Fri Aug 26 10:58:54 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.084030	100.788785	0.000000
2.183414	109.717227	0.005005
2.169628	108.416184	0.010010
1.469249	97.354578	0.015014
1.023955	99.879151	0.020019
1.545678	81.284419	0.025024
0.830777	84.686173	0.030029
0.730081	72.971246	0.035034
0.364516	73.680117	0.040038
0.363043	67.486147	0.045043
0.321414	56.885132	0.050048
-0.146285	51.893181	0.055053
-0.841245	42.020301	0.060058
-1.019259	45.749730	0.065062
-1.191189	36.026365	0.070067
-1.278154	34.170428	0.075072
-1.843209	29.155679	0.080077
-1.793110	27.911132	0.085082
-2.076871	20.299523	0.090086
-2.419104	17.679766	0.095091
-2.563302	15.332886	0.100096
-2.733207	15.717072	0.105101
-3.083715	6.056328	0.110106
-3.374965	5.918423	0.115110
-3.657983	4.118324	0.120115
-4.165324	5.080213	0.125120
-5.141901	5.140758	0.130125
-4.826785	4.028950	0.135130
-5.337381	13.223153	0.140134
-5.684776	14.932069	0.145139
-5.502448	5.090291	0.150144
-5.578094	3.764087	0.155149
-5.526088	1.921316	0.160154
-5.730227	-4.930749	0.165158
-6.719268	9.779412	0.170163
-6.477137	4.721247	0.175168
-6.956068	12.575461	0.180173
-7.456737	12.435363	0.185178
-8.308497	11.888036	0.190182
-7.929226	11.566642	0.195187
-7.855510	8.553105	0.200192
-8.259499	9.577993	0.205197
-8.321635	6.968409	0.210202
-8.451260	7.010977	0.215206
-9.065625	12.728672	0.220211
-9.530914	6.179846	0.225216
-9.880152	11.375386	0.230221
-9.786979	5.476738	0.235226
-9.888795	13.170999	0.240230
-10.325894	14.583845	0.245235
-9.945619	8.814495	0.250240
-11.074744	13.138078	0.255245
-11.430248	17.790448	0.260250
-11.945340	19.066746	0.265254
-11.646747	23.528694	0.270259
-11.622631	12.696015	0.275264
-11.987231	17.311837	0.280269
-11.805714	17.660290	0.285274
-12.081409	17.750910	0.290278
-12.496160	16.512303	0.295283
-12.694868	3.746534	0.300288
-12.951999	8.105185	0.305293
-13.618419	6.440708	0.310298
-14.043993	8.841979	0.315302
-14.381498	9.461061	0.320307
-14.249316	7.890534	0.325312
-14.576583	11.624213	0.330317
-14.624899	10.331717	0.335322
-14.628233	11.721317	0.340326
-15.524679	14.613505	0.345331
-16.072758	14.547224	0.350336
-15.976374	9.511752	0.355341
-16.097251	10.299578	0.360346
-16.252444	14.095048	0.365350
-16.292215	17.372691	0.370355
-16.413267	11.646596	0.375360
-17.321804	9.143486	0.380365
-17.439734	6.397062	0.385370
-17.684191	11.152359	0.390374
-17.936659	14.776319	0.395379
-17.811611	2.592873	0.400384
-18.026034	12.262962	0.405389
-18.456776	12.149940	0.410394
-18.946428	6.977930	0.415398
-19.236799	11.566376	0.420403
-18.735072	8.622235	0.425408
-19.513099	20.477577	0.430413
-19.527010	8.708055	0.435418
-19.988589	8.729544	0.440422
-20.420716	18.686623	0.445427
-19.965002	5.040705	0.450432
-20.891448	7.507307	0.455437
-21.703546	7.317625	0.460442
-21.676353	16.491368	0.465446
-22.200879	13.533012	0.470451
-21.833637	14.266984	0.475456
-22.381662	12.413236	0.480461
-22.062262	6.109219	0.485466
-22.357330	11.093851	0.490470
-22.464671	9.908619	0.495475
-22.732158	6.695116	0.500480
-23.399343	15.638462	0.505485
-23.588722	4.396119	0.510490
-23.624282	11.694098	0.515494
-23.832693	10.208237	0.520499
-23.968130	0.023647	0.525504
-24.762797	14.535873	0.530509
-24.596996	-1.102289	0.535514
-24.555286	5.199763	0.540518
-25.759044	8.848454	0.545523
-25.861630	4.160327	0.550528
-26.050719	9.071512	0.555533
-26.181038	9.025606	0.560538
-26.271265	11.785939	0.565542
-26.436717	8.882404	0.570547
-26.313353	16.354950	0.575552
-26.988170	10.563222	0.580557
-27.256443	11.294907	0.585562
-27.409097	17.320352	0.590566
-27.947074	8.698001	0.595571
-27.607348	8.044254	0.600576
-28.398815	11.255442	0.605581
-28.741613	5.997295	0.610586
-29.002407	11.720047	0.615590
-29.112866	9.484970	0.620595
-29.230627	12.205299	0.625600
-29.358470	5.926627	0.630605
-29.393668	4.138561	0.635610
-29.944036	1.225358	0.640614
-30.239309	8.358135	0.645619
-30.499705	3.637634	0.650624
-30.798293	12.900061	0.655629
-31.012434	11.525821	0.660634
-31.724682	5.575413	0.665638
-32.079726	12.170188	0.670643
-32.308634	9.883953	0.675648
-32.200471	10.867064	0.680653
-32.049928	15.010386	0.685658
-32.188028	14.453181	0.690662
-32.739874	11.723699	0.695667
-33.097058	8.236269	0.700672
-33.370038	17.754131	0.705677
-33.609629	12.176204	0.710682
-33.715817	10.411845	0.715686
-34.176038	8.642499	0.720691
-34.184639	7.701313	0.725696
-35.084666	6.142809	0.730701
-35.189785	8.032294	0.735706
-35.367929	8.439908	0.740710
-35.432432	20.446737	0.745715
-34.902110	8.263461	0.750720
-35.216813	9.454776	0.755725
-35.885700	7.091518	0.760730
-36.471205	8.657179	0.765734
-36.620091	8.234527	0.770739
-36.629643	-2.814354	0.775744
-37.010693	3.275120	0.780749
-37.561094	9.049290	0.785754
-37.982859	7.795958	0.790758
-38.597291	12.763879	0.795763
-38.310295	1.953551	0.800768
-38.344505	2.696247	0.805773
-38.263018	1.057687	0.810778
-38.257568	8.896588	0.815782
-38.895061	18.173822	0.820787
-39.139430	7.155169	0.825792
-39.297197	13.561046	0.830797
-39.714206	13.097885	0.835802
-39.695995	11.067393	0.840806
-40.458013	10.588350	0.845811
-40.632452	8.312617	0.850816
-41.097005	12.023379	0.855821
-40.982779	2.587665	0.860826
-40.978468	5.627495	0.865830
-41.647894	9.743466	0.870835
-41.894043	18.159365	0.875840
-42.338937	13.651079	0.880845
-42.675372	11.372096	0.885850
-42.913467	9.685220	0.890854
-43.112570	14.072800	0.895859
-42.996368	1.539570	0.900864
-43.118269	14.915698	0.905869
-43.385181	6.108781	0.910874
-43.775158	13.781470	0.915878
-44.101567	8.609354	0.920883
-44.188767	9.407755	0.925888
-44.374000	3.210783	0.930893
-45.065930	5.612399	0.935898
-45.294491	2.234654	0.940902
-45.790873	6.801391	0.945907
-45.526786	8.336008	0.950912
-45.823400	1.261068	0.955917
-45.838447	8.280614	0.960922
-45.735722	3.184047	0.965926
-46.828539	17.650950	0.970931
-47.129012	17.011462	0.975936
-47.032643	13.048468	0.980941
-46.816900	14.992396	0.985946
-47.784497	12.536446	0.990950
-48.836578	8.163828	0.995955
-48.209330	4.039087	1.000960
-48.438707	15.809000	1.005965
-48.913943	8.761869	1.010970
-48.800102	10.807080	1.015974
-49.080747	3.536671	1.020979
-48.925740	6.230347	1.025984
-49.080399	13.300104	1.030989
-49.369371	10.033001	1.035994
-49.598687	4.529404	1.040998
-50.448509	19.565894	1.046003
-50.717975	6.023397	1.051008
-51.051328	14.762909	1.056013
-51.200772	9.047565	1.061018
-50.976917	9.553934	1.066022
-51.534347	7.594088	1.071027
-52.012433	7.978804	1.076032
-52.292717	-2.148430	1.081037
-52.737884	13.878543	1.086042
-52.806858	6.964304	1.091046
-53.047656	10.924955	1.096051
-52.716723	-3.963819	1.101056
-52.509164	8.117695	1.106061
-53.795912	7.207842	1.111066
-53.756917	5.417715	1.116070
-54.460083	7.631262	1.121075
-54.293385	2.372880	1.126080
-54.426890	4.235148	1.131085
-55.243263	6.020246	1.136090
-55.196613	10.575198	1.141094
-56.016784	12.670926	1.146099
-55.892872	10.861250	1.151104
-56.097293	6.185816	1.156109
-55.624240	4.650798	1.161114
-55.743011	5.134587	1.166118
-56.573735	15.261288	1.171123
-56.943297	6.172972	1.176128
-57.081789	7.077432	1.181133
-57.522232	9.177309	1.186138
-57.361243	3.537015	1.191142
-58.245637	11.884612	1.196147
-58.696394	6.956476	1.201152
-58.699800	7.634267	1.206157
-58.677258	11.734244	1.211162
-58.990764	17.471531	1.216166
-59.513693	12.380631	1.221171
-59.358546	14.134684	1.226176
-59.059835	4.705045	1.231181
-59.327414	12.070784	1.236186
-60.207116	5.048667	1.241190
-60.440678	14.924207	1.246195
-60.311120	9.750697	1.251200
-60.448125	8.971867	1.256205
-61.314227	6.920881	1.261210
-61.447882	3.733997	1.266214
-61.952850	15.907474	1.271219
-61.638668	6.829753	1.276224
-61.698158	12.473707	1.281229
-62.469754	10.097969	1.286234
-62.876345	1.762042	1.291238
-63.318114	4.823872	1.296243
-63.450504	12.402671	1.301248
-63.449422	15.253187	1.306253
-63.560979	9.253544	1.311258
-63.357567	7.308108	1.316262
-64.252492	4.825028	1.321267
-64.161126	7.421048	1.326272
-64.875355	6.108855	1.331277
-65.110690	12.251570	1.336282
-65.485696	12.797400	1.341286
-65.266335	14.111198	1.346291
-65.532199	5.414848	1.351296
-66.254325	12.190158	1.356301
-66.436627	15.183118	1.361306
-66.332273	7.450981	1.366310
-66.580050	11.896757	1.371315
-66.580163	8.989625	1.376320
-66.744968	8.506179	1.381325
-67.493685	16.801016	1.386330
-67.437902	5.871670	1.391334
-67.908623	15.831591	1.396339
-67.565341	11.997826	1.401344
-68.415847	13.766094	1.406349
-68.931565	18.316863	1.411354
-69.091952	4.286003	1.416358
-69.596858	11.014837	1.421363
-69.657173	11.451560	1.426368
-69.683904	17.185323	1.431373
-69.623078	10.962694	1.436378
-69.849210	9.647267	1.441382
-70.570061	8.541741	1.446387
-70.361364	-1.414861	1.451392
-70.717118	-0.761301	1.456397
-71.072954	8.418289	1.461402
-71.470721	-1.447050	1.466406
-72.123303	17.215896	1.471411
-72.020650	8.164784	1.476416
-72.395330	3.797425	1.481421
-72.613905	10.956223	1.486426
-72.419997	12.134783	1.491430
-72.275865	11.242580	1.496435
-73.200614	1.171399	1.501440
-73.176051	5.941752	1.506445
-73.666510	11.456661	1.511450
-73.636663	7.801409	1.516454
-74.697229	15.752509	1.521459
-74.870460	8.338829	1.526464
-75.191571	4.896404	1.531469
-75.365173	17.091050	1.536474
-75.214030	4.745363	1.541478
-75.423154	6.730132	1.546483
-75.276359	6.081115	1.551488
-75.248591	3.368953	1.556493
-75.980223	7.146608	1.561498
-76.432232	5.663877	1.566502
-76.989640	10.670372	1.571507
-76.631889	6.809046	1.576512
-76.820465	6.076210	1.581517
-77.620905	11.987384	1.586522
-77.969754	2.503555	1.591526
-78.286930	13.069131	1.596531
-78.291019	-0.536822	1.601536
-78.162728	3.875706	1.606541
-78.430598	4.588346	1.611546
-78.752101	3.873043	1.616550
-79.625496	12.070236	1.621555
-79.718326	4.008147	1.626560
-79.864120	7.330768	1.631565
-80.179491	7.649021	1.636570
-79.340446	6.354400	1.641574
-79.887578	15.693489	1.646579
-80.480255	10.006031	1.651584
-80.883733	13.960375	1.656589
-80.991585	20.937428	1.661594
-81.419712	2.158499	1.666598
-82.506615	16.776333	1.671603
-82.848897	7.038388	1.676608
-82.099708	0.420692	1.681613
-82.299628	18.956213	1.686618
-82.842473	3.874465	1.691622
-82.903909	8.490535	1.696627
-82.688567	11.586090	1.701632
-83.044801	7.886551	1.706637
-83.701065	12.554110	1.711642
-83.767149	4.171494	1.716646
-84.064703	16.246237	1.721651
-84.466999	6.916256	1.726656
-84.561963	5.700625	1.731661
-85.025984	12.419929	1.736666
-85.161389	5.262945	1.741670
-85.116250	7.894635	1.746675
-85.632522	-0.291339	1.751680
-86.215535	0.239423	1.756685
-87.114976	11.933332	1.761690
-86.725998	4.751647	1.766694
-86.628743	14.626294	1.771699
-86.691874	6.129326	1.776704
-87.171089	4.872286	1.781709
-87.344979	14.020386	1.786714
-87.278947	4.876906	1.791718
-88.072956	16.234873	1.796723
-88.599207	6.158591	1.801728
-88.699654	4.336394	1.806733
-88.664339	5.390956	1.811738
-88.718317	8.386080	1.816742
-89.072945	8.356118	1.821747
-89.510300	2.926043	1.826752
-89.851524	6.317056	1.831757
-89.936344	12.044043	1.836762
-89.681826	6.015877	1.841766
-90.278035	9.810410	1.846771
-90.822222	10.107345	1.851776
-90.873859	8.635040	1.856781
-91.736117	16.536281	1.861786
-91.129238	3.135745	1.866790
-91.416308	9.270695	1.871795
-91.891307	12.040317	1.876800
-92.602510	7.026190	1.881805
-93.231922	8.861271	1.886810
-92.836905	11.226521	1.891814
-93.223759	11.138304	1.896819
-93.349507	2.685887	1.901824
-93.272296	5.053165	1.906829
-93.370090	14.866436	1.911834
-93.496383	3.215659	1.916838
-94.358051	14.891034	1.921843
-94.471915	7.752840	1.926848
-94.378953	12.917491	1.931853
-95.076554	14.158933	1.936858
-95.454262	13.151835	1.941862
-95.918631	21.905419	1.946867
-96.442637	9.525653	1.951872
-96.177607	6.678476	1.956877
-96.604544	6.811627	1.961882
-96.237806	0.123771	1.966886
-96.534600	13.504978	1.971891
-96.530770	9.572212	1.976896
-96.561235	6.062389	1.981901
-97.604438	12.552344	1.986906
-97.360161	7.478029	1.991910
-97.516271	10.666219	1.996915
-98.430862	4.340826	2.006912
-97.886054	8.466343	2.016909
-97.594293	10.420210	2.026906
-97.353909	7.595690	2.036902
-96.773068	4.483753	2.046899
-95.990549	7.555428	2.056896
-95.406670	9.109030	2.066893
-95.329498	11.390904	2.076890
-94.379656	14.031064	2.086886
-93.798892	5.081077	2.096883
-93.524729	4.250113	2.106880
-92.670898	2.958275	2.116877
-92.372292	6.048277	2.126874
-92.471831	7.160278	2.136870
-91.876917	0.400134	2.146867
-91.088444	-0.023083	2.156864
-89.978820	6.140013	2.166861
-89.841653	-2.306928	2.176858
-89.979379	0.692627	2.186854
-89.036209	1.702461	2.196851
-88.066811	4.143178	2.206848
-88.141988	4.177536	2.216845
-87.289907	2.996839	2.226842
-86.866048	4.809766	2.236838
-86.626372	6.217396	2.246835
-86.508152	3.041278	2.256832
-85.565163	0.797921	2.266829
-84.500595	4.405369	2.276826
-84.387507	7.847362	2.286822
-84.089480	8.042184	2.296819
-83.420184	9.053482	2.306816
-82.843585	11.504675	2.316813
-82.777520	12.613065	2.326810
-82.148779	14.891421	2.336806
-81.207777	10.868126	2.346803
-81.084120	6.699673	2.356800
-80.341426	10.553636	2.366797
-79.931366	8.225367	2.376794
-79.712903	3.776066	2.386790
-78.690678	4.121048	2.396787
-78.365193	8.879409	2.406784
-78.187026	13.543504	2.416781
-77.260654	7.263922	2.426778
-76.806390	8.844041	2.436774
-76.405335	6.938478	2.446771
-75.984666	2.083907	2.456768
-75.303864	6.327628	2.466765
-75.175137	9.200170	2.476762
-74.411457	3.326044	2.486758
-73.986797	2.949970	2.496755
-73.635633	7.241850	2.506752
-72.773958	8.036300	2.516749
-72.338395	10.332063	2.526746
-72.354681	4.414657	2.536742
-71.145435	10.546407	2.546739
-70.743031	11.976217	2.556736
-70.713153	10.546582	2.566733
-69.845165	11.837378	2.576730
-69.533375	8.165469	2.586726
-69.026314	9.807057	2.596723
-68.341505	16.175681	2.606720
-68.077331	17.791734	2.616717
-67.173789	11.971853	2.626714
-66.553989	15.059364	2.636710
-66.462503	14.282185	2.646707
-66.146035	15.861586	2.656704
-65.676427	9.992065	2.666701
-65.348751	12.558042	2.676698
-63.819823	6.700976	2.686694
-63.556651	7.971905	2.696691
-63.513657	6.289980	2.706688
-63.080852	9.203873	2.716685
-62.519843	7.102349	2.726682
-62.231574	8.632290	2.736678
-61.313890	8.930196	2.746675
-60.792479	7.677444	2.756672
-60.439931	12.897245	2.766669
-59.610658	9.271471	2.776666
-59.366023	12.420563	2.786662
-59.472379	5.018860	2.796659
-58.300455	4.374388	2.806656
-58.093759	4.830510	2.816653
-57.145300	8.452871	2.826650
-56.381283	12.566435	2.836646
-56.195447	11.378603	2.846643
-56.560682	12.066321	2.856640
-55.359866	8.205308	2.866637
-54.673078	2.983028	2.876634
-54.621496	3.235227	2.886630
-53.811318	9.723709	2.896627
-53.630545	11.368585	2.906624
-52.350308	8.429676	2.916621
-52.229004	11.578964	2.926618
-51.686168	7.456113	2.936614
-51.619467	2.590131	2.946611
-51.389063	7.813110	2.956608
-50.644977	5.888982	2.966605
-49.533210	4.363755	2.976602
-49.556422	12.293422	2.986598
-48.980644	7.782150	2.996595
-48.040673	12.796453	3.006592
-47.801320	7.859240	3.016589
-47.954111	10.443007	3.026586
-46.935426	11.761025	3.036582
-46.251258	13.771001	3.046579
-45.634146	15.281418	3.056576
-44.889448	16.471040	3.066573
-44.669062	13.621123	3.076570
-44.854504	9.576819	3.086566
-44.173921	6.962518	3.096563
-43.579182	10.079273	3.106560
-42.543686	12.816968	3.116557
-41.694270	12.425443	3.126554
-41.931967	10.473619	3.136550
-41.784662	10.799610	3.146547
-40.762990	8.784746	3.156544
-40.145519	14.337088	3.166541
-40.349076	6.792133	3.176538
-39.245253	9.892978	3.186534
-38.548894	10.763853	3.196531
-38.417010	17.459315	3.206528
-38.273345	20.563944	3.216525
-37.543546	23.051475	3.226522
-36.469296	15.979114	3.236518
-36.103542	17.205563	3.246515
-35.759080	16.572722	3.256512
-35.707824	14.480877	3.266509
-34.684436	21.550701	3.276506
-34.648932	12.099580	3.286502
-33.778151	11.131376	3.296499
-32.905231	5.677382	3.306496
-32.864867	7.550020	3.316493
-32.455905	9.761230	3.326490
-31.295406	11.250398	3.336486
-31.453120	15.494805	3.346483
-31.096842	14.220249	3.356480
-30.140055	13.688467	3.366477
-29.753819	12.193844	3.376474
-29.693383	5.485237	3.386470
-28.961687	10.899421	3.396467
-28.070543	8.550099	3.406464
-27.829056	10.343908	3.416461
-27.176316	6.419348	3.426458
-26.976768	10.069621	3.436454
-26.482448	11.219034	3.446451
-25.493699	9.719296	3.456448
-25.417470	11.580016	3.466445
-24.880990	12.374418	3.476442
-23.850644	9.290691	3.486438
-23.669124	5.417325	3.496435
-23.693454	8.491090	3.506432
-22.789267	6.298122	3.516429
-22.305095	1.782109	3.526426
-22.153285	5.797763	3.536422
-21.028801	9.009429	3.546419
-20.684020	3.925926	3.556416
-20.366171	5.682504	3.566413
-19.594444	11.844368	3.576410
-19.357460	10.639070	3.586406
-19.221270	14.977096	3.596403
-18.131442	11.950628	3.606400
-17.828267	8.707699	3.616397
-17.135236	11.448034	3.626394
-16.407686	8.500147	3.636390
-16.101446	8.579653	3.646387
-16.254895	0.402861	3.656384
-15.458057	3.830261	3.666381
-15.144075	14.840282	3.676378
-13.988413	8.816427	3.686374
-13.647190	8.082724	3.696371
-13.390397	7.428688	3.706368
-12.918281	12.899129	3.716365
-12.167696	18.240687	3.726362
-11.921059	17.933512	3.736358
-10.708098	12.017939	3.746355
-10.549619	5.718537	3.756352
-10.259146	9.006207	3.766349
-10.291638	13.155093	3.776346
-9.132600	15.037284	3.786342
-8.735708	11.640383	3.796339
-8.361131	4.128953	3.806336
-7.804169	11.508975	3.816333
-7.454276	9.560694	3.826330
-6.565634	5.754622	3.836326
-5.666344	9.219922	3.846323
-5.657984	5.962709	3.856320
-5.570542	10.108759	3.866317
-5.268970	15.906686	3.876314
-4.660559	17.899951	3.886310
-3.945166	26.474876	3.896307
-3.845781	32.934661	3.906304
-3.208223	42.139414	3.916301
-2.543404	61.463913	3.926298
-2.263814	69.789942	3.936294
-1.684708	75.221571	3.946291
-0.966644	94.582164	3.956288
-0.613713	101.401630	3.966285
0.000000	107.523594	3.971290
0.035917	120.704396	3.976294
0.296111	123.071675	3.981299
0.162312	120.299230	3.986304
0.271349	114.208256	3.991309
0.365409	127.990598	3.996314
0.381909	120.594781	4.001318
0.659137	127.287303	4.006323
0.460704	121.237872	4.011328
0.606618	120.962300	4.016333
0.583494	128.473521	4.021338
0.409978	119.560256	4.026342
0.976356	122.528414	4.031347
0.830475	125.474595	4.036352
0.733374	117.296059	4.041357
0.434637	126.764209	4.046362
0.577615	116.919005	4.051366
0.511953	112.563612	4.056371
0.201268	119.331849	4.061376
0.500964	127.412886	4.066381
0.904445	134.892489	4.071386
0.938256	129.765486	4.076390
1.078027	134.056044	4.081395
0.491551	132.413907	4.086400
0.898343	122.546606	4.091405
0.547112	117.969926	4.096410
0.815308	127.925593	4.101414
1.270443	133.546408	4.106419
0.815702	125.588063	4.111424
0.801988	118.782229	4.116429
0.464379	114.842488	4.121434
0.549410	109.792936	4.126438
1.041398	119.131641	4.131443
0.970995	125.973198	4.136448
0.862533	123.143025	4.141453
0.630671	117.677751	4.146458
1.112404	131.871123	4.151462
1.159081	123.315867	4.156467
0.563153	115.268780	4.161472
0.964864	124.358960	4.166477
1.040180	134.879322	4.171482
1.132702	126.215690	4.176486
0.852381	128.448833	4.181491
0.375933	127.017349	4.186496
1.237486	123.650180	4.191501
1.245994	127.733389	4.196506
1.333912	132.139584	4.201510
1.043814	119.609417	4.206515
0.784938	122.490935	4.211520
0.942074	115.857813	4.216525
1.081097	129.794502	4.221530
1.247454	135.817774	4.226534
1.201829	125.489416	4.231539
0.483858	124.320158	4.236544
0.959863	132.164944	4.241549
1.085351	139.713141	4.246554
1.226879	141.991333	4.251558
1.726996	135.288983	4.256563
1.152473	139.978650	4.261568
1.377045	135.736245	4.266573
1.050499	135.192558	4.271578
1.218455	134.157438	4.276582
1.194860	131.886674	4.281587
1.501650	138.650526	4.286592
1.193541	129.112824	4.291597
0.779748	137.058187	4.296602
1.073586	131.549023	4.301606
1.380787	136.848032	4.306611
1.307978	143.139491	4.311616
1.553032	147.049837	4.316621
1.484042	139.698960	4.321626
1.122731	134.902387	4.326630
1.180164	144.729533	4.331635
1.257182	145.198659	4.336640
1.329998	141.631597	4.341645
1.139664	139.114718	4.346650
1.410463	145.153368	4.351654
1.379751	143.389899	4.356659
1.456883	142.343610	4.361664
1.502044	139.609735	4.366669
1.455318	140.705553	4.371674
1.345905	147.069150	4.376678
1.200278	140.714106	4.381683
1.262311	142.197939	4.386688
1.470992	138.211102	4.391693
1.561249	144.803031	4.396698
1.304210	139.933276	4.401702
1.398526	134.758888	4.406707
1.515094	138.271633	4.411712
1.743380	139.473324	4.416717
1.570615	137.206804	4.421722
1.675918	139.870276	4.426726
1.615602	135.975940	4.431731
1.582689	146.763090	4.436736
1.631048	140.207004	4.441741
1.705091	145.766938	4.446746
1.698097	139.678203	4.451750
1.788935	138.886038	4.456755
1.601748	144.660646	4.461760
1.315441	142.563659	4.466765
1.938232	144.023458	4.471770
1.522963	144.838144	4.476774
1.589838	141.784522	4.481779
1.774414	140.756304	4.486784
1.594895	136.554670	4.491789
1.672865	131.259444	4.496794
1.398171	139.822213	4.501798
1.604061	129.622367	4.506803
1.757231	144.648331	4.511808
2.102209	152.678037	4.516813
1.971371	147.200188	4.521818
1.624419	150.146043	4.526822
1.711318	143.508028	4.531827
1.713974	148.357761	4.536832
2.245932	148.537761	4.541837
2.109410	146.278251	4.546842
1.726945	135.103850	4.551846
1.847189	142.630719	4.556851
1.966161	143.052186	4.561856
2.006663	139.556592	4.566861
1.848565	138.410891	4.571866
1.533824	150.285934	4.576870
2.254786	155.295906	4.581875
1.927266	161.415064	4.586880
1.935236	156.067457	4.591885
2.087820	164.544729	4.596890
2.237948	156.485865	4.601894
1.706173	149.456968	4.606899
1.994147	163.398966	4.611904
2.161310	165.666842	4.616909
2.459945	171.157016	4.621914
2.059705	166.148202	4.626918
2.018881	153.079339	4.631923
1.813649	150.118701	4.636928
2.236845	161.711182	4.641933
2.533363	174.437008	4.646938
2.001274	159.669807	4.651942
1.575277	158.347521	4.656947
1.806545	167.739500	4.661952
2.201097	165.201153	4.666957
2.438176	162.972055	4.671962
2.304608	165.742323	4.676966
2.492332	159.275260	4.681971
2.594698	168.244395	4.686976
2.291684	153.874956	4.691981
1.898575	151.762960	4.696986
1.862137	168.099752	4.701990
2.326404	161.893344	4.706995
2.318359	167.984908	4.712000
2.450278	169.321825	4.717005
2.649797	167.791419	4.722010
2.273498	169.375139	4.727014
2.338736	169.811300	4.732019
2.242673	174.568846	4.737024
2.291476	165.408977	4.742029
2.539149	157.863259	4.747034
2.529665	163.616533	4.752038
2.533241	162.553222	4.757043
2.222376	164.958800	4.762048
2.286997	159.551752	4.767053
2.404187	163.535793	4.772058
2.407245	163.937343	4.777062
2.500131	164.198361	4.782067
2.194886	165.230030	4.787072
2.713961	159.005598	4.792077
2.359556	165.274472	4.797082
2.210743	165.076425	4.802086
2.415737	160.315056	4.807091
1.934667	166.834601	4.812096
2.221649	163.243680	4.817101
1.980035	172.133499	4.822106
2.289666	176.005324	4.827110
2.465255	181.154000	4.832115
2.718942	190.321043	4.837120
2.741086	190.941080	4.842125
3.147864	188.403989	4.847130
2.800065	182.102553	4.852134
2.159831	165.716565	4.857139
2.339002	176.353656	4.862144
2.572884	182.021589	4.867149
2.450746	184.451568	4.872154
2.288132	186.115911	4.877158
2.654655	184.303244	4.882163
2.751966	186.009374	4.887168
2.395885	186.191602	4.892173
2.674331	180.156484	4.897178
2.755848	191.574399	4.902182
2.880442	192.333505	4.907187
3.052951	186.700849	4.912192
2.824386	192.225657	4.917197
3.082644	188.604403	4.922202
2.649474	184.682690	4.927206
3.184660	185.273466	4.932211
2.842114	185.409295	4.937216
2.767742	185.389478	4.942221
2.679919	198.972409	4.947226
2.634366	191.931065	4.952230
3.182692	181.257104	4.957235
2.869660	186.921609	4.962240
2.959771	185.870133	4.967245
3.163938	183.624011	4.972250
2.722731	185.050163	4.977254
3.158534	186.659299	4.982259
3.002637	182.612159	4.987264
3.069650	179.071303	4.992269
3.267400	180.220805	4.997274
2.770090	184.898461	5.002278
3.140212	178.890198	5.007283
2.753302	185.395089	5.012288
3.021313	179.428034	5.017293
3.054536	179.979908	5.022298
2.932023	187.876779	5.027302
3.079012	186.313423	5.032307
3.040388	182.785849	5.037312
3.208510	185.711624	5.042317
3.200962	177.297659	5.047322
2.844044	182.371061	5.052326
3.264763	174.042275	5.057331
2.981261	187.563917	5.062336
3.119336	192.462179	5.067341
3.268115	189.892494	5.072346
2.934640	189.473267	5.077350
3.143390	185.350370	5.082355
3.272625	197.634034	5.087360
3.333545	196.840197	5.092365
3.350196	179.706529	5.097370
3.239892	179.486667	5.102374
2.994935	178.974567	5.107379
3.154931	191.503368	5.112384
3.879858	196.316586	5.117389
3.327357	175.180902	5.122394
2.953023	183.341599	5.127398
3.214526	185.885849	5.132403
3.189377	189.082155	5.137408
3.288121	199.503998	5.142413
3.649855	201.051903	5.147418
3.369938	197.321455	5.152422
4.012355	203.938165	5.157427
3.622903	195.792457	5.162432
3.150936	191.819836	5.167437
3.359555	188.820064	5.172442
3.230880	191.453537	5.177446
3.583770	191.813275	5.182451
3.866629	197.546352	5.187456
3.667156	186.922381	5.192461
3.890642	183.572291	5.197466
3.423365	179.655889	5.202470
3.615649	181.657271	5.207475
3.613929	185.394081	5.212480
3.716670	183.318771	5.217485
3.775589	187.387818	5.222490
3.283428	187.556433	5.227494
3.551182	186.822139	5.232499
3.561359	185.637579	5.237504
3.505666	184.077307	5.242509
3.449586	184.576648	5.247514
3.369809	186.572935	5.252518
3.553801	182.637387	5.257523
3.342724	194.793705	5.262528
3.819081	203.021273	5.267533
4.117696	207.268135	5.272538
3.972975	199.312105	5.277542
3.314673	184.523407	5.282547
3.398400	183.371687	5.287552
3.979251	202.235089	5.292557
4.002893	205.221327	5.297562
3.670004	199.553463	5.302566
3.567590	201.138834	5.307571
3.535934	196.113752	5.312576
3.588650	211.085812	5.317581
3.807388	212.513616	5.322586
3.921019	215.897123	5.327590
3.823628	213.871951	5.332595
3.763675	207.747147	5.337600
3.743939	210.195986	5.342605
4.068624	209.917888	5.347610
3.789006	211.809254	5.352614
3.848734	210.398684	5.357619
3.960717	212.573920	5.362624
3.606794	206.292411	5.367629
3.578082	203.959161	5.372634
3.631629	205.472795	5.377638
3.805162	204.227999	5.382643
3.828509	213.165168	5.387648
3.754360	206.906536	5.392653
3.990684	211.982491	5.397658
3.791107	213.791794	5.402662
4.358578	222.527192	5.407667
4.054333	221.983194	5.412672
3.735432	217.078758	5.417677
4.093952	223.983281	5.422682
4.433497	222.510161	5.427686
4.123255	207.578668	5.432691
4.143585	203.462958	5.437696
3.981677	209.932825	5.442701
4.245517	210.809454	5.447706
4.153516	220.308739	5.452710
4.071561	211.216660	5.457715
4.161648	216.005344	5.462720
4.242621	215.214711	5.467725
4.347045	216.207907	5.472730
4.156779	221.271191	5.477734
4.196975	207.022275	5.482739
4.259005	211.729906	5.487744
4.483166	205.959491	5.492749
4.405368	209.787243	5.497754
3.871302	211.616989	5.502758
4.469690	208.493254	5.507763
4.166119	210.245984	5.512768
3.686691	209.397075	5.517773
4.581228	221.374942	5.522778
4.414285	222.688795	5.527782
4.274358	227.019759	5.532787
4.273960	227.469304	5.537792
4.453830	229.422006	5.542797
4.544475	236.526426	5.547802
4.722078	229.500941	5.552806
4.532407	229.726861	5.557811
4.411218	206.448607	5.562816
4.208240	206.910711	5.567821
4.120101	212.546537	5.572826
4.472198	231.439259	5.577830
4.687534	225.088093	5.582835
4.467382	236.087943	5.587840
4.650058	229.640623	5.592845
4.955148	219.225968	5.597850
4.512078	214.932474	5.602854
4.424953	217.682865	5.607859
4.232955	214.413278	5.612864
4.468638	228.708310	5.617869
4.545061	228.225262	5.622874
4.432086	235.487932	5.627878
4.723680	229.115401	5.632883
4.645168	234.585223	5.637888
4.328813	230.806659	5.642893
4.611196	231.487417	5.647898
4.377437	242.464080	5.652902
4.794021	235.762044	5.657907
5.030446	226.269218	5.662912
4.647535	234.848881	5.667917
4.749778	234.200465	5.672922
4.452315	239.179207	5.677926
4.599116	227.482589	5.682931
4.408060	234.985202	5.687936
4.497334	234.750084	5.692941
4.529816	231.638527	5.697946
4.579714	232.728797	5.702950
4.366305	239.466116	5.707955
4.520230	243.979118	5.712960
4.663398	250.917182	5.717965
5.318775	252.640830	5.722970
4.699396	248.792386	5.727974
4.580637	244.245915	5.732979
5.032595	261.167961	5.737984
5.042726	256.430579	5.742989
5.117298	244.207370	5.747994
5.019674	245.219372	5.752998
4.863227	233.475055	5.758003
4.723219	229.817728	5.763008
4.821466	230.941598	5.768013
4.963165	232.023902	5.773018
4.733906	238.504266	5.778022
5.279755	248.021311	5.783027
5.012309	246.155487	5.788032
4.632174	240.605696	5.793037
5.092314	241.163867	5.798042
5.389540	252.481798	5.803046
5.117903	249.559955	5.808051
4.986657	235.673059	5.813056
5.055205	234.852723	5.818061
4.952205	235.678904	5.823066
4.811671	248.086861	5.828070
5.355597	253.516723	5.833075
5.648333	258.802202	5.838080
5.139844	245.290404	5.843085
5.152086	238.904417	5.848090
4.913212	241.665784	5.853094
4.849819	232.982083	5.858099
4.766673	232.922504	5.863104
5.032851	249.285020	5.868109
5.572601	256.202466	5.873114
5.243706	256.696831	5.878118
5.515183	256.670622	5.883123
5.344630	252.761787	5.888128
5.233139	252.339633	5.893133
5.348524	242.780224	5.898138
5.248925	244.953606	5.903142
5.224213	238.696757	5.908147
5.547071	243.148656	5.913152
5.162179	248.397271	5.918157
5.216062	245.165323	5.923162
5.160433	249.695135	5.928166
5.191974	251.895556	5.933171
5.525098	258.550952	5.938176
5.137458	264.578267	5.943181
5.442228	262.952374	5.948186
5.251764	268.411163	5.953190
5.345238	256.131220	5.958195
5.626440	255.530868	5.963200
5.502799	264.608005	5.968205
5.578161	265.817697	5.973210
5.516706	268.273039	5.978214
5.416833	260.484002	5.983219
5.773209	267.607171	5.988224
5.289481	265.699092	5.993229
5.381606	262.552934	5.998234
5.441929	267.029897	6.003238
5.382548	250.752704	6.008243
5.292949	250.728930	6.013248
5.223804	254.836914	6.018253
5.791672	245.412693	6.023258
5.297627	258.135120	6.028262
5.198680	260.934814	6.033267
5.444914	259.061775	6.038272
5.233324	249.936078	6.043277
5.483918	248.780519	6.048282
5.622678	246.734394	6.053286
5.620354	249.961958	6.058291
5.581024	256.640543	6.063296
5.560050	256.204296	6.068301
5.601296	243.929329	6.073306
5.451406	248.024573	6.078310
5.240351	251.553550	6.083315
5.652812	258.677474	6.088320
5.535073	256.810487	6.093325
5.608470	242.217858	6.098330
5.430500	232.552272	6.103334
5.106983	229.369596	6.108339
5.354450	231.893892	6.113344
5.468797	250.576884	6.118349
5.801715	244.346606	6.123354
5.249636	244.233491	6.128358
5.305108	235.891943	6.133363
5.463508	248.614017	6.138368
5.423482	254.539751	6.143373
5.753489	248.126432	6.148378
5.441113	248.181635	6.153382
5.224193	236.418259	6.158387
5.744395	241.680972	6.163392
5.416390	239.751814	6.168397
5.367431	229.224602	6.173402
5.353537	237.364005	6.178406
5.515577	246.665567	6.183411
5.650186	233.189688	6.188416
4.869597	228.755757	6.193421
5.279398	246.130432	6.198426
5.474477	247.049405	6.203430
5.290606	246.613212	6.208435
5.328662	244.364472	6.213440
5.328701	253.378055	6.218445
5.393976	254.171709	6.223450
5.451613	252.438765	6.228454
5.653301	253.008703	6.233459
5.429142	247.143565	6.238464
5.242250	252.320225	6.243469
5.406418	252.218976	6.248474
5.610686	257.065822	6.253478
5.359534	258.215621	6.258483
5.433380	260.741643	6.263488
5.242709	253.529884	6.268493
5.696923	246.638491	6.273498
5.620661	255.758866	6.278502
5.480961	242.477546	6.283507
5.746766	259.371628	6.288512
5.641940	254.626836	6.293517
5.653222	253.809088	6.298522
5.410773	248.060689	6.303526
5.173874	238.290382	6.308531
5.275246	234.880204	6.313536
5.252044	255.843489	6.318541
5.180205	257.189992	6.323546
5.364801	253.981983	6.328550
5.671681	247.708302	6.333555
5.313230	252.193517	6.338560
5.463014	258.124500	6.343565
5.413549	253.114830	6.348570
5.712301	264.600206	6.353574
5.505853	263.632864	6.358579
5.540656	251.374713	6.363584
5.642765	260.432518	6.368589
5.624117	260.704575	6.373594
5.622886	258.316420	6.378598
5.063282	244.730325	6.383603
5.500125	244.912481	6.388608
5.226576	257.398101	6.393613
5.694712	250.545667	6.398618
5.327055	254.567253	6.403622
5.659854	258.441817	6.408627
5.419366	246.198059	6.413632
5.256166	259.112579	6.418637
5.756988	255.519983	6.423642
5.347125	250.658173	6.428646
5.471114	249.841859	6.433651
5.654713	238.117360	6.438656
5.026342	232.305670	6.443661
5.340057	242.817451	6.448666
5.447315	248.438684	6.453670
5.294455	256.757917	6.458675
5.588686	249.831322	6.463680
5.451335	258.018430	6.468685
5.589557	257.690271	6.473690
5.290151	249.394479	6.478694
5.665999	257.251751	6.483699
5.428876	249.645437	6.488704
5.424105	259.912593	6.493709
5.558504	246.857508	6.498714
5.424891	256.790389	6.503718
5.352609	256.877812	6.508723
5.515630	254.138224	6.513728
5.340104	255.456579	6.518733
5.477912	253.812390	6.523738
5.722879	253.616305	6.528742
5.463823	247.838855	6.533747
5.427922	230.928451	6.538752
5.047989	231.408616	6.543757
5.699495	241.946896	6.548762
5.721064	241.358496	6.553766
5.507343	232.416633	6.558771
5.342318	227.747658	6.563776
5.214405	229.928611	6.568781
5.411257	230.518284	6.573786
5.510856	242.664228	6.578790
5.629724	237.720100	6.583795
5.597763	236.307984	6.588800
5.296065	230.882022	6.593805
5.735954	224.543349	6.598810
5.201157	237.053812	6.603814
5.282643	230.090747	6.608819
5.265564	230.871913	6.613824
5.105357	252.599992	6.618829
5.411810	250.182915	6.623834
5.516690	253.697503	6.628838
5.456533	247.765701	6.633843
5.451957	248.633505	6.638848
5.185309	258.470044	6.643853
5.706024	249.837757	6.648858
5.439027	255.223039	6.653862
5.410033	262.032891	6.658867
5.622243	262.363915	6.663872
5.107262	253.902373	6.668877
5.716213	253.678090	6.673882
5.481591	262.519410	6.678886
5.650416	255.248514	6.683891
5.800215	249.568754	6.688896
5.358532	244.860594	6.693901
5.270816	241.929098	6.698906
5.511446	243.543318	6.703910
4.923771	237.412085	6.708915
5.238360	246.819606	6.713920
5.530687	260.643946	6.718925
5.661924	256.697613	6.723930
5.472884	256.948745	6.728934
5.596802	258.204658	6.733939
5.647603	254.274013	6.738944
5.225679	245.007064	6.743949
5.404364	249.759817	6.748954
5.432771	253.510933	6.753958
5.632423	253.862894	6.758963
5.722674	244.168195	6.763968
5.273480	239.897795	6.768973
5.073815	240.593496	6.773978
5.300019	246.395521	6.778982
5.608207	254.877082	6.783987
5.850475	257.721724	6.788992
5.518671	255.024378	6.793997
5.283995	242.311492	6.799002
5.312567	242.085825	6.804006
5.522660	243.217592	6.809011
5.705232	232.477163	6.814016
5.377857	240.010493	6.819021
5.360509	230.177534	6.824026
5.313075	237.192723	6.829030
5.476073	246.937052	6.834035
5.363511	235.144773	6.839040
5.292777	234.709947	6.844045
5.505427	244.456034	6.849050
5.560637	251.866528	6.854054
5.303670	248.774725	6.859059
5.643060	241.825283	6.864064
5.494853	249.204174	6.869069
5.096570	237.266558	6.874074
5.552589	243.279568	6.879078
5.514080	249.388558	6.884083
5.947326	245.398369	6.889088
5.306377	236.858374	6.894093
5.372918	230.615793	6.899098
5.526992	236.119003	6.904102
5.215032	230.625037	6.909107
5.657937	227.693183	6.914112
5.520045	232.672387	6.919117
5.498516	224.766767	6.924122
5.471956	231.212405	6.929126
5.340993	233.058482	6.934131
5.394185	228.849066	6.939136
5.640069	233.252837	6.944141
5.774404	223.111534	6.949146
5.459434	229.000976	6.954150
5.255882	227.390956	6.959155
5.835727	226.611232	6.964160
5.188257	231.973490	6.969165
5.503028	233.509728	6.974170
5.399772	229.701149	6.979174
5.534255	228.699708	6.984179
5.588474	225.654369	6.989184
5.104837	230.431146	6.994189
5.421601	225.620721	6.999194
5.231877	234.961227	7.004198
5.216653	232.891623	7.009203
5.424214	230.293797	7.014208
5.041880	240.293868	7.019213
5.618385	245.335849	7.024218
5.891659	253.512804	7.029222
5.166875	233.555457	7.034227
5.866992	230.947379	7.039232
5.540508	236.699414	7.044237
5.897515	228.617798	7.049242
5.519636	239.572608	7.054246
5.285552	237.900904	7.059251
5.290749	237.884516	7.064256
5.179848	237.139575	7.069261
5.201200	232.694675	7.074266
5.271969	228.077571	7.079270
4.856387	234.226283	7.084275
5.343545	248.523306	7.089280
5.178684	247.600108	7.094285
5.663610	252.422236	7.099290
5.927084	257.250373	7.104294
5.402560	250.071613	7.109299
5.948409	248.866920	7.114304
5.507670	238.837290	7.119309
5.517767	230.094694	7.124314
5.206213	231.940416	7.129318
5.237138	236.232127	7.134323
5.620127	226.801900	7.139328
5.327595	236.288124	7.144333
5.321344	231.284386	7.149338
5.496737	229.966535	7.154342
5.430423	234.203784	7.159347
5.681803	228.473414	7.164352
5.710776	229.377121	7.169357
5.771291	234.543729	7.174362
5.651862	236.913183	7.179366
5.660903	236.715867	7.184371
5.916569	225.201613	7.189376
5.591780	240.004689	7.194381
5.455394	228.459728	7.199386
5.595149	223.993232	7.204390
5.041845	246.067239	7.209395
5.244440	231.308973	7.214400
5.733687	230.919834	7.219405
5.571824	228.290944	7.224410
5.488732	230.053639	7.229414
5.793311	239.962577	7.234419
5.464937	234.910918	7.239424
5.608196	232.446488	7.244429
5.297682	232.425473	7.249434
5.628518	235.506252	7.254438
5.290410	236.625297	7.259443
5.602708	234.314878	7.264448
5.652225	230.805208	7.269453
5.188221	217.549091	7.274458
5.444140	222.258174	7.279462
5.532248	237.439876	7.284467
5.824225	221.506629	7.289472
5.118923	216.633882	7.294477
5.085938	219.201841	7.299482
5.535462	219.543370	7.304486
5.178627	229.162986	7.309491
5.586141	233.525773	7.314496
5.578160	237.988054	7.319501
5.531268	229.333423	7.324506
5.718558	232.961723	7.329510
5.433470	233.351192	7.334515
5.251371	212.856967	7.339520
5.351103	230.311540	7.344525
5.639483	231.225477	7.349530
5.637592	223.079524	7.354534
5.058970	219.648674	7.359539
5.674284	225.570438	7.364544
5.646453	222.762496	7.369549
5.443218	224.379385	7.374554
5.242244	216.754802	7.379558
5.336769	223.820649	7.384563
5.496858	223.299265	7.389568
5.341256	230.454677	7.394573
5.513371	236.764983	7.399578
5.816808	226.224034	7.404582
5.413436	223.392306	7.409587
5.269779	216.739542	7.414592
5.353507	217.302536	7.419597
5.563149	221.265867	7.424602
5.422950	214.773912	7.429606
5.053659	217.349942	7.434611
5.711006	223.711240	7.439616
5.083626	226.213562	7.444621
5.473328	225.447625	7.449626
6.015091	224.692813	7.454630
5.465488	216.840943	7.459635
5.339376	210.058901	7.464640
5.224281	217.059308	7.469645
5.391796	229.137722	7.474650
5.396485	226.704358	7.479654
5.525602	231.933049	7.484659
5.570524	221.527263	7.489664
5.285676	220.793587	7.494669
5.323379	231.690014	7.499674
5.459457	235.864115	7.504678
5.305466	230.361372	7.509683
5.662192	231.419688	7.514688
5.710686	241.754469	7.519693
5.469039	228.397286	7.524698
5.183401	221.092760	7.529702
5.499333	225.453986	7.534707
5.220310	227.655302	7.539712
5.260526	230.737038	7.544717
5.726470	232.771746	7.549722
5.788914	228.288813	7.554726
5.284614	219.483946	7.559731
5.487644	225.305390	7.564736
5.415124	222.865066	7.569741
5.366716	216.599259	7.574746
5.226035	219.652212	7.579750
5.342658	235.281879	7.584755
5.587457	227.271517	7.589760
5.468380	230.868425	7.594765
5.207164	233.914837	7.599770
5.482091	232.565670	7.604774
5.519304	233.502894	7.609779
5.671812	233.558481	7.614784
5.468312	242.138687	7.619789
5.484155	241.206337	7.624794
5.431094	229.661056	7.629798
5.549472	231.487294	7.634803
5.627813	213.442338	7.639808
5.162182	211.161296	7.644813
5.377551	221.258116	7.649818
5.474683	227.614894	7.654822
5.455370	228.573574	7.659827
5.364102	227.170693	7.664832
5.443269	231.492856	7.669837
5.225895	230.074809	7.674842
5.807160	226.884136	7.679846
5.268231	232.001709	7.684851
5.125841	233.109264	7.689856
5.499566	237.274837	7.694861
5.590571	229.288419	7.699866
5.943309	229.958223	7.704870
5.592704	221.325574	7.709875
5.374825	216.199770	7.714880
5.408203	214.726864	7.719885
5.102980	209.488114	7.724890
5.344804	216.005853	7.729894
5.548487	231.457450	7.734899
5.786582	228.491047	7.739904
5.622548	225.701147	7.744909
5.315352	209.392976	7.749914
5.068957	207.678899	7.754918
5.099116	217.149672	7.759923
5.387415	223.584248	7.764928
5.402078	226.942039	7.769933
5.431126	227.909007	7.774938
5.723533	228.490130	7.779942
5.417611	225.507192	7.784947
5.762732	232.831411	7.789952
5.712065	228.081357	7.794957
5.295387	221.834922	7.799962
5.119952	212.893436	7.804966
5.216101	223.144858	7.809971
5.503565	228.677916	7.814976
5.453848	231.678744	7.819981
5.455886	233.475640	7.824986
5.558054	225.256537	7.829990
5.689010	235.170360	7.834995
5.503567	224.582145	7.840000
5.441377	222.500873	7.845005
5.083604	228.422289	7.850010
5.509861	232.829613	7.855014
5.648731	236.354723	7.860019
5.682853	232.107148	7.865024
5.365076	221.947654	7.870029
4.865674	217.077649	7.875034
5.216091	225.176143	7.880038
5.231231	231.653253	7.885043
5.449162	229.335381	7.890048
5.331591	230.777585	7.895053
5.327471	226.659349	7.900058
5.599402	228.085200	7.905062
5.350347	237.694367	7.910067
5.602188	235.760348	7.915072
5.708406	233.380776	7.920077
5.388924	242.719343	7.925082
5.858242	224.063021	7.930086
