620506
1526.664235	93108.402541	36.625524
1528.088464	93234.585391	36.630541
1529.641054	93367.542440	36.635559
1531.747321	93480.767976	36.640576
1533.123945	93608.506102	36.645594
1535.035279	93717.744935	36.650612
1536.133003	93849.152487	36.655629
1537.059713	93973.590627	36.660647
1538.995658	94095.451257	36.665664
1540.243037	94201.879896	36.670682
1541.889711	94314.026609	36.675700
1543.466984	94416.842936	36.680717
1544.726856	94540.242848	36.685735
1546.226654	94639.091957	36.690752
1547.255648	94768.131177	36.695770
1548.951909	94881.869325	36.700788
1550.390296	94999.932313	36.705805
1551.908576	95122.381699	36.710823
1553.583338	95251.550580	36.715840
1554.887555	95385.746491	36.720858
1556.312715	95510.911796	36.725876
1557.538315	95654.209515	36.730893
1559.074223	95788.599263	36.735911
1561.046184	95923.530160	36.740928
1562.250393	96065.172569	36.745946
1563.694565	96190.439050	36.750964
1565.382514	96351.325520	36.755981
1566.918750	96486.047792	36.760999
1568.831136	96622.347309	36.766016
1570.561547	96757.585596	36.771034
1572.222697	96891.833828	36.776052
1573.664457	97038.919767	36.781069
1575.357252	97169.982528	36.786087
1577.173117	97318.900313	36.791104
1578.373983	97446.263238	36.796122
1580.389297	97597.699252	36.801140
1582.840709	97725.071485	36.806157
1584.234661	97871.585626	36.811175
1586.134587	97986.913282	36.816192
1588.105155	98121.283379	36.821210
1589.582837	98248.606446	36.826228
1590.960458	98376.465345	36.831245
1592.547737	98511.467203	36.836263
1594.106217	98639.717344	36.841280
1595.670549	98777.893119	36.846298
1597.310863	98913.623687	36.851316
1598.614749	99057.279631	36.856333
1600.037203	99188.063198	36.861351
1601.782673	99325.275042	36.866368
1603.216701	99470.547933	36.871386
1604.942717	99604.810214	36.876404
1606.506053	99742.559280	36.881421
1607.685995	99883.614012	36.886439
1609.532586	100021.370893	36.891456
1611.393598	100167.049538	36.896474
1612.605481	100305.641714	36.901492
1614.699130	100453.643463	36.906509
1615.873575	100601.472015	36.911527
1617.942754	100740.579183	36.916544
1619.272912	100887.712887	36.921562
1621.124502	101029.086443	36.926580
1622.813620	101171.779043	36.931597
1624.618197	101320.818615	36.936615
1626.536211	101456.491304	36.941632
1628.199193	101591.481605	36.946650
1629.969492	101730.094369	36.951668
1631.777196	101857.456398	36.956685
1633.003780	101989.372088	36.961703
1635.336845	102114.028966	36.966720
1636.813149	102247.846599	36.971738
1638.208858	102364.396761	36.976756
1639.990351	102499.816103	36.981773
1641.054356	102638.491924	36.986791
1642.975497	102760.882539	36.991808
1644.560025	102906.553064	36.996826
1646.120038	103027.809095	37.001844
1648.215109	103159.416804	37.006861
1649.660192	103274.187492	37.011879
1651.144782	103383.006110	37.016896
1652.683579	103504.013616	37.021914
1654.143327	103613.724372	37.026932
1655.579935	103738.184592	37.031949
1657.419117	103865.726988	37.036967
1658.904443	103983.993245	37.041984
1660.132225	104106.509430	37.047002
1661.815561	104233.342109	37.052020
1663.711355	104352.801014	37.057037
1665.297552	104492.442995	37.062055
1666.920363	104617.663626	37.067072
1668.749679	104753.477782	37.072090
1670.891466	104872.088785	37.077108
1673.281151	104978.616270	37.082125
1674.885512	105106.719806	37.087143
1676.893931	105219.456891	37.092160
1678.293923	105340.543375	37.097178
1679.969287	105462.880745	37.102196
1681.675746	105567.576472	37.107213
1683.258818	105688.255326	37.112231
1684.692702	105811.240164	37.117248
1686.565052	105938.252743	37.122266
1688.400267	106068.682426	37.127284
1689.965944	106197.024360	37.132301
1691.411907	106326.640714	37.137319
1692.894268	106464.747415	37.142336
1694.236435	106608.772664	37.147354
1695.486234	106760.750570	37.152372
1697.240316	106903.178674	37.157389
1698.459709	107052.461763	37.162407
1700.340696	107199.639068	37.167424
1701.756412	107360.507965	37.172442
1703.111221	107519.142687	37.177460
1705.020215	107686.479358	37.182477
1706.447263	107853.283194	37.187495
1708.225772	108014.060644	37.192512
1710.091314	108171.997546	37.197530
1711.802331	108350.666592	37.202548
1713.611774	108515.385223	37.207565
1715.297072	108685.462532	37.212583
1717.794816	108842.378410	37.217600
1720.037340	108982.786268	37.222618
1722.021975	109121.954065	37.227636
1724.378249	109273.174845	37.232653
1725.933822	109432.674765	37.237671
1727.635488	109574.120262	37.242688
1729.444465	109717.578602	37.247706
1730.830141	109856.804512	37.252724
1732.853805	109997.250521	37.257741
1734.362940	110155.074368	37.262759
1735.468902	110302.537658	37.267776
1737.437394	110453.113745	37.272794
1739.146860	110609.424736	37.277812
1740.797634	110751.276025	37.282829
1742.485297	110916.227834	37.287847
1744.442298	111067.442409	37.292864
1746.276673	111216.622295	37.297882
1747.689170	111375.519218	37.302900
1749.562789	111521.942360	37.307917
1751.093153	111686.427650	37.312935
1752.680060	111834.710198	37.317952
1754.982826	111993.357186	37.322970
1756.636862	112155.758247	37.327988
1758.224059	112307.010289	37.333005
1759.751676	112465.450285	37.338023
1761.488807	112622.602845	37.343040
1763.619767	112772.643515	37.348058
1765.110990	112916.608142	37.353076
1766.598712	113063.706409	37.358093
1767.934979	113196.332963	37.363111
1769.586504	113351.003615	37.368128
1771.418502	113491.569356	37.373146
1772.980941	113660.142444	37.378164
1774.771387	113804.305008	37.383181
1776.390683	113957.816478	37.388199
1777.781920	114119.886821	37.393216
1779.596278	114276.857004	37.398234
1781.040364	114447.012136	37.403252
1783.007871	114606.521819	37.408269
1785.047791	114780.390612	37.413287
1787.072393	114946.449935	37.418304
1788.787983	115113.002009	37.423322
1790.581403	115293.887244	37.428340
1792.738202	115461.209310	37.433357
1794.213265	115628.422628	37.438375
1796.139666	115792.560537	37.443392
1798.080618	115964.826888	37.448410
1800.128666	116141.782889	37.453428
1802.506243	116308.478320	37.458445
1804.201213	116473.720676	37.463463
1805.834596	116645.822444	37.468480
1808.260595	116811.827689	37.473498
1809.725315	116969.688201	37.478516
1812.018350	117127.927810	37.483533
1813.715001	117308.140337	37.488551
1815.339382	117465.965412	37.493568
1817.323919	117627.134366	37.498586
1818.944557	117793.370786	37.503604
1820.695645	117965.612513	37.508621
1822.402164	118131.862430	37.513639
1824.266034	118300.067303	37.518656
1826.164234	118472.313816	37.523674
1827.789659	118643.398571	37.528692
1829.886728	118816.795329	37.533709
1831.545512	118992.163736	37.538727
1833.509614	119165.113459	37.543744
1835.965829	119336.249613	37.548762
1837.488802	119506.060384	37.553780
1839.647079	119666.259643	37.558797
1841.716682	119837.306000	37.563815
1843.460634	120005.625869	37.568832
1845.687118	120165.372637	37.573850
1847.067264	120347.158336	37.578868
1849.095183	120502.231368	37.583885
1851.017343	120678.517866	37.588903
1852.384994	120853.787882	37.593920
1854.297182	121024.990862	37.598938
1855.908928	121193.184268	37.603956
1857.859085	121365.524494	37.608973
1859.994065	121543.342065	37.613991
1861.405309	121721.539477	37.619008
1863.444616	121893.500293	37.624026
1865.012577	122081.924639	37.629044
1866.858823	122254.602095	37.634061
1868.886980	122438.592766	37.639079
1870.457013	122622.960051	37.644096
1872.443133	122785.533113	37.649114
1874.148633	122975.056659	37.654132
1876.003969	123157.415771	37.659149
1877.787302	123350.557100	37.664167
1879.481484	123536.418923	37.669184
1881.664085	123716.814121	37.674202
1883.590115	123906.333166	37.679220
1885.249715	124090.503048	37.684237
1887.290485	124274.309992	37.689255
1889.015827	124444.313687	37.694272
1890.965190	124598.996470	37.699290
1892.655066	124780.285064	37.704308
1894.655438	124936.001471	37.709325
1896.379999	125106.832695	37.714343
1897.683213	125271.856450	37.719360
1899.846957	125443.635653	37.724378
1901.441672	125624.574944	37.729396
1903.155748	125808.274808	37.734413
1904.932644	125999.641087	37.739431
1906.380264	126184.931879	37.744448
1908.778817	126373.234494	37.749466
1910.412143	126580.522238	37.754484
1912.301569	126766.355867	37.759501
1914.056620	126964.796604	37.764519
1916.308313	127173.944880	37.769536
1918.897948	127365.470160	37.774554
1920.672100	127560.015891	37.779572
1922.250347	127758.221534	37.784589
1924.896429	127949.525054	37.789607
1927.162559	128132.210538	37.794624
1929.788664	128312.531720	37.799642
1931.587264	128499.491064	37.804660
1934.091358	128682.890480	37.809677
1936.180829	128864.655115	37.814695
1937.786441	129043.869534	37.819712
1939.712362	129226.054500	37.824730
1941.658190	129410.876176	37.829748
1943.698344	129588.426646	37.834765
1945.506401	129768.411961	37.839783
1947.235014	129966.224017	37.844800
1949.793752	130149.798947	37.849818
1951.391773	130341.390670	37.854836
1953.280845	130518.765544	37.859853
1955.027154	130718.544971	37.864871
1956.540820	130912.728048	37.869888
1958.719902	131097.102049	37.874906
1960.442776	131308.789311	37.879924
1961.711316	131520.218429	37.884941
1964.029810	131724.976087	37.889959
1965.730895	131928.828425	37.894976
1967.468618	132139.946474	37.899994
1970.013165	132363.247791	37.905012
1971.987848	132565.411036	37.910029
1973.895823	132779.830086	37.915047
1975.870616	132990.509325	37.920064
1978.303678	133192.857906	37.925082
1980.074896	133396.947276	37.930100
1982.000674	133613.144056	37.935117
1983.894097	133824.829685	37.940135
1986.181892	134036.531084	37.945152
1988.558905	134230.886426	37.950170
1990.325760	134451.680076	37.955188
1992.457203	134651.557153	37.960205
1994.196084	134864.299608	37.965223
1996.121984	135075.338987	37.970240
1998.078409	135284.242806	37.975258
2000.070068	135500.641526	37.980276
2002.226898	135700.176715	37.985293
2004.127470	135918.736130	37.990311
2005.850954	136141.702054	37.995328
2007.919052	136339.591542	38.000346
2009.576887	136552.786020	38.005364
2011.599477	136775.962296	38.010381
2013.376585	137000.916366	38.015399
2015.098218	137226.019763	38.020416
2017.464492	137446.011422	38.025434
2018.902548	137677.226935	38.030452
2021.001122	137881.983617	38.035469
2023.034368	138084.086455	38.040487
2024.707138	138303.174920	38.045504
2026.776694	138506.339917	38.050522
2028.815660	138726.566261	38.055540
2030.990571	138944.259804	38.060557
2032.982612	139151.043718	38.065575
2034.731866	139372.346107	38.070592
2036.864806	139583.183622	38.075610
2038.992712	139797.208189	38.080628
2040.967301	140022.602984	38.085645
2043.288273	140243.757024	38.090663
2045.220998	140467.231464	38.095680
2047.295678	140700.418690	38.100698
2049.083703	140929.311396	38.105716
2051.461967	141159.052462	38.110733
2053.430805	141379.746233	38.115751
2055.419306	141619.182597	38.120768
2057.183871	141855.304551	38.125786
2058.754386	142089.820697	38.130804
2060.928082	142333.127947	38.135821
2063.417532	142582.428319	38.140839
2065.270278	142830.280709	38.145856
2067.328299	143061.705110	38.150874
2069.278962	143309.544679	38.155892
2071.436554	143565.374335	38.160909
2073.850325	143816.456862	38.165927
2076.053521	144066.063123	38.170944
2078.559978	144310.318299	38.175962
2081.216261	144550.350373	38.180980
2083.186330	144799.501602	38.185997
2085.647977	145027.014015	38.191015
2087.733084	145263.597350	38.196032
2090.387050	145504.180091	38.201050
2092.650556	145724.492030	38.206068
2095.123391	145945.457722	38.211085
2097.408282	146155.157577	38.216103
2099.370290	146381.776528	38.221120
2101.420639	146615.401573	38.226138
2103.774354	146834.866570	38.231156
2105.852273	147054.159652	38.236173
2108.286035	147268.702075	38.241191
2110.437905	147489.191276	38.246208
2112.357616	147710.567945	38.251226
2114.443040	147927.160032	38.256244
2116.865439	148155.111286	38.261261
2119.184411	148378.586402	38.266279
2120.271978	148605.376536	38.271296
2122.493283	148832.803542	38.276314
2124.409569	149064.734202	38.281332
2126.290448	149294.742057	38.286349
2128.795970	149518.751448	38.291367
2130.516130	149758.382226	38.296384
2132.723419	149993.279892	38.301402
2134.803518	150236.550486	38.306420
2136.956724	150464.477383	38.311437
2139.022851	150704.591648	38.316455
2140.865364	150940.565671	38.321472
2143.367408	151177.098130	38.326490
2145.452118	151414.838975	38.331508
2147.109405	151659.209912	38.336525
2149.625818	151899.221276	38.341543
2151.340395	152143.458512	38.346560
2153.637970	152377.616178	38.351578
