Fri Aug 26 10:49:52 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.625556	105.617071	0.000000
1.511375	98.709819	0.005005
1.335291	89.142074	0.010010
1.471473	78.794909	0.015014
0.748909	84.311187	0.020019
0.605058	71.043274	0.025024
0.654989	69.583618	0.030029
0.397348	54.792730	0.035034
0.071156	51.069511	0.040038
0.051557	54.900829	0.045043
-0.494111	44.811701	0.050048
-0.998242	33.241849	0.055053
-1.396524	36.929649	0.060058
-1.096805	26.943018	0.065062
-1.647718	22.625226	0.070067
-1.719747	25.464986	0.075072
-2.220811	19.361461	0.080077
-2.962970	17.933389	0.085082
-2.838261	4.974877	0.090086
-2.901160	17.895770	0.095091
-2.996098	5.360585	0.100096
-3.749196	0.694641	0.105101
-4.094711	0.631620	0.110106
-3.713644	2.714319	0.115110
-4.395473	10.321732	0.120115
-4.837030	0.089875	0.125120
-5.255118	-2.113127	0.130125
-5.399743	-0.081454	0.135130
-5.636150	-4.290024	0.140134
-5.602843	-7.933166	0.145139
-5.816519	-5.640814	0.150144
-5.989516	-6.983499	0.155149
-6.303507	-5.244985	0.160154
-6.874671	-5.959384	0.165158
-6.989363	0.189864	0.170163
-7.336204	-1.071973	0.175168
-6.993909	1.032580	0.180173
-7.699543	8.178642	0.185178
-8.140538	-5.954080	0.190182
-8.197757	-3.315940	0.195187
-8.355188	-5.512071	0.200192
-8.273240	-0.374171	0.205197
-9.391747	0.546838	0.210202
-9.394669	-2.780627	0.215206
-9.746080	-4.557427	0.220211
-9.578319	-2.286499	0.225216
-9.753105	-4.337564	0.230221
-10.112200	-5.559529	0.235226
-10.325791	-10.515107	0.240230
-10.979165	-6.740144	0.245235
-11.073992	-4.029713	0.250240
-11.088034	-11.740261	0.255245
-11.595186	-1.537386	0.260250
-11.626234	-9.802090	0.265254
-12.326956	5.802802	0.270259
-12.598719	-7.758337	0.275264
-12.219138	-2.951507	0.280269
-12.868662	-2.783702	0.285274
-12.431917	-3.667685	0.290278
-13.144038	-1.541326	0.295283
-13.792101	0.217567	0.300288
-13.988644	1.108919	0.305293
-14.446104	-9.262819	0.310298
-14.089971	-12.529132	0.315302
-14.002903	-8.189271	0.320307
-14.310023	-3.633015	0.325312
-14.658725	3.574526	0.330317
-15.229373	-2.201792	0.335322
-15.235068	-5.563624	0.340326
-15.958317	-2.631967	0.345331
-16.420960	-8.855355	0.350336
-16.801680	-12.747234	0.355341
-17.068316	-5.204472	0.360346
-16.670306	-17.091916	0.365350
-17.247346	-9.858319	0.370355
-17.000527	-4.480344	0.375360
-17.005563	-6.368019	0.380365
-17.562383	-0.282807	0.385370
-18.296866	-2.132837	0.390374
-18.568838	-5.168482	0.395379
-18.324844	-4.665249	0.400384
-18.854281	-5.031816	0.405389
-18.908096	3.256071	0.410394
-18.869932	-7.097927	0.415398
-19.468073	3.492428	0.420403
-20.125742	-1.257974	0.425408
-20.275753	-4.749192	0.430413
-19.982913	-1.463226	0.435418
-20.034396	-5.782842	0.440422
-20.747548	-0.682493	0.445427
-20.962014	-0.642535	0.450432
-21.539228	-0.334134	0.455437
-21.640041	3.193452	0.460442
-21.876863	-7.013330	0.465446
-21.853459	-2.663556	0.470451
-22.313417	-7.359320	0.475456
-22.628430	-7.385961	0.480461
-23.126733	0.635783	0.485466
-22.979871	1.957707	0.490470
-23.125650	-2.049846	0.495475
-23.103279	-8.731551	0.500480
-23.919325	-1.343683	0.505485
-24.374694	-6.403981	0.510490
-24.488987	-0.387670	0.515494
-25.052910	-2.381310	0.520499
-24.761263	0.053820	0.525504
-24.936969	-10.219421	0.530509
-24.880642	-10.101407	0.535514
-25.144216	-9.304018	0.540518
-26.002518	-5.196602	0.545523
-26.067914	-5.084944	0.550528
-26.121302	-5.376940	0.555533
-26.190263	-5.650692	0.560538
-27.052999	-14.345865	0.565542
-27.771435	-2.920565	0.570547
-27.579178	-9.312355	0.575552
-27.410986	-8.363900	0.580557
-27.988539	-0.684146	0.585562
-27.745228	-2.702234	0.590566
-27.651436	-2.159797	0.595571
-28.439087	-2.362778	0.600576
-28.729296	-14.408813	0.605581
-29.462035	2.020442	0.610586
-29.060490	-1.743308	0.615590
-29.589519	4.217360	0.620595
-29.505675	2.755593	0.625600
-30.021113	-8.372721	0.630605
-30.360565	1.857826	0.635610
-30.535649	-0.632939	0.640614
-30.914404	0.188710	0.645619
-31.031143	-6.714937	0.650624
-31.646313	-7.289610	0.655629
-31.851476	5.726186	0.660634
-31.869036	-6.751435	0.665638
-32.009134	-5.362687	0.670643
-31.988275	-6.014244	0.675648
-32.072459	-2.242484	0.680653
-32.658903	10.794717	0.685658
-33.449310	2.404639	0.690662
-33.530463	-0.742971	0.695667
-33.728751	8.187486	0.700672
-33.630654	-9.332016	0.705677
-33.649929	-2.492134	0.710682
-33.993659	-0.435787	0.715686
-34.739652	-2.755407	0.720691
-35.027892	5.537342	0.725696
-35.127889	5.300059	0.730701
-35.068301	-3.899380	0.735706
-35.345981	-8.781705	0.740710
-36.001602	-0.558303	0.745715
-36.140565	-11.308648	0.750720
-36.296613	-13.005136	0.755725
-36.893241	1.963467	0.760730
-36.576788	-2.742456	0.765734
-36.603753	3.162186	0.770739
-37.529261	2.676959	0.775744
-37.788648	2.002600	0.780749
-38.243444	8.527495	0.785754
-37.674612	-2.899351	0.790758
-38.231053	7.270074	0.795763
-38.823747	4.936075	0.800768
-39.268439	-1.872220	0.805773
-39.766374	5.282629	0.810778
-39.189235	-1.083671	0.815782
-39.677128	-5.211956	0.820787
-39.693455	-1.476071	0.825792
-39.711123	-2.355739	0.830797
-39.867922	-1.900830	0.835802
-40.431430	2.448580	0.840806
-40.794823	9.079463	0.845811
-41.365218	-1.771387	0.850816
-41.132684	-10.175200	0.855821
-41.670567	-3.615228	0.860826
-41.548195	-8.512387	0.865830
-42.476647	-7.355221	0.870835
-42.609749	3.026688	0.875840
-42.726293	-3.392952	0.880845
-42.836219	-8.880343	0.885850
-42.764916	-11.890343	0.890854
-43.050462	-1.446737	0.895859
-43.628609	-9.015672	0.900864
-43.585713	-5.659155	0.905869
-44.282207	-1.285875	0.910874
-44.218620	-9.473565	0.915878
-44.285395	1.350417	0.920883
-44.998976	-0.455411	0.925888
-45.756674	-6.756240	0.930893
-46.032057	0.541120	0.935898
-45.843753	-3.347610	0.940902
-45.876807	-1.576910	0.945907
-46.111308	5.745723	0.950912
-45.608700	2.001037	0.955917
-46.213524	8.947911	0.960922
-46.418086	-5.398783	0.965926
-46.807238	3.184915	0.970931
-47.404965	6.248886	0.975936
-47.492568	-1.804540	0.980941
-48.199385	-0.586973	0.985946
-48.447704	6.899158	0.990950
-48.734623	13.021441	0.995955
-48.756958	6.020837	1.000960
-48.659230	-2.403118	1.005965
-49.041451	4.347749	1.010970
-48.967962	5.763351	1.015974
-49.890873	-2.375145	1.020979
-50.226694	-12.645599	1.025984
-50.021594	-9.991358	1.030989
-50.577435	-7.607768	1.035994
-50.305314	-10.630053	1.040998
-50.402874	-7.568033	1.046003
-50.964155	-2.029439	1.051008
-51.182325	-9.755657	1.056013
-51.917391	-7.179652	1.061018
-51.802501	-2.920050	1.066022
-51.957145	0.758280	1.071027
-52.142208	-5.992364	1.076032
-52.751671	-11.193176	1.081037
-53.451221	0.858750	1.086042
-53.244754	-6.740603	1.091046
-53.388954	-5.917510	1.096051
-53.506391	-4.956219	1.101056
-53.323827	-4.677532	1.106061
-53.898980	-1.430422	1.111066
-54.192121	-7.104415	1.116070
-54.452561	-2.406737	1.121075
-54.696182	-10.954704	1.126080
-55.029699	-3.920369	1.131085
-55.842163	-5.147670	1.136090
-55.803154	-6.687874	1.141094
-56.069775	-7.225070	1.146099
-55.981933	2.828219	1.151104
-55.800355	-0.936083	1.156109
-56.230913	3.133209	1.161114
-56.888032	0.110076	1.166118
-57.471408	-1.424968	1.171123
-57.520978	-5.899900	1.176128
-56.924099	-9.134096	1.181133
-57.836396	-6.226785	1.186138
-58.415448	-11.040040	1.191142
-58.813835	2.967584	1.196147
-59.003098	-5.886231	1.201152
-58.780106	-11.346366	1.206157
-58.765236	-2.816087	1.211162
-58.854148	-12.318254	1.216166
-59.691525	-8.119187	1.221171
-60.577256	-1.865710	1.226176
-60.292848	-16.611217	1.231181
-60.280049	-9.950334	1.236186
-60.263902	-13.847057	1.241190
-60.333100	-14.696556	1.246195
-61.060746	-7.142127	1.251200
-61.458003	-5.688031	1.256205
-62.184858	-0.566568	1.261210
-61.724765	-7.367042	1.266214
-61.842474	-1.774130	1.271219
-62.275518	-5.585098	1.276224
-62.705303	-2.604223	1.281229
-63.352589	-0.563886	1.286234
-63.140172	-4.845498	1.291238
-63.449175	-2.380122	1.296243
-63.544948	-7.815934	1.301248
-63.720124	-12.208034	1.306253
-64.141496	0.139089	1.311258
-64.241662	-7.456811	1.316262
-64.679474	-3.652138	1.321267
-64.893098	-11.638482	1.326272
-64.599750	-10.149549	1.331277
-65.740411	-1.189426	1.336282
-66.078739	-11.111487	1.341286
-65.964965	-6.139893	1.346291
-66.202226	-15.786632	1.351296
-66.145853	-9.344498	1.356301
-66.019537	-1.122627	1.361306
-66.569539	-6.677535	1.366310
-67.211500	-4.957556	1.371315
-67.512437	-4.445405	1.376320
-67.544963	-2.649478	1.381325
-68.043427	1.202604	1.386330
-68.297586	-1.044902	1.391334
-68.696542	-0.027124	1.396339
-69.107740	9.809648	1.401344
-69.241550	3.399023	1.406349
-69.219938	1.662218	1.411354
-69.412342	-6.469795	1.416358
-69.135557	-3.418605	1.421363
-69.461060	3.949831	1.426368
-69.658821	-3.342983	1.431373
-70.432976	0.713369	1.436378
-70.657189	1.254702	1.441382
-70.528003	-4.428102	1.446387
-71.621224	2.227828	1.451392
-71.992124	4.886335	1.456397
-72.331454	-0.647594	1.461402
-71.765892	-9.166532	1.466406
-72.348722	2.462274	1.471411
-72.264228	3.528161	1.476416
-72.148751	-1.352106	1.481421
-72.504864	6.932228	1.486426
-73.154737	2.193270	1.491430
-73.654302	2.480092	1.496435
-73.762677	-2.210302	1.501440
-73.695249	-3.286711	1.506445
-74.114129	-2.319613	1.511450
-74.167906	-1.589690	1.516454
-74.859967	-1.355151	1.521459
-75.452505	3.735910	1.526464
-75.643795	6.695471	1.531469
-75.618863	7.334048	1.536474
-75.699907	1.212592	1.541478
-75.884946	2.187572	1.546483
-75.917589	6.580873	1.551488
-75.862984	-0.400070	1.556493
-76.569320	3.712160	1.561498
-76.931624	-4.364927	1.566502
-77.157065	1.222614	1.571507
-77.065882	2.856916	1.576512
-77.642272	0.564672	1.581517
-78.327254	-0.888115	1.586522
-78.059359	-5.194184	1.591526
-78.428510	0.643515	1.596531
-78.832426	2.396032	1.601536
-78.625274	2.171034	1.606541
-79.205100	8.905214	1.611546
-79.394491	-9.524941	1.616550
-79.632334	-6.814389	1.621555
-79.973117	6.681247	1.626560
-79.912616	5.074424	1.631565
-80.492186	0.574449	1.636570
-80.816177	3.023178	1.641574
-81.027940	5.517707	1.646579
-81.337181	10.662733	1.651584
-81.001125	-2.056599	1.656589
-81.426897	4.356210	1.661594
-82.236578	4.223097	1.666598
-82.626881	1.085659	1.671603
-82.953210	-5.516442	1.676608
-82.729263	3.370413	1.681613
-82.995590	-2.617793	1.686618
-82.999387	1.391378	1.691622
-82.980811	-3.075181	1.696627
-83.531790	12.525375	1.701632
-84.126445	7.309599	1.706637
-84.301473	7.166253	1.711642
-84.483512	5.375738	1.716646
-84.774879	2.899915	1.721651
-84.719688	2.682760	1.726656
-84.815569	-2.515763	1.731661
-85.830809	-3.357162	1.736666
-85.965076	-1.532739	1.741670
-85.763469	2.235649	1.746675
-85.959370	-0.156964	1.751680
-86.150956	-7.529828	1.756685
-86.961576	13.356481	1.761690
-87.528271	8.471699	1.766694
-87.718462	-0.185826	1.771699
-87.833166	4.365779	1.776704
-87.792016	-4.043036	1.781709
-87.480593	5.440783	1.786714
-87.552766	6.913864	1.791718
-87.960027	-0.058438	1.796723
-89.216728	-0.618641	1.801728
-88.716341	-1.645407	1.806733
-88.964410	9.092913	1.811738
-88.865494	-3.032693	1.816742
-89.772021	1.727618	1.821747
-90.332466	7.538157	1.826752
-90.585368	3.907941	1.831757
-90.649976	10.429028	1.836762
-90.466790	2.741552	1.841766
-90.576702	6.295863	1.846771
-91.088768	4.847789	1.851776
-91.251310	-13.817486	1.856781
-91.689126	7.286006	1.861786
-91.580819	1.486234	1.866790
-92.199497	-2.849468	1.871795
-93.128162	4.584408	1.876800
-93.052958	-6.262553	1.881805
-93.174373	-6.740102	1.886810
-93.431012	-9.540858	1.891814
-93.746989	-9.554694	1.896819
-93.606503	-2.454962	1.901824
-93.341609	-8.098784	1.906829
-93.996864	-6.440008	1.911834
-94.496441	-12.246364	1.916838
-94.686182	-6.123402	1.921843
-95.154598	-3.854660	1.926848
-94.951730	-8.207548	1.931853
-95.132124	4.117872	1.936858
-96.036031	-6.820240	1.941862
-96.235926	-2.919738	1.946867
-96.714362	-0.991109	1.951872
-96.388543	-3.591500	1.956877
-96.794574	-8.048891	1.961882
-96.807159	0.444533	1.966886
-96.736905	-5.871314	1.971891
-97.565220	0.275150	1.976896
-97.769946	-3.758020	1.981901
-98.277591	-5.425073	1.986906
-98.129682	-8.671619	1.991910
-98.149892	-0.164353	1.996915
-98.691199	-5.913641	2.006912
-98.512284	1.021577	2.016909
-98.613876	-1.540633	2.026906
-97.697575	-7.539897	2.036902
-96.898423	-2.066529	2.046899
-96.228801	-1.403730	2.056896
-95.697141	5.723647	2.066893
-95.460141	0.067727	2.076890
-95.087686	-5.745494	2.086886
-94.091801	-6.277033	2.096883
-94.303176	2.283796	2.106880
-93.696657	1.312385	2.116877
-92.857239	-0.005723	2.126874
-92.679574	-8.826435	2.136870
-92.131023	-8.173295	2.146867
-91.417859	-4.523802	2.156864
-91.046490	-3.634006	2.166861
-90.406642	-0.974090	2.176858
-89.890644	-5.685128	2.186854
-89.536087	-8.128299	2.196851
-88.949532	1.632389	2.206848
-88.652562	1.979422	2.216845
-87.907843	-6.311881	2.226842
-87.324786	2.505379	2.236838
-86.936201	-6.310163	2.246835
-86.552822	-11.374339	2.256832
-85.946269	2.247826	2.266829
-85.563119	-0.206134	2.276826
-84.948554	5.134425	2.286822
-84.662914	0.215340	2.296819
-83.681236	-5.965159	2.306816
-83.073076	-2.631925	2.316813
-83.193726	-1.690862	2.326810
-82.736848	-5.673628	2.336806
-81.779652	-9.290815	2.346803
-81.408485	-0.655968	2.356800
-81.127781	-5.577450	2.366797
-80.396362	-6.552469	2.376794
-80.161191	-7.009912	2.386790
-79.239413	-5.097121	2.396787
-78.727241	-4.460490	2.406784
-78.468133	-8.304761	2.416781
-78.342236	-2.964142	2.426778
-77.150003	-5.971715	2.436774
-76.966975	0.082244	2.446771
-76.599052	-9.705731	2.456768
-75.910917	-7.892773	2.466765
-75.650335	2.086559	2.476762
-74.737137	2.290130	2.486758
-74.239192	-2.766545	2.496755
-74.200170	2.039590	2.506752
-73.199274	-1.426017	2.516749
-73.158169	0.288120	2.526746
-72.674789	-1.205794	2.536742
-71.534565	0.153483	2.546739
-71.068573	2.282955	2.556736
-71.512783	-3.431621	2.566733
-70.254562	-3.582701	2.576730
-69.839908	-6.228460	2.586726
-69.473866	-4.919698	2.596723
-68.507236	-5.139414	2.606720
-68.480589	-10.613699	2.616717
-68.153570	1.262242	2.626714
-67.722189	-8.608471	2.636710
-66.999175	-11.371930	2.646707
-65.626813	-0.114897	2.656704
-66.023003	0.191179	2.666701
-65.478426	3.569161	2.676698
-64.921469	5.402545	2.686694
-64.293590	-0.497963	2.696691
-64.028991	-1.530174	2.706688
-63.540782	1.546149	2.716685
-62.719040	-0.269702	2.726682
-62.307680	-1.885446	2.736678
-62.216380	1.746837	2.746675
-61.271736	0.222284	2.756672
-61.133682	3.406977	2.766669
-60.107236	5.069064	2.776666
-59.575208	3.272979	2.786662
-59.511955	4.970997	2.796659
-59.010257	3.014914	2.806656
-58.226315	4.192088	2.816653
-57.846614	3.585434	2.826650
-57.851643	4.080855	2.836646
-57.256589	2.623404	2.846643
-56.067950	2.974152	2.856640
-55.396372	4.086461	2.866637
-55.178505	-0.606669	2.876634
-55.118276	6.283679	2.886630
-54.708256	8.025905	2.896627
-53.660405	3.266900	2.906624
-53.725618	8.497900	2.916621
-52.646566	8.406394	2.926618
-52.216559	3.930481	2.936614
-52.219709	-2.986806	2.946611
-51.144947	7.882595	2.956608
-50.721290	10.737729	2.966605
-50.646678	7.134417	2.976602
-49.879001	4.797977	2.986598
-49.115433	6.171554	2.996595
-48.994793	3.577907	3.006592
-47.982549	15.930028	3.016589
-47.967898	16.400212	3.026586
-47.634163	12.332081	3.036582
-46.850209	7.772548	3.046579
-46.598116	3.425703	3.056576
-45.670711	6.436812	3.066573
-45.005892	8.025330	3.076570
-44.857011	9.355234	3.086566
-44.796080	5.174363	3.096563
-43.762346	3.176623	3.106560
-43.434545	2.825130	3.116557
-42.572767	4.500185	3.126554
-41.839982	5.162655	3.136550
-41.680080	6.592210	3.146547
-41.625417	5.063680	3.156544
-41.389196	4.960856	3.166541
-40.736340	6.861670	3.176538
-39.519462	6.175352	3.186534
-38.828422	-0.140457	3.196531
-38.737327	6.285770	3.206528
-38.697090	7.170106	3.216525
-37.773289	5.211656	3.226522
-37.146654	5.627734	3.236518
-36.900569	9.882130	3.246515
-36.084611	11.041650	3.256512
-35.714631	9.112411	3.266509
-35.402671	7.581832	3.276506
-34.737038	-1.200827	3.286502
-34.064176	-1.007350	3.296499
-34.231960	2.139435	3.306496
-33.666508	5.859447	3.316493
-32.983978	4.996575	3.326490
-32.146297	6.377619	3.336486
-31.282611	2.832008	3.346483
-31.421078	1.938579	3.356480
-31.233804	-3.424508	3.366477
-30.435387	2.986621	3.376474
-29.893760	-0.866795	3.386470
-28.777851	-1.109753	3.396467
-28.464792	1.201917	3.406464
-28.175633	5.313395	3.416461
-28.437043	4.819232	3.426458
-27.465559	10.126399	3.436454
-26.578300	7.841030	3.446451
-26.456974	3.688768	3.456448
-25.588982	4.906708	3.466445
-25.493817	2.560940	3.476442
-24.816538	3.871928	3.486438
-24.086067	1.126313	3.496435
-24.032571	5.379018	3.506432
-23.292062	3.629665	3.516429
-22.561658	3.823687	3.526426
-22.527283	7.410984	3.536422
-21.705055	4.103070	3.546419
-21.092382	2.877286	3.556416
-20.879997	8.147426	3.566413
-20.604252	7.940250	3.576410
-19.583974	4.731375	3.586406
-19.342717	3.639445	3.596403
-18.362080	10.506864	3.606400
-18.310502	4.195585	3.616397
-18.005508	13.211369	3.626394
-17.256100	2.736782	3.636390
-16.379835	2.325236	3.646387
-16.450103	2.593237	3.656384
-15.931135	3.719806	3.666381
-15.007063	2.078085	3.676378
-14.550534	9.210833	3.686374
-14.602882	-1.639417	3.696371
-13.758906	1.926360	3.706368
-13.305196	0.085451	3.716365
-12.767617	4.421170	3.726362
-11.868626	6.537080	3.736358
-11.367680	1.166333	3.746355
-11.472858	-2.485011	3.756352
-11.260600	7.790115	3.766349
-10.566744	0.121259	3.776346
-9.661570	3.218192	3.786342
-9.265650	-2.981977	3.796339
-8.844538	-1.951042	3.806336
-8.304154	2.175172	3.816333
-7.535977	-8.571586	3.826330
-7.471566	4.387424	3.836326
-6.531237	-1.742291	3.846323
-6.274220	2.006738	3.856320
-5.956466	2.309356	3.866317
-5.518334	2.637580	3.876314
-4.980564	13.299171	3.886310
-4.363276	22.725654	3.896307
-4.020997	19.346750	3.906304
-3.554958	31.159893	3.916301
-2.995363	38.384309	3.926298
-2.194095	53.940187	3.936294
-1.899572	60.515322	3.946291
-1.810213	65.288298	3.956288
-1.448803	82.347660	3.966285
-0.680528	87.151148	3.976282
-0.318309	108.616702	3.986278
0.000000	112.868840	3.991283
0.641611	133.238135	3.996288
0.659908	128.913948	4.001293
1.080544	127.668646	4.006298
0.341481	138.711281	4.011302
0.781517	134.520741	4.016307
1.083588	147.315303	4.021312
1.184526	142.396129	4.026317
1.196709	136.127233	4.031322
0.935603	140.723816	4.036326
1.284134	129.093908	4.041331
0.978354	133.501297	4.046336
0.603443	136.821656	4.051341
1.134651	140.310975	4.056346
1.115962	152.630312	4.061350
1.602056	142.643072	4.066355
1.289885	148.022708	4.071360
1.363017	137.305684	4.076365
1.383627	129.428332	4.081370
0.901559	128.696891	4.086374
1.071869	131.682429	4.091379
1.259198	135.199979	4.096384
1.167746	141.453222	4.101389
1.380735	122.852702	4.106394
1.170446	143.693161	4.111398
0.832396	138.133675	4.116403
1.368380	141.521013	4.121408
1.565591	147.821061	4.126413
1.371934	139.689170	4.131418
1.090264	143.972588	4.136422
1.393800	148.686898	4.141427
1.423124	153.871001	4.146432
1.641215	152.549667	4.151437
1.507094	150.096793	4.156442
1.168964	150.494519	4.161446
1.270777	141.462431	4.166451
1.079052	145.573661	4.171456
1.441388	151.424068	4.176461
1.750826	153.995652	4.181466
1.220206	158.039431	4.186470
1.524339	153.613788	4.191475
1.813529	160.396217	4.196480
1.575375	148.073050	4.201485
1.419231	139.637933	4.206490
1.191412	140.572126	4.211494
1.725307	145.775740	4.216499
1.604368	158.398895	4.221504
1.472891	151.731592	4.226509
1.734576	137.514658	4.231514
1.511901	150.273868	4.236518
1.675755	137.185781	4.241523
1.095749	140.373562	4.246528
1.546369	157.533020	4.251533
2.064385	154.130744	4.256538
1.659847	161.090785	4.261542
1.677306	150.926575	4.266547
1.241992	147.296254	4.271552
1.193425	153.451077	4.276557
1.983635	156.191410	4.281562
1.741255	163.913960	4.286566
1.669761	153.871163	4.291571
1.878895	160.802094	4.296576
1.620534	154.325383	4.301581
2.002144	164.358339	4.306586
1.749630	159.712486	4.311590
1.656351	156.522442	4.316595
1.655979	163.340465	4.321600
1.593549	155.782907	4.326605
1.679362	159.426996	4.331610
1.675810	164.875642	4.336614
1.746907	162.308559	4.341619
1.675265	155.353534	4.346624
1.919066	157.792972	4.351629
1.936077	153.892912	4.356634
1.735034	171.055771	4.361638
1.662702	161.187103	4.366643
1.803802	166.337987	4.371648
1.810631	168.200569	4.376653
1.867831	162.294805	4.381658
1.746199	166.857024	4.386662
2.031660	166.496450	4.391667
1.640831	167.724937	4.396672
1.870434	171.292859	4.401677
1.727070	163.706770	4.406682
1.539828	174.739439	4.411686
1.774860	182.479413	4.416691
2.089222	183.579123	4.421696
2.112549	180.358265	4.426701
2.283492	183.584154	4.431706
2.319336	189.254458	4.436710
2.199297	180.968721	4.441715
2.626177	177.976090	4.446720
2.090927	178.391852	4.451725
2.080777	165.473203	4.456730
1.932855	171.725757	4.461734
2.063307	172.623152	4.466739
2.219293	180.210920	4.471744
2.348959	177.312021	4.476749
2.359748	172.542913	4.481754
2.157949	165.665095	4.486758
2.000497	159.416275	4.491763
2.528914	168.923351	4.496768
2.382315	159.218103	4.501773
2.198563	157.687258	4.506778
1.778257	173.207509	4.511782
2.197208	173.189973	4.516787
2.425318	178.457025	4.521792
2.682712	185.276050	4.526797
2.356889	175.013417	4.531802
1.860783	167.140571	4.536806
2.462789	167.746252	4.541811
2.499011	174.166285	4.546816
2.286172	169.827456	4.551821
2.409945	166.261940	4.556826
2.418437	170.168000	4.561830
2.305292	169.777741	4.566835
2.236739	164.160468	4.571840
2.420383	182.993976	4.576845
2.705357	182.750533	4.581850
2.230660	178.436655	4.586854
2.272614	175.323627	4.591859
2.454328	190.930489	4.596864
2.028922	186.589952	4.601869
2.181521	184.418292	4.606874
2.252230	179.836001	4.611878
2.275747	186.542748	4.616883
2.315343	191.152635	4.621888
2.004121	193.128014	4.626893
2.422481	188.709887	4.631898
2.295654	196.360677	4.636902
2.966388	206.165147	4.641907
2.740193	204.061952	4.646912
2.490144	196.631662	4.651917
2.419388	197.351583	4.656922
2.854779	209.331347	4.661926
2.908829	205.216706	4.666931
2.743000	198.757209	4.671936
2.565447	195.776428	4.676941
2.643077	191.525244	4.681946
2.623480	188.481907	4.686950
2.717044	189.935527	4.691955
2.522637	185.666589	4.696960
2.172243	199.638428	4.701965
2.917627	207.223023	4.706970
3.011104	219.373086	4.711974
3.159897	214.509716	4.716979
2.920136	199.598867	4.721984
2.761781	192.793367	4.726989
2.894690	180.187783	4.731994
2.620850	196.934904	4.736998
2.828195	190.698875	4.742003
3.106288	192.408497	4.747008
2.655841	200.571573	4.752013
2.701593	199.954097	4.757018
2.862285	215.523127	4.762022
2.833422	220.918784	4.767027
3.098803	224.863952	4.772032
2.875699	228.388478	4.777037
2.927778	217.478536	4.782042
3.084046	224.503142	4.787046
3.160776	208.094040	4.792051
3.143557	207.166836	4.797056
2.744969	199.430649	4.802061
3.096970	189.239639	4.807066
2.808858	195.023658	4.812070
2.798089	200.732860	4.817075
2.711316	200.635881	4.822080
2.878767	217.500971	4.827085
3.233853	211.662703	4.832090
3.084081	217.105657	4.837094
3.227073	211.819257	4.842099
3.578138	215.741591	4.847104
3.007162	214.815185	4.852109
3.315712	219.813466	4.857114
2.965547	215.502335	4.862118
3.127513	214.566214	4.867123
3.373342	221.114977	4.872128
3.234609	208.130896	4.877133
3.308879	191.488079	4.882138
2.890941	195.182135	4.887142
3.265617	207.063786	4.892147
2.976255	211.911554	4.897152
2.786217	213.073981	4.902157
3.377468	211.792618	4.907162
3.303760	217.986178	4.912166
3.382018	212.048646	4.917171
3.428987	213.936620	4.922176
3.112348	207.418345	4.927181
3.213068	216.463702	4.932186
3.224776	220.163633	4.937190
3.231356	216.942213	4.942195
3.407208	210.565551	4.947200
3.253113	215.635863	4.952205
3.056989	213.724134	4.957210
3.171488	214.320301	4.962214
3.396570	212.548631	4.967219
3.424418	222.402586	4.972224
3.300378	216.749644	4.977229
3.542397	216.316740	4.982234
3.096033	219.746313	4.987238
3.198975	216.402324	4.992243
3.220679	223.729450	4.997248
3.448882	224.089620	5.002253
3.474430	223.298122	5.007258
3.314799	232.570681	5.012262
3.701964	236.867042	5.017267
3.961214	234.182070	5.022272
3.606017	226.407479	5.027277
3.448918	222.025158	5.032282
3.210896	224.893958	5.037286
3.693762	229.317783	5.042291
3.895239	226.230528	5.047296
3.233058	224.343906	5.052301
3.582968	234.226816	5.057306
4.052763	237.523240	5.062310
3.542079	231.743835	5.067315
3.530058	224.282800	5.072320
3.419174	236.550113	5.077325
3.969982	233.275592	5.082330
3.544575	240.096547	5.087334
3.635010	240.724935	5.092339
3.752728	241.754027	5.097344
3.500850	255.156924	5.102349
3.909957	241.979956	5.107354
3.732888	250.913561	5.112358
3.654054	251.900492	5.117363
3.895060	250.059901	5.122368
3.655017	250.097514	5.127373
3.590189	251.414452	5.132378
3.439983	248.277547	5.137382
3.545051	244.332120	5.142387
3.820645	231.716939	5.147392
3.595274	245.786404	5.152397
3.726047	236.809869	5.157402
3.860492	236.808158	5.162406
3.490500	245.525029	5.167411
3.795048	243.927641	5.172416
3.568995	250.771344	5.177421
4.323801	257.342112	5.182426
3.913250	260.861028	5.187430
3.882988	248.872412	5.192435
3.879581	249.091476	5.197440
4.109332	265.466030	5.202445
3.999406	265.293562	5.207450
3.923181	261.920514	5.212454
4.152745	266.000979	5.217459
4.353189	253.169697	5.222464
3.968615	251.970662	5.227469
3.930539	243.586715	5.232474
3.751334	259.582019	5.237478
3.758859	260.697871	5.242483
4.012405	268.131285	5.247488
4.183754	272.910502	5.252493
4.431623	266.146127	5.257498
4.327685	269.243990	5.262502
4.390390	260.701976	5.267507
4.519208	259.286969	5.272512
4.014066	257.236690	5.277517
4.093338	235.743109	5.282522
3.910584	247.888744	5.287526
4.124130	253.085320	5.292531
4.519918	263.112960	5.297536
4.324604	267.740460	5.302541
4.397421	255.508004	5.307546
4.192861	250.712295	5.312550
3.971125	250.209229	5.317555
4.358671	247.089836	5.322560
4.128458	264.399693	5.327565
4.419470	263.680755	5.332570
4.476369	262.242144	5.337574
4.529126	267.153717	5.342579
4.279545	248.906656	5.347584
4.294805	260.103998	5.352589
4.490049	263.686778	5.357594
4.425170	258.233416	5.362598
4.410031	240.905297	5.367603
4.062963	249.723003	5.372608
4.252908	260.681180	5.377613
4.383798	258.342051	5.382618
4.222833	266.200663	5.387622
4.232598	261.118485	5.392627
4.560807	263.519487	5.397632
4.348793	263.540081	5.402637
4.304610	260.282265	5.407642
4.431221	268.219487	5.412646
4.554703	264.809018	5.417651
4.104439	273.459308	5.422656
4.304099	273.146891	5.427661
4.849634	261.957615	5.432666
4.581791	274.005787	5.437670
4.849759	266.339793	5.442675
4.809747	277.286329	5.447680
4.923321	268.568715	5.452685
4.860102	256.145471	5.457690
4.738323	267.440083	5.462694
4.887790	268.100409	5.467699
4.749483	263.923956	5.472704
4.724802	265.250463	5.477709
4.911407	259.270735	5.482714
4.701876	269.784924	5.487718
4.737812	269.906116	5.492723
5.055807	270.189032	5.497728
4.467559	261.928700	5.502733
4.807030	261.774846	5.507738
5.211629	267.710458	5.512742
4.575333	254.414678	5.517747
4.650537	249.433044	5.522752
4.664756	262.712261	5.527757
4.788648	260.197054	5.532762
5.001919	266.589554	5.537766
5.026255	263.501400	5.542771
4.692274	253.872730	5.547776
4.541997	259.894733	5.552781
4.690562	261.928243	5.557786
4.807303	265.773179	5.562790
4.999958	261.864730	5.567795
5.239336	258.129338	5.572800
4.930242	263.141541	5.577805
4.920382	271.112667	5.582810
4.849370	274.705268	5.587814
4.670389	278.229261	5.592819
4.439991	274.864396	5.597824
4.411376	276.330719	5.602829
4.697923	274.233103	5.607834
4.568330	264.224599	5.612838
4.604148	275.102380	5.617843
5.024610	286.888372	5.622848
4.928093	290.817136	5.627853
5.238201	289.696597	5.632858
5.409286	286.845014	5.637862
5.411024	283.431350	5.642867
5.363367	273.378446	5.647872
4.936588	277.570596	5.652877
4.888515	269.425469	5.657882
4.804676	275.051161	5.662886
4.993497	290.407073	5.667891
5.186627	289.200345	5.672896
5.115615	290.859929	5.677901
5.024974	288.403430	5.682906
5.212609	293.891949	5.687910
4.616996	299.717552	5.692915
4.936470	290.385748	5.697920
5.284843	288.961864	5.702925
5.511319	288.056823	5.707930
5.040159	287.820378	5.712934
5.298266	289.355953	5.717939
5.312529	285.155740	5.722944
4.725325	285.541629	5.727949
5.034283	280.064855	5.732954
5.328346	283.338030	5.737958
5.436985	280.625882	5.742963
5.407622	275.641540	5.747968
5.332394	285.733038	5.752973
5.329189	284.904886	5.757978
5.430119	284.297798	5.762982
5.240283	287.200234	5.767987
5.668176	294.647641	5.772992
5.571396	291.584667	5.777997
5.598013	293.811171	5.783002
5.384598	291.693321	5.788006
5.723793	286.939489	5.793011
5.311393	288.351673	5.798016
5.167473	293.683011	5.803021
5.326838	282.063474	5.808026
5.587021	292.330539	5.813030
5.471236	305.807196	5.818035
5.679116	305.806706	5.823040
5.302041	310.218911	5.828045
5.717603	313.770563	5.833050
5.966916	312.067876	5.838054
5.330843	306.909072	5.843059
5.560373	301.827467	5.848064
5.315007	309.287958	5.853069
5.472185	312.133204	5.858074
5.628385	317.794302	5.863078
5.466076	321.682697	5.868083
5.856087	315.573206	5.873088
5.455069	328.360311	5.878093
5.984162	318.068889	5.883098
5.700018	317.411026	5.888102
5.620055	323.874512	5.893107
5.389412	314.128482	5.898112
5.003376	313.701615	5.903117
5.466894	315.173573	5.908122
5.506399	313.095434	5.913126
5.928091	318.987275	5.918131
6.001272	311.826145	5.923136
5.949871	313.985706	5.928141
5.772367	314.339444	5.933146
6.155232	308.993521	5.938150
5.967500	313.053549	5.943155
6.145499	306.467714	5.948160
5.750032	317.814461	5.953165
5.695737	314.169074	5.958170
6.063741	313.422328	5.963174
5.812165	320.848989	5.968179
6.191577	312.102619	5.973184
5.702159	312.735871	5.978189
5.677798	313.638395	5.983194
6.056751	312.896272	5.988198
5.895889	313.459386	5.993203
5.888587	315.457060	5.998208
5.863847	313.895116	6.003213
6.057515	319.129608	6.008218
5.985902	317.910315	6.013222
5.629942	318.095688	6.018227
5.572028	309.233914	6.023232
5.583162	319.020924	6.028237
6.250301	324.441123	6.033242
6.136501	331.371781	6.038246
5.932722	328.660813	6.043251
6.021496	320.374136	6.048256
5.822577	318.465994	6.053261
5.935196	318.100690	6.058266
6.210767	321.212239	6.063270
5.964279	325.547169	6.068275
6.050511	313.970635	6.073280
5.718689	316.983766	6.078285
5.857648	312.036480	6.083290
5.878662	316.019716	6.088294
5.948215	319.549313	6.093299
6.025879	309.862848	6.098304
5.945251	312.931779	6.103309
5.928932	303.547849	6.108314
5.932569	322.529752	6.113318
5.746378	323.723224	6.118323
6.078771	330.214258	6.123328
5.981387	330.077801	6.128333
6.174578	327.890311	6.133338
5.991579	323.344322	6.138342
5.826142	315.666694	6.143347
5.793556	316.485079	6.148352
5.613768	328.275972	6.153357
6.319113	331.149767	6.158362
6.387293	335.707786	6.163366
5.997645	330.048707	6.168371
6.174401	313.709354	6.173376
5.808914	320.065436	6.178381
5.655880	318.716453	6.183386
5.788747	320.369605	6.188390
5.598856	333.902114	6.193395
6.006468	331.668585	6.198400
6.245791	337.921015	6.203405
6.263959	328.487409	6.208410
5.989267	321.807539	6.213414
5.921548	315.592148	6.218419
5.658769	317.082278	6.223424
5.859993	323.951230	6.228429
6.135660	327.515175	6.233434
5.979396	317.596213	6.238438
5.931904	325.035393	6.243443
5.937987	318.514286	6.248448
6.035426	316.730842	6.253453
5.929997	310.353647	6.258458
5.969209	312.726887	6.263462
6.150749	318.596008	6.268467
5.978020	308.325280	6.273472
5.633742	310.913249	6.278477
5.916873	318.873580	6.283482
5.904489	321.802175	6.288486
5.899549	330.240791	6.293491
6.373403	334.878014	6.298496
6.022313	324.033942	6.303501
6.045216	315.865089	6.308506
6.198831	317.464392	6.313510
5.794684	319.118899	6.318515
5.739899	313.230520	6.323520
5.721728	318.501158	6.328525
6.077726	322.226598	6.333530
6.051844	313.287070	6.338534
5.838589	315.142807	6.343539
6.153087	312.974396	6.348544
6.096703	310.284774	6.353549
6.167065	302.535638	6.358554
6.072565	303.287733	6.363558
5.779059	307.826129	6.368563
5.955134	307.878046	6.373568
6.198949	309.441158	6.378573
6.009050	301.947676	6.383578
5.982697	310.911627	6.388582
5.741801	315.229866	6.393587
5.798386	313.990613	6.398592
5.875825	316.348410	6.403597
6.271664	326.281167	6.408602
6.192576	313.600930	6.413606
5.974651	308.693392	6.418611
6.294663	307.093591	6.423616
6.037173	320.978295	6.428621
6.044973	322.404151	6.433626
5.906960	324.722729	6.438630
5.683587	319.547122	6.443635
5.959298	323.022475	6.448640
5.931010	318.465053	6.453645
5.942131	318.185154	6.458650
5.851986	312.590179	6.463654
5.966489	325.635532	6.468659
5.797389	326.358115	6.473664
5.652415	314.257603	6.478669
6.141816	312.919325	6.483674
5.852400	317.653237	6.488678
5.750956	318.767076	6.493683
5.973734	319.245150	6.498688
5.738775	319.633142	6.503693
5.902114	316.384133	6.508698
5.963558	326.039929	6.513702
5.651991	324.402422	6.518707
6.037788	329.724060	6.523712
6.363502	336.475560	6.528717
6.389130	325.648762	6.533722
5.990876	318.735034	6.538726
5.939093	335.188288	6.543731
5.967749	321.096074	6.548736
5.634671	325.333757	6.553741
5.815254	315.080780	6.558746
5.882220	309.182938	6.563750
5.971245	320.792769	6.568755
5.847526	315.997110	6.573760
5.951684	326.326452	6.578765
5.860264	332.943584	6.583770
6.152712	341.595326	6.588774
6.032726	325.466677	6.593779
5.964276	322.861188	6.598784
5.771771	312.849796	6.603789
5.837970	322.871840	6.608794
6.073812	333.294576	6.613798
6.088810	331.058902	6.618803
6.190963	322.425297	6.623808
5.738735	324.691559	6.628813
6.044527	313.954023	6.633818
6.239424	311.791580	6.638822
6.312878	316.965695	6.643827
6.158286	315.082289	6.648832
5.776465	320.181760	6.653837
5.941402	316.100447	6.658842
6.216165	313.742074	6.663846
6.064858	312.588973	6.668851
6.238835	305.886707	6.673856
5.823373	315.354163	6.678861
6.250279	312.108410	6.683866
6.064091	326.823562	6.688870
5.553705	322.799938	6.693875
6.005576	318.579039	6.698880
6.223539	313.657416	6.703885
5.795786	322.800928	6.708890
5.890731	322.140988	6.713894
5.921991	312.287743	6.718899
6.015295	314.481721	6.723904
6.015906	321.479982	6.728909
5.828235	309.958752	6.733914
5.971284	307.997368	6.738918
5.803233	310.700265	6.743923
6.063339	311.675556	6.748928
5.912689	316.938346	6.753933
5.815639	315.276932	6.758938
6.006778	312.254546	6.763942
5.849474	319.875333	6.768947
6.139641	315.265166	6.773952
5.576947	326.536718	6.778957
5.955830	322.067758	6.783962
5.765491	311.802933	6.788966
5.974134	322.299500	6.793971
6.167933	309.450230	6.798976
5.948798	316.194805	6.803981
5.741502	328.034273	6.808986
5.898440	319.123224	6.813990
6.064523	320.476980	6.818995
6.053882	320.779428	6.824000
6.022108	325.340352	6.829005
5.949326	323.023434	6.834010
6.097020	315.208469	6.839014
5.971377	324.352399	6.844019
6.138206	317.129231	6.849024
5.797647	317.432427	6.854029
5.901740	312.003359	6.859034
5.866446	313.515016	6.864038
5.607703	325.612425	6.869043
5.955484	312.704377	6.874048
5.887433	321.753919	6.879053
5.848549	324.433544	6.884058
5.865034	322.659541	6.889062
5.722037	323.137617	6.894067
6.059796	324.907563	6.899072
6.036835	333.744450	6.904077
5.923541	320.765817	6.909082
6.005009	322.797126	6.914086
5.955987	323.849021	6.919091
5.925028	312.180005	6.924096
6.092236	318.586023	6.929101
5.779104	315.354253	6.934106
6.016370	326.150081	6.939110
6.357861	329.687959	6.944115
6.235485	315.764795	6.949120
6.240511	319.301275	6.954125
6.299082	317.527047	6.959130
6.170564	320.394631	6.964134
5.825131	325.937684	6.969139
6.214708	327.136422	6.974144
6.105914	326.846720	6.979149
5.991164	318.927085	6.984154
6.031171	318.421229	6.989158
5.806510	322.907782	6.994163
6.209282	312.316497	6.999168
6.061775	319.024612	7.004173
6.029599	326.322205	7.009178
6.068360	320.577444	7.014182
5.952892	317.102930	7.019187
5.978206	318.497585	7.024192
5.885278	321.473522	7.029197
5.927325	317.961828	7.034202
6.160884	310.620706	7.039206
5.621438	317.051328	7.044211
6.129939	316.162486	7.049216
5.832110	319.901141	7.054221
6.113490	320.841482	7.059226
6.124475	316.540534	7.064230
6.034613	329.703130	7.069235
5.983356	314.826109	7.074240
5.553131	311.308855	7.079245
5.829321	311.892506	7.084250
5.871453	314.866395	7.089254
5.745584	325.320134	7.094259
5.706193	314.411720	7.099264
6.071320	322.425723	7.104269
5.845802	314.023471	7.109274
6.129476	311.878842	7.114278
5.852981	319.113233	7.119283
5.951285	316.244504	7.124288
5.834898	321.261519	7.129293
6.098531	325.273420	7.134298
6.067730	316.938924	7.139302
6.173992	330.362045	7.144307
5.981811	317.769015	7.149312
5.949224	313.006623	7.154317
5.986046	308.777583	7.159322
5.867256	311.301971	7.164326
5.606004	314.462299	7.169331
5.959573	307.156277	7.174336
5.878350	320.434578	7.179341
5.667384	311.701036	7.184346
5.821646	313.078778	7.189350
5.625483	323.695319	7.194355
5.895221	305.190176	7.199360
5.953916	318.196758	7.204365
6.126999	315.857379	7.209370
5.950829	319.985210	7.214374
5.521297	325.386336	7.219379
6.029886	316.806509	7.224384
5.876781	328.912782	7.229389
5.888667	322.808379	7.234394
5.999599	313.578634	7.239398
5.831741	323.842761	7.244403
6.242642	322.760310	7.249408
6.016817	314.541600	7.254413
6.002176	315.328717	7.259418
6.153011	320.984324	7.264422
5.921837	328.616617	7.269427
6.105467	309.479480	7.274432
6.225487	324.159609	7.279437
6.042074	323.017833	7.284442
6.019339	320.022418	7.289446
6.002396	317.896120	7.294451
6.163706	313.767917	7.299456
6.126696	315.703779	7.304461
6.002271	315.755027	7.309466
6.088531	313.141270	7.314470
5.571505	320.466894	7.319475
5.970710	312.714010	7.324480
6.111614	322.987009	7.329485
5.970848	319.003912	7.334490
6.178643	312.729807	7.339494
6.024161	318.787285	7.344499
6.435985	312.209334	7.349504
6.332395	317.613492	7.354509
5.993989	318.764226	7.359514
6.266934	305.655866	7.364518
5.607084	305.537382	7.369523
5.779788	301.594067	7.374528
6.065135	313.926289	7.379533
6.364049	311.576810	7.384538
5.876086	302.215694	7.389542
5.711017	305.614142	7.394547
6.024854	297.251306	7.399552
5.736715	301.364929	7.404557
6.007664	314.363770	7.409562
6.267643	311.726129	7.414566
5.796106	295.924321	7.419571
6.043456	302.871503	7.424576
5.918621	300.521565	7.429581
5.302884	303.436532	7.434586
5.873691	304.831675	7.439590
5.808527	323.568031	7.444595
6.181982	322.440791	7.449600
6.284762	320.710298	7.454605
5.732467	318.268726	7.459610
6.069935	315.467162	7.464614
5.946772	317.932122	7.469619
5.914347	318.642915	7.474624
6.067804	314.974672	7.479629
6.162321	325.906619	7.484634
6.395643	318.179560	7.489638
5.671173	315.033979	7.494643
5.960630	303.254971	7.499648
6.215245	306.407744	7.504653
5.744178	301.906611	7.509658
5.901245	303.900838	7.514662
6.117736	317.167584	7.519667
6.107662	304.524064	7.524672
5.625222	306.880448	7.529677
5.964030	308.697684	7.534682
6.106208	313.415016	7.539686
5.684770	309.500931	7.544691
5.979671	319.256413	7.549696
6.236370	314.376215	7.554701
5.785534	311.067811	7.559706
6.074160	317.268266	7.564710
5.757639	316.735664	7.569715
6.439949	303.193416	7.574720
6.141407	301.699413	7.579725
5.826660	305.348952	7.584730
5.768589	294.010031	7.589734
5.625750	295.889602	7.594739
6.360802	306.339000	7.599744
6.047668	300.104878	7.604749
5.699170	301.257182	7.609754
6.032369	294.966721	7.614758
5.745378	302.367252	7.619763
6.347904	305.817027	7.624768
6.222625	304.571290	7.629773
5.742450	296.597830	7.634778
6.232954	299.710711	7.639782
6.108741	298.050364	7.644787
5.914613	291.285196	7.649792
6.108097	295.595909	7.654797
6.175147	295.114316	7.659802
6.216688	293.257322	7.664806
6.242796	306.806799	7.669811
6.352457	291.316294	7.674816
6.091100	297.475825	7.679821
5.816086	286.075775	7.684826
5.912320	294.432183	7.689830
5.934064	298.029329	7.694835
5.914362	295.409927	7.699840
5.879883	300.442657	7.704845
5.936192	301.044723	7.709850
6.143126	296.491812	7.714854
5.902014	299.095354	7.719859
5.824219	295.640288	7.724864
5.908268	297.661701	7.729869
5.830020	295.111524	7.734874
6.178201	290.637861	7.739878
6.094819	299.430355	7.744883
6.025894	291.117625	7.749888
5.959846	300.669873	7.754893
5.922852	305.794743	7.759898
5.974661	294.353294	7.764902
5.852285	300.184307	7.769907
5.794874	298.905858	7.774912
5.974071	303.019484	7.779917
5.658310	298.174637	7.784922
5.948274	291.824472	7.789926
5.682915	299.762626	7.794931
6.115193	293.931295	7.799936
5.695269	297.938888	7.804941
5.878822	297.205042	7.809946
6.016378	286.474735	7.814950
5.776839	302.893917	7.819955
5.649017	296.428467	7.824960
5.846240	299.058673	7.829965
6.023450	295.336116	7.834970
5.698185	296.402546	7.839974
5.885691	293.776192	7.844979
6.229684	288.872918	7.849984
5.930092	292.703589	7.854989
5.720913	302.512236	7.859994
6.151789	301.202054	7.864998
5.859178	305.025313	7.870003
5.708763	296.076710	7.875008
6.213579	306.637883	7.880013
5.788961	307.580580	7.885018
5.855289	308.111485	7.890022
6.021042	311.629266	7.895027
6.197161	311.807724	7.900032
5.871439	304.768816	7.905037
5.688728	299.646993	7.910042
5.977668	311.662284	7.915046
5.874179	316.221716	7.920051
6.297397	314.124962	7.925056
6.128989	307.880959	7.930061