5.404034	240.116920	7.935091
5.630784	231.527248	7.940096
5.409855	235.930937	7.945101
5.533225	234.421872	7.950106
5.875640	219.920251	7.955110
5.367415	220.898107	7.960115
5.527483	207.763124	7.965120
5.335297	204.654916	7.970125
5.164294	209.943338	7.975142
5.114983	213.678034	7.980160
5.349913	225.475244	7.985178
5.467918	229.594122	7.990195
5.594194	235.141207	7.995213
5.799153	236.283425	8.000230
5.787421	228.611037	8.005248
5.584420	215.190505	8.010266
5.460961	207.841616	8.015283
5.295369	209.884074	8.020301
5.019067	212.997744	8.025318
5.738886	223.697040	8.030336
5.487683	237.794656	8.035354
5.523833	229.559424	8.040371
5.487140	225.813352	8.045389
5.422324	222.264153	8.050406
5.779802	227.926707	8.055424
5.626053	223.397335	8.060442
5.398414	210.690656	8.065459
5.238879	215.379730	8.070477
5.395832	228.672222	8.075494
5.880240	220.506048	8.080512
5.780604	230.118023	8.085530
5.909299	220.773388	8.090547
5.392500	211.125341	8.095565
5.395871	209.402093	8.100582
5.362139	207.649910	8.105600
5.625726	224.602083	8.110618
5.770774	225.977677	8.115635
5.586712	232.440874	8.120653
5.424204	221.683683	8.125670
5.766732	221.090983	8.130688
5.633203	231.957860	8.135706
5.739500	231.253626	8.140723
5.301708	218.693264	8.145741
5.638147	224.075088	8.150758
5.682042	225.378074	8.155776
5.497299	233.204602	8.160794
5.679287	230.014582	8.165811
5.538756	232.848356	8.170829
5.402047	237.880999	8.175846
5.661982	233.255659	8.180864
5.612443	237.018796	8.185882
5.528893	232.642584	8.190899
5.475817	233.638796	8.195917
5.544727	233.902846	8.200934
5.688511	235.881360	8.205952
5.568443	238.651992	8.210970
5.628374	235.906983	8.215987
5.845380	221.726817	8.221005
5.351809	231.942894	8.226022
5.589407	236.693210	8.231040
5.618276	230.396659	8.236058
5.739109	228.645654	8.241075
5.698871	227.068041	8.246093
5.404156	234.918004	8.251110
5.836227	227.454211	8.256128
5.588885	234.044018	8.261146
5.521847	235.582015	8.266163
5.530151	235.972259	8.271181
5.787188	245.699113	8.276198
6.070398	240.521070	8.281216
5.910992	240.457773	8.286234
5.691802	241.445137	8.291251
6.038896	233.006865	8.296269
5.421422	241.156376	8.301286
5.547074	240.890915	8.306304
5.866380	248.449634	8.311322
5.808744	253.002939	8.316339
5.992422	249.642248	8.321357
5.789886	247.487180	8.326374
5.883455	235.014478	8.331392
5.706685	240.372077	8.336410
5.480005	238.369083	8.341427
5.802221	255.725543	8.346445
5.753696	256.604290	8.351462
6.168200	258.177760	8.356480
6.007843	252.314582	8.361498
5.814405	245.440449	8.366515
5.903720	242.974869	8.371533
5.491455	242.468132	8.376550
5.809937	254.883476	8.381568
5.971657	262.280555	8.386586
6.055289	267.114808	8.391603
5.903136	253.831489	8.396621
5.862875	259.574915	8.401638
6.066206	258.625212	8.406656
6.193426	246.238775	8.411674
5.847154	251.518633	8.416691
5.929018	236.999756	8.421709
5.517101	240.289171	8.426726
5.736324	247.560533	8.431744
6.006262	254.164477	8.436762
6.145423	255.121293	8.441779
6.046487	247.074333	8.446797
5.781350	247.964716	8.451814
6.130352	244.480462	8.456832
5.952026	236.692005	8.461850
6.181376	228.202644	8.466867
6.090949	229.665391	8.471885
5.292298	243.545309	8.476902
6.056393	249.340209	8.481920
6.304327	259.090577	8.486938
6.156276	255.358682	8.491955
5.729599	238.321908	8.496973
5.921205	243.921936	8.501990
6.001315	249.170119	8.507008
6.033747	259.064486	8.512026
6.196610	263.747555	8.517043
6.431271	247.204216	8.522061
6.071794	246.802862	8.527078
5.947526	242.997843	8.532096
6.211812	242.505682	8.537114
5.865437	245.210570	8.542131
6.029645	235.437545	8.547149
5.685411	245.838649	8.552166
6.158067	248.984028	8.557184
6.180046	245.771584	8.562202
5.779656	244.619252	8.567219
6.096639	249.764286	8.572237
5.983971	250.356391	8.577255
6.263311	252.490516	8.582272
6.202916	258.281254	8.587290
5.852980	250.992854	8.592307
6.054406	244.868235	8.597325
6.374409	258.523504	8.602343
6.459676	259.233105	8.607360
6.256547	251.842956	8.612378
5.840500	250.342788	8.617395
5.922526	235.713440	8.622413
6.114380	250.871794	8.627431
6.261322	248.674935	8.632448
6.335109	263.573989	8.637466
5.996179	253.740444	8.642483
6.205965	253.572330	8.647501
6.179161	252.724727	8.652519
6.054589	259.368008	8.657536
5.902678	258.864912	8.662554
5.815162	267.342153	8.667571
6.093550	259.397376	8.672589
6.128397	265.533028	8.677607
6.248901	255.668972	8.682624
6.412056	266.401319	8.687642
6.360640	269.852348	8.692659
6.597388	258.547007	8.697677
6.568829	260.782717	8.702695
6.062175	262.076756	8.707712
6.445674	257.201812	8.712730
6.226167	251.975812	8.717747
6.147420	232.647538	8.722765
6.024857	249.606212	8.727783
6.309915	254.636304	8.732800
6.550450	258.862336	8.737818
6.285216	258.020300	8.742835
5.950458	253.964045	8.747853
6.006099	254.880219	8.752871
6.316481	258.893416	8.757888
6.628463	259.924304	8.762906
6.356372	265.735383	8.767923
6.356397	260.648760	8.772941
5.987067	256.635755	8.777959
6.407003	261.250397	8.782976
6.606152	263.318118	8.787994
6.363159	263.775890	8.793011
6.536065	264.203619	8.798029
6.455758	256.765944	8.803047
5.892613	254.020119	8.808064
6.288691	251.371085	8.813082
6.436060	264.579893	8.818099
6.119658	268.734860	8.823117
6.330374	266.493358	8.828135
6.236014	267.265640	8.833152
6.355661	261.040146	8.838170
6.039496	271.140265	8.843187
6.442963	269.544055	8.848205
6.297795	265.180585	8.853223
6.340144	255.669504	8.858240
6.527106	256.653590	8.863258
6.474836	255.607992	8.868275
6.424155	276.629404	8.873293
6.128247	266.325277	8.878311
6.322450	265.020410	8.883328
6.403445	260.795287	8.888346
6.300316	267.551990	8.893363
5.861805	267.765664	8.898381
5.990839	265.445367	8.903399
6.229158	274.742831	8.908416
6.814528	278.375567	8.913434
6.465470	290.721311	8.918451
6.660814	286.920166	8.923469
6.799280	281.139833	8.928487
6.328163	279.815485	8.933504
6.654943	276.921630	8.938522
6.239390	279.138706	8.943539
6.574129	284.072715	8.948557
6.784213	291.011021	8.953575
6.356545	275.526933	8.958592
6.272194	271.898719	8.963610
6.680507	284.997491	8.968627
6.467571	289.950505	8.973645
6.919195	290.877606	8.978663
6.337609	284.792841	8.983680
6.844387	273.820965	8.988698
6.766875	289.030759	8.993715
6.490010	272.731132	8.998733
6.518549	272.013758	9.003751
6.241391	269.135046	9.008768
6.888688	283.689217	9.013786
6.675757	289.273354	9.018803
6.410599	273.517827	9.023821
6.646855	280.739216	9.028839
6.882607	283.621703	9.033856
6.871372	274.100022	9.038874
6.575954	273.082814	9.043891
6.309090	265.017813	9.048909
6.735997	265.961384	9.053927
6.554405	271.761530	9.058944
6.504169	269.431277	9.063962
6.688857	280.097167	9.068979
6.794212	286.196604	9.073997
6.789272	273.499385	9.079015
6.616774	278.439788	9.084032
6.468089	270.413185	9.089050
6.682412	286.202351	9.094067
6.896241	289.287057	9.099085
7.019325	281.751436	9.104103
6.524274	279.092830	9.109120
6.649533	268.275028	9.114138
6.502590	275.376208	9.119155
6.844656	285.124556	9.124173
6.889420	282.123140	9.129191
6.685591	281.053804	9.134208
6.779167	279.266015	9.139226
6.642071	288.066548	9.144243
6.908552	277.838944	9.149261
6.943173	281.645787	9.154279
6.549901	279.731839	9.159296
6.768596	281.215884	9.164314
6.528221	287.347061	9.169331
7.002923	288.115944	9.174349
7.009951	288.276027	9.179367
6.679551	297.750409	9.184384
7.087419	297.194868	9.189402
6.751861	284.037907	9.194419
6.313044	291.922953	9.199437
6.693063	282.242526	9.204455
6.730773	290.353162	9.209472
6.777627	291.728272	9.214490
6.786406	299.512076	9.219507
6.749366	296.889446	9.224525
6.987635	282.970994	9.229543
6.630423	305.207747	9.234560
6.931718	290.601015	9.239578
6.564693	297.165301	9.244595
6.737114	294.286011	9.249613
6.925900	295.471774	9.254631
6.827900	293.467672	9.259648
7.118838	290.162854	9.264666
7.023162	295.706647	9.269683
7.104777	296.445220	9.274701
7.297964	289.473005	9.279719
6.935679	292.117266	9.284736
6.761289	283.514024	9.289754
7.025140	300.153821	9.294771
6.660887	303.312757	9.299789
6.849249	289.730255	9.304807
7.054063	296.085593	9.309824
7.001164	299.079293	9.314842
7.374971	298.188247	9.319859
6.922979	297.548846	9.324877
7.013137	295.963548	9.329895
6.754202	302.419493	9.334912
6.896501	292.394242	9.339930
6.831614	291.767149	9.344947
6.820631	299.711812	9.349965
6.898352	296.045736	9.354983
6.762606	302.359432	9.360000
6.886761	288.190514	9.365018
6.874051	297.662767	9.370035
6.665132	318.967627	9.375053
7.163803	301.963433	9.380071
7.201802	322.759665	9.385088
7.089510	320.672584	9.390106
6.862593	314.008752	9.395123
6.692819	321.416445	9.400141
7.382979	309.936340	9.405159
7.307401	319.352125	9.410176
7.120704	313.540363	9.415194
6.988699	309.591375	9.420211
7.049354	321.018174	9.425229
7.649304	313.250512	9.430247
7.036949	309.868591	9.435264
7.080992	319.432999	9.440282
7.391466	312.142730	9.445299
7.016924	317.695237	9.450317
7.477213	314.771123	9.455335
6.976653	323.770267	9.460352
7.257030	309.283535	9.465370
7.151041	315.769318	9.470387
6.952698	321.272303	9.475405
7.061535	312.492414	9.480423
7.192571	323.068859	9.485440
6.959128	311.271833	9.490458
7.102551	316.541734	9.495475
7.148323	317.727676	9.500493
7.527899	310.221533	9.505511
6.986165	319.201840	9.510528
6.944164	322.222248	9.515546
7.293899	317.917401	9.520563
7.233482	324.607519	9.525581
7.449818	319.900587	9.530599
6.973140	327.558028	9.535616
7.409950	318.108567	9.540634
7.299852	312.489995	9.545651
7.268876	318.061589	9.550669
7.236393	316.164043	9.555687
7.050429	317.016857	9.560704
7.255001	308.667008	9.565722
7.251031	315.206330	9.570739
6.876994	326.167512	9.575757
7.362284	314.744546	9.580775
7.226426	324.277010	9.585792
7.237039	317.910691	9.590810
7.644474	334.909996	9.595827
7.362560	328.917405	9.600845
7.556136	321.594842	9.605863
7.207573	317.332450	9.610880
7.010835	319.837337	9.615898
7.397356	331.812976	9.620915
7.456168	345.856098	9.625933
7.602529	344.394581	9.630951
7.386390	336.924376	9.635968
7.422076	340.311367	9.640986
7.793613	338.186820	9.646003
7.415476	332.742511	9.651021
7.440322	318.661611	9.656039
7.334913	328.908821	9.661056
7.163373	325.300482	9.666074
7.392433	338.357778	9.671091
7.143912	345.165549	9.676109
7.767585	344.503827	9.681127
7.639279	348.771530	9.686144
7.391358	338.119081	9.691162
7.386025	344.604980	9.696179
7.841359	355.872527	9.701197
7.595342	339.912000	9.706215
7.404689	326.394793	9.711232
7.232603	339.924780	9.716250
7.547266	339.446862	9.721267
7.523122	348.255083	9.726285
7.579769	345.447456	9.731303
7.709171	340.252308	9.736320
7.854555	347.592009	9.741338
7.585795	345.027540	9.746355
7.330455	340.226793	9.751373
7.795822	343.408037	9.756391
7.520506	333.633967	9.761408
7.065140	339.956417	9.766426
7.351794	334.951370	9.771443
7.604643	346.212569	9.776461
7.571966	345.132359	9.781479
7.960905	345.640058	9.786496
7.618297	350.004240	9.791514
7.522622	342.922353	9.796531
7.747221	343.509284	9.801549
7.591967	344.982134	9.806567
7.713938	342.240072	9.811584
7.780271	350.226364	9.816602
7.910567	337.681604	9.821619
7.765423	352.520149	9.826637
7.813405	348.218099	9.831655
7.898217	350.265765	9.836672
7.450159	347.318979	9.841690
7.713351	344.955694	9.846707
7.484196	346.616766	9.851725
7.595038	342.812987	9.856743
7.496063	346.823672	9.861760
7.497659	353.999580	9.866778
7.437967	340.200055	9.871795
7.507859	347.059230	9.876813
7.646345	348.511591	9.881831
7.961192	341.889623	9.886848
8.041408	355.910486	9.891866
8.112511	343.873528	9.896883
7.757455	348.103956	9.901901
7.427820	350.910390	9.906919
7.497786	344.143522	9.911936
7.352017	349.108183	9.916954
7.873168	344.694595	9.921971
7.903177	342.108854	9.926989
7.691035	345.682747	9.932007
7.883314	344.378174	9.937024
7.756229	346.632391	9.942042
7.692754	338.687160	9.947059
7.815724	359.192509	9.952077
7.922429	357.888636	9.957095
8.311894	360.554709	9.962112
8.061238	362.215974	9.967130
8.226703	349.290209	9.972147
7.723425	344.679535	9.977165
7.690227	343.571005	9.982183
7.794778	343.580213	9.987200
7.680555	343.001823	9.992218
8.476381	348.460474	9.997235
7.816658	348.247868	10.002253
7.818857	349.510021	10.007271
7.899175	343.218042	10.012288
7.721719	337.963381	10.017306
8.012788	355.151227	10.022323
8.219791	367.612409	10.027341
7.918744	364.800513	10.032359
8.234530	365.714057	10.037376
8.245821	356.920932	10.042394
8.195565	348.639141	10.047411
7.815436	349.531655	10.052429
7.683230	344.913695	10.057447
8.193104	345.939022	10.062464
7.941661	351.955186	10.067482
8.044923	347.909602	10.072499
7.727199	354.920645	10.077517
7.871764	363.683673	10.082535
8.600557	362.869891	10.087552
8.446744	365.951893	10.092570
8.590705	351.962868	10.097587
8.450721	356.481686	10.102605
8.058310	352.626879	10.107623
8.151915	344.363714	10.112640
7.788327	353.250034	10.117658
8.110860	344.733486	10.122675
8.196177	347.910791	10.127693
8.305484	347.821433	10.132711
8.053149	345.566815	10.137728
7.984444	349.579098	10.142746
7.792689	348.962290	10.147763
7.880886	354.083018	10.152781
7.903675	353.527475	10.157799
8.470688	361.363238	10.162816
8.316241	360.794266	10.167834
8.501593	358.152780	10.172851
7.980156	357.129734	10.177869
8.060000	355.208383	10.182887
8.251413	347.504314	10.187904
7.762697	352.279388	10.192922
8.422333	362.915559	10.197939
8.103619	371.905348	10.202957
8.211461	373.460307	10.207975
8.226132	367.749711	10.212992
8.265682	373.464969	10.218010
8.497311	373.258741	10.223027
8.356021	372.258553	10.228045
8.486360	379.524874	10.233063
8.796274	361.590697	10.238080
7.973435	359.863537	10.243098
7.818071	352.140879	10.248115
7.988559	371.313476	10.253133
8.227657	369.645025	10.258151
8.599720	368.609088	10.263168
8.617785	373.437800	10.268186
8.733763	371.772740	10.273203
8.677948	368.405136	10.278221
7.874134	363.926452	10.283239
8.362464	362.900814	10.288256
8.282829	366.738088	10.293274
8.437312	369.999296	10.298291
8.298751	374.240201	10.303309
8.108590	378.350292	10.308327
8.139873	381.561261	10.313344
8.490754	370.474751	10.318362
8.120905	372.413338	10.323379
8.265137	364.085480	10.328397
8.345201	370.924147	10.333415
8.179555	372.001007	10.338432
8.221430	369.000026	10.343450
7.963952	373.395138	10.348467
8.547113	383.806555	10.353485
8.735967	392.988713	10.358503
8.600057	384.224805	10.363520
8.415244	380.848883	10.368538
8.688357	386.669784	10.373555
8.733386	376.078992	10.378573
8.262203	380.229683	10.383591
8.393817	376.173367	10.388608
8.514101	386.432804	10.393626
8.622056	393.753106	10.398643
8.809360	393.200348	10.403661
8.482787	380.253344	10.408679
8.548369	376.049527	10.413696
8.832524	383.534886	10.418714
8.835198	388.766765	10.423731
8.677813	381.451487	10.428749
8.460380	381.914748	10.433767
8.268224	370.332150	10.438784
8.334066	380.798866	10.443802
8.745502	403.919559	10.448819
9.133296	386.399244	10.453837
8.600740	385.573577	10.458855
8.689058	379.327675	10.463872
8.421430	381.985611	10.468890
8.675951	386.910048	10.473907
8.730156	387.062787	10.478925
8.564014	391.270123	10.483943
8.963438	388.355473	10.488960
8.806927	390.415472	10.493978
8.857521	380.461251	10.498995
9.019916	374.102837	10.504013
8.727623	368.755598	10.509031
8.641971	370.293349	10.514048
8.262635	371.952560	10.519066
8.648548	381.081941	10.524083
9.197293	389.302394	10.529101
8.959831	388.320334	10.534119
8.789507	384.418319	10.539136
8.584954	384.794373	10.544154
8.893642	383.859817	10.549171
8.949418	375.735064	10.554189
8.505613	385.886678	10.559207
8.675217	383.935571	10.564224
8.720174	392.742522	10.569242
8.832676	398.885063	10.574259
9.163569	395.687608	10.579277
9.014082	398.888857	10.584295
8.996179	400.775805	10.589312
8.983269	395.886807	10.594330
8.907370	396.318566	10.599347
8.874210	381.227374	10.604365
8.846009	390.875649	10.609383
9.316220	391.433808	10.614400
8.958621	385.557117	10.619418
8.536375	381.899443	10.624435
9.081817	384.743196	10.629453
8.751109	393.116357	10.634471
8.879571	388.732342	10.639488
8.905376	393.698703	10.644506
8.839608	399.111646	10.649523
8.843271	395.734778	10.654541
8.874798	392.252590	10.659559
8.851041	400.713656	10.664576
8.896554	404.771282	10.669594
8.574211	400.908710	10.674611
8.886068	389.143490	10.679629
9.015241	398.527437	10.684647
8.833842	401.370756	10.689664
8.840004	399.628122	10.694682
8.888508	403.909332	10.699699
9.089877	397.260833	10.704717
8.973857	407.121595	10.709735
8.735847	407.449213	10.714752
9.220220	417.121831	10.719770
8.922570	430.617791	10.724787
9.308371	426.925811	10.729805
9.420650	423.674030	10.734823
9.219492	415.333656	10.739840
9.102451	405.200405	10.744858
8.798520	404.515857	10.749875
9.369091	410.161070	10.754893
9.340680	419.799926	10.759911
9.083256	411.676587	10.764928
8.626140	407.800285	10.769946
9.053212	421.899733	10.774963
9.466478	416.332179	10.779981
9.397842	418.495258	10.784999
9.194125	423.188110	10.790016
9.002977	416.436624	10.795034
9.303934	420.053714	10.800051
9.403462	421.553170	10.805069
9.617686	416.152299	10.810087
9.293114	419.096804	10.815104
9.078241	407.808038	10.820122
8.989928	423.224744	10.825139
9.099317	416.552691	10.830157
9.314986	411.899485	10.835175
9.651743	420.935559	10.840192
9.246577	417.770655	10.845210
9.262365	413.890147	10.850227
9.487248	411.132051	10.855245
9.419110	418.716454	10.860263
9.288077	414.959786	10.865280
9.653519	418.825599	10.870298
9.219303	426.908794	10.875315
9.333173	419.620690	10.880333
9.439005	414.927783	10.885351
9.224107	416.952696	10.890368
8.888252	420.003095	10.895386
9.401340	420.381018	10.900403
9.468483	412.200833	10.905421
9.338569	408.986763	10.910439
9.386674	414.707013	10.915456
9.866717	412.934774	10.920474
9.253855	418.470772	10.925491
9.719200	419.566150	10.930509
9.388936	426.405613	10.935527
9.026078	413.505258	10.940544
9.303547	405.267084	10.945562
9.396940	417.752300	10.950579
9.465328	410.717422	10.955597
9.324014	419.607035	10.960615
9.372692	427.176409	10.965632
9.295396	416.068179	10.970650
9.287618	423.163528	10.975667
9.525394	428.421928	10.980685
9.834670	441.716107	10.985703
9.880844	437.180799	10.990720
9.570098	427.661489	10.995738
9.373126	427.850181	11.000755
9.622518	416.934071	11.005773
9.540986	430.983332	11.010791
9.805366	438.443392	11.015808
9.771739	424.071726	11.020826
9.416233	425.559983	11.025843
9.749273	431.119115	11.030861
9.695838	424.273605	11.035879
9.297024	434.932612	11.040896
10.043532	441.913684	11.045914
9.689801	447.336765	11.050931
9.619182	438.490085	11.055949
9.847457	433.655039	11.060967
9.932219	430.243447	11.065984
9.906279	429.165338	11.071002
9.541663	425.981497	11.076019
9.643474	422.914373	11.081037
9.697020	416.897923	11.086055
9.823616	431.435462	11.091072
9.677963	421.833649	11.096090
9.653147	422.999033	11.101107
10.049868	440.470299	11.106125
9.742143	434.749921	11.111143
9.910636	430.530068	11.116160
9.812578	430.993678	11.121178
9.744512	437.792322	11.126195
9.795867	433.376122	11.131213
10.243773	433.836774	11.136231
9.934588	422.051468	11.141248
10.141333	418.986941	11.146266
9.913258	422.547552	11.151283
9.916081	419.994433	11.156301
9.923697	421.334639	11.161319
9.491669	415.627309	11.166336
9.669024	421.068675	11.171354
9.806654	430.867868	11.176371
10.018979	433.971766	11.181389
9.953342	442.972678	11.186407
9.788134	450.871996	11.191424
10.314112	442.162788	11.196442
10.068807	453.012490	11.201459
9.487413	433.907418	11.206477
10.137309	437.934064	11.211495
9.611348	444.024556	11.216512
10.087508	439.106734	11.221530
10.320756	444.223839	11.226547
10.296995	453.334995	11.231565
10.052475	439.295939	11.236583
10.066109	448.066771	11.241600
10.238239	443.849505	11.246618
10.140825	442.596340	11.251635
9.825174	424.273529	11.256653
10.130835	434.317947	11.261671
10.272821	440.967128	11.266688
10.154926	438.959797	11.271706
10.260333	438.542858	11.276723
9.988093	438.440326	11.281741
10.017470	431.342090	11.286759
9.977718	448.688826	11.291776
10.218521	442.545387	11.296794
10.442516	446.057706	11.301811
10.436230	438.403313	11.306829
10.223343	426.776571	11.311847
10.074490	427.424806	11.316864
10.368957	424.558049	11.321882
9.923977	431.276526	11.326899
10.049984	432.872840	11.331917
10.576315	443.141670	11.336935
10.295613	438.568896	11.341952
10.291318	437.414837	11.346970
10.197962	434.677885	11.351987
10.429178	440.435903	11.357005
10.257825	431.314590	11.362023
10.040644	442.396580	11.367040
10.336096	437.986553	11.372058
10.335895	446.617535	11.377075
10.335015	445.478722	11.382093
10.424687	441.873868	11.387111
10.602156	451.581667	11.392128
10.426415	439.469474	11.397146
10.169390	426.694636	11.402163
10.031847	435.315438	11.407181
10.532460	437.329932	11.412199
10.237890	448.726918	11.417216
10.330898	449.148158	11.422234
10.509871	445.576734	11.427251
10.357838	447.449859	11.432269
10.513368	443.913643	11.437287
9.997845	446.026389	11.442304
10.607684	447.162384	11.447322
10.494670	445.447768	11.452339
10.304482	442.334590	11.457357
10.488896	443.284370	11.462375
10.364338	443.692150	11.467392
10.438060	445.886714	11.472410
10.424955	443.954580	11.477427
10.277685	448.282061	11.482445
10.606938	442.377302	11.487463
10.147036	442.783647	11.492480
10.599731	435.379670	11.497498
10.922346	453.664022	11.502515
10.535972	452.061391	11.507533
10.544508	444.284773	11.512551
10.428613	455.177440	11.517568
10.214679	445.217035	11.522586
10.598763	434.478749	11.527603
10.376649	448.581470	11.532621
10.552477	439.746908	11.537639
10.822452	466.824807	11.542656
10.633788	456.598541	11.547674
10.812988	448.937353	11.552691
10.487530	443.809841	11.557709
10.713920	459.647772	11.562727
10.774564	464.466724	11.567744
10.705210	453.303588	11.572762
10.730925	452.245837	11.577779
10.425357	453.120435	11.582797
10.659065	465.018976	11.587815
10.885632	466.596482	11.592832
11.037663	473.695370	11.597850
10.730669	463.086755	11.602867
10.810197	471.213052	11.607885
10.904561	465.070315	11.612903
10.687466	455.012571	11.617920
10.700459	459.719026	11.622938
10.296007	465.819009	11.627955
10.756142	474.555047	11.632973
11.193157	471.344211	11.637991
10.723683	468.429140	11.643008
10.448872	463.199066	11.648026
10.699693	466.757703	11.653043
10.348503	474.585007	11.658061
10.863430	471.507200	11.663079
10.672937	470.716629	11.668096
10.836573	481.774064	11.673114
11.014064	467.691370	11.678131
10.724516	477.386693	11.683149
11.092392	471.895613	11.688167
10.886550	476.771838	11.693184
11.213136	476.203703	11.698202
11.266131	471.074059	11.703219
10.839765	480.140621	11.708237
10.746302	478.258863	11.713255
10.852617	475.383525	11.718272
10.712130	482.830904	11.723290
11.001791	490.006195	11.728307
11.205476	491.994346	11.733325
11.159857	496.684691	11.738343
11.635031	493.105009	11.743360
11.109535	484.565803	11.748378
11.179462	475.952830	11.753395
10.848294	476.468515	11.758413
11.290313	467.740810	11.763431
11.148319	473.067819	11.768448
11.130603	471.587659	11.773466
11.404642	475.776969	11.778483
11.265182	469.616990	11.783501
11.481985	473.610095	11.788519
11.414827	472.172345	11.793536
11.258707	476.015239	11.798554
11.484522	465.620298	11.803571
11.129131	469.225986	11.808589
11.455918	466.972699	11.813607
11.415985	463.072454	11.818624
11.142037	467.454375	11.823642
11.498938	468.083825	11.828659
11.094904	470.778791	11.833677
11.191934	469.359657	11.838695
11.432512	475.005780	11.843712
11.235305	473.522009	11.848730
11.469760	463.176215	11.853747
11.184851	474.502289	11.858765
11.313520	466.284099	11.863783
11.411804	466.635093	11.868800
11.224847	475.244675	11.873818
11.396644	467.199642	11.878835
10.859537	473.115163	11.883853
11.104179	466.996363	11.888871
11.128875	463.698253	11.893888
11.139975	473.043821	11.898906
11.232521	464.547247	11.903923
10.993218	473.234403	11.908941
11.228424	481.494248	11.913959
11.520207	488.492492	11.918976
11.606398	491.634974	11.923994
11.687609	486.769164	11.929011
11.516382	484.669150	11.934029
11.440863	478.133156	11.939047
11.642773	478.752026	11.944064
11.248657	482.789760	11.949082
11.477462	475.827705	11.954099
11.808288	492.239514	11.959117
11.959257	488.199093	11.964135
11.570631	483.182385	11.969152
11.141434	482.075545	11.974170
11.195896	480.003505	11.979187
11.384826	487.327017	11.984205
11.774651	497.844339	11.989223
11.922984	495.868130	11.994240
11.577484	498.730704	11.999258
11.775783	498.012135	12.004275
11.713896	503.149963	12.009293
11.646536	497.411075	12.014311
11.627037	497.783564	12.019328
11.393473	499.483204	12.024346
11.502992	499.614709	12.029363
11.707970	498.803587	12.034381
11.775729	504.154749	12.039399
11.999401	500.399638	12.044416
11.700367	501.039702	12.049434
11.884200	496.735398	12.054451
11.722238	499.638820	12.059469
11.573852	501.274707	12.064487
11.693735	500.789245	12.069504
11.507763	504.217090	12.074522
11.616054	484.982491	12.079539
11.865272	495.815181	12.084557
11.674019	498.678984	12.089575
11.683592	497.816238	12.094592
11.596051	499.493143	12.099610
11.674018	493.412907	12.104627
11.588859	496.957592	12.109645
11.764996	497.990711	12.114663
12.017259	492.463979	12.119680
11.176433	488.820964	12.124698
12.090699	502.809910	12.129715
12.109215	510.589134	12.134733
12.139674	514.592327	12.139751
11.959244	505.652262	12.144768
11.822432	513.449361	12.149786
11.983810	505.279706	12.154803
12.188686	516.012019	12.159821
11.833084	516.828142	12.164839
11.990142	513.660887	12.169856
11.977141	517.724493	12.174874
11.937917	517.756086	12.179891
12.136787	517.394018	12.184909
11.955116	517.996876	12.189927
12.246514	514.426869	12.194944
11.947252	521.725423	12.199962
11.841819	511.479856	12.204979
11.891090	518.506403	12.209997
11.996471	508.086009	12.215015
12.377168	515.038863	12.220032
12.301086	522.037594	12.225050
12.140669	523.561753	12.230067
12.110181	528.369665	12.235085
12.184457	519.617145	12.240103
12.173942	515.286294	12.245120
12.063575	519.185187	12.250138
11.970047	514.864106	12.255155
12.104959	512.132625	12.260173
12.218633	524.491688	12.265191
12.100290	511.824578	12.270208
12.029815	512.744623	12.275226
11.954447	511.469087	12.280243
12.510033	518.003410	12.285261
12.445343	520.187977	12.290279
12.348775	506.330951	12.295296
11.712996	521.533193	12.300314
12.289996	522.677462	12.305331
12.364066	516.903924	12.310349
12.128147	517.534162	12.315367
12.583584	527.545847	12.320384
12.480282	534.643490	12.325402
12.364259	516.908013	12.330419
12.099990	521.824903	12.335437
12.268364	530.470702	12.340455
12.697207	528.419258	12.345472
12.687192	537.635610	12.350490
12.852511	533.564543	12.355507
12.564033	519.936193	12.360525
12.220276	523.375986	12.365543
12.015209	529.479659	12.370560
12.374811	528.988428	12.375578
12.388510	537.844497	12.380595
12.454418	542.403886	12.385613
12.455444	546.869241	12.390631
12.704781	539.708313	12.395648
12.759474	545.089922	12.400666
12.779822	538.507423	12.405683
13.170082	538.317519	12.410701
12.873176	530.206584	12.415719
12.894654	524.144600	12.420736
12.191188	523.036281	12.425754
12.432965	520.297627	12.430771
12.442352	523.871777	12.435789
12.306774	523.852103	12.440807
12.778211	527.537342	12.445824
12.823729	540.143702	12.450842
12.629666	533.010790	12.455859
12.896437	534.197050	12.460877
12.763667	536.477421	12.465895
12.573286	525.831679	12.470912
12.782912	532.413561	12.475930
12.597404	535.125003	12.480947
12.906958	535.894365	12.485965
12.661173	534.648517	12.490983
12.869285	543.616324	12.496000
12.785612	545.687090	12.501018
12.638731	538.108191	12.506035
13.017889	534.448780	12.511053
12.853929	537.709109	12.516071
12.767970	535.580034	12.521088
12.704808	545.833413	12.526106
12.753163	543.995836	12.531123
12.653891	546.668608	12.536141
13.033860	542.030811	12.541159
13.201511	530.515158	12.546176
12.883948	544.462410	12.551194
12.908281	542.104732	12.556211
12.938023	536.416981	12.561229
12.972589	535.843820	12.566247
13.086324	534.816538	12.571264
13.004609	537.890501	12.576282
12.681729	543.861050	12.581299
13.136459	543.307673	12.586317
13.248907	540.791115	12.591335
13.352914	539.967311	12.596352
12.961351	533.758202	12.601370
12.824411	542.240114	12.606387
13.255414	537.367164	12.611405
12.737566	544.119118	12.616423
12.851672	532.936834	12.621440
13.025629	542.184502	12.626458
12.740278	541.127843	12.631475
13.050061	541.010426	12.636493
12.708171	538.574075	12.641511
13.279740	541.599970	12.646528
12.994180	547.807696	12.651546
12.998046	552.796451	12.656563
13.221242	556.627640	12.661581
13.332136	568.343409	12.666599
13.560317	562.848806	12.671616
13.089513	557.021241	12.676634
13.029898	555.260432	12.681651
13.263468	551.822492	12.686669
13.116103	561.255892	12.691687
13.320792	570.653418	12.696704
13.522046	561.890574	12.701722
13.190835	565.905909	12.706739
13.666480	569.309647	12.711757
13.411434	568.185153	12.716775
13.811502	563.143451	12.721792
12.966148	551.211174	12.726810
13.112140	545.574746	12.731827
13.334532	559.144462	12.736845
13.304637	567.259439	12.741863
13.272479	570.486630	12.746880
13.354604	569.782991	12.751898
13.253747	568.568222	12.756915
13.693514	567.777343	12.761933
13.344825	569.097299	12.766951
13.536088	557.423325	12.771968
13.634753	562.791782	12.776986
13.182435	563.206416	12.782003
13.892282	561.382605	12.787021
12.979358	564.784796	12.792039
13.145330	565.614384	12.797056
13.646788	568.307231	12.802074
13.319878	571.207945	12.807091
13.301905	568.743246	12.812109
13.058110	574.000932	12.817127
13.641702	581.222011	12.822144
13.868347	581.796009	12.827162
13.882135	589.402442	12.832179
13.896913	583.906347	12.837197
13.662871	579.711265	12.842215
13.714331	562.464040	12.847232
13.552699	571.334802	12.852250
13.455979	575.537683	12.857267
13.999889	575.052468	12.862285
13.940597	571.574919	12.867303
13.897008	571.992184	12.872320
13.884251	563.158522	12.877338
13.721158	565.752875	12.882355
13.719115	565.444178	12.887373
13.597479	566.848698	12.892391
14.023826	562.948414	12.897408
13.984469	564.100292	12.902426
13.639042	563.816657	12.907443
14.211938	559.701061	12.912461
13.948232	566.482879	12.917479
13.843303	559.932500	12.922496
13.450222	558.895768	12.927514
13.832551	565.586467	12.932531
14.103381	573.847120	12.937549
13.973407	574.385129	12.942567
13.960126	576.227196	12.947584
14.505273	572.201120	12.952602
14.102507	572.134688	12.957619
13.971772	567.349191	12.962637
13.833887	568.090394	12.967655
13.838793	565.865120	12.972672
13.957051	565.635519	12.977690
13.890477	584.851568	12.982707
14.143409	578.204440	12.987725
14.243974	579.987759	12.992743
14.185080	581.489804	12.997760
13.942647	573.752205	13.002778
13.935785	586.717034	13.007795
14.154271	577.080532	13.012813
14.270210	584.484873	13.017831
13.931179	590.874502	13.022848
13.924086	591.465959	13.027866
14.312055	594.151235	13.032883
14.373633	585.978148	13.037901
14.265648	597.519740	13.042919
13.928964	591.087481	13.047936
14.185366	592.477323	13.052954
14.174104	595.843271	13.057971
14.556838	586.749214	13.062989
14.314924	594.445952	13.068007
14.083418	590.098999	13.073024
14.402944	594.887146	13.078042
14.200573	594.953608	13.083059
14.059518	580.642721	13.088077
14.024407	591.914198	13.093095
13.888315	590.140047	13.098112
14.150948	592.119031	13.103130
14.096786	602.128054	13.108147
14.215565	606.205875	13.113165
14.327054	608.388267	13.118183
14.470771	614.791100	13.123200
14.852897	609.909963	13.128218
14.460217	623.045338	13.133235
14.530568	609.092817	13.138253
14.706801	610.154330	13.143271
14.618922	601.165094	13.148288
14.490602	585.558392	13.153306
14.239725	599.627842	13.158323
14.579494	605.220694	13.163341
14.972217	610.382442	13.168359
14.162835	615.068662	13.173376
14.660976	609.424720	13.178394
14.629330	616.975125	13.183411
14.908588	609.023746	13.188429
14.478311	605.572395	13.193447
14.760940	619.120155	13.198464
15.141328	608.944052	13.203482
14.655334	600.755232	13.208499
14.533135	588.524151	13.213517
14.243182	594.527458	13.218535
14.700002	611.623477	13.223552
14.774481	608.241853	13.228570
14.866549	609.903426	13.233587
14.962704	603.820321	13.238605
14.783538	609.677001	13.243623
14.959749	614.632628	13.248640
15.094323	601.667310	13.253658
14.436786	600.895804	13.258675
14.508622	599.376445	13.263693
14.851474	606.934807	13.268711
14.669726	622.877454	13.273728
15.031859	613.269058	13.278746
14.659402	617.619018	13.283763
14.469408	612.186353	13.288781
14.863943	615.432321	13.293799
14.833598	621.237433	13.298816
14.920685	612.751105	13.303834
14.670728	620.701561	13.308851
14.736899	613.398715	13.313869
14.813890	618.685361	13.318887
14.342223	614.363172	13.323904
14.985905	625.071410	13.328922
15.166823	633.021055	13.333939
15.048169	643.008585	13.338957
15.102501	643.338025	13.343975
15.016631	643.809210	13.348992
15.264471	633.871473	13.354010
15.216107	636.990750	13.359027
15.236352	642.595495	13.364045
15.417081	640.014646	13.369063
14.957573	643.463016	13.374080
15.150430	638.018070	13.379098
15.134700	636.629102	13.384115
15.316928	632.760501	13.389133
15.399541	630.870246	13.394151
15.481457	638.715391	13.399168
15.395504	633.149761	13.404186
15.052638	630.517896	13.409203
15.073607	633.818875	13.414221
15.114023	638.874545	13.419239
15.467909	647.046565	13.424256
15.097084	636.365737	13.429274
15.373819	643.088684	13.434291
15.435749	647.049139	13.439309
15.247705	640.495892	13.444327
14.963137	638.293590	13.449344
15.594570	639.486195	13.454362
15.322042	642.943321	13.459379
15.387285	638.351346	13.464397
15.079472	634.076221	13.469415
14.877459	636.847051	13.474432
15.019725	639.094080	13.479450
15.469798	646.793549	13.484467
15.380274	658.852996	13.489485
15.782988	660.078057	13.494503
15.514527	659.678299	13.499520
15.583122	647.313335	13.504538
15.452878	644.111897	13.509555
15.529834	651.822126	13.514573
16.015061	653.400400	13.519591
15.895522	646.328419	13.524608
15.972982	639.768547	13.529626
15.735865	635.299386	13.534643
15.566067	640.176354	13.539661
15.693844	633.318327	13.544679
15.305240	633.379073	13.549696
15.396902	630.502835	13.554714
15.579479	635.564771	13.559731
15.922257	643.489219	13.564749
16.129683	648.916505	13.569767
15.414038	644.758523	13.574784
16.062595	643.155678	13.579802
15.634059	636.217015	13.584819
15.683029	635.076740	13.589837
15.860032	642.301191	13.594855
16.017707	655.234140	13.599872
15.888763	638.305254	13.604890
15.778963	645.558582	13.609907
15.923513	650.298251	13.614925
16.068534	653.239105	13.619943
15.936410	656.791134	13.624960
15.939914	644.960151	13.629978
15.631350	648.388176	13.634995
15.894742	661.689665	13.640013
16.004633	658.299362	13.645031
15.787661	667.027315	13.650048
15.785798	672.562930	13.655066
15.932060	664.250395	13.660083
15.854850	663.659920	13.665101
16.013803	660.558613	13.670119
15.954855	663.666921	13.675136
16.031347	662.891575	13.680154
16.194557	666.467048	13.685171
16.170145	659.336072	13.690189
15.870442	658.521472	13.695207
15.841967	667.431507	13.700224
15.747202	663.015911	13.705242
16.056819	669.228838	13.710259
16.313499	676.699664	13.715277
16.319101	669.873269	13.720295
15.999864	671.327497	13.725312
16.652411	682.927451	13.730330
16.423581	676.860207	13.735347
16.303960	672.306473	13.740365
16.674435	658.212515	13.745383
16.661277	669.651030	13.750400
16.293958	664.577306	13.755418
16.230255	656.013453	13.760435
16.060417	659.044354	13.765453
16.114171	653.255001	13.770471
16.348942	655.124726	13.775488
15.886570	660.659457	13.780506
16.780395	674.708524	13.785523
16.638595	674.292201	13.790541
16.357229	662.474002	13.795559
16.488167	671.545405	13.800576
16.525386	674.225346	13.805594
16.621926	671.436701	13.810611
16.475400	674.053735	13.815629
16.699824	662.172565	13.820647
16.309639	669.027761	13.825664
16.461459	681.904839	13.830682
16.886973	679.894921	13.835699
16.843390	681.369346	13.840717
16.670547	664.734438	13.845735
16.682369	663.439004	13.850752
16.390085	663.828723	13.855770
16.569084	660.001642	13.860787
16.689508	673.842933	13.865805
16.760235	666.627715	13.870823
16.923418	680.314036	13.875840
16.823240	672.601580	13.880858
16.702264	658.776636	13.885875
16.443050	665.125463	13.890893
17.055386	665.582611	13.895911
16.740934	666.878309	13.900928
16.636478	677.564211	13.905946
17.030840	670.683598	13.910963
16.473482	675.778703	13.915981
16.877804	689.626295	13.920999
16.857773	689.137366	13.926016
16.886633	687.567888	13.931034
16.849898	691.603672	13.936051
16.818085	683.441925	13.941069
16.894108	677.617540	13.946087
16.746666	689.338899	13.951104
16.878646	690.978487	13.956122
17.250359	683.612262	13.961139
16.599283	689.586623	13.966157
17.050919	685.609794	13.971175
17.096733	691.851179	13.976192
16.840810	691.190702	13.981210
16.934278	677.004163	13.986227
16.486016	685.338961	13.991245
16.621563	691.395968	13.996263
17.136683	699.729095	14.001280
17.310738	705.363559	14.006298
17.555847	703.460619	14.011315
17.576402	699.033370	14.016333
17.123427	682.773409	14.021351
17.354243	696.619620	14.026368
17.275928	686.259280	14.031386
17.409817	683.010399	14.036403
17.035275	691.737650	14.041421
16.869365	686.910262	14.046439
17.241300	695.786370	14.051456
17.058672	705.569309	14.056474
17.445532	710.482699	14.061491
17.318448	716.148274	14.066509
17.505331	705.967531	14.071527
17.454217	711.378287	14.076544
17.045804	715.105885	14.081562
17.181587	706.359475	14.086579
17.238116	710.639510	14.091597
17.526133	706.571390	14.096615
17.362565	710.323979	14.101632
17.094345	707.513229	14.106650
17.189339	707.388229	14.111667
17.329914	711.308052	14.116685
17.442871	700.075352	14.121703
17.622915	705.715195	14.126720
17.329114	708.923190	14.131738
17.512877	697.067262	14.136755
17.278531	714.438244	14.141773
17.630747	721.676471	14.146791
17.729964	723.377965	14.151808
17.630539	736.407806	14.156826
17.622780	733.411336	14.161843
17.709185	737.415336	14.166861
17.934507	736.149770	14.171879
17.980142	731.623937	14.176896
17.683747	721.193393	14.181914
17.968108	712.243972	14.186931
17.739945	716.177027	14.191949
17.640413	705.889405	14.196967
17.656781	717.323354	14.201984
17.816362	723.666954	14.207002
17.964512	725.057883	14.212019
17.624292	735.954091	14.217037
17.959834	725.838551	14.222055
18.179417	730.487666	14.227072
18.123765	732.137538	14.232090
17.819747	713.203566	14.237107
17.791365	718.077472	14.242125
18.256967	724.256665	14.247143
18.180458	721.835772	14.252160
17.991854	713.187200	14.257178
18.072285	705.392963	14.262195
17.994033	708.810387	14.267213
17.894681	714.635740	14.272231
18.337496	718.893502	14.277248
18.060134	719.388192	14.282266
18.053044	716.978581	14.287283
17.990887	725.859177	14.292301
18.223953	726.435336	14.297319
18.697706	725.516087	14.302336
18.067330	718.321649	14.307354
17.960319	706.088123	14.312371
18.199875	711.441000	14.317389
18.170689	729.048288	14.322407
18.227159	729.809728	14.327424
18.068186	733.785662	14.332442
18.356193	729.739628	14.337459
18.600554	731.046153	14.342477
17.926949	732.435643	14.347495
18.103074	724.090029	14.352512
18.081485	726.930607	14.357530
18.266696	725.444077	14.362547
18.411158	728.224089	14.367565
18.182402	730.989630	14.372583
18.410221	730.935466	14.377600
18.083103	733.596405	14.382618
18.178081	734.575904	14.387635
18.211930	741.213633	14.392653
18.392111	753.638237	14.397671
18.892266	748.265329	14.402688
18.606787	757.931770	14.407706
18.749326	752.362084	14.412723
18.341533	743.293202	14.417741
18.434533	751.865640	14.422759
18.900248	755.255182	14.427776
18.718342	763.160393	14.432794
18.699000	746.959086	14.437811
18.460453	741.492917	14.442829
18.239891	749.265290	14.447847
18.471943	755.080082	14.452864
18.759664	757.812548	14.457882
18.845453	749.783935	14.462899
18.856131	760.404625	14.467917
18.725882	755.495929	14.472935
18.750063	754.940156	14.477952
18.674751	758.467582	14.482970
18.870871	755.489856	14.487987
19.013021	756.689223	14.493005
18.751785	762.798565	14.498023
19.033369	753.628656	14.503040
18.540811	755.984007	14.508058
19.154535	762.663999	14.513075
19.037378	747.402544	14.518093
18.770314	755.538755	14.523111
18.827232	752.409139	14.528128
18.837053	763.673729	14.533146
18.672894	757.479627	14.538163
18.895873	748.706997	14.543181
19.026769	761.076166	14.548199
19.129130	755.847239	14.553216
18.792524	757.373604	14.558234
18.735872	762.946180	14.563251
19.149096	768.840063	14.568269
19.103889	773.558818	14.573287
19.588808	778.337042	14.578304
19.495290	773.561473	14.583322
19.346894	756.809068	14.588339
19.179019	753.553510	14.593357
19.063593	761.574598	14.598375
19.086757	752.141977	14.603392
19.416171	768.835119	14.608410
19.259775	776.638537	14.613427
19.710510	770.197219	14.618445
18.969959	767.904955	14.623463
19.380735	761.580312	14.628480
19.190112	772.800379	14.633498
19.046001	770.582503	14.638515
19.674057	771.920805	14.643533
19.198814	780.291405	14.648551
19.633397	778.983788	14.653568
19.487238	777.867574	14.658586
19.324805	774.639566	14.663603