2155.803326	152615.451202	38.356596
2157.990696	152863.895814	38.361613
2160.335736	153095.129545	38.366631
2162.054809	153340.094881	38.371648
2164.557336	153561.468265	38.376666
2166.872913	153770.329957	38.381684
2168.780231	153995.072722	38.386701
2170.917336	154206.553382	38.391719
2172.547857	154428.637101	38.396736
2174.575294	154665.423243	38.401754
2176.618734	154895.378377	38.406772
2177.949366	155128.923598	38.411789
2180.420691	155378.439437	38.416807
2182.499169	155624.234563	38.421824
2184.171929	155876.428399	38.426842
2186.581591	156132.431245	38.431860
2188.379501	156396.984995	38.436877
2190.460388	156658.931585	38.441895
2192.600671	156932.993510	38.446912
2194.632261	157203.493705	38.451930
2196.726793	157474.683550	38.456948
2198.712538	157764.159449	38.461965
2200.718501	158034.908606	38.466983
2203.249830	158322.728122	38.472000
2205.149798	158605.353441	38.477018
2207.869504	158890.086837	38.482036
2210.502668	159183.302699	38.487053
2213.022682	159455.869777	38.492071
2215.211921	159745.196511	38.497088
2217.295644	160032.382818	38.502106
2220.080438	160313.824599	38.507124
2221.891358	160598.923158	38.512141
2224.680158	160869.017101	38.517159
2227.117996	161152.878021	38.522176
2229.221681	161434.202319	38.527194
2231.821113	161711.375407	38.532212
2233.953978	162002.054387	38.537229
2236.129324	162279.765689	38.542247
2238.853324	162560.236674	38.547264
2241.123918	162834.799680	38.552282
2243.555556	163117.603845	38.557300
2245.748991	163393.158811	38.562317
2248.079539	163664.135719	38.567335
2250.582274	163940.152694	38.572352
2252.788585	164217.854762	38.577370
2254.830473	164482.024036	38.582388
2256.973863	164766.898855	38.587405
2259.686946	165038.570939	38.592423
2262.102917	165315.889459	38.597440
2264.187193	165589.109013	38.602458
2267.061301	165865.774458	38.607476
2268.911030	166138.296332	38.612493
2271.578836	166408.952548	38.617511
2273.863248	166671.378608	38.622528
2276.040615	166945.071571	38.627546
2278.680357	167207.888754	38.632564
2281.013305	167473.116274	38.637581
2283.255071	167748.224413	38.642599
2285.800058	168012.595684	38.647616
2288.041699	168281.128954	38.652634
2290.302037	168530.526022	38.657652
2293.236379	168764.646164	38.662669
2296.079940	169018.271152	38.667687
2298.413901	169274.947463	38.672704
2300.524012	169522.416015	38.677722
2302.721192	169762.278955	38.682740
2304.753855	170020.795101	38.687757
2306.669119	170273.959491	38.692775
2308.444635	170532.644434	38.697792
2310.281615	170793.301504	38.702810
2312.775655	171053.603288	38.707828
2314.119448	171326.033279	38.712845
2316.606588	171578.554438	38.717863
2318.642733	171833.000471	38.722880
2320.620965	172096.649413	38.727898
2322.916125	172345.660393	38.732916
2325.018265	172614.802609	38.737933
2327.315633	172879.445798	38.742951
2329.832593	173148.106301	38.747968
2331.665327	173415.058437	38.752986
2334.224318	173683.892023	38.758004
2336.185640	173965.199972	38.763021
2338.437296	174233.067440	38.768039
2340.907074	174513.117309	38.773056
2343.339530	174813.236826	38.778074
2345.987628	175089.756319	38.783092
2347.579587	175381.501070	38.788109
2350.182253	175677.013308	38.793127
2352.636666	175971.610025	38.798144
2354.830366	176270.768950	38.803162
2357.308367	176563.408592	38.808180
2359.439011	176866.490559	38.813197
2361.497041	177174.334121	38.818215
2364.474835	177463.292805	38.823232
2366.600897	177782.632773	38.828250
2369.587790	178079.566784	38.833268
2372.576799	178384.501588	38.838285
2374.995933	178684.294337	38.843303
2377.166115	178984.152265	38.848320
2379.472067	179287.494934	38.853338
2382.132816	179584.789636	38.858356
2384.456736	179887.877605	38.863373
2386.917570	180194.780343	38.868391
2389.238654	180505.388554	38.873408
2391.249231	180819.424068	38.878426
2393.800794	181125.477731	38.883444
2396.088328	181441.758101	38.888461
2398.123295	181751.399173	38.893479
2400.728990	182062.146173	38.898496
2403.284367	182386.845674	38.903514
2406.149861	182696.919395	38.908532
2408.385582	183018.216645	38.913549
2410.867387	183332.365102	38.918567
2413.562280	183663.727060	38.923584
2415.843192	183974.632457	38.928602
2418.696366	184292.358244	38.933620
2420.987745	184601.536888	38.938637
2423.747216	184955.853711	38.943655
2426.183460	185283.426145	38.948672
2428.419911	185595.918286	38.953690
2431.213453	185901.390723	38.958708
2433.759264	186229.533342	38.963725
2435.854847	186537.605416	38.968743
2438.803350	186843.996307	38.973760
2440.590585	187155.420113	38.978778
2443.383978	187465.875469	38.983796
2445.370519	187780.521234	38.988813
2447.895201	188093.153798	38.993831
2450.675890	188406.661816	38.998848
2453.157694	188723.620826	39.003866
2455.837627	189038.340123	39.008884
2458.501933	189346.204753	39.013901
2460.934652	189648.721463	39.018919
2463.566153	189952.909855	39.023936
2465.590944	190257.422081	39.028954
2468.925069	190550.174241	39.033972
2471.537378	190843.496679	39.038989
2474.091690	191143.534578	39.044007
2476.908009	191436.852154	39.049024
2478.829820	191730.639868	39.054042
2481.259719	191995.036993	39.059060
2483.349965	192274.016703	39.064077
2485.100878	192546.090079	39.069095
2487.487501	192823.424678	39.074112
2489.692687	193106.985925	39.079130
2491.792240	193386.627126	39.084148
2494.115996	193692.650987	39.089165
2496.329225	193982.842588	39.094183
2498.954204	194284.528229	39.099200
2501.267095	194591.622769	39.104218
2503.649633	194899.215213	39.109236
2506.515978	195214.836063	39.114253
2508.526368	195531.683120	39.119271
2511.354216	195841.113530	39.124288
2513.836046	196167.363396	39.129306
2516.105062	196481.835488	39.134324
2518.627808	196805.362536	39.139341
2520.836181	197126.653113	39.144359
2524.225987	197440.089273	39.149376
2526.854220	197762.916240	39.154394
2529.186261	198087.923761	39.159412
2531.773961	198410.352035	39.164429
2534.281178	198754.054861	39.169447
2537.202207	199079.252303	39.174464
2539.931445	199416.571607	39.179482
2542.250786	199737.774367	39.184500
2544.295235	200074.058575	39.189517
2546.530344	200423.192688	39.194535
2549.376958	200770.835276	39.199552
2552.169187	201119.680973	39.204570
2554.996437	201468.013910	39.209588
2557.501668	201808.472162	39.214605
2559.605176	202164.133421	39.219623
2562.083091	202524.614411	39.224640
2564.348486	202873.494883	39.229658
2566.709960	203239.507786	39.234676
2569.504607	203603.980669	39.239693
2571.679936	203971.675176	39.244711
2574.627676	204329.647992	39.249728
2577.132527	204712.178625	39.254746
2579.727275	205067.794493	39.259764
2582.972742	205443.555779	39.264781
2585.556316	205808.649961	39.269799
2588.478213	206167.493836	39.274816
2591.462674	206535.016403	39.279834
2594.394821	206874.401235	39.284852
2596.998537	207232.508938	39.289869
2599.271141	207580.812362	39.294887
2602.144812	207944.467877	39.299904
2604.954950	208303.281857	39.304922
2607.681903	208654.869425	39.309940
2610.583988	209010.570983	39.314957
2613.163789	209357.889333	39.319975
2615.829708	209701.511289	39.324992
2618.329680	210050.570444	39.330010
2620.865947	210391.368328	39.335028
2623.330584	210751.306554	39.340045
2625.597207	211103.502622	39.345063
2629.020654	211447.008952	39.350080
2631.008990	211809.639227	39.355098
2633.717234	212152.470189	39.360116
2636.043996	212513.168800	39.365133
2638.992659	212859.926101	39.370151
2641.869776	213208.295344	39.375168
2644.691414	213567.825791	39.380186
2647.447858	213914.512518	39.385204
2649.823737	214263.291113	39.390221
2652.081309	214608.150887	39.395239
2654.803503	214926.264761	39.400256
2657.202777	215263.177128	39.405274
2659.429157	215579.387212	39.410292
2662.157420	215911.625450	39.415309
2664.288215	216251.476462	39.420327
2666.836821	216590.500609	39.425344
2669.094985	216935.438503	39.430362
2671.558516	217277.956732	39.435380
2674.797449	217623.758659	39.440397
2677.415952	217978.751976	39.445415
2680.202678	218328.333722	39.450432
2682.697932	218684.997942	39.455450
2685.235896	219048.387786	39.460468
2688.011789	219408.565324	39.465485
2690.084437	219787.092567	39.470503
2692.643033	220156.322743	39.475520
2695.503475	220535.261276	39.480538
2698.252883	220912.210354	39.485556
2700.651466	221299.350407	39.490573
2703.546581	221685.625828	39.495591
2706.152497	222088.281213	39.500608
2708.804500	222478.761024	39.505626
2711.591060	222868.661130	39.510644
2714.659828	223261.565916	39.515661
2717.441042	223673.619418	39.520679
2720.217569	224056.027164	39.525696
2723.164191	224447.604783	39.530714
2726.108039	224845.686332	39.535732
2729.111821	225242.158133	39.540749
2731.744868	225633.810060	39.545767
2734.639125	226033.144190	39.550784
2737.003795	226437.743159	39.555802
2739.685664	226833.629942	39.560820
2742.501493	227227.565127	39.565837
2745.014184	227644.792172	39.570855
2747.863073	228050.966850	39.575872
2750.962979	228466.146223	39.580890
2753.724876	228870.073273	39.585908
2756.598584	229276.396185	39.590925
2759.383898	229688.397815	39.595943
2762.291057	230094.029310	39.600960
2764.567787	230514.416862	39.605978
2767.935333	230932.779964	39.610996
2770.902236	231339.976624	39.616013
2773.436805	231748.078668	39.621031
2776.613538	232159.891131	39.626048
2779.513157	232569.815752	39.631066
2782.381474	232970.294700	39.636084
2785.549312	233368.897672	39.641101
2788.373660	233774.920932	39.646119
2791.018307	234177.999580	39.651136
2794.034685	234573.856157	39.656154
2796.757517	234974.559402	39.661172
2800.038492	235371.593490	39.666189
2802.579999	235779.615103	39.671207
2804.820546	236180.316052	39.676224
2807.877324	236574.894290	39.681242
2811.038504	236982.411759	39.686260
2813.564698	237385.708962	39.691277
2816.372666	237795.744627	39.696295
2819.181748	238185.380518	39.701312
2821.839658	238587.106176	39.706330
2824.755907	238994.659347	39.711348
2827.664830	239388.266586	39.716365
2830.751821	239792.667482	39.721383
2833.694279	240190.663236	39.726400
2836.852828	240573.840013	39.731418
2839.403790	240961.302368	39.736436
2842.461028	241340.378484	39.741453
2844.933880	241700.771948	39.746471
2847.391799	242051.971243	39.751488
2850.431758	242415.425444	39.756506
2852.775551	242785.490661	39.761524
2855.621002	243158.195377	39.766541
2858.353307	243526.878013	39.771559
2860.762893	243912.477921	39.776576
2863.861644	244294.388094	39.781594
2866.058131	244681.162968	39.786612
2869.028581	245078.130300	39.791629
2871.653480	245481.145742	39.796647
2874.470874	245886.162672	39.801664
2877.070761	246282.829720	39.806682
2879.484188	246706.426492	39.811700
2882.574350	247123.490153	39.816717
2885.096648	247562.512932	39.821735
2887.733950	247987.240545	39.826752
2890.698415	248429.875833	39.831770
2893.646353	248854.349861	39.836788
2896.383467	249299.685627	39.841805
2899.264632	249750.916570	39.846823
2902.396830	250194.969222	39.851840
2905.604305	250653.793044	39.856858
2908.582430	251099.213561	39.861876
2911.703785	251548.725686	39.866893
2914.843738	251988.098258	39.871911
2917.851728	252436.685608	39.876928
2921.033627	252882.806006	39.881946
2924.485365	253327.689208	39.886964
2927.661501	253769.895983	39.891981
2930.442203	254218.589553	39.896999
2933.577262	254650.080560	39.902016
2936.691072	255095.468135	39.907034
2939.397035	255532.992533	39.912052
2942.783229	255980.874999	39.917069
2945.567360	256422.270765	39.922087
2949.006785	256880.454818	39.927104
2951.529141	257315.868278	39.932122
2954.684390	257764.187052	39.937140
2957.400838	258204.723679	39.942157
2960.451252	258666.314803	39.947175
2963.447394	259109.547993	39.952192
2966.737783	259555.883455	39.957210
2969.322561	260015.662309	39.962228
2972.714526	260465.204436	39.967245
2975.773390	260911.240644	39.972263
2978.794535	261353.648785	39.977280
2982.045779	261790.050397	39.982298
2985.143887	262235.313344	39.987316
2988.226399	262670.975798	39.992333
2990.791393	263120.432939	39.997351
2994.168194	263565.367761	40.002368
2997.291872	264005.107830	40.007386
2999.997146	264450.905466	40.012404
3003.039076	264893.372314	40.017421
3005.788835	265346.931414	40.022439
3008.545629	265796.067978	40.027456
3011.760781	266241.245188	40.032474
3014.628527	266697.472211	40.037492
3018.082522	267140.220763	40.042509
3021.268703	267584.482124	40.047527
3023.891031	268032.385002	40.052544
3027.145045	268474.295067	40.057562
3029.825305	268941.360498	40.062580
3032.906754	269388.372823	40.067597
3035.681425	269839.062673	40.072615
3038.590353	270275.405000	40.077632