5.842023	307.929041	7.935066
6.047698	296.662947	7.940070
5.877505	298.284191	7.945075
5.764833	296.302512	7.950080
5.998632	304.153460	7.955085
6.141666	309.307249	7.960090
6.034944	296.498451	7.965094
5.749490	302.971778	7.970099
5.641563	295.794561	7.975104
5.787098	324.074641	7.980109
6.170001	319.295013	7.985114
6.686863	315.212690	7.990118
6.037941	312.008578	7.995136
5.967601	304.774435	8.000154
6.041164	293.724820	8.005171
6.116493	303.344320	8.010189
6.374333	290.401037	8.015206
5.816954	304.394927	8.020224
6.042027	299.374224	8.025242
6.000640	302.126307	8.030259
6.143597	305.420859	8.035277
5.952185	294.889000	8.040294
6.203933	309.337552	8.045312
5.815040	304.188390	8.050330
5.780601	294.544069	8.055347
5.865160	304.764857	8.060365
6.314861	297.891536	8.065382
5.990299	304.793187	8.070400
6.024575	302.067934	8.075418
6.035952	299.737546	8.080435
5.995120	299.665252	8.085453
6.074678	299.542657	8.090470
5.752872	299.432063	8.095488
5.999957	295.364091	8.100506
6.022288	300.681249	8.105523
5.880496	310.202020	8.110541
5.971098	295.486061	8.115558
5.916087	304.068718	8.120576
6.141448	313.892069	8.125594
6.356460	319.570531	8.130611
6.041994	315.918172	8.135629
5.978965	303.911571	8.140646
6.044343	308.161736	8.145664
6.443026	321.725932	8.150682
6.054449	306.737451	8.155699
6.203242	312.495644	8.160717
6.196171	312.149865	8.165734
5.810924	301.853298	8.170752
6.026432	322.173824	8.175770
6.471423	313.584564	8.180787
6.209627	317.245078	8.185805
6.258189	301.368074	8.190822
5.986697	308.359288	8.195840
5.814810	312.321365	8.200858
5.956335	308.840995	8.205875
6.177358	329.053378	8.210893
6.242770	326.168648	8.215910
6.310567	323.652756	8.220928
6.422578	328.441591	8.225946
6.740340	322.232553	8.230963
5.844640	319.166124	8.235981
6.080639	323.134121	8.240998
6.446644	327.523667	8.246016
6.287527	311.297157	8.251034
6.164896	313.339252	8.256051
5.829263	321.820450	8.261069
6.186535	317.760561	8.266086
6.494575	329.495986	8.271104
5.995536	330.466969	8.276122
6.021516	331.056424	8.281139
6.488572	335.307168	8.286157
6.738878	327.155291	8.291174
6.235711	331.456115	8.296192
6.093719	326.814430	8.301210
6.336575	323.065829	8.306227
6.355636	326.354430	8.311245
6.567535	326.908625	8.316262
6.581880	315.644167	8.321280
6.101919	310.799501	8.326298
6.713605	298.861412	8.331315
5.954755	313.580917	8.336333
6.379985	301.037575	8.341350
6.452094	304.459915	8.346368
6.334381	300.947330	8.351386
6.416684	304.330215	8.356403
6.057686	308.141553	8.361421
6.250718	301.024187	8.366438
6.218444	302.039253	8.371456
5.861214	318.163600	8.376474
6.483706	317.378991	8.381491
6.594460	334.964128	8.386509
6.314427	329.908457	8.391526
6.714402	336.820382	8.396544
6.345926	325.748058	8.401562
6.095746	313.672764	8.406579
6.455532	327.072617	8.411597
6.154943	320.723182	8.416614
6.348936	326.461721	8.421632
6.255567	329.518532	8.426650
6.511543	331.441723	8.431667
6.544269	329.676021	8.436685
6.553221	322.129739	8.441702
6.506332	334.384307	8.446720
6.359553	331.819776	8.451738
6.737652	321.874537	8.456755
6.151709	336.238953	8.461773
6.268336	327.514629	8.466790
6.253323	327.633965	8.471808
6.166962	328.881505	8.476826
6.382867	328.062375	8.481843
6.123345	327.175264	8.486861
6.165392	330.324593	8.491878
6.411521	333.524196	8.496896
6.214869	339.468720	8.501914
6.689231	334.677423	8.506931
6.561345	327.736237	8.511949
6.642972	334.612524	8.516966
6.167803	330.464503	8.521984
6.333175	334.976802	8.527002
6.638590	330.328569	8.532019
6.424404	325.937953	8.537037
6.594021	331.169075	8.542054
6.674521	330.017596	8.547072
6.605083	327.617740	8.552090
6.677595	327.237480	8.557107
6.905485	336.931069	8.562125
6.863742	326.899724	8.567143
6.824621	327.903235	8.572160
6.414757	337.282732	8.577178
6.808209	329.398886	8.582195
6.568073	337.713753	8.587213
6.835848	328.031826	8.592231
6.614923	329.407609	8.597248
6.811479	330.020995	8.602266
6.757031	327.195950	8.607283
6.597915	335.813765	8.612301
6.681541	328.625063	8.617319
6.724809	325.478707	8.622336
6.691114	334.477760	8.627354
6.870930	340.300556	8.632371
6.819120	333.912383	8.637389
6.547705	327.255462	8.642407
6.699118	320.062521	8.647424
6.453441	332.392217	8.652442
6.601844	332.719627	8.657459
6.370412	331.335862	8.662477
6.466524	328.944942	8.667495
6.668857	327.427374	8.672512
6.557173	329.205848	8.677530
6.779292	330.307533	8.682547
6.732111	333.082613	8.687565
6.480053	332.257453	8.692583
6.530165	336.841343	8.697600
6.567966	336.277149	8.702618
6.590976	336.381098	8.707635
6.631045	333.421421	8.712653
6.924838	333.814551	8.717671
6.641686	328.999195	8.722688
6.439028	334.319836	8.727706
6.634453	327.129507	8.732723
6.504374	321.577146	8.737741
6.455359	329.303704	8.742759
6.668683	342.641169	8.747776
6.926885	352.320580	8.752794
6.938410	346.695673	8.757811
6.793148	351.805423	8.762829
6.777873	354.591316	8.767847
6.700386	354.366947	8.772864
7.066660	360.362680	8.777882
7.034683	351.147113	8.782899
6.884909	344.720542	8.787917
6.221538	333.394342	8.792935
6.696205	341.269731	8.797952
6.517980	345.485254	8.802970
6.885473	348.612317	8.807987
6.846320	353.749725	8.813005
6.857306	354.341514	8.818023
7.018438	354.483915	8.823040
7.054140	358.760802	8.828058
6.931197	356.498654	8.833075
6.909124	354.675213	8.838093
7.038932	356.640141	8.843111
7.332739	346.297778	8.848128
6.844719	343.647528	8.853146
6.349601	332.493937	8.858163
6.756011	339.815094	8.863181
6.934865	350.131674	8.868199
6.916534	346.392178	8.873216
7.140900	366.130737	8.878234
7.016014	360.258835	8.883251
7.140749	357.806653	8.888269
6.999514	360.003120	8.893287
7.122455	346.146730	8.898304
7.009613	343.813587	8.903322
6.494301	339.207934	8.908339
6.696715	344.168880	8.913357
6.663391	349.425294	8.918375
6.903531	352.180886	8.923392
7.124399	356.428943	8.928410
7.267929	354.081127	8.933427
7.141265	352.621092	8.938445
7.185901	349.095842	8.943463
7.294785	339.795236	8.948480
7.059456	353.486571	8.953498
7.132749	336.766285	8.958515
6.803804	338.079995	8.963533
7.330719	342.125772	8.968551
7.322344	333.465086	8.973568
6.744733	338.231915	8.978586
6.534090	326.538600	8.983603
7.109636	343.833640	8.988621
6.806529	349.157303	8.993639
6.960443	345.529837	8.998656
6.860661	356.057053	9.003674
7.347588	354.409970	9.008691
7.015268	352.407628	9.013709
7.203689	357.298176	9.018727
7.351501	351.740406	9.023744
7.355538	352.525772	9.028762
7.414297	353.734940	9.033779
7.359458	343.768737	9.038797
6.834630	332.919558	9.043815
7.344352	325.945367	9.048832
6.913063	330.840882	9.053850
6.914636	336.767165	9.058867
7.114009	351.236528	9.063885
7.109886	346.709065	9.068903
7.166795	343.481691	9.073920
7.213297	351.644643	9.078938
7.181945	352.744772	9.083955
7.167616	356.634993	9.088973
6.974070	358.293678	9.093991
7.049381	358.099165	9.099008
7.193911	357.606711	9.104026
7.193033	361.580041	9.109043
7.238987	353.920693	9.114061
7.141278	358.158394	9.119079
7.398391	361.665544	9.124096
7.017464	351.718552	9.129114
6.749889	365.222422	9.134131
7.248204	358.575027	9.139149
7.161581	356.061084	9.144167
7.731788	342.488490	9.149184
7.524695	354.749082	9.154202
7.313630	355.463802	9.159219
7.455412	359.825153	9.164237
6.903244	356.967149	9.169255
7.135224	351.626636	9.174272
7.056864	352.506878	9.179290
6.933251	355.224437	9.184307
7.064793	352.865865	9.189325
6.955877	361.744106	9.194343
7.184921	354.993477	9.199360
7.200685	356.954071	9.204378
7.265493	358.916497	9.209395
7.509693	370.687133	9.214413
7.485474	369.084920	9.219431
7.739522	350.237975	9.224448
7.184734	351.974993	9.229466
7.310538	361.305813	9.234483
7.788455	355.406326	9.239501
7.226364	361.256285	9.244519
7.411336	358.908327	9.249536
7.400724	351.510239	9.254554
7.001199	354.987087	9.259571
7.080721	356.650591	9.264589
7.216790	367.939470	9.269607
7.455305	365.807226	9.274624
8.003344	374.296023	9.279642
7.519690	365.267532	9.284659
7.459721	357.634141	9.289677
7.084486	356.866025	9.294695
7.455441	365.707421	9.299712
7.541522	364.103814	9.304730
7.365117	371.957516	9.309747
7.465118	376.782946	9.314765
7.262099	378.326349	9.319783
7.779685	374.471850	9.324800
7.737657	373.579274	9.329818
7.221343	366.903667	9.334835
7.399643	369.763560	9.339853
7.471081	382.024982	9.344871
7.581757	373.424633	9.349888
7.479500	377.549444	9.354906
7.598760	382.835756	9.359923
7.756472	376.112004	9.364941
7.471048	369.413069	9.369959
7.690388	362.796485	9.374976
7.431096	363.158971	9.379994
7.380806	380.289569	9.385011
7.548485	370.550625	9.390029
7.386576	377.900326	9.395047
7.489820	378.379927	9.400064
7.829806	376.127746	9.405082
7.408338	383.438971	9.410099
7.914134	383.890608	9.415117
7.634293	384.871645	9.420135
7.526795	374.635927	9.425152
7.817762	381.325012	9.430170
7.369961	381.120432	9.435187
7.782264	371.090948	9.440205
7.517933	382.173947	9.445223
8.028725	379.702678	9.450240
7.956400	375.365698	9.455258
7.342219	364.814419	9.460275
7.503810	362.324942	9.465293
7.472102	368.420510	9.470311
7.723075	375.639657	9.475328
7.590102	381.015731	9.480346
7.467557	386.522721	9.485363
7.556719	371.904748	9.490381
7.762884	373.005764	9.495399
7.790794	372.304261	9.500416
7.463897	377.874621	9.505434
7.360978	373.258397	9.510451
7.679921	372.827145	9.515469
7.709863	380.913798	9.520487
7.158950	376.616621	9.525504
7.707490	380.460233	9.530522
7.622391	386.892308	9.535539
7.681690	383.169118	9.540557
7.880822	386.770503	9.545575
7.738447	386.319563	9.550592
7.659519	374.627799	9.555610
7.743566	385.874299	9.560627
7.953262	374.557298	9.565645
7.673198	381.982198	9.570663
7.957945	380.552775	9.575680
8.103283	378.659087	9.580698
7.998391	389.767757	9.585715
7.923697	376.033629	9.590733
8.036604	387.386084	9.595751
8.253550	374.635290	9.600768
8.235142	370.835843	9.605786
7.975865	378.879168	9.610803
8.064887	375.249177	9.615821
7.543375	378.754490	9.620839
7.754915	372.959584	9.625856
8.054133	369.359980	9.630874
8.055502	382.332866	9.635891
8.219103	384.608100	9.640909
8.129716	380.554628	9.645927
7.987469	374.063761	9.650944
8.433583	372.659704	9.655962
7.979326	368.659889	9.660979
7.992312	358.399110	9.665997
7.532085	367.410942	9.671015
8.042474	374.097418	9.676032
8.334819	364.326444	9.681050
7.757000	369.503546	9.686067
7.845417	373.721739	9.691085
7.948747	378.098549	9.696103
7.851530	374.500711	9.701120
8.016302	371.862421	9.706138
7.977063	369.246430	9.711155
8.031835	370.721294	9.716173
7.948052	372.378669	9.721191
8.083178	369.707128	9.726208
8.213260	372.410436	9.731226
7.831926	377.626372	9.736243
8.071011	382.493261	9.741261
8.084029	374.738052	9.746279
8.129110	379.960177	9.751296
8.165097	379.812809	9.756314
8.378740	383.948394	9.761331
8.071306	377.363332	9.766349
8.290001	375.464534	9.771367
7.784404	377.979652	9.776384
8.104010	368.942853	9.781402
8.178805	379.417656	9.786419
8.231681	371.832958	9.791437
7.954771	375.306498	9.796455
7.953775	375.019729	9.801472
7.968325	384.762338	9.806490
7.936806	381.482457	9.811507
7.982875	384.943579	9.816525
7.949228	384.207480	9.821543
7.899604	378.374344	9.826560
8.043694	377.263452	9.831578
7.599994	381.277331	9.836595
7.781477	372.202078	9.841613
8.129063	393.515084	9.846631
8.181769	394.624217	9.851648
8.587554	392.065159	9.856666
8.244667	389.562710	9.861683
7.976109	393.464121	9.866701
8.474654	385.933098	9.871719
8.103359	389.058436	9.876736
8.452954	391.150085	9.881754
8.178710	392.288034	9.886771
8.127730	390.664740	9.891789
8.291328	402.369056	9.896807
8.334695	400.096787	9.901824
8.725784	390.947865	9.906842
8.127813	389.308756	9.911859
7.939975	383.620209	9.916877
8.224722	390.329199	9.921895
8.094449	393.944005	9.926912
8.216722	399.201453	9.931930
8.231839	409.095459	9.936947
8.302632	398.232394	9.941965
8.422600	399.747601	9.946983
8.335989	403.847892	9.952000
8.514922	398.802788	9.957018
8.538366	402.538823	9.962035
8.375391	402.378254	9.967053
8.321380	407.246605	9.972071
8.221157	408.587822	9.977088
8.595518	404.411650	9.982106
8.355402	407.112644	9.987123
8.280130	396.461661	9.992141
8.600387	398.759841	9.997159
8.177226	405.597990	10.002176
8.325308	397.361017	10.007194
8.237269	399.820592	10.012211
8.203470	403.243663	10.017229
8.522704	397.949508	10.022247
8.099040	399.798653	10.027264
8.258976	395.267724	10.032282
8.237034	399.392657	10.037299
8.433744	398.630159	10.042317
8.235446	406.149631	10.047335
8.088832	409.893211	10.052352
8.550385	414.662358	10.057370
8.464153	425.717654	10.062387
8.564394	429.205063	10.067405
8.413974	433.706598	10.072423
8.632099	433.590829	10.077440
8.501109	427.931283	10.082458
8.727237	433.655386	10.087475
8.413781	425.619641	10.092493
8.899316	427.832134	10.097511
8.530748	433.427933	10.102528
8.712186	432.797193	10.107546
8.889481	435.313287	10.112563
8.741372	418.056222	10.117581
8.422567	405.726476	10.122599
8.280086	402.489112	10.127616
8.605076	417.380762	10.132634
8.603701	419.564928	10.137651
8.202729	430.643986	10.142669
8.755129	419.920508	10.147687
8.408821	424.900642	10.152704
8.394061	423.656696	10.157722
8.504133	427.401338	10.162739
8.606178	427.496137	10.167757
8.851735	422.847733	10.172775
8.707695	425.940851	10.177792
8.509521	420.146608	10.182810
8.556643	420.859000	10.187827
8.560411	424.752729	10.192845
8.245908	416.240648	10.197863
8.377070	428.136215	10.202880
8.790307	432.733017	10.207898
9.026447	444.990929	10.212915
8.871888	434.210263	10.217933
9.092157	424.239050	10.222951
8.478951	426.512165	10.227968
8.797776	423.748902	10.232986
8.706956	419.777691	10.238003
8.638237	428.573971	10.243021
8.790152	419.096218	10.248039
8.948349	433.250182	10.253056
8.913133	429.011548	10.258074
9.028376	436.122471	10.263091
8.704770	421.186890	10.268109
9.011905	421.672614	10.273127
8.877312	426.645031	10.278144
8.727712	422.651415	10.283162
9.001404	421.488784	10.288179
8.696974	421.100942	10.293197
8.988467	421.387141	10.298215
8.765597	422.580205	10.303232
8.776321	422.411525	10.308250
9.057036	435.688078	10.313267
8.939788	433.384010	10.318285
9.070592	425.007709	10.323303
8.891482	427.134346	10.328320
9.299654	425.799305	10.333338
8.937734	429.876198	10.338355
9.041191	432.501613	10.343373
9.058051	424.988769	10.348391
8.853641	425.027146	10.353408
9.168431	433.978302	10.358426
9.022042	426.989468	10.363443
8.619967	420.996609	10.368461
8.866036	427.746348	10.373479
8.988943	427.452909	10.378496
8.809113	431.876975	10.383514
8.697842	435.823331	10.388531
8.901292	450.923271	10.393549
9.321023	439.106490	10.398567
9.182987	454.821309	10.403584
9.331615	448.919415	10.408602
9.344738	438.384026	10.413619
9.179074	426.683643	10.418637
9.312663	420.661029	10.423655
9.215110	421.588441	10.428672
8.765538	427.061157	10.433690
9.273946	419.938820	10.438707
8.991908	429.165925	10.443725
9.051868	422.621469	10.448743
8.877213	436.827260	10.453760
8.915143	435.789694	10.458778
9.323362	446.998382	10.463795
9.325809	451.390917	10.468813
9.477686	435.993146	10.473831
8.989956	434.680835	10.478848
8.947218	428.568913	10.483866
9.216567	432.235110	10.488883
9.289427	439.084402	10.493901
9.268610	433.464503	10.498919
9.544620	434.734522	10.503936
9.249380	436.096638	10.508954
9.308275	431.253243	10.513971
9.091166	437.630154	10.518989
9.302399	423.242429	10.524007
9.009303	432.098891	10.529024
9.163040	431.185299	10.534042
9.245242	421.920361	10.539059
8.760900	440.604910	10.544077
9.646155	442.035680	10.549095
9.854162	453.376526	10.554112
9.286289	441.653553	10.559130
9.454217	431.848267	10.564147
9.157038	431.093240	10.569165
9.353435	427.957736	10.574183
8.960250	443.592357	10.579200
9.165877	444.273759	10.584218
9.577179	454.027214	10.589235
9.728967	451.659166	10.594253
9.450236	432.854061	10.599271
9.024952	430.014158	10.604288
9.349534	439.942045	10.609306
9.486701	447.109516	10.614323
9.579898	452.907968	10.619341
9.327683	448.750450	10.624359
9.411168	446.557131	10.629376
9.194047	449.958264	10.634394
9.491180	452.888027	10.639411
9.461421	460.867252	10.644429
9.643407	447.361335	10.649447
9.591523	450.329661	10.654464
9.369811	455.631215	10.659482
9.397654	456.135181	10.664499
9.375049	460.301255	10.669517
9.689912	457.327175	10.674535
9.549549	452.849298	10.679552
9.729183	457.327851	10.684570
9.813268	453.506117	10.689587
9.438249	447.799357	10.694605
9.469129	436.876214	10.699623
9.589832	436.280175	10.704640
9.238654	433.864213	10.709658
9.561968	447.184633	10.714675
9.617525	460.370034	10.719693
9.649958	449.339349	10.724711
9.817123	448.127034	10.729728
9.635795	454.902304	10.734746
9.312525	449.787062	10.739763
9.201488	459.476686	10.744781
9.741182	454.037742	10.749799
9.629039	455.658517	10.754816
9.369748	456.014693	10.759834
9.698735	448.137676	10.764851
9.530211	456.933730	10.769869
9.637819	455.541348	10.774887
9.596823	457.081621	10.779904
9.440450	455.282236	10.784922
9.387635	453.473039	10.789939
9.361113	457.548208	10.794957
9.564707	448.160219	10.799975
9.598566	455.264887	10.804992
9.276842	462.263981	10.810010
9.609815	466.548257	10.815027
9.742915	484.420383	10.820045
9.984182	487.068529	10.825063
10.231115	479.885897	10.830080
9.670410	475.669111	10.835098
9.687614	463.186028	10.840115
9.912033	481.753958	10.845133
9.980257	474.315143	10.850151
9.845428	463.910067	10.855168
9.588702	466.632590	10.860186
9.999078	469.459522	10.865203
9.665763	474.368222	10.870221
9.888263	468.287569	10.875239
9.979527	473.669782	10.880256
9.895344	475.055842	10.885274
9.939186	473.117989	10.890291
9.937550	474.112518	10.895309
9.745345	467.944962	10.900327
10.014897	464.996868	10.905344
9.621521	460.021920	10.910362
10.161463	478.717438	10.915379
9.891820	485.427579	10.920397
10.032594	475.531827	10.925415
10.083911	481.775447	10.930432
9.794308	479.573943	10.935450
10.063630	475.802256	10.940467
10.266852	471.870455	10.945485
10.321557	461.057192	10.950503
10.209471	459.137307	10.955520
9.865186	458.569485	10.960538
10.059593	459.631315	10.965555
10.042993	468.492080	10.970573
10.105174	465.216528	10.975591
10.357173	466.749051	10.980608
10.027502	461.155142	10.985626
10.035772	463.539773	10.990643
9.412947	459.985885	10.995661
10.099366	458.800015	11.000679
10.192932	456.791310	11.005696
9.706940	463.995854	11.010714
10.154974	471.607216	11.015731
9.874977	479.537053	11.020749
9.990015	479.989575	11.025767
10.116528	489.190969	11.030784
9.906687	486.169197	11.035802
10.255941	491.302972	11.040819
9.878246	491.803811	11.045837
9.928883	491.269170	11.050855
9.860915	485.498813	11.055872
9.805679	491.957833	11.060890
10.105248	478.452519	11.065907
10.265929	480.570437	11.070925
9.925219	479.064826	11.075943
10.560305	478.814713	11.080960
10.097068	484.198060	11.085978
10.099076	474.904556	11.090995
10.130864	494.076821	11.096013
10.322506	488.032523	11.101031
10.669004	482.188169	11.106048
10.325006	488.755260	11.111066
10.438381	485.253993	11.116083
10.180251	487.569657	11.121101
10.234115	485.292587	11.126119
10.259359	490.353739	11.131136
10.522942	493.348690	11.136154
10.202682	486.494196	11.141171
10.285805	494.878721	11.146189
10.243928	499.464353	11.151207
10.730108	487.116509	11.156224
10.568766	485.829112	11.161242
10.579389	478.367707	11.166259
10.516546	485.263391	11.171277
10.162795	478.783327	11.176295
10.498940	475.010703	11.181312
10.118152	488.122057	11.186330
10.481173	482.855772	11.191347
10.151731	489.654117	11.196365
10.261009	485.992549	11.201383
10.632321	489.418831	11.206400
10.367979	492.593804	11.211418
10.204141	490.943893	11.216435
10.465614	497.732285	11.221453
10.343478	510.557242	11.226471
10.780280	508.296283	11.231488
10.677168	510.486832	11.236506
10.785614	500.138528	11.241523
10.723235	499.037685	11.246541
10.502562	489.835647	11.251559
10.537618	481.698279	11.256576
10.481547	485.329952	11.261594
10.302210	486.408950	11.266611
10.671742	505.815807	11.271629
10.491734	498.598660	11.276647
10.809426	497.037871	11.281664
10.418416	502.962220	11.286682
10.754370	499.360026	11.291699
10.889724	496.019430	11.296717
10.236981	494.685471	11.301735
10.597507	501.048204	11.306752
10.310014	510.260423	11.311770
10.916439	514.861880	11.316787
10.791059	507.617290	11.321805
10.631155	524.657800	11.326823
11.080495	508.244862	11.331840
10.900143	510.709358	11.336858
10.471721	499.791419	11.341875
10.916341	501.170884	11.346893
10.761007	500.933388	11.351911
10.815549	487.661869	11.356928
10.553442	497.289832	11.361946
10.715387	499.237149	11.366963
10.890235	506.222060	11.371981
10.828746	511.479750	11.376999
10.984526	506.696986	11.382016
10.491252	509.614129	11.387034
10.966153	514.684170	11.392051
11.281656	509.576748	11.397069
10.651958	505.840891	11.402087
11.069545	486.968339	11.407104
10.750066	487.974487	11.412122
10.656943	490.106677	11.417139
10.871495	486.002703	11.422157
10.729754	504.198495	11.427175
11.227757	509.542636	11.432192
10.782726	509.994001	11.437210
10.922590	509.843082	11.442227
11.037789	509.333101	11.447245
10.965607	514.131730	11.452263
10.703710	505.560924	11.457280
10.739045	510.358590	11.462298
10.990171	516.637381	11.467315
11.389350	515.947491	11.472333
10.962551	518.488228	11.477351
11.121536	510.293684	11.482368
10.584090	504.104133	11.487386
10.871673	507.287845	11.492403
10.979850	521.250860	11.497421
11.039485	520.497076	11.502439
10.976624	509.651597	11.507456
10.831706	516.638963	11.512474
10.854032	516.613637	11.517491
11.317929	515.206801	11.522509
11.072999	513.610538	11.527527
10.958543	511.075661	11.532544
11.186619	510.765846	11.537562
10.790809	514.510379	11.542579
11.261942	508.485671	11.547597
11.040676	515.888850	11.552615
10.934196	510.679879	11.557632
11.105335	510.303193	11.562650
11.139177	513.160356	11.567667
11.089388	509.368921	11.572685
10.989743	521.761214	11.577703
10.871894	511.018966	11.582720
10.960155	511.485125	11.587738
11.076442	532.357804	11.592755
11.442878	532.259966	11.597773
10.955845	537.255731	11.602791
11.145532	537.264305	11.607808
11.089083	535.654472	11.612826
11.249729	533.777319	11.617843
11.497865	537.468931	11.622861
11.340401	539.134638	11.627879
11.407591	544.902457	11.632896
11.427503	530.642260	11.637914
11.175633	530.290411	11.642931
11.165970	537.483935	11.647949
10.948415	538.966502	11.652967
11.080165	543.263191	11.657984
11.445642	542.297692	11.663002
11.041649	537.135035	11.668019
11.303778	544.109527	11.673037
11.129385	546.008234	11.678055
11.370485	547.065955	11.683072
11.590109	547.170849	11.688090
11.255595	541.407262	11.693107
11.213229	547.185828	11.698125
11.554455	559.597863	11.703143
11.606887	556.330124	11.708160
11.539256	547.530244	11.713178
11.184624	546.020483	11.718195
11.340059	548.779828	11.723213
11.411721	567.450523	11.728231
11.485577	569.310581	11.733248
11.784487	561.409796	11.738266
11.752814	568.291191	11.743283
12.049874	556.809000	11.748301
11.332531	548.665677	11.753319
11.357428	537.071245	11.758336
11.586221	539.184876	11.763354
11.569848	560.870318	11.768371
11.871919	550.289874	11.773389
11.574439	548.843796	11.778407
11.379204	536.526276	11.783424
11.659121	545.192596	11.788442
11.583176	560.945176	11.793459
12.045534	561.548743	11.798477
11.565003	547.969184	11.803495
11.421831	534.116213	11.808512
11.714849	545.494372	11.813530
11.760986	554.604177	11.818547
11.914654	559.613797	11.823565
11.504058	555.660787	11.828583
11.816459	564.684962	11.833600
12.240202	553.208294	11.838618
11.728321	555.424625	11.843635
11.797475	548.484231	11.848653
12.017804	547.607601	11.853671
11.535033	541.936521	11.858688
11.665689	545.207787	11.863706
11.667439	542.856776	11.868723
11.716708	539.062535	11.873741
11.563246	550.071574	11.878759
11.439834	560.949714	11.883776
12.036718	555.725888	11.888794
11.655686	555.826477	11.893811
11.768452	558.469395	11.898829
11.847465	563.294988	11.903847
11.773156	561.852029	11.908864
11.914993	549.188541	11.913882
11.818457	565.212564	11.918899
12.398001	568.540171	11.923917
11.970839	563.021366	11.928935
12.092050	559.269565	11.933952
11.828275	571.586466	11.938970
11.931881	552.926825	11.943987
12.035637	562.882852	11.949005
12.276681	562.126067	11.954023
12.339266	570.895662	11.959040
12.346086	567.612932	11.964058
11.606736	570.069801	11.969075
12.049802	561.067328	11.974093
12.107361	569.607341	11.979111
12.059869	559.078163	11.984128
12.315519	561.452692	11.989146
11.776805	572.143046	11.994163
12.018421	564.459455	11.999181
12.002284	570.467465	12.004199
12.323755	559.852438	12.009216
12.316034	565.092307	12.014234
12.004018	572.799961	12.019251
11.951247	564.477422	12.024269
12.006319	568.779745	12.029287
12.153173	568.570934	12.034304
12.230096	570.723994	12.039322
12.184746	561.693428	12.044339
12.091224	565.908437	12.049357
12.127046	569.945525	12.054375
12.147090	564.846221	12.059392
12.273390	565.050849	12.064410
11.952408	564.561444	12.069427
12.029107	561.807457	12.074445
11.934274	569.714815	12.079463
12.097061	563.984241	12.084480
12.139017	563.678158	12.089498
12.419552	574.966765	12.094515
11.997348	573.880917	12.099533
12.154089	574.459487	12.104551
12.343620	588.488781	12.109568
12.813146	592.537239	12.114586
12.301053	592.175414	12.119603
12.470945	578.232641	12.124621
12.046575	584.048606	12.129639
12.361755	584.731892	12.134656
12.446560	581.828322	12.139674
12.315768	592.044937	12.144691
12.389517	585.981093	12.149709
12.499410	586.232456	12.154727
12.285233	596.162266	12.159744
12.326018	592.842687	12.164762
12.272836	589.411511	12.169779
12.631188	584.281618	12.174797
12.583579	594.977570	12.179815
12.601042	583.901798	12.184832
12.586400	589.275289	12.189850
12.199930	594.466843	12.194867
12.341616	590.673980	12.199885
12.495460	585.052084	12.204903
12.214764	583.448761	12.209920
12.892293	586.139446	12.214938
12.425819	583.851863	12.219955
12.435046	588.177107	12.224973
12.737918	597.414213	12.229991
12.785762	590.899982	12.235008
12.963394	585.252293	12.240026
12.450852	591.141946	12.245043
12.914151	594.579172	12.250061
12.835264	595.652004	12.255079
12.507021	590.408112	12.260096
12.555171	591.849314	12.265114
12.396469	599.416348	12.270131
12.670104	596.234077	12.275149
12.808100	598.106242	12.280167
12.227950	594.002904	12.285184
12.677369	586.646697	12.290202
12.855858	601.558155	12.295219
13.066749	602.854103	12.300237
13.216748	600.640943	12.305255
12.706681	587.873808	12.310272
12.911768	588.997096	12.315290
12.828708	597.344429	12.320307
12.602082	594.476723	12.325325
12.448141	590.379608	12.330343
12.651594	607.193217	12.335360
13.320458	615.436109	12.340378
13.330955	605.655240	12.345395
12.872487	596.777337	12.350413
13.053909	601.968833	12.355431
12.711414	594.600227	12.360448
12.788063	587.232634	12.365466
12.681405	593.302080	12.370483
12.919999	600.232923	12.375501
13.354979	605.053595	12.380519
12.533983	603.950943	12.385536
13.000762	603.641830	12.390554
12.713074	620.733885	12.395571
13.020145	616.647033	12.400589
13.126872	612.307363	12.405607
13.065879	611.859524	12.410624
13.465598	611.169547	12.415642
13.397259	618.776168	12.420659
12.950342	610.568621	12.425677
13.216939	607.112899	12.430695
12.939433	614.120947	12.435712
13.364228	615.109047	12.440730
12.942306	620.738457	12.445747
12.823891	610.270782	12.450765
13.243577	612.051755	12.455783
12.982331	627.019077	12.460800
13.098582	614.555179	12.465818
13.577678	625.809748	12.470835
13.673483	623.182160	12.475853
13.607027	610.102952	12.480871
13.072308	599.946244	12.485888
13.210327	591.493005	12.490906
12.949795	598.820284	12.495923
13.323687	602.022132	12.500941
13.431245	602.232835	12.505959
13.202892	609.028108	12.510976
13.168690	599.333094	12.515994
13.043852	598.497579	12.521011
12.977641	609.559340	12.526029
13.279669	614.059900	12.531047
13.471473	615.620743	12.536064
13.373698	612.919158	12.541082
13.698976	618.896117	12.546099
13.206897	615.340774	12.551117
13.422691	611.971854	12.556135
13.093431	622.894704	12.561152
13.422369	618.340561	12.566170
13.401037	615.888996	12.571187
13.449707	612.864820	12.576205
13.099650	611.407988	12.581223
13.231412	621.037807	12.586240
13.630074	615.393563	12.591258
13.494737	625.276402	12.596275
13.831955	617.013035	12.601293
13.887754	609.367822	12.606311
13.113728	616.484734	12.611328
13.434754	612.332597	12.616346
13.285080	608.910130	12.621363
13.387972	619.093532	12.626381
13.759155	610.152718	12.631399
13.314552	620.232023	12.636416
13.585100	614.232200	12.641434
13.729443	616.475749	12.646451
13.400394	622.478849	12.651469
13.973508	623.254516	12.656487
13.631542	620.606728	12.661504
13.934851	613.765546	12.666522
13.813038	626.584226	12.671539
13.610223	625.994372	12.676557
13.834267	620.689727	12.681575
13.590089	617.155745	12.686592
13.614608	610.815546	12.691610
13.760744	622.327073	12.696627
13.707310	626.251842	12.701645
13.940124	628.895014	12.706663
13.989538	625.024995	12.711680
14.019105	617.585828	12.716698
13.859120	614.436354	12.721715
13.434996	613.117282	12.726733
13.493953	615.648670	12.731751
13.745329	631.284081	12.736768
13.940107	631.825174	12.741786
13.983886	636.012511	12.746803
13.952100	641.619053	12.751821
14.194674	640.379205	12.756839
13.883990	639.206564	12.761856
14.259572	636.888851	12.766874
13.933199	614.619712	12.771891
13.746826	616.270992	12.776909
13.895538	628.198673	12.781927
13.821928	637.778429	12.786944
14.033766	633.327717	12.791962
14.040579	637.340936	12.796979
14.015729	644.495843	12.801997
14.000035	643.621244	12.807015
14.062999	647.133433	12.812032
13.965503	645.801372	12.817050
14.082436	641.611579	12.822067
14.325450	634.350603	12.827085
14.255234	639.284654	12.832103
14.318389	646.271231	12.837120
14.304864	638.059308	12.842138
14.210202	632.128964	12.847155
14.178414	640.095962	12.852173
13.800144	628.453794	12.857191
14.046604	637.431470	12.862208
14.030421	644.386219	12.867226
14.471247	635.163160	12.872243
14.129114	644.626943	12.877261
14.280851	637.225548	12.882279
14.014177	639.059741	12.887296
14.061029	636.244120	12.892314
14.456070	629.492788	12.897331
14.340370	647.217629	12.902349
13.934419	636.321354	12.907367
13.972988	636.151492	12.912384
14.052440	638.600801	12.917402
14.318065	635.593333	12.922419
14.060632	637.577560	12.927437
14.288079	635.320780	12.932455
14.058877	642.955612	12.937472
14.158526	644.420356	12.942490
14.600386	653.048892	12.947507
14.465753	661.521045	12.952525
14.353039	660.639461	12.957543
14.378701	659.938296	12.962560
14.398400	662.595720	12.967578
14.364955	657.384801	12.972595
14.520210	662.009208	12.977613
14.519163	667.822404	12.982631
14.749417	663.592872	12.987648
14.641233	661.789119	12.992666
14.276180	661.407554	12.997683
14.299220	671.732803	13.002701
14.359120	659.100929	13.007719
14.602617	657.513810	13.012736
14.801532	668.628999	13.017754
14.531368	660.520137	13.022771
14.580599	675.221416	13.027789
14.718934	659.285937	13.032807
14.739395	668.131564	13.037824
14.772629	662.780878	13.042842
14.864606	655.174193	13.047859
14.718270	665.847691	13.052877
14.492831	657.602483	13.057895
14.634573	662.696037	13.062912
14.805786	665.819005	13.067930
14.795738	660.288872	13.072947
14.515196	669.938732	13.077965
14.749809	664.916442	13.082983
14.943933	662.055797	13.088000
14.501631	667.101435	13.093018
14.954648	664.553919	13.098035
14.990571	670.102593	13.103053
14.672421	661.584650	13.108071
14.926111	661.245599	13.113088
14.740687	656.714728	13.118106
15.160500	664.459952	13.123123
14.790875	659.083632	13.128141
14.822155	662.140026	13.133159
14.881901	661.379908	13.138176
14.745678	659.539496	13.143194
14.891596	663.777206	13.148211
14.809771	668.583689	13.153229
15.238827	685.901872	13.158247
14.987903	668.654260	13.163264
14.990121	672.220093	13.168282
15.027088	670.327469	13.173299
15.279506	682.169614	13.178317
15.403614	668.129761	13.183335
14.916509	665.971608	13.188352
14.787164	672.006745	13.193370
15.112679	661.236400	13.198387
15.058491	684.231182	13.203405
15.319161	688.138617	13.208423
15.257533	681.679266	13.213440
14.919616	680.567665	13.218458
15.052722	675.946171	13.223475
15.051989	682.201120	13.228493
14.980163	681.571936	13.233511
15.154004	687.793395	13.238528
15.493633	687.134861	13.243546
15.632842	686.371837	13.248563
15.561669	688.506944	13.253581
15.279411	681.879979	13.258599
15.325525	678.827789	13.263616
14.923647	677.773482	13.268634
15.562218	685.146995	13.273651
15.703746	690.240590	13.278669
15.843801	682.001579	13.283687
15.522798	674.689552	13.288704
15.108229	671.601796	13.293722
14.980180	660.693793	13.298739
15.099225	671.130322	13.303757
15.319479	683.261488	13.308775
15.350903	684.317150	13.313792
14.991521	686.298321	13.318810
15.472911	687.618429	13.323827
15.101647	684.662779	13.328845
15.205999	682.078032	13.333863
15.546543	689.870321	13.338880
15.027972	693.883304	13.343898
15.443237	677.529163	13.348915
15.153458	689.588270	13.353933
15.426413	704.264207	13.358951
15.787928	693.245248	13.363968
15.316320	705.925949	13.368986
15.784021	705.711362	13.374003
15.514049	704.071645	13.379021
15.841527	713.579526	13.384039
15.639969	707.902477	13.389056
15.254668	706.675180	13.394074
15.898098	701.333615	13.399091
15.807992	707.066019	13.404109
15.473418	708.689891	13.409127
15.683315	705.555393	13.414144
15.630136	710.682465	13.419162
15.776572	695.894368	13.424179
15.951453	704.747527	13.429197
15.758309	707.513834	13.434215
15.734883	703.683541	13.439232
15.671653	708.136856	13.444250
16.131576	710.201899	13.449267
15.863214	707.268092	13.454285
15.829106	701.025349	13.459303
15.785438	707.479490	13.464320
15.614350	710.684161	13.469338
15.771354	704.531578	13.474355
15.989827	698.808069	13.479373
15.827733	712.081191	13.484391
16.106624	712.104278	13.489408
16.092459	709.026755	13.494426
15.901029	709.864660	13.499443
16.188088	707.257773	13.504461
15.914679	708.420856	13.509479
16.016058	706.212097	13.514496
15.843085	701.407885	13.519514
16.053431	702.514583	13.524531
15.933007	704.628960	13.529549
15.720433	711.131490	13.534567
16.381443	709.826489	13.539584
16.042596	711.214349	13.544602
16.184939	704.612782	13.549619
16.156033	705.744109	13.554637
15.859325	711.953636	13.559655
16.215607	721.255071	13.564672
16.246093	734.681257	13.569690
16.171216	726.447288	13.574707
16.180607	732.372486	13.579725
16.198518	736.466047	13.584743
16.290841	727.953588	13.589760
16.127605	737.941816	13.594778
16.300458	728.791988	13.599795
16.536680	736.619475	13.604813
16.345403	729.227268	13.609831
16.047474	729.737783	13.614848
15.990613	733.448522	13.619866
16.250228	729.615179	13.624883
16.298159	728.497146	13.629901
16.388798	733.207369	13.634919
16.426354	733.135491	13.639936
16.055041	733.487024	13.644954
16.184081	731.857760	13.649971
16.177378	729.492262	13.654989
16.143938	730.482289	13.660007
16.561526	743.968128	13.665024
16.606615	749.177738	13.670042
16.837811	751.423561	13.675059
16.804399	743.789025	13.680077
16.377177	733.230507	13.685095
16.657882	731.126364	13.690112
16.426645	732.330218	13.695130
16.401851	725.022542	13.700147
16.697620	741.193919	13.705165
16.804557	753.143966	13.710183
16.969911	745.071396	13.715200
16.408899	744.218581	13.720218
16.462300	745.226645	13.725235
16.649933	747.211014	13.730253
16.588883	753.516404	13.735271
16.923485	748.996059	13.740288
16.881900	755.992676	13.745306
17.074054	748.509205	13.750323
16.770462	744.495313	13.755341
16.708165	743.227189	13.760359
16.800935	743.888306	13.765376
16.647159	749.734775	13.770394
16.551373	748.834772	13.775411
16.977933	746.307142	13.780429
16.766622	756.921385	13.785447
17.263087	745.449050	13.790464
16.854069	751.171163	13.795482
16.868957	756.382322	13.800499
16.843934	758.743775	13.805517
16.691199	759.938564	13.810535
17.117599	760.301592	13.815552
16.821408	754.336314	13.820570
16.775301	757.313257	13.825587
16.818065	750.682998	13.830605
16.591896	759.100024	13.835623
16.940777	754.934050	13.840640
17.067649	760.212978	13.845658
17.014605	752.433177	13.850675
17.231501	749.865609	13.855693
17.155824	759.294278	13.860711
17.405985	749.311918	13.865728
16.974612	762.904706	13.870746
17.082270	759.063459	13.875763
16.855134	753.778530	13.880781
16.734783	763.883168	13.885799
17.279140	769.930207	13.890816
17.168815	780.544519	13.895834
17.199507	778.779089	13.900851
17.580885	765.951923	13.905869
17.354108	786.720528	13.910887
17.596492	777.301081	13.915904
17.351638	762.472869	13.920922
17.007171	754.536475	13.925939
17.053922	761.134343	13.930957
17.294496	770.968201	13.935975
17.366405	765.374785	13.940992
17.636545	785.258157	13.946010
17.293720	772.322842	13.951027
17.780399	778.069604	13.956045
17.316910	781.569116	13.961063
17.826978	781.019737	13.966080
17.373689	777.398363	13.971098
17.624208	772.054839	13.976115
17.601729	760.546531	13.981133
17.374322	761.800283	13.986151
17.574034	772.397875	13.991168
17.780956	780.356172	13.996186
17.496970	776.752618	14.001203
17.493676	774.421296	14.006221
17.318865	779.501055	14.011239
17.368475	778.026162	14.016256
17.563586	780.476417	14.021274
17.552130	782.905187	14.026291
17.637990	775.753826	14.031309
17.350038	785.436459	14.036327
17.539547	776.602741	14.041344
17.616070	781.700172	14.046362
17.343169	788.268926	14.051379
17.724128	779.064582	14.056397
17.980639	786.368238	14.061415
17.697909	780.467125	14.066432
17.741752	779.602184	14.071450
17.580067	780.703696	14.076467
17.986581	791.284880	14.081485
17.853881	790.961807	14.086503
18.013280	793.515452	14.091520
17.894601	787.424697	14.096538
17.624472	783.307758	14.101555
18.228561	787.051296	14.106573
18.168589	792.056376	14.111591
18.140183	777.194451	14.116608
18.189603	782.737902	14.121626
17.772114	773.484311	14.126643
17.826009	780.787955	14.131661
17.901149	786.939612	14.136679
17.986655	800.414084	14.141696
18.137287	801.012548	14.146714
18.020364	804.259294	14.151731
18.074518	796.267129	14.156749
17.684533	800.329541	14.161767
17.974636	799.779697	14.166784
18.243937	803.136718	14.171802
17.847728	800.585709	14.176819
18.286506	805.752974	14.181837
18.302025	805.848624	14.186855
18.411251	802.086017	14.191872
18.714024	801.041907	14.196890
18.489852	804.819735	14.201907
18.559717	792.605926	14.206925
18.302682	784.144679	14.211943
17.871654	780.336807	14.216960
18.295973	784.651117	14.221978
18.317693	791.622113	14.226995
18.437924	800.332354	14.232013
18.358050	798.233853	14.237031
18.484853	802.581867	14.242048
18.628372	800.271863	14.247066
18.196343	797.821103	14.252083
18.557176	790.961430	14.257101
18.233103	795.991852	14.262119
18.285850	801.522169	14.267136
18.418531	791.971475	14.272154
18.250707	804.279908	14.277171
18.466088	786.754458	14.282189
18.683306	793.827556	14.287207
18.686257	792.927956	14.292224
18.663903	795.948544	14.297242
18.326449	795.398582	14.302259
18.324160	796.841341	14.307277
18.534481	802.501755	14.312295
18.601852	798.701484	14.317312
18.398864	795.236790	14.322330
18.342317	800.244494	14.327347
18.344221	806.795715	14.332365
18.742049	816.545156	14.337383
18.904923	819.647359	14.342400
19.013215	809.185294	14.347418
18.920687	818.686043	14.352435
19.019450	815.073380	14.357453
18.966513	813.504000	14.362471
18.932198	805.535072	14.367488
18.985459	795.258304	14.372506
18.965384	797.789400	14.377523
19.321749	788.301710	14.382541
18.786510	788.151761	14.387559
18.779867	791.233016	14.392576
18.795786	793.528141	14.397594
18.974676	792.440206	14.402611
18.957430	792.739768	14.407629
18.628620	795.034919	14.412647
18.561134	808.214489	14.417664
18.973009	824.140652	14.422682
18.721906	823.949619	14.427699
19.225821	820.289654	14.432717
18.893866	829.089247	14.437735
19.233228	827.048542	14.442752
19.391490	815.600418	14.447770
19.716326	814.341439	14.452787
19.513833	811.381581	14.457805
19.154265	812.864191	14.462823
19.146887	818.915101	14.467840
19.231513	812.092113	14.472858
19.187810	821.399074	14.477875
19.669488	820.021004	14.482893
19.456319	812.285042	14.487911
18.948826	807.618090	14.492928
19.470011	797.691332	14.497946
19.565581	810.103923	14.502963
19.219927	803.890715	14.507981
19.563511	798.333883	14.512999
19.204181	796.982617	14.518016
19.226867	793.239797	14.523034
19.378289	810.036453	14.528051
19.604642	805.908479	14.533069
19.510169	816.302599	14.538087
19.516777	811.088555	14.543104
19.715529	814.185171	14.548122
19.271796	815.649328	14.553139
19.433269	810.199738	14.558157
19.614349	813.516851	14.563175
19.209696	813.283455	14.568192
19.405896	801.993531	14.573210
19.426656	809.813572	14.578227
19.469072	812.659981	14.583245
19.681191	815.580951	14.588263
19.449168	820.922087	14.593280
19.529106	814.693105	14.598298
19.599756	813.546284	14.603315
19.758709	815.923280	14.608333
19.479248	817.614319	14.613351
19.376673	809.514009	14.618368
19.686325	809.709027	14.623386
19.899515	828.481033	14.628403
19.586979	833.137294	14.633421
19.901893	838.872950	14.638439
19.621347	843.375913	14.643456
20.169581	839.327200	14.648474
20.092656	841.182361	14.653491
19.851948	843.757283	14.658509
20.169452	840.886868	14.663527