19.583421	772.469436	14.668621
19.577271	775.667370	14.673639
19.494344	773.673490	14.678656
19.054700	784.872378	14.683674
19.106643	778.641466	14.688691
19.696770	779.887848	14.693709
19.501966	780.000468	14.698727
19.320041	772.111354	14.703744
19.178328	777.293247	14.708762
19.580354	787.613187	14.713779
19.973785	789.237323	14.718797
19.786205	798.219532	14.723815
19.961527	789.558440	14.728832
19.973484	797.619670	14.733850
19.733419	788.127031	14.738867
19.816059	776.984207	14.743885
19.504086	772.886416	14.748903
19.912694	784.376099	14.753920
19.988600	786.488316	14.758938
19.904749	795.113556	14.763955
20.077674	789.961993	14.768973
20.110532	789.597366	14.773991
19.777003	780.258135	14.779008
19.621313	785.151880	14.784026
19.790217	791.251063	14.789043
19.854543	792.989555	14.794061
20.003100	804.696460	14.799079
20.065404	798.069464	14.804096
20.251134	797.261325	14.809114
20.143313	800.339397	14.814131
20.310693	801.143531	14.819149
20.191584	796.630709	14.824167
20.515502	800.357908	14.829184
20.112967	793.601322	14.834202
20.199037	792.928618	14.839219
20.419894	789.688266	14.844237
20.272667	784.286759	14.849255
19.846531	775.741409	14.854272
19.953269	782.298379	14.859290
20.013410	789.411701	14.864307
20.141975	793.178781	14.869325
20.346651	799.619526	14.874343
20.443068	797.723949	14.879360
20.560024	794.329365	14.884378
20.603567	793.347710	14.889395
20.496991	792.651353	14.894413
20.206876	795.325474	14.899431
20.080327	790.715985	14.904448
20.032347	787.075691	14.909466
20.126390	793.991238	14.914483
20.611741	790.422535	14.919501
20.459987	796.000461	14.924519
20.233349	799.018139	14.929536
20.480321	792.113092	14.934554
20.498581	792.703764	14.939571
20.487514	793.112815	14.944589
20.068042	798.836563	14.949607
20.695753	807.502495	14.954624
21.122731	814.565023	14.959642
20.928317	816.245974	14.964659
20.772432	801.205092	14.969677
20.260610	805.280158	14.974695
20.408845	805.651784	14.979712
20.853914	812.471659	14.984730
20.845446	820.091123	14.989747
21.157192	812.434389	14.994765
21.158748	815.624818	14.999783
20.904833	813.932103	15.004800
20.786729	799.065217	15.009818
20.534516	811.942181	15.014835
20.739053	806.681553	15.019853
20.938126	819.623955	15.024871
21.140977	826.721383	15.029888
21.007970	825.401152	15.034906
20.910030	826.259219	15.039923
21.290643	815.227763	15.044941
21.053929	826.414016	15.049959
21.008304	822.555604	15.054976
20.760944	814.386333	15.059994
20.927926	823.474291	15.065011
21.024219	814.339512	15.070029
20.985349	817.081812	15.075047
20.939846	822.179313	15.080064
21.180458	816.013685	15.085082
20.864448	823.621075	15.090099
20.945877	825.170718	15.095117
20.908686	826.909240	15.100135
20.807332	829.033283	15.105152
21.320139	833.242306	15.110170
21.316420	841.205013	15.115187
21.419150	836.310512	15.120205
21.717711	842.831327	15.125223
21.512170	836.814049	15.130240
21.621845	813.965579	15.135258
21.270498	819.931184	15.140275
21.687990	812.592492	15.145293
21.650109	811.216426	15.150311
21.754278	807.937436	15.155328
22.014420	812.349891	15.160346
21.344697	812.798379	15.165363
21.540093	809.561988	15.170381
21.555501	818.424242	15.175399
21.593950	819.500908	15.180416
21.921740	811.207376	15.185434
21.368977	824.203726	15.190451
21.548352	812.787049	15.195469
21.418537	810.857268	15.200487
21.356569	811.230065	15.205504
21.440298	804.116906	15.210522
21.717854	814.563537	15.215539
21.365714	814.413483	15.220557
21.363024	831.445562	15.225575
21.611806	833.972669	15.230592
21.968418	842.276895	15.235610
21.597600	835.408060	15.240627
22.058738	834.273025	15.245645
21.570965	837.527023	15.250663
21.952123	836.104646	15.255680
21.866235	836.178218	15.260698
22.015850	838.496710	15.265715
22.107627	837.324512	15.270733
22.200735	824.504340	15.275751
22.192788	835.787520	15.280768
22.261591	824.722558	15.285786
22.083101	834.350292	15.290803
22.510630	830.901034	15.295821
22.035303	819.529485	15.300839
21.774335	820.602278	15.305856
22.277968	823.051836	15.310874
22.574091	828.888234	15.315891
22.242319	822.231070	15.320909
21.899987	814.871826	15.325927
21.963923	823.167965	15.330944
22.065501	828.495025	15.335962
21.977873	826.700681	15.340979
22.041846	826.791945	15.345997
22.072893	823.631631	15.351015
21.548496	836.377427	15.356032
21.605344	832.320026	15.361050
21.685712	846.476949	15.366067
21.966362	851.163924	15.371085
22.383457	845.690313	15.376103
22.375351	853.227685	15.381120
22.447100	850.177792	15.386138
22.466483	851.945377	15.391155
22.708705	858.396076	15.396173
22.782775	854.553733	15.401191
22.704163	858.902180	15.406208
22.832113	858.554304	15.411226
22.757312	854.211290	15.416243
22.730443	854.988867	15.421261
23.073468	850.460882	15.426279
22.882793	860.494460	15.431296
22.935050	848.718865	15.436314
22.925546	852.633684	15.441331
22.675620	838.036591	15.446349
22.818699	836.742798	15.451367
22.997228	843.493735	15.456384
22.702613	828.417627	15.461402
22.458433	832.069186	15.466419
22.969097	839.500536	15.471437
22.894080	841.794045	15.476455
22.864456	852.146517	15.481472
23.027370	841.133162	15.486490
22.962626	846.842720	15.491507
23.056503	850.457427	15.496525
22.662387	843.967747	15.501543
22.781842	849.484529	15.506560
22.991385	838.924651	15.511578
22.867710	843.753469	15.516595
23.018233	842.546878	15.521613
23.118286	852.636169	15.526631
23.201283	855.760279	15.531648
23.204964	853.629832	15.536666
23.420239	853.214712	15.541683
23.080564	852.519933	15.546701
23.093376	846.247754	15.551719
22.877468	855.827678	15.556736
23.143235	851.131845	15.561754
23.063207	851.251841	15.566771
22.911423	851.326206	15.571789
22.703039	850.778238	15.576807
22.495188	857.081266	15.581824
23.191726	858.402602	15.586842
23.161021	868.562753	15.591859
23.239484	873.480025	15.596877
23.539586	870.505024	15.601895
23.196010	872.477442	15.606912
23.578280	875.255164	15.611930
23.745948	882.762026	15.616947
23.437687	876.577696	15.621965
23.590476	877.898489	15.626983
23.630626	878.356371	15.632000
23.678411	875.950817	15.637018
23.452152	870.930809	15.642035
23.777894	870.590005	15.647053
23.838332	861.066318	15.652071
23.710863	871.771699	15.657088
23.303364	871.936369	15.662106
23.633029	870.809179	15.667123
23.509698	861.686479	15.672141
24.084051	868.404199	15.677159
23.653440	871.573565	15.682176
23.511304	870.106432	15.687194
23.839243	874.360028	15.692211
23.937993	862.450955	15.697229
23.731662	863.572047	15.702247
23.797617	884.733803	15.707264
24.042318	881.950459	15.712282
24.181045	891.071253	15.717299
24.031003	877.604107	15.722317
24.144773	877.375200	15.727335
23.941829	871.508982	15.732352
23.734866	875.606024	15.737370
24.292060	883.052239	15.742387
24.338572	886.188345	15.747405
24.414185	877.337613	15.752423
24.147989	868.748382	15.757440
24.402920	868.825693	15.762458
24.324738	870.172979	15.767475
24.376970	867.861406	15.772493
24.298012	865.627063	15.777511
24.392841	871.403299	15.782528
24.461629	863.150070	15.787546
24.358277	871.406007	15.792563
24.398968	871.422002	15.797581
24.529310	861.158458	15.802599
24.220186	859.048311	15.807616
24.125161	855.143936	15.812634
24.301040	867.411503	15.817651
24.199705	861.365370	15.822669
24.234189	869.088618	15.827687
24.554833	886.007292	15.832704
24.574481	890.883235	15.837722
24.705144	883.399828	15.842739
24.514269	884.843554	15.847757
24.790015	889.720647	15.852775
24.469415	897.082636	15.857792
24.785066	883.552445	15.862810
24.952308	884.426030	15.867827
24.175536	881.580825	15.872845
24.687444	887.175367	15.877863
24.551483	888.976609	15.882880
24.912759	898.659190	15.887898
24.599684	889.689093	15.892915
24.639790	891.090545	15.897933
25.058172	888.188643	15.902951
24.444616	895.025056	15.907968
24.428205	893.071297	15.912986
24.556390	887.977164	15.918003
24.342663	890.838217	15.923021
24.960503	904.081545	15.928039
25.189959	916.173550	15.933056
25.442234	910.867590	15.938074
25.121816	891.762415	15.943091
24.965046	889.609610	15.948109
24.912845	884.994832	15.953127
24.936248	900.116853	15.958144
25.344458	907.718815	15.963162
25.223555	908.072387	15.968179
25.280298	914.924362	15.973197
25.532785	906.841322	15.978215
25.270305	898.734326	15.983232
24.807884	892.561369	15.988250
25.358734	903.287385	15.993267
25.163819	918.159397	15.998285
25.109046	908.631532	16.003303
25.253437	913.273469	16.008320
25.356982	910.177590	16.013338
25.511948	900.516090	16.018355
25.282046	917.324857	16.023373
25.661080	904.759905	16.028391
25.351737	912.928015	16.033408
25.416720	912.927606	16.038426
25.759993	918.396938	16.043443
25.897307	920.291332	16.048461
25.882714	911.277906	16.053479
25.712876	921.137865	16.058496
25.724529	915.045719	16.063514
25.655835	914.532803	16.068531
25.450556	926.383241	16.073549
25.665577	913.215826	16.078567
25.628811	902.334507	16.083584
25.722013	918.427109	16.088602
25.610314	908.930197	16.093619
25.482938	908.107689	16.098637
25.439315	912.652669	16.103655
25.695797	927.602727	16.108672
25.841877	934.002152	16.113690
25.797209	928.868648	16.118707
25.763935	939.032395	16.123725
26.358408	933.764665	16.128743
26.263573	933.328401	16.133760
25.795263	937.216845	16.138778
26.139154	935.033419	16.143795
26.309329	938.816142	16.148813
26.242325	923.155416	16.153831
25.916896	928.403825	16.158848
25.903174	928.346243	16.163866
26.211651	931.949645	16.168883
25.805787	930.545659	16.173901
26.131784	927.778052	16.178919
26.136234	930.314814	16.183936
25.869659	943.446569	16.188954
26.267463	932.282979	16.193971
26.136209	931.300130	16.198989
26.013801	931.666561	16.204007
26.360041	932.487033	16.209024
26.149396	934.956301	16.214042
26.419797	943.681088	16.219059
26.190316	951.088871	16.224077
26.466944	956.129944	16.229095
26.358125	958.630698	16.234112
26.249524	957.912559	16.239130
26.559852	956.103578	16.244147
26.636484	957.625579	16.249165
26.525261	951.880749	16.254183
26.971209	956.756607	16.259200
26.745914	958.786355	16.264218
27.104479	953.574284	16.269235
27.178877	950.792199	16.274253
27.057840	955.260882	16.279271
26.853487	956.271221	16.284288
26.257884	944.735284	16.289306
27.023998	947.712026	16.294323
27.230404	954.774239	16.299341
27.095719	949.739951	16.304359
26.789941	940.503609	16.309376
26.694928	942.989588	16.314394
26.987619	946.074753	16.319411
26.792046	949.422128	16.324429
27.034363	943.284593	16.329447
27.140726	946.534465	16.334464
27.130182	960.232272	16.339482
27.157503	947.835656	16.344499
26.823578	945.255999	16.349517
26.685177	951.292633	16.354535
26.798640	953.392711	16.359552
26.670453	954.832995	16.364570
26.893952	949.102322	16.369587
26.910570	966.456565	16.374605
26.972463	971.994970	16.379623
27.274083	973.055917	16.384640
27.292195	973.943258	16.389658
27.708946	973.244307	16.394675
27.335354	978.964125	16.399693
27.621000	979.879239	16.404711
27.579022	974.287720	16.409728
27.422464	972.990079	16.414746
27.792377	972.898012	16.419763
27.598954	978.147973	16.424781
27.736735	975.046753	16.429799
27.621860	980.458051	16.434816
27.612336	974.356560	16.439834
27.647087	971.492284	16.444851
27.531246	978.191276	16.449869
27.503582	976.706312	16.454887
27.467535	975.298391	16.459904
27.248282	973.373050	16.464922
27.452010	966.105446	16.469939
27.443403	979.566284	16.474957
27.732538	992.759873	16.479975
28.199587	995.448678	16.484992
27.855216	988.297959	16.490010
27.976710	988.029980	16.495027
28.145276	992.680796	16.500045
28.168538	995.034760	16.505063
28.310614	977.138720	16.510080
28.010649	974.459099	16.515098
28.293682	964.556723	16.520115
28.128726	960.155137	16.525133
28.094273	968.397236	16.530151
28.205082	965.536898	16.535168
27.900419	964.123464	16.540186
27.728909	961.919296	16.545203
28.087417	972.656368	16.550221
28.104920	985.245315	16.555239
28.530499	986.151266	16.560256
28.664841	991.640528	16.565274
28.249562	974.822173	16.570291
28.615545	970.397879	16.575309
28.195815	966.121165	16.580327
28.217799	963.757485	16.585344
28.296639	972.632030	16.590362
28.648372	983.442745	16.595379
28.641197	985.908743	16.600397
28.739091	989.409246	16.605415
28.980460	982.602826	16.610432
28.649273	977.750599	16.615450
28.725638	960.978785	16.620467
28.381280	964.283058	16.625485
28.227121	968.242515	16.630503
28.568267	968.562018	16.635520
28.786369	989.674965	16.640538
28.894068	976.776673	16.645555
28.772238	986.039068	16.650573
28.522740	994.750154	16.655591
28.923019	992.980812	16.660608
28.127409	990.340490	16.665626
28.637538	991.596187	16.670643
28.774127	990.451715	16.675661
28.211817	990.198684	16.680679
28.659783	991.473528	16.685696
29.238133	1002.207946	16.690714
29.368362	1011.216518	16.695731
29.501032	1015.342762	16.700749
29.258871	1010.019082	16.705767
29.360418	998.298828	16.710784
28.797001	992.125783	16.715802
29.048243	988.896443	16.720819
28.985071	1003.867933	16.725837
29.287723	1016.134799	16.730855
29.679551	1011.586552	16.735872
29.396699	1015.114784	16.740890
29.568511	1018.408128	16.745907
29.537856	999.582765	16.750925
29.202603	1004.785390	16.755943
29.233845	1000.596240	16.760960
29.297262	1012.073545	16.765978
29.551871	1011.096885	16.770995
29.527002	1013.862282	16.776013
29.281185	1015.636460	16.781031
29.377010	1004.021234	16.786048
29.482749	1011.730294	16.791066
29.435915	1011.996598	16.796083
29.622277	1007.373047	16.801101
29.370151	1006.361677	16.806119
30.026575	1005.798975	16.811136
30.022897	1018.173497	16.816154
29.882267	1011.761052	16.821171
29.844847	1007.535254	16.826189
29.944447	1009.123110	16.831207
30.053946	1003.536399	16.836224
29.661502	1006.942839	16.841242
30.014126	1009.343353	16.846259
29.942655	1001.329644	16.851277
29.855008	1013.259653	16.856295
29.818207	1012.287340	16.861312
29.620886	1001.367842	16.866330
29.891692	1004.797246	16.871347
29.786526	1005.337716	16.876365
29.850852	1019.705553	16.881383
30.105149	1023.203802	16.886400
30.288968	1033.510524	16.891418
30.231999	1028.158005	16.896435
30.422866	1025.651260	16.901453
30.279802	1031.808565	16.906471
30.593186	1018.123993	16.911488
30.425064	1021.119975	16.916506
30.022846	1025.244297	16.921523
30.403452	1021.748661	16.926541
30.241412	1030.768035	16.931559
30.434175	1024.685523	16.936576
30.288904	1019.637084	16.941594
30.487271	1023.740478	16.946611
30.784596	1017.995133	16.951629
30.437906	1036.441098	16.956647
30.458318	1027.166548	16.961664
30.181315	1022.630916	16.966682
30.369860	1020.916627	16.971699
30.620556	1027.340823	16.976717
30.375902	1028.070266	16.981735
30.729664	1027.340095	16.986752
30.941040	1039.018440	16.991770
30.829531	1038.550056	16.996787
30.902595	1039.078555	17.001805
30.724409	1037.172059	17.006823
30.803988	1042.215434	17.011840
30.900142	1048.341812	17.016858
30.942251	1042.743491	17.021875
31.254172	1041.186714	17.026893
31.286569	1050.090619	17.031911
31.304842	1044.025801	17.036928
30.925718	1048.171778	17.041946
31.230010	1052.457500	17.046963
31.512056	1041.542236	17.051981
31.053491	1036.615153	17.056999
31.180778	1031.612635	17.062016
31.138486	1033.920007	17.067034
31.243125	1041.692367	17.072051
31.610457	1045.706344	17.077069
31.503385	1043.851891	17.082087
31.828378	1030.272798	17.087104
31.145032	1027.734909	17.092122
31.105379	1029.685270	17.097139
31.463456	1033.381954	17.102157
31.175160	1043.512884	17.107175
31.485462	1041.555578	17.112192
31.590180	1039.971102	17.117210
31.415349	1037.770599	17.122227
31.396783	1034.346577	17.127245
31.016875	1036.640245	17.132263
31.265752	1036.860508	17.137280
31.312084	1053.411803	17.142298
31.733806	1056.909238	17.147315
32.075576	1051.926968	17.152333
31.999556	1059.856849	17.157351
32.090986	1054.250845	17.162368
31.851761	1048.185093	17.167386
31.797540	1053.167253	17.172403
32.446329	1059.333821	17.177421
32.007334	1056.555915	17.182439
32.192764	1041.392261	17.187456
31.820081	1036.076272	17.192474
31.764775	1035.741146	17.197491
32.170868	1036.694313	17.202509
32.273771	1046.653885	17.207527
32.241251	1042.897524	17.212544
32.246889	1032.574403	17.217562
32.183676	1036.071598	17.222579
32.310969	1021.216809	17.227597
31.695076	1047.019741	17.232615
31.884459	1047.056766	17.237632
32.334833	1053.374144	17.242650
32.313121	1060.737000	17.247667
32.341321	1050.221011	17.252685
32.295028	1064.596640	17.257703
32.382308	1059.802312	17.262720
32.575768	1054.253005	17.267738
32.563110	1056.558923	17.272755
32.588372	1054.488207	17.277773
32.550769	1056.403538	17.282791
32.311725	1058.104083	17.287808
32.740734	1048.314630	17.292826
32.667927	1056.023106	17.297843
32.672657	1047.729272	17.302861
32.619253	1052.364172	17.307879
32.334938	1054.100167	17.312896
32.885962	1064.734738	17.317914
32.982080	1071.577487	17.322931
32.926980	1077.891524	17.327949
32.977947	1077.685016	17.332967
32.978824	1081.806550	17.337984
33.265857	1077.823706	17.343002
33.105949	1080.221979	17.348019
33.074901	1071.596038	17.353037
32.616000	1078.244341	17.358055
32.731276	1081.218299	17.363072
33.115146	1080.619137	17.368090
32.874435	1083.512823	17.373107
33.363930	1067.222533	17.378125
33.491248	1064.940269	17.383143
33.448276	1072.246481	17.388160
33.714540	1066.370259	17.393178
33.486743	1069.751076	17.398195
33.374897	1065.031930	17.403213
33.418516	1069.465538	17.408231
33.392632	1068.482055	17.413248
33.892767	1065.147679	17.418266
33.405383	1067.353944	17.423283
33.477714	1067.854157	17.428301
33.576759	1065.633098	17.433319
33.187711	1068.439426	17.438336
33.761068	1063.724049	17.443354
33.534113	1069.913364	17.448371
33.492219	1074.634839	17.453389
33.395001	1071.683798	17.458407
33.295566	1078.301379	17.463424
33.686990	1093.833319	17.468442
33.871753	1094.126681	17.473459
33.907735	1092.224703	17.478477
33.717689	1094.775992	17.483495
33.755738	1088.099016	17.488512
34.479078	1095.588879	17.493530
34.166197	1101.390801	17.498547
34.062526	1090.163181	17.503565
34.259602	1088.939858	17.508583
34.196325	1097.912331	17.513600
34.007739	1096.045317	17.518618
34.338831	1095.309206	17.523635
34.191843	1088.127715	17.528653
33.777048	1091.714374	17.533671
34.068554	1095.692833	17.538688
34.057577	1093.993823	17.543706
33.922014	1097.981971	17.548723
34.105847	1091.149754	17.553741
34.271223	1100.263351	17.558759
34.486520	1103.679327	17.563776
34.643116	1114.520504	17.568794
34.205449	1113.569574	17.573811
34.220813	1111.396252	17.578829
34.688565	1111.639242	17.583847
34.466788	1117.527969	17.588864
34.780272	1111.997827	17.593882
34.586849	1112.529950	17.598899
34.940725	1116.722762	17.603917
35.143570	1109.953849	17.608935
35.110096	1110.028729	17.613952
34.880898	1097.807646	17.618970
34.726903	1105.279478	17.623987
34.716583	1107.831188	17.629005
34.792351	1109.160834	17.634023
35.160427	1108.917576	17.639040
35.067199	1112.107038	17.644058
34.876246	1111.120851	17.649075
35.113168	1109.585213	17.654093
35.322756	1104.522524	17.659111
35.136731	1107.372987	17.664128
35.122243	1110.556500	17.669146
34.760616	1111.575555	17.674163
34.663645	1103.635197	17.679181
35.075495	1110.416179	17.684199
35.095239	1120.237263	17.689216
35.132724	1122.175623	17.694234
35.465970	1125.052536	17.699251
35.551770	1127.715514	17.704269
35.305675	1131.528377	17.709287
35.631229	1132.030191	17.714304
35.749926	1134.798500	17.719322
35.568911	1134.047448	17.724339
35.745378	1130.823414	17.729357
35.638118	1128.912176	17.734375
35.445645	1137.384082	17.739392
35.806650	1134.169185	17.744410
35.603151	1135.592806	17.749427
35.596170	1128.897580	17.754445
35.429757	1126.970307	17.759463
35.331772	1131.542741	17.764480
35.421441	1122.828553	17.769498
35.888828	1141.993625	17.774515
36.079344	1154.322228	17.779533
36.320738	1151.763418	17.784551
36.294675	1159.269002	17.789568
36.169114	1152.235627	17.794586
36.184862	1157.424672	17.799603
36.121889	1158.513993	17.804621
36.141074	1157.899026	17.809639
36.198219	1160.957787	17.814656
35.998256	1159.587995	17.819674
36.260165	1162.214092	17.824691
35.781632	1155.264073	17.829709
36.335688	1155.787115	17.834727
35.958944	1155.584084	17.839744
36.394910	1148.371765	17.844762
36.131702	1153.459075	17.849779
36.224479	1162.707082	17.854797
36.686048	1172.544611	17.859815
36.580202	1178.500513	17.864832
36.888847	1176.451933	17.869850
36.942723	1167.434029	17.874867
36.889941	1164.403471	17.879885
36.770377	1156.286728	17.884903
36.496201	1155.278782	17.889920
36.836231	1151.868334	17.894938
36.392008	1159.098200	17.899955
36.627315	1169.355960	17.904973
36.956287	1169.232398	17.909991
36.844056	1173.194839	17.915008
37.070872	1171.550317	17.920026
37.228009	1175.966277	17.925043
37.055815	1177.467079	17.930061
37.597213	1175.284430	17.935079
37.217652	1187.556649	17.940096
36.967093	1173.120323	17.945114
36.823160	1173.518512	17.950131
37.043565	1172.714426	17.955149
37.405234	1167.107337	17.960167
37.098160	1175.622350	17.965184
36.938776	1164.984021	17.970202
37.231700	1169.558718	17.975219
37.009112	1173.424733	17.980237
37.228912	1163.560494	17.985255
37.333806	1179.815613	17.990272
37.377034	1187.815347	17.995290
37.770900	1198.266185	18.000307
37.442771	1201.817282	18.005325
37.724017	1194.016811	18.010343
37.687117	1197.948595	18.015360
37.759885	1187.734852	18.020378
37.763719	1196.425528	18.025395
37.759352	1200.977093	18.030413
37.806992	1196.943133	18.035431
37.796399	1199.397069	18.040448
37.653449	1187.986156	18.045466
37.768015	1197.306527	18.050483
37.536274	1202.789737	18.055501
38.030682	1191.030280	18.060519
37.897088	1198.136060	18.065536
37.973884	1197.196543	18.070554
37.997560	1199.582028	18.075571
37.772482	1205.218834	18.080589
38.390713	1202.572943	18.085607
38.765455	1209.552244	18.090624
38.719131	1200.663532	18.095642
38.420309	1184.540055	18.100659
38.179302	1194.859366	18.105677
38.420491	1181.160664	18.110695
38.537485	1180.278004	18.115712
38.081367	1185.616264	18.120730
38.670788	1199.511174	18.125747
38.815436	1196.383600	18.130765
38.773173	1196.917437	18.135783
38.110848	1197.222770	18.140800
38.520420	1203.010070	18.145818
38.774784	1210.036516	18.150835
38.962644	1212.061926	18.155853
39.114049	1204.407899	18.160871
38.910750	1209.489053	18.165888
38.870551	1209.962609	18.170906
39.058847	1213.041985	18.175923
39.011063	1219.055132	18.180941
39.524812	1203.499397	18.185959
38.665414	1186.276621	18.190976
39.083782	1198.651830	18.195994
38.785699	1194.955718	18.201011
38.689013	1208.480937	18.206029
39.216940	1194.949017	18.211047
38.924603	1205.866459	18.216064
39.013762	1209.302094	18.221082
39.060891	1207.575093	18.226099
38.867794	1213.008108	18.231117
39.214948	1204.127559	18.236135
38.765295	1208.300333	18.241152
39.239951	1218.934263	18.246170
39.263786	1225.280244	18.251187
39.338910	1243.521893	18.256205
39.476733	1223.448769	18.261223
39.270208	1230.916210	18.266240
39.615289	1227.041059	18.271258
39.607761	1225.931633	18.276275
39.262069	1230.154498	18.281293
39.753465	1218.010486	18.286311
39.716879	1237.787457	18.291328
39.889155	1241.241715	18.296346
39.948751	1237.048095	18.301363
39.851477	1251.532798	18.306381
39.692767	1250.882409	18.311399
40.348302	1245.747093	18.316416
40.099412	1245.937563	18.321434
40.489720	1243.402891	18.326451
39.924304	1246.299822	18.331469
40.118306	1236.045085	18.336487
40.065185	1236.255568	18.341504
40.092435	1242.619957	18.346522
40.550217	1245.284997	18.351539
40.179398	1241.773769	18.356557
40.055296	1250.004710	18.361575
40.278386	1252.397024	18.366592
40.187414	1246.147175	18.371610
40.477830	1243.978349	18.376627
40.103076	1248.978912	18.381645
40.128231	1242.202901	18.386663
40.385599	1252.637154	18.391680
40.533691	1267.872617	18.396698
40.810341	1267.346948	18.401715
40.654325	1272.862570	18.406733
41.256612	1271.311058	18.411751
40.841262	1268.703005	18.416768
40.830900	1260.212607	18.421786
40.858098	1251.915179	18.426803
41.022104	1269.559195	18.431821
40.984241	1259.154353	18.436839
40.862996	1256.961257	18.441856
40.979628	1263.011937	18.446874
41.432029	1267.883721	18.451891
41.266604	1267.821355	18.456909
41.407771	1268.023679	18.461927
41.381224	1255.953971	18.466944
40.987355	1243.550144	18.471962
40.894549	1243.751026	18.476979
41.531027	1268.605053	18.481997
41.505497	1268.625048	18.487015
41.552432	1266.001824	18.492032
41.204903	1267.687721	18.497050
41.621275	1259.673680	18.502067
41.410843	1271.742898	18.507085
41.477070	1264.556542	18.512103
41.399558	1264.979105	18.517120
41.233956	1258.210697	18.522138
41.652071	1257.195944	18.527155
41.244079	1266.831242	18.532173
41.451101	1254.075075	18.537191
41.543325	1279.626080	18.542208
41.736721	1284.279419	18.547226
41.884702	1283.691731	18.552243
41.947400	1287.415523	18.557261
41.856262	1292.409810	18.562279
42.039043	1288.124415	18.567296
41.866281	1288.826896	18.572314
42.138334	1281.879885	18.577331
42.196371	1284.443068	18.582349
41.842063	1285.347384	18.587367
41.940061	1282.877153	18.592384
41.962264	1284.142569	18.597402
42.166486	1280.838447	18.602419
42.247984	1289.542323	18.607437
42.515093	1304.894987	18.612455
42.768285	1306.998599	18.617472
42.159065	1300.564332	18.622490
42.371494	1298.391864	18.627507
42.197732	1305.589147	18.632525
42.802628	1311.024179	18.637543
42.494956	1305.527572	18.642560
42.506313	1319.285361	18.647578
42.600049	1311.643422	18.652595
42.504220	1309.544193	18.657613
42.487569	1320.904776	18.662631
42.846853	1308.746558	18.667648
42.405900	1315.401621	18.672666
42.626769	1316.247944	18.677683
43.093624	1331.162431	18.682701
42.949144	1328.793063	18.687719
43.460772	1332.475371	18.692736
43.524922	1336.934251	18.697754
43.453663	1325.278558	18.702771
43.511559	1313.145172	18.707789
43.205251	1303.419573	18.712807
43.255787	1297.447475	18.717824
43.340468	1306.848297	18.722842
43.407526	1302.495709	18.727859
43.422464	1312.727902	18.732877
43.154275	1310.213695	18.737895
43.429352	1316.264970	18.742912
43.675322	1319.549980	18.747930
43.361985	1319.602162	18.752947
43.680695	1322.263620	18.757965
43.731527	1320.835833	18.762983
43.844923	1323.731229	18.768000
43.714511	1325.534806	18.773018
43.940474	1319.191405	18.778035
43.753895	1321.208854	18.783053
43.888909	1321.737184	18.788071
44.042723	1321.681919	18.793088
43.903698	1319.740893	18.798106
43.664312	1309.045506	18.803123
44.088278	1315.382868	18.808141
44.019181	1322.295618	18.813159
44.173181	1325.506586	18.818176
43.947352	1326.640209	18.823194
44.234536	1322.385887	18.828211
44.486842	1329.905007	18.833229
44.575328	1337.900918	18.838247
44.479990	1321.979164	18.843264
44.480491	1328.991534	18.848282
44.444281	1323.408475	18.853299
44.196815	1327.802261	18.858317
44.484143	1342.520648	18.863335
44.754282	1340.048854	18.868352
44.364654	1354.026892	18.873370
44.511010	1340.216600	18.878387
44.398105	1346.375630	18.883405
44.416554	1341.885434	18.888423
44.909878	1338.747729	18.893440
44.560222	1334.403209	18.898458
45.110808	1338.707459	18.903475
44.828038	1341.598268	18.908493
44.633120	1344.885654	18.913511
44.996852	1336.248612	18.918528
45.346504	1353.848027	18.923546
44.880157	1349.657373	18.928563
45.159387	1341.200743	18.933581
44.948974	1362.425031	18.938599
45.018908	1349.112627	18.943616
45.234542	1361.077700	18.948634
45.409472	1359.018360	18.953651
45.616770	1369.040753	18.958669
45.387759	1361.556341	18.963687
45.300846	1356.385110	18.968704
45.154679	1358.670828	18.973722
45.137931	1362.094580	18.978739
45.220806	1369.116231	18.983757
45.265861	1375.178093	18.988775
45.835396	1371.327925	18.993792
45.786557	1374.740897	18.998810
45.887968	1370.370321	19.003827
46.212957	1372.036726	19.008845
46.057682	1375.418932	19.013863
46.268003	1363.776178	19.018880
46.428407	1372.799170	19.023898
46.331720	1362.138338	19.028915
46.409383	1357.761995	19.033933
45.711846	1358.685039	19.038951
46.068861	1348.723595	19.043968
46.063095	1359.710122	19.048986
46.491857	1372.298428	19.054003
46.211943	1366.693339	19.059021
46.354727	1369.656751	19.064039
46.726835	1364.817994	19.069056
46.547065	1364.978769	19.074074
46.350311	1368.938634	19.079091
46.361302	1366.311525	19.084109
46.482947	1369.401305	19.089127
46.721505	1356.706427	19.094144
46.521120	1370.494067	19.099162
46.318219	1367.704599	19.104179
46.329348	1368.653008	19.109197
46.279712	1368.525277	19.114215
46.732937	1382.043903	19.119232
46.826821	1389.089095	19.124250
47.098344	1388.564220	19.129267
46.907213	1392.403294	19.134285
47.138945	1393.146943	19.139303
47.272350	1384.059742	19.144320
46.858569	1391.556363	19.149338
47.232018	1387.244413	19.154355
47.102935	1382.319583	19.159373
47.167705	1392.174832	19.164391
47.258114	1386.698272	19.169408
47.122805	1387.164550	19.174426
47.045588	1387.419811	19.179443
47.194457	1393.408712	19.184461
47.492958	1404.833890	19.189479
47.718048	1405.594352	19.194496
47.867492	1409.579221	19.199514
47.569224	1406.441675	19.204531
48.101949	1403.900586	19.209549
47.723220	1405.054864	19.214567
47.890367	1404.016062	19.219584
47.888259	1411.540114	19.224602
47.684655	1407.586250	19.229619
47.618670	1405.277234	19.234637
47.362436	1411.578523	19.239655
47.756712	1410.763135	19.244672
47.643108	1403.980264	19.249690
47.431464	1423.169311	19.254707
48.047138	1431.045312	19.259725
48.402440	1441.849440	19.264743
48.265567	1434.956570	19.269760
48.001233	1430.068564	19.274778
48.397273	1433.216619	19.279795
48.267864	1436.004670	19.284813
48.374021	1435.622306	19.289831
48.420082	1426.621267	19.294848
48.589494	1430.041294	19.299866
48.506510	1432.200418	19.304883
48.364219	1424.588867	19.309901
48.739647	1448.423433	19.314919
48.872441	1435.637668	19.319936
48.824054	1445.633642	19.324954
48.918484	1450.305589	19.329971
48.981428	1436.637598	19.334989
48.871432	1447.031332	19.340007
49.612098	1446.941501	19.345024
48.985535	1441.339866	19.350042
49.064915	1447.440591	19.355059
49.171646	1446.338608	19.360077
49.078560	1456.505651	19.365095
49.203230	1449.483691	19.370112
49.215336	1458.750724	19.375130
49.211510	1449.381897	19.380147
49.256420	1441.397207	19.385165
49.051498	1456.337497	19.390183
49.224698	1448.332830	19.395200
49.154746	1448.820492	19.400218
49.580644	1462.015228	19.405235
49.968094	1463.735034	19.410253
49.868162	1473.041610	19.415271
49.808473	1463.703563	19.420288
49.890177	1462.586541	19.425306
49.451564	1467.527679	19.430323
49.879457	1460.897166	19.435341
49.629692	1472.871657	19.440359
49.890680	1476.735032	19.445376
49.798469	1472.097928	19.450394
49.868225	1471.983166	19.455411
50.118677	1472.310489	19.460429
50.065362	1465.628662	19.465447
50.355206	1464.419273	19.470464
50.474831	1470.485337	19.475482
50.563994	1471.140732	19.480499
50.583684	1461.815574	19.485517
50.509503	1475.896073	19.490535
50.408777	1461.114290	19.495552
50.651370	1470.313886	19.500570
50.483923	1468.932695	19.505587
50.323062	1462.725210	19.510605
50.426274	1480.217952	19.515623
50.435221	1489.595947	19.520640
50.767094	1491.419084	19.525658
50.959699	1487.829552	19.530675
51.113810	1495.323005	19.535693
50.821694	1492.067720	19.540711
51.155264	1491.993934	19.545728
51.079517	1484.813815	19.550746
50.884938	1497.038509	19.555763
51.117031	1488.510253	19.560781
51.212146	1482.613204	19.565799
51.053149	1483.373510	19.570816
51.170810	1491.229246	19.575834
51.221870	1492.985650	19.580851
51.532644	1483.299577	19.585869
51.409015	1502.768499	19.590887
51.074556	1503.527722	19.595904
51.637985	1505.504159	19.600922
51.679980	1507.845807	19.605939
51.759682	1514.157945	19.610957
51.811423	1512.414417	19.615975
51.457331	1510.711984	19.620992
52.030446	1504.017818	19.626010
52.026263	1507.559563	19.631027
52.139515	1511.610051	19.636045
51.668584	1510.348693	19.641063
51.605874	1509.831672	19.646080
52.328001	1508.750637	19.651098
52.063866	1502.811684	19.656115
51.877853	1500.470851	19.661133
52.070587	1498.336138	19.666151
52.254885	1509.438334	19.671168
52.036822	1505.291037	19.676186
51.875269	1510.735010	19.681203
52.263906	1523.998710	19.686221
52.398235	1534.894104	19.691239
52.314307	1526.528643	19.696256
52.425983	1529.878783	19.701274
52.280676	1531.930855	19.706291
52.486990	1531.311987	19.711309
52.557951	1534.993519	19.716327
52.453086	1547.743929	19.721344
52.399206	1546.471284	19.726362
52.638512	1561.822187	19.731379
52.556681	1555.895859	19.736397
52.714052	1564.146237	19.741415
52.681209	1559.316828	19.746432
53.328978	1571.082215	19.751450
53.464255	1585.007110	19.756467
53.450940	1574.500431	19.761485
53.450320	1561.501815	19.766503
53.054183	1548.662620	19.771520
53.580093	1561.280117	19.776538
53.326046	1574.533463	19.781555
53.756851	1567.448014	19.786573
53.355736	1570.556104	19.791591
53.630796	1574.742361	19.796608
54.037343	1562.036962	19.801626
53.537145	1568.158537	19.806643
54.129305	1571.746304	19.811661
54.002914	1563.781919	19.816679
53.892754	1573.213217	19.821696
54.062522	1567.799986	19.826714
54.286598	1573.600510	19.831731
54.383311	1570.287827	19.836749
54.353651	1558.234179	19.841767
53.898081	1551.062675	19.846784
54.163711	1556.351788	19.851802
54.168974	1564.752083	19.856819
54.017038	1568.077000	19.861837
54.311600	1570.710697	19.866855
54.276084	1577.217525	19.871872
54.374432	1564.856759	19.876890
53.799866	1570.781627	19.881907
54.117214	1571.493018	19.886925
54.330745	1583.619517	19.891943
54.392374	1590.773953	19.896960
54.622985	1592.063748	19.901978
54.502335	1590.164013	19.906995
54.465950	1591.347053	19.912013
54.653707	1590.399707	19.917031
54.553790	1588.758680	19.922048
55.581684	1599.499211	19.927066
55.239542	1593.783815	19.932083
55.143813	1590.829300	19.937101
54.982154	1578.505851	19.942119
55.204405	1581.324380	19.947136
55.665660	1589.095105	19.952154
55.044047	1587.895071	19.957171
55.132642	1603.171643	19.962189
55.448168	1602.611509	19.967207
55.396445	1606.438391	19.972224
55.862327	1600.890683	19.977242
55.803506	1613.564543	19.982259
55.759043	1603.084787	19.987277
55.957194	1605.531525	19.992295
55.748298	1604.011608	19.997312
55.711357	1600.101181	20.002330
55.766744	1603.905074	20.007347
55.989908	1593.560384	20.012365
55.835889	1605.327550	20.017383
55.842048	1607.015216	20.022400
55.882491	1600.479690	20.027418
55.834645	1603.185638	20.032435
55.727763	1598.140524	20.037453
56.141398	1605.076056	20.042471
55.819361	1617.996032	20.047488
56.127215	1625.932670	20.052506
55.990777	1626.291831	20.057523
56.317338	1626.345371	20.062541
56.192934	1631.736259	20.067559
56.091496	1640.626582	20.072576
56.691808	1640.978334	20.077594
56.787242	1651.567424	20.082611
56.619367	1658.306332	20.087629
57.051651	1647.846999	20.092647
56.688117	1658.378162	20.097664
57.109608	1646.396226	20.102682
57.473204	1637.434006	20.107699
57.357389	1651.966103	20.112717
57.358424	1643.574736	20.117735
57.254873	1650.698108	20.122752
57.528515	1644.037894	20.127770
57.137337	1648.012312	20.132787
57.217421	1650.142918	20.137805
57.480800	1643.036168	20.142823
57.346873	1654.632977	20.147840
57.407960	1649.179838	20.152858
57.484585	1647.741697	20.157875
57.489750	1647.138363	20.162893
57.956862	1645.560529	20.167911
57.600762	1647.639122	20.172928
57.758156	1640.659331	20.177946
57.988607	1652.335109	20.182963
57.834961	1655.221643	20.187981
58.319309	1650.630427	20.192999
58.206319	1659.939133	20.198016
58.122797	1653.965697	20.203034
58.344290	1655.954364	20.208051
58.392246	1657.073782	20.213069
58.283395	1648.690053	20.218087
58.404197	1654.980063	20.223104
58.717755	1652.586675	20.228122
59.021316	1645.366369	20.233139
58.440015	1645.690650	20.238157
58.436209	1628.577233	20.243175
58.251862	1636.801953	20.248192
58.175584	1651.005995	20.253210
58.303679	1661.539513	20.258227
58.572754	1656.312769	20.263245
58.642249	1655.655237	20.268263
58.394207	1658.382896	20.273280
58.523926	1658.179899	20.278298
58.945917	1671.097683	20.283315
58.971141	1676.168636	20.288333
58.822124	1675.788126	20.293351
58.911020	1679.555260	20.298368
59.026085	1672.067639	20.303386
59.148224	1674.829186	20.308403
58.765313	1680.238245	20.313421
59.580282	1688.468349	20.318439
59.782265	1691.176440	20.323456
59.825821	1688.045585	20.328474
59.994584	1689.357640	20.333491
59.592636	1676.560284	20.338509
59.673766	1680.666305	20.343527
59.548579	1694.893777	20.348544
59.797394	1691.459558	20.353562
60.021056	1691.039959	20.358579
59.745393	1697.221294	20.363597
60.077110	1693.395463	20.368615
60.065382	1695.120637	20.373632
59.940323	1687.481043	20.378650
59.938839	1691.615709	20.383667
60.049352	1695.802368	20.388685
59.766966	1693.817348	20.393703
60.381220	1711.672572	20.398720
60.140397	1712.369886	20.403738
60.327892	1720.088615	20.408755
60.236489	1712.970803	20.413773
60.664294	1723.681761	20.418791
60.402800	1724.849364	20.423808
60.418906	1726.115761	20.428826
60.877282	1727.259648	20.433843
60.961467	1737.882100	20.438861
61.258351	1733.323207	20.443879
61.010813	1743.596513	20.448896
60.998196	1731.906177	20.453914
60.873265	1735.349999	20.458931
60.789417	1739.655294	20.463949
61.117279	1746.752562	20.468967
61.185577	1738.006687	20.473984
61.300818	1740.870305	20.479002
61.276488	1744.260596	20.484019
60.968881	1740.714180	20.489037
61.308437	1747.964266	20.494055
61.464798	1757.606636	20.499072
61.569051	1760.620295	20.504090
61.601111	1761.221475	20.509107
61.649278	1770.053855	20.514125
61.809340	1754.962974	20.519143
61.920075	1749.290629	20.524160
62.067361	1746.699049	20.529178
62.433335	1745.196915	20.534195
62.132153	1754.048964	20.539213
62.050497	1750.546264	20.544231
62.324180	1746.170865	20.549248
62.166376	1756.083060	20.554266
62.460507	1764.523683	20.559283
62.404498	1769.215980	20.564301
62.802876	1781.869270	20.569319
62.550345	1787.788251	20.574336
62.732041	1776.935502	20.579354
62.629961	1768.272944	20.584371
62.605009	1780.824881	20.589389
62.909020	1771.218603	20.594407
63.260503	1775.377230	20.599424
63.045965	1778.920221	20.604442
63.079433	1777.990576	20.609459
62.609977	1780.361396	20.614477
62.957482	1771.076558	20.619495
63.096063	1770.487163	20.624512
63.084820	1773.597704	20.629530
63.181780	1767.230047	20.634547
62.992661	1767.871974	20.639565
63.314246	1772.549665	20.644583
63.194188	1769.668338	20.649600
63.394818	1778.085654	20.654618
63.412105	1782.984300	20.659635
63.558564	1793.174199	20.664653
63.477260	1799.880746	20.669671
63.426991	1791.806574	20.674688
63.423511	1798.863931	20.679706
63.563726	1792.227591	20.684723
63.593744	1801.192204	20.689741
63.863080	1812.578002	20.694759
64.251013	1815.954614	20.699776
64.167007	1821.216189	20.704794
64.519679	1815.083265	20.709811
64.431219	1819.622833	20.714829
64.355928	1810.447985	20.719847
64.171923	1818.833685	20.724864
64.316124	1814.497365	20.729882
64.502569	1808.488157	20.734899
64.038906	1817.668501	20.739917
64.281335	1819.313089	20.744935
64.252972	1820.924097	20.749952
64.768918	1831.488849	20.754970
64.955027	1830.860493	20.759987
64.750315	1844.279932	20.765005
64.474832	1832.112889	20.770023
64.942134	1853.942321	20.775040
65.183647	1862.129243	20.780058
65.848144	1854.644367	20.785075
65.583386	1847.345202	20.790093
65.551227	1835.364341	20.795111
65.206108	1838.779348	20.800128
65.282613	1844.221073	20.805146
65.524601	1846.108737	20.810163
65.817487	1858.333524	20.815181
65.640660	1860.706132	20.820199
65.727061	1860.266873	20.825216
66.057488	1860.537570	20.830234
66.280197	1851.552996	20.835251
65.824759	1851.551561	20.840269
65.896931	1848.753904	20.845287
65.949551	1855.316540	20.850304
65.943581	1852.802456	20.855322
65.672647	1845.870337	20.860339
65.958997	1849.127068	20.865357
66.354319	1851.858732	20.870375
66.432580	1864.489335	20.875392
66.461464	1877.222312	20.880410
66.514717	1875.456422	20.885427
66.366304	1882.416453	20.890445
66.466258	1875.843157	20.895463
66.748401	1872.321661	20.900480
66.447337	1880.709837	20.905498
66.586308	1877.848124	20.910515
66.504363	1875.134421	20.915533
66.865584	1888.503650	20.920551
67.123664	1892.878825	20.925568
66.883907	1899.774187	20.930586
67.400767	1894.827542	20.935603
66.871060	1896.557641	20.940621
67.261544	1903.405373	20.945639
67.456645	1898.707646	20.950656
67.569043	1901.057319	20.955674
67.631151	1892.709976	20.960691
67.578889	1894.826501	20.965709
67.370195	1895.875438	20.970727
67.659534	1895.511883	20.975744
67.541722	1895.410542	20.980762
67.855673	1891.618994	20.985779
67.843176	1909.647741	20.990797
68.277029	1920.067532	20.995815
68.216776	1907.349358	21.000832
67.661711	1912.498102	21.005850
67.932946	1915.173354	21.010867
68.041524	1918.744963	21.015885
68.247636	1922.200398	21.020903
67.901125	1914.693020	21.025920
67.932330	1918.077853	21.030938
68.129190	1928.480897	21.035955
68.620466	1945.392950	21.040973
68.453263	1951.838362	21.045991
68.914499	1943.659235	21.051008
68.535202	1948.865834	21.056026
68.925966	1939.110254	21.061043
68.843601	1940.013287	21.066061
68.827715	1945.775552	21.071079
69.134950	1933.164251	21.076096
68.656418	1937.821388	21.081114
69.577070	1945.555458	21.086131