3041.733553	270696.647886	40.082650
3044.811680	271115.867128	40.087668
3047.980874	271521.863498	40.092685
3050.769367	271939.244534	40.097703
3053.537051	272356.550643	40.102720
3056.774088	272771.597562	40.107738
3059.638822	273205.570479	40.112756
3062.416969	273637.878479	40.117773
3065.375299	274065.838783	40.122791
3068.241574	274501.328669	40.127808
3071.400974	274933.748481	40.132826
3074.345516	275387.811848	40.137844
3077.196422	275829.062144	40.142861
3080.017789	276279.863605	40.147879
3083.111595	276742.886430	40.152896
3086.544820	277198.209599	40.157914
3089.630899	277668.186714	40.162932
3092.102408	278133.202936	40.167949
3095.291737	278609.227870	40.172967
3097.881499	279092.910955	40.177984
3101.577979	279561.892766	40.183002
3104.542012	280051.860290	40.188020
3107.976844	280535.174111	40.193037
3111.259942	281020.895498	40.198055
3114.302854	281497.026574	40.203072
3117.639333	281977.171950	40.208090
3121.073677	282472.357619	40.213108
3124.549739	282951.255880	40.218125
3128.224184	283425.244451	40.223143
3131.060333	283912.361810	40.228160
3134.755666	284367.447959	40.233178
3137.942673	284857.322798	40.238196
3141.112985	285328.456677	40.243213
3144.770016	285807.408761	40.248231
3147.997352	286281.371183	40.253248
3151.379911	286747.967674	40.258266
3154.351006	287226.178457	40.263284
3157.587629	287699.291431	40.268301
3161.710976	288145.601428	40.273319
3165.264891	288598.192590	40.278336
3169.194142	289042.063635	40.283354
3172.275974	289494.366500	40.288372
3175.349074	289950.298479	40.293389
3178.478714	290386.413324	40.298407
3181.539385	290847.368213	40.303424
3184.516540	291298.684225	40.308442
3187.425083	291754.958797	40.313460
3190.348085	292212.878123	40.318477
3193.309381	292672.666943	40.323495
3196.631872	293131.177367	40.328512
3199.919931	293589.867401	40.333530
3203.315278	294044.830358	40.338548
3206.247262	294507.021761	40.343565
3209.924727	294966.630802	40.348583
3212.520109	295435.138458	40.353600
3216.073209	295885.924279	40.358618
3218.944173	296366.898242	40.363636
3221.872483	296836.028287	40.368653
3225.099895	297307.976813	40.373671
3228.174049	297776.492514	40.378688
3231.635981	298250.783176	40.383706
3234.899596	298727.284024	40.388724
3238.185749	299190.169693	40.393741
3241.331768	299658.201504	40.398759
3244.896899	300129.489806	40.403776
3247.845432	300583.327808	40.408794
3250.900509	301069.792441	40.413812
3253.951755	301528.303052	40.418829
3256.974475	301974.273495	40.423847
3259.800669	302418.798422	40.428864
3263.346862	302857.191201	40.433882
3265.741290	303321.348046	40.438900
3268.591252	303774.336588	40.443917
3271.764067	304233.287191	40.448935
3274.792501	304704.085482	40.453952
3277.375883	305186.980975	40.458970
3280.638715	305680.478338	40.463988
3283.570679	306171.128636	40.469005
3286.715506	306668.239295	40.474023
3289.656739	307177.992318	40.479040
3293.249568	307695.786762	40.484058
3295.889425	308212.581876	40.489076
3299.510253	308735.589986	40.494093
3302.597940	309272.559663	40.499111
3305.718337	309803.452012	40.504128
3308.868491	310345.501926	40.509146
3312.307064	310891.079656	40.514164
3315.833153	311441.231554	40.519181
3319.065141	311988.097944	40.524199
3322.215426	312550.351402	40.529216
3326.016139	313105.771114	40.534234
3329.888853	313665.462233	40.539252
3333.203069	314226.959322	40.544269
3337.097998	314768.639367	40.549287
3340.172162	315326.861025	40.554304
3344.143694	315871.586923	40.559322
3347.470980	316428.334412	40.564340
3351.074807	316992.442402	40.569357
3354.516435	317546.442726	40.574375
3357.847193	318104.437662	40.579392
3361.103951	318658.909616	40.584410
3364.977332	319222.109769	40.589428
3368.507408	319778.352121	40.594445
3372.225533	320329.888832	40.599463
3375.352606	320886.230376	40.604480
3379.302654	321433.479031	40.609498
3382.862024	321990.906179	40.614516
3386.147122	322540.071052	40.619533
3390.005289	323086.728989	40.624551
3393.263158	323646.134963	40.629568
3396.802143	324189.047348	40.634586
3400.351983	324740.882429	40.639604
3403.401559	325286.622245	40.644621
3407.252147	325824.694368	40.649639
3410.528044	326383.476722	40.654656
3414.195858	326930.848976	40.659674
3417.399039	327478.387571	40.664692
3420.721477	328025.494170	40.669709
3424.518163	328571.783683	40.674727
3427.765517	329125.457942	40.679744
3431.346253	329670.649532	40.684762
3434.791619	330221.689728	40.689780
3438.064370	330767.624292	40.694797
3442.162028	331308.932410	40.699815
3445.576588	331864.419055	40.704832
3448.987983	332399.324127	40.709850
3452.392299	332948.505180	40.714868
3455.866700	333488.408067	40.719885
3459.446086	334036.429902	40.724903
3462.362696	334573.537494	40.729920
3465.966745	335116.060376	40.734938
3469.852364	335652.722597	40.739956
3473.546069	336201.049957	40.744973
3476.664135	336729.774894	40.749991
3480.046986	337283.588109	40.755008
3484.153061	337801.167854	40.760013
3487.077240	338290.311611	40.765018
3490.032504	338749.717149	40.770023
3493.103010	339152.697527	40.775028
3495.555741	339501.809847	40.780032
3498.200128	339819.993350	40.785037
3500.613433	340090.709974	40.790042
3503.093648	340309.845926	40.795047
3505.103756	340500.548916	40.800052
3506.899574	340659.117979	40.805056
3508.918236	340754.972171	40.810061
3509.950799	340827.026617	40.815066
3511.987304	340871.513618	40.820071
3513.465671	340879.090110	40.825076
3514.541825	340858.758699	40.830080
3515.337289	340814.899429	40.835085
3515.827045	340742.455971	40.840090
3516.770319	340659.160377	40.845095
3517.317650	340544.141272	40.850100
3517.742387	340433.870487	40.855104
3518.430251	340288.721884	40.860109
3518.775704	340137.675763	40.865114
3518.893373	339981.426207	40.870119
3519.558577	339812.529099	40.875124
3519.674069	339628.281573	40.880128
3520.048627	339432.142990	40.885133
3520.172606	339231.795704	40.890138
3519.970750	339016.876308	40.895143
3520.138002	338812.171582	40.900148
3520.153557	338600.470804	40.905152
3520.342868	338369.135609	40.910157
3520.252667	338149.489213	40.915162
3520.060222	337935.858830	40.920167
3519.884055	337696.667547	40.925172
3519.326292	337471.368064	40.930176
3519.464434	337243.568450	40.935181
3519.503039	337013.748471	40.940186
3519.122591	336793.172706	40.945191
3518.955131	336548.810142	40.950196
3518.710458	336339.094888	40.955200
3518.292678	336112.748031	40.960205
3518.202181	335879.711308	40.965210
3517.767635	335666.792014	40.970215
3517.804517	335436.046931	40.975220
3517.266147	335242.799930	40.980224
3517.234205	335024.677107	40.985229
3516.995591	334807.220969	40.990234
3516.813658	334598.808574	40.995239
3516.716692	334387.457089	41.000244
3516.377201	334189.901073	41.005248
3515.865493	333980.061478	41.010253
3516.195303	333782.475468	41.015258
3515.708185	333584.659489	41.020263
3515.747532	333379.588464	41.025268
3515.401559	333192.379431	41.030272
3514.935637	332992.395248	41.035277
3515.189668	332805.599602	41.040282
3514.669948	332617.041371	41.045287
3514.205398	332424.811189	41.050292
3514.477117	332246.352261	41.055296
3514.109398	332059.802320	41.060301
3513.987518	331882.547467	41.065306
3513.479483	331710.845639	41.070311
3513.621540	331527.672814	41.075316
3513.610420	331354.467757	41.080320
3513.184638	331184.378576	41.085325
3513.070525	331023.065916	41.090330
3512.900313	330859.421331	41.095335
3512.765874	330681.934005	41.100340
3512.699641	330521.908980	41.105344
3512.317408	330374.014058	41.110349
3512.236174	330202.900431	41.115354
3511.735337	330057.032129	41.120359
3511.588680	329899.611447	41.125364
3511.586249	329748.373909	41.130368
3511.332445	329602.414600	41.135373
3511.544969	329456.661973	41.140378
3511.156355	329311.918031	41.145383
3510.984684	329169.556190	41.150388
3510.875824	329029.218923	41.155392
3510.567720	328885.198524	41.160397
3510.871716	328755.835212	41.165402
3510.337256	328627.390469	41.170407
3510.486526	328490.114318	41.175412
3509.995168	328359.398183	41.180416
3509.823267	328230.615938	41.185421
3510.059779	328105.076451	41.190426
3510.018466	327986.142409	41.195431
3509.761019	327857.092467	41.200436
3509.910719	327734.694018	41.205440
3509.778410	327606.285144	41.210445
3509.833899	327479.093037	41.215450
3509.136363	327356.825273	41.220455
3509.274529	327222.522601	41.225460
3509.093703	327123.830072	41.230464
3509.020617	327001.998232	41.235469
3509.237827	326892.330685	41.240474
3508.924859	326786.026744	41.245479
3508.847035	326660.557086	41.250484
3508.675800	326556.672465	41.255488
3508.604336	326449.083625	41.260493
3508.969493	326325.909677	41.265498
3508.595762	326224.853842	41.270503
3508.526677	326119.502263	41.275508
3508.434744	326014.382905	41.280512
3508.253029	325898.237252	41.285517
3508.392133	325791.784040	41.290522
3508.057833	325696.673211	41.295527
3508.071743	325593.189759	41.300532
3508.142040	325483.592142	41.305536
3508.052724	325388.976672	41.310541
3507.991391	325285.605902	41.315546
3507.919504	325191.979353	41.320551
3507.914634	325089.337010	41.325556
3507.781912	324994.981767	41.330560
3507.792208	324893.481300	41.335565
3507.787202	324798.978541	41.340570
3507.533466	324702.733574	41.345575
3507.540459	324599.096059	41.350580
3507.651088	324517.243073	41.355584
3507.609791	324407.023984	41.360589
3507.673745	324315.358520	41.365594
3507.618635	324228.392123	41.370599
3507.900842	324123.362331	41.375604
3507.357561	324026.575752	41.380608
3507.296621	323940.779849	41.385613
3507.334861	323844.589206	41.390618
3507.089549	323760.347964	41.395623
3507.245222	323667.089571	41.400628
3507.001011	323584.145198	41.405632
3507.003111	323495.540255	41.410637
3507.209230	323398.432082	41.415642
3507.207927	323320.130220	41.420647
3507.101364	323231.160034	41.425652
3507.155708	323142.978683	41.430656
3506.861182	323052.256603	41.435661
3506.971448	322962.387161	41.440666
3507.196727	322877.663875	41.445671
3507.032297	322784.656843	41.450676
3506.864317	322705.743777	41.455680
3506.362241	322628.841416	41.460685
3506.711548	322546.972859	41.465690
3506.424778	322463.473213	41.470695
3506.669696	322379.687145	41.475700
3506.743656	322297.733752	41.480704
3506.563899	322218.770726	41.485709
3506.454414	322128.653861	41.490714
3506.299220	322053.019354	41.495719
3506.378195	321975.898183	41.500724
3506.442044	321909.794842	41.505728
3506.182057	321835.677228	41.510733
3506.429570	321746.699688	41.515738
3506.114794	321672.005187	41.520743
3506.496559	321586.415429	41.525748
3506.203487	321509.402187	41.530752
3506.503474	321442.243754	41.535757
3506.504908	321368.084644	41.540762
3506.120253	321281.901205	41.545767
3506.312743	321198.935064	41.550772
3506.290016	321126.763665	41.555776
3506.141683	321052.271142	41.560781
3506.464620	320977.679714	41.565786
3505.905667	320900.884833	41.570791
3506.372720	320823.065165	41.575796
3506.041505	320744.530027	41.580800
3505.916296	320661.383315	41.585805
3506.457969	320596.933571	41.590810
3506.127336	320528.599788	41.595815
3506.060811	320440.864130	41.600820
3505.988750	320361.575613	41.605824
3505.888940	320298.446421	41.610829
3506.058585	320220.951798	41.615834
3505.914191	320151.697993	41.620839
3505.980922	320073.710296	41.625844
3505.938333	320011.538549	41.630848
3505.863165	319940.212884	41.635853
3505.886535	319875.511980	41.640858
3505.198263	319802.958541	41.645863
3505.819517	319727.962348	41.650868
3505.873609	319669.133345	41.655872
3505.913376	319597.865556	41.660877
3505.983747	319524.837414	41.665882
3505.722673	319451.148360	41.670887
3505.806473	319376.616822	41.675892
3505.786826	319317.518959	41.680896
3505.671030	319239.151098	41.685901
3505.747336	319167.368082	41.690906
3505.632703	319109.404159	41.695911
3505.753479	319034.357445	41.700916
3505.930849	318965.891262	41.705920
3505.253412	318897.023709	41.710925
3505.676333	318820.911931	41.715930
3505.477701	318767.463868	41.720935
3505.817565	318696.605866	41.725940
3505.805802	318633.104365	41.730944
3505.704265	318566.436469	41.735949
3505.834229	318490.496917	41.740954
3505.777414	318417.435833	41.745959
3505.710995	318353.967877	41.750964
3505.827366	318282.482486	41.755968
3505.397476	318206.349698	41.760973
3505.311983	318141.688611	41.765978
3505.720379	318095.498133	41.770983
3505.530555	318020.065498	41.775988
3505.227089	317957.727887	41.780992
3505.209635	317892.496112	41.785997
3505.398182	317817.411332	41.791002
3505.290657	317760.971084	41.796007
3505.495987	317689.038365	41.801012