19.969548	841.530443	14.668544
20.119850	828.654005	14.673562
19.978282	831.926684	14.678579
19.676173	824.939848	14.683597
20.242011	837.301328	14.688615
19.917697	841.738524	14.693632
20.213435	836.135482	14.698650
19.977316	844.096516	14.703667
19.821319	842.388549	14.708685
20.140624	838.056751	14.713703
20.132060	841.125691	14.718720
20.138124	841.282773	14.723738
19.854241	846.676172	14.728755
20.229919	846.971361	14.733773
20.110814	844.086874	14.738791
19.975472	840.475943	14.743808
19.907140	830.072923	14.748826
19.975793	837.633061	14.753843
19.745628	843.753380	14.758861
20.265313	842.400948	14.763879
20.122296	857.567800	14.768896
20.656202	865.472069	14.773914
20.584827	872.075747	14.778931
20.397422	870.426315	14.783949
20.517143	862.594321	14.788967
20.702415	870.593897	14.793984
20.228039	846.163744	14.799002
20.336825	847.781714	14.804019
20.650515	855.751822	14.809037
21.128001	855.911243	14.814055
20.324734	852.274918	14.819072
20.243833	835.095345	14.824090
20.253093	841.497113	14.829107
20.465524	851.508963	14.834125
20.848274	847.943594	14.839143
20.892873	854.563922	14.844160
20.722355	848.910397	14.849178
20.809019	852.791314	14.854195
20.637209	858.501774	14.859213
20.536696	853.130831	14.864231
20.841393	846.746925	14.869248
20.783410	854.411992	14.874266
20.911840	853.152034	14.879283
20.543952	858.631097	14.884301
20.858533	861.608704	14.889319
20.201190	859.988260	14.894336
20.454626	854.814666	14.899354
20.602865	856.773624	14.904371
20.567963	857.258969	14.909389
20.876266	856.299200	14.914407
20.660689	860.230332	14.919424
20.964547	856.595196	14.924442
20.849014	867.554345	14.929459
20.677569	861.828378	14.934477
21.270139	866.138603	14.939495
21.325591	869.686719	14.944512
20.961293	864.773400	14.949530
20.897537	856.569197	14.954547
20.642546	865.647152	14.959565
20.834989	878.152002	14.964583
20.882767	881.414144	14.969600
21.442601	883.728734	14.974618
20.793070	881.472769	14.979635
21.146673	873.661158	14.984653
20.878288	879.326703	14.989671
21.253872	886.668664	14.994688
21.526947	881.201678	14.999706
21.335670	880.439609	15.004723
21.016324	882.648092	15.009741
21.206249	881.340688	15.014759
21.152675	877.404600	15.019776
21.333736	880.759597	15.024794
21.330495	874.467806	15.029811
21.260215	881.667751	15.034829
21.359039	878.790353	15.039847
20.762261	888.618952	15.044864
21.497839	901.206508	15.049882
21.493963	910.106536	15.054899
21.061081	907.636959	15.059917
21.363878	905.052839	15.064935
20.952498	910.343034	15.069952
21.311480	908.049962	15.074970
21.746269	904.934062	15.079987
21.312862	906.939405	15.085005
22.062782	905.197679	15.090023
21.954850	908.023331	15.095040
22.089850	905.619968	15.100058
21.812487	908.677123	15.105075
21.876475	899.651453	15.110093
22.089647	905.185226	15.115111
21.686430	910.638248	15.120128
21.524082	906.848475	15.125146
21.879197	906.509408	15.130163
21.434436	908.734265	15.135181
22.097529	907.798148	15.140199
21.760232	913.777384	15.145216
21.928659	913.060292	15.150234
22.092959	913.527246	15.155251
21.924227	911.155394	15.160269
21.846662	909.791807	15.165287
21.903154	913.188295	15.170304
21.746192	916.188837	15.175322
22.168890	916.479862	15.180339
21.827035	915.510867	15.185357
21.853588	913.888077	15.190375
21.795559	911.148702	15.195392
21.893405	913.229119	15.200410
21.678852	913.824485	15.205427
21.880146	926.192294	15.210445
22.169881	935.598875	15.215463
22.555024	938.821124	15.220480
22.238788	929.450703	15.225498
22.394515	928.644072	15.230515
22.078796	924.666740	15.235533
22.419986	932.474814	15.240551
22.233814	924.927099	15.245568
22.095764	916.450420	15.250586
22.398677	930.986183	15.255603
22.459685	937.130625	15.260621
22.435513	940.359800	15.265639
22.393383	943.733779	15.270656
22.179116	948.680877	15.275674
22.665617	940.028051	15.280691
22.416268	951.954811	15.285709
22.397318	945.596015	15.290727
22.557132	946.682194	15.295744
22.704249	945.962108	15.300762
22.895645	935.505965	15.305779
22.304228	933.745864	15.310797
22.488824	925.108494	15.315815
22.495446	937.001701	15.320832
22.628315	936.719326	15.325850
22.667444	934.573878	15.330867
22.865141	949.855016	15.335885
22.716168	947.158196	15.340903
22.848351	939.895418	15.345920
22.648655	942.258845	15.350938
23.020859	934.949231	15.355955
22.496892	941.579222	15.360973
22.761951	938.868432	15.365991
22.632882	937.273025	15.371008
22.322408	942.724241	15.376026
22.548715	940.622231	15.381043
22.493810	938.917449	15.386061
22.647620	942.803710	15.391079
22.868193	944.461087	15.396096
22.739017	944.150085	15.401114
22.807979	944.025981	15.406131
22.930948	963.115128	15.411149
22.813373	966.592375	15.416167
23.352574	964.132383	15.421184
23.166121	966.998672	15.426202
23.563494	958.829921	15.431219
22.958050	953.846827	15.436237
22.814657	941.918579	15.441255
22.900234	963.610727	15.446272
23.251672	959.706234	15.451290
23.191910	964.503050	15.456307
22.941951	961.799861	15.461325
23.210296	966.438297	15.466343
23.163669	968.740027	15.471360
23.286743	963.630879	15.476378
23.648137	964.448993	15.481395
23.240170	967.185672	15.486413
23.465721	965.099557	15.491431
23.523695	971.957683	15.496448
23.381778	971.642353	15.501466
23.592948	967.261089	15.506483
23.219210	971.579782	15.511501
23.280322	966.593888	15.516519
23.238907	973.464333	15.521536
23.071017	967.905033	15.526554
23.342900	969.967827	15.531571
23.361064	971.413728	15.536589
23.585415	964.016671	15.541607
23.802459	965.879724	15.546624
23.301994	966.412312	15.551642
23.445008	967.901889	15.556659
23.670968	975.920424	15.561677
23.422948	964.197796	15.566695
23.434882	975.105607	15.571712
23.421792	983.584236	15.576730
23.613766	982.039824	15.581747
23.660475	999.219030	15.586765
23.920967	993.009210	15.591783
23.802733	993.946182	15.596800
23.852558	989.044089	15.601818
23.794719	990.637522	15.606835
24.028174	997.802847	15.611853
23.731699	994.529392	15.616871
23.754125	984.023789	15.621888
23.912565	990.645378	15.626906
24.204238	982.688730	15.631923
24.250857	987.626777	15.636941
24.082414	978.460534	15.641959
24.187726	978.889338	15.646976
23.900102	990.683229	15.651994
24.237467	982.157743	15.657011
23.991920	985.405614	15.662029
23.922397	996.872067	15.667047
24.288299	994.457988	15.672064
24.085603	984.186249	15.677082
23.940586	986.856744	15.682099
24.181944	994.923382	15.687117
24.393104	990.564205	15.692135
24.043829	975.941418	15.697152
24.001088	989.319237	15.702170
24.051425	1004.598119	15.707187
24.260376	1009.368888	15.712205
24.228856	1015.297393	15.717223
24.578916	1010.512648	15.722240
24.292348	1013.552319	15.727258
24.305993	1006.046042	15.732275
24.580666	1008.098939	15.737293
24.376320	1006.909716	15.742311
24.760770	1005.527836	15.747328
24.448099	1016.864904	15.752346
24.958656	1006.374805	15.757363
24.746029	1009.967845	15.762381
24.639749	1006.058869	15.767399
25.130971	1010.463803	15.772416
24.822431	1015.037438	15.777434
24.721994	996.872998	15.782451
24.716348	1010.169320	15.787469
24.456118	1004.655943	15.792487
24.715129	1007.834728	15.797504
24.663806	1000.464799	15.802522
24.738061	1001.321310	15.807539
25.068315	1005.735526	15.812557
24.792399	1008.675709	15.817575
25.044354	1005.190633	15.822592
24.926322	1013.003971	15.827610
25.064612	999.955714	15.832627
24.755992	1002.976727	15.837645
24.491842	1007.016437	15.842663
24.902757	1005.182319	15.847680
24.582849	1012.143476	15.852698
24.582756	1000.199189	15.857715
24.610750	1008.330611	15.862733
24.632198	1021.629034	15.867751
24.631316	1035.035084	15.872768
24.844433	1037.043920	15.877786
24.760555	1029.240397	15.882803
25.149315	1031.878284	15.887821
25.079957	1035.089265	15.892839
25.237139	1031.805129	15.897856
25.072995	1044.239385	15.902874
25.495201	1027.536709	15.907891
25.452151	1032.536065	15.912909
25.110527	1039.661558	15.917927
25.416260	1038.714804	15.922944
25.333252	1043.736163	15.927962
25.632769	1043.869648	15.932979
25.328141	1034.620439	15.937997
25.273434	1028.450215	15.943015
25.524397	1040.015117	15.948032
25.566379	1058.511069	15.953050
25.842107	1046.034663	15.958067
25.811744	1041.296517	15.963085
25.550660	1037.916559	15.968103
25.817295	1028.635214	15.973120
25.411516	1036.625905	15.978138
25.744982	1029.691508	15.983155
25.855644	1025.849736	15.988173
25.540372	1029.319907	15.993191
25.457476	1037.758938	15.998208
25.498614	1047.447278	16.003226
25.897631	1054.205000	16.008243
26.048728	1052.812112	16.013261
25.750163	1051.782721	16.018279
26.112154	1055.270524	16.023296
26.099067	1056.033341	16.028314
25.939012	1057.933025	16.033331
26.028988	1043.841388	16.038349
25.643856	1043.522899	16.043367
26.169165	1051.513796	16.048384
26.152399	1058.563470	16.053402
25.961338	1053.932391	16.058419
26.283956	1044.494000	16.063437
26.171688	1047.418178	16.068455
26.193336	1052.820872	16.073472
26.075384	1043.552061	16.078490
26.400851	1047.692481	16.083507
26.159564	1040.487810	16.088525
26.308702	1040.871923	16.093543
26.263889	1039.329660	16.098560
25.982946	1034.327576	16.103578
26.257663	1049.577873	16.108595
26.278100	1048.407298	16.113613
25.969997	1048.891003	16.118631
26.138555	1044.491109	16.123648
26.084200	1047.895414	16.128666
26.050819	1048.976966	16.133683
26.514525	1044.165051	16.138701
26.060828	1050.531679	16.143719
26.316118	1044.663474	16.148736
26.335704	1049.050332	16.153754
26.332460	1060.541220	16.158771
26.581901	1062.730594	16.163789
26.603834	1069.275636	16.168807
26.929629	1064.835477	16.173824
26.645957	1064.434920	16.178842
26.796232	1076.466798	16.183859
26.798500	1065.797031	16.188877
26.788646	1081.725971	16.193895
26.585296	1069.545044	16.198912
26.571210	1073.804608	16.203930
26.743282	1072.657759	16.208947
26.751950	1072.962758	16.213965
26.776847	1078.506964	16.218983
26.655586	1072.643729	16.224000
26.860924	1079.718791	16.229018
26.844616	1067.859033	16.234035
27.035915	1070.240495	16.239053
26.685974	1076.433190	16.244071
27.112101	1065.388164	16.249088
27.051954	1068.594561	16.254106
27.001644	1064.979812	16.259123
27.298631	1056.899229	16.264141
26.612025	1070.926461	16.269159
27.182693	1066.811089	16.274176
26.925615	1062.912956	16.279194
26.982889	1076.956915	16.284211
26.921768	1068.619662	16.289229
26.875228	1087.665908	16.294247
27.270230	1087.036608	16.299264
27.487396	1087.593165	16.304282
27.137238	1099.570431	16.309299
27.607967	1086.927938	16.314317
27.375159	1093.392732	16.319335
27.398135	1090.571290	16.324352
27.354009	1082.726840	16.329370
27.367054	1087.771127	16.334387
27.381044	1080.217428	16.339405
27.039036	1090.675494	16.344423
27.556158	1089.986156	16.349440
27.803810	1091.901260	16.354458
27.625819	1094.113006	16.359475
27.767929	1093.990135	16.364493
27.404784	1091.673774	16.369511
27.490106	1094.387316	16.374528
27.454300	1099.890488	16.379546
27.418836	1100.855604	16.384563
27.575673	1096.337603	16.389581
27.610784	1110.798446	16.394599
28.055791	1111.048133	16.399616
28.083681	1114.461735	16.404634
27.794525	1102.748576	16.409651
27.857305	1099.141459	16.414669
27.613526	1119.408174	16.419687
27.653658	1115.473223	16.424704
28.228027	1116.387572	16.429722
27.848017	1129.164762	16.434739
27.920581	1125.480378	16.439757
27.978762	1126.572925	16.444775
28.248313	1123.031438	16.449792
28.342804	1121.331781	16.454810
27.845248	1121.377930	16.459827
28.388320	1105.420061	16.464845
28.373900	1116.130092	16.469863
28.178491	1111.411313	16.474880
28.008123	1118.295580	16.479898
27.878522	1121.828378	16.484915
28.123909	1117.564826	16.489933
27.982142	1121.866372	16.494951
28.106489	1113.361367	16.499968
28.302963	1115.890351	16.504986
28.036337	1120.375437	16.510003
28.509409	1127.468793	16.515021
28.684007	1136.268563	16.520039
28.405729	1137.069517	16.525056
28.477770	1143.426905	16.530074
28.534434	1137.274017	16.535091
28.763764	1130.425222	16.540109
28.414401	1125.601022	16.545127
28.070581	1126.614150	16.550144
28.773120	1133.791700	16.555162
28.378716	1143.011422	16.560179
28.923944	1137.094889	16.565197
28.663406	1134.330204	16.570215
28.542027	1140.051837	16.575232
28.542636	1136.126191	16.580250
28.738458	1137.604404	16.585267
28.658940	1132.002892	16.590285
29.023119	1141.192866	16.595303
28.480249	1140.403477	16.600320
28.750443	1137.931697	16.605338
28.574859	1143.040082	16.610355
29.338416	1160.985140	16.615373
29.234282	1155.134990	16.620391
28.950051	1157.558944	16.625408
29.439123	1149.577800	16.630426
29.178546	1142.391870	16.635443
29.160975	1138.626842	16.640461
29.220460	1143.752276	16.645479
29.224095	1142.985095	16.650496
29.429220	1134.426478	16.655514
29.032672	1138.294329	16.660531
29.224723	1135.105731	16.665549
29.162283	1139.685262	16.670567
29.492754	1158.887477	16.675584
29.698390	1143.524907	16.680602
29.301559	1139.175149	16.685619
29.659333	1130.330838	16.690637
28.952937	1141.726130	16.695655
28.866513	1146.293618	16.700672
29.409170	1149.592367	16.705690
29.433580	1161.467175	16.710707
29.925775	1162.021938	16.715725
29.311740	1158.548589	16.720743
29.441388	1167.715132	16.725760
29.465318	1159.557097	16.730778
29.390691	1156.810801	16.735795
29.840777	1151.622283	16.740813
30.111585	1154.994916	16.745831
29.931471	1159.094160	16.750848
30.098921	1156.486896	16.755866
29.735473	1156.909794	16.760883
30.020523	1157.503121	16.765901
29.771389	1160.413913	16.770919
29.831222	1154.563481	16.775936
29.879122	1163.152618	16.780954
29.826078	1159.648728	16.785971
29.871253	1160.194196	16.790989
30.062430	1168.394958	16.796007
29.781028	1161.518373	16.801024
30.418135	1143.636580	16.806042
29.889460	1155.575407	16.811059
30.152584	1153.754817	16.816077
29.996056	1161.444827	16.821095
29.780648	1167.588205	16.826112
30.161146	1173.916513	16.831130
30.112115	1179.308160	16.836147
30.110694	1174.088948	16.841165
30.294180	1180.107108	16.846183
30.224414	1181.131218	16.851200
30.424546	1175.921650	16.856218
30.039451	1184.508787	16.861235
30.207354	1181.854112	16.866253
30.454871	1184.258395	16.871271
30.198780	1183.519027	16.876288
30.152508	1174.396776	16.881306
30.022522	1190.477061	16.886323
30.625456	1192.750269	16.891341
30.618092	1200.271904	16.896359
30.667827	1199.623774	16.901376
30.494535	1196.930703	16.906394
30.689079	1204.824845	16.911411
30.979977	1203.148248	16.916429
30.894894	1200.321522	16.921447
30.840795	1202.996829	16.926464
31.174866	1206.223923	16.931482
31.033306	1199.612728	16.936499
30.958585	1180.986507	16.941517
30.978545	1171.131271	16.946535
30.961627	1169.916011	16.951552
30.982243	1167.101235	16.956570
30.676558	1169.803084	16.961587
31.278382	1195.934224	16.966605
31.004162	1196.321140	16.971623
31.311271	1190.498467	16.976640
31.462591	1191.879473	16.981658
30.898556	1178.145176	16.986675
30.982245	1179.631384	16.991693
31.149119	1184.819004	16.996711
30.894685	1191.473393	17.001728
31.185264	1193.006285	17.006746
31.241498	1193.925571	17.011763
30.923604	1189.128012	17.016781
31.182513	1185.244189	17.021799
31.178278	1192.291966	17.026816
30.972571	1193.596017	17.031834
31.253217	1199.144622	17.036851
31.442666	1208.876230	17.041869
31.601821	1215.365248	17.046887
31.770312	1212.394898	17.051904
31.617770	1207.398021	17.056922
31.509864	1225.153781	17.061939
31.748789	1216.473098	17.066957
31.898877	1217.320968	17.071975
31.560689	1213.697362	17.076992
31.715225	1214.430931	17.082010
32.177552	1218.398605	17.087027
31.916827	1215.785415	17.092045
31.945404	1185.697044	17.097063
31.846121	1198.203358	17.102080
32.148752	1187.414169	17.107098
32.126584	1195.414632	17.112115
31.881379	1196.459746	17.117133
31.937343	1184.853744	17.122151
31.759618	1198.735573	17.127168
31.777980	1208.354964	17.132186
31.764228	1207.663070	17.137203
31.837358	1204.991590	17.142221
32.034805	1218.862359	17.147239
32.051587	1217.076961	17.152256
31.982839	1209.422481	17.157274
32.063443	1225.006108	17.162291
31.540927	1213.051499	17.167309
32.066143	1213.762069	17.172327
31.771136	1239.657366	17.177344
32.402992	1230.789266	17.182362
32.510590	1235.651616	17.187379
32.689123	1242.156561	17.192397
32.780437	1244.244345	17.197415
32.328287	1237.851907	17.202432
32.718630	1236.279744	17.207450
32.679457	1241.019780	17.212467
32.545689	1233.388037	17.217485
32.882045	1232.048341	17.222503
32.576297	1241.939119	17.227520
32.500770	1231.779981	17.232538
32.516053	1235.561642	17.237555
32.603571	1242.456297	17.242573
32.333765	1237.439799	17.247591
32.722009	1243.280934	17.252608
32.759829	1245.257127	17.257626
32.631496	1243.462763	17.262643
32.599833	1244.534592	17.267661
32.676623	1240.754852	17.272679
32.639805	1244.424706	17.277696
33.044572	1248.707461	17.282714
33.019851	1256.885074	17.287731
33.112841	1259.477527	17.292749
33.404570	1262.143180	17.297767
33.012897	1250.032475	17.302784
33.272422	1250.061735	17.307802
32.890292	1245.854829	17.312819
32.911575	1251.560597	17.317837
33.224594	1257.271438	17.322855
33.362380	1261.305430	17.327872
33.180762	1251.270096	17.332890
33.228872	1258.798898	17.337907
33.605674	1262.035129	17.342925
33.400027	1254.433502	17.347943
33.226017	1264.524687	17.352960
33.059528	1258.289736	17.357978
33.424493	1254.998455	17.362995
33.508584	1255.253845	17.368013
33.669765	1247.197477	17.373031
33.502500	1261.790937	17.378048
33.759152	1260.927552	17.383066
34.091319	1256.404303	17.388083
33.652080	1264.453954	17.393101
33.863068	1255.531449	17.398119
33.699598	1250.539417	17.403136
33.616165	1249.763696	17.408154
33.864315	1253.695297	17.413171
33.710656	1252.857927	17.418189
33.807493	1252.467549	17.423207
33.539624	1255.785216	17.428224
33.798442	1266.869362	17.433242
34.044357	1272.486513	17.438259
33.685035	1279.851542	17.443277
34.355272	1274.344690	17.448295
33.984530	1271.991618	17.453312
34.392673	1272.524758	17.458330
34.593138	1272.654732	17.463347
34.486443	1275.776895	17.468365
34.736664	1274.068755	17.473383
34.105008	1267.252975	17.478400
34.464756	1261.119126	17.483418
34.400921	1264.199900	17.488435
34.297712	1257.781528	17.493453
34.705155	1262.928560	17.498471
34.597480	1256.444612	17.503488
34.320659	1249.601993	17.508506
34.370583	1251.576303	17.513523
34.324890	1269.139384	17.518541
34.610424	1270.919221	17.523559
34.844368	1265.780102	17.528576
34.615461	1262.070044	17.533594
34.633107	1270.979524	17.538611
34.478340	1270.644099	17.543629
34.559006	1268.324886	17.548647
34.561731	1274.304950	17.553664
34.527335	1272.701084	17.558682
34.857182	1269.822367	17.563699
34.424298	1273.083679	17.568717
34.683332	1265.744214	17.573735
34.641582	1271.137910	17.578752
34.685979	1270.885084	17.583770
35.214079	1280.838561	17.588787
34.856787	1297.847426	17.593805
34.957429	1289.207172	17.598823
35.271144	1293.317922	17.603840
35.123571	1292.943506	17.608858
35.348855	1295.057775	17.613875
35.132024	1299.967499	17.618893
35.236745	1289.808666	17.623911
35.043950	1300.196285	17.628928
35.068325	1299.075573	17.633946
35.156914	1300.403239	17.638963
35.217740	1298.352199	17.643981
35.148754	1293.957671	17.648999
35.428834	1304.719793	17.654016
35.270967	1296.444833	17.659034
35.813501	1297.452512	17.664051
35.541845	1296.769211	17.669069
35.519268	1294.876325	17.674087
35.526557	1282.731884	17.679104
35.383731	1295.996128	17.684122
35.365387	1310.055200	17.689139
35.716808	1316.081973	17.694157
36.026416	1311.271888	17.699175
35.832422	1312.703512	17.704192
35.848859	1314.821898	17.709210
36.034247	1308.263899	17.714227
36.003238	1320.879591	17.719245
36.113607	1313.348657	17.724263
36.018420	1308.446963	17.729280
36.069662	1316.139404	17.734298
36.308161	1302.750274	17.739315
36.222307	1315.813159	17.744333
36.427231	1304.029252	17.749351
36.200778	1292.836382	17.754368
35.546967	1300.332476	17.759386
36.054384	1306.458035	17.764403
36.067817	1305.373740	17.769421
35.884128	1311.471203	17.774439
36.330422	1316.678473	17.779456
36.291846	1311.439760	17.784474
36.447606	1307.590905	17.789491
35.859600	1312.637318	17.794509
36.099471	1308.500812	17.799527
36.383343	1324.532561	17.804544
36.301608	1333.211392	17.809562
36.756833	1328.271333	17.814579
36.680551	1340.395468	17.819597
37.044068	1334.014854	17.824615
36.914125	1335.221912	17.829632
36.714602	1334.000358	17.834650
36.749236	1323.713562	17.839667
36.866893	1336.523869	17.844685
37.084654	1329.055103	17.849703
36.807640	1320.877578	17.854720
36.776454	1328.491340	17.859738
37.037587	1326.598459	17.864755
36.791223	1325.024435	17.869773
37.064106	1323.410593	17.874791
37.319835	1322.474765	17.879808
37.333564	1336.219595	17.884826
37.035473	1331.210630	17.889843
36.872639	1334.366790	17.894861
36.790256	1331.489130	17.899879
36.971901	1331.991265	17.904896
36.796874	1338.541826	17.909914
37.108822	1323.058407	17.914931
37.051949	1329.994513	17.919949
37.572706	1343.934962	17.924967
37.491452	1345.651993	17.929984
37.134457	1349.207617	17.935002
37.837472	1349.284593	17.940019
37.557610	1355.797834	17.945037
37.341781	1362.338977	17.950055
37.479113	1363.002647	17.955072
37.423284	1358.211577	17.960090
37.864422	1353.816505	17.965107
37.512088	1361.972590	17.970125
37.730055	1355.807135	17.975143
37.751663	1355.936555	17.980160
37.701876	1352.984388	17.985178
37.806176	1346.669376	17.990195
37.932286	1343.001856	17.995213
37.892417	1350.629602	18.000231
38.094831	1350.080772	18.005248
37.831478	1358.491246	18.010266
38.141792	1350.348495	18.015283
38.255779	1356.361757	18.020301
38.155587	1346.903829	18.025319
38.202953	1352.495115	18.030336
38.112214	1353.475162	18.035354
38.314962	1351.831212	18.040371
38.048356	1351.538444	18.045389
38.360906	1349.205208	18.050407
37.758767	1348.450283	18.055424
37.918292	1365.347188	18.060442
38.441578	1368.024142	18.065459
38.402845	1380.019380	18.070477
38.532569	1367.625443	18.075495
38.577751	1378.228522	18.080512
38.525723	1382.756001	18.085530
38.881026	1370.961260	18.090547
38.576188	1375.158868	18.095565
38.726685	1385.480465	18.100583
38.684390	1379.967754	18.105600
38.555451	1378.306014	18.110618
38.833625	1375.754064	18.115635
39.028690	1377.052534	18.120653
38.977340	1375.511260	18.125671
38.800833	1368.308992	18.130688
38.679285	1376.287140	18.135706
39.095934	1371.179504	18.140723
38.991308	1372.515167	18.145741
38.955421	1375.821984	18.150759
38.887603	1371.872226	18.155776
38.730063	1380.288326	18.160794
38.874988	1386.760687	18.165811
39.161815	1388.751776	18.170829
39.141529	1388.486928	18.175847
39.259846	1385.199312	18.180864
39.551336	1390.503291	18.185882
39.753006	1377.735225	18.190899
39.628767	1380.383609	18.195917
39.590890	1389.809881	18.200935
39.834532	1380.494063	18.205952
39.660276	1375.431091	18.210970
39.720892	1367.589142	18.215987
39.807150	1365.016581	18.221005
39.712188	1362.017797	18.226023
39.687386	1356.432941	18.231040
39.301033	1364.717401	18.236058
39.636289	1367.742368	18.241075
39.724280	1383.337606	18.246093
39.522409	1376.738891	18.251111
40.050349	1377.183955	18.256128
39.509999	1385.861632	18.261146
40.135104	1372.765710	18.266163
40.092798	1380.340199	18.271181
39.956356	1381.472532	18.276199
39.928273	1376.882265	18.281216
39.698601	1389.898167	18.286234
40.107296	1386.565340	18.291251
39.936709	1387.229616	18.296269
39.790020	1381.010474	18.301287
39.972971	1375.907665	18.306304
39.777797	1383.546982	18.311322
40.411307	1403.980389	18.316339
40.293463	1400.477073	18.321357
40.096826	1402.259413	18.326375
40.389954	1397.436091	18.331392
40.163275	1399.753286	18.336410
40.491335	1405.177809	18.341427
40.522460	1390.987762	18.346445
40.074267	1398.922101	18.351463
40.501363	1402.702797	18.356480
40.608840	1422.381832	18.361498
40.742127	1423.857183	18.366515
40.803647	1421.919631	18.371533
40.870758	1431.935499	18.376551
41.190321	1429.295046	18.381568
40.826197	1427.174454	18.386586
40.793921	1421.758000	18.391603
40.794933	1421.309954	18.396621
40.372125	1429.884144	18.401639
40.699830	1424.881862	18.406656
40.761592	1428.672106	18.411674
40.995596	1419.786962	18.416691
41.297429	1444.466155	18.421709
41.140557	1447.258486	18.426727
41.263997	1442.079717	18.431744
41.286229	1453.387008	18.436762
41.520603	1445.047753	18.441779
41.562306	1448.257296	18.446797
41.504534	1444.993929	18.451815
41.792410	1436.968243	18.456832
41.693545	1448.414308	18.461850
41.737485	1436.011588	18.466867
41.626793	1422.916580	18.471885
41.476360	1421.182443	18.476903
41.695833	1428.507910	18.481920
41.929141	1440.508171	18.486938
41.804852	1444.324231	18.491955
42.244871	1439.402288	18.496973
41.776003	1429.345305	18.501991
41.770913	1416.038197	18.507008
41.666241	1436.100576	18.512026
41.657958	1431.750211	18.517043
41.852011	1438.934472	18.522061
41.962803	1440.416483	18.527079
42.160106	1437.031351	18.532096
41.703200	1442.679088	18.537114
42.062043	1445.021891	18.542131
42.355645	1443.111320	18.547149
41.847571	1441.634838	18.552167
42.176568	1444.761779	18.557184
42.058398	1451.975722	18.562202
42.139685	1461.702218	18.567219
42.343953	1467.306981	18.572237
42.376921	1473.635857	18.577255
42.610741	1473.047420	18.582272
42.283906	1478.384579	18.587290
42.349233	1470.977358	18.592307
42.508115	1469.034110	18.597325
42.548177	1472.313340	18.602343
42.458644	1474.735426	18.607360
42.605966	1476.416881	18.612378
42.560100	1463.264412	18.617395
42.778103	1464.319474	18.622413
42.583373	1470.851060	18.627431
43.186210	1473.821761	18.632448
42.857067	1476.274840	18.637466
42.927122	1470.552102	18.642483
43.320089	1480.053354	18.647501
43.205706	1479.048910	18.652519
43.233508	1463.792649	18.657536
43.165506	1463.850813	18.662554
43.017580	1462.671710	18.667571
43.322750	1480.041514	18.672589
43.372920	1484.953899	18.677607
43.673446	1481.196078	18.682624
42.938465	1477.902443	18.687642
43.440060	1484.357177	18.692659
43.349997	1483.980115	18.697677
43.205380	1490.964659	18.702695
43.664810	1494.352171	18.707712
43.689050	1497.788506	18.712730
43.547121	1488.254950	18.717747
43.678929	1491.835484	18.722765
43.699483	1493.217938	18.727783
43.679864	1484.978171	18.732800
43.538645	1492.233589	18.737818
43.597468	1499.975423	18.742835
43.719443	1492.590931	18.747853
43.719834	1496.169837	18.752871
43.969766	1502.774215	18.757888
44.285246	1501.668128	18.762906
44.147753	1492.689307	18.767923
44.444583	1486.470503	18.772941
44.046481	1479.034446	18.777959
43.975410	1476.874532	18.782976
44.070615	1503.536288	18.787994
44.415626	1501.848083	18.793011
44.600620	1508.519380	18.798029
44.502932	1504.542684	18.803047
44.607391	1502.200802	18.808064
44.524211	1503.479486	18.813082
44.303864	1501.263915	18.818099
44.500530	1492.087898	18.823117
44.401556	1500.965157	18.828135
44.412077	1502.061993	18.833152
44.591610	1499.948266	18.838170
44.354916	1506.006710	18.843187
44.587776	1501.129628	18.848205
44.617555	1500.127984	18.853223
44.671622	1500.889832	18.858240
44.759453	1502.028279	18.863258
44.587477	1514.886965	18.868275
44.981977	1518.972566	18.873293
44.928374	1533.072018	18.878311
45.294533	1529.363929	18.883328
44.852560	1529.123709	18.888346
44.714480	1536.738423	18.893363
45.232703	1522.371445	18.898381
45.243926	1524.635837	18.903399
45.220597	1532.813359	18.908416
45.202755	1528.729550	18.913434
44.987026	1526.273413	18.918451
45.263323	1516.567426	18.923469
45.064533	1526.501669	18.928487
45.478430	1539.991844	18.933504
45.709084	1543.171985	18.938522
45.597197	1541.886277	18.943539
45.698314	1533.589820	18.948557
46.128429	1545.278639	18.953575
45.952492	1546.780054	18.958592
46.310536	1547.093783	18.963610
45.563933	1526.968636	18.968627
45.770925	1517.920388	18.973645
45.812312	1534.188898	18.978663
46.223903	1539.871860	18.983680
45.903588	1540.082919	18.988698
45.709349	1543.483850	18.993715
46.335985	1538.504423	18.998733
45.977436	1538.923409	19.003751
46.022691	1542.100857	19.008768
46.403338	1538.125420	19.013786
46.305936	1539.999621	19.018803
46.321900	1538.353176	19.023821
46.191232	1545.067322	19.028839
46.302675	1542.039527	19.033856
46.478256	1545.688997	19.038874
46.247948	1552.465997	19.043891
46.204752	1544.681161	19.048909
46.296506	1540.545571	19.053927
46.179601	1552.294317	19.058944
46.806385	1563.728463	19.063962
46.387054	1561.038928	19.068979
46.648507	1563.030832	19.073997
47.014865	1565.571300	19.079015
47.045463	1571.499786	19.084032
47.078128	1567.083052	19.089050
46.792465	1569.750285	19.094067
46.937894	1558.303683	19.099085
46.959838	1560.332877	19.104103
46.925192	1565.009177	19.109120
46.981080	1559.345422	19.114138
47.200786	1566.216466	19.119155
47.221304	1555.246914	19.124173
47.152363	1566.606343	19.129191
47.286136	1580.828140	19.134208
47.286055	1584.492344	19.139226
47.150828	1596.897235	19.144243
47.396887	1581.480657	19.149261
47.489431	1587.762427	19.154279
47.080403	1590.382597	19.159296
47.487738	1591.730086	19.164314
47.552059	1598.761038	19.169331
47.526907	1589.161908	19.174349
47.884581	1591.508069	19.179367
47.499694	1592.757993	19.184384
47.800690	1602.210513	19.189402
47.633900	1614.759188	19.194419
47.918572	1611.445630	19.199437
48.034683	1622.006251	19.204455
48.064525	1619.808518	19.209472
48.240495	1610.045516	19.214490
48.164839	1616.624889	19.219507
48.359238	1614.988526	19.224525
48.546657	1616.174593	19.229543
48.274774	1623.409382	19.234560
48.451273	1614.302716	19.239578
48.183621	1620.145108	19.244595
48.044813	1618.500662	19.249613
48.190936	1619.377572	19.254631
48.129776	1616.673290	19.259648
48.502096	1613.292435	19.264666
48.409880	1604.792511	19.269683
48.552504	1620.594050	19.274701
48.841962	1634.059489	19.279719
48.752165	1634.644921	19.284736
49.060787	1618.994503	19.289754
48.765344	1619.794994	19.294771
49.112441	1627.873860	19.299789
48.675415	1615.795213	19.304807
48.670307	1631.228435	19.309824
49.123986	1627.721299	19.314842
49.269596	1636.693091	19.319859
48.932247	1635.404610	19.324877
49.167572	1637.176523	19.329895
49.227816	1633.298288	19.334912
49.385375	1620.300227	19.339930
49.010654	1624.991621	19.344947
49.020325	1628.862603	19.349965
49.443189	1619.080092	19.354983
49.041551	1624.050236	19.360000
49.228657	1623.292339	19.365018
49.257880	1642.040196	19.370035
49.859789	1646.263951	19.375053
49.777103	1650.408099	19.380071
49.675880	1662.277555	19.385088
49.682396	1649.536524	19.390106
49.520260	1651.275645	19.395123
49.726393	1648.454001	19.400141
49.444316	1647.582956	19.405159
49.558839	1658.535174	19.410176
49.947379	1645.854590	19.415194
50.036332	1666.603463	19.420211
50.210841	1677.331754	19.425229
50.196377	1667.349056	19.430247
50.071926	1680.904222	19.435264
50.229645	1663.730880	19.440282
50.300274	1674.001962	19.445299
50.339389	1671.894298	19.450317
50.996087	1665.515259	19.455335
50.376786	1670.516149	19.460352
50.776807	1659.941892	19.465370
50.767763	1662.039039	19.470387
50.864423	1657.520798	19.475405
51.118039	1657.418433	19.480423
50.803153	1658.111497	19.485440
50.699487	1641.449098	19.490458
50.721964	1650.339081	19.495475
50.771153	1655.504135	19.500493
51.465861	1660.723325	19.505511
51.047700	1659.314877	19.510528
50.885670	1654.414027	19.515546
50.751082	1652.680557	19.520563
50.550271	1656.363405	19.525581
50.899454	1654.709251	19.530599
50.912292	1661.243304	19.535616
51.068030	1660.244131	19.540634
50.950297	1666.789047	19.545651
50.963800	1672.635020	19.550669
51.582911	1679.093620	19.555687
51.337990	1690.878168	19.560704
51.460728	1692.686552	19.565722
51.069752	1687.035525	19.570739
51.353757	1689.992786	19.575757
51.482855	1689.578441	19.580775
51.287805	1705.514681	19.585792
51.540972	1712.096543	19.590810
51.613700	1707.458936	19.595827
51.592124	1712.126928	19.600845
51.838738	1712.748350	19.605863
52.101451	1711.164460	19.610880
51.905392	1708.339152	19.615898
51.785491	1713.221273	19.620915
51.883031	1716.368521	19.625933
51.827905	1708.020567	19.630951
51.727095	1719.277755	19.635968
52.237030	1724.304820	19.640986
52.456952	1728.827916	19.646003
52.190439	1728.311059	19.651021
52.401159	1719.533535	19.656039
52.701327	1721.658287	19.661056
52.712690	1730.284946	19.666074
52.964775	1727.680202	19.671091
53.062788	1726.027278	19.676109
53.217655	1712.635083	19.681127
52.798533	1699.433254	19.686144
52.828222	1689.188044	19.691162
52.905504	1695.579528	19.696179
52.283370	1696.594992	19.701197
52.385297	1704.895106	19.706215
52.886134	1718.696937	19.711232
53.289394	1716.434740	19.716250
53.337687	1718.466161	19.721267
53.149039	1720.954205	19.726285
53.318293	1709.850944	19.731303
53.008511	1721.320555	19.736320
53.250583	1710.679339	19.741338
53.522906	1716.226246	19.746355
53.490536	1715.278449	19.751373
53.710642	1719.864632	19.756391
53.437657	1725.004126	19.761408
53.908157	1714.011754	19.766426
53.275726	1714.836313	19.771443
53.234070	1717.891621	19.776461
53.872185	1719.348359	19.781479
53.917564	1728.278997	19.786496
53.932543	1736.529546	19.791514
53.872933	1738.647199	19.796531
54.178323	1743.829195	19.801549
54.309110	1744.538082	19.806567
53.869510	1747.008396	19.811584
53.727062	1738.926494	19.816602
53.767462	1735.322733	19.821619
53.770183	1743.666714	19.826637
53.814241	1729.319746	19.831655
53.863473	1744.470043	19.836672
54.081779	1757.369126	19.841690
54.222581	1759.897402	19.846707
54.344798	1770.248873	19.851725
54.642404	1755.654118	19.856743
54.441357	1767.299338	19.861760
54.575552	1765.047468	19.866778
54.497150	1755.693232	19.871795
54.865043	1765.902304	19.876813
54.794987	1757.635549	19.881831
54.618074	1757.858998	19.886848
54.936964	1773.317639	19.891866
55.326908	1776.485645	19.896883
55.249994	1767.797063	19.901901
55.214710	1758.107899	19.906919
54.902320	1765.576275	19.911936
55.410202	1777.941125	19.916954
55.385559	1777.389764	19.921971
55.489758	1781.148229	19.926989
55.402759	1772.918820	19.932007
55.381275	1773.976472	19.937024
55.404336	1775.917151	19.942042
55.701668	1773.011859	19.947059
55.556654	1772.201520	19.952077
55.656011	1777.718571	19.957095
55.462832	1777.909838	19.962112
55.545719	1779.948503	19.967130
56.182978	1777.990703	19.972147
55.588198	1789.829787	19.977165
55.637201	1778.659997	19.982183
55.822950	1775.702647	19.987200
55.591685	1780.942962	19.992218
55.701821	1768.756930	19.997235
55.442509	1781.036097	20.002253
55.803061	1789.008797	20.007271
56.027877	1797.674840	20.012288
56.397379	1795.247471	20.017306
56.678529	1797.716031	20.022323
56.500168	1805.116218	20.027341
56.677790	1801.917124	20.032359
56.861613	1792.102307	20.037376
56.520936	1792.944562	20.042394
56.946232	1787.327364	20.047411
56.762492	1795.201768	20.052429
56.660055	1791.711756	20.057447
56.979309	1792.523849	20.062464
56.977561	1793.313334	20.067482
56.949970	1795.870990	20.072499
56.863313	1801.738911	20.077517
56.816987	1782.643723	20.082535
57.017897	1793.494210	20.087552
56.740417	1793.477690	20.092570
56.947074	1791.119858	20.097587
56.859677	1793.327053	20.102605
57.551124	1804.038053	20.107623
56.822372	1810.248952	20.112640
57.023606	1812.098777	20.117658
57.301784	1815.157955	20.122675
57.184522	1813.898312	20.127693
57.531584	1810.937932	20.132711
57.124134	1809.934915	20.137728
57.263448	1823.155623	20.142746
57.887754	1820.978922	20.147763
57.964108	1833.300540	20.152781
58.222291	1827.510526	20.157799
57.814832	1833.803958	20.162816
57.765084	1835.689705	20.167834
58.036022	1836.951149	20.172851
57.942127	1842.725534	20.177869
58.163712	1835.366419	20.182887
58.169830	1841.844778	20.187904
58.172370	1841.339677	20.192922
58.191868	1837.552951	20.197939
57.798227	1845.346445	20.202957
58.150527	1846.052407	20.207975
58.472306	1852.102914	20.212992
58.478513	1864.400760	20.218010
58.780588	1859.515960	20.223027
58.458959	1864.672535	20.228045
58.508860	1865.204666	20.233063
58.890171	1865.088731	20.238080
58.835833	1867.584287	20.243098
58.896600	1865.021934	20.248115
58.658400	1867.845928	20.253133
58.654291	1859.644600	20.258151
58.824324	1876.126930	20.263168
58.809392	1880.146969	20.268186
59.061806	1877.112949	20.273203
59.117460	1886.704808	20.278221
59.183063	1877.684704	20.283239
59.392016	1881.452128	20.288256
59.234227	1886.049852	20.293274
59.420551	1877.020420	20.298291
59.532477	1878.183544	20.303309
59.393370	1884.192207	20.308327
59.890392	1881.022269	20.313344
59.531315	1889.305879	20.318362
60.224628	1892.660210	20.323379
59.783146	1890.942939	20.328397
59.916191	1895.498539	20.333415
59.562332	1892.915528	20.338432
59.827161	1901.685849	20.343450
60.185281	1900.828729	20.348467
60.217607	1904.162894	20.353485
60.039300	1907.378370	20.358503
60.240317	1904.311321	20.363520
60.251480	1906.055044	20.368538
60.344486	1897.715498	20.373555
60.592832	1906.033935	20.378573
60.544521	1898.189778	20.383591
60.547155	1882.286959	20.388608
60.192573	1902.357211	20.393626
60.359791	1902.192556	20.398643
60.501727	1908.889642	20.403661
60.867602	1917.158227	20.408679
60.633622	1921.392268	20.413696
60.633559	1925.236427	20.418714
60.774711	1920.433472	20.423731
60.899685	1921.209545	20.428749
60.811199	1924.518341	20.433767
60.778919	1921.030004	20.438784
60.744351	1932.829298	20.443802
61.084944	1936.178592	20.448819
60.900419	1955.471317	20.453837
60.803772	1950.894734	20.458855
61.367067	1944.151428	20.463872
61.131708	1950.500159	20.468890
61.473524	1957.188234	20.473907
61.844213	1972.544305	20.478925
62.119889	1969.481401	20.483943
62.309967	1969.016528	20.488960
61.929763	1962.558974	20.493978
62.098553	1949.397973	20.498995
62.059178	1944.462167	20.504013
61.790679	1941.035851	20.509031
62.231353	1950.744531	20.514048
61.794782	1960.403598	20.519066
62.213830	1962.377322	20.524083
62.269035	1957.231119	20.529101
62.471286	1963.912524	20.534119
62.731786	1956.711409	20.539136
62.304059	1963.677097	20.544154
62.968209	1966.464761	20.549171
62.815595	1962.635375	20.554189
62.808612	1964.252536	20.559207
62.868525	1954.617874	20.564224
62.241431	1956.707137	20.569242
62.717487	1957.352808	20.574259
62.632204	1962.608318	20.579277
62.595188	1965.378913	20.584295
62.888045	1953.662942	20.589312
62.775833	1968.860657	20.594330
63.089796	1976.632404	20.599347
63.216525	1984.827797	20.604365
63.325777	1990.485389	20.609383
63.237525	1982.398096	20.614400
63.184567	1980.632948	20.619418
63.156548	1984.475160	20.624435
63.268631	1984.041366	20.629453
63.100020	1983.499790	20.634471
63.519995	1982.339534	20.639488
63.651369	1979.100271	20.644506
63.362469	1973.840374	20.649523
63.267354	1983.979644	20.654541
63.780355	1997.716679	20.659559
63.986196	2005.789306	20.664576
64.100849	2004.717613	20.669594
64.126429	2003.978537	20.674611
64.124500	1998.058546	20.679629
63.887714	1997.398191	20.684647
63.869304	1998.303894	20.689664
63.943433	1995.799405	20.694682
63.932238	2010.552220	20.699699
64.159787	2007.130714	20.704717
64.139034	2016.365294	20.709735
64.391298	2007.858884	20.714752
64.279786	2014.371399	20.719770
64.573648	2017.147292	20.724787
65.191641	2012.645627	20.729805
65.010254	2015.157829	20.734823
65.192178	2006.583472	20.739840
65.036768	2008.984326	20.744858
64.863035	2003.258348	20.749875
65.029929	2007.818174	20.754893
64.724303	2002.586121	20.759911
65.366221	2019.648391	20.764928
64.945352	2031.309071	20.769946
65.156237	2027.154822	20.774963
65.304743	2037.000560	20.779981
65.141117	2035.268417	20.784999
65.297275	2031.308887	20.790016
65.568346	2036.180719	20.795034
65.461236	2030.460139	20.800051
65.955649	2053.535379	20.805069
65.636018	2055.314839	20.810087
65.889158	2052.343796	20.815104
66.072791	2062.849982	20.820122
65.839223	2055.962447	20.825139
66.009561	2060.278744	20.830157
65.783895	2063.081881	20.835175
66.477339	2048.223279	20.840192
66.283979	2057.753009	20.845210
66.219590	2055.711911	20.850227
66.392438	2050.294889	20.855245
66.263649	2051.296678	20.860263
66.266766	2059.921624	20.865280
66.475033	2067.646748	20.870298
66.568733	2077.204382	20.875315
66.654434	2080.908984	20.880333
66.626080	2087.777824	20.885351
66.804832	2080.194894	20.890368
66.651393	2089.791013	20.895386
66.682659	2083.465020	20.900403
66.928038	2083.165112	20.905421
66.970638	2087.592826	20.910439
67.276502	2083.082933	20.915456
66.940661	2098.426034	20.920474
67.167975	2105.763183	20.925491
67.430092	2105.410173	20.930509
67.468063	2117.166735	20.935527
67.220471	2098.263500	20.940544
67.287698	2110.208016	20.945562
67.570250	2109.690871	20.950579
67.620863	2105.160751	20.955597
67.706570	2109.067339	20.960615
67.541652	2101.774604	20.965632
67.800625	2115.636491	20.970650
67.798075	2130.454334	20.975667
68.126202	2123.409889	20.980685
67.727766	2125.116416	20.985703
68.270793	2129.169566	20.990720
68.254503	2127.976234	20.995738
68.149443	2129.507690	21.000755
68.411803	2125.029808	21.005773
68.186660	2129.780098	21.010791
68.221766	2128.629260	21.015808
68.389512	2129.777398	21.020826
68.333641	2123.124115	21.025843
68.739362	2136.139466	21.030861
68.458594	2142.236546	21.035879
68.737329	2143.143331	21.040896
69.013579	2143.880082	21.045914
68.816525	2155.007354	21.050931
69.204942	2140.290846	21.055949
68.985031	2148.073202	21.060967
69.133478	2149.259061	21.065984