69.552849	1959.000532	21.091149
69.712656	1962.191775	21.096167
69.408180	1945.724492	21.101184
69.598647	1951.580867	21.106202
69.721234	1959.237220	21.111219
69.798621	1955.214237	21.116237
70.120791	1953.397002	21.121255
70.067553	1939.273328	21.126272
69.583333	1943.104502	21.131290
69.667360	1941.425335	21.136307
69.988064	1956.448313	21.141325
70.306854	1951.759718	21.146343
70.560826	1944.884696	21.151360
70.304122	1948.857179	21.156378
70.332650	1949.036021	21.161395
70.145678	1948.364759	21.166413
70.026309	1947.307416	21.171431
70.562748	1950.086555	21.176448
70.472662	1949.311842	21.181466
70.345885	1945.734073	21.186483
70.394090	1949.144669	21.191501
70.410673	1969.576916	21.196519
70.780882	1972.262014	21.201536
70.970319	1984.461967	21.206554
70.801111	1972.016340	21.211571
70.798289	1972.834404	21.216589
70.879342	1971.111515	21.221607
71.122998	1973.314525	21.226624
71.164757	1972.497192	21.231642
71.218852	1977.396472	21.236659
71.175700	1985.043925	21.241677
71.291554	1998.678666	21.246695
71.831975	1992.857290	21.251712
71.346095	1991.225824	21.256730
71.726671	1994.366921	21.261747
71.548290	1995.770919	21.266765
71.442202	1992.972590	21.271783
71.731590	1992.738419	21.276800
71.551496	2007.624809	21.281818
71.527211	2008.783901	21.286835
72.044070	2014.778835	21.291853
71.608101	2015.617001	21.296871
71.769432	2013.411375	21.301888
72.142871	2027.189078	21.306906
72.299769	2030.639573	21.311923
72.568192	2039.595590	21.316941
73.256722	2044.443449	21.321959
72.883174	2024.224972	21.326976
72.499438	2018.389678	21.331994
72.257515	2025.752503	21.337011
72.646020	2032.726831	21.342029
72.874359	2039.031793	21.347047
72.906335	2031.459124	21.352064
73.019381	2040.439334	21.357082
73.141950	2031.441858	21.362099
72.944019	2032.353421	21.367117
72.995479	2041.239073	21.372135
73.225839	2034.086815	21.377152
73.480501	2053.872995	21.382170
73.417700	2056.092170	21.387187
73.554762	2053.634687	21.392205
73.666179	2067.371162	21.397223
74.075651	2055.958894	21.402240
73.812131	2060.071323	21.407258
74.141925	2056.927397	21.412275
74.094790	2056.919197	21.417293
73.852673	2060.599087	21.422311
73.999465	2051.522087	21.427328
73.793212	2048.101845	21.432346
73.787751	2049.276945	21.437363
73.993583	2054.588141	21.442381
73.865016	2074.916869	21.447399
74.127173	2075.649499	21.452416
74.131837	2079.044807	21.457434
74.362637	2075.938382	21.462451
74.294357	2077.558784	21.467469
74.316175	2090.087877	21.472487
74.623200	2089.043037	21.477504
74.860067	2092.206526	21.482522
74.480545	2099.764382	21.487539
74.763824	2097.631281	21.492557
74.793283	2104.724658	21.497575
75.002521	2117.136223	21.502592
75.105807	2122.311919	21.507610
75.306280	2119.295419	21.512627
75.880075	2119.297845	21.517645
75.764317	2126.420152	21.522663
75.644348	2120.777297	21.527680
75.774169	2122.530969	21.532698
75.697166	2117.629386	21.537715
76.001087	2116.588184	21.542733
75.923832	2115.827246	21.547751
76.078562	2119.126610	21.552768
76.070863	2117.928789	21.557786
76.135852	2117.306657	21.562803
76.312182	2112.075285	21.567821
76.001468	2118.120204	21.572839
76.030958	2111.453647	21.577856
76.478408	2129.385757	21.582874
76.393394	2137.721478	21.587891
76.455382	2139.463621	21.592909
76.637407	2140.391776	21.597927
76.538912	2147.868025	21.602944
76.684528	2139.220374	21.607962
76.711162	2141.690735	21.612979
77.110745	2134.445815	21.617997
76.791546	2140.337421	21.623015
76.684850	2137.681182	21.628032
77.077213	2137.812847	21.633050
77.085882	2155.027467	21.638067
77.265824	2160.762467	21.643085
77.000628	2165.436942	21.648103
77.458097	2156.914306	21.653120
77.562264	2160.972668	21.658138
77.233779	2168.099707	21.663155
77.591054	2163.509212	21.668173
77.441780	2169.604756	21.673191
77.759102	2177.079397	21.678208
77.694083	2183.947661	21.683226
77.741486	2192.603635	21.688243
77.990788	2185.028625	21.693261
77.639275	2191.771077	21.698279
77.778431	2197.329393	21.703296
77.731459	2209.619959	21.708314
78.185719	2213.084155	21.713331
78.481122	2209.184969	21.718349
78.319225	2222.336079	21.723367
78.552066	2228.851857	21.728384
78.428919	2215.650925	21.733402
78.665465	2233.590728	21.738419
79.020883	2233.573504	21.743437
79.002147	2235.403968	21.748455
79.310062	2240.509967	21.753472
79.387915	2243.054423	21.758490
79.339798	2230.668662	21.763507
79.828362	2234.869174	21.768525
79.536905	2227.428835	21.773543
79.478524	2226.368292	21.778560
79.468166	2232.628431	21.783578
79.778969	2231.103288	21.788595
79.725967	2220.996904	21.793613
79.679589	2223.324001	21.798631
79.644882	2233.125771	21.803648
79.604519	2228.559298	21.808666
79.465637	2229.278631	21.813683
79.942390	2229.709599	21.818701
80.092740	2245.198023	21.823719
80.196961	2247.867769	21.828736
80.393479	2250.633604	21.833754
80.357957	2249.010894	21.838771
80.357747	2244.390825	21.843789
80.713988	2259.642067	21.848807
80.353354	2245.023184	21.853824
80.507442	2245.333968	21.858842
80.478378	2253.051929	21.863859
80.828425	2259.931343	21.868877
80.836512	2263.543915	21.873895
81.200684	2268.925201	21.878912
81.343039	2267.877586	21.883930
81.108429	2277.284447	21.888947
81.165098	2274.258751	21.893965
81.589761	2270.374143	21.898983
81.885561	2257.130044	21.904000
81.944336	2253.958849	21.909018
81.897465	2252.776585	21.914035
81.836716	2257.094187	21.919053
81.755415	2256.286533	21.924071
81.896010	2249.984498	21.929088
81.864031	2247.695327	21.934106
81.449592	2250.799294	21.939123
81.727618	2252.772914	21.944141
81.970103	2266.760549	21.949159
81.918670	2274.702921	21.954176
82.220384	2275.956449	21.959194
82.233603	2279.148481	21.964211
82.568572	2282.375629	21.969229
82.832787	2279.873071	21.974247
82.484625	2274.972634	21.979264
82.755537	2273.841884	21.984282
82.893378	2272.621393	21.989299
82.995918	2269.023636	21.994317
82.889439	2272.988581	21.999335
82.616581	2282.698061	22.004352
82.682532	2290.644256	22.009370
82.581902	2306.238085	22.014387
82.628728	2303.851425	22.019405
83.406798	2305.182276	22.024423
83.600554	2313.692439	22.029440
84.030733	2322.970573	22.034458
83.603789	2319.186985	22.039475
83.748743	2312.729606	22.044493
83.930034	2315.138040	22.049511
83.745160	2311.313609	22.054528
84.066213	2317.768346	22.059546
83.865109	2314.943732	22.064563
84.151514	2312.791184	22.069581
84.311940	2318.623954	22.074599
83.867688	2318.636554	22.079616
83.893049	2307.817292	22.084634
84.210581	2330.301822	22.089651
84.447918	2331.480166	22.094669
84.206331	2330.006303	22.099687
84.404776	2336.202409	22.104704
84.824076	2337.279834	22.109722
85.146932	2343.769016	22.114739
85.105404	2359.079118	22.119757
85.293076	2358.144369	22.124775
85.475273	2362.597751	22.129792
85.855397	2343.369324	22.134810
85.564046	2326.495679	22.139827
85.648886	2326.198672	22.144845
85.568721	2322.689315	22.149863
85.282294	2318.653462	22.154880
85.765974	2327.730754	22.159898
85.831996	2336.390210	22.164915
85.717819	2343.121014	22.169933
85.652136	2341.894334	22.174951
86.336447	2347.995862	22.179968
86.444289	2337.649762	22.184986
86.315789	2337.499586	22.190003
86.680189	2326.823197	22.195021
86.818572	2316.390298	22.200039
86.403477	2329.773424	22.205056
86.604734	2320.933974	22.210074
86.598359	2333.780070	22.215091
86.505804	2329.581479	22.220109
86.784106	2326.095209	22.225127
86.677711	2334.595306	22.230144
86.993931	2340.665774	22.235162
86.853887	2351.187794	22.240179
87.001954	2345.787175	22.245197
87.156146	2345.899117	22.250215
86.965311	2347.355577	22.255232
87.218344	2340.048180	22.260250
87.292303	2358.732989	22.265267
87.774229	2360.412928	22.270285
88.081556	2360.516807	22.275303
87.815854	2374.520529	22.280320
88.076384	2363.563626	22.285338
88.094328	2368.648533	22.290355
87.924636	2363.773937	22.295373
88.120680	2369.642206	22.300391
87.844848	2370.092515	22.305408
87.870593	2362.785780	22.310426
88.053184	2375.870744	22.315443
87.981256	2381.140071	22.320461
88.763186	2382.924791	22.325479
88.484989	2385.319563	22.330496
88.721294	2386.217187	22.335514
88.535019	2401.452026	22.340531
88.365616	2400.920030	22.345549
88.751654	2386.355202	22.350567
88.572392	2393.342326	22.355584
89.314665	2405.103022	22.360602
89.238440	2405.481226	22.365619
89.399956	2418.986095	22.370637
89.482902	2413.706055	22.375655
88.704004	2420.597189	22.380672
89.220548	2408.265411	22.385690
89.699349	2424.551817	22.390707
89.921700	2433.884458	22.395725
90.067535	2434.234402	22.400743
89.805314	2439.773230	22.405760
89.941304	2441.409201	22.410778
90.292042	2438.807937	22.415795
90.324166	2440.788304	22.420813
90.577905	2426.297694	22.425831
90.367431	2440.488541	22.430848
90.576892	2430.656774	22.435866
90.390414	2436.663521	22.440883
90.124129	2432.779151	22.445901
90.739396	2447.516825	22.450919
90.757132	2460.939964	22.455936
90.674698	2457.468805	22.460954
90.897311	2465.422246	22.465971
90.754621	2464.538928	22.470989
91.065305	2460.933974	22.476007
90.964229	2471.633046	22.481024
90.911951	2477.836678	22.486042
91.261525	2481.847436	22.491059
91.390301	2485.498071	22.496077
91.575365	2490.648517	22.501095
91.383423	2504.369439	22.506112
91.862333	2500.331159	22.511130
91.721890	2505.652218	22.516147
91.782445	2511.339643	22.521165
92.000465	2507.080031	22.526183
92.010192	2518.970635	22.531200
92.120808	2529.194940	22.536218
92.670979	2530.955795	22.541235
92.519064	2531.825502	22.546253
92.845086	2531.793919	22.551271
92.440835	2534.593370	22.556288
92.227689	2536.359453	22.561306
92.192600	2536.649199	22.566323
92.419846	2549.465388	22.571341
92.812777	2547.668638	22.576359
92.776788	2558.105146	22.581376
93.308224	2569.516897	22.586394
93.476060	2576.166008	22.591411
93.762815	2583.402565	22.596429
93.581511	2580.552734	22.601447
93.574127	2589.851792	22.606464
93.862271	2582.538830	22.611482
93.714060	2575.782994	22.616499
93.630957	2576.645145	22.621517
94.223061	2580.801215	22.626535
94.108134	2581.529456	22.631552
94.115594	2575.910802	22.636570
94.104786	2568.944214	22.641587
94.340406	2587.061254	22.646605
94.353590	2602.097939	22.651623
94.364364	2600.335435	22.656640
94.593170	2602.547148	22.661658
95.067382	2593.153790	22.666675
94.836333	2593.265749	22.671693
95.530292	2586.984746	22.676711
95.005862	2586.782594	22.681728
95.365253	2584.015849	22.686746
95.302928	2589.763459	22.691763
95.005952	2589.888838	22.696781
95.244768	2581.071818	22.701799
95.160398	2584.679913	22.706816
95.377265	2590.437707	22.711834
95.559611	2599.533649	22.716851
95.409963	2608.277312	22.721869
95.755971	2601.031079	22.726887
95.582924	2605.419901	22.731904
95.665121	2610.845193	22.736922
95.827900	2629.753158	22.741939
95.404065	2625.050613	22.746957
95.748527	2632.025722	22.751975
96.238169	2647.209185	22.756992
96.456978	2643.949884	22.762010
96.599108	2652.790163	22.767027
96.532799	2644.673919	22.772045
96.861632	2654.229955	22.777063
96.717680	2653.293171	22.782080
96.695305	2668.818323	22.787098
96.998110	2678.207998	22.792115
96.737920	2680.521103	22.797133
97.355095	2671.367399	22.802151
97.219765	2681.222952	22.807168
97.598837	2685.759380	22.812186
97.835283	2693.887508	22.817203
97.894310	2701.352088	22.822221
98.467779	2693.148836	22.827239
97.912156	2696.031845	22.832256
98.059104	2692.670105	22.837274
98.365894	2688.099961	22.842291
97.926654	2690.011722	22.847309
98.215762	2679.283726	22.852327
98.221023	2691.118330	22.857344
98.485148	2697.184406	22.862362
98.980294	2692.812171	22.867379
98.923978	2709.440947	22.872397
99.148857	2707.316869	22.877415
98.895862	2717.708355	22.882432
99.191760	2715.450132	22.887450
99.244785	2711.803187	22.892467
98.843267	2715.530120	22.897485
99.149842	2709.681803	22.902503
99.137711	2715.633093	22.907520
99.143109	2711.356041	22.912538
99.757674	2725.200891	22.917555
99.381605	2745.448983	22.922573
99.523312	2733.307897	22.927591
99.554994	2741.527893	22.932608
99.577780	2740.997524	22.937626
100.025914	2751.036851	22.942643
99.829039	2758.127853	22.947661
100.324127	2757.088413	22.952679
100.135283	2758.819172	22.957696
100.227763	2757.381631	22.962714
100.465545	2770.335204	22.967731
100.540519	2779.722532	22.972749
100.874204	2789.435689	22.977767
100.898117	2784.297286	22.982784
100.977470	2785.143622	22.987802
100.995014	2773.908695	22.992819
100.950577	2794.174643	22.997837
101.218582	2781.142786	23.002855
101.067750	2782.615145	23.007872
101.011284	2798.044721	23.012890
101.434520	2807.160073	23.017907
101.188595	2802.764324	23.022925
101.550484	2803.370996	23.027943
101.805164	2811.212292	23.032960
101.940191	2826.346969	23.037978
102.313217	2821.592895	23.042995
101.954214	2826.746088	23.048013
102.134855	2812.938792	23.053031
102.379796	2823.565265	23.058048
102.327479	2832.407502	23.063066
102.493765	2828.903859	23.068083
102.680660	2844.538604	23.073101
102.718720	2847.493319	23.078119
102.901285	2851.457574	23.083136
102.816537	2845.755353	23.088154
102.805576	2849.793923	23.093171
102.767454	2854.218608	23.098189
102.838923	2859.917069	23.103207
103.972316	2854.940451	23.108224
104.192803	2855.834251	23.113242
104.320213	2859.024387	23.118259
104.391119	2865.208973	23.123277
104.283768	2847.135284	23.128295
104.210907	2829.643273	23.133312
104.015545	2827.493083	23.138330
104.321844	2840.833705	23.143347
104.638151	2852.780948	23.148365
104.660735	2850.303308	23.153383
104.828765	2848.450018	23.158400
104.979321	2857.787747	23.163418
104.803691	2852.131234	23.168435
104.690795	2857.347114	23.173453
104.622377	2853.015242	23.178471
104.692373	2854.598405	23.183488
104.683848	2855.477363	23.188506
104.990895	2867.110449	23.193523
105.044218	2866.723659	23.198541
105.110608	2875.519030	23.203559
105.433282	2871.094703	23.208576
105.070034	2871.457639	23.213594
105.627644	2887.309282	23.218611
106.059397	2895.034676	23.223629
105.741848	2897.533480	23.228647
105.868859	2895.743381	23.233664
105.626194	2901.083628	23.238682
105.939123	2907.161113	23.243699
106.100334	2916.595052	23.248717
106.289920	2922.789585	23.253735
107.041433	2914.495392	23.258752
106.824380	2924.471109	23.263770
106.496547	2920.350040	23.268787
106.702193	2929.956965	23.273805
107.180195	2947.500097	23.278823
107.423791	2943.492044	23.283840
107.103981	2952.218182	23.288858
107.183398	2944.164328	23.293875
107.209233	2952.094969	23.298893
107.268698	2956.334057	23.303911
107.421816	2962.906701	23.308928
107.528840	2962.139128	23.313946
107.669135	2969.742658	23.318963
107.698167	2973.203776	23.323981
107.828394	2967.982490	23.328999
107.790281	2974.528102	23.334016
107.900725	2991.535156	23.339034
108.323767	2982.660852	23.344051
108.014301	2986.963700	23.349069
108.245690	2995.386269	23.354087
108.501741	3007.137850	23.359104
108.902070	3019.933740	23.364122
109.126116	3011.364985	23.369139
109.183247	3008.073981	23.374157
109.155804	3015.324914	23.379175
109.161007	3008.440878	23.384192
109.408103	3010.706604	23.389210
109.505160	3001.195014	23.394227
109.252321	3011.460401	23.399245
109.889838	3021.419897	23.404263
109.729591	3020.731807	23.409280
110.032349	3030.898078	23.414298
110.378800	3027.738767	23.419315
110.148037	3023.176486	23.424333
110.118925	3027.344166	23.429351
110.080611	3024.228981	23.434368
110.125024	3023.471153	23.439386
110.286197	3040.909055	23.444403
110.702345	3040.481552	23.449421
110.631486	3047.874970	23.454439
110.758789	3040.586866	23.459456
110.795471	3058.287188	23.464474
110.995386	3068.662015	23.469491
111.243264	3069.583122	23.474509
111.279419	3083.843385	23.479527
111.848272	3088.375617	23.484544
111.296800	3078.384232	23.489562
111.285711	3075.615128	23.494579
112.030943	3101.111251	23.499597
112.004008	3100.067853	23.504615
112.200383	3102.969557	23.509632
112.260309	3105.860944	23.514650
111.755870	3099.191933	23.519667
112.285591	3098.298577	23.524685
112.203405	3110.153385	23.529703
112.596080	3114.299602	23.534720
112.913292	3122.964515	23.539738
112.774097	3125.331429	23.544755
112.749686	3123.949932	23.549773
112.667218	3131.016955	23.554791
112.927505	3130.026676	23.559808
113.168359	3141.364102	23.564826
113.504649	3142.912143	23.569843
113.309016	3146.209436	23.574861
113.802416	3141.764775	23.579879
113.589649	3137.161789	23.584896
113.409450	3150.900311	23.589914
113.635256	3156.587461	23.594931
114.097335	3162.988986	23.599949
113.917039	3166.646851	23.604967
114.468310	3168.685340	23.609984
114.552837	3189.158896	23.615002
114.471411	3186.220826	23.620019
114.447565	3188.629756	23.625037
114.476775	3186.173131	23.630055
115.193532	3180.027245	23.635072
114.901478	3188.443030	23.640090
115.002313	3183.579746	23.645107
115.491605	3198.703766	23.650125
115.465466	3209.767190	23.655143
115.394519	3205.561873	23.660160
115.343942	3212.844893	23.665178
115.625512	3201.404472	23.670195
115.949820	3204.879629	23.675213
115.780823	3212.048527	23.680231
115.589477	3202.913127	23.685248
115.911131	3222.825883	23.690266
116.172660	3221.715473	23.695283
116.015396	3221.045847	23.700301
116.203953	3219.899457	23.705319
116.379113	3220.929734	23.710336
116.591151	3234.897617	23.715354
116.856549	3243.176138	23.720371
117.181491	3245.170971	23.725389
117.253856	3234.533201	23.730407
117.131606	3239.820082	23.735424
117.229278	3254.127713	23.740442
117.481244	3242.180579	23.745459
117.408776	3242.943266	23.750477
117.551906	3249.388168	23.755495
117.979608	3255.422653	23.760512
117.813104	3268.518435	23.765530
117.833950	3266.094662	23.770547
117.818680	3264.837976	23.775565
117.978705	3269.812645	23.780583
118.161089	3273.524530	23.785600
118.389563	3290.582926	23.790618
118.641767	3295.287602	23.795635
118.633259	3287.783831	23.800653
118.909411	3297.035954	23.805671
118.735183	3294.541552	23.810688
118.902843	3296.235795	23.815706
119.272994	3303.289226	23.820723
119.552320	3305.338511	23.825741
119.365150	3303.897123	23.830759
119.671656	3306.169419	23.835776
119.470366	3302.145337	23.840794
119.492716	3300.993257	23.845811
119.977939	3312.292744	23.850829
119.879430	3326.605728	23.855847
120.147091	3317.951133	23.860864
120.282700	3323.816500	23.865882
120.068338	3328.808444	23.870899
120.495401	3329.711136	23.875917
120.420435	3342.316139	23.880935
120.635553	3340.499655	23.885952
121.239710	3347.683948	23.890970
121.114935	3342.606409	23.895987
121.366512	3342.791569	23.901005
121.422968	3336.574846	23.906023
121.571598	3338.660263	23.911040
121.665419	3335.417142	23.916058
121.680449	3354.042726	23.921075
122.035331	3354.183396	23.926093
121.888698	3354.932385	23.931111
122.006340	3353.494035	23.936128
122.112770	3360.137217	23.941146
122.040257	3363.125013	23.946163
122.022169	3351.235634	23.951181
122.233320	3365.276349	23.956199
122.369219	3374.629253	23.961216
122.650608	3374.917081	23.966234
122.480560	3383.749513	23.971251
122.766519	3388.808762	23.976269
123.085981	3403.069355	23.981287
123.181032	3404.430890	23.986304
123.183703	3408.388558	23.991322
123.191911	3418.184293	23.996339
123.831850	3405.195076	24.001357
123.366338	3410.516514	24.006375
123.851335	3420.146488	24.011392
123.853392	3430.470269	24.016410
123.849877	3440.378307	24.021427
124.229671	3436.298442	24.026445
124.095365	3435.934540	24.031463
124.152933	3435.417673	24.036480
124.272871	3443.087697	24.041498
124.128834	3454.267469	24.046515
124.256828	3458.454975	24.051533
124.334425	3464.329420	24.056551
124.527345	3484.013170	24.061568
125.054487	3479.998727	24.066586
124.980832	3480.774233	24.071603
125.131191	3493.322167	24.076621
125.201772	3502.738962	24.081639
125.511802	3507.829215	24.086656
125.768141	3505.993672	24.091674
125.429359	3514.076015	24.096691
126.032643	3519.183737	24.101709
126.281616	3527.158796	24.106727
126.173856	3526.572980	24.111744
126.587087	3533.973290	24.116762
126.172227	3527.454294	24.121779
126.562239	3524.780483	24.126797
127.486352	3526.356973	24.131815
127.678533	3529.758078	24.136832
127.898909	3524.718280	24.141850
127.358845	3521.573817	24.146867
127.737962	3504.733548	24.151885
127.571258	3508.367272	24.156903
127.413994	3513.243067	24.161920
128.129536	3526.747730	24.166938
128.088150	3539.830541	24.171955
128.129946	3529.329916	24.176973
127.979699	3527.450363	24.181991
127.973073	3530.737236	24.187008
128.116304	3530.358527	24.192026
127.878630	3545.782239	24.197043
128.429270	3546.807731	24.202061
128.542195	3550.101245	24.207079
128.583262	3560.109718	24.212096
128.849497	3558.828121	24.217114
128.753011	3571.225169	24.222131
129.039846	3582.688276	24.227149
129.295912	3586.546564	24.232167
129.445479	3596.187826	24.237184
129.770238	3604.586677	24.242202
129.764722	3615.498798	24.247219
129.648475	3606.196846	24.252237
129.635488	3603.367988	24.257255
129.731438	3614.497871	24.262272
129.883196	3621.042562	24.267290
129.830399	3631.902086	24.272307
130.540883	3651.044630	24.277325
130.570926	3651.636718	24.282343
129.963983	3657.649366	24.287360
130.954294	3648.664323	24.292378
130.893792	3669.366159	24.297395
131.108803	3672.924704	24.302413
131.382246	3673.930238	24.307431
131.432329	3676.182536	24.312448
131.478618	3669.755815	24.317466
131.717850	3683.741906	24.322483
131.848467	3690.829628	24.327501
131.778772	3702.730224	24.332519
131.993188	3693.566119	24.337536
132.259485	3687.244011	24.342554
131.972250	3703.309975	24.347571
132.136326	3720.542929	24.352589
132.573059	3716.286857	24.357607
132.384658	3719.636784	24.362624
132.292782	3728.378308	24.367642
132.806793	3741.463168	24.372659
132.870549	3745.698618	24.377677
132.899185	3749.747006	24.382695
132.998292	3753.494049	24.387712
133.834853	3769.041075	24.392730
133.574425	3783.720504	24.397747
133.859872	3776.779917	24.402765
133.884803	3771.325450	24.407783
134.052200	3771.432191	24.412800
134.345018	3762.167470	24.417818
134.399285	3781.314477	24.422835
134.476840	3790.064370	24.427853
134.739584	3797.706000	24.432871
134.635468	3797.100670	24.437888
134.815098	3793.721014	24.442906
134.684693	3798.384392	24.447923
134.825410	3815.674730	24.452941
135.208671	3817.332298	24.457959
135.189825	3817.872035	24.462976
135.205270	3806.772509	24.467994
135.375787	3829.540620	24.473011
135.697022	3838.798629	24.478029
135.794204	3839.121458	24.483047
135.703453	3850.103804	24.488064
135.952388	3857.324670	24.493082
136.547280	3873.502789	24.498099
136.180227	3865.088785	24.503117
136.581753	3871.752493	24.508135
136.476218	3891.110716	24.513152
136.906140	3886.581070	24.518170
137.033520	3892.870842	24.523187
136.776132	3895.467728	24.528205
137.030869	3894.939087	24.533223
137.350842	3917.216913	24.538240
137.755538	3918.400870	24.543258
137.675053	3912.918586	24.548275
137.811257	3915.690914	24.553293
138.302962	3928.675227	24.558311
138.337878	3933.435995	24.563328
138.700090	3932.893777	24.568346
138.562563	3932.530365	24.573363
138.908320	3938.994468	24.578381
139.012050	3933.717060	24.583399
138.734567	3937.964651	24.588416
139.179750	3922.189996	24.593434
139.091430	3936.871160	24.598451
139.197922	3947.904919	24.603469
139.749551	3952.796714	24.608487
139.884235	3953.473521	24.613504
140.159843	3946.105148	24.618522
140.011686	3943.237313	24.623539
140.203674	3948.118818	24.628557
140.250827	3943.607721	24.633575
140.014502	3957.159906	24.638592
140.395202	3963.959454	24.643610
140.322572	3972.306721	24.648627
140.275018	3969.249624	24.653645
140.809511	3977.379275	24.658663
140.980724	3991.272038	24.663680
141.029976	3994.764923	24.668698
141.349079	3995.245736	24.673715
140.731579	3995.332648	24.678733
141.394343	3999.960964	24.683751
141.613058	4009.405461	24.688768
141.830606	4008.128257	24.693786
141.716680	4007.439228	24.698803
141.940410	4016.917667	24.703821
142.323230	4016.703648	24.708839
142.001746	4034.015656	24.713856
142.368354	4034.542732	24.718874
142.509115	4034.202273	24.723891
142.634973	4030.913007	24.728909
143.009019	4042.896241	24.733927
142.825814	4062.594995	24.738944
142.941967	4054.310830	24.743962
143.039500	4059.718390	24.748979
143.254174	4071.256169	24.753997
143.147134	4073.491948	24.759015
143.365378	4085.597313	24.764032
143.533501	4085.552441	24.769050
143.606080	4103.617486	24.774067
143.854751	4109.888450	24.779085
144.142658	4127.601209	24.784103
144.464666	4139.194915	24.789120
144.356335	4137.589682	24.794138
144.621042	4131.270825	24.799155
144.326348	4141.666464	24.804173
144.989881	4153.986614	24.809191
145.115435	4157.303523	24.814208
145.316625	4158.563370	24.819226
145.293073	4165.943568	24.824243
145.207569	4180.125793	24.829261
145.585376	4181.601180	24.834279
145.356266	4197.838442	24.839296
145.909249	4202.411307	24.844314
146.383519	4207.062711	24.849331
146.351433	4205.606573	24.854349
146.604372	4211.696998	24.859367
146.792695	4215.572282	24.864384
147.057063	4226.209186	24.869402
147.105159	4232.445137	24.874419
147.139836	4230.621939	24.879437
147.284910	4222.090158	24.884455
147.557147	4248.245471	24.889472
147.911245	4245.125793	24.894490
147.815229	4249.714494	24.899507
147.703840	4251.225017	24.904525
147.928507	4247.282752	24.909543
148.279541	4264.635465	24.914560
148.482086	4271.112515	24.919578
148.618337	4281.084475	24.924595
148.871267	4264.935445	24.929613
149.172706	4264.803534	24.934631
149.115629	4270.298355	24.939648
149.143604	4265.824883	24.944666
149.583367	4266.930809	24.949683
149.315128	4280.491361	24.954701
149.782501	4280.327302	24.959719
149.445172	4281.352211	24.964736
149.688085	4277.530195	24.969754
149.693441	4283.826477	24.974771
150.093245	4293.561718	24.979789
150.599828	4287.558657	24.984807
150.711126	4299.911228	24.989824
150.698422	4296.084817	24.994842
150.927932	4302.374613	24.999859
150.860657	4301.286925	25.004877
151.302593	4310.472727	25.009895
151.198368	4314.349391	25.014912
151.200736	4313.348705	25.019930
151.668834	4318.168385	25.024947
151.568135	4321.201760	25.029965
151.618703	4320.139912	25.034983
151.512890	4336.399134	25.040000
151.670990	4356.199728	25.045018
151.896653	4352.629733	25.050035
151.890376	4366.563044	25.055053
152.137740	4359.625008	25.060071
152.315582	4363.066380	25.065088
152.419468	4370.549918	25.070106
153.049288	4391.691151	25.075123
153.305849	4386.913770	25.080141
153.292596	4380.331937	25.085159
153.443372	4382.669650	25.090176
153.125860	4393.716037	25.095194
153.526212	4395.519348	25.100211
153.601345	4417.264612	25.105229
154.083182	4404.463428	25.110247
154.525545	4416.234268	25.115264
154.395854	4423.940419	25.120282
154.879296	4428.060186	25.125299
154.905771	4433.223256	25.130317
155.164385	4432.697155	25.135335
154.810954	4437.644772	25.140352
154.951763	4441.293932	25.145370
155.435707	4438.415983	25.150387
155.694866	4453.071872	25.155405
155.712852	4456.588652	25.160423
155.962461	4452.879186	25.165440
155.573630	4459.899736	25.170458
155.834991	4456.450417	25.175475
155.913251	4474.511793	25.180493
156.013497	4478.145181	25.185511
156.491649	4489.212941	25.190528
156.260871	4503.837834	25.195546
156.688748	4497.490289	25.200563
156.452873	4508.817578	25.205581
156.910606	4526.898834	25.210599
157.098596	4535.527734	25.215616
157.450332	4536.738918	25.220634
157.726916	4552.730478	25.225651
157.768454	4556.032133	25.230669
158.262580	4550.359189	25.235687
158.357706	4543.470036	25.240704
158.163539	4558.944651	25.245722
158.547019	4553.191084	25.250739
158.513844	4567.397030	25.255757
158.558712	4570.032173	25.260775
158.813405	4574.572667	25.265792
159.006199	4587.300981	25.270810
159.406494	4596.736454	25.275827
159.300755	4614.337376	25.280845
159.498817	4602.827007	25.285863
159.516691	4606.997206	25.290880
159.851519	4609.274729	25.295898
160.254421	4616.282546	25.300915
160.097198	4622.522191	25.305933
160.177168	4626.891048	25.310951
160.589377	4631.129270	25.315968
160.368705	4644.799473	25.320986
160.685979	4638.513289	25.326003
160.945752	4655.807990	25.331021
160.975134	4671.645602	25.336039
161.189231	4670.675060	25.341056
160.982406	4684.696654	25.346074
161.522502	4694.366081	25.351091
161.361998	4706.095246	25.356109
161.626604	4700.880947	25.361127
162.033850	4718.263222	25.366144
162.164665	4730.777182	25.371162
162.226433	4724.877952	25.376179
162.212816	4736.363320	25.381197
162.278338	4740.513505	25.386215
162.855509	4743.053174	25.391232
162.546309	4754.357311	25.396250
162.836883	4760.798737	25.401267
162.854963	4764.770085	25.406285
162.918523	4773.699392	25.411303
163.458599	4789.842679	25.416320
163.673080	4795.390073	25.421338
163.766049	4794.959192	25.426355
163.872540	4819.083151	25.431373
164.294760	4813.806405	25.436391
164.554738	4813.573627	25.441408
164.749152	4822.858200	25.446426
165.138522	4825.262986	25.451443
165.180573	4832.465951	25.456461
165.555950	4827.101800	25.461479
165.721039	4828.667176	25.466496
165.751169	4817.318543	25.471514
165.979828	4818.921366	25.476531
165.904732	4819.978075	25.481549
166.426496	4828.441518	25.486567
166.780861	4843.483767	25.491584
166.273348	4851.239453	25.496602
166.854769	4841.234836	25.501619
166.761842	4846.909017	25.506637
166.853825	4842.886275	25.511655
166.866438	4853.082967	25.516672
167.213251	4863.104533	25.521690
167.396507	4870.730586	25.526707
167.280589	4871.212869	25.531725
167.518716	4890.711197	25.536743
167.760697	4889.010323	25.541760
167.707981	4896.692064	25.546778
168.129286	4911.888083	25.551795
167.883999	4920.603563	25.556813
168.316014	4915.880795	25.561831
168.721022	4936.053919	25.566848
168.811931	4938.034878	25.571866
168.941531	4945.495712	25.576883
169.138389	4954.183403	25.581901
169.019230	4969.495180	25.586919
169.254820	4961.741228	25.591936
169.162982	4982.790340	25.596954
169.820272	4978.007231	25.601971
170.147335	4990.497130	25.606989
170.282030	5001.258842	25.612007
170.413656	5015.158555	25.617024
170.313754	5015.508934	25.622042
170.653412	5020.367739	25.627059
171.304291	5036.124690	25.632077
171.200088	5040.149858	25.637095
171.724124	5034.891917	25.642112
171.849768	5041.488537	25.647130
171.751703	5041.589270	25.652147
171.895904	5038.906164	25.657165
171.989456	5050.592841	25.662183
172.301205	5059.461553	25.667200
172.064918	5066.010367	25.672218
172.443595	5062.852003	25.677236
172.389386	5073.302270	25.682253
172.704015	5083.691962	25.687271
172.908053	5085.093473	25.692288
172.685402	5090.917341	25.697306
172.939070	5106.111215	25.702324
173.448220	5109.008739	25.707341
173.563900	5124.615513	25.712359
173.888007	5123.119628	25.717376
174.117821	5139.775535	25.722394
173.913732	5135.451612	25.727412
173.942611	5139.667567	25.732429
174.561564	5155.063441	25.737447
174.816010	5153.931924	25.742464
174.956771	5168.840407	25.747482
174.865338	5164.236949	25.752500
175.220492	5169.165981	25.757517
175.529150	5176.520121	25.762535
175.540083	5178.087432	25.767552
175.771828	5184.247772	25.772570
175.788821	5189.538793	25.777588
176.211786	5203.166025	25.782605
175.910482	5206.773695	25.787623
176.445184	5206.330848	25.792640
176.594659	5213.233156	25.797658
176.367827	5224.414283	25.802676
176.827316	5224.519749	25.807693
176.808217	5239.686759	25.812711
177.332819	5253.026745	25.817728
176.986442	5265.198711	25.822746
177.547589	5266.472038	25.827764
178.109166	5284.017061	25.832781
178.062459	5284.384415	25.837799
178.244312	5286.701625	25.842816
178.320729	5302.046362	25.847834
178.545677	5305.748884	25.852852
178.860144	5309.415373	25.857869
178.580667	5313.041762	25.862887
179.044315	5321.325095	25.867904
179.121859	5332.916594	25.872922
179.426105	5340.969076	25.877940
179.695325	5347.344592	25.882957
179.626613	5357.462690	25.887975
180.040225	5347.629123	25.892992
180.096358	5356.651413	25.898010
180.777029	5368.344737	25.903028
180.925527	5368.643823	25.908045
180.849817	5372.415264	25.913063
181.479835	5369.795359	25.918080
181.606961	5381.578030	25.923098
181.764013	5391.749381	25.928116
181.756391	5385.463019	25.933133
181.533492	5399.686527	25.938151
182.151227	5391.017478	25.943168
182.281582	5393.986650	25.948186
181.967725	5409.619510	25.953204
182.279653	5412.809781	25.958221
182.517925	5416.210381	25.963239
182.750620	5414.277321	25.968256
182.650566	5430.119964	25.973274
182.888232	5432.807286	25.978292
183.340570	5452.168702	25.983309
183.561855	5462.992963	25.988327
183.785390	5456.471726	25.993344
184.110934	5461.771607	25.998362
184.122378	5474.737110	26.003380
184.480274	5474.858396	26.008397
184.530708	5479.863364	26.013415
184.598431	5472.346818	26.018432
184.928522	5479.258985	26.023450
185.194230	5487.749978	26.028468
185.192374	5490.057937	26.033485
185.092323	5504.821108	26.038503
185.417187	5512.554803	26.043520
185.575556	5523.739272	26.048538
185.498375	5529.379648	26.053556
186.125506	5531.706478	26.058573
185.826407	5559.350984	26.063591
186.082380	5552.196510	26.068608
186.381344	5558.845247	26.073626
186.248027	5579.327014	26.078644
186.711328	5579.135174	26.083661
186.994443	5582.579329	26.088679
187.534426	5590.052293	26.093696
187.790729	5590.378790	26.098714
187.556828	5596.614924	26.103732
187.826160	5613.495541	26.108749
187.969604	5625.626208	26.113767
188.436451	5616.636480	26.118784
188.766980	5625.685627	26.123802
188.548988	5635.003258	26.128820
188.725709	5634.328889	26.133837
188.684054	5643.858969	26.138855
189.080148	5656.464842	26.143872
189.335319	5661.415889	26.148890
189.338389	5672.930816	26.153908
189.813658	5685.003547	26.158925
189.831304	5699.486556	26.163943
190.126073	5694.406168	26.168960
190.591156	5696.663552	26.173978
190.589818	5720.205746	26.178996
190.920485	5717.850204	26.184013
190.662837	5717.612779	26.189031
191.233863	5724.260255	26.194048
191.269999	5739.021352	26.199066
191.623277	5740.055612	26.204084
191.928282	5743.417475	26.209101
191.796038	5759.606326	26.214119
192.227863	5757.080356	26.219136
192.003573	5761.856708	26.224154
192.274188	5779.182358	26.229172
192.752948	5781.718559	26.234189
192.629245	5787.034816	26.239207
192.853969	5799.354967	26.244224
193.148717	5797.967767	26.249242
193.139881	5824.727831	26.254260
193.469736	5834.711539	26.259277
193.824792	5845.259517	26.264295
193.758183	5857.157887	26.269312
193.875053	5862.061075	26.274330
194.408382	5876.454468	26.279348
194.377676	5879.717107	26.284365
194.345927	5882.493791	26.289383
195.029953	5906.210459	26.294400
195.463551	5912.787859	26.299418
195.677563	5910.349442	26.304436
195.787549	5911.247977	26.309453
195.825622	5928.774117	26.314471
196.161775	5942.661637	26.319488
196.475679	5938.304225	26.324506
196.208375	5943.658668	26.329524
196.929729	5958.256441	26.334541
196.941805	5961.180989	26.339559
197.054990	5970.245206	26.344576
197.376046	5962.935233	26.349594
197.201129	5984.588725	26.354612
197.698020	5985.793194	26.359629
197.920705	5995.137098	26.364647
197.993922	6007.048519	26.369664
198.256938	6011.963718	26.374682
198.462510	6018.702923	26.379700
198.382343	6020.025646	26.384717
198.684520	6035.061226	26.389735
198.845483	6034.654454	26.394752
199.169993	6035.649017	26.399770
199.244837	6071.929449	26.404788
199.323989	6061.263713	26.409805
199.407842	6071.819323	26.414823
199.854381	6081.014780	26.419840
200.023175	6091.074211	26.424858
199.747921	6086.407597	26.429876
200.052638	6104.934085	26.434893
200.198499	6121.670251	26.439911
200.531908	6139.990282	26.444928
201.040671	6140.167003	26.449946
201.173336	6155.674161	26.454964
201.613449	6158.670991	26.459981
201.722148	6172.215300	26.464999
201.304829	6177.141764	26.470016
202.362305	6188.521266	26.475034
202.259033	6198.790418	26.480052
202.484519	6200.614826	26.485069
202.842741	6213.858314	26.490087
202.795196	6222.957151	26.495104
203.323426	6215.690583	26.500122
203.318818	6235.067155	26.505140
203.451533	6248.121653	26.510157
203.464783	6250.626227	26.515175
203.801053	6263.235522	26.520192
204.367426	6260.208723	26.525210
204.396673	6269.693367	26.530228
204.584289	6271.668886	26.535245
204.550166	6290.971195	26.540263
204.645979	6296.455451	26.545280
204.952556	6302.067885	26.550298
205.208925	6313.016614	26.555316
205.424722	6325.231183	26.560333
205.420454	6340.930278	26.565351
205.618759	6352.153233	26.570368
205.951969	6352.044776	26.575386
206.221213	6371.508280	26.580404
206.224503	6387.723936	26.585421
206.653764	6399.384466	26.590439
206.768515	6422.031930	26.595456
207.006427	6419.573942	26.600474
207.436226	6431.449064	26.605492
207.509835	6437.871203	26.610509
207.998729	6450.198015	26.615527
208.072086	6472.971941	26.620544
208.237980	6468.287053	26.625562
208.219498	6482.646883	26.630580
208.964285	6494.798147	26.635597
208.820474	6501.547733	26.640615
208.959105	6515.842090	26.645632
209.593275	6520.305052	26.650650
209.608736	6520.315513	26.655668
209.554337	6535.624834	26.660685
209.746046	6548.698773	26.665703
210.085016	6549.075554	26.670720
210.405852	6565.377668	26.675738
210.636060	6576.194889	26.680756
210.973803	6581.385870	26.685773
211.565641	6585.508199	26.690791
211.081009	6594.381694	26.695808
212.204583	6587.391629	26.700826
212.068334	6581.582607	26.705844
212.445555	6599.694248	26.710861
212.813940	6610.423685	26.715879
212.511620	6609.738632	26.720896
212.832456	6608.060049	26.725914
213.159947	6614.060758	26.730932
213.151433	6621.546939	26.735949
213.468468	6630.683919	26.740967
213.764662	6627.752790	26.745984
213.599492	6640.377280	26.751002
213.997205	6631.217886	26.756020
214.047427	6641.589658	26.761037
214.132276	6642.668920	26.766055
214.553486	6659.545801	26.771072
214.838768	6661.521941	26.776090
214.587930	6665.803894	26.781108
214.798442	6681.757107	26.786125
215.261457	6687.626255	26.791143
214.920251	6699.173331	26.796160
215.318157	6714.690177	26.801178
215.172803	6718.734748	26.806196
215.644132	6734.319098	26.811213
215.764264	6743.218466	26.816231
215.875982	6768.515348	26.821248
216.239361	6781.133408	26.826266
216.615979	6807.964327	26.831284
216.624306	6817.531431	26.836301
217.051002	6830.944643	26.841319
217.229945	6847.505858	26.846336
217.683545	6849.730453	26.851354
218.009758	6869.226656	26.856372
218.104820	6871.087222	26.861389
218.250614	6892.698169	26.866407
218.469182	6913.751688	26.871424
219.070732	6909.415556	26.876442
219.574900	6928.303269	26.881460
219.693251	6929.633032	26.886477
219.996129	6931.341291	26.891495
220.362812	6937.793740	26.896512
220.856419	6945.899529	26.901530
220.817756	6951.575385	26.906548
220.900820	6950.663008	26.911565
221.108147	6944.945591	26.916583
220.766777	6949.090179	26.921600
221.376774	6962.998978	26.926618
221.233588	6961.840870	26.931636
221.642109	6989.348956	26.936653
222.053586	6994.029801	26.941671
221.964827	6993.882864	26.946688
222.261310	7008.175128	26.951706
222.528750	7020.157989	26.956724
222.665715	7022.384549	26.961741
223.145965	7040.938324	26.966759
222.947187	7056.513632	26.971776
223.482915	7057.491154	26.976794
223.651009	7059.996985	26.981812
223.614141	7070.862394	26.986829
224.195658	7078.998751	26.991847
224.314842	7094.300455	26.996864
224.596573	7103.193779	27.001882
224.667758	7107.195252	27.006900
224.609247	7121.511305	27.011917
225.100251	7133.560452	27.016935
225.161710	7139.665889	27.021952
225.634740	7156.610926	27.026970
225.877788	7160.418342	27.031988
226.408075	7178.077397	27.037005
226.696570	7180.302484	27.042023
226.622716	7193.175153	27.047040
226.830477	7192.385408	27.052058
226.796898	7209.949186	27.057076
226.957200	7227.403874	27.062093
227.499144	7229.892564	27.067111
227.154993	7250.071242	27.072128
227.611165	7257.264357	27.077146
228.382247	7272.448932	27.082164
228.206301	7279.828861	27.087181
228.776598	7294.798481	27.092199
228.333128	7299.650393	27.097216
229.162272	7310.087527	27.102234
229.010235	7319.979762	27.107252
229.521374	7332.259512	27.112269
229.291077	7334.186564	27.117287
229.599797	7356.366181	27.122304
229.977605	7359.025659	27.127322
230.690157	7362.996785	27.132340
230.774368	7368.795698	27.137357
231.194676	7361.848542	27.142375
231.337022	7382.668232	27.147392
231.526487	7394.063673	27.152410
231.519867	7391.119588	27.157428
232.048830	7404.176357	27.162445
232.144871	7409.231577	27.167463
232.186077	7422.866241	27.172480
232.684077	7427.814689	27.177498
233.026018	7443.962771	27.182516
232.803126	7448.205829	27.187533
233.167621	7452.442674	27.192551
233.383185	7464.118215	27.197568
233.487379	7473.216145	27.202586
233.563846	7479.297261	27.207604
233.538084	7498.574284	27.212621
234.065756	7515.937326	27.217639
233.978451	7535.789053	27.222656
234.488452	7548.230127	27.227674
234.773958	7570.164222	27.232692
234.852858	7581.447560	27.237709
235.436955	7590.060436	27.242727
235.677607	7604.895374	27.247744
235.744406	7614.892600	27.252762
236.223188	7636.664094	27.257780
236.338863	7647.007302	27.262797
236.865175	7650.827544	27.267815
236.700879	7664.235514	27.272832
236.977094	7686.338510	27.277850
237.153179	7686.810130	27.282868
237.231198	7710.566668	27.287885
237.989007	7715.534727	27.292903
238.240087	7723.871194	27.297920
238.454049	7736.832024	27.302938
238.814548	7741.801966	27.307956