3505.399532	317625.319609	41.806016
3505.017941	317567.115327	41.811021
3505.466399	317510.740899	41.816026
3504.948507	317445.382798	41.821031
3505.294047	317380.653526	41.826036
3505.246900	317324.101555	41.831040
3505.198918	317257.855882	41.836045
3505.263459	317195.612590	41.841050
3504.988111	317139.986401	41.846055
3505.387822	317068.327747	41.851060
3505.504189	317005.592708	41.856064
3504.900203	316947.193236	41.861069
3505.176432	316882.957448	41.866074
3504.915282	316830.407285	41.871079
3504.931968	316763.336633	41.876084
3505.317560	316705.927800	41.881088
3505.079138	316642.891257	41.886093
3505.206939	316578.271037	41.891098
3504.995634	316517.825318	41.896103
3505.349469	316455.739528	41.901108
3504.931851	316397.030459	41.906112
3505.076685	316336.808955	41.911117
3505.263222	316275.359593	41.916122
3505.223706	316214.912178	41.921127
3505.082399	316159.594679	41.926132
3505.164639	316108.287857	41.931136
3504.948382	316047.257075	41.936141
3505.360598	315979.436727	41.941146
3504.818560	315925.657033	41.946151
3504.971095	315857.902356	41.951156
3505.035433	315805.682003	41.956160
3505.192412	315739.529415	41.961165
3505.397172	315671.359232	41.966170
3505.062594	315616.172919	41.971175
3505.041788	315548.902744	41.976180
3504.875221	315484.657538	41.981184
3504.667162	315436.957283	41.986189
3504.904923	315377.966797	41.991194
3504.608288	315320.331595	41.996199
3504.875586	315276.577358	42.001204
3504.658734	315221.982904	42.006208
3504.658408	315156.591825	42.011213
3504.979086	315095.247211	42.016218
3504.753963	315039.712392	42.021223
3504.867828	314980.231788	42.026228
3505.110337	314929.229470	42.031232
3505.056811	314876.695617	42.036237
3505.048354	314815.325512	42.041242
3505.063145	314759.040577	42.046247
3504.766573	314698.656591	42.051252
3504.571717	314635.915811	42.056256
3504.806194	314578.247914	42.061261
3504.847620	314530.762334	42.066266
3504.778251	314467.950908	42.071271
3504.669260	314410.946917	42.076276
3504.669246	314363.289501	42.081280
3504.982080	314308.891423	42.086285
3504.871150	314249.648410	42.091290
3504.757194	314204.324021	42.096295
3504.806920	314141.111946	42.101300
3504.906541	314076.899676	42.106304
3504.700962	314031.233149	42.111309
3504.340274	313966.201789	42.116314
3504.433483	313917.435279	42.121319
3504.698439	313866.122952	42.126324
3504.586628	313813.011723	42.131328
3504.784885	313755.221210	42.136333
3504.776807	313704.460090	42.141338
3504.520215	313649.793618	42.146343
3504.435502	313593.191960	42.151348
3504.895317	313545.563925	42.156352
3504.481754	313498.860547	42.161357
3504.808815	313436.113254	42.166362
3504.224051	313385.619641	42.171367
3504.237775	313336.712219	42.176372
3504.902721	313282.716157	42.181376
3504.623798	313233.370708	42.186381
3504.586570	313167.473647	42.191386
3504.526808	313119.544352	42.196391
3504.551100	313067.861472	42.201396
3504.545535	313005.954165	42.206400
3504.251392	312964.320729	42.211405
3504.480509	312909.501469	42.216410
3504.519092	312861.582051	42.221415
3504.434728	312805.157500	42.226420
3504.798642	312755.253495	42.231424
3504.418413	312707.449982	42.236429
3504.361256	312646.440820	42.241434
3504.457130	312605.458849	42.246439
3504.421403	312546.176518	42.251444
3504.228046	312504.043524	42.256448
3504.086521	312457.907466	42.261453
3504.503802	312400.055748	42.266458
3504.372167	312356.869746	42.271463
3503.957848	312300.317814	42.276468
3504.478655	312242.602467	42.281472
3504.435032	312202.608790	42.286477
3504.392119	312153.327261	42.291482
3504.360667	312107.351851	42.296487
3504.528937	312053.584340	42.301492
3504.652356	312003.844193	42.306496
3504.409283	311959.733672	42.311501
3504.636909	311900.027860	42.316506
3504.386216	311849.302484	42.321511
3504.313358	311792.595024	42.326516
3504.086009	311743.265431	42.331520
3504.162585	311705.033848	42.336525
3504.448368	311643.537442	42.341530
3504.213740	311608.763979	42.346535
3504.106965	311554.326213	42.351540
3504.218685	311497.386109	42.356544
3504.079150	311457.762973	42.361549
3504.408458	311401.883080	42.366554
3504.355195	311367.183003	42.371559
3504.304468	311313.423286	42.376564
3503.954209	311265.130172	42.381568
3504.102386	311221.823255	42.386573
3504.321302	311170.795061	42.391578
3504.149425	311125.044123	42.396583
3504.302225	311070.743535	42.401588
3504.231031	311024.696923	42.406592
3503.729309	310975.103873	42.411597
3504.302539	310933.180996	42.416602
3504.692455	310894.212950	42.421607
3503.774581	310836.796115	42.426612
3503.593491	310791.987811	42.431616
3503.520836	310754.109493	42.436621
3504.243134	310705.165426	42.441626
3504.180691	310658.226471	42.446631
3504.058611	310612.543634	42.451636
3504.035268	310573.079811	42.456640
3503.748241	310529.458292	42.461645
3504.079439	310478.539123	42.466650
3504.131904	310436.951317	42.471655
3504.114980	310390.768419	42.476660
3504.391986	310342.453104	42.481664
3504.166827	310303.605740	42.486669
3504.640201	310245.462767	42.491674
3504.341927	310202.478872	42.496679
3504.335337	310155.734310	42.501684
3504.351699	310104.176674	42.506688
3503.809778	310058.049706	42.511693
3504.117919	310011.281476	42.516698
3504.099252	309965.963638	42.521703
3504.193738	309912.892271	42.526708
3504.310811	309871.472055	42.531712
3504.012634	309822.176953	42.536717
3504.186074	309771.179800	42.541722
3503.902768	309720.991635	42.546727
3504.196362	309680.587116	42.551732
3504.206386	309624.220456	42.556736
3503.841897	309583.409320	42.561741
3504.194234	309542.664733	42.566746
3504.054059	309500.826183	42.571751
3503.967280	309449.233007	42.576756
3503.763029	309410.534357	42.581760
3503.832186	309369.655561	42.586765
3503.859310	309328.045301	42.591770
3503.832922	309281.557451	42.596775
3503.871351	309238.316729	42.601780
3504.046796	309192.051860	42.606784
3503.677395	309155.821652	42.611789
3504.310531	309105.108531	42.616794
3504.114385	309062.438551	42.621799
3503.891448	309013.029132	42.626804
3503.807365	308975.278440	42.631808
3503.638367	308926.394937	42.636813
3504.166340	308884.935389	42.641818
3504.033966	308842.357083	42.646823
3503.804093	308786.713871	42.651828
3503.993056	308744.009133	42.656832
3503.366042	308713.340810	42.661837
3503.746437	308666.305572	42.666842
3503.921808	308625.435075	42.671847
3503.877876	308582.562857	42.676852
3503.811413	308538.421724	42.681856
3503.759341	308492.598764	42.686861
3504.183945	308448.940984	42.691866
3503.964702	308405.256118	42.696871
3503.815303	308367.006168	42.701876
3503.908624	308332.001183	42.706880
3503.592389	308278.610241	42.711885
3503.705064	308231.997968	42.716890
3503.899392	308207.410790	42.721895
3503.776057	308157.247025	42.726900
3503.901033	308117.503656	42.731904
3503.684794	308080.052770	42.736909
3503.772942	308034.411148	42.741914
3503.665813	307992.922442	42.746919
3503.790802	307938.291867	42.751924
3503.245837	307896.514941	42.756928
3503.784550	307868.540315	42.761933
3503.901750	307824.242724	42.766938
3503.536270	307792.413416	42.771943
3503.599769	307748.862108	42.776948
3503.764345	307701.605058	42.781952
3503.774522	307674.654150	42.786957
3503.949331	307629.660323	42.791962
3503.762681	307588.107309	42.796967
3503.792670	307546.011585	42.801972
3503.485617	307510.101292	42.806977
3503.533561	307464.439955	42.811981
3503.635457	307421.900317	42.816986
3503.297824	307392.076831	42.821991
3503.595105	307353.909280	42.826996
3503.722174	307313.477841	42.832001
3503.258515	307278.686029	42.837005
3503.587263	307241.404188	42.842010
3503.835120	307195.431565	42.847015
3503.880354	307167.431545	42.852020
3504.213571	307116.839409	42.857025
3503.618267	307071.710434	42.862029
3503.719331	307027.338303	42.867034
3503.580876	306984.683004	42.872039
3503.698766	306946.873890	42.877044
3503.595562	306901.031972	42.882049
3503.677966	306878.242953	42.887053
3503.800640	306830.864359	42.892058
3503.844352	306794.542690	42.897063
3503.888996	306751.985944	42.902068
3503.895490	306711.420091	42.907073
3503.512638	306671.500111	42.912077
3503.518334	306613.298395	42.917082
3503.729209	306583.592662	42.922087
3503.001952	306545.354891	42.927092
3503.503220	306506.595084	42.932097
3503.708551	306476.610215	42.937101
3503.984909	306434.831504	42.942106
3503.625942	306391.726491	42.947111
3503.659713	306349.934562	42.952116
3503.572734	306318.849891	42.957121
3503.647452	306279.087436	42.962125
3503.936340	306228.857591	42.967130
3503.547996	306200.797260	42.972135
3503.528997	306145.652714	42.977140
3503.631380	306115.251020	42.982145
3503.254242	306076.144046	42.987149
3503.799045	306035.112149	42.992154
3503.644101	306000.958536	42.997159
3503.482037	305969.681743	43.002164
3503.537005	305922.211038	43.007169
3503.250937	305886.296321	43.012173
3503.544284	305848.128246	43.017178
3503.128166	305811.801080	43.022183
3503.481504	305781.283788	43.027188
3503.306544	305737.335214	43.032193
3503.524062	305699.586013	43.037197
3503.972852	305659.128635	43.042202
3503.594552	305624.093357	43.047207
3503.750404	305585.539295	43.052212
3503.556987	305545.283559	43.057217
3503.630113	305520.942973	43.062221
3503.537255	305464.027737	43.067226
3503.566712	305430.863017	43.072231
3503.508361	305401.096692	43.077236
3503.310589	305359.060038	43.082241
3503.142703	305328.063700	43.087245
3503.764188	305277.908410	43.092250
3503.340942	305250.591017	43.097255
3503.482536	305219.571904	43.102260
3503.644696	305182.390823	43.107265
3503.278765	305149.720087	43.112269
3503.739455	305098.571668	43.117274
3503.764282	305062.429847	43.122279
3503.679147	305019.790050	43.127284
3503.834903	304970.063226	43.132289
3503.220661	304936.591162	43.137293
3503.461970	304907.210562	43.142298
3503.636526	304870.587215	43.147303
3503.584934	304835.169714	43.152308
3503.794549	304793.120102	43.157313
3503.221555	304757.580087	43.162317
3503.838455	304718.342839	43.167322
3503.712617	304678.432203	43.172327
3503.291015	304638.211265	43.177332
3503.670262	304603.082855	43.182337
3503.228587	304564.544661	43.187341
3503.741777	304516.797754	43.192346
3503.681416	304496.294912	43.197351
3503.715857	304447.044558	43.202356
3503.512480	304407.476625	43.207361
3503.374436	304369.247334	43.212365
3503.463199	304330.244676	43.217370
3503.281033	304284.972593	43.222375
3503.288835	304261.023325	43.227380
3503.379506	304215.581476	43.232385
3503.483693	304185.941856	43.237389
3503.550129	304153.126859	43.242394
3503.414097	304113.497322	43.247399
3503.237174	304072.601622	43.252404
3503.454174	304051.622795	43.257409
3503.284789	304014.008918	43.262413
3503.471842	303967.253907	43.267418
3503.374219	303931.232151	43.272423
3503.355988	303905.148971	43.277428
3503.601131	303866.350681	43.282433
3503.660469	303825.876123	43.287437
3503.672469	303783.042044	43.292442
3503.494852	303752.275327	43.297447
3503.291569	303710.772644	43.302452
3503.634490	303674.860308	43.307457
3503.515632	303641.972023	43.312461
3503.712332	303598.650949	43.317466
3503.674706	303553.661141	43.322471
3503.238535	303527.719160	43.327476
3503.622321	303485.259636	43.332481
3503.036283	303450.458813	43.337485
3503.243687	303408.459328	43.342490
3503.265045	303385.372857	43.347495
3503.100845	303358.370460	43.352500
3503.383243	303308.876844	43.357505
3503.182569	303279.640456	43.362509
3503.573311	303239.877384	43.367514
3503.195535	303213.417154	43.372519
3503.225806	303176.000659	43.377524
3503.655803	303141.652332	43.382529
3503.246047	303111.837577	43.387533
3502.960234	303064.926292	43.392538
3502.788875	303038.255700	43.397543
3503.467065	303002.316184	43.402548
3503.083575	302969.799514	43.407553
3503.194687	302949.040328	43.412557
3503.341826	302908.678653	43.417562
3503.169637	302875.798188	43.422567
3503.258675	302835.369147	43.427572
3503.560924	302808.242981	43.432577
3503.301424	302780.389799	43.437581
3503.126879	302741.732341	43.442586
3503.193447	302709.527235	43.447591
3503.249846	302677.552746	43.452596
3503.061669	302635.563303	43.457601
3502.704762	302611.949993	43.462605
3503.255495	302574.782941	43.467610
3503.321958	302547.158870	43.472615
3503.154293	302526.213844	43.477620
3503.271318	302477.890466	43.482625
3503.090236	302450.559372	43.487629
3503.322197	302413.645418	43.492634
3503.131602	302379.113211	43.497639
3503.305530	302342.869958	43.502644
3503.023473	302308.555545	43.507649
3502.902209	302275.234119	43.512653
3503.081854	302243.291093	43.517658
3502.988812	302222.588843	43.522663
