Fri Aug 26 10:52:53 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
3.086648	103.800885	0.000000
2.846036	99.102574	0.005005
2.790716	92.954931	0.010010
2.679452	89.030563	0.015014
2.523968	88.343179	0.020019
2.158570	74.825037	0.025024
1.824160	78.521870	0.030029
2.122740	71.727529	0.035034
1.401426	73.194112	0.040038
1.783399	64.004555	0.045043
1.209047	53.122653	0.050048
0.664469	46.649418	0.055053
0.447390	39.100172	0.060058
-0.067029	36.266773	0.065062
-0.395658	26.694344	0.070067
-0.350634	36.191173	0.075072
-0.568303	34.545396	0.080077
-0.699969	26.359617	0.085082
-1.480745	30.024701	0.090086
-1.347217	24.113426	0.095091
-1.883847	18.069221	0.100096
-2.481639	8.804456	0.105101
-2.505208	5.904130	0.110106
-2.859926	17.399339	0.115110
-2.786262	14.037797	0.120115
-3.004959	18.317695	0.125120
-3.101652	3.283511	0.130125
-3.872286	14.153800	0.135130
-4.251273	15.820172	0.140134
-4.294713	12.530646	0.145139
-4.590496	15.180611	0.150144
-4.858085	9.303321	0.155149
-4.469316	5.168245	0.160154
-5.371363	9.545046	0.165158
-5.598875	6.996001	0.170163
-5.552546	17.527128	0.175168
-6.041283	14.439807	0.180173
-5.899163	10.865134	0.185178
-6.751797	13.646091	0.190182
-7.302379	11.071419	0.195187
-7.511257	14.394366	0.200192
-7.155532	12.168949	0.205197
-7.096563	7.506274	0.210202
-7.488512	16.223270	0.215206
-7.511413	18.640930	0.220211
-7.928081	13.274052	0.225216
-8.686537	9.485269	0.230221
-8.675307	9.951972	0.235226
-8.839791	17.839477	0.240230
-8.941473	9.142854	0.245235
-9.245421	5.390870	0.250240
-9.998490	9.722330	0.255245
-10.130008	12.198028	0.260250
-10.429309	11.387511	0.265254
-10.360946	13.901689	0.270259
-10.539260	8.035809	0.275264
-11.749107	11.530422	0.280269
-11.444953	6.206334	0.285274
-11.985743	9.397466	0.290278
-12.005701	16.015992	0.295283
-11.882754	10.220260	0.300288
-12.038173	13.503246	0.305293
-11.940446	14.586047	0.310298
-12.324875	12.573944	0.315302
-12.679720	14.274521	0.320307
-13.011579	7.771345	0.325312
-13.428429	19.532484	0.330317
-13.556044	3.047837	0.335322
-14.356618	15.941195	0.340326
-14.616196	20.034475	0.345331
-14.591901	10.894309	0.350336
-14.843656	9.427842	0.355341
-14.883586	5.558823	0.360346
-14.955627	9.047118	0.365350
-15.093295	16.962084	0.370355
-15.813433	17.064949	0.375360
-16.294805	11.315854	0.380365
-16.309065	12.545800	0.385370
-16.611179	21.887868	0.390374
-16.686436	14.212151	0.395379
-16.992468	10.147290	0.400384
-17.413880	20.105860	0.405389
-17.347466	11.490629	0.410394
-17.700155	19.625730	0.415398
-17.775096	14.964921	0.420403
-17.839717	7.907626	0.425408
-19.080609	28.519247	0.430413
-19.277127	13.370890	0.435418
-19.598048	21.279590	0.440422
-19.588826	16.748040	0.445427
-19.279199	15.475731	0.450432
-19.592774	14.487109	0.455437
-19.386542	16.574874	0.460442
-20.341859	15.831698	0.465446
-20.353310	17.668628	0.470451
-20.510280	10.334655	0.475456
-21.146278	14.723816	0.480461
-20.769750	10.973446	0.485466
-21.802490	15.092196	0.490470
-22.043686	7.976975	0.495475
-22.374028	6.627145	0.500480
-22.579572	14.688715	0.505485
-22.177947	7.302571	0.510490
-22.605992	10.162948	0.515494
-22.626802	3.465817	0.520499
-23.070743	5.718084	0.525504
-23.720167	14.446694	0.530509
-23.801154	5.360887	0.535514
-23.916804	13.886170	0.540518
-23.829474	3.562481	0.545523
-24.496233	10.272219	0.550528
-24.922051	5.685025	0.555533
-25.237480	-2.519581	0.560538
-25.655992	12.832548	0.565542
-25.589757	14.011997	0.570547
-25.082738	7.833775	0.575552
-26.157240	18.488795	0.580557
-26.469590	9.492791	0.585562
-26.962220	19.016375	0.590566
-26.986099	12.879684	0.595571
-26.863038	11.130240	0.600576
-27.000703	12.619838	0.605581
-26.780973	9.795521	0.610586
-27.974092	12.009417	0.615590
-28.520064	6.773402	0.620595
-28.324179	18.163899	0.625600
-28.757129	24.422800	0.630605
-28.447355	13.387450	0.635610
-28.593764	16.915798	0.640614
-29.180304	8.275688	0.645619
-29.509226	11.835616	0.650624
-29.816055	15.841342	0.655629
-30.006443	11.201674	0.660634
-30.125994	21.742810	0.665638
-30.527993	14.174914	0.670643
-30.797000	6.485077	0.675648
-31.172422	16.360557	0.680653
-31.044986	14.224466	0.685658
-31.172707	12.567850	0.690662
-31.871088	17.985419	0.695667
-32.332281	15.732176	0.700672
-32.476092	21.367110	0.705677
-32.108291	8.848468	0.710682
-32.618843	22.272456	0.715686
-33.104606	18.308342	0.720691
-33.633062	15.619498	0.725696
-34.035522	16.498613	0.730701
-33.716821	11.194405	0.735706
-34.240827	4.543985	0.740710
-34.575605	11.249488	0.745715
-33.844231	15.928769	0.750720
-34.375253	21.810647	0.755725
-34.792429	10.711320	0.760730
-35.529510	12.876357	0.765734
-36.095904	12.692702	0.770739
-35.509953	4.803313	0.775744
-36.042272	13.716163	0.780749
-35.858477	10.647513	0.785754
-36.891851	14.051377	0.790758
-37.174055	15.392642	0.795763
-37.214416	7.891825	0.800768
-37.298453	11.998898	0.805773
-37.298360	4.482292	0.810778
-37.426186	7.121924	0.815782
-37.940683	8.723976	0.820787
-38.386854	10.356517	0.825792
-38.608146	18.834977	0.830797
-38.499132	2.895603	0.835802
-38.573409	17.308316	0.840806
-39.325034	5.890920	0.845811
-39.767528	4.681934	0.850816
-40.326869	10.587199	0.855821
-40.136115	13.547376	0.860826
-40.144591	13.941219	0.865830
-40.389405	12.821673	0.870835
-40.889661	5.053951	0.875840
-40.845403	15.202596	0.880845
-41.434834	9.201418	0.885850
-41.875180	12.503457	0.890854
-41.748348	8.127600	0.895859
-41.425117	8.972816	0.900864
-41.920011	23.099858	0.905869
-42.412852	8.450048	0.910874
-42.628932	5.225367	0.915878
-43.255731	14.965984	0.920883
-43.763579	11.239420	0.925888
-43.842698	14.099252	0.930893
-44.010437	11.607337	0.935898
-43.823748	11.746174	0.940902
-44.310841	13.932398	0.945907
-44.163680	16.098960	0.950912
-44.615778	20.816980	0.955917
-45.181575	16.276890	0.960922
-45.381759	13.021260	0.965926
-45.539218	15.073905	0.970931
-45.232130	21.372600	0.975936
-46.116801	19.485839	0.980941
-46.305989	10.331460	0.985946
-46.952136	20.385129	0.990950
-47.031538	18.664044	0.995955
-47.318609	11.745785	1.000960
-47.594803	18.907225	1.005965
-47.165675	17.347400	1.010970
-47.409226	20.156907	1.015974
-48.181524	20.758259	1.020979
-48.491464	15.384256	1.025984
-49.157296	17.405328	1.030989
-48.982334	19.105669	1.035994
-48.842646	13.468677	1.040998
-48.485881	19.525526	1.046003
-49.337654	7.443539	1.051008
-50.132363	21.345187	1.056013
-50.003689	21.426620	1.061018
-49.942618	14.681938	1.066022
-50.939200	16.741852	1.071027
-51.217858	14.893609	1.076032
-52.078947	14.815948	1.081037
-50.973337	16.039204	1.086042
-51.624268	12.948665	1.091046
-51.904551	21.648275	1.096051
-51.399826	11.553814	1.101056
-52.063900	14.798942	1.106061
-52.407367	8.262776	1.111066
-52.693005	19.307480	1.116070
-53.117753	8.199845	1.121075
-53.058739	8.140269	1.126080
-53.918791	8.366157	1.131085
-54.158024	11.137026	1.136090
-54.437089	18.052148	1.141094
-54.653626	11.477236	1.146099
-54.556790	7.647033	1.151104
-54.846192	5.414500	1.156109
-54.570163	13.511813	1.161114
-54.895908	8.659112	1.166118
-55.622393	12.739669	1.171123
-55.725705	6.068039	1.176128
-56.122291	6.876639	1.181133
-56.033782	5.967777	1.186138
-56.864134	8.609229	1.191142
-57.147527	6.378923	1.196147
-57.239934	11.797049	1.201152
-57.647130	10.231403	1.206157
-57.243554	4.164198	1.211162
-57.136341	3.391625	1.216166
-58.026402	7.674814	1.221171
-58.425640	7.787825	1.226176
-59.051024	11.368602	1.231181
-58.962896	8.428739	1.236186
-59.190190	12.653027	1.241190
-59.208165	11.880964	1.246195
-59.115831	3.103521	1.251200
-60.090855	19.640086	1.256205
-60.488024	11.549439	1.261210
-60.603782	7.891538	1.266214
-61.043084	10.693558	1.271219
-60.707493	5.848615	1.276224
-60.909833	15.735107	1.281229
-60.839808	11.883768	1.286234
-61.666835	10.706182	1.291238
-62.294827	11.155357	1.296243
-62.200022	10.735880	1.301248
-62.547589	11.362847	1.306253
-62.739088	-1.502121	1.311258
-62.868617	2.861961	1.316262
-62.769282	8.398922	1.321267
-63.340348	7.852176	1.326272
-63.944462	18.696537	1.331277
-63.794999	14.728429	1.336282
-64.275856	13.338762	1.341286
-64.490238	19.424428	1.346291
-64.109221	17.255183	1.351296
-64.740766	9.593322	1.356301
-64.850405	10.436335	1.361306
-65.252361	15.371166	1.366310
-65.541162	10.253293	1.371315
-66.077911	7.594216	1.376320
-66.609886	14.270313	1.381325
-66.727861	8.831625	1.386330
-66.684607	12.608841	1.391334
-66.764661	14.997435	1.396339
-66.693022	9.203367	1.401344
-66.977778	13.591621	1.406349
-67.311220	10.657287	1.411354
-67.971108	13.363944	1.416358
-68.121468	8.980628	1.421363
-67.984543	3.480107	1.426368
-68.388891	17.931555	1.431373
-69.039535	6.447821	1.436378
-69.227054	27.898300	1.441382
-69.613832	21.590330	1.446387
-69.721311	12.540284	1.451392
-70.167340	14.036767	1.456397
-69.958800	16.548099	1.461402
-70.426590	12.653954	1.466406
-71.042314	20.589569	1.471411
-71.209870	22.283131	1.476416
-71.331301	15.826284	1.481421
-71.164297	10.444460	1.486426
-71.059806	15.316255	1.491430
-71.590911	21.568290	1.496435
-71.967534	17.913041	1.501440
-72.551847	25.464130	1.506445
-72.821640	11.956469	1.511450
-72.903791	10.178868	1.516454
-72.960535	12.933978	1.521459
-73.450841	12.896659	1.526464
-74.007413	14.103480	1.531469
-74.313714	12.474670	1.536474
-74.200005	15.639824	1.541478
-74.223355	8.459052	1.546483
-74.101544	1.856773	1.551488
-74.666467	16.763477	1.556493
-75.189286	22.122074	1.561498
-75.464132	14.439474	1.566502
-75.981901	13.134646	1.571507
-75.571320	17.221652	1.576512
-76.137994	19.765105	1.581517
-76.055303	14.171789	1.586522
-77.374214	22.302310	1.591526
-77.506226	22.854589	1.596531
-77.122462	20.504587	1.601536
-77.597540	25.213531	1.606541
-77.822452	15.492095	1.611546
-77.581632	18.213529	1.616550
-77.755153	20.265512	1.621555
-78.110881	14.531657	1.626560
-78.484538	19.772120	1.631565
-78.541318	21.745816	1.636570
-78.806783	15.045650	1.641574
-79.701838	30.158785	1.646579
-79.778117	14.925276	1.651584
-79.963876	17.216437	1.656589
-80.211248	14.664158	1.661594
-79.924457	19.400005	1.666598
-80.425857	30.430853	1.671603
-81.048819	19.869751	1.676608
-81.244465	20.055463	1.681613
-81.474151	14.526603	1.686618
-81.443338	17.008662	1.691622
-82.025943	31.282237	1.696627
-82.127102	23.980701	1.701632
-82.857397	18.941059	1.706637
-82.717176	21.200447	1.711642
-82.748264	18.127290	1.716646
-83.304278	21.488468	1.721651
-83.155755	13.793732	1.726656
-83.230454	19.215428	1.731661
-83.978214	9.641840	1.736666
-84.437768	16.803354	1.741670
-84.765688	22.621970	1.746675
-84.409578	18.273686	1.751680
-84.739573	15.585580	1.756685
-85.036057	14.951790	1.761690
-85.670479	15.971423	1.766694
-86.174502	18.764539	1.771699
-86.138126	14.193965	1.776704
-86.633166	16.397245	1.781709
-86.373745	19.435312	1.786714
-86.113171	6.439843	1.791718
-86.668171	11.224501	1.796723
-86.973505	9.633505	1.801728
-87.384039	19.160121	1.806733
-87.782485	14.382012	1.811738
-88.097582	13.229119	1.816742
-88.235097	13.861345	1.821747
-87.702108	9.903124	1.826752
-88.718224	16.028201	1.831757
-89.121179	24.133162	1.836762
-89.089636	21.290691	1.841766
-89.361429	15.047075	1.846771
-89.290977	15.042664	1.851776
-90.258806	11.916051	1.856781
-90.881022	12.797746	1.861786
-90.894671	11.531481	1.866790
-91.019307	13.009558	1.871795
-90.767219	19.332631	1.876800
-90.897228	5.815867	1.881805
-90.847260	15.460598	1.886810
-91.296075	13.831833	1.891814
-91.740462	20.294984	1.896819
-91.716204	12.929634	1.901824
-92.717916	17.315628	1.906829
-93.143297	17.521292	1.911834
-93.257585	22.974463	1.916838
-93.563800	22.952772	1.921843
-93.320368	13.117288	1.926848
-93.691178	20.445313	1.931853
-93.684442	12.946655	1.936858
-93.512863	25.834175	1.941862
-94.646479	14.545858	1.946867
-94.698540	10.308583	1.951872
-94.934448	16.397599	1.956877
-94.908160	9.262881	1.961882
-94.738026	11.096845	1.966886
-95.879485	7.143084	1.971891
-95.886562	14.613782	1.976896
-96.147246	11.054374	1.981901
-96.451796	10.500931	1.986906
-96.793499	15.397907	1.991910
-97.334564	12.967285	1.996915
-97.460709	10.128421	2.006912
-96.572904	12.578657	2.016909
-96.820338	11.870068	2.026906
-96.304055	14.451008	2.036902
-95.317959	8.048069	2.046899
-95.151116	16.423283	2.056896
-94.101844	9.326284	2.066893
-93.849552	8.533552	2.076890
-93.865543	12.081155	2.086886
-93.009167	12.128836	2.096883
-92.355342	6.620240	2.106880
-92.080506	14.012491	2.116877
-91.351582	7.158601	2.126874
-91.337154	8.287684	2.136870
-90.860147	9.335239	2.146867
-89.969240	12.301326	2.156864
-88.768865	6.546079	2.166861
-88.746873	15.102231	2.176858
-88.386769	12.198865	2.186854
-88.463910	10.459601	2.196851
-87.389422	9.706740	2.206848
-87.001063	1.847869	2.216845
-86.683052	5.812285	2.226842
-85.992882	11.210740	2.236838
-85.332905	5.903919	2.246835
-84.657735	4.795097	2.256832
-84.310680	12.755791	2.266829
-84.315145	6.136464	2.276826
-82.940778	9.667151	2.286822
-82.686817	16.951784	2.296819
-82.881810	4.973871	2.306816
-81.956287	13.528720	2.316813
-81.409339	4.476275	2.326810
-81.086535	8.968951	2.336806
-80.353889	11.934339	2.346803
-80.079997	18.240219	2.356800
-79.540208	12.131676	2.366797
-78.920153	10.888888	2.376794
-78.712400	14.154574	2.386790
-78.395824	12.423698	2.396787
-76.851644	10.641061	2.406784
-76.685086	14.676576	2.416781
-75.977895	11.449914	2.426778
-75.846945	17.752709	2.436774
-75.594038	16.421373	2.446771
-75.319274	12.618997	2.456768
-74.508585	16.779128	2.466765
-73.684476	18.162266	2.476762
-72.927533	18.130399	2.486758
-72.699003	15.725841	2.496755
-72.387160	15.104395	2.506752
-72.267705	13.682968	2.516749
-71.382237	13.089413	2.526746
-71.366828	15.051448	2.536742
-70.358233	15.240149	2.546739
-70.036774	13.866462	2.556736
-69.206265	11.295319	2.566733
-68.815556	12.340473	2.576730
-68.749467	9.606426	2.586726
-67.912343	8.209468	2.596723
-67.197598	9.270691	2.606720
-66.951520	7.227687	2.616717
-65.987429	10.328095	2.626714
-65.740469	18.554626	2.636710
-65.675240	15.396240	2.646707
-64.808447	8.818647	2.656704
-64.459185	12.005282	2.666701
-64.215296	8.762061	2.676698
-63.164564	18.409280	2.686694
-62.912509	14.303173	2.696691
-62.490334	6.359842	2.706688
-61.796738	9.587894	2.716685
-61.107884	12.208487	2.726682
-61.333162	17.578427	2.736678
-60.265373	12.046554	2.746675
-59.941881	11.793916	2.756672
-59.205311	13.086150	2.766669
-58.244812	9.699676	2.776666
-58.181870	16.491383	2.786662
-58.012268	10.817434	2.796659
-57.437315	11.837069	2.806656
-56.651041	11.268462	2.816653
-56.288939	15.656823	2.826650
-56.366395	16.885741	2.836646
-55.551307	17.560721	2.846643
-54.883840	17.884897	2.856640
-54.035427	21.525989	2.866637
-53.725810	17.037131	2.876634
-53.611298	15.426411	2.886630
-52.684636	20.693019	2.896627
-51.824937	11.446160	2.906624
-51.817156	20.289622	2.916621
-51.868612	19.569524	2.926618
-50.831101	19.699874	2.936614
-50.417168	9.816024	2.946611
-50.020642	12.406109	2.956608
-49.278544	11.955250	2.966605
-48.797081	13.961925	2.976602
-47.970177	19.424624	2.986598
-47.507443	19.368877	2.996595
-47.670726	19.949109	3.006592
-47.229818	21.436261	3.016589
-46.267057	20.304835	3.026586
-45.994389	21.419052	3.036582
-45.162401	23.611897	3.046579
-44.999673	21.398142	3.056576
-44.471468	21.677480	3.066573
-43.536100	23.150999	3.076570
-43.381250	20.152881	3.086566
-42.882806	18.089589	3.096563
-41.768686	20.209996	3.106560
-41.870092	23.137362	3.116557
-41.673509	24.972990	3.126554
-40.664313	19.323530	3.136550
-40.522461	18.693708	3.146547
-39.835253	23.680831	3.156544
-39.025159	14.929518	3.166541
-39.106909	18.930840	3.176538
-38.279842	9.970987	3.186534
-37.649084	12.933236	3.196531
-37.362496	15.020936	3.206528
-37.178815	14.311744	3.216525
-36.172805	13.575882	3.226522
-36.105214	16.239356	3.236518
-35.037269	7.875539	3.246515
-34.703505	10.152291	3.256512
-34.480692	11.106382	3.266509
-33.530162	16.511821	3.276506
-33.141904	15.295622	3.286502
-33.104807	17.932168	3.296499
-32.371568	18.138402	3.306496
-31.790960	16.375919	3.316493
-31.332965	12.982156	3.326490
-30.409948	19.947219	3.336486
-30.269581	19.938497	3.346483
-30.029639	19.515140	3.356480
-29.325227	14.017671	3.366477
-28.838927	22.992531	3.376474
-28.628598	15.839258	3.386470
-27.670316	14.822567	3.396467
-27.397150	13.060437	3.406464
-26.262624	9.783078	3.416461
-25.823954	11.115361	3.426458
-26.069166	18.027907	3.436454
-25.728376	15.092703	3.446451
-24.737693	18.271335	3.456448
-24.290844	12.921669	3.466445
-23.880661	10.004171	3.476442
-23.190226	13.166196	3.486438
-22.708718	14.567835	3.496435
-21.941912	9.811396	3.506432
-21.389033	11.787947	3.516429
-21.292548	15.973753	3.526426
-21.315547	17.840403	3.536422
-20.444595	17.946003	3.546419
-19.789519	11.277832	3.556416
-18.782470	15.087455	3.566413
-18.485444	13.543349	3.576410
-18.672444	10.585787	3.586406
-17.932474	8.180792	3.596403
-17.033759	16.391376	3.606400
-16.869153	13.474100	3.616397
-16.381467	19.309556	3.626394
-15.806877	20.440119	3.636390
-15.535076	16.283421	3.646387
-14.653182	13.678935	3.656384
-14.063910	21.339008	3.666381
-13.768655	22.921696	3.676378
-12.881603	27.852366	3.686374
-12.478240	17.564689	3.696371
-12.454805	17.878272	3.706368
-12.212271	21.125876	3.716365
-10.811061	15.174636	3.726362
-10.809316	21.481715	3.736358
-10.500782	22.086685	3.746355
-9.679980	14.078113	3.756352
-9.314672	16.954986	3.766349
-8.564137	21.637655	3.776346
-8.419934	13.987845	3.786342
-7.893000	22.161288	3.796339
-6.632161	24.334879	3.806336
-6.447530	17.698773	3.816333
-6.392695	16.670698	3.826330
-6.201010	18.272679	3.836326
-5.335116	14.447954	3.846323
-4.789769	19.764433	3.856320
-4.232811	20.555630	3.866317
-3.978102	24.612270	3.876314
-3.291375	34.471398	3.886310
-2.985006	42.438447	3.896307
-2.756184	52.932732	3.906304
-1.869532	64.566341	3.916301
-1.337060	73.949011	3.926298
-1.038880	79.389520	3.936294
-0.693988	86.599844	3.946291
-0.417970	100.051786	3.956288
0.000000	110.200119	3.961293
0.503013	115.595173	3.966298
0.670576	118.872183	3.971302
1.566296	123.475289	3.976307
1.296379	129.749971	3.981312
1.236872	113.523528	3.986317
1.298642	128.585851	3.991322
1.217642	128.304473	3.996326
1.247357	122.276454	4.001331
0.831114	127.403362	4.006336
1.126995	130.935634	4.011341
1.239797	132.781702	4.016346
0.896676	127.298937	4.021350
1.477534	118.866139	4.026355
1.347087	117.039099	4.031360
0.887539	113.703613	4.036365
1.107580	120.405029	4.041370
1.318450	125.060983	4.046374
1.118808	117.192622	4.051379
0.780861	123.465240	4.056384
1.631734	127.410959	4.061389
1.537315	128.855869	4.066394
1.002157	127.370244	4.071398
1.348118	118.303322	4.076403
1.235760	121.933954	4.081408
1.448984	126.175101	4.086413
1.312864	119.170021	4.091418
1.319657	113.917509	4.096422
1.427512	108.706209	4.101427
1.039733	122.145960	4.106432
1.515083	121.278100	4.111437
1.234410	122.024365	4.116442
1.349326	126.511766	4.121446
1.356971	123.846999	4.126451
1.562514	132.075565	4.131456
1.635532	132.368140	4.136461
1.541565	114.669628	4.141466
1.105031	115.522415	4.146470
1.770253	111.768203	4.151475
1.334468	118.419873	4.156480
1.514405	116.266105	4.161485
1.462663	117.558840	4.166490
1.282318	124.964822	4.171494
1.602031	117.961535	4.176499
1.682928	122.669361	4.181504
1.570433	117.989062	4.186509
1.333698	119.278964	4.191514
1.301421	126.497382	4.196518
1.652475	131.925592	4.201523
1.633827	126.477726	4.206528
1.692290	123.045767	4.211533
1.792663	122.495710	4.216538
1.700914	132.766838	4.221542
1.925458	125.743565	4.226547
1.281762	126.505225	4.231552
1.646941	112.911268	4.236557
1.783987	123.358734	4.241562
1.613428	125.783581	4.246566
1.590091	119.842915	4.251571
1.571985	129.406568	4.256576
1.449564	134.063799	4.261581
1.787634	131.338093	4.266586
1.341115	133.059281	4.271590
1.656147	123.614368	4.276595
1.550707	124.355495	4.281600
1.585439	120.525445	4.286605
1.918993	125.975360	4.291610
1.350141	127.490974	4.296614
1.646413	120.155987	4.301619
1.910994	136.284532	4.306624
1.920675	131.480806	4.311629
1.736456	121.737149	4.316634
1.849740	129.489710	4.321638
2.086544	129.063940	4.326643
2.032327	133.590332	4.331648
2.178228	129.761953	4.336653
2.048952	129.026195	4.341658
2.012337	127.750841	4.346662
2.184256	122.962985	4.351667
2.084518	134.617881	4.356672
2.023458	133.086912	4.361677
2.001746	139.133133	4.366682
2.075897	140.808055	4.371686
2.061857	130.436800	4.376691
2.112991	124.278899	4.381696
1.896018	136.692347	4.386701
2.317433	129.094269	4.391706
2.057832	132.333388	4.396710
2.011607	119.803201	4.401715
1.809352	133.255202	4.406720
2.024020	128.384760	4.411725
2.187856	130.751216	4.416730
1.871104	139.912133	4.421734
1.924130	134.478414	4.426739
1.856318	139.582712	4.431744
1.699036	131.979824	4.436749
2.228960	131.631799	4.441754
2.504095	148.546465	4.446758
2.502102	129.748479	4.451763
1.985739	133.802674	4.456768
1.940192	125.711006	4.461773
2.152659	135.972734	4.466778
2.596235	147.581010	4.471782
2.476838	140.177858	4.476787
1.927484	129.092706	4.481792
2.155603	139.598766	4.486797
2.415970	140.551851	4.491802
2.284924	144.859260	4.496806
2.552848	150.654750	4.501811
2.177127	152.636993	4.506816
2.603295	144.762928	4.511821
2.605337	135.278158	4.516826
2.058354	140.267241	4.521830
2.492739	131.841424	4.526835
2.112859	141.496212	4.531840
2.498721	150.924216	4.536845
2.879589	154.889339	4.541850
2.244882	143.032876	4.546854
2.086310	138.650803	4.551859
2.288532	150.518116	4.556864
2.361334	148.453789	4.561869
2.510870	150.661126	4.566874
2.479975	151.036317	4.571878
2.961142	142.834160	4.576883
2.620126	150.088003	4.581888
2.612675	151.864214	4.586893
2.689150	145.243628	4.591898
2.448055	145.164341	4.596902
2.748761	142.912674	4.601907
2.758642	141.358004	4.606912
2.366825	132.178161	4.611917
2.455500	138.286286	4.616922
2.510441	143.184816	4.621926
2.953110	148.022979	4.626931
2.891378	144.831186	4.631936
2.438253	144.307197	4.636941
2.400099	139.242005	4.641946
2.661441	154.339714	4.646950
2.977340	148.959972	4.651955
2.647030	148.967341	4.656960
2.506217	147.483588	4.661965
2.814070	147.464360	4.666970
2.694123	151.678296	4.671974
2.711132	155.396358	4.676979
2.573151	152.969390	4.681984
2.604472	157.251521	4.686989
2.752866	152.945034	4.691994
2.645615	156.018072	4.696998
2.732749	149.326224	4.702003
2.613919	147.013330	4.707008
2.659206	152.979523	4.712013
2.623305	152.849306	4.717018
2.571379	152.364089	4.722022
2.959413	150.797996	4.727027
2.575541	151.481239	4.732032
2.501574	145.500992	4.737037
3.071571	157.940619	4.742042
3.074906	163.682399	4.747046
3.549764	164.665363	4.752051
3.170022	157.302740	4.757056
2.982264	148.625777	4.762061
2.976584	145.355656	4.767066
2.720610	150.783475	4.772070
3.130813	141.146569	4.777075
2.928822	141.406034	4.782080
3.218837	146.375529	4.787085
3.066507	138.737067	4.792090
2.962145	154.704779	4.797094
3.220782	141.304555	4.802099
2.762857	142.654207	4.807104
2.787333	153.328019	4.812109
3.024301	151.503880	4.817114
3.373409	163.620407	4.822118
3.504073	160.436620	4.827123
2.966817	154.123553	4.832128
3.226235	144.525940	4.837133
3.027375	145.607472	4.842138
3.046294	156.449826	4.847142
3.416276	153.000995	4.852147
3.360618	159.979464	4.857152
3.493055	157.326898	4.862157
3.526449	144.800115	4.867162
3.059078	150.017245	4.872166
2.918172	143.139447	4.877171
3.179985	153.219501	4.882176
3.300715	160.461565	4.887181
3.257448	156.820817	4.892186
3.404881	167.529276	4.897190
3.438542	160.905859	4.902195
3.486261	151.062800	4.907200
3.239555	157.052312	4.912205
3.190884	153.276368	4.917210
3.317805	161.441261	4.922214
3.673197	160.990699	4.927219
3.308262	165.432602	4.932224
3.147019	161.671020	4.937229
3.351022	152.594546	4.942234
3.131366	166.292884	4.947238
3.405248	156.528502	4.952243
3.647551	162.277367	4.957248
3.411869	161.026677	4.962253
3.441000	158.099138	4.967258
3.321580	170.487931	4.972262
3.595685	163.710020	4.977267
3.433986	163.650008	4.982272
3.031713	162.074089	4.987277
3.558102	158.502830	4.992282
3.116805	164.582751	4.997286
3.549319	160.330099	5.002291
3.451871	159.893098	5.007296
3.693827	161.614660	5.012301
3.710575	163.709799	5.017306
3.368335	170.403870	5.022310
3.584405	165.523709	5.027315
3.289914	169.862899	5.032320
3.926988	187.651371	5.037325
4.167127	181.419731	5.042330
3.771481	174.742931	5.047334
3.877208	162.413675	5.052339
3.363922	157.090269	5.057344
3.437004	161.976488	5.062349
3.785261	165.924545	5.067354
3.734970	176.119643	5.072358
3.925818	177.042426	5.077363
3.766055	169.246924	5.082368
3.551722	172.298673	5.087373
3.915730	170.499044	5.092378
3.767708	179.355306	5.097382
3.863857	185.538212	5.102387
4.134905	188.954143	5.107392
3.360381	186.955301	5.112397
4.005890	177.142537	5.117402
4.047409	183.776862	5.122406
3.902063	179.769198	5.127411
3.769753	184.886715	5.132416
4.067383	189.434267	5.137421
4.205674	174.860048	5.142426
4.121288	175.338479	5.147430
3.939257	167.011784	5.152435
3.765971	163.511497	5.157440
3.643232	171.807013	5.162445
4.100919	169.578357	5.167450
4.084706	183.941042	5.172454
4.395344	187.154659	5.177459
3.862683	169.499087	5.182464
3.755231	171.901460	5.187469
3.872058	184.800795	5.192474
4.114794	188.183169	5.197478
4.197642	179.334348	5.202483
4.129963	190.180715	5.207488
4.189141	191.114508	5.212493
4.774224	178.970029	5.217498
3.840600	176.679592	5.222502
3.652369	172.811480	5.227507
4.047723	178.713687	5.232512
3.941837	183.991600	5.237517
4.239050	177.140485	5.242522
4.136527	193.291439	5.247526
4.552067	178.566485	5.252531
4.555576	186.965735	5.257536
4.357197	183.646517	5.262541
4.403029	177.362876	5.267546
3.912683	164.572783	5.272550
3.988283	179.446339	5.277555
4.279835	184.564299	5.282560
4.191175	190.801290	5.287565
4.501771	176.285662	5.292570
4.547689	187.215578	5.297574
4.362889	182.277608	5.302579
4.261144	182.062732	5.307584
3.994954	190.105351	5.312589
4.379551	185.758916	5.317594
4.346507	181.632529	5.322598
4.655200	186.162539	5.327603
4.345107	175.777242	5.332608
4.528126	181.415124	5.337613
4.245585	179.665541	5.342618
4.469725	186.973770	5.347622
4.367938	189.204425	5.352627
4.241133	188.461952	5.357632
4.117470	184.653386	5.362637
4.590954	182.381141	5.367642
4.411802	187.822319	5.372646
4.381531	186.520664	5.377651
4.710510	183.100357	5.382656
4.575341	192.002080	5.387661
4.691086	190.326521	5.392666
4.372561	194.659969	5.397670
4.687331	192.399778	5.402675
4.527402	187.296586	5.407680
4.295673	188.870445	5.412685
4.526201	184.690364	5.417690
4.053102	185.048987	5.422694
4.305510	194.627503	5.427699
4.450809	193.292185	5.432704
4.853570	211.424039	5.437709
4.758584	206.060799	5.442714
4.818291	212.591066	5.447718
5.033155	210.982329	5.452723
4.882865	200.334860	5.457728
4.625852	191.953390	5.462733
4.877059	179.898858	5.467738
4.400977	187.724226	5.472742
4.685071	192.090393	5.477747
5.266122	199.817610	5.482752
4.777120	192.702932	5.487757
4.591795	182.807557	5.492762
4.493990	194.670994	5.497766
4.651164	201.135463	5.502771
4.959133	199.173717	5.507776
4.938956	211.806508	5.512781
5.087641	203.058153	5.517786
4.835328	212.316639	5.522790
4.705779	206.544338	5.527795
5.257197	203.358306	5.532800
5.017837	203.879848	5.537805
4.610999	183.743327	5.542810
4.447020	198.758602	5.547814
5.046050	202.933372	5.552819
5.225867	208.752090	5.557824
5.039510	211.862764	5.562829
5.186064	207.161090	5.567834
4.913205	203.859793	5.572838
5.034202	205.201568	5.577843
5.053437	201.677627	5.582848
4.542478	202.424950	5.587853
5.022399	202.733264	5.592858
5.004347	205.321034	5.597862
5.240761	198.814727	5.602867
5.084974	200.449528	5.607872
4.793270	204.576325	5.612877
5.123085	202.275828	5.617882
4.742459	207.833800	5.622886
5.220996	202.109188	5.627891
5.177400	201.274668	5.632896
4.934798	212.572217	5.637901
5.104464	204.785518	5.642906
5.095768	207.760964	5.647910
5.002415	207.288523	5.652915
5.208945	201.745464	5.657920
5.144337	197.864427	5.662925
5.053201	199.609381	5.667930
5.490774	207.352613	5.672934
5.076343	205.190138	5.677939
5.110512	214.078162	5.682944
5.191827	222.674117	5.687949
5.568794	221.574803	5.692954
5.609657	226.301545	5.697958
5.284994	215.222483	5.702963
5.271709	208.919561	5.707968
5.107562	215.899126	5.712973
5.554593	222.539930	5.717978
5.609948	223.180098	5.722982
5.488156	219.491453	5.727987
5.341343	211.333256	5.732992
5.421457	209.454441	5.737997
5.189903	202.736263	5.743002
5.240322	218.183235	5.748006
5.396702	225.163516	5.753011
6.053591	224.580591	5.758016
5.301167	209.486980	5.763021
5.737350	220.656703	5.768026
5.275197	216.071947	5.773030
5.430911	217.946144	5.778035
5.311556	220.758492	5.783040
5.437811	234.548555	5.788045
5.802838	226.424552	5.793050
5.669620	232.282526	5.798054
5.857652	234.120056	5.803059
5.630746	222.181064	5.808064
5.556296	220.813520	5.813069
5.439363	228.655752	5.818074
5.588025	228.322795	5.823078
5.694023	224.038711	5.828083
5.915231	219.186208	5.833088
5.707459	228.213146	5.838093
5.859035	220.122379	5.843098
5.360697	214.938994	5.848102
5.288808	215.747666	5.853107
5.568788	214.394540	5.858112
5.128680	225.169203	5.863117
5.903574	228.728152	5.868122
5.795764	229.482308	5.873126
5.693416	229.185269	5.878131
5.342496	225.121019	5.883136
5.153705	234.388608	5.888141
5.437036	227.191630	5.893146
5.825300	243.630039	5.898150
6.028897	247.603801	5.903155
6.268845	246.051266	5.908160
5.684675	235.471330	5.913165
5.728562	228.786185	5.918170
5.428976	242.022474	5.923174
5.972839	233.775712	5.928179
6.460634	244.953233	5.933184
6.183318	247.986328	5.938189
5.879285	229.339665	5.943194
5.867231	227.228430	5.948198
5.797264	225.265415	5.953203
6.110472	220.983870	5.958208
5.734405	238.667550	5.963213
6.053050	244.758888	5.968218
6.418116	236.774077	5.973222
6.135987	242.136394	5.978227
6.261262	231.490294	5.983232
5.906836	227.353824	5.988237
6.107278	238.066727	5.993242
6.180711	233.240393	5.998246
6.305608	221.847727	6.003251
5.843932	231.116674	6.008256
5.801571	232.531341	6.013261
5.989767	225.887003	6.018266
6.104222	228.726222	6.023270
6.014600	228.300655	6.028275
6.368487	227.435883	6.033280
5.941568	241.444953	6.038285
6.093425	233.436393	6.043290
6.171851	235.794015	6.048294
6.060417	236.282986	6.053299
6.019096	234.546459	6.058304
6.062484	235.511186	6.063309
6.196149	224.825819	6.068314
6.062229	228.222554	6.073318
6.073095	230.492620	6.078323
5.937697	219.248049	6.083328
5.819950	224.208288	6.088333
6.504218	227.031553	6.093338
5.868419	222.059389	6.098342
5.863532	206.688043	6.103347
6.050483	213.907163	6.108352
5.903960	222.336117	6.113357
6.362919	221.005743	6.118362
5.710498	216.871381	6.123366
5.813282	218.371013	6.128371
6.083913	215.329935	6.133376
5.873171	232.013454	6.138381
5.844815	227.095404	6.143386
6.052800	232.808507	6.148390
5.854803	232.156209	6.153395
6.155352	225.937294	6.158400
6.046369	227.106075	6.163405
6.094151	221.429542	6.168410
6.118752	226.060742	6.173414
5.853562	216.861139	6.178419
5.787986	214.271032	6.183424
5.842166	230.138199	6.188429
5.865861	228.426350	6.193434
6.085984	225.529173	6.198438
6.018225	231.813544	6.203443
6.202980	230.548007	6.208448
6.197773	226.762117	6.213453
5.772481	215.198860	6.218458
5.991389	218.167344	6.223462
5.942548	222.240514	6.228467
5.696260	215.799866	6.233472
5.682802	221.433550	6.238477
5.961820	220.289377	6.243482
5.802187	225.537707	6.248486
6.006846	228.888053	6.253491
6.330473	221.153304	6.258496
6.041167	224.773544	6.263501
6.140840	228.203510	6.268506
6.036481	225.274598	6.273510
5.964014	221.230267	6.278515
6.389346	222.768264	6.283520
6.170958	224.482414	6.288525
5.951303	210.489069	6.293530
5.715859	205.324865	6.298534
5.829965	220.021621	6.303539
5.803118	218.308151	6.308544
5.863528	222.788245	6.313549
6.019288	228.433549	6.318554
5.843483	241.989080	6.323558
5.806370	229.903476	6.328563
6.000514	226.599064	6.333568
5.859468	228.152480	6.338573
6.096454	226.084727	6.343578
5.815534	223.664185	6.348582
5.806535	225.959489	6.353587
5.724400	226.228767	6.358592
5.633951	231.320797	6.363597
6.105094	222.360879	6.368602
5.826549	224.419747	6.373606
6.140991	218.312563	6.378611
5.723470	224.904483	6.383616
5.604536	235.888569	6.388621
5.791965	221.977363	6.393626
6.018148	224.558746	6.398630
6.184449	230.370085	6.403635
6.184878	229.047828	6.408640
5.941152	234.008704	6.413645
6.057711	224.483910	6.418650
6.096805	220.301990	6.423654
5.894277	219.055625	6.428659
5.877514	224.215273	6.433664
5.838546	225.284569	6.438669
6.026957	228.937996	6.443674
5.345946	226.402581	6.448678
5.620678	230.393736	6.453683
6.103718	237.987537	6.458688
6.041412	252.680150	6.463693
6.316697	242.048651	6.468698
6.456892	232.896652	6.473702
5.923676	234.583893	6.478707
6.043014	231.949174	6.483712
5.583111	234.884148	6.488717
5.744029	230.857260	6.493722
5.909192	232.290235	6.498726
6.078545	246.804409	6.503731
6.207223	243.089417	6.508736
6.275610	233.546808	6.513741
5.957282	232.973356	6.518746
5.985780	228.951268	6.523750
5.769914	232.060212	6.528755
6.009061	224.167777	6.533760
5.861393	229.736940	6.538765
6.033464	225.509006	6.543770
6.122299	225.720027	6.548774
5.856864	227.096661	6.553779
5.866350	227.190326	6.558784
5.892894	234.374320	6.563789
6.422416	227.983715	6.568794
6.153560	226.330070	6.573798
5.795504	232.672294	6.578803
6.101229	230.264815	6.583808
5.792235	226.048507	6.588813
5.871899	227.216389	6.593818
5.889968	231.174742	6.598822
6.328997	228.926837	6.603827
6.141220	237.023707	6.608832
5.655884	233.306242	6.613837
5.750661	225.923491	6.618842
6.124616	231.063435	6.623846
5.690446	233.181334	6.628851
6.033569	235.814112	6.633856
6.085716	240.722595	6.638861
6.018383	232.204008	6.643866
6.127412	228.941322	6.648870
5.761819	229.539465	6.653875
6.129056	220.216084	6.658880
5.939759	220.622266	6.663885
6.302919	234.903779	6.668890
6.144257	234.131464	6.673894
6.063461	231.720891	6.678899
6.211732	231.527198	6.683904
5.985317	230.195968	6.688909
5.893310	231.105848	6.693914
5.999807	229.257723	6.698918
5.756415	240.419374	6.703923
5.925095	234.173532	6.708928
5.932924	241.872961	6.713933
6.228115	231.345934	6.718938
5.887672	233.582116	6.723942
5.944551	240.188762	6.728947
6.301008	228.386723	6.733952
5.764588	235.626733	6.738957
5.931678	229.128045	6.743962
6.031105	227.040581	6.748966
5.903193	232.157427	6.753971
5.625982	228.758728	6.758976
5.635443	229.975505	6.763981
6.028040	227.231804	6.768986
6.326853	236.287437	6.773990
6.171201	233.145052	6.778995
6.276270	233.293436	6.784000
5.890954	233.420097	6.789005
6.294278	236.264960	6.794010
6.326868	225.990791	6.799014
6.015352	226.602660	6.804019
6.174857	235.059900	6.809024
6.182489	230.490579	6.814029
6.224148	225.900143	6.819034
6.391981	226.930914	6.824038
5.819856	236.473320	6.829043
6.404031	222.933766	6.834048
5.991458	218.768387	6.839053
5.729877	218.878946	6.844058
5.997374	219.312081	6.849062
6.014220	224.001434	6.854067
6.430516	215.711269	6.859072
5.771675	209.610098	6.864077
5.636998	213.449863	6.869082
5.994858	215.580482	6.874086
6.107128	225.364328	6.879091
6.265950	223.169542	6.884096
5.622750	215.189868	6.889101
5.822741	214.570516	6.894106
6.083310	223.496059	6.899110
6.144026	225.217372	6.904115
6.141616	227.211101	6.909120
6.019196	216.837687	6.914125
5.958045	205.613201	6.919130
5.508652	208.989450	6.924134
5.827234	214.346813	6.929139
6.533413	221.633787	6.934144
5.889470	225.869215	6.939149
6.225783	218.730429	6.944154
5.928013	207.302343	6.949158
5.778213	208.550242	6.954163
5.996243	210.269207	6.959168
6.060013	217.472708	6.964173
6.210967	221.998814	6.969178
5.996894	207.786308	6.974182
5.702995	211.366132	6.979187
5.935057	209.058707	6.984192
5.871231	213.915639	6.989197
6.319655	221.850172	6.994202
6.261146	224.441080	6.999206
5.835278	218.752875	7.004211
5.894132	216.687548	7.009216
5.633207	215.269946	7.014221
6.144859	212.640586	7.019226
5.754082	220.898765	7.024230
6.016757	230.978729	7.029235
6.345797	229.156065	7.034240
6.089651	226.121074	7.039245
5.765523	213.969440	7.044250
5.886500	214.710119	7.049254
5.651326	224.029217	7.054259
6.032361	223.163382	7.059264
6.248557	227.476855	7.064269
5.815622	224.333353	7.069274
6.118678	226.406068	7.074278
5.870443	224.717576	7.079283
6.200970	227.004309	7.084288
5.767434	218.194740	7.089293
5.656376	219.866870	7.094298
6.077482	221.484616	7.099302
5.931442	234.744448	7.104307
6.249585	230.035034	7.109312
6.309683	234.065936	7.114317
6.276583	215.671326	7.119322
6.001286	212.092002	7.124326
5.618576	205.935184	7.129331
5.664051	213.027639	7.134336
5.725054	222.974486	7.139341
6.159666	221.189169	7.144346
6.222545	224.593226	7.149350
6.083657	234.280143	7.154355
6.212490	220.166095	7.159360
5.959092	212.707848	7.164365
5.672236	212.933072	7.169370
5.897979	221.544504	7.174374
5.922303	229.950024	7.179379
6.394687	228.165152	7.184384
6.101569	215.803049	7.189389
6.096268	203.190502	7.194394
6.285323	200.835992	7.199398
5.910791	204.934558	7.204403
5.956057	204.934069	7.209408
5.819584	204.424050	7.214413
5.716738	207.698886	7.219418
5.856214	208.784690	7.224422
5.996518	209.500215	7.229427
5.829129	216.954836	7.234432
5.845161	219.407590	7.239437
6.414558	221.258506	7.244442
5.872096	224.699867	7.249446
5.680247	213.040155	7.254451
6.331620	220.484355	7.259456
6.211542	223.670131	7.264461
5.550248	215.822985	7.269466
6.112115	211.914005	7.274470
5.564083	217.055130	7.279475
6.042992	221.748468	7.284480
6.382049	229.510213	7.289485
5.887918	227.714476	7.294490
5.852555	210.841957	7.299494
5.714918	219.528948	7.304499
6.117504	229.859204	7.309504
6.553322	232.101070	7.314509
5.932705	226.598205	7.319514
6.145981	217.865096	7.324518
6.002871	217.109343	7.329523
5.860999	207.868398	7.334528
5.714372	212.643310	7.339533
5.664257	209.392751	7.344538
6.131725	216.580852	7.349542
6.112572	230.814321	7.354547
6.365763	216.510074	7.359552
6.050962	218.112688	7.364557
5.630622	217.893633	7.369562
5.626770	218.910007	7.374566
5.466917	221.165524	7.379571
5.975077	228.951558	7.384576
6.202701	241.741937	7.389581
5.951107	240.120405	7.394586
6.165687	236.721062	7.399590
5.979840	243.318046	7.404595
6.083719	233.614891	7.409600
5.781166	237.332106	7.414605
5.914049	231.215223	7.419610
6.064064	234.184945	7.424614
6.157090	240.178535	7.429619
6.114084	234.943231	7.434624
6.247017	237.311349	7.439629
5.557770	227.209677	7.444634
5.788027	224.004045	7.449638
5.878267	240.719801	7.454643
5.919113	239.900605	7.459648
5.952202	242.793623	7.464653
6.083062	240.293148	7.469658
5.705420	235.802794	7.474662
5.513605	240.388600	7.479667
6.013359	230.433989	7.484672
5.817087	234.273858	7.489677
5.585772	233.085758	7.494682
6.079360	237.824270	7.499686
6.097913	243.819966	7.504691
6.298413	237.461603	7.509696
6.093255	236.753474	7.514701
6.122762	242.516514	7.519706
6.358002	232.995383	7.524710
6.157403	237.547756	7.529715
5.921939	234.354524	7.534720
5.975324	242.154424	7.539725
6.189670	226.559105	7.544730
6.077309	233.625524	7.549734
5.936485	244.179598	7.554739
6.433825	233.475567	7.559744
5.915121	227.387370	7.564749
5.815786	224.283674	7.569754
5.848936	220.400066	7.574758
6.061933	231.971533	7.579763
6.049808	237.513268	7.584768
6.195069	239.904776	7.589773
5.939543	231.766660	7.594778
5.807768	220.575306	7.599782
5.879646	230.232569	7.604787
6.040871	234.605223	7.609792
6.111390	240.542207	7.614797
6.021953	235.456499	7.619802
6.001363	224.877404	7.624806
5.618021	231.144473	7.629811
6.137488	238.637691	7.634816
6.047863	232.852838	7.639821
6.048421	230.628911	7.644826
6.359314	229.688577	7.649830
5.883880	223.122255	7.654835
5.975464	212.899018	7.659840
5.790113	217.860291	7.664845
5.561494	219.436832	7.669850
5.925418	223.388790	7.674854
6.063124	237.670607	7.679859
6.248428	231.014062	7.684864
6.239333	234.789987	7.689869
5.963047	226.965147	7.694874
5.952225	214.663493	7.699878
5.754709	223.353481	7.704883
6.185494	221.065733	7.709888
6.118578	216.220128	7.714893
5.860654	217.386789	7.719898
5.858437	216.419278	7.724902
5.891190	221.485795	7.729907
6.333862	229.547775	7.734912
6.114060	223.789520	7.739917
5.888563	230.924172	7.744922
5.678397	219.416001	7.749926
5.632555	226.076599	7.754931
6.042923	227.493542	7.759936
6.296274	233.256528	7.764941
6.251286	238.208607	7.769946
6.335733	228.739429	7.774950
5.672757	227.261041	7.779955
5.957923	217.466395	7.784960
5.609424	216.071920	7.789965
5.593790	225.844043	7.794970
6.084177	235.910701	7.799974
6.311982	244.262401	7.804979
6.374091	236.115956	7.809984
5.680044	228.103065	7.814989
5.918463	222.738528	7.819994
6.017120	227.769477	7.824998
5.778546	232.944680	7.830003
5.874300	243.996583	7.835008
6.381993	241.557656	7.840013
6.436362	241.378582	7.845018
6.270577	218.154695	7.850022
5.859762	223.353549	7.855027
6.103819	219.588961	7.860032
5.873060	214.069691	7.865037
5.844366	218.411801	7.870042
5.940132	216.777315	7.875046
5.963625	234.139358	7.880051
5.898857	220.492042	7.885056
5.946769	214.556069	7.890061
5.656590	214.775483	7.895066
5.903378	217.780753	7.900070