239.053699	7752.795278	27.312973
239.146162	7762.229813	27.317991
239.382146	7784.695924	27.323008
240.021945	7791.595479	27.328026
240.189702	7788.807284	27.333044
240.427022	7808.390936	27.338061
240.818799	7797.505045	27.343079
241.122526	7809.148137	27.348096
241.596595	7812.528261	27.353114
241.927253	7815.719199	27.358132
241.637534	7838.788117	27.363149
241.764248	7828.559079	27.368167
241.731626	7839.493733	27.373184
241.911116	7851.797054	27.378202
242.594325	7844.287892	27.383220
242.411158	7857.518994	27.388237
242.843659	7860.293152	27.393255
243.065659	7865.543560	27.398272
243.336393	7883.205822	27.403290
243.283999	7889.345019	27.408308
243.629666	7909.647480	27.413325
244.217165	7924.144550	27.418343
244.015675	7913.401467	27.423360
244.410364	7933.547945	27.428378
244.752739	7945.870167	27.433396
244.808047	7950.369939	27.438413
245.127556	7961.947532	27.443431
245.406859	7978.115307	27.448448
245.289668	7993.044154	27.453466
245.943607	8000.831853	27.458484
246.350786	8008.427514	27.463501
246.806247	8011.779003	27.468519
247.254875	8018.089641	27.473536
247.344979	8020.683514	27.478554
247.803259	8017.117636	27.483572
247.688120	8026.439407	27.488589
247.955193	8025.305754	27.493607
248.106389	8039.589872	27.498624
248.253804	8038.301214	27.503642
248.412550	8047.337268	27.508660
248.543413	8063.304083	27.513677
248.726191	8063.904107	27.518695
248.981968	8077.010203	27.523712
248.697497	8087.422270	27.528730
249.270503	8104.592550	27.533748
249.484008	8125.133657	27.538765
249.990651	8144.372665	27.543783
250.204194	8150.060137	27.548800
250.617593	8169.010616	27.553818
250.834871	8172.156128	27.558836
250.937006	8193.317638	27.563853
251.110766	8204.889662	27.568871
251.927184	8217.627600	27.573888
251.480289	8235.862850	27.578906
252.333156	8243.607054	27.583924
252.315924	8259.530798	27.588941
252.617642	8269.015097	27.593959
252.740201	8278.890350	27.598976
253.265372	8291.080163	27.603994
253.332773	8306.741367	27.609012
253.515935	8321.147008	27.614029
253.503545	8339.595688	27.619047
253.649912	8345.337876	27.624064
253.930361	8376.801639	27.629082
254.402592	8387.563308	27.634100
254.328495	8397.904913	27.639117
254.791728	8416.165967	27.644135
255.401066	8436.749978	27.649152
255.222563	8457.766059	27.654170
255.730530	8463.249937	27.659188
256.277688	8478.820810	27.664205
256.585536	8494.479466	27.669223
257.213009	8483.089233	27.674240
257.701195	8493.873737	27.679258
258.188674	8497.289787	27.684276
257.725719	8516.771693	27.689293
257.624255	8507.944810	27.694311
258.342775	8521.818957	27.699328
258.586636	8532.650992	27.704346
259.337927	8532.616350	27.709364
258.628558	8541.961439	27.714381
259.258620	8559.893585	27.719399
259.706633	8566.207666	27.724416
259.815311	8588.429384	27.729434
260.432416	8595.225437	27.734452
260.411729	8597.707201	27.739469
260.259116	8605.276608	27.744487
260.681731	8614.192931	27.749504
260.633020	8628.597027	27.754522
260.993157	8638.656480	27.759540
261.315803	8652.797569	27.764557
261.745058	8663.433492	27.769575
262.071339	8669.236171	27.774592
262.120570	8677.759193	27.779610
262.610658	8677.266398	27.784628
263.116940	8689.800382	27.789645
262.801631	8690.942065	27.794663
263.024343	8710.238498	27.799680
263.475007	8720.691167	27.804698
263.644514	8729.653267	27.809716
263.501215	8744.937223	27.814733
263.669951	8760.583035	27.819751
264.240063	8767.563267	27.824768
264.358532	8789.060726	27.829786
264.776285	8797.652714	27.834804
264.578262	8820.203443	27.839821
265.402798	8842.525543	27.844839
265.848100	8839.293027	27.849856
265.912998	8860.612640	27.854874
266.585708	8876.199031	27.859892
266.338773	8889.248214	27.864909
266.422357	8908.970627	27.869927
267.040538	8920.297110	27.874944
267.542628	8939.525030	27.879962
267.697531	8951.997084	27.884980
267.520107	8963.763173	27.889997
268.014349	8981.338019	27.895015
268.178931	9000.798505	27.900032
268.613550	9014.448867	27.905050
268.796127	9032.195412	27.910068
269.008292	9045.823602	27.915085
269.360132	9072.510140	27.920103
269.769748	9074.902875	27.925120
269.730997	9105.798772	27.930138
270.006160	9111.682163	27.935156
270.188564	9130.849552	27.940173
270.593451	9152.773259	27.945191
270.961913	9160.574327	27.950208
271.032071	9181.445172	27.955226
271.778885	9194.317755	27.960244
271.908922	9208.113553	27.965261
272.873467	9227.257145	27.970279
272.679424	9229.835440	27.975296
272.989585	9247.991706	27.980314
273.474758	9258.240405	27.985332
273.734415	9267.940141	27.990349
273.949209	9283.175105	27.995367
274.199518	9282.435479	28.000384
274.510759	9303.578333	28.005402
274.737656	9308.320083	28.010420
274.875751	9323.999557	28.015437
275.005830	9342.856435	28.020455
275.540333	9349.570913	28.025472
275.543697	9364.788346	28.030490
275.857296	9375.221682	28.035508
276.771441	9387.449538	28.040525
276.653345	9393.867825	28.045543
276.949358	9403.486199	28.050560
277.184752	9417.161561	28.055578
277.360540	9428.582490	28.060596
277.832032	9442.435805	28.065613
277.936485	9455.563282	28.070631
278.217693	9456.662656	28.075648
278.605771	9481.389823	28.080666
278.515712	9488.504682	28.085684
279.223542	9495.637398	28.090701
279.151236	9519.732230	28.095719
279.536446	9524.919816	28.100736
279.698525	9541.268230	28.105754
280.201413	9543.327625	28.110772
280.066077	9555.302228	28.115789
280.138741	9581.452032	28.120807
280.533691	9589.230214	28.125824
281.065268	9609.110946	28.130842
281.150608	9621.051235	28.135860
281.443954	9634.304136	28.140877
281.315903	9655.057981	28.145895
281.909658	9658.347200	28.150912
282.497254	9685.313643	28.155930
282.621804	9689.316840	28.160948
282.979077	9716.972740	28.165965
282.762845	9730.488165	28.170983
283.360363	9752.183684	28.176000
283.658111	9774.847823	28.181018
283.728764	9787.456689	28.186036
284.168934	9807.642335	28.191053
284.160538	9821.314905	28.196071
284.511212	9840.106372	28.201088
285.268513	9872.600330	28.206106
285.314820	9871.987162	28.211124
286.141144	9887.698885	28.216141
286.115256	9907.433087	28.221159
286.857025	9906.089656	28.226176
286.905026	9929.512729	28.231194
287.232069	9941.159852	28.236212
287.617876	9958.897746	28.241229
287.955646	9967.089124	28.246247
288.568091	9977.387870	28.251264
288.964849	9991.224815	28.256282
289.167257	9991.632409	28.261300
289.302389	9989.262573	28.266317
288.948385	10015.005817	28.271335
289.453049	10025.561326	28.276352
289.836444	10036.132562	28.281370
289.918869	10047.483160	28.286388
290.107110	10067.872492	28.291405
290.594475	10092.891277	28.296423
290.876262	10099.939006	28.301440
291.069743	10113.062559	28.306458
291.605047	10123.622825	28.311476
291.891891	10143.056003	28.316493
291.883584	10159.763008	28.321511
292.529014	10165.175478	28.326528
292.232880	10184.219544	28.331546
292.724241	10201.256092	28.336564
293.399472	10219.489082	28.341581
293.876216	10238.128715	28.346599
293.913846	10247.162598	28.351616
294.187743	10269.786851	28.356634
294.441659	10275.383444	28.361652
294.847092	10289.891778	28.366669
294.853941	10318.922906	28.371687
295.351369	10331.124703	28.376704
295.730762	10343.297524	28.381722
296.085555	10362.249904	28.386740
296.326160	10376.907105	28.391757
296.379545	10385.067166	28.396775
296.855491	10400.177140	28.401792
297.141875	10411.546724	28.406810
297.299338	10425.373887	28.411828
298.067597	10431.982906	28.416845
298.325633	10458.275582	28.421863
298.821696	10461.226529	28.426880
298.913632	10466.418993	28.431898
299.438921	10478.411319	28.436916
299.572584	10492.065422	28.441933
299.428098	10506.672170	28.446951
299.755377	10507.606566	28.451968
300.006931	10525.441679	28.456986
300.200747	10537.700353	28.462004
300.679759	10541.553827	28.467021
300.414582	10568.291216	28.472039
300.588557	10579.738394	28.477056
301.832909	10593.835349	28.482074
301.752476	10606.102033	28.487092
301.909847	10619.477843	28.492109
302.200469	10636.100847	28.497127
303.019481	10654.583418	28.502144
303.304814	10658.006086	28.507162
303.375320	10680.779328	28.512180
303.880105	10689.238665	28.517197
304.024574	10698.426635	28.522215
304.038251	10711.660696	28.527232
304.753709	10735.435539	28.532250
305.109704	10743.662313	28.537268
305.123631	10763.896413	28.542285
305.465517	10781.916627	28.547303
305.912291	10794.565500	28.552320
305.851766	10798.294635	28.557338
305.956153	10827.014568	28.562356
306.509355	10839.141710	28.567373
306.689464	10859.542646	28.572391
307.189937	10878.144495	28.577408
307.406247	10894.280420	28.582426
307.702042	10903.789094	28.587444
308.063034	10923.672533	28.592461
308.755467	10940.391125	28.597479
308.740404	10959.041742	28.602496
309.188263	10974.462830	28.607514
309.358447	11001.436176	28.612532
309.839094	11015.993359	28.617549
309.948813	11038.981956	28.622567
310.420020	11050.995702	28.627584
310.836879	11065.003979	28.632602
310.958889	11084.195414	28.637620
311.457516	11093.868372	28.642637
311.703690	11116.924231	28.647655
312.098421	11117.983931	28.652672
312.586859	11142.470342	28.657690
312.805074	11160.810139	28.662708
313.153761	11165.684965	28.667725
313.463856	11189.248793	28.672743
313.367631	11205.020009	28.677760
313.973537	11227.060114	28.682778
313.987479	11235.908712	28.687796
314.863225	11259.302470	28.692813
314.610462	11276.815810	28.697831
314.840672	11297.310465	28.702848
315.411465	11312.018037	28.707866
315.478949	11332.275988	28.712884
316.272559	11344.681786	28.717901
316.229983	11365.215826	28.722919
316.581119	11380.203937	28.727936
317.323732	11400.761021	28.732954
316.865498	11425.950915	28.737972
318.111298	11421.077711	28.742989
318.726157	11443.883964	28.748007
319.230947	11448.557738	28.753024
319.696151	11439.196026	28.758042
319.959246	11446.215600	28.763060
320.482313	11460.839151	28.768077
320.624415	11461.073031	28.773095
320.593475	11468.192069	28.778112
321.047917	11469.431947	28.783130
321.165199	11480.736942	28.788148
321.450434	11484.194513	28.793165
321.243816	11496.825599	28.798183
321.306926	11509.335762	28.803200
321.665245	11524.117629	28.808218
321.900414	11544.782291	28.813236
322.108204	11547.137307	28.818253
322.634263	11567.358853	28.823271
322.464292	11591.976777	28.828288
323.353077	11602.012374	28.833306
324.096409	11611.113874	28.838324
324.583314	11614.085380	28.843341
324.686174	11640.953298	28.848359
324.795586	11648.931522	28.853376
325.358220	11660.303067	28.858394
325.657977	11683.370228	28.863412
325.888548	11687.742576	28.868429
326.167292	11699.050984	28.873447
326.347889	11718.729691	28.878464
326.930013	11726.274387	28.883482
327.227737	11743.983488	28.888500
327.240670	11753.138775	28.893517
327.586586	11774.964238	28.898535
327.844589	11795.189871	28.903552
328.382238	11812.406987	28.908570
328.636461	11833.337399	28.913588
328.825166	11850.305744	28.918605
329.533138	11874.026367	28.923623
329.463166	11892.133876	28.928640
329.662214	11910.060584	28.933658
329.667671	11929.024734	28.938676
330.452693	11949.080071	28.943693
330.938437	11974.550019	28.948711
330.823556	11994.830762	28.953728
331.343870	12012.663345	28.958746
331.490038	12040.996559	28.963764
332.196142	12063.757786	28.968781
332.745487	12081.822739	28.973799
332.793397	12101.598289	28.978816
333.029985	12118.808877	28.983834
333.183365	12151.362938	28.988852
333.892583	12169.409402	28.993869
334.540841	12179.520651	28.998887
334.623833	12202.849550	29.003904
335.306377	12209.324142	29.008922
335.674035	12229.482650	29.013940
335.563833	12244.044362	29.018957
336.319343	12266.384486	29.023975
336.247859	12281.511742	29.028992
336.601366	12302.761936	29.034010
336.893367	12322.518663	29.039028
337.415901	12343.016317	29.044045
337.808487	12365.615154	29.049063
337.781213	12384.468024	29.054080
338.156248	12393.526199	29.059098
338.758962	12429.607425	29.064116
338.991531	12449.086185	29.069133
339.298665	12469.229111	29.074151
339.338981	12479.552005	29.079168
339.967261	12506.298310	29.084186
339.981358	12526.414290	29.089204
340.582011	12543.057034	29.094221
341.026238	12560.750412	29.099239
341.519204	12581.688698	29.104256
341.677164	12596.954162	29.109274
342.185308	12614.969204	29.114292
342.210059	12635.636249	29.119309
342.878603	12650.234924	29.124327
343.020708	12671.711071	29.129344
343.202489	12682.839386	29.134362
343.847817	12707.230789	29.139380
344.034840	12716.021561	29.144397
344.593065	12737.183535	29.149415
345.030644	12752.118235	29.154432
345.004968	12774.631108	29.159450
345.492161	12785.705621	29.164468
345.532962	12804.491473	29.169485
345.829159	12824.885946	29.174503
346.189365	12845.415735	29.179520
346.718421	12855.706956	29.184538
346.934843	12892.070254	29.189556
347.306235	12904.378618	29.194573
348.045998	12926.589353	29.199591
347.776928	12954.129664	29.204608
348.938149	12963.226766	29.209626
348.825142	12984.240893	29.214644
349.386509	13010.502556	29.219661
349.890116	13016.417934	29.224679
349.907038	13041.172860	29.229696
350.018855	13061.514191	29.234714
350.737053	13075.657056	29.239732
350.914623	13096.509230	29.244749
351.380203	13117.408166	29.249767
351.463666	13143.024429	29.254784
351.717638	13149.303970	29.259802
352.395039	13178.617225	29.264820
352.695899	13208.137566	29.269837
353.369048	13211.670853	29.274855
353.481236	13248.205800	29.279872
353.972044	13270.095703	29.284890
354.186106	13291.479247	29.289908
354.485774	13313.316854	29.294925
355.228573	13328.441334	29.299943
355.023923	13350.995388	29.304960
355.654451	13370.135251	29.309978
355.882454	13385.286239	29.314996
356.430147	13408.076915	29.320013
357.002219	13415.333335	29.325031
357.222369	13447.481345	29.330048
358.101055	13465.177409	29.335066
358.381357	13479.682436	29.340084
358.378145	13495.627404	29.345101
358.783429	13511.136156	29.350119
358.840838	13540.003336	29.355136
359.851688	13543.070427	29.360154
359.938000	13564.499433	29.365172
360.359201	13583.113151	29.370189
360.979762	13590.930515	29.375207
361.316237	13611.616413	29.380224
361.609621	13618.398400	29.385242
361.725672	13644.859749	29.390260
361.895263	13666.474854	29.395277
362.249366	13683.842263	29.400295
362.590873	13708.828585	29.405312
362.920435	13726.414593	29.410330
363.266307	13737.530617	29.415348
363.758419	13758.792454	29.420365
364.360049	13767.200216	29.425383
364.553983	13793.501224	29.430400
364.723829	13803.252035	29.435418
365.234923	13824.706784	29.440436
365.703410	13846.076610	29.445453
366.041159	13860.588776	29.450471
366.454256	13884.721010	29.455488
367.062530	13904.935431	29.460506
367.485253	13908.106778	29.465524
367.574523	13944.630846	29.470541
367.847658	13944.133816	29.475559
368.280560	13963.172414	29.480576
368.201901	13965.408117	29.485594
368.760384	13985.766169	29.490612
368.805234	14005.894724	29.495629
369.554831	14021.463980	29.500647
369.656606	14036.410924	29.505664
369.994972	14061.489783	29.510682
369.942505	14076.069180	29.515700
370.513209	14101.787732	29.520717
371.218317	14123.616840	29.525735
371.797455	14152.621630	29.530752
372.076576	14166.527346	29.535770
372.237883	14191.011814	29.540788
372.553064	14211.243769	29.545805
373.283416	14233.612253	29.550823
373.488141	14246.923270	29.555840
373.755255	14268.343872	29.560858
374.327165	14285.886354	29.565876
374.777548	14314.573528	29.570893
374.836476	14346.416568	29.575911
375.203521	14362.813067	29.580928
375.608811	14374.949737	29.585946
376.305090	14409.330627	29.590964
376.595918	14422.985222	29.595981
376.910507	14438.843609	29.600999
377.355313	14468.624572	29.606016
377.794206	14487.940674	29.611034
378.261314	14508.916705	29.616052
378.511047	14522.460921	29.621069
379.226238	14544.974247	29.626087
379.629735	14560.499929	29.631104
380.075218	14586.153366	29.636122
380.308254	14596.870594	29.641140
380.258512	14628.715235	29.646157
380.970170	14646.732115	29.651175
381.370224	14657.792873	29.656192
381.676449	14684.178693	29.661210
382.101599	14698.422088	29.666228
382.742171	14717.587018	29.671245
382.923131	14732.149526	29.676263
383.653595	14755.443934	29.681280
383.669280	14770.679613	29.686298
384.465591	14788.964522	29.691316
384.246326	14818.827311	29.696333
384.788406	14827.930131	29.701351
384.788476	14858.320981	29.706368
385.286597	14877.107167	29.711386
385.747854	14894.174772	29.716404
385.828116	14926.656562	29.721421
386.290176	14940.190128	29.726439
387.034889	14977.668957	29.731456
387.554500	14991.856811	29.736474
387.881579	15006.778916	29.741492
388.393755	15040.343225	29.746509
388.423991	15051.341777	29.751527
388.826630	15079.342745	29.756544
388.896354	15097.321032	29.761562
389.971215	15120.799134	29.766580
389.968804	15139.859311	29.771597
390.355315	15168.826163	29.776615
390.920875	15196.811414	29.781632
391.335586	15211.824257	29.786650
391.510173	15235.505822	29.791668
391.685375	15266.744875	29.796685
391.880924	15291.588620	29.801703
392.416127	15316.202659	29.806720
392.909356	15341.385425	29.811738
393.681455	15363.158158	29.816756
394.128618	15388.089184	29.821773
394.233876	15404.669457	29.826791
395.006078	15421.745974	29.831808
395.248338	15432.057986	29.836826
395.573474	15442.319202	29.841844
395.602279	15473.117126	29.846861
396.205355	15490.194769	29.851879
396.808477	15521.332879	29.856896
396.928616	15549.526954	29.861914
397.689794	15566.163164	29.866932
397.849284	15588.754765	29.871949
398.525542	15598.389759	29.876967
398.806462	15622.923768	29.881984
399.110816	15627.601373	29.887002
399.782440	15651.013420	29.892020
400.073206	15681.799321	29.897037
400.350974	15696.135890	29.902055
400.549673	15719.413202	29.907072
401.215263	15738.827929	29.912090
401.638309	15762.082999	29.917108
401.951065	15782.977083	29.922125
401.922266	15806.154111	29.927143
402.917678	15821.683421	29.932160
403.375225	15837.896555	29.937178
403.792980	15857.593175	29.942196
404.444954	15883.254111	29.947213
404.748178	15899.428156	29.952231
405.165123	15915.606619	29.957248
405.358995	15945.975343	29.962266
405.852378	15954.195643	29.967284
406.145821	15977.287970	29.972301
406.438299	15998.880276	29.977319
406.857087	16020.812990	29.982336
407.053448	16040.635857	29.987354
407.849482	16065.671372	29.992372
407.919242	16090.883154	29.997389
408.484644	16114.571289	30.002407
409.289088	16133.949011	30.007424
409.553861	16157.582936	30.012442
410.219376	16170.349809	30.017460
410.411782	16191.443102	30.022477
410.433543	16209.966821	30.027495
411.147132	16236.566144	30.032512
411.417735	16260.549866	30.037530
412.371760	16275.773314	30.042548
412.846314	16306.253672	30.047565
412.716185	16320.281524	30.052583
413.291297	16345.588677	30.057600
413.823507	16361.519012	30.062618
414.269301	16383.495313	30.067636
414.313194	16401.276711	30.072653
414.410415	16426.023535	30.077671
414.960056	16450.403068	30.082688
415.192108	16483.539765	30.087706
415.934674	16505.602657	30.092724
416.537924	16535.539051	30.097741
416.676439	16560.023788	30.102759
417.550140	16581.804205	30.107776
417.769088	16607.713557	30.112794
418.129494	16621.687371	30.117812
418.283808	16645.020093	30.122829
418.586025	16670.325942	30.127847
419.279342	16706.015864	30.132864
419.432585	16734.064398	30.137882
419.867310	16746.690715	30.142900
420.430193	16785.351071	30.147917
420.464396	16810.938871	30.152935
421.205169	16830.412490	30.157952
421.734820	16858.364704	30.162970
421.693841	16875.240643	30.167988
421.840481	16903.419948	30.173005
422.687514	16930.776443	30.178023
423.230942	16961.414519	30.183040
423.595313	16983.344172	30.188058
424.394792	16990.910840	30.193076
424.761576	17019.596143	30.198093
425.110615	17044.541446	30.203111
425.839935	17061.228139	30.208128
426.052558	17087.372851	30.213146
426.658947	17100.803360	30.218164
426.724154	17122.915563	30.223181
427.221659	17150.873207	30.228199
427.803370	17174.218996	30.233216
428.218410	17199.454282	30.238234
428.223785	17216.452802	30.243252
428.787205	17234.150930	30.248269
429.060725	17254.282048	30.253287
429.842778	17290.098216	30.258304
430.004552	17324.043251	30.263322
430.882721	17351.591328	30.268340
431.271156	17379.023016	30.273357
431.155614	17406.946972	30.278375
431.812223	17419.239127	30.283392
431.921793	17459.399073	30.288410
432.313862	17484.714115	30.293428
433.036168	17516.986629	30.298445
433.544510	17552.675334	30.303463
434.213310	17575.976467	30.308480
434.670020	17606.878598	30.313498
434.895447	17634.020168	30.318516
435.620839	17673.004452	30.323533
435.592757	17684.664261	30.328551
436.570723	17707.134091	30.333568
436.634430	17738.899899	30.338586
437.184170	17766.212268	30.343604
437.643792	17778.225777	30.348621
438.484215	17815.941634	30.353639
438.800692	17839.165274	30.358656
439.180865	17868.361452	30.363674
439.562096	17891.796177	30.368692
439.964224	17909.889597	30.373709
440.486889	17941.198934	30.378727
441.098087	17966.973241	30.383744
441.240006	17997.767073	30.388762
441.775487	18031.967878	30.393780
442.222943	18049.466863	30.398797
441.950486	18070.236594	30.403815
442.671880	18103.334640	30.408832
443.200209	18142.843303	30.413850
443.238763	18165.099828	30.418868
443.939077	18199.629040	30.423885
444.295275	18231.767066	30.428903
445.275962	18259.392084	30.433920
445.560561	18296.437327	30.438938
446.258725	18317.915380	30.443956
446.542226	18346.438734	30.448973
446.791676	18386.244005	30.453991
447.309224	18412.602053	30.459008
447.785860	18432.017338	30.464026
448.159056	18461.266036	30.469044
448.931884	18488.032983	30.474061
449.144898	18513.661533	30.479079
449.737862	18543.368903	30.484096
450.551514	18563.761600	30.489114
451.062704	18576.911041	30.494132
451.745314	18601.879077	30.499149
452.066433	18617.793605	30.504167
452.627974	18634.245609	30.509184
452.964214	18644.579462	30.514202
453.291169	18653.329074	30.519220
453.778285	18671.327848	30.524237
454.097563	18697.578166	30.529255
455.060424	18708.206187	30.534272
454.740652	18721.933634	30.539290
455.342465	18738.695334	30.544308
455.655532	18758.932420	30.549325
455.893041	18792.839811	30.554343
456.498078	18805.090342	30.559360
456.955260	18843.518575	30.564378
457.174062	18868.097978	30.569396
458.017567	18882.882683	30.574413
458.229672	18914.425153	30.579431
458.967560	18930.957355	30.584448
459.475918	18955.605507	30.589466
459.491893	18980.570414	30.594484
460.187008	19001.171554	30.599501
460.655940	19032.844809	30.604519
461.405864	19054.056600	30.609536
461.919742	19077.971204	30.614554
462.106676	19104.539605	30.619572
463.146026	19123.097228	30.624589
463.066083	19145.834513	30.629607
463.592246	19162.557816	30.634624
464.054552	19192.703489	30.639642
464.600475	19220.732403	30.644660
465.240781	19245.057133	30.649677
465.318716	19277.126493	30.654695
465.770766	19285.762151	30.659712
466.775438	19307.237811	30.664730
467.257079	19343.117188	30.669748
467.865031	19358.614925	30.674765
468.030486	19392.345048	30.679783
468.551994	19405.967277	30.684800
468.909701	19427.891265	30.689818
469.276207	19454.520637	30.694836
469.972489	19473.289949	30.699853
470.343228	19501.321269	30.704871
470.644752	19528.396784	30.709888
470.853870	19550.931597	30.714906
471.329890	19574.056664	30.719924
472.195150	19604.001252	30.724941
472.630816	19634.284430	30.729959
472.922235	19662.492594	30.734976
473.218737	19684.609617	30.739994
473.735495	19719.340692	30.745012
474.339389	19743.210512	30.750029
474.297452	19778.066577	30.755047
474.831687	19810.874465	30.760064
475.631069	19847.368682	30.765082
475.874501	19884.278048	30.770100
476.565389	19917.314443	30.775117
476.831056	19936.991523	30.780135
477.554054	19967.148354	30.785152
478.114847	20008.620632	30.790170
478.140665	20031.917417	30.795188
478.607515	20067.629846	30.800205
479.195779	20104.991382	30.805223
479.915699	20130.170386	30.810240
480.718749	20154.009705	30.815258
481.059747	20186.879899	30.820276
481.506472	20211.387606	30.825293
482.001701	20234.320926	30.830311
482.305439	20264.511897	30.835328
482.640609	20289.315061	30.840346
483.155492	20314.766309	30.845364
483.593404	20338.466839	30.850381
484.037213	20367.530505	30.855399
484.597256	20389.739978	30.860416
485.047100	20420.464433	30.865434
485.664846	20449.943408	30.870452
486.183342	20475.691253	30.875469
486.705356	20508.773895	30.880487
487.312298	20531.993442	30.885504
487.566394	20552.968155	30.890522
487.778705	20593.390256	30.895540
488.390339	20613.879740	30.900557
488.741101	20645.694056	30.905575
489.435307	20689.130906	30.910592
489.723182	20716.759872	30.915610
490.292668	20750.783257	30.920628
490.603034	20781.258310	30.925645
491.041490	20819.345852	30.930663
491.615286	20861.272824	30.935680
492.470126	20885.003883	30.940698
492.731398	20922.525296	30.945716
493.597952	20956.079468	30.950733
493.818579	20980.743384	30.955751
494.043598	21021.284435	30.960768
494.714633	21042.257945	30.965786
494.728199	21090.066476	30.970804
495.563562	21126.829167	30.975821
496.487923	21154.176432	30.980839
496.782227	21185.911958	30.985856
497.670727	21225.800447	30.990874
497.930356	21259.544400	30.995892
498.788484	21288.980898	31.000909
499.708339	21314.218760	31.005927
500.407285	21337.962001	31.010944
500.874544	21352.592339	31.015962
501.294673	21373.548400	31.020980
502.065748	21394.386664	31.025997
502.370374	21422.866999	31.031015
502.962018	21443.537379	31.036032
503.299040	21458.706180	31.041050
503.768063	21485.050666	31.046068
504.129569	21505.087187	31.051085
504.489988	21535.663032	31.056103
504.742138	21561.864466	31.061120
505.219281	21591.708244	31.066138
505.527126	21617.193416	31.071156
506.476815	21648.031533	31.076173
506.837110	21686.158197	31.081191
507.108173	21709.715761	31.086208
507.552278	21744.303777	31.091226
507.990490	21785.748351	31.096244
508.853115	21813.358887	31.101261
509.097620	21844.566154	31.106279
509.626819	21883.570454	31.111296
510.067629	21912.320949	31.116314
510.505329	21945.791932	31.121332
511.403354	21976.196308	31.126349
511.562318	22012.907995	31.131367
511.608819	22048.044972	31.136384
512.402388	22077.814952	31.141402
513.115526	22123.672050	31.146420
513.673015	22155.879975	31.151437
513.803120	22187.895421	31.156455
514.554791	22232.628376	31.161472
515.194746	22258.422837	31.166490
515.487492	22298.267238	31.171508
516.248121	22331.960307	31.176525
516.893487	22367.535391	31.181543
517.075219	22388.535964	31.186560
517.960577	22411.088841	31.191578
518.350286	22443.626653	31.196596
519.481552	22450.559340	31.201613
520.049171	22465.547688	31.206631
520.686497	22486.553265	31.211648
521.399104	22517.018935	31.216666
521.440865	22542.338207	31.221684
522.095557	22551.360804	31.226701
522.852835	22575.077503	31.231719
523.205071	22607.507680	31.236736
523.651148	22621.068070	31.241754
523.628787	22651.294514	31.246772
524.211178	22678.589720	31.251789
525.114514	22700.217586	31.256807
525.201786	22728.897932	31.261824
526.115867	22754.997903	31.266842
526.335046	22778.988181	31.271860
526.837013	22813.992425	31.276877
527.136854	22848.263616	31.281895
527.643896	22895.216157	31.286912
528.279134	22916.159328	31.291930
528.775396	22958.936926	31.296948
529.625251	22980.099509	31.301965
530.426723	23016.093782	31.306983
530.572389	23058.414343	31.312000
530.798308	23070.006219	31.317018
531.204167	23119.635307	31.322036
532.038401	23165.412782	31.327053
532.729948	23191.535335	31.332071
532.844300	23226.126728	31.337088
533.366188	23257.577395	31.342106
534.195469	23290.326202	31.347124
534.546803	23320.527084	31.352141
535.466008	23358.563644	31.357159
535.991569	23405.419724	31.362176
536.374892	23430.857570	31.367194
537.193629	23455.545208	31.372212
537.886216	23494.426145	31.377229
538.331785	23520.871783	31.382247
538.387282	23560.130068	31.387264
539.319977	23590.316685	31.392282
539.661183	23625.347388	31.397300
540.048098	23664.636432	31.402317
540.724042	23693.706780	31.407335
541.344429	23735.430393	31.412352
542.305293	23766.156338	31.417370
542.929028	23796.688367	31.422388
543.559636	23828.925546	31.427405
544.463467	23853.391900	31.432423
544.255227	23881.456401	31.437440
544.984093	23904.894754	31.442458
545.527309	23934.302077	31.447476
545.714841	23973.148830	31.452493
546.560649	23995.475864	31.457511
547.307170	24031.676430	31.462528
549.409137	24019.519863	31.467546
549.671225	24031.972403	31.472564
550.045683	24046.233714	31.477581
550.518063	24060.087999	31.482599
550.739817	24081.987784	31.487616
551.273367	24106.088706	31.492634
551.410468	24130.175543	31.497652
551.640255	24153.818271	31.502669
552.109643	24188.040102	31.507687
552.139949	24220.624139	31.512704
552.930407	24243.010622	31.517722
553.371060	24273.135853	31.522740
553.847915	24310.238332	31.527757
554.438936	24328.826457	31.532775
554.691996	24361.281257	31.537792
555.203920	24391.755773	31.542810
556.001947	24420.694432	31.547828
556.420829	24457.477603	31.552845
557.076811	24488.612332	31.557863
557.587551	24524.901056	31.562880
557.901110	24562.516017	31.567898
558.776438	24597.781248	31.572916
558.758044	24635.087817	31.577933
559.600597	24665.542878	31.582951
560.290858	24712.673406	31.587968
560.637670	24744.722428	31.592986
561.247536	24784.446610	31.598004
561.876217	24832.888818	31.603021
562.469792	24866.157195	31.608039
562.888229	24907.718796	31.613056
563.571639	24946.262743	31.618074
564.048620	24988.744367	31.623092
564.574729	25037.670683	31.628109
565.459968	25054.892899	31.633127
565.830721	25110.308473	31.638144
566.615981	25148.994945	31.643162
567.127762	25193.980458	31.648180
568.046626	25230.655617	31.653197
568.188524	25266.200515	31.658215
568.339733	25306.723891	31.663232
569.573358	25342.958439	31.668250
569.913856	25383.806402	31.673268
570.429917	25421.966540	31.678285
571.218183	25457.682899	31.683303
571.626925	25512.240514	31.688320
572.274861	25541.122005	31.693338
572.859418	25592.492618	31.698356
573.225489	25631.984686	31.703373
574.052449	25660.282343	31.708391
575.257338	25700.421290	31.713408
576.632488	25711.165901	31.718426
577.264368	25734.861656	31.723444
577.802023	25768.923888	31.728461
578.289901	25789.254728	31.733479
578.606957	25816.513385	31.738496
579.089480	25834.683737	31.743514
579.632150	25866.021524	31.748532
579.939434	25895.234628	31.753549
580.294796	25930.854907	31.758567
580.707564	25967.528044	31.763584
581.467711	26004.210369	31.768602
581.792387	26044.562870	31.773620
582.274392	26092.538004	31.778637
582.621150	26127.780778	31.783655
583.181551	26174.315609	31.788672
583.892246	26210.361378	31.793690
585.090812	26246.533500	31.798708
585.424935	26289.033793	31.803725
586.148899	26315.724186	31.808743
586.882267	26346.786557	31.813760
587.640208	26386.642538	31.818778
587.968155	26412.750073	31.823796
588.282537	26455.689869	31.828813
589.398230	26476.561987	31.833831
589.595057	26527.167427	31.838848
589.929390	26555.960157	31.843866
591.040419	26593.473734	31.848884
591.100786	26642.773501	31.853901
591.576319	26674.559080	31.858919
592.119453	26714.910514	31.863936
592.574394	26745.827242	31.868954
593.406124	26782.777924	31.873972
593.644177	26819.176445	31.878989
594.325728	26861.661778	31.884007
595.041422	26901.955121	31.889024
595.053152	26929.224893	31.894042
595.806258	26975.813734	31.899060
596.722439	27028.432012	31.904077
597.274995	27060.269409	31.909095
597.464129	27103.963219	31.914112
598.220717	27147.467662	31.919130
599.401131	27180.212418	31.924148
600.041482	27222.736525	31.929165
600.911487	27261.742518	31.934183
601.736322	27290.668504	31.939200
602.251081	27318.302908	31.944218
603.232713	27352.096450	31.949236
603.291256	27393.466395	31.954253
603.822047	27414.367340	31.959271
604.463989	27451.165501	31.964288
604.674480	27486.495061	31.969306
605.420847	27528.611447	31.974324
606.084281	27559.775056	31.979341
606.775680	27605.401621	31.984359
607.147530	27651.924963	31.989376
607.698722	27683.978445	31.994394
608.288474	27727.756601	31.999412
609.028208	27775.442789	32.004429
609.883222	27817.043549	32.009447
610.319337	27858.659043	32.014464
611.085897	27896.058013	32.019482
611.946997	27935.376392	32.024500
612.604327	27986.520548	32.029517
613.220931	28020.403633	32.034535
613.651439	28058.228125	32.039552
614.613113	28077.975553	32.044570
615.575009	28104.157233	32.049588
616.024786	28146.801431	32.054605
617.136031	28173.889067	32.059623
617.818011	28204.526176	32.064640
618.158967	28238.629511	32.069658
619.099548	28258.974531	32.074676
619.327424	28288.323541	32.079693
619.602359	28328.283820	32.084711
620.428683	28364.694662	32.089728
620.545352	28396.273342	32.094746
620.976610	28421.040058	32.099764
621.350130	28471.578593	32.104781
622.360111	28511.968377	32.109799
622.645751	28547.269117	32.114816
623.257927	28599.945117	32.119834
624.289873	28640.635128	32.124852
624.389982	28692.032138	32.129869
624.979351	28733.676127	32.134887
625.834630	28773.603819	32.139904
626.973618	28824.295855	32.144922
627.722480	28862.887654	32.149940
627.989768	28905.719866	32.154957
628.482774	28938.372213	32.159975
629.134331	28984.008071	32.164992
629.165128	29035.821264	32.170010
630.128184	29078.716187	32.175028
630.627255	29120.710024	32.180045
631.189628	29167.023861	32.185063
631.664339	29222.118457	32.190080
632.309747	29264.620760	32.195098
633.291327	29319.434446	32.200116
633.713681	29358.204426	32.205133
634.261392	29399.521250	32.210151
634.906712	29441.360240	32.215168
635.367511	29482.659156	32.220186
636.519314	29520.285577	32.225204
636.902741	29572.108439	32.230221
637.226606	29601.829969	32.235239
637.897672	29653.153148	32.240256
638.188662	29709.567134	32.245274
638.980026	29753.387781	32.250292
639.672713	29801.402078	32.255309
640.606701	29854.031207	32.260327
641.532006	29893.988113	32.265344
642.026688	29946.110651	32.270362
642.652751	29982.732542	32.275380
643.967353	30027.104428	32.280397
644.506663	30066.394832	32.285415
645.912386	30089.956247	32.290432
646.293113	30127.899775	32.295450
646.938258	30157.723803	32.300468
647.551303	30198.520053	32.305485
647.682028	30236.363634	32.310503
648.568818	30270.138857	32.315520
649.084186	30321.709186	32.320538
649.850053	30347.500745	32.325556
650.266263	30390.907065	32.330573
650.868384	30426.098560	32.335591
651.592184	30468.211880	32.340608
652.026918	30517.077123	32.345626
652.925526	30553.872527	32.350644
653.499264	30597.766781	32.355661
654.289962	30641.330254	32.360679
655.289647	30693.218037	32.365696
655.741470	30734.109981	32.370714
656.397013	30764.236692	32.375732
656.922431	30815.496947	32.380749
657.635328	30857.138659	32.385767
658.102290	30894.811000	32.390784
658.741416	30958.216204	32.395802
659.350667	30994.229339	32.400820
660.001484	31037.695318	32.405837
660.839618	31084.324544	32.410855
661.542770	31127.023994	32.415872
662.032197	31179.460219	32.420890
662.516737	31224.071371	32.425908
663.315703	31276.503906	32.430925
664.378155	31312.428081	32.435943
665.553626	31338.270904	32.440960
665.964590	31395.246081	32.445978
666.597704	31427.798391	32.450996
667.116064	31473.485796	32.456013
667.835649	31516.423711	32.461031
668.561908	31544.732590	32.466048
669.298331	31594.362575	32.471066
670.174675	31628.622090	32.476084
670.525928	31668.513764	32.481101
670.755459	31704.555640	32.486119
671.597993	31752.355184	32.491136
672.168063	31798.977178	32.496154
672.963112	31848.592323	32.501172
674.096172	31894.962528	32.506189
674.611701	31934.759602	32.511207
675.156762	31971.739004	32.516224
675.846936	32017.318679	32.521242
676.803212	32051.490591	32.526260
677.358824	32094.000065	32.531277
677.857722	32137.024195	32.536295
678.802287	32178.752616	32.541312
679.239048	32215.964252	32.546330
679.718000	32249.085522	32.551348
680.044377	32282.521399	32.556365
680.344327	32331.456157	32.561383
681.588343	32371.109053	32.566400
681.948541	32413.333511	32.571418
682.584400	32452.524915	32.576436
683.035315	32503.522781	32.581453
683.530007	32551.125439	32.586471
684.458934	32591.124933	32.591488
684.953186	32646.054930	32.596506
686.123276	32688.065361	32.601524
687.196086	32734.010609	32.606541
687.410368	32792.436341	32.611559
688.265611	32828.275285	32.616576
688.819886	32876.103322	32.621594
689.279423	32927.492845	32.626612
690.422309	32976.734113	32.631629
690.959180	33029.325670	32.636647
691.524873	33074.516107	32.641664
692.491008	33115.320035	32.646682
693.214822	33162.015979	32.651700
694.112260	33201.541072	32.656717
694.778424	33244.610992	32.661735
696.123265	33275.595004	32.666752
697.385588	33305.460254	32.671770
698.232156	33344.140055	32.676788
699.081970	33377.192741	32.681805
699.076337	33413.021296	32.686823
700.323123	33434.493373	32.691840
700.344043	33473.896223	32.696858
700.885200	33510.246750	32.701876
701.744940	33559.109887	32.706893
701.785917	33604.775129	32.711911
702.484256	33640.658861	32.716928
703.267488	33691.835496	32.721946
703.934966	33733.629133	32.726964
705.134995	33779.974147	32.731981
705.404616	33817.511802	32.736999
706.413275	33869.595793	32.742016
706.636106	33919.987751	32.747034
707.430537	33958.246889	32.752052
708.400602	34005.949560	32.757069
709.094118	34059.259029	32.762087
709.823253	34104.887777	32.767104
710.677087	34145.034709	32.772122
710.880865	34203.055058	32.777140
711.966630	34242.691894	32.782157
712.386989	34298.263644	32.787175
713.197829	34348.413356	32.792192
713.757044	34393.809965	32.797210
714.179608	34452.707371	32.802228
715.066652	34510.211244	32.807245
715.561133	34568.282182	32.812263
716.090882	34615.940979	32.817280
716.886534	34679.750414	32.822298
717.538813	34733.143880	32.827316
718.221832	34788.619133	32.832333
718.919277	34846.596017	32.837351
720.015815	34903.429773	32.842368
720.566311	34967.164436	32.847386
721.193240	35028.769318	32.852404
722.270687	35078.721202	32.857421
722.695497	35143.904875	32.862439
723.824708	35185.680102	32.867456
724.308157	35230.647721	32.872474
725.192250	35300.590901	32.877492
726.010028	35334.827679	32.882509
726.847479	35388.990638	32.887527
727.464144	35432.515339	32.892544
727.686012	35477.587431	32.897562
728.327152	35529.713774	32.902580
729.114794	35585.168509	32.907597
729.657123	35634.800352	32.912615
730.562717	35679.829667	32.917632
731.296227	35734.053950	32.922650
731.988467	35782.353979	32.927668
732.738016	35825.125352	32.932685
733.665653	35891.807442	32.937703
734.677565	35942.840134	32.942720
735.306725	35989.772068	32.947738
735.821356	36031.701545	32.952756
737.262565	36083.546632	32.957773
738.056611	36143.016887	32.962791
738.978521	36171.813729	32.967808
739.846878	36208.516321	32.972826
740.743114	36255.609602	32.977844
741.598835	36299.990410	32.982861
741.756382	36341.027638	32.987879
742.749081	36378.602712	32.992896
743.553628	36423.560815	32.997914
744.007750	36477.463756	33.002932
744.800676	36516.037596	33.007949
745.242717	36576.069703	33.012967
746.211483	36623.753201	33.017984
746.930331	36668.339456	33.023002
747.086143	36730.035266	33.028020
747.878189	36779.845898	33.033037
748.659453	36834.476560	33.038055
749.383660	36895.850412	33.043072
749.989768	36954.195052	33.048090
750.706244	37006.989874	33.053108
751.734459	37061.247546	33.058125
752.577088	37125.898019	33.063143
753.343637	37179.931150	33.068160
754.402206	37228.487277	33.073178
754.444610	37298.391008	33.078196
755.630889	37350.108143	33.083213
756.681124	37413.209576	33.088231
757.388181	37466.424339	33.093248
758.073834	37522.507043	33.098266
758.938517	37578.328060	33.103284
759.793669	37622.294370	33.108301
760.385706	37680.927736	33.113319
761.419271	37732.751775	33.118336
762.382856	37785.377261	33.123354
763.370049	37834.179843	33.128372
763.999851	37878.301905	33.133389
764.591050	37923.606232	33.138407
765.377459	37968.513504	33.143424
766.398953	38015.325588	33.148442
766.942643	38061.162451	33.153460
767.527167	38106.518791	33.158477
768.300779	38165.017716	33.163495
769.357851	38218.881775	33.168512
770.135513	38261.995135	33.173530
770.235554	38327.030423	33.178548
771.332261	38377.676330	33.183565
772.022189	38436.049901	33.188583
773.076310	38482.111738	33.193600
773.899962	38518.755705	33.198618
774.313565	38587.265236	33.203636
774.771003	38630.821252	33.208653
775.658786	38692.143169	33.213671
776.749911	38741.987695	33.218688
777.550422	38791.011226	33.223706
778.256472	38849.402380	33.228724
778.952641	38884.606033	33.233741
779.584140	38933.169269	33.238759
780.106838	38976.393313	33.243776
780.925619	39028.854675	33.248794
781.331982	39082.234080	33.253812
782.382968	39131.232042	33.258829
783.223657	39182.855625	33.263847
783.786518	39249.731446	33.268864
784.642487	39299.158551	33.273882
785.133715	39362.820700	33.278900
786.093464	39421.641878	33.283917
786.858876	39489.821256	33.288935
787.680093	39536.610913	33.293952
788.819763	39588.309078	33.298970
789.402879	39645.640126	33.303988
790.510353	39702.896025	33.309005
791.335189	39752.360633	33.314023
792.260601	39817.626068	33.319040