3503.254410	302183.964291	43.527668
3503.373306	302146.762337	43.532673
3503.107463	302122.854679	43.537677
3503.386512	302089.674451	43.542682
3503.201090	302053.537823	43.547687
3502.796170	302021.049357	43.552692
3503.177452	301984.468183	43.557697
3502.999493	301957.009096	43.562701
3503.291043	301917.184118	43.567706
3503.092668	301894.716565	43.572711
3502.957980	301855.899556	43.577716
3502.962344	301828.335678	43.582721
3502.956681	301803.343899	43.587725
3503.296196	301762.875068	43.592730
3503.106822	301735.519447	43.597735
3503.015448	301699.240690	43.602740
3503.214607	301664.112898	43.607745
3503.048219	301638.866092	43.612749
3502.809062	301611.416350	43.617754
3502.988843	301575.706141	43.622759
3502.846314	301549.946557	43.627764
3503.025426	301524.315068	43.632769
3502.985389	301490.267882	43.637773
3503.213314	301456.178976	43.642778
3503.360376	301433.453866	43.647783
3503.302357	301400.402018	43.652788
3503.246195	301361.012506	43.657793
3502.802316	301330.387624	43.662797
3503.231560	301300.161331	43.667802
3503.032229	301271.738072	43.672807
3503.171831	301230.714571	43.677812
3503.423281	301201.152173	43.682817
3503.343617	301164.184048	43.687821
3503.171966	301138.097932	43.692826
3503.232327	301093.828887	43.697831
3503.250320	301068.731281	43.702836
3503.285941	301038.973318	43.707841
3502.983917	301004.381213	43.712845
3502.929073	300971.099546	43.717850
3503.142098	300942.331980	43.722855
3502.875635	300907.428862	43.727860
3503.336037	300873.456121	43.732865
3503.135019	300851.904797	43.737869
3502.856336	300808.222759	43.742874
3503.049127	300787.577284	43.747879
3503.041562	300760.269233	43.752884
3503.208258	300725.374947	43.757889
3502.898945	300698.368335	43.762893
3503.100131	300674.921842	43.767898
3502.668153	300643.225754	43.772903
3503.029263	300612.017070	43.777908
3503.152143	300569.468577	43.782913
3503.006659	300553.991425	43.787917
3502.925147	300510.227563	43.792922
3502.885663	300481.193627	43.797927
3503.057243	300461.009459	43.802932
3503.239169	300414.888426	43.807937
3503.035995	300391.530186	43.812941
3503.186865	300356.816289	43.817946
3503.540064	300322.198144	43.822951
3503.565120	300297.837184	43.827956
3503.571805	300263.883765	43.832961
3503.146569	300228.317722	43.837965
3503.367372	300191.862118	43.842970
3503.487447	300151.426234	43.847975
3503.288701	300111.345354	43.852980
3503.224652	300080.737016	43.857985
3503.061646	300050.474935	43.862989
3503.278405	300020.357355	43.867994
3503.302884	299998.897863	43.872999
3503.146124	299963.137158	43.878004
3503.252109	299922.906913	43.883009
3502.995680	299888.917850	43.888013
3503.245580	299855.460822	43.893018
3502.917598	299828.202166	43.898023
3502.630981	299791.647095	43.903028
3502.984765	299758.479266	43.908033
3502.913483	299738.841664	43.913037
3502.982878	299706.227098	43.918042
3503.073472	299678.419644	43.923047
3503.139703	299653.008458	43.928052
3502.563946	299610.771554	43.933057
3502.790601	299594.956249	43.938061
3503.117978	299556.905614	43.943066
3502.673792	299528.646810	43.948071
3502.883936	299504.765738	43.953076
3503.248906	299461.466056	43.958081
3503.103634	299442.068932	43.963085
3503.121809	299414.858014	43.968090
3502.755835	299384.907124	43.973095
3503.034171	299358.393806	43.978100
3502.994248	299318.873035	43.983105
3503.234568	299297.583300	43.988109
3502.923682	299251.868860	43.993114
3502.951981	299233.259123	43.998119
3502.857854	299196.368277	44.003124
3503.054976	299162.689974	44.008129
3502.525521	299136.251348	44.013133
3503.091058	299100.937636	44.018138
3502.741702	299082.335712	44.023143
3502.872203	299059.510386	44.028148
3503.338868	299023.499347	44.033153
3503.067329	298998.751278	44.038157
3503.086856	298964.464182	44.043162
3502.643232	298937.706677	44.048167
3502.741890	298907.759584	44.053172
3502.846183	298878.778789	44.058177
3502.868721	298847.214557	44.063181
3503.286811	298820.933760	44.068186
3503.004072	298798.478062	44.073191
3502.934672	298764.586467	44.078196
3503.362953	298724.916058	44.083201
3503.246624	298695.714976	44.088205
3503.257471	298650.815360	44.093210
3503.215083	298637.205111	44.098215
3503.030357	298603.178650	44.103220
3503.077984	298565.145418	44.108225
3502.924421	298530.859538	44.113229
3502.973973	298507.333912	44.118234
3502.921193	298477.791944	44.123239
3503.035010	298445.500610	44.128244
3503.080965	298409.936432	44.133249
3502.753674	298394.410609	44.138253
3503.055565	298350.509019	44.143258
3503.581202	298324.185801	44.148263
3502.852127	298293.985397	44.153268
3503.197490	298255.803814	44.158273
3502.981170	298238.631708	44.163277
3502.933568	298205.729038	44.168282
3503.067713	298171.245452	44.173287
3502.904178	298142.916819	44.178292
3502.796031	298109.590819	44.183297
3502.663957	298081.282712	44.188301
3502.578071	298059.381497	44.193306
3502.791164	298033.972173	44.198311
3502.972638	298000.117437	44.203316
3502.798706	297969.855924	44.208321
3502.630027	297958.810442	44.213325
3502.292749	297928.294345	44.218330
3502.747790	297907.657895	44.223335
3502.440199	297877.213509	44.228340
3502.980129	297860.763550	44.233345
3502.741995	297833.897182	44.238349
3502.681228	297801.098137	44.243354
3502.925042	297771.942343	44.248359
3502.730146	297750.388859	44.253364
3502.760421	297723.455219	44.258369
3502.713725	297704.474852	44.263373
3502.448895	297671.554768	44.268378
3502.745645	297648.423017	44.273383
3502.694827	297622.825500	44.278388
3502.863035	297594.521328	44.283393
3502.614929	297573.612381	44.288397
3502.916220	297548.392739	44.293402
3502.753759	297518.790978	44.298407
3502.633017	297488.800914	44.303412
3502.972431	297459.019211	44.308417
3502.713277	297437.475608	44.313421
3502.985212	297411.522335	44.318426
3503.111423	297386.788021	44.323431
3502.851406	297354.732408	44.328436
3502.973895	297331.322209	44.333441
3503.194455	297292.726696	44.338445
3502.780268	297264.792972	44.343450
3503.042650	297238.713842	44.348455
3502.830964	297209.654095	44.353460
3502.756875	297176.398606	44.358465
3502.769561	297159.292349	44.363469
3502.902259	297125.953745	44.368474
3502.573886	297099.482870	44.373479
3502.578240	297074.563758	44.378484
3502.950672	297050.427313	44.383489
3502.586242	297020.016765	44.388493
3503.304905	296998.397195	44.393498
3502.777656	296972.797166	44.398503
3503.053139	296944.119633	44.403508
3503.032438	296907.241317	44.408513
3502.570181	296881.911119	44.413517
3502.926616	296846.933981	44.418522
3502.813277	296823.992977	44.423527
3502.794906	296785.077957	44.428532
3503.174052	296761.500318	44.433537
3502.955761	296745.651641	44.438541
3502.891617	296716.110524	44.443546
3502.844855	296686.770314	44.448551
3502.856658	296667.933220	44.453556
3503.328577	296616.164195	44.458561
3502.451556	296596.879962	44.463565
3502.477524	296569.819181	44.468570
3502.818367	296543.294817	44.473575
3502.491811	296517.561540	44.478580
3502.748506	296490.617539	44.483585
3502.412596	296483.593986	44.488589
3502.237793	296441.088685	44.493594
3503.034756	296425.463735	44.498599
3502.655058	296401.113163	44.503604
3503.025265	296369.188011	44.508609
3502.742449	296353.883790	44.513613
3502.697826	296320.266871	44.518618
3502.584066	296292.922261	44.523623
3502.890480	296274.064646	44.528628
3503.313974	296238.720354	44.533633
3503.094046	296206.912398	44.538637
3502.755186	296176.064714	44.543642
3502.990728	296143.345878	44.548647
3502.895238	296116.176517	44.553652
3502.837345	296084.623269	44.558657
3502.721690	296066.314885	44.563661
3502.786378	296028.251853	44.568666
3503.018446	296010.347507	44.573671
3502.679319	295977.412558	44.578676
3502.752424	295948.740570	44.583681
3502.834520	295930.935899	44.588685
3502.878396	295896.032277	44.593690
3502.690865	295878.982251	44.598695
3502.620946	295853.997808	44.603700
3502.801270	295826.810845	44.608705
3502.649949	295810.773314	44.613709
3502.701941	295781.493639	44.618714
3502.692557	295752.579853	44.623719
3502.570846	295736.766777	44.628724
3502.959136	295706.263858	44.633729
3502.677473	295682.534074	44.638733
3502.623786	295651.310836	44.643738
3502.406021	295624.796618	44.648743
3502.690687	295599.604165	44.653748
3502.804467	295575.252817	44.658753
3502.602329	295557.695893	44.663757
3502.736904	295534.588531	44.668762
3502.779804	295499.888455	44.673767
3502.635175	295477.460865	44.678772
3502.919967	295444.148532	44.683777
3502.918848	295427.552990	44.688781
3502.788630	295399.905075	44.693786
3502.859125	295368.586000	44.698791
3502.695177	295341.961463	44.703796
3502.585729	295307.743152	44.708801
3502.565095	295283.845317	44.713805
3502.588576	295258.260643	44.718810
3502.928755	295247.924529	44.723815
3502.647029	295221.700076	44.728820
3502.756060	295193.734840	44.733825
3502.431213	295175.076919	44.738829
3502.613574	295149.060210	44.743834
3502.664357	295122.198527	44.748839
3502.683947	295100.025232	44.753844
3502.649650	295064.115117	44.758849
3502.239191	295050.586747	44.763853
3502.438992	295033.399838	44.768858
3502.270431	295004.637724	44.773863
3502.496876	294990.984776	44.778868
3502.621081	294956.271727	44.783873
3502.544196	294944.345942	44.788877
3502.350416	294909.198719	44.793882
3502.817240	294882.475819	44.798887
3502.580956	294865.025818	44.803892
3502.720895	294837.310144	44.808897
3502.565007	294818.167642	44.813901
3502.413575	294790.115475	44.818906
3502.672552	294764.723028	44.823911
3502.541603	294749.903838	44.828916
3502.643452	294717.943183	44.833921
3502.829868	294703.049141	44.838925
3503.078116	294673.763828	44.843930
3502.950219	294639.726179	44.848935
3502.865032	294620.801700	44.853940
3502.986343	294585.757979	44.858945
3502.934028	294558.784812	44.863949
3502.902282	294529.135729	44.868954
3502.779897	294509.427920	44.873959
3502.598495	294491.485636	44.878964
3502.750226	294454.171668	44.883969
3502.687116	294438.298215	44.888973
3502.726579	294405.227108	44.893978
3503.070041	294380.457710	44.898983
3502.628656	294363.217657	44.903988
3502.789054	294326.054987	44.908993
3502.579903	294294.549769	44.913997
3502.900252	294267.925749	44.919002
3502.601135	294242.390836	44.924007
3502.294754	294219.147943	44.929012
3502.873769	294185.712754	44.934017
3502.794222	294171.241783	44.939021
3502.747725	294140.500261	44.944026
3502.846750	294124.677858	44.949031
3502.603091	294082.639743	44.954036
3502.649100	294060.080131	44.959041
3502.649236	294037.476740	44.964045
3502.401971	294004.399120	44.969050
3502.783569	293988.150891	44.974055
3502.493456	293976.079911	44.979060
3502.324798	293943.142753	44.984065
3502.375360	293918.469651	44.989069
3502.650307	293896.103443	44.994074
3502.684334	293863.414700	44.999079
3502.720252	293848.798410	45.004084
3503.057533	293817.156999	45.009089
3502.602495	293789.635242	45.014093
3502.479358	293771.429128	45.019098
3502.405490	293753.469888	45.024103
3502.055343	293739.957288	45.029108
3502.152409	293707.945926	45.034113
3502.707752	293689.506934	45.039117
3502.539728	293667.540483	45.044122
3502.413161	293642.207555	45.049127
3502.206052	293632.847241	45.054132
3502.677093	293606.428570	45.059137
3502.282427	293591.039216	45.064141
3502.205230	293565.749483	45.069146
3502.273099	293541.429899	45.074151
3502.344335	293526.986218	45.079156
3502.612054	293496.348198	45.084161
3502.685547	293480.885965	45.089165
3502.545928	293465.049614	45.094170
3502.727324	293428.723127	45.099175
3502.495795	293413.130158	45.104180
3502.504066	293387.368864	45.109185
3502.590890	293371.471797	45.114189
3502.692268	293340.452306	45.119194
3502.629997	293312.411024	45.124199
3502.565075	293296.664825	45.129204
3502.505769	293262.692083	45.134209
3502.410566	293238.448663	45.139213
3502.524398	293221.860073	45.144218
3502.361283	293194.445346	45.149223
3502.320954	293178.466195	45.154228
3502.645368	293155.073819	45.159233
3502.336103	293138.474681	45.164237
3502.491596	293118.112254	45.169242
3502.577744	293090.455052	45.174247
3502.332392	293077.155090	45.179252
3502.733132	293047.972529	45.184257
3502.394002	293031.658013	45.189261
3502.264097	293009.507206	45.194266
3502.592602	292986.674138	45.199271
3502.736187	292968.273546	45.204276
3502.741555	292937.828798	45.209281
3502.600027	292923.188987	45.214285
3502.859941	292897.668331	45.219290
3502.542140	292865.797446	45.224295
3502.549932	292844.490622	45.229300
3502.945125	292811.541468	45.234305
3502.534392	292794.194374	45.239309
3502.926911	292766.591169	45.244314