69.011481	2149.098405	21.071002
68.998140	2150.577711	21.076019
69.137005	2158.073827	21.081037
69.539581	2174.384519	21.086055
69.651833	2166.335356	21.091072
69.884661	2169.723564	21.096090
69.735866	2173.026016	21.101107
69.990318	2171.942015	21.106125
69.825595	2180.107132	21.111143
69.962371	2168.001891	21.116160
70.026526	2166.597207	21.121178
69.423744	2168.007332	21.126195
69.793960	2169.770922	21.131213
70.009566	2172.682106	21.136231
69.950620	2167.462092	21.141248
70.059584	2183.559718	21.146266
70.229239	2190.318870	21.151283
69.949928	2194.354894	21.156301
70.221317	2188.534305	21.161319
70.214859	2189.100468	21.166336
70.250182	2192.872900	21.171354
70.175639	2209.207413	21.176371
70.811744	2217.790689	21.181389
70.736842	2215.776457	21.186407
70.719928	2215.829825	21.191424
70.701633	2209.435761	21.196442
70.848907	2217.681714	21.201459
71.111060	2222.195205	21.206477
71.253973	2235.952172	21.211495
71.127346	2236.480239	21.216512
71.471941	2240.002546	21.221530
71.373899	2240.775484	21.226547
71.787020	2237.719539	21.231565
71.620362	2239.683495	21.236583
71.724641	2238.584999	21.241600
71.729846	2229.965462	21.246618
71.629013	2239.963748	21.251635
71.786315	2230.727207	21.256653
71.600129	2236.396160	21.261671
71.836048	2238.534135	21.266688
71.933681	2240.873531	21.271706
72.069778	2259.049944	21.276723
72.028246	2258.636904	21.281741
72.237686	2259.958450	21.286759
72.325322	2261.939623	21.291776
72.451975	2256.586540	21.296794
72.569941	2257.038653	21.301811
72.597457	2246.859738	21.306829
72.633793	2252.033278	21.311847
72.924168	2254.522558	21.316864
72.826253	2258.255784	21.321882
72.939657	2249.193335	21.326899
73.058193	2255.575442	21.331917
73.245477	2253.649779	21.336935
73.138877	2254.184196	21.341952
72.781290	2250.225707	21.346970
72.802686	2254.214926	21.351987
73.341162	2239.332954	21.357005
73.248682	2240.979232	21.362023
72.936150	2258.101966	21.367040
73.132504	2260.530141	21.372058
73.293807	2276.932144	21.377075
73.616941	2272.179661	21.382093
73.872567	2282.469629	21.387111
73.724457	2275.612887	21.392128
73.687628	2276.291085	21.397146
73.609213	2286.869763	21.402163
73.978391	2274.441072	21.407181
73.707242	2293.422582	21.412199
74.003905	2297.908627	21.417216
74.416279	2282.430836	21.422234
74.382480	2292.046308	21.427251
74.460994	2287.849488	21.432269
74.497721	2290.741202	21.437287
74.300976	2292.886583	21.442304
74.903917	2285.341670	21.447322
74.538070	2292.755468	21.452339
74.591758	2279.937212	21.457357
74.792766	2286.129754	21.462375
74.454535	2292.302107	21.467392
74.836339	2298.974618	21.472410
74.908763	2308.456788	21.477427
74.912450	2313.799541	21.482445
75.016278	2310.608691	21.487463
75.204698	2308.127392	21.492480
75.500127	2310.372882	21.497498
75.307508	2316.904447	21.502515
74.980181	2318.833462	21.507533
75.452797	2324.276788	21.512551
75.155043	2327.905435	21.517568
75.477277	2339.314910	21.522586
75.871731	2345.758237	21.527603
75.824737	2334.199080	21.532621
76.064970	2334.360744	21.537639
75.595922	2339.925438	21.542656
76.195800	2340.444543	21.547674
76.209870	2347.729780	21.552691
76.427253	2344.101498	21.557709
76.294729	2351.917676	21.562727
76.005529	2348.933187	21.567744
76.417874	2351.946322	21.572762
76.475440	2361.153106	21.577779
76.712948	2353.696620	21.582797
76.914509	2354.075757	21.587815
76.453663	2361.873626	21.592832
76.899069	2356.398297	21.597850
76.777114	2362.786324	21.602867
76.704867	2356.741455	21.607885
76.983962	2368.735213	21.612903
76.742705	2375.700432	21.617920
77.096183	2380.758356	21.622938
76.902463	2381.561976	21.627955
77.070107	2376.716903	21.632973
76.794507	2375.024252	21.637991
77.183646	2393.388636	21.643008
77.572172	2395.196738	21.648026
77.602975	2405.654333	21.653043
77.629926	2400.461906	21.658061
77.680391	2410.588218	21.663079
77.885747	2408.306253	21.668096
77.772705	2410.577480	21.673114
78.007694	2404.948692	21.678131
78.075549	2413.503765	21.683149
78.335468	2409.862534	21.688167
78.395618	2416.686161	21.693184
78.376167	2421.170958	21.698202
78.780342	2420.609621	21.703219
78.720327	2413.666522	21.708237
78.728965	2412.964784	21.713255
78.881648	2413.190575	21.718272
78.853552	2412.469308	21.723290
78.524950	2412.653261	21.728307
78.916269	2410.165606	21.733325
78.770281	2408.698941	21.738343
78.842403	2408.504903	21.743360
79.217894	2408.967421	21.748378
78.921341	2412.753699	21.753395
78.905287	2411.086911	21.758413
79.520242	2426.462150	21.763431
79.255313	2435.987444	21.768448
79.743816	2431.316477	21.773466
79.634684	2434.978898	21.778483
79.567859	2438.656825	21.783501
80.120185	2436.819485	21.788519
79.546523	2427.062292	21.793536
79.881650	2426.410713	21.798554
79.720421	2432.927964	21.803571
79.974585	2431.159139	21.808589
80.173822	2444.762322	21.813607
79.923796	2458.545923	21.818624
80.293865	2450.573265	21.823642
80.363567	2462.505006	21.828659
80.218612	2456.184226	21.833677
80.229554	2458.587645	21.838695
80.443419	2467.145258	21.843712
80.984332	2471.855268	21.848730
80.788453	2480.394626	21.853747
81.094876	2483.809308	21.858765
81.466856	2474.375105	21.863783
81.402935	2485.740648	21.868800
81.308742	2474.734739	21.873818
81.219286	2461.540982	21.878835
81.477691	2469.078581	21.883853
81.607471	2466.694759	21.888871
81.286240	2479.978189	21.893888
81.488861	2480.603333	21.898906
81.624293	2468.201434	21.903923
81.943748	2478.333244	21.908941
82.008749	2470.101941	21.913959
81.411238	2471.394495	21.918976
81.764444	2473.586826	21.923994
81.758633	2466.000908	21.929011
81.658245	2476.813508	21.934029
81.858541	2481.017938	21.939047
81.872513	2502.211829	21.944064
82.038398	2498.323271	21.949082
82.164975	2504.274996	21.954099
82.302792	2513.885959	21.959117
82.709406	2518.746288	21.964135
82.668603	2527.154219	21.969152
82.701607	2524.640279	21.974170
82.614562	2524.404745	21.979187
82.847304	2526.066690	21.984205
82.704461	2528.588741	21.989223
82.881496	2525.323335	21.994240
82.874737	2525.633917	21.999258
83.221756	2543.203383	22.004275
83.316537	2537.975107	22.009293
83.558365	2540.749716	22.014311
83.502844	2546.455231	22.019328
83.644182	2540.026727	22.024346
83.558299	2541.110232	22.029363
83.701008	2539.866869	22.034381
83.727066	2537.319293	22.039399
83.804417	2537.168624	22.044416
83.814229	2530.476559	22.049434
83.840362	2536.134642	22.054451
83.908030	2556.423925	22.059469
84.274516	2560.129094	22.064487
84.171139	2564.276675	22.069504
84.191969	2565.971616	22.074522
84.296193	2554.070014	22.079539
83.980847	2553.219882	22.084557
84.553248	2550.893377	22.089575
84.572066	2566.254247	22.094592
84.732889	2566.920618	22.099610
85.098979	2569.281381	22.104627
85.247142	2566.774754	22.109645
85.835564	2561.337061	22.114663
85.368359	2573.027398	22.119680
85.637758	2564.158270	22.124698
85.560654	2563.106931	22.129715
85.640268	2563.359881	22.134733
85.592148	2565.832474	22.139751
85.706163	2561.775241	22.144768
85.873587	2550.100504	22.149786
85.631520	2555.450030	22.154803
85.516563	2560.044413	22.159821
86.203478	2549.810001	22.164839
85.988340	2559.150871	22.169856
85.818806	2555.699559	22.174874
85.953162	2556.382675	22.179891
86.070867	2561.871864	22.184909
86.091919	2574.480333	22.189927
86.171411	2585.047226	22.194944
86.433761	2575.279719	22.199962
86.304963	2582.915523	22.204979
86.703896	2581.300882	22.209997
86.646632	2586.634269	22.215015
86.646373	2602.225375	22.220032
86.669663	2606.501578	22.225050
86.811731	2607.830483	22.230067
86.817587	2607.763534	22.235085
87.324875	2608.625292	22.240103
87.228271	2612.077500	22.245120
87.359867	2621.282360	22.250138
87.803519	2624.079212	22.255155
87.569153	2636.304582	22.260173
87.694971	2627.284195	22.265191
87.749286	2634.642184	22.270208
87.725417	2632.320135	22.275226
87.941976	2628.436284	22.280243
87.854684	2633.190493	22.285261
87.781917	2633.962668	22.290279
87.770466	2639.800218	22.295296
88.085629	2649.964354	22.300314
88.206087	2647.594584	22.305331
87.990203	2660.135854	22.310349
88.427981	2653.471793	22.315367
88.149600	2655.809821	22.320384
88.562307	2663.506529	22.325402
88.534012	2668.964829	22.330419
88.787264	2670.115470	22.335437
88.811638	2659.365564	22.340455
88.593104	2673.564181	22.345472
88.554278	2669.445507	22.350490
88.974452	2681.922478	22.355507
89.085608	2694.513847	22.360525
89.270878	2694.504178	22.365543
89.286217	2696.468251	22.370560
89.230288	2697.203092	22.375578
89.023676	2701.054327	22.380595
89.416217	2716.732710	22.385613
89.880233	2715.234166	22.390631
90.011117	2716.438579	22.395648
89.887617	2716.044602	22.400666
90.576606	2718.405609	22.405683
90.313978	2719.444053	22.410701
90.561629	2712.516058	22.415719
90.184902	2712.922118	22.420736
90.336986	2721.650431	22.425754
90.710576	2709.886682	22.430771
90.527992	2728.886423	22.435789
90.774331	2721.583057	22.440807
90.796469	2742.305707	22.445824
90.589038	2747.577309	22.450842
91.056745	2738.273243	22.455859
90.649557	2743.891550	22.460877
90.967159	2733.547264	22.465895
91.038093	2746.451070	22.470912
90.994114	2759.921932	22.475930
91.546447	2771.633558	22.480947
91.339903	2766.559436	22.485965
91.793229	2759.665678	22.490983
91.773866	2765.258327	22.496000
91.549474	2770.595697	22.501018
91.524845	2778.149089	22.506035
91.580649	2791.961075	22.511053
91.767599	2784.310295	22.516071
91.895187	2782.681074	22.521088
91.970397	2793.889438	22.526106
92.364870	2801.645854	22.531123
92.439337	2817.771513	22.536141
92.532948	2810.176283	22.541159
92.401108	2814.460907	22.546176
92.641165	2814.584731	22.551194
92.680239	2802.292287	22.556211
92.716833	2824.098470	22.561229
93.265954	2830.672540	22.566247
93.216558	2827.978867	22.571264
93.675170	2824.877868	22.576282
93.918147	2823.022377	22.581299
93.517192	2833.304425	22.586317
94.020209	2825.815875	22.591335
94.110144	2825.574874	22.596352
94.005619	2820.437512	22.601370
94.002573	2803.464850	22.606387
94.007410	2796.864986	22.611405
93.776763	2792.640438	22.616423
94.148199	2804.695857	22.621440
94.142402	2813.152125	22.626458
94.124456	2828.121277	22.631475
93.854492	2835.037489	22.636493
94.012117	2823.259949	22.641511
94.347749	2832.575174	22.646528
94.120089	2846.159913	22.651546
94.555828	2847.026511	22.656563
94.603094	2856.276182	22.661581
94.692429	2852.307941	22.666599
95.042114	2846.373955	22.671616
94.665816	2855.762162	22.676634
94.887653	2866.404896	22.681651
94.831509	2869.494217	22.686669
94.818221	2872.147637	22.691687
95.175188	2869.434875	22.696704
95.039223	2879.609414	22.701722
95.278731	2894.121934	22.706739
95.746496	2897.795625	22.711757
95.597990	2897.481284	22.716775
95.852906	2900.250756	22.721792
95.495566	2894.644604	22.726810
96.019248	2913.758661	22.731827
96.228900	2921.992070	22.736845
96.424097	2928.495037	22.741863
96.468626	2931.003752	22.746880
95.973316	2930.288928	22.751898
96.250025	2924.397839	22.756915
96.243923	2930.250431	22.761933
96.426672	2940.009276	22.766951
96.774240	2948.814571	22.771968
96.814472	2943.206470	22.776986
97.093567	2937.258196	22.782003
96.906257	2941.914439	22.787021
97.157899	2956.163163	22.792039
97.738514	2963.196326	22.797056
97.612122	2975.862751	22.802074
97.631328	2971.381488	22.807091
97.525460	2969.138440	22.812109
97.551797	2972.678884	22.817127
97.511216	2979.994980	22.822144
97.707956	2973.772311	22.827162
98.429623	2976.185075	22.832179
98.260352	2994.469743	22.837197
98.060982	2995.602505	22.842215
98.555904	2990.400169	22.847232
98.220694	2998.377586	22.852250
98.472528	2998.316523	22.857267
98.596773	3003.596526	22.862285
98.478320	3002.740965	22.867303
98.738456	2993.147163	22.872320
98.768502	3008.124773	22.877338
99.329428	3011.907072	22.882355
98.831003	3023.406882	22.887373
99.480928	3022.535841	22.892391
99.146370	3020.634535	22.897408
98.916049	3019.600712	22.902426
99.446881	3017.791911	22.907443
99.498327	3031.109250	22.912461
99.575867	3041.951297	22.917479
99.768300	3029.562229	22.922496
99.695069	3041.324086	22.927514
99.943482	3040.610241	22.932531
99.855556	3033.122084	22.937549
99.917294	3041.283893	22.942567
100.473019	3060.402587	22.947584
100.115878	3063.166381	22.952602
100.347074	3055.319230	22.957619
100.505785	3060.237241	22.962637
100.347714	3061.047965	22.967655
100.907260	3067.813024	22.972672
100.918822	3081.404880	22.977690
100.909516	3086.166003	22.982707
101.261509	3085.710611	22.987725
101.290217	3078.081187	22.992743
101.672422	3078.697330	22.997760
101.411609	3076.718258	23.002778
101.490158	3082.971172	23.007795
101.518193	3080.331684	23.012813
101.618907	3080.395146	23.017831
101.620882	3071.807269	23.022848
101.984822	3093.528096	23.027866
101.964176	3104.041450	23.032883
102.571723	3104.594105	23.037901
102.300692	3106.119922	23.042919
102.383806	3106.672168	23.047936
102.059932	3105.678154	23.052954
102.156371	3106.364039	23.057971
102.351469	3107.078749	23.062989
102.061570	3108.200363	23.068007
102.753050	3110.807214	23.073024
102.354815	3129.541120	23.078042
102.468122	3127.345988	23.083059
102.538506	3139.644185	23.088077
102.499959	3146.533954	23.093095
102.967044	3146.029081	23.098112
103.148431	3160.453025	23.103130
103.537315	3179.004467	23.108147
103.705851	3168.563207	23.113165
103.939879	3167.914718	23.118183
104.224980	3168.833192	23.123200
104.085081	3164.149411	23.128218
103.937595	3163.282582	23.133235
104.177054	3165.915632	23.138253
104.389807	3156.180782	23.143271
104.870922	3161.695633	23.148288
104.453083	3163.272717	23.153306
104.836115	3159.463830	23.158323
104.399131	3164.405180	23.163341
104.277384	3171.629839	23.168359
104.879719	3172.549419	23.173376
105.128717	3183.964524	23.178394
105.083960	3182.699807	23.183411
105.025808	3188.727862	23.188429
104.776165	3186.898533	23.193447
105.414775	3194.983222	23.198464
105.534024	3207.049771	23.203482
105.224059	3213.795611	23.208499
105.477604	3205.831294	23.213517
105.716636	3209.966742	23.218535
105.614385	3209.481074	23.223552
106.068386	3226.374918	23.228570
106.219314	3229.081728	23.233587
106.350491	3230.579652	23.238605
106.087835	3233.773778	23.243623
106.182250	3231.868784	23.248640
106.006269	3255.848457	23.253658
106.280546	3253.776587	23.258675
106.515651	3259.339239	23.263693
106.529720	3265.131988	23.268711
107.070089	3264.218027	23.273728
107.327251	3270.238047	23.278746
107.201602	3273.262510	23.283763
107.439529	3273.610757	23.288781
107.857092	3271.248302	23.293799
107.854121	3269.124911	23.298816
107.675490	3277.614619	23.303834
108.033281	3281.444383	23.308851
108.359164	3281.592723	23.313869
108.180040	3280.140612	23.318887
108.110378	3274.473770	23.323904
108.045029	3271.965571	23.328922
107.997204	3268.050154	23.333939
108.116539	3277.377194	23.338957
108.179972	3296.083581	23.343975
108.445915	3292.043559	23.348992
108.419082	3305.073454	23.354010
108.457920	3302.899363	23.359027
108.958431	3303.926333	23.364045
108.886791	3320.428681	23.369063
109.129116	3322.698349	23.374080
109.303382	3330.804896	23.379098
108.976522	3320.759450	23.384115
108.952233	3324.200536	23.389133
109.197348	3326.678077	23.394151
109.293493	3342.100162	23.399168
109.420651	3357.640522	23.404186
109.630417	3355.389314	23.409203
109.704633	3352.316513	23.414221
109.593223	3362.001451	23.419239
110.006437	3370.275965	23.424256
110.250808	3371.027201	23.429274
110.293834	3372.908134	23.434291
110.370103	3377.728602	23.439309
110.364169	3380.456701	23.444327
110.723885	3389.446536	23.449344
110.836088	3392.468705	23.454362
110.767158	3396.263934	23.459379
111.206741	3390.804982	23.464397
111.067016	3386.619791	23.469415
111.224415	3393.535958	23.474432
111.352248	3403.442477	23.479450
111.296333	3409.277730	23.484467
111.470909	3398.339877	23.489485
111.572580	3410.428236	23.494503
111.487156	3414.639496	23.499520
111.841142	3417.949112	23.504538
112.210965	3423.872739	23.509555
112.333280	3418.245398	23.514573
112.366696	3423.274546	23.519591
112.380442	3420.927601	23.524608
112.555746	3416.466111	23.529626
112.734736	3442.129822	23.534643
113.065499	3440.247976	23.539661
113.074844	3444.561267	23.544679
112.872081	3439.379055	23.549696
112.964538	3441.397484	23.554714
113.079048	3438.952788	23.559731
113.474417	3436.858887	23.564749
113.157752	3452.481055	23.569767
113.632884	3457.147915	23.574784
113.756127	3460.165220	23.579802
113.720546	3474.831505	23.584819
114.165461	3463.434905	23.589837
113.866032	3469.011409	23.594855
114.123406	3466.481343	23.599872
114.229442	3468.343007	23.604890
114.204288	3482.941395	23.609907
114.436201	3496.619193	23.614925
114.369859	3500.593944	23.619943
114.617514	3490.503142	23.624960
114.514046	3495.228534	23.629978
114.553354	3501.118428	23.634995
114.968872	3511.447332	23.640013
114.706355	3515.196977	23.645031
115.048587	3512.884095	23.650048
115.338449	3524.454020	23.655066
115.442949	3528.316961	23.660083
115.608532	3528.086267	23.665101
115.852271	3536.974298	23.670119
115.571446	3542.623677	23.675136
115.783121	3543.853441	23.680154
115.646662	3547.485624	23.685171
116.163982	3552.647778	23.690189
116.230706	3554.275699	23.695207
116.476139	3566.849930	23.700224
116.396110	3560.266155	23.705242
116.530060	3557.089333	23.710259
116.901076	3555.071804	23.715277
116.818607	3558.083279	23.720295
117.030744	3565.035177	23.725312
117.010216	3572.951227	23.730330
117.054458	3580.330110	23.735347
117.814265	3577.961675	23.740365
117.642713	3581.706639	23.745383
117.785910	3578.465250	23.750400
117.975999	3577.656310	23.755418
117.928961	3578.162554	23.760435
117.993326	3578.083335	23.765453
117.923308	3575.263356	23.770471
117.991117	3581.366617	23.775488
117.931481	3579.854848	23.780506
117.811639	3603.608464	23.785523
118.396453	3597.653406	23.790541
118.644605	3604.580775	23.795559
118.196465	3609.056862	23.800576
118.377989	3624.093463	23.805594
118.439788	3628.288164	23.810611
118.824921	3628.260003	23.815629
118.882189	3651.373800	23.820647
118.667459	3655.327501	23.825664
119.223310	3653.943991	23.830682
119.031515	3669.029283	23.835699
119.125982	3679.247302	23.840717
119.667367	3675.296873	23.845735
119.773595	3683.852889	23.850752
120.586643	3692.671296	23.855770
120.351869	3695.349853	23.860787
120.419086	3697.709957	23.865805
120.510646	3699.813772	23.870823
120.574962	3699.191689	23.875840
120.722831	3696.681796	23.880858
120.460989	3694.352473	23.885875
121.195847	3708.264594	23.890893
121.067857	3717.882868	23.895911
121.234270	3724.573666	23.900928
121.539582	3726.047676	23.905946
121.387735	3717.376129	23.910963
121.379594	3718.520193	23.915981
121.397688	3725.480270	23.920999
121.733497	3725.320915	23.926016
121.593216	3733.590241	23.931034
121.575319	3752.745325	23.936051
121.976293	3747.191278	23.941069
121.844227	3750.816505	23.946087
121.931021	3773.812238	23.951104
122.430510	3765.380134	23.956122
122.300476	3767.512145	23.961139
122.651787	3772.567646	23.966157
122.655431	3788.714670	23.971175
122.631613	3787.137338	23.976192
123.274275	3787.877082	23.981210
122.838556	3807.993650	23.986227
123.058030	3794.712941	23.991245
123.360616	3812.789255	23.996263
123.268475	3817.781249	24.001280
123.717457	3815.650553	24.006298
123.366348	3827.266811	24.011315
123.534518	3844.805427	24.016333
123.666644	3851.713080	24.021351
123.826097	3838.470091	24.026368
124.238595	3842.663897	24.031386
124.062448	3864.801150	24.036403
124.500195	3869.716971	24.041421
124.720054	3867.454660	24.046439
124.820819	3870.226190	24.051456
125.154380	3864.288070	24.056474
125.066318	3873.549864	24.061491
124.981035	3860.752120	24.066509
125.474038	3880.951425	24.071527
125.358955	3878.037414	24.076544
125.490201	3882.849458	24.081562
125.433599	3891.980113	24.086579
125.778890	3882.729240	24.091597
125.940443	3880.933663	24.096615
125.868224	3884.009878	24.101632
126.039242	3894.784228	24.106650
126.306575	3906.228500	24.111667
126.716543	3898.349994	24.116685
126.615360	3902.349195	24.121703
126.704344	3902.326111	24.126720
127.261138	3904.673144	24.131738
126.546999	3912.217580	24.136755
126.763479	3904.075663	24.141773
126.953176	3915.853967	24.146791
127.164804	3922.130641	24.151808
127.396796	3920.040029	24.156826
126.987293	3936.352510	24.161843
127.783168	3941.645002	24.166861
127.715787	3951.544340	24.171879
127.717374	3956.161964	24.176896
127.846537	3955.286743	24.181914
127.890481	3963.694774	24.186931
128.032651	3971.737170	24.191949
128.807942	3968.703457	24.196967
128.658633	3972.088380	24.201984
128.750694	3971.484062	24.207002
128.751974	3966.642371	24.212019
129.052208	3980.224680	24.217037
129.282704	3990.775200	24.222055
129.190360	3993.595752	24.227072
129.596603	3991.891476	24.232090
129.368659	3997.605357	24.237107
129.183366	4000.307817	24.242125
129.853301	4012.121885	24.247143
129.697749	4021.776173	24.252160
130.210727	4012.338156	24.257178
129.807106	4020.945304	24.262195
130.146345	4020.384564	24.267213
130.543519	4025.679187	24.272231
130.496293	4048.844482	24.277248
130.443371	4042.682410	24.282266
130.585755	4044.942480	24.287283
130.356106	4035.632697	24.292301
130.806456	4049.873445	24.297319
131.029226	4068.805173	24.302336
130.958760	4067.086733	24.307354
131.507419	4071.799121	24.312371
131.636737	4085.619591	24.317389
132.050181	4092.025874	24.322407
132.067895	4093.320595	24.327424
131.782881	4091.013765	24.332442
132.114973	4086.751797	24.337459
132.554195	4081.466292	24.342477
132.355071	4072.820872	24.347495
132.067628	4077.300461	24.352512
132.862194	4087.182458	24.357530
132.690354	4101.977781	24.362547
133.001037	4093.817956	24.367565
133.170362	4092.560876	24.372583
132.995510	4097.521636	24.377600
133.124920	4093.158658	24.382618
133.519264	4095.982360	24.387635
133.686036	4100.261829	24.392653
134.115766	4107.965978	24.397671
134.055792	4106.261683	24.402688
134.309564	4100.916668	24.407706
134.189600	4112.468714	24.412723
134.192543	4102.800741	24.417741
134.221142	4104.826030	24.422759
133.922875	4109.089527	24.427776
134.257959	4102.065325	24.432794
134.398628	4114.833002	24.437811
134.576361	4127.408696	24.442829
134.774288	4128.959429	24.447847
135.106713	4145.042958	24.452864
135.146373	4151.093981	24.457882
135.692275	4154.484325	24.462899
135.146261	4156.826337	24.467917
135.279952	4146.045900	24.472935
135.720992	4168.213686	24.477952
135.800745	4176.802464	24.482970
135.757842	4177.816248	24.487987
136.171441	4178.572735	24.493005
136.043590	4185.107515	24.498023
136.172928	4204.682039	24.503040
136.375050	4194.844128	24.508058
136.695336	4203.707945	24.513075
136.514852	4214.139516	24.518093
136.902505	4227.143419	24.523111
136.912810	4232.110108	24.528128
137.367607	4227.200895	24.533146
137.276513	4236.299218	24.538163
137.498718	4259.378645	24.543181
137.662950	4250.742851	24.548199
137.577081	4257.750883	24.553216
137.901013	4261.683976	24.558234
138.219560	4279.388982	24.563251
137.886270	4288.105247	24.568269
138.281840	4284.423585	24.573287
138.242662	4288.488969	24.578304
138.256595	4297.987608	24.583322
138.867574	4302.832389	24.588339
138.686942	4310.126640	24.593357
139.164322	4309.992585	24.598375
139.224899	4328.002935	24.603392
139.513715	4329.735228	24.608410
139.396708	4327.222299	24.613427
139.602862	4330.116370	24.618445
139.856073	4329.550078	24.623463
140.049935	4345.027246	24.628480
140.222424	4355.457601	24.633498
140.327619	4348.099803	24.638515
140.189992	4354.462567	24.643533
140.698169	4350.179436	24.648551
140.700194	4351.132576	24.653568
140.739012	4357.370024	24.658586
140.950143	4370.243696	24.663603
141.253618	4369.881052	24.668621
141.382752	4364.580616	24.673639
141.363632	4378.465454	24.678656
141.539916	4379.593472	24.683674
141.643516	4374.783086	24.688691
141.591152	4394.288258	24.693709
141.962735	4390.373582	24.698727
141.826547	4400.287035	24.703744
142.103103	4395.257179	24.708762
142.071637	4405.757193	24.713779
142.240530	4420.812206	24.718797
142.812731	4425.438957	24.723815
142.780175	4424.402667	24.728832
142.756641	4423.538572	24.733850
142.632972	4418.915064	24.738867
142.693472	4437.724093	24.743885
143.084698	4445.964651	24.748903
143.271890	4446.497579	24.753920
143.333426	4444.376632	24.758938
143.294058	4459.107432	24.763955
143.387025	4465.061882	24.768973
143.712445	4463.467994	24.773991
143.900150	4471.762345	24.779008
143.997233	4486.632898	24.784026
144.122444	4486.825120	24.789043
144.128963	4500.867034	24.794061
144.449683	4512.530637	24.799079
144.737332	4516.829262	24.804096
144.636327	4516.595874	24.809114
145.113213	4527.124129	24.814131
145.392597	4531.663929	24.819149
145.902579	4533.440718	24.824167
145.634302	4536.197210	24.829184
146.186433	4527.617678	24.834202
146.247491	4528.170246	24.839219
146.111795	4525.947429	24.844237
146.336339	4526.796494	24.849255
146.686362	4530.441511	24.854272
146.823655	4540.978457	24.859290
147.061599	4549.962581	24.864307
146.729733	4556.229402	24.869325
147.165116	4543.470054	24.874343
146.816598	4552.179347	24.879360
146.823844	4550.407729	24.884378
147.172611	4566.640595	24.889395
146.937644	4578.213999	24.894413
147.439699	4574.850277	24.899431
147.618602	4589.184216	24.904448
147.631650	4609.026637	24.909466
148.282305	4615.591872	24.914483
147.975136	4603.967604	24.919501
148.577906	4616.288080	24.924519
148.668564	4624.079962	24.929536
148.523292	4630.077871	24.934554
148.471438	4628.198660	24.939571
148.706266	4639.774714	24.944589
148.616428	4649.138186	24.949607
148.601580	4653.405030	24.954624
148.987033	4678.359727	24.959642
149.262365	4673.011188	24.964659
149.300341	4688.222531	24.969677
149.469754	4692.605891	24.974695
149.727300	4704.614033	24.979712
150.035912	4709.221924	24.984730
150.439978	4717.744684	24.989747
150.289335	4725.908758	24.994765
150.514609	4729.592176	24.999783
150.798864	4732.549906	25.004800
150.955119	4750.820388	25.009818
151.283487	4748.070770	25.014835
151.227604	4754.676616	25.019853
151.876436	4752.694615	25.024871
151.737868	4742.922075	25.029888
151.834548	4741.458468	25.034906
152.088562	4743.177282	25.039923
152.313847	4756.487767	25.044941
151.883080	4766.144267	25.049959
152.649242	4775.339811	25.054976
152.329200	4777.659344	25.059994
152.522362	4773.557729	25.065011
152.409710	4770.034006	25.070029
152.684942	4777.326911	25.075047
153.223333	4789.408172	25.080064
152.695080	4796.851432	25.085082
153.250629	4788.549011	25.090099
153.076565	4802.612961	25.095117
153.349438	4818.056138	25.100135
153.795794	4819.385180	25.105152
153.891392	4819.017016	25.110170
154.184040	4818.488760	25.115187
153.955521	4838.798316	25.120205
154.259322	4840.610394	25.125223
154.289104	4843.490974	25.130240
154.143242	4857.304374	25.135258
154.676571	4860.015022	25.140275
154.430468	4867.480668	25.145293
154.876550	4878.364288	25.150311
155.373702	4890.635111	25.155328
155.363001	4899.465578	25.160346
155.815809	4888.972756	25.165363
155.968974	4894.785405	25.170381
156.423668	4903.884312	25.175399
156.912612	4905.143602	25.180416
156.698687	4897.330236	25.185434
157.030630	4884.662508	25.190451
157.483374	4891.880476	25.195469
157.236817	4878.169658	25.200487
157.153328	4870.541164	25.205504
156.989070	4882.990711	25.210522
157.382956	4881.253558	25.215539
157.566596	4887.847413	25.220557
157.575629	4888.502785	25.225575
157.537751	4888.673057	25.230592
157.394040	4906.968303	25.235610
157.920889	4905.081032	25.240627
157.634521	4922.981855	25.245645
157.949607	4930.742084	25.250663
158.032240	4938.090292	25.255680
158.460587	4952.739205	25.260698
158.709961	4956.466264	25.265715
158.860079	4974.592730	25.270733
158.779556	4968.317852	25.275751
159.128749	4970.025026	25.280768
159.268354	4997.818213	25.285786
159.476740	5002.934192	25.290803
159.511491	5008.525423	25.295821
159.558720	5015.737134	25.300839
160.071877	5021.525340	25.305856
159.552611	5027.890941	25.310874
160.065386	5032.085197	25.315891
160.382205	5053.749437	25.320909
160.808194	5052.335542	25.325927
160.714984	5049.784086	25.330944
161.254281	5069.958576	25.335962
161.380828	5067.928442	25.340979
161.857653	5055.512651	25.345997
162.216533	5058.218926	25.351015
162.327714	5047.271009	25.356032
162.319330	5059.611185	25.361050
162.084554	5046.763277	25.366067
162.212119	5052.343228	25.371085
162.274621	5063.090979	25.376103
162.614336	5065.762361	25.381120
162.563975	5086.394825	25.386138
162.764929	5076.373543	25.391155
162.771633	5088.547252	25.396173
162.916739	5100.415339	25.401191
163.019661	5109.414451	25.406208
162.951076	5113.768681	25.411226
163.329148	5110.673527	25.416243
163.395890	5135.233411	25.421261
163.713351	5139.764280	25.426279
163.862008	5129.097719	25.431296
164.028132	5149.942755	25.436314
164.151739	5164.942308	25.441331
164.315456	5169.812769	25.446349
164.521566	5168.559359	25.451367
164.805174	5183.783378	25.456384
164.604569	5192.823475	25.461402
164.898969	5189.892846	25.466419
164.958661	5208.406090	25.471437
164.928267	5214.825059	25.476455
165.273699	5221.718965	25.481472
165.632613	5232.300721	25.486490
165.491481	5234.494605	25.491507
165.796311	5251.861797	25.496525
165.920291	5266.975009	25.501543
166.468499	5265.927164	25.506560
166.405099	5286.486128	25.511578
166.785225	5294.517316	25.516595
166.955619	5296.110316	25.521613
166.963285	5307.646407	25.526631
167.465187	5308.120895	25.531648
167.396160	5317.642453	25.536666
167.184302	5319.604306	25.541683
167.560415	5335.663153	25.546701
168.096643	5342.508461	25.551719
168.239235	5339.904469	25.556736
168.122585	5363.435780	25.561754
168.275465	5368.336391	25.566771
168.719198	5368.336989	25.571789
168.587235	5393.127018	25.576807
169.069099	5392.531409	25.581824
168.776043	5402.769700	25.586842
169.505324	5404.837558	25.591859
169.832774	5408.700912	25.596877
169.939426	5411.534893	25.601895
170.197278	5404.335980	25.606912
169.902495	5407.093572	25.611930
170.786580	5415.084231	25.616947
170.799780	5421.767947	25.621965
170.702945	5432.673299	25.626983
170.911163	5429.361483	25.632000
171.059324	5434.701605	25.637018
171.212723	5434.283395	25.642035
171.131461	5436.120762	25.647053
171.380018	5455.447648	25.652071
171.761628	5456.670028	25.657088
171.613691	5457.245694	25.662106
172.071046	5474.387334	25.667123
172.245985	5476.973953	25.672141
171.934357	5478.477875	25.677159
172.653609	5485.837668	25.682176
172.231851	5507.181835	25.687194
172.399914	5498.869977	25.692212
172.889832	5509.835537	25.697229
172.782435	5530.502636	25.702247
173.499398	5524.870446	25.707264
173.409326	5533.180122	25.712282
173.855198	5544.572382	25.717300
174.195980	5553.294782	25.722317
174.022631	5551.532245	25.727335
174.334464	5551.490248	25.732352
174.226042	5557.700527	25.737370
174.279322	5570.823743	25.742388
174.922557	5576.759175	25.747405
174.789538	5579.860926	25.752423
175.216092	5580.808010	25.757440
175.109978	5586.260365	25.762458
175.543265	5590.893264	25.767476
175.353872	5592.921093	25.772493
175.411617	5597.972310	25.777511
175.555581	5594.137009	25.782528
176.201642	5612.003818	25.787546
175.930981	5612.585969	25.792564
175.900384	5619.838445	25.797581
175.936030	5638.005491	25.802599
176.170829	5637.704023	25.807616
176.166249	5653.797169	25.812634
176.225897	5665.331707	25.817652
177.077822	5680.679153	25.822669
177.156286	5699.597172	25.827687
177.422016	5707.744209	25.832704
177.677379	5721.407413	25.837722
177.725758	5713.038333	25.842740
178.077339	5727.614597	25.847757
178.230970	5744.961608	25.852775
178.263493	5738.725682	25.857792
178.575875	5756.246853	25.862810
178.746849	5779.424575	25.867828
178.680140	5776.370149	25.872845
178.954290	5790.402957	25.877863
179.212037	5796.515273	25.882880
179.582668	5809.223087	25.887898
179.771675	5818.628975	25.892916
180.436234	5825.896411	25.897933
180.094870	5831.325490	25.902951
180.548444	5829.916714	25.907968
180.671153	5844.591836	25.912986
180.740978	5850.780776	25.918004
180.999138	5840.851181	25.923021
180.884819	5855.632660	25.928039
181.274995	5865.698549	25.933056
181.233934	5873.940773	25.938074
181.425852	5879.671946	25.943092
181.938600	5892.610222	25.948109
181.921378	5907.408192	25.953127
182.070221	5907.972389	25.958144
181.961815	5917.143693	25.963162
182.263101	5931.147132	25.968180
182.654944	5930.167789	25.973197
182.642281	5948.064883	25.978215
182.737670	5958.003104	25.983232
183.261381	5966.173224	25.988250
183.189877	5982.352838	25.993268
183.757910	5985.266594	25.998285
183.504388	5991.206044	26.003303
183.850014	5993.062234	26.008320
184.157428	5999.747706	26.013338
183.861491	6009.914182	26.018356
184.436371	6022.290466	26.023373
184.620012	6029.576040	26.028391
185.246490	6045.940609	26.033408
185.578711	6056.605918	26.038426
185.605698	6058.442277	26.043444
186.171955	6052.489318	26.048461
185.549470	6054.433106	26.053479
185.730311	6042.668805	26.058496
185.826562	6066.748697	26.063514
185.964789	6073.975069	26.068532
186.699518	6074.921551	26.073549
186.398480	6078.564077	26.078567
186.327913	6092.009989	26.083584
186.666081	6101.932586	26.088602
186.739654	6122.281768	26.093620
187.284636	6130.372890	26.098637
187.196338	6139.837901	26.103655
187.551071	6135.070026	26.108672
187.643657	6148.904100	26.113690
187.434497	6165.146344	26.118708
188.008078	6174.568301	26.123725
188.100357	6189.018002	26.128743
188.197998	6192.529033	26.133760
188.497995	6201.627426	26.138778
188.452005	6214.365664	26.143796
188.872590	6223.451606	26.148813
189.067348	6240.451765	26.153831
188.904113	6244.158099	26.158848
189.226308	6263.313387	26.163866
189.556386	6283.209288	26.168884
189.626139	6292.119448	26.173901
189.833079	6298.905902	26.178919
190.206191	6309.694417	26.183936
190.648237	6321.100387	26.188954
190.709541	6324.187792	26.193972
191.148434	6326.894429	26.198989
191.658107	6332.958233	26.204007
192.187130	6333.980950	26.209024
192.226063	6325.003820	26.214042
192.201963	6320.970409	26.219060
192.668032	6324.641917	26.224077
192.691355	6329.948074	26.229095
192.755344	6323.164099	26.234112
192.891514	6338.585658	26.239130
193.084729	6350.750113	26.244148
193.022352	6348.455679	26.249165
193.200498	6357.314271	26.254183
193.340128	6376.750637	26.259200
193.446911	6371.200564	26.264218
193.605978	6378.559550	26.269236
194.082951	6392.368687	26.274253
193.870910	6400.640925	26.279271
194.171075	6411.993281	26.284288
194.776117	6421.129522	26.289306
194.433003	6428.936047	26.294324
194.942728	6434.699990	26.299341
194.973254	6449.181608	26.304359
195.096687	6460.283718	26.309376
195.459380	6462.989612	26.314394
195.356837	6476.497605	26.319412
195.869741	6479.123295	26.324429
196.146653	6506.332354	26.329447
196.237090	6517.827913	26.334464
196.413690	6509.634223	26.339482
196.548605	6529.500799	26.344500
196.957916	6541.448647	26.349517
196.793483	6539.391049	26.354535
197.041613	6556.638888	26.359552
197.543867	6566.422550	26.364570
197.337417	6572.509539	26.369588
197.900319	6575.907171	26.374605
198.032092	6592.841703	26.379623
198.142378	6601.300603	26.384640
198.490974	6610.129624	26.389658
198.680884	6621.625546	26.394676
198.908897	6620.157127	26.399693
199.105938	6633.255568	26.404711
199.221249	6628.449080	26.409728
199.420172	6633.282886	26.414746
199.289339	6660.277862	26.419764
199.644892	6658.413931	26.424781
199.967626	6675.025231	26.429799
200.122340	6676.093618	26.434816
200.448330	6679.764910	26.439834
200.396798	6689.862144	26.444852
201.161413	6687.527302	26.449869
201.182332	6707.721182	26.454887
201.494257	6716.799034	26.459904
202.067555	6701.788043	26.464922
202.410516	6698.748599	26.469940
202.692307	6692.423032	26.474957
202.630836	6695.169744	26.479975
202.510439	6699.573456	26.484992
202.784086	6684.880612	26.490010
203.064169	6702.123614	26.495028
203.316511	6702.172955	26.500045
203.197885	6714.824991	26.505063
203.320568	6715.860486	26.510080
203.527671	6710.130540	26.515098
203.546612	6723.989142	26.520116
203.785552	6725.975662	26.525133
204.070753	6739.417168	26.530151
204.039113	6753.463602	26.535168
204.229994	6754.665260	26.540186
204.574047	6782.037899	26.545204
205.147529	6777.608300	26.550221
205.115075	6779.346657	26.555239
205.204960	6783.379876	26.560256
205.433890	6787.596639	26.565274
205.698159	6803.674195	26.570292
205.740300	6810.151880	26.575309
206.077609	6822.931883	26.580327
206.490764	6821.870258	26.585344
207.128372	6814.832643	26.590362
207.191216	6830.928955	26.595380
207.990174	6828.995974	26.600397
208.183284	6835.611160	26.605415
208.029022	6831.414807	26.610432
208.236960	6834.315317	26.615450
208.336907	6839.881176	26.620468
208.377457	6842.681476	26.625485
208.647926	6833.503897	26.630503
208.288829	6845.571577	26.635520
208.466207	6846.134518	26.640538
208.787218	6865.577890	26.645556
209.022567	6874.973951	26.650573
209.315951	6895.431826	26.655591
209.176660	6895.595807	26.660608
209.430879	6897.267445	26.665626
209.655641	6917.117298	26.670644
210.121585	6924.766504	26.675661
210.393423	6940.726201	26.680679
210.877136	6944.783375	26.685696
210.655787	6941.620243	26.690714
210.642672	6962.779368	26.695732
210.870195	6968.107585	26.700749
211.014208	6974.730464	26.705767
211.341131	6990.934173	26.710784
211.501899	7007.141667	26.715802
211.969189	7018.108504	26.720820
212.230116	7029.953502	26.725837
212.189399	7033.423100	26.730855
212.079118	7049.956944	26.735872
212.583797	7051.968421	26.740890
212.721586	7077.043886	26.745908
212.886669	7085.267188	26.750925
213.510086	7102.791738	26.755943
213.658945	7108.517374	26.760960
213.854472	7121.887888	26.765978
213.980301	7134.439018	26.770996
213.967040	7136.164949	26.776013
214.421680	7139.428016	26.781031
214.126264	7154.036700	26.786048
214.477540	7165.283706	26.791066
214.367868	7188.314341	26.796084
214.655043	7192.266425	26.801101
214.897943	7205.440215	26.806119
215.149923	7229.614195	26.811136
215.593218	7246.137794	26.816154
215.608430	7258.453682	26.821172
215.977992	7271.080605	26.826189
216.523033	7280.722246	26.831207
216.611028	7297.550599	26.836224
216.905197	7298.666762	26.841242
216.962240	7314.795971	26.846260
217.709442	7318.474423	26.851277
218.040803	7318.107387	26.856295
218.099761	7336.837569	26.861312
218.498578	7340.491343	26.866330
218.276824	7350.555461	26.871348
218.668174	7358.854150	26.876365
219.465590	7355.810140	26.881383
219.527335	7361.893517	26.886400
219.955953	7347.330703	26.891418
220.402002	7350.222636	26.896436
220.561357	7350.617928	26.901453
220.409287	7340.517783	26.906471
220.506611	7338.046831	26.911488
220.873874	7336.424089	26.916506
220.761197	7357.955895	26.921524
221.259977	7363.661859	26.926541
221.375203	7358.836252	26.931559
221.332217	7377.560249	26.936576
221.571747	7383.985307	26.941594
221.796983	7384.263010	26.946612
221.930339	7403.212128	26.951629
222.715284	7413.129020	26.956647
222.342049	7422.121326	26.961664
222.111655	7429.730783	26.966682
222.627464	7439.980023	26.971700
222.858753	7458.172084	26.976717
223.234786	7463.676207	26.981735
223.092964	7477.026893	26.986752
223.520080	7490.569975	26.991770
223.770661	7505.987333	26.996788
223.769479	7526.220280	27.001805
224.150820	7529.043393	27.006823
224.360084	7551.194565	27.011840
224.301532	7555.165828	27.016858
224.509415	7577.935999	27.021876
224.835579	7595.276846	27.026893
225.165863	7599.231778	27.031911
225.054434	7618.048754	27.036928
225.362674	7630.713885	27.041946
225.810425	7652.310315	27.046964
225.990462	7664.095707	27.051981
226.753371	7659.585899	27.056999
226.750518	7689.807774	27.062016
226.777898	7703.946767	27.067034
227.313569	7713.091302	27.072052
227.766140	7708.547718	27.077069
228.304190	7716.369132	27.082087
228.561730	7739.106516	27.087104
228.837638	7724.466158	27.092122
228.982422	7730.003208	27.097140
228.963328	7738.675350	27.102157
229.543082	7728.492624	27.107175
229.357162	7728.613360	27.112192
229.401245	7745.799379	27.117210
229.368875	7758.081970	27.122228
229.491070	7762.482893	27.127245
229.942339	7767.842803	27.132263
230.102323	7777.074273	27.137280
230.173712	7793.678366	27.142298
230.415000	7799.825486	27.147316
230.475103	7811.127692	27.152333
230.800865	7824.361635	27.157351
230.771418	7842.591513	27.162368
231.217760	7849.233936	27.167386
231.709758	7859.338742	27.172404
231.915691	7878.949481	27.177421
232.190185	7881.940819	27.182439
232.362873	7909.079792	27.187456
232.483135	7917.780833	27.192474
232.813923	7928.687389	27.197492
233.058363	7944.832172	27.202509
233.790855	7951.464809	27.207527
233.738337	7955.368922	27.212544
234.035696	7958.950223	27.217562
234.502714	7970.356494	27.222580
234.567297	7984.710899	27.227597
235.055752	7977.260405	27.232615
234.954753	7983.138865	27.237632
235.118362	7999.706688	27.242650
235.732676	8008.138278	27.247668
235.411721	8017.798326	27.252685
235.863365	8022.864655	27.257703
236.231295	8034.759939	27.262720
236.423954	8048.551454	27.267738
236.895977	8061.538651	27.272756
236.706428	8069.119913	27.277773
237.316375	8074.714083	27.282791
237.113831	8083.626466	27.287808
237.533887	8089.051313	27.292826
237.860872	8092.141851	27.297844