792.925914	39853.639255	33.324058
793.698197	39920.162023	33.329076
794.653233	39967.444030	33.334093
795.357535	40029.462334	33.339111
796.258090	40084.765691	33.344128
797.451908	40131.378475	33.349146
797.753153	40199.594398	33.354164
798.589464	40251.088405	33.359181
799.423247	40305.928410	33.364199
799.948054	40369.101327	33.369216
800.947835	40419.754467	33.374234
801.394119	40488.328170	33.379252
802.140643	40549.297890	33.384269
803.209850	40606.334460	33.389287
803.630197	40679.535829	33.394304
804.916862	40740.320814	33.399322
805.370546	40799.698830	33.404340
806.527556	40855.166606	33.409357
807.639687	40920.494830	33.414375
808.561644	40975.215283	33.419392
809.529533	41030.453646	33.424410
810.272805	41086.821234	33.429428
810.917464	41150.091598	33.434445
811.318467	41211.319338	33.439463
812.339306	41271.103656	33.444480
813.154655	41321.686415	33.449498
813.992218	41386.280868	33.454516
815.787569	41424.903520	33.459533
816.893193	41478.863005	33.464551
817.381268	41518.068792	33.469568
818.284271	41565.248532	33.474586
819.167551	41610.635274	33.479604
819.790758	41656.720349	33.484621
820.765673	41717.354203	33.489639
821.641434	41766.201980	33.494656
822.537988	41809.563202	33.499674
822.885413	41858.550351	33.504692
823.837506	41905.995143	33.509709
824.798306	41954.943947	33.514727
825.005462	42001.322199	33.519744
825.730761	42060.674009	33.524762
826.642572	42133.715197	33.529780
827.286506	42189.095464	33.534797
828.032071	42247.464295	33.539815
828.751753	42303.895614	33.544832
829.585468	42355.268496	33.549850
831.317765	42388.804920	33.554868
832.183439	42440.735932	33.559885
833.096693	42486.891448	33.564903
833.565171	42545.607794	33.569920
834.546237	42576.035794	33.574938
835.157139	42627.064508	33.579956
835.827940	42672.170284	33.584973
836.409436	42719.282385	33.589991
837.180775	42772.582386	33.595008
838.296142	42822.774041	33.600026
838.660607	42872.975177	33.605044
839.456105	42926.531111	33.610061
840.265487	42975.100966	33.615079
840.906869	43044.702240	33.620096
841.845283	43108.514421	33.625114
842.235508	43165.220608	33.630132
843.108255	43231.465836	33.635149
843.683807	43293.949862	33.640167
844.763136	43376.760239	33.645184
845.725981	43436.009204	33.650202
846.228581	43506.474769	33.655220
847.185887	43566.933038	33.660237
847.776192	43645.057743	33.665255
848.983718	43722.909538	33.670272
849.982352	43788.833234	33.675290
850.932631	43869.401134	33.680308
851.922604	43920.867195	33.685325
853.090196	43985.386280	33.690343
853.848253	44055.503890	33.695360
854.998942	44110.019440	33.700378
855.449021	44185.878135	33.705396
856.502374	44245.570598	33.710413
857.530682	44300.358679	33.715431
858.458288	44376.497908	33.720448
859.569026	44436.624726	33.725466
860.377371	44491.308361	33.730484
861.487104	44548.741033	33.735501
862.332585	44605.234552	33.740519
863.025003	44674.339619	33.745536
863.425007	44739.941848	33.750554
864.680909	44796.017739	33.755572
865.414255	44864.509781	33.760589
866.706591	44922.092106	33.765607
867.108019	44988.302092	33.770624
867.640561	45054.441259	33.775642
868.793565	45127.701485	33.780660
869.590492	45196.273206	33.785677
870.786998	45253.896609	33.790695
870.807569	45328.877217	33.795712
872.161935	45393.984900	33.800730
872.962765	45465.953700	33.805748
873.553742	45541.611631	33.810765
874.889945	45602.256831	33.815783
875.674515	45671.957906	33.820800
876.890156	45745.539345	33.825818
877.690168	45804.143117	33.830836
878.447739	45869.414668	33.835853
879.453998	45933.724135	33.840871
879.993529	46001.857634	33.845888
881.179445	46075.204403	33.850906
882.189995	46144.283469	33.855924
882.777950	46207.994625	33.860941
883.912189	46263.093655	33.865959
884.533145	46342.045396	33.870976
885.204608	46406.806866	33.875994
886.044326	46473.750078	33.881012
886.965439	46549.834462	33.886029
887.978511	46624.247386	33.891047
888.868553	46705.328321	33.896064
889.823973	46761.822825	33.901082
890.475329	46823.425620	33.906100
891.443889	46875.578712	33.911117
892.760577	46938.969741	33.916135
893.095846	47004.367259	33.921152
893.732694	47072.229481	33.926170
894.980011	47131.260519	33.931188
895.866207	47203.765643	33.936205
896.616917	47270.870581	33.941223
897.377817	47330.066423	33.946240
898.444168	47390.018298	33.951258
899.144298	47455.145235	33.956276
900.082345	47532.735935	33.961293
900.950973	47600.449791	33.966311
901.529894	47665.583549	33.971328
902.866969	47742.499207	33.976346
904.008490	47809.924485	33.981364
905.154758	47865.721456	33.986381
906.475239	47923.863820	33.991399
907.344911	47991.698884	33.996416
908.394581	48048.156630	34.001434
909.349494	48113.600076	34.006452
909.542304	48175.973837	34.011469
910.704032	48237.026556	34.016487
911.487806	48314.637621	34.021504
912.536950	48376.062520	34.026522
913.995352	48434.867984	34.031540
915.181950	48492.229185	34.036557
916.642717	48535.597915	34.041575
917.172621	48602.570351	34.046592
918.267365	48651.525657	34.051610
918.814749	48708.480784	34.056628
919.626642	48771.190013	34.061645
920.830357	48820.609539	34.066663
921.540791	48894.096415	34.071680
922.086586	48949.091144	34.076698
923.402092	49015.695767	34.081716
924.028947	49081.395518	34.086733
925.263676	49138.485138	34.091751
925.726431	49205.248363	34.096768
926.849343	49259.869304	34.101786
927.906018	49329.615219	34.106804
928.733534	49395.120142	34.111821
929.424033	49459.956964	34.116839
930.360907	49535.897072	34.121856
931.039172	49599.850446	34.126874
932.100870	49663.465933	34.131892
932.961529	49727.638018	34.136909
933.749537	49800.407127	34.141927
934.851274	49877.695632	34.146944
935.930357	49946.136601	34.151962
936.984952	50020.573172	34.156980
937.507709	50093.359192	34.161997
938.668652	50156.321579	34.167015
939.620594	50221.992978	34.172032
940.263496	50303.428907	34.177050
941.602944	50371.843272	34.182068
942.161028	50451.818737	34.187085
943.337236	50517.411782	34.192103
944.229433	50598.575849	34.197120
945.065760	50674.117787	34.202138
946.246790	50744.291542	34.207156
947.051669	50823.843928	34.212173
948.068725	50878.035977	34.217191
949.000204	50961.941191	34.222208
949.896412	51042.448171	34.227226
950.887107	51102.098890	34.232244
952.042612	51175.239065	34.237261
953.304835	51235.316077	34.242279
954.262243	51303.533263	34.247296
954.832878	51361.921316	34.252314
955.933008	51406.984070	34.257332
956.458159	51480.248641	34.262349
957.430526	51535.347670	34.267367
958.599170	51598.198908	34.272384
959.125103	51663.466176	34.277402
960.267149	51729.656431	34.282420
960.711676	51805.965397	34.287437
961.978928	51871.149492	34.292455
962.697592	51944.398062	34.297472
963.371474	52021.222520	34.302490
964.566098	52100.984381	34.307508
965.201773	52175.550059	34.312525
966.429465	52264.013975	34.317543
967.561137	52328.252348	34.322560
968.289744	52422.938600	34.327578
969.473212	52489.814280	34.332596
970.195118	52570.397991	34.337613
971.382637	52640.804279	34.342631
972.589303	52721.952146	34.347648
973.376896	52808.354219	34.352666
975.092171	52881.520210	34.357684
975.851890	52964.352054	34.362701
976.958661	53034.215262	34.367719
977.921683	53105.632371	34.372736
979.000046	53169.122031	34.377754
980.865706	53234.026965	34.382772
981.343892	53308.911860	34.387789
982.385926	53380.165642	34.392807
983.619736	53447.586754	34.397824
984.537092	53509.349588	34.402842
985.581626	53569.188097	34.407860
986.435537	53645.622865	34.412877
987.012967	53707.818809	34.417895
988.485001	53777.475511	34.422912
989.133942	53841.584371	34.427930
990.603222	53910.760974	34.432948
991.363514	53984.401799	34.437965
992.286576	54055.897635	34.442983
993.264157	54121.145767	34.448000
994.191581	54198.988371	34.453018
995.066956	54269.555729	34.458036
995.901184	54349.748395	34.463053
996.803729	54420.179086	34.468071
997.908824	54506.107683	34.473088
998.993521	54583.389186	34.478106
1000.260177	54651.992010	34.483124
1000.955875	54730.612838	34.488141
1001.624881	54798.113089	34.493159
1003.283881	54865.206302	34.498176
1004.026091	54954.901362	34.503194
1005.021141	55019.737929	34.508212
1005.963891	55104.459964	34.513229
1007.056505	55180.622083	34.518247
1008.134165	55250.148358	34.523264
1008.869438	55333.542919	34.528282
1010.138737	55409.893437	34.533300
1010.993769	55493.769861	34.538317
1011.931080	55569.647315	34.543335
1013.243005	55648.093000	34.548352
1014.196061	55731.208251	34.553370
1015.192688	55806.760807	34.558388
1015.961325	55881.975712	34.563405
1017.339714	55965.177458	34.568423
1018.257200	56041.629074	34.573440
1018.665103	56115.774390	34.578458
1020.133986	56184.476750	34.583476
1021.034667	56267.038784	34.588493
1021.792319	56337.605319	34.593511
1022.526982	56415.877593	34.598528
1023.398965	56488.762047	34.603546
1024.358527	56561.550818	34.608564
1025.675575	56638.094041	34.613581
1026.535462	56721.005746	34.618599
1027.401629	56786.632975	34.623616
1028.504593	56874.602010	34.628634
1029.530534	56961.355574	34.633652
1031.136309	57039.462652	34.638669
1032.063300	57110.372183	34.643687
1032.825334	57185.168194	34.648704
1034.062497	57265.890243	34.653722
1034.849730	57348.802776	34.658740
1036.109316	57419.547531	34.663757
1036.893605	57504.492638	34.668775
1039.373971	57554.966093	34.673792
1040.973647	57616.614440	34.678810
1042.151227	57691.435954	34.683828
1042.940959	57751.780375	34.688845
1043.778048	57820.225036	34.693863
1044.880023	57883.692019	34.698880
1045.509268	57953.599773	34.703898
1046.589529	58014.488231	34.708916
1047.103576	58101.445854	34.713933
1047.857112	58167.980469	34.718951
1049.382635	58248.167266	34.723968
1050.035357	58332.237043	34.728986
1051.240144	58409.107198	34.734004
1051.991671	58488.295012	34.739021
1052.971877	58580.738824	34.744039
1054.153372	58661.645116	34.749056
1054.923899	58755.767836	34.754074
1056.196306	58841.141690	34.759092
1057.287321	58917.208366	34.764109
1058.505675	59000.591139	34.769127
1059.733861	59085.833495	34.774144
1060.684867	59179.543681	34.779162
1061.791203	59266.748756	34.784180
1062.804624	59350.082350	34.789197
1064.010666	59442.671524	34.794215
1065.103467	59523.429937	34.799232
1065.807666	59604.033905	34.804250
1066.900144	59701.376192	34.809268
1068.116275	59782.875809	34.814285
1068.876947	59878.327289	34.819303
1070.260486	59961.890199	34.824320
1071.388287	60053.170998	34.829338
1072.441143	60142.058550	34.834356
1073.450649	60235.485197	34.839373
1074.599355	60325.004120	34.844391
1075.678912	60408.710824	34.849408
1076.411948	60501.846051	34.854426
1077.812012	60594.630945	34.859444
1079.190920	60677.690650	34.864461
1079.655773	60772.014336	34.869479
1081.097873	60843.158457	34.874496
1081.893388	60939.159351	34.879514
1083.426256	61028.000728	34.884532
1084.728807	61115.852839	34.889549
1085.598648	61211.235561	34.894567
1087.104189	61284.232078	34.899584
1088.040466	61365.084247	34.904602
1089.182316	61441.815534	34.909620
1090.257418	61538.041108	34.914637
1090.804758	61616.315044	34.919655
1091.982359	61700.314739	34.924672
1093.278118	61785.518027	34.929690
1094.117737	61857.524807	34.934708
1095.230363	61933.831734	34.939725
1096.689783	62011.015441	34.944743
1097.948256	62070.170852	34.949760
1098.683912	62142.321249	34.954778
1099.570905	62222.892720	34.959796
1100.884827	62299.840443	34.964813
1101.457996	62383.746647	34.969831
1102.783033	62465.599056	34.974848
1103.977291	62547.845577	34.979866
1105.293687	62630.231616	34.984884
1106.265740	62712.861438	34.989901
1107.395958	62788.547901	34.994919
1108.450852	62862.144656	34.999936
1109.339248	62955.492873	35.004954
1110.711693	63038.162740	35.009972
1111.567983	63114.418258	35.014989
1112.259134	63210.710110	35.020007
1113.417625	63288.875218	35.025024
1114.923920	63383.173381	35.030042
1115.922708	63488.167102	35.035060
1117.188347	63575.843798	35.040077
1118.167497	63671.079724	35.045095
1119.258699	63764.696944	35.050112
1120.310147	63860.808616	35.055130
1121.210612	63955.950257	35.060148
1122.673413	64046.991119	35.065165
1123.396131	64146.934440	35.070183
1124.822982	64243.641207	35.075200
1126.802577	64314.154562	35.080218
1128.148396	64395.244079	35.085236
1130.009556	64475.044474	35.090253
1130.999949	64567.724456	35.095271
1132.175754	64645.916445	35.100288
1133.068708	64722.196492	35.105306
1134.177185	64790.042247	35.110324
1135.542989	64876.454418	35.115341
1136.598526	64965.859026	35.120359
1137.680087	65040.236752	35.125376
1138.551308	65125.606202	35.130394
1139.559250	65212.543719	35.135412
1140.824223	65296.700234	35.140429
1141.528069	65393.644266	35.145447
1142.771736	65467.504208	35.150464
1143.581513	65561.760727	35.155482
1144.883418	65656.890648	35.160500
1146.152385	65741.738110	35.165517
1146.658137	65844.127748	35.170535
1148.536542	65940.150317	35.175552
1149.673579	66021.207937	35.180570
1150.829760	66107.891214	35.185588
1152.204326	66195.952643	35.190605
1153.095105	66282.798122	35.195623
1154.638405	66370.422367	35.200640
1155.383950	66462.406678	35.205658
1156.755382	66557.662122	35.210676
1158.395185	66630.957305	35.215693
1159.287220	66720.944396	35.220711
1160.331566	66804.158924	35.225728
1161.466933	66896.014483	35.230746
1162.091701	66989.007187	35.235764
1163.342283	67075.989315	35.240781
1164.810428	67180.228924	35.245799
1165.934622	67261.773693	35.250816
1167.395811	67360.164889	35.255834
1168.347719	67441.971315	35.260852
1169.149338	67524.789108	35.265869
1170.648641	67628.785105	35.270887
1171.573253	67707.107966	35.275904
1172.868533	67784.018420	35.280922
1173.748183	67866.198350	35.285940
1175.111594	67942.465519	35.290957
1175.819657	68024.349754	35.295975
1176.995599	68103.248874	35.300992
1178.103273	68187.414131	35.306010
1179.026985	68280.092739	35.311028
1180.475446	68366.263333	35.316045
1181.635029	68452.973054	35.321063
1183.504262	68537.457809	35.326080
1184.433977	68621.626864	35.331098
1185.489957	68713.703927	35.336116
1187.034540	68793.687509	35.341133
1187.726433	68901.113212	35.346151
1189.336474	68981.511423	35.351168
1190.722916	69067.896641	35.356186
1191.465478	69170.440043	35.361204
1192.391713	69262.077033	35.366221
1193.798166	69364.017644	35.371239
1194.725637	69459.663259	35.376256
1196.083538	69558.439883	35.381274
1196.989880	69655.900460	35.386292
1198.310585	69755.918369	35.391309
1199.369549	69861.125369	35.396327
1200.414420	69971.710930	35.401344
1201.678490	70065.368770	35.406362
1202.501093	70175.812498	35.411380
1204.297877	70286.352014	35.416397
1205.697661	70393.198808	35.421415
1206.949770	70483.725584	35.426432
1208.228488	70584.766375	35.431450
1209.465527	70692.551571	35.436468
1210.690817	70795.437852	35.441485
1211.768828	70892.825687	35.446503
1213.211005	71002.391274	35.451520
1214.582975	71094.389614	35.456538
1215.959265	71203.599024	35.461556
1217.353706	71301.496380	35.466573
1218.319939	71399.929354	35.471591
1219.573753	71499.698410	35.476608
1220.815139	71603.243940	35.481626
1222.877009	71684.675713	35.486644
1223.887684	71767.474541	35.491661
1225.372200	71857.127677	35.496679
1226.720712	71950.145882	35.501696
1228.151736	72037.034295	35.506714
1229.318748	72136.591312	35.511732
1230.452834	72216.763312	35.516749
1231.789832	72304.465155	35.521767
1232.852902	72387.625075	35.526784
1234.101599	72482.319860	35.531802
1234.815949	72580.492493	35.536820
1236.280145	72660.145838	35.541837
1237.246600	72754.454905	35.546855
1238.025496	72864.359483	35.551872
1239.829381	72951.458852	35.556890
1241.312245	73038.633808	35.561908
1243.402941	73121.408104	35.566925
1244.336855	73217.142444	35.571943
1245.424781	73287.331614	35.576960
1246.795033	73375.475142	35.581978
1247.646669	73461.837805	35.586996
1248.781609	73549.562567	35.592013
1250.064263	73633.819491	35.597031
1251.078606	73722.057566	35.602048
1252.748503	73815.994932	35.607066
1253.432842	73908.882759	35.612084
1254.653646	73993.315109	35.617101
1256.022697	74076.673362	35.622119
1256.959047	74161.201184	35.627136
1258.012173	74233.095539	35.632154
1258.834207	74327.521337	35.637172
1260.576280	74414.609799	35.642189
1261.559392	74514.179038	35.647207
1262.518860	74604.632521	35.652224
1263.811293	74706.548279	35.657242
1264.750797	74799.918811	35.662260
1266.282331	74898.656795	35.667277
1267.350681	74999.633224	35.672295
1268.416086	75104.359815	35.677312
1269.880520	75209.886038	35.682330
1271.332316	75327.790044	35.687348
1272.565703	75436.380471	35.692365
1273.644500	75535.913276	35.697383
1274.780901	75645.140316	35.702400
1276.169948	75754.252473	35.707418
1277.274512	75863.016675	35.712436
1278.902348	75980.376791	35.717453
1280.079355	76087.699246	35.722471
1281.646656	76192.668625	35.727488
1283.024972	76304.394107	35.732506
1284.215394	76423.698978	35.737524
1285.332437	76533.439313	35.742541
1286.964027	76640.845214	35.747559
1287.959382	76757.116415	35.752576
1289.568084	76859.523119	35.757594
1290.624337	76965.575767	35.762612
1292.216977	77067.415718	35.767629
1293.804386	77177.161447	35.772647
1294.852865	77299.671828	35.777664
1297.011972	77400.968821	35.782682
1298.474315	77513.699617	35.787700
1299.610209	77613.041148	35.792717
1300.741701	77717.324187	35.797735
1301.877488	77834.566222	35.802752
1303.291040	77922.198519	35.807770
1304.430047	78041.645162	35.812788
1305.782761	78147.618257	35.817805
1307.247088	78252.636950	35.822823
1308.338082	78359.614377	35.827840
1309.967425	78470.182204	35.832858
1310.869270	78583.334022	35.837876
1312.594158	78685.488794	35.842893
1314.136583	78794.652607	35.847911
1315.131546	78904.244113	35.852928
1316.388346	79012.237081	35.857946
1318.216335	79127.539969	35.862964
1319.302183	79223.398613	35.867981
1320.794651	79324.464433	35.872999
1321.834698	79433.126215	35.878016
1323.257371	79538.561695	35.883034
1324.598387	79639.335523	35.888052
1325.942206	79734.091610	35.893069
1327.688906	79839.414458	35.898087
1328.991002	79948.734262	35.903104
1330.337049	80039.525689	35.908122
1331.491173	80151.466452	35.913140
1332.988010	80250.444592	35.918157
1334.567241	80348.358729	35.923175
1335.564615	80460.236449	35.928192
1336.939059	80546.020813	35.933210
1338.354252	80639.932720	35.938228
1339.328824	80747.051525	35.943245
1340.825961	80840.381236	35.948263
1342.150118	80939.794123	35.953280
1343.389977	81029.895827	35.958298
1344.633913	81127.370785	35.963316
1345.618874	81212.482995	35.968333
1346.801004	81303.924861	35.973351
1348.429614	81398.946356	35.978368
1349.652824	81485.377954	35.983386
1350.892023	81595.854267	35.988404
1352.138452	81697.486458	35.993421
1353.413110	81798.683852	35.998439
1354.234991	81898.127640	36.003456
1355.989743	81999.922531	36.008474
1357.296374	82104.004764	36.013492
1358.676231	82212.447100	36.018509
1360.087019	82319.795423	36.023527
1361.788787	82428.137804	36.028544
1362.633750	82529.746798	36.033562
1364.018607	82648.085336	36.038580
1365.086797	82757.807277	36.043597
1366.747072	82871.238545	36.048615
1368.035832	82996.131319	36.053632
1369.536891	83107.915843	36.058650
1371.188991	83218.384923	36.063668
1372.328561	83337.524742	36.068685
1373.531582	83451.713705	36.073703
1375.038818	83577.943441	36.078720
1376.429042	83699.085712	36.083738
1377.625517	83817.369754	36.088756
1379.133507	83935.694494	36.093773
1380.565294	84066.841689	36.098791
1382.127362	84189.086989	36.103808
1383.533973	84301.689161	36.108826
1385.442088	84417.013983	36.113844
1386.625759	84531.286304	36.118861
1387.881988	84654.721580	36.123879
1389.793980	84772.289995	36.128896
1390.990327	84883.672750	36.133914
1392.510423	85000.834269	36.138932
1394.067198	85110.590581	36.143949
1395.519785	85224.063531	36.148967
1396.847621	85343.587879	36.153984
1398.153620	85453.802686	36.159002
1399.581978	85573.565768	36.164020
1400.786138	85701.765412	36.169037
1402.278758	85810.685389	36.174055
1403.792408	85932.299393	36.179072
1405.145329	86046.589396	36.184090
1406.740969	86169.750243	36.189108
1407.704002	86295.481059	36.194125
1409.319511	86399.201394	36.199143
1410.622206	86534.295490	36.204160
1412.104412	86645.665885	36.209178
1413.605272	86768.882040	36.214196
1414.719225	86890.207455	36.219213
1416.367219	87006.216709	36.224231
1417.515942	87139.487463	36.229248
1418.740195	87252.725106	36.234266
1420.491728	87364.715279	36.239284
1422.258040	87488.121253	36.244301
1423.962617	87603.148310	36.249319
1425.215764	87719.880812	36.254336
1426.964844	87832.151947	36.259354
1428.268224	87941.983745	36.264372
1429.518186	88066.435627	36.269389
1431.094265	88177.835265	36.274407
1432.305324	88291.345097	36.279424
1433.713057	88409.336207	36.284442
1435.207065	88528.923790	36.289460
1436.420439	88649.924193	36.294477
1438.011860	88744.114029	36.299495
1439.300601	88857.081691	36.304512
1440.629627	88961.907537	36.309530
1441.850446	89049.984351	36.314548
1443.385040	89164.815855	36.319565
1444.720459	89275.446026	36.324583
1446.084578	89386.883217	36.329600
1447.598278	89487.968981	36.334618
1449.274205	89597.812316	36.339636
1450.795607	89699.493238	36.344653
1452.159686	89811.527667	36.349671
1453.643094	89928.461173	36.354688
1454.805855	90048.765456	36.359706
1456.414596	90163.361158	36.364724
1457.733769	90288.990227	36.369741
1459.182434	90398.339602	36.374759
1460.765905	90528.630398	36.379776
1461.980141	90647.370234	36.384794
1463.361336	90775.767205	36.389812
1464.888530	90895.397161	36.394829
1466.866778	91004.400175	36.399847
1468.916832	91113.810642	36.404864
1470.614052	91219.803801	36.409882
1472.200420	91329.832201	36.414900
1473.555728	91445.917073	36.419917
1475.327985	91553.230488	36.424935
1476.550271	91657.347319	36.429952
1478.078049	91773.862874	36.434970
1479.682788	91886.070381	36.439988
1480.831476	92003.799168	36.445005
1482.083611	92118.128303	36.450023
1483.698605	92238.345610	36.455040
1484.819584	92357.220765	36.460058
1486.716222	92471.197430	36.465076
1487.296863	92604.631753	36.470093
1489.459173	92718.453927	36.475111
1490.637632	92849.185338	36.480128
1491.976832	92977.915062	36.485146
1493.970719	93103.615596	36.490164
1495.155218	93240.862492	36.495181
1496.681203	93368.157902	36.500199
1497.697179	93498.004801	36.505216
1498.866135	93636.637439	36.510234
1500.711152	93769.626556	36.515252
1502.022754	93915.323509	36.520269
1503.661593	94052.427272	36.525287
1504.867070	94187.507715	36.530304
1506.608128	94330.630132	36.535322
1508.111877	94468.517280	36.540340
1509.568723	94617.883423	36.545357
1511.579682	94748.176468	36.550375
1513.281488	94885.413564	36.555392
1514.488109	95022.208649	36.560410
1516.279593	95154.337472	36.565428
1517.382718	95300.250863	36.570445
1519.062302	95429.001237	36.575463
1520.877641	95567.402506	36.580480
1522.620943	95695.117340	36.585498
1524.580002	95825.562424	36.590516
1525.575420	95961.038211	36.595533
1527.075108	96089.667208	36.600551
1529.056422	96223.127336	36.605568
1530.479915	96354.139670	36.610586
1532.087019	96476.719798	36.615604
1533.369879	96616.945208	36.620621
1534.978878	96738.372544	36.625639
1537.102292	96863.345659	36.630656
1538.161762	96987.711621	36.635674
1539.981276	97087.938317	36.640692
1541.441444	97198.374956	36.645709
1542.807871	97307.001182	36.650727
1544.542064	97418.828367	36.655744
1545.892002	97523.819791	36.660762
1547.489470	97642.210072	36.665780
1548.241079	97757.106972	36.670797
1549.835855	97867.119351	36.675815
1551.309749	97992.083948	36.680832
1552.463249	98119.596202	36.685850
1553.751440	98244.692109	36.690868
1555.751789	98379.438758	36.695885
1557.431127	98500.722477	36.700903
1559.205877	98633.477029	36.705920
1560.437920	98775.215786	36.710938
1562.337554	98904.516589	36.715956
1563.615127	99045.805768	36.720973
1565.055873	99166.546012	36.725991
1566.943927	99302.277495	36.731008
1568.364931	99436.244058	36.736026
1570.125753	99564.276062	36.741044
1571.676284	99708.796400	36.746061
1572.858103	99846.338860	36.751079
1574.653603	99983.165200	36.756096
1575.954456	100132.404254	36.761114
1578.044547	100266.257457	36.766132
1579.811138	100407.945579	36.771149
1581.393214	100549.916592	36.776167
1582.981495	100691.151958	36.781184
1584.684965	100825.029617	36.786202
1586.387674	100955.282108	36.791220
1588.507566	101096.182942	36.796237
1590.175115	101229.535393	36.801255
1592.166536	101350.971453	36.806272
1593.427162	101490.752622	36.811290
1595.291724	101609.749866	36.816308
1596.604370	101745.175470	36.821325
1598.475076	101875.671736	36.826343
1599.902869	101996.094927	36.831360
1601.301520	102129.962002	36.836378
1603.219883	102262.721794	36.841396
1604.978068	102393.643342	36.846413
1606.842266	102520.060770	36.851431
1608.396655	102638.907178	36.856448
1609.325925	102771.683510	36.861466
1611.345572	102906.078337	36.866484
1612.820644	103050.764718	36.871501
1614.103147	103175.107161	36.876519
1616.289816	103302.124009	36.881536
1617.389084	103441.393407	36.886554
1619.093431	103583.612119	36.891572
1620.233495	103714.660471	36.896589
1622.097671	103853.926657	36.901607
1623.674765	103996.204979	36.906624
1625.087191	104137.812194	36.911642
1627.122117	104282.099832	36.916660
1628.628709	104426.546401	36.921677
1630.169294	104566.018077	36.926695
1631.678531	104696.163325	36.931712
1633.145123	104848.631194	36.936730
1634.771278	104992.199405	36.941748
1636.385617	105147.346328	36.946765
1638.108504	105288.200044	36.951783
1639.866177	105424.661839	36.956800
1641.671447	105570.372830	36.961818
1643.506596	105704.680862	36.966836
1645.146388	105857.392615	36.971853
1646.457592	105981.284560	36.976871
1648.308874	106103.698131	36.981888
1649.212896	106224.370291	36.986906
1650.791107	106363.564601	36.991924
1652.752905	106495.003097	36.996941
1654.135320	106629.752978	37.001959
1655.869690	106755.724795	37.006976
1657.578783	106888.700380	37.011994
1659.472876	107010.704796	37.017012
1661.201656	107147.951510	37.022029
1662.616437	107280.226301	37.027047
1664.539572	107399.044864	37.032064
1666.131826	107546.217666	37.037082
1667.603749	107689.846660	37.042100
1669.291054	107817.845887	37.047117
1670.735629	107959.692335	37.052135
1672.651048	108091.080786	37.057152
1674.631820	108247.148525	37.062170
1676.116084	108382.193779	37.067188
1678.177019	108518.253020	37.072205
1679.351456	108673.611265	37.077223
1681.322008	108804.943129	37.082240
1683.167158	108949.343524	37.087258
1684.885445	109085.990919	37.092276
1686.719612	109234.731052	37.097293
1688.264694	109372.611214	37.102311
1690.272648	109515.631764	37.107328
1691.513024	109667.433512	37.112346
1693.217006	109816.006172	37.117364
1695.129897	109964.978107	37.122381
1696.574651	110110.739108	37.127399
1698.680288	110251.908693	37.132416
1699.992595	110407.988716	37.137434
1701.571170	110564.116759	37.142452
1703.544926	110705.892037	37.147469
1704.932472	110857.435078	37.152487
1706.813226	111009.193682	37.157504
1708.758537	111156.605793	37.162522
1710.972503	111296.317004	37.167540
1713.093617	111439.213637	37.172557
1714.776532	111584.981708	37.177575
1716.416451	111732.177429	37.182592
1718.069274	111874.311700	37.187610
1719.851868	112023.236511	37.192628
1721.369314	112166.420250	37.197645
1723.159041	112313.658466	37.202663
1724.809676	112450.354803	37.207680
1726.311551	112606.630588	37.212698
1727.794796	112757.025440	37.217716
1729.635439	112911.322140	37.222733
1731.064904	113064.871836	37.227751
1732.999739	113213.435479	37.232768
1734.540790	113386.449197	37.237786
1736.332485	113548.124697	37.242804
1737.863944	113696.778476	37.247821
1739.749556	113856.728605	37.252839
1741.754236	114013.832692	37.257856
1743.559467	114173.175281	37.262874
1745.127904	114329.574989	37.267892
1747.070727	114485.321012	37.272909
1748.520577	114649.299467	37.277927
1750.386942	114803.486080	37.282944
1752.237436	114960.960688	37.287962
1754.266990	115115.199314	37.292980
1756.081708	115267.024205	37.297997
1757.373021	115420.123394	37.303015
1759.714916	115569.711365	37.308032
1761.315185	115719.263172	37.313050
1762.931093	115857.854850	37.318068
1764.602207	116006.940201	37.323085
1766.100500	116140.782337	37.328103
1767.814978	116282.201327	37.333120
1769.205595	116433.716526	37.338138
1770.465129	116580.610597	37.343156
1772.282438	116725.401757	37.348173
1773.694261	116885.946163	37.353191
1775.314323	117039.317970	37.358208
1777.538485	117211.089187	37.363226
1778.781287	117371.700038	37.368244
1780.745416	117532.567142	37.373261
1782.047264	117701.199054	37.378279
1784.235109	117869.769932	37.383296
1785.798761	118040.290571	37.388314
1787.291853	118212.497255	37.393332
1789.179365	118404.582708	37.398349
1790.674781	118587.305843	37.403367
1792.984457	118761.975502	37.408384
1794.920696	118940.915262	37.413402
1796.648501	119128.298011	37.418420
1798.344328	119304.105817	37.423437
1800.341178	119484.992096	37.428455
1802.274328	119666.371158	37.433472
1803.849307	119858.576019	37.438490
1805.494252	120043.870517	37.443508
1807.722406	120226.056183	37.448525
1809.168293	120425.222496	37.453543
1811.145925	120610.658216	37.458560
1813.353007	120803.162646	37.463578
1814.695682	120998.111227	37.468596
1817.020973	121187.465991	37.473613
1818.599240	121380.248745	37.478631
1820.607262	121568.576515	37.483648
1822.303442	121773.901143	37.488666
1824.189847	121962.414650	37.493684
1826.716856	122145.425420	37.498701
1828.868135	122330.702778	37.503719
1830.806765	122507.743206	37.508736
1832.791548	122690.980453	37.513754
1834.878533	122875.420457	37.518772
1836.641411	123050.384878	37.523789
1838.326609	123237.794112	37.528807
1840.267025	123410.157302	37.533824
1842.215845	123583.889997	37.538842
1844.085065	123767.429303	37.543860
1845.993648	123943.973404	37.548877
1847.352619	124130.549608	37.553895
1849.631867	124308.255481	37.558912
1851.445357	124493.697015	37.563930
1852.912946	124678.635052	37.568948
1854.958318	124856.468559	37.573965
1856.890146	125041.589737	37.578983
1859.153009	125212.553087	37.584000
1861.126680	125384.906922	37.589018
1862.921144	125563.264678	37.594036
1864.747108	125743.013825	37.599053
1866.787333	125925.343844	37.604071
1868.897422	126086.337689	37.609088
1870.923389	126258.395305	37.614106
1872.975985	126435.118197	37.619124
1874.422453	126590.495627	37.624141
1876.111958	126768.659323	37.629159
1877.837052	126936.148631	37.634176
1879.959505	127113.256866	37.639194
1881.561444	127290.408815	37.644212
1883.657252	127472.077350	37.649229
1885.257358	127646.909395	37.654247
1886.631055	127813.670360	37.659264
1888.621973	127982.327816	37.664282
1889.935975	128150.596509	37.669300
1891.675294	128317.962329	37.674317
1893.097482	128488.917935	37.679335
1894.938988	128661.052340	37.684352
1896.854431	128841.727258	37.689370
1898.537641	129027.691708	37.694388
1900.519624	129210.578166	37.699405
1902.311151	129391.223985	37.704423
1904.060819	129581.748068	37.709440
1906.176586	129769.348615	37.714458
1907.524808	129975.695061	37.719476
1909.786388	130156.017236	37.724493
1911.488337	130356.575595	37.729511
1913.869869	130549.822393	37.734528
1916.089813	130746.597097	37.739546
1918.191265	130949.265710	37.744564
1919.977946	131139.067790	37.749581
1921.700240	131339.297702	37.754599
1924.285861	131516.923365	37.759616
1926.357657	131713.839755	37.764634
1928.457536	131903.456890	37.769652
1930.405875	132097.640878	37.774669
1932.016694	132296.331905	37.779687
1933.797631	132488.805381	37.784704
1935.702029	132688.886309	37.789722
1937.711387	132890.372942	37.794740
1939.856972	133083.883510	37.799757
1941.680068	133300.640105	37.804775
1943.484442	133501.730034	37.809792
1945.449384	133697.149358	37.814810
1947.192571	133902.717109	37.819828
1949.112077	134110.872300	37.824845
1951.286293	134325.155688	37.829863
1953.086288	134543.393899	37.834880
1955.489913	134731.935475	37.839898
1958.039940	134934.971496	37.844916
1960.574337	135126.121047	37.849933
1962.102035	135326.919687	37.854951
1964.504157	135535.539363	37.859968
1966.651449	135719.315722	37.864986
1968.174579	135911.197022	37.870004
1970.546744	136111.169808	37.875021
1972.066668	136301.746242	37.880039
1973.814089	136498.899365	37.885056
1975.671432	136696.645340	37.890074
1977.670361	136906.856842	37.895092
1980.036211	137111.479452	37.900109
1981.595261	137318.601544	37.905127
1982.999824	137537.385266	37.910144
1985.375713	137736.755473	37.915162
1986.853143	137968.042211	37.920180
1988.709257	138176.276713	37.925197
1990.819543	138394.840446	37.930215
1992.578476	138612.533503	37.935232
1995.064785	138828.147379	37.940250
1996.597789	139054.760849	37.945268
1998.426711	139274.349643	37.950285
2000.667554	139487.885462	37.955303
2002.442607	139720.632029	37.960320
2004.620389	139938.062997	37.965338
2006.625487	140170.255660	37.970356
2008.947379	140384.836238	37.975373
2010.624299	140611.282485	37.980391
2012.530717	140846.019259	37.985408
2014.674022	141063.904914	37.990426
2016.578381	141290.737776	37.995444
2018.792711	141511.469865	38.000461
2020.912089	141718.562181	38.005479
2022.557785	141925.107240	38.010496
2024.518852	142116.057442	38.015514
2026.208532	142334.552457	38.020532
2028.256717	142536.785923	38.025549
2030.176513	142752.467611	38.030567
2031.848451	142975.854409	38.035584
2033.926996	143191.411791	38.040602
2035.919727	143415.232933	38.045620
2037.819002	143640.986057	38.050637
2039.559291	143860.089174	38.055655
2041.795544	144097.595116	38.060672
2043.605994	144327.324981	38.065690
2045.632492	144573.737344	38.070708
2047.592871	144810.629641	38.075725
2049.683341	145043.746007	38.080743
2051.284297	145294.010316	38.085760
2053.738300	145548.077628	38.090778
2055.815303	145799.615702	38.095796
2057.848147	146034.027498	38.100813
2060.107641	146287.303787	38.105831
2062.216278	146553.969767	38.110848
2064.732150	146791.368696	38.115866
2066.776809	147049.467190	38.120884
2069.103655	147295.363684	38.125901
2071.378583	147540.520567	38.130919
2073.551873	147788.816798	38.135936
2076.033087	148027.077186	38.140954
2077.860316	148280.113191	38.145972
2080.063566	148535.224277	38.150989
2082.603947	148768.604808	38.156007
2084.812387	149008.257536	38.161024
2087.149465	149243.639198	38.166042
2089.463443	149494.142838	38.171060
2091.336888	149718.568556	38.176077
2093.798136	149958.732019	38.181095
2095.883682	150187.569275	38.186112
2097.797653	150422.311159	38.191130
2100.137528	150655.007631	38.196148
2102.378353	150883.480954	38.201165
2104.880384	151116.738064	38.206183
2106.599282	151347.414356	38.211200
2108.671353	151582.288969	38.216218
2110.915674	151807.427233	38.221236
2112.902301	152039.867252	38.226253
2115.026029	152270.598659	38.231271
2116.895663	152523.038696	38.236288
2119.097686	152748.200071	38.241306
2121.349731	152977.162709	38.246324
2123.423437	153203.031355	38.251341
2125.949634	153445.586432	38.256359
2127.865026	153676.787672	38.261376
2130.034511	153909.752864	38.266394
2132.286834	154152.252051	38.271412
2134.072972	154382.587706	38.276429
2135.923979	154621.622389	38.281447
2138.244618	154865.599197	38.286464
2140.360194	155105.838760	38.291482
2142.422803	155349.553117	38.296500
2144.342309	155589.292046	38.301517
2146.178213	155837.537550	38.306535
2147.677818	156101.399887	38.311552
2150.062611	156352.304168	38.316570
2152.506432	156606.323206	38.321588
2154.186944	156853.213492	38.326605
2156.316927	157109.111570	38.331623
2158.217791	157372.574402	38.336640
2160.737969	157618.994441	38.341658
2162.780259	157864.423504	38.346676
2164.423191	158099.709012	38.351693
2166.727953	158322.921092	38.356711
2169.092817	158568.302826	38.361728
2171.663959	158802.189811	38.366746
2173.484919	159043.646478	38.371764
2175.179018	159291.852279	38.376781
2177.487809	159534.517176	38.381799
2179.315608	159783.173880	38.386816
2181.566051	160029.721866	38.391834
2183.900512	160283.925759	38.396852
2185.534999	160550.744617	38.401869
2188.049100	160792.290686	38.406887
2191.518134	161026.719234	38.411904
2194.273935	161273.891745	38.416922
2196.911177	161509.492580	38.421940
2198.810328	161749.068642	38.426957
2201.158070	161981.885154	38.431975
2203.322006	162220.241080	38.436992
2206.216356	162446.347033	38.442010
2208.706017	162677.163444	38.447028
2210.670711	162918.282575	38.452045
2213.520980	163144.067744	38.457063
2215.180835	163375.802937	38.462080
2217.179173	163611.206212	38.467098
2219.141662	163853.446400	38.472116
2221.247366	164093.138665	38.477133
2223.574334	164329.966120	38.482151
2225.200668	164583.484715	38.487168
2227.004732	164843.743725	38.492186
2229.477867	165095.164559	38.497204
2231.325492	165360.548109	38.502221
2233.260961	165622.935376	38.507239
2235.376079	165901.661442	38.512256
2238.240729	166163.880802	38.517274
2240.710128	166424.791454	38.522292
2242.771417	166700.126478	38.527309
2244.804930	166960.091269	38.532327
2246.761617	167233.108512	38.537344
2248.960277	167513.821495	38.542362
2251.212181	167794.121022	38.547380
2253.233008	168079.637950	38.552397
2255.181802	168370.347584	38.557415
2257.637876	168651.850344	38.562432
2259.765106	168942.813882	38.567450
2261.869708	169239.267257	38.572468
2263.987094	169531.402842	38.577485
2266.202265	169824.070366	38.582503
2268.379603	170134.025875	38.587520
2270.703064	170437.865264	38.592538
2272.917843	170738.396121	38.597556
2274.960353	171048.528834	38.602573
2277.260945	171347.626697	38.607591
2279.624692	171662.867128	38.612608
2281.854636	171965.305190	38.617626
2284.434954	172269.086668	38.622644
2286.533226	172583.940533	38.627661
2289.017921	172890.812196	38.632679
2291.726718	173199.262820	38.637696
2294.439893	173507.256870	38.642714
2296.532602	173807.488737	38.647732
2298.741170	174122.776118	38.652749
2300.895716	174418.899278	38.657767
2303.361275	174723.292323	38.662784
2305.513346	175020.141892	38.667802
2308.246763	175325.701858	38.672820
2310.244589	175629.866381	38.677837
2313.012293	175907.677798	38.682855
2315.994384	176181.025120	38.687872
2317.810762	176453.450020	38.692890
2320.755669	176713.865376	38.697908
2322.916063	176968.486216	38.702925
2325.386282	177227.758015	38.707943
2327.300092	177495.980702	38.712960
2329.601551	177763.001053	38.717978
2331.531173	178026.524533	38.722996
2333.628859	178312.422891	38.728013
2336.103563	178586.377658	38.733031
2338.161995	178868.626783	38.738048
2340.306152	179160.438275	38.743066
2342.156142	179446.632901	38.748084
2344.503619	179739.735345	38.753101
2346.960262	180031.907460	38.758119
2349.174125	180331.712217	38.763136
2351.233253	180638.831211	38.768154
2353.953057	180950.394644	38.773172
2355.957122	181270.756624	38.778189
2358.108650	181574.207099	38.783207
2360.681309	181884.094946	38.788224
2362.888323	182210.041585	38.793242
2365.233023	182532.589963	38.798260
2367.461213	182872.580852	38.803277
2370.106023	183176.112148	38.808295
2372.405664	183502.353610	38.813312
2374.435265	183838.721451	38.818330
2377.559331	184168.621252	38.823348
2379.289707	184506.841273	38.828365
2382.082017	184833.543892	38.833383
2384.390732	185196.490962	38.838400
2386.201658	185587.658971	38.843418
2389.018317	185929.092823	38.848436
2391.525271	186279.414947	38.853453
2393.674089	186618.542098	38.858471
2396.682241	186957.435023	38.863488
2399.115017	187298.679141	38.868506
2401.610514	187634.072698	38.873524
2403.765995	187993.014895	38.878541
2406.412628	188333.746445	38.883559
2408.924587	188677.116201	38.888576
2411.648970	189024.467155	38.893594
2414.469655	189350.798441	38.898612
2417.300816	189677.916452	38.903629
2419.804874	190002.724107	38.908647
2422.555658	190328.764301	38.913664
2425.174122	190651.854184	38.918682
2427.787129	190974.666413	38.923700
2430.295054	191306.741629	38.928717
2433.070566	191602.682083	38.933735
2436.529123	191904.816302	38.938752
2438.793388	192218.516604	38.943770
2441.811499	192511.170266	38.948788
2443.878057	192815.834844	38.953805
2446.284798	193110.718737	38.958823
2448.817854	193408.606370	38.963840
2450.882490	193707.736046	38.968858
2453.327209	194009.144164	38.973876
2455.361345	194319.989861	38.978893
2457.962005	194621.527551	38.983911
2460.240130	194928.805983	38.988928
2462.588146	195242.780169	38.993946
2465.173677	195553.974795	38.998964
2466.767419	195857.780300	39.003981
2469.142533	196174.902202	39.008999
2471.417236	196491.024406	39.014016
2473.702299	196822.005582	39.019034
2476.060659	197127.752402	39.024052
2478.098233	197438.274498	39.029069
2480.863422	197725.898755	39.034087
2483.431438	198024.959628	39.039104
2485.707975	198331.686996	39.044122
2488.415040	198616.197630	39.049140
2490.565019	198927.467439	39.054157
2493.167773	199225.763260	39.059175
2495.299805	199534.039677	39.064192
2497.768513	199855.320939	39.069210
2500.567272	200161.284862	39.074228
2502.717824	200475.148696	39.079245
2505.279517	200800.430930	39.084263
2508.066093	201111.047149	39.089280
2510.136499	201456.246258	39.094298
2512.664564	201780.519567	39.099316