3502.904876	292729.761363	45.249319
3502.318785	292713.459737	45.254324
3502.322014	292684.669775	45.259329
3502.847149	292669.824341	45.264333
3502.706369	292632.707494	45.269338
3502.742974	292616.716224	45.274343
3502.655325	292596.595100	45.279348
3502.644991	292562.588891	45.284353
3502.689252	292542.650864	45.289357
3502.296427	292509.595076	45.294362
3502.745950	292486.870264	45.299367
3502.397861	292463.124080	45.304372
3502.607990	292436.643681	45.309377
3502.550432	292425.401679	45.314381
3502.258834	292401.443038	45.319386
3502.491065	292375.341002	45.324391
3502.232723	292358.300987	45.329396
3502.665080	292334.942411	45.334401
3502.373938	292327.555023	45.339405
3502.249558	292296.977415	45.344410
3502.432093	292274.981363	45.349415
3502.416519	292252.328840	45.354420
3502.549558	292233.166011	45.359425
3502.452327	292214.726300	45.364429
3502.569371	292197.831469	45.369434
3502.435310	292162.138787	45.374439
3502.504688	292154.033439	45.379444
3502.612274	292117.590379	45.384449
3502.298838	292102.340739	45.389453
3502.467414	292068.051862	45.394458
3502.740604	292054.441886	45.399463
3502.570421	292040.289974	45.404468
3502.830890	292004.917637	45.409473
3502.739219	291987.597030	45.414477
3502.481325	291954.799955	45.419482
3502.711481	291927.603469	45.424487
3502.663088	291903.275868	45.429492
3502.669557	291879.372463	45.434497
3502.509984	291863.233336	45.439501
3502.333129	291841.445788	45.444506
3502.475427	291812.506499	45.449511
3502.463020	291801.002802	45.454516
3502.879906	291764.002293	45.459521
3502.668862	291744.154647	45.464525
3502.393349	291722.993341	45.469530
3502.424928	291696.947696	45.474535
3502.537699	291681.606173	45.479540
3502.549800	291665.669380	45.484545
3502.577798	291640.667945	45.489549
3502.220756	291618.221059	45.494554
3502.731021	291589.402594	45.499559
3502.364936	291576.299282	45.504564
3502.432647	291540.931220	45.509569
3502.535490	291517.470877	45.514573
3502.670829	291500.700286	45.519578
3502.972597	291473.645191	45.524583
3502.425195	291457.769954	45.529588
3502.269652	291427.451320	45.534593
3502.651315	291406.696753	45.539597
3502.537082	291376.804411	45.544602
3502.681988	291360.134116	45.549607
3502.660531	291333.511093	45.554612
3502.682240	291315.841730	45.559617
3502.398107	291285.695771	45.564621
3502.409788	291267.977045	45.569626
3502.975287	291234.465977	45.574631
3502.716593	291213.760082	45.579636
3503.071017	291178.423565	45.584641
3502.612104	291154.286831	45.589645
3502.304250	291139.239730	45.594650
3502.607013	291105.820390	45.599655
3502.526195	291093.894460	45.604660
3502.480969	291070.227889	45.609665
3502.673065	291042.222355	45.614669
3502.704917	291026.995086	45.619674
3502.441295	290997.787659	45.624679
3502.159715	290976.525220	45.629684
3502.251223	290961.746855	45.634689
3502.140395	290936.410360	45.639693
3502.062429	290929.269646	45.644698
3502.400544	290902.946866	45.649703
3502.224064	290889.152052	45.654708
3502.319884	290864.877971	45.659713
3502.330503	290843.162723	45.664717
3502.294034	290832.579002	45.669722
3502.409412	290801.530597	45.674727
3502.102013	290789.945338	45.679732
3502.401938	290767.446824	45.684737
3502.208529	290754.291012	45.689741
3502.283172	290734.780425	45.694746
3502.503345	290703.944767	45.699751
3502.255760	290693.368419	45.704756
3502.430748	290661.114241	45.709761
3502.208391	290641.166179	45.714765
3502.151881	290620.835921	45.719770
3502.724361	290597.836726	45.724775
3502.449783	290580.926029	45.729780
3502.673755	290556.479151	45.734785
3502.339385	290532.399164	45.739789
3502.317662	290516.798269	45.744794
3502.253895	290495.247212	45.749799
3502.413542	290470.072087	45.754804
3502.567958	290455.360182	45.759809
3502.586576	290426.388585	45.764813
3502.490253	290396.518444	45.769818
3502.452173	290320.971081	45.774823
3501.875080	290221.120571	45.779828
3501.758450	290066.645729	45.784833
3501.072415	289871.732806	45.789837
3500.229199	289635.400854	45.794842
3499.743030	289359.835018	45.799847
3498.442575	289043.206005	45.804852
3498.111347	288683.300966	45.809857
3496.811155	288297.986034	45.814861
3495.463115	287869.399345	45.819866
3494.412152	287394.762473	45.824871
3493.105295	286905.702219	45.829876
3491.751373	286380.546845	45.834881
3489.830270	285821.082148	45.839885
3487.751994	285235.975617	45.844890
3486.457177	284611.052770	45.849895
3484.157683	283973.729597	45.854900
3482.291527	283291.424002	45.859905
3479.798798	282600.145947	45.864909
3478.006698	281885.202418	45.869914
3475.982581	281128.254348	45.874919
3473.200497	280366.451795	45.879924
3470.925592	279580.655590	45.884929
3468.708885	278767.676052	45.889933
3466.059602	277943.272525	45.894938
3463.987553	277088.446622	45.899943
3460.830346	276226.880426	45.904948
3458.222339	275335.022375	45.909953
3455.520251	274429.521842	45.914957
3452.467367	273521.290759	45.919962
3449.718328	272581.404123	45.924967
3446.903703	271645.184149	45.929972
3443.827631	270684.881765	45.934977
3440.580753	269721.107364	45.939981
3437.154021	268735.274260	45.944986
3434.291087	267737.910039	45.949991
3431.240105	266761.954447	45.954996
3428.118420	265744.875811	45.960001
3425.046094	264741.046261	45.965005
3421.513673	263712.043292	45.970010
3418.664140	262684.910454	45.975015
3414.921286	261650.624073	45.980020
3411.621094	260603.195704	45.985025
3408.225351	259564.380164	45.990029
3404.801368	258514.024102	45.995034
3401.858773	257448.151912	46.000039
3397.779027	256401.623846	46.005044
3394.601180	255332.078430	46.010049
3391.243346	254255.676761	46.015053
3387.302031	253191.378076	46.020058
3384.049489	252117.847434	46.025063
3380.600799	251049.713410	46.030068
3376.963573	249974.394416	46.035073
3373.361049	248892.721767	46.040077
3369.589303	247810.686792	46.045082
3365.781717	246734.101139	46.050087
3361.879320	245653.373013	46.055092
3358.374574	244565.446270	46.060097
3354.979737	243505.053420	46.065101
3350.694964	242422.611353	46.070106
3347.454609	241336.563738	46.075111
3343.241892	240271.088583	46.080116
3340.024608	239202.067160	46.085121
3336.570028	238134.352313	46.090125
3332.566110	237069.291813	46.095130
3328.948416	235992.707118	46.100135
3325.313319	234946.710240	46.105140
3322.059967	233866.650549	46.110145
3318.219298	232797.147639	46.115149
3314.693735	231724.664773	46.120154
3310.622644	230663.063953	46.125159
3307.025062	229589.952482	46.130164
3303.465157	228530.714678	46.135169
3299.754083	227469.181932	46.140173
3295.621684	226412.986355	46.145178
3291.921295	225352.240796	46.150183
3288.178089	224306.554208	46.155188
3284.334520	223254.796503	46.160193
3280.548061	222207.742340	46.165197
3277.067864	221167.416206	46.170202
3273.297438	220121.787949	46.175207
3269.269938	219082.288259	46.180212
3265.719567	218048.293753	46.185217
3261.834253	217013.767584	46.190221
3258.139939	215978.959276	46.195226
3254.184449	214954.152421	46.200231
3250.735913	213934.490506	46.205236
3246.757463	212920.135098	46.210241
3243.198101	211898.917604	46.215245
3239.331119	210887.200271	46.220250
3236.030844	209871.043379	46.225255
3231.919996	208866.349964	46.230260
3228.284390	207854.175539	46.235265
3224.919364	206837.863135	46.240269
3221.043636	205831.338217	46.245274
3217.124364	204840.487643	46.250279
3213.383468	203843.094618	46.255284
3209.444776	202845.151941	46.260289
3206.135978	201841.055593	46.265293
3201.974019	200849.169322	46.270298
3198.119437	199861.570589	46.275303
3194.547828	198886.005265	46.280308
3190.699420	197898.596325	46.285313
3187.383995	196921.552338	46.290317
3183.133455	195957.572014	46.295322
3179.254616	194980.018092	46.300327
3175.765359	194022.910816	46.305332
3171.903043	193065.868694	46.310337
3168.357666	192099.107654	46.315341
3164.266436	191151.640119	46.320346
3160.623729	190199.195603	46.325351
3156.316190	189262.319644	46.330356
3152.795230	188320.643601	46.335361
3148.976684	187383.503731	46.340365
3145.372767	186452.704767	46.345370
3141.739004	185532.002533	46.350375
3137.735972	184608.284976	46.355380
3133.976119	183681.788094	46.360385
3130.609310	182769.498344	46.365389
3126.830489	181855.931911	46.370394
3122.971524	180944.882266	46.375399
3119.195440	180049.717469	46.380404
3115.230262	179141.146948	46.385409
3111.812893	178235.581499	46.390413
3107.683920	177346.941096	46.395418
3104.209147	176445.668443	46.400423
3100.136731	175575.994146	46.405428
3096.469722	174682.600074	46.410433
3092.817000	173806.145104	46.415437
3088.770446	172934.102182	46.420442
3085.211423	172057.244910	46.425447
3081.110073	171199.169640	46.430452
3077.548436	170345.284682	46.435457
3073.984476	169485.719834	46.440461
3069.629308	168635.949946	46.445466
3065.758796	167794.897961	46.450471
3061.915680	166959.401662	46.455476
3058.308462	166127.646486	46.460481
3054.904659	165293.922236	46.465485
3050.690422	164478.052736	46.470490
3047.339934	163649.623024	46.475495
3042.812394	162839.703053	46.480500
3039.060211	162025.637683	46.485505
3035.806249	161225.238700	46.490509
3031.657875	160427.636424	46.495514
3028.072844	159628.569338	46.500519
3024.002117	158841.717549	46.505524
3020.222934	158051.890506	46.510529
3016.360574	157277.703077	46.515533
3012.737328	156506.822984	46.520538
3008.696110	155747.077700	46.525543
3004.568356	154993.146452	46.530548
3000.943782	154240.203062	46.535553
2997.091234	153495.144550	46.540557
2992.889577	152746.523212	46.545562
2988.706339	152006.588217	46.550567
2985.413573	151291.683665	46.555572
2981.273979	150576.398462	46.560577
2977.408136	149861.347322	46.565581
2973.593103	149163.413459	46.570586
2969.514782	148467.336696	46.575591
2965.740717	147781.070973	46.580596
2961.475979	147095.475955	46.585601
2958.083595	146415.989370	46.590605
2953.806139	145750.939195	46.595610
2950.170250	145087.095747	46.600615
2946.028216	144441.853557	46.605620
2942.042435	143797.244281	46.610625
2938.758556	143162.967742	46.615629
2934.525327	142520.156758	46.620634
2930.801279	141899.121378	46.625639
2926.932160	141280.712085	46.630644
2923.159834	140665.870891	46.635649
2919.725840	140053.542279	46.640653
2915.625080	139459.544564	46.645658
2912.009260	138849.409977	46.650663
2908.211625	138269.209777	46.655668
2904.334466	137669.525641	46.660673
2900.530840	137087.661772	46.665677
2896.531996	136510.275674	46.670682
2892.414733	135932.826251	46.675687
2888.685963	135376.022122	46.680692
2885.115770	134824.670507	46.685697
2881.119998	134261.815330	46.690701
2877.551820	133718.911406	46.695706
2874.219279	133174.590859	46.700711
2870.177313	132640.080873	46.705716
2866.666162	132104.655235	46.710721
2863.066773	131496.601909	46.715725
2859.505780	130952.191997	46.720730
2855.948964	130422.213249	46.725735
2852.468056	129901.756714	46.730740
2848.707175	129371.492063	46.735745
2845.154353	128836.533480	46.740749
2841.552060	128319.613294	46.745754
2838.134620	127799.948739	46.750759
2834.294922	127290.201236	46.755764
2830.950762	126769.736862	46.760769
2827.347121	126249.065068	46.765773
2823.761472	125741.332279	46.770778
2820.269184	125225.616605	46.775783
2816.450708	124715.071149	46.780788
2812.947854	124203.325665	46.785793
2809.665575	123689.644637	46.790797
2805.571105	123179.161690	46.795802
2801.854885	122678.114068	46.800807
2798.536786	122172.852116	46.805812
2795.186928	121665.884716	46.810817
2791.702521	121166.791523	46.815821
2787.754942	120676.004926	46.820826
2784.281239	120163.607908	46.825831
2780.823583	119665.407381	46.830836
2777.133905	119167.961573	46.835841
2773.742798	118674.545119	46.840845
2770.039512	118192.386900	46.845850
2766.917831	117688.208611	46.850855
2763.252077	117198.312994	46.855860
2759.521077	116699.685316	46.860865
2756.205212	116201.851660	46.865869
2752.273866	115712.245771	46.870874
2749.142491	115231.511738	46.875879
2745.412363	114736.903000	46.880884
2741.602173	114243.178028	46.885889
2738.262886	113751.865880	46.890893
2734.767724	113271.087078	46.895898
2731.062028	112788.249512	46.900903
2727.497020	112309.821168	46.905908
2723.634251	111819.188945	46.910913
2720.065906	111345.961449	46.915917
2716.315293	110872.527052	46.920922
2712.933824	110386.327736	46.925927
2709.278591	109920.074558	46.930932
2705.748728	109452.257018	46.935937
2702.584381	108971.917117	46.940941
2698.759083	108499.619681	46.945946
2695.016398	108029.426171	46.950951
2691.771911	107561.691372	46.955956
2687.694761	107106.792398	46.960961
2684.322822	106626.034340	46.965965