5.767573	217.223175	7.905075
6.350952	229.309599	7.910080
6.050312	236.285114	7.915085
5.780627	235.647141	7.920090
6.358812	217.132045	7.925094
5.958343	223.743455	7.930099
6.003056	219.054471	7.935104
6.395071	222.625577	7.940109
5.843206	224.271429	7.945114
6.055186	214.266721	7.950118
6.179935	219.695393	7.955123
6.071288	210.964955	7.960128
5.940157	222.441174	7.965146
6.093630	219.451233	7.970163
5.902774	223.526678	7.975181
5.905933	224.681373	7.980198
5.864326	220.106131	7.985216
5.943170	229.157012	7.990234
6.156508	227.170702	7.995251
6.149604	221.690706	8.000269
6.182594	224.405941	8.005286
5.794987	213.115779	8.010304
6.056726	218.578648	8.015322
6.031064	223.215317	8.020339
6.118633	220.595377	8.025357
5.861835	222.977057	8.030374
5.947459	227.242971	8.035392
6.043765	221.491301	8.040410
5.895598	229.028121	8.045427
6.123821	215.038692	8.050445
6.105992	218.351938	8.055462
5.966566	226.389139	8.060480
5.996749	219.732636	8.065498
5.801612	219.526579	8.070515
6.123435	221.701411	8.075533
5.856702	228.969531	8.080550
6.289484	236.567371	8.085568
6.285431	236.303162	8.090586
6.286061	223.248514	8.095603
6.174722	216.639291	8.100621
5.813313	219.529535	8.105638
6.186395	220.011288	8.110656
6.106683	225.928086	8.115674
6.059557	223.401696	8.120691
6.540260	236.195684	8.125709
6.230426	238.472022	8.130726
5.590588	221.307501	8.135744
6.161932	237.773136	8.140762
6.327954	245.005439	8.145779
6.448196	236.122820	8.150797
6.151018	221.435752	8.155814
5.970961	212.262250	8.160832
6.220909	222.469842	8.165850
6.077154	229.529478	8.170867
6.452442	231.809589	8.175885
5.981380	227.518948	8.180902
5.930169	225.027906	8.185920
6.086549	230.137976	8.190938
6.224065	236.156646	8.195955
6.371452	239.343192	8.200973
6.374396	235.360577	8.205990
6.437570	234.435844	8.211008
6.545055	236.296932	8.216026
5.920447	231.269693	8.221043
6.345174	229.073755	8.226061
6.252361	233.149715	8.231078
6.313185	225.579622	8.236096
6.213961	222.998232	8.241114
6.292811	225.185650	8.246131
6.229498	221.424780	8.251149
6.138031	238.435399	8.256166
6.229170	229.102905	8.261184
6.539399	236.271730	8.266202
6.264557	240.918799	8.271219
6.213614	232.110169	8.276237
5.915607	230.212940	8.281254
5.884675	229.334415	8.286272
6.517273	232.896668	8.291290
6.433595	243.105727	8.296307
6.248226	240.275830	8.301325
6.356955	241.360444	8.306342
6.531047	246.366781	8.311360
6.337189	242.960727	8.316378
6.349334	241.983982	8.321395
6.375260	237.634892	8.326413
6.371399	241.911587	8.331430
6.089332	239.816227	8.336448
6.651067	247.031098	8.341466
6.642337	245.631594	8.346483
6.807092	244.053610	8.351501
6.427084	234.261170	8.356518
6.099488	229.033062	8.361536
6.306336	228.467789	8.366554
6.654579	245.447821	8.371571
6.642450	235.863175	8.376589
6.223345	232.766732	8.381606
6.224656	232.265017	8.386624
6.460030	242.506446	8.391642
6.069638	241.709133	8.396659
6.447418	240.716482	8.401677
6.292575	244.906238	8.406694
6.255101	251.759998	8.411712
6.170163	238.589280	8.416730
6.299564	244.139030	8.421747
6.608718	238.900136	8.426765
6.418787	239.627331	8.431782
6.265740	246.221388	8.436800
6.549756	244.804705	8.441818
6.520985	243.244230	8.446835
6.339997	244.923029	8.451853
6.425768	245.042443	8.456870
6.403766	243.430424	8.461888
6.453174	245.205887	8.466906
6.443918	241.218859	8.471923
6.524101	236.460558	8.476941
6.344264	238.192823	8.481958
6.143647	243.595151	8.486976
6.572077	238.703738	8.491994
6.248865	248.041277	8.497011
6.584558	258.226073	8.502029
6.897378	259.143219	8.507046
6.307880	256.035435	8.512064
6.708382	259.050040	8.517082
6.677452	260.522451	8.522099
6.840549	249.629333	8.527117
6.578318	241.468941	8.532134
6.258933	248.720021	8.537152
6.803507	250.225896	8.542170
6.330915	259.485719	8.547187
6.499119	257.645280	8.552205
6.820243	271.922037	8.557223
6.451173	247.959145	8.562240
6.941358	258.918259	8.567258
6.455373	253.219372	8.572275
6.614394	250.477856	8.577293
6.511728	250.926392	8.582311
6.751615	265.414596	8.587328
7.121459	256.748709	8.592346
6.884881	250.799565	8.597363
6.570943	238.163090	8.602381
6.803862	243.254936	8.607399
6.434246	249.497728	8.612416
6.554689	248.775504	8.617434
6.544485	245.400812	8.622451
6.283776	243.617689	8.627469
6.540582	251.239779	8.632487
6.564553	270.280452	8.637504
6.701293	268.003123	8.642522
7.226214	273.283030	8.647539
6.962050	266.634471	8.652557
6.974890	252.277783	8.657575
6.881677	252.873162	8.662592
6.708951	241.451702	8.667610
6.397570	257.953814	8.672627
6.787432	242.859974	8.677645
7.055174	242.954211	8.682663
6.748311	243.996240	8.687680
6.588771	244.308473	8.692698
6.733211	246.539327	8.697715
6.738132	249.735435	8.702733
6.636434	245.251588	8.707751
6.619253	257.971642	8.712768
7.292534	257.665085	8.717786
6.986999	260.972645	8.722803
6.869482	255.374168	8.727821
6.985305	249.550027	8.732839
6.630920	246.736978	8.737856
6.921383	246.341711	8.742874
6.658233	252.649974	8.747891
6.820347	250.359230	8.752909
6.882512	250.810504	8.757927
6.590574	252.402443	8.762944
6.958521	251.597504	8.767962
6.615383	254.118857	8.772979
6.791653	249.632753	8.777997
6.904510	248.668727	8.783015
6.966773	261.982293	8.788032
7.139055	258.194201	8.793050
6.981883	248.846713	8.798067
6.654837	245.300459	8.803085
6.687422	242.190489	8.808103
6.901016	260.456903	8.813120
7.068185	266.038646	8.818138
6.745562	264.350362	8.823155
6.810130	262.563925	8.828173
7.243398	262.342073	8.833191
7.024053	265.169181	8.838208
6.868338	256.118091	8.843226
6.795556	247.104583	8.848243
6.908695	271.265566	8.853261
6.935368	263.495659	8.858279
6.826404	272.900833	8.863296
7.258872	265.929228	8.868314
7.179402	263.868589	8.873331
7.223922	259.794293	8.878349
7.364170	254.354488	8.883367
6.806723	246.868026	8.888384
6.688299	245.009103	8.893402
6.950207	243.712620	8.898419
6.396209	244.957220	8.903437
7.076242	256.189713	8.908455
6.938943	273.671378	8.913472
7.269657	263.632573	8.918490
7.350652	273.948546	8.923507
6.692960	266.796402	8.928525
7.242082	278.689883	8.933543
7.044607	268.174768	8.938560
7.128562	275.779602	8.943578
7.358588	265.466155	8.948595
7.426544	260.327921	8.953613
7.182967	252.107819	8.958631
6.986947	251.311798	8.963648
7.069084	242.643379	8.968666
6.984366	246.156382	8.973683
6.568054	254.385020	8.978701
7.273942	254.366859	8.983719
7.332751	268.166933	8.988736
6.888086	260.530370	8.993754
7.131206	261.060760	8.998771
6.922003	266.079446	9.003789
7.130222	265.984146	9.008807
7.275318	278.678949	9.013824
7.331113	261.257766	9.018842
7.355925	260.206469	9.023859
7.097094	255.949044	9.028877
6.794394	254.017832	9.033895
7.024076	268.151042	9.038912
6.929253	267.683227	9.043930
7.179181	273.009105	9.048947
7.159149	276.660356	9.053965
7.292080	269.157908	9.058983
7.135850	275.051923	9.064000
7.151970	276.614835	9.069018
7.247833	269.821862	9.074035
7.121591	282.101348	9.079053
7.412797	268.020025	9.084071
7.441630	274.339636	9.089088
7.087426	276.515596	9.094106
7.585670	270.502524	9.099123
7.103161	269.836310	9.104141
7.053681	275.442322	9.109159
7.196060	277.301137	9.114176
7.540272	271.734901	9.119194
7.266211	275.460416	9.124211
7.416928	273.916171	9.129229
7.062676	263.128840	9.134247
7.103657	269.342422	9.139264
7.154967	270.738917	9.144282
7.114407	264.711914	9.149299
6.987519	276.357217	9.154317
7.032185	271.560257	9.159335
6.968006	270.387123	9.164352
7.197314	270.285384	9.169370
7.220486	277.650389	9.174387
7.425652	284.731455	9.179405
7.486283	290.392906	9.184423
7.638212	284.926028	9.189440
7.372949	277.476107	9.194458
7.199738	261.460122	9.199475
7.071470	276.292817	9.204493
7.554008	275.145007	9.209511
7.700005	287.536735	9.214528
7.115423	275.235846	9.219546
7.796195	279.642626	9.224563
7.264347	286.248342	9.229581
7.355388	270.689793	9.234599
7.352159	286.332958	9.239616
7.505554	295.700451	9.244634
7.668358	291.389993	9.249651
7.356448	281.760484	9.254669
7.399979	278.377420	9.259687
7.619968	282.571937	9.264704
7.609154	276.565543	9.269722
7.782819	269.154577	9.274739
7.096828	274.073941	9.279757
6.943603	276.098695	9.284775
7.174327	287.934464	9.289792
7.384996	299.423090	9.294810
7.630232	294.866280	9.299827
7.607793	289.417082	9.304845
7.590643	289.874394	9.309863
7.514094	289.892856	9.314880
7.577477	294.544080	9.319898
7.780298	296.254639	9.324915
7.737974	293.755892	9.329933
7.735624	292.869759	9.334951
7.820287	299.486782	9.339968
7.523895	286.008145	9.344986
7.647384	275.982663	9.350003
7.398708	285.879785	9.355021
7.651929	272.845729	9.360039
7.561511	281.336045	9.365056
7.228023	289.816876	9.370074
8.191258	278.600356	9.375091
7.214832	284.047753	9.380109
7.117115	288.083467	9.385127
7.522977	282.520251	9.390144
7.715247	295.914581	9.395162
7.579638	289.249153	9.400179
7.761289	296.908210	9.405197
7.959681	296.987999	9.410215
7.987636	292.648046	9.415232
7.555682	292.125430	9.420250
7.936874	293.303317	9.425267
7.459947	302.024225	9.430285
8.111376	283.986447	9.435303
8.093519	286.072172	9.440320
7.696013	284.512303	9.445338
7.590501	275.879396	9.450355
7.126770	277.046831	9.455373
7.410177	278.564971	9.460391
7.893658	289.020247	9.465408
7.951915	290.437751	9.470426
8.032622	282.703601	9.475443
7.541623	280.820637	9.480461
7.557708	282.882143	9.485479
8.112770	287.179117	9.490496
7.656168	285.003635	9.495514
7.839571	282.308808	9.500531
7.791368	293.708354	9.505549
7.801923	292.485715	9.510567
7.854128	287.384638	9.515584
7.654936	293.357928	9.520602
7.867247	295.783337	9.525619
7.890556	290.459552	9.530637
7.744954	287.298427	9.535655
7.798917	283.175321	9.540672
7.960872	280.348142	9.545690
7.964464	278.280880	9.550707
7.881953	291.080553	9.555725
7.719840	282.194538	9.560743
7.981031	281.049634	9.565760
8.174946	282.376593	9.570778
7.756589	264.719980	9.575795
7.584141	269.868637	9.580813
8.164411	279.624068	9.585831
8.071069	280.475073	9.590848
7.508558	271.124415	9.595866
7.756899	282.834369	9.600883
7.953262	291.895386	9.605901
7.758329	292.992570	9.610919
7.842619	298.214864	9.615936
8.043016	294.498121	9.620954
8.110844	285.980224	9.625971
8.110523	296.662301	9.630989
8.152877	297.561604	9.636007
8.293408	291.986051	9.641024
7.616165	283.044548	9.646042
8.204270	277.771678	9.651059
7.948051	288.411547	9.656077
8.102238	286.349238	9.661095
8.071538	283.722458	9.666112
7.919997	282.376743	9.671130
7.675724	276.832708	9.676147
7.786744	291.744917	9.681165
7.622727	292.875155	9.686183
8.046325	285.024504	9.691200
7.897411	285.060544	9.696218
8.080039	289.696356	9.701235
8.024737	294.100986	9.706253
7.944427	303.567983	9.711271
8.404368	288.106608	9.716288
7.890056	297.312990	9.721306
7.914214	282.799890	9.726323
8.019669	285.510163	9.731341
7.826719	287.563193	9.736359
8.144693	293.373915	9.741376
7.872547	287.701680	9.746394
8.143846	291.815631	9.751411
7.993468	285.789940	9.756429
7.766798	297.056339	9.761447
8.029385	295.261158	9.766464
8.291678	320.168958	9.771482
8.408829	300.131633	9.776499
8.007552	297.120761	9.781517
7.906295	302.242565	9.786535
8.282788	304.686591	9.791552
8.503845	317.663068	9.796570
8.184434	305.907818	9.801587
8.051587	304.208916	9.806605
7.988562	299.655922	9.811623
8.447079	302.670968	9.816640
8.477767	306.137614	9.821658
8.450323	293.573251	9.826675
8.370450	294.460028	9.831693
7.944611	294.763234	9.836711
8.302318	291.965531	9.841728
8.269502	295.710291	9.846746
8.642506	287.151188	9.851763
8.488427	293.022785	9.856781
7.787373	286.319172	9.861799
7.951804	285.605876	9.866816
8.141134	304.665019	9.871834
8.212781	308.415606	9.876851
8.424270	314.413318	9.881869
8.675438	315.548338	9.886887
8.573398	304.680690	9.891904
8.124328	296.644032	9.896922
7.915454	288.159748	9.901939
8.280523	305.317087	9.906957
8.301309	311.890415	9.911975
8.865568	317.277812	9.916992
8.519768	309.064132	9.922010
8.335326	299.023469	9.927027
7.980515	298.129100	9.932045
8.017497	309.344990	9.937063
8.387413	307.817103	9.942080
8.294427	317.803605	9.947098
8.251136	307.390685	9.952115
8.370560	310.849827	9.957133
8.070591	315.226288	9.962151
8.542699	310.324899	9.967168
8.473367	310.894472	9.972186
8.038018	303.672983	9.977203
8.443526	309.097717	9.982221
8.380100	303.632807	9.987239
8.468922	308.570392	9.992256
8.469581	317.292684	9.997274
8.351606	319.457113	10.002291
8.382781	306.965661	10.007309
8.224000	314.106560	10.012327
8.206611	328.312999	10.017344
8.872911	335.126638	10.022362
8.727463	328.872960	10.027379
8.649646	320.721686	10.032397
8.586100	313.357102	10.037415
8.510371	316.445865	10.042432
8.642016	313.658111	10.047450
8.641145	312.595031	10.052467
8.363597	307.236038	10.057485
8.270148	320.719051	10.062503
8.623357	331.841540	10.067520
8.524228	341.481892	10.072538
8.918201	340.650808	10.077555
8.732700	335.510992	10.082573
8.363228	329.257481	10.087591
8.753427	335.546096	10.092608
8.647132	323.126526	10.097626
8.571479	332.270939	10.102643
8.843183	335.147828	10.107661
8.614913	332.274107	10.112679
8.632052	329.015056	10.117696
8.824445	336.385294	10.122714
8.510040	327.674438	10.127731
8.539931	328.881779	10.132749
8.650120	344.602005	10.137767
9.021576	338.283621	10.142784
8.497008	327.753129	10.147802
8.499768	342.335118	10.152819
9.082725	332.376915	10.157837
8.732929	336.221525	10.162855
9.038053	342.046887	10.167872
8.732564	327.490407	10.172890
8.564511	320.637525	10.177907
8.812878	329.942915	10.182925
8.609658	326.632972	10.187943
8.762493	337.123980	10.192960
9.189629	339.967203	10.197978
9.146077	334.786352	10.202995
9.051818	311.140329	10.208013
8.654980	318.302517	10.213031
8.628791	307.937424	10.218048
8.840572	315.919983	10.223066
8.594619	317.157649	10.228083
8.877617	321.635838	10.233101
8.915935	334.246325	10.238119
8.756164	339.512942	10.243136
9.337556	336.541558	10.248154
8.656634	330.671037	10.253171
8.796427	323.789157	10.258189
8.926887	334.075374	10.263207
8.969196	329.070495	10.268224
8.922533	328.614114	10.273242
9.094732	327.561954	10.278259
9.234394	316.019228	10.283277
8.444214	319.307587	10.288295
8.817938	318.085203	10.293312
8.730509	328.730372	10.298330
8.893741	337.051841	10.303347
9.068288	337.514019	10.308365
8.865645	339.685323	10.313383
8.810350	348.141801	10.318400
9.192769	335.097051	10.323418
9.003387	341.573731	10.328435
9.104557	343.650397	10.333453
8.905203	342.883292	10.338471
9.299773	334.863579	10.343488
9.077987	336.573984	10.348506
8.986008	346.901153	10.353523
9.113144	332.365668	10.358541
8.912003	341.166726	10.363559
9.161836	329.988670	10.368576
9.419314	334.988360	10.373594
8.774166	341.056345	10.378611
9.015370	335.790135	10.383629
8.973907	342.272186	10.388647
8.867638	341.575789	10.393664
8.820151	338.058570	10.398682
8.926924	344.340826	10.403699
9.069225	348.070953	10.408717
9.162118	351.502678	10.413735
9.026070	348.068669	10.418752
9.166115	334.689291	10.423770
9.197067	352.185860	10.428787
9.207420	346.229793	10.433805
9.073137	345.689229	10.438823
8.880041	339.682794	10.443840
9.129572	336.172976	10.448858
9.150988	344.696400	10.453875
9.469395	337.871907	10.458893
9.125023	348.206818	10.463911
8.926061	350.721514	10.468928
9.092200	339.742665	10.473946
9.192581	355.385537	10.478963
9.379344	345.757242	10.483981
9.207704	353.354570	10.488999
8.877798	355.309017	10.494016
9.581217	351.895776	10.499034
9.238516	353.962662	10.504051
9.529848	353.336896	10.509069
9.472080	359.676333	10.514087
9.359636	350.135644	10.519104
9.546374	340.131836	10.524122
9.547106	343.997607	10.529139
9.574721	339.054970	10.534157
9.467381	345.850219	10.539175
9.204391	350.334534	10.544192
9.348386	344.897274	10.549210
8.961364	349.766954	10.554227
8.915225	343.551454	10.559245
9.280105	350.386785	10.564263
9.606602	361.204200	10.569280
9.643406	349.440794	10.574298
9.144607	347.524325	10.579315
9.400468	349.122495	10.584333
9.490473	357.259725	10.589351
9.659557	359.657161	10.594368
9.481347	342.931862	10.599386
9.222386	350.274556	10.604403
9.314182	341.557250	10.609421
9.734525	364.411431	10.614439
9.188826	358.892212	10.619456
9.746682	357.824183	10.624474
9.503017	365.615758	10.629491
9.289558	351.527742	10.634509
9.512331	362.572735	10.639527
9.870415	365.448803	10.644544
9.574590	355.324470	10.649562
9.506050	351.097352	10.654579
9.504913	341.791789	10.659597
9.473628	348.897073	10.664615
9.625630	354.203510	10.669632
9.746383	349.438862	10.674650
9.577798	365.268779	10.679667
9.580591	354.738209	10.684685
9.342624	353.273408	10.689703
9.633594	369.640815	10.694720
9.966048	356.771077	10.699738
9.485404	355.362994	10.704755
9.751898	344.687237	10.709773
9.404879	348.111718	10.714791
9.561923	351.255758	10.719808
9.712458	363.350203	10.724826
9.883156	363.162919	10.729843
9.758386	359.651417	10.734861
9.852931	351.643698	10.739879
9.554692	350.200904	10.744896
9.620058	349.389426	10.749914
9.693612	362.814913	10.754931
9.818024	352.230697	10.759949
9.858344	359.766626	10.764967
9.485155	364.583666	10.769984
9.982051	358.065873	10.775002
9.786836	364.003855	10.780019
9.477208	362.218869	10.785037
9.695174	361.686573	10.790055
9.910953	370.236548	10.795072
10.101660	376.912825	10.800090
9.719021	364.451051	10.805107
9.933321	359.905352	10.810125
9.756126	361.485747	10.815143
9.526214	362.963903	10.820160
9.742107	364.650344	10.825178
9.595915	369.517245	10.830195
9.691675	366.785561	10.835213
9.630034	362.248113	10.840231
9.762360	362.593796	10.845248
10.077805	359.982535	10.850266
9.899879	373.513453	10.855283
9.811431	369.071691	10.860301
9.919084	366.316066	10.865319
9.769236	366.292294	10.870336
9.987635	358.899570	10.875354
9.768333	366.987138	10.880371
9.954388	365.626722	10.885389
9.760138	364.925089	10.890407
9.984980	372.476473	10.895424
9.929540	360.459193	10.900442
9.615339	357.974367	10.905459
9.639114	366.061956	10.910477
10.001775	370.486731	10.915495
9.448963	375.338052	10.920512
10.093564	374.821377	10.925530
10.182183	388.727350	10.930547
10.101538	386.875153	10.935565
10.108731	382.958111	10.940583
9.981146	386.146473	10.945600
10.514138	386.858942	10.950618
10.118524	378.722409	10.955635
10.118055	371.720346	10.960653
10.081969	364.878457	10.965671
10.003849	368.251608	10.970688
10.445507	370.527715	10.975706
10.341616	376.634510	10.980723
10.071413	375.846878	10.985741
10.125937	365.251446	10.990759
9.774429	367.165079	10.995776
10.229384	360.612792	11.000794
9.971329	373.850089	11.005811
10.456371	386.760269	11.010829
10.351681	374.340414	11.015847
9.863777	375.035117	11.020864
10.731333	364.246830	11.025882
10.281688	373.834481	11.030899
10.265500	372.366705	11.035917
10.055285	366.132565	11.040935
10.124481	372.859315	11.045952
10.307463	369.725906	11.050970
10.007093	379.609039	11.055987
9.858394	373.220159	11.061005
10.399810	379.131813	11.066023
10.110740	388.464109	11.071040
10.682010	393.326601	11.076058
10.514407	387.281469	11.081075
10.223657	383.489708	11.086093
10.476595	372.954892	11.091111
10.393934	374.063001	11.096128
10.511980	367.648370	11.101146
10.144387	361.486069	11.106163
9.938448	370.246865	11.111181
10.496118	369.768969	11.116199
10.117111	397.351730	11.121216
10.132363	385.878819	11.126234
10.246663	394.876930	11.131251
10.366797	389.853605	11.136269
10.378721	387.819745	11.141287
10.655302	388.225016	11.146304
10.659518	392.617248	11.151322
10.706038	386.898521	11.156339
10.308279	391.615257	11.161357
10.902611	391.027517	11.166375
10.604565	388.126782	11.171392
10.628355	378.416552	11.176410
10.167823	370.176528	11.181427
10.640894	381.554927	11.186445
10.664596	379.298340	11.191463
10.291905	380.975443	11.196480
10.426784	387.777175	11.201498
10.463936	384.739049	11.206515
10.546391	394.704589	11.211533
10.898614	391.964527	11.216551
10.633647	392.479360	11.221568
10.847626	387.078525	11.226586
10.631397	383.451877	11.231603
10.577564	371.216600	11.236621
10.521856	367.012725	11.241639
10.472312	360.756726	11.246656
10.608615	371.133569	11.251674
10.882483	383.388697	11.256691
10.561570	388.544725	11.261709
10.654381	375.444056	11.266727
10.625720	382.223914	11.271744
10.466317	377.332473	11.276762
10.752039	386.859283	11.281779
11.159947	389.847512	11.286797
10.692125	377.559929	11.291815
10.460002	373.610726	11.296832
10.800885	378.780470	11.301850
10.868339	377.217624	11.306867
10.588483	379.467222	11.311885
10.562179	381.746768	11.316903
10.859879	386.797012	11.321920
11.001594	385.279404	11.326938
10.486645	383.545317	11.331955
10.660092	392.202875	11.336973
10.813575	386.202420	11.341991
10.806040	388.621048	11.347008
10.783610	382.938303	11.352026
11.255882	385.001373	11.357043
10.590615	390.624406	11.362061
10.592223	383.533656	11.367079
10.487891	395.017743	11.372096
10.531688	394.742925	11.377114
10.778596	385.351385	11.382131
10.427271	384.327087	11.387149
10.607713	391.412045	11.392167
10.502419	384.053932	11.397184
10.558243	392.906520	11.402202
11.318275	404.934497	11.407219
10.741961	424.460098	11.412237
11.145100	414.507757	11.417255
11.335397	416.226589	11.422272
10.999514	402.299599	11.427290
10.675255	391.668457	11.432307
10.950700	403.339558	11.437325
11.239566	403.152810	11.442343
10.752719	401.300743	11.447360
11.140296	401.922250	11.452378
11.145844	405.790440	11.457395
11.036683	400.171683	11.462413
11.187341	397.680743	11.467431
11.030116	394.212155	11.472448
11.366404	401.294942	11.477466
10.894620	389.225707	11.482483
10.655967	388.915976	11.487501
11.046254	393.109249	11.492519
11.174174	397.987125	11.497536
11.117358	402.849587	11.502554
11.019225	412.852721	11.507571
10.947001	403.362544	11.512589
10.854620	402.717629	11.517607
11.207927	401.021916	11.522624
11.229746	408.955202	11.527642
11.676614	407.024025	11.532659
11.242173	417.025878	11.537677
11.403294	406.025680	11.542695
11.041947	408.773940	11.547712
11.266596	414.144819	11.552730
11.256901	411.249675	11.557747
11.225669	413.324875	11.562765
11.421930	400.760319	11.567783
11.476184	405.261522	11.572800
11.141341	407.664845	11.577818
11.481221	410.559533	11.582835
11.185697	407.964500	11.587853
11.247348	407.519654	11.592871
11.068384	406.642079	11.597888
11.118192	405.479589	11.602906
11.273229	406.430777	11.607923
11.154124	410.640253	11.612941
11.005994	412.102523	11.617959
11.357255	412.786486	11.622976
10.990105	411.726783	11.627994
11.377930	416.564197	11.633011
11.225624	418.670871	11.638029
11.302850	412.978911	11.643047
10.975167	416.046962	11.648064
11.368084	430.820728	11.653082
11.866323	428.474472	11.658099
11.592004	433.134133	11.663117
11.390066	419.120005	11.668135
11.672453	420.546803	11.673152
11.306342	417.410520	11.678170
11.261216	416.231254	11.683187
11.551607	426.697741	11.688205
11.695784	431.816081	11.693223
12.033352	434.414501	11.698240
11.364122	425.907158	11.703258
11.601962	407.466615	11.708275
11.270972	414.792149	11.713293
11.375410	417.183880	11.718311
11.585689	426.463694	11.723328
11.698933	438.860628	11.728346
11.976678	429.448485	11.733363
11.467859	426.795145	11.738381
11.228878	420.720091	11.743399
11.626246	427.663997	11.748416
11.823164	436.049691	11.753434
11.811260	439.500905	11.758451
11.821766	442.229141	11.763469
11.440170	425.535430	11.768487
11.742594	433.128407	11.773504
11.408957	438.254873	11.778522
11.652879	430.555204	11.783539
11.442383	435.369022	11.788557
11.600803	431.267486	11.793575
11.892344	438.148981	11.798592
12.047393	439.721833	11.803610
12.234711	439.478315	11.808627
11.740683	433.786933	11.813645
11.879765	431.969944	11.818663
12.077409	419.209510	11.823680
11.488628	424.489301	11.828698
11.826433	420.404017	11.833715
11.918631	433.577358	11.838733
11.974302	433.531054	11.843751
11.625592	416.999481	11.848768
11.583631	428.328717	11.853786
11.859165	435.114879	11.858803
11.652997	434.910537	11.863821
11.741913	440.091128	11.868839
12.030686	433.028228	11.873856
12.201950	444.128626	11.878874
12.057174	431.601368	11.883891
12.168120	439.817423	11.888909
11.985678	434.121707	11.893927
12.200007	429.093172	11.898944
11.501894	434.254296	11.903962
12.094467	438.046873	11.908979
12.130973	436.728670	11.913997
12.055700	429.482622	11.919015
11.663307	438.875211	11.924032
12.002464	435.297773	11.929050
11.970922	433.497883	11.934067
11.843715	440.851657	11.939085
12.126371	432.962928	11.944103
12.315955	428.402126	11.949120
12.096400	432.709294	11.954138
12.328324	432.310516	11.959155
12.466692	437.486563	11.964173
12.301901	438.017357	11.969191
12.351215	426.283509	11.974208
11.737036	421.346105	11.979226
11.887317	423.891637	11.984243
12.113167	429.429584	11.989261
12.157315	431.237441	11.994279
12.492160	436.499656	11.999296
12.412444	428.077243	12.004314
12.484372	431.269261	12.009331
12.041783	428.236398	12.014349
11.854874	427.407394	12.019367
12.305631	423.481239	12.024384
12.084525	428.962549	12.029402
12.166076	430.890809	12.034419
12.252035	434.490878	12.039437
12.179350	441.548999	12.044455
12.325681	432.299320	12.049472
12.269149	437.878080	12.054490
12.218146	437.750559	12.059507
12.294122	432.633117	12.064525
12.019202	437.422253	12.069543
12.176989	433.945635	12.074560
12.079494	444.169583	12.079578
12.181133	432.465452	12.084595
12.263935	437.457656	12.089613
11.989391	434.644768	12.094631
12.032520	435.708051	12.099648
12.121950	453.347086	12.104666
12.223585	459.204169	12.109683
12.161306	462.148858	12.114701
12.393256	470.686897	12.119719
12.833143	460.031409	12.124736
12.432019	458.626714	12.129754
12.376969	464.880562	12.134771
12.594609	460.081866	12.139789
12.268372	460.038222	12.144807
12.826316	461.166511	12.149824
12.414642	462.237494	12.154842
12.379100	466.509708	12.159859
12.584509	462.410316	12.164877
12.594304	454.358943	12.169895
12.293831	463.800347	12.174912
12.585974	466.481581	12.179930
12.457360	452.459166	12.184947
12.083353	459.116106	12.189965
12.351488	456.938211	12.194983
12.923781	459.765164	12.200000
12.314435	465.710857	12.205018
12.002265	472.856768	12.210035
12.504324	476.360504	12.215053
12.810228	480.207191	12.220071
13.091257	472.151448	12.225088
12.889820	478.967711	12.230106
13.038213	483.577347	12.235123
13.059633	480.106173	12.240141
12.875357	472.511023	12.245159
12.758419	470.241609	12.250176
12.770387	453.350902	12.255194
12.836235	439.159372	12.260211
12.471872	457.355036	12.265229
13.068785	464.889552	12.270247
12.960440	455.711069	12.275264
12.710480	460.243874	12.280282
12.710225	460.518687	12.285299
12.971045	463.766504	12.290317
13.148192	469.952645	12.295335
12.968625	452.511119	12.300352
12.601362	454.670199	12.305370
12.579444	460.593854	12.310387
13.132101	468.870531	12.315405
13.146996	481.232316	12.320423
12.884393	464.169764	12.325440
12.966312	467.073068	12.330458
13.069343	467.786215	12.335475
13.139851	456.263633	12.340493
12.586511	467.508421	12.345511
12.959482	468.447770	12.350528
13.245972	479.656476	12.355546
13.131656	480.491822	12.360563
13.183896	475.535846	12.365581
12.681386	470.962876	12.370599
12.739360	477.445272	12.375616
13.205757	471.998799	12.380634
13.118492	486.594922	12.385651
13.245729	485.562376	12.390669
12.809147	488.710508	12.395687
12.967144	478.177790	12.400704
13.129075	488.036339	12.405722
13.102990	485.383565	12.410739
13.050026	493.457914	12.415757
13.089383	496.285803	12.420775
13.082111	482.979742	12.425792
13.035360	482.482347	12.430810
12.942758	488.701026	12.435827
13.571034	482.535101	12.440845
13.309833	488.997771	12.445863
13.320739	475.941337	12.450880
13.240601	481.634234	12.455898
13.130377	483.920547	12.460915
13.585000	482.543552	12.465933
13.106552	486.146305	12.470951
13.235709	476.779362	12.475968
13.267834	481.012643	12.480986
13.242875	478.889846	12.486003
13.210567	482.688211	12.491021
12.958137	485.738246	12.496039
13.275199	480.756814	12.501056
13.041355	487.950494	12.506074
13.233766	485.443573	12.511091
13.384654	490.415724	12.516109
13.336792	497.492092	12.521127
13.411469	504.391601	12.526144
13.650951	509.643440	12.531162
13.547322	508.586880	12.536179
13.799670	493.672023	12.541197
13.135733	482.705567	12.546215
13.492278	484.815069	12.551232
13.852618	491.755298	12.556250
13.216210	490.806937	12.561267
13.638562	491.675486	12.566285
13.723893	497.175374	12.571303
13.408068	486.369301	12.576320
13.421578	483.303283	12.581338
13.717807	494.087623	12.586355
13.958725	495.397812	12.591373
13.549890	488.001713	12.596391
13.419060	475.626881	12.601408
13.497498	494.485753	12.606426
13.336569	502.917728	12.611443
14.053155	494.819405	12.616461
13.715712	506.052692	12.621479
14.040724	500.158030	12.626496
13.742986	483.359694	12.631514
13.758452	480.451155	12.636531
13.512884	472.774033	12.641549
13.358704	488.901604	12.646567
13.687515	486.540697	12.651584
13.869492	511.325577	12.656602
13.807102	505.926712	12.661619
13.732891	508.115907	12.666637
13.620506	509.799828	12.671655
13.976072	509.801501	12.676672
14.128065	507.212512	12.681690
13.623381	514.476773	12.686707
13.787550	503.589644	12.691725
13.926178	506.537772	12.696743
14.078081	503.484915	12.701760
14.000812	505.368486	12.706778
13.829440	514.348022	12.711795
14.021044	508.748672	12.716813
13.997696	511.965006	12.721831
14.079137	506.408054	12.726848
14.161104	500.226200	12.731866
13.696840	500.292405	12.736883
14.130035	496.173318	12.741901
13.781477	502.236203	12.746919
13.687133	502.730784	12.751936
14.099829	503.648172	12.756954
13.546317	511.163019	12.761971
13.855731	515.485673	12.766989
13.637795	516.122569	12.772007
13.679059	514.279779	12.777024
14.013092	505.329026	12.782042
13.759197	508.524453	12.787059
13.887016	497.340044	12.792077
13.952246	512.644560	12.797095
14.269637	525.631435	12.802112
14.366509	526.033132	12.807130
13.920126	522.019430	12.812147
14.380747	524.702842	12.817165
14.260705	523.503676	12.822183
13.855242	514.929977	12.827200
14.218498	519.035975	12.832218
14.209570	534.301564	12.837235
14.437451	525.080164	12.842253
14.611775	536.700828	12.847271
14.215964	530.015865	12.852288
14.024981	514.851293	12.857306
14.399762	527.589403	12.862323
14.320670	526.481687	12.867341
14.178997	526.156854	12.872359
14.303540	526.876121	12.877376
14.424967	530.186677	12.882394
14.156542	534.826512	12.887411
14.419491	532.321225	12.892429
14.600709	525.016270	12.897447
14.526125	530.089806	12.902464
14.770146	522.197586	12.907482
14.246486	515.175944	12.912499
14.684122	510.099996	12.917517
14.236037	504.350947	12.922535
14.221465	511.851307	12.927552
14.617638	516.274058	12.932570
14.017887	526.566786	12.937587
14.358295	532.055372	12.942605
14.331452	523.851889	12.947623
14.427827	526.746641	12.952640
14.683792	522.582562	12.957658
14.487406	541.986024	12.962675
14.569660	533.304823	12.967693
14.101168	525.125924	12.972711
14.160216	527.319618	12.977728
14.638279	530.230679	12.982746
14.836067	537.950441	12.987763
14.129559	527.132591	12.992781
14.509071	542.183080	12.997799
14.785340	547.719525	13.002816
14.809855	542.338675	13.007834
14.707704	542.392680	13.012851
14.914957	544.885180	13.017869
14.994671	534.219456	13.022887
14.550400	528.760127	13.027904
14.517591	528.850670	13.032922
14.620206	538.103126	13.037939
14.854944	550.919860	13.042957
14.914445	553.277582	13.047975
14.833243	556.174742	13.052992
14.990385	550.138950	13.058010
14.740597	552.611097	13.063027
14.879966	563.924810	13.068045
15.119539	550.371990	13.073063
14.788262	543.705375	13.078080
15.083655	532.829354	13.083098
14.568784	538.198653	13.088115
14.864960	550.803858	13.093133
15.026257	557.652032	13.098151
15.075047	560.024046	13.103168
15.025439	556.248348	13.108186
14.819255	553.289104	13.113203
15.355064	549.889300	13.118221
15.036582	539.039429	13.123239
15.028566	540.492517	13.128256
14.920095	529.209184	13.133274
14.858693	541.314658	13.138291
15.164954	549.806453	13.143309
15.175431	549.596780	13.148327
15.090029	554.258614	13.153344
15.148641	547.048475	13.158362
14.539343	550.744195	13.163379
14.783256	555.698725	13.168397
15.194151	557.436871	13.173415
14.916624	558.228208	13.178432
15.034260	555.849680	13.183450
14.707485	560.088369	13.188467
14.478922	557.574403	13.193485
14.984388	553.418805	13.198503
15.177151	577.611986	13.203520
15.350467	579.904656	13.208538
15.254224	577.559426	13.213555
15.184299	578.024962	13.218573
15.454353	582.079217	13.223591
15.328184	585.639764	13.228608
15.498480	577.487610	13.233626
15.396591	581.082244	13.238643
15.523229	577.399017	13.243661
15.807954	563.242734	13.248679
15.383707	569.112307	13.253696
15.549284	556.053823	13.258714
15.573874	555.876664	13.263731
15.142362	553.798223	13.268749
15.134224	556.138075	13.273767
15.206146	559.771912	13.278784
15.634416	568.935813	13.283802
15.650376	567.393590	13.288819
15.291701	569.065372	13.293837
15.432187	562.732380	13.298855
15.359669	582.514216	13.303872
15.433607	580.830426	13.308890
15.561058	581.943703	13.313907
15.327775	572.383841	13.318925
15.449048	572.150605	13.323943
15.373163	580.897566	13.328960
15.670368	571.109949	13.333978
15.893015	581.350400	13.338995
15.891099	574.670361	13.344013
15.820157	575.028762	13.349031
15.452798	581.438570	13.354048
15.373524	578.765662	13.359066
15.052933	577.272683	13.364083
15.520870	581.384487	13.369101
15.809615	576.101337	13.374119
15.827525	583.075983	13.379136
15.748863	578.108803	13.384154
16.119590	569.846554	13.389171
15.648055	582.732251	13.394189
15.789573	581.186257	13.399207
15.742562	584.633497	13.404224
15.710015	586.768880	13.409242
16.066866	595.341179	13.414259
15.917462	583.502473	13.419277
16.076403	581.149068	13.424295
15.962258	588.062229	13.429312
15.511201	586.539071	13.434330
16.041096	594.756237	13.439347
15.407909	595.060174	13.444365
15.740962	590.215072	13.449383
15.653123	606.386067	13.454400
16.341232	610.728675	13.459418
16.375421	599.489355	13.464435
16.065155	595.536490	13.469453
16.132073	583.705128	13.474471
16.143629	582.621163	13.479488
15.755960	572.062899	13.484506
15.849265	582.383447	13.489523
15.674857	607.066164	13.494541
16.127477	609.062896	13.499559
16.266248	605.305194	13.504576
16.028608	620.940969	13.509594
16.221157	623.729249	13.514611
16.115286	611.097981	13.519629
16.393534	607.113442	13.524647
16.085309	609.569450	13.529664
16.431921	608.651058	13.534682
16.629081	602.861472	13.539699
16.333576	601.926296	13.544717
16.398884	587.532768	13.549735
15.821023	594.284611	13.554752
15.920816	600.833122	13.559770
16.588459	605.649111	13.564787
16.440400	603.321412	13.569805
16.516074	616.364923	13.574823
16.607724	605.375418	13.579840
16.452108	602.108503	13.584858
16.409655	584.879019	13.589875
15.952482	593.871537	13.594893
16.536220	596.734599	13.599911
15.969495	603.689831	13.604928
16.218640	609.315722	13.609946
16.396850	611.882178	13.614963
16.276209	614.447830	13.619981
16.265828	602.435994	13.624999
16.280555	607.855394	13.630016
16.413841	606.077159	13.635034
16.665382	606.483177	13.640051
16.394363	610.523856	13.645069
16.486819	601.563333	13.650087
16.453866	615.213868	13.655104
16.114724	612.070196	13.660122
16.384364	615.881535	13.665139
15.790200	623.768818	13.670157
16.584767	630.774033	13.675175
16.700302	640.734560	13.680192
16.858811	628.327195	13.685210
16.707496	625.447755	13.690227
16.403879	631.102913	13.695245
16.938470	628.649990	13.700263
16.712697	631.894707	13.705280
17.047582	633.452199	13.710298
17.020647	626.290060	13.715315
16.565974	635.417904	13.720333
16.781641	633.718354	13.725351
16.806766	636.109841	13.730368
16.694717	631.766358	13.735386
16.980570	629.913875	13.740403
16.482144	636.637588	13.745421
16.756957	635.885002	13.750439
16.616078	638.892449	13.755456
16.739393	630.725496	13.760474
17.035937	629.969527	13.765491
17.054087	633.681176	13.770509
17.037756	628.644319	13.775527
16.834782	633.176162	13.780544
16.790716	633.729189	13.785562
17.115087	626.985705	13.790579
16.846269	631.975908	13.795597
16.987472	625.923638	13.800615
17.128495	638.856008	13.805632
16.893960	650.420489	13.810650
17.232075	656.651057	13.815667
16.996875	645.781843	13.820685
17.462617	642.733745	13.825703
17.298032	633.425077	13.830720
16.974173	634.179451	13.835738
17.392125	628.020977	13.840755
17.361840	632.696341	13.845773
17.089110	632.022695	13.850791
16.882030	629.565331	13.855808
17.004632	643.374698	13.860826
17.471028	649.294968	13.865843
17.345767	655.746000	13.870861
17.336573	651.635798	13.875879
17.379117	653.014754	13.880896
17.132536	655.274984	13.885914
17.234622	651.459869	13.890931
17.076509	656.609561	13.895949
17.368885	652.629123	13.900967
17.527590	643.901253	13.905984
17.599621	656.951671	13.911002
17.812135	650.853577	13.916019
17.285780	655.202255	13.921037
17.349822	650.619920	13.926055
17.435712	649.224586	13.931072
17.231436	656.145496	13.936090
17.700737	648.334905	13.941107
17.473705	654.741824	13.946125
17.374722	647.385775	13.951143
17.744934	651.291912	13.956160
17.050495	657.203582	13.961178
17.677264	648.295539	13.966195
17.667456	660.610804	13.971213
17.813094	647.189297	13.976231
17.808951	652.671607	13.981248
17.741641	655.825387	13.986266
17.638986	655.813201	13.991283
17.750790	650.759542	13.996301
17.790753	650.021432	14.001319
17.767154	655.238539	14.006336
17.354982	654.719142	14.011354
17.739505	647.770632	14.016371
17.485630	660.549916	14.021389
17.543630	644.718484	14.026407
18.089673	651.049216	14.031424
17.534500	655.443404	14.036442
17.906683	647.701582	14.041459
18.132397	656.950712	14.046477
17.866885	653.827125	14.051495
17.936766	653.409392	14.056512
17.464314	652.066278	14.061530
17.702273	651.808562	14.066547
17.908553	656.254602	14.071565
17.837668	655.641044	14.076583
17.557153	654.479477	14.081600
17.844628	683.637737	14.086618
18.018483	676.722017	14.091635
17.826246	683.540081	14.096653
17.775529	688.190238	14.101671
17.851364	680.573435	14.106688
17.864855	676.904648	14.111706
18.051076	684.859796	14.116723
18.054895	685.335943	14.121741
18.175548	684.206584	14.126759
18.202641	677.310558	14.131776
17.959611	675.893854	14.136794
17.698120	682.710077	14.141811
17.934391	679.836551	14.146829
18.013118	688.701499	14.151847
18.294244	684.104290	14.156864
17.969103	687.418135	14.161882
18.380752	690.017683	14.166899
18.334760	690.782443	14.171917
18.548188	686.284133	14.176935
18.263750	687.401588	14.181952
18.008782	683.954473	14.186970
18.416015	695.384349	14.191987
18.458271	699.694997	14.197005
18.256039	704.239366	14.202023
18.425472	701.884311	14.207040
18.276961	706.881048	14.212058
18.479341	717.415057	14.217075
18.749365	709.761695	14.222093
18.454570	705.475049	14.227111
18.712278	704.684100	14.232128
18.332125	709.268794	14.237146
18.542129	706.481403	14.242163
18.770056	702.100748	14.247181
18.495163	701.039285	14.252199
18.489263	702.327961	14.257216
18.591303	704.600187	14.262234
18.893316	705.115111	14.267251
18.876075	700.826276	14.272269
18.479392	696.296728	14.277287
18.615462	697.301376	14.282304
18.507841	707.435537	14.287322
18.692665	704.484813	14.292339
18.894728	701.736527	14.297357
18.983294	704.411625	14.302375
18.786835	693.555284	14.307392
18.908430	704.669890	14.312410
18.440738	699.368784	14.317427
18.318238	698.583385	14.322445
18.752648	707.468700	14.327463
18.773466	695.568704	14.332480
18.807523	710.710991	14.337498
18.871423	708.340810	14.342515
18.816892	704.991867	14.347533
18.814791	705.746638	14.352551
18.823847	702.599227	14.357568
18.610144	701.184265	14.362586
18.908569	702.879979	14.367603
18.597480	708.059815	14.372621
18.776760	704.636600	14.377639
19.218756	715.477272	14.382656
18.682430	721.133978	14.387674
18.900604	721.917568	14.392691
19.477989	726.368959	14.397709
19.017962	743.626787	14.402727
19.464902	731.736157	14.407744
19.051705	723.838882	14.412762
19.248495	722.217999	14.417779
19.152803	719.197344	14.422797
18.967490	728.434770	14.427815
18.990561	734.294709	14.432832
18.997082	737.074102	14.437850
19.513661	728.268380	14.442867
19.170889	727.236418	14.447885
19.103095	737.566360	14.452903
19.267143	731.425293	14.457920
19.194052	723.664406	14.462938
19.446537	727.756143	14.467955
19.524014	725.847733	14.472973
19.337548	729.471344	14.477991
19.580490	720.323235	14.483008
19.442644	731.604479	14.488026
19.357991	727.057899	14.493043
19.593105	730.353947	14.498061
19.393485	732.026226	14.503079
19.334368	733.137003	14.508096
19.211441	732.777689	14.513114
19.222204	737.563450	14.518131
19.492678	736.290844	14.523149
19.169623	737.998120	14.528167
19.350395	725.385256	14.533184
19.224296	727.730875	14.538202
19.502685	746.379006	14.543219
19.875210	746.737790	14.548237
19.590287	747.751186	14.553255
19.783036	747.790833	14.558272
19.661425	747.582788	14.563290
19.735700	747.369490	14.568307
19.828704	746.733567	14.573325
19.843537	745.948874	14.578343
19.860655	737.167265	14.583360
19.759255	737.640862	14.588378
19.719910	733.459598	14.593395
19.644952	740.991547	14.598413
20.046832	744.296346	14.603431
20.090246	751.857205	14.608448
19.662558	742.753541	14.613466
19.974635	746.690841	14.618483
20.021900	749.975117	14.623501
19.789234	746.877956	14.628519
20.335345	738.313777	14.633536