2515.373536	202113.960993	39.104333
2517.603972	202433.048974	39.109351
2520.415678	202757.889642	39.114368
2522.864633	203095.920448	39.119386
2525.220022	203440.012256	39.124404
2527.738819	203775.417002	39.129421
2529.743457	204132.113569	39.134439
2532.708465	204473.114917	39.139456
2534.853420	204843.965683	39.144474
2537.498559	205192.156249	39.149492
2539.841896	205546.846712	39.154509
2542.722322	205906.509387	39.159527
2545.638293	206252.373382	39.164544
2548.130188	206608.312710	39.169562
2550.952108	206974.286264	39.174580
2553.481476	207330.830633	39.179597
2555.847436	207695.275961	39.184615
2558.890647	208053.164092	39.189632
2560.914914	208423.277852	39.194650
2563.561005	208791.085348	39.199668
2566.126522	209165.815627	39.204685
2568.142011	209531.969561	39.209703
2570.913052	209906.668978	39.214720
2573.496525	210292.499395	39.219738
2575.878434	210661.087446	39.224756
2579.014200	211038.221250	39.229773
2581.998752	211407.529436	39.234791
2584.962686	211772.217878	39.239808
2587.689301	212145.225257	39.244826
2589.964295	212519.065491	39.249844
2592.897791	212891.990789	39.254861
2595.657462	213249.396572	39.259879
2598.158266	213618.300073	39.264896
2600.495979	213992.665745	39.269914
2603.163310	214361.569542	39.274932
2605.701521	214736.489093	39.279949
2608.012387	215119.649814	39.284967
2610.719421	215484.788805	39.289984
2613.355006	215868.915883	39.295002
2616.204404	216236.472166	39.300020
2619.395843	216599.809308	39.305037
2621.878815	216971.183005	39.310055
2624.621687	217337.003914	39.315072
2627.076080	217712.777513	39.320090
2629.609610	218089.021753	39.325108
2632.465884	218452.844321	39.330125
2635.242734	218822.115932	39.335143
2637.683261	219179.068388	39.340160
2640.329491	219548.716431	39.345178
2642.890917	219916.345563	39.350196
2645.474240	220285.343299	39.355213
2647.916826	220668.792602	39.360231
2650.905301	221028.912454	39.365248
2652.864450	221387.287341	39.370266
2655.124232	221725.470174	39.375284
2658.015532	222074.631012	39.380301
2660.050858	222431.698813	39.385319
2662.677389	222791.062698	39.390336
2665.913922	223134.250970	39.395354
2668.833496	223484.423960	39.400372
2671.616260	223821.230357	39.405389
2674.005888	224180.301165	39.410407
2676.802669	224536.056940	39.415424
2679.274284	224897.807915	39.420442
2681.817200	225260.995858	39.425460
2684.269063	225625.950871	39.430477
2686.580890	226000.428817	39.435495
2689.706311	226372.341350	39.440512
2692.064537	226747.828214	39.445530
2694.786812	227133.420030	39.450548
2697.188839	227524.650534	39.455565
2699.295223	227913.056322	39.460583
2702.484184	228306.628417	39.465600
2705.454727	228699.954964	39.470618
2707.952289	229114.643614	39.475636
2710.514054	229511.158234	39.480653
2713.385693	229909.097924	39.485671
2716.100979	230315.343503	39.490688
2719.086930	230727.719957	39.495706
2721.675655	231138.278126	39.500724
2724.233528	231555.090260	39.505741
2726.984755	231966.105357	39.510759
2729.755158	232376.151864	39.515776
2732.190531	232806.547993	39.520794
2735.069582	233230.218930	39.525812
2737.957954	233643.142239	39.530829
2740.292776	234074.442162	39.535847
2743.665409	234500.245394	39.540864
2746.702988	234937.760744	39.545882
2749.647053	235355.907108	39.550900
2752.818003	235762.865492	39.555917
2755.772696	236189.443429	39.560935
2758.310206	236607.118307	39.565952
2761.248695	237025.492434	39.570970
2763.865899	237445.313282	39.575988
2766.726526	237862.529978	39.581005
2768.955230	238289.853524	39.586023
2772.558993	238728.165506	39.591040
2775.049135	239137.766349	39.596058
2777.818063	239568.636807	39.601076
2780.847875	239994.131311	39.606093
2783.604477	240422.055627	39.611111
2786.332556	240838.552197	39.616128
2788.991952	241262.324178	39.621146
2791.839920	241688.250819	39.626164
2795.154279	242105.695691	39.631181
2797.827397	242536.982806	39.636199
2800.694173	242953.327351	39.641216
2803.688826	243373.487143	39.646234
2806.241469	243808.169321	39.651252
2809.490041	244227.500540	39.656269
2812.510089	244641.404884	39.661287
2815.222671	245044.585435	39.666304
2818.067664	245460.750900	39.671322
2820.892176	245883.244026	39.676340
2823.606431	246300.672875	39.681357
2826.647073	246708.549432	39.686375
2829.739844	247116.417025	39.691392
2832.333733	247523.116655	39.696410
2835.258536	247939.874136	39.701428
2838.146769	248335.247443	39.706445
2840.641823	248729.791988	39.711463
2843.331627	249094.254298	39.716480
2845.559684	249478.677754	39.721498
2848.463148	249862.995249	39.726516
2851.608893	250241.126826	39.731533
2854.100020	250643.872525	39.736551
2856.633086	251028.778422	39.741568
2859.288334	251431.547441	39.746586
2861.986798	251834.765952	39.751604
2864.605873	252237.106713	39.756621
2867.485478	252654.951821	39.761639
2870.398619	253069.183509	39.766656
2872.981380	253484.481532	39.771674
2875.683094	253898.947022	39.776692
2878.947476	254321.096649	39.781709
2881.641175	254753.494439	39.786727
2885.047820	255179.556608	39.791744
2887.752024	255606.742836	39.796762
2890.637130	256031.638869	39.801780
2894.023937	256467.301794	39.806797
2896.800400	256908.240096	39.811815
2899.548031	257333.991601	39.816832
2902.821682	257761.844327	39.821850
2905.825462	258212.928580	39.826868
2908.627678	258649.589561	39.831885
2911.741498	259085.692504	39.836903
2914.791826	259513.421588	39.841920
2917.881886	259957.297682	39.846938
2920.245329	260398.313356	39.851956
2923.515959	260838.983006	39.856973
2925.806500	261293.951411	39.861991
2929.060045	261751.612966	39.867008
2931.822655	262201.297280	39.872026
2935.066444	262663.909649	39.877044
2937.931992	263104.150946	39.882061
2940.831632	263576.160152	39.887079
2944.043938	264024.751048	39.892096
2947.436798	264470.137030	39.897114
2950.490504	264919.155218	39.902132
2953.890418	265374.975390	39.907149
2956.133516	265825.690550	39.912167
2959.429780	266287.516987	39.917184
2962.397287	266733.873746	39.922202
2965.453674	267191.898112	39.927220
2968.300342	267644.746262	39.932237
2971.329511	268110.491764	39.937255
2973.805894	268569.285679	39.942272
2977.103985	269035.873784	39.947290
2980.354656	269486.237534	39.952308
2983.088986	269954.000928	39.957325
2986.418341	270410.494277	39.962343
2989.074233	270869.401348	39.967360
2992.129298	271334.390208	39.972378
2995.050867	271805.873798	39.977396
2998.216222	272272.847005	39.982413
3000.990012	272741.250113	39.987431
3003.876880	273199.880608	39.992448
3007.020106	273672.310119	39.997466
3009.874654	274152.324794	40.002484
3013.180319	274621.498342	40.007501
3015.847353	275089.270239	40.012519
3018.656450	275569.233057	40.017536
3021.673239	276044.817985	40.022554
3024.784767	276529.096247	40.027572
3027.949371	276988.119759	40.032589
3030.989751	277470.676472	40.037607
3033.873429	277946.143840	40.042624
3036.818208	278410.704144	40.047642
3039.742223	278860.408618	40.052660
3042.924975	279293.182388	40.057677
3045.513623	279741.308584	40.062695
3048.165771	280191.098306	40.067712
3051.101584	280638.403292	40.072730
3054.170543	281104.502264	40.077748
3057.336434	281548.007553	40.082765
3061.488721	281968.679554	40.087783
3065.124166	282410.024193	40.092800
3068.520621	282847.213311	40.097818
3071.338522	283291.117575	40.102836
3074.672264	283721.861049	40.107853
3077.380785	284174.410633	40.112871
3080.060210	284616.575936	40.117888
3083.659888	285062.353405	40.122906
3086.957654	285506.372063	40.127924
3089.997355	285951.291349	40.132941
3093.059185	286394.629926	40.137959
3096.064811	286848.791539	40.142976
3099.509627	287300.697977	40.147994
3102.134436	287751.890999	40.153012
3105.214711	288216.950254	40.158029
3108.436488	288691.125227	40.163047
3111.209383	289158.409283	40.168064
3113.874682	289619.333438	40.173082
3116.533228	290112.959246	40.178100
3119.924692	290584.503903	40.183117
3123.057598	291073.503390	40.188135
3125.984956	291559.966578	40.193152
3129.846497	292046.940729	40.198170
3132.465381	292545.580795	40.203188
3135.393108	293040.284054	40.208205
3138.918029	293541.110854	40.213223
3141.636203	294044.826496	40.218240
3144.765739	294540.400047	40.223258
3148.073892	295055.237446	40.228276
3150.944733	295568.564278	40.233293
3154.163316	296077.592568	40.238311
3157.510944	296593.781260	40.243328
3160.710839	297111.714717	40.248346
3163.885700	297632.008466	40.253364
3166.803989	298143.934002	40.258381
3170.107251	298671.916100	40.263399
3172.979683	299211.409950	40.268416
3176.221785	299728.906579	40.273434
3179.493162	300271.425239	40.278452
3182.437632	300807.972768	40.283469
3185.512654	301333.908574	40.288487
3188.746687	301881.875035	40.293504
3192.473567	302407.622740	40.298522
3196.592193	302927.338671	40.303540
3199.962231	303446.252105	40.308557
3203.226670	303966.928413	40.313575
3206.299263	304486.207824	40.318592
3209.723292	305005.300416	40.323610
3212.574590	305525.644575	40.328628
3215.915155	306057.101676	40.333645
3219.115165	306584.564445	40.338663
3222.312258	307100.574175	40.343680
3225.637493	307623.894420	40.348698
3229.206590	308156.156800	40.353716
3232.842936	308654.060140	40.358733
3236.431995	309166.662255	40.363751
3239.852078	309670.350746	40.368768
3243.054195	310163.077542	40.373786
3246.482704	310661.449582	40.378804
3249.637534	311177.651420	40.383821
3253.089972	311660.577419	40.388839
3255.468147	312137.828062	40.393856
3258.778725	312602.010027	40.398874
3261.638264	313075.140730	40.403892
3264.529041	313543.287267	40.408909
3267.511388	314014.511181	40.413927
3270.706794	314501.559400	40.418944
3274.096653	314977.303756	40.423962
3276.998468	315482.888776	40.428980
3279.744623	315964.128736	40.433997
3282.856667	316464.340535	40.439015
3285.709845	316973.520190	40.444032
3289.305568	317479.076333	40.449050
3292.963859	318001.416995	40.454068
3295.998805	318521.412254	40.459085
3299.349213	319033.434624	40.464103
3302.414530	319567.700016	40.469120
3305.961679	320096.199534	40.474138
3309.010597	320616.497495	40.479156
3312.263755	321155.560853	40.484173
3315.821387	321698.249472	40.489191
3319.154220	322245.229162	40.494208
3321.913186	322782.953126	40.499226
3325.734363	323335.704242	40.504244
3328.656201	323888.055127	40.509261
3332.326886	324441.017973	40.514279
3335.359481	325006.099737	40.519296
3338.821511	325554.639729	40.524314
3342.569405	326137.152773	40.529332
3345.733118	326707.442736	40.534349
3349.473117	327263.375857	40.539367
3352.469838	327837.227880	40.544384
3355.977445	328401.376408	40.549402
3359.377533	328980.553265	40.554420
3362.909260	329560.233916	40.559437
3366.383674	330129.360902	40.564455
3369.334959	330716.294520	40.569472
3373.363325	331295.973569	40.574490
3376.982294	331873.982514	40.579508
3379.975655	332445.839398	40.584525
3383.662548	333025.748393	40.589543
3387.323868	333606.464278	40.594560
3391.002916	334179.710408	40.599578
3394.154504	334764.521187	40.604596
3397.541318	335348.956435	40.609613
3401.231671	335922.605280	40.614631
3404.722896	336497.772796	40.619648
3408.647612	337079.053051	40.624666
3412.373902	337647.393337	40.629684
3415.642298	338225.586796	40.634701
3419.347631	338796.068348	40.639719
3422.608074	339354.714386	40.644736
3426.569405	339913.090462	40.649754
3430.535911	340476.073081	40.654772
3433.369603	341041.632503	40.659789
3437.262660	341602.934672	40.664807
3440.398983	342171.903488	40.669824
3443.750223	342726.373515	40.674842
3447.399871	343292.631918	40.679860
3450.702975	343858.300964	40.684877
3454.251284	344424.658011	40.689895
3457.942916	344982.208874	40.694912
3461.280150	345533.947731	40.699930
3464.917278	346084.109411	40.704948
3468.333833	346638.505994	40.709965
3472.117405	347199.885917	40.714983
3475.373217	347761.718918	40.720000
3478.588524	348318.477277	40.725018
3482.117160	348859.867053	40.730023
3484.745868	349364.890949	40.735028
3487.982182	349835.824596	40.740032
3491.302759	350278.877263	40.745037
3493.963043	350658.145200	40.750042
3496.569912	351002.896476	40.755047
3498.968229	351291.676487	40.760052
3501.279532	351527.569018	40.765056
3503.278868	351736.207754	40.770061
3505.165584	351921.324278	40.775066
3507.017900	352048.692417	40.780071
3508.498655	352150.978240	40.785076
3510.048446	352215.607179	40.790080
3510.940250	352245.692059	40.795085
3512.327650	352244.027509	40.800090
3513.100116	352235.188765	40.805095
3514.065448	352183.717411	40.810100
3514.821390	352125.872904	40.815104
3515.187040	352048.058601	40.820109
3516.135035	351936.116903	40.825114
3516.770674	351816.826347	40.830119
3517.085915	351687.925756	40.835124
3517.772752	351526.480412	40.840128
3518.197754	351385.843036	40.845133
3518.327060	351217.619553	40.850138
3518.765750	351033.891620	40.855143
3518.648922	350855.943235	40.860148
3519.126328	350657.641336	40.865152
3519.118084	350458.956236	40.870157
3518.845888	350246.024547	40.875162
3519.119956	350040.581896	40.880167
3518.671074	349830.064561	40.885172
3518.787891	349616.102242	40.890176
3518.998364	349405.149104	40.895181
3518.764943	349186.255899	40.900186
3518.421144	348962.878771	40.905191
3518.208397	348743.674354	40.910196
3518.224324	348529.822380	40.915200
3517.658146	348308.585474	40.920205
3517.519932	348088.729574	40.925210
3517.765050	347885.311817	40.930215
3517.475678	347660.468369	40.935220
3517.626874	347441.478386	40.940224
3517.092080	347235.178132	40.945229
3517.018521	347008.237452	40.950234
3516.703138	346800.502105	40.955239
3516.098913	346591.640940	40.960244
3515.871301	346365.508027	40.965248
3515.909694	346172.205267	40.970253
3515.551989	345978.403712	40.975258
3515.465710	345771.668767	40.980263
3515.226967	345580.897327	40.985268
3515.189399	345378.881330	40.990272
3515.164569	345187.184539	40.995277
3514.475916	344991.801684	41.000282
3514.610228	344796.976118	41.005287
3514.149662	344610.733973	41.010292
3514.084372	344417.895039	41.015296
3513.689679	344240.463163	41.020301
3513.649600	344061.805619	41.025306
3513.152599	343875.107496	41.030311
3512.931866	343705.070054	41.035316
3513.019117	343529.288466	41.040320
3512.670880	343367.202058	41.045325
3512.427165	343194.241698	41.050330
3512.171741	343023.748638	41.055335
3511.737787	342873.343880	41.060340
3511.540639	342712.883614	41.065344
3511.944957	342550.727141	41.070349
3511.677919	342396.480369	41.075354
3511.343784	342252.464913	41.080359
3511.137442	342088.570595	41.085364
3511.191360	341934.932941	41.090368
3511.037288	341789.590785	41.095373
3510.830630	341657.758048	41.100378
3510.506848	341508.754197	41.105383
3510.325099	341355.913502	41.110388
3510.139006	341220.490663	41.115392
3509.875336	341081.341518	41.120397
3509.932624	340955.008295	41.125402
3509.685170	340807.871255	41.130407
3509.507754	340690.015636	41.135412
3509.652692	340552.504496	41.140416
3509.613323	340432.668586	41.145421
3509.129729	340315.215361	41.150426
3508.990148	340178.433608	41.155431
3508.918915	340069.077868	41.160436
3508.739565	339935.886766	41.165440
3508.642348	339821.753768	41.170445
3508.713226	339704.034246	41.175450
3508.745046	339591.101003	41.180455
3508.447252	339474.811245	41.185460
3508.583028	339348.638109	41.190464
3508.380336	339246.420385	41.195469
3508.483839	339128.922757	41.200474
3508.353869	339011.333931	41.205479
3508.108385	338917.004941	41.210484
3508.385581	338801.310113	41.215488
3508.138035	338689.282102	41.220493
3507.840125	338574.972936	41.225498
3507.986802	338464.535792	41.230503
3507.801153	338363.152081	41.235508
3508.006222	338237.193138	41.240512
3508.089235	338135.360108	41.245517
3507.601102	338035.726340	41.250522
3507.674529	337932.114148	41.255527
3507.175116	337830.599764	41.260532
3507.459871	337725.097713	41.265536
3507.288688	337633.195094	41.270541
3507.224219	337530.391547	41.275546
3507.263514	337425.206556	41.280551
3507.108329	337341.463802	41.285556
3507.024790	337227.040742	41.290560
3507.277387	337135.223505	41.295565
3507.057930	337042.970885	41.300570
3506.726163	336945.751128	41.305575
3506.787044	336865.483073	41.310580
3506.994028	336766.246279	41.315584
3506.838418	336671.134556	41.320589
3506.611156	336576.160890	41.325594
3506.795733	336486.819401	41.330599
3506.454651	336403.866357	41.335604
3506.912837	336307.666375	41.340608
3506.968758	336220.734772	41.345613
3506.409149	336134.865129	41.350618
3506.398327	336033.015420	41.355623
3506.292182	335950.711439	41.360628
3506.255924	335850.848821	41.365632
3506.220100	335777.180146	41.370637
3506.245580	335684.784283	41.375642
3506.185137	335612.339818	41.380647
3505.940747	335529.802100	41.385652
3506.013472	335439.814267	41.390656
3506.075148	335361.450187	41.395661
3505.852565	335288.547120	41.400666
3506.089168	335197.287048	41.405671
3506.052481	335122.727098	41.410676
3505.710669	335036.871883	41.415680
3505.711877	334964.213107	41.420685
3505.961871	334886.327360	41.425690
3505.963263	334801.079426	41.430695
3505.536248	334721.518447	41.435700
3505.766175	334640.990379	41.440704
3505.355765	334562.265736	41.445709
3505.386666	334478.233219	41.450714
3505.532892	334409.721682	41.455719
3505.507011	334344.975352	41.460724
3505.512107	334266.287160	41.465728
3505.530022	334189.021022	41.470733
3505.085696	334121.389262	41.475738
3505.458471	334039.744079	41.480743
3505.432446	333979.651292	41.485748
3505.629872	333900.398322	41.490752
3505.238797	333826.653919	41.495757
3505.146601	333758.356327	41.500762
3505.244088	333686.061585	41.505767
3505.033799	333619.130054	41.510772
3505.275681	333539.131856	41.515776
3505.310624	333470.585064	41.520781
3505.320711	333407.230335	41.525786
3505.756836	333323.717143	41.530791
3505.207427	333261.110492	41.535796
3505.159291	333184.132341	41.540800
3505.293996	333106.362586	41.545805
3505.372802	333039.130711	41.550810
3505.095728	332969.588807	41.555815
3505.062539	332898.508260	41.560820
3505.176127	332823.691474	41.565824
3504.717597	332765.266362	41.570829
3505.002760	332696.475769	41.575834
3505.226770	332626.906130	41.580839
3504.746747	332559.963837	41.585844
3504.861787	332493.590101	41.590848
3505.274880	332426.457727	41.595853
3504.937734	332361.832745	41.600858
3505.119651	332282.171873	41.605863
3504.944890	332218.386124	41.610868
3505.016327	332145.812738	41.615872
3504.961212	332074.937540	41.620877
3504.733441	332022.019957	41.625882
3504.932922	331953.495699	41.630887
3504.757188	331884.673633	41.635892
3504.851098	331816.038388	41.640896
3504.961474	331745.899851	41.645901
3504.627456	331688.115003	41.650906
3504.858392	331614.294956	41.655911
3504.735588	331553.094299	41.660916
3504.380970	331496.355170	41.665920
3504.558384	331428.316661	41.670925
3504.652797	331373.516783	41.675930
3504.360141	331298.480461	41.680935
3504.666639	331245.504105	41.685940
3504.655521	331185.277425	41.690944
3504.677120	331123.341451	41.695949
3504.635569	331062.000198	41.700954
3504.780614	330998.467876	41.705959
3504.748248	330935.344576	41.710964
3504.645810	330863.965825	41.715968
3504.473242	330796.667402	41.720973
3504.361596	330741.084785	41.725978
3504.761684	330687.737017	41.730983
3504.551090	330623.165729	41.735988
3504.732432	330562.984438	41.740992
3504.649373	330498.240487	41.745997
3504.626161	330435.140384	41.751002
3504.704121	330365.233304	41.756007
3504.889052	330311.842198	41.761012
3504.549729	330239.354588	41.766016
3504.676966	330178.265460	41.771021
3504.586134	330120.338691	41.776026
3504.616799	330053.363450	41.781031
3504.293763	329982.348067	41.786036
3504.409543	329931.078323	41.791040
3504.296883	329867.050118	41.796045
3504.252344	329800.340499	41.801050
3504.606824	329740.436222	41.806055
3504.649026	329691.415926	41.811060
3504.656371	329625.689916	41.816064
3504.583039	329557.203884	41.821069
3504.438568	329504.422517	41.826074
3504.841239	329440.669521	41.831079
3504.696377	329386.921506	41.836084
3504.557151	329319.284688	41.841088
3504.540638	329249.771853	41.846093
3504.101411	329188.540413	41.851098
3504.640329	329126.393593	41.856103
3504.431843	329061.972016	41.861108
3504.221522	329000.348561	41.866112
3504.312350	328947.478960	41.871117
3504.168240	328892.229437	41.876122
3504.447598	328825.442328	41.881127
3504.014930	328774.663399	41.886132
3504.312965	328721.150788	41.891136
3504.212825	328657.398464	41.896141
3503.612818	328588.636602	41.901146
3504.118465	328538.906854	41.906151
3504.017391	328484.006170	41.911156
3504.387268	328438.697881	41.916160
3504.374110	328380.807338	41.921165
3504.186372	328324.648108	41.926170
3504.815133	328260.018631	41.931175
3504.106195	328208.340824	41.936180
3504.025946	328137.106283	41.941184
3504.411860	328089.404080	41.946189
3504.253655	328039.649830	41.951194
3504.243052	327979.265533	41.956199
3504.100925	327913.941487	41.961204
3504.217380	327861.320819	41.966208
3504.543163	327797.704330	41.971213
3504.078613	327739.984845	41.976218
3504.041724	327678.052548	41.981223
3504.176047	327638.579569	41.986228
3504.306685	327576.799103	41.991232
3504.402985	327524.333748	41.996237
3503.894679	327471.199304	42.001242
3503.842147	327416.111539	42.006247
3503.898726	327361.032156	42.011252
3503.822510	327300.936851	42.016256
3504.238009	327246.437381	42.021261
3503.814662	327186.624856	42.026266
3504.021224	327130.122783	42.031271
3504.086828	327085.801481	42.036276
3504.053447	327027.327073	42.041280
3504.235140	326976.043258	42.046285
3503.849513	326921.973260	42.051290
3503.803410	326863.627780	42.056295
3503.709486	326816.253105	42.061300
3503.902398	326756.496667	42.066304
3503.929234	326710.273189	42.071309
3503.674066	326655.419414	42.076314
3504.095077	326593.388754	42.081319
3503.859255	326549.597079	42.086324
3503.963618	326491.482021	42.091328
3503.759919	326431.456134	42.096333
3503.461146	326388.742454	42.101338
3503.789953	326326.929234	42.106343
3503.644045	326290.118609	42.111348
3503.687644	326237.430843	42.116352
3503.680328	326190.550709	42.121357
3503.627174	326134.087659	42.126362
3503.898868	326092.226089	42.131367
3503.853474	326050.795384	42.136372
3503.795711	325988.711115	42.141376
3503.818816	325937.730478	42.146381
3503.780547	325890.778503	42.151386
3503.571298	325829.633325	42.156391
3503.385600	325783.365552	42.161396
3503.646525	325742.090369	42.166400
3503.366983	325682.736562	42.171405
3503.507623	325651.578866	42.176410
3503.400753	325605.654756	42.181415
3503.570101	325569.455809	42.186420
3503.304353	325513.940749	42.191424
3503.578146	325465.260813	42.196429
3503.463996	325416.437682	42.201434
3503.505976	325363.494657	42.206439
3503.585585	325326.953326	42.211444
3503.876748	325281.068665	42.216448
3503.980118	325213.590684	42.221453
3503.778785	325170.657058	42.226458
3503.722649	325115.795674	42.231463
3504.096948	325060.765482	42.236468
3503.649390	325000.495613	42.241472
3503.901977	324949.706980	42.246477
3503.399233	324912.518188	42.251482
3503.649472	324867.300832	42.256487
3503.589672	324817.145732	42.261492
3503.508297	324773.480746	42.266496
3503.654225	324714.288275	42.271501
3503.740464	324667.976925	42.276506
3503.645006	324607.956953	42.281511
3503.520630	324563.001067	42.286516
3503.322983	324514.444244	42.291520
3503.571780	324468.616148	42.296525
3503.137392	324421.291674	42.301530
3503.650844	324377.762656	42.306535
3503.393301	324327.663170	42.311540
3503.555268	324288.767734	42.316544
3503.754656	324230.024148	42.321549
3503.387038	324182.714449	42.326554
3503.784381	324133.097914	42.331559
3503.605557	324090.541244	42.336564
3503.064212	324039.773283	42.341568
3503.133421	323989.113762	42.346573
3503.115909	323946.913427	42.351578
3503.519352	323903.426469	42.356583
3503.572451	323861.418572	42.361588
3503.328357	323818.464754	42.366592
3503.606613	323766.093451	42.371597
3503.376659	323727.156720	42.376602
3503.599225	323666.577113	42.381607
3503.673561	323630.976352	42.386612
3503.435315	323575.454404	42.391616
3503.862299	323531.149339	42.396621
3503.225260	323485.839596	42.401626
3503.332478	323434.232231	42.406631
3503.935647	323397.200693	42.411636
3503.923275	323342.101194	42.416640
3503.709478	323296.165716	42.421645
3503.719078	323247.753238	42.426650
3503.717582	323187.487637	42.431655
3503.732365	323138.311041	42.436660
3503.488748	323090.039542	42.441664
3503.734314	323036.705710	42.446669
3503.213158	322992.700256	42.451674
3503.615211	322948.500213	42.456679
3503.234609	322893.991657	42.461684
3503.485647	322852.409858	42.466688
3503.495686	322810.102328	42.471693
3503.032219	322770.310654	42.476698
3503.433401	322715.629332	42.481703
3503.216492	322676.791352	42.486708
3503.315229	322631.671465	42.491712
3503.235857	322582.254471	42.496717
3502.988010	322540.699117	42.501722
3503.470663	322488.930408	42.506727
3503.243000	322445.412947	42.511732
3503.063122	322407.586553	42.516736
3503.495431	322365.721666	42.521741
3503.181661	322324.201796	42.526746
3503.546440	322270.746683	42.531751
3503.123222	322239.496093	42.536756
3503.475289	322194.005595	42.541760
3503.075572	322141.941288	42.546765
3502.834208	322103.132025	42.551770
3503.435887	322063.835377	42.556775
3503.327434	322021.952538	42.561780
3503.014589	321977.710085	42.566784
3503.139908	321923.070666	42.571789
3502.886096	321890.826727	42.576794
3503.248771	321845.944772	42.581799
3503.192179	321803.341319	42.586804
3502.881893	321765.331122	42.591808
3503.464850	321722.449984	42.596813
3503.127099	321680.882335	42.601818
3503.007497	321637.728833	42.606823
3503.187493	321594.197941	42.611828
3502.986336	321549.174448	42.616832
3503.241182	321509.575092	42.621837
3502.855562	321479.946282	42.626842
3502.808474	321432.303759	42.631847
3502.949665	321389.567352	42.636852
3502.905053	321352.685710	42.641856
3503.176817	321309.801702	42.646861
3502.831415	321276.553925	42.651866
3503.041859	321234.976856	42.656871
3503.306415	321196.037156	42.661876
3502.941079	321146.790194	42.666880
3502.871094	321100.422899	42.671885
3502.518900	321066.794404	42.676890
3502.941475	321019.078335	42.681895
3503.057892	320988.353428	42.686900
3502.978602	320953.613865	42.691904
3503.078042	320910.578187	42.696909
3503.142544	320874.569582	42.701914
3503.138203	320840.072672	42.706919
3502.992690	320787.636419	42.711924
3503.184393	320752.116735	42.716928
3503.097325	320706.743869	42.721933
3503.194441	320671.849421	42.726938
3503.190583	320622.418401	42.731943
3502.932138	320584.602613	42.736948
3503.008416	320538.135627	42.741952
3503.109540	320489.985611	42.746957
3503.113740	320464.594981	42.751962
3503.109253	320409.439564	42.756967
3502.834822	320373.915781	42.761972
3502.815885	320331.076033	42.766976
3502.810545	320294.212810	42.771981
3502.698858	320269.272598	42.776986
3503.060984	320216.756655	42.781991
3502.887721	320182.285504	42.786996
3502.853083	320153.389838	42.792001
3503.010809	320110.751351	42.797005
3502.901651	320077.262352	42.802010
3502.861008	320023.714873	42.807015
3503.224627	319989.160022	42.812020
3503.296422	319942.057058	42.817025
3503.096774	319901.000461	42.822029
3503.002877	319864.048887	42.827034
3503.083255	319824.220715	42.832039
3503.045438	319785.097820	42.837044
3503.111759	319745.449854	42.842049
3503.398994	319696.939255	42.847053
3502.811155	319664.974595	42.852058
3503.181842	319620.648785	42.857063
3503.206214	319581.973978	42.862068
3502.821205	319545.016549	42.867073
3503.038293	319493.641733	42.872077
3502.614125	319464.297390	42.877082
3502.966128	319418.931173	42.882087
3502.707431	319379.002707	42.887092
3502.506585	319345.578294	42.892097
3502.937088	319302.082430	42.897101
3502.911803	319269.317568	42.902106
3502.949547	319226.595118	42.907111
3502.743095	319193.909274	42.912116
3502.668577	319160.973899	42.917121
3502.927262	319121.549850	42.922125
3502.997863	319085.564250	42.927130
3502.695758	319036.432251	42.932135
3502.658041	319002.346142	42.937140
3502.954117	318972.813063	42.942145
3502.930857	318933.381835	42.947149
3502.909137	318899.598460	42.952154
3503.329588	318856.129159	42.957159
3503.036228	318810.455664	42.962164
3502.675839	318769.651994	42.967169
3502.941800	318732.261830	42.972173
3502.449486	318702.164315	42.977178
3502.697991	318654.294638	42.982183
3502.794213	318620.314601	42.987188
3503.153877	318577.083463	42.992193
3502.769757	318546.205738	42.997197
3502.738553	318501.712353	43.002202
3502.862471	318471.696883	43.007207
3502.692688	318428.522545	43.012212
3502.699391	318394.632590	43.017217
3503.019408	318359.116428	43.022221
3502.699685	318331.256170	43.027226
3502.495198	318292.895703	43.032231
3502.736208	318251.285579	43.037236
3502.387013	318221.267233	43.042241
3502.682704	318186.390778	43.047245
3502.417378	318144.884789	43.052250
3502.564018	318114.814654	43.057255
3502.735012	318076.192030	43.062260
3502.437640	318045.529438	43.067265
3502.919510	318003.169208	43.072269
3502.642619	317973.444753	43.077274
3502.414392	317937.173961	43.082279
3502.421311	317905.471659	43.087284
3502.550173	317878.660783	43.092289
3502.574903	317845.378224	43.097293
3502.552484	317812.993470	43.102298
3502.453237	317776.269951	43.107303
3502.908741	317745.617207	43.112308
3502.695830	317706.646918	43.117313
3502.725356	317677.739633	43.122317
3502.349491	317640.830063	43.127322
3502.758930	317598.429833	43.132327
3502.682809	317559.972428	43.137332
3502.606451	317531.590381	43.142337
3502.558375	317494.655123	43.147341
3502.503592	317465.022978	43.152346
3502.549752	317435.146118	43.157351
3502.524322	317398.309028	43.162356
3502.259310	317366.648657	43.167361
3502.618104	317324.281491	43.172365
3502.504978	317301.349805	43.177370
3502.590151	317268.515382	43.182375
3502.934239	317230.246731	43.187380
3502.563674	317198.450008	43.192385
3502.943357	317153.586015	43.197389
3502.603790	317123.514540	43.202394
3502.520255	317092.029278	43.207399
3502.346660	317048.625202	43.212404
3502.294284	317020.289984	43.217409
3502.680734	316987.204926	43.222413
3502.262182	316966.712250	43.227418
3502.406064	316934.300978	43.232423
3502.113426	316896.792647	43.237428
3502.397063	316867.692635	43.242433
3502.416082	316831.865889	43.247437
3502.146257	316811.578986	43.252442
3502.617103	316772.934015	43.257447
3502.469245	316737.413037	43.262452
3502.574396	316713.505682	43.267457
3502.772347	316671.595463	43.272461
3502.329049	316635.128089	43.277466
3502.498020	316600.549990	43.282471
3502.693782	316574.364003	43.287476
3502.504351	316543.429145	43.292481
3502.492037	316508.293987	43.297485
3502.782271	316481.711594	43.302490
3502.544442	316436.713986	43.307495
3502.587278	316409.991946	43.312500
3502.668493	316367.616183	43.317505
3502.512565	316324.666639	43.322509
3502.664521	316303.168916	43.327514
3502.498317	316270.296548	43.332519
3502.503485	316242.969625	43.337524
3502.197933	316211.212971	43.342529
3502.555590	316181.592126	43.347533
3502.369125	316150.834642	43.352538
3502.613445	316108.713134	43.357543
3502.187485	316082.089294	43.362548
3502.542540	316050.687713	43.367553
3502.815711	316020.698255	43.372557
3502.563372	315986.388795	43.377562
3502.373456	315938.966084	43.382567
3502.696511	315911.335056	43.387572
3502.600914	315886.517084	43.392577
3502.575997	315840.798768	43.397581
3502.561655	315811.464563	43.402586
3502.742022	315773.296482	43.407591
3502.730491	315740.959424	43.412596
3502.426140	315705.054883	43.417601
3502.679231	315666.341075	43.422605
3502.574936	315634.476366	43.427610
3502.886599	315599.951628	43.432615
3502.758874	315567.810635	43.437620
3502.507913	315534.238492	43.442625
3502.374681	315507.874088	43.447629
3502.605620	315473.310928	43.452634
3502.960184	315432.418392	43.457639
3502.862235	315404.445466	43.462644
3502.509073	315362.289022	43.467649
3502.939869	315321.689853	43.472653
3502.525575	315294.427632	43.477658
3502.461496	315252.836759	43.482663
3502.792377	315218.283297	43.487668
3502.604665	315181.291539	43.492673
3502.492605	315135.280744	43.497677
3502.310290	315113.681809	43.502682
3502.433744	315077.608424	43.507687
3503.021667	315043.981711	43.512692
3502.301209	315005.800502	43.517697
3502.262364	314980.082655	43.522701
3502.571733	314946.651883	43.527706
3502.416632	314918.636664	43.532711
3502.771757	314882.730628	43.537716
3502.514597	314846.716290	43.542721
3502.715595	314817.042603	43.547725
3502.392258	314795.541795	43.552730
3502.510922	314753.336810	43.557735
3502.594685	314720.704311	43.562740
3502.238832	314690.913640	43.567745
3502.311551	314657.672149	43.572749
3502.563401	314625.802204	43.577754
3502.420384	314592.823238	43.582759
3502.484300	314563.221607	43.587764
3501.979827	314533.886517	43.592769
3502.595129	314496.998247	43.597773
3502.477757	314468.595214	43.602778
3502.771142	314434.835778	43.607783
3502.633727	314400.252794	43.612788
3502.296737	314357.176902	43.617793
3502.239541	314327.135963	43.622797
3502.381400	314298.768819	43.627802
3502.318767	314267.380122	43.632807
3502.231602	314236.173334	43.637812
3502.223858	314218.083619	43.642817
3502.533923	314182.387607	43.647821
3502.370204	314153.279141	43.652826
3502.311373	314119.523393	43.657831
3502.434709	314080.192318	43.662836
3502.197644	314050.255524	43.667841
3502.549684	314013.535059	43.672845
3502.100428	313995.971968	43.677850
3502.202939	313961.631213	43.682855
3502.121659	313934.367251	43.687860
3502.506730	313900.542267	43.692865
3502.628123	313868.590320	43.697869
3502.642890	313840.395342	43.702874
3502.448219	313799.866716	43.707879
3502.754578	313759.361867	43.712884
3502.418507	313729.287601	43.717889
3502.537668	313686.089210	43.722893
3502.268337	313666.564178	43.727898
3502.431074	313630.483547	43.732903
3502.682447	313595.203336	43.737908
3502.448852	313577.530192	43.742913
3502.271749	313549.873794	43.747917
3502.301439	313517.147080	43.752922
3502.565281	313488.353337	43.757927
3502.552978	313449.704407	43.762932
3502.431488	313427.789874	43.767937
3502.651599	313383.455908	43.772941
3502.545556	313350.724753	43.777946
3502.481294	313313.864956	43.782951
3502.630749	313281.653787	43.787956
3502.570096	313250.671217	43.792961
3502.452537	313212.165695	43.797965
3502.302843	313187.303792	43.802970
3502.585536	313151.356795	43.807975
3502.499584	313118.596905	43.812980
3502.389233	313084.008728	43.817985
3502.429365	313049.600671	43.822989
3502.687406	313018.441126	43.827994
3502.782863	312979.876819	43.832999
3502.540113	312947.344772	43.838004
3502.343568	312929.767398	43.843009
3502.579297	312889.985256	43.848013
3502.316421	312861.044082	43.853018
3502.073409	312827.290612	43.858023
3502.572292	312800.648178	43.863028
3502.195913	312773.505794	43.868033
3502.051206	312729.940451	43.873037
3501.948106	312703.544311	43.878042
3502.304211	312671.784030	43.883047
3502.077618	312643.600441	43.888052
3502.186663	312620.631835	43.893057
3502.460248	312588.935230	43.898061
3502.214579	312575.334875	43.903066
3502.394323	312535.790155	43.908071
3502.322165	312504.249078	43.913076
3502.208732	312481.060567	43.918081
3502.271496	312443.289721	43.923085
3502.434809	312418.276919	43.928090
3502.529963	312386.429825	43.933095
3502.641090	312349.694651	43.938100
3502.213379	312335.308292	43.943105
3502.294927	312280.918346	43.948109
3502.512371	312248.899455	43.953114
3502.434066	312232.270358	43.958119
3502.523314	312206.123910	43.963124
3502.181594	312172.512559	43.968129
3502.433116	312136.060721	43.973133
3502.499234	312102.055059	43.978138
3502.275187	312074.888566	43.983143
3502.334396	312043.352184	43.988148
3502.289415	312020.305470	43.993153
3502.271351	311987.941362	43.998157
3502.108494	311956.235911	44.003162
3502.414368	311919.317422	44.008167
3502.458621	311890.633209	44.013172
3502.437010	311860.127119	44.018177
3502.618231	311826.357807	44.023181
3502.279216	311791.702479	44.028186
3502.056754	311765.731524	44.033191
3502.023105	311741.843193	44.038196
3502.042012	311714.969485	44.043201
3502.212060	311677.359455	44.048205
3502.383962	311655.245764	44.053210
3502.122892	311616.583146	44.058215
3502.334235	311592.402155	44.063220
3502.154602	311569.808759	44.068225
3502.158445	311541.639546	44.073229
3501.816544	311518.867808	44.078234
3502.422738	311487.093261	44.083239
3502.322250	311458.965680	44.088244
3501.971880	311440.037594	44.093249
3502.028755	311397.457502	44.098253
3501.866267	311376.362672	44.103258
3501.883550	311353.611300	44.108263
3502.208177	311321.956798	44.113268
3502.024732	311293.892921	44.118273
3501.939911	311266.729747	44.123277
3501.975693	311249.751751	44.128282
3502.049286	311216.507681	44.133287
3502.263973	311188.254556	44.138292
3502.152546	311165.421338	44.143297
3502.343297	311132.667904	44.148301
3502.143486	311107.660027	44.153306
3502.336014	311081.827691	44.158311
3502.482806	311054.068534	44.163316
3502.080001	311022.170782	44.168321
3502.265107	310990.232414	44.173325
3502.325227	310969.967943	44.178330
3502.102733	310942.317079	44.183335
3502.361416	310905.506934	44.188340
3501.854733	310885.839558	44.193345
3502.040305	310854.715316	44.198349
3501.978634	310837.116176	44.203354
3502.188533	310808.838126	44.208359
3502.153506	310766.755257	44.213364
3502.271514	310752.919660	44.218369
3501.800221	310729.684196	44.223373
3501.939929	310699.508512	44.228378
3502.296929	310672.937859	44.233383
3502.262513	310638.361526	44.238388
3502.194721	310615.546702	44.243393
3502.125526	310574.588633	44.248397
3502.044469	310553.862469	44.253402
3502.253806	310531.946007	44.258407
3502.449810	310502.652073	44.263412
3502.439946	310472.219609	44.268417
3502.477166	310441.016397	44.273421
3501.887307	310403.523617	44.278426
3501.827764	310373.811330	44.283431
3502.340020	310343.984599	44.288436
3502.071699	310319.826714	44.293441
3502.130143	310286.329890	44.298445
3502.171423	310273.193158	44.303450
3502.106988	310248.901724	44.308455
3502.530168	310220.030310	44.313460
3502.145903	310182.479918	44.318465
3502.423456	310162.919230	44.323469
3502.445691	310125.025622	44.328474
3502.002358	310104.355639	44.333479
3502.343964	310065.801561	44.338484
3501.995924	310050.944068	44.343489
3502.098385	310016.702247	44.348493
3502.070102	309981.208399	44.353498
3501.919199	309964.004530	44.358503
3501.892494	309942.811600	44.363508
3501.828798	309925.772276	44.368513
3502.009910	309879.125435	44.373517
3502.018013	309859.021274	44.378522
3501.755367	309843.590595	44.383527
3501.714834	309816.012557	44.388532
3501.568016	309799.367829	44.393537
3501.847606	309773.114092	44.398541
3501.944605	309746.303472	44.403546
3501.945464	309731.086223	44.408551
3502.173545	309697.867960	44.413556
3501.769226	309674.239858	44.418561
3502.370043	309643.610054	44.423565
3502.372155	309621.521850	44.428570
3502.061892	309585.231837	44.433575
3502.155262	309553.459479	44.438580
3502.126458	309536.465482	44.443585
3502.328125	309504.574451	44.448589
3502.474844	309477.832288	44.453594
3502.245355	309458.935505	44.458599
3502.185381	309418.738441	44.463604
3501.857223	309391.179473	44.468609
3502.157573	309365.303995	44.473613
3502.187417	309340.997435	44.478618
3502.100727	309314.953134	44.483623
3502.146824	309287.819368	44.488628
3501.684275	309258.449031	44.493633
3502.226329	309235.360526	44.498637
3502.287151	309211.074529	44.503642
3502.088002	309184.742290	44.508647
3502.240256	309149.550558	44.513652
3502.355625	309131.388853	44.518657
3502.209943	309095.887181	44.523661
3502.103287	309066.130531	44.528666
3501.826572	309036.069509	44.533671
3501.897915	309010.814772	44.538676
3502.127435	308989.556108	44.543681
3501.997990	308959.115857	44.548685
3502.406275	308935.589973	44.553690
3501.817379	308903.159937	44.558695
3501.832059	308881.247575	44.563700
3501.872397	308855.157814	44.568705
3502.090086	308840.975343	44.573709
3501.987054	308800.479101	44.578714
3501.642534	308776.841259	44.583719
3501.744650	308754.635311	44.588724
3501.439576	308744.631224	44.593729
3501.400151	308712.217346	44.598733
3501.582181	308707.379660	44.603738
3501.647057	308682.838294	44.608743
3501.565062	308658.752381	44.613748
3501.768233	308653.529685	44.618753
3502.019513	308623.666172	44.623757
3502.023591	308593.281260	44.628762
3501.725164	308576.965080	44.633767
3501.689365	308548.647608	44.638772
3501.666665	308529.921869	44.643777
3501.656845	308506.384499	44.648781
3501.850316	308490.882415	44.653786
3501.715415	308466.117552	44.658791
3501.871080	308438.940819	44.663796
3501.864114	308419.296470	44.668801
3502.107029	308387.830907	44.673805
3502.080835	308362.998180	44.678810
3502.300372	308331.154501	44.683815
3502.043914	308306.841087	44.688820
3502.063306	308278.998380	44.693825
3501.921936	308257.568086	44.698829
3502.049747	308222.379495	44.703834
3502.060161	308208.127306	44.708839
3502.326325	308176.428959	44.713844
3501.772498	308148.929859	44.718849
3502.333947	308125.456099	44.723853
3502.446262	308095.944715	44.728858
3502.174305	308085.171902	44.733863
3502.612381	308043.089406	44.738868
3502.112890	308011.662788	44.743873