238.006061	8101.814609	27.302861
238.201858	8118.768994	27.307879
238.483691	8123.394553	27.312896
238.720934	8137.008714	27.317914
239.416024	8153.948539	27.322932
239.382110	8157.950823	27.327949
239.256198	8160.688844	27.332967
239.355222	8175.423190	27.337984
239.459416	8184.319436	27.343002
239.966408	8199.643787	27.348020
240.260349	8217.154401	27.353037
240.692657	8230.681437	27.358055
241.359494	8240.241483	27.363072
241.254167	8244.049698	27.368090
241.103809	8254.077936	27.373108
241.662459	8264.302027	27.378125
241.982166	8281.748708	27.383143
242.278276	8292.139970	27.388160
242.337503	8296.197238	27.393178
242.584436	8300.518886	27.398196
242.643635	8320.929570	27.403213
243.496499	8328.550697	27.408231
243.331503	8348.124974	27.413248
243.484599	8338.775500	27.418266
243.906948	8349.933241	27.423284
243.868518	8367.899846	27.428301
244.245904	8371.206734	27.433319
244.588031	8389.066756	27.438336
244.876233	8392.125499	27.443354
245.033397	8395.441421	27.448372
245.036111	8417.319559	27.453389
245.267400	8417.125937	27.458407
245.384262	8434.143415	27.463424
245.548051	8441.792943	27.468442
245.692525	8451.406012	27.473460
246.325902	8474.957139	27.478477
246.854729	8478.597216	27.483495
246.844347	8492.786893	27.488512
246.898327	8501.981560	27.493530
247.198404	8518.392848	27.498548
246.996567	8529.300600	27.503565
247.663038	8538.349414	27.508583
247.641101	8547.773761	27.513600
247.890026	8570.639796	27.518618
248.173592	8584.051337	27.523636
248.188805	8615.455819	27.528653
248.499921	8624.588414	27.533671
248.916311	8640.182961	27.538688
249.287092	8664.223518	27.543706
249.687073	8677.901142	27.548724
249.575861	8702.903932	27.553741
250.304245	8703.295907	27.558759
250.414357	8723.743308	27.563776
250.759517	8745.208610	27.568794
251.226761	8744.021648	27.573812
251.499200	8762.328561	27.578829
252.356195	8767.556143	27.583847
252.568880	8774.352093	27.588864
252.248525	8778.468563	27.593882
252.663628	8778.426276	27.598900
252.701246	8799.759566	27.603917
253.044478	8803.861129	27.608935
253.160409	8817.819863	27.613952
253.451738	8827.943816	27.618970
253.680147	8829.240799	27.623988
254.114712	8850.966974	27.629005
254.234560	8843.582993	27.634023
254.647367	8860.147520	27.639040
254.470117	8872.260823	27.644058
254.678740	8885.254882	27.649076
254.770001	8908.669965	27.654093
255.184251	8918.920059	27.659111
255.710859	8934.339839	27.664128
255.711713	8951.574753	27.669146
256.187221	8952.110290	27.674164
256.587364	8974.713340	27.679181
256.969584	8976.336829	27.684199
257.070250	8994.023500	27.689216
257.356178	9006.383652	27.694234
257.198400	9009.783446	27.699252
257.708436	9034.983579	27.704269
257.673425	9046.749665	27.709287
258.014157	9063.802325	27.714304
258.391706	9081.850090	27.719322
258.676538	9092.761333	27.724340
258.789913	9112.267821	27.729357
259.271986	9119.201916	27.734375
259.561094	9138.504271	27.739392
259.641563	9145.980791	27.744410
260.195424	9158.384574	27.749428
260.364677	9179.792524	27.754445
260.392276	9178.923400	27.759463
260.797026	9198.334101	27.764480
261.181118	9210.382331	27.769498
261.705267	9220.887001	27.774516
261.829584	9238.456565	27.779533
261.940609	9247.655350	27.784551
262.216687	9250.993957	27.789568
262.263246	9253.165408	27.794586
262.841448	9266.440016	27.799604
262.955334	9275.493138	27.804621
262.922440	9284.739605	27.809639
263.704925	9300.552390	27.814656
263.896214	9301.700483	27.819674
264.069946	9303.864770	27.824692
264.488292	9317.113786	27.829709
264.573148	9326.114624	27.834727
265.217023	9336.727009	27.839744
265.175422	9354.594033	27.844762
265.412309	9355.476140	27.849780
265.404593	9362.189803	27.854797
265.722482	9374.131631	27.859815
265.622903	9392.579174	27.864832
266.004662	9413.600701	27.869850
266.174776	9420.002550	27.874868
266.611461	9439.904216	27.879885
266.917185	9451.516479	27.884903
267.556539	9468.829272	27.889920
267.369463	9484.701604	27.894938
267.798946	9500.784210	27.899956
268.267820	9513.788709	27.904973
268.647267	9522.933211	27.909991
269.338050	9520.821061	27.915008
269.308193	9538.146547	27.920026
269.828800	9536.477644	27.925044
270.087418	9551.598681	27.930061
270.780084	9550.019808	27.935079
270.937322	9550.655430	27.940096
270.695275	9558.940066	27.945114
270.913429	9568.779038	27.950132
271.423367	9578.162146	27.955149
271.598859	9584.541114	27.960167
271.869034	9599.284678	27.965184
271.754015	9607.429583	27.970202
272.570698	9619.685413	27.975220
272.619651	9637.017665	27.980237
272.319618	9639.243121	27.985255
272.753894	9645.117704	27.990272
273.220629	9675.077122	27.995290
273.082633	9690.572588	28.000308
273.330765	9698.149518	28.005325
273.771350	9709.854609	28.010343
274.235897	9725.322599	28.015360
274.296665	9735.110388	28.020378
274.946702	9741.185049	28.025396
275.090341	9769.240569	28.030413
275.308209	9779.660637	28.035431
275.737225	9785.131952	28.040448
275.905847	9804.185390	28.045466
276.566935	9804.897286	28.050484
276.876977	9821.844919	28.055501
277.041283	9842.885002	28.060519
277.447868	9848.400873	28.065536
277.388516	9849.651168	28.070554
277.796831	9854.282730	28.075572
277.968032	9867.539046	28.080589
278.293157	9887.569067	28.085607
278.367529	9886.449516	28.090624
278.679677	9909.916721	28.095642
278.795206	9916.990273	28.100660
278.951969	9924.164757	28.105677
279.549129	9946.378388	28.110695
279.892673	9952.952331	28.115712
279.694587	9968.087978	28.120730
279.940337	9989.453379	28.125748
280.334592	10010.205267	28.130765
280.293599	10033.285582	28.135783
280.915409	10041.379108	28.140800
281.127825	10061.644719	28.145818
281.240251	10067.421151	28.150836
281.767782	10088.856461	28.155853
281.958374	10097.866469	28.160871
282.125419	10108.503018	28.165888
282.404982	10137.958733	28.170906
282.644926	10155.716390	28.175924
282.785942	10176.589980	28.180941
283.116607	10192.205497	28.185959
283.690176	10211.010024	28.190976
284.002148	10226.053842	28.195994
284.201090	10243.890586	28.201012
284.517700	10250.730889	28.206029
284.781306	10270.928769	28.211047
285.312254	10284.476684	28.216064
285.477198	10310.044857	28.221082
285.950863	10315.484120	28.226100
286.084225	10328.080450	28.231117
286.094174	10336.351456	28.236135
286.950431	10355.585725	28.241152
286.984722	10368.361689	28.246170
287.782394	10379.304358	28.251188
288.044509	10388.123401	28.256205
288.326663	10400.402979	28.261223
289.042844	10408.333578	28.266240
288.995423	10420.244546	28.271258
288.998655	10422.217650	28.276276
289.661218	10438.299514	28.281293
289.339078	10448.652473	28.286311
290.325808	10454.693897	28.291328
290.539705	10466.441074	28.296346
290.176247	10468.060809	28.301364
290.643151	10496.480716	28.306381
290.676405	10510.690400	28.311399
291.292212	10519.489172	28.316416
291.256554	10527.606336	28.321434
291.800138	10540.798842	28.326452
292.010043	10553.885436	28.331469
292.189113	10577.809924	28.336487
292.440732	10596.908086	28.341504
292.382195	10616.465019	28.346522
292.653572	10631.865959	28.351540
292.995097	10648.102181	28.356557
293.231795	10664.657850	28.361575
294.394166	10687.295876	28.366592
294.700020	10703.240900	28.371610
295.379923	10700.767213	28.376628
295.784224	10711.142990	28.381645
295.754482	10719.009879	28.386663
296.467787	10722.236479	28.391680
296.744440	10717.874273	28.396698
297.207871	10722.816374	28.401716
297.498751	10732.685688	28.406733
297.338185	10747.601419	28.411751
297.428130	10737.657500	28.416768
298.218590	10745.737710	28.421786
297.745072	10771.405915	28.426804
298.627040	10765.272855	28.431821
298.370570	10776.812444	28.436839
298.883914	10793.255694	28.441856
298.985258	10800.625434	28.446874
298.973771	10818.953320	28.451892
299.167400	10828.143184	28.456909
299.466841	10856.501304	28.461927
299.730700	10872.588783	28.466944
299.746819	10882.248355	28.471962
299.923210	10906.827277	28.476980
300.726497	10926.379817	28.481997
300.758598	10946.115590	28.487015
300.959284	10953.637270	28.492032
301.256655	10975.415711	28.497050
301.526285	10993.264269	28.502068
302.120154	11012.975803	28.507085
302.114184	11035.284635	28.512103
302.351046	11043.170146	28.517120
302.542088	11069.982506	28.522138
302.856679	11095.291645	28.527156
303.572816	11113.282357	28.532173
303.667387	11144.928196	28.537191
304.176792	11149.759057	28.542208
304.302591	11161.634058	28.547226
304.812085	11186.881402	28.552244
305.192567	11205.252840	28.557261
305.389446	11218.253518	28.562279
306.179873	11234.827684	28.567296
306.586872	11249.292338	28.572314
306.739042	11273.206117	28.577332
307.450539	11275.624769	28.582349
307.735875	11288.245450	28.587367
307.866288	11302.266945	28.592384
308.550382	11311.664868	28.597402
308.296949	11333.406334	28.602420
308.835900	11324.213161	28.607437
308.992192	11360.693424	28.612455
309.211623	11359.484894	28.617472
309.549502	11376.208580	28.622490
310.005184	11390.918368	28.627508
310.050769	11397.204511	28.632525
309.823078	11420.224036	28.637543
310.619635	11441.091708	28.642560
311.105684	11451.916176	28.647578
311.244843	11472.257876	28.652596
311.844415	11481.268033	28.657613
311.732514	11506.511509	28.662631
312.038521	11519.204909	28.667648
312.476130	11542.187315	28.672666
312.580333	11561.656748	28.677684
313.055572	11579.524378	28.682701
313.023238	11594.929189	28.687719
313.396484	11624.372665	28.692736
313.764842	11637.425877	28.697754
313.895270	11671.801499	28.702772
314.511194	11679.871400	28.707789
315.091127	11706.084178	28.712807
315.906535	11718.467903	28.717824
316.059888	11732.738757	28.722842
316.411852	11747.698636	28.727860
316.988784	11746.677561	28.732877
316.963765	11765.040055	28.737895
317.352852	11765.608085	28.742912
317.786295	11783.646613	28.747930
318.049042	11803.508419	28.752948
318.458001	11807.881447	28.757965
318.771647	11816.686829	28.762983
319.106458	11823.490144	28.768000
319.261494	11827.965862	28.773018
318.978182	11839.507124	28.778036
319.524524	11861.067849	28.783053
320.175158	11877.190707	28.788071
320.088220	11886.393195	28.793088
320.491749	11911.718011	28.798106
320.331735	11923.347488	28.803124
320.823468	11937.224792	28.808141
321.414683	11964.724494	28.813159
321.799823	11975.991259	28.818176
322.331681	11992.429527	28.823194
322.227278	11995.158444	28.828212
322.327018	12016.700463	28.833229
322.524192	12033.437169	28.838247
322.965930	12050.138973	28.843264
323.401496	12066.317580	28.848282
323.395810	12094.065125	28.853300
324.062628	12102.515680	28.858317
324.388459	12135.879695	28.863335
324.505527	12150.440707	28.868352
324.927506	12160.764017	28.873370
325.082237	12178.514760	28.878388
325.508612	12212.011668	28.883405
325.852143	12226.496432	28.888423
326.252672	12243.902674	28.893440
326.915455	12258.511433	28.898458
326.988236	12285.495513	28.903476
327.476224	12285.445042	28.908493
328.127200	12309.089865	28.913511
328.074461	12314.460100	28.918528
328.371065	12342.148318	28.923546
328.722005	12367.140903	28.928564
329.324085	12377.464713	28.933581
330.071853	12391.169869	28.938599
330.297471	12402.948015	28.943616
330.997561	12418.912070	28.948634
331.007632	12431.450067	28.953652
331.705070	12428.269259	28.958669
332.022813	12434.500748	28.963687
332.396910	12444.512739	28.968704
332.691425	12446.361765	28.973722
332.332482	12466.681041	28.978740
332.991279	12482.010559	28.983757
333.085833	12494.844904	28.988775
333.593524	12505.830816	28.993792
333.919135	12521.218553	28.998810
333.710273	12539.992512	29.003828
334.472998	12560.503562	29.008845
334.507027	12566.959256	29.013863
334.824285	12591.546875	29.018880
335.080325	12595.050253	29.023898
335.426954	12619.680702	29.028916
335.591976	12643.467916	29.033933
335.858922	12666.781415	29.038951
335.876466	12689.473797	29.043968
336.412508	12712.208637	29.048986
336.637647	12732.898302	29.054004
337.258056	12751.878091	29.059021
337.647050	12779.742037	29.064039
338.257280	12808.575758	29.069056
338.502342	12814.736587	29.074074
339.076785	12840.920227	29.079092
339.359017	12862.848475	29.084109
339.373774	12867.731532	29.089127
339.886880	12881.224114	29.094144
340.349661	12912.986128	29.099162
340.569292	12928.182282	29.104180
341.198043	12954.746037	29.109197
341.434357	12968.329141	29.114215
341.576317	12997.273947	29.119232
342.114612	13006.524903	29.124250
342.356009	13025.819759	29.129268
342.715369	13045.822570	29.134285
343.213331	13062.374419	29.139303
343.225031	13076.589400	29.144320
343.838438	13092.239108	29.149338
344.019351	13105.069897	29.154356
344.306021	13114.060086	29.159373
344.567540	13130.446703	29.164391
345.020976	13150.027617	29.169408
345.405848	13147.552186	29.174426
345.605390	13177.192503	29.179444
345.990337	13177.571753	29.184461
346.725913	13187.256290	29.189479
347.248596	13208.664354	29.194496
347.786676	13222.023821	29.199514
347.973910	13223.078057	29.204532
348.773972	13225.236872	29.209549
349.157942	13230.157278	29.214567
349.229819	13241.805148	29.219584
349.393121	13241.811543	29.224602
349.619493	13261.996339	29.229620
349.861564	13270.519866	29.234637
350.183265	13296.572964	29.239655
350.457998	13301.993549	29.244672
350.549043	13320.791065	29.249690
350.748430	13336.590696	29.254708
350.896242	13359.854126	29.259725
351.169232	13376.059172	29.264743
351.599520	13404.208138	29.269760
352.002115	13422.521463	29.274778
352.510190	13452.578389	29.279796
352.895277	13471.156592	29.284813
353.199102	13499.072755	29.289831
353.333456	13530.804835	29.294848
353.786068	13541.348348	29.299866
354.161909	13580.568219	29.304884
354.586544	13595.578257	29.309901
355.221123	13608.648237	29.314919
355.237582	13635.447224	29.319936
355.870719	13652.262760	29.324954
355.999754	13680.477984	29.329972
356.391976	13696.813166	29.334989
356.909886	13714.947767	29.340007
357.195805	13732.344807	29.345024
358.017635	13747.687872	29.350042
358.111212	13777.734055	29.355060
358.401400	13792.604125	29.360077
358.757872	13807.072301	29.365095
358.869742	13847.735954	29.370112
359.704551	13850.435763	29.375130
359.817458	13869.287263	29.380148
359.977983	13897.608437	29.385165
360.792255	13913.928628	29.390183
361.024013	13929.376337	29.395200
361.471505	13960.924593	29.400218
361.652552	13977.810803	29.405236
362.165532	13998.968636	29.410253
362.540307	14015.894195	29.415271
362.891983	14019.373476	29.420288
363.600672	14030.177405	29.425306
363.601869	14056.606720	29.430324
364.179050	14065.665822	29.435341
364.859417	14097.076995	29.440359
365.048437	14101.885870	29.445376
365.590176	14110.173643	29.450394
365.719973	14134.732454	29.455412
365.794444	14141.204496	29.460429
366.392704	14154.893163	29.465447
366.282152	14179.527346	29.470464
366.752544	14193.624385	29.475482
367.077413	14212.967459	29.480500
367.317713	14243.961050	29.485517
367.560189	14270.173091	29.490535
367.706705	14293.911575	29.495552
368.298163	14301.045324	29.500570
368.667661	14322.112166	29.505588
368.866556	14343.227698	29.510605
369.666815	14369.195137	29.515623
370.191713	14391.450554	29.520640
370.340086	14398.173297	29.525658
370.619125	14424.651451	29.530676
370.913976	14443.535199	29.535693
371.570631	14458.478220	29.540711
371.760686	14476.250887	29.545728
372.395950	14485.916973	29.550746
372.802046	14512.767070	29.555764
373.068336	14523.981229	29.560781
373.183927	14543.489861	29.565799
373.780592	14570.281948	29.570816
374.189351	14590.095534	29.575834
374.102264	14619.719568	29.580852
374.600068	14633.531596	29.585869
375.366784	14653.248465	29.590887
375.339349	14673.430064	29.595904
375.987411	14688.851478	29.600922
376.371807	14715.342058	29.605940
376.377499	14743.082241	29.610957
377.157577	14758.407364	29.615975
377.428732	14781.789134	29.620992
377.587516	14808.902378	29.626010
378.338957	14834.303276	29.631028
379.042877	14847.034874	29.636045
379.159597	14860.429518	29.641063
379.418221	14890.856006	29.646080
379.986353	14904.373051	29.651098
380.295807	14922.834970	29.656116
380.437895	14942.144080	29.661133
380.936575	14959.385955	29.666151
381.444000	14987.035749	29.671168
381.628583	15010.623925	29.676186
381.995795	15027.302070	29.681204
382.218579	15052.166562	29.686221
382.740154	15078.130985	29.691239
383.132668	15100.859462	29.696256
383.670261	15125.264478	29.701274
384.289764	15143.785719	29.706292
384.279238	15167.483419	29.711309
385.010282	15185.235689	29.716327
384.871256	15214.442377	29.721344
385.443110	15243.721614	29.726362
385.547446	15262.152631	29.731380
386.341776	15293.680686	29.736397
387.059831	15308.671667	29.741415
386.785534	15344.904513	29.746432
387.516141	15369.128198	29.751450
387.572286	15392.957917	29.756468
387.912696	15415.625400	29.761485
388.673857	15423.383749	29.766503
389.172440	15452.879999	29.771520
389.787254	15470.085307	29.776538
390.507195	15488.196470	29.781556
390.389077	15511.200742	29.786573
391.123314	15520.896165	29.791591
391.113534	15543.533046	29.796608
391.757839	15554.556316	29.801626
392.175690	15576.005484	29.806644
392.167723	15594.157430	29.811661
392.553075	15618.801540	29.816679
392.970778	15648.705466	29.821696
393.307651	15664.731974	29.826714
394.096036	15673.449458	29.831732
394.280950	15699.833499	29.836749
394.728981	15718.015636	29.841767
394.824044	15736.546461	29.846784
395.124968	15745.936781	29.851802
395.381625	15760.598849	29.856820
395.954543	15792.964403	29.861837
396.657470	15807.380167	29.866855
397.010522	15825.826698	29.871872
397.369758	15849.931946	29.876890
397.683170	15862.251277	29.881908
397.989434	15883.288634	29.886925
398.416104	15888.844224	29.891943
398.599021	15918.800916	29.896960
399.114137	15936.312731	29.901978
400.013849	15961.919450	29.906996
399.984461	15990.292249	29.912013
400.542442	15999.339478	29.917031
400.999999	16028.113431	29.922048
401.131923	16045.034388	29.927066
401.450612	16065.697328	29.932084
401.952825	16089.717454	29.937101
402.291455	16112.133374	29.942119
402.799454	16143.470535	29.947136
403.421126	16162.497765	29.952154
403.783391	16176.278324	29.957172
404.283002	16199.076712	29.962189
404.650723	16218.686770	29.967207
405.054407	16242.343423	29.972224
405.384746	16269.763660	29.977242
406.110636	16275.234879	29.982260
406.565329	16296.028497	29.987277
407.582526	16304.347438	29.992295
407.732507	16325.510680	29.997312
407.870214	16339.891665	30.002330
408.451063	16337.584298	30.007348
408.514624	16360.760284	30.012365
409.122792	16376.356673	30.017383
409.799589	16405.785590	30.022400
409.617389	16417.437058	30.027418
410.299246	16420.438999	30.032436
410.669654	16451.438028	30.037453
411.105221	16474.452010	30.042471
411.680101	16494.402791	30.047488
411.499027	16515.816761	30.052506
411.984026	16535.257282	30.057524
412.288590	16566.178312	30.062541
412.847514	16567.828665	30.067559
413.423658	16595.994387	30.072576
414.018118	16618.863786	30.077594
414.262150	16631.355493	30.082612
414.857601	16653.965789	30.087629
415.163918	16667.654342	30.092647
415.812882	16690.982790	30.097664
415.887983	16712.976150	30.102682
416.264226	16729.752288	30.107700
416.407608	16759.406921	30.112717
417.067024	16780.725080	30.117735
417.454721	16801.640222	30.122752
417.632058	16825.626570	30.127770
418.142349	16846.453190	30.132788
418.566381	16871.964626	30.137805
418.986601	16895.660572	30.142823
419.738414	16912.915340	30.147840
419.581742	16940.453414	30.152858
420.182407	16965.545825	30.157876
420.656671	16988.042725	30.162893
421.080954	17013.923853	30.167911
421.351728	17031.326262	30.172928
421.888124	17055.765515	30.177946
422.459322	17068.550849	30.182964
422.665680	17097.176005	30.187981
422.921138	17106.153992	30.192999
423.385038	17131.792223	30.198016
423.880511	17157.387672	30.203034
424.493378	17174.414785	30.208052
424.798035	17197.465807	30.213069
425.122506	17216.515086	30.218087
425.982412	17234.407129	30.223104
425.853074	17258.779722	30.228122
426.362701	17283.981478	30.233140
426.750977	17312.790255	30.238157
427.088339	17327.958957	30.243175
427.572860	17355.303045	30.248192
427.735122	17388.423786	30.253210
428.614360	17413.176511	30.258228
428.985884	17448.027248	30.263245
429.556808	17463.548199	30.268263
430.077297	17494.519228	30.273280
430.117799	17520.043854	30.278298
430.739567	17537.338382	30.283316
431.137008	17554.705751	30.288333
431.818088	17584.739097	30.293351
432.236344	17604.263739	30.298368
432.543464	17636.149458	30.303386
433.085386	17651.314997	30.308404
433.435362	17692.789936	30.313421
433.685544	17705.050806	30.318439
434.383129	17722.270526	30.323456
434.640534	17763.014597	30.328474
434.974635	17776.146858	30.333492
435.568029	17805.145540	30.338509
436.035937	17833.563664	30.343527
436.623013	17849.019239	30.348544
436.771744	17881.315373	30.353562
437.367655	17906.150744	30.358580
437.592599	17941.423179	30.363597
437.854929	17967.176027	30.368615
438.234753	17995.336459	30.373632
438.861478	18029.813699	30.378650
439.149183	18059.340468	30.383668
439.764924	18090.035456	30.388685
440.598086	18124.626026	30.393703
441.283357	18146.345984	30.398720
441.380200	18171.670020	30.403738
442.093170	18195.091405	30.408756
442.497464	18217.259496	30.413773
442.859740	18239.320442	30.418791
443.189215	18261.304393	30.423808
443.690230	18292.661936	30.428826
443.837182	18300.194897	30.433844
444.336426	18337.674342	30.438861
444.561040	18365.897380	30.443879
445.812711	18379.613708	30.448896
446.561754	18408.626969	30.453914
447.162957	18425.085278	30.458932
447.433412	18444.918065	30.463949
447.899480	18452.173977	30.468967
448.398820	18476.601848	30.473984
448.640816	18500.981369	30.479002
449.153009	18500.567045	30.484020
449.507817	18528.574211	30.489037
449.874162	18546.389537	30.494055
450.679522	18567.124701	30.499072
450.609509	18590.017760	30.504090
451.281446	18608.423634	30.509108
451.536480	18625.624613	30.514125
451.683694	18642.090609	30.519143
452.128727	18652.369638	30.524160
452.434927	18677.573297	30.529178
452.942086	18694.545560	30.534196
453.126488	18718.207806	30.539213
453.742111	18752.662794	30.544231
454.201730	18774.993485	30.549248
454.085478	18798.917430	30.554266
454.894120	18817.845532	30.559284
455.443744	18844.350834	30.564301
455.740549	18877.623751	30.569319
456.206712	18904.476960	30.574336
456.656199	18940.644942	30.579354
457.216244	18964.350089	30.584372
457.519518	19004.438916	30.589389
457.861288	19029.359518	30.594407
458.695767	19049.452586	30.599424
458.968798	19080.480474	30.604442
459.710775	19105.269376	30.609460
459.669573	19139.656728	30.614477
460.309598	19181.165510	30.619495
460.871794	19203.594443	30.624512
461.663236	19241.522925	30.629530
462.261020	19255.468031	30.634548
462.660199	19272.925121	30.639565
463.030502	19309.921102	30.644583
463.764856	19318.215904	30.649600
463.823905	19357.755932	30.654618
464.179336	19378.991617	30.659636
464.970768	19411.815698	30.664653
465.228130	19452.733904	30.669671
465.758239	19471.099501	30.674688
466.380564	19498.245108	30.679706
466.751386	19523.484028	30.684724
467.134827	19555.259936	30.689741
467.351758	19583.877643	30.694759
467.959829	19612.061748	30.699776
468.619014	19641.495185	30.704794
468.865854	19663.108201	30.709812
469.739762	19701.043695	30.714829
470.005489	19726.532999	30.719847
470.915724	19752.793865	30.724864
471.255139	19783.761996	30.729882
471.521157	19800.513735	30.734900
472.193046	19832.902251	30.739917
472.427968	19866.338121	30.744935
473.201361	19890.225992	30.749952
473.651096	19915.244643	30.754970
473.967009	19946.854801	30.759988
474.713959	19967.821685	30.765005
474.959923	19990.774603	30.770023
475.315527	20017.716057	30.775040
475.725466	20049.772954	30.780058
476.072326	20079.179859	30.785076
476.741097	20103.235910	30.790093
477.251999	20127.019623	30.795111
477.747027	20161.085211	30.800128
478.205985	20185.711058	30.805146
478.787891	20211.334994	30.810164
479.608562	20237.326148	30.815181
480.022380	20273.236800	30.820199
480.624058	20295.395488	30.825216
480.290428	20315.652763	30.830234
480.801245	20345.205130	30.835252
481.378076	20377.988433	30.840269
481.647686	20409.486504	30.845287
482.192747	20446.988152	30.850304
482.506873	20485.208178	30.855322
482.813261	20521.300280	30.860340
483.739759	20540.060081	30.865357
483.674545	20570.940816	30.870375
484.274604	20593.352819	30.875392
484.697304	20633.420082	30.880410
485.271934	20651.735634	30.885428
485.826671	20689.659557	30.890445
486.069275	20727.518419	30.895463
486.906885	20745.887892	30.900480
486.954252	20789.918543	30.905498
488.039935	20823.558468	30.910516
488.175922	20856.524929	30.915533
488.584100	20891.729952	30.920551
488.971021	20918.351860	30.925568
489.735061	20952.490674	30.930586
490.170504	20990.711754	30.935604
490.868860	21019.250294	30.940621
491.410932	21057.202173	30.945639
492.072730	21084.577618	30.950656
492.794985	21116.859327	30.955674
493.004930	21139.756015	30.960692
494.071048	21161.066230	30.965709
494.372342	21185.913748	30.970727
494.949027	21209.625353	30.975744
495.507549	21246.475647	30.980762
495.807039	21259.906295	30.985780
496.803828	21285.068994	30.990797
497.134928	21313.867325	30.995815
497.795127	21333.743469	31.000832
498.053376	21354.945883	31.005850
498.447578	21374.775020	31.010868
499.236678	21403.097805	31.015885
499.590369	21435.247864	31.020903
500.236519	21451.891292	31.025920
501.017188	21486.357005	31.030938
500.882554	21517.363764	31.035956
502.224847	21529.633944	31.040973
502.226879	21546.251358	31.045991
502.459027	21559.547370	31.051008
503.177112	21589.511639	31.056026
503.585604	21610.412927	31.061044
504.029088	21644.640760	31.066061
504.386559	21667.957390	31.071079
505.135631	21683.201245	31.076096
505.765068	21717.848870	31.081114
506.121009	21738.651061	31.086132
506.490000	21765.990900	31.091149
506.796512	21812.220248	31.096167
507.375824	21832.469646	31.101184
507.641195	21857.917547	31.106202
508.368128	21890.837974	31.111220
508.938009	21920.939553	31.116237
509.602291	21953.775061	31.121255
509.895173	21974.024965	31.126272
510.616549	22009.056859	31.131290
510.529453	22036.019456	31.136308
511.559554	22063.850736	31.141325
511.517407	22104.840057	31.146343
512.161058	22143.308982	31.151360
512.901130	22175.324275	31.156378
513.007067	22210.022669	31.161396
513.738110	22240.775744	31.166413
514.147044	22274.580381	31.171431
514.824456	22306.959488	31.176448
514.990299	22341.238072	31.181466
515.401061	22386.852260	31.186484
516.182119	22421.092076	31.191501
516.671251	22451.693578	31.196519
517.347780	22487.144021	31.201536
517.824570	22517.526390	31.206554
518.155368	22532.829702	31.211572
518.830541	22556.830899	31.216589
519.120483	22589.858436	31.221607
520.147145	22620.363880	31.226624
520.428016	22655.219066	31.231642
520.859103	22675.669332	31.236660
521.319676	22703.286877	31.241677
521.635663	22740.063983	31.246695
522.387651	22774.517458	31.251712
523.281343	22811.596529	31.256730
523.313703	22840.569972	31.261748
523.987403	22865.405863	31.266765
524.802446	22899.603305	31.271783
524.985967	22925.172743	31.276800
525.673242	22953.791642	31.281818
526.153073	22990.587938	31.286836
527.053927	23013.379242	31.291853
527.426097	23055.057979	31.296871
527.786591	23078.432674	31.301888
528.583985	23103.723528	31.306906
529.099402	23136.792702	31.311924
529.139418	23169.784285	31.316941
529.815956	23205.305523	31.321959
530.154988	23252.285129	31.326976
530.750992	23283.098763	31.331994
531.244934	23318.756052	31.337012
531.837217	23351.864170	31.342029
532.672238	23402.438267	31.347047
533.132252	23424.357138	31.352064
533.629749	23468.380552	31.357082
534.057345	23505.748331	31.362100
534.514561	23534.132163	31.367117
534.936970	23569.851592	31.372135
535.352345	23604.181979	31.377152
536.201443	23633.933062	31.382170
536.792663	23685.518976	31.387188
537.612680	23709.018770	31.392205
538.212966	23763.529232	31.397223
538.875212	23784.317485	31.402240
539.416196	23814.413806	31.407258
539.999068	23856.516402	31.412276
540.614651	23868.420929	31.417293
541.028738	23910.505680	31.422311
541.670843	23932.940215	31.427328
542.017822	23971.370406	31.432346
542.529645	24006.116178	31.437364
543.397644	24030.771621	31.442381
544.188637	24056.538630	31.447399
544.910726	24077.520090	31.452416
545.719913	24094.829167	31.457434
545.830554	24125.315234	31.462452
546.390222	24151.586003	31.467469
546.473237	24164.736362	31.472487
546.925996	24195.219831	31.477504
548.329307	24230.408585	31.482522
548.522062	24262.468222	31.487540
548.791003	24285.618456	31.492557
549.502568	24310.500817	31.497575
549.811789	24344.583594	31.502592
550.613864	24363.271627	31.507610
551.012167	24408.190949	31.512628
551.804044	24429.244068	31.517645
552.073216	24457.096068	31.522663
551.977693	24488.853380	31.527680
552.767550	24523.834824	31.532698
553.214093	24567.211383	31.537716
553.880012	24591.064819	31.542733
554.606902	24619.698910	31.547751
554.763555	24643.650647	31.552768
555.617508	24671.165451	31.557786
555.793453	24708.511467	31.562804
556.170531	24734.476499	31.567821
556.757828	24776.422362	31.572839
557.240229	24812.532804	31.577856
558.059927	24840.280675	31.582874
558.374425	24887.034132	31.587892
559.077574	24915.071990	31.592909
559.866992	24952.708448	31.597927
560.605906	24987.407938	31.602944
561.042388	25026.458179	31.607962
561.341492	25057.617797	31.612980
562.076443	25080.494179	31.617997
562.877009	25128.935689	31.623015
563.193916	25155.422520	31.628032
564.115971	25186.845578	31.633050
564.197863	25230.179227	31.638068
565.090424	25266.902835	31.643085
565.677048	25288.342714	31.648103
565.951490	25331.469657	31.653120
566.680495	25370.999561	31.658138
567.446909	25408.741573	31.663156
568.291861	25438.047301	31.668173
568.666177	25479.465341	31.673191
568.902918	25512.088901	31.678208
569.702238	25545.895197	31.683226
569.987820	25578.783010	31.688244
570.502465	25615.338580	31.693261
571.511431	25659.015450	31.698279
571.676731	25703.076544	31.703296
572.519025	25733.438518	31.708314
572.778762	25781.081030	31.713332
573.231788	25807.288419	31.718349
573.768518	25855.538924	31.723367
574.320200	25903.528105	31.728384
575.468614	25932.117413	31.733402
576.483783	25967.306458	31.738420
576.893521	25995.909733	31.743437
577.180626	26029.208836	31.748455
578.062715	26065.948178	31.753472
578.909567	26095.412568	31.758490
579.280088	26134.152917	31.763508
579.880012	26164.306797	31.768525
580.613639	26193.839517	31.773543
580.951477	26234.373682	31.778560
581.303120	26260.186649	31.783578
581.690358	26292.996605	31.788596
582.591319	26322.105307	31.793613
583.142447	26378.558124	31.798631
583.988481	26410.133973	31.803648
584.690394	26433.958721	31.808666
585.052333	26476.568897	31.813684
585.339610	26501.387313	31.818701
586.272508	26529.808783	31.823719
587.015521	26565.534206	31.828736
587.602883	26595.513727	31.833754
588.423512	26619.509815	31.838772
588.881559	26654.654073	31.843789
589.605300	26681.686305	31.848807
589.798649	26716.941399	31.853824
590.152421	26744.973002	31.858842
590.741289	26782.700993	31.863860
591.405638	26823.273992	31.868877
592.140367	26848.541427	31.873895
592.205592	26888.721177	31.878912
592.742329	26922.456902	31.883930
593.455588	26956.304247	31.888948
594.009756	26986.978413	31.893965
594.639490	27011.308053	31.898983
594.857624	27058.871575	31.904000
595.470805	27089.245981	31.909018
595.898342	27130.020786	31.914036
596.515611	27167.264737	31.919053
597.279969	27211.937409	31.924071
597.559670	27263.543094	31.929088
598.366192	27300.372293	31.934106
598.964103	27347.991136	31.939124
599.505153	27380.014158	31.944141
600.316840	27422.853365	31.949159
600.637142	27471.033978	31.954176
601.367962	27508.058629	31.959194
602.015291	27542.789422	31.964212
602.464718	27583.637576	31.969229
603.647642	27625.174312	31.974247
603.851554	27684.017035	31.979264
604.516751	27721.267184	31.984282
605.045617	27756.636184	31.989300
605.684436	27799.819118	31.994317
606.648316	27845.100487	31.999335
606.923279	27901.056983	32.004352
607.923796	27932.370986	32.009370
608.821348	27970.691500	32.014388
609.032371	28011.887331	32.019405
609.807137	28045.726921	32.024423
610.692822	28094.048532	32.029440
611.361608	28124.169334	32.034458
611.759710	28157.290323	32.039476
612.380724	28200.894037	32.044493
613.453279	28234.706546	32.049511
614.287957	28278.087546	32.054528
614.829889	28293.393994	32.059546
615.296345	28320.013387	32.064564
615.996546	28351.785626	32.069581
616.725891	28368.244905	32.074599
617.202061	28411.536627	32.079616
617.672981	28435.254320	32.084634
618.693814	28472.020680	32.089652
618.915823	28503.728545	32.094669
619.703679	28533.812456	32.099687
620.138570	28568.154591	32.104704
620.495132	28608.766434	32.109722
621.365277	28648.306060	32.114740
621.468738	28692.389597	32.119757
622.318317	28718.501100	32.124775
622.407084	28771.347584	32.129792
623.380680	28802.951553	32.134810
624.173872	28854.626711	32.139828
624.717086	28892.776577	32.144845
625.315231	28931.929285	32.149863
626.041551	28977.281759	32.154880
626.775736	29014.643630	32.159898
627.406248	29054.392010	32.164916
627.493679	29103.472362	32.169933
628.359050	29136.294650	32.174951
628.717045	29186.534039	32.179968
629.473213	29230.226367	32.184986
630.086279	29286.835643	32.190004
630.523771	29326.766300	32.195021
631.867461	29362.953053	32.200039
632.028634	29405.929306	32.205056
632.766715	29453.164636	32.210074
633.309651	29485.475118	32.215092
634.110144	29540.677954	32.220109
634.984627	29565.648893	32.225127
635.406439	29598.717961	32.230144
636.011138	29622.681688	32.235162
636.520417	29658.727059	32.240180
637.003582	29696.723426	32.245197
637.573217	29745.275135	32.250215
638.283174	29780.474069	32.255232
638.649759	29823.027314	32.260250
639.608402	29867.511217	32.265268
640.407023	29911.900027	32.270285
640.803413	29959.309815	32.275303
641.425103	30001.324351	32.280320
642.272166	30040.807053	32.285338
642.982223	30074.552622	32.290356
643.332324	30112.703216	32.295373
644.168816	30152.718753	32.300391
644.819529	30198.591391	32.305408
645.401369	30246.415452	32.310426
645.936332	30279.701885	32.315444
646.441830	30333.246057	32.320461
646.854561	30376.792012	32.325479
647.841449	30426.323375	32.330496
648.187778	30474.184627	32.335514
649.205343	30519.103255	32.340532
649.770134	30572.689388	32.345549
650.607494	30615.322695	32.350567
651.266559	30655.278333	32.355584
651.799044	30702.580147	32.360602
652.388559	30747.129737	32.365620
653.114038	30797.379068	32.370637
654.052800	30833.637777	32.375655
654.751111	30879.788983	32.380672
655.136486	30922.215147	32.385690
656.383682	30960.056980	32.390708
656.998390	31001.094828	32.395725
658.332696	31033.208691	32.400743
658.915830	31071.653496	32.405760
659.912596	31100.261050	32.410778
660.769728	31130.514991	32.415796
660.894887	31158.758917	32.420813
661.864298	31182.787796	32.425831
662.395072	31222.397859	32.430848
662.354232	31257.728841	32.435866
663.376004	31299.538349	32.440884
663.625174	31337.631063	32.445901
664.845197	31378.354178	32.450919
664.793689	31425.565235	32.455936
665.625268	31452.814579	32.460954
665.809544	31500.362071	32.465972
666.248993	31555.455830	32.470989
667.208967	31595.834240	32.476007
667.938348	31650.427963	32.481024
668.401760	31688.551186	32.486042
668.793710	31734.214654	32.491060
669.625006	31795.158767	32.496077
670.485526	31850.959002	32.501095
670.941635	31899.830570	32.506112
671.401333	31954.852698	32.511130
672.350321	31998.773751	32.516148
672.794358	32055.897389	32.521165
673.713126	32105.689930	32.526183
674.302552	32157.430383	32.531200
674.720200	32212.756862	32.536218
675.771801	32259.083728	32.541236
676.564959	32319.858308	32.546253
676.997664	32365.282911	32.551271
678.084922	32413.387323	32.556288
678.788187	32458.833230	32.561306
679.727430	32488.362005	32.566324
680.488552	32520.832929	32.571341
681.387735	32556.139897	32.576359
682.224960	32594.162336	32.581376
682.386790	32629.900308	32.586394
682.597295	32659.839899	32.591412
683.612817	32703.619325	32.596429
684.048491	32737.121146	32.601447
685.078086	32784.577913	32.606464
685.450797	32819.360378	32.611482
686.079356	32858.673851	32.616500
686.892809	32907.745037	32.621517
687.974151	32957.046481	32.626535
688.038652	32999.185450	32.631552
688.578861	33057.036536	32.636570
689.122067	33097.293084	32.641588
689.735683	33151.902446	32.646605
690.859934	33191.069839	32.651623
691.473031	33248.448598	32.656640
692.169656	33292.658228	32.661658
692.886870	33340.398806	32.666676
693.719819	33396.099997	32.671693
694.701920	33437.635491	32.676711
695.290839	33482.785322	32.681728
695.749571	33531.262010	32.686746
696.823918	33574.882376	32.691764
697.390277	33626.048422	32.696781
698.427071	33673.006635	32.701799
698.741455	33720.469389	32.706816
699.577822	33763.798440	32.711834
699.942759	33806.878533	32.716852
700.619288	33859.102780	32.721869
701.414073	33905.656630	32.726887
701.914912	33956.353188	32.731904
702.388519	34014.229931	32.736922
703.110323	34073.503364	32.741940
703.915170	34121.447039	32.746957
705.180768	34169.110460	32.751975
706.483514	34213.853594	32.756992
707.107026	34262.110326	32.762010
708.013495	34291.261091	32.767028
708.533969	34338.402329	32.772045
709.525539	34377.915043	32.777063
710.239268	34413.842006	32.782080
710.783131	34458.065231	32.787098
711.720069	34499.394898	32.792116
712.082386	34538.734004	32.797133
712.553437	34584.581059	32.802151
713.439898	34618.976733	32.807168
714.020971	34667.468611	32.812186
714.803533	34720.095778	32.817204
715.348209	34765.299512	32.822221
715.865788	34805.803585	32.827239
716.575702	34853.706805	32.832256
717.359345	34910.210010	32.837274
717.796500	34964.118136	32.842292
718.642082	34998.640924	32.847309
719.745332	35047.046065	32.852327
720.221357	35093.298099	32.857344
721.038216	35139.718470	32.862362
721.917113	35183.303055	32.867380
722.749048	35242.145339	32.872397
723.308620	35289.415394	32.877415
724.233339	35325.209904	32.882432
724.896179	35373.172214	32.887450
725.579012	35404.799906	32.892468
726.447243	35455.139388	32.897485
726.998160	35507.703415	32.902503
727.630853	35540.312821	32.907520
728.018239	35588.476567	32.912538
728.516486	35623.863764	32.917556
729.467633	35676.068734	32.922573
729.826633	35712.653799	32.927591
730.616688	35757.302987	32.932608
731.087107	35819.554255	32.937626
731.627045	35861.858884	32.942644
732.546336	35919.336359	32.947661
732.986242	35978.134227	32.952679
734.040790	36024.361466	32.957696
734.830014	36093.063864	32.962714
735.375205	36138.643506	32.967732
736.283385	36198.602063	32.972749
736.749053	36260.494955	32.977767
738.106392	36309.552638	32.982784
738.194702	36375.058131	32.987802
738.909254	36419.012287	32.992820
739.954023	36484.002488	32.997837
740.548616	36533.565131	33.002855
741.714923	36592.833343	33.007872
742.291249	36661.741443	33.012890
743.237564	36707.841588	33.017908
743.932876	36761.075458	33.022925
744.946717	36815.315842	33.027943
745.820910	36862.938783	33.032960
746.565529	36922.488544	33.037978
747.083650	36968.099469	33.042996
748.095800	37017.585591	33.048013
748.828191	37074.519872	33.053031
749.443546	37126.470841	33.058048
749.817263	37177.985308	33.063066
750.754512	37236.272923	33.068084
751.605697	37294.706884	33.073101
752.219132	37350.515903	33.078119
753.407104	37393.683840	33.083136
753.676054	37463.837485	33.088154
754.962701	37509.184493	33.093172
755.686623	37558.602918	33.098189
756.273113	37615.871199	33.103207
757.793411	37663.926513	33.108224
758.384571	37725.627063	33.113242
759.180243	37775.186581	33.118260
759.962990	37802.015451	33.123277
760.816552	37866.097435	33.128295
761.448020	37902.239141	33.133312
762.457775	37961.826406	33.138330
763.358402	38001.461209	33.143348
764.164915	38035.400609	33.148365
764.683514	38076.713839	33.153383
765.790331	38120.231024	33.158400
766.035157	38172.880890	33.163418
767.129477	38203.139713	33.168436
767.793564	38249.767711	33.173453
768.473789	38298.954351	33.178471
769.705449	38325.897381	33.183488
770.006091	38380.878796	33.188506
771.191774	38422.822388	33.193524
771.789322	38470.112556	33.198541
772.391380	38507.524588	33.203559
773.031708	38543.653350	33.208576
773.597063	38586.534873	33.213594
774.458815	38639.949865	33.218612
775.004810	38690.600096	33.223629
775.373527	38750.498022	33.228647
776.382339	38804.377455	33.233664
776.986470	38859.173726	33.238682
777.743307	38915.173175	33.243700
778.399708	38968.216227	33.248717
779.066854	39014.826437	33.253735
779.853272	39060.273570	33.258752
780.285472	39119.656733	33.263770
781.207549	39166.012575	33.268788
781.910090	39216.247593	33.273805
782.405113	39277.714606	33.278823
783.995246	39334.015449	33.283840
784.543342	39387.398909	33.288858
785.343893	39439.889472	33.293876
786.231417	39499.923728	33.298893
786.638531	39556.611675	33.303911
787.743829	39599.980317	33.308928
787.960291	39665.551782	33.313946