20.083724	746.150936	14.638554
19.455817	736.298989	14.643571
19.815054	737.543439	14.648589
20.117290	751.530042	14.653607
20.056486	749.378081	14.658624
20.150801	756.183114	14.663642
20.174388	751.805861	14.668659
20.044326	752.656294	14.673677
20.129070	760.191788	14.678695
20.338551	752.459474	14.683712
20.304493	754.617201	14.688730
20.252096	752.564913	14.693747
20.471949	747.421824	14.698765
20.167531	762.377021	14.703783
20.385123	751.481423	14.708800
20.130041	744.616682	14.713818
19.846691	750.404418	14.718835
20.123208	750.749749	14.723853
20.312499	753.854127	14.728871
20.384816	758.412566	14.733888
20.204633	759.744159	14.738906
20.069236	750.926332	14.743923
20.323092	749.709960	14.748941
19.943930	755.089750	14.753959
20.180699	748.441909	14.758976
19.798488	758.208609	14.763994
20.037173	766.780455	14.769011
20.329219	771.819067	14.774029
20.170230	778.502606	14.779047
20.535765	770.578734	14.784064
20.819578	772.816357	14.789082
20.521032	782.661559	14.794099
20.784200	772.241677	14.799117
20.790625	788.701109	14.804135
21.079004	781.593953	14.809152
20.937590	784.595196	14.814170
20.828330	784.517768	14.819187
20.999668	777.286829	14.824205
20.618133	768.785018	14.829223
20.377114	766.336076	14.834240
20.600793	772.382537	14.839258
20.535989	788.720519	14.844275
20.918955	784.470335	14.849293
20.858062	784.208656	14.854311
20.610706	786.084026	14.859328
20.836014	781.593310	14.864346
20.745890	789.698825	14.869363
20.723784	788.717916	14.874381
20.328250	792.159502	14.879399
20.677841	781.871321	14.884416
20.729861	784.851915	14.889434
20.597945	793.049142	14.894451
20.494934	795.031423	14.899469
20.746218	805.595739	14.904487
20.882490	816.903784	14.909504
21.042091	822.442701	14.914522
20.583869	817.244224	14.919539
21.031365	807.672912	14.924557
20.927368	808.629740	14.929575
20.931629	812.930552	14.934592
21.214925	807.641872	14.939610
21.112825	809.298973	14.944627
21.412114	807.990319	14.949645
21.219433	798.777455	14.954663
21.180293	809.386991	14.959680
21.523368	802.713111	14.964698
21.321496	806.957657	14.969715
21.350879	803.832309	14.974733
21.062497	811.116658	14.979751
21.451608	811.277206	14.984768
21.471892	809.652241	14.989786
21.103298	807.806963	14.994803
21.312729	802.103763	14.999821
21.341940	809.597432	15.004839
21.200606	811.367937	15.009856
21.787844	815.609540	15.014874
21.732015	827.483973	15.019891
21.646659	814.278181	15.024909
21.372207	808.688187	15.029927
21.435719	803.455817	15.034944
21.657075	806.015584	15.039962
21.482878	815.068293	15.044979
21.650443	817.525986	15.049997
21.831241	822.847014	15.055015
21.646015	818.631641	15.060032
21.597622	810.712241	15.065050
21.544886	822.822868	15.070067
21.537607	821.517765	15.075085
21.533555	832.169187	15.080103
21.691379	838.481538	15.085120
22.081977	833.529584	15.090138
22.001445	826.088539	15.095155
22.069534	827.545580	15.100173
21.857003	831.056508	15.105191
21.729462	836.068950	15.110208
21.953392	834.980305	15.115226
21.935606	840.130291	15.120243
21.953446	836.328254	15.125261
21.753598	835.668498	15.130279
21.843420	832.836684	15.135296
21.968600	836.143558	15.140314
21.818156	837.937574	15.145331
22.023793	832.115037	15.150349
21.960664	836.110776	15.155367
21.989407	835.121946	15.160384
21.961779	832.554566	15.165402
21.790597	832.152272	15.170419
21.727376	835.475856	15.175437
21.919777	829.365054	15.180455
21.881052	839.359178	15.185472
22.216343	835.409887	15.190490
21.922788	831.416500	15.195507
21.957514	839.013461	15.200525
22.305186	847.981778	15.205543
22.285319	851.942382	15.210560
22.428302	851.970844	15.215578
22.422933	867.826285	15.220595
22.536327	854.460135	15.225613
22.759785	841.897345	15.230631
22.550671	839.645391	15.235648
22.398988	836.636589	15.240666
22.441231	829.413106	15.245683
21.913283	831.572003	15.250701
21.966596	837.745995	15.255719
22.185220	838.277062	15.260736
22.325630	845.377902	15.265754
22.702261	854.234418	15.270771
22.679793	851.407461	15.275789
22.620326	854.929275	15.280807
22.474238	855.930528	15.285824
22.496632	851.155815	15.290842
22.371485	867.222404	15.295859
23.141094	863.820853	15.300877
22.619530	864.981549	15.305895
22.585559	862.468799	15.310912
22.699726	847.556227	15.315930
22.486027	855.756749	15.320947
22.614304	852.442430	15.325965
22.640001	844.915412	15.330983
22.444340	867.137177	15.336000
22.474743	852.124036	15.341018
22.885209	867.381416	15.346035
22.870700	870.902544	15.351053
22.852907	878.637085	15.356071
22.620865	875.142182	15.361088
23.148983	879.670710	15.366106
22.664986	881.481950	15.371123
22.815458	875.525980	15.376141
23.190215	877.639006	15.381159
22.883082	879.176562	15.386176
23.062748	875.844771	15.391194
23.153571	874.865208	15.396211
23.050246	881.325529	15.401229
23.154391	874.682512	15.406247
22.708358	892.193917	15.411264
22.884695	872.613783	15.416282
22.782907	880.067919	15.421299
23.181265	890.000330	15.426317
23.849681	896.100663	15.431335
23.099557	883.178199	15.436352
23.175639	877.426311	15.441370
23.116610	879.215565	15.446387
23.252917	890.457381	15.451405
23.547576	892.847961	15.456423
23.290008	895.015259	15.461440
23.581299	885.944742	15.466458
23.383364	890.447464	15.471475
23.476171	885.500837	15.476493
23.742059	887.416224	15.481511
23.294709	882.727264	15.486528
23.447783	880.128585	15.491546
23.475359	891.964830	15.496563
23.668912	897.040903	15.501581
23.689307	893.052268	15.506599
23.607991	884.181773	15.511616
23.863982	882.128791	15.516634
23.560480	867.196027	15.521651
23.335497	875.057497	15.526669
23.761891	885.651399	15.531687
23.924675	898.530079	15.536704
23.743418	892.370138	15.541722
23.479525	885.137494	15.546739
23.697999	892.822631	15.551757
23.840585	895.145373	15.556775
23.573889	904.436586	15.561792
23.645726	894.545028	15.566810
23.807206	899.755481	15.571827
23.737205	897.585999	15.576845
23.758451	890.182728	15.581863
23.722219	903.537355	15.586880
23.888554	885.552410	15.591898
24.044193	891.098277	15.596915
23.888320	896.683180	15.601933
24.222298	901.147268	15.606951
23.759402	897.574698	15.611968
24.103896	895.350148	15.616986
24.044824	903.005921	15.622003
23.845193	899.553304	15.627021
23.929090	904.933624	15.632039
24.177857	916.044339	15.637056
24.411566	914.670151	15.642074
24.113629	913.867877	15.647091
24.111094	919.772888	15.652109
24.340392	912.018486	15.657127
24.598288	927.353319	15.662144
24.614977	914.507098	15.667162
24.261769	905.426467	15.672179
24.371148	899.448485	15.677197
24.309090	897.448176	15.682215
24.106254	902.544943	15.687232
24.483241	921.398808	15.692250
24.510150	920.867842	15.697267
24.639026	924.707476	15.702285
24.689378	920.748884	15.707303
24.602370	920.693236	15.712320
23.951115	921.542776	15.717338
24.588613	930.181993	15.722355
24.543698	924.294296	15.727373
24.636620	919.331863	15.732391
24.647154	922.006520	15.737408
24.379154	915.279421	15.742426
24.825987	918.182787	15.747443
24.742357	920.575466	15.752461
24.859499	924.120288	15.757479
24.370070	928.867216	15.762496
24.851268	918.703630	15.767514
24.812154	927.334585	15.772531
24.446329	924.005667	15.777549
24.546979	925.852114	15.782567
24.879475	921.723362	15.787584
24.508879	921.087032	15.792602
24.767694	935.866320	15.797619
24.964064	946.230991	15.802637
25.141990	940.387487	15.807655
25.138460	947.854755	15.812672
24.909096	937.713430	15.817690
25.187941	941.337218	15.822707
25.190945	944.300223	15.827725
25.170883	930.882212	15.832743
24.930929	928.433081	15.837760
25.099362	940.077016	15.842778
25.344734	942.140768	15.847795
25.231536	950.360400	15.852813
25.235015	934.818060	15.857831
24.893482	944.777340	15.862848
25.207320	942.425017	15.867866
25.161438	936.117753	15.872883
25.171687	939.789672	15.877901
25.123363	945.430427	15.882919
25.200767	951.379806	15.887936
25.252463	945.590667	15.892954
25.359872	940.341955	15.897971
25.052324	944.842823	15.902989
25.300962	947.010207	15.908007
25.086297	945.150416	15.913024
25.229377	944.345746	15.918042
25.432734	963.857839	15.923059
25.385113	972.587968	15.928077
25.855703	965.660649	15.933095
26.139691	967.778351	15.938112
25.562564	958.663129	15.943130
25.773896	943.599651	15.948147
25.767216	951.799543	15.953165
25.528376	947.977487	15.958183
25.716273	952.167693	15.963200
25.564802	962.217308	15.968218
25.660019	967.008916	15.973235
25.719573	962.417732	15.978253
25.962982	976.113876	15.983271
25.761153	968.918870	15.988288
25.498133	974.706669	15.993306
25.922566	974.246349	15.998323
25.539931	968.569008	16.003341
25.860930	967.310610	16.008359
25.777510	967.784569	16.013376
25.774072	973.569820	16.018394
26.017784	971.032755	16.023411
26.232252	968.108930	16.028429
26.031942	971.362367	16.033447
26.070079	976.847662	16.038464
26.030231	970.675144	16.043482
26.293912	968.661980	16.048499
25.920790	986.774341	16.053517
26.192659	982.301571	16.058535
26.595812	996.787042	16.063552
25.886331	984.337851	16.068570
26.582051	990.225686	16.073587
26.359610	994.495569	16.078605
26.784915	999.358866	16.083623
26.098499	985.953045	16.088640
25.891238	982.340656	16.093658
26.391145	979.725832	16.098675
26.148499	986.725426	16.103693
26.469165	988.704878	16.108711
26.838785	992.115731	16.113728
26.501391	998.928113	16.118746
26.415209	996.789540	16.123763
26.291245	1009.842331	16.128781
26.620357	994.716292	16.133799
26.636522	991.053335	16.138816
26.718508	1000.044161	16.143834
26.614063	996.109653	16.148851
26.505972	997.325900	16.153869
26.612981	992.238178	16.158887
26.620313	989.113075	16.163904
26.369518	995.069388	16.168922
26.835932	987.508404	16.173939
26.565079	997.185314	16.178957
26.855128	991.463190	16.183975
26.812064	998.359131	16.188992
26.971402	1008.928417	16.194010
27.257958	1000.562312	16.199027
27.075619	998.056864	16.204045
26.810278	987.930579	16.209063
27.072465	992.333286	16.214080
26.824943	996.667033	16.219098
27.135163	993.851371	16.224115
27.048866	1007.785062	16.229133
27.398251	1002.426075	16.234151
26.845655	1004.399484	16.239168
27.072344	1019.426836	16.244186
27.032547	1017.217924	16.249203
26.839951	1015.316820	16.254221
26.931491	1015.476366	16.259239
27.258700	1018.287922	16.264256
26.968132	1017.938925	16.269274
27.200660	1011.439967	16.274291
27.035655	1021.580084	16.279309
27.124582	1009.410502	16.284327
27.016927	1021.315224	16.289344
27.171953	1040.295291	16.294362
27.404088	1040.578112	16.299379
27.670245	1048.603026	16.304397
27.618859	1045.379760	16.309415
27.836762	1036.446823	16.314432
27.533428	1045.784839	16.319450
27.811548	1043.586384	16.324467
27.859015	1039.618747	16.329485
27.911308	1028.998022	16.334503
28.079754	1010.649710	16.339520
27.725023	1021.516789	16.344538
27.812240	1018.120471	16.349555
27.768073	1007.095062	16.354573
27.373671	1008.889210	16.359591
27.540144	1010.113200	16.364608
27.636063	1034.056998	16.369626
28.192396	1032.279124	16.374643
28.046828	1037.370168	16.379661
27.732545	1023.862198	16.384679
27.761198	1027.550204	16.389696
27.629515	1034.630368	16.394714
27.978057	1038.025577	16.399731
27.893885	1037.003825	16.404749
27.658393	1038.684873	16.409767
28.113375	1043.502536	16.414784
27.677094	1041.487894	16.419802
28.362807	1039.784548	16.424819
27.976946	1040.122564	16.429837
27.915490	1034.344703	16.434855
28.227281	1041.021312	16.439872
27.964471	1045.527862	16.444890
28.123022	1046.112470	16.449907
28.271260	1048.914027	16.454925
28.105783	1058.498825	16.459943
28.691449	1055.861170	16.464960
28.553752	1062.980151	16.469978
28.415603	1056.015034	16.474995
28.501835	1058.441244	16.480013
28.374620	1065.148344	16.485031
28.730319	1055.944638	16.490048
28.433499	1058.462046	16.495066
28.516718	1056.852505	16.500083
28.547222	1055.983308	16.505101
28.208449	1067.046743	16.510119
28.587476	1064.280316	16.515136
28.708361	1067.622615	16.520154
28.769280	1063.299433	16.525171
28.688782	1064.776472	16.530189
28.382225	1066.001533	16.535207
28.791058	1058.645142	16.540224
28.307983	1066.720447	16.545242
28.788352	1065.512968	16.550259
28.665111	1059.561684	16.555277
28.448142	1064.228357	16.560295
29.018975	1062.356705	16.565312
28.674628	1059.090688	16.570330
28.904199	1060.863429	16.575347
28.774865	1064.102676	16.580365
28.627576	1085.266312	16.585383
29.103663	1085.129303	16.590400
29.040584	1089.235542	16.595418
29.132871	1090.685682	16.600435
29.540814	1085.112428	16.605453
29.255219	1093.008676	16.610471
29.357170	1081.553377	16.615488
29.012158	1092.674602	16.620506
29.272739	1087.449336	16.625523
29.451518	1081.836024	16.630541
29.409136	1089.719650	16.635559
29.420296	1080.011004	16.640576
29.281000	1082.191468	16.645594
29.328580	1085.491536	16.650611
29.624972	1087.430598	16.655629
29.334551	1087.636991	16.660647
29.562015	1079.283206	16.665664
29.561920	1091.013439	16.670682
29.510828	1087.199991	16.675699
29.375539	1078.369361	16.680717
29.494022	1079.878536	16.685735
29.625089	1083.626346	16.690752
29.451114	1082.372424	16.695770
29.360670	1075.267329	16.700787
29.432303	1078.633077	16.705805
29.320825	1075.059404	16.710823
29.648442	1072.995249	16.715840
29.274137	1071.624197	16.720858
29.591802	1091.819212	16.725875
29.754464	1099.601491	16.730893
29.751755	1097.932742	16.735911
30.103984	1103.167203	16.740928
29.898739	1108.147640	16.745946
30.149271	1105.038299	16.750963
29.858402	1102.928427	16.755981
30.110751	1106.461701	16.760999
29.875842	1095.409131	16.766016
29.737504	1105.308462	16.771034
29.837263	1114.078829	16.776051
30.079205	1111.879687	16.781069
29.871120	1106.269798	16.786087
30.041206	1102.627035	16.791104
30.101718	1105.328652	16.796122
30.078065	1115.361609	16.801139
30.206131	1112.905644	16.806157
30.438292	1130.270665	16.811175
30.687241	1128.616380	16.816192
30.455225	1121.410234	16.821210
30.205020	1115.472387	16.826227
30.519551	1118.175481	16.831245
30.257539	1119.579801	16.836263
30.483087	1125.121168	16.841280
30.656638	1130.822110	16.846298
30.553022	1136.357926	16.851315
30.795491	1124.543053	16.856333
30.247668	1117.165175	16.861351
30.701433	1119.076582	16.866368
30.691519	1125.825402	16.871386
30.470571	1134.162879	16.876403
30.917830	1123.824582	16.881421
31.018822	1140.408469	16.886439
31.111892	1130.018018	16.891456
30.750411	1118.622227	16.896474
30.408451	1115.071808	16.901491
30.698055	1120.098276	16.906509
30.841689	1132.967484	16.911527
30.763814	1138.404620	16.916544
30.596443	1133.788764	16.921562
30.508901	1147.640708	16.926579
30.671770	1131.672597	16.931597
30.674063	1136.699622	16.936615
30.835457	1149.158981	16.941632
31.107998	1156.416096	16.946650
30.934684	1157.904438	16.951667
31.197564	1157.507137	16.956685
31.055082	1156.851060	16.961703
31.117425	1159.101124	16.966720
31.204008	1156.118286	16.971738
31.102699	1152.757607	16.976755
31.093475	1147.419697	16.981773
30.900020	1161.360725	16.986791
31.055810	1147.561724	16.991808
31.373037	1159.861129	16.996826
31.216987	1168.355773	17.001843
31.684612	1165.887959	17.006861
31.861280	1174.349739	17.011879
31.863684	1168.662876	17.016896
31.543799	1158.639659	17.021914
31.346494	1156.086027	17.026931
31.410032	1154.018798	17.031949
31.774697	1166.929355	17.036967
31.874721	1171.319485	17.041984
32.103124	1177.791379	17.047002
31.652477	1161.246582	17.052019
31.804957	1145.504137	17.057037
31.680096	1156.278703	17.062055
31.493184	1164.408925	17.067072
31.984138	1178.656814	17.072090
31.731676	1171.662112	17.077107
32.131602	1172.284882	17.082125
31.681674	1177.852540	17.087143
31.693666	1176.326661	17.092160
32.226643	1170.756003	17.097178
31.779494	1181.470312	17.102195
32.338787	1169.940594	17.107213
32.102665	1178.223650	17.112231
31.940409	1170.227144	17.117248
32.230417	1167.386199	17.122266
31.986993	1183.420996	17.127283
32.101438	1170.530968	17.132301
32.175906	1177.219333	17.137319
32.288853	1171.821369	17.142336
32.205959	1173.377685	17.147354
32.437061	1193.507398	17.152371
32.612635	1184.031872	17.157389
32.473196	1176.003409	17.162407
32.425984	1172.779469	17.167424
32.560695	1180.373632	17.172442
32.616258	1185.051553	17.177459
32.530746	1180.498679	17.182477
32.596123	1183.745501	17.187495
32.702411	1173.040544	17.192512
32.520410	1189.545462	17.197530
32.437480	1195.671364	17.202547
32.784859	1194.557166	17.207565
32.549984	1195.846814	17.212583
32.575398	1198.093165	17.217600
32.448756	1197.655525	17.222618
32.769380	1190.748313	17.227635
32.923982	1190.033356	17.232653
32.801872	1205.149885	17.237671
32.616514	1200.110781	17.242688
33.245249	1194.215940	17.247706
32.652091	1200.421284	17.252723
33.119713	1195.397279	17.257741
33.222059	1196.858484	17.262759
32.935338	1193.293137	17.267776
33.316478	1192.312537	17.272794
32.816807	1199.948675	17.277811
33.027586	1199.064027	17.282829
33.491148	1208.156492	17.287847
33.313291	1210.806877	17.292864
33.415531	1205.628319	17.297882
33.258577	1205.438394	17.302899
33.618589	1206.465009	17.307917
33.341192	1198.596870	17.312935
33.301734	1196.135420	17.317952
33.403993	1197.555613	17.322970
33.488820	1206.864835	17.327987
33.266022	1210.333254	17.333005
33.539468	1208.719328	17.338023
33.591605	1215.540571	17.343040
33.713986	1211.185693	17.348058
33.762148	1218.891177	17.353075
33.716982	1215.001040	17.358093
34.078432	1218.078695	17.363111
33.628732	1219.755241	17.368128
33.516057	1208.721439	17.373146
33.468123	1210.581582	17.378163
33.715541	1210.284517	17.383181
33.790547	1222.321879	17.388199
34.015180	1207.221394	17.393216
34.141865	1208.817665	17.398234
33.796185	1208.199535	17.403251
34.023146	1204.500559	17.408269
33.985018	1208.584006	17.413287
33.673709	1211.160494	17.418304
33.784557	1214.886234	17.423322
34.122246	1225.449970	17.428339
34.269824	1230.650061	17.433357
34.462046	1229.629445	17.438375
34.250417	1220.179472	17.443392
34.584908	1217.656640	17.448410
34.453092	1221.783080	17.453427
34.804193	1214.517664	17.458445
34.864118	1207.688905	17.463463
34.379142	1199.629024	17.468480
34.403657	1204.314939	17.473498
33.886615	1200.870657	17.478515
34.046438	1207.056596	17.483533
34.197246	1217.999717	17.488551
34.366709	1223.534068	17.493568
34.078042	1221.502734	17.498586
34.453405	1227.585694	17.503603
34.621840	1219.973177	17.508621
34.751839	1224.150371	17.513639
34.419591	1227.923012	17.518656
35.157702	1238.153013	17.523674
34.818058	1234.450731	17.528691
34.999385	1232.743849	17.533709
35.185363	1222.162154	17.538727
34.847344	1218.207160	17.543744
34.922334	1210.795388	17.548762
34.726087	1222.603585	17.553779
35.032367	1236.470020	17.558797
35.295234	1240.389846	17.563815
34.955474	1232.424105	17.568832
34.994539	1242.267488	17.573850
35.171542	1250.277972	17.578867
35.296202	1240.939731	17.583885
35.771725	1238.751543	17.588903
35.553211	1230.864754	17.593920
35.481838	1216.441507	17.598938
35.129162	1215.253267	17.603955
35.214848	1215.136017	17.608973
35.431128	1221.669775	17.613991
35.594624	1230.575443	17.619008
35.675061	1222.973471	17.624026
35.408512	1217.382116	17.629043
35.358827	1223.812118	17.634061
35.461489	1234.491348	17.639079
35.548164	1244.601873	17.644096
35.915444	1244.589102	17.649114
35.697966	1242.764431	17.654131
35.836347	1247.520991	17.659149
36.124083	1248.164387	17.664167
35.887827	1241.075617	17.669184
36.165189	1232.067054	17.674202
35.791026	1221.395847	17.679219
35.609426	1213.970376	17.684237
35.766351	1223.388301	17.689255
35.801968	1235.630619	17.694272
36.110125	1226.689847	17.699290
35.983732	1244.161298	17.704307
36.190640	1228.760598	17.709325
36.319003	1232.786570	17.714343
36.396196	1233.813039	17.719360
36.390822	1239.188425	17.724378
36.061170	1231.984812	17.729395
36.275624	1241.100301	17.734413
36.317800	1239.796935	17.739431
36.140377	1232.796837	17.744448
36.306606	1232.383025	17.749466
35.857129	1237.029140	17.754483
36.009062	1237.160350	17.759501
36.261451	1236.348116	17.764519
35.987345	1238.590614	17.769536
36.246722	1249.920792	17.774554
36.771874	1254.459346	17.779571
36.514562	1263.575715	17.784589
36.609884	1254.036907	17.789607
36.570453	1263.081483	17.794624
36.788974	1258.926220	17.799642
36.674541	1257.401083	17.804659
36.552845	1266.120799	17.809677
36.558391	1261.430650	17.814695
36.600418	1266.419968	17.819712
36.794045	1255.530950	17.824730
36.744015	1262.863579	17.829747
36.973305	1260.508599	17.834765
37.049327	1254.671392	17.839783
36.611571	1265.204407	17.844800
37.056762	1275.729345	17.849818
37.611894	1283.684127	17.854835
37.390257	1280.111785	17.859853
37.486419	1264.826127	17.864871
37.051069	1260.482334	17.869888
37.136730	1261.917740	17.874906
37.033400	1269.015673	17.879923
37.333542	1277.395162	17.884941
37.461446	1284.479189	17.889959
37.764720	1290.021129	17.894976
37.545718	1282.677192	17.899994
37.446330	1262.407413	17.905011
37.273903	1262.327194	17.910029
37.334377	1263.608731	17.915047
37.223332	1282.497939	17.920064
37.468466	1281.639496	17.925082
37.628717	1287.617114	17.930099
37.327101	1291.564879	17.935117
37.730475	1281.245947	17.940135
37.556763	1285.233757	17.945152
37.827992	1287.422912	17.950170
38.050756	1285.703262	17.955187
37.323528	1286.615138	17.960205
37.626157	1276.318207	17.965223
37.653021	1283.373784	17.970240
37.821125	1293.130833	17.975258
37.879255	1304.880544	17.980275
38.028583	1301.660694	17.985293
38.024279	1298.900266	17.990311
37.921099	1308.481810	17.995328
37.713924	1292.684779	18.000346
38.132718	1305.908901	18.005363
37.931798	1304.362512	18.010381
38.050529	1297.038569	18.015399
38.135327	1315.827892	18.020416
38.461680	1330.451825	18.025434
38.665076	1328.716251	18.030451
38.635277	1330.273781	18.035469
38.609319	1327.999559	18.040487
38.823435	1315.744005	18.045504
38.244491	1299.698737	18.050522
38.625991	1309.365765	18.055539
38.581889	1312.336166	18.060557
39.039617	1305.931427	18.065575
38.733293	1314.152893	18.070592
38.908489	1320.431152	18.075610
38.980830	1307.828447	18.080627
38.709591	1310.537567	18.085645
38.965547	1301.525990	18.090663
38.992097	1313.921252	18.095680
38.601504	1311.047396	18.100698
38.874246	1314.284047	18.105715
38.897474	1316.193082	18.110733
39.053414	1315.380082	18.115751
39.229900	1324.646693	18.120768
39.153737	1332.005509	18.125786
39.319017	1324.503893	18.130803
38.833220	1323.200673	18.135821
38.951953	1309.662936	18.140839
39.066314	1317.074133	18.145856
39.192423	1315.760849	18.150874
39.314292	1318.004821	18.155891
39.265629	1323.674150	18.160909
39.200287	1316.454597	18.165927
39.342135	1328.626791	18.170944
39.447150	1331.605536	18.175962
39.974647	1331.899180	18.180979
39.551040	1340.883690	18.185997
39.906040	1334.400260	18.191015
39.542573	1327.586883	18.196032
39.281903	1329.495939	18.201050
39.685723	1331.137436	18.206067
39.760102	1348.072799	18.211085
39.694668	1339.755028	18.216103
39.992745	1344.562490	18.221120
39.684117	1341.331884	18.226138
39.739343	1337.479738	18.231155
39.580147	1338.337890	18.236173
40.003378	1336.700632	18.241191
39.911096	1336.046200	18.246208
39.851064	1343.257342	18.251226
39.931349	1326.115329	18.256243
39.826062	1337.767429	18.261261
40.004335	1353.522126	18.266279
40.348743	1358.805218	18.271296
40.007341	1368.878323	18.276314
40.510018	1357.581362	18.281331
40.377150	1363.588864	18.286349
40.211495	1355.741127	18.291367
40.551321	1355.413893	18.296384
40.160104	1356.781543	18.301402
40.617958	1356.341258	18.306419
40.248260	1369.050718	18.311437
40.823025	1361.523201	18.316455
40.719179	1358.945521	18.321472
40.713766	1357.760008	18.326490
40.910155	1351.203438	18.331507
40.631206	1349.842763	18.336525
40.623633	1349.124649	18.341543
40.822692	1353.070214	18.346560
40.303530	1355.117350	18.351578
40.742337	1343.312789	18.356595
41.030236	1370.408207	18.361613
40.817619	1372.338189	18.366631
40.915677	1365.897909	18.371648
41.110507	1377.872538	18.376666
41.155570	1372.510330	18.381683
41.425683	1379.297697	18.386701
41.241228	1385.496276	18.391719
41.507902	1372.184768	18.396736
41.313610	1376.431423	18.401754
41.542456	1373.902928	18.406771
40.961163	1373.886367	18.411789
41.348044	1381.365614	18.416807
41.485942	1374.676130	18.421824
41.345266	1384.096295	18.426842
41.438574	1371.524995	18.431859
41.351679	1379.150590	18.436877
41.264155	1375.614152	18.441895
41.374797	1376.121024	18.446912
41.246578	1385.889545	18.451930
41.584137	1392.028941	18.456947
41.780732	1399.405278	18.461965
41.646006	1401.635563	18.466983
41.744134	1395.697037	18.472000
41.905273	1400.333330	18.477018
42.082155	1402.603461	18.482035
41.733410	1395.670999	18.487053
41.937947	1400.010199	18.492071
41.661737	1397.238442	18.497088
41.855506	1405.770253	18.502106
42.120895	1404.880248	18.507123
41.831046	1406.260522	18.512141
42.081597	1419.201653	18.517159
42.432149	1422.479858	18.522176
42.215463	1419.058196	18.527194
42.447645	1423.348917	18.532211
42.301901	1420.421142	18.537229
42.352176	1424.762276	18.542247
42.494489	1426.157316	18.547264
42.475909	1433.535611	18.552282
42.362677	1412.901741	18.557299
42.541143	1418.857632	18.562317
42.505510	1423.729696	18.567335
42.651352	1413.999899	18.572352
42.426046	1430.600145	18.577370
42.509997	1420.258283	18.582387
42.852591	1427.892769	18.587405
42.305961	1432.194296	18.592423
43.061075	1431.385833	18.597440
42.988785	1450.906662	18.602458
43.148035	1446.050521	18.607475
42.749974	1444.181361	18.612493
43.103724	1447.061438	18.617511
43.262067	1448.299349	18.622528
43.170659	1443.109847	18.627546
43.228161	1452.909450	18.632563
43.327923	1450.126484	18.637581
43.471769	1453.168633	18.642599
43.493043	1440.788382	18.647616
43.344188	1451.361733	18.652634
43.322371	1445.943643	18.657651
43.339523	1453.155435	18.662669
43.459961	1446.276137	18.667687
43.659569	1438.210546	18.672704
43.268042	1446.394845	18.677722
43.294678	1446.413020	18.682739
43.080673	1446.190949	18.687757
43.479714	1441.991758	18.692775
43.635540	1444.198900	18.697792
43.479084	1455.199474	18.702810
43.773120	1462.750017	18.707827
43.907425	1460.681202	18.712845
44.238797	1468.497335	18.717863
44.358330	1469.207954	18.722880
44.148810	1467.937447	18.727898
43.819116	1447.943158	18.732915
44.368796	1453.137514	18.737933
43.772077	1456.765185	18.742951
44.262432	1461.994026	18.747968
44.407719	1472.647827	18.752986
44.614598	1462.031178	18.758003
44.668897	1462.821382	18.763021
44.288118	1451.431537	18.768039
44.583158	1435.780249	18.773056
44.402702	1442.751403	18.778074
44.290935	1442.737478	18.783091
44.510004	1453.559662	18.788109
44.346199	1458.274965	18.793127
44.644056	1449.193673	18.798144
44.539220	1463.149541	18.803162
44.781230	1460.849360	18.808179
44.656787	1458.353768	18.813197
44.494011	1463.365560	18.818215
44.536759	1449.359861	18.823232
44.576656	1463.110157	18.828250
44.487787	1455.837406	18.833267
44.932917	1464.806640	18.838285
44.805023	1478.633565	18.843303
45.426188	1471.468011	18.848320
45.203138	1487.190636	18.853338
45.135237	1485.513066	18.858355
45.292862	1483.481643	18.863373
45.460797	1485.453374	18.868391
45.447421	1477.070628	18.873408
45.238690	1480.641052	18.878426
45.558646	1480.676675	18.883443
45.632505	1480.457122	18.888461
45.303225	1471.192592	18.893479
45.648808	1465.152399	18.898496
45.493809	1465.101024	18.903514
45.591641	1469.819775	18.908531
45.760802	1472.551870	18.913549
45.656295	1479.426005	18.918567
45.448679	1471.559504	18.923584
45.621267	1474.287909	18.928602
45.724512	1480.384921	18.933619
45.820948	1484.258130	18.938637
45.591913	1473.409540	18.943655
45.867322	1473.471034	18.948672
45.659238	1477.031889	18.953690
45.722272	1475.980880	18.958707
45.821855	1476.984943	18.963725
45.991172	1478.334757	18.968743
46.266787	1473.059700	18.973760
46.121206	1495.066165	18.978778
46.265537	1498.426985	18.983795
46.361555	1493.501780	18.988813
46.009109	1502.734070	18.993831
46.450076	1494.984329	18.998848
46.219798	1498.397163	19.003866
46.111441	1501.623756	19.008883
46.085499	1502.312844	19.013901
46.165347	1499.324686	19.018919
46.131532	1500.986999	19.023936
46.440327	1515.639065	19.028954
46.767868	1511.214301	19.033971
46.903130	1513.443589	19.038989
46.790049	1513.272076	19.044007
46.477551	1517.543481	19.049024
46.623158	1520.279250	19.054042
46.686893	1514.402845	19.059059
46.676829	1503.892533	19.064077
46.555051	1511.050240	19.069095
46.807544	1517.550066	19.074112
47.497180	1529.327836	19.079130
47.085447	1532.090421	19.084147
47.642702	1539.066676	19.089165
47.129300	1543.902705	19.094183
47.505027	1530.678243	19.099200
47.581810	1537.031863	19.104218
47.500136	1534.851497	19.109235
47.906180	1529.723376	19.114253
48.023953	1523.469320	19.119271
47.784858	1516.462934	19.124288
47.639866	1503.032384	19.129306
47.295270	1499.769479	19.134323
47.424152	1504.483406	19.139341
47.605373	1523.564053	19.144359
47.959682	1526.201056	19.149376
47.835419	1524.409179	19.154394
47.656852	1526.100344	19.159411
47.948205	1527.680473	19.164429
48.036899	1521.131141	19.169447
48.095146	1524.303395	19.174464
47.741032	1524.017930	19.179482
47.921457	1521.140342	19.184499
47.904637	1520.928595	19.189517
47.643097	1523.699353	19.194535
48.129435	1533.769908	19.199552
48.285232	1536.469379	19.204570
48.369276	1548.855853	19.209587
48.645853	1547.231942	19.214605
48.517435	1546.898713	19.219623
48.634857	1541.989097	19.224640
48.834119	1550.469629	19.229658
48.558545	1540.410895	19.234675
48.660942	1528.936304	19.239693
48.388731	1538.487484	19.244711
48.329361	1542.015729	19.249728
48.596474	1527.201854	19.254746
48.576865	1539.206823	19.259763
48.979076	1534.041427	19.264781
48.652684	1538.901988	19.269799
48.486570	1536.453899	19.274816
48.689015	1535.785129	19.279834
48.992893	1548.074259	19.284851
48.642460	1553.699126	19.289869
48.930305	1571.718637	19.294887
48.991075	1562.352304	19.299904
49.132724	1565.300138	19.304922
49.170982	1565.843532	19.309939
49.137322	1567.837191	19.314957
49.255512	1557.325814	19.319975
49.145540	1558.425625	19.324992
49.627271	1565.726078	19.330010
49.571803	1582.432569	19.335027
49.713694	1580.615027	19.340045
49.813942	1588.429328	19.345063
49.662223	1587.806231	19.350080
50.025673	1586.298182	19.355098
49.934009	1581.399018	19.360115
49.746163	1564.601485	19.365133
50.114770	1578.474263	19.370151
49.738962	1570.182617	19.375168
50.056307	1582.305569	19.380186
49.721493	1580.669547	19.385203
50.257451	1582.293650	19.390221
49.948219	1586.233198	19.395239
49.953325	1586.706013	19.400256
50.181906	1579.800358	19.405274
50.273552	1590.475205	19.410291
49.987089	1589.342903	19.415309
49.884251	1591.375739	19.420327
50.001479	1591.566005	19.425344
50.398152	1594.057565	19.430362
50.259655	1610.025914	19.435379
50.469173	1607.418343	19.440397
50.298652	1606.501522	19.445415
50.544582	1613.074990	19.450432
50.917290	1607.828959	19.455450
50.645523	1611.346105	19.460467
50.470169	1607.034331	19.465485
50.660075	1612.818090	19.470503
51.001878	1619.493400	19.475520
50.968278	1622.651569	19.480538
51.226747	1630.700035	19.485555
51.282641	1633.014281	19.490573
51.374357	1627.490095	19.495591
51.122504	1623.938167	19.500608
51.182213	1627.615150	19.505626
50.840606	1628.640574	19.510643
51.088161	1627.898505	19.515661
51.267151	1627.681517	19.520679
51.039858	1624.469754	19.525696
51.250342	1629.568648	19.530714
51.311884	1631.506466	19.535731
51.742032	1644.561812	19.540749
51.890497	1645.230063	19.545767
51.840302	1646.677185	19.550784
51.789211	1640.282119	19.555802
51.753937	1633.941399	19.560819
52.159530	1645.362675	19.565837
51.791061	1634.163304	19.570855
51.843204	1638.198080	19.575872
52.225198	1637.722263	19.580890
52.124422	1638.198941	19.585907
52.355146	1625.299949	19.590925
52.027639	1624.458063	19.595943
52.278342	1631.983866	19.600960
52.481687	1626.524352	19.605978
52.376861	1629.532663	19.610995
52.115055	1618.692242	19.616013
52.274173	1633.812687	19.621031
52.243881	1646.627293	19.626048
52.589104	1644.541397	19.631066
52.348188	1649.088871	19.636083
52.413171	1640.504497	19.641101
52.439198	1643.672321	19.646119
52.364416	1638.836787	19.651136
52.475479	1643.865956	19.656154
52.532451	1644.239177	19.661171
52.764391	1665.095143	19.666189
52.905021	1665.376442	19.671207
52.852272	1668.506042	19.676224
53.134351	1671.520394	19.681242
52.973498	1672.672316	19.686259
52.956975	1671.652618	19.691277
52.939108	1668.395617	19.696295
52.983679	1666.593219	19.701312
53.121281	1654.516607	19.706330
53.246525	1657.306062	19.711347
53.061004	1663.258744	19.716365
53.320298	1668.378452	19.721383
53.518233	1682.946929	19.726400
53.768126	1675.394121	19.731418
53.696947	1692.686997	19.736435
53.640007	1682.786650	19.741453
53.845360	1675.455376	19.746471
54.078258	1686.262925	19.751488
54.396380	1681.214724	19.756506
54.359545	1668.575113	19.761523
54.287581	1654.034836	19.766541
53.674274	1655.020512	19.771559
53.705343	1656.240383	19.776576
54.146612	1665.693168	19.781594
53.904011	1672.749828	19.786611
54.131915	1674.702775	19.791629
54.169222	1681.431830	19.796647
54.079444	1682.178202	19.801664
54.198472	1675.990171	19.806682
54.405957	1674.673658	19.811699
53.939818	1673.165374	19.816717
53.839559	1680.313486	19.821735
53.806423	1699.030055	19.826752
54.480224	1706.127089	19.831770
54.505640	1709.017303	19.836787
54.880299	1703.524782	19.841805
55.303592	1702.042120	19.846823
55.193409	1711.479800	19.851840
55.278486	1710.886104	19.856858
54.879690	1708.297490	19.861875
55.057009	1697.082531	19.866893
55.475788	1691.781964	19.871911
55.125916	1696.261206	19.876928
55.761864	1700.706885	19.881946
55.384943	1696.331796	19.886963
55.539927	1697.885835	19.891981
55.563204	1696.916745	19.896999
55.344214	1702.142488	19.902016
55.417279	1699.022806	19.907034
55.536769	1701.974113	19.912051
55.357062	1693.083820	19.917069
55.331683	1692.860780	19.922087
55.069338	1706.857141	19.927104
55.326364	1696.390340	19.932122
55.480291	1697.272342	19.937139
55.195661	1702.738684	19.942157
55.171817	1704.582504	19.947175
55.295626	1716.884007	19.952192
55.436655	1719.153449	19.957210
55.836670	1731.683364	19.962227
56.109802	1737.611999	19.967245
56.262382	1749.969007	19.972263
55.790040	1759.788155	19.977280
56.543549	1749.442843	19.982298
56.393299	1757.220479	19.987315
56.333018	1753.143224	19.992333
56.626909	1746.460872	19.997351
56.395686	1752.168229	20.002368
57.073684	1743.179085	20.007386
56.667110	1747.361047	20.012403
56.629300	1739.023009	20.017421
56.925986	1731.248293	20.022439
56.540018	1753.958394	20.027456
56.561802	1753.191510	20.032474
56.984719	1753.753916	20.037491
56.413257	1747.045346	20.042509
56.708462	1740.946631	20.047527
56.550229	1747.560984	20.052544
56.936926	1751.187082	20.057562
57.376188	1763.597296	20.062579
57.092785	1768.530123	20.067597
57.282036	1764.716979	20.072615
57.361467	1777.558778	20.077632
57.369328	1771.451141	20.082650
57.079361	1764.458889	20.087667
57.059151	1760.962388	20.092685
57.440465	1764.223244	20.097703
57.384918	1771.231884	20.102720
57.402160	1769.701981	20.107738
57.577055	1781.326526	20.112755
57.585547	1791.301208	20.117773
57.943083	1803.790448	20.122791
57.746692	1799.784869	20.127808
57.790553	1805.184318	20.132826
57.791712	1795.565205	20.137843
57.741701	1801.137063	20.142861
58.009930	1798.463518	20.147879
57.974097	1806.084501	20.152896
58.014813	1815.205243	20.157914
58.294568	1820.097741	20.162931
58.561151	1824.357955	20.167949
58.590131	1822.046713	20.172967
58.418789	1826.826405	20.177984
58.720752	1816.639723	20.183002
58.766725	1824.238510	20.188019
58.924903	1818.337833	20.193037
58.888246	1821.398680	20.198055
58.971664	1821.985545	20.203072
59.000771	1819.636413	20.208090
58.936269	1811.365615	20.213107
58.654324	1807.382822	20.218125
58.812099	1816.848267	20.223143
58.915220	1814.001605	20.228160
59.023087	1814.723522	20.233178
59.006130	1815.856204	20.238195
58.861288	1817.737810	20.243213
59.522026	1806.242384	20.248231
58.986619	1819.697508	20.253248
58.886273	1813.953851	20.258266
59.166875	1826.363565	20.263283
59.235156	1834.312343	20.268301
59.380968	1835.801549	20.273319
59.114380	1833.220734	20.278336
59.412393	1837.144689	20.283354
59.584553	1831.973999	20.288371
59.462402	1836.436756	20.293389
59.722109	1841.603788	20.298407
59.718800	1845.846067	20.303424
60.085473	1856.557149	20.308442
60.067889	1844.810693	20.313459
60.260803	1844.812448	20.318477
60.293565	1846.287697	20.323495
60.089904	1844.397694	20.328512
60.344173	1837.743568	20.333530
60.199984	1840.032186	20.338547
60.145357	1851.623083	20.343565
60.450619	1835.057799	20.348583
60.461505	1833.393176	20.353600
60.605674	1839.881584	20.358618
60.622811	1833.851378	20.363635
60.621845	1838.973786	20.368653
60.728461	1834.277218	20.373671
60.299325	1839.242221	20.378688
60.411439	1849.244985	20.383706
60.979527	1860.110908	20.388723
61.119357	1860.720550	20.393741
61.471492	1864.112204	20.398759
61.278667	1868.169393	20.403776
61.014677	1869.381567	20.408794
61.342730	1861.194799	20.413811
61.245715	1870.627357	20.418829
61.049148	1865.040681	20.423847
61.154961	1860.666134	20.428864
61.021069	1864.625781	20.433882
61.335345	1871.362279	20.438899
61.363599	1879.926399	20.443917
61.987637	1884.247742	20.448935
61.425310	1892.215831	20.453952
61.895707	1888.627141	20.458970
62.104708	1883.652679	20.463987
62.062063	1890.766657	20.469005
62.071471	1887.559020	20.474023
61.791450	1886.785469	20.479040
62.017512	1889.657097	20.484058
61.973005	1888.288281	20.489075
61.927346	1883.227232	20.494093
61.835642	1883.323796	20.499111
62.063766	1892.134523	20.504128
62.355799	1911.453960	20.509146
62.404592	1904.850737	20.514163
62.349743	1908.106943	20.519181
62.730856	1909.433283	20.524199
62.406824	1906.103982	20.529216
62.181105	1898.006573	20.534234
62.420701	1901.646137	20.539251
62.804391	1906.812821	20.544269
62.940358	1918.361462	20.549287
62.897942	1927.372124	20.554304
62.965654	1931.537091	20.559322
63.147819	1918.781152	20.564339
63.268422	1928.082025	20.569357
63.504563	1935.853229	20.574375
63.423204	1928.317175	20.579392
63.032465	1933.992619	20.584410
63.235112	1925.452948	20.589427
62.970135	1925.207247	20.594445
63.362445	1917.846766	20.599463
63.436273	1923.699193	20.604480
63.328390	1924.461018	20.609498
63.522629	1933.166584	20.614515
64.007557	1946.563931	20.619533
63.715419	1946.249872	20.624551
63.921778	1957.910660	20.629568
63.827467	1949.085841	20.634586
64.104849	1945.893278	20.639603
64.219077	1948.675026	20.644621
64.036831	1947.201415	20.649639
64.055896	1942.666778	20.654656
63.958746	1945.516151	20.659674
64.293822	1944.492190	20.664691
64.358384	1949.819029	20.669709
64.190127	1939.424613	20.674727
64.215156	1939.878556	20.679744
64.132780	1953.862869	20.684762
64.633649	1961.289899	20.689779
64.401365	1964.176094	20.694797
64.427079	1964.759324	20.699815
64.659725	1972.884552	20.704832
64.507098	1970.415367	20.709850
64.722008	1970.543090	20.714867
64.839250	1989.138716	20.719885
64.913717	1985.362333	20.724903
65.379267	1986.344160	20.729920
65.255453	1990.914516	20.734938
65.283087	1985.302363	20.739955
65.517798	1988.229466	20.744973
65.345225	1987.533860	20.749991
65.207670	1976.333036	20.755008
65.392225	1984.068110	20.760026
65.605863	1978.177681	20.765043
65.768011	1981.264410	20.770061
65.763901	1974.902936	20.775079
65.647275	1983.511755	20.780096
65.748953	2007.752620	20.785114
65.906872	2012.660984	20.790131
65.759217	2010.736996	20.795149
65.907535	2010.862464	20.800167
66.193864	2006.270419	20.805184
65.889167	2011.582183	20.810202
66.376077	2010.749182	20.815219
66.277980	2005.424853	20.820237
66.248240	1999.786913	20.825255
66.301109	2004.733722	20.830272
66.371835	2019.360151	20.835290
66.657371	2021.282072	20.840307
66.856174	2027.932462	20.845325
66.567878	2027.848186	20.850343
67.013599	2018.604724	20.855360
66.767622	2035.808377	20.860378
66.915539	2014.255801	20.865395
66.997040	2022.322530	20.870413
66.956623	2015.341820	20.875431
66.772125	2014.297761	20.880448
66.869078	2032.574686	20.885466
67.570962	2032.844349	20.890483
67.162196	2028.518319	20.895501
67.076906	2039.334596	20.900519
67.533816	2040.690172	20.905536
67.495853	2052.783554	20.910554
67.956842	2054.977975	20.915571
68.187018	2044.710820	20.920589
67.728670	2040.187370	20.925607
68.104107	2035.543574	20.930624
67.945236	2043.843405	20.935642
68.115917	2044.000107	20.940659
67.919022	2036.485151	20.945677
68.090955	2041.205141	20.950695
68.366180	2029.917924	20.955712
68.295543	2045.475293	20.960730
68.206902	2035.797445	20.965747
68.427001	2034.336926	20.970765
68.519687	2039.949760	20.975783
68.675132	2037.603021	20.980800
68.497592	2035.702618	20.985818
68.214847	2035.860486	20.990835
68.418800	2035.213555	20.995853
68.338180	2032.619537	21.000871
68.565884	2032.650591	21.005888
68.405742	2035.355145	21.010906
68.454553	2049.060321	21.015923
68.697753	2060.283076	21.020941
68.880390	2064.796270	21.025959
68.886528	2052.926058	21.030976
68.776039	2060.820716	21.035994
68.872800	2065.135833	21.041011
69.194987	2071.492462	21.046029