2680.462083	106180.050853	46.970970
2677.312036	105713.724976	46.975975
2672.926674	105267.263087	46.980980
2668.757201	104811.468515	46.985985
2665.502744	104365.414622	46.990989
2661.757463	103935.624676	46.995994
2657.996824	103487.068149	47.000999
2654.653356	103055.727103	47.006004
2650.895107	102625.295142	47.011009
2647.220184	102192.885662	47.016013
2643.282667	101766.966997	47.021018
2639.643307	101348.150722	47.026023
2635.630935	100933.833745	47.031028
2632.055513	100521.474950	47.036033
2628.623405	100100.291112	47.041037
2624.912273	99704.563010	47.046042
2621.037293	99305.903925	47.051047
2617.524925	98908.095730	47.056052
2613.854773	98508.283543	47.061057
2610.571481	98113.881092	47.066061
2606.502124	97718.957700	47.071066
2603.224555	97328.148046	47.076071
2599.463031	96931.445461	47.081076
2596.103323	96550.227847	47.086081
2592.641942	96150.540019	47.091085
2588.972361	95771.388010	47.096090
2585.725995	95381.411029	47.101095
2582.276157	95000.772767	47.106100
2578.570076	94614.066629	47.111105
2575.350047	94215.268324	47.116109
2571.553903	93834.901609	47.121114
2568.242390	93447.869116	47.126119
2564.797499	93059.680501	47.131124
2561.015832	92672.514948	47.136129
2557.817608	92281.146521	47.141133
2554.467227	91900.086450	47.146138
2550.877725	91504.011246	47.151143
2547.585388	91115.861818	47.156148
2544.110549	90730.858786	47.161153
2540.973803	90337.155319	47.166157
2536.925874	89947.448674	47.171162
2533.780706	89543.846445	47.176167
2530.145124	89152.802743	47.181172
2526.671623	88764.864463	47.186177
2523.698605	88369.649579	47.191181
2520.191452	87977.902618	47.196186
2516.572535	87569.687475	47.201191
2513.293646	87174.053450	47.206196
2509.630646	86766.389942	47.211201
2506.232882	86360.799753	47.216205
2502.413219	85970.944984	47.221210
2499.136993	85557.407049	47.226215
2495.527582	85151.828579	47.231220
2492.182706	84754.903858	47.236225
2488.564508	84344.536183	47.241229
2484.906947	83949.525939	47.246234
2481.447283	83540.720301	47.251239
2478.064273	83146.605752	47.256244
2474.728870	82738.287700	47.261249
2471.298448	82322.673700	47.266253
2467.280296	81929.297330	47.271258
2464.210134	81523.165738	47.276263
2460.775129	81120.564409	47.281268
2457.317324	80720.195211	47.286273
2453.775947	80300.970257	47.291277
2449.810592	79900.983929	47.296282
2446.193151	79489.784883	47.301287
2442.771800	79080.504669	47.306292
2439.078487	78687.377448	47.311297
2435.883440	78283.179556	47.316301
2432.529406	77873.551164	47.321306
2429.222108	77465.356744	47.326311
2425.661054	77058.668413	47.331316
2421.917600	76645.588407	47.336321
2418.544430	76245.144017	47.341325
2415.142752	75832.264488	47.346330
2411.713445	75425.199135	47.351335
2408.158049	75020.000917	47.356340
2404.290786	74620.432158	47.361345
2401.352051	74200.368818	47.366349
2397.590727	73795.259248	47.371354
2393.946862	73371.877375	47.376359
2391.055271	72965.654602	47.381364
2387.215314	72553.008114	47.386369
2384.037353	72143.287098	47.391373
2380.214939	71724.517822	47.396378
2376.799284	71309.628080	47.401383
2373.391467	70902.653986	47.406388
2370.124092	70489.639672	47.411393
2366.394942	70065.714746	47.416397
2362.944366	69651.599518	47.421402
2359.544111	69229.985894	47.426407
2355.829512	68821.695487	47.431412
2352.082991	68412.191351	47.436417
2348.350423	67981.007301	47.441421
2344.807956	67572.240182	47.446426
2341.514310	67157.093219	47.451431
2338.178954	66744.638157	47.456436
2334.629903	66325.939065	47.461441
2331.380381	65915.896105	47.466445
2327.716193	65505.200728	47.471450
2324.188981	65082.316918	47.476455
2320.846256	64666.069515	47.481460
2317.168883	64245.634997	47.486465
2313.777567	63829.466147	47.491469
2310.414132	63413.280843	47.496474
2307.018966	62981.583647	47.501479
2303.424586	62565.156509	47.506484
2299.559074	62146.208272	47.511489
2296.409016	61718.309082	47.516493
2292.728120	61304.969171	47.521498
2289.372662	60875.295228	47.526503
2285.824129	60456.465993	47.531508
2282.301835	60038.299805	47.536513
2279.228784	59609.022949	47.541517
2275.598005	59189.949016	47.546522
2271.985644	58761.113712	47.551527
2268.476908	58332.840952	47.556532
2264.699493	57903.310466	47.561537
2261.468227	57489.508451	47.566541
2257.660840	57071.532988	47.571546
2254.293207	56638.750712	47.576551
2250.477409	56203.990284	47.581556
2247.050764	55786.955111	47.586561
2243.292920	55364.294018	47.591565
2239.863654	54949.278841	47.596570
2236.404715	54521.618508	47.601575
2233.115145	54104.604271	47.606580
2229.906469	53693.592740	47.611585
2226.342574	53260.744029	47.616589
2222.591825	52838.590184	47.621594
2218.896689	52413.948529	47.626599
2215.641636	51988.440462	47.631604
2211.840972	51561.413814	47.636609
2208.759738	51128.167958	47.641613
2205.153499	50716.503169	47.646618
2201.861778	50290.955828	47.651623
2198.147436	49865.558232	47.656628
2194.645906	49440.312992	47.661633
2191.301359	49015.672807	47.666637
2187.679553	48593.227506	47.671642
2184.292147	48157.262739	47.676647
2180.747414	47731.199770	47.681652
2177.272673	47304.252307	47.686657
2174.173217	46866.872163	47.691661
2170.485827	46446.823638	47.696666
2167.015005	46008.934432	47.701671
2163.563006	45580.424179	47.706676
2159.448980	45150.763123	47.711681
2156.561468	44711.286430	47.716685
2152.937419	44288.547879	47.721690
2149.415314	43850.512293	47.726695
2145.470630	43425.798099	47.731700
2141.948714	42996.340113	47.736705
2138.979540	42556.588993	47.741709
2135.020067	42137.564416	47.746714
2131.492594	41712.653375	47.751719
2128.337651	41271.371640	47.756724
2124.595559	40851.323275	47.761729
2121.221720	40416.496823	47.766733
2117.508685	39987.235227	47.771738
2114.274240	39555.200361	47.776743
2110.699324	39118.269153	47.781748
2107.163604	38688.168778	47.786753
2104.000433	38257.201153	47.791757
2099.387257	37828.147831	47.796762
2096.626743	37395.232898	47.801767
2093.159757	36967.964634	47.806772
2089.419272	36534.775844	47.811777
2086.445045	36108.506738	47.816781
2082.881381	35677.019437	47.821786
2079.179344	35234.184079	47.826791
2075.846812	34804.288638	47.831796
2072.339465	34377.756939	47.836801
2068.735446	33930.274720	47.841805
2065.085323	33491.797029	47.846810
2061.745643	33062.800249	47.851815
2058.041629	32628.202665	47.856820
2054.600066	32198.358463	47.861825
2051.216527	31761.960732	47.866829
2047.770848	31325.835334	47.871834
2043.951816	30891.792562	47.876839
2040.556972	30463.624743	47.881844
2036.860164	30025.848349	47.886849
2033.380909	29594.029713	47.891853
2029.275573	29162.057760	47.896858
2026.161049	28735.320761	47.901863
2023.014224	28306.893078	47.906868
2019.189478	27885.258738	47.911873
2015.561910	27439.137043	47.916877
2012.140439	27020.537404	47.921882
2008.752469	26588.863111	47.926887
2005.144267	26165.589661	47.931892
2001.783846	25740.246319	47.936897
1998.041119	25299.473906	47.941901
1994.550340	24864.779584	47.946906
1991.462171	24447.214156	47.951911
1987.779288	24011.681238	47.956916
1984.176854	23587.637573	47.961921
1980.424595	23153.166840	47.966925
1977.063219	22725.397925	47.971930
1973.400998	22290.741977	47.976935
1970.139549	21862.500998	47.981940
1966.556046	21445.512730	47.986945
1963.181123	21001.509478	47.991949
1959.664811	20581.412461	47.996954
1956.128254	20162.024343	48.001959
1952.521013	19735.771036	48.006964
1948.704053	19305.271569	48.011969
1945.794595	18874.469345	48.016973
1941.742278	18450.802556	48.021978
1938.270275	18028.327729	48.026983
1934.757180	17604.012812	48.031988
1931.009688	17181.459991	48.036993
1928.019472	16748.760555	48.041997
1924.498682	16332.407003	48.047002
1920.912344	15895.468754	48.052007
1917.158165	15481.627104	48.057012
1913.732549	15060.090353	48.062017
1909.985116	14622.193009	48.067021
1906.569784	14202.465662	48.072026
1902.783105	13783.058650	48.077031
1899.440443	13358.329899	48.082036
1895.628511	12943.304959	48.087041
1892.084547	12527.652236	48.092045
1888.981393	12116.501963	48.097050
1884.965306	11698.221581	48.102055
1881.401923	11284.074535	48.107060
1877.616748	10875.226014	48.112065
1874.322046	10460.403233	48.117069
1870.625198	10056.870577	48.122074
1867.019741	9638.078481	48.127079
1863.405403	9240.219850	48.132084
1859.834429	8838.586856	48.137089
1856.273615	8426.307019	48.142093
1852.840533	8036.631117	48.147098
1849.286594	7636.009068	48.152103
1845.863149	7235.979919	48.157108
1842.014732	6848.356039	48.162113
1838.253169	6447.162360	48.167117
1834.771137	6060.646924	48.172122
1831.273022	5663.502448	48.177127
1827.249800	5280.540407	48.182132
1823.428204	4892.906289	48.187137
1819.420701	4517.413547	48.192141
1814.912180	4171.749036	48.197146
1808.160071	3891.316417	48.202151
1803.140236	3600.372432	48.207156
1797.705755	3336.169436	48.212161
1793.391674	3076.384090	48.217165
1788.745426	2843.065762	48.222170
1784.853655	2617.647857	48.227175
1781.292893	2406.100243	48.232180
1777.361972	2215.492561	48.237185
1774.030413	2008.704395	48.242189
1770.324760	1814.265890	48.247194
1766.682861	1641.983316	48.252199
1763.323941	1452.130030	48.257204
1759.570191	1272.366689	48.262209
1756.150323	1091.531256	48.267213
1752.624077	923.777801	48.272218
1749.267566	752.111158	48.277223
1745.668804	593.116943	48.282228
1742.006179	437.168152	48.287233
1738.332610	267.703737	48.292237
1734.772604	125.187646	48.297242
1730.109290	1.921522	48.302247
1720.259267	39.315395	48.307252
1712.321639	59.792720	48.312257
1708.006741	55.279210	48.317261
1704.428410	53.574329	48.322266
1702.400534	55.089230	48.327271
1700.206707	55.354986	48.332276
1697.900881	61.294885	48.337281
1695.185327	52.704366	48.342285
1691.695180	49.666495	48.347290
1688.009149	58.548327	48.352295
1684.918165	51.556968	48.357300
1681.257180	64.737547	48.362305
1678.651111	60.717366	48.367309
1675.054112	58.347850	48.372314
1671.159936	64.743769	48.377319
1668.044716	62.527055	48.382324
1664.465079	60.882491	48.387329
1661.210657	58.722244	48.392333
1657.810308	59.144151	48.397338
1654.354550	65.231393	48.402343
1651.216795	55.298741	48.407348
1647.601949	68.760038	48.412353
1644.455317	54.257209	48.417357
1640.787441	62.256708	48.422362
1636.948290	60.782249	48.427367
1633.703890	58.481243	48.432372
1629.940122	70.222517	48.437377
1627.054653	61.035199	48.442381
1623.311104	62.026210	48.447386
1619.865392	58.241122	48.452391
1617.032380	53.123664	48.457396
1613.203691	58.440058	48.462401
1609.689306	51.141293	48.467405
1606.188408	64.625980	48.472410
1602.648351	57.802601	48.477415
1599.100276	56.304989	48.482420
1595.743194	58.801886	48.487425
1592.647656	57.116783	48.492429
1589.069879	57.332197	48.497434
1585.729644	62.395402	48.502439
1582.214583	67.321306	48.507444
1578.688095	60.144646	48.512449
1575.435528	54.747650	48.517453
1571.598018	55.395791	48.522458
1567.971245	59.054617	48.527463
1564.819009	51.639382	48.532468
1561.080763	64.578887	48.537473
1557.871335	48.352145	48.542477
1554.224266	61.467279	48.547482
1550.750166	64.754337	48.552487
1547.323379	50.165425	48.557492
1543.552051	61.480771	48.562497
1540.346722	60.103822	48.567501
1536.753061	62.688165	48.572506
1533.336713	63.175847	48.577511
1529.901745	55.991279	48.582516
1526.327612	61.002308	48.587521
1522.953790	62.492593	48.592525
1518.989190	56.890059	48.597530
1515.431669	67.574189	48.602535
1512.397730	59.330638	48.607540
1508.940760	66.531698	48.612545
1505.607239	60.701227	48.617549
1502.254169	61.175899	48.622554
1498.578861	63.864700	48.627559
1495.150818	58.681685	48.632564
1491.283739	68.148516	48.637569
1488.314155	59.148317	48.642573
1484.497275	62.393820	48.647578
1480.983751	65.022641	48.652583
1477.894605	51.327139	48.657588
1474.047270	56.564187	48.662593
1470.716234	60.721146	48.667597
1467.116658	63.227322	48.672602
1463.360173	65.903451	48.677607
1460.033183	53.649655	48.682612
1456.495114	57.282027	48.687617
1453.169086	51.545312	48.692621
1449.560214	59.829855	48.697626
1445.981347	62.323318	48.702631
1442.626317	60.397050	48.707636
1439.303670	65.647347	48.712641
1435.576878	58.830913	48.717645
1432.263743	53.933738	48.722650
1428.694067	55.078035	48.727655
1425.423157	60.282314	48.732660
1421.650475	65.254652	48.737665
1418.403483	56.158442	48.742669
1414.744333	47.635744	48.747674
1411.087860	55.953005	48.752679
1407.770051	52.527682	48.757684
1403.867767	53.410545	48.762689
1400.637200	51.388981	48.767693
1397.340945	54.075737	48.772698
1393.789888	58.972451	48.777703