788.756506	39724.595361	33.318964
789.567584	39787.892852	33.323981
790.187021	39854.306492	33.328999
791.155203	39919.932457	33.334016
792.305308	39985.985634	33.339034
793.025767	40047.773888	33.344052
794.036711	40107.038047	33.349069
794.572910	40162.341475	33.354087
795.506572	40219.638518	33.359104
796.324361	40281.184617	33.364122
797.132820	40336.022386	33.369140
797.998481	40392.584219	33.374157
798.466139	40467.580001	33.379175
799.746921	40526.974055	33.384192
800.473091	40583.418966	33.389210
801.265967	40654.405785	33.394228
802.494915	40709.982223	33.399245
803.214757	40767.061024	33.404263
803.929093	40820.966022	33.409280
804.651525	40881.478826	33.414298
805.421516	40941.497419	33.419316
806.660216	41000.418667	33.424333
807.233327	41062.397174	33.429351
808.352216	41123.550942	33.434368
808.996228	41179.219634	33.439386
809.896346	41232.780509	33.444404
810.903964	41284.680424	33.449421
811.747745	41338.674067	33.454439
812.952614	41379.317569	33.459456
813.935941	41420.476295	33.464474
814.871635	41464.868012	33.469492
816.029909	41519.167318	33.474509
816.539733	41561.968502	33.479527
817.312159	41606.891886	33.484544
817.876799	41655.338866	33.489562
818.371503	41706.883232	33.494580
819.935438	41748.641575	33.499597
820.756946	41778.871982	33.504615
822.099304	41829.392919	33.509632
822.337199	41868.530809	33.514650
823.104652	41898.067762	33.519668
824.362048	41934.017570	33.524685
824.883310	41997.429844	33.529703
825.482664	42038.434468	33.534720
826.002767	42088.685547	33.539738
826.877843	42140.443684	33.544756
827.513637	42184.282700	33.549773
827.981035	42247.476391	33.554791
828.942027	42291.302947	33.559808
829.613004	42353.832779	33.564826
830.059891	42413.753914	33.569844
830.967184	42466.924557	33.574861
831.723499	42534.722825	33.579879
832.573750	42584.563130	33.584896
833.128820	42647.510304	33.589914
833.573096	42710.519179	33.594932
834.736678	42758.299796	33.599949
835.531658	42818.484090	33.604967
836.142682	42873.637254	33.609984
836.757309	42936.215462	33.615002
837.710040	43003.535527	33.620020
838.639471	43052.080601	33.625037
839.317317	43126.319067	33.630055
840.285108	43198.817547	33.635072
840.963656	43272.955197	33.640090
841.593716	43331.370255	33.645108
842.443297	43398.555781	33.650125
843.366258	43476.432129	33.655143
844.289317	43537.344806	33.660160
845.027991	43597.514689	33.665178
846.031908	43678.263400	33.670196
847.326095	43745.893108	33.675213
847.714796	43815.156719	33.680231
848.707660	43875.882356	33.685248
849.538238	43948.872719	33.690266
850.455445	44031.015111	33.695284
851.330178	44084.972726	33.700301
852.366571	44156.331443	33.705319
853.485295	44220.492036	33.710336
853.995577	44298.713826	33.715354
855.088411	44365.630382	33.720372
856.350817	44422.090232	33.725389
857.058495	44505.196822	33.730407
857.856046	44563.867371	33.735424
858.934098	44613.929807	33.740442
860.110298	44686.255227	33.745460
861.258468	44750.982057	33.750477
861.770832	44805.725258	33.755495
862.729161	44863.391124	33.760512
863.803128	44927.269752	33.765530
864.188159	44982.001579	33.770548
865.563885	45032.644846	33.775565
866.140991	45107.645708	33.780583
867.238264	45166.252212	33.785600
867.684761	45227.566313	33.790618
868.655692	45295.795061	33.795636
869.793506	45354.231282	33.800653
870.543661	45420.464254	33.805671
871.349005	45476.567785	33.810688
872.258087	45545.053622	33.815706
873.276475	45607.905440	33.820724
874.651600	45653.856552	33.825741
875.414250	45710.625189	33.830759
876.362296	45760.596576	33.835776
877.079091	45807.548736	33.840794
878.010737	45880.441133	33.845812
878.653043	45929.239616	33.850829
879.405533	45981.405354	33.855847
880.488005	46047.822507	33.860864
881.445321	46108.129608	33.865882
882.014892	46170.331725	33.870900
882.884398	46223.416036	33.875917
884.147108	46297.270391	33.880935
885.175329	46343.593215	33.885952
885.781053	46401.925224	33.890970
886.250588	46459.848420	33.895988
887.297964	46521.667162	33.901005
888.460906	46588.585791	33.906023
889.384643	46645.565779	33.911040
889.989026	46704.885635	33.916058
890.506601	46761.840578	33.921076
891.307465	46814.165196	33.926093
892.356684	46874.074160	33.931111
892.948136	46937.331441	33.936128
893.864809	46986.968835	33.941146
894.355583	47054.518545	33.946164
895.215041	47114.470338	33.951181
896.317983	47172.397985	33.956199
897.195533	47236.630077	33.961216
898.373351	47291.560433	33.966234
899.010921	47369.330293	33.971252
900.246497	47429.679861	33.976269
901.538269	47484.795388	33.981287
902.800525	47517.204483	33.986304
904.019261	47569.111537	33.991322
904.920813	47621.125020	33.996340
905.746073	47675.554481	34.001357
906.661026	47733.487526	34.006375
907.597726	47780.207130	34.011392
908.271589	47826.765302	34.016410
908.912381	47896.868985	34.021428
910.047143	47943.380958	34.026445
910.699675	48001.203704	34.031463
911.054490	48067.506004	34.036480
912.029399	48129.941438	34.041498
912.785146	48197.371068	34.046516
913.613055	48268.085738	34.051533
914.444158	48341.027043	34.056551
915.544847	48412.288060	34.061568
916.477420	48483.271798	34.066586
916.918598	48555.458369	34.071604
917.506816	48629.210241	34.076621
919.490350	48703.510665	34.081639
920.162621	48771.840710	34.086656
921.140255	48853.017027	34.091674
921.868774	48931.511965	34.096692
923.129802	49000.636775	34.101709
924.176991	49085.181516	34.106727
924.640979	49158.695044	34.111744
925.803223	49233.485663	34.116762
926.368046	49303.732037	34.121780
927.526655	49378.498390	34.126797
928.551675	49450.622216	34.131815
929.708053	49525.572873	34.136832
930.729960	49594.907528	34.141850
931.503959	49668.589548	34.146868
932.646419	49734.400800	34.151885
933.394672	49811.389898	34.156903
934.471897	49883.317155	34.161920
935.142660	49956.491039	34.166938
935.757439	50035.336466	34.171956
937.361374	50101.842497	34.176973
938.049669	50184.732563	34.181991
938.861298	50253.798248	34.187008
939.995416	50328.634784	34.192026
940.632374	50404.902937	34.197044
942.095230	50477.335131	34.202061
943.097842	50543.645002	34.207079
944.029971	50617.077676	34.212096
945.250693	50680.595382	34.217114
946.312607	50749.705848	34.222132
947.827456	50803.029411	34.227149
949.054228	50865.255950	34.232167
949.952814	50921.042070	34.237184
950.841364	50971.945303	34.242202
951.241740	51027.771270	34.247220
952.331106	51087.666082	34.252237
953.012753	51162.442890	34.257255
953.572154	51230.354918	34.262272
954.690554	51289.454828	34.267290
955.603982	51342.727731	34.272308
956.799379	51389.895317	34.277325
957.573169	51446.562645	34.282343
958.179143	51505.287306	34.287360
959.128901	51558.245013	34.292378
960.041512	51618.788795	34.297396
960.823352	51685.636175	34.302413
961.949566	51754.587783	34.307431
962.464888	51819.458596	34.312448
963.440076	51882.290177	34.317466
964.501955	51962.002721	34.322484
965.540079	52032.848121	34.327501
966.516423	52090.814264	34.332519
967.382087	52172.146270	34.337536
968.328540	52237.830666	34.342554
969.095300	52319.412701	34.347572
969.709658	52397.601859	34.352589
970.953839	52474.358118	34.357607
971.450985	52554.970533	34.362624
972.924499	52631.090488	34.367642
974.119501	52722.737817	34.372660
974.751906	52804.038735	34.377677
975.660133	52879.526140	34.382695
976.415040	52965.073420	34.387712
977.834741	53043.430457	34.392730
978.971250	53132.886446	34.397748
979.506135	53209.091118	34.402765
980.654697	53292.971063	34.407783
981.704845	53378.689044	34.412800
982.852684	53456.722771	34.417818
983.898993	53549.712683	34.422836
985.014320	53633.390201	34.427853
986.104739	53707.061119	34.432871
987.102261	53787.884650	34.437888
988.279330	53857.461029	34.442906
989.486942	53940.011555	34.447924
990.026929	54025.874594	34.452941
991.289695	54097.583541	34.457959
992.093607	54182.108822	34.462976
993.285629	54254.556985	34.467994
994.517383	54340.547630	34.473012
995.299125	54411.750227	34.478029
996.695871	54496.690606	34.483047
997.755126	54564.369992	34.488064
998.864304	54625.637694	34.493082
999.972500	54700.504983	34.498100
1001.317817	54764.381472	34.503117
1002.592136	54829.060214	34.508135
1003.437043	54895.407020	34.513152
1004.660248	54961.600203	34.518170
1005.520296	55022.654586	34.523188
1006.358993	55079.921804	34.528205
1007.353637	55150.783405	34.533223
1007.840656	55226.445169	34.538240
1008.593787	55298.148503	34.543258
1009.812761	55371.576797	34.548276
1010.927136	55447.559286	34.553293
1012.143482	55512.065398	34.558311
1012.772184	55582.947285	34.563328
1013.566767	55660.910406	34.568346
1014.379639	55745.787951	34.573364
1014.989107	55828.457175	34.578381
1016.594701	55902.858478	34.583399
1017.494019	55998.285755	34.588416
1018.229222	56075.354497	34.593434
1019.240290	56151.380634	34.598452
1020.107599	56236.795715	34.603469
1021.296122	56308.409012	34.608487
1022.108341	56386.479352	34.613504
1023.270712	56461.337443	34.618522
1024.359732	56534.795891	34.623540
1025.403036	56599.376193	34.628557
1026.483313	56671.830162	34.633575
1027.502692	56749.837802	34.638592
1028.575417	56824.932494	34.643610
1030.204591	56890.289427	34.648628
1030.921431	56959.832649	34.653645
1031.799200	57026.154975	34.658663
1032.688105	57109.399037	34.663680
1033.903874	57180.067714	34.668698
1034.505611	57258.521754	34.673716
1035.412077	57333.365452	34.678733
1036.712581	57406.837965	34.683751
1037.644339	57499.582733	34.688768
1038.811829	57567.405720	34.693786
1039.764387	57644.407716	34.698804
1040.600010	57735.681052	34.703821
1041.809602	57813.206860	34.708839
1042.707285	57906.977477	34.713856
1043.957279	57985.541843	34.718874
1045.341766	58072.022201	34.723892
1046.198700	58155.603978	34.728909
1047.051345	58243.895584	34.733927
1048.271417	58332.408803	34.738944
1049.150782	58415.076591	34.743962
1050.236313	58495.807483	34.748980
1051.087888	58578.094074	34.753997
1052.374999	58660.908098	34.759015
1053.458616	58762.729208	34.764032
1054.794601	58843.858998	34.769050
1055.826552	58938.365908	34.774068
1056.715503	59023.464739	34.779085
1058.253525	59103.646198	34.784103
1058.983541	59186.668998	34.789120
1060.083402	59266.412849	34.794138
1061.269583	59356.985819	34.799156
1062.267145	59441.961613	34.804173
1063.694826	59523.281948	34.809191
1064.706236	59609.009377	34.814208
1065.773024	59693.380304	34.819226
1066.840760	59772.421914	34.824244
1067.950663	59861.027495	34.829261
1069.191609	59939.928755	34.834279
1069.817780	60037.788155	34.839296
1070.981976	60123.784777	34.844314
1072.338599	60214.271113	34.849332
1073.136885	60298.679601	34.854349
1074.649204	60380.571957	34.859367
1075.492928	60457.675797	34.864384
1076.649251	60547.859075	34.869402
1077.704025	60622.367043	34.874420
1078.916018	60716.232519	34.879437
1080.295097	60788.190254	34.884455
1081.290261	60864.809731	34.889472
1082.584294	60935.477196	34.894490
1083.281936	61011.940890	34.899508
1084.430893	61084.650590	34.904525
1085.487904	61161.229717	34.909543
1086.579897	61249.691205	34.914560
1087.645902	61325.104741	34.919578
1088.767399	61399.376810	34.924596
1089.698306	61488.307328	34.929613
1090.721666	61568.070608	34.934631
1091.672416	61648.775961	34.939648
1092.947189	61724.936819	34.944666
1094.729481	61789.656476	34.949684
1096.227975	61843.108657	34.954701
1097.254653	61891.753908	34.959719
1098.283953	61948.950796	34.964736
1099.725102	62011.616221	34.969754
1100.743323	62060.845493	34.974772
1101.170264	62119.320270	34.979789
1102.153728	62184.665391	34.984807
1103.099144	62251.168698	34.989824
1103.756846	62319.793269	34.994842
1104.617249	62388.348497	34.999860
1105.533795	62471.264777	35.004877
1106.759555	62548.714516	35.009895
1107.732078	62632.553168	35.014912
1109.181697	62703.404064	35.019930
1110.551414	62780.300377	35.024948
1111.475506	62858.519696	35.029965
1112.677090	62946.489108	35.034983
1113.651920	63029.651399	35.040000
1114.769732	63113.317134	35.045018
1115.653592	63197.089202	35.050036
1116.780530	63274.588244	35.055053
1118.111160	63353.948625	35.060071
1119.060345	63450.980001	35.065088
1119.947627	63539.576509	35.070106
1120.921973	63628.951095	35.075124
1122.094085	63725.151193	35.080141
1123.171796	63803.393887	35.085159
1123.548637	63906.169315	35.090176
1125.092627	64014.676284	35.095194
1126.455750	64104.555483	35.100212
1127.282881	64212.719089	35.105229
1128.523462	64314.652714	35.110247
1130.349143	64400.510627	35.115264
1131.278092	64500.657611	35.120282
1132.804929	64592.330001	35.125300
1133.787435	64687.917580	35.130317
1134.968521	64771.496726	35.135335
1136.676885	64858.178483	35.140352
1137.755206	64939.241853	35.145370
1139.173345	65025.247645	35.150388
1140.354764	65123.306614	35.155405
1141.356839	65201.375523	35.160423
1142.399263	65283.198969	35.165440
1143.165825	65366.160876	35.170458
1144.528028	65456.842766	35.175476
1145.698761	65555.658468	35.180493
1146.584692	65644.192984	35.185511
1147.747436	65736.609974	35.190528
1148.836634	65828.785506	35.195546
1150.456616	65918.415960	35.200564
1151.099418	66002.950341	35.205581
1152.254482	66106.044138	35.210599
1153.508844	66205.729393	35.215616
1154.736242	66298.176358	35.220634
1155.832186	66370.909744	35.225652
1157.164626	66471.748836	35.230669
1158.011794	66563.806437	35.235687
1159.121056	66658.628331	35.240704
1160.368232	66761.140639	35.245722
1162.146602	66843.120493	35.250740
1162.950092	66931.666010	35.255757
1164.215381	67017.392139	35.260775
1165.593961	67096.731548	35.265792
1166.660660	67196.190316	35.270810
1167.806749	67279.074083	35.275828
1168.853427	67364.740439	35.280845
1170.324685	67456.995375	35.285863
1171.442964	67534.787464	35.290880
1172.410003	67618.187729	35.295898
1173.650763	67681.569669	35.300916
1174.442754	67762.616996	35.305933
1175.567554	67845.512248	35.310951
1176.508663	67930.829703	35.315968
1177.768755	68024.544166	35.320986
1178.924228	68101.287474	35.326004
1180.081432	68196.557168	35.331021
1180.996224	68269.919348	35.336039
1182.519697	68360.485190	35.341056
1183.344733	68457.390481	35.346074
1184.923632	68543.579454	35.351092
1185.830725	68629.366744	35.356109
1186.948534	68730.685057	35.361127
1187.956684	68815.190878	35.366144
1189.011590	68922.110725	35.371162
1190.498497	69010.955959	35.376180
1191.355194	69113.988033	35.381197
1192.179746	69222.711577	35.386215
1193.621830	69325.406432	35.391232
1194.637244	69437.254473	35.396250
1196.276890	69532.276721	35.401268
1197.388965	69637.860914	35.406285
1198.439927	69745.449643	35.411303
1200.094889	69848.689656	35.416320
1201.073082	69945.842640	35.421338
1202.175932	70055.279879	35.426356
1203.477769	70171.424004	35.431373
1204.681686	70285.183998	35.436391
1206.252181	70379.909840	35.441408
1206.974311	70488.901589	35.446426
1208.709519	70588.237738	35.451444
1209.954233	70700.201170	35.456461
1211.319472	70799.975650	35.461479
1212.608014	70898.014729	35.466496
1213.562287	71009.087512	35.471514
1215.028237	71105.744635	35.476532
1216.508559	71212.898988	35.481549
1217.580788	71311.783836	35.486567
1218.675030	71411.045578	35.491584
1219.573196	71516.303401	35.496602
1221.233804	71622.836117	35.501620
1222.768381	71728.894947	35.506637
1224.261601	71828.906732	35.511655
1225.582001	71922.017969	35.516672
1226.148715	72023.048601	35.521690
1227.598040	72113.493427	35.526708
1228.884992	72219.238154	35.531725
1230.194227	72322.244128	35.536743
1231.346103	72419.740230	35.541760
1232.328845	72524.064349	35.546778
1233.714207	72620.549614	35.551796
1235.070706	72722.625215	35.556813
1236.048971	72825.165383	35.561831
1237.834280	72923.957964	35.566848
1239.146221	73020.810756	35.571866
1240.584654	73122.026548	35.576884
1241.478885	73216.829902	35.581901
1242.787121	73309.073992	35.586919
1243.987974	73410.492521	35.591936
1245.215804	73515.301698	35.596954
1247.024191	73591.383240	35.601972
1248.487858	73684.491057	35.606989
1250.106072	73754.320346	35.612007
1251.611045	73833.831635	35.617024
1252.513168	73917.262155	35.622042
1254.042577	73988.891801	35.627060
1255.005544	74066.182916	35.632077
1256.378889	74141.333124	35.637095
1257.520631	74205.955962	35.642112
1258.434835	74279.075432	35.647130
1259.546698	74346.578502	35.652148
1260.472548	74426.169036	35.657165
1261.298562	74519.645019	35.662183
1262.331391	74593.937525	35.667200
1263.334777	74679.710619	35.672218
1264.448362	74775.726690	35.677236
1265.543996	74880.498479	35.682253
1266.461282	74982.448454	35.687271
1268.038633	75077.392759	35.692288
1268.979265	75184.406521	35.697306
1270.127652	75292.794380	35.702324
1271.598403	75401.398501	35.707341
1272.925040	75516.738917	35.712359
1274.165737	75619.464313	35.717376
1275.564737	75725.914874	35.722394
1276.885640	75832.517349	35.727412
1278.297741	75940.828767	35.732429
1279.291684	76050.827094	35.737447
1280.420631	76165.453697	35.742464
1281.601824	76280.363999	35.747482
1283.432064	76384.545941	35.752500
1285.521179	76487.940621	35.757517
1287.023007	76598.001460	35.762535
1288.075528	76698.720806	35.767552
1289.340521	76810.820820	35.772570
1290.595268	76907.215200	35.777588
1291.749567	77009.642636	35.782605
1293.009579	77127.875823	35.787623
1294.237092	77229.203276	35.792640
1295.262529	77351.400914	35.797658
1296.712824	77454.303326	35.802676
1297.901390	77571.054762	35.807693
1298.606383	77677.519664	35.812711
1300.386650	77799.183777	35.817728
1301.554097	77917.688151	35.822746
1302.888463	78031.353213	35.827764
1304.652013	78149.018393	35.832781
1306.527449	78247.322451	35.837799
1307.954865	78351.308590	35.842816
1309.465486	78456.637671	35.847834
1310.190635	78571.603278	35.852852
1311.992424	78674.151528	35.857869
1313.536038	78788.585261	35.862887
1314.668287	78887.957419	35.867904
1315.652837	78994.269900	35.872922
1317.008562	79097.319885	35.877940
1318.547958	79208.626900	35.882957
1319.872930	79317.598710	35.887975
1321.563817	79416.176377	35.892992
1322.303640	79517.841566	35.898010
1324.054422	79617.411455	35.903028
1325.212109	79722.952335	35.908045
1326.703854	79848.623084	35.913063
1327.985725	79938.258727	35.918080
1329.217288	80054.785966	35.923098
1330.511856	80149.247181	35.928116
1331.802424	80253.451822	35.933133
1332.441028	80368.324344	35.938151
1334.452097	80480.082483	35.943168
1335.857456	80577.277109	35.948186
1336.870873	80681.273107	35.953204
1338.641861	80788.559610	35.958221
1339.905751	80897.065695	35.963239
1340.688428	80995.106188	35.968256
1342.091940	81100.398650	35.973274
1343.331228	81204.678174	35.978292
1344.844202	81302.403362	35.983309
1345.854259	81405.883128	35.988327
1347.625669	81500.844829	35.993344
1348.721041	81600.194415	35.998362
1350.277432	81683.192056	36.003380
1351.496355	81789.922175	36.008397
1352.462651	81897.325509	36.013415
1353.862282	81990.712335	36.018432
1355.272610	82095.931455	36.023450
1356.392990	82194.088280	36.028468
1358.221580	82297.367905	36.033485
1358.916384	82416.041054	36.038503
1360.317024	82520.008934	36.043520
1361.413891	82646.703965	36.048538
1362.989730	82765.621552	36.053556
1364.322403	82874.897445	36.058573
1365.450249	83003.945912	36.063591
1366.868538	83127.919639	36.068608
1367.722499	83255.276044	36.073626
1369.319070	83365.615075	36.078644
1371.163531	83492.602975	36.083661
1372.113094	83618.577714	36.088679
1373.275444	83739.096874	36.093696
1375.321374	83875.570744	36.098714
1376.860346	84002.025615	36.103732
1378.460012	84117.105923	36.108749
1379.541061	84248.473392	36.113767
1381.061622	84370.409277	36.118784
1382.283837	84495.965320	36.123802
1383.925632	84622.204194	36.128820
1385.791271	84736.016507	36.133837
1387.270531	84859.988269	36.138855
1388.342375	84974.495279	36.143872
1390.127320	85095.784882	36.148890
1391.476584	85217.979111	36.153908
1393.332969	85333.189068	36.158925
1394.389082	85439.970887	36.163943
1396.041371	85548.877801	36.168960
1397.425674	85666.646162	36.173978
1399.009727	85789.566555	36.178996
1400.607760	85898.356517	36.184013
1401.305894	86015.865626	36.189031
1403.202433	86126.016530	36.194048
1404.243018	86245.412029	36.199066
1405.797093	86361.534815	36.204084
1408.089317	86464.681301	36.209101
1409.450016	86585.827770	36.214119
1410.894839	86684.126896	36.219136
1412.166266	86792.742954	36.224154
1413.661651	86899.537809	36.229172
1415.069817	87003.482753	36.234189
1415.957968	87114.237877	36.239207
1417.715873	87217.634936	36.244224
1419.013440	87326.261584	36.249242
1420.569206	87445.277682	36.254260
1421.964261	87557.856421	36.259277
1423.013701	87666.649675	36.264295
1424.681430	87782.266208	36.269312
1426.235229	87891.070499	36.274330
1427.140435	88009.239714	36.279348
1428.700037	88124.164765	36.284365
1430.037360	88250.935691	36.289383
1430.710328	88362.907571	36.294400
1432.360073	88483.129818	36.299418
1433.741040	88611.973822	36.304436
1435.426188	88727.882831	36.309453
1437.015017	88837.559589	36.314471
1438.649701	88951.766502	36.319488
1440.308112	89038.824791	36.324506
1441.441832	89139.765839	36.329524
1443.290036	89238.200829	36.334541
1444.322641	89346.812807	36.339559
1445.409951	89445.265530	36.344576
1447.041283	89558.550169	36.349594
1447.680325	89675.069269	36.354612
1449.327959	89779.088121	36.359629
1450.531531	89909.143982	36.364647
1451.494749	90017.667821	36.369664
1452.923037	90144.483381	36.374682
1454.285107	90278.191459	36.379700
1455.838392	90410.501635	36.384717
1456.886270	90548.682871	36.389735
1458.473073	90665.349807	36.394752
1460.531549	90804.414160	36.399770
1462.719893	90918.960671	36.404788
1464.480068	91036.349815	36.409805
1465.663256	91170.254472	36.414823
1467.132438	91293.164995	36.419840
1469.140594	91405.751613	36.424858
1470.378984	91527.697776	36.429876
1472.190075	91636.171545	36.434893
1474.062309	91763.076931	36.439911
1475.728792	91888.532005	36.444928
1477.187380	91993.944094	36.449946
1478.585254	92100.836207	36.454964
1479.630919	92214.779699	36.459981
1481.185470	92348.416314	36.464999
1482.395025	92469.927162	36.470016
1484.148769	92590.175074	36.475034
1485.111289	92708.632772	36.480052
1486.760609	92835.374552	36.485069
1488.123423	92965.913121	36.490087
1489.459304	93096.393067	36.495104
1490.887647	93226.681735	36.500122
1492.188426	93363.961908	36.505140
1493.757066	93481.276261	36.510157
1495.387643	93624.070493	36.515175
1496.999640	93755.714383	36.520192
1498.641054	93882.068812	36.525210
1499.742862	94022.919211	36.530228
1501.757469	94148.735000	36.535245
1503.122130	94292.625757	36.540263
1504.585882	94421.785902	36.545280
1506.009090	94559.546692	36.550298
1507.370097	94700.017611	36.555316
1509.020129	94827.870258	36.560333
1510.522979	94976.901552	36.565351
1512.197717	95103.737463	36.570368
1513.597429	95231.630738	36.575386
1515.268128	95373.070545	36.580404
1517.004953	95501.419484	36.585421
1518.627702	95633.500673	36.590439
1520.130103	95763.725151	36.595456
1522.097728	95893.712978	36.600474
1523.628453	96029.929793	36.605492
1525.228050	96148.428300	36.610509
1526.624313	96271.750398	36.615527
1527.835866	96399.766485	36.620544
1529.730913	96527.004884	36.625562
1531.059388	96657.767198	36.630580
1532.504173	96778.231622	36.635597
1533.962177	96917.176302	36.640615
1535.325682	97051.319339	36.645632
1537.127009	97174.911522	36.650650
1538.160426	97295.429277	36.655668
1539.416034	97408.433852	36.660685
1541.005435	97544.128372	36.665703
1541.947871	97675.702904	36.670720
1543.786021	97793.980337	36.675738
1545.094925	97929.973700	36.680756
1546.888651	98060.745474	36.685773
1548.179868	98187.691583	36.690791
1549.548962	98313.016133	36.695808
1550.939147	98439.783047	36.700826
1552.960894	98573.094827	36.705844
1554.351030	98705.187076	36.710861
1556.278028	98844.155951	36.715879
1557.781371	98977.829003	36.720896
1559.442335	99110.578010	36.725914
1560.748415	99253.727318	36.730932
1562.109117	99398.174511	36.735949
1563.714458	99539.922062	36.740967
1565.393888	99684.625188	36.745984
1567.126629	99819.014002	36.751002
1568.822052	99965.034343	36.756020
1570.658237	100088.176022	36.761037
1572.709327	100225.382083	36.766055
1574.549424	100351.997791	36.771072
1576.549590	100468.079368	36.776090
1578.025273	100600.394292	36.781108
1579.765318	100726.874910	36.786125
1581.514319	100846.267778	36.791143
1582.625781	100972.657023	36.796160
1584.523729	101098.607404	36.801178
1586.026951	101226.052309	36.806196
1588.111543	101347.955720	36.811213
1589.475396	101467.917934	36.816231
1591.058137	101589.253782	36.821248
1593.075605	101716.836094	36.826266
1594.455457	101843.301047	36.831284
1596.194255	101969.976863	36.836301
1597.860654	102091.643865	36.841319
1598.933556	102222.798283	36.846336
1600.640285	102343.306221	36.851354
1602.188190	102477.062847	36.856372
1603.189654	102604.756038	36.861389
1605.192034	102739.444590	36.866407
1606.174922	102884.891606	36.871424
1608.156137	103017.061562	36.876442
1609.771845	103157.403251	36.881460
1611.087480	103307.605536	36.886477
1612.691568	103444.463615	36.891495
1614.121774	103585.368498	36.896512
1615.474741	103724.878649	36.901530
1617.198192	103878.734944	36.906548
1618.723030	104025.205677	36.911565
1620.558417	104169.447930	36.916583
1621.782188	104327.327240	36.921600
1623.474507	104478.351039	36.926618
1625.034019	104629.421548	36.931636
1626.625524	104774.401727	36.936653
1627.948313	104943.350184	36.941671
1629.076151	105099.713870	36.946688
1631.244045	105258.908749	36.951706
1632.829392	105422.785021	36.956724
1634.769454	105583.817383	36.961741
1636.261235	105738.377611	36.966759
1637.599055	105895.536480	36.971776
1639.345300	106057.755115	36.976794
1641.040536	106220.527696	36.981812
1643.098735	106373.924886	36.986829
1644.621987	106532.617466	36.991847
1646.337217	106678.385396	36.996864
1648.602240	106791.848508	37.001882
1650.586992	106912.190160	37.006900
1652.694608	107036.925782	37.011917
1654.617295	107152.332710	37.016935
1656.030341	107265.549600	37.021952
1657.909865	107376.640067	37.026970
1659.302509	107508.247240	37.031988
1661.063402	107615.210502	37.037005
1664.044026	107706.374770	37.042023
1665.535852	107817.666494	37.047040
1666.951631	107925.140930	37.052058
1668.674714	108044.360693	37.057076
1669.805085	108145.603415	37.062093
1671.463474	108269.424364	37.067111
1672.569102	108396.425851	37.072128
1674.127072	108511.627822	37.077146
1675.266896	108646.727827	37.082164
1676.859790	108788.022119	37.087181
1678.639894	108919.079826	37.092199
1679.603607	109070.808028	37.097216
1681.276937	109214.158511	37.102234
1682.581968	109364.947210	37.107252
1684.430915	109520.851113	37.112269
1686.160665	109677.154695	37.117287
1687.547964	109845.774907	37.122304
1689.410779	109999.091839	37.127322
1690.997817	110155.787525	37.132340
1692.428461	110328.943192	37.137357
1694.326958	110493.936197	37.142375
1695.662047	110659.956088	37.147392
1697.496807	110822.880803	37.152410
1699.542914	110990.845985	37.157428
1701.099067	111161.957165	37.162445
1703.121993	111328.836944	37.167463
1704.436629	111518.172914	37.172480
1706.299894	111670.051324	37.177498
1708.154917	111830.238258	37.182516
1709.830983	112010.085318	37.187533
1711.843646	112175.207885	37.192551
1713.639362	112350.421810	37.197568
1715.436495	112527.158221	37.202586
1717.586002	112685.717900	37.207604
1719.719008	112853.564206	37.212621
1721.447303	112994.828902	37.217639
1722.724171	113171.814329	37.222656
1724.562233	113329.943396	37.227674
1726.503932	113491.252992	37.232692
1728.085560	113646.848829	37.237709
1730.016028	113815.999384	37.242727
1731.289874	113984.885130	37.247744
1732.994520	114149.024718	37.252762
1734.510493	114314.183662	37.257780
1736.293321	114480.164249	37.262797
1738.164788	114649.949322	37.267815
1739.728508	114826.860124	37.272832
1741.713728	114981.371540	37.277850
1743.788183	115143.695118	37.282868
1745.446658	115308.354422	37.287885
1747.630012	115472.907405	37.292903
1749.307277	115640.241404	37.297920
1751.438131	115784.130417	37.302938
1753.286409	115934.469014	37.307956
1755.117852	116087.829470	37.312973
1756.875306	116233.198878	37.317991
1758.655177	116395.129900	37.323008
1760.611062	116543.006323	37.328026
1762.421751	116690.043454	37.333044
1763.884377	116849.133989	37.338061
1765.847415	116969.842807	37.343079
1767.132345	117117.902042	37.348096
1768.524524	117252.005779	37.353114
1769.924969	117379.969777	37.358132
1772.138409	117505.207502	37.363149
1775.081396	117627.846070	37.368167
1777.046242	117755.964503	37.373184
1778.384677	117888.353876	37.378202
1780.308789	118012.864609	37.383220
1781.471317	118151.789158	37.388237
1783.051165	118286.336689	37.393255
1784.404886	118427.997621	37.398272
1786.329914	118581.049321	37.403290
1787.569066	118725.849499	37.408308
1788.916798	118883.875688	37.413325
1790.930472	119036.065582	37.418343
1792.509894	119223.484714	37.423360
1793.885466	119372.578807	37.428378
1795.805097	119546.551839	37.433396
1797.151903	119725.130508	37.438413
1799.291150	119893.895650	37.443431
1800.910763	120069.363794	37.448448
1802.697887	120248.713557	37.453466
1804.750544	120425.232181	37.458484
1806.306254	120615.782261	37.463501
1808.003747	120790.353630	37.468519
1809.916357	120976.486343	37.473536
1811.623955	121171.544044	37.478554
1813.330670	121353.702150	37.483572
1814.989648	121551.826428	37.488589
1817.087882	121746.382235	37.493607
1818.936037	121954.398935	37.498624
1820.599964	122151.802427	37.503642
1822.457434	122337.366695	37.508660
1824.111159	122555.235333	37.513677
1826.138785	122750.276473	37.518695
1828.053351	122947.987462	37.523712
1829.895657	123150.188718	37.528730
1832.706451	123340.924624	37.533748
1834.958801	123532.408023	37.538765
1836.671597	123708.436183	37.543783
1838.405099	123897.122409	37.548800
1840.126931	124086.268038	37.553818
1842.429149	124278.051723	37.558836
1844.116088	124471.340242	37.563853
1846.062189	124638.760412	37.568871
1848.350572	124821.173810	37.573888
1850.517660	125002.389036	37.578906
1852.668219	125166.125946	37.583924
1854.333427	125346.849948	37.588941
1856.152733	125518.162840	37.593959
1857.765820	125697.259973	37.598976
1859.737045	125866.152953	37.603994
1861.850057	126038.602177	37.609012
1863.449934	126224.326070	37.614029
1865.679290	126391.595228	37.619047
1867.331505	126576.043908	37.624064
1868.958904	126751.350114	37.629082
1870.976742	126934.906177	37.634100
1872.349031	127126.708515	37.639117
1874.101229	127310.637457	37.644135
1876.053511	127478.398210	37.649152
1877.585954	127674.263381	37.654170
1879.834451	127858.054081	37.659188
1881.034324	128057.537902	37.664205
1882.760429	128239.762261	37.669223
1884.814339	128434.915497	37.674240
1885.939193	128623.210823	37.679258
1888.205442	128809.312056	37.684276
1889.697025	128980.715728	37.689293
1891.400557	129172.780446	37.694311
1893.324826	129349.345537	37.699328
1895.307702	129537.168857	37.704346
1897.092220	129715.685751	37.709364
1898.873579	129912.664544	37.714381
1900.348700	130109.806104	37.719399
1903.087279	130291.729523	37.724416
1905.472350	130471.082342	37.729434
1907.837656	130645.478002	37.734452
1909.651427	130832.318333	37.739469
1911.562425	131007.674338	37.744487
1913.318925	131191.492703	37.749504
1915.320588	131376.745526	37.754522
1917.198285	131551.779043	37.759540
1919.083405	131748.331433	37.764557
1920.860815	131931.553352	37.769575
1922.886549	132118.988007	37.774592
1925.124906	132311.554578	37.779610
1927.174481	132500.700111	37.784628
1928.829605	132699.411585	37.789645
1930.914865	132883.439735	37.794663
1932.914013	133073.217339	37.799680
1934.337541	133271.992834	37.804698
1935.982411	133478.360738	37.809716
1937.966753	133684.879795	37.814733
1939.725107	133882.337049	37.819751
1942.342500	134084.534048	37.824768
1944.363578	134280.429514	37.829786
1946.571801	134484.011672	37.834804
1948.183725	134685.974533	37.839821
1950.089295	134898.894132	37.844839
1951.752810	135101.548748	37.849856
1953.578978	135306.374214	37.854874
1956.131748	135506.252883	37.859892
1958.359584	135706.779414	37.864909
1960.615145	135918.088574	37.869927
1962.344864	136122.615522	37.874944
1963.886277	136326.576289	37.879962
1965.842403	136534.293011	37.884980
1967.623194	136754.867262	37.889997
1969.967746	136970.532726	37.895015
1971.932797	137180.420948	37.900032
1973.646648	137405.640539	37.905050
1975.008473	137621.576216	37.910068
1977.322508	137845.676663	37.915085
1979.030259	138071.078111	37.920103
1980.966845	138294.389238	37.925120
1982.719844	138517.184333	37.930138
1984.791710	138736.073028	37.935156
1986.741228	138967.811698	37.940173
1988.635014	139198.570338	37.945191
1990.749570	139424.790647	37.950208
1992.964923	139650.209544	37.955226
1996.047248	139855.887678	37.960244
1998.526268	140081.496027	37.965261
2000.450076	140290.947799	37.970279
2002.571693	140498.542242	37.975296
2003.724550	140716.605967	37.980314
2005.956727	140929.439061	37.985332
2007.880587	141142.828722	37.990349
2009.597461	141363.079276	37.995367
2011.802482	141576.706304	38.000384
2014.179593	141796.678409	38.005402
2016.024330	142008.815108	38.010420
2017.987707	142229.043933	38.015437
2020.025171	142435.276481	38.020455
2022.475923	142611.151485	38.025472
2024.635002	142804.015439	38.030490
2026.027296	142993.496669	38.035508
2028.102093	143183.215077	38.040525
2029.706735	143382.069104	38.045543
2031.586793	143582.708648	38.050560
2033.141584	143796.510033	38.055578
2034.777619	144001.034799	38.060596
2036.810271	144220.271808	38.065613
2038.966494	144435.606873	38.070631
2041.067390	144646.534730	38.075648
2042.901636	144873.674400	38.080666
2044.986804	145090.609820	38.085684
2046.759014	145314.232779	38.090701
2048.734313	145541.099663	38.095719
2050.913926	145772.238380	38.100736
2052.804825	146011.761818	38.105754
2054.903514	146241.252588	38.110772
2057.023731	146479.663694	38.115789
2059.085486	146719.493854	38.120807
2061.370277	146956.904254	38.125824
2063.847034	147190.858912	38.130842
2066.436726	147406.748333	38.135860
2068.921265	147621.804617	38.140877
2070.793848	147868.015811	38.145895
2072.776938	148095.806615	38.150912
2074.653541	148324.097306	38.155930
2076.605509	148551.019133	38.160948
2079.023050	148788.226821	38.165965
2080.803009	149043.723699	38.170983
2083.171846	149272.398828	38.176000
2085.068643	149525.430103	38.181018
2086.844251	149763.770187	38.186036
2088.951965	149998.454802	38.191053
2090.844134	150252.201046	38.196071
2093.552343	150485.855038	38.201088
2095.637836	150739.154607	38.206106
2098.047309	150978.251864	38.211124
2100.469643	151202.078019	38.216141
2102.677481	151439.393526	38.221159
2104.954244	151666.176424	38.226176
2107.296145	151907.319223	38.231194
2109.264312	152142.758343	38.236212
2111.247420	152376.926776	38.241229
2113.490843	152616.044314	38.246247
2116.334847	152823.753888	38.251264
2118.250899	153048.453344	38.256282
2120.156795	153272.723692	38.261300
2122.196984	153507.243414	38.266317
2123.931091	153734.893535	38.271335
2126.185475	153970.562388	38.276352
2128.171118	154206.934137	38.281370
2130.302102	154449.656702	38.286388
2132.407776	154698.020455	38.291405
2133.850456	154935.495258	38.296423
2135.683489	155185.439555	38.301440
2137.565717	155448.731733	38.306458
2139.826174	155694.219466	38.311476
2141.727658	155969.304112	38.316493
2143.638238	156222.769872	38.321511
2145.789705	156488.081361	38.326528
2147.913805	156751.024411	38.331546
2150.249807	157000.669707	38.336564
2152.776502	157266.459478	38.341581
2154.689863	157523.243722	38.346599
2156.848290	157788.737685	38.351616
2159.000639	158045.652013	38.356634
2161.323308	158302.312423	38.361652
2163.815280	158528.720752	38.366669
2165.385959	158774.811004	38.371687
2167.584818	159010.775351	38.376704
2169.487042	159250.290641	38.381722
2171.786966	159492.068198	38.386740
2174.273747	159732.586186	38.391757
2175.767976	159984.520323	38.396775
2178.311276	160219.496257	38.401792
2180.214897	160467.686990	38.406810
2182.445533	160710.584594	38.411828
2184.991692	160963.400010	38.416845
2186.541129	161217.679206	38.421863
2189.316573	161466.741162	38.426880
2191.134872	161718.631843	38.431898
2193.260471	161981.305140	38.436916
2195.537303	162228.251322	38.441933
2197.549772	162501.608804	38.446951
2199.723587	162761.535499	38.451968
2201.800352	163045.841815	38.456986
2204.236661	163320.507959	38.462004
2206.337788	163583.039235	38.467021
2208.217751	163870.439518	38.472039
2210.445214	164141.980285	38.477056
2212.749757	164432.656025	38.482074
2214.791501	164706.729160	38.487092
2217.088192	164982.896722	38.492109
2219.298452	165279.519997	38.497127
2221.964659	165558.273260	38.502144
2224.672742	165837.376656	38.507162
2227.456946	166104.648905	38.512180
2230.145865	166372.851182	38.517197
2231.610753	166643.631964	38.522215
2234.006000	166918.001837	38.527232
2236.698063	167195.691233	38.532250
2238.811800	167484.822645	38.537268
2241.101419	167754.908058	38.542285
2243.070818	168032.192678	38.547303
2245.472626	168306.719348	38.552320
2247.643194	168591.542211	38.557338
2249.826412	168867.577914	38.562356
2253.095710	169132.259552	38.567373
2255.339024	169394.790965	38.572391
2257.682107	169663.173887	38.577408
2260.136349	169934.562435	38.582426
2262.524729	170194.775974	38.587444
2264.630576	170469.928324	38.592461
2266.411215	170743.976856	38.597479
2268.847758	171019.790840	38.602496
2271.421881	171292.575146	38.607514
2272.650039	171570.433049	38.612532
2275.006872	171845.526032	38.617549
2277.076447	172136.308127	38.622567
2279.161857	172415.394364	38.627584
2281.519332	172699.759603	38.632602
2283.590830	173001.566266	38.637620
2286.093398	173286.139650	38.642637
2288.193100	173575.830501	38.647655
2290.884096	173869.277857	38.652672
2293.430449	174146.190757	38.657690
2295.496297	174428.360171	38.662708
2297.948393	174702.394557	38.667725
2299.993930	175003.616157	38.672743
2302.682622	175287.266234	38.677760
2305.038009	175579.845170	38.682778
2306.875746	175857.445690	38.687796
2309.162555	176146.024713	38.692813
2311.666964	176438.837501	38.697831
2313.799248	176713.322097	38.702848
2315.598248	176986.234080	38.707866
2317.986028	177253.341052	38.712884
2320.449940	177518.176707	38.717901
2322.324759	177801.644630	38.722919
2324.527295	178072.795740	38.727936
2326.855701	178356.601272	38.732954
2328.642122	178634.980901	38.737972
2330.880572	178919.386422	38.742989
2332.940078	179215.909859	38.748007
2335.649764	179502.682091	38.753024
2338.068320	179799.735763	38.758042
2340.419504	180092.915083	38.763060
2342.371573	180403.427907	38.768077
2344.412216	180705.851527	38.773095
2346.492482	181011.419327	38.778112
2349.240434	181319.982792	38.783130
2351.474480	181645.745548	38.788148
2353.855683	181953.758662	38.793165
2356.259910	182273.858759	38.798183
2358.380753	182593.013519	38.803200
2361.332975	182907.722249	38.808218
2363.177958	183243.862851	38.813236
2366.397223	183569.021772	38.818253
2368.535860	183875.351783	38.823271
2371.285507	184209.754846	38.828288
2374.079955	184510.981244	38.833306
2376.187269	184835.047491	38.838324
2378.878279	185140.431917	38.843341
2382.005876	185449.178198	38.848359
2384.684820	185751.112087	38.853376
2387.976199	186087.062673	38.858394
2390.265123	186421.875004	38.863412
2393.231238	186701.085446	38.868429
2395.576688	186986.260493	38.873447
2397.865611	187282.239891	38.878464
2400.980489	187553.733407	38.883482
2402.965821	187851.844402	38.888500
2405.628046	188133.163288	38.893517
2407.864910	188418.181266	38.898535
2409.985136	188717.162642	38.903552
2412.108945	189003.825328	38.908570
2414.401173	189307.455115	38.913588
2416.634359	189603.500308	38.918605
2418.585486	189909.648610	38.923623
2420.785932	190217.511548	38.928640
2423.094030	190530.362405	38.933658
2425.611833	190848.744139	38.938676
2428.049169	191152.965860	38.943693
2430.226425	191475.339350	38.948711
2432.705177	191792.231087	38.953728
2435.760281	192084.649424	38.958746
2437.728204	192409.623462	38.963764
2440.593920	192721.961502	38.968781
2442.721568	193033.703974	38.973799
2444.972315	193346.444102	38.978816
2447.858799	193666.020515	38.983834
2449.602124	193981.686083	38.988852
2452.507442	194303.623451	38.993869
2454.737018	194630.315179	38.998887
2457.866685	194938.197810	39.003904
2460.661059	195243.771027	39.008922
2462.894680	195563.428302	39.013940
2465.480350	195869.391041	39.018957
2467.724167	196183.510706	39.023975
2470.232103	196500.231732	39.028992
2472.027342	196804.414452	39.034010
2474.421704	197132.432843	39.039028
2476.761409	197435.389118	39.044045
2479.077836	197756.334024	39.049063
2481.208207	198053.939022	39.054080
2483.590311	198353.791605	39.059098
2485.498879	198677.901009	39.064116
2488.094336	198977.899454	39.069133
2490.383880	199293.034834	39.074151
2493.023469	199607.252718	39.079168
2495.618722	199920.004819	39.084186
2497.667694	200242.850969	39.089204
2500.619074	200560.832543	39.094221
2503.023446	200884.285129	39.099239
2505.116011	201218.125582	39.104256