69.342806	2076.904211	21.051047
69.418916	2079.909674	21.056064
69.314799	2078.913058	21.061082
69.441340	2081.699222	21.066099
69.446740	2087.581292	21.071117
69.206599	2084.541867	21.076135
69.647725	2099.274801	21.081152
69.978052	2107.555303	21.086170
70.362611	2112.725067	21.091187
70.577450	2104.016148	21.096205
70.450251	2103.143051	21.101223
70.321093	2098.265362	21.106240
70.199241	2101.689832	21.111258
70.020569	2107.616348	21.116275
70.259366	2101.311689	21.121293
70.375403	2102.407903	21.126311
70.491666	2096.201222	21.131328
70.603503	2096.704773	21.136346
70.619177	2100.454984	21.141363
70.885266	2098.239340	21.146381
70.678965	2094.326759	21.151399
71.089885	2085.751429	21.156416
70.998022	2097.076871	21.161434
70.786535	2087.689534	21.166451
71.082040	2094.738321	21.171469
70.905133	2115.121958	21.176487
71.245726	2118.720595	21.181504
71.093530	2112.378973	21.186522
71.157581	2126.656218	21.191539
71.283423	2121.420070	21.196557
71.101868	2118.551407	21.201575
71.262486	2108.433906	21.206592
71.156296	2131.495419	21.211610
71.763824	2135.279727	21.216627
71.910912	2135.733607	21.221645
71.868084	2153.486439	21.226663
71.965269	2133.617431	21.231680
72.083424	2137.118154	21.236698
71.961459	2147.403693	21.241715
72.278878	2144.889704	21.246733
71.765077	2136.262655	21.251751
72.193046	2143.915717	21.256768
71.819077	2143.639643	21.261786
72.054693	2153.336156	21.266803
72.244644	2157.788271	21.271821
72.227762	2158.554873	21.276839
72.396330	2159.305225	21.281856
72.549891	2165.871188	21.286874
72.572052	2164.356265	21.291891
72.813033	2182.383690	21.296909
73.250363	2189.091681	21.301927
73.378411	2184.587355	21.306944
73.021125	2183.273527	21.311962
72.972328	2170.780597	21.316979
73.452931	2166.748429	21.321997
73.253258	2174.843225	21.327015
73.543150	2171.497188	21.332032
73.571915	2168.122377	21.337050
73.347965	2170.379272	21.342067
73.621054	2164.451122	21.347085
73.440896	2161.781060	21.352103
73.627041	2170.207122	21.357120
73.688143	2172.823598	21.362138
73.709934	2167.979196	21.367155
74.009391	2163.706976	21.372173
73.722566	2165.800081	21.377191
73.927942	2186.086408	21.382208
73.870771	2189.055833	21.387226
73.874668	2186.593808	21.392243
74.310413	2190.480617	21.397261
74.028505	2196.656776	21.402279
74.325018	2188.424275	21.407296
74.349523	2200.848874	21.412314
74.294753	2208.652868	21.417331
74.698817	2213.589239	21.422349
74.542534	2214.345987	21.427367
74.535329	2221.025368	21.432384
75.063051	2212.703205	21.437402
74.484265	2216.041041	21.442419
75.063253	2210.115745	21.447437
75.137328	2219.979464	21.452455
75.650630	2229.364527	21.457472
75.743345	2221.435154	21.462490
75.603756	2215.142028	21.467507
75.709058	2206.879325	21.472525
75.495285	2211.047155	21.477543
75.118707	2206.125904	21.482560
75.595202	2215.674489	21.487578
75.561970	2237.361402	21.492595
75.990175	2233.851800	21.497613
75.746017	2230.693048	21.502631
76.088270	2229.702670	21.507648
75.878558	2235.813951	21.512666
75.900941	2229.571345	21.517683
76.571297	2221.653027	21.522701
76.109073	2225.913195	21.527719
76.089089	2231.382677	21.532736
76.563006	2239.883894	21.537754
76.335372	2255.068236	21.542771
76.656135	2256.587046	21.547789
76.849561	2255.597746	21.552807
76.759581	2261.652522	21.557824
76.659993	2251.162021	21.562842
76.107124	2255.335318	21.567859
76.563877	2260.474949	21.572877
76.851541	2258.596772	21.577895
76.912163	2264.744872	21.582912
76.990192	2278.694997	21.587930
77.222779	2271.763205	21.592947
77.446842	2275.026548	21.597965
77.283694	2282.872695	21.602983
77.462305	2276.179692	21.608000
77.468140	2275.838169	21.613018
77.354611	2279.523323	21.618035
77.371384	2274.651270	21.623053
77.273686	2282.222124	21.628071
77.373025	2296.380395	21.633088
77.818503	2299.233707	21.638106
78.310006	2307.047371	21.643123
78.143649	2299.679036	21.648141
77.714602	2303.962460	21.653159
77.742935	2296.314493	21.658176
77.712091	2313.866791	21.663194
78.012026	2330.064183	21.668211
78.400695	2324.692375	21.673229
78.607334	2329.400726	21.678247
78.181372	2331.152575	21.683264
78.395184	2321.515850	21.688282
78.336378	2330.750186	21.693299
78.842044	2337.434970	21.698317
78.585137	2348.631624	21.703335
78.572198	2351.575254	21.708352
78.581766	2348.907183	21.713370
78.640108	2367.966836	21.718387
79.101466	2368.191900	21.723405
79.411093	2369.078099	21.728423
79.858610	2365.508657	21.733440
79.505529	2363.471439	21.738458
79.875147	2365.582290	21.743475
79.978148	2365.351877	21.748493
80.223540	2361.084872	21.753511
80.518603	2366.262333	21.758528
80.303058	2353.621658	21.763546
80.045053	2338.743695	21.768563
80.288083	2328.064097	21.773581
80.101335	2328.068157	21.778599
79.735425	2336.056355	21.783616
80.347345	2342.674103	21.788634
80.240974	2362.876615	21.793651
80.258840	2351.963801	21.798669
79.895993	2355.965515	21.803687
79.972229	2363.010676	21.808704
80.590831	2370.400612	21.813722
80.180342	2382.956184	21.818739
80.529341	2381.765920	21.823757
81.059241	2389.248574	21.828775
80.800511	2388.452749	21.833792
81.332829	2403.092836	21.838810
81.233066	2401.085604	21.843827
81.299963	2401.968568	21.848845
81.566276	2405.758721	21.853863
81.421534	2413.403231	21.858880
81.813742	2403.107487	21.863898
81.593892	2410.637450	21.868915
81.602372	2404.362231	21.873933
81.766240	2401.679598	21.878951
82.091239	2400.742393	21.883968
82.123715	2397.657313	21.888986
81.804343	2404.214940	21.894003
81.506398	2403.898620	21.899021
81.407566	2399.170772	21.904039
81.367351	2413.407672	21.909056
82.320373	2419.678832	21.914074
82.012183	2424.644100	21.919091
81.793018	2423.523358	21.924109
82.189096	2436.325797	21.929127
82.189766	2457.663693	21.934144
82.517617	2453.162907	21.939162
82.786297	2452.651062	21.944179
82.981551	2451.658311	21.949197
83.231114	2449.549345	21.954215
83.206348	2452.374904	21.959232
83.077836	2449.829310	21.964250
83.107475	2444.494430	21.969267
83.049566	2446.791783	21.974285
83.595533	2451.920736	21.979303
83.480536	2454.681444	21.984320
83.861644	2465.737807	21.989338
83.475187	2447.348177	21.994355
83.626828	2462.483110	21.999373
83.928729	2459.135151	22.004391
83.599447	2465.164134	22.009408
83.830640	2461.464242	22.014426
83.816669	2466.683535	22.019443
83.893536	2466.902187	22.024461
84.121191	2457.645112	22.029479
83.596922	2467.321241	22.034496
83.596298	2468.975320	22.039514
84.113783	2481.604246	22.044531
84.076297	2490.166269	22.049549
84.450786	2489.407560	22.054567
84.320355	2505.902506	22.059584
84.822168	2507.904424	22.064602
84.598632	2518.729889	22.069619
84.912548	2510.841693	22.074637
85.167984	2506.200680	22.079655
85.367389	2510.402086	22.084672
85.405849	2504.986914	22.089690
84.950583	2505.140085	22.094707
85.077710	2504.419888	22.099725
85.225348	2509.576159	22.104743
85.392963	2530.670384	22.109760
85.733085	2526.694725	22.114778
86.096693	2528.001746	22.119795
86.182611	2536.673976	22.124813
86.009960	2532.459393	22.129831
85.660323	2537.216536	22.134848
85.495017	2538.656403	22.139866
85.786480	2528.777088	22.144883
85.663328	2536.923253	22.149901
86.227932	2542.484862	22.154919
86.221938	2560.661582	22.159936
86.322168	2556.555996	22.164954
86.541969	2555.089170	22.169971
86.244058	2559.828797	22.174989
86.539216	2558.195593	22.180007
86.383391	2575.792854	22.185024
86.742523	2578.344052	22.190042
86.764680	2578.337678	22.195059
87.012505	2570.077867	22.200077
86.946359	2573.856696	22.205095
87.344745	2582.492923	22.210112
87.494489	2593.077265	22.215130
87.679559	2596.826455	22.220147
87.697568	2595.479412	22.225165
88.155529	2599.328137	22.230183
88.051461	2590.289910	22.235200
88.067817	2566.551087	22.240218
88.092263	2566.676910	22.245235
87.911293	2571.814929	22.250253
87.817286	2580.773987	22.255271
87.844363	2589.559553	22.260288
87.961240	2590.497865	22.265306
88.602131	2586.980330	22.270323
88.305227	2589.914558	22.275341
88.490304	2596.008680	22.280359
88.150982	2594.903477	22.285376
88.409182	2593.736805	22.290394
88.605307	2609.859088	22.295411
88.792195	2615.971870	22.300429
88.855381	2615.286872	22.305447
88.540912	2624.438079	22.310464
88.802058	2618.880896	22.315482
89.047031	2622.112643	22.320499
88.930853	2619.303152	22.325517
89.205971	2622.637511	22.330535
89.186708	2639.938998	22.335552
89.582709	2642.219358	22.340570
89.507531	2634.505305	22.345587
89.427535	2640.069468	22.350605
90.005918	2644.435980	22.355623
89.532279	2639.340358	22.360640
89.517191	2645.295234	22.365658
89.793217	2653.451891	22.370675
89.850667	2666.168352	22.375693
90.261278	2669.854037	22.380711
89.870405	2668.195080	22.385728
90.259563	2662.103518	22.390746
90.460006	2657.385815	22.395763
90.301463	2678.272199	22.400781
90.511262	2680.540525	22.405799
90.497992	2691.854106	22.410816
90.578348	2690.453164	22.415834
90.823282	2690.768739	22.420851
90.645411	2697.411747	22.425869
91.087119	2696.301710	22.430887
91.100934	2713.623367	22.435904
91.232337	2707.783376	22.440922
91.459697	2712.624312	22.445939
91.417243	2705.422727	22.450957
91.851454	2709.672836	22.455975
91.743762	2713.660151	22.460992
91.925666	2710.902074	22.466010
91.687208	2707.653980	22.471027
91.797033	2703.423782	22.476045
92.202685	2717.250650	22.481063
92.289218	2726.412064	22.486080
91.905732	2722.391221	22.491098
92.382683	2733.252932	22.496115
92.396896	2736.927759	22.501133
92.572372	2736.960635	22.506151
92.283655	2733.145959	22.511168
92.363543	2730.754085	22.516186
92.819925	2741.423328	22.521203
92.686888	2752.411583	22.526221
93.052527	2752.894573	22.531239
93.002158	2763.020983	22.536256
93.144652	2764.769581	22.541274
93.181546	2761.418641	22.546291
92.827511	2764.453318	22.551309
93.068227	2768.714631	22.556327
93.103563	2775.545397	22.561344
93.315335	2784.153967	22.566362
93.542596	2779.346843	22.571379
93.466204	2788.407412	22.576397
93.850759	2793.892983	22.581415
93.996773	2802.095198	22.586432
93.860230	2804.032423	22.591450
94.331906	2804.893415	22.596467
94.353868	2803.993903	22.601485
94.581581	2802.566854	22.606503
94.428592	2801.416847	22.611520
94.442275	2801.869423	22.616538
94.304403	2803.251386	22.621555
94.327799	2809.336036	22.626573
94.657358	2805.529233	22.631591
94.993964	2815.898406	22.636608
94.945879	2817.386322	22.641626
95.314834	2810.603520	22.646643
95.167338	2812.599261	22.651661
95.292535	2800.975127	22.656679
94.781746	2799.694619	22.661696
95.170098	2813.224428	22.666714
95.584854	2816.139417	22.671731
95.674243	2830.085046	22.676749
95.538729	2822.250908	22.681767
95.887813	2820.517758	22.686784
95.961543	2830.659601	22.691802
96.179997	2823.126988	22.696819
96.220315	2826.207583	22.701837
96.248994	2821.510267	22.706855
96.030324	2831.359936	22.711872
96.411138	2834.270745	22.716890
96.648502	2837.106049	22.721907
96.626065	2845.978351	22.726925
96.882087	2843.836774	22.731943
96.666757	2845.076153	22.736960
96.619449	2844.367321	22.741978
96.729964	2847.758910	22.746995
96.806224	2853.055793	22.752013
96.840742	2846.318735	22.757031
97.292226	2860.378440	22.762048
97.270713	2873.400857	22.767066
97.095440	2869.697889	22.772083
97.021845	2874.017631	22.777101
97.595916	2878.700481	22.782119
97.742677	2878.346474	22.787136
97.985848	2893.129820	22.792154
98.067680	2884.927270	22.797171
98.192096	2900.994701	22.802189
98.245773	2888.065558	22.807207
97.898900	2886.611187	22.812224
97.754485	2904.285896	22.817242
98.491474	2902.243013	22.822259
98.305973	2908.284474	22.827277
98.731590	2912.191956	22.832295
99.010912	2910.570654	22.837312
98.896748	2914.003550	22.842330
99.105319	2912.320673	22.847347
98.988820	2918.281961	22.852365
98.829815	2918.875045	22.857383
99.165863	2926.949891	22.862400
98.420067	2938.633320	22.867418
99.330251	2937.153658	22.872435
99.070492	2937.939171	22.877453
99.346270	2956.044015	22.882471
99.847604	2956.082968	22.887488
99.489591	2977.328989	22.892506
100.069369	2965.473013	22.897523
100.201380	2971.278850	22.902541
100.229588	2967.739859	22.907559
100.333457	2962.797248	22.912576
100.067597	2962.289712	22.917594
100.540009	2975.200585	22.922611
100.143007	2983.187598	22.927629
100.422808	2981.682991	22.932647
100.541064	2991.227802	22.937664
100.558532	2993.106351	22.942682
100.679849	2990.319792	22.947699
100.571121	3010.075232	22.952717
100.666703	3015.924630	22.957735
101.255199	3010.625659	22.962752
100.985329	3014.493110	22.967770
101.195658	3030.932327	22.972787
101.236254	3030.459134	22.977805
101.398020	3029.013930	22.982823
101.485257	3037.417926	22.987840
101.484558	3039.008947	22.992858
102.213287	3036.380300	22.997875
102.007437	3049.702970	23.002893
102.006222	3058.108124	23.007911
102.648468	3057.326641	23.012928
102.689271	3066.507973	23.017946
102.619189	3066.367622	23.022963
102.708924	3062.923184	23.027981
102.676032	3062.934849	23.032999
102.787570	3061.718391	23.038016
102.939833	3059.577163	23.043034
103.168559	3055.716572	23.048051
102.680379	3054.580862	23.053069
102.829203	3058.676653	23.058087
102.890009	3055.050510	23.063104
102.853909	3065.547290	23.068122
103.328997	3069.907898	23.073139
103.429631	3081.718436	23.078157
103.419460	3082.121079	23.083175
103.530795	3077.455013	23.088192
103.865255	3085.078853	23.093210
103.862246	3096.214348	23.098227
104.042941	3097.180625	23.103245
104.257107	3096.099680	23.108263
104.595387	3087.734020	23.113280
104.501659	3089.266939	23.118298
104.396742	3095.614685	23.123315
104.645966	3089.955062	23.128333
104.568251	3105.722755	23.133351
104.995653	3105.230366	23.138368
105.165715	3111.188131	23.143386
105.174130	3111.041871	23.148403
105.118092	3114.724557	23.153421
104.823324	3118.690590	23.158439
105.165964	3116.384001	23.163456
105.246134	3126.502916	23.168474
105.418892	3114.647089	23.173491
105.659080	3130.488397	23.178509
105.362302	3136.758721	23.183527
105.729142	3137.030075	23.188544
105.560041	3139.171241	23.193562
105.923181	3140.629877	23.198579
106.239466	3158.270980	23.203597
106.136290	3162.847888	23.208615
106.243883	3158.602150	23.213632
106.501024	3165.811984	23.218650
106.282480	3159.107897	23.223667
106.608691	3162.036729	23.228685
106.647530	3177.716904	23.233703
106.843254	3177.330019	23.238720
106.660274	3177.671197	23.243738
106.919449	3184.883879	23.248755
107.155007	3183.004252	23.253773
107.048551	3200.136797	23.258791
107.676044	3205.764571	23.263808
107.418235	3210.766396	23.268826
107.660251	3202.182118	23.273843
107.889332	3198.479248	23.278861
107.988552	3198.344099	23.283879
108.256829	3194.638283	23.288896
107.879442	3184.566068	23.293914
108.254561	3189.706055	23.298931
108.694960	3206.712435	23.303949
108.254776	3220.286334	23.308967
108.204396	3222.503710	23.313984
108.637635	3218.705928	23.319002
108.574423	3221.742743	23.324019
109.061671	3221.301001	23.329037
108.682002	3214.505201	23.334055
109.101000	3213.919434	23.339072
108.974498	3221.454138	23.344090
108.954514	3233.343523	23.349107
109.475529	3241.187720	23.354125
109.345698	3238.673779	23.359143
109.271890	3243.624873	23.364160
109.413144	3241.883012	23.369178
109.428636	3249.856417	23.374195
109.647887	3251.896103	23.379213
109.601984	3267.431742	23.384231
109.680455	3258.465756	23.389248
109.868869	3271.417903	23.394266
110.068395	3291.062535	23.399283
110.673899	3295.923660	23.404301
110.934696	3296.262026	23.409319
110.561019	3291.396832	23.414336
110.708998	3289.912725	23.419354
111.008567	3289.168805	23.424371
111.376166	3271.879202	23.429389
110.932961	3291.911115	23.434407
111.341278	3302.843825	23.439424
111.436104	3305.287940	23.444442
111.051591	3322.309242	23.449459
111.819761	3319.901658	23.454477
111.689747	3316.466136	23.459495
111.757309	3314.325440	23.464512
111.897964	3320.423568	23.469530
111.894740	3315.068297	23.474547
111.997018	3331.309993	23.479565
112.001367	3337.369382	23.484583
111.781755	3337.716266	23.489600
112.191776	3342.459499	23.494618
112.377705	3355.462592	23.499635
112.698087	3358.932070	23.504653
112.245064	3369.680153	23.509671
112.851094	3362.579334	23.514688
112.627914	3365.991414	23.519706
112.820109	3387.237471	23.524723
112.827949	3382.887276	23.529741
113.373275	3386.037681	23.534759
113.244794	3382.961711	23.539776
113.181649	3393.999443	23.544794
113.534240	3408.018164	23.549811
114.107700	3405.451513	23.554829
113.760908	3401.421647	23.559847
114.404772	3410.547136	23.564864
114.475985	3413.957576	23.569882
114.109407	3404.947186	23.574899
114.650713	3408.006691	23.579917
114.882392	3425.468703	23.584935
114.827182	3428.346498	23.589952
114.908391	3430.183607	23.594970
114.951139	3425.840592	23.599987
115.296028	3420.573119	23.605005
115.029597	3432.516786	23.610023
114.833635	3426.680189	23.615040
115.409155	3430.068926	23.620058
114.930448	3430.058472	23.625075
115.344124	3430.290979	23.630093
115.456473	3444.599627	23.635111
115.577018	3445.300700	23.640128
115.826031	3452.085831	23.645146
116.118434	3438.702508	23.650163
116.223678	3433.810054	23.655181
116.005677	3448.274292	23.660199
116.392836	3460.848453	23.665216
116.512935	3469.083413	23.670234
116.843660	3468.587131	23.675251
116.923390	3460.106901	23.680269
116.735039	3467.102161	23.685287
116.912652	3469.328257	23.690304
117.245755	3470.719004	23.695322
116.921554	3468.828657	23.700339
117.092279	3474.338261	23.705357
116.981809	3466.291633	23.710375
117.023304	3480.090570	23.715392
117.437981	3483.684263	23.720410
117.134561	3494.850995	23.725427
117.716110	3484.051728	23.730445
117.633003	3505.454410	23.735463
118.036780	3503.005694	23.740480
117.740779	3508.755253	23.745498
117.898997	3510.151139	23.750515
117.948283	3520.792700	23.755533
117.831419	3531.314950	23.760551
118.285039	3538.844683	23.765568
118.741979	3540.809521	23.770586
118.722234	3551.790093	23.775603
119.303433	3551.125407	23.780621
119.029623	3552.970460	23.785639
119.266827	3549.111601	23.790656
119.050608	3553.150716	23.795674
119.116297	3565.257384	23.800691
119.774254	3569.150931	23.805709
119.908069	3576.730471	23.810727
119.975759	3566.415154	23.815744
119.816754	3573.614195	23.820762
119.828286	3575.159172	23.825779
120.008207	3579.417519	23.830797
120.001711	3592.387619	23.835815
120.717010	3599.835605	23.840832
120.424812	3598.827156	23.845850
120.396336	3606.065856	23.850867
120.881836	3602.966848	23.855885
120.883999	3614.682601	23.860903
120.938352	3622.473373	23.865920
121.234505	3615.528013	23.870938
121.460409	3620.565108	23.875955
121.360279	3614.966026	23.880973
121.521150	3624.340415	23.885991
121.574097	3634.088265	23.891008
122.010569	3644.016279	23.896026
121.785172	3648.628120	23.901043
122.180107	3637.321260	23.906061
122.025932	3643.638993	23.911079
122.031685	3639.607839	23.916096
122.400039	3633.699095	23.921114
121.997773	3653.624035	23.926131
122.437105	3657.621077	23.931149
122.778120	3667.409312	23.936167
122.867298	3671.309375	23.941184
122.908399	3671.120147	23.946202
122.848658	3683.697762	23.951219
123.017181	3694.478672	23.956237
123.333652	3696.380180	23.961255
123.057170	3684.496080	23.966272
123.469148	3688.800386	23.971290
123.515912	3715.412963	23.976307
123.330981	3705.916487	23.981325
123.872189	3715.433706	23.986343
123.649892	3728.405940	23.991360
124.117635	3733.206571	23.996378
124.196571	3746.453854	24.001395
124.485984	3741.431643	24.006413
124.279175	3737.562968	24.011431
124.236997	3749.926427	24.016448
124.331547	3746.938764	24.021466
124.576199	3766.109766	24.026483
124.835685	3765.892848	24.031501
125.258212	3775.668451	24.036519
125.329794	3783.702798	24.041536
125.470513	3779.839974	24.046554
125.555795	3784.892696	24.051571
125.405600	3789.243521	24.056589
125.527297	3785.724532	24.061607
125.530053	3797.326686	24.066624
126.228899	3798.310173	24.071642
126.034326	3816.874177	24.076659
126.376855	3812.295020	24.081677
126.366762	3806.325205	24.086695
126.161899	3818.909727	24.091712
126.674166	3824.637700	24.096730
126.593956	3836.382203	24.101747
126.776427	3835.123087	24.106765
127.102560	3834.207729	24.111783
127.265605	3841.385142	24.116800
127.263389	3843.866533	24.121818
127.555159	3863.270178	24.126835
127.619176	3860.946907	24.131853
127.340214	3862.578168	24.136871
127.359475	3863.875779	24.141888
128.007872	3862.954433	24.146906
127.867213	3872.218084	24.151923
128.313904	3878.874756	24.156941
128.624150	3877.179117	24.161959
128.128811	3886.163433	24.166976
128.512163	3883.481128	24.171994
128.713488	3899.139788	24.177011
128.715060	3899.827840	24.182029
129.002707	3900.708072	24.187047
129.301131	3903.594010	24.192064
129.271933	3901.562998	24.197082
129.220193	3906.488743	24.202099
129.591352	3920.059939	24.207117
129.701285	3927.864284	24.212135
129.904601	3930.547251	24.217152
130.032213	3918.846271	24.222170
129.906559	3921.444736	24.227187
130.023110	3926.511567	24.232205
130.295112	3931.693073	24.237223
130.549397	3943.395035	24.242240
130.686422	3939.643222	24.247258
130.420606	3938.106705	24.252275
130.956570	3939.945659	24.257293
131.051709	3938.785352	24.262311
130.821166	3952.810068	24.267328
131.343392	3954.067253	24.272346
131.353361	3956.597263	24.277363
131.535672	3954.167187	24.282381
131.617425	3959.858074	24.287399
131.167120	3955.872605	24.292416
131.744361	3980.335623	24.297434
131.822734	3988.716194	24.302451
131.896778	3981.549617	24.307469
132.221860	3978.898464	24.312487
132.291566	4006.754627	24.317504
132.468768	4011.761539	24.322522
132.602327	4008.518413	24.327539
132.502301	4011.267558	24.332557
132.723413	4012.634753	24.337575
132.975826	4029.156706	24.342592
133.082131	4032.227234	24.347610
133.293442	4034.776408	24.352627
132.931306	4038.446970	24.357645
133.445417	4026.382742	24.362663
133.209764	4043.555140	24.367680
133.478404	4048.402636	24.372698
133.588533	4054.963428	24.377715
133.735915	4058.778762	24.382733
134.128667	4073.732324	24.387751
134.524055	4080.204524	24.392768
134.652525	4086.500499	24.397786
134.501197	4080.678834	24.402803
134.708112	4071.458881	24.407821
134.851150	4067.898639	24.412839
134.913459	4081.849454	24.417856
135.192494	4089.902139	24.422874
135.416731	4094.235772	24.427891
135.399665	4089.573655	24.432909
135.720222	4091.698666	24.437927
135.576202	4098.463170	24.442944
135.548094	4099.177945	24.447962
135.784644	4115.516225	24.452979
136.123918	4120.693625	24.457997
136.444425	4118.207292	24.463015
136.490028	4120.160486	24.468032
135.989428	4129.773845	24.473050
136.048131	4133.157963	24.478067
136.487192	4139.901140	24.483085
136.625426	4137.383213	24.488103
136.953923	4161.973582	24.493120
137.157176	4162.011607	24.498138
136.983539	4162.461818	24.503155
137.545095	4163.918055	24.508173
137.723268	4167.633928	24.513191
137.747679	4185.195229	24.518208
138.027381	4188.279819	24.523226
138.321567	4184.462455	24.528243
138.137880	4190.444091	24.533261
138.345587	4187.145200	24.538279
138.208285	4194.180137	24.543296
138.587333	4202.715998	24.548314
138.844215	4212.457659	24.553331
139.004216	4216.747666	24.558349
139.142650	4208.690361	24.563367
138.759912	4214.554649	24.568384
139.208241	4215.842296	24.573402
139.450521	4230.156589	24.578419
139.464845	4234.687066	24.583437
139.641160	4229.698111	24.588455
139.557291	4231.829292	24.593472
139.843284	4232.192162	24.598490
139.946828	4246.790042	24.603507
140.054784	4251.921430	24.608525
140.477380	4249.627502	24.613543
140.185440	4258.113198	24.618560
140.613729	4269.927159	24.623578
140.591548	4275.921554	24.628595
140.371549	4287.473483	24.633613
141.055209	4282.089891	24.638631
141.474178	4298.194774	24.643648
141.324725	4301.251510	24.648666
141.715897	4297.333801	24.653683
141.623393	4312.233702	24.658701
141.768902	4300.955794	24.663719
141.782260	4323.057756	24.668736
142.202251	4324.697020	24.673754
142.032586	4319.976537	24.678771
142.276055	4322.066233	24.683789
142.850662	4310.304876	24.688807
143.163491	4303.274593	24.693824
142.792417	4298.863231	24.698842
143.504417	4290.584024	24.703859
142.887154	4293.568401	24.708877
143.374456	4300.686044	24.713895
143.380353	4312.433231	24.718912
143.384206	4323.985051	24.723930
143.838326	4318.851817	24.728947
143.476417	4320.742226	24.733965
143.766765	4326.545944	24.738983
143.859386	4331.717618	24.744000
144.271014	4345.806787	24.749018
144.304499	4340.937885	24.754035
144.417057	4347.365839	24.759053
144.607073	4353.541853	24.764071
144.499544	4347.293490	24.769088
144.889414	4360.344465	24.774106
144.997363	4362.067035	24.779123
145.149650	4370.013325	24.784141
145.154308	4363.030999	24.789159
145.142989	4377.934096	24.794176
145.049774	4384.400413	24.799194
145.405206	4390.067764	24.804211
145.055545	4407.943185	24.809229
145.221696	4417.295070	24.814247
145.510996	4428.625759	24.819264
146.112753	4444.415086	24.824282
146.438982	4443.799539	24.829299
146.687287	4453.792018	24.834317
146.786243	4457.652852	24.839335
147.000676	4473.695046	24.844352
146.864400	4476.522501	24.849370
147.273552	4474.369519	24.854387
147.731172	4481.750677	24.859405
147.825858	4487.294525	24.864423
147.902923	4494.021598	24.869440
148.384625	4488.158058	24.874458
148.320745	4480.722372	24.879475
148.207682	4496.247429	24.884493
148.447268	4487.909117	24.889511
148.870324	4496.943285	24.894528
148.475542	4490.439739	24.899546
148.674048	4499.139575	24.904563
148.684207	4509.860407	24.909581
148.789984	4515.074274	24.914599
149.169026	4517.452209	24.919616
149.113212	4515.519963	24.924634
149.548123	4528.267349	24.929651
149.467462	4534.684419	24.934669
149.818375	4539.124693	24.939687
149.351456	4550.929866	24.944704
149.869641	4558.440506	24.949722
150.143489	4567.056047	24.954739
149.893192	4576.630671	24.959757
150.236796	4584.335791	24.964775
150.491495	4594.832374	24.969792
150.150257	4590.059624	24.974810
150.739051	4600.100177	24.979827
150.837511	4619.522106	24.984845
150.732570	4611.944408	24.989863
151.121210	4628.123749	24.994880
151.161377	4644.382609	24.999898
151.622817	4646.069109	25.004915
151.539983	4652.331895	25.009933
151.484247	4662.239258	25.014951
151.798726	4670.144646	25.019968
152.268853	4682.738307	25.024986
152.802243	4672.706528	25.030003
153.052077	4684.371787	25.035021
153.072442	4676.610421	25.040039
153.215257	4681.875384	25.045056
153.167800	4685.506551	25.050074
153.165556	4676.262040	25.055091
153.867851	4681.897576	25.060109
153.204370	4677.850442	25.065127
153.247612	4673.393420	25.070144
153.544617	4692.045918	25.075162
154.050902	4698.955598	25.080179
153.892828	4708.307610	25.085197
153.980935	4710.307910	25.090215
154.064694	4730.000541	25.095232
154.435309	4734.257880	25.100250
154.225264	4736.797002	25.105267
154.361536	4745.295165	25.110285
154.638172	4760.772401	25.115303
154.601082	4772.589707	25.120320
154.992409	4791.552733	25.125338
155.341604	4785.738136	25.130355
155.264078	4793.805616	25.135373
155.378277	4803.607687	25.140391
155.731020	4803.338364	25.145408
155.757064	4824.921309	25.150426
156.209492	4824.731158	25.155443
156.396828	4827.293647	25.160461
156.495508	4840.712261	25.165479
156.727435	4847.068148	25.170496
156.972571	4859.356068	25.175514
157.059161	4863.749194	25.180531
157.312012	4853.966161	25.185549
157.143361	4863.474565	25.190567
157.451368	4877.059470	25.195584
157.455828	4885.897022	25.200602
157.937431	4883.492823	25.205619
157.981948	4884.414116	25.210637
158.444455	4907.564239	25.215655
158.449635	4909.176604	25.220672
158.484083	4907.741606	25.225690
159.116731	4899.319815	25.230707
159.142255	4900.092556	25.235725
158.899855	4903.277495	25.240743
159.268583	4922.679765	25.245760
159.313394	4917.657437	25.250778
159.290934	4923.778347	25.255795
159.616689	4932.509082	25.260813
159.735007	4948.860210	25.265831
160.105591	4951.056447	25.270848
159.870028	4956.418279	25.275866
159.980349	4954.270733	25.280883
160.154280	4962.441178	25.285901
160.157549	4973.232798	25.290919
160.207462	4971.931114	25.295936
160.351500	4995.541271	25.300954
160.959146	5001.788214	25.305971
160.736694	4999.777697	25.310989
161.018668	5023.237000	25.316007
161.571186	5022.983917	25.321024
161.461901	5025.368507	25.326042
161.625651	5034.623235	25.331059
161.666115	5055.648673	25.336077
161.945447	5053.758884	25.341095
162.478505	5066.081029	25.346112
163.013895	5067.743430	25.351130
163.602569	5060.748821	25.356147
163.491876	5050.735044	25.361165
163.339222	5056.516432	25.366183
163.861306	5045.163651	25.371200
163.993577	5048.394445	25.376218
163.880797	5033.772568	25.381235
163.721380	5033.797620	25.386253
163.992843	5048.508887	25.391271
164.070573	5042.562868	25.396288
164.098302	5043.856089	25.401306
164.220730	5039.137288	25.406323
164.677464	5033.586795	25.411341
163.993738	5044.889444	25.416359
164.376890	5054.959112	25.421376
164.327774	5062.974941	25.426394
164.703500	5081.685026	25.431411
164.798759	5092.528681	25.436429
164.848205	5102.874440	25.441447
165.482673	5110.566065	25.446464
165.593939	5113.389800	25.451482
165.929088	5110.209787	25.456499
165.911907	5119.053977	25.461517
166.117147	5137.459234	25.466535
166.134196	5145.543710	25.471552
166.348615	5141.950050	25.476570
166.658673	5153.176954	25.481587
166.752247	5158.822188	25.486605
166.633417	5169.364634	25.491623
167.272869	5170.739386	25.496640
167.505746	5188.076656	25.501658
167.665524	5185.788811	25.506675
168.009848	5176.692103	25.511693
167.999469	5187.785842	25.516711
168.151980	5206.032084	25.521728
168.666723	5210.885769	25.526746
168.565373	5214.102462	25.531763
168.446047	5212.565121	25.536781
168.434024	5228.447538	25.541799
168.748131	5233.512387	25.546816
168.929279	5240.119369	25.551834
168.962939	5241.547409	25.556851
168.931777	5250.715803	25.561869
169.328769	5263.548524	25.566887
169.420880	5275.336572	25.571904
169.760356	5292.439547	25.576922
170.089168	5296.163765	25.581939
170.209512	5294.977354	25.586957
170.100074	5312.225995	25.591975
170.664701	5314.587770	25.596992
170.837241	5320.204977	25.602010
170.899596	5325.732020	25.607027
171.420037	5336.986257	25.612045
171.206514	5338.304433	25.617063
171.436348	5332.385142	25.622080
171.707486	5338.555177	25.627098
171.660215	5348.660456	25.632115
172.325575	5353.528608	25.637133
171.953463	5359.865085	25.642151
172.541870	5351.099601	25.647168
172.471832	5374.816181	25.652186
172.384021	5385.874748	25.657203
172.635561	5373.610615	25.662221
172.551383	5383.828982	25.667239
173.232939	5402.374992	25.672256
173.260891	5410.293749	25.677274
173.308804	5416.640608	25.682292
173.810422	5425.274757	25.687309
173.836834	5430.488618	25.692327
173.817146	5432.991886	25.697344
174.305070	5447.805507	25.702362
174.213076	5456.301665	25.707380
174.620557	5457.175946	25.712397
174.532593	5466.179682	25.717415
174.775524	5465.570759	25.722432
175.010136	5481.383433	25.727450
174.868039	5483.602738	25.732468
175.124063	5484.443783	25.737485
175.055890	5507.642573	25.742503
175.802343	5505.894657	25.747520
175.701916	5505.544365	25.752538
175.663813	5523.880577	25.757556
176.227839	5530.475402	25.762573
176.170270	5539.322928	25.767591
176.548339	5543.967555	25.772608
176.635512	5557.281167	25.777626
176.672814	5565.141718	25.782644
177.120221	5571.019238	25.787661
177.120034	5581.439284	25.792679
177.385148	5587.032691	25.797696
177.476689	5594.398700	25.802714
177.658075	5607.615611	25.807732
178.302972	5614.886006	25.812749
178.449933	5615.538861	25.817767
178.591102	5606.565110	25.822784
178.658040	5620.715251	25.827802
178.825416	5628.959617	25.832820
179.008249	5633.287441	25.837837
178.735602	5636.496156	25.842855
179.323054	5646.606946	25.847872
179.662183	5652.441376	25.852890
179.299249	5660.320088	25.857908
180.006694	5671.270797	25.862925
179.986431	5690.134703	25.867943
180.040638	5689.466771	25.872960
179.985549	5688.209794	25.877978
180.066508	5707.313640	25.882996
180.668237	5709.019437	25.888013
180.627551	5724.805739	25.893031
180.568539	5732.252062	25.898048
180.994084	5735.162696	25.903066
180.978844	5753.621843	25.908084
181.394289	5750.167222	25.913101
181.621178	5769.658770	25.918119
181.931588	5785.800818	25.923136
182.488785	5777.595551	25.928154
182.258729	5792.243457	25.933172
182.572063	5799.110998	25.938189
182.692159	5800.793936	25.943207
182.931479	5809.996258	25.948224
183.395319	5822.673764	25.953242
183.216401	5827.389398	25.958260
183.280564	5827.379640	25.963277
183.384249	5836.173795	25.968295
183.674344	5847.101204	25.973312
183.778644	5860.664899	25.978330
184.254009	5878.580613	25.983348
184.471730	5876.776091	25.988365
184.484252	5881.919642	25.993383
184.400249	5891.563763	25.998400
185.213202	5903.227363	26.003418
185.005036	5906.227218	26.008436
185.336739	5910.434076	26.013453
185.547916	5929.865109	26.018471
185.865157	5934.500367	26.023488
185.779825	5932.231651	26.028506
185.823283	5944.924186	26.033524
186.446391	5949.761200	26.038541
186.450659	5956.414921	26.043559
186.820289	5956.120858	26.048576
186.745150	5953.178192	26.053594
186.892849	5975.081320	26.058612
187.281819	5973.606826	26.063629
187.215294	5990.931500	26.068647
187.256080	5994.397670	26.073664
187.577346	5993.132582	26.078682
187.542972	5998.649636	26.083700
187.846266	6003.331276	26.088717
187.963960	6018.610210	26.093735
188.491979	6028.512659	26.098752
188.641905	6024.108144	26.103770
188.638328	6045.166834	26.108788
189.087852	6051.577653	26.113805
189.069748	6058.193857	26.118823
189.249170	6071.076807	26.123840
189.619196	6077.073865	26.128858
189.750014	6085.390420	26.133876
190.291044	6084.065858	26.138893
189.929858	6080.908862	26.143911
190.137281	6099.927140	26.148928
190.503509	6100.239681	26.153946
190.703946	6108.592758	26.158964
190.914025	6116.088885	26.163981
190.822036	6121.343474	26.168999
191.173543	6126.244918	26.174016
191.173717	6136.800961	26.179034
191.659002	6152.054343	26.184052
191.800441	6155.842635	26.189069
191.975843	6165.844252	26.194087
192.159894	6177.830066	26.199104
192.699498	6166.514900	26.204122
192.665328	6188.336116	26.209140
192.922728	6197.829389	26.214157
192.871700	6205.369361	26.219175
193.161262	6213.105687	26.224192
193.858840	6220.538585	26.229210
193.474981	6220.930030	26.234228
194.244752	6215.327288	26.239245
194.230210	6234.317132	26.244263
194.779497	6235.788083	26.249280
194.728869	6235.240623	26.254298
195.032222	6238.542851	26.259316
194.966519	6229.149598	26.264333
195.321432	6240.966802	26.269351
195.306021	6255.909954	26.274368
195.634242	6254.687960	26.279386
195.628713	6271.293152	26.284404
195.721825	6263.750220	26.289421
195.787913	6272.970277	26.294439
195.890536	6281.543845	26.299456
195.704257	6296.671467	26.304474
196.019376	6307.942491	26.309492
196.345133	6324.508780	26.314509
196.621066	6332.086287	26.319527
196.672784	6340.263753	26.324544
196.988507	6353.971673	26.329562
197.293458	6375.083723	26.334580
197.211305	6397.089433	26.339597
197.825440	6397.016147	26.344615
197.756614	6406.295156	26.349632
198.219068	6428.244524	26.354650
198.515877	6438.644073	26.359668
198.597601	6445.522666	26.364685
198.535338	6448.316805	26.369703
198.581248	6462.540320	26.374720
199.486157	6473.830107	26.379738
199.384372	6488.171338	26.384756
199.195044	6494.820672	26.389773
199.948412	6501.496859	26.394791
200.096798	6505.760807	26.399808
200.147464	6499.758550	26.404826
200.341794	6513.703303	26.409844
200.366204	6525.070230	26.414861
200.942498	6526.988411	26.419879
200.901256	6540.022845	26.424896
201.516980	6545.795560	26.429914
201.062677	6554.408613	26.434932
201.214575	6554.221046	26.439949
201.395615	6573.749002	26.444967
201.484784	6587.167227	26.449984
201.771861	6596.684497	26.455002
202.231381	6615.951327	26.460020
202.774781	6626.454645	26.465037
202.813673	6630.931387	26.470055
202.640528	6643.563428	26.475072
203.333565	6647.502700	26.480090
203.063497	6667.770218	26.485108
203.311349	6677.745052	26.490125
203.885115	6677.880083	26.495143
203.786642	6691.378106	26.500160
204.010526	6708.790829	26.505178
204.319957	6714.324020	26.510196
204.351611	6727.703951	26.515213
205.094932	6735.016297	26.520231
204.703558	6745.466343	26.525248
205.453256	6755.669293	26.530266
205.391521	6767.902106	26.535284
205.393108	6772.204755	26.540301
206.203586	6784.279688	26.545319
206.374285	6799.642568	26.550336
206.705411	6790.720739	26.555354
206.917472	6790.214440	26.560372
206.723904	6807.685936	26.565389
207.052532	6806.545920	26.570407
207.097863	6822.790135	26.575424
207.818033	6830.567013	26.580442
208.016511	6832.588244	26.585460
208.156435	6834.501792	26.590477
208.536551	6828.962689	26.595495
208.579370	6834.587934	26.600512
209.144100	6847.897586	26.605530
209.164212	6845.792275	26.610548
209.079348	6844.066337	26.615565
209.348282	6843.393344	26.620583
209.472223	6855.846694	26.625600
209.448892	6866.700397	26.630618
209.897599	6868.199688	26.635636
209.809427	6870.947417	26.640653
210.239919	6892.592955	26.645671
210.304545	6899.818470	26.650688
210.615728	6892.651710	26.655706
210.708027	6905.390973	26.660724
210.561272	6911.516117	26.665741
211.182708	6925.426257	26.670759
211.045209	6938.324435	26.675776
211.399008	6948.573347	26.680794
211.805187	6956.064543	26.685812
211.849217	6970.626523	26.690829
212.058899	6965.675823	26.695847
212.112437	6988.863857	26.700864
212.665210	6989.677715	26.705882
212.407461	7006.711128	26.710900
212.834880	7019.729760	26.715917
213.162828	7018.684540	26.720935
213.646943	7034.674379	26.725952
213.652198	7050.498867	26.730970
214.085117	7052.736168	26.735988
214.322100	7068.833962	26.741005
214.722829	7067.736370	26.746023
214.507833	7076.403956	26.751040
214.484039	7072.752303	26.756058
214.857682	7079.541490	26.761076
215.131186	7095.030670	26.766093
215.234551	7088.855861	26.771111
215.418817	7121.244769	26.776128
215.648862	7130.221910	26.781146
215.789714	7128.577606	26.786164
216.199096	7145.753515	26.791181
216.673486	7134.492105	26.796199
216.683666	7149.466726	26.801216
216.752133	7163.800920	26.806234
217.354028	7169.045640	26.811252
217.283793	7168.485420	26.816269
217.636292	7176.427021	26.821287
217.860864	7190.140290	26.826304
218.000912	7198.680050	26.831322
218.398780	7208.890679	26.836340
218.166705	7227.921734	26.841357
218.420006	7224.037499	26.846375
218.569036	7247.829734	26.851392
218.669116	7250.156761	26.856410
219.241487	7260.671719	26.861428
219.575568	7275.242449	26.866445
219.888666	7280.345910	26.871463
219.859289	7293.003367	26.876480
220.244458	7305.905664	26.881498
220.473419	7309.345944	26.886516
220.507767	7320.774954	26.891533
220.893072	7326.549067	26.896551
220.793811	7330.678136	26.901568
221.203330	7342.244474	26.906586
221.395583	7351.385451	26.911604
221.506209	7355.125124	26.916621
222.088751	7371.030482	26.921639
222.426017	7383.741409	26.926656
222.465763	7394.661369	26.931674
222.725184	7400.193084	26.936692
222.745527	7411.772704	26.941709
223.037275	7420.156360	26.946727
223.236419	7429.233166	26.951744
223.699459	7444.563700	26.956762
223.985856	7448.437027	26.961780
223.547396	7448.616013	26.966797
224.420516	7465.000254	26.971815
224.274978	7486.458371	26.976832
224.619814	7487.036293	26.981850
225.178803	7493.919896	26.986868
225.070744	7502.138540	26.991885
224.787693	7506.952895	26.996903
225.436529	7521.017068	27.001920
225.356817	7536.403768	27.006938
225.988767	7545.239619	27.011956
226.160889	7552.647539	27.016973
226.781539	7564.373718	27.021991
226.967438	7567.375628	27.027008
227.376839	7570.203839	27.032026
228.021328	7552.260953	27.037044
227.603409	7565.989296	27.042061
228.325644	7574.504886	27.047079
228.454972	7585.208970	27.052096
228.659368	7583.794658	27.057114
228.477210	7582.904591	27.062132
228.478696	7588.909017	27.067149
228.681914	7590.708612	27.072167
229.271257	7608.699830	27.077184
228.848287	7604.665095	27.082202
229.086203	7612.719432	27.087220
229.432075	7636.102695	27.092237
229.569451	7641.858684	27.097255
229.576080	7654.078287	27.102272
229.905592	7676.750686	27.107290
230.393395	7689.520469	27.112308
230.251305	7696.143940	27.117325
230.325153	7711.301679	27.122343
230.775881	7730.501600	27.127360
230.552423	7746.198135	27.132378
230.955580	7746.741730	27.137396
231.036207	7777.916729	27.142413
231.615401	7778.931713	27.147431
231.918651	7802.271312	27.152448
232.266994	7817.506366	27.157466
232.441847	7819.465091	27.162484
232.898399	7843.099725	27.167501
233.273006	7850.176331	27.172519
233.459879	7870.958068	27.177536
233.730071	7880.907981	27.182554
234.144527	7882.870450	27.187572
234.404396	7895.682177	27.192589
234.576715	7901.852682	27.197607
234.830377	7905.005103	27.202624
234.816031	7920.170430	27.207642
235.093212	7930.292915	27.212660
235.384642	7941.492868	27.217677
235.636900	7950.883673	27.222695
235.919687	7956.440332	27.227712
235.932747	7977.874329	27.232730
236.312039	7981.805917	27.237748
236.514655	7992.325195	27.242765
236.582162	8018.669323	27.247783
236.897078	8013.335751	27.252800
236.636182	8036.813990	27.257818
237.217239	8053.638853	27.262836
237.522381	8063.782314	27.267853
238.057056	8083.364157	27.272871