3502.265260	307982.348687	44.748877
3502.152384	307951.065452	44.753882
3502.012754	307934.011804	44.758887
3501.937515	307899.032717	44.763892
3501.934353	307891.857102	44.768897
3502.123994	307857.829241	44.773901
3501.903886	307826.282685	44.778906
3501.933774	307808.871790	44.783911
3502.593835	307772.353099	44.788916
3502.436038	307746.242690	44.793921
3501.999298	307708.902152	44.798925
3502.234093	307678.837050	44.803930
3502.064675	307657.639895	44.808935
3502.389843	307624.023402	44.813940
3502.439660	307607.779952	44.818945
3502.196143	307568.933247	44.823949
3502.281627	307536.346473	44.828954
3502.330549	307512.290527	44.833959
3502.366810	307478.642550	44.838964
3501.999223	307449.638082	44.843969
3501.829496	307419.457635	44.848973
3502.008629	307401.209028	44.853978
3501.710289	307381.227886	44.858983
3501.844809	307344.841561	44.863988
3501.645735	307334.947934	44.868993
3502.135749	307304.206684	44.873997
3502.209315	307284.981977	44.879002
3502.052915	307263.935319	44.884007
3502.359740	307227.725682	44.889012
3502.075782	307199.929577	44.894017
3502.066830	307169.418580	44.899021
3501.906903	307143.206393	44.904026
3501.800821	307121.032113	44.909031
3501.901240	307095.237460	44.914036
3501.688552	307081.146908	44.919041
3501.694521	307042.617249	44.924045
3502.108702	307023.008608	44.929050
3501.782417	307009.164749	44.934055
3501.874316	306978.587045	44.939060
3501.988831	306947.293245	44.944065
3502.015539	306933.623472	44.949069
3501.753399	306901.472109	44.954074
3501.838900	306887.182409	44.959079
3502.409952	306852.356504	44.964084
3501.875816	306838.723083	44.969089
3501.596160	306804.945675	44.974093
3501.933036	306780.208353	44.979098
3501.878424	306758.967503	44.984103
3501.928783	306734.656474	44.989108
3501.899427	306720.511843	44.994113
3502.184267	306694.230210	44.999117
3502.059545	306677.911825	45.004122
3501.737362	306648.009124	45.009127
3501.922124	306616.755085	45.014132
3501.536156	306596.583676	45.019137
3502.201528	306571.260712	45.024141
3502.103689	306555.294385	45.029146
3501.937892	306531.220484	45.034151
3501.671569	306502.199710	45.039156
3502.019077	306478.020459	45.044161
3502.050946	306438.315665	45.049165
3502.210179	306419.713516	45.054170
3501.922175	306402.631538	45.059175
3502.134537	306371.169461	45.064180
3502.004740	306351.034438	45.069185
3501.848058	306318.331867	45.074189
3501.722109	306300.104887	45.079194
3501.659525	306272.986389	45.084199
3502.081519	306252.587319	45.089204
3501.809637	306232.067177	45.094209
3501.679411	306198.825985	45.099213
3502.061246	306177.567872	45.104218
3501.702900	306156.272238	45.109223
3502.230577	306125.269920	45.114228
3502.006986	306104.182335	45.119233
3502.029203	306079.417289	45.124237
3502.063757	306045.692274	45.129242
3501.862968	306033.991782	45.134247
3501.682673	306005.746254	45.139252
3501.455050	305990.105333	45.144257
3501.568720	305970.975682	45.149261
3501.938026	305946.843683	45.154266
3501.842814	305932.607285	45.159271
3502.046986	305907.050370	45.164276
3501.633596	305880.622479	45.169281
3501.774595	305860.954103	45.174285
3501.532237	305831.140295	45.179290
3501.448850	305814.204420	45.184295
3501.691547	305800.627977	45.189300
3501.627385	305776.665147	45.194305
3501.606393	305758.014455	45.199309
3501.460631	305735.769395	45.204314
3501.504941	305725.303148	45.209319
3501.716037	305698.116306	45.214324
3501.552100	305685.162990	45.219329
3501.716116	305659.612201	45.224333
3501.477407	305645.194458	45.229338
3501.657285	305627.199588	45.234343
3501.752172	305595.882559	45.239348
3501.731844	305579.394880	45.244353
3501.814381	305550.955505	45.249357
3501.691757	305544.408928	45.254362
3501.865974	305517.660366	45.259367
3501.638959	305497.311090	45.264372
3501.938135	305467.667292	45.269377
3501.590715	305455.073311	45.274381
3501.932844	305422.445238	45.279386
3501.593579	305404.887365	45.284391
3501.662544	305375.661077	45.289396
3501.907677	305364.196431	45.294401
3501.806628	305347.670340	45.299405
3501.793897	305324.717268	45.304410
3501.683881	305306.920093	45.309415
3502.026609	305281.824842	45.314420
3501.961871	305258.141803	45.319425
3502.051077	305231.202725	45.324429
3502.177151	305212.579848	45.329434
3501.823024	305187.211250	45.334439
3501.893323	305157.933731	45.339444
3501.927382	305131.308577	45.344449
3501.946991	305103.031443	45.349453
3501.914817	305081.430109	45.354458
3501.737794	305061.480071	45.359463
3502.021543	305026.901224	45.364468
3501.877421	305006.615203	45.369473
3502.097729	304981.080765	45.374477
3502.017674	304953.989735	45.379482
3501.938501	304932.115707	45.384487
3502.077118	304896.261431	45.389492
3502.029818	304879.599577	45.394497
3502.116812	304854.467566	45.399501
3501.852404	304819.872082	45.404506
3501.562430	304812.842461	45.409511
3501.749023	304789.272793	45.414516
3501.542774	304767.545718	45.419521
3501.648718	304742.919695	45.424525
3501.609094	304723.126293	45.429530
3501.630642	304706.682717	45.434535
3501.812658	304675.682415	45.439540
3501.820140	304654.201979	45.444545
3501.888183	304637.293051	45.449549
3501.809483	304611.855860	45.454554
3501.657666	304599.103982	45.459559
3501.730341	304572.930624	45.464564
3501.728193	304548.015933	45.469569
3501.698856	304532.089213	45.474573
3501.525053	304511.807616	45.479578
3501.455281	304505.176333	45.484583
3501.783000	304468.197994	45.489588
3501.763096	304460.464606	45.494593
3501.481512	304431.419581	45.499597
3501.918344	304411.017472	45.504602
3501.632317	304393.476419	45.509607
3502.003056	304356.873054	45.514612
3501.630695	304341.788599	45.519617
3501.602141	304328.661175	45.524621
3501.604826	304299.317343	45.529626
3501.509653	304285.004133	45.534631
3501.970848	304263.885579	45.539636
3501.948469	304248.008590	45.544641
3501.666621	304220.363231	45.549645
3501.931657	304201.387516	45.554650
3501.884405	304175.029021	45.559655
3501.946526	304145.523154	45.564660
3501.847274	304128.894593	45.569665
3501.697762	304100.185131	45.574669
3501.754985	304077.856868	45.579674
3501.813582	304061.509122	45.584679
3501.921528	304033.752107	45.589684
3501.820194	304010.812240	45.594689
3501.491194	303985.820892	45.599693
3501.795324	303970.707409	45.604698
3501.642186	303955.359678	45.609703
3501.904726	303929.156451	45.614708
3501.726523	303912.438307	45.619713
3501.708462	303888.798277	45.624717
3502.018886	303871.571433	45.629722
3502.099740	303854.354857	45.634727
3502.283972	303816.304033	45.639732
3501.792854	303789.963514	45.644737
3501.826470	303776.444525	45.649741
3502.083536	303740.240168	45.654746
3502.010731	303730.071693	45.659751
3502.045210	303693.876491	45.664756
3501.915847	303675.496412	45.669761
3501.609902	303653.275382	45.674765
3501.808134	303631.739391	45.679770
3501.882300	303606.074320	45.684775
3502.387992	303573.648685	45.689780
3502.333139	303544.160680	45.694785
3502.179432	303522.094056	45.699789
3501.840236	303481.706670	45.704794
3501.534314	303464.677405	45.709799
3501.935184	303440.259375	45.714804
3501.513166	303430.221534	45.719809
3501.501155	303401.464840	45.724813
3501.670287	303380.518631	45.729818
3501.588887	303365.719470	45.734823
3501.856633	303317.755124	45.739828
3501.574524	303265.320688	45.744833
3500.856852	303152.662027	45.749837
3501.016491	302997.949697	45.754842
3500.315492	302807.434661	45.759847
3499.708588	302565.773911	45.764852
3498.949460	302290.769750	45.769857
3498.330314	301974.969966	45.774861
3497.769153	301613.907205	45.779866
3496.144207	301226.232785	45.784871
3495.215972	300799.811783	45.789876
3493.900454	300337.102646	45.794881
3492.472817	299843.788345	45.799885
3490.939549	299306.021077	45.804890
3489.118415	298750.502124	45.809895
3487.633369	298152.139327	45.814900
3486.017070	297534.395413	45.819905
3484.140899	296883.952294	45.824909
3482.420395	296213.725590	45.829914
3480.400659	295504.873227	45.834919
3478.352607	294770.664282	45.839924
3476.137622	294022.141292	45.844929
3473.675730	293240.352386	45.849933
3471.736041	292432.711442	45.854938
3468.965581	291605.791993	45.859943
3466.493088	290758.144955	45.864948
3463.722587	289898.313850	45.869953
3461.175690	289025.962601	45.874957
3458.738613	288110.331122	45.879962
3455.839796	287212.426053	45.884967
3452.950367	286277.517425	45.889972
3449.988070	285333.111339	45.894977
3447.416446	284380.612059	45.899981
3444.243466	283400.519713	45.904986
3441.214816	282421.587917	45.909991
3438.160892	281429.611534	45.914996
3435.169094	280428.675689	45.920001
3431.556067	279404.221591	45.925005
3428.394271	278382.280444	45.930010
3425.679789	277361.045508	45.935015
3422.331807	276322.556965	45.940020
3418.898920	275269.911723	45.945025
3415.483792	274217.657664	45.950029
3412.559824	273158.642969	45.955034
3409.330908	272094.544770	45.960039
3406.003105	271016.342781	45.965044
3402.560670	269945.937415	45.970049
3398.971247	268859.067781	45.975053
3395.735668	267769.558792	45.980058
3392.353722	266678.914491	45.985063
3388.664650	265581.532604	45.990068
3384.959059	264483.326679	45.995073
3381.770541	263395.316569	46.000077
3378.538035	262283.747353	46.005082
3374.431094	261161.735116	46.010087
3371.127599	260055.477345	46.015092
3367.431023	258957.444931	46.020097
3363.620899	257842.434653	46.025101
3360.541078	256727.988543	46.030106
3356.560291	255624.037995	46.035111
3353.058262	254506.481322	46.040116
3348.907406	253401.113497	46.045121
3345.382145	252286.726640	46.050125
3341.889850	251179.813897	46.055130
3338.114517	250067.869590	46.060135
3334.524378	248955.481622	46.065140
3330.815711	247856.169918	46.070145
3326.976664	246750.046619	46.075149
3323.712413	245648.258983	46.080154
3320.051155	244540.058347	46.085159
3316.509792	243435.526275	46.090164
3312.459290	242323.911580	46.095169
3308.796568	241220.865285	46.100173
3305.015759	240109.988480	46.105178
3301.141179	239018.528939	46.110183
3297.567428	237914.157064	46.115188
3294.011461	236816.222365	46.120193
3290.105493	235738.331838	46.125197
3286.416503	234640.819177	46.130202
3282.458923	233554.017147	46.135207
3278.923981	232462.613619	46.140212
3275.374583	231381.958285	46.145217
3271.591998	230305.743763	46.150221
3267.833273	229219.463963	46.155226
3263.620362	228150.725606	46.160231
3260.288215	227079.073384	46.165236
3256.654355	226002.475798	46.170241
3252.305442	224935.158273	46.175245
3249.135940	223858.590452	46.180250
3245.424309	222807.245473	46.185255
3241.708857	221735.806821	46.190260
3237.870245	220668.514435	46.195265
3233.861574	219621.599619	46.200269
3230.253411	218553.994300	46.205274
3226.380681	217517.962603	46.210279
3222.641715	216462.988927	46.215284
3218.994774	215418.496576	46.220289
3215.642885	214371.516072	46.225293
3212.018515	213324.886642	46.230298
3207.638039	212302.853435	46.235303
3204.198201	211266.618718	46.240308
3200.458188	210230.383578	46.245313
3196.415732	209204.819824	46.250317
3192.947293	208174.815953	46.255322
3188.892983	207153.261314	46.260327
3185.298890	206125.629386	46.265332
3181.648136	205119.964540	46.270337
3177.978310	204098.568779	46.275341
3174.708265	203081.216594	46.280346
3170.324184	202065.622483	46.285351
3166.315659	201057.234050	46.290356
3162.607422	200054.051235	46.295361
3158.763758	199063.960317	46.300365
3155.227813	198059.821236	46.305370
3151.368252	197079.194002	46.310375
3147.803924	196099.011430	46.315380
3144.483745	195113.373545	46.320385
3140.236423	194142.020828	46.325389
3136.711370	193154.315854	46.330394
3133.031406	192190.809587	46.335399
3129.123330	191203.638192	46.340404
3125.633496	190228.709615	46.345409
3121.276741	189271.520471	46.350413
3118.132935	188312.240900	46.355418
3114.040562	187358.057482	46.360423
3110.382526	186404.782672	46.365428
3106.662389	185447.808531	46.370433
3102.833846	184510.059979	46.375437
3099.391898	183564.977574	46.380442
3095.372222	182626.538359	46.385447
3091.323213	181686.839854	46.390452
3087.523577	180758.137448	46.395457
3083.751537	179838.861375	46.400461
3080.287106	178916.847935	46.405466
3076.139503	177998.209687	46.410471
3072.327838	177088.988049	46.415476
3068.805217	176185.383718	46.420481
3064.989162	175283.515394	46.425485
3061.178744	174378.371794	46.430490
3057.230150	173492.826447	46.435495
3053.639941	172592.621169	46.440500
3049.610642	171710.316751	46.445505
3045.648487	170831.500166	46.450509
3042.147796	169969.565374	46.455514
3038.159109	169103.210415	46.460519
3034.247862	168229.318025	46.465524
3030.858592	167373.137899	46.470529
3026.350875	166518.695250	46.475533
3022.854802	165674.403460	46.480538
3018.798577	164831.647680	46.485543
3015.392254	164001.453590	46.490548
3011.545472	163175.500669	46.495553
3007.408298	162356.705775	46.500557
3003.928061	161525.014585	46.505562
2999.791248	160712.808388	46.510567
2995.809087	159898.819478	46.515572
2992.336006	159091.571313	46.520577
2988.396490	158308.410348	46.525581
2984.768952	157522.194606	46.530586
2980.562713	156733.915646	46.535591
2976.568876	155954.561189	46.540596
2972.486863	155177.623482	46.545601
2968.706337	154410.741501	46.550605
2964.834445	153651.774416	46.555610
2960.792243	152914.987725	46.560615
2956.905927	152178.237376	46.565620
2953.337391	151441.523722	46.570625
2948.978663	150722.886253	46.575629
2945.263139	149997.566333	46.580634
2941.134836	149287.603660	46.585639
2937.229132	148585.225504	46.590644
2933.336644	147893.136502	46.595649
2929.386651	147212.645277	46.600653
2925.872522	146524.842033	46.605658
2921.798084	145860.306654	46.610663
2917.743987	145191.819468	46.615668
2914.123972	144524.762302	46.620673
2909.924554	143880.071325	46.625677
2906.264879	143237.811318	46.630682
2901.949936	142607.825553	46.635687
2898.185576	141976.833382	46.640692
2894.451994	141361.010944	46.645697
2890.157834	140742.204564	46.650701
2886.443562	140144.639872	46.655706
2882.728189	139545.072627	46.660711
2878.569986	138952.464932	46.665716
2875.204415	138365.364778	46.670721
2871.360661	137792.417492	46.675725
2867.423592	137210.484411	46.680730
2863.355376	136651.733437	46.685735
2859.617584	136081.373567	46.690740
2856.268679	135523.389586	46.695745
2852.366525	134980.128546	46.700749
2848.817298	134432.404786	46.705754
2845.244985	133854.427183	46.710759
2841.551807	133268.626940	46.715764
2838.070755	132716.321425	46.720769
2834.699311	132172.859559	46.725773
2830.856548	131637.835345	46.730778
2826.892107	131110.570795	46.735783
2822.812613	130581.308065	46.740788
2819.449258	130052.652774	46.745793
2815.923578	129537.347263	46.750797
2812.760591	129000.507590	46.755802
2809.016928	128491.710504	46.760807
2805.518042	127977.132235	46.765812
2801.895922	127457.771541	46.770817
2798.362279	126946.861938	46.775821
2794.956550	126425.534492	46.780826
2790.914612	125914.704105	46.785831
2787.670728	125414.376161	46.790836
2783.751773	124910.979771	46.795841
2780.300338	124400.699775	46.800845
2777.002816	123889.728238	46.805850
2773.293727	123391.443739	46.810855
2770.023379	122885.504537	46.815860
2766.518573	122370.273369	46.820865
2762.848581	121870.730154	46.825869
2759.319025	121358.301296	46.830874
2755.869085	120858.088188	46.835879
2752.284747	120364.172035	46.840884
2748.719772	119861.230078	46.845889
2744.974358	119367.987621	46.850893
2741.476564	118856.172006	46.855898
2737.916598	118359.264033	46.860903
2734.230415	117877.540160	46.865908
2731.065957	117375.929366	46.870913
2727.119191	116881.758750	46.875917
2723.958393	116368.716427	46.880922
2720.179824	115886.231449	46.885927
2716.593398	115400.429531	46.890932
2713.386709	114895.183968	46.895937
2709.389206	114415.397117	46.900941
2705.984035	113916.121241	46.905946
2702.293963	113436.439303	46.910951
2698.462423	112949.462070	46.915956
2695.243338	112469.617956	46.920961
2691.345332	111985.448600	46.925965
2688.099541	111493.187086	46.930970
2684.210457	111027.973474	46.935975
2680.318942	110553.866658	46.940980
2677.068486	110079.132476	46.945985
2673.106710	109611.965513	46.950989
2669.492452	109136.639601	46.955994
2665.735473	108677.424528	46.960999
2662.012215	108222.189450	46.966004
2658.318770	107763.968211	46.971009
2654.549315	107311.015225	46.976013
2650.872990	106867.511821	46.981018
2646.971985	106426.756864	46.986023
2643.362808	105975.271268	46.991028
2639.636294	105549.132240	46.996033
2635.564640	105104.213352	47.001037
2631.851154	104680.994274	47.006042
2628.353020	104267.839967	47.011047
2624.892113	103844.668419	47.016052
2621.026473	103429.814798	47.021057
2617.100494	103030.635756	47.026061
2613.695643	102612.199700	47.031066
2610.128177	102209.746220	47.036071
2606.436951	101809.884465	47.041076
2603.196095	101400.996656	47.046081
2599.232429	100991.006265	47.051085
2595.908539	100604.180965	47.056090
2592.260893	100201.980777	47.061095
2588.420294	99808.712474	47.066100
2585.021281	99401.323391	47.071105
2581.340912	99025.007095	47.076109
2578.187211	98621.631350	47.081114
2574.730360	98234.702702	47.086119
2571.297064	97844.229276	47.091124
2567.891972	97438.302295	47.096129
2564.361750	97055.123140	47.101133
2560.999480	96664.576965	47.106138
2557.370184	96267.811963	47.111143
2553.824421	95864.837372	47.116148
2550.384771	95477.380710	47.121153
2546.699972	95086.027567	47.126157
2543.605805	94692.414416	47.131162
2539.809575	94304.392490	47.136167
2536.272662	93902.598367	47.141172
2533.090199	93500.881401	47.146177
2529.440549	93105.900909	47.151181
2526.182360	92709.924284	47.156186
2522.659363	92319.013179	47.161191
2518.679384	91917.974821	47.166196
2515.701760	91524.091974	47.171201
2512.025564	91127.260762	47.176205
2508.990853	90723.549893	47.181210
2505.775831	90325.310640	47.186215
2502.171189	89921.241845	47.191220
2498.907962	89507.596203	47.196225
2495.056347	89093.984346	47.201229
2491.811148	88687.081172	47.206234
2487.739914	88283.081842	47.211239
2484.591571	87878.118604	47.216244
2481.297155	87464.048993	47.221249
2477.753317	87065.205943	47.226253
2474.250713	86650.024125	47.231258
2470.203808	86247.598977	47.236263
2467.237927	85830.858924	47.241268
2463.898884	85418.057593	47.246273
2460.120783	85010.767635	47.251277
2456.882105	84600.680951	47.256282
2453.039642	84188.661560	47.261287
2449.590796	83778.873394	47.266292
2446.600131	83360.242100	47.271297
2442.652249	82968.441622	47.276301
2439.089184	82538.263115	47.281306
2435.815138	82128.420716	47.286311
2432.003771	81721.030487	47.291316
2428.445274	81298.605772	47.296321
2425.149498	80895.250009	47.301325
2421.701217	80480.987713	47.306330
2418.464357	80055.534125	47.311335
2414.329745	79648.516504	47.316340
2411.225651	79227.779781	47.321345
2407.635012	78822.658297	47.326349
2404.187243	78394.976876	47.331354
2400.721186	77982.291479	47.336359
2397.257215	77575.974798	47.341364
2393.738604	77150.584448	47.346369
2390.313893	76738.051089	47.351373
2386.496975	76317.508028	47.356378
2383.025226	75902.086460	47.361383
2379.415294	75490.591461	47.366388
2376.409830	75075.110046	47.371393
2372.624813	74664.226379	47.376397
2369.375750	74230.115866	47.381402
2366.125573	73811.365050	47.386407
2362.343811	73392.640045	47.391412
2358.867959	72963.728247	47.396417
2355.113240	72545.012400	47.401421
2351.827629	72129.049065	47.406426
2348.433782	71709.655416	47.411431
2344.788684	71291.678864	47.416436
2341.223839	70865.646531	47.421441
2337.713895	70450.576348	47.426445
2334.135148	70020.065276	47.431450
2330.890626	69600.314005	47.436455
2327.422435	69183.689526	47.441460
2324.257485	68760.359134	47.446465
2320.296129	68339.730538	47.451469
2316.887553	67907.088893	47.456474
2313.409023	67480.844878	47.461479
2309.800536	67059.960179	47.466484
2306.669454	66629.785203	47.471489
2302.614278	66199.247173	47.476493
2299.339304	65770.321489	47.481498
2296.007350	65351.345276	47.486503
2292.495444	64915.825467	47.491508
2288.951572	64491.438044	47.496513
2285.420309	64058.449497	47.501517
2282.143930	63635.094864	47.506522
2278.582773	63201.414972	47.511527
2275.130994	62772.948802	47.516532
2271.630841	62336.380483	47.521537
2267.868826	61914.406345	47.526541
2264.139051	61478.415646	47.531546
2260.609112	61045.866525	47.536551
2257.069194	60623.429362	47.541556
2253.830783	60191.909698	47.546561
2250.246922	59765.223418	47.551565
2246.938584	59338.901502	47.556570
2243.666212	58909.725972	47.561575
2239.990453	58482.886128	47.566580
2236.654840	58042.510761	47.571585
2232.898256	57616.250850	47.576589
2229.261805	57175.830272	47.581594
2225.559520	56750.985866	47.586599
2222.343620	56314.988854	47.591604
2218.983924	55873.527643	47.596609
2215.558253	55456.587788	47.601613
2212.172076	55013.687393	47.606618
2208.695449	54575.313865	47.611623
2204.801121	54146.809024	47.616628
2201.192006	53713.496785	47.621633
2197.499720	53269.744165	47.626637
2194.173562	52838.840140	47.631642
2190.981448	52412.275036	47.636647
2187.520203	51972.964409	47.641652
2183.987257	51536.261406	47.646657
2180.193489	51102.759901	47.651661
2176.836789	50669.376107	47.656666
2173.587826	50233.091176	47.661671
2169.883573	49801.338208	47.666676
2166.816943	49350.078310	47.671681
2162.871463	48917.631043	47.676685
2159.343713	48471.020739	47.681690
2155.755726	48037.931941	47.686695
2152.145462	47609.649768	47.691700
2148.952699	47171.930359	47.696705
2145.502909	46741.159764	47.701709
2141.677808	46296.858311	47.706714
2138.485095	45863.730572	47.711719
2135.168174	45431.600816	47.716724
2131.491187	44984.093291	47.721729
2127.967568	44549.032125	47.726733
2124.511201	44111.806533	47.731738
2120.949807	43660.661218	47.736743
2117.506390	43216.431342	47.741748
2113.864102	42772.596434	47.746753
2110.449635	42335.741776	47.751757
2107.024089	41891.263115	47.756762
2103.599600	41449.995348	47.761767
2099.764894	41018.793094	47.766772
2096.255573	40568.020042	47.771777
2092.584990	40138.686405	47.776781
2089.313867	39693.721151	47.781786
2085.782822	39259.482178	47.786791
2082.058894	38819.366747	47.791796
2078.935587	38378.596221	47.796801
2074.977662	37943.042704	47.801805
2071.478171	37500.402416	47.806810
2068.094262	37060.301730	47.811815
2064.433710	36620.665205	47.816820
2061.072985	36173.884849	47.821825
2057.123373	35747.148169	47.826829
2053.993391	35307.994987	47.831834
2050.714777	34873.723209	47.836839
2047.204094	34445.702017	47.841844
2043.759475	34000.939158	47.846849
2039.854656	33570.696193	47.851853
2036.687263	33125.053032	47.856858
2033.007528	32685.571016	47.861863
2029.266826	32255.519664	47.866868
2025.491018	31811.773829	47.871873
2021.946736	31376.069363	47.876877
2018.833086	30937.055831	47.881882
2015.260275	30500.607350	47.886887
2012.204792	30072.852110	47.891892
2008.882907	29625.210362	47.896897
2005.089639	29203.773105	47.901901
2001.646386	28757.823117	47.906906
1998.126761	28326.988977	47.911911
1994.274825	27883.396570	47.916916
1991.159358	27438.976835	47.921921
1987.363700	27004.836233	47.926925
1983.981145	26570.691319	47.931930
1980.390511	26130.929945	47.936935
1976.438164	25691.367495	47.941940
1973.051540	25249.293626	47.946945
1969.565810	24821.905711	47.951949
1966.239429	24393.000568	47.956954
1962.598637	23951.146906	47.961959
1958.914337	23510.697217	47.966964
1955.895214	23074.867087	47.971969
1951.864848	22641.649204	47.976973
1948.521992	22209.942838	47.981978
1944.788500	21791.337237	47.986983
1941.464097	21349.827923	47.991988
1937.849949	20918.008301	47.996993
1934.290901	20494.354524	48.001997
1930.937800	20057.781435	48.007002
1927.329770	19627.123073	48.012007
1923.617270	19205.047567	48.017012
1920.247923	18772.768422	48.022017
1916.561345	18345.893830	48.027021
1912.986071	17926.484816	48.032026
1909.415294	17496.919147	48.037031
1905.513208	17078.443870	48.042036
1902.138891	16652.859482	48.047041
1898.638717	16231.012017	48.052045
1895.352948	15809.564737	48.057050
1891.613416	15393.453445	48.062055
1887.974908	14975.901159	48.067060
1884.542047	14553.304415	48.072065
1880.853022	14153.068572	48.077069
1877.480947	13730.816225	48.082074
1873.604578	13322.401625	48.087079
1870.113718	12899.872828	48.092084
1866.752814	12480.340798	48.097089
1863.001759	12079.316295	48.102093
1859.665215	11665.430523	48.107098
1856.109709	11259.296272	48.112103
1852.014170	10856.784474	48.117108
1848.628733	10449.739107	48.122113
1844.980349	10043.208848	48.127117
1841.202460	9651.698783	48.132122
1837.965556	9257.032916	48.137127
1834.179825	8862.441856	48.142132
1830.419101	8469.494857	48.147137
1825.869627	8091.263745	48.152141
1822.299567	7722.864148	48.157146
1817.945380	7356.521420	48.162151
1813.940590	7003.531855	48.167156
1810.452390	6659.257476	48.172161
1806.371514	6315.069140	48.177165
1802.432649	5961.408937	48.182170
1798.674484	5630.807441	48.187175
1795.048019	5299.204072	48.192180
1791.509168	4975.127928	48.197185
1787.538236	4656.786111	48.202189
1783.888848	4345.915409	48.207194
1780.412904	4021.928749	48.212199
1776.295681	3730.067706	48.217204
1772.947671	3421.795529	48.222209
1769.197486	3137.395805	48.227213
1765.348701	2837.451242	48.232218
1761.825025	2538.638135	48.237223
1757.885912	2266.906486	48.242228
1754.000135	1986.880853	48.247233
1750.212045	1723.205408	48.252237
1745.590768	1468.557388	48.257242
1741.359606	1229.956572	48.262247
1736.439524	1025.616987	48.267252
1732.039110	818.746892	48.272257
1727.562518	636.806002	48.277261
1723.258391	464.869293	48.282266
1719.387802	298.156554	48.287271
1714.665552	156.906653	48.292276
1710.335231	31.421685	48.297281
1702.681192	-6.300218	48.302285
1692.807800	62.452617	48.307290
1688.252131	66.347758	48.312295
1685.164033	74.734730	48.317300
1683.419514	73.791629	48.322305
1681.241374	71.191799	48.327309
1679.115734	76.954957	48.332314
1676.434566	69.295565	48.337319
1673.122874	74.120208	48.342324
1669.609230	65.596985	48.347329
1666.184765	75.184734	48.352333
1662.766834	71.816103	48.357338
1659.566861	72.899681	48.362343
1656.044320	71.815708	48.367348
1652.957333	68.553756	48.372353
1649.723443	67.715918	48.377357
1646.410479	78.959913	48.382362
1642.835101	71.993350	48.387367
1639.267635	77.000172	48.392372
1636.137403	71.213989	48.397377
1632.390663	66.147014	48.402381
1628.984901	63.763570	48.407386
1625.932600	70.196129	48.412391
1622.203719	74.747191	48.417396
1619.058881	70.146510	48.422401
1615.775508	70.743206	48.427405
1612.073761	67.222607	48.432410
1608.868083	64.842825	48.437415
1604.496471	76.548978	48.442420
1601.452707	70.515228	48.447425
1598.216751	67.194212	48.452429
1594.729720	70.663611	48.457434
1591.645424	65.566301	48.462439
1588.075905	71.244148	48.467444
1584.940038	73.080205	48.472449
1581.178707	77.424353	48.477453
1577.207712	78.007856	48.482458
1573.900739	70.926764	48.487463
1570.563919	71.772224	48.492468
1566.932456	72.809075	48.497473
1563.473930	70.892586	48.502477
1560.140347	71.218697	48.507482
1556.931190	67.456924	48.512487
1553.519710	82.006500	48.517492
1550.341325	65.316223	48.522497
1546.312635	68.790840	48.527501
1542.602549	64.970997	48.532506
1539.320784	66.927840	48.537511
1535.720634	70.832458	48.542516
1532.481053	65.572667	48.547521
1528.894504	76.656765	48.552525
1525.500980	72.205531	48.557530
1522.093877	66.930687	48.562535
1518.650647	73.949271	48.567540
1515.235128	69.741904	48.572545
1511.809531	67.219194	48.577549
1507.908473	65.849309	48.582554
1504.786750	70.770939	48.587559
1501.062246	69.186917	48.592564
1497.686609	70.493997	48.597569
1493.707249	66.371230	48.602573
1490.525843	71.390734	48.607578
1487.679794	72.979212	48.612583
1483.807619	72.221755	48.617588
1480.145310	71.877715	48.622593
1476.600597	66.776153	48.627597
1473.142116	73.401650	48.632602
1469.847836	63.702224	48.637607
1466.331497	71.336454	48.642612
1462.353613	75.407437	48.647617
1459.140214	62.420997	48.652621
1455.910436	72.354924	48.657626
1452.415719	56.663024	48.662631
1448.745216	69.930480	48.667636
1445.541341	67.265701	48.672641
1441.852927	72.965225	48.677645
1438.291435	73.791884	48.682650
1434.985059	63.043999	48.687655
1431.084420	66.324691	48.692660
1427.979376	65.261180	48.697665
1424.695584	64.538697	48.702669
1421.036648	65.159066	48.707674
1417.431259	71.127236	48.712679
1413.777126	76.223488	48.717684
1410.621293	67.543377	48.722689
1406.795441	66.440204	48.727693
1403.043144	76.458627	48.732698
1400.132381	67.778336	48.737703
1396.520876	78.072233	48.742708
1392.982902	65.819683	48.747713
1389.424259	67.386207	48.752717
1385.902432	70.161860	48.757722
1382.538912	68.705159	48.762727
1378.942689	66.326080	48.767732
1374.994867	70.645485	48.772737
1371.540298	65.074336	48.777741
1368.535852	74.065212	48.782746
1365.290175	67.670626	48.787751
1361.370881	66.847753	48.792756
1357.805345	65.153585	48.797761
1354.243539	69.080720	48.802765
1350.945838	64.842383	48.807770
1347.828478	57.143371	48.812775
1343.766082	72.012544	48.817780
1340.632835	72.987687	48.822785
1337.513874	67.509835	48.827789
1333.547778	70.674176	48.832794
1330.339242	74.869023	48.837799
1326.477309	71.623328	48.842804
1323.029080	68.389168	48.847809
1319.469667	69.164896	48.852813
1315.732884	62.128603	48.857818
1312.415566	58.206531	48.862823
1308.998619	61.959263	48.867828
1305.533624	63.916171	48.872833
1301.988080	61.304592	48.877837
1298.730060	62.704111	48.882842
1295.321434	61.925144	48.887847
1291.612973	75.537026	48.892852
1287.743772	67.996174	48.897857
1284.452855	67.002737	48.902861
1281.045604	69.127826	48.907866
1277.628989	62.035377	48.912871
1274.191906	68.366491	48.917876
1270.600759	67.397641	48.922881
1266.663241	61.313236	48.927885
1263.304188	66.480621	48.932890
1259.984851	53.618285	48.937895
1256.211606	73.333514	48.942900
1253.458768	68.918632	48.947905
1249.923316	69.073717	48.952909
1246.050353	73.653558	48.957914
1242.717138	65.801501	48.962919
1239.054078	70.354997	48.967924
1235.524281	67.035472	48.972929
1231.702754	75.887782	48.977933
1228.276976	71.938309	48.982938
1225.162770	72.454926	48.987943
1221.712581	59.717362	48.992948
1218.005634	63.467786	48.997953
1214.447424	61.168231	49.002957
1210.967644	63.959499	49.007962
1207.491132	63.352456	49.012967
1203.708577	71.686182	49.017972
1200.505216	67.436343	49.022977
1196.642983	74.001316	49.027981
1193.416275	67.907517	49.032986
1190.363682	63.624723	49.037991
1186.460117	66.940692	49.042996
1183.154087	61.030084	49.048001
1179.431017	67.358263	49.053005
1175.803764	71.169051	49.058010
1173.000083	70.077639	49.063015
1169.236730	58.110156	49.068020
1165.489588	62.180045	49.073025
1162.233657	59.431657	49.078029
1158.649575	59.050168	49.083034
1155.171107	68.883604	49.088039
1151.447615	66.723677	49.093044
1147.862640	68.939715	49.098049
1144.159347	66.767153	49.103053
1140.592827	70.290086	49.108058
1137.177327	68.256223	49.113063
1134.036936	69.567846	49.118068
1130.816067	69.740414	49.123073
1127.449784	65.360926	49.128077
1123.437399	63.559176	49.133082
1120.069198	59.809563	49.138087
1116.421143	68.084391	49.143092
1113.146843	66.117135	49.148097
1109.552691	63.449873	49.153101
1105.679898	63.091184	49.158106
1102.412683	61.534106	49.163111
1098.883779	73.665905	49.168116
1095.488275	65.386981	49.173121
1092.302517	62.111998	49.178125
1088.777346	74.458347	49.183130
1085.000879	62.942164	49.188135
1081.544078	57.830144	49.193140
1077.681436	63.680192	49.198145
1074.742165	65.216773	49.203149
1070.589005	67.603517	49.208154
1067.495420	66.193418	49.213159
1064.059843	70.547007	49.218164
1060.474908	64.116695	49.223169
1057.072417	62.473114	49.228173
1053.551718	66.665950	49.233178
1050.191237	53.674025	49.238183
1046.316324	56.802052	49.243188
1042.815000	70.046336	49.248193
1039.417102	64.121577	49.253197
1036.055492	64.205334	49.258202
1032.590051	52.602791	49.263207
1028.856851	57.103945	49.268212
1025.488729	61.076883	49.273217
1021.827191	61.340203	49.278221
1018.117114	57.928553	49.283226
1014.536994	64.620459	49.288231
1011.403125	63.147037	49.293236
1008.569636	70.592736	49.298241
1004.712590	57.251017	49.303245
1000.766204	63.664587	49.308250
997.215092	62.958453	49.313255
993.260829	69.468161	49.318260
990.030572	61.413466	49.323265
987.357751	72.709669	49.328269
983.457248	64.759305	49.333274
979.868686	67.577017	49.338279
976.490413	64.170669	49.343284
973.045139	57.810382	49.348289
969.665308	54.299878	49.353293
966.183493	58.328482	49.358298
962.111119	57.029629	49.363303
958.878302	60.693615	49.368308
955.498074	57.157865	49.373313
952.156039	55.359358	49.378317
948.572386	53.778793	49.383322
944.801592	55.542896	49.388327
941.283012	65.863459	49.393332
937.603996	57.157311	49.398337
934.731211	58.209002	49.403341
930.895133	58.758925	49.408346
927.417957	54.412550	49.413351
924.008367	54.636663	49.418356
920.155956	52.923935	49.423361
916.866494	54.875700	49.428365
913.410153	59.330603	49.433370
909.831208	65.221922	49.438375
906.237580	60.966441	49.443380
902.800171	56.357621	49.448385
899.373301	61.380564	49.453389
895.855334	72.488794	49.458394
892.527254	68.021137	49.463399
888.724327	61.178712	49.468404
885.357613	63.556948	49.473409
881.780206	61.336355	49.478413
878.299520	70.445663	49.483418
874.867160	59.277751	49.488423
871.275576	53.474920	49.493428
867.893725	63.878603	49.498433
864.150579	62.044472	49.503437
860.465383	66.361003	49.508442
857.001720	62.407994	49.513447
853.540538	57.056254	49.518452
850.537413	52.386167	49.523457
847.402234	53.456566	49.528461
843.450679	68.172444	49.533466
840.134291	52.392830	49.538471
836.458866	51.832615	49.543476
832.529767	55.661944	49.548481
829.363175	56.803672	49.553485
825.337210	56.513156	49.558490
822.278790	59.476142	49.563495
818.834613	62.660525	49.568500
815.249456	58.065227	49.573505
812.179497	55.987109	49.578509
808.208663	62.407663	49.583514
804.712053	59.826500	49.588519
800.996007	64.717301	49.593524
797.775536	62.210208	49.598529
794.118185	58.489836	49.603533
790.781804	63.229789	49.608538
787.234828	48.302316	49.613543
783.617329	60.862344	49.618548
780.215306	59.006760	49.623553
776.783895	63.078153	49.628557
773.353908	56.237807	49.633562
769.901111	50.783540	49.638567
766.427920	56.525530	49.643572
762.428343	65.405575	49.648577
759.306700	59.377750	49.653581
755.658371	63.131745	49.658586
752.424402	53.340816	49.663591
748.886970	61.588948	49.668596
745.166508	60.159418	49.673601
741.749521	49.498501	49.678605
737.983955	57.171556	49.683610
734.683112	45.227093	49.688615
731.192244	57.840171	49.693620
727.412545	52.417818	49.698625
724.473098	47.294925	49.703629
720.730610	56.384877	49.708634
717.078711	51.034378	49.713639
713.343656	57.589073	49.718644
709.787089	52.540102	49.723649
706.739712	55.453923	49.728653
703.159011	53.711585	49.733658
699.887667	47.627986	49.738663
696.634822	49.849311	49.743668
693.255498	54.194169	49.748673
689.669969	56.995618	49.753677
685.497668	62.311787	49.758682
682.354357	48.226312	49.763687
678.099016	57.237921	49.768692
674.704852	57.889921	49.773697
671.516513	49.844583	49.778701
667.764636	55.595163	49.783706
664.937171	56.791680	49.788711
661.203399	56.275372	49.793716
657.606101	66.120994	49.798721
654.426726	52.746636	49.803725
650.676433	63.286772	49.808730
647.188644	59.334389	49.813735
643.466230	60.432951	49.818740
639.986905	60.028892	49.823745
636.988274	56.655242	49.828749
632.901691	62.277603	49.833754
629.498522	55.369834	49.838759
625.966542	55.774383	49.843764
622.754644	50.801482	49.848769
619.274721	51.027089	49.853773
615.396578	50.106168	49.858778
612.517032	54.120136	49.863783
608.408945	65.892860	49.868788
604.926071	60.044679	49.873793
601.534071	60.582459	49.878797
597.944421	57.718425	49.883802
595.145156	57.844401	49.888807
591.244450	54.807336	49.893812
587.741553	59.494136	49.898817
584.227999	52.492833	49.903821
580.308864	61.360366	49.908826
576.765522	64.727885	49.913831
573.162175	59.395161	49.918836
569.703806	61.695950	49.923841
566.224224	57.289898	49.928845
562.467706	68.115740	49.933850
559.926407	52.705904	49.938855
556.248557	55.907708	49.943860
552.885671	56.010703	49.948865
549.258624	51.418810	49.953869
545.282466	58.722878	49.958874
541.887861	62.421577	49.963879
538.372638	64.898895	49.968884
534.957413	58.464407	49.973889
532.004111	62.654376	49.978893
528.155448	66.822386	49.983898
524.652207	65.820967	49.988903
521.127500	64.224958	49.993908
517.535330	66.945206	49.998913
514.330733	64.856449	50.003917
509.961454	62.088491	50.008922
506.658513	61.486152	50.013927
503.494933	72.105800	50.018932
500.153512	67.621301	50.023937
496.747250	62.210452	50.028941
492.981823	68.975536	50.033946
489.456509	63.700277	50.038951
486.028574	60.295408	50.043956
482.483659	62.869101	50.048961
479.018786	63.712462	50.053965
475.157328	64.143014	50.058970
471.790208	60.206674	50.063975
468.299606	64.515095	50.068980
464.996488	59.638673	50.073985
461.859006	53.572239	50.078989
458.083890	62.126302	50.083994
454.695677	52.593560	50.088999
451.138737	58.199921	50.094004
447.444404	57.781905	50.099009
443.788550	55.345807	50.104013
440.095030	55.940039	50.109018
436.723086	50.381498	50.114023
433.115912	59.953426	50.119028
429.245140	55.016693	50.124033
426.671695	45.217916	50.129037
422.812745	55.575664	50.134042
419.599533	49.074951	50.139047
416.268155	50.770709	50.144052
412.392654	63.260185	50.149057
409.041511	49.067930	50.154061
405.293427	55.219729	50.159066
401.844887	48.458272	50.164071
398.137401	58.140728	50.169076
394.755541	56.658537	50.174081
391.706281	44.643349	50.179085
388.031153	53.169193	50.184090
384.397951	49.533715	50.189095
380.759991	46.310255	50.194100
377.152542	53.534789	50.199105
374.274131	47.810842	50.204109
370.333674	50.911185	50.209114
366.844313	52.460706	50.214119
363.209007	49.303272	50.219124
359.909357	54.122960	50.224129
356.582774	51.686234	50.229133
352.549055	52.738390	50.234138
349.413305	56.244952	50.239143
345.882452	47.420957	50.244148
342.144579	45.222267	50.249153
338.810737	50.170662	50.254157
334.914053	46.418030	50.259162
331.989800	47.901722	50.264167
328.398350	55.636283	50.269172
325.027525	53.601907	50.274177
322.065557	42.737374	50.279181
317.613155	54.275819	50.284186
314.243263	40.222552	50.289191
310.288308	41.860384	50.294196
306.821886	51.214256	50.299201
303.653893	44.845727	50.304205
300.291221	47.761216	50.309210
297.048128	42.527481	50.314215
293.634462	45.849530	50.319220
289.899931	52.059339	50.324225
286.147392	48.252638	50.329229
282.659017	48.887718	50.334234
279.526409	46.623279	50.339239
275.970680	49.480245	50.344244
272.004432	47.544905	50.349249
269.022947	50.904074	50.354253
265.042326	47.930128	50.359258
261.830350	49.275130	50.364263
258.151130	48.506788	50.369268
254.512412	58.567677	50.374273
251.200146	45.887971	50.379277
247.369614	49.024998	50.384282
244.131645	52.474719	50.389287
241.222541	49.558575	50.394292
237.391046	61.237637	50.399297
233.508849	60.671736	50.404301
230.043295	50.606935	50.409306
226.644123	53.686299	50.414311
223.376110	48.775984	50.419316
219.658539	53.803115	50.424321
216.336908	40.425710	50.429325
212.560111	46.306757	50.434330
208.933606	47.159499	50.439335
205.890303	38.250143	50.444340
201.913419	45.187367	50.449345
199.018444	35.236223	50.454349
195.660750	55.405536	50.459354
191.762725	47.581511	50.464359
188.197252	50.576041	50.469364
184.260731	58.649068	50.474369
180.777939	51.538656	50.479373
177.753461	50.934136	50.484378
174.406070	48.864499	50.489383
171.150951	51.041944	50.494388
167.242597	56.484750	50.499393
163.456006	50.582704	50.504397
159.949223	50.989720	50.509402
156.561432	51.561702	50.514407
152.799682	40.606598	50.519412
149.169675	41.671858	50.524417
146.461183	41.059274	50.529421
142.805693	48.041376	50.534426
139.353673	49.332020	50.539431
135.913779	48.596036	50.544436
131.711578	51.914327	50.549441
128.688906	42.141258	50.554445
124.990403	62.211782	50.559450
121.648039	57.265604	50.564455
118.244730	42.569040	50.569460
114.598981	45.721605	50.574465
111.317986	46.716714	50.579469
107.400387	48.374070	50.584474
103.930261	52.157335	50.589479
100.346492	55.262289	50.594484
96.551189	59.520114	50.599489
93.641590	51.915529	50.604493
90.233578	58.979328	50.609498
86.938047	51.248177	50.614503
83.328742	51.127017	50.619508
79.635454	60.130263	50.624513
76.077748	50.193737	50.629517
72.531358	53.368803	50.634522
69.128850	52.525771	50.639527
65.805419	54.115933	50.644532
62.252235	56.023433	50.649537
58.702161	43.260583	50.654541
54.913633	57.691670	50.659546
51.272543	52.614852	50.664551
47.802794	49.067877	50.669556
44.676916	56.337681	50.674561
40.785029	51.733334	50.679565
37.610035	48.925056	50.684570
34.097969	54.568760	50.689575
29.979140	52.125726	50.694580
26.413136	57.179899	50.699585
23.403980	38.027680	50.704589
20.098575	45.670270	50.709594
16.917423	45.776678	50.714599
13.595298	42.254182	50.719604
9.750235	54.201112	50.724609
6.219399	47.354475	50.729613
2.385305	49.878340	50.734618