2507.954582	201541.613496	39.109274
2510.420179	201882.459054	39.114292
2512.853706	202216.375439	39.119309
2515.482792	202560.880245	39.124327
2517.723233	202900.264106	39.129344
2519.916484	203241.256316	39.134362
2522.557595	203597.471815	39.139380
2524.719930	203953.559293	39.144397
2527.444405	204301.939169	39.149415
2530.110642	204665.367152	39.154432
2533.132163	205008.011879	39.159450
2535.152849	205382.160015	39.164468
2538.129505	205734.872492	39.169485
2540.926804	206093.278339	39.174503
2543.338119	206452.430754	39.179520
2545.854587	206819.975801	39.184538
2548.554642	207186.552996	39.189556
2550.805659	207548.069264	39.194573
2553.419943	207920.605339	39.199591
2556.136950	208294.269177	39.204608
2558.773408	208666.853812	39.209626
2561.011900	209029.365077	39.214644
2563.647625	209409.622750	39.219661
2566.339357	209789.872287	39.224679
2568.964799	210173.485950	39.229696
2571.874763	210541.737662	39.234714
2574.487343	210926.929429	39.239732
2576.963816	211291.108866	39.244749
2580.059378	211662.407017	39.249767
2582.683795	212041.501634	39.254784
2585.763061	212413.463767	39.259802
2587.949359	212780.332183	39.264820
2590.542644	213150.745004	39.269837
2593.587482	213511.104352	39.274855
2596.448848	213888.767130	39.279872
2599.089461	214249.799862	39.284890
2601.895393	214614.389159	39.289908
2604.543498	214976.208970	39.294925
2607.080396	215330.526923	39.299943
2609.668277	215704.448983	39.304960
2612.836687	216054.325258	39.309978
2615.506577	216432.757095	39.314996
2617.818741	216790.718622	39.320013
2620.335431	217136.327728	39.325031
2622.579062	217512.565858	39.330048
2625.292324	217860.939321	39.335066
2628.046512	218230.823771	39.340084
2630.744445	218596.119117	39.345101
2633.334805	218957.036555	39.350119
2635.536217	219327.744460	39.355136
2638.723319	219680.999076	39.360154
2641.086326	220038.522978	39.365172
2643.650173	220406.736296	39.370189
2646.413347	220769.583930	39.375207
2648.588673	221150.229817	39.380224
2651.214429	221495.519559	39.385242
2654.177936	221845.075554	39.390260
2656.556551	222181.309347	39.395277
2659.295330	222513.447944	39.400295
2661.767821	222849.565701	39.405312
2665.000091	223175.835541	39.410330
2668.186431	223509.860842	39.415348
2670.574801	223834.737895	39.420365
2673.443239	224161.445597	39.425383
2675.674104	224496.737528	39.430400
2678.731545	224827.582166	39.435418
2681.278614	225157.413879	39.440436
2683.468622	225508.615213	39.445453
2686.028911	225845.989912	39.450471
2688.371051	226207.329217	39.455488
2690.834417	226561.561901	39.460506
2693.276233	226925.095814	39.465524
2695.660326	227284.319978	39.470541
2698.306012	227661.337055	39.475559
2701.219984	228037.575598	39.480576
2703.799966	228413.307149	39.485594
2706.381374	228803.620324	39.490612
2708.967943	229186.285960	39.495629
2712.920826	229540.311712	39.500647
2715.547326	229923.174121	39.505664
2718.404421	230291.240751	39.510682
2721.711831	230663.581242	39.515700
2724.492320	231029.601756	39.520717
2727.452875	231406.365373	39.525735
2730.155982	231775.344430	39.530752
2733.253197	232141.213480	39.535770
2735.942914	232516.291161	39.540788
2738.197873	232895.145243	39.545805
2740.667935	233267.640024	39.550823
2743.248003	233642.505399	39.555840
2746.074915	234025.715372	39.560858
2748.849347	234413.226470	39.565876
2751.363392	234808.322714	39.570893
2754.171098	235191.966598	39.575911
2756.781217	235597.411947	39.580928
2759.537776	235983.628859	39.585946
2762.499246	236383.937995	39.590964
2764.948509	236781.277978	39.595981
2768.147259	237177.942020	39.600999
2770.780919	237579.240818	39.606016
2773.596687	237972.508665	39.611034
2776.476236	238387.689438	39.616052
2779.151173	238790.047312	39.621069
2781.753801	239186.827144	39.626087
2784.647763	239596.008841	39.631104
2787.283800	240003.426463	39.636122
2790.073041	240413.741060	39.641140
2792.500249	240833.307422	39.646157
2795.247349	241245.532592	39.651175
2797.848382	241678.077097	39.656192
2801.029466	242083.349106	39.661210
2803.716365	242492.863493	39.666228
2806.682527	242921.614755	39.671245
2809.361300	243334.507602	39.676263
2812.560950	243755.142812	39.681280
2815.337383	244160.525064	39.686298
2818.476133	244580.660143	39.691316
2821.503063	244993.444955	39.696333
2824.554561	245402.363901	39.701351
2827.201043	245821.252183	39.706368
2829.994400	246227.085111	39.711386
2832.801111	246632.356275	39.716404
2835.327928	247055.350432	39.721421
2838.005242	247440.673527	39.726439
2840.413377	247832.693201	39.731456
2843.352883	248222.038296	39.736474
2846.463925	248608.993432	39.741492
2848.887009	248994.784668	39.746509
2852.139007	249371.097992	39.751527
2854.579550	249763.819657	39.756544
2857.885099	250140.961235	39.761562
2860.867656	250527.271615	39.766580
2863.437124	250923.044165	39.771597
2866.550919	251307.731945	39.776615
2869.453994	251691.638726	39.781632
2872.242374	252084.300691	39.786650
2875.192062	252487.249724	39.791668
2877.370574	252890.165293	39.796685
2880.382004	253292.315123	39.801703
2883.224488	253692.661233	39.806720
2886.134596	254116.873232	39.811738
2889.025233	254533.187136	39.816756
2891.558554	254942.900243	39.821773
2894.311224	255368.504680	39.826791
2897.335034	255795.081662	39.831808
2899.991510	256227.251935	39.836826
2902.857781	256661.420257	39.841844
2905.391361	257106.612180	39.846861
2908.441484	257548.699483	39.851879
2910.883695	258006.425201	39.856896
2913.920502	258470.102121	39.861914
2916.621940	258931.010032	39.866932
2919.530638	259394.678028	39.871949
2922.733876	259861.270276	39.876967
2925.809561	260323.181483	39.881984
2928.999601	260787.689317	39.887002
2932.468716	261241.763195	39.892020
2935.756997	261702.975445	39.897037
2938.875728	262148.743617	39.902055
2941.834002	262598.243370	39.907072
2944.758954	263063.189551	39.912090
2947.764498	263525.251054	39.917108
2950.506959	263985.903746	39.922125
2953.587457	264446.019258	39.927143
2956.697788	264896.984359	39.932160
2959.775504	265367.205200	39.937178
2963.366194	265820.021874	39.942196
2965.811465	266282.590205	39.947213
2969.053671	266735.355422	39.952231
2971.746272	267219.825569	39.957248
2974.410662	267679.940430	39.962266
2978.049097	268135.177414	39.967284
2980.189671	268618.913754	39.972301
2983.264824	269081.091464	39.977319
2985.950252	269557.702903	39.982336
2988.942347	270032.283137	39.987354
2992.267752	270498.529351	39.992372
2995.043951	270979.919513	39.997389
2997.994313	271459.121207	40.002407
3001.342907	271936.683716	40.007424
3004.254716	272417.537076	40.012442
3007.966185	272873.018536	40.017460
3010.729300	273346.245347	40.022477
3013.822941	273812.408561	40.027495
3017.403063	274269.198286	40.032512
3020.600572	274753.930589	40.037530
3023.837420	275201.829025	40.042548
3026.614377	275668.691490	40.047565
3029.414269	276124.551159	40.052583
3032.827198	276592.782337	40.057600
3035.118919	277052.017332	40.062618
3037.932231	277502.153008	40.067636
3040.904758	277951.372490	40.072653
3043.834914	278381.930298	40.077671
3047.063029	278817.619999	40.082688
3049.675396	279254.266488	40.087706
3052.169474	279688.389379	40.092724
3054.736108	280149.671044	40.097741
3057.470820	280611.457008	40.102759
3060.463523	281065.276844	40.107776
3063.705214	281536.983613	40.112794
3066.767812	281995.586372	40.117812
3069.549176	282465.301827	40.122829
3073.461633	282933.543109	40.127847
3076.494239	283396.763298	40.132864
3079.497756	283874.764062	40.137882
3082.674741	284339.072909	40.142900
3085.434238	284823.402731	40.147917
3088.840537	285304.225832	40.152935
3091.895797	285782.637073	40.157952
3094.562852	286276.391775	40.162970
3097.850109	286759.000595	40.167988
3100.919746	287262.004461	40.173005
3104.059480	287751.053310	40.178023
3107.603821	288242.650934	40.183040
3110.475243	288740.468988	40.188058
3114.240528	289228.876191	40.193076
3117.133899	289728.232093	40.198093
3120.377890	290231.135070	40.203111
3123.703290	290720.970416	40.208128
3127.240246	291210.642064	40.213146
3130.771163	291703.814703	40.218164
3134.068871	292205.880941	40.223181
3137.000221	292695.990530	40.228199
3140.142399	293189.135556	40.233216
3143.295887	293681.513107	40.238234
3146.696937	294175.701532	40.243252
3149.858112	294672.055891	40.248269
3153.397052	295159.562663	40.253287
3156.555693	295662.941861	40.258304
3159.602847	296160.545443	40.263322
3162.777235	296655.256051	40.268340
3166.537387	297143.727292	40.273357
3169.370977	297632.795524	40.278375
3172.752943	298128.628917	40.283392
3175.871275	298626.225326	40.288410
3179.210001	299117.385396	40.293428
3182.170448	299608.092246	40.298445
3185.202877	300108.963688	40.303463
3188.571822	300603.533063	40.308480
3191.233666	301112.982896	40.313498
3194.751597	301611.784821	40.318516
3198.040501	302110.973159	40.323533
3201.398921	302605.271949	40.328551
3205.107135	303094.637682	40.333568
3208.326810	303595.980582	40.338586
3211.724561	304076.373710	40.343604
3215.224018	304573.678231	40.348621
3218.367672	305065.499506	40.353639
3221.288734	305553.466913	40.358656
3224.463788	306054.056779	40.363674
3227.619560	306538.475222	40.368692
3230.446143	307033.753638	40.373709
3233.403854	307533.220387	40.378727
3236.609396	308035.029570	40.383744
3239.983880	308524.623636	40.388762
3243.279260	309024.555839	40.393780
3246.469959	309525.032250	40.398797
3249.726688	310025.873967	40.403815
3253.356836	310511.245657	40.408832
3256.366331	310970.515303	40.413850
3259.638322	311429.841213	40.418868
3263.014302	311896.329335	40.423885
3266.031262	312347.056496	40.428903
3269.426821	312797.238192	40.433920
3272.220256	313271.214449	40.438938
3275.158632	313740.087320	40.443956
3278.275092	314215.069634	40.448973
3281.364070	314689.391459	40.453991
3284.324201	315169.007303	40.459008
3287.252283	315672.758483	40.464026
3290.756180	316164.714885	40.469044
3294.343107	316664.875596	40.474061
3297.674416	317155.705973	40.479079
3300.835477	317658.002842	40.484096
3303.545591	318170.642096	40.489114
3306.843732	318681.965776	40.494132
3309.698849	319206.929097	40.499149
3312.964486	319744.282140	40.504167
3316.799961	320281.083070	40.509184
3319.703845	320827.233764	40.514202
3322.907981	321365.134431	40.519220
3326.333616	321908.627165	40.524237
3329.122347	322463.300917	40.529255
3332.950740	322998.343194	40.534272
3336.054130	323563.991431	40.539290
3339.644851	324126.130657	40.544308
3343.427152	324684.959233	40.549325
3346.620950	325238.213548	40.554343
3350.504594	325796.681360	40.559360
3353.697579	326363.114494	40.564378
3357.071619	326924.640050	40.569396
3360.402574	327490.579187	40.574413
3363.642318	328048.304131	40.579431
3367.566578	328622.888067	40.584448
3370.642145	329196.504780	40.589466
3374.567364	329769.448136	40.594484
3377.721337	330343.264219	40.599501
3381.465625	330911.626974	40.604519
3385.340563	331462.735270	40.609536
3388.688299	332043.979944	40.614554
3392.285422	332594.354156	40.619572
3395.728569	333147.915404	40.624589
3399.854118	333706.233001	40.629607
3403.997777	334243.306925	40.634624
3407.408395	334797.863701	40.639642
3411.221511	335345.551316	40.644660
3414.862126	335880.320844	40.649677
3418.113253	336422.296451	40.654695
3421.966774	336961.024991	40.659712
3425.044211	337488.172978	40.664730
3428.401396	338027.470314	40.669748
3432.056728	338558.698041	40.674765
3435.125108	339100.789036	40.679783
3438.727848	339628.534260	40.684800
3443.122888	340153.256968	40.689818
3447.142814	340657.257986	40.694836
3450.950251	341174.245209	40.699853
3454.247809	341679.434638	40.704871
3457.943297	342175.728917	40.709888
3461.505444	342679.163492	40.714906
3464.560309	343181.224129	40.719924
3468.188340	343696.908501	40.724941
3471.027211	344206.773617	40.729959
3474.390154	344719.542097	40.734976
3477.498104	345222.147969	40.739994
3480.416133	345745.646684	40.745012
3483.439988	346253.497676	40.750016
3486.393139	346734.535848	40.755021
3489.439393	347178.867165	40.760026
3492.446895	347581.962904	40.765031
3494.806072	347946.690449	40.770036
3497.197481	348259.242554	40.775040
3499.430986	348541.640340	40.780045
3501.766291	348776.023443	40.785050
3503.703052	348989.671960	40.790055
3505.289872	349144.776872	40.795060
3506.956198	349264.100675	40.800064
3508.066686	349369.655881	40.805069
3509.796108	349425.746195	40.810074
3511.261072	349460.269443	40.815079
3511.942740	349478.899121	40.820084
3513.204657	349453.790091	40.825088
3513.986967	349417.951598	40.830093
3514.754434	349358.498897	40.835098
3515.549075	349283.153448	40.840103
3516.017570	349191.614223	40.845108
3516.282653	349072.600207	40.850112
3516.823582	348964.652127	40.855117
3517.045757	348827.467377	40.860122
3517.343204	348683.050519	40.865127
3517.347455	348527.315004	40.870132
3517.679203	348371.095618	40.875136
3517.974179	348214.143974	40.880141
3518.236632	348032.231839	40.885146
3518.070185	347843.012908	40.890151
3517.996000	347663.261217	40.895156
3518.095372	347465.838093	40.900160
3518.007989	347283.645821	40.905165
3517.868743	347081.096693	40.910170
3517.788036	346892.545469	40.915175
3518.241879	346680.011969	40.920180
3518.005685	346485.228489	40.925184
3517.872582	346286.995636	40.930189
3517.134883	346073.703057	40.935194
3516.905369	345877.796382	40.940199
3517.389523	345678.040162	40.945204
3517.338913	345476.484582	40.950208
3516.684561	345281.759251	40.955213
3516.693587	345083.268427	40.960218
3516.574254	344889.830532	40.965223
3516.226467	344692.791326	40.970228
3516.288548	344492.178544	40.975232
3515.811441	344300.369349	40.980237
3515.659360	344103.398003	40.985242
3515.420174	343913.736209	40.990247
3515.083518	343727.648130	40.995252
3515.501829	343536.356407	41.000256
3515.180226	343350.747046	41.005261
3514.968618	343162.729522	41.010266
3514.793439	342983.121384	41.015271
3514.288757	342787.926395	41.020276
3514.225339	342613.740194	41.025280
3513.715841	342435.172883	41.030285
3513.945578	342256.642185	41.035290
3513.311347	342089.865093	41.040295
3512.987074	341929.700838	41.045300
3512.950712	341765.193871	41.050304
3512.600845	341598.548179	41.055309
3512.526066	341440.097343	41.060314
3512.625156	341275.567007	41.065319
3512.484827	341125.007461	41.070324
3512.100312	340971.739083	41.075328
3511.904587	340824.492471	41.080333
3511.616538	340667.037608	41.085338
3511.524124	340512.399537	41.090343
3511.200135	340370.027742	41.095348
3511.055790	340234.493032	41.100352
3510.797669	340100.196069	41.105357
3510.562513	339958.419082	41.110362
3510.653537	339830.118725	41.115367
3510.382403	339696.508835	41.120372
3510.302837	339569.480089	41.125376
3510.181409	339438.795665	41.130381
3510.323196	339303.340039	41.135386
3509.997631	339172.864414	41.140391
3510.191954	339049.427543	41.145396
3510.325166	338918.015015	41.150400
3509.621113	338792.174147	41.155405
3509.585341	338666.686574	41.160410
3509.444698	338554.336446	41.165415
3509.376378	338441.516984	41.170420
3509.542295	338314.598183	41.175424
3509.173138	338204.901772	41.180429
3509.215172	338092.445494	41.185434
3509.120918	337972.075982	41.190439
3508.996388	337849.345804	41.195444
3508.826728	337739.108343	41.200448
3508.436737	337640.500925	41.205453
3508.983213	337514.410158	41.210458
3508.490096	337408.850310	41.215463
3508.303143	337299.122812	41.220468
3508.338598	337196.328285	41.225472
3508.184620	337088.807463	41.230477
3508.614478	336994.978790	41.235482
3508.526772	336885.107453	41.240487
3508.260640	336781.697499	41.245492
3508.151380	336668.624610	41.250496
3507.955884	336566.372870	41.255501
3507.885016	336456.904524	41.260506
3507.730935	336363.572000	41.265511
3507.405756	336269.909831	41.270516
3507.744663	336160.503993	41.275520
3507.366775	336082.260760	41.280525
3507.676576	335992.618914	41.285530
3507.509912	335884.257315	41.290535
3507.664081	335800.056074	41.295540
3507.357146	335700.489561	41.300544
3507.297495	335612.277579	41.305549
3507.160021	335514.566121	41.310554
3507.334227	335435.726979	41.315559
3507.095910	335354.459566	41.320564
3506.928856	335252.123470	41.325568
3506.938741	335166.391912	41.330573
3507.084843	335072.983992	41.335578
3506.955861	334994.114799	41.340583
3507.118522	334909.528741	41.345588
3506.812276	334818.199694	41.350592
3506.434842	334739.928129	41.355597
3506.930200	334651.398617	41.360602
3506.836272	334564.461092	41.365607
3506.237602	334483.909094	41.370612
3506.468365	334400.303143	41.375616
3506.385899	334325.392732	41.380621
3506.507971	334246.838949	41.385626
3506.535080	334161.611055	41.390631
3506.614333	334092.677063	41.395636
3506.666043	334013.294470	41.400640
3506.371117	333933.406134	41.405645
3506.407634	333843.343868	41.410650
3506.176243	333773.567490	41.415655
3506.354792	333692.155302	41.420660
3506.279641	333605.238070	41.425664
3506.022236	333539.432821	41.430669
3506.058154	333457.559099	41.435674
3505.943455	333384.203239	41.440679
3505.494796	333308.584803	41.445684
3505.724689	333250.307684	41.450688
3505.843385	333172.388016	41.455693
3506.051403	333103.686513	41.460698
3506.010793	333026.325431	41.465703
3506.039188	332962.992592	41.470708
3505.912976	332884.703513	41.475712
3505.823682	332808.595793	41.480717
3505.507772	332733.108153	41.485722
3505.771742	332666.965925	41.490727
3505.719891	332599.855390	41.495732
3505.741359	332524.162236	41.500736
3505.573813	332456.891418	41.505741
3505.917648	332395.288898	41.510746
3505.688353	332317.828571	41.515751
3505.345099	332264.700429	41.520756
3506.000632	332179.980701	41.525760
3505.817330	332119.756887	41.530765
3505.820404	332038.037827	41.535770
3505.474814	331975.600863	41.540775
3505.298067	331903.141993	41.545780
3505.825696	331830.446206	41.550784
3505.326512	331772.000512	41.555789
3505.464047	331706.206942	41.560794
3505.464295	331634.508479	41.565799
3505.126575	331570.314679	41.570804
3505.388535	331505.569638	41.575808
3505.157786	331451.990483	41.580813
3505.599214	331376.941872	41.585818
3505.451736	331313.226725	41.590823
3505.203003	331251.053291	41.595828
3505.300836	331176.413839	41.600832
3505.014486	331125.691536	41.605837
3505.059076	331070.161422	41.610842
3504.979862	331004.476688	41.615847
3505.018584	330942.334329	41.620852
3505.251228	330879.424090	41.625856
3505.341056	330817.299013	41.630861
3505.154558	330757.353349	41.635866
3504.938014	330691.969238	41.640871
3504.885968	330631.366588	41.645876
3505.125448	330575.754570	41.650880
3504.735959	330517.239036	41.655885
3504.851912	330464.901740	41.660890
3504.942883	330395.247088	41.665895
3504.574423	330340.110860	41.670900
3504.820992	330288.668660	41.675904
3505.201152	330236.544293	41.680909
3504.797180	330172.918057	41.685914
3504.503542	330114.056347	41.690919
3504.613103	330063.143872	41.695924
3505.048598	329996.461676	41.700928
3504.954222	329947.997128	41.705933
3505.200050	329882.310791	41.710938
3505.107582	329817.796139	41.715943
3504.815146	329765.267103	41.720948
3505.211879	329697.471277	41.725952
3505.136469	329633.793035	41.730957
3504.865949	329572.383371	41.735962
3505.274147	329520.101076	41.740967
3505.114836	329456.461038	41.745972
3504.936604	329396.588305	41.750976
3504.644014	329336.504356	41.755981
3505.002920	329279.701874	41.760986
3505.225947	329225.540330	41.765991
3505.032022	329160.353623	41.770996
3505.147415	329103.894010	41.776000
3504.718917	329036.021975	41.781005
3504.690290	328981.009003	41.786010
3505.021807	328913.450897	41.791015
3504.825126	328864.263293	41.796020
3505.018453	328799.600755	41.801024
3504.757936	328739.154801	41.806029
3504.887796	328689.585498	41.811034
3504.818457	328629.491167	41.816039
3504.620408	328569.060669	41.821044
3504.838875	328517.900325	41.826048
3504.769928	328461.392173	41.831053
3504.948764	328395.128752	41.836058
3504.892501	328341.212948	41.841063
3504.708187	328280.398329	41.846068
3504.613872	328216.084837	41.851072
3504.477546	328168.514901	41.856077
3504.456175	328107.725535	41.861082
3504.442056	328055.150914	41.866087
3504.513596	327999.892066	41.871092
3504.813333	327944.343266	41.876096
3504.498728	327893.341381	41.881101
3504.453665	327840.618673	41.886106
3504.369444	327784.951344	41.891111
3504.674061	327738.863912	41.896116
3504.647898	327683.289154	41.901120
3504.665873	327629.437145	41.906125
3504.144444	327576.177736	41.911130
3504.223640	327515.219198	41.916135
3503.875158	327470.810168	41.921140
3504.372735	327414.517616	41.926144
3504.187353	327370.693578	41.931149
3504.192020	327327.730210	41.936154
3504.390652	327277.792333	41.941159
3504.067571	327232.387046	41.946164
3504.141319	327181.451006	41.951168
3504.328901	327129.149025	41.956173
3504.368667	327077.149786	41.961178
3504.670064	327032.257585	41.966183
3504.481826	326977.546493	41.971188
3504.471205	326917.974630	41.976192
3504.139860	326869.873882	41.981197
3504.055723	326822.777533	41.986202
3503.990727	326764.485765	41.991207
3503.935645	326730.052532	41.996212
3504.041318	326662.449455	42.001216
3504.397260	326629.045980	42.006221
3504.053448	326577.919781	42.011226
3503.964623	326526.219653	42.016231
3503.939130	326480.665460	42.021236
3504.418382	326429.563619	42.026240
3503.995403	326389.107793	42.031245
3503.977432	326346.859152	42.036250
3504.376637	326297.702852	42.041255
3503.805463	326248.697495	42.046260
3504.208775	326186.083945	42.051264
3503.989713	326157.195703	42.056269
3503.906808	326112.006157	42.061274
3504.394606	326058.664006	42.066279
3504.117589	326012.003731	42.071284
3504.468374	325967.942110	42.076288
3503.996367	325921.566452	42.081293
3504.043086	325867.020799	42.086298
3504.119013	325807.357522	42.091303
3504.205660	325773.435616	42.096308
3504.325305	325701.478890	42.101312
3504.140682	325664.877251	42.106317
3504.260812	325619.909943	42.111322
3504.134304	325569.308294	42.116327
3503.769012	325531.437312	42.121332
3504.190878	325471.032884	42.126336
3503.837693	325436.034430	42.131341
3504.026084	325378.617013	42.136346
3503.898768	325335.748386	42.141351
3503.892564	325295.302931	42.146356
3504.295072	325241.286155	42.151360
3503.944314	325190.947877	42.156365
3503.887276	325145.575168	42.161370
3504.422367	325095.505937	42.166375
3504.025512	325054.357885	42.171380
3504.157496	324997.915370	42.176384
3504.046578	324955.450807	42.181389
3503.741867	324905.639219	42.186394
3503.886702	324861.939156	42.191399
3503.634369	324814.841220	42.196404
3504.131264	324771.264345	42.201408
3503.854580	324729.181482	42.206413
3503.795132	324682.511273	42.211418
3503.997868	324638.344068	42.216423
3503.460467	324603.933219	42.221428
3503.889529	324558.840359	42.226432
3503.825878	324511.839909	42.231437
3503.754517	324475.016074	42.236442
3503.814829	324427.360270	42.241447
3503.733372	324388.884414	42.246452
3503.886231	324338.746551	42.251456
3503.635546	324294.471466	42.256461
3503.634034	324249.012812	42.261466
3503.804503	324207.343172	42.266471
3503.644592	324160.637128	42.271476
3503.885542	324133.532913	42.276480
3503.774141	324086.793798	42.281485
3503.555477	324039.638861	42.286490
3503.671756	323998.002882	42.291495
3503.594101	323961.535715	42.296500
3503.706338	323918.373946	42.301504
3503.767664	323873.057736	42.306509
3503.773419	323831.413350	42.311514
3503.643392	323780.860930	42.316519
3503.694541	323753.277220	42.321524
3503.736122	323711.627139	42.326528
3503.527596	323661.671889	42.331533
3503.731028	323617.859638	42.336538
3503.653952	323571.496191	42.341543
3503.722788	323534.751462	42.346548
3503.930166	323498.773759	42.351552
3504.060194	323456.728071	42.356557
3503.818951	323409.296100	42.361562
3503.519735	323355.487819	42.366567
3503.445923	323319.197567	42.371572
3503.658656	323269.888598	42.376576
3503.684447	323238.848734	42.381581
3503.810352	323197.185017	42.386586
3503.886029	323153.748313	42.391591
3503.860496	323110.022038	42.396596
3503.729660	323064.582216	42.401600
3503.834652	323021.929438	42.406605
3503.832789	322980.666982	42.411610
3503.975316	322930.223757	42.416615
3503.864413	322885.111354	42.421620
3504.022737	322843.264164	42.426624
3504.001388	322803.403748	42.431629
3503.466211	322763.674131	42.436634
3503.762974	322712.316253	42.441639
3504.023986	322678.288361	42.446644
3503.793243	322633.448733	42.451648
3504.274570	322571.199170	42.456653
3504.044973	322526.689968	42.461658
3503.814743	322484.317768	42.466663
3503.851331	322433.432515	42.471668
3503.722786	322388.653044	42.476672
3503.578675	322347.920902	42.481677
3503.645597	322303.645162	42.486682
3503.692769	322256.930208	42.491687
3503.630754	322218.016847	42.496692
3503.640108	322181.407390	42.501696
3503.673992	322147.287213	42.506701
3503.616131	322091.328228	42.511706
3503.407536	322045.009001	42.516711
3503.907042	322010.180254	42.521716
3503.852153	321967.500408	42.526720
3503.613633	321932.099557	42.531725
3503.570812	321889.748479	42.536730
3503.577406	321838.561894	42.541735
3503.520415	321809.696283	42.546740
3503.850939	321761.588354	42.551744
3503.737803	321724.437876	42.556749
3503.459188	321678.358108	42.561754
3503.737674	321633.845224	42.566759
3503.715508	321599.987734	42.571764
3503.495472	321552.957419	42.576768
3503.666291	321521.944605	42.581773
3503.639607	321484.017251	42.586778
3504.054815	321441.289164	42.591783
3503.693705	321390.693511	42.596788
3503.398281	321346.778445	42.601792
3503.682523	321304.732057	42.606797
3503.474689	321263.881587	42.611802
3503.692263	321218.868937	42.616807
3503.464140	321178.403152	42.621812
3503.317255	321135.355178	42.626816
3503.761253	321101.450191	42.631821
3503.629118	321062.979177	42.636826
3503.547060	321016.969870	42.641831
3503.267235	320982.923017	42.646836
3503.397755	320941.637976	42.651840
3503.198268	320894.578297	42.656845
3503.063967	320864.808206	42.661850
3503.474586	320829.508952	42.666855
3503.301726	320792.977538	42.671860
3503.492785	320754.684922	42.676864
3503.633713	320728.408195	42.681869
3503.642532	320685.004806	42.686874
3503.533085	320643.095355	42.691879
3503.352506	320609.770550	42.696884
3503.412031	320563.687843	42.701888
3503.634072	320522.846096	42.706893
3503.281195	320486.367876	42.711898
3503.489004	320439.040789	42.716903
3503.381619	320418.348674	42.721908
3503.316684	320363.431610	42.726912
3503.424410	320324.922609	42.731917
3503.182036	320289.368349	42.736922
3503.345512	320254.692230	42.741927
3503.035628	320230.088147	42.746932
3503.340389	320200.300155	42.751936
3503.287848	320164.283751	42.756941
3502.814558	320133.599137	42.761946
3503.071035	320077.181540	42.766951
3503.027790	320057.522364	42.771956
3503.277963	320019.830489	42.776960
3503.673251	319979.368330	42.781965
3503.194883	319948.353636	42.786970
3503.429784	319907.127685	42.791975
3503.286368	319871.125178	42.796980
3503.309596	319825.988665	42.801985
3503.557314	319793.207177	42.806989
3503.433735	319754.224832	42.811994
3503.591656	319706.192344	42.816999
3503.406591	319680.092916	42.822004
3503.223195	319638.422970	42.827009
3503.450390	319597.757639	42.832013
3503.345043	319563.377215	42.837018
3503.276617	319529.423526	42.842023
3503.034889	319491.705971	42.847028
3503.140791	319455.969622	42.852033
3503.314574	319424.267912	42.857037
3503.176669	319392.970865	42.862042
3503.170698	319352.061729	42.867047
3503.066136	319317.859081	42.872052
3503.303388	319281.542431	42.877057
3503.030899	319241.565127	42.882061
3503.103367	319206.291729	42.887066
3503.228808	319179.533078	42.892071
3503.321598	319140.312978	42.897076
3503.219104	319115.955851	42.902081
3503.252277	319080.637583	42.907085
3502.839933	319039.028133	42.912090
3503.343668	318997.479626	42.917095
3503.084004	318972.917899	42.922100
3503.383856	318932.851249	42.927105
3503.507815	318895.076273	42.932109
3503.295891	318865.902053	42.937114
3503.456075	318830.818239	42.942119
3502.858353	318786.006255	42.947124
3502.920734	318748.189850	42.952129
3503.108452	318717.452258	42.957133
3502.993982	318680.350252	42.962138
3503.015464	318643.074406	42.967143
3502.911617	318617.928506	42.972148
3502.823005	318584.155318	42.977153
3503.037158	318559.087110	42.982157
3503.026124	318528.303988	42.987162
3503.213089	318483.344146	42.992167
3503.050069	318453.347889	42.997172
3502.983634	318426.771291	43.002177
3503.129294	318385.786772	43.007181
3503.021778	318364.483085	43.012186
3503.453556	318323.555754	43.017191
3503.133951	318289.563863	43.022196
3503.104033	318254.610941	43.027201
3502.998455	318227.684120	43.032205
3502.718567	318198.138397	43.037210
3503.118286	318162.787793	43.042215
3503.156965	318126.068567	43.047220
3502.779932	318099.463776	43.052225
3503.108449	318061.478155	43.057229
3502.958936	318036.796994	43.062234
3503.345043	317992.848805	43.067239
3503.108106	317959.530744	43.072244
3502.871661	317921.734688	43.077249
3503.425233	317886.232710	43.082253
3503.085548	317853.083212	43.087258
3503.594959	317815.908837	43.092263
3503.445001	317792.118101	43.097268
3502.885359	317745.416376	43.102273
3503.023802	317700.514173	43.107277
3503.126229	317683.960715	43.112282
3503.489503	317648.106519	43.117287
3503.265494	317604.659971	43.122292
3503.170869	317575.924614	43.127297
3503.298913	317543.083741	43.132301
3503.000280	317509.087986	43.137306
3502.886914	317474.147433	43.142311
3502.695794	317449.675962	43.147316
3502.795296	317416.254252	43.152321
3502.799185	317383.585239	43.157325
3502.903030	317350.213690	43.162330
3502.930414	317318.609575	43.167335
3502.676651	317286.616658	43.172340
3502.676315	317251.912771	43.177345
3503.253399	317228.797327	43.182349
3502.897066	317193.996135	43.187354
3503.124990	317150.122615	43.192359
3502.733118	317131.356000	43.197364
3502.942764	317096.950076	43.202369
3503.512489	317066.711641	43.207373
3502.656281	317037.356599	43.212378
3503.005183	317000.537281	43.217383
3503.061046	316969.640894	43.222388
3503.102410	316930.172405	43.227393
3502.979208	316893.935328	43.232397
3502.880886	316878.710412	43.237402
3502.662439	316839.867466	43.242407
3502.873793	316820.396214	43.247412
3503.409608	316788.076526	43.252417
3503.092953	316749.935751	43.257421
3502.920207	316712.306858	43.262426
3503.369661	316683.206384	43.267431
3503.198594	316639.597998	43.272436
3502.866656	316605.810284	43.277441
3503.044995	316572.859099	43.282445
3502.776790	316543.539448	43.287450
3503.421249	316513.238124	43.292455
3503.302280	316472.903665	43.297460
3503.128003	316434.842240	43.302465
3503.381476	316401.904681	43.307469
3502.739743	316369.106404	43.312474
3503.336614	316335.250282	43.317479
3503.248695	316311.449102	43.322484
3503.089171	316270.968111	43.327489
3503.206989	316241.104766	43.332493
3502.782205	316206.033579	43.337498
3503.154751	316169.108127	43.342503
3502.828493	316137.939865	43.347508
3502.847963	316106.437902	43.352513
3503.065686	316078.594391	43.357517
3503.066310	316050.708315	43.362522
3503.288334	316019.505539	43.367527
3502.839385	315980.341508	43.372532
3502.770580	315949.769145	43.377537
3502.957699	315920.225571	43.382541
3502.913376	315877.385479	43.387546
3503.064794	315862.452125	43.392551
3503.153407	315828.089509	43.397556
3503.086469	315798.152847	43.402561
3503.279177	315753.062143	43.407565
3502.597002	315726.885080	43.412570
3503.066573	315691.623433	43.417575
3502.739109	315668.113628	43.422580
3502.969989	315632.303870	43.427585
3503.081097	315599.260661	43.432589
3502.815480	315570.881399	43.437594
3503.176616	315539.300430	43.442599
3502.809618	315511.852888	43.447604
3502.992703	315472.030299	43.452609
3503.272737	315441.886744	43.457613
3503.095560	315412.246865	43.462618
3503.075008	315371.667112	43.467623
3502.896089	315345.513292	43.472628
3502.945055	315312.683097	43.477633
3502.937585	315272.152108	43.482637
3502.634247	315247.569680	43.487642
3502.858239	315214.177853	43.492647
3502.729390	315197.099700	43.497652
3502.776889	315163.709856	43.502657
3503.029419	315122.171398	43.507661
3502.719019	315095.987005	43.512666
3503.083339	315053.667763	43.517671
3502.948763	315034.936568	43.522676
3502.800728	315009.922738	43.527681
3503.048622	314968.919189	43.532685
3502.805309	314939.620070	43.537690
3502.903898	314903.652216	43.542695
3502.991444	314879.288650	43.547700
3502.446804	314850.647027	43.552705
3502.641940	314818.175396	43.557709
3502.613640	314793.091926	43.562714
3502.664376	314764.586600	43.567719
3502.444669	314743.120543	43.572724
3502.610719	314712.027358	43.577729
3502.598788	314689.154946	43.582733
3502.324032	314662.455870	43.587738
3502.811299	314632.864757	43.592743
3502.634124	314611.086685	43.597748
3502.779080	314583.737029	43.602753
3502.733779	314548.096621	43.607757
3502.760779	314532.113524	43.612762
3503.081732	314490.029511	43.617767
3502.865269	314459.453681	43.622772
3502.830683	314439.078233	43.627777
3502.668900	314396.127805	43.632781
3502.588852	314378.431084	43.637786
3502.748662	314345.837393	43.642791
3502.560136	314312.687215	43.647796
3502.628115	314294.254977	43.652801
3502.819229	314261.961691	43.657805
3502.543533	314245.007813	43.662810
3502.597721	314210.471225	43.667815
3502.479332	314193.441960	43.672820
3502.381888	314160.735502	43.677825
3502.951460	314134.286402	43.682829
3502.823862	314112.958385	43.687834
3502.835884	314082.372194	43.692839
3502.714915	314053.028026	43.697844
3502.947828	314022.763649	43.702849
3502.760544	313983.633520	43.707853
3502.734807	313967.403986	43.712858
3502.585075	313931.804797	43.717863
3502.512513	313897.389478	43.722868
3502.729977	313879.671713	43.727873
3502.750996	313846.819375	43.732877
3502.660051	313829.073249	43.737882
3502.339434	313794.492895	43.742887
3502.393245	313772.067805	43.747892
3502.630247	313747.604050	43.752897
3502.768531	313719.618797	43.757901
3502.711965	313689.908148	43.762906
3502.999040	313664.902213	43.767911
3502.695908	313639.911773	43.772916
3503.084359	313613.108886	43.777921
3502.721983	313584.285442	43.782925
3502.847003	313545.259014	43.787930
3502.520567	313510.959250	43.792935
3502.696760	313491.034040	43.797940
3502.952387	313462.521472	43.802945
3502.836577	313434.219357	43.807949
3502.418898	313403.292463	43.812954
3502.642249	313370.306522	43.817959
3502.549217	313348.870993	43.822964
3502.558741	313330.269352	43.827969
3502.966436	313289.443008	43.832973
3502.664399	313259.643056	43.837978
3502.648281	313226.796058	43.842983
3502.879306	313204.673906	43.847988
3502.648402	313168.908646	43.852993
3502.547447	313148.466623	43.857997
3502.369852	313119.665026	43.863002
3502.726032	313086.632770	43.868007
3502.735815	313065.766353	43.873012
3502.695796	313035.289352	43.878017
3502.764452	313003.268701	43.883021
3502.453530	312990.365651	43.888026
3502.682365	312951.653361	43.893031
3502.670456	312930.484916	43.898036
3502.782943	312906.040095	43.903041
3502.904990	312871.212053	43.908045
3502.697378	312855.264888	43.913050
3502.569789	312822.562180	43.918055
3502.787270	312795.200184	43.923060
3502.621951	312769.806150	43.928065
3503.136872	312735.578454	43.933069
3502.613075	312711.563336	43.938074
3502.598218	312684.059312	43.943079
3502.646549	312655.120491	43.948084
3502.177840	312631.020423	43.953089
3502.566163	312601.850543	43.958093
3502.261756	312581.160030	43.963098
3502.358103	312546.183073	43.968103
3502.727840	312539.331808	43.973108
3502.616514	312510.799426	43.978113
3502.886477	312476.329758	43.983117
3502.636355	312459.778378	43.988122
3502.624220	312421.586616	43.993127
3502.366247	312402.390092	43.998132
3502.612855	312371.817166	44.003137
3502.867727	312343.940176	44.008141
3502.694591	312328.063803	44.013146
3502.726137	312277.651195	44.018151
3502.522458	312259.082306	44.023156
3502.618529	312233.392849	44.028161
3503.089751	312197.441251	44.033165
3502.629352	312182.932711	44.038170
3502.817133	312149.442532	44.043175
3502.688306	312126.205363	44.048180
3502.484957	312096.491098	44.053185
3502.478698	312071.886201	44.058189
3502.510830	312043.891021	44.063194
3502.276148	312023.545654	44.068199
3502.606342	311987.437722	44.073204
3502.077577	311976.858421	44.078209
3502.461662	311943.057643	44.083213
3502.617508	311929.750870	44.088218
3502.421060	311900.213529	44.093223
3502.579034	311873.038380	44.098228
3502.453406	311852.141605	44.103233
3502.705520	311820.167938	44.108237
3502.608731	311805.373686	44.113242
3502.646805	311765.494146	44.118247
3502.380175	311741.769313	44.123252
3502.505591	311717.678108	44.128257
3502.821122	311689.053359	44.133261
3502.270452	311663.744141	44.138266
3502.476464	311640.098384	44.143271
3502.722898	311618.609241	44.148276
3502.420630	311591.022075	44.153281
3502.409543	311554.228984	44.158285
3502.406097	311547.588325	44.163290
3502.640998	311514.217595	44.168295
3502.443156	311496.207313	44.173300
3502.323004	311470.474752	44.178305
3502.419681	311445.319143	44.183309
3502.481230	311428.388102	44.188314
3502.135044	311393.402818	44.193319
3502.209067	311383.849215	44.198324
3502.166330	311351.819332	44.203329
3502.480893	311327.749388	44.208333
3502.194396	311311.432283	44.213338
3502.715704	311288.017196	44.218343
3502.306261	311264.212562	44.223348
3502.217714	311237.304429	44.228353
3502.498985	311213.417732	44.233357
3502.332845	311195.784098	44.238362
3502.513258	311169.164874	44.243367
3502.596049	311147.319289	44.248372
3502.610205	311116.832620	44.253377
3503.230272	311097.727950	44.258381
3502.774866	311068.866547	44.263386
3502.819982	311031.504487	44.268391
3502.807602	310998.171877	44.273396
3502.918595	310967.975401	44.278401
3502.887327	310937.470240	44.283405
3502.968065	310921.477552	44.288410
3502.741400	310877.236231	44.293415
3502.558014	310853.905145	44.298420
3502.113154	310831.912507	44.303425
3502.450054	310798.118261	44.308429
3502.504507	310783.147477	44.313434
3502.145248	310762.948190	44.318439
3502.553790	310735.275364	44.323444
3502.278037	310711.449651	44.328449
3502.661206	310684.722268	44.333453
3502.470507	310676.889191	44.338458
3502.821184	310646.120837	44.343463
3502.487545	310620.115680	44.348468
3502.551486	310593.158008	44.353473
3502.759915	310564.676486	44.358477
3502.177579	310538.048373	44.363482
3502.446074	310508.259692	44.368487
3502.544546	310476.894309	44.373492
3502.245596	310460.146257	44.378497
3502.462576	310432.910215	44.383501
3502.560225	310406.685148	44.388506
3502.411272	310380.014953	44.393511
3502.462081	310355.731099	44.398516
3502.330460	310338.956967	44.403521
3502.495684	310309.515041	44.408525
3502.331958	310283.559601	44.413530
3502.189058	310259.636651	44.418535
3502.447594	310237.534283	44.423540
3501.770013	310215.297662	44.428545
3502.654235	310202.589576	44.433549
3502.339993	310170.117663	44.438554
3502.602177	310158.193427	44.443559
3502.613072	310135.976868	44.448564
3502.199309	310116.447408	44.453569
3502.684039	310089.296741	44.458573
3502.649438	310062.837599	44.463578
3502.510402	310040.797009	44.468583
3502.401929	310017.046709	44.473588
3502.519806	309983.565892	44.478593
3502.635898	309960.645815	44.483597
3502.547207	309938.393768	44.488602
3502.595730	309903.829469	44.493607
3502.255072	309882.252781	44.498612
3502.722547	309852.916225	44.503617
3502.366695	309825.031017	44.508621
3502.632145	309805.701102	44.513626
3502.840764	309782.079473	44.518631
3502.908739	309757.538177	44.523636
3502.765161	309728.856469	44.528641
3502.689984	309695.303707	44.533645
3502.497279	309674.009267	44.538650
3502.277700	309638.315932	44.543655
3502.828646	309616.778510	44.548660
3502.693569	309594.686207	44.553665
3502.457854	309559.809634	44.558669
3502.376196	309540.966231	44.563674
3502.602923	309509.961972	44.568679
3502.444817	309487.618731	44.573684
3502.278114	309462.375837	44.578689
3501.948439	309439.804801	44.583693
3502.027455	309426.382055	44.588698
3502.170583	309411.422495	44.593703
3502.484323	309379.386723	44.598708
3502.110564	309357.611374	44.603713
3502.297878	309325.926055	44.608717
3501.914398	309315.730712	44.613722
3502.183541	309289.885512	44.618727
3502.064633	309281.761117	44.623732
3502.226590	309264.966376	44.628737
3502.398086	309238.703739	44.633741
3502.144061	309219.479876	44.638746
3502.391393	309184.833235	44.643751
3502.137699	309170.189825	44.648756
3502.269930	309155.180987	44.653761
3502.634943	309134.181234	44.658765
3501.799936	309115.760265	44.663770
3502.175171	309093.537429	44.668775
3502.300942	309066.111235	44.673780
3502.270350	309055.224738	44.678785
3502.497628	309023.991059	44.683789
3502.136260	309010.636728	44.688794
3502.092051	308982.422620	44.693799
3502.190477	308959.886534	44.698804
3502.262804	308939.746562	44.703809
3502.415662	308920.179343	44.708813
3502.165051	308892.379014	44.713818
3502.542861	308878.985965	44.718823
3502.486064	308841.001888	44.723828
3502.086487	308826.304733	44.728833
3502.390004	308798.112751	44.733837
3502.239433	308789.535146	44.738842
3502.340675	308764.860937	44.743847
3502.721971	308739.252470	44.748852
3502.591225	308719.856541	44.753857