238.186308	8094.021195	27.277888
238.052713	8104.431875	27.282906
239.168545	8109.170661	27.287924
239.088352	8118.865869	27.292941
239.525323	8132.186877	27.297959
239.813883	8140.782879	27.302976
240.017034	8151.526312	27.307994
240.120084	8143.649577	27.313012
240.169580	8166.795527	27.318029
240.281712	8173.332235	27.323047
240.602384	8189.503221	27.328064
240.808404	8196.438887	27.333082
240.789399	8211.706204	27.338100
241.133729	8229.215270	27.343117
241.482386	8232.927534	27.348135
241.919337	8248.442753	27.353152
241.999597	8257.857335	27.358170
242.291799	8268.605914	27.363188
242.070859	8287.172246	27.368205
242.608037	8296.414686	27.373223
243.009250	8299.610501	27.378240
243.406472	8320.647286	27.383258
243.791688	8332.050710	27.388276
244.030006	8337.409201	27.393293
244.213443	8350.081607	27.398311
244.607013	8360.426143	27.403328
244.639203	8361.605250	27.408346
245.048234	8369.535411	27.413364
245.285191	8378.048004	27.418381
245.167606	8377.646656	27.423399
245.526593	8382.575959	27.428416
245.500521	8401.260447	27.433434
245.908947	8397.970597	27.438452
246.144674	8408.516528	27.443469
246.156344	8439.592885	27.448487
246.192834	8440.102035	27.453504
246.707579	8454.153074	27.458522
246.688611	8457.130199	27.463540
247.206347	8478.704042	27.468557
247.143254	8490.414140	27.473575
247.555429	8501.068408	27.478592
247.606116	8522.266714	27.483610
248.115277	8542.992718	27.488628
248.276943	8553.992252	27.493645
248.419914	8566.374342	27.498663
248.747571	8593.035537	27.503680
249.146383	8605.346251	27.508698
249.194053	8612.003648	27.513716
249.590587	8627.156100	27.518733
249.622602	8645.190904	27.523751
250.239183	8656.419598	27.528768
250.302690	8682.200177	27.533786
250.862004	8683.224625	27.538804
251.618556	8694.652547	27.543821
251.676387	8706.066131	27.548839
251.841920	8706.337358	27.553856
252.132950	8720.745454	27.558874
251.913218	8727.444523	27.563892
252.446282	8752.899529	27.568909
252.515774	8759.853506	27.573927
253.003868	8761.867749	27.578944
253.416090	8788.743372	27.583962
253.340203	8794.315083	27.588980
253.934946	8798.658457	27.593997
254.381849	8808.259336	27.599015
254.567945	8816.063385	27.604032
254.847109	8828.705431	27.609050
255.201799	8824.473581	27.614068
255.475944	8838.155105	27.619085
255.461328	8848.285639	27.624103
256.101639	8847.456889	27.629120
256.127800	8860.911839	27.634138
256.143117	8870.122161	27.639156
256.658528	8878.392734	27.644173
256.603850	8885.056692	27.649191
256.867618	8894.203088	27.654208
257.022538	8898.775974	27.659226
257.674244	8917.604875	27.664244
257.618071	8933.901485	27.669261
257.339719	8932.439101	27.674279
257.818834	8953.293372	27.679296
258.160309	8971.214016	27.684314
258.202888	8977.556623	27.689332
258.372324	8994.039160	27.694349
258.661233	9010.351569	27.699367
259.383464	9020.178050	27.704384
260.117164	9015.647208	27.709402
260.560280	9015.701581	27.714420
261.253774	9033.074965	27.719437
261.044328	9039.542073	27.724455
261.559778	9039.402070	27.729472
261.510697	9038.083940	27.734490
261.502545	9040.431203	27.739508
261.911222	9048.712156	27.744525
261.632072	9072.409236	27.749543
262.371187	9063.495409	27.754560
262.071912	9068.925181	27.759578
262.297101	9078.080832	27.764596
262.554654	9091.098966	27.769613
262.798742	9110.042040	27.774631
262.888290	9114.830372	27.779648
263.215179	9138.793101	27.784666
263.258219	9152.573981	27.789684
263.147912	9166.533447	27.794701
263.505234	9183.217375	27.799719
263.846704	9205.883479	27.804736
264.095002	9225.627938	27.809754
264.408446	9245.618008	27.814772
264.790502	9261.710920	27.819789
264.837378	9288.612577	27.824807
265.194179	9304.845217	27.829824
265.722998	9328.574693	27.834842
265.818377	9347.212812	27.839860
266.159569	9359.514058	27.844877
266.190316	9383.949432	27.849895
266.927585	9401.054299	27.854912
267.449523	9413.905211	27.859930
267.610782	9427.680519	27.864948
267.979287	9436.378339	27.869965
268.451281	9460.596727	27.874983
268.585460	9465.084581	27.880000
269.122091	9469.137227	27.885018
269.859041	9465.897075	27.890036
270.401842	9449.685718	27.895053
270.403871	9454.604582	27.900071
270.737826	9453.529882	27.905088
270.899257	9469.111124	27.910106
271.210034	9472.592747	27.915124
271.509733	9473.796579	27.920141
271.910806	9475.461370	27.925159
271.856601	9465.306942	27.930176
272.335200	9471.405031	27.935194
272.274542	9493.878359	27.940212
272.652774	9494.713200	27.945229
272.150480	9505.731426	27.950247
272.647556	9516.032083	27.955264
273.036688	9536.225375	27.960282
272.881900	9552.749415	27.965300
273.417747	9562.466287	27.970317
273.228381	9576.337338	27.975335
273.587755	9592.598245	27.980352
274.214317	9608.454487	27.985370
274.441389	9622.447015	27.990388
274.796225	9639.857909	27.995405
274.666155	9662.462223	28.000423
275.222287	9675.993119	28.005440
275.579056	9692.541830	28.010458
275.516994	9706.030073	28.015476
275.833430	9722.433542	28.020493
276.107622	9736.721918	28.025511
276.827735	9752.630021	28.030528
276.933988	9779.971479	28.035546
276.769579	9786.791764	28.040564
277.086600	9807.817470	28.045581
277.317825	9830.229975	28.050599
277.804660	9836.601587	28.055616
277.805072	9858.690131	28.060634
278.300525	9875.053236	28.065652
278.345296	9883.880600	28.070669
278.777274	9910.795821	28.075687
279.262908	9939.515019	28.080704
279.325061	9949.160606	28.085722
279.551298	9972.552824	28.090740
280.359574	9989.227260	28.095757
280.544969	10004.486332	28.100775
280.380200	10020.595575	28.105792
280.900685	10030.640289	28.110810
281.420422	10045.825241	28.115828
281.894395	10052.861968	28.120845
281.848288	10068.093988	28.125863
281.754316	10084.946865	28.130880
282.486322	10100.477694	28.135898
282.803930	10120.777477	28.140916
283.166108	10122.249472	28.145933
283.167594	10135.759705	28.150951
283.227062	10144.348105	28.155968
283.636559	10162.013038	28.160986
283.730430	10188.400349	28.166004
284.067894	10200.289122	28.171021
284.219886	10224.053153	28.176039
284.887954	10237.140789	28.181056
285.421090	10255.563271	28.186074
285.061027	10267.380713	28.191092
285.730375	10283.060374	28.196109
286.235615	10302.185022	28.201127
286.675806	10313.783184	28.206144
286.903242	10333.724669	28.211162
287.338840	10353.652712	28.216180
287.703872	10363.582884	28.221197
287.956898	10372.434890	28.226215
288.209954	10377.794837	28.231232
288.676816	10391.583272	28.236250
288.549057	10397.971828	28.241268
288.917221	10418.579804	28.246285
289.191865	10430.500606	28.251303
289.063276	10447.125554	28.256320
289.717459	10459.934502	28.261338
289.785008	10480.232562	28.266356
289.969516	10489.995149	28.271373
290.590426	10500.756999	28.276391
291.381311	10518.861764	28.281408
291.709579	10525.375125	28.286426
291.568390	10537.824873	28.291444
291.927680	10545.962632	28.296461
291.992637	10559.659050	28.301479
292.295558	10581.063557	28.306496
292.598626	10599.818996	28.311514
292.688554	10607.092540	28.316532
293.138756	10632.998754	28.321549
293.313145	10642.425152	28.326567
293.596280	10663.532879	28.331584
293.920536	10683.649111	28.336602
294.185673	10694.876928	28.341620
294.339431	10708.265989	28.346637
294.626549	10727.412404	28.351655
295.104903	10749.121322	28.356672
295.792785	10765.319483	28.361690
295.904922	10782.200893	28.366708
296.340622	10801.753664	28.371725
296.573318	10812.055156	28.376743
296.789053	10838.484405	28.381760
297.089694	10833.379591	28.386778
297.665584	10852.759032	28.391796
298.020680	10866.950430	28.396813
297.794246	10879.230544	28.401831
298.261549	10890.897467	28.406848
298.477055	10906.427290	28.411866
298.302006	10927.631908	28.416884
299.290867	10944.323295	28.421901
299.407396	10969.789359	28.426919
299.567392	10975.855454	28.431936
300.047473	10997.349685	28.436954
300.139691	11012.055742	28.441972
300.559856	11019.391702	28.446989
300.813073	11034.325310	28.452007
300.806597	11052.182149	28.457024
301.402634	11058.518238	28.462042
301.829963	11077.472678	28.467060
301.999325	11099.113282	28.472077
302.027913	11104.085281	28.477095
302.358441	11121.119289	28.482112
302.996212	11135.756296	28.487130
303.379872	11143.221132	28.492148
303.319261	11159.580371	28.497165
303.827951	11179.403193	28.502183
303.550594	11200.898752	28.507200
304.331210	11219.283660	28.512218
304.637027	11230.221290	28.517236
304.746561	11248.890684	28.522253
305.823796	11269.847049	28.527271
305.781806	11280.693611	28.532288
306.278257	11301.424679	28.537306
306.504078	11314.136716	28.542324
306.635412	11322.866031	28.547341
307.045285	11337.737602	28.552359
307.019157	11359.952040	28.557376
307.435965	11369.101091	28.562394
307.507818	11390.454089	28.567412
308.030800	11408.086748	28.572429
308.239179	11424.170682	28.577447
308.518031	11437.809182	28.582464
309.342626	11459.824985	28.587482
309.452356	11465.886435	28.592500
309.627538	11482.117677	28.597517
309.889351	11504.325348	28.602535
310.610026	11523.866085	28.607552
311.025892	11527.625390	28.612570
311.315896	11541.265388	28.617588
311.782393	11546.248267	28.622605
312.353125	11547.732116	28.627623
312.668886	11566.893877	28.632640
312.941618	11558.051483	28.637658
313.101036	11574.730478	28.642676
313.146769	11589.368444	28.647693
313.946295	11593.595348	28.652711
314.276096	11611.267748	28.657728
314.659312	11600.797765	28.662746
314.927652	11605.464177	28.667764
314.642932	11625.575190	28.672781
315.387593	11633.628168	28.677799
315.618907	11652.099021	28.682816
316.169201	11652.885076	28.687834
316.153510	11666.661170	28.692852
316.250559	11680.296575	28.697869
316.576300	11688.730557	28.702887
316.802914	11709.744065	28.707904
316.964659	11714.913370	28.712922
317.167291	11749.587290	28.717940
317.492071	11762.947324	28.722957
317.953939	11777.432237	28.727975
317.683957	11801.721823	28.732992
318.129465	11822.126693	28.738010
318.553643	11839.096254	28.743028
318.708743	11858.415946	28.748045
319.255682	11885.871862	28.753063
319.095155	11909.086739	28.758080
319.741995	11933.783188	28.763098
320.065956	11950.291649	28.768116
320.542127	11985.283389	28.773133
321.097605	11998.029825	28.778151
321.435886	12009.916467	28.783168
321.468852	12021.361215	28.788186
321.664203	12034.372146	28.793204
321.935545	12058.353593	28.798221
322.594511	12066.322214	28.803239
322.546125	12096.814062	28.808256
323.015320	12109.106672	28.813274
323.243142	12133.508645	28.818292
323.608266	12155.827311	28.823309
323.902171	12172.640626	28.828327
324.399849	12197.013299	28.833344
324.815174	12218.209562	28.838362
325.056742	12229.704060	28.843380
325.142980	12252.107309	28.848397
325.753212	12265.581144	28.853415
325.828718	12293.796272	28.858432
326.464223	12305.829449	28.863450
326.993629	12329.799486	28.868468
326.971532	12344.379130	28.873485
327.721252	12360.420639	28.878503
327.852949	12372.529136	28.883520
328.398063	12396.181040	28.888538
328.819942	12418.437502	28.893556
328.868877	12427.966432	28.898573
329.315779	12450.354817	28.903591
329.424604	12464.895226	28.908608
329.473764	12480.193317	28.913626
330.202098	12497.643463	28.918644
330.261078	12520.745977	28.923661
330.917549	12536.764261	28.928679
330.777980	12553.639087	28.933696
331.455907	12579.282027	28.938714
331.622641	12582.003541	28.943732
332.245755	12604.705713	28.948749
332.980516	12619.401413	28.953767
333.401453	12640.988841	28.958784
333.781819	12651.303091	28.963802
334.327176	12656.706605	28.968820
334.138716	12673.794404	28.973837
334.512481	12672.012308	28.978855
335.205613	12689.357591	28.983872
335.483879	12703.818123	28.988890
335.685738	12717.564275	28.993908
335.892280	12734.167492	28.998925
336.280124	12735.326243	29.003943
336.346791	12752.923847	29.008960
336.574270	12764.964003	29.013978
337.504438	12778.281035	29.018996
337.411278	12792.603678	29.024013
337.835661	12807.104697	29.029031
338.144642	12822.757340	29.034048
338.395327	12842.211577	29.039066
338.701707	12862.424509	29.044084
339.031673	12875.137179	29.049101
339.474462	12897.220431	29.054119
339.343812	12924.979140	29.059136
339.571953	12930.555274	29.064154
340.269402	12947.451716	29.069172
340.352061	12965.448070	29.074189
340.816928	12979.620822	29.079207
340.970155	13016.663656	29.084224
341.283426	13032.966316	29.089242
341.920248	13046.329208	29.094260
342.066569	13080.673302	29.099277
342.584357	13096.445240	29.104295
342.744475	13114.347573	29.109312
342.877529	13144.133932	29.114330
343.577626	13156.400755	29.119348
344.200429	13183.448868	29.124365
344.702791	13188.268713	29.129383
345.005088	13213.238377	29.134400
345.040692	13225.633958	29.139418
345.303400	13232.212156	29.144436
345.764589	13247.977243	29.149453
346.223852	13260.303733	29.154471
346.321945	13263.948654	29.159488
347.010898	13285.662462	29.164506
347.714905	13299.147705	29.169524
347.565440	13329.572020	29.174541
348.025227	13332.709069	29.179559
348.372716	13346.862478	29.184576
348.383089	13367.049402	29.189594
348.727946	13368.240149	29.194612
349.214933	13395.041291	29.199629
349.284741	13423.521100	29.204647
349.810716	13428.962593	29.209664
349.787599	13450.939028	29.214682
350.261263	13475.654992	29.219700
350.711598	13505.215682	29.224717
351.084475	13518.354739	29.229735
351.219091	13543.742525	29.234752
351.279532	13568.014518	29.239770
352.053951	13588.458520	29.244788
352.413885	13622.340865	29.249805
352.517362	13640.100934	29.254823
353.012505	13673.340209	29.259840
353.683077	13694.122603	29.264858
353.852442	13713.277763	29.269876
354.277998	13744.377442	29.274893
354.735736	13761.940365	29.279911
355.002756	13779.864580	29.284928
355.155745	13806.257243	29.289946
355.712189	13828.207046	29.294964
356.218695	13859.325891	29.299981
356.486453	13867.201446	29.304999
356.810482	13899.567739	29.310016
357.084842	13923.191080	29.315034
357.545222	13949.637142	29.320052
357.635522	13972.310226	29.325069
358.520405	13977.752846	29.330087
358.944762	13995.618034	29.335104
359.121232	14016.442967	29.340122
359.595678	14042.217475	29.345140
359.546902	14066.614481	29.350157
359.899523	14083.840373	29.355175
360.893241	14107.535115	29.360192
360.796674	14131.652267	29.365210
361.013543	14149.960443	29.370228
361.251193	14181.393262	29.375245
361.622703	14195.376192	29.380263
362.401070	14227.738631	29.385280
362.615238	14245.447296	29.390298
363.073885	14266.806492	29.395316
363.705484	14281.538502	29.400333
364.176334	14298.013519	29.405351
364.911814	14316.231642	29.410368
364.981827	14331.019540	29.415386
365.767414	14334.387102	29.420404
366.153040	14358.328415	29.425421
365.881176	14363.733330	29.430439
366.698895	14380.479696	29.435456
366.763898	14395.423168	29.440474
367.353135	14411.475622	29.445492
367.602970	14420.055286	29.450509
368.088320	14443.150612	29.455527
368.046143	14445.554376	29.460544
368.667112	14468.281233	29.465562
369.064046	14458.897073	29.470580
369.335377	14474.244297	29.475597
369.931807	14476.570751	29.480615
370.033554	14481.510144	29.485632
370.769098	14502.649648	29.490650
370.818918	14505.711765	29.495668
371.083221	14528.901613	29.500685
371.713673	14542.332879	29.505703
372.130077	14547.851760	29.510720
372.113937	14556.084450	29.515738
372.740543	14582.148653	29.520756
373.107334	14588.670065	29.525773
373.607625	14597.997181	29.530791
373.868392	14607.462649	29.535808
374.049400	14619.883876	29.540826
374.518595	14641.863997	29.545844
374.433688	14658.520593	29.550861
375.070794	14669.604451	29.555879
375.522510	14687.298652	29.560896
375.342791	14710.418892	29.565914
375.969898	14721.346432	29.570932
376.282678	14755.904503	29.575949
376.749758	14775.263877	29.580967
376.924920	14800.669139	29.585984
376.888940	14828.207456	29.591002
377.352134	14851.050921	29.596020
377.694122	14877.813572	29.601037
378.258744	14907.560778	29.606055
378.824357	14930.612621	29.611072
378.943753	14978.332747	29.616090
379.515820	14986.120336	29.621108
379.748565	15016.686810	29.626125
379.955067	15043.761337	29.631143
380.518265	15062.000684	29.636160
381.180809	15093.024623	29.641178
381.773888	15112.851082	29.646196
382.609696	15134.304130	29.651213
382.991782	15153.598167	29.656231
383.396763	15157.347269	29.661248
383.759220	15182.657559	29.666266
384.425336	15196.911181	29.671284
384.300095	15209.077285	29.676301
384.659134	15231.792146	29.681319
385.165841	15234.350579	29.686336
385.256232	15263.092070	29.691354
385.710052	15278.556810	29.696372
386.125824	15305.990747	29.701389
386.153054	15325.930787	29.706407
386.989628	15342.242396	29.711424
387.236891	15378.324577	29.716442
387.488285	15395.848499	29.721460
388.188351	15411.720320	29.726477
388.425519	15435.821906	29.731495
389.028985	15441.567742	29.736512
389.493556	15465.147595	29.741530
389.875744	15483.409211	29.746548
390.484672	15497.542474	29.751565
390.582204	15518.011828	29.756583
391.087717	15526.207939	29.761600
391.604484	15547.932201	29.766618
391.745136	15565.385089	29.771636
392.443620	15582.950118	29.776653
392.445568	15594.471333	29.781671
392.873655	15609.744538	29.786688
392.908192	15636.950901	29.791706
393.066070	15659.634424	29.796724
393.835394	15666.797832	29.801741
394.227368	15684.379090	29.806759
394.952544	15692.976917	29.811776
394.944356	15718.550909	29.816794
395.356606	15729.259819	29.821812
395.590946	15742.090367	29.826829
395.804843	15778.649081	29.831847
395.994065	15795.276623	29.836864
396.307943	15826.204439	29.841882
396.889903	15846.911398	29.846900
397.584580	15873.415251	29.851917
397.642717	15895.893501	29.856935
398.359055	15917.047044	29.861952
398.567022	15948.525299	29.866970
399.297375	15957.741469	29.871988
399.978101	15987.068021	29.877005
400.530903	16011.418075	29.882023
400.578162	16025.623381	29.887040
400.957313	16044.640845	29.892058
401.337168	16058.390131	29.897076
401.914087	16080.629917	29.902093
401.921680	16107.029452	29.907111
402.163595	16127.249580	29.912128
402.745230	16158.508932	29.917146
403.053781	16174.376016	29.922164
403.534127	16195.004422	29.927181
403.529069	16235.122810	29.932199
404.140151	16261.981319	29.937216
404.536523	16284.536860	29.942234
404.843445	16316.537235	29.947252
405.251753	16346.971120	29.952269
405.609853	16384.942442	29.957287
406.420121	16396.976290	29.962304
406.817191	16426.941452	29.967322
407.104655	16460.540082	29.972340
407.772235	16475.887239	29.977357
407.769757	16507.844508	29.982375
408.492664	16524.515934	29.987392
409.180830	16548.251819	29.992410
409.425615	16582.271057	29.997428
410.202689	16597.016959	30.002445
410.254024	16630.106241	30.007463
410.831169	16642.937717	30.012480
411.386831	16668.065133	30.017498
411.520116	16692.130779	30.022516
411.747787	16714.049819	30.027533
412.028755	16742.852296	30.032551
412.509907	16771.566798	30.037568
412.747790	16803.739815	30.042586
413.286329	16831.589534	30.047604
414.231419	16863.210367	30.052621
413.932881	16896.089265	30.057639
414.726694	16902.920850	30.062656
414.972323	16935.051820	30.067674
415.641769	16960.022932	30.072692
416.593827	16971.295987	30.077709
417.077295	16992.398537	30.082727
417.615199	16995.587211	30.087744
418.156984	17018.045173	30.092762
418.573122	17033.949914	30.097780
419.161035	17046.104069	30.102797
419.035362	17061.022455	30.107815
419.363385	17069.960683	30.112832
419.706026	17099.647946	30.117850
420.015963	17118.588812	30.122868
420.944423	17133.551607	30.127885
421.166505	17142.430557	30.132903
421.768200	17169.942451	30.137920
422.217995	17185.478850	30.142938
422.562358	17205.295667	30.147956
422.595019	17191.860820	30.152973
422.702030	17221.297530	30.157991
423.319190	17235.907736	30.163008
423.966152	17262.139832	30.168026
423.770852	17289.952852	30.173044
424.405640	17298.489674	30.178061
424.682301	17324.574200	30.183079
425.050855	17346.430967	30.188096
425.756657	17372.985700	30.193114
425.897973	17394.527300	30.198132
426.378171	17413.205060	30.203149
426.725073	17434.395686	30.208167
427.291449	17463.717031	30.213184
427.334931	17482.273333	30.218202
427.827112	17517.326461	30.223220
428.230702	17540.561444	30.228237
428.876308	17566.323540	30.233255
429.207537	17590.978573	30.238272
429.769936	17632.129666	30.243290
430.055924	17664.675661	30.248308
430.509538	17692.779902	30.253325
430.821079	17728.714356	30.258343
431.184778	17749.365751	30.263360
431.599849	17781.190637	30.268378
432.020118	17816.994618	30.273396
432.564062	17840.580830	30.278413
433.090938	17880.499804	30.283431
433.363854	17912.599727	30.288448
433.626473	17936.330929	30.293466
434.228313	17969.851663	30.298484
434.666861	17993.138605	30.303501
435.297449	18037.179578	30.308519
435.796031	18065.909091	30.313536
436.004224	18103.458609	30.318554
436.504789	18130.798099	30.323572
437.219626	18162.539042	30.328589
437.474406	18191.445678	30.333607
437.833433	18221.681725	30.338624
438.480940	18254.216652	30.343642
438.861062	18277.879441	30.348660
439.404618	18308.503843	30.353677
439.788517	18344.781950	30.358695
440.238934	18375.465180	30.363712
440.702681	18405.666259	30.368730
441.064637	18432.200173	30.373748
441.978547	18464.883504	30.378765
442.047219	18489.706906	30.383783
442.466710	18508.878463	30.388800
443.227723	18539.279853	30.393818
443.590547	18562.800381	30.398836
444.220880	18591.965022	30.403853
444.653356	18622.506134	30.408871
444.645780	18638.061208	30.413888
445.615928	18661.285148	30.418906
445.602231	18696.374946	30.423924
446.440033	18721.691706	30.428941
446.781144	18751.318569	30.433959
447.452174	18773.774250	30.438976
447.911933	18792.674481	30.443994
448.160232	18832.000714	30.449012
448.398198	18852.085328	30.454029
449.035618	18874.830648	30.459047
449.505657	18902.359190	30.464064
450.170772	18926.363775	30.469082
450.501353	18940.160698	30.474100
450.874854	18962.953527	30.479117
451.429044	18979.672304	30.484135
451.679170	18999.047605	30.489152
452.120638	19016.788462	30.494170
452.357104	19047.607146	30.499188
452.818377	19068.225805	30.504205
453.212172	19090.775554	30.509223
453.727693	19123.054513	30.514240
454.144402	19145.265922	30.519258
454.305196	19169.519898	30.524276
454.644856	19200.790266	30.529293
455.482000	19230.504898	30.534311
455.472147	19258.765694	30.539328
456.483883	19294.189711	30.544346
456.194261	19328.420172	30.549364
457.216114	19357.777721	30.554381
457.755373	19388.518217	30.559399
458.187410	19407.985643	30.564416
458.773367	19435.452670	30.569434
458.926965	19467.238899	30.574452
459.584339	19489.198432	30.579469
460.114963	19527.351237	30.584487
460.528139	19551.079928	30.589504
461.444990	19578.925254	30.594522
461.828886	19610.581097	30.599540
462.692799	19629.735116	30.604557
462.888220	19636.673477	30.609575
463.466832	19670.276581	30.614592
464.339043	19687.439249	30.619610
464.386906	19712.703383	30.624628
464.869661	19725.175698	30.629645
465.411042	19745.706791	30.634663
465.333175	19772.671125	30.639680
466.036765	19797.081458	30.644698
466.220096	19830.354668	30.649716
467.041655	19857.867746	30.654733
467.418583	19880.307314	30.659751
467.816716	19902.396122	30.664768
467.850373	19932.470676	30.669786
468.413748	19949.801697	30.674804
469.250141	19985.431173	30.679821
470.534531	19994.108147	30.684839
471.648962	19998.963960	30.689856
472.216548	20016.477605	30.694874
472.723143	20028.516784	30.699892
472.717626	20032.656129	30.704909
473.153366	20048.219129	30.709927
473.463559	20067.680912	30.714944
473.773923	20081.652379	30.719962
473.744105	20100.061483	30.724980
474.461738	20128.633588	30.729997
474.615569	20156.547985	30.735015
474.912419	20176.523711	30.740032
475.668427	20195.732995	30.745050
476.058120	20223.579179	30.750068
476.387699	20246.336123	30.755085
476.903326	20272.090461	30.760103
477.173090	20301.610749	30.765120
477.867523	20316.956786	30.770138
478.191216	20351.921221	30.775156
478.607084	20377.211057	30.780173
478.656241	20414.916155	30.785191
479.130493	20453.047956	30.790208
479.789819	20481.970832	30.795226
479.846429	20523.225745	30.800244
480.841043	20555.811579	30.805261
481.785863	20577.695999	30.810279
481.962078	20602.056763	30.815296
482.628354	20629.974193	30.820314
482.870053	20653.408696	30.825332
483.590187	20680.054184	30.830349
484.605017	20702.287981	30.835367
484.647040	20717.356810	30.840384
485.039493	20738.430224	30.845402
485.271006	20771.084670	30.850420
485.738348	20802.470409	30.855437
486.424458	20816.497633	30.860455
486.598396	20839.412178	30.865472
486.837305	20880.456234	30.870490
487.132823	20910.428341	30.875508
487.714953	20928.130088	30.880525
488.117883	20970.323989	30.885543
488.358795	21009.080796	30.890560
488.996790	21042.102054	30.895578
489.455909	21087.806737	30.900596
489.918917	21122.302259	30.905613
490.498042	21156.760810	30.910631
491.153047	21192.256449	30.915648
491.829291	21225.625888	30.920666
492.273516	21272.805491	30.925684
492.895184	21300.307492	30.930701
493.556368	21323.892315	30.935719
493.723587	21358.541712	30.940736
494.353143	21399.033202	30.945754
494.884252	21436.412495	30.950772
495.227439	21477.517384	30.955789
495.678310	21498.544609	30.960807
495.853080	21540.415103	30.965824
496.800793	21572.542367	30.970842
497.364947	21618.528899	30.975860
497.658666	21656.855424	30.980877
498.484365	21683.226786	30.985895
498.883738	21727.002483	30.990912
499.114114	21757.674738	30.995930
499.625595	21795.708574	31.000948
500.181330	21829.363176	31.005965
500.994718	21854.624624	31.010983
501.101017	21896.095827	31.016000
501.746269	21930.141052	31.021018
502.862447	21957.187876	31.026036
503.418946	21992.340137	31.031053
504.502681	22017.332238	31.036071
505.093892	22045.307599	31.041088
505.776915	22051.482181	31.046106
506.585405	22070.704095	31.051124
507.382254	22074.156603	31.056141
507.587858	22081.852478	31.061159
508.193225	22096.126979	31.066176
508.560164	22114.672079	31.071194
509.113550	22139.342509	31.076212
509.410876	22151.605134	31.081229
509.762321	22166.803824	31.086247
509.991971	22186.507719	31.091264
510.271135	22208.055288	31.096282
510.978285	22231.684594	31.101300
511.909909	22249.781750	31.106317
512.401354	22258.848574	31.111335
512.908158	22283.558030	31.116352
513.703365	22294.207799	31.121370
513.957558	22312.479979	31.126388
514.261983	22341.037495	31.131405
514.359917	22361.052728	31.136423
514.865327	22380.404271	31.141440
514.813536	22408.840416	31.146458
515.732155	22437.529928	31.151476
516.114292	22473.354701	31.156493
516.577775	22501.022020	31.161511
516.661988	22535.174589	31.166528
517.147006	22569.997796	31.171546
517.742735	22595.881725	31.176564
517.977880	22617.063786	31.181581
518.316646	22649.925807	31.186599
518.552209	22688.301301	31.191616
519.803193	22723.233011	31.196634
519.933833	22753.821239	31.201652
520.412947	22788.879547	31.206669
520.921660	22825.266584	31.211687
521.187943	22864.882450	31.216704
521.974223	22905.902377	31.221722
522.519284	22946.871477	31.226740
522.692960	22984.972831	31.231757
523.554028	23018.948424	31.236775
524.004578	23064.362031	31.241792
524.611398	23097.296804	31.246810
525.536242	23138.959130	31.251828
525.688500	23178.264788	31.256845
526.497979	23210.270908	31.261863
527.427827	23243.231463	31.266880
527.540608	23270.916540	31.271898
527.937765	23308.086427	31.276916
528.760411	23354.561235	31.281933
529.272090	23387.207988	31.286951
529.910362	23428.106700	31.291968
530.167477	23456.034965	31.296986
530.461691	23502.061582	31.302004
531.190293	23546.042813	31.307021
531.812601	23578.957017	31.312039
532.204397	23618.712824	31.317056
532.770993	23662.176090	31.322074
533.282603	23696.270437	31.327092
533.744616	23741.127725	31.332109
534.113256	23764.956902	31.337127
535.066910	23813.485066	31.342144
535.840317	23841.301901	31.347162
536.656215	23888.461478	31.352180
537.121257	23920.408619	31.357197
537.792515	23943.900218	31.362215
538.170834	23982.300221	31.367232
538.803723	24012.129722	31.372250
539.348228	24041.429573	31.377268
539.681318	24080.140130	31.382285
540.620762	24115.501952	31.387303
540.774844	24141.741021	31.392320
541.420614	24181.028702	31.397338
542.271630	24211.665008	31.402356
542.562779	24243.683974	31.407373
543.246204	24272.501231	31.412391
543.843285	24301.426760	31.417408
544.293535	24339.809935	31.422426
545.134937	24366.517358	31.427444
545.383440	24403.984165	31.432461
545.861641	24425.541071	31.437479
546.341809	24476.653344	31.442496
546.837209	24518.770899	31.447514
547.300534	24541.752107	31.452532
547.817885	24575.606930	31.457549
549.475548	24572.499055	31.462567
550.250645	24591.899244	31.467584
550.971665	24617.709432	31.472602
551.594144	24616.923943	31.477620
551.906827	24645.401332	31.482637
552.671935	24659.469555	31.487655
553.238669	24684.318018	31.492672
553.013835	24705.049397	31.497690
553.326128	24723.580167	31.502708
553.623771	24750.372756	31.507725
553.976593	24775.001855	31.512743
554.703059	24801.967895	31.517760
554.907279	24833.141891	31.522778
555.645099	24861.022567	31.527796
556.240392	24892.312721	31.532813
556.519659	24918.084637	31.537831
556.772684	24951.690548	31.542848
557.307504	24990.586328	31.547866
558.026197	25019.386535	31.552884
558.278355	25073.619763	31.557901
558.613796	25104.691600	31.562919
558.979432	25144.498755	31.567936
560.047138	25188.007406	31.572954
560.718575	25225.896519	31.577972
561.292224	25267.447344	31.582989
562.475804	25299.063646	31.588007
562.486097	25335.981555	31.593024
563.126444	25380.252313	31.598042
563.724347	25403.365234	31.603060
564.134946	25445.580096	31.608077
564.808002	25490.996187	31.613095
565.898634	25532.941057	31.618112
565.962367	25572.037695	31.623130
566.410885	25604.975977	31.628148
566.959287	25644.243774	31.633165
567.729801	25683.255879	31.638183
568.485186	25711.741702	31.643200
568.588071	25759.699227	31.648218
569.575121	25795.454759	31.653236
570.026126	25833.309817	31.658253
570.435306	25858.639290	31.663271
571.074359	25913.282220	31.668288
571.604701	25944.470370	31.673306
571.860487	25990.628770	31.678324
572.829651	26032.991745	31.683341
573.306778	26081.308886	31.688359
573.881711	26124.662447	31.693376
574.393851	26165.649595	31.698394
575.990242	26197.942480	31.703412
576.646615	26227.430354	31.708429
577.368469	26259.499247	31.713447
578.050289	26283.617626	31.718464
578.288131	26312.007912	31.723482
578.609668	26339.184417	31.728500
579.477316	26380.685455	31.733517
580.437428	26406.877847	31.738535
580.620911	26431.061341	31.743552
580.535111	26476.818993	31.748570
581.155193	26513.220689	31.753588
581.487694	26550.684744	31.758605
582.372393	26592.891406	31.763623
582.989681	26635.752831	31.768640
583.067989	26676.201829	31.773658
583.979756	26711.092222	31.778676
584.943740	26736.026747	31.783693
585.628560	26778.245953	31.788711
586.260213	26797.550531	31.793728
587.104795	26828.571049	31.798746
588.776786	26841.273531	31.803764
588.823644	26872.058055	31.808781
589.498664	26896.974563	31.813799
590.253357	26918.857675	31.818816
590.575967	26943.070685	31.823834
590.782291	26966.682453	31.828852
591.319321	26991.904966	31.833869
592.050924	27015.751025	31.838887
593.002018	27028.755457	31.843904
593.457988	27054.647965	31.848922
594.172725	27075.741126	31.853940
594.221639	27094.687974	31.858957
594.607932	27118.227661	31.863975
595.176538	27143.875221	31.868992
595.181619	27170.185680	31.874010
595.693743	27202.731139	31.879028
595.894822	27238.561029	31.884045
596.597346	27278.945659	31.889063
597.161301	27319.061210	31.894080
597.354105	27362.426355	31.899098
598.025137	27404.825984	31.904116
598.604807	27452.599538	31.909133
599.024181	27498.887602	31.914151
599.777598	27545.300740	31.919168
600.313479	27600.356155	31.924186
600.987288	27649.246857	31.929204
601.911960	27701.871889	31.934221
602.242882	27741.278747	31.939239
603.353576	27781.746206	31.944256
603.921199	27826.589849	31.949274
604.412924	27860.043357	31.954292
605.263318	27904.937959	31.959309
605.652794	27945.347368	31.964327
606.422843	27995.051900	31.969344
606.744035	28038.904138	31.974362
607.437138	28091.768484	31.979380
608.248051	28128.472044	31.984397
609.248897	28176.124848	31.989415
610.137632	28204.075149	31.994432
610.340354	28244.811290	31.999450
610.999281	28283.169490	32.004468
611.596318	28321.625885	32.009485
612.416287	28365.160998	32.014503
612.901625	28400.695861	32.019520
613.466387	28437.577351	32.024538
614.457709	28468.684990	32.029556
615.529416	28511.252096	32.034573
615.984359	28546.178844	32.039591
616.640922	28578.994771	32.044608
617.242522	28617.381487	32.049626
617.388949	28645.315219	32.054644
618.252080	28691.909836	32.059661
618.716456	28732.890649	32.064679
619.197514	28761.556213	32.069696
619.297616	28807.416582	32.074714
619.691326	28860.032455	32.079732
620.563444	28900.267490	32.084749
621.212560	28953.166201	32.089767
621.796175	28990.614625	32.094784
622.236931	29047.073008	32.099802
622.879227	29099.878348	32.104820
623.437506	29143.771901	32.109837
623.871756	29199.934639	32.114855
624.965857	29243.346780	32.119872
625.887078	29288.505201	32.124890
626.891419	29319.902873	32.129908
627.690380	29366.932517	32.134925
628.316882	29406.694794	32.139943
629.123728	29436.675904	32.144960
629.618062	29463.324014	32.149978
630.349835	29489.271499	32.154996
631.331881	29524.073616	32.160013
631.778585	29553.219709	32.165031
632.266425	29580.842409	32.170048
633.029048	29619.844358	32.175066
633.146246	29641.406143	32.180084
634.321790	29674.945804	32.185101
634.448639	29702.549013	32.190119
635.545264	29733.730684	32.195136
635.959391	29765.770849	32.200154
636.363328	29790.271671	32.205172
637.175625	29819.298020	32.210189
637.322170	29853.902069	32.215207
638.092011	29866.481431	32.220224
638.932746	29911.666400	32.225242
639.426788	29951.406107	32.230260
640.248206	29972.953428	32.235277
640.483727	30024.187316	32.240295
640.689587	30054.850750	32.245312
641.742589	30096.463265	32.250330
641.969030	30133.217168	32.255348
642.759606	30173.947808	32.260365
643.059139	30231.607167	32.265383
643.886327	30263.552200	32.270400
644.112870	30322.013320	32.275418
645.223939	30356.632415	32.280436
645.850956	30398.059008	32.285453
646.105632	30454.809399	32.290471
647.630892	30476.342499	32.295488
648.636773	30520.352633	32.300506
649.337919	30559.587182	32.305524
650.002723	30603.214423	32.310541
650.660842	30647.329537	32.315559
651.233225	30676.065738	32.320576
651.838897	30722.420594	32.325594
652.518272	30762.695612	32.330612
653.342023	30793.864483	32.335629
653.426711	30827.639060	32.340647
653.687942	30876.886164	32.345664
654.718490	30908.136799	32.350682
655.181146	30966.057279	32.355700
655.938999	31008.766935	32.360717
656.121764	31065.896841	32.365735
656.934727	31117.384908	32.370752
657.644022	31163.149371	32.375770
658.156810	31209.741030	32.380788
658.661237	31257.162208	32.385805
659.541712	31320.132705	32.390823
659.833544	31370.912342	32.395840
661.037570	31429.003174	32.400858
661.038034	31487.325781	32.405876
661.838486	31538.102508	32.410893
662.949536	31584.993814	32.415911
663.514476	31639.859580	32.420928
664.885486	31681.059139	32.425946
665.932921	31714.312314	32.430964
667.278450	31750.660983	32.435981
667.583035	31793.145705	32.440999
668.183147	31812.921419	32.446016
669.184308	31842.098225	32.451034
669.750387	31880.977010	32.456052
670.643970	31908.381627	32.461069
671.212438	31949.795159	32.466087
672.025810	31976.535933	32.471104
672.561479	32004.078576	32.476122
672.695512	32032.404453	32.481140
673.841871	32065.510038	32.486157
673.836708	32099.003553	32.491175
674.376875	32145.485584	32.496192
675.038589	32191.601101	32.501210
675.560358	32246.102207	32.506228
675.913058	32282.170164	32.511245
676.546199	32332.601897	32.516263
677.349469	32377.014191	32.521280
677.746421	32419.100183	32.526298
678.860839	32471.897556	32.531316
679.403921	32505.274768	32.536333
679.779126	32556.063289	32.541351
680.160194	32591.691157	32.546368
681.060781	32631.391691	32.551386
681.887399	32683.709688	32.556404
682.665159	32737.514752	32.561421
683.007895	32775.064442	32.566439
683.408426	32824.193327	32.571456
684.063518	32870.298734	32.576474
684.870633	32923.840508	32.581492
685.499225	32964.525994	32.586509
686.546953	33014.174131	32.591527
687.594983	33050.767375	32.596544
688.652026	33090.400175	32.601562
689.129884	33130.116891	32.606580
689.995778	33161.523002	32.611597
690.777839	33204.644343	32.616615
691.406779	33245.532628	32.621632
692.429194	33285.291309	32.626650
692.938436	33336.585596	32.631668
693.979119	33368.179760	32.636685
694.351189	33404.676546	32.641703
694.953956	33443.799100	32.646720
695.686385	33490.842159	32.651738
695.784974	33537.244301	32.656756
696.562243	33582.263815	32.661773
697.177133	33634.534967	32.666791
697.614415	33687.131041	32.671808
698.502873	33733.638257	32.676826
699.319645	33795.058248	32.681844
700.073812	33841.624543	32.686861
700.864849	33897.384102	32.691879
701.259625	33939.195313	32.696896
702.086749	33982.513555	32.701914
702.686949	34043.576006	32.706932
703.649989	34082.327553	32.711949
704.419884	34135.283923	32.716967
704.811461	34185.226654	32.721984
705.708617	34237.177183	32.727002
706.174930	34281.595402	32.732020
706.947637	34347.424249	32.737037
707.886428	34400.342350	32.742055
708.657324	34448.323609	32.747072
709.265033	34490.545340	32.752090
710.087602	34549.058308	32.757108
710.728263	34592.413157	32.762125
711.556482	34648.232146	32.767143
711.640918	34695.890901	32.772160
712.740075	34743.081997	32.777178
713.619518	34803.034675	32.782196
714.727517	34844.167628	32.787213
715.603025	34894.390771	32.792231
716.187075	34938.855273	32.797248
716.960854	34976.411351	32.802266
717.417319	35035.855181	32.807284
718.080336	35086.111858	32.812301
718.988048	35123.950836	32.817319
719.580070	35183.860823	32.822336
720.110191	35215.891321	32.827354
720.667403	35271.520209	32.832372
721.604561	35321.393346	32.837389
722.162275	35371.300379	32.842407
722.768872	35438.176446	32.847424
724.068068	35478.604342	32.852442
724.425364	35534.024777	32.857460
724.956462	35590.341426	32.862477
725.925568	35642.967079	32.867495
726.153606	35693.925194	32.872512
727.333623	35731.684934	32.877530
727.815703	35784.209716	32.882548
728.589612	35831.055539	32.887565
729.040091	35877.174103	32.892583
729.713461	35933.020591	32.897600
731.009003	35964.952040	32.902618
731.520981	36013.565191	32.907636
732.126601	36062.688677	32.912653
732.694227	36110.882398	32.917671
733.453719	36162.106667	32.922688
734.121338	36213.155672	32.927706
734.779760	36279.166401	32.932724
735.573752	36319.851595	32.937741
736.499528	36369.001827	32.942759
737.275371	36426.661012	32.947776
738.108912	36469.060198	32.952794
738.665893	36532.564613	32.957812
739.473860	36579.710294	32.962829
740.446072	36635.727094	32.967847
741.289346	36685.333518	32.972864
741.774115	36739.428370	32.977882
742.286994	36801.340703	32.982900
742.957739	36859.093297	32.987917
743.817621	36910.316386	32.992935
744.235805	36974.254729	32.997952
745.395257	37027.151373	33.002970
746.058494	37089.199214	33.007988
746.979922	37144.997623	33.013005
747.546352	37197.822601	33.018023
747.959038	37254.724859	33.023040
749.025365	37310.836279	33.028058
749.490523	37373.680899	33.033076
750.626237	37428.991414	33.038093
751.823086	37491.836300	33.043111
752.318925	37556.940438	33.048128
754.080748	37597.825197	33.053146
754.581212	37657.560380	33.058164
755.306930	37706.883955	33.063181
756.334564	37745.910387	33.068199
756.748531	37797.710893	33.073216
758.105568	37844.116259	33.078234
758.265684	37901.204992	33.083252
758.810688	37953.111944	33.088269
759.903906	37988.657021	33.093287
760.297205	38050.863495	33.098304
761.293508	38103.611144	33.103322
761.771425	38145.727551	33.108340
762.311132	38207.816835	33.113357
763.070864	38245.475730	33.118375
763.847294	38304.758724	33.123392
764.907980	38366.312068	33.128410
765.722352	38418.924400	33.133428
766.463019	38461.645533	33.138445
766.967383	38522.242528	33.143463
767.876350	38565.342382	33.148480
769.727332	38610.863090	33.153498
770.385877	38658.397064	33.158516
770.911364	38705.566111	33.163533
771.981045	38744.050301	33.168551
772.047516	38790.310813	33.173568
772.801398	38837.596364	33.178586
773.691971	38884.443374	33.183604
774.549142	38934.489186	33.188621
774.998821	38984.579576	33.193639
775.932844	39048.993969	33.198656
776.495742	39093.584256	33.203674
777.271313	39149.107042	33.208692
777.464955	39195.487749	33.213709
778.389054	39255.275252	33.218727
779.443602	39302.616201	33.223744
780.160523	39349.092849	33.228762
780.955745	39400.591232	33.233780
781.553024	39446.941265	33.238797
782.253847	39485.654946	33.243815
782.677555	39549.467288	33.248832
783.549903	39600.618973	33.253850
784.747115	39658.423622	33.258868
785.543222	39708.189830	33.263885
786.403151	39754.113872	33.268903
786.620923	39803.407491	33.273920
787.712342	39862.639411	33.278938
788.676241	39923.737966	33.283956
789.125276	39976.904245	33.288973