1390.003287	50.089950	48.782708
1386.943039	62.617044	48.787713
1383.664154	49.596491	48.792717
1379.936197	58.769588	48.797722
1376.100054	59.056875	48.802727
1372.498186	51.224444	48.807732
1369.001629	65.632251	48.812737
1365.693223	49.923987	48.817741
1362.592982	60.090857	48.822746
1358.839704	54.471275	48.827751
1355.160596	54.639211	48.832756
1351.283049	62.513169	48.837761
1348.108500	49.998393	48.842765
1344.771005	60.259139	48.847770
1341.494959	61.484288	48.852775
1338.145301	54.757865	48.857780
1334.079251	54.454529	48.862785
1330.510424	50.327982	48.867789
1327.393667	52.183224	48.872794
1323.916820	58.517366	48.877799
1320.450866	57.886512	48.882804
1316.533005	58.581987	48.887809
1313.212971	56.118786	48.892813
1309.865009	49.936261	48.897818
1306.169022	55.747701	48.902823
1303.086310	56.838359	48.907828
1299.262061	60.376084	48.912833
1296.050564	57.611258	48.917837
1292.244786	48.681142	48.922842
1288.519199	58.100641	48.927847
1285.200081	61.183263	48.932852
1281.730032	66.570405	48.937857
1277.895691	65.563469	48.942861
1274.548741	69.732410	48.947866
1270.964632	69.237009	48.952871
1268.127316	61.823416	48.957876
1264.334940	56.943912	48.962881
1261.000600	56.219814	48.967885
1257.173805	55.151597	48.972890
1253.611215	59.774874	48.977895
1250.142362	57.334844	48.982900
1246.733963	68.995495	48.987905
1243.701591	60.656831	48.992909
1240.055727	56.763745	48.997914
1236.059471	67.690173	49.002919
1232.943518	58.222426	49.007924
1229.305080	60.604960	49.012929
1225.599825	53.658663	49.017933
1222.480546	52.888439	49.022938
1218.352516	62.180763	49.027943
1215.527065	55.385419	49.032948
1211.774498	50.183359	49.037953
1208.311135	54.155291	49.042957
1204.771766	62.422698	49.047962
1201.284871	58.795933	49.052967
1197.845251	49.777203	49.057972
1194.079094	58.997381	49.062977
1190.757895	50.235461	49.067981
1187.470772	49.500858	49.072986
1183.415036	56.064315	49.077991
1180.192400	53.655571	49.082996
1176.694196	56.617383	49.088001
1173.008742	46.523304	49.093005
1169.436329	48.610832	49.098010
1166.104980	52.296467	49.103015
1162.760401	48.840543	49.108020
1159.182847	52.488573	49.113025
1156.030250	52.501811	49.118029
1152.522772	49.330667	49.123034
1148.748729	51.765952	49.128039
1145.188559	41.870675	49.133044
1141.125845	49.352690	49.138049
1137.917287	53.376711	49.143053
1134.892602	43.651179	49.148058
1131.378431	53.717967	49.153063
1128.347722	48.023917	49.158068
1124.342904	55.740527	49.163073
1120.867353	48.983118	49.168077
1117.526973	33.406452	49.173082
1113.515536	56.942544	49.178087
1109.904035	47.229264	49.183092
1106.443096	48.891330	49.188097
1103.103523	44.264070	49.193101
1099.755283	48.439547	49.198106
1096.087309	47.602888	49.203111
1093.160168	44.474295	49.208116
1089.096762	48.036608	49.213121
1085.660640	48.714069	49.218125
1082.171922	49.722414	49.223130
1078.334137	51.746857	49.228135
1075.375043	43.045653	49.233140
1072.029506	47.034053	49.238145
1067.915288	50.243618	49.243149
1064.350219	49.909790	49.248154
1060.489239	53.200158	49.253159
1057.464437	41.228440	49.258164
1054.569352	45.058140	49.263169
1051.282075	50.685756	49.268173
1047.479385	56.232253	49.273178
1043.532736	51.813390	49.278183
1040.107677	48.727507	49.283188
1036.625621	58.251473	49.288193
1033.122011	47.078772	49.293197
1029.600841	47.392999	49.298202
1026.227962	49.677267	49.303207
1022.754137	45.798565	49.308212
1018.949201	54.730561	49.313217
1015.890236	41.913136	49.318221
1012.172128	40.682504	49.323226
1008.761815	43.263659	49.328231
1005.070678	50.102560	49.333236
1001.644714	49.674322	49.338241
998.235799	51.103679	49.343245
994.645664	53.222456	49.348250
990.877799	51.230795	49.353255
987.822729	44.414285	49.358260
983.994552	55.349351	49.363265
980.383232	45.066607	49.368269
977.262582	44.505427	49.373274
973.641579	55.123512	49.378279
970.324346	41.210536	49.383284
966.631590	45.325756	49.388289
962.751274	49.501811	49.393293
959.916749	44.969959	49.398298
956.153233	45.916691	49.403303
952.785386	47.020127	49.408308
948.900529	44.828389	49.413313
945.474228	57.308053	49.418317
942.184195	51.208316	49.423322
938.354091	50.428552	49.428327
935.546822	48.610066	49.433332
931.929100	56.291741	49.438337
928.078353	55.739813	49.443341
924.379220	51.681065	49.448346
920.739631	48.669721	49.453351
917.747073	44.099201	49.458356
913.937605	49.577161	49.463361
910.458054	50.590425	49.468365
906.941094	45.392870	49.473370
903.559051	47.586829	49.478375
900.327747	51.408767	49.483380
896.796839	47.263729	49.488385
893.094963	48.960158	49.493389
889.604845	44.625277	49.498394
885.827497	55.963714	49.503399
882.630130	45.986703	49.508404
879.072700	45.003154	49.513409
875.449692	44.536002	49.518413
871.986191	49.713344	49.523418
868.679560	48.102309	49.528423
865.234255	44.304611	49.533428
861.394765	50.502242	49.538433
858.139635	51.955129	49.543437
854.614263	49.416387	49.548442
850.823967	54.714203	49.553447
847.254041	44.013765	49.558452
843.700324	47.193049	49.563457
840.531130	44.757049	49.568461
837.126770	49.336742	49.573466
833.690924	54.437018	49.578471
830.078519	55.081838	49.583476
826.283245	53.556365	49.588481
822.909624	48.475712	49.593485
819.672877	44.591772	49.598490
815.970855	54.548610	49.603495
812.903226	45.715653	49.608500
809.125069	52.011306	49.613505
805.550221	44.851805	49.618509
801.670717	39.704379	49.623514
798.113145	47.433641	49.628519
795.149226	43.102284	49.633524
791.592635	52.549275	49.638529
787.897144	52.188328	49.643533
784.703689	47.380186	49.648538
780.842237	53.941903	49.653543
777.712409	51.509273	49.658548
773.856907	57.219034	49.663553
770.193005	57.732676	49.668557
766.819553	47.700843	49.673562
763.018706	56.227265	49.678567
760.404861	47.630554	49.683572
756.525983	49.420990	49.688577
753.009541	47.200404	49.693581
749.722510	42.163232	49.698586
746.060644	49.823314	49.703591
742.656579	53.086878	49.708596
739.112079	41.044271	49.713601
735.450514	52.798110	49.718605
731.762712	47.291829	49.723610
728.351986	49.692745	49.728615
724.823163	34.395442	49.733620
721.304342	48.813021	49.738625
717.824905	50.990523	49.743629
714.174974	48.436391	49.748634
710.939339	45.355868	49.753639
707.360015	49.307927	49.758644
703.777113	52.349403	49.763649
700.274595	48.684019	49.768653
697.148157	47.560636	49.773658
693.490641	54.881533	49.778663
690.126208	40.574184	49.783668
686.370997	53.396107	49.788673
682.735922	48.992078	49.793677
679.441348	52.694173	49.798682
676.165630	58.456053	49.803687
672.563350	53.499602	49.808692
668.565536	54.223422	49.813697
665.033624	44.602248	49.818701
661.642100	37.138999	49.823706
658.113827	57.126128	49.828711
655.018873	46.067060	49.833716
651.559932	42.290500	49.838721
647.982755	51.373716	49.843725
644.526386	40.538591	49.848730
640.158562	45.695380	49.853735
637.454776	48.157093	49.858740
633.968857	46.779639	49.863745
630.438505	50.765209	49.868749
626.995368	42.515916	49.873754
623.205360	46.665291	49.878759
619.951583	45.277010	49.883764
616.068999	47.349607	49.888769
612.719572	38.797836	49.893773
609.179017	42.380044	49.898778
605.607193	51.304244	49.903783
602.578981	42.838506	49.908788
598.707791	47.358017	49.913793
595.136999	48.122935	49.918797
591.705451	45.911303	49.923802
588.586735	48.643253	49.928807
585.204191	45.610929	49.933812
581.093514	53.147908	49.938817
577.684861	46.993936	49.943821
574.241280	44.879090	49.948826
570.708694	47.232557	49.953831
567.295379	51.617518	49.958836
563.855625	49.097127	49.963841
560.487226	50.491751	49.968845
557.016948	46.773916	49.973850
552.884538	48.081839	49.978855
549.716251	39.558827	49.983860
545.770395	52.388287	49.988865
542.386604	49.409945	49.993869
539.457283	47.993310	49.998874
535.764584	45.642012	50.003879
532.419912	47.482187	50.008884
528.666173	52.869251	50.013889
525.006121	49.810535	50.018893
521.722946	41.457269	50.023898
517.871591	43.442761	50.028903
514.546406	41.796699	50.033908
511.562762	46.016701	50.038913
507.972537	41.779724	50.043917
504.472498	42.963898	50.048922
500.856996	55.071234	50.053927
497.196055	36.282878	50.058932
493.596227	40.133746	50.063937
489.789182	47.617134	50.068941
487.006143	37.733891	50.073946
483.245348	39.543941	50.078951
480.174002	36.605553	50.083956
475.922111	30.646154	50.088961
472.088875	34.757980	50.093965
469.104308	38.206191	50.098970
465.543137	46.290366	50.103975
462.514064	36.442267	50.108980
458.947945	42.597371	50.113985
455.208606	46.903386	50.118989
451.574042	42.489829	50.123994
447.595839	50.648420	50.128999
444.749985	40.525032	50.134004
441.202425	38.616215	50.139009
437.550748	43.528664	50.144013
434.393555	41.002269	50.149018
430.694543	52.126050	50.154023
426.894900	46.757456	50.159028
423.615101	39.169294	50.164033
419.960799	35.331441	50.169037
416.740613	42.226775	50.174042
412.942654	53.827858	50.179047
409.526258	46.476090	50.184052
405.944144	42.155613	50.189057
403.082902	37.729238	50.194061
399.678124	36.756791	50.199066
395.473960	39.505886	50.204071
391.700184	40.141084	50.209076
388.169357	44.531701	50.214081
384.728958	35.231696	50.219085
381.290235	39.918012	50.224090
377.426365	42.617296	50.229095
374.787587	40.937157	50.234100
371.653756	46.189762	50.239105
367.725808	43.536603	50.244109
364.257075	38.660658	50.249114
360.420132	41.542409	50.254119
357.454086	34.519168	50.259124
353.504363	44.122291	50.264129
349.848748	43.321775	50.269133
346.762589	33.210513	50.274138
343.031614	44.779020	50.279143
339.456195	35.477899	50.284148
335.859852	43.191080	50.289153
332.387659	47.202425	50.294157
328.984486	34.669695	50.299162
325.990532	41.789234	50.304167
322.548376	42.882165	50.309172
318.504913	43.799798	50.314177
314.906341	41.231408	50.319181
311.200027	35.652164	50.324186
307.716424	41.826071	50.329191
304.591388	40.199498	50.334196
301.110101	39.387668	50.339201
297.169321	44.952565	50.344205
293.992781	37.791266	50.349210
290.665918	39.622368	50.354215
287.101452	31.812806	50.359220
283.685570	37.640823	50.364225
279.997889	38.126595	50.369229
276.540724	38.124076	50.374234
272.805927	39.306865	50.379239
269.289205	34.751613	50.384244
266.165118	32.862314	50.389249
262.500047	38.257741	50.394253
259.467289	35.920802	50.399258
255.348806	41.437440	50.404263
251.998354	37.530166	50.409268
248.427106	44.239729	50.414273
244.729698	39.244388	50.419277
241.450690	37.357065	50.424282
237.925415	48.004564	50.429287
234.367029	29.497714	50.434292
230.900213	38.339145	50.439297
226.608384	45.436135	50.444301
223.804914	43.753182	50.449306
220.344692	40.419807	50.454311
217.080847	41.918412	50.459316
213.590219	49.950495	50.464321
209.937573	43.401158	50.469325
206.617469	40.333864	50.474330
202.750009	42.578163	50.479335
199.056464	37.794195	50.484340
195.722286	42.593964	50.489345
191.840623	44.849966	50.494349
188.847287	47.761746	50.499354
185.778422	49.568511	50.504359
182.462690	42.438394	50.509364
178.778811	50.044999	50.514369
174.587723	46.069304	50.519373
171.348197	43.011615	50.524378
167.481976	44.366736	50.529383
164.061956	51.185638	50.534388
160.787893	39.281396	50.539393
157.279465	45.544602	50.544397
154.049065	43.937617	50.549402
150.381651	42.246817	50.554407
147.031531	44.663671	50.559412
143.483872	44.089982	50.564417
139.769429	48.056808	50.569421
136.427821	40.687127	50.574426
133.023462	42.194965	50.579431
129.294767	46.894818	50.584436
125.789664	46.333488	50.589441
122.215010	59.022922	50.594445
119.056369	44.243926	50.599450
114.980767	45.925875	50.604455
111.916584	40.015746	50.609460
108.349501	41.074373	50.614465
104.781398	53.114233	50.619469
101.348483	48.982546	50.624474
97.922220	51.227769	50.629479
94.244910	47.121479	50.634484
90.883316	48.809321	50.639489
87.095288	45.447913	50.644493
84.123739	38.688161	50.649498
80.299742	43.475621	50.654503
76.407598	41.990659	50.659508
73.218396	43.379588	50.664513
69.516417	46.980661	50.669517
66.373051	44.819152	50.674522
62.662179	38.310550	50.679527
58.877757	37.201115	50.684532
55.657655	36.914952	50.689537
52.784498	40.412292	50.694541
49.192335	40.044858	50.699546
45.280941	44.121451	50.704551
41.292177	39.994064	50.709556
37.955244	36.284033	50.714561
34.705282	43.971781	50.719565
30.811702	38.567277	50.724570
27.656168	42.209822	50.729575
24.451468	47.378580	50.734580
20.986509	37.724984	50.739585
17.150200	44.874459	50.744589
13.952899	40.316975	50.749594
9.942899	41.473049	50.754599
6.376786	45.141559	50.759604
3.442049	35.089049	50.764609