3502.427835	308691.482679	44.758861
3502.049984	308678.767013	44.763866
3502.222473	308642.655674	44.768871
3502.544030	308619.448519	44.773876
3502.346991	308605.076048	44.778881
3502.405563	308583.614793	44.783885
3502.097253	308560.251148	44.788890
3502.134073	308544.722570	44.793895
3502.315075	308507.311975	44.798900
3502.202700	308497.481437	44.803905
3502.199093	308468.446389	44.808909
3502.504277	308452.646992	44.813914
3502.212120	308426.685101	44.818919
3502.539191	308411.671165	44.823924
3502.471247	308380.253987	44.828929
3502.550245	308363.370057	44.833933
3502.337814	308341.340121	44.838938
3502.457821	308301.852143	44.843943
3502.588237	308283.484211	44.848948
3502.109219	308265.160211	44.853953
3502.499427	308235.707474	44.858957
3502.431992	308221.620097	44.863962
3502.620327	308194.005547	44.868967
3502.438928	308171.945259	44.873972
3502.283148	308141.457722	44.878977
3502.214750	308111.821797	44.883981
3501.999482	308098.088212	44.888986
3502.170867	308072.919232	44.893991
3502.422484	308068.147001	44.898996
3501.990561	308052.614866	44.904001
3502.326768	308029.812322	44.909005
3502.359665	308000.287808	44.914010
3502.059742	307975.879215	44.919015
3502.309755	307955.965672	44.924020
3502.291849	307948.537883	44.929025
3502.411415	307918.669009	44.934029
3502.205181	307892.108163	44.939034
3502.550461	307874.750013	44.944039
3502.234827	307859.047034	44.949044
3502.296448	307835.854513	44.954049
3502.362184	307807.928001	44.959053
3502.619072	307780.378897	44.964058
3502.462970	307752.283290	44.969063
3502.482370	307734.899458	44.974068
3502.512764	307719.117140	44.979073
3502.635435	307675.174829	44.984077
3502.492902	307657.510792	44.989082
3502.429522	307629.197101	44.994087
3502.560490	307600.115155	44.999092
3502.322524	307582.847664	45.004097
3502.535092	307552.200652	45.009101
3502.500140	307524.696821	45.014106
3502.119011	307506.306412	45.019111
3502.288857	307478.974272	45.024116
3502.220125	307462.240265	45.029121
3502.200247	307435.166659	45.034125
3502.239459	307427.958939	45.039130
3502.274222	307401.691156	45.044135
3502.762908	307379.729829	45.049140
3502.396098	307370.269488	45.054145
3502.737612	307339.475039	45.059149
3502.448463	307313.613892	45.064154
3502.305786	307284.879724	45.069159
3502.330136	307268.080271	45.074164
3502.017200	307241.739269	45.079169
3502.433714	307212.968940	45.084173
3502.226013	307198.953997	45.089178
3502.137896	307175.555436	45.094183
3502.074050	307156.911937	45.099188
3502.161583	307150.918181	45.104193
3502.064482	307116.654521	45.109197
3502.215589	307093.600421	45.114202
3501.912303	307085.529805	45.119207
3502.298446	307068.572192	45.124212
3502.242515	307049.825628	45.129217
3502.255646	307011.778372	45.134221
3502.281985	306997.116190	45.139226
3502.306717	306971.689543	45.144231
3502.759441	306956.121198	45.149236
3502.195130	306932.771176	45.154241
3502.291176	306899.266216	45.159245
3502.533172	306884.901273	45.164250
3502.255586	306861.252115	45.169255
3502.422904	306834.607128	45.174260
3502.397852	306816.135606	45.179265
3502.397032	306789.389518	45.184269
3502.540529	306755.342657	45.189274
3502.408224	306732.078009	45.194279
3502.634865	306715.221443	45.199284
3502.158610	306701.858918	45.204289
3502.158796	306673.102170	45.209293
3501.993210	306657.858987	45.214298
3502.318477	306631.596493	45.219303
3502.329504	306617.852735	45.224308
3502.268326	306598.241565	45.229313
3502.198746	306568.350422	45.234317
3501.848167	306550.896509	45.239322
3501.757887	306534.445482	45.244327
3502.468441	306519.574894	45.249332
3502.464881	306497.435295	45.254337
3502.217590	306469.989377	45.259341
3502.205292	306453.093560	45.264346
3502.250943	306430.386401	45.269351
3502.218061	306408.353120	45.274356
3502.031518	306390.466446	45.279361
3502.336112	306367.108193	45.284365
3502.427869	306352.664683	45.289370
3502.136482	306318.176225	45.294375
3502.209471	306301.954204	45.299380
3501.995913	306277.811281	45.304385
3502.311679	306253.076999	45.309389
3502.255731	306236.111555	45.314394
3502.361914	306212.911351	45.319399
3502.479745	306198.743677	45.324404
3502.215580	306184.075567	45.329409
3502.097226	306144.266696	45.334413
3502.444303	306132.048345	45.339418
3501.879782	306112.617109	45.344423
3502.111199	306097.566468	45.349428
3502.312419	306082.622317	45.354433
3502.234945	306054.538974	45.359437
3502.147631	306034.778959	45.364442
3502.109595	306009.946922	45.369447
3502.117221	305996.890647	45.374452
3501.627857	305977.422214	45.379457
3501.803021	305960.420714	45.384461
3502.049992	305946.589161	45.389466
3502.026942	305927.608022	45.394471
3502.532596	305902.284143	45.399476
3502.223347	305891.287624	45.404481
3502.155943	305864.907695	45.409485
3502.253253	305850.717669	45.414490
3502.047415	305825.988001	45.419495
3502.213066	305800.055304	45.424500
3502.010749	305796.244214	45.429505
3502.337971	305770.439054	45.434509
3502.243933	305747.524286	45.439514
3502.189924	305727.555376	45.444519
3502.322359	305709.517027	45.449524
3502.406999	305687.465147	45.454529
3502.163780	305659.738216	45.459533
3502.002811	305634.390694	45.464538
3502.138884	305622.179607	45.469543
3502.461284	305592.914020	45.474548
3502.165905	305590.873391	45.479553
3502.120291	305555.862636	45.484557
3502.416239	305541.056281	45.489562
3502.348046	305516.254146	45.494567
3502.341437	305490.602590	45.499572
3502.421365	305469.238478	45.504577
3502.290803	305455.592786	45.509581
3502.208824	305428.655016	45.514586
3502.366145	305407.151588	45.519591
3502.693681	305379.844675	45.524596
3502.407168	305367.063055	45.529601
3502.429355	305338.862012	45.534605
3502.383193	305318.051894	45.539610
3502.273151	305304.428418	45.544615
3502.390855	305280.029879	45.549620
3501.940668	305249.484607	45.554625
3502.088487	305226.888260	45.559629
3502.175206	305206.795450	45.564634
3502.054090	305188.236488	45.569639
3502.382347	305155.992163	45.574644
3501.904470	305162.480014	45.579649
3502.089899	305129.316270	45.584653
3502.031699	305122.097931	45.589658
3501.973626	305101.518623	45.594663
3501.959391	305071.897933	45.599668
3501.833699	305060.745425	45.604673
3501.914785	305034.443758	45.609677
3502.061666	305025.081187	45.614682
3501.794622	305010.056895	45.619687
3502.064281	304990.164578	45.624692
3501.867788	304973.831372	45.629697
3502.312272	304960.757752	45.634701
3502.172706	304934.541270	45.639706
3502.120372	304923.453664	45.644711
3502.386625	304900.762396	45.649716
3502.108499	304881.693316	45.654721
3502.223475	304851.390704	45.659725
3502.316369	304838.168168	45.664730
3502.134990	304811.703635	45.669735
3502.217734	304796.064958	45.674740
3502.027238	304784.337133	45.679745
3502.178692	304764.081379	45.684749
3502.218804	304735.851767	45.689754
3502.091004	304724.546816	45.694759
3502.320737	304701.504849	45.699764
3502.180152	304690.430926	45.704769
3502.000537	304659.563253	45.709773
3501.999506	304636.735314	45.714778
3502.136945	304627.908583	45.719783
3502.597463	304598.493691	45.724788
3502.077845	304587.987722	45.729793
3502.268823	304551.590634	45.734797
3502.229091	304542.384263	45.739802
3502.177207	304515.543131	45.744807
3502.103038	304495.704128	45.749812
3502.125272	304479.642126	45.754817
3501.991271	304445.789609	45.759821
3501.888189	304383.301261	45.764826
3501.853801	304276.035907	45.769831
3501.534412	304118.449330	45.774836
3501.210185	303932.969834	45.779841
3500.366545	303686.337546	45.784845
3499.599052	303412.358679	45.789850
3498.843900	303090.987817	45.794855
3498.166727	302735.982655	45.799860
3496.589451	302347.342023	45.804865
3495.442938	301909.714766	45.809869
3494.262514	301440.326123	45.814874
3492.735179	300957.116349	45.819879
3491.640427	300428.251026	45.824884
3490.146695	299867.398693	45.829889
3488.334983	299275.945679	45.834893
3486.675632	298645.393083	45.839898
3484.725684	297990.647551	45.844903
3482.775381	297309.575986	45.849908
3480.694355	296602.579606	45.854913
3479.144394	295871.336317	45.859917
3476.704054	295115.175602	45.864922
3474.148030	294336.241485	45.869927
3472.177775	293531.089456	45.874932
3469.896568	292707.571022	45.879937
3467.097594	291862.663100	45.884941
3464.695340	290999.226429	45.889946
3461.998854	290104.996231	45.894951
3459.353235	289201.708441	45.899956
3456.583155	288287.124480	45.904961
3453.814345	287341.266022	45.909965
3451.307492	286397.415358	45.914970
3448.039092	285435.951225	45.919975
3444.909210	284454.365401	45.924980
3442.168064	283476.269435	45.929985
3439.140368	282476.564352	45.934989
3435.850221	281463.851011	45.939994
3432.879203	280448.833548	45.944999
3429.451591	279409.100665	45.950004
3426.370100	278375.079222	45.955009
3423.098000	277321.519780	45.960013
3420.075735	276281.936500	45.965018
3416.613223	275226.927796	45.970023
3413.633048	274152.301370	45.975028
3409.941900	273083.246230	45.980033
3406.716362	272009.674921	45.985037
3403.639886	270930.643795	45.990042
3399.486763	269845.477958	45.995047
3395.979045	268745.481172	46.000052
3392.618230	267647.842354	46.005057
3389.194320	266550.786653	46.010061
3386.112109	265466.397819	46.015066
3382.557563	264363.685736	46.020071
3378.954388	263243.118972	46.025076
3375.454778	262142.590925	46.030081
3371.918291	261030.394761	46.035085
3368.209953	259914.547621	46.040090
3364.679558	258802.685939	46.045095
3361.284270	257684.426746	46.050100
3357.589527	256574.149790	46.055105
3353.463854	255441.494754	46.060109
3350.256692	254328.067470	46.065114
3346.242666	253202.940506	46.070119
3342.668590	252099.026889	46.075124
3339.446375	250981.196555	46.080129
3335.639745	249858.177714	46.085133
3331.721303	248741.586606	46.090138
3328.116401	247635.330447	46.095143
3324.724701	246528.805334	46.100148
3320.848761	245401.898644	46.105153
3317.490441	244296.986034	46.110157
3313.630682	243174.700240	46.115162
3310.006712	242071.549952	46.120167
3306.203684	240955.713950	46.125172
3302.689142	239843.495864	46.130177
3298.888796	238731.343443	46.135181
3295.319696	237621.188583	46.140186
3291.338161	236506.917443	46.145191
3287.724995	235401.423363	46.150196
3284.170210	234317.209249	46.155201
3280.304432	233214.550635	46.160205
3276.661270	232101.438347	46.165210
3272.601021	231011.922365	46.170215
3268.894370	229917.026792	46.175220
3265.256051	228825.252042	46.180225
3261.374249	227734.533034	46.185229
3257.865843	226647.652097	46.190234
3254.014988	225568.668651	46.195239
3250.306872	224496.692494	46.200244
3246.567682	223409.363672	46.205249
3242.641089	222329.654450	46.210253
3239.197159	221255.932706	46.215258
3235.077509	220184.864266	46.220263
3231.580457	219112.987361	46.225268
3227.713890	218056.985990	46.230273
3223.729310	217002.482264	46.235277
3220.526745	215947.579057	46.240282
3216.441203	214892.917785	46.245287
3212.694801	213829.318130	46.250292
3209.143079	212790.039402	46.255297
3205.382855	211729.097402	46.260301
3201.986610	210688.859332	46.265306
3197.768759	209639.711857	46.270311
3194.281415	208603.138176	46.275316
3190.431584	207564.155000	46.280321
3186.440057	206524.358225	46.285325
3182.795898	205485.225570	46.290330
3178.712063	204454.188992	46.295335
3175.065129	203424.414267	46.300340
3171.802273	202409.916919	46.305345
3167.417497	201393.384378	46.310349
3163.930207	200369.256472	46.315354
3159.818972	199367.719446	46.320359
3156.264093	198366.560711	46.325364
3152.708027	197354.840243	46.330369
3148.712392	196360.716156	46.335373
3145.156938	195368.135040	46.340378
3141.194595	194384.512199	46.345383
3137.765724	193391.977120	46.350388
3133.808131	192412.264920	46.355393
3130.007125	191427.392163	46.360397
3126.506721	190453.659990	46.365402
3122.584580	189476.793041	46.370407
3118.864242	188507.211539	46.375412
3115.212633	187538.977524	46.380417
3111.080810	186570.394106	46.385421
3107.600497	185604.315628	46.390426
3103.487212	184667.017075	46.395431
3100.412828	183707.259588	46.400436
3096.471067	182762.058791	46.405441
3092.497233	181818.400164	46.410445
3088.880507	180873.906191	46.415450
3084.826252	179937.103399	46.420455
3081.429959	178995.828543	46.425460
3077.439593	178067.590965	46.430465
3073.731661	177146.576081	46.435469
3070.062928	176218.805173	46.440474
3066.112618	175300.751024	46.445479
3062.060672	174389.992174	46.450484
3058.536215	173475.775410	46.455489
3054.698544	172580.522334	46.460493
3050.969772	171673.360204	46.465498
3046.994470	170786.946042	46.470503
3043.282939	169895.307694	46.475508
3039.557004	169010.836453	46.480513
3035.178379	168132.256783	46.485517
3031.761228	167258.133628	46.490522
3027.577952	166404.990828	46.495527
3024.097527	165534.807070	46.500532
3020.433241	164683.845287	46.505537
3016.507809	163832.374914	46.510541
3012.678190	162972.474420	46.515546
3008.702274	162136.893538	46.520551
3004.917026	161298.391862	46.525556
3001.183191	160471.386582	46.530561
2997.379035	159645.739593	46.535565
2993.683660	158818.813958	46.540570
2989.657853	158020.218497	46.545575
2985.894668	157205.480083	46.550580
2981.898558	156406.214249	46.555585
2977.650070	155612.560190	46.560589
2973.946180	154816.528674	46.565594
2970.089472	154033.500287	46.570599
2966.470635	153257.623322	46.575604
2962.443769	152511.994330	46.580609
2958.350282	151747.296664	46.585613
2954.570897	150992.372345	46.590618
2950.479209	150240.103103	46.595623
2946.599207	149508.121268	46.600628
2942.651976	148781.809949	46.605633
2938.277439	148059.939803	46.610637
2934.648628	147341.844650	46.615642
2930.534086	146643.991068	46.620647
2926.699647	145940.186395	46.625652
2922.861472	145263.176959	46.630657
2919.198151	144592.918677	46.635661
2915.230997	143909.343577	46.640666
2911.299704	143246.550463	46.645671
2907.283218	142577.468507	46.650676
2903.686414	141925.481779	46.655681
2899.502826	141279.078900	46.660685
2895.436203	140628.887673	46.665690
2891.447379	140011.416942	46.670695
2887.862702	139395.876115	46.675700
2884.017432	138775.561943	46.680705
2879.673099	138177.140167	46.685709
2875.984994	137574.667292	46.690714
2872.143628	136985.342774	46.695719
2868.375812	136404.970738	46.700724
2864.295335	135816.029266	46.705729
2860.620425	135243.494317	46.710733
2857.162365	134682.433247	46.715738
2853.323313	134124.936903	46.720743
2850.080195	133559.238622	46.725748
2846.027249	132916.876172	46.730753
2842.373281	132362.375453	46.735757
2838.567506	131816.415618	46.740762
2834.753740	131276.137303	46.745767
2831.072794	130735.959575	46.750772
2827.597062	130199.114881	46.755777
2823.778213	129666.820559	46.760781
2819.872125	129135.004418	46.765786
2816.594764	128618.030235	46.770791
2813.027349	128085.704031	46.775796
2809.582570	127568.578082	46.780801
2805.826932	127042.043752	46.785805
2802.403724	126527.305984	46.790810
2798.728808	126011.125715	46.795815
2795.120015	125490.820767	46.800820
2791.710710	124980.869913	46.805825
2787.832474	124469.510399	46.810829
2784.627638	123947.000315	46.815834
2780.715688	123438.927820	46.820839
2777.482538	122934.978578	46.825844
2773.941906	122431.490572	46.830849
2770.317550	121921.472393	46.835853
2767.343829	121403.919817	46.840858
2763.161089	120901.886728	46.845863
2759.374579	120386.661562	46.850868
2756.425133	119893.148219	46.855873
2752.613476	119397.142986	46.860877
2749.380639	118883.937370	46.865882
2745.767308	118388.473917	46.870887
2742.336674	117882.014251	46.875892
2738.993757	117369.100602	46.880897
2734.971843	116880.854343	46.885901
2731.791706	116368.157956	46.890906
2727.962838	115872.723097	46.895911
2724.402439	115358.357782	46.900916
2720.817307	114870.960085	46.905921
2716.950317	114373.872878	46.910925
2713.973069	113876.348815	46.915930
2710.402364	113386.590970	46.920935
2706.657334	112885.321945	46.925940
2703.042909	112384.064998	46.930945
2699.527622	111898.743397	46.935949
2695.999213	111401.504550	46.940954
2692.360210	110919.343221	46.945959
2688.704840	110430.020414	46.950964
2685.016900	109936.361404	46.955969
2681.513433	109460.250622	46.960973
2678.075526	108977.576066	46.965978
2673.967635	108495.851528	46.970983
2670.269622	108010.713686	46.975988
2666.946681	107546.487623	46.980993
2662.791327	107082.715180	46.985997
2659.498142	106604.475246	46.991002
2655.489369	106146.286159	46.996007
2651.914477	105680.967821	47.001012
2648.052656	105224.992923	47.006017
2644.282136	104782.319158	47.011021
2640.545097	104331.116562	47.016026
2636.779012	103898.127274	47.021031
2633.190203	103453.497964	47.026036
2629.306289	103014.602369	47.031041
2625.414415	102591.780393	47.036045
2621.882063	102158.180037	47.041050
2618.129123	101743.977909	47.046055
2614.570894	101328.466967	47.051060
2610.987581	100912.799983	47.056065
2607.046259	100506.955365	47.061069
2603.559910	100092.478537	47.066074
2599.983942	99687.743934	47.071079
2596.222611	99286.805304	47.076084
2592.293087	98879.695648	47.081089
2588.818944	98483.945947	47.086093
2585.468756	98089.160466	47.091098
2581.907023	97699.229504	47.096103
2578.798839	97300.768687	47.101108
2575.088021	96907.452008	47.106113
2571.645804	96520.643314	47.111117
2568.082655	96111.427990	47.116122
2564.578004	95734.932449	47.121127
2561.303825	95333.319952	47.126132
2557.665795	94945.531863	47.131137
2554.302881	94553.779127	47.136141
2550.546085	94146.373432	47.141146
2547.024932	93759.153863	47.146151
2543.934147	93363.523560	47.151156
2540.360075	92973.679033	47.156161
2536.808084	92572.844590	47.161165
2533.493035	92175.638078	47.166170
2529.730863	91785.863432	47.171175
2526.470236	91387.870956	47.176180
2523.249101	90994.477228	47.181185
2519.611855	90595.219669	47.186189
2516.154333	90190.526747	47.191194
2512.649766	89789.620210	47.196199
2509.106958	89397.504536	47.201204
2505.991351	88994.464454	47.206209
2502.222912	88594.796677	47.211213
2498.804738	88178.093179	47.216218
2495.460519	87779.653619	47.221223
2491.931297	87368.810375	47.226228
2488.536790	86960.772320	47.231233
2484.870129	86560.773328	47.236237
2481.329821	86150.749299	47.241242
2477.855305	85737.925945	47.246247
2474.470735	85333.974417	47.251252
2471.039698	84928.320780	47.256257
2467.607859	84523.524110	47.261261
2464.110560	84105.468444	47.266266
2460.475908	83708.425708	47.271271
2457.298749	83292.707574	47.276276
2453.753495	82876.189009	47.281281
2449.881229	82468.873252	47.286285
2446.691378	82056.287311	47.291290
2443.100550	81647.859890	47.296295
2439.735705	81236.951750	47.301300
2436.054973	80819.112814	47.306305
2432.701073	80410.895157	47.311309
2429.087839	79998.252939	47.316314
2425.744490	79580.468958	47.321319
2422.239884	79172.445339	47.326324
2418.552193	78748.326184	47.331329
2415.142196	78336.451843	47.336333
2411.265589	77912.400363	47.341338
2408.170970	77502.673918	47.346343
2404.713172	77088.565112	47.351348
2400.940445	76675.286296	47.356353
2397.514746	76267.623809	47.361357
2394.280903	75849.155735	47.366362
2390.469892	75425.081984	47.371367
2387.027424	75009.618318	47.376372
2383.730963	74587.268255	47.381377
2380.046244	74170.826659	47.386381
2376.654135	73754.066645	47.391386
2373.191022	73343.889209	47.396391
2369.492824	72926.999301	47.401396
2366.397088	72506.073146	47.406401
2362.890510	72083.274880	47.411405
2359.532432	71654.657533	47.416410
2355.529471	71234.438852	47.421415
2352.081125	70815.461090	47.426420
2348.776407	70393.439485	47.431425
2345.238988	69985.179670	47.436429
2341.878531	69553.245210	47.441434
2338.451479	69133.865853	47.446439
2334.843550	68718.450871	47.451444
2331.436416	68278.597231	47.456449
2327.741251	67855.490677	47.461453
2324.173572	67425.991816	47.466458
2320.768211	67006.421594	47.471463
2317.322143	66580.650407	47.476468
2313.390467	66156.834397	47.481473
2310.146283	65730.595369	47.486477
2306.990061	65306.603076	47.491482
2303.226394	64882.458556	47.496487
2299.797639	64457.431262	47.501492
2296.008233	64032.930611	47.506497
2292.492894	63618.041565	47.511501
2289.377644	63183.904898	47.516506
2286.140084	62759.993706	47.521511
2282.317043	62319.921330	47.526516
2279.053703	61882.669931	47.531521
2275.135990	61468.082497	47.536525
2271.801110	61035.204395	47.541530
2268.350177	60608.755071	47.546535
2264.726552	60183.050779	47.551540
2261.557554	59746.159034	47.556545
2258.099004	59323.153681	47.561549
2254.672787	58884.236055	47.566554
2251.087030	58450.173717	47.571559
2247.894543	58023.374100	47.576564
2243.785237	57579.903611	47.581569
2240.121182	57149.150983	47.586573
2236.800838	56710.992440	47.591578
2233.323687	56283.532004	47.596583
2229.758119	55841.144793	47.601588
2226.224721	55410.955141	47.606593
2222.811409	54983.831673	47.611597
2219.793854	54540.641088	47.616602
2216.189520	54112.040433	47.621607
2212.087698	53675.785133	47.626612
2208.918340	53235.281880	47.631617
2205.270940	52803.799870	47.636621
2201.619297	52368.786643	47.641626
2198.196755	51935.820256	47.646631
2194.593814	51503.505325	47.651636
2191.332834	51068.867932	47.656641
2187.321208	50639.043236	47.661645
2184.482430	50202.282155	47.666650
2180.885640	49773.804527	47.671655
2177.493096	49338.008692	47.676660
2173.721218	48898.867726	47.681665
2170.437318	48465.646783	47.686669
2166.736778	48018.646668	47.691674
2163.064317	47590.278824	47.696679
2159.704288	47156.917060	47.701684
2156.211935	46712.314032	47.706689
2152.499562	46286.057336	47.711693
2148.957559	45853.789009	47.716698
2145.641528	45414.511431	47.721703
2141.694051	44981.961516	47.726708
2138.466290	44549.954807	47.731713
2135.160550	44117.797380	47.736717
2131.448564	43685.939859	47.741722
2127.910159	43254.196893	47.746727
2124.357072	42810.727200	47.751732
2120.892568	42372.896116	47.756737
2117.140728	41939.290746	47.761741
2114.085451	41516.333101	47.766746
2110.632554	41079.090305	47.771751
2107.040495	40642.619745	47.776756
2103.988853	40208.812850	47.781761
2100.178796	39775.595468	47.786765
2096.640043	39335.294288	47.791770
2093.183583	38895.832466	47.796775
2089.984672	38468.074587	47.801780
2086.528580	38016.838447	47.806785
2082.618052	37583.965916	47.811789
2079.324985	37137.946697	47.816794
2075.878284	36686.971614	47.821799
2072.311142	36261.838070	47.826804
2069.389872	35797.449628	47.831809
2065.135380	35364.789712	47.836813
2061.799714	34917.822032	47.841818
2058.023097	34481.866648	47.846823
2054.690798	34049.235908	47.851828
2051.111836	33599.519689	47.856833
2047.686678	33159.398000	47.861837
2044.402205	32724.733484	47.866842
2040.940366	32279.711250	47.871847
2037.139901	31836.760320	47.876852
2033.613723	31393.167706	47.881857
2030.277478	30952.806205	47.886861
2026.653294	30503.810190	47.891866
2023.407486	30059.765205	47.896871
2019.469346	29618.340727	47.901876
2016.121067	29176.523404	47.906881
2012.306329	28750.529140	47.911885
2008.828440	28293.244538	47.916890
2005.279076	27855.010281	47.921895
2001.690907	27412.127802	47.926900
1998.514582	26977.846377	47.931905
1994.744196	26546.676421	47.936909
1991.536021	26101.311278	47.941914
1987.824682	25666.799087	47.946919
1983.913860	25224.236441	47.951924
1980.422099	24785.331036	47.956929
1977.168795	24356.566701	47.961933
1973.546020	23914.583655	47.966938
1970.088494	23482.600760	47.971943
1966.578459	23056.907200	47.976948
1963.300166	22616.597140	47.981953
1959.428491	22189.527730	47.986957
1956.462665	21739.306115	47.991962
1952.518409	21308.972953	47.996967
1948.708048	20872.863993	48.001972
1945.529605	20432.897435	48.006977
1941.823332	20004.785446	48.011981
1938.287819	19577.771030	48.016986
1934.769598	19141.446087	48.021991
1930.943070	18714.540181	48.026996
1927.527693	18284.343171	48.032001
1924.188854	17862.446970	48.037005
1920.580580	17418.625198	48.042010
1916.865004	16998.820452	48.047015
1913.132128	16577.349271	48.052020
1909.921142	16153.823887	48.057025
1906.344061	15725.745048	48.062029
1902.868926	15305.857500	48.067034
1899.455640	14881.593780	48.072039
1895.962974	14454.980369	48.077044
1892.380681	14035.251415	48.082049
1888.607871	13607.494306	48.087053
1885.248743	13185.511001	48.092058
1881.634177	12767.458243	48.097063
1878.010908	12347.877492	48.102068
1874.546547	11931.317303	48.107073
1870.559099	11507.110801	48.112077
1866.992125	11093.237991	48.117082
1863.585572	10684.534516	48.122087
1859.574925	10272.081598	48.127092
1855.748666	9871.922537	48.132097
1852.192489	9476.873716	48.137101
1848.587175	9076.235227	48.142106
1844.699098	8684.888633	48.147111
1840.343260	8303.691425	48.152116
1836.666651	7936.898760	48.157121
1832.614684	7581.777928	48.162125
1828.928770	7217.859023	48.167130
1825.111583	6857.097828	48.172135
1820.687756	6506.606749	48.177140
1816.859901	6171.404102	48.182145
1812.717644	5831.756296	48.187149
1809.394496	5507.285293	48.192154
1805.760261	5179.089936	48.197159
1802.093931	4859.769389	48.202164
1798.659282	4542.924670	48.207169
1794.611731	4229.940224	48.212173
1790.775043	3916.460033	48.217178
1787.246725	3632.707334	48.222183
1783.612466	3325.746556	48.227188
1780.214533	3024.057465	48.232193
1776.501171	2743.881978	48.237197
1772.663426	2452.285547	48.242202
1769.334967	2169.695490	48.247207
1765.644542	1883.907263	48.252212
1761.748848	1601.215108	48.257217
1758.055103	1337.511217	48.262221
1754.165027	1069.437642	48.267226
1750.024586	818.033041	48.272231
1745.404704	601.878578	48.277236
1741.076345	382.799181	48.282241
1736.223077	182.125329	48.287245
1730.652178	25.063119	48.292250
1718.300383	65.747513	48.297255
1709.927591	82.388567	48.302260
1705.188962	63.103216	48.307265
1702.515891	69.796292	48.312269
1700.689371	75.639450	48.317274
1698.850164	72.249715	48.322279
1696.058962	78.948526	48.327284
1693.997449	69.506416	48.332289
1691.180253	75.927701	48.337293
1687.932183	69.118980	48.342298
1684.494686	71.938435	48.347303
1681.041707	81.154156	48.352308
1677.818615	74.493405	48.357313
1673.722376	79.816644	48.362317
1670.708107	76.122589	48.367322
1666.792671	65.165719	48.372327
1663.461116	75.419218	48.377332
1660.199867	71.146682	48.382337
1656.677571	68.702273	48.387341
1653.893457	72.729810	48.392346
1651.247757	58.879844	48.397351
1647.125490	71.404564	48.402356
1643.772835	72.530887	48.407361
1640.179847	76.529300	48.412365
1636.621197	72.575134	48.417370
1633.794913	71.003147	48.422375
1629.911339	76.910211	48.427380
1626.636185	66.859752	48.432385
1623.023030	71.952781	48.437389
1619.793542	62.980370	48.442394
1616.193092	64.107298	48.447399
1612.538269	78.017737	48.452404
1609.451825	60.281742	48.457409
1605.610841	71.933793	48.462413
1602.325203	75.384504	48.467418
1598.902391	70.668894	48.472423
1595.497820	76.757666	48.477428
1592.254779	65.009633	48.482433
1588.566722	78.703785	48.487437
1584.891193	72.667116	48.492442
1581.927163	82.259147	48.497447
1578.223223	67.064809	48.502452
1574.773387	66.551646	48.507457
1571.182657	68.822327	48.512461
1567.500535	72.685922	48.517466
1564.399917	67.315902	48.522471
1560.668188	76.730030	48.527476
1557.426590	69.664061	48.532481
1553.789945	79.980866	48.537485
1550.106110	71.870105	48.542490
1547.072870	65.527835	48.547495
1543.042055	73.599647	48.552500
1540.137179	73.368656	48.557505
1536.655397	69.206391	48.562509
1533.568249	76.318256	48.567514
1529.792496	72.337785	48.572519
1526.120547	79.803260	48.577524
1522.823830	78.481670	48.582529
1519.067124	69.673588	48.587533
1515.566392	67.769995	48.592538
1512.626361	75.017147	48.597543
1508.515568	66.998159	48.602548
1504.915538	56.827453	48.607553
1501.299520	68.374885	48.612557
1498.203591	68.999362	48.617562
1494.816377	69.162983	48.622567
1491.187157	75.451237	48.627572
1487.997572	65.137553	48.632577
1484.307881	65.000248	48.637581
1480.635698	63.714958	48.642586
1477.256340	61.279961	48.647591
1473.731000	66.738973	48.652596
1470.441150	62.417133	48.657601
1466.748110	72.625655	48.662605
1463.048668	72.410778	48.667610
1459.978026	60.790961	48.672615
1456.406849	68.114201	48.677620
1452.784105	64.945145	48.682625
1449.375492	74.780374	48.687629
1445.988432	74.488402	48.692634
1442.454718	65.316603	48.697639
1438.541572	74.743151	48.702644
1435.653816	66.960913	48.707649
1432.037838	68.713525	48.712653
1428.319559	68.916028	48.717658
1424.925129	63.291208	48.722663
1421.155287	67.415234	48.727668
1417.804930	61.226745	48.732673
1414.435653	62.286073	48.737677
1411.250842	68.555776	48.742682
1407.846367	67.146570	48.747687
1403.369572	71.431254	48.752692
1400.475244	64.798469	48.757697
1397.115279	65.087570	48.762701
1393.690197	70.331670	48.767706
1390.140905	64.256404	48.772711
1386.170939	70.388894	48.777716
1382.915135	66.023801	48.782721
1379.364467	64.365275	48.787725
1375.912827	64.943890	48.792730
1372.629642	68.106336	48.797735
1368.775504	68.054750	48.802740
1366.001159	59.327910	48.807745
1361.874690	74.608869	48.812749
1358.509885	71.127597	48.817754
1355.270419	69.967954	48.822759
1351.427949	83.537447	48.827764
1348.012991	70.901906	48.832769
1344.490207	68.270952	48.837773
1341.090727	67.269093	48.842778
1337.783291	59.947659	48.847783
1333.609678	69.057252	48.852788
1330.323486	63.143521	48.857793
1327.056300	68.597161	48.862797
1323.792317	72.069828	48.867802
1320.408154	61.859228	48.872807
1316.253634	73.243714	48.877812
1312.922478	67.045922	48.882817
1309.142001	64.515194	48.887821
1305.801223	68.281384	48.892826
1302.759169	66.366533	48.897831
1299.045499	76.236593	48.902836
1295.648794	66.420245	48.907841
1291.809624	67.381885	48.912845
1288.429362	73.318192	48.917850
1284.997357	66.604601	48.922855
1281.548442	79.995775	48.927860
1277.944851	71.407509	48.932865
1274.366206	70.091865	48.937869
1271.093561	72.670558	48.942874
1267.688222	62.460100	48.947879
1264.131661	72.641055	48.952884
1260.691611	65.106160	48.957889
1257.350057	73.282667	48.962893
1253.585557	72.369271	48.967898
1250.285957	71.184200	48.972903
1246.486786	74.192857	48.977908
1243.023740	59.663451	48.982913
1239.071701	64.511863	48.987917
1236.099142	62.959519	48.992922
1232.817730	56.200354	48.997927
1229.122436	50.400940	49.002932
1225.638411	65.882442	49.007937
1222.269133	52.876007	49.012941
1218.117240	65.531886	49.017946
1215.071578	57.859685	49.022951
1211.248371	64.877321	49.027956
1207.795837	68.955138	49.032961
1204.472962	57.032955	49.037965
1200.972666	68.306116	49.042970
1197.717871	57.376229	49.047975
1193.884636	69.973020	49.052980
1190.641862	67.190935	49.057985
1187.233640	56.762650	49.062989
1183.398427	72.409549	49.067994
1180.070938	64.455358	49.072999
1176.325517	66.209160	49.078004
1173.169813	66.491798	49.083009
1169.616071	65.216583	49.088013
1165.987228	59.644110	49.093018
1162.697587	59.912797	49.098023
1158.804282	64.818511	49.103028
1155.366380	67.729814	49.108033
1151.952012	59.966320	49.113037
1148.412150	55.414528	49.118042
1145.157406	57.275449	49.123047
1141.245792	66.208229	49.128052
1137.851751	61.010492	49.133057
1134.573870	59.818890	49.138061
1130.828772	65.603188	49.143066
1127.684344	56.386675	49.148071
1123.978154	70.105784	49.153076
1120.432003	60.527866	49.158081
1117.134048	65.062508	49.163085
1113.632656	61.197580	49.168090
1110.005589	64.413572	49.173095
1106.025938	70.860795	49.178100
1103.204409	61.666787	49.183105
1099.821207	59.795571	49.188109
1095.908521	61.800039	49.193114
1092.713556	64.062939	49.198119
1088.912506	60.662266	49.203124
1085.163907	57.845040	49.208129
1081.759266	70.520648	49.213133
1077.956035	71.024309	49.218138
1075.415932	64.425017	49.223143
1071.673805	65.991658	49.228148
1067.959280	65.589352	49.233153
1064.585066	64.602574	49.238157
1061.150302	67.842421	49.243162
1057.790044	61.614401	49.248167
1053.982058	69.066269	49.253172
1050.029426	62.063607	49.258177
1046.982388	51.765789	49.263181
1043.401882	59.175916	49.268186
1039.773421	60.323079	49.273191
1036.576208	69.261719	49.278196
1033.024787	63.319718	49.283201
1029.885817	62.590549	49.288205
1025.650221	59.637170	49.293210
1022.267219	63.378316	49.298215
1018.939360	64.842514	49.303220
1015.561479	63.308994	49.308225
1012.201756	63.984067	49.313229
1008.373525	56.218585	49.318234
1005.419133	58.232078	49.323239
1000.899923	68.543902	49.328244
997.895897	63.449987	49.333249
994.398859	63.149875	49.338253
990.992674	65.958181	49.343258
987.817413	63.152959	49.348263
983.757691	67.056394	49.353268
979.967464	52.527367	49.358273
976.997040	55.495626	49.363277
973.187402	67.095348	49.368282
969.859246	61.257806	49.373287
966.556711	55.634574	49.378292
962.860753	63.334756	49.383297
959.249388	62.055882	49.388301
956.036881	68.715887	49.393306
952.733537	53.940237	49.398311
949.141711	59.241954	49.403316
945.318984	66.996672	49.408321
941.631712	60.680373	49.413325
938.209731	62.760331	49.418330
934.754348	61.004773	49.423335
931.455862	57.911864	49.428340
927.931715	63.633309	49.433345
924.643730	63.484157	49.438349
920.755110	63.311446	49.443354
917.598655	49.237427	49.448359
913.806730	59.116508	49.453364
910.374071	48.976819	49.458369
906.874411	49.588266	49.463373
902.590318	58.582201	49.468378
899.919747	50.715629	49.473383
896.410320	60.006582	49.478388
893.075650	61.079556	49.483393
889.536214	59.023884	49.488397
885.837580	73.573868	49.493402
882.309941	64.996003	49.498407
878.647340	61.652903	49.503412
875.017583	64.347328	49.508417
871.815518	57.091828	49.513421
868.379299	60.233842	49.518426
865.145870	55.969743	49.523431
861.311151	62.827846	49.528436
857.826500	59.257736	49.533441
854.476683	58.254532	49.538445
850.889832	55.779150	49.543450
847.526822	49.478833	49.548455
843.634557	62.132269	49.553460
840.280649	60.721587	49.558465
836.785741	59.848536	49.563469
833.127743	64.894815	49.568474
829.925373	56.984487	49.573479
826.259863	56.175958	49.578484
822.478121	49.523223	49.583489
819.469164	51.364894	49.588493
815.598466	56.884034	49.593498
812.704699	54.474770	49.598503
808.847547	50.402685	49.603508
805.035540	62.249544	49.608513
801.857785	58.163444	49.613517
797.766102	60.543815	49.618522
794.707261	58.989133	49.623527
791.417227	65.094915	49.628532
787.937038	55.003774	49.633537
784.452096	52.816251	49.638541
780.566213	59.432392	49.643546
777.417476	54.120600	49.648551
773.774869	54.235472	49.653556
770.341572	48.389026	49.658561
766.639496	46.570657	49.663565
763.128769	51.856598	49.668570
759.794499	56.510809	49.673575
756.041542	55.548228	49.678580
752.922149	59.121812	49.683585
749.397751	50.847189	49.688589
745.518986	59.227558	49.693594
742.010426	43.674012	49.698599
738.130740	61.507595	49.703604
735.055734	55.728761	49.708609
731.924237	50.971101	49.713613
728.229848	50.701743	49.718618
724.874171	54.068508	49.723623
720.777148	61.622335	49.728628
717.634546	57.540267	49.733633
714.477600	54.232371	49.738637
710.540330	57.284724	49.743642
707.039334	54.106316	49.748647
703.536203	60.058618	49.753652
700.540116	56.073964	49.758657
696.968485	51.021002	49.763661
693.390002	58.076503	49.768666
690.003613	50.773803	49.773671
686.045650	57.388517	49.778676
682.453485	56.862813	49.783681
679.102350	57.406874	49.788685
675.448347	65.764916	49.793690
672.203481	58.228218	49.798695
668.701050	56.666679	49.803700
664.955941	61.062159	49.808705
661.776639	55.002188	49.813709
658.008322	59.540483	49.818714
654.615572	55.380310	49.823719
651.120636	52.795739	49.828724
647.477148	51.907879	49.833729
644.244323	55.657314	49.838733
640.379447	53.655505	49.843738
637.218173	50.655171	49.848743
633.697377	53.873647	49.853748
630.301370	55.756607	49.858753
626.991735	48.264806	49.863757
623.008256	57.559967	49.868762
619.630019	56.137284	49.873767
616.063645	54.212393	49.878772
613.000656	49.235284	49.883777
609.454381	55.586603	49.888781
605.435920	52.843099	49.893786
601.774039	57.665380	49.898791
598.751388	55.140168	49.903796
594.959020	52.861329	49.908801
591.474514	50.012559	49.913805
587.837655	53.964098	49.918810
584.393374	52.308099	49.923815
581.066894	56.337868	49.928820
577.478821	52.239752	49.933825
573.857903	54.531045	49.938829
570.456415	56.911563	49.943834
566.870761	56.536717	49.948839
563.494877	53.591949	49.953844
559.572716	54.294521	49.958849
556.709065	47.663424	49.963853
553.006502	55.535495	49.968858
549.863881	54.152071	49.973863
546.430019	51.048657	49.978868
542.241082	56.364271	49.983873
539.152597	45.218817	49.988877
535.426488	61.218868	49.993882
532.057550	57.928182	49.998887
528.710048	59.237306	50.003892
524.625588	57.832833	50.008897
521.795110	59.045649	50.013901
517.793293	60.972315	50.018906
514.883139	53.399360	50.023911
511.199307	68.405771	50.028916
506.855736	65.032704	50.033921
503.538651	62.316065	50.038925
500.192180	59.936188	50.043930
497.405779	49.452375	50.048935
493.906023	55.100453	50.053940
490.067045	59.614966	50.058945
486.652143	54.651533	50.063949
482.482066	62.197771	50.068954
479.295874	55.477695	50.073959
476.050906	60.956401	50.078964
472.553222	52.876986	50.083969
469.098611	60.786393	50.088973
465.279838	60.277015	50.093978
461.726293	60.140787	50.098983
458.399528	56.764456	50.103988
455.339352	59.598038	50.108993
451.621649	56.311042	50.113997
447.809673	61.811585	50.119002
444.568362	56.264328	50.124007
440.829907	61.747098	50.129012
437.258751	63.707967	50.134017
433.926402	58.975293	50.139021
430.372328	61.015758	50.144026
427.508550	57.054838	50.149031
423.483916	59.766496	50.154036
419.349682	62.814748	50.159041
416.052799	59.610936	50.164045
412.377627	63.951263	50.169050
409.418397	56.060108	50.174055
406.342458	62.664081	50.179060
402.211901	65.521943	50.184065
398.883428	57.653473	50.189069
395.269508	70.921639	50.194074
391.816986	61.408389	50.199079
388.607276	62.461966	50.204084
385.172263	57.745283	50.209089
381.514147	55.356996	50.214093
377.985472	56.656379	50.219098
374.145130	50.724680	50.224103
371.114863	53.974381	50.229108
367.242754	58.066970	50.234113
363.673973	48.885036	50.239117
359.984743	46.495270	50.244122
356.817978	48.722212	50.249127
353.382475	53.183415	50.254132
349.808522	62.155420	50.259137
346.499169	54.369405	50.264141
342.676397	59.678655	50.269146
339.424746	57.809209	50.274151
336.079199	59.959587	50.279156
332.261554	58.858447	50.284161
328.981623	48.726743	50.289165
325.050019	56.248522	50.294170
322.233570	47.332276	50.299175
318.307675	43.059018	50.304180
314.147462	52.119129	50.309185
311.247332	47.875994	50.314189
307.490710	61.156881	50.319194
304.332028	44.593553	50.324199
300.748341	59.748879	50.329204
297.375063	62.327510	50.334209
294.481879	55.435304	50.339213
290.387577	56.661411	50.344218
286.776073	60.441362	50.349223
283.414684	53.909945	50.354228
279.534242	70.351638	50.359233
276.140479	56.789263	50.364237
272.469341	54.368222	50.369242
269.241982	56.743809	50.374247
265.731128	56.923657	50.379252
262.241921	67.037215	50.384257
258.843682	62.805196	50.389261
255.080523	64.058846	50.394266
251.576965	56.815598	50.399271
248.288438	66.768202	50.404276
244.463140	69.312813	50.409281
241.492173	63.473570	50.414285
237.804289	63.804367	50.419290
234.101040	59.964680	50.424295
230.777409	66.120024	50.429300
226.740046	64.224228	50.434305
223.954867	51.240982	50.439309
220.358695	58.378364	50.444314
216.863301	57.749078	50.449319
213.520860	49.661367	50.454324
209.340207	65.963140	50.459329
206.231205	57.206350	50.464333
202.608758	60.155970	50.469338
199.204712	63.147516	50.474343
195.586167	60.914445	50.479348
192.057117	61.638123	50.484353
189.057958	57.027619	50.489357
185.184017	57.934705	50.494362
181.321981	65.698764	50.499367
178.125143	63.305130	50.504372
174.796508	67.601023	50.509377
170.612183	59.793082	50.514381
167.628717	57.543396	50.519386
164.338718	50.675032	50.524391
160.782532	48.343678	50.529396
156.966434	50.921667	50.534401
153.749312	49.062692	50.539405
150.153133	61.138560	50.544410
146.786105	53.355237	50.549415
143.343948	51.562937	50.554420
139.592590	58.329029	50.559425
136.469612	46.860012	50.564429
132.628616	61.074668	50.569434
129.040737	57.751698	50.574439
125.595413	54.105986	50.579444
121.703491	59.530428	50.584449
118.651157	43.542199	50.589453
115.150399	50.591968	50.594458
111.705465	59.759030	50.599463
108.170961	51.198221	50.604468
104.259952	58.539651	50.609473
100.783104	54.155391	50.614477
97.388179	55.313768	50.619482
94.096937	57.152007	50.624487
90.777293	56.618759	50.629492
87.333892	48.752432	50.634497
83.380419	53.357581	50.639501
79.777985	56.889377	50.644506
76.536665	46.245533	50.649511
73.200366	50.194623	50.654516
69.574485	59.971974	50.659521
65.927493	48.318811	50.664525
62.446100	53.524320	50.669530
59.119098	52.887822	50.674535
55.798346	47.166351	50.679540
52.141490	51.029315	50.684545
48.670061	52.044590	50.689549
44.902067	49.315976	50.694554
41.635257	55.589032	50.699559
37.906763	58.738675	50.704564
34.308806	58.853027	50.709569
30.900098	46.719862	50.714573
27.763092	49.378792	50.719578
24.271740	55.247061	50.724583
20.692749	47.132949	50.729588
16.956425	42.691035	50.734593
13.619367	37.089169	50.739597
9.502739	48.486790	50.744602
6.469685	43.176102	50.749607
2.911536	44.056194	50.754612