789.840986	40026.734294	33.293991
790.934789	40092.840752	33.299008
791.937610	40139.748900	33.304026
792.873209	40193.010717	33.309044
793.638002	40240.133212	33.314061
794.994850	40291.736013	33.319079
795.644176	40346.275981	33.324096
796.247842	40394.132200	33.329114
797.441830	40446.076930	33.334132
797.682762	40487.336757	33.339149
798.583718	40540.301258	33.344167
799.451827	40596.205452	33.349184
800.075894	40645.412438	33.354202
800.245063	40711.127151	33.359220
801.189974	40769.062577	33.364237
802.895136	40822.275709	33.369255
803.652246	40882.264452	33.374272
804.375184	40927.636789	33.379290
804.866035	40991.822376	33.384308
805.584810	41038.650195	33.389325
806.504602	41094.427460	33.394343
807.199326	41160.997727	33.399360
808.223177	41210.725602	33.404378
808.593053	41271.408138	33.409396
809.478395	41348.827351	33.414413
810.516211	41398.591427	33.419431
810.937869	41467.924664	33.424448
811.648180	41526.569019	33.429466
812.475208	41594.252099	33.434484
813.148845	41662.629669	33.439501
814.389309	41722.431635	33.444519
814.899908	41792.314940	33.449536
815.457072	41860.641688	33.454554
816.439710	41930.116747	33.459572
817.441755	41996.040874	33.464589
818.774762	42058.688097	33.469607
819.772184	42108.086921	33.474624
821.038005	42163.692880	33.479642
822.675175	42189.009043	33.484660
823.623860	42238.327202	33.489677
824.653117	42275.268071	33.494695
825.276454	42311.911681	33.499712
826.042754	42355.850839	33.504730
826.358277	42401.492048	33.509748
826.875226	42442.832767	33.514765
828.155076	42484.661986	33.519783
828.528286	42527.581140	33.524800
829.445629	42580.307692	33.529818
830.035070	42623.294570	33.534836
830.361188	42682.583708	33.539853
831.410918	42734.973781	33.544871
832.293277	42797.073427	33.549888
832.904494	42845.541024	33.554906
833.815310	42899.755710	33.559924
833.933645	42949.830890	33.564941
835.047460	42999.637372	33.569959
835.658502	43060.508683	33.574976
836.262715	43116.555268	33.579994
837.426210	43173.659758	33.585012
837.704722	43231.876209	33.590029
838.907120	43293.313909	33.595047
839.399534	43365.304949	33.600064
839.845262	43429.631186	33.605082
840.919134	43491.886404	33.610100
841.671549	43574.040010	33.615117
842.657836	43639.067023	33.620135
843.291023	43700.847468	33.625152
844.268304	43766.274740	33.630170
845.398262	43836.371723	33.635188
846.685669	43891.713031	33.640205
848.519946	43947.639821	33.645223
848.902360	44002.761746	33.650240
849.775359	44052.785198	33.655258
850.796363	44106.081182	33.660276
851.655559	44165.240711	33.665293
852.788222	44216.685250	33.670311
853.067780	44282.317538	33.675328
853.881335	44327.859895	33.680346
855.373227	44382.411561	33.685364
855.855068	44439.948023	33.690381
856.850130	44501.762923	33.695399
857.679971	44555.614750	33.700416
858.235727	44617.555285	33.705434
859.437074	44667.162137	33.710452
860.377121	44724.229506	33.715469
861.264175	44771.621010	33.720487
862.501797	44826.548597	33.725504
863.265403	44874.883056	33.730522
864.286539	44921.178676	33.735540
864.623499	44975.247405	33.740557
865.355248	45030.981677	33.745575
866.180675	45094.165639	33.750592
867.081603	45158.154025	33.755610
867.856442	45218.891899	33.760628
868.602350	45276.003554	33.765645
869.396529	45341.508247	33.770663
870.056286	45414.403413	33.775680
870.930823	45485.196895	33.780698
871.792331	45540.342931	33.785716
872.688066	45612.189901	33.790733
873.805051	45679.327966	33.795751
874.565603	45748.912840	33.800768
875.122522	45827.119989	33.805786
876.129349	45887.538908	33.810804
876.756424	45959.188434	33.815821
877.574903	46028.195837	33.820839
878.559275	46104.306830	33.825856
879.603826	46178.763994	33.830874
880.763053	46242.348373	33.835892
881.416211	46316.050882	33.840909
882.245374	46385.665005	33.845927
883.708179	46456.686278	33.850944
884.215987	46521.783532	33.855962
884.954330	46585.984757	33.860980
885.526323	46664.641616	33.865997
886.806870	46741.550019	33.871015
887.723874	46803.687081	33.876032
888.447567	46886.464644	33.881050
889.452366	46942.477466	33.886068
889.963450	47015.249145	33.891085
891.016052	47083.192189	33.896103
891.937750	47151.035619	33.901120
892.896059	47222.650257	33.906138
893.629844	47277.542090	33.911156
894.337099	47342.060288	33.916173
895.390322	47411.389655	33.921191
896.314727	47470.421243	33.926208
897.186119	47535.275036	33.931226
898.348239	47586.836613	33.936244
899.126493	47644.872882	33.941261
900.807441	47693.190812	33.946279
902.481009	47734.791484	33.951296
903.073524	47784.556948	33.956314
904.135833	47831.940290	33.961332
904.985928	47890.858017	33.966349
905.889508	47933.996013	33.971367
906.660805	47994.824177	33.976384
907.156982	48053.632935	33.981402
908.176905	48101.529548	33.986420
908.956488	48159.997125	33.991437
909.722940	48218.928726	33.996455
910.483251	48281.113220	34.001472
911.284070	48348.744980	34.006490
911.989255	48409.363120	34.011508
912.886852	48483.028318	34.016525
913.475282	48549.630885	34.021543
914.624548	48614.621654	34.026560
915.245105	48703.008230	34.031578
916.657047	48765.712616	34.036596
917.365666	48841.869426	34.041613
918.279586	48901.007595	34.046631
919.738739	48960.953098	34.051648
920.374939	49037.874703	34.056666
921.444899	49109.718330	34.061684
922.304635	49178.760555	34.066701
923.293960	49248.010577	34.071719
924.324062	49316.153613	34.076736
924.874585	49393.260573	34.081754
925.846997	49459.369479	34.086772
927.031413	49527.337281	34.091789
927.830660	49605.564039	34.096807
928.830224	49674.181078	34.101824
929.631652	49748.491685	34.106842
930.932485	49817.252062	34.111860
931.699418	49884.431786	34.116877
932.329268	49957.789114	34.121895
934.025269	50027.766643	34.126912
934.518532	50099.861323	34.131930
935.703301	50159.485722	34.136948
936.286799	50238.678285	34.141965
937.380490	50312.280891	34.146983
938.622451	50372.415753	34.152000
939.046600	50448.546263	34.157018
940.047522	50515.855913	34.162036
940.981837	50592.495901	34.167053
941.847973	50663.540954	34.172071
942.830476	50727.709528	34.177088
943.215277	50821.468394	34.182106
944.460138	50895.669393	34.187124
945.587699	50962.713877	34.192141
946.444498	51035.697645	34.197159
947.842708	51110.837200	34.202176
948.602678	51189.929634	34.207194
949.932828	51251.078076	34.212212
950.635220	51330.477335	34.217229
951.525758	51407.443207	34.222247
952.679320	51475.484845	34.227264
953.628872	51549.740243	34.232282
954.599821	51607.883115	34.237300
955.400313	51662.344833	34.242317
956.393411	51720.092243	34.247335
957.480987	51770.447350	34.252352
957.873551	51841.860804	34.257370
958.901490	51893.193555	34.262388
959.968870	51962.458579	34.267405
961.094499	52030.968101	34.272423
962.101736	52086.740056	34.277440
963.190048	52157.628566	34.282458
964.048118	52205.856341	34.287476
965.278531	52263.188513	34.292493
966.230378	52325.664188	34.297511
966.651685	52387.817651	34.302528
967.670232	52459.749335	34.307546
968.622204	52535.766578	34.312564
970.012869	52603.084909	34.317581
970.518036	52670.066701	34.322599
971.454870	52740.676840	34.327616
972.364953	52810.158705	34.332634
973.294741	52881.112061	34.337652
973.931215	52954.408251	34.342669
975.093086	53030.198274	34.347687
975.907624	53106.650074	34.352704
977.428168	53184.953837	34.357722
978.173507	53265.150315	34.362740
979.763465	53341.918800	34.367757
980.933961	53407.413347	34.372775
982.348921	53463.321294	34.377792
982.929941	53543.462043	34.382810
984.143870	53604.742346	34.387828
984.930419	53660.229698	34.392845
985.851091	53730.604884	34.397863
986.826963	53799.883284	34.402880
987.523559	53879.532593	34.407898
988.895649	53949.420523	34.412916
989.422616	54024.540582	34.417933
990.167346	54094.431679	34.422951
991.327718	54168.251277	34.427968
992.336810	54252.902985	34.432986
992.984748	54324.917078	34.438004
994.962151	54385.669255	34.443021
996.116169	54459.345210	34.448039
998.050587	54514.472386	34.453056
998.908561	54575.253758	34.458074
999.964356	54632.846739	34.463092
1000.862531	54695.432018	34.468109
1001.109437	54759.707218	34.473127
1002.262388	54817.519670	34.478144
1003.058873	54889.860419	34.483162
1004.157718	54956.933515	34.488180
1005.181764	55019.987337	34.493197
1006.284728	55079.276371	34.498215
1007.427320	55139.363079	34.503232
1008.736709	55206.695213	34.508250
1009.614469	55249.085153	34.513268
1010.906331	55321.375426	34.518285
1011.571414	55392.364915	34.523303
1012.616066	55453.878895	34.528320
1013.624451	55527.258106	34.533338
1014.235077	55601.743650	34.538356
1015.224743	55643.724516	34.543373
1016.074231	55718.185901	34.548391
1017.118417	55794.022134	34.553408
1017.944201	55861.254211	34.558426
1018.659268	55929.155550	34.563444
1020.101645	56004.373564	34.568461
1020.700026	56091.342416	34.573479
1022.099314	56154.644619	34.578496
1022.540380	56215.836843	34.583514
1023.132072	56292.099501	34.588532
1024.287918	56356.433728	34.593549
1024.802677	56434.221358	34.598567
1025.874484	56511.720014	34.603584
1026.687154	56599.663622	34.608602
1027.928740	56680.636164	34.613620
1028.873693	56754.940372	34.618637
1030.311215	56833.566619	34.623655
1031.176014	56906.807889	34.628672
1031.977730	56989.590361	34.633690
1032.854849	57081.677399	34.638708
1034.092499	57159.842184	34.643725
1034.895456	57255.662792	34.648743
1036.379844	57339.637627	34.653760
1036.766836	57423.397513	34.658778
1038.010436	57515.536763	34.663796
1039.201176	57597.203848	34.668813
1040.339262	57690.366497	34.673831
1041.392482	57777.669406	34.678848
1042.914368	57862.070606	34.683866
1043.807944	57950.183789	34.688884
1044.844268	58048.933229	34.693901
1045.978937	58135.224764	34.698919
1047.337960	58210.557633	34.703936
1048.230652	58303.495032	34.708954
1049.188627	58381.226313	34.713972
1050.319672	58463.196772	34.718989
1051.137958	58559.918932	34.724007
1052.434622	58644.687053	34.729024
1053.475265	58730.590283	34.734042
1054.096771	58826.192216	34.739060
1055.240514	58910.371133	34.744077
1056.665668	59010.253888	34.749095
1057.734353	59100.812450	34.754112
1059.117660	59173.372291	34.759130
1060.217527	59262.717696	34.764148
1061.964918	59325.999404	34.769165
1062.843783	59411.860611	34.774183
1063.987651	59496.756772	34.779200
1065.155312	59567.655068	34.784218
1066.356182	59644.466473	34.789236
1067.848007	59715.776797	34.794253
1068.991839	59780.571452	34.799271
1070.327717	59849.140440	34.804288
1071.373529	59918.444695	34.809306
1072.000887	59986.105298	34.814324
1073.332844	60049.643449	34.819341
1074.178886	60118.605924	34.824359
1075.290870	60203.693075	34.829376
1076.535277	60272.764878	34.834394
1077.330465	60341.438405	34.839412
1078.284893	60422.683418	34.844429
1079.127814	60499.654515	34.849447
1080.092943	60567.694574	34.854464
1081.007258	60665.910315	34.859482
1081.638646	60747.959933	34.864500
1082.943923	60823.663753	34.869517
1084.060696	60908.746285	34.874535
1085.153205	60997.599143	34.879552
1086.663555	61066.157054	34.884570
1087.190097	61153.016050	34.889588
1088.238475	61228.564884	34.894605
1089.026296	61319.821059	34.899623
1090.273285	61415.335781	34.904640
1091.224190	61505.478509	34.909658
1091.925922	61598.021440	34.914676
1093.352559	61689.458069	34.919693
1094.167334	61766.886955	34.924711
1095.147235	61849.879821	34.929728
1096.481975	61927.114333	34.934746
1097.114773	62016.352605	34.939764
1098.279727	62101.678641	34.944781
1099.630124	62195.002730	34.949799
1100.403284	62281.232282	34.954816
1101.582936	62369.924607	34.959834
1102.619909	62449.068180	34.964852
1104.323722	62533.533215	34.969869
1105.632961	62627.454056	34.974887
1106.587072	62709.618233	34.979904
1108.103050	62785.339604	34.984922
1108.891673	62874.727635	34.989940
1110.368040	62940.580351	34.994957
1111.283086	63031.601487	34.999975
1112.256630	63111.124210	35.004992
1113.398301	63195.837266	35.010010
1114.497561	63297.788630	35.015028
1115.564168	63368.612346	35.020045
1117.118692	63449.191528	35.025063
1118.914800	63513.799539	35.030080
1120.389078	63583.123391	35.035098
1121.388335	63662.118443	35.040116
1122.607129	63730.051775	35.045133
1123.672479	63805.631166	35.050151
1124.707597	63889.584513	35.055168
1126.040290	63963.571777	35.060186
1126.688319	64044.509229	35.065204
1127.821438	64108.607915	35.070221
1128.936786	64190.175798	35.075239
1129.574195	64279.453135	35.080256
1130.991630	64353.681592	35.085274
1132.003685	64442.502361	35.090292
1133.359791	64520.577275	35.095309
1134.689282	64600.657094	35.100327
1135.512005	64685.798373	35.105344
1137.260027	64753.474851	35.110362
1138.254939	64843.489899	35.115380
1139.017450	64915.163021	35.120397
1140.408508	65001.805948	35.125415
1141.246902	65094.410256	35.130432
1142.846692	65167.549153	35.135450
1143.562682	65247.036463	35.140468
1144.643945	65330.208752	35.145485
1146.018505	65411.170474	35.150503
1146.644671	65507.550935	35.155520
1147.937190	65595.008947	35.160538
1149.040776	65686.124352	35.165556
1150.385314	65782.406705	35.170573
1151.054351	65873.603088	35.175591
1151.961584	65969.017223	35.180608
1153.236793	66051.978101	35.185626
1153.920905	66163.002259	35.190644
1155.317441	66257.853821	35.195661
1156.632175	66362.582477	35.200679
1157.528521	66459.582953	35.205696
1158.991062	66555.121788	35.210714
1160.230003	66643.959317	35.215732
1161.701228	66736.813028	35.220749
1163.294481	66821.638971	35.225767
1164.553756	66909.486580	35.230784
1165.633909	66982.629311	35.235802
1166.590108	67080.167337	35.240820
1168.106050	67165.082437	35.245837
1168.978546	67254.764234	35.250855
1170.281421	67345.500020	35.255872
1171.418502	67424.149846	35.260890
1172.410559	67499.561775	35.265908
1173.647668	67585.344770	35.270925
1174.876278	67653.686036	35.275943
1175.746600	67727.965252	35.280960
1176.318650	67804.861723	35.285978
1177.165301	67899.361789	35.290996
1178.482773	67985.994715	35.296013
1179.835009	68078.061388	35.301031
1180.737622	68170.932849	35.306048
1181.458723	68263.744257	35.311066
1182.968883	68366.487908	35.316084
1183.994663	68461.145781	35.321101
1185.371795	68555.616346	35.326119
1186.637158	68647.084405	35.331136
1188.093856	68743.550445	35.336154
1189.185436	68849.235813	35.341172
1190.318305	68933.950475	35.346189
1192.067898	69040.389002	35.351207
1192.904464	69140.986454	35.356224
1194.375509	69230.822604	35.361242
1195.677627	69329.879324	35.366260
1197.069339	69413.016610	35.371277
1198.491930	69503.336147	35.376295
1199.906853	69593.935801	35.381312
1201.160496	69675.005864	35.386330
1202.092169	69773.710365	35.391348
1203.413181	69854.897145	35.396365
1204.650659	69948.096475	35.401383
1205.732976	70032.436350	35.406400
1206.864564	70123.354239	35.411418
1208.226598	70221.638858	35.416436
1209.326659	70322.225212	35.421453
1210.913151	70414.035802	35.426471
1211.930092	70496.949953	35.431488
1213.366834	70588.049929	35.436506
1214.617725	70674.366635	35.441524
1215.925905	70763.296275	35.446541
1217.146184	70841.082385	35.451559
1218.309587	70937.431281	35.456576
1219.576661	71030.218281	35.461594
1220.672570	71121.145208	35.466612
1221.928173	71218.379985	35.471629
1223.201897	71308.254038	35.476647
1224.270897	71393.157644	35.481664
1225.451907	71491.861507	35.486682
1226.748641	71587.457479	35.491700
1227.677170	71681.502656	35.496717
1228.690434	71776.256889	35.501735
1229.889387	71872.299731	35.506752
1231.197167	71980.763158	35.511770
1232.143853	72084.635110	35.516788
1232.967382	72192.275555	35.521805
1234.353713	72301.361339	35.526823
1235.778432	72410.808895	35.531840
1236.835975	72516.185136	35.536858
1238.190421	72617.576626	35.541876
1239.468464	72729.619423	35.546893
1240.623214	72839.668062	35.551911
1242.352327	72938.000727	35.556928
1243.829810	73039.412683	35.561946
1244.732989	73150.717676	35.566964
1246.083388	73243.512182	35.571981
1247.576332	73334.739598	35.576999
1248.895287	73443.498608	35.582016
1250.141039	73534.093896	35.587034
1251.576864	73634.058034	35.592052
1252.605961	73727.993517	35.597069
1254.015512	73820.223529	35.602087
1255.136510	73906.178407	35.607104
1256.155479	73997.139890	35.612122
1257.400598	74082.632703	35.617140
1258.385043	74175.449428	35.622157
1259.745355	74253.781126	35.627175
1260.629194	74350.920640	35.632192
1262.133965	74441.554698	35.637210
1262.868077	74543.442756	35.642228
1264.125614	74648.137673	35.647245
1265.388632	74749.209537	35.652263
1266.476514	74859.732932	35.657280
1267.956017	74964.369204	35.662298
1268.862888	75072.831668	35.667316
1269.907245	75181.247837	35.672333
1271.305898	75291.648638	35.677351
1272.618392	75406.332008	35.682368
1273.699192	75522.483283	35.687386
1275.190044	75632.111122	35.692404
1276.863251	75745.485770	35.697421
1279.197997	75836.337362	35.702439
1280.465214	75941.707164	35.707456
1281.878966	76042.317083	35.712474
1283.027222	76144.324084	35.717492
1284.109038	76240.894927	35.722509
1285.746331	76341.357161	35.727527
1286.585760	76443.958051	35.732544
1288.449672	76543.283709	35.737562
1289.355528	76647.078423	35.742580
1290.314900	76749.003096	35.747597
1291.854772	76848.329639	35.752615
1292.808071	76971.904778	35.757632
1294.231256	77078.825500	35.762650
1295.676996	77186.769207	35.767668
1296.743182	77303.969143	35.772685
1298.463458	77401.584829	35.777703
1299.876278	77515.096087	35.782720
1300.837038	77615.643002	35.787738
1302.623969	77722.243607	35.792756
1304.052740	77831.066590	35.797773
1305.199190	77925.745838	35.802791
1306.563761	78043.624579	35.807808
1307.861068	78151.240500	35.812826
1309.025008	78242.016359	35.817844
1310.474651	78362.632208	35.822861
1312.126673	78462.529908	35.827879
1312.961855	78566.102223	35.832896
1314.682677	78678.430222	35.837914
1315.812793	78780.044523	35.842932
1316.728233	78881.743286	35.847949
1318.501081	78980.597924	35.852967
1320.264326	79089.639874	35.857984
1321.383928	79198.123674	35.863002
1322.894958	79289.254359	35.868020
1323.940406	79390.909427	35.873037
1325.710624	79488.258729	35.878055
1328.332679	79559.961004	35.883072
1330.677169	79624.358803	35.888090
1332.047761	79686.589957	35.893108
1333.196238	79759.877674	35.898125
1334.454605	79830.209311	35.903143
1335.519474	79907.805166	35.908160
1336.371446	79987.917479	35.913178
1337.414193	80061.501166	35.918196
1338.542118	80158.712092	35.923213
1339.787323	80233.455606	35.928231
1340.835183	80320.557022	35.933248
1342.150252	80396.126257	35.938266
1343.768365	80473.852955	35.943284
1344.370400	80553.017609	35.948301
1345.815212	80636.840264	35.953319
1346.934336	80719.421603	35.958336
1347.854486	80802.515589	35.963354
1349.230018	80888.731608	35.968372
1349.856532	80978.890621	35.973389
1351.088785	81084.855731	35.978407
1352.482228	81180.559243	35.983424
1353.585960	81284.518002	35.988442
1354.712238	81390.817502	35.993460
1355.322807	81500.403080	35.998477
1356.937297	81621.805632	36.003495
1358.106168	81742.973997	36.008512
1359.298053	81863.391787	36.013530
1360.980042	81983.074978	36.018548
1362.691080	82111.078253	36.023565
1364.145844	82219.242907	36.028583
1365.528242	82338.518124	36.033600
1367.210781	82464.538257	36.038618
1368.672425	82569.358298	36.043636
1370.195052	82679.845447	36.048653
1371.568727	82792.079355	36.053671
1372.741571	82911.947097	36.058688
1374.303370	83037.279044	36.063706
1375.697149	83150.752930	36.068724
1377.531803	83267.617661	36.073741
1378.654435	83379.766267	36.078759
1380.160914	83492.957900	36.083776
1381.301261	83609.374605	36.088794
1382.676422	83723.968684	36.093812
1383.715796	83852.223750	36.098829
1385.284019	83967.472973	36.103847
1387.029309	84083.455346	36.108864
1388.664033	84218.816374	36.113882
1390.385348	84311.666536	36.118900
1391.876720	84429.387729	36.123917
1393.090822	84537.700039	36.128935
1394.516431	84659.791218	36.133952
1395.954293	84774.215026	36.138970
1397.607218	84885.400030	36.143988
1399.054932	84987.925003	36.149005
1401.110770	85088.011520	36.154023
1402.302603	85185.356499	36.159040
1403.490937	85300.061994	36.164058
1404.855799	85406.681506	36.169076
1406.488857	85526.273168	36.174093
1407.603015	85631.994854	36.179111
1409.343684	85736.060821	36.184128
1411.088928	85843.078913	36.189146
1412.348474	85937.932275	36.194164
1413.546681	86053.716309	36.199181
1414.783693	86152.273990	36.204199
1416.592873	86257.864440	36.209216
1417.673276	86370.842288	36.214234
1419.012313	86468.941654	36.219252
1420.412745	86585.279235	36.224269
1421.505719	86696.013475	36.229287
1423.102856	86805.795301	36.234304
1424.247022	86921.122341	36.239322
1425.464452	87031.813142	36.244340
1426.794867	87147.695002	36.249357
1428.278040	87265.124889	36.254375
1429.701289	87382.108377	36.259392
1431.141222	87498.088630	36.264410
1432.763166	87623.101696	36.269428
1434.464866	87742.590414	36.274445
1435.597425	87849.787282	36.279463
1436.762239	87963.645221	36.284480
1438.126071	88074.950800	36.289498
1439.253754	88181.161183	36.294516
1440.339284	88302.686981	36.299533
1441.315503	88411.684392	36.304551
1443.317315	88515.478852	36.309568
1444.028165	88651.080381	36.314586
1445.975330	88768.482078	36.319604
1447.338808	88894.427870	36.324621
1448.523961	89015.624276	36.329639
1450.014143	89135.759865	36.334656
1451.381880	89261.440423	36.339674
1452.573703	89390.481905	36.344692
1454.105758	89529.153240	36.349709
1455.330847	89670.192189	36.354727
1457.032826	89807.203534	36.359744
1458.377346	89948.795509	36.364762
1460.539692	90080.806552	36.369780
1462.071757	90228.213071	36.374797
1463.235789	90355.602842	36.379815
1465.317511	90486.360882	36.384832
1466.269598	90623.175853	36.389850
1468.159421	90755.637849	36.394868
1469.449519	90897.103372	36.399885
1471.093120	91035.092631	36.404903
1472.185785	91155.222180	36.409920
1473.863583	91296.033569	36.414938
1476.276597	91413.183067	36.419956
1478.111110	91537.406411	36.424973
1479.629034	91665.925334	36.429991
1481.566226	91781.984318	36.435008
1482.714413	91898.597474	36.440026
1484.875158	92015.801254	36.445044
1486.006149	92135.789326	36.450061
1487.060870	92256.917751	36.455079
1488.999274	92366.819105	36.460096
1491.084789	92476.305056	36.465114
1492.774382	92589.541273	36.470132
1494.508134	92692.137188	36.475149
1495.722767	92798.096937	36.480167
1497.187058	92904.740644	36.485184
1498.565443	93027.482125	36.490202
1500.081996	93132.318705	36.495220
1502.199674	93243.285341	36.500237
1503.313889	93366.398843	36.505255
1504.717465	93460.417255	36.510272
1505.961964	93579.683561	36.515290
1507.494685	93690.261224	36.520308
1509.159885	93798.638584	36.525325
1510.229397	93912.445193	36.530343
1511.845298	94026.712205	36.535360
1512.927373	94149.935253	36.540378
1514.092489	94279.660865	36.545396
1515.426361	94401.933124	36.550413
1516.626554	94529.702356	36.555431
1518.628096	94664.483555	36.560448
1520.048498	94799.279743	36.565466
1521.497149	94915.997065	36.570484
1523.229983	95048.552874	36.575501
1524.425363	95177.415616	36.580519
1526.322620	95311.239853	36.585536
1527.856899	95439.303079	36.590554
1529.174574	95569.137106	36.595572
1530.652656	95701.773382	36.600589
1532.190497	95830.978476	36.605607
1533.653153	95957.838113	36.610624
1535.023005	96092.128070	36.615642
1536.817386	96217.466735	36.620660
1538.160974	96346.945040	36.625677
1539.838989	96474.660571	36.630695
1541.330605	96587.726789	36.635712
1542.541507	96711.231490	36.640730
1544.019899	96822.310468	36.645748
1545.678763	96942.691411	36.650765
1546.602798	97077.308500	36.655783
1548.474046	97190.660059	36.660800
1550.004871	97325.982372	36.665818
1551.681909	97444.207429	36.670836
1553.378253	97573.040090	36.675853
1554.630570	97697.581678	36.680871
1556.406519	97820.014013	36.685888
1558.553515	97940.449554	36.690906
1560.325168	98058.598800	36.695924
1562.012668	98185.419748	36.700941
1563.329794	98300.420764	36.705959
1564.879480	98421.559583	36.710976
1566.709899	98553.050158	36.715994
1567.910953	98674.992136	36.721012
1569.781151	98799.048893	36.726029
1570.869969	98932.317133	36.731047
1572.604467	99057.245371	36.736064
1574.389376	99193.157269	36.741082
1575.588386	99319.716480	36.746100
1577.184327	99456.432211	36.751117
1578.535761	99595.379741	36.756135
1580.380158	99722.473952	36.761152
1582.225186	99855.679040	36.766170
1584.122197	99979.901003	36.771188
1585.889775	100109.252595	36.776205
1587.229008	100240.788515	36.781223
1589.199906	100375.294619	36.786240
1590.500795	100504.580980	36.791258
1591.847008	100644.231111	36.796276
1593.866697	100762.820799	36.801293
1595.239051	100908.933622	36.806311
1597.376792	101040.094953	36.811328
1598.255324	101182.926253	36.816346
1600.007977	101321.235574	36.821364
1601.736107	101451.650932	36.826381
1603.391965	101594.996951	36.831399
1604.618178	101718.873577	36.836416
1606.068137	101868.338311	36.841434
1607.746660	102008.728616	36.846452
1609.651955	102149.680104	36.851469
1610.909239	102303.867757	36.856487
1612.264375	102441.064605	36.861504
1613.792682	102589.341344	36.866522
1614.948119	102739.654625	36.871540
1616.879771	102888.034751	36.876557
1618.535405	103038.563147	36.881575
1620.327578	103193.597247	36.886592
1622.004054	103347.394892	36.891610
1623.053759	103503.801194	36.896628
1625.170767	103652.865913	36.901645
1626.769392	103815.248715	36.906663
1628.865532	103972.026865	36.911680
1630.189053	104115.296102	36.916698
1631.724505	104260.789837	36.921716
1633.561431	104407.720738	36.926733
1634.946258	104563.128925	36.931751
1636.719416	104713.760728	36.936768
1638.280357	104855.436643	36.941786
1640.138361	105006.956786	36.946804
1642.130507	105148.820414	36.951821
1643.584075	105306.744541	36.956839
1646.350804	105426.908406	36.961856
1648.396864	105538.778349	36.966874
1650.263421	105647.050248	36.971892
1652.362181	105746.854425	36.976909
1653.677482	105851.193347	36.981927
1655.057228	105958.768558	36.986944
1656.471388	106068.773259	36.991962
1657.700395	106182.991455	36.996980
1659.695724	106296.393375	37.001997
1660.436200	106416.292863	37.007015
1661.758688	106542.632331	37.012032
1663.125433	106663.373529	37.017050
1664.161781	106798.165279	37.022068
1665.908792	106933.835996	37.027085
1667.834349	107082.032751	37.032103
1669.625610	107230.301771	37.037120
1670.958721	107374.813321	37.042138
1672.420785	107511.862103	37.047156
1674.583781	107655.510218	37.052173
1676.006197	107810.597759	37.057191
1677.598953	107964.835260	37.062208
1679.430176	108121.876763	37.067226
1681.224124	108274.055459	37.072244
1683.003155	108422.420292	37.077261
1684.845932	108575.023855	37.082279
1686.792439	108715.806220	37.087296
1688.546864	108869.439287	37.092314
1690.415280	109015.345366	37.097332
1692.141384	109162.212590	37.102349
1693.913739	109305.991775	37.107367
1695.765160	109452.308122	37.112384
1698.186840	109592.107054	37.117402
1699.680337	109743.565415	37.122420
1701.649347	109871.591808	37.127437
1702.907197	110012.473921	37.132455
1705.157796	110144.388647	37.137472
1707.281265	110276.260249	37.142490
1708.703454	110416.306806	37.147508
1710.541824	110543.227349	37.152525
1711.758744	110690.509956	37.157543
1713.298682	110832.213787	37.162560
1715.110970	110973.381219	37.167578
1716.540073	111118.286507	37.172596
1718.525568	111264.640266	37.177613
1719.853329	111422.688044	37.182631
1721.717535	111567.679631	37.187648
1723.643009	111715.414219	37.192666
1725.308086	111859.245901	37.197684
1727.258396	112004.022957	37.202701
1728.453708	112149.818526	37.207719
1730.030531	112305.257027	37.212736
1732.121460	112463.875472	37.217754
1733.587693	112611.216010	37.222772
1735.540556	112771.784986	37.227789
1737.315019	112930.277200	37.232807
1739.020452	113067.056153	37.237824
1740.676886	113218.503994	37.242842
1742.490896	113372.718064	37.247860
1743.844032	113524.404630	37.252877
1745.549914	113683.722505	37.257895
1747.187961	113842.683846	37.262912
1748.996631	114003.382207	37.267930
1750.830555	114171.915219	37.272948
1752.593311	114312.203050	37.277965
1754.330400	114475.780928	37.282983
1756.142722	114626.284548	37.288000
1758.163033	114782.856868	37.293018
1759.498014	114936.086773	37.298036
1761.642275	115097.524067	37.303053
1763.679491	115262.301683	37.308071
1764.759084	115393.771150	37.313088
1766.156789	115542.161578	37.318106
1767.506922	115684.636970	37.323124
1769.609480	115825.118691	37.328141
1771.374488	115981.545610	37.333159
1772.683102	116132.831380	37.338176
1774.433773	116282.133778	37.343194
1775.999402	116447.319853	37.348212
1778.155925	116601.443489	37.353229
1780.026756	116759.353871	37.358247
1781.204320	116927.050396	37.363264
1783.365965	117090.485014	37.368282
1785.152645	117252.202989	37.373300
1787.134932	117402.044598	37.378317
1789.155960	117566.898397	37.383335
1791.199180	117728.882915	37.388352
1793.117022	117884.177856	37.393370
1795.016704	118052.502697	37.398388
1797.158667	118186.911572	37.403405
1798.954040	118353.528966	37.408423
1800.457394	118514.915950	37.413440
1802.487999	118672.987096	37.418458
1804.264462	118842.958211	37.423476
1805.748450	118997.361252	37.428493
1807.359904	119166.458911	37.433511
1808.745923	119339.270882	37.438528
1810.898232	119507.727765	37.443546
1812.475496	119690.418119	37.448564
1814.191681	119866.200000	37.453581
1816.047786	120032.219117	37.458599
1818.170619	120208.370554	37.463616
1820.028196	120386.213099	37.468634
1821.458484	120567.890353	37.473652
1823.204763	120746.728612	37.478669
1825.325413	120939.069613	37.483687
1826.707835	121132.300249	37.488704
1828.726898	121314.003534	37.493722
1830.510223	121507.896690	37.498740
1832.810937	121691.574836	37.503757
1835.078356	121866.709187	37.508775
1836.817189	122048.155064	37.513792
1838.840782	122208.043128	37.518810
1840.725127	122409.231789	37.523828
1842.775526	122573.062329	37.528845
1844.622447	122745.893873	37.533863
1846.566885	122918.190891	37.538880
1848.851704	123093.848117	37.543898
1850.439718	123281.158540	37.548916
1852.161292	123451.589716	37.553933
1854.021511	123613.563996	37.558951
1855.994374	123797.911916	37.563968
1857.259968	123976.319591	37.568986
1859.465225	124158.362233	37.574004
1861.010666	124341.535963	37.579021
1863.136984	124522.501551	37.584039
1864.439964	124711.372697	37.589056
1866.632237	124891.454340	37.594074
1868.051283	125072.976501	37.599092
1870.111268	125261.427939	37.604109
1871.961729	125451.904625	37.609127
1873.844263	125643.100342	37.614144
1875.867867	125831.395173	37.619162
1877.401389	126019.221628	37.624180
1879.446963	126210.762551	37.629197
1881.266337	126393.573095	37.634215
1882.761898	126589.984269	37.639232
1884.884146	126777.836767	37.644250
1886.979307	126954.212755	37.649268
1888.813991	127128.156097	37.654285
1890.902952	127293.674533	37.659303
1892.619252	127456.790357	37.664320
1894.727173	127623.804231	37.669338
1895.974270	127796.497013	37.674356
1897.946464	127963.152767	37.679373
1899.731805	128137.869266	37.684391
1901.143830	128325.712468	37.689408
1903.623706	128495.945273	37.694426
1905.037921	128678.600615	37.699444
1906.756082	128875.419358	37.704461
1908.770787	129067.067130	37.709479
1909.614080	129266.434486	37.714496
1911.704344	129459.188789	37.719514
1913.597966	129660.107364	37.724532
1915.820612	129877.380905	37.729549
1917.970351	130073.655941	37.734567
1919.543607	130280.818956	37.739584
1922.406580	130479.890380	37.744602
1924.321458	130669.632386	37.749620
1926.415981	130883.581388	37.754637
1928.672640	131083.270198	37.759655
1930.065164	131284.604315	37.764672
1932.142548	131486.264185	37.769690
1933.612376	131705.973444	37.774708
1935.362079	131902.039979	37.779725
1937.849240	132112.609641	37.784743
1940.033498	132311.236892	37.789760
1942.420037	132510.455304	37.794778
1944.096189	132731.431870	37.799796
1946.143473	132933.927911	37.804813
1948.195684	133145.636105	37.809831
1949.854701	133353.422250	37.814848
1951.639443	133570.071971	37.819866
1953.393199	133784.735426	37.824884
1955.120636	134008.400471	37.829901
1957.225304	134217.859710	37.834919
1958.881493	134460.863459	37.839936
1961.037021	134668.997246	37.844954
1962.927414	134904.150466	37.849972
1964.975730	135127.035218	37.854989
1967.395821	135348.403946	37.860007
1968.974830	135563.039717	37.865024
1971.289571	135779.871481	37.870042
1973.743353	135999.740814	37.875060
1975.765430	136226.035871	37.880077
1978.073496	136431.730368	37.885095
1979.931447	136655.565944	37.890112
1981.776500	136864.151562	37.895130
1983.535841	137083.334759	37.900148
1985.381244	137306.858231	37.905165
1987.326691	137528.819049	37.910183
1988.745058	137757.169887	37.915200
1991.211956	137978.061892	37.920218
1993.716124	138200.154712	37.925236
1995.535985	138413.116659	37.930253
1997.852192	138634.568230	37.935271
1999.584548	138857.850287	37.940288
2001.936910	139073.257739	37.945306
2004.057592	139297.115971	37.950324
2005.756485	139516.941895	37.955341
2007.486931	139727.753668	37.960359
2009.387786	139950.253258	37.965376
2011.197735	140168.199413	37.970394
2013.230769	140401.048793	37.975412
2015.577173	140632.162671	37.980429
2017.449941	140844.391304	37.985447
2019.506680	141069.321188	37.990464
2021.586593	141260.922148	37.995482
2024.050358	141462.959566	38.000500
2025.685153	141662.982062	38.005517
2027.517596	141862.200470	38.010535
2028.817712	142061.223339	38.015552
2031.236504	142269.045588	38.020570
2033.193568	142481.674418	38.025588
2034.989093	142684.798152	38.030605
2036.770222	142905.502487	38.035623
2038.590124	143129.146187	38.040640
2040.422400	143360.086571	38.045658
2042.200050	143582.660130	38.050676
2044.086024	143822.630685	38.055693
2046.220209	144058.477060	38.060711
2048.065726	144306.337759	38.065728
2050.379701	144552.108790	38.070746
2052.309454	144786.442025	38.075764
2054.780489	145028.789538	38.080781
2057.743414	145245.601613	38.085799
2060.496985	145473.705008	38.090816
2062.850762	145689.484203	38.095834
2064.993170	145903.672621	38.100852
2066.922335	146123.898521	38.105869
2070.268857	146327.925282	38.110887
2072.490288	146524.398369	38.115904
2075.120007	146725.035206	38.120922
2077.833426	146923.172097	38.125940
2079.383296	147111.819218	38.130957
2081.245036	147308.833590	38.135975
2083.156875	147519.904212	38.140992
2085.092105	147712.783614	38.146010
2087.137644	147929.965597	38.151028
2088.879913	148140.658961	38.156045
2090.626956	148346.161110	38.161063
2092.776140	148565.144653	38.166080
2094.725607	148789.884649	38.171098
2096.615869	149014.520580	38.176116
2098.717680	149228.868657	38.181133
2100.940918	149446.168857	38.186151
2102.940246	149680.386517	38.191168
2105.251440	149899.705760	38.196186
2107.879867	150106.829203	38.201204
2109.961964	150318.874572	38.206221
2112.503919	150527.713980	38.211239
2114.474600	150738.547095	38.216256
2116.150753	150962.970650	38.221274
2118.212478	151176.126867	38.226292
2119.588743	151408.862322	38.231309
2121.936577	151632.320943	38.236327
2123.742147	151863.734861	38.241344
2125.741426	152102.850003	38.246362
2128.175938	152336.148223	38.251380
2129.424871	152586.552643	38.256397
2131.896579	152811.761184	38.261415
2133.632808	153064.338710	38.266432
2135.770733	153311.117229	38.271450
2137.748461	153563.291295	38.276468
2139.499067	153814.486318	38.281485
2141.938969	154072.836172	38.286503
2143.902684	154328.062399	38.291520
2145.967161	154577.853684	38.296538
2147.976075	154832.783169	38.301556
2150.224779	155097.222557	38.306573
2152.288535	155362.872514	38.311591
2154.866036	155620.306640	38.316608
2156.902887	155874.081190	38.321626
2159.106687	156122.067565	38.326644
2161.093359	156375.877497	38.331661
2163.424873	156612.636791	38.336679
2165.803772	156834.752735	38.341696
2167.603687	157077.004547	38.346714
2169.977649	157306.498652	38.351732
2171.915674	157539.666811	38.356749
2173.844625	157775.871362	38.361767
2176.242798	158021.588467	38.366784
2178.297927	158260.034981	38.371802
2180.099854	158488.975205	38.376820
2182.370567	158756.893308	38.381837
2184.355085	159005.103548	38.386855
2186.364842	159267.808741	38.391872
2188.198894	159526.149862	38.396890
2190.587428	159788.036622	38.401908
2193.137958	160051.511589	38.406925
2195.264083	160311.956055	38.411943
2197.632435	160580.615943	38.416960
2199.932112	160834.307008	38.421978
2202.788980	161078.416128	38.426996
2205.049322	161342.500311	38.432013
2207.549850	161593.801803	38.437031
2209.983676	161856.490004	38.442048
2211.990633	162115.805178	38.447066
2214.272564	162368.095927	38.452084
2216.340700	162630.691873	38.457101
2218.600396	162887.723668	38.462119
2220.728512	163150.807533	38.467136
2222.548607	163420.402659	38.472154
2224.815347	163686.006310	38.477172
2226.976681	163963.320546	38.482189
2229.047965	164240.675357	38.487207
2231.434487	164517.982270	38.492224
2233.600422	164804.427887	38.497242
2235.990399	165073.204689	38.502260
2237.855003	165348.463297	38.507277
2240.041458	165632.116056	38.512295
2242.446921	165924.636143	38.517312
2244.272207	166220.637753	38.522330
2246.461474	166501.411588	38.527348
2248.799242	166798.719864	38.532365
2251.141386	167095.127275	38.537383
2253.486650	167385.352155	38.542400
2255.655049	167687.286817	38.547418
2258.085767	167973.856862	38.552436
2260.592173	168286.648086	38.557453
2262.783629	168572.076982	38.562471
2265.547171	168857.443385	38.567488
2267.766408	169148.914040	38.572506
2270.305341	169420.287395	38.577524
2272.634615	169724.770481	38.582541
2274.983930	170014.345204	38.587559
2277.333345	170301.178452	38.592576
2278.898397	170589.125279	38.597594
2281.133957	170885.501502	38.602612
2283.511015	171182.161627	38.607629
2285.683454	171484.492446	38.612647
2288.154499	171776.048619	38.617664
2290.035051	172077.601911	38.622682
2292.464662	172382.842141	38.627700
2294.962257	172674.308753	38.632717
2297.091646	172977.249013	38.637735
2299.464113	173269.626195	38.642752
2301.755748	173579.933659	38.647770
2303.850107	173870.794551	38.652788
2306.418166	174175.817147	38.657805
2309.173816	174473.878647	38.662823
2311.775389	174772.650938	38.667840
2313.826101	175060.932606	38.672858
2316.276675	175312.722275	38.677876
2318.136308	175592.565964	38.682893
2320.578270	175855.621901	38.687911
2322.694346	176125.116602	38.692928
2325.010053	176393.031935	38.697946
2327.489452	176664.554374	38.702964
2329.426242	176943.641466	38.707981
2331.289828	177230.563084	38.712999
2332.986999	177506.413163	38.718016
2335.270236	177809.195264	38.723034
2337.993093	178093.954338	38.728052
2339.859083	178405.692449	38.733069
2341.755413	178707.039516	38.738087
2344.027457	179014.221331	38.743104
2346.393225	179339.345588	38.748122
2349.081372	179646.185496	38.753140
2351.546826	179958.343820	38.758157
2354.126456	180283.946224	38.763175
2356.599131	180593.921451	38.768192
2358.857476	180912.388575	38.773210
2361.649339	181231.357938	38.778228
2363.779744	181546.748645	38.783245
2366.145911	181868.097690	38.788263
2368.795911	182178.126887	38.793280
2371.078798	182509.320200	38.798298
2373.511900	182826.953980	38.803316
2376.234815	183149.064643	38.808333
2378.284526	183469.325473	38.813351
2380.815449	183798.605181	38.818368
2382.915951	184122.238286	38.823386
2385.341061	184449.225380	38.828404
2387.992731	184793.703514	38.833421
2390.200542	185122.123586	38.838439
2393.219750	185440.538238	38.843456
2395.308154	185845.836740	38.848474
2397.957829	186174.648650	38.853492
2400.075312	186503.696830	38.858509
2402.485488	186834.986447	38.863527
2405.246438	187168.508475	38.868544
2407.203617	187525.397219	38.873562
2409.764683	187850.621452	38.878580
2412.312066	188196.346353	38.883597
2414.545605	188530.208704	38.888615
2417.262869	188866.511380	38.893632
2419.792768	189210.134020	38.898650
2421.978312	189543.956107	38.903668
2424.930979	189888.099236	38.908685
2427.175538	190229.686591	38.913703
2429.902198	190540.618059	38.918720
2432.393405	190883.083377	38.923738
2435.148413	191201.606895	38.928756
2438.077753	191522.593386	38.933773
2440.349290	191866.873782	38.938791
2443.001672	192171.572590	38.943808
2444.970078	192504.192314	38.948826
2447.587832	192828.863065	38.953844
2450.412681	193152.029195	38.958861
2453.119886	193467.848226	38.963879
2455.282091	193787.563000	38.968896
2457.645113	194118.322148	38.973914
2460.169984	194438.388524	38.978932
2462.413223	194763.503533	38.983949
2464.691681	195097.123256	38.988967
2467.675158	195402.616548	38.993984
2469.872911	195725.251673	38.999002
2472.394814	196037.701986	39.004020
2474.900730	196361.382917	39.009037
2477.206639	196671.607558	39.014055
2479.558268	196979.742847	39.019072
2481.557142	197287.730492	39.024090
2483.793983	197591.465099	39.029108
2485.877476	197892.430024	39.034125
2487.868602	198215.179224	39.039143
2490.089303	198535.734250	39.044160
2492.183516	198871.753966	39.049178
2494.993097	199190.339008	39.054196
2497.360997	199525.326900	39.059213
2499.847009	199848.713822	39.064231
2502.163120	200184.219228	39.069248
2504.386912	200528.401828	39.074266
2507.050759	200880.416752	39.079284
2509.529616	201230.505252	39.084301
2511.943963	201580.477519	39.089319
2514.614330	201933.535157	39.094336
2516.950111	202298.559309	39.099354
2519.304151	202660.075852	39.104372
2521.788692	203019.921667	39.109389
2524.610659	203389.165437	39.114407
2526.979661	203749.564141	39.119424
2529.192860	204125.051557	39.124442
2531.513221	204509.134556	39.129460
2534.272143	204882.480925	39.134477
2536.921602	205277.107177	39.139495
2539.414534	205656.186633	39.144512
2541.953242	206044.379311	39.149530
2545.051869	206427.201774	39.154548
2548.070482	206802.772135	39.159565
2550.414827	207183.579494	39.164583
2553.471535	207554.242447	39.169600
2556.248384	207927.921731	39.174618
2559.048388	208290.928704	39.179636
2562.742296	208661.545101	39.184653
2565.348999	209016.708290	39.189671
2568.283441	209379.975441	39.194688
2570.809292	209728.725218	39.199706
2573.490993	210083.293987	39.204724
2576.156570	210438.958095	39.209741
2578.191880	210806.203100	39.214759
2580.482998	211173.637421	39.219776
2583.123710	211536.724638	39.224794
2585.930116	211903.317616	39.229812
2588.831558	212249.065370	39.234829
2591.201389	212623.272026	39.239847
2593.402264	212979.799127	39.244864
2596.169784	213342.919597	39.249882
2598.789693	213709.873987	39.254900
2601.759750	214080.127571	39.259917
2603.743853	214458.384729	39.264935
2606.435525	214818.216087	39.269952
2609.052452	215193.149252	39.274970
2611.150691	215570.576860	39.279988
2613.724725	215940.335047	39.285005
2616.262402	216332.556199	39.290023
2619.164176	216710.647319	39.295040
2621.594449	217088.786730	39.300058
2623.834224	217470.588847	39.305076
2626.950775	217858.351754	39.310093
2629.638491	218251.033839	39.315111
2631.736172	218636.110639	39.320128
2634.791073	219021.623027	39.325146
2637.586030	219412.612566	39.330164
2640.204635	219784.170335	39.335181
2642.732488	220168.977915	39.340199
2645.397860	220548.658093	39.345216
2648.409606	220925.464708	39.350234
2651.006560	221285.086703	39.355252
2654.026249	221643.576086	39.360269
2656.331746	221982.336178	39.365287
2658.809180	222326.099626	39.370304
2662.034109	222673.506650	39.375322
2664.321750	223009.119715	39.380340
2667.620156	223336.446255	39.385357
2670.187506	223692.440820	39.390375
2673.207613	224022.046356	39.395392
2675.431202	224362.801270	39.400410
2677.875591	224716.731995	39.405428
2680.305818	225059.131497	39.410445
2682.589857	225431.886263	39.415463
2685.325760	225791.360593	39.420480
2687.479400	226156.870094	39.425498
2689.987259	226536.042673	39.430516
2692.702919	226916.249860	39.435533
2695.197814	227295.449796	39.440551
2697.752917	227687.952053	39.445568
2701.164445	228067.009222	39.450586
2703.569862	228453.539258	39.455604
2706.162381	228838.261796	39.460621
2708.572761	229229.744644	39.465639
2711.233486	229630.079825	39.470656
2714.400046	230024.772653	39.475674
2716.675014	230431.239116	39.480692
2719.615571	230834.578735	39.485709
2722.609921	231239.789679	39.490727
2725.916291	231637.330651	39.495744
2728.596933	232029.557726	39.500762
2731.649286	232433.615775	39.505780
2734.834869	232823.909292	39.510797
2737.275724	233224.607032	39.515815
2740.077498	233626.620126	39.520832
2742.876610	234040.115883	39.525850
2745.101618	234446.485939	39.530868
2747.772910	234847.527599	39.535885
2750.216485	235273.500085	39.540903
2752.854022	235682.294405	39.545920
2755.769245	236098.335989	39.550938
2758.182925	236521.796868	39.555956
2761.180562	236945.064788	39.560973
2763.768087	237374.315098	39.565991
2766.551474	237808.665944	39.571008
2769.359113	238234.527653	39.576026
2772.230689	238665.434174	39.581044
2775.448785	239080.586790	39.586061
2778.569168	239508.074758	39.591079
2781.703454	239910.461311	39.596096
2785.153103	240331.672987	39.601114
2788.216522	240734.475860	39.606132
2791.297706	241133.972938	39.611149
2794.250487	241543.777746	39.616167
2797.205005	241926.755763	39.621184
2799.815908	242329.321775	39.626202
2802.484764	242752.378500	39.631220
2804.928829	243145.773166	39.636237
2807.769421	243554.601372	39.641255
2810.758703	243961.373467	39.646272
2813.376409	244355.043880	39.651290
2815.786996	244780.067698	39.656308
2818.643041	245176.544669	39.661325
2821.255157	245588.554613	39.666343
2823.936031	245999.460713	39.671360
2826.955400	246406.477482	39.676378
2829.384063	246825.219788	39.681396
2831.972157	247244.749266	39.686413
2834.552286	247671.595012	39.691431
2837.132296	248089.193271	39.696448
2839.713142	248495.638752	39.701466
2841.995613	248903.120442	39.706484
2844.937176	249302.166644	39.711501
2846.900726	249718.815523	39.716519
2849.825636	250151.317202	39.721536
2852.632237	250567.781991	39.726554
2855.387333	250996.141939	39.731572
2857.908756	251423.775056	39.736589
2860.893326	251861.495747	39.741607
2863.440605	252299.232462	39.746624
2866.573121	252731.339258	39.751642
2868.900687	253185.644224	39.756660
2872.234715	253641.391490	39.761677
2874.256109	254102.752152	39.766695
2877.596167	254570.078702	39.771712
2880.615074	255032.678218	39.776730
2883.314205	255489.509053	39.781748
2886.703881	255949.990298	39.786765
2889.565296	256422.947962	39.791783
2892.623706	256885.966865	39.796800
2895.948014	257349.806391	39.801818
2898.783920	257824.541046	39.806836
2901.785844	258288.757561	39.811853
2905.607267	258749.923748	39.816871
2909.175735	259208.917727	39.821888
2912.273219	259661.302934	39.826906
2915.345456	260114.757190	39.831924
2918.343296	260562.455416	39.836941
2921.405537	261007.424087	39.841959
2924.100256	261464.665713	39.846976
2927.451710	261919.593509	39.851994
2930.160963	262379.216800	39.857012
2933.476335	262825.713759	39.862029
2936.208630	263287.209289	39.867047
2939.121509	263737.778322	39.872064
2942.005843	264187.308529	39.877082
2945.032465	264640.827800	39.882100
2948.129131	265095.121591	39.887117
2951.210617	265554.673389	39.892135
2954.024814	266014.493316	39.897152
2956.840718	266470.983630	39.902170
2959.909931	266937.109406	39.907188
2962.779090	267389.802801	39.912205
2966.393626	267839.558869	39.917223
2969.849798	268276.816041	39.922240
2973.623253	268714.021847	39.927258
2976.479764	269160.257723	39.932276
2979.310770	269607.181201	39.937293
2981.972966	270038.966190	39.942311
2985.083622	270480.355968	39.947328
2988.544268	270929.308479	39.952346
2991.288087	271367.576311	39.957364
2994.286615	271804.938845	39.962381
2997.168440	272247.219080	39.967399
2999.990272	272682.674559	39.972416
3003.467922	273132.908525	39.977434
3005.835244	273574.500164	39.982452
3009.100111	274013.308572	39.987469
3011.922393	274457.770860	39.992487
3014.828767	274909.709703	39.997504
3017.806051	275347.692393	40.002522
3020.812136	275798.569607	40.007540
3023.765285	276243.281293	40.012557
3026.625799	276693.414307	40.017575
3029.282458	277150.611180	40.022592
3032.200237	277591.562296	40.027610
3035.395395	278054.181027	40.032628
3038.237971	278497.068818	40.037645
3041.231494	278929.366131	40.042663
3043.855338	279356.969639	40.047680
3046.623065	279780.281989	40.052698
3049.415430	280214.380964	40.057716
3052.465921	280649.580020	40.062733
3055.485582	281084.806720	40.067751
3057.800218	281535.681965	40.072768
3061.151747	281975.905235	40.077786
3063.847608	282431.286587	40.082804
3066.840605	282894.110041	40.087821
3069.609400	283365.497701	40.092839
3072.449230	283844.438471	40.097856
3075.199708	284319.580863	40.102874
3078.157735	284804.007051	40.107892
3081.587665	285291.581332	40.112909
3084.562630	285778.842049	40.117927
3086.887152	286284.559436	40.122944
3089.943308	286790.463887	40.127962
3093.194635	287292.195188	40.132980
3095.917432	287821.555416	40.137997
3099.361067	288342.343695	40.143015
3102.330711	288866.883375	40.148032
3106.022896	289389.071908	40.153050
3109.084187	289912.268451	40.158068
3112.053768	290443.320813	40.163085
3115.438617	290965.721962	40.168103
3118.514853	291510.637522	40.173120
3121.801253	292037.970790	40.178138
3124.973293	292576.717552	40.183156
3128.017003	293116.545911	40.188173
3131.698432	293644.692479	40.193191
3134.775240	294181.154709	40.198208
3138.143846	294713.352076	40.203226
3141.653948	295260.121367	40.208244
3144.950020	295794.986105	40.213261
3148.203979	296323.733825	40.218279
3151.976637	296858.920808	40.223296
3156.060658	297372.550569	40.228314
3159.668429	297885.538944	40.233332
3163.548450	298377.789312	40.238349
3167.719649	298847.141301	40.243367
3170.863878	299346.453822	40.248384
3174.427434	299820.538019	40.253402
3177.510879	300293.753533	40.258420
3180.415803	300786.591201	40.263437
3183.867996	301259.309379	40.268455
3186.792203	301740.736877	40.273472
3190.195910	302227.137240	40.278490
3192.944548	302701.475350	40.283508
3195.947916	303185.796839	40.288525
3198.878473	303665.327393	40.293543
3202.378519	304153.471989	40.298560
3205.820991	304629.867813	40.303578
3209.109308	305110.192453	40.308596
3211.841286	305607.073582	40.313613
3215.172491	306092.306888	40.318631
3217.726947	306584.205447	40.323648
3220.859778	307075.729987	40.328666
3224.240981	307566.551091	40.333684
3226.938499	308067.525439	40.338701
3230.440432	308561.592336	40.343719
3233.447328	309066.112765	40.348736
3236.340894	309565.061527	40.353754
3239.694507	310056.775852	40.358772
3242.371116	310573.896134	40.363789
3245.587632	311067.652020	40.368807
3248.617959	311583.208859	40.373824
3252.266509	312091.988710	40.378842
3255.590717	312569.087708	40.383860
3259.128475	313043.864386	40.388877
3262.315593	313500.366317	40.393895
3265.624777	313981.742463	40.398912
3268.497543	314443.182338	40.403930
3271.132779	314925.491026	40.408948
3274.135538	315418.650453	40.413965
3277.175390	315900.378277	40.418983
3280.287121	316405.539579	40.424000
3283.329762	316922.786011	40.429018
3286.080989	317432.001609	40.434036
3288.854643	317952.145665	40.439053
3292.352261	318481.408308	40.444071
3295.538539	319029.441297	40.449088
3298.653928	319559.207184	40.454106
3302.188624	320097.351712	40.459124
3305.314633	320646.997759	40.464141
3309.137253	321193.584775	40.469159
3312.779040	321743.364861	40.474176
3316.128225	322276.131264	40.479194
3319.874635	322831.057464	40.484212
3323.349475	323375.640423	40.489229
3327.086114	323909.467642	40.494247
3330.801041	324455.521551	40.499264
3333.976981	324999.368492	40.504282
3337.462811	325538.136120	40.509300
3340.828391	326081.609316	40.514317
3344.456573	326629.296946	40.519335
3347.567927	327190.454047	40.524352
3350.948536	327743.391698	40.529370
3354.719263	328291.922471	40.534388
3358.201935	328833.386591	40.539405
3362.293959	329357.750078	40.544423
3366.141421	329884.707030	40.549440
3369.807842	330413.435583	40.554458
3373.504235	330945.044429	40.559476
3376.924799	331474.684714	40.564493
3380.175995	332007.083921	40.569511
3382.950303	332540.793002	40.574528
3386.165847	333082.873589	40.579546
3389.377805	333623.526383	40.584564
3392.616001	334176.242303	40.589581
3395.836581	334733.823324	40.594599
3398.829780	335285.622407	40.599616
3401.894611	335843.160328	40.604634
3405.399568	336407.901401	40.609652
3408.377357	336983.851350	40.614669
3411.808746	337554.014470	40.619687
3415.111210	338136.566758	40.624704
3418.212045	338718.405482	40.629722
3422.035811	339289.697703	40.634740
3425.638684	339876.182623	40.639757
3429.659198	340436.595634	40.644775
3433.075685	341020.757266	40.649792
3436.480850	341597.200832	40.654810
3440.293714	342172.709187	40.659828
3443.613783	342752.367952	40.664845
3447.087961	343324.410100	40.669863
3450.861215	343896.802021	40.674880
3454.189117	344467.250264	40.679898
3457.909258	345028.549145	40.684916
3461.867956	345590.207413	40.689933
3465.317527	346155.485871	40.694951
3468.574244	346718.096868	40.699968
3472.344290	347276.814844	40.704986
3475.507255	347832.904679	40.710004
3478.735384	348408.601652	40.715021
3482.032559	348948.467290	40.720026
3485.264447	349464.962578	40.725031
3488.263728	349946.328756	40.730036
3491.727944	350380.917831	40.735040
3494.758441	350765.109276	40.740045
3497.279437	351094.086839	40.745050
3499.902035	351384.127484	40.750055
3501.917845	351637.045600	40.755060
3504.454195	351840.287340	40.760064
3506.064974	352000.204738	40.765069
3507.649008	352119.302178	40.770074
3509.000603	352223.768478	40.775079
3510.240062	352285.242728	40.780084
3511.592032	352314.747538	40.785088
3512.459962	352322.695987	40.790093
3513.726195	352299.215262	40.795098
3514.722018	352266.269837	40.800103
3514.947692	352207.465809	40.805108
3516.336341	352121.739640	40.810112
3516.749395	352031.462482	40.815117
3517.264807	351909.420282	40.820122
3517.601086	351770.043951	40.825127
3517.738917	351638.857610	40.830132
3518.150270	351475.116293	40.835136
3517.898493	351317.781477	40.840141
3518.448313	351147.890764	40.845146
3518.774319	350977.525588	40.850151
3518.242929	350799.412648	40.855156
3518.523495	350614.232600	40.860160
3518.331514	350419.414367	40.865165
3518.062219	350223.742696	40.870170
3518.491481	350035.536580	40.875175
3518.178150	349842.335311	40.880180
3518.317463	349633.936848	40.885184
3517.640736	349441.654090	40.890189
3517.356427	349238.454158	40.895194
3517.292299	349048.234604	40.900199
3517.399810	348850.157327	40.905204
3517.199756	348650.525142	40.910208
3516.853842	348452.617733	40.915213
3516.737207	348253.859953	40.920218
3516.415898	348053.912558	40.925223
3516.018595	347864.449888	40.930228
3516.215984	347669.173489	40.935232
3515.542764	347488.242806	40.940237
3516.017038	347289.489017	40.945242
3515.578077	347102.113195	40.950247
3515.460373	346911.610116	40.955252
3515.223040	346729.768541	40.960256
3514.548885	346560.324387	40.965261
3514.274967	346375.664578	40.970266
3514.480149	346203.234341	40.975271
3514.101649	346032.953393	40.980276
3513.750428	345858.777458	40.985280
3513.448854	345690.999805	40.990285
3513.543982	345525.549478	40.995290
3513.138148	345354.913440	41.000295
3512.971950	345202.011040	41.005300
3513.269603	345035.052190	41.010304
3512.715830	344878.166122	41.015309
3512.638986	344716.882879	41.020314
3512.409708	344562.614487	41.025319
3512.270623	344400.907216	41.030324
3511.913547	344255.047634	41.035328
3511.779103	344123.365577	41.040333
3511.705033	343968.765261	41.045338
3511.117026	343822.710952	41.050343
3510.817709	343679.255374	41.055348
3511.230922	343538.841121	41.060352
3510.916390	343406.599559	41.065357
3510.533939	343268.698061	41.070362
3510.783331	343138.859472	41.075367
3510.385800	343008.409133	41.080372
3510.444589	342871.962968	41.085376
3510.419711	342747.377986	41.090381
3510.183778	342630.885595	41.095386
3509.642935	342489.217107	41.100391
3509.563097	342375.852469	41.105396
3509.689982	342249.080825	41.110400
3509.453999	342144.918792	41.115405
3509.539157	342027.357349	41.120410
3509.213388	341914.105765	41.125415
3508.941450	341799.752075	41.130420
3508.530131	341682.037888	41.135424
3508.535111	341585.083436	41.140429
3508.768315	341474.515020	41.145434
3508.274628	341368.687155	41.150439
3508.293129	341268.271601	41.155444
3507.905418	341159.248183	41.160448
3507.862277	341072.063982	41.165453
3507.671271	340965.297839	41.170458
3507.353138	340882.198963	41.175463
3507.456417	340798.271480	41.180468
3507.728928	340699.925292	41.185472
3507.251847	340617.664221	41.190477
3507.723267	340520.659691	41.195482
3507.466191	340435.109177	41.200487
3507.635232	340344.559092	41.205492
3507.726969	340244.408948	41.210496
3507.325707	340162.491019	41.215501
3507.402601	340068.445471	41.220506
3507.269098	339967.210752	41.225511
3507.314885	339891.706874	41.230516
3507.228001	339798.550668	41.235520
3507.052423	339721.199166	41.240525
3506.822343	339636.685105	41.245530
3506.845501	339544.426543	41.250535
3506.853407	339476.556291	41.255540
3507.029929	339389.384642	41.260544
3506.577164	339313.524835	41.265549
3506.362346	339223.819937	41.270554
3506.771346	339141.595578	41.275559
3506.279420	339068.945399	41.280564
3506.363968	338989.288655	41.285568
3505.893558	338916.405958	41.290573
3506.166745	338849.891843	41.295578
3506.353586	338770.905287	41.300583
3506.069757	338700.434325	41.305588
3506.155189	338610.274306	41.310592
3506.199722	338553.000652	41.315597
3506.135019	338466.144028	41.320602
3505.981902	338394.533233	41.325607
3506.065998	338324.512875	41.330612
3506.299836	338254.596227	41.335616
3506.161654	338189.797836	41.340621
3506.169559	338108.828736	41.345626
3506.305559	338030.204489	41.350631
3505.800603	337963.530107	41.355636
3505.777221	337888.363379	41.360640
3505.985098	337810.973537	41.365645
3506.122330	337744.732848	41.370650
3505.888290	337678.626104	41.375655
3505.536418	337620.217452	41.380660
3505.680548	337543.676153	41.385664
3505.636657	337474.589556	41.390669
3505.605025	337406.314688	41.395674
3505.788964	337337.497541	41.400679
3505.531759	337270.554463	41.405684
3505.504651	337194.980001	41.410688
3505.433663	337137.289777	41.415693
3505.650332	337068.517891	41.420698
3505.699001	337013.453617	41.425703
3505.484659	336955.988858	41.430708
3505.552693	336877.042107	41.435712
3505.157221	336820.241085	41.440717
3505.352171	336749.488394	41.445722
3505.511801	336682.123347	41.450727
3505.450733	336635.162543	41.455732
3505.530704	336559.417524	41.460736
3505.346146	336495.666005	41.465741
3505.496881	336437.355268	41.470746
3505.279877	336373.862896	41.475751
3504.675334	336316.839321	41.480756
3505.313515	336246.143845	41.485760
3505.148086	336190.425017	41.490765
3505.075160	336120.017974	41.495770
3505.506188	336065.350540	41.500775
3504.908645	336005.680557	41.505780
3505.191649	335942.236790	41.510784
3505.063111	335886.104863	41.515789
3504.947937	335825.952627	41.520794
3505.167802	335774.369379	41.525799
3504.845443	335716.334574	41.530804
3504.959491	335652.789446	41.535808
3504.959427	335598.239270	41.540813
3504.920353	335536.116500	41.545818
3504.879321	335485.768729	41.550823
3504.734161	335424.450657	41.555828
3504.628110	335372.256346	41.560832
3504.776213	335321.828058	41.565837
3504.964368	335261.169935	41.570842
3504.763638	335209.676784	41.575847
3504.487291	335156.567696	41.580852
3504.792494	335101.130039	41.585856
3504.467758	335050.469782	41.590861
3504.494739	334994.236011	41.595866
3505.186426	334944.917922	41.600871
3504.925450	334890.763356	41.605876
3504.587606	334826.142701	41.610880
3504.297301	334763.396505	41.615885
3504.408401	334721.467457	41.620890
3504.344478	334675.852514	41.625895
3504.204965	334628.570760	41.630900
3504.413310	334582.557286	41.635904
3504.623206	334538.679816	41.640909
3504.811637	334473.976658	41.645914
3504.877752	334426.815243	41.650919
3504.550092	334374.145377	41.655924
3504.601166	334311.650489	41.660928
3504.893038	334261.910504	41.665933
3504.713984	334208.988389	41.670938
3504.521318	334143.987912	41.675943
3504.520290	334096.607640	41.680948
3504.631131	334043.843641	41.685952
3504.404910	333993.548111	41.690957
3504.631950	333945.954131	41.695962
3504.772645	333885.886116	41.700967
3504.379814	333839.532929	41.705972
3504.591126	333785.837359	41.710976
3504.341857	333739.716036	41.715981
3504.581179	333682.404516	41.720986
3504.781993	333630.490651	41.725991
3504.217006	333578.212661	41.730996
3504.231963	333524.191215	41.736000
3504.283251	333473.495747	41.741005
3504.047331	333432.992641	41.746010
3504.380052	333381.032475	41.751015
3504.214302	333337.313795	41.756020
3504.288479	333288.878054	41.761024
3504.223909	333249.797769	41.766029
3504.164507	333201.255537	41.771034
3504.008018	333152.117957	41.776039
3504.033276	333108.064091	41.781044
3504.369211	333054.042894	41.786048
3504.355022	333005.035579	41.791053
3504.176573	332951.780977	41.796058
3504.494030	332904.146185	41.801063
3504.523757	332854.648610	41.806068
3504.783684	332805.038848	41.811072
3504.229393	332756.700227	41.816077
3504.304574	332706.254351	41.821082
3504.402305	332651.760982	41.826087
3504.296919	332611.338420	41.831092
3504.471737	332559.884941	41.836096
3504.040904	332511.806565	41.841101
3503.668663	332467.076241	41.846106
3503.809089	332419.773596	41.851111
3503.709525	332377.315192	41.856116
3503.951744	332326.435883	41.861120
3503.994524	332284.896272	41.866125
3503.896487	332247.244453	41.871130
3504.192103	332201.367109	41.876135
3503.973785	332156.230963	41.881140
3504.349854	332108.408022	41.886144
3504.044884	332068.880693	41.891149
3503.685259	332024.249624	41.896154
3503.677301	331982.870184	41.901159
3503.833255	331945.560052	41.906164
3503.909704	331891.704761	41.911168
3503.942489	331850.064498	41.916173
3503.753692	331805.279421	41.921178
3503.971688	331762.669184	41.926183
3503.797371	331723.858756	41.931188
3503.904007	331675.136143	41.936192
3504.054656	331637.953709	41.941197
3503.839090	331580.328306	41.946202
3504.332552	331535.284141	41.951207
3503.696287	331502.420670	41.956212
3503.708673	331457.909092	41.961216
3503.674011	331421.899827	41.966221
3503.909633	331382.465709	41.971226
3503.745896	331339.965276	41.976231
3503.895723	331302.680909	41.981236
3503.793840	331248.267480	41.986240
3504.140619	331210.113042	41.991245
3504.271373	331165.557273	41.996250
3504.236485	331115.151870	42.001255
3504.200088	331068.638113	42.006260
3503.829872	331025.101216	42.011264
3504.072515	330976.865248	42.016269
3503.835007	330926.440261	42.021274
3503.977655	330879.059073	42.026279
3503.735337	330853.102828	42.031284
3503.943771	330812.146283	42.036288
3503.984418	330767.883860	42.041293
3503.931146	330721.931876	42.046298
3503.864979	330673.819891	42.051303
3503.594378	330638.050090	42.056308
3503.557990	330588.025756	42.061312
3503.922279	330542.797062	42.066317
3503.589341	330522.526665	42.071322
3503.706149	330465.687230	42.076327
3503.576401	330425.952908	42.081332
3503.853021	330372.649356	42.086336
3503.831262	330340.528625	42.091341
3503.776710	330298.010060	42.096346
3503.828687	330259.035774	42.101351
3503.433482	330224.429558	42.106356
3503.393774	330181.043763	42.111360
3503.395880	330148.359589	42.116365
3503.187941	330115.657202	42.121370
3503.843855	330075.851135	42.126375
3503.493179	330029.919179	42.131380
3504.076887	329986.919426	42.136384
3503.842044	329939.901062	42.141389
3503.713285	329899.937133	42.146394
3503.812349	329855.003267	42.151399
3503.431701	329818.359604	42.156404
3503.425096	329772.526416	42.161408
3503.270032	329732.769892	42.166413
3503.571156	329696.833954	42.171418
3503.448834	329662.337389	42.176423
3503.662233	329620.183356	42.181428
3503.725168	329581.130384	42.186432
3503.459729	329555.126002	42.191437
3503.072243	329519.932945	42.196442
3503.420147	329476.028214	42.201447
3503.414858	329444.158539	42.206452
3503.472577	329405.055332	42.211456
3503.309453	329374.431070	42.216461
3503.331475	329345.583901	42.221466
3503.593314	329303.498299	42.226471
3503.198818	329258.742298	42.231476
3503.291509	329221.312220	42.236480
3503.124875	329189.848982	42.241485
3503.391221	329157.962242	42.246490
3503.466401	329119.746286	42.251495
3503.292321	329091.819699	42.256500
3503.381455	329046.657533	42.261504
3503.530298	329007.844981	42.266509
3503.409420	328981.817724	42.271514
3503.585183	328934.581646	42.276519
3503.248936	328906.959958	42.281524
3503.334105	328862.739327	42.286528
3503.159482	328831.531406	42.291533
3502.922403	328796.848452	42.296538
3503.323300	328757.004429	42.301543
3503.400194	328732.828496	42.306548
3503.562678	328693.810026	42.311552
3503.605608	328653.716371	42.316557
3503.361040	328627.021355	42.321562
3503.465095	328578.218973	42.326567
3503.022997	328536.089479	42.331572
3503.369817	328509.200612	42.336576
3503.402807	328469.769658	42.341581
3503.241961	328437.211165	42.346586
3503.394468	328398.931607	42.351591
3503.227194	328362.634929	42.356596
3503.537862	328332.063312	42.361600
3503.270025	328298.631085	42.366605
3503.360873	328270.128530	42.371610
3503.306577	328227.098963	42.376615
3503.285591	328192.559908	42.381620
3503.569169	328156.777920	42.386624
3503.589355	328120.248358	42.391629
3503.351457	328083.708051	42.396634
3503.799891	328043.118260	42.401639
3503.607685	328012.141359	42.406644
3503.454149	327977.190324	42.411648
3503.450098	327935.856868	42.416653
3503.385643	327903.537304	42.421658
3503.473993	327852.955920	42.426663
3503.471664	327819.532848	42.431668
3503.652673	327775.779389	42.436672
3503.378099	327740.974165	42.441677
3503.629198	327709.012326	42.446682
3503.587283	327676.154901	42.451687
3503.630718	327644.657749	42.456692
3503.585122	327584.227427	42.461696
3503.210278	327554.321498	42.466701
3503.498537	327509.177473	42.471706
3503.450559	327470.979097	42.476711
3503.248983	327446.515039	42.481716
3503.181454	327400.256163	42.486720
3503.403889	327359.242983	42.491725
3503.482653	327333.946688	42.496730
3503.606158	327296.026704	42.501735
3503.433219	327257.084462	42.506740
3503.753546	327210.688701	42.511744
3503.393496	327182.637091	42.516749
3503.018272	327156.114044	42.521754
3503.116980	327106.649335	42.526759
3503.088698	327077.096113	42.531764
3503.204257	327037.600023	42.536768
3503.447244	327004.392468	42.541773
3503.124724	326975.520886	42.546778
3503.255259	326935.767995	42.551783
3503.206336	326898.586708	42.556788
3503.115127	326879.599559	42.561792
3503.158897	326840.445131	42.566797
3503.057223	326806.578805	42.571802
3502.862856	326769.445469	42.576807
3502.590845	326746.111184	42.581812
3502.922013	326715.586020	42.586816
3503.234376	326682.494591	42.591821
3503.238777	326653.953466	42.596826
3503.247062	326610.658052	42.601831
3503.113719	326583.359304	42.606836
3502.776529	326543.653374	42.611840
3503.040750	326510.772795	42.616845
3503.050336	326484.087674	42.621850
3503.082925	326448.953721	42.626855
3503.199074	326422.251977	42.631860
3502.912880	326395.841762	42.636864
3503.028223	326372.497859	42.641869
3502.847892	326347.470202	42.646874
3502.801166	326305.022460	42.651879
3502.910034	326286.767024	42.656884
3503.029197	326251.415928	42.661888
3502.892641	326218.317665	42.666893
3502.512394	326188.742250	42.671898
3502.933328	326146.374194	42.676903
3503.212500	326131.628020	42.681908
3503.382091	326095.861939	42.686912
3503.245479	326059.380344	42.691917
3502.970746	326033.629490	42.696922
3503.196743	325993.352064	42.701927
3502.736167	325967.223083	42.706932
3503.027711	325932.099262	42.711936
3503.242650	325902.583648	42.716941
3502.943791	325876.175065	42.721946
3503.383895	325837.390437	42.726951
3502.990580	325817.355974	42.731956
3502.947089	325769.310842	42.736960
3502.852968	325743.048378	42.741965
3502.964597	325727.132549	42.746970
3503.375746	325685.121667	42.751975
3503.278423	325655.654466	42.756980
3503.115891	325614.241542	42.761984
3502.837360	325573.380825	42.766989
3503.032658	325538.602337	42.771994
3503.180082	325516.601166	42.776999
3503.207134	325486.427661	42.782004
3503.009588	325453.033011	42.787009
3503.166230	325419.583216	42.792013
3503.005412	325392.211630	42.797018
3502.862729	325353.898804	42.802023
3502.911566	325329.063802	42.807028
3503.206138	325295.745072	42.812033
3503.271380	325260.808519	42.817037
3502.896811	325241.712069	42.822042
3503.084461	325195.156586	42.827047
3502.693737	325174.307381	42.832052
3503.116741	325142.647466	42.837057
3502.894688	325109.358101	42.842061
3502.504605	325082.861448	42.847066
3502.684482	325062.330405	42.852071
3503.101558	325032.044997	42.857076
3502.888778	325003.790895	42.862081
3502.894935	324974.357977	42.867085
3502.589760	324950.976946	42.872090
3502.652861	324906.348396	42.877095
3502.843292	324884.798086	42.882100
3502.963278	324854.787724	42.887105
3503.193621	324825.904898	42.892109
3502.957495	324788.445555	42.897114
3502.962007	324753.568898	42.902119
3503.101998	324727.218475	42.907124
3503.307078	324701.697379	42.912129
3503.216328	324663.452143	42.917133
3503.314143	324630.621387	42.922138
3503.442338	324595.547279	42.927143
3503.499974	324567.963079	42.932148
3503.050042	324517.054285	42.937153
3503.371059	324485.867632	42.942157
3503.247419	324459.252799	42.947162
3503.247411	324419.441456	42.952167
3503.039041	324389.354658	42.957172
3502.929771	324359.328733	42.962177
3502.902677	324320.411866	42.967181
3502.806933	324298.269813	42.972186
3502.977270	324262.756406	42.977191
3502.851552	324231.562763	42.982196
3502.894212	324212.095643	42.987201
3503.178781	324179.566172	42.992205
3502.933476	324145.618237	42.997210
3503.105666	324110.765822	43.002215
3503.032157	324083.456095	43.007220
3502.842707	324053.086281	43.012225
3503.006688	324012.816566	43.017229
3502.952649	323982.374750	43.022234
3503.039809	323950.766184	43.027239
3502.830435	323930.549542	43.032244
3502.874502	323904.773182	43.037249
3502.931422	323856.786509	43.042253
3502.936358	323842.896240	43.047258
3503.359357	323799.889471	43.052263
3502.854670	323783.381942	43.057268
3502.941609	323746.100333	43.062273
3502.563609	323715.530661	43.067277
3502.516769	323686.410343	43.072282
3502.996550	323655.605388	43.077287
3502.719331	323633.084193	43.082292
3502.698005	323607.088871	43.087297
3502.872845	323575.669890	43.092301
3502.715971	323553.511513	43.097306
3502.799837	323518.010926	43.102311
3502.731530	323485.535825	43.107316
3502.897559	323464.751754	43.112321
3502.687507	323437.157579	43.117325
3502.737986	323411.659749	43.122330
3503.124685	323374.000449	43.127335
3502.612156	323342.611938	43.132340
3502.736250	323314.863928	43.137345
3502.964820	323283.410926	43.142349
3502.816724	323259.419390	43.147354
3502.986506	323225.889460	43.152359
3502.934036	323206.284037	43.157364
3502.570278	323172.557256	43.162369
3503.072701	323146.251190	43.167373
3502.369115	323122.295137	43.172378
3502.844655	323093.856303	43.177383
3502.738383	323072.681939	43.182388
3502.784062	323042.809029	43.187393
3503.060367	323011.958945	43.192397
3502.616506	322980.355959	43.197402
3502.764850	322952.146022	43.202407
3502.506305	322928.960112	43.207412
3502.721417	322898.221225	43.212417
3502.558612	322866.091064	43.217421
3502.827445	322849.310157	43.222426
3502.768908	322820.877928	43.227431
3502.747616	322791.320538	43.232436
3502.826287	322765.334572	43.237441
3502.648761	322735.572497	43.242445
3502.876254	322712.387152	43.247450
3503.027625	322678.121897	43.252455
3502.668332	322656.427020	43.257460
3502.637123	322623.996358	43.262465
3502.744401	322598.438315	43.267469
3502.825896	322579.905665	43.272474
3502.957301	322541.903750	43.277479
3502.761560	322514.510259	43.282484
3502.462354	322494.917459	43.287489
3502.569416	322469.791850	43.292493
3502.496645	322454.106979	43.297498
3502.748064	322424.990253	43.302503
3502.511135	322406.608837	43.307508
3502.564392	322376.428995	43.312513
3502.675364	322344.357593	43.317517
3502.659910	322324.084558	43.322522
3502.523556	322292.331443	43.327527
3502.653832	322265.319538	43.332532
3502.496960	322237.919819	43.337537
3502.654979	322218.306621	43.342541
3502.853614	322196.066765	43.347546
3502.779924	322152.525039	43.352551
3502.167332	322130.869308	43.357556
3502.939059	322112.686966	43.362561
3502.997018	322085.330039	43.367565
3502.824670	322060.934550	43.372570
3502.809776	322026.440238	43.377575
3502.702512	322004.629486	43.382580
3502.569817	321972.544839	43.387585
3502.791802	321944.653492	43.392589
3502.561302	321911.668170	43.397594
3502.596797	321884.696213	43.402599
3502.604752	321873.501491	43.407604
3502.497277	321839.886402	43.412609
3502.815829	321814.498531	43.417613
3502.662425	321802.870975	43.422618
3502.898368	321763.656399	43.427623
3502.665133	321744.002103	43.432628
3502.690249	321711.587417	43.437633
3502.556176	321678.764992	43.442637
3502.613927	321656.190611	43.447642
3503.084446	321628.184061	43.452647
3502.711289	321605.396864	43.457652
3502.670828	321585.356331	43.462657
3502.730164	321561.356989	43.467661
3502.433236	321526.728076	43.472666
3502.955852	321506.320039	43.477671
3502.805836	321488.789677	43.482676
3502.508552	321462.734213	43.487681
3502.810241	321424.781119	43.492685
3502.691839	321402.539303	43.497690
3502.836050	321361.634115	43.502695
3502.823305	321341.182105	43.507700
3502.667244	321319.149630	43.512705
3502.708497	321279.786821	43.517709
3502.654311	321260.994862	43.522714
3502.547019	321222.647300	43.527719
3502.463648	321203.707213	43.532724
3502.582010	321183.056641	43.537729
3502.387225	321151.133681	43.542733
3502.262243	321135.939821	43.547738
3502.420414	321110.780014	43.552743
3502.508918	321091.329758	43.557748
3502.520699	321061.129997	43.562753
3502.896087	321043.466810	43.567757
3502.316260	321023.535386	43.572762
3502.270228	320988.434500	43.577767
3502.351061	320971.224173	43.582772
3502.444377	320943.021464	43.587777
3502.790739	320920.528987	43.592781
3502.437439	320913.053709	43.597786
3502.534941	320871.239450	43.602791
3502.580276	320852.533588	43.607796
3502.230336	320830.480150	43.612801
3502.276321	320799.995032	43.617805
3502.147324	320783.224336	43.622810
3502.676137	320761.771903	43.627815
3502.137227	320740.358406	43.632820
3502.396209	320726.681990	43.637825
3502.684495	320692.826326	43.642829
3502.273934	320677.600421	43.647834
3502.748815	320651.347981	43.652839
3502.736168	320629.827095	43.657844
3502.293265	320604.175383	43.662849
3502.615806	320572.553104	43.667853
3502.243593	320545.262130	43.672858
3502.221747	320515.067216	43.677863
3502.432396	320507.224257	43.682868
3502.641139	320474.373002	43.687873
3502.407044	320454.692806	43.692877
3502.242350	320445.559865	43.697882
3502.766780	320412.786644	43.702887
3502.623817	320382.025339	43.707892
3502.679741	320350.876886	43.712897
3502.436148	320332.724582	43.717901
3502.309793	320315.037410	43.722906
3502.601716	320292.247783	43.727911
3502.314944	320269.624520	43.732916
3502.540273	320250.763181	43.737921
3502.501080	320222.071794	43.742925
3502.448574	320192.059515	43.747930
3502.725678	320177.947604	43.752935
3502.524291	320159.228951	43.757940
3502.642776	320126.976626	43.762945
3502.634256	320095.456398	43.767949
3502.490360	320070.928139	43.772954
3502.485278	320046.505472	43.777959
3502.669094	320022.460459	43.782964
3502.605148	319988.251993	43.787969
3502.435947	319968.917656	43.792973
3502.501504	319942.957454	43.797978
3502.422816	319922.515031	43.802983
3502.571617	319893.387110	43.807988
3502.253317	319871.811643	43.812993
3502.877203	319849.733369	43.817997
3502.386796	319825.640515	43.823002
3502.173627	319808.653565	43.828007
3502.313307	319787.286645	43.833012
3502.411126	319760.558069	43.838017
3502.794024	319728.747690	43.843021
3502.400463	319711.839657	43.848026
3502.455504	319686.822275	43.853031
3502.782314	319669.369620	43.858036
3502.453825	319641.969504	43.863041
3502.513768	319615.882772	43.868045
3502.560813	319592.011453	43.873050
3502.360890	319570.366532	43.878055
3502.605566	319549.491989	43.883060
3502.485427	319523.738525	43.888065
3502.848532	319492.210912	43.893069
3502.636516	319469.422948	43.898074
3502.707815	319438.093355	43.903079
3502.816090	319406.172825	43.908084
3502.760827	319390.407783	43.913089
3502.624292	319368.625689	43.918093
3502.539787	319335.361253	43.923098
3502.475481	319308.861162	43.928103
3502.486308	319285.809448	43.933108
3502.169679	319261.765564	43.938113
3502.666072	319235.279944	43.943117
3502.408264	319214.992270	43.948122
3502.813392	319187.630359	43.953127
3502.316811	319169.771355	43.958132
3502.212292	319154.700823	43.963137
3502.611997	319121.589851	43.968141
3502.214175	319107.964249	43.973146
3502.366021	319076.240233	43.978151
3502.407045	319060.918044	43.983156
3502.636851	319038.340962	43.988161
3502.596908	319013.770488	43.993165
3502.626501	318995.982185	43.998170
3502.869999	318962.615539	44.003175
3502.671319	318932.370716	44.008180
3502.318807	318909.349902	44.013185
3502.776786	318873.227516	44.018189
3502.523675	318865.380103	44.023194
3502.690832	318838.843709	44.028199
3502.365647	318803.962587	44.033204
3502.650285	318783.513975	44.038209
3502.774267	318748.130397	44.043213
3502.566923	318737.833397	44.048218
3502.946805	318704.190910	44.053223
3502.782312	318678.062217	44.058228
3502.434134	318645.499783	44.063233
3502.506238	318616.052196	44.068237
3502.492739	318604.096699	44.073242
3502.501655	318570.893471	44.078247
3502.611673	318548.589199	44.083252
3502.199059	318527.867337	44.088257
3502.341873	318506.346650	44.093261
3502.287933	318485.314531	44.098266
3502.421475	318463.998804	44.103271
3502.180543	318445.768972	44.108276
3502.528195	318425.055965	44.113281
3502.571586	318391.898121	44.118285
3502.080612	318388.158407	44.123290
3502.639651	318354.284235	44.128295
3502.316357	318327.849295	44.133300
3502.036693	318316.342217	44.138305
3502.262502	318279.924722	44.143309
3502.140081	318278.824539	44.148314
3501.950047	318251.376563	44.153319
3502.572858	318233.190330	44.158324
3502.578529	318209.095714	44.163329
3502.443157	318183.242062	44.168333
3502.547905	318149.641967	44.173338
3502.572397	318136.815388	44.178343
3502.457016	318119.888892	44.183348
3502.330281	318087.240699	44.188353
3502.617324	318054.121014	44.193357
3502.409862	318037.946647	44.198362
3502.001748	318015.213884	44.203367
3502.127611	317991.787394	44.208372
3502.287837	317979.982792	44.213377
3502.359034	317954.096861	44.218381
3502.340122	317932.880930	44.223386
3502.395740	317912.823750	44.228391
3502.428042	317894.856482	44.233396
3502.069188	317872.294077	44.238401
3502.505105	317847.979657	44.243405
3502.635677	317834.347762	44.248410
3502.494653	317811.064478	44.253415
3502.393637	317789.861254	44.258420
3502.109518	317768.050447	44.263425
3502.473385	317737.615493	44.268429
3502.182790	317723.514806	44.273434
3502.007262	317694.130582	44.278439
3502.164215	317685.379537	44.283444
3502.037683	317662.806316	44.288449
3502.196583	317647.541620	44.293453
3502.233056	317636.951993	44.298458
3502.070570	317613.799159	44.303463
3502.112197	317587.663189	44.308468
3501.942450	317574.663131	44.313473
3502.453775	317549.751629	44.318477
3502.254620	317532.685287	44.323482
3502.215848	317513.634885	44.328487
3502.490496	317486.088681	44.333492
3502.494200	317469.423276	44.338497
3502.554470	317439.188019	44.343501
3502.207739	317415.961981	44.348506
3502.376795	317381.257253	44.353511
3502.113799	317368.729617	44.358516
3502.239050	317357.006621	44.363521
3502.234820	317336.118878	44.368525
3502.344439	317318.978962	44.373530
3502.251851	317311.487936	44.378535
3502.527662	317279.870554	44.383540
3502.159990	317253.111119	44.388545
3502.442215	317227.878887	44.393549
3502.386101	317208.576623	44.398554
3502.625735	317186.429597	44.403559
3502.595015	317166.996148	44.408564
3502.360160	317140.979268	44.413569
3501.970283	317120.202321	44.418573
3502.247113	317110.999977	44.423578
3502.252468	317079.678971	44.428583
3502.508180	317059.437610	44.433588
3502.439020	317027.797403	44.438593
3502.509105	317013.742136	44.443597
3502.174357	316990.132365	44.448602
3501.773880	316973.962203	44.453607
3502.120149	316949.025165	44.458612
3502.104752	316929.512899	44.463617
3502.369639	316910.135110	44.468621
3502.549569	316892.984090	44.473626
3502.220685	316862.885329	44.478631
3502.416600	316846.953077	44.483636
3502.103565	316824.459340	44.488641
3502.498552	316799.031217	44.493645
3502.451355	316782.856897	44.498650
3502.323899	316763.005791	44.503655
3502.356351	316736.005679	44.508660
3502.161288	316717.742555	44.513665
3502.650823	316697.108439	44.518669
3502.066249	316687.556632	44.523674
3502.215008	316655.017178	44.528679
3502.626141	316632.232552	44.533684
3502.059049	316622.652566	44.538689
3502.087833	316596.874221	44.543693
3502.046535	316570.648787	44.548698
3502.620257	316556.311458	44.553703
3502.712759	316537.596418	44.558708
3502.440886	316511.381386	44.563713
3502.460533	316479.421651	44.568717
3502.395192	316469.839884	44.573722
3502.527343	316442.569647	44.578727
3502.526160	316411.223748	44.583732
3502.330830	316396.115522	44.588737
3502.421570	316363.457669	44.593741
3501.782395	316348.698373	44.598746
3501.930003	316341.169806	44.603751
3502.085206	316313.208930	44.608756
3502.142922	316307.297287	44.613761
3502.298095	316286.384249	44.618765
3502.254757	316265.985519	44.623770
3502.307725	316247.734494	44.628775
3502.524107	316219.687709	44.633780
3502.140574	316203.692737	44.638785
3502.464965	316177.969926	44.643789
3502.270327	316157.111263	44.648794
3502.205628	316134.018777	44.653799
3502.599322	316104.188720	44.658804
3502.404361	316098.825241	44.663809
3502.343212	316060.771313	44.668813
3502.220894	316051.605422	44.673818
3502.235186	316030.357977	44.678823
3502.565361	316002.675005	44.683828
3502.112423	315988.370039	44.688833
3502.457153	315961.269981	44.693837
3502.438962	315942.979019	44.698842
3502.236828	315923.139163	44.703847
3502.332497	315903.329287	44.708852
3502.382422	315877.191028	44.713857
3502.470990	315849.749109	44.718861
3502.219511	315833.402688	44.723866
3502.193328	315817.122977	44.728871
3502.408628	315793.859526	44.733876
3502.068912	315767.959944	44.738881
3502.299552	315750.698823	44.743885
3501.885552	315729.263447	44.748890
3501.849955	315716.089311	44.753895
3502.005755	315694.794245	44.758900
3501.907245	315686.922211	44.763905
3501.783090	315658.724519	44.768909
3501.908735	315646.212257	44.773914
3502.102579	315640.533782	44.778919
3502.303712	315628.136987	44.783924
3502.262461	315595.702670	44.788929
3502.229126	315569.271863	44.793933
3502.154408	315551.371199	44.798938
3502.287129	315538.679698	44.803943
3502.280606	315518.885556	44.808948
3501.977218	315504.175506	44.813953
3502.479963	315479.823963	44.818957
3502.286414	315469.015180	44.823962
3502.357086	315435.443797	44.828967
3502.501304	315409.366928	44.833972
3502.185627	315398.271805	44.838977
3502.406240	315373.989553	44.843981
3502.076170	315350.632634	44.848986
3502.159196	315327.287753	44.853991
3502.483863	315300.139535	44.858996
3502.131392	315290.144206	44.864001
3502.096759	315266.308721	44.869005
3502.262192	315252.823284	44.874010
3502.500040	315230.751909	44.879015
3502.906781	315197.535160	44.884020
3502.585898	315182.878617	44.889025
3502.433262	315156.618800	44.894029
3502.642576	315135.722251	44.899034
3502.350361	315110.018456	44.904039
3502.585135	315089.728584	44.909044
3502.254336	315061.715344	44.914049
3502.406457	315041.667311	44.919053
3502.543843	315024.013319	44.924058
3502.107875	315004.591112	44.929063
3502.198465	314980.964990	44.934068
3502.217051	314965.975664	44.939073
3502.059846	314934.882022	44.944077
3501.727699	314920.049037	44.949082
3501.993109	314910.975246	44.954087
3502.197759	314884.557897	44.959092
3501.871003	314879.901780	44.964097
3502.463376	314852.711638	44.969101
3502.661098	314827.923771	44.974106
3502.437177	314799.257630	44.979111
3502.306156	314783.044752	44.984116
3502.102725	314765.799917	44.989121
3502.775123	314747.121123	44.994125
3502.017940	314725.586010	44.999130
3502.574083	314696.620306	45.004135
3502.483861	314667.806056	45.009140
3501.974478	314657.224339	45.014145
3501.896047	314631.029007	45.019149
3502.077866	314622.324389	45.024154
3502.134664	314596.413327	45.029159
3502.084186	314581.561845	45.034164
3501.941487	314572.984050	45.039169
3502.135194	314543.998316	45.044173
3502.117024	314530.032347	45.049178
3502.059396	314518.998632	45.054183
3502.023780	314493.636228	45.059188
3501.752768	314483.170044	45.064193
3502.078248	314454.392750	45.069197
3502.188912	314449.134184	45.074202
3501.828812	314428.198699	45.079207
3502.267861	314415.077549	45.084212
3501.937530	314393.119633	45.089217
3502.188925	314367.534384	45.094221
3501.849768	314364.101484	45.099226
3501.732121	314342.975563	45.104231
3502.236309	314322.719762	45.109236
3501.821121	314321.130702	45.114241
3502.069358	314290.507868	45.119245
3502.045089	314290.486431	45.124250
3502.004135	314263.572607	45.129255
3502.116497	314237.449139	45.134260
3501.904197	314223.971291	45.139265
3502.398715	314198.602562	45.144269
3501.954220	314192.743351	45.149274
3501.989678	314171.084632	45.154279
3502.327738	314143.348419	45.159284
3502.247147	314130.206273	45.164289
3501.889255	314117.081830	45.169293
3502.387838	314103.671436	45.174298
3502.328456	314080.424415	45.179303
3502.180504	314050.041188	45.184308
3501.949217	314033.487421	45.189313
3502.010182	314011.468432	45.194317
3502.382529	313995.507728	45.199322
3502.053067	313975.305167	45.204327
3502.546348	313943.677069	45.209332
3501.843585	313939.944491	45.214337
3502.143896	313917.837322	45.219341
3502.411791	313904.666328	45.224346
3502.202167	313878.847211	45.229351
3502.099217	313850.161654	45.234356
3502.103120	313842.705929	45.239361
3502.066448	313816.834419	45.244365
3502.331337	313806.182909	45.249370
3502.136795	313780.768509	45.254375
3502.028068	313766.256613	45.259380
3502.240780	313752.534374	45.264385
3502.270204	313734.209676	45.269389
3502.431572	313708.765297	45.274394
3502.090552	313688.971529	45.279399
3502.460830	313667.540367	45.284404
3502.245162	313659.050092	45.289409
3502.345485	313621.198014	45.294413
3502.331784	313612.269181	45.299418
3502.173658	313590.004190	45.304423
3502.145733	313566.726571	45.309428
3502.293388	313550.368114	45.314433
3502.407057	313520.758068	45.319437
3502.443362	313509.633160	45.324442
3502.303214	313486.347519	45.329447
3502.302139	313447.798616	45.334452
3502.350475	313444.050897	45.339457
3502.270216	313425.005236	45.344461
3502.272234	313399.483705	45.349466
3502.257255	313373.023334	45.354471
3502.521114	313351.328691	45.359476
3502.120315	313334.063143	45.364481
3502.022580	313308.048181	45.369485
3502.173631	313290.136949	45.374490
3501.968090	313277.115785	45.379495
3502.076986	313264.910825	45.384500
3501.746791	313249.669874	45.389505
3502.199447	313224.179903	45.394509
3502.170385	313207.543482	45.399514
3501.938336	313187.274529	45.404519
3502.055153	313176.696807	45.409524
3502.073529	313149.900331	45.414529
3501.920173	313136.438439	45.419533
3501.893793	313132.778657	45.424538
3501.782393	313104.399298	45.429543
3502.011089	313094.516616	45.434548
3501.896587	313081.074106	45.439553
3502.027153	313049.985306	45.444557
3502.102772	313051.933058	45.449562
3502.145081	313034.038649	45.454567
3502.375035	313005.046314	45.459572
3502.219215	312997.386301	45.464577
3502.389940	312973.314113	45.469581
3502.014634	312944.365035	45.474586
3501.976748	312933.149753	45.479591
3502.087371	312911.376969	45.484596
3501.678959	312891.873249	45.489601
3501.735380	312889.421942	45.494605
3501.648172	312870.300800	45.499610
3501.858986	312849.021305	45.504615
3502.214965	312829.983854	45.509620
3501.861077	312818.461482	45.514625
3502.118115	312791.195089	45.519629
3502.264058	312793.106464	45.524634
3502.217825	312771.510697	45.529639
3502.332909	312753.045056	45.534644
3502.421486	312722.089799	45.539649
3502.309063	312705.364390	45.544653
3502.114289	312679.542297	45.549658
3502.171327	312666.251093	45.554663
3502.019347	312636.936281	45.559668
3502.174984	312627.319325	45.564673
3502.241178	312605.324304	45.569677
3501.976235	312593.202788	45.574682
3501.840466	312580.374137	45.579687
3502.192200	312546.248009	45.584692
3502.053894	312542.860054	45.589697
3502.126139	312518.370383	45.594701
3502.064719	312495.708137	45.599706
3501.641286	312491.397614	45.604711
3501.940267	312457.101511	45.609716
3501.860417	312453.831681	45.614721
3501.905956	312439.956953	45.619725
3502.113806	312419.364757	45.624730
3502.147882	312420.555631	45.629735
3501.772264	312385.244843	45.634740
3501.803938	312378.140802	45.639745
3501.706931	312367.265379	45.644749
3501.788972	312350.255125	45.649754
3501.798992	312346.284269	45.654759
3502.243569	312329.090364	45.659764
3501.849788	312315.258517	45.664769
3501.786599	312296.133404	45.669773
3501.876824	312279.350863	45.674778
3501.643296	312263.789200	45.679783
3501.870982	312252.430646	45.684788
3501.751197	312248.683547	45.689793
3501.829440	312227.042714	45.694797
3501.789567	312205.827384	45.699802
3501.671283	312201.698361	45.704807
3501.804334	312190.965217	45.709812
3502.075214	312168.327441	45.714817
3501.894286	312155.861943	45.719821
3501.905682	312141.279958	45.724826
3502.092108	312112.879100	45.729831
3502.192313	312044.694342	45.734836
3501.498073	311938.337029	45.739841
3501.487647	311785.739503	45.744845
3500.827293	311592.401653	45.749850
3500.600276	311350.724116	45.754855
3499.928603	311079.596766	45.759860
3498.793021	310756.400130	45.764865
3497.839084	310404.418254	45.769869
3496.854543	310007.982789	45.774874
3495.693305	309582.434582	45.779879
3494.904850	309113.487731	45.784884
3493.062137	308620.423380	45.789889
3491.576215	308074.036051	45.794893
3490.475158	307524.707157	45.799898
3488.514604	306928.578901	45.804903
3486.928462	306301.515872	45.809908
3485.061553	305659.651909	45.814913
3483.297516	304970.147862	45.819917
3481.551773	304257.192423	45.824922
3479.231978	303523.091057	45.829927
3477.272429	302756.677477	45.834932
3475.016100	301978.718809	45.839937
3472.611839	301173.589830	45.844941
3470.808737	300340.689300	45.849946
3467.856953	299489.451150	45.854951
3465.478590	298610.901931	45.859956
3462.635877	297725.946146	45.864961
3460.027896	296823.046334	45.869965
3457.455463	295884.058855	45.874970
3454.678021	294946.539010	45.879975
3452.349313	293990.887156	45.884980
3449.283472	293024.389105	45.889985
3446.266119	292026.507092	45.894989
3443.425280	291027.563206	45.899994
3440.590851	290019.387220	45.904999
3437.529586	288995.269240	45.910004
3434.371879	287956.359495	45.915009
3431.277600	286901.588918	45.920013
3428.180176	285855.839686	45.925018
3424.969374	284793.391413	45.930023
3422.029295	283719.530150	45.935028
3418.957651	282621.690623	45.940033
3415.688235	281531.910242	45.945037
3412.199944	280427.813853	45.950042
3408.935967	279320.432794	45.955047
3405.685942	278204.478746	45.960052
3402.225349	277089.916350	45.965057
3398.691966	275965.699861	45.970061
3395.468900	274836.378148	45.975066
3391.833000	273708.862215	45.980071
3388.742453	272581.857577	45.985076
3385.135511	271440.354144	45.990081
3381.627465	270297.598521	45.995085
3378.249273	269142.280549	46.000090
3374.346949	267995.000033	46.005095
3370.925343	266840.399369	46.010100
3367.459627	265684.264309	46.015105
3363.853618	264533.943886	46.020109
3360.450763	263365.830415	46.025114
3356.738494	262213.642638	46.030119
3353.191813	261048.098946	46.035124
3349.467937	259903.732862	46.040129
3346.008829	258737.006690	46.045133
3342.367392	257571.189202	46.050138
3338.593731	256414.294847	46.055143
3334.828673	255249.087069	46.060148
3331.293260	254095.955831	46.065153
3327.402478	252926.852067	46.070157
3323.975935	251770.069373	46.075162
3320.119425	250607.793223	46.080167
3316.678114	249444.196339	46.085172
3312.858674	248290.124344	46.090177
3309.128190	247127.575896	46.095181
3305.616375	245974.562233	46.100186
3301.532610	244810.450565	46.105191
3298.177888	243662.009322	46.110196
3294.471788	242517.640946	46.115201
3290.824885	241357.111070	46.120205
3287.208578	240204.466492	46.125210
3283.060768	239058.521733	46.130215
3279.705838	237903.382482	46.135220
3275.794724	236763.326867	46.140225
3271.609718	235627.767398	46.145229
3268.304228	234488.476835	46.150234
3264.746827	233351.565829	46.155239
3261.217611	232208.153447	46.160244
3257.219174	231081.341380	46.165249
3253.463167	229939.998055	46.170253
3249.647508	228814.326131	46.175258
3245.715098	227688.569542	46.180263
3242.369822	226557.474351	46.185268
3238.690316	225439.089041	46.190273
3234.758051	224323.137244	46.195277
3231.165176	223194.907918	46.200282
3227.155755	222073.136929	46.205287
3223.838347	220963.790126	46.210292
3219.761356	219855.403436	46.215297
3215.768838	218746.572396	46.220301
3212.120787	217633.563897	46.225306
3208.562564	216531.164365	46.230311
3204.571896	215438.334705	46.235316
3200.571763	214341.943912	46.240321
3196.968320	213249.365964	46.245325
3193.467329	212156.953997	46.250330
3189.704599	211074.570338	46.255335
3186.022566	209986.167805	46.260340
3182.343339	208912.362672	46.265345
3178.434704	207831.925349	46.270349
3174.890671	206749.628177	46.275354
3170.828637	205674.649915	46.280359
3166.772640	204587.782980	46.285364
3163.126865	203532.463531	46.290369
3159.327907	202468.056645	46.295373
3155.941646	201405.782170	46.300378
3152.046851	200362.490110	46.305383
3148.488034	199307.361352	46.310388
3144.522978	198261.954898	46.315393
3140.732143	197213.498163	46.320397
3137.070090	196167.422897	46.325402
3133.363562	195133.739021	46.330407
3129.576247	194090.933442	46.335412
3125.919553	193051.171849	46.340417
3122.071013	192020.438090	46.345421
3118.389384	190996.868343	46.350426
3114.693664	189985.074568	46.355431
3110.610729	188950.329775	46.360436
3106.525331	187938.131196	46.365441
3103.070026	186929.740096	46.370445
3099.430083	185923.831944	46.375450
3095.763050	184918.217972	46.380455
3091.911894	183927.157024	46.385460
3087.791442	182939.738371	46.390465
3084.143714	181939.575749	46.395469
3080.495811	180950.372894	46.400474
3076.338515	179966.581711	46.405479
3072.988066	178995.432412	46.410484
3068.914876	178021.554634	46.415489
3065.240824	177048.682487	46.420493
3061.717023	176076.969466	46.425498
3057.439478	175118.446761	46.430503
3053.931627	174170.916573	46.435508
3050.091619	173222.991123	46.440513
3045.951089	172276.791638	46.445517
3042.731926	171333.515678	46.450522
3038.380329	170408.987798	46.455527
3034.591724	169471.323318	46.460532
3030.787524	168551.940130	46.465537
3026.637475	167626.538008	46.470541
3023.160864	166712.715872	46.475546
3019.141400	165813.997710	46.480551
3015.573795	164904.732581	46.485556
3011.435371	164018.632825	46.490561
3007.754627	163123.385624	46.495565
3003.618832	162234.127441	46.500570
2999.899026	161360.701472	46.505575
2996.313840	160497.818020	46.510580
2992.191259	159632.306366	46.515585
2988.228711	158774.443931	46.520589
2984.292128	157914.476790	46.525594
2980.101354	157081.364961	46.530599
2976.536875	156232.729486	46.535604
2972.402849	155407.548640	46.540609
2968.310230	154577.256979	46.545613
2964.578638	153761.951116	46.550618
2960.720364	152965.867931	46.555623
2957.152356	152174.701337	46.560628
2953.448577	151373.030098	46.565633
2949.275571	150576.330278	46.570637
2945.237068	149790.374314	46.575642
2941.420429	149026.791972	46.580647
2937.470312	148258.609403	46.585652
2933.300886	147505.105923	46.590657
2929.261044	146753.870915	46.595661
2924.978627	146009.008732	46.600666
2921.262123	145299.392406	46.605671
2917.231342	144572.351772	46.610676
2913.206933	143865.831903	46.615681
2909.064199	143169.735910	46.620685
2905.441243	142467.830444	46.625690
2901.321346	141782.998316	46.630695
2897.077661	141110.829424	46.635700
2893.096689	140454.991069	46.640705
2889.342884	139796.861666	46.645709
2885.599664	139139.477676	46.650714
2881.186272	138507.054544	46.655719
2877.572330	137880.482425	46.660724
2873.519084	137249.865099	46.665729
2869.458482	136634.129762	46.670733
2865.458550	136025.199543	46.675738
2861.931928	135447.448641	46.680743
2858.326918	134756.736351	46.685748
2854.353714	134167.939965	46.690753
2850.791457	133583.527157	46.695757
2847.090812	133007.908472	46.700762
2843.072977	132437.460522	46.705767
2839.197943	131862.736338	46.710772
2835.543904	131307.511552	46.715777
2831.669306	130754.846893	46.720781
2827.955987	130189.647478	46.725786
2823.971447	129653.499689	46.730791
2820.812677	129107.512113	46.735796
2817.153617	128563.899033	46.740801
2813.329634	128026.500423	46.745805
2809.855948	127490.148108	46.750810
2806.074428	126962.105484	46.755815
2802.905279	126431.379620	46.760820
2799.309346	125901.439306	46.765825
2795.485529	125379.210801	46.770829
2792.359769	124847.341388	46.775834
2788.559729	124333.529724	46.780839
2785.153012	123800.763978	46.785844
2781.933884	123277.578365	46.790849
2778.141330	122748.333366	46.795853
2774.611703	122227.677229	46.800858
2770.694100	121717.351521	46.805863
2767.079082	121193.721032	46.810868
2763.884134	120673.249700	46.815873
2760.168514	120154.430599	46.820877
2756.806856	119642.188949	46.825882
2752.817930	119123.833234	46.830887
2749.704170	118607.650080	46.835892
2746.246590	118100.556141	46.840897
2742.897707	117593.706415	46.845901
2739.288207	117074.874619	46.850906
2735.234431	116566.876847	46.855911
2731.923674	116047.669500	46.860916
2728.314539	115545.046136	46.865921
2724.685227	115035.935172	46.870925
2721.586308	114524.917728	46.875930
2718.006338	114016.550728	46.880935
2714.414174	113508.345305	46.885940
2710.421623	113001.595222	46.890945
2707.079220	112509.131229	46.895949
2703.733127	111998.938023	46.900954
2699.568852	111495.083943	46.905959
2695.977895	110988.630407	46.910964
2692.193313	110499.009202	46.915969
2689.120390	110004.033307	46.920973
2685.752144	109509.199337	46.925978
2681.628348	109031.271491	46.930983
2678.095652	108526.382693	46.935988
2674.151292	108048.249748	46.940993
2670.648623	107569.686018	46.945997
2666.903824	107084.111145	46.951002
2663.112618	106611.478889	46.956007
2659.552529	106141.181689	46.961012
2655.749894	105671.691467	46.966017
2651.580509	105212.281793	46.971021
2648.211985	104752.359687	46.976026
2644.053283	104297.994672	46.981031
2640.954677	103843.750506	46.986036
2637.136083	103404.293288	46.991041
2633.170264	102963.771651	46.996045
2629.954640	102516.084609	47.001050
2625.630137	102084.528119	47.006055
2622.094844	101653.833193	47.011060
2618.523382	101231.258769	47.016065
2614.584496	100805.442349	47.021069
2610.972682	100383.851176	47.026074
2607.134878	99968.325133	47.031079
2603.391823	99554.734277	47.036084
2600.036145	99141.215549	47.041089
2596.492406	98746.592129	47.046093
2593.003699	98335.061757	47.051098
2589.064246	97929.656354	47.056103
2585.745756	97529.192211	47.061108
2582.117372	97130.497038	47.066113
2578.611416	96739.196947	47.071117
2575.693928	96336.016734	47.076122
2572.055035	95937.846644	47.081127
2568.481166	95532.338939	47.086132
2565.276388	95130.299163	47.091137
2561.303754	94737.597210	47.096141
2557.962100	94320.073060	47.101146
2554.461323	93929.709667	47.106151
2551.193574	93521.944127	47.111156
2547.689352	93123.064942	47.116161
2544.014176	92722.006554	47.121165
2540.858232	92324.799025	47.126170
2537.240305	91925.101844	47.131175
2533.912027	91516.419530	47.136180
2530.356711	91103.877253	47.141185
2526.883008	90714.236990	47.146189
2523.338847	90289.201356	47.151194
2520.060893	89895.068789	47.156199
2516.912736	89479.588572	47.161204
2513.280939	89078.965785	47.166209
2509.570050	88667.192826	47.171213
2505.980917	88244.086459	47.176218
2502.588408	87845.005858	47.181223
2499.027159	87428.958057	47.186228
2495.610840	87008.218347	47.191233
2492.059620	86607.997757	47.196237
2488.942594	86191.123471	47.201242
2485.218075	85785.808680	47.206247
2481.685135	85369.392041	47.211252
2478.311157	84948.866104	47.216257
2474.525523	84539.322605	47.221261
2471.245725	84134.012625	47.226266
2467.816357	83722.100659	47.231271
2464.293752	83304.759611	47.236276
2461.174959	82892.315886	47.241281
2457.020133	82467.654445	47.246285
2453.570536	82052.390955	47.251290
2450.190435	81642.483057	47.256295
2446.676763	81220.077804	47.261300
2443.599684	80796.886966	47.266305
2439.705070	80380.764806	47.271309
2436.733917	79960.529614	47.276314
2432.764121	79542.145440	47.281319
2429.541623	79129.633445	47.286324
2425.957659	78702.616047	47.291329
2422.717921	78277.901302	47.296333
2419.201216	77858.214777	47.301338
2415.291934	77437.655958	47.306343
2411.933796	77012.953836	47.311348
2408.691601	76593.625008	47.316353
2404.900916	76174.299111	47.321357
2401.265208	75737.024011	47.326362
2398.142533	75321.353700	47.331367
2394.887204	74887.931821	47.336372
2391.298800	74453.705250	47.341377
2387.430901	74032.278613	47.346381
2384.399228	73610.499917	47.351386
2380.861990	73188.108174	47.356391
2377.103756	72751.865931	47.361396
2373.523116	72319.272896	47.366401
2370.052244	71888.739570	47.371405
2366.722352	71456.020091	47.376410
2363.366721	71032.339432	47.381415
2359.669868	70605.150885	47.386420
2356.216009	70174.960470	47.391425
2352.692327	69740.382328	47.396429
2349.035248	69305.260884	47.401434
2345.297654	68886.289701	47.406439
2342.003588	68448.771045	47.411444
2338.806608	68022.124921	47.416449
2335.082137	67588.591807	47.421453
2331.732946	67156.607234	47.426458
2328.329319	66723.337196	47.431463
2324.840159	66289.332496	47.436468
2321.544644	65858.021725	47.441473
2317.772923	65415.462656	47.446477
2314.060549	64985.462996	47.451482
2310.727342	64550.029429	47.456487
2307.111432	64121.851104	47.461492
2303.759549	63676.261573	47.466497
2299.945912	63243.565735	47.471501
2296.810590	62804.399922	47.476506
2293.255090	62365.313607	47.481511
2289.560215	61928.173350	47.486516
2286.435833	61491.777049	47.491521
2282.220708	61062.342195	47.496525
2279.097822	60623.194165	47.501530
2275.705054	60190.042077	47.506535
2272.201533	59745.003922	47.511540
2269.088773	59303.295300	47.516545
2265.422298	58878.858204	47.521549
2261.959608	58426.318381	47.526554
2258.250645	57990.779968	47.531559
2254.598441	57545.158100	47.536564
2251.050153	57101.895022	47.541569
2247.772318	56670.748606	47.546573
2244.301473	56230.820684	47.551578
2240.697147	55786.315385	47.556583
2237.573376	55352.472302	47.561588
2233.977467	54906.142217	47.566593
2230.339455	54451.287597	47.571597
2226.922297	54003.557315	47.576602
2223.099920	53563.181648	47.581607
2219.617996	53116.366508	47.586612
2216.336718	52678.435460	47.591617
2212.777324	52231.903019	47.596621
2209.481970	51792.423877	47.601626
2205.812823	51346.103130	47.606631
2201.976452	50904.618946	47.611636
2198.778898	50454.309090	47.616641
2195.318952	50014.756088	47.621645
2192.285092	49568.757744	47.626650
2188.330236	49119.657492	47.631655
2185.059958	48672.958566	47.636660
2181.302035	48224.650782	47.641665
2177.978808	47774.330674	47.646669
2174.398193	47319.613528	47.651674
2170.805693	46881.860255	47.656679
2167.285217	46425.566147	47.661684
2164.028431	45979.070370	47.666689
2160.257761	45530.190094	47.671693
2156.728135	45087.382073	47.676698
2153.046288	44631.618821	47.681703
2149.737310	44193.265039	47.686708
2145.982250	43741.057279	47.691713
2142.325510	43293.618397	47.696717
2139.333038	42843.757979	47.701722
2135.444491	42396.519167	47.706727
2132.099770	41951.760171	47.711732
2128.793820	41511.987966	47.716737
2125.025822	41064.795535	47.721741
2121.903294	40611.900460	47.726746
2118.303009	40169.144944	47.731751
2114.716535	39710.615458	47.736756
2111.369524	39262.063055	47.741761
2107.951685	38816.073288	47.746765
2104.698860	38351.992188	47.751770
2100.541155	37899.796680	47.756775
2097.306542	37451.587740	47.761780
2093.665479	36993.314675	47.766785
2089.925574	36557.241662	47.771789
2086.742949	36096.051131	47.776794
2082.919727	35652.130028	47.781799
2079.270107	35200.685937	47.786804
2076.120893	34748.482661	47.791809
2072.503759	34300.836948	47.796813
2069.302420	33848.179330	47.801818
2065.823597	33394.300627	47.806823
2062.383206	32946.935107	47.811828
2058.846763	32495.822938	47.816833
2055.409912	32042.930388	47.821837
2051.721920	31586.480557	47.826842
2048.373946	31136.021291	47.831847
2044.705360	30677.883586	47.836852
2041.252245	30232.023363	47.841857
2037.591696	29775.431729	47.846861
2034.316841	29320.564585	47.851866
2030.683375	28861.663306	47.856871
2027.334866	28407.385523	47.861876
2023.447538	27954.481703	47.866881
2019.711618	27504.967104	47.871885
2016.384967	27048.111874	47.876890
2013.045972	26602.192565	47.881895
2009.648280	26152.414499	47.886900
2006.005902	25708.817759	47.891905
2002.401606	25249.448601	47.896909
1998.670445	24796.014550	47.901914
1995.236780	24347.182073	47.906919
1991.791233	23895.801999	47.911924
1988.167980	23442.381813	47.916929
1984.706061	22987.597452	47.921933
1981.270338	22539.490152	47.926938
1977.883358	22093.273169	47.931943
1974.378219	21642.960746	47.936948
1970.593685	21192.068619	47.941953
1967.311718	20751.598376	47.946957
1963.616002	20297.133987	47.951962
1960.078945	19856.153444	47.956967
1956.315397	19401.562032	47.961972
1953.010908	18970.667958	47.966977
1949.298536	18518.008323	47.971981
1945.639602	18074.749888	47.976986
1942.089759	17636.614656	47.981991
1938.986195	17192.191125	47.986996
1935.619568	16751.856116	47.992001
1931.155873	16311.967894	47.997005
1928.329266	15861.677106	48.002010
1924.608710	15420.724715	48.007015
1921.299293	14992.136579	48.012020
1917.586603	14546.991973	48.017025
1913.631272	14115.452845	48.022029
1910.288442	13676.957856	48.027034
1906.831977	13242.726752	48.032039
1902.853842	12815.219356	48.037044
1899.276972	12378.595403	48.042049
1895.507527	11960.315942	48.047053
1892.075243	11531.983391	48.052058
1888.400676	11116.579207	48.057063
1884.737242	10692.910918	48.062068
1881.418335	10275.608688	48.067073
1877.354044	9859.463711	48.072077
1873.269410	9449.956242	48.077082
1869.952774	9048.438179	48.082087
1865.996225	8648.171030	48.087092
1861.819829	8243.347811	48.092097
1858.064650	7870.786366	48.097101
1854.523732	7493.457921	48.102106
1850.525781	7124.655553	48.107111
1846.206676	6767.272473	48.112116
1842.517459	6403.291458	48.117121
1838.349929	6057.978712	48.122125
1834.652382	5702.295094	48.127130
1830.650527	5371.571433	48.132135
1826.827791	5035.297376	48.137140
1823.141377	4714.954334	48.142145
1819.172656	4398.983538	48.147149
1815.304046	4086.920205	48.152154
1811.411729	3785.181749	48.157159
1807.638730	3492.226532	48.162164
1804.094478	3205.695552	48.167169
1799.590300	2926.928447	48.172173
1795.748084	2662.877241	48.177178
1791.584241	2403.550207	48.182183
1787.608036	2167.042334	48.187188
1783.899471	1921.491083	48.192193
1779.299524	1703.988346	48.197197
1775.682802	1469.031557	48.202202
1771.520285	1267.206731	48.207207
1767.670530	1061.750832	48.212212
1763.824794	854.464809	48.217217
1759.884745	675.334810	48.222221
1756.330929	491.907036	48.227226
1752.754843	323.271984	48.232231
1748.554798	157.627289	48.237236
1743.709606	25.736777	48.242241
1732.144134	92.696707	48.247245
1725.506290	90.876394	48.252250
1721.007475	93.626909	48.257255
1717.745169	96.836697	48.262260
1715.976150	80.281333	48.267265
1713.934549	92.105727	48.272269
1711.570571	86.054727	48.277274
1707.976910	81.384673	48.282279
1705.165145	88.513772	48.287284
1702.033554	86.147745	48.292289
1698.453887	98.395025	48.297293
1695.114678	84.289153	48.302298
1691.627950	87.473761	48.307303
1688.194122	91.871327	48.312308
1685.281466	77.132770	48.317313
1681.337835	81.729902	48.322317
1678.103866	87.921820	48.327322
1674.506934	90.073231	48.332327
1671.057329	83.741959	48.337332
1668.224619	81.386364	48.342337
1664.468240	87.305257	48.347341
1661.417206	85.581583	48.352346
1657.705234	74.327298	48.357351
1654.184345	86.495819	48.362356
1650.935977	87.270551	48.367361
1647.638655	83.503493	48.372365
1644.285124	78.027294	48.377370
1640.851169	83.794764	48.382375
1637.009353	90.223658	48.387380
1633.771073	79.142417	48.392385
1630.563728	89.797344	48.397389
1626.880817	85.982737	48.402394
1623.430321	76.943482	48.407399
1620.019039	90.398392	48.412404
1616.536710	89.010765	48.417409
1612.915095	95.914746	48.422413
1609.581453	90.707530	48.427418
1605.957940	79.585014	48.432423
1602.897881	82.042004	48.437428
1599.612906	80.183909	48.442433
1595.732080	93.468297	48.447437
1591.956675	82.499135	48.452442
1588.652522	86.465241	48.457447
1585.361678	84.250561	48.462452
1582.140024	86.071490	48.467457
1578.266851	88.158338	48.472461
1574.788555	80.524937	48.477466
1571.708876	75.553446	48.482471
1567.935317	87.713838	48.487476
1564.501860	78.551720	48.492481
1560.802476	84.056791	48.497485
1557.584464	85.408927	48.502490
1554.046632	76.433898	48.507495
1550.476760	76.300076	48.512500
1547.124839	78.071681	48.517505
1543.609727	86.724430	48.522509
1540.424007	74.189217	48.527514
1537.108886	74.474482	48.532519
1533.198397	75.016928	48.537524
1529.537633	80.503334	48.542529
1525.902931	89.782129	48.547533
1523.123718	88.582463	48.552538
1519.282886	87.851751	48.557543
1515.578763	89.301697	48.562548
1512.485474	89.514473	48.567553
1508.506825	91.522833	48.572557
1505.246132	88.610618	48.577562
1502.017982	77.356986	48.582567
1498.017853	82.943671	48.587572
1494.837911	74.950642	48.592577
1491.454248	79.299280	48.597581
1487.669437	86.162225	48.602586
1484.352236	79.747101	48.607591
1480.707348	88.056226	48.612596
1477.263750	83.894348	48.617601
1473.822587	78.001549	48.622605
1470.539680	86.447317	48.627610
1467.035322	80.494753	48.632615
1463.110198	88.297012	48.637620
1459.859313	82.320814	48.642625
1456.507997	86.661258	48.647629
1453.161068	84.066187	48.652634
1449.389462	84.931867	48.657639
1446.111158	95.319436	48.662644
1442.494659	83.635883	48.667649
1438.773235	89.134902	48.672653
1435.222253	79.810768	48.677658
1432.325610	81.179330	48.682663
1428.495103	86.059424	48.687668
1425.553934	81.139156	48.692673
1421.460088	85.620485	48.697677
1417.665439	81.424673	48.702682
1414.517573	79.165613	48.707687
1410.547357	80.587384	48.712692
1407.723235	75.044636	48.717697
1404.225885	84.425436	48.722701
1400.481668	86.315061	48.727706
1396.863592	85.429470	48.732711
1393.223579	81.867642	48.737716
1390.253159	84.592262	48.742721
1386.439208	86.002369	48.747725
1382.711047	79.328529	48.752730
1379.870217	84.624048	48.757735
1375.942978	84.821111	48.762740
1372.766650	77.662754	48.767745
1368.883462	76.884870	48.772749
1365.196563	81.223768	48.777754
1362.043140	78.709319	48.782759
1358.253153	82.058208	48.787764
1355.331730	79.396920	48.792769
1351.621986	81.945559	48.797773
1348.080005	79.213186	48.802778
1344.628112	74.872289	48.807783
1341.104516	82.273538	48.812788
1337.786088	79.544334	48.817793
1333.597854	81.411329	48.822797
1330.298448	78.900625	48.827802
1327.026617	71.893182	48.832807
1323.473286	71.101925	48.837812
1320.657828	73.505041	48.842817
1316.889977	79.460536	48.847821
1313.167279	76.031811	48.852826
1310.065054	70.772805	48.857831
1306.038974	83.386944	48.862836
1302.670242	74.828557	48.867841
1298.856160	71.091363	48.872845
1295.552427	74.456316	48.877850
1292.090479	77.295414	48.882855
1288.468623	76.960908	48.887860
1285.140903	73.344160	48.892865
1281.475439	77.537361	48.897869
1278.331177	78.694546	48.902874
1274.705024	74.912283	48.907879
1270.883900	86.725746	48.912884
1267.753317	69.053659	48.917889
1264.030480	81.066951	48.922893
1260.513957	85.274936	48.927898
1257.096712	78.056022	48.932903
1253.552586	73.356179	48.937908
1250.204181	73.368248	48.942913
1246.533397	73.031871	48.947917
1242.670801	74.686841	48.952922
1239.709654	75.714288	48.957927
1235.949993	75.154469	48.962932
1232.725245	71.119912	48.967937
1229.392457	78.576884	48.972941
1225.377520	78.094766	48.977946
1222.166477	78.503063	48.982951
1218.465207	85.732662	48.987956
1214.965007	72.237248	48.992961
1211.458304	79.639036	48.997965
1208.144462	74.934991	49.002970
1204.628962	79.437043	49.007975
1200.525570	80.670763	49.012980
1197.511481	70.924593	49.017985
1193.966360	68.974163	49.022989
1190.797835	74.700337	49.027994
1187.634879	78.454666	49.032999
1183.565426	81.135240	49.038004
1179.932098	73.026179	49.043009
1176.380362	72.392875	49.048013
1172.908469	69.339575	49.053018
1169.544375	69.683118	49.058023
1166.141373	74.563122	49.063028
1162.823210	76.512999	49.068033
1159.353871	78.739502	49.073037
1155.333648	76.891502	49.078042
1152.295544	72.906995	49.083047
1148.621767	77.737402	49.088052
1144.926588	70.685157	49.093057
1141.410025	68.255734	49.098061
1137.907933	72.831631	49.103066
1134.543039	71.606112	49.108071
1131.034139	69.744963	49.113076
1127.687439	65.593365	49.118081
1123.817266	67.879100	49.123085
1120.343722	75.089071	49.128090
1117.153753	70.732747	49.133095
1113.643799	74.598040	49.138100
1110.188290	66.799830	49.143105
1106.801348	60.519012	49.148109
1102.770501	73.782446	49.153114
1099.406335	68.374422	49.158119
1095.504525	79.333592	49.163124
1092.452730	75.161402	49.168129
1089.203069	65.913822	49.173133
1085.572239	73.420354	49.178138
1082.086989	71.682076	49.183143
1078.287315	68.894943	49.188148
1075.046911	70.927633	49.193153
1071.506163	74.826196	49.198157
1068.044659	70.948735	49.203162
1064.659362	64.503154	49.208167
1061.088402	63.600780	49.213172
1057.916029	66.461259	49.218177
1054.270336	71.151261	49.223181
1049.961827	69.265896	49.228186
1046.616888	63.816925	49.233191
1042.960835	62.450082	49.238196
1040.008298	63.675518	49.243201
1036.649078	62.955318	49.248205
1032.875611	69.414729	49.253210
1029.866263	63.328240	49.258215
1026.078229	73.288956	49.263220
1022.405348	57.998194	49.268225
1019.279854	65.365956	49.273229
1015.389611	63.583164	49.278234
1011.672217	66.958746	49.283239
1008.453769	68.174957	49.288244
1005.175774	62.196729	49.293249
1001.841238	65.449441	49.298253
997.891941	63.391113	49.303258
994.432621	69.725698	49.308263
990.638323	72.825358	49.313268
987.418360	61.776203	49.318273
984.383276	70.550389	49.323277
980.509038	66.126597	49.328282
977.091357	62.232839	49.333287
973.005471	59.578859	49.338292
969.903738	63.636875	49.343297
966.116448	61.831737	49.348301
962.882351	59.127422	49.353306
959.702278	66.646048	49.358311
956.096097	68.707214	49.363316
952.538699	60.444016	49.368321
949.004518	67.106624	49.373325
945.237205	59.331674	49.378330
941.661994	63.355830	49.383335
938.333233	68.784264	49.388340
934.916459	67.946487	49.393345
931.557973	68.365111	49.398349
927.795004	59.017139	49.403354
924.226040	57.630428	49.408359
920.766207	63.183666	49.413364
917.546083	65.887078	49.418369
914.118516	71.811774	49.423373
910.300341	62.716000	49.428378
906.963749	67.588846	49.433383
903.122158	64.634262	49.438388
899.855299	60.913186	49.443393
896.312768	67.140509	49.448397
892.732241	61.965512	49.453402
889.487638	59.332444	49.458407
885.644240	59.794920	49.463412
882.396869	59.044673	49.468417
878.927039	53.687938	49.473421
874.947876	63.982121	49.478426
871.957914	52.688389	49.483431
868.278019	62.183030	49.488436
865.111005	62.926187	49.493441
861.759603	58.386230	49.498445
857.754148	67.194415	49.503450
854.527739	55.159227	49.508455
850.587971	58.310018	49.513460
847.371410	50.082371	49.518465
843.995246	50.399356	49.523469
840.004271	61.982994	49.528474
836.953325	49.132744	49.533479
833.183424	63.633680	49.538484
829.625689	59.502325	49.543489
826.424009	66.141654	49.548493
822.979562	64.520443	49.553498
819.474310	53.610649	49.558503
815.584620	58.816366	49.563508
812.412163	59.168080	49.568513
808.858929	56.247717	49.573517
804.915083	58.994197	49.578522
801.813807	58.664132	49.583527
798.316472	64.976172	49.588532
794.557131	74.018128	49.593537
791.169294	68.851115	49.598541
787.952246	71.680607	49.603546
784.880417	69.425607	49.608551
781.172881	72.306143	49.613556
777.212804	58.183258	49.618561
773.537868	62.067933	49.623565
769.917280	65.105773	49.628570
766.703952	55.140777	49.633575
763.084569	66.356536	49.638580
759.734336	58.560988	49.643585
756.648225	59.880007	49.648589
752.542522	66.125407	49.653594
748.795771	58.154312	49.658599
745.689817	59.428966	49.663604
742.576477	61.786747	49.668609
738.740129	63.649654	49.673613
734.970793	66.470214	49.678618
731.532315	62.497475	49.683623
728.383050	64.772268	49.688628
725.163266	56.988057	49.693633
721.176127	70.766699	49.698637
717.733594	68.914256	49.703642
714.143907	64.708800	49.708647
710.749460	55.657839	49.713652
707.453492	69.003027	49.718657
703.954097	65.912949	49.723661
699.911414	69.728333	49.728666
697.009007	63.391137	49.733671
693.016241	61.111838	49.738676
689.483666	52.531628	49.743681
686.085906	53.956115	49.748685
682.162982	55.841996	49.753690
678.986883	53.040110	49.758695
675.429674	61.490630	49.763700
672.254283	57.486438	49.768705
669.082984	51.428386	49.773709
665.168387	62.734393	49.778714
662.136819	58.638211	49.783719
658.120724	68.235821	49.788724
654.642828	63.054379	49.793729
651.173654	59.927969	49.798733
647.706887	56.845478	49.803738
644.673574	55.046398	49.808743
640.834656	50.718409	49.813748
637.327740	59.398377	49.818753
633.606183	54.428875	49.823757
629.892063	64.862140	49.828762
626.804596	45.759878	49.833767
623.157040	58.077816	49.838772
619.318233	51.339095	49.843777
616.024165	57.856777	49.848781
612.649112	52.953558	49.853786
609.306577	53.300135	49.858791
605.352365	57.484559	49.863796
602.168937	57.141997	49.868801
598.673648	65.016587	49.873805
594.981429	63.937004	49.878810
591.831520	65.332408	49.883815
588.083717	63.752128	49.888820
584.131914	66.971261	49.893825
581.142254	55.554157	49.898829
577.160561	62.438311	49.903834
573.897693	56.584349	49.908839
570.441950	62.111667	49.913844
567.001496	63.004990	49.918849
563.567912	49.847382	49.923853
560.116351	55.114626	49.928858
557.158290	62.136811	49.933863
553.139806	59.630592	49.938868
549.410071	58.661258	49.943873
545.915235	61.878857	49.948877
542.225609	69.616031	49.953882
538.893975	66.012657	49.958887
535.381527	66.521732	49.963892
532.160073	65.707384	49.968897
528.725950	62.145277	49.973901
524.943150	61.924506	49.978906
521.639834	63.369110	49.983911
517.858539	61.699144	49.988916
514.534982	59.970575	49.993921
511.435918	57.741998	49.998925
507.647234	63.922250	50.003930
504.501012	62.422331	50.008935
500.348914	67.229182	50.013940
496.860450	59.423568	50.018945
493.170413	62.484904	50.023949
489.680007	63.117101	50.028954
486.414412	53.536777	50.033959
482.907182	61.381595	50.038964
479.466535	63.530935	50.043969
476.245091	58.913862	50.048973
472.502632	61.749250	50.053978
469.004801	60.319894	50.058983
465.520520	64.178083	50.063988
462.027127	60.571432	50.068993
458.357780	61.832587	50.073997
454.792107	57.420964	50.079002
451.552371	51.686807	50.084007
447.865092	56.936976	50.089012
444.258203	61.560880	50.094017
440.694831	54.776151	50.099021
437.096614	61.027994	50.104026
433.946732	51.660615	50.109031
430.682063	60.774268	50.114036
427.319923	66.865978	50.119041
423.380495	56.444632	50.124045
419.700952	58.450841	50.129050
416.219542	56.576023	50.134055
413.189521	48.142254	50.139060
409.600530	52.424861	50.144065
406.286331	51.944499	50.149069
402.296668	44.128356	50.154074
398.837128	46.002243	50.159079
395.328033	49.272694	50.164084
391.793684	57.801926	50.169089
389.039733	51.653640	50.174093
384.760369	58.014693	50.179098
381.325366	48.625278	50.184103
377.574714	46.270379	50.189108
374.201398	54.369592	50.194113
371.066752	54.158666	50.199117
367.448183	52.903141	50.204122
364.163437	49.536102	50.209127
360.095359	50.403778	50.214132
356.996220	42.616680	50.219137
353.322472	51.192924	50.224141
350.065064	52.092576	50.229146
346.524734	43.029609	50.234151
342.896494	50.190938	50.239156
339.422820	46.726770	50.244161
336.202311	48.234430	50.249165
332.165790	48.186063	50.254170
328.754810	47.179793	50.259175
325.280836	46.746462	50.264180
321.927458	47.920480	50.269185
318.296916	41.029183	50.274189
314.420876	58.204123	50.279194
311.199535	44.352333	50.284199
307.837513	52.544700	50.289204
304.467390	47.178873	50.294209
300.702899	48.556099	50.299213
297.013564	51.712258	50.304218
293.911341	40.686063	50.309223
289.968720	57.874532	50.314228
286.661099	47.389661	50.319233
283.476545	47.695866	50.324237
279.845598	54.636167	50.329242
276.484881	50.325543	50.334247
272.413702	59.289528	50.339252
268.920022	55.986667	50.344257
265.888199	47.730373	50.349261
262.037859	58.539191	50.354266
258.825310	54.388994	50.359271
255.238250	56.330207	50.364276
251.679696	59.405902	50.369281
248.515143	59.085755	50.374285
244.467335	53.401514	50.379290
241.856037	55.478707	50.384295
237.913497	58.471821	50.389300
234.463800	54.798297	50.394305
230.915721	48.846439	50.399309
227.027684	54.561307	50.404314
223.412998	48.891894	50.409319
219.915509	53.875263	50.414324
216.640245	58.374794	50.419329
213.252480	40.287491	50.424333
209.899218	47.190891	50.429338
206.484669	43.163900	50.434343
202.451216	49.600578	50.439348
198.768919	49.022534	50.444353
195.652709	47.163658	50.449357
192.194895	47.676928	50.454362
188.544190	42.940085	50.459367
185.374482	53.032351	50.464372
181.684000	49.918330	50.469377
177.851482	42.340357	50.474381
175.005890	50.620002	50.479386
171.239512	42.683731	50.484391
167.739685	51.194946	50.489396
164.398151	52.088738	50.494401
161.031770	52.533995	50.499405
156.944123	51.319899	50.504410
153.778542	58.257360	50.509415
150.112726	51.672133	50.514420
146.709027	58.738413	50.519425
143.475496	49.216446	50.524429
139.663921	48.921123	50.529434
136.386407	50.507283	50.534439
132.600557	55.728540	50.539444
128.790070	52.392774	50.544449
125.607669	50.503085	50.549453
122.063145	57.486891	50.554458
119.050063	49.145452	50.559463
115.431108	56.640705	50.564468
111.601680	56.857515	50.569473
107.930322	50.485126	50.574477
104.101394	59.012788	50.579482
100.775563	53.216171	50.584487
97.456946	58.013520	50.589492
94.300367	61.320869	50.594497
90.888651	50.722539	50.599501
87.007323	59.732909	50.604506
83.340643	48.364382	50.609511
79.984667	53.332059	50.614516
76.483912	53.219300	50.619521
73.458271	44.566626	50.624525
69.513524	49.300116	50.629530
65.881405	44.601529	50.634535
62.495251	47.413129	50.639540
59.000960	55.391998	50.644545
56.029713	55.696658	50.649549
51.790071	61.491600	50.654554
48.506604	47.665365	50.659559
45.277003	54.144579	50.664564
41.604858	48.623350	50.669569
38.052044	48.404811	50.674573
34.488298	63.525379	50.679578
31.042333	52.907084	50.684583
27.292811	47.287178	50.689588
23.748600	58.285623	50.694593
20.908904	57.753581	50.699597
17.128096	60.585508	50.704602
13.608688	57.542953	50.709607
10.002017	68.842186	50.714612
6.401311	61.908337	50.719617
2.858719	56.692799	50